Thu Aug 25 09:49:54 2022

Number of Points = 9923

Depth (nm)	Load (N)	Time (s)
2.875342	104.456023	0.000000
2.470927	103.130626	0.005005
2.447968	105.273063	0.010010
2.633275	101.090132	0.015014
2.809930	103.058922	0.020019
2.507825	88.815651	0.025024
2.084523	92.887437	0.030029
2.239850	83.476337	0.035034
1.936828	81.575068	0.040038
1.693171	70.090948	0.045043
1.506955	58.230840	0.050048
1.033441	58.732272	0.055053
1.043646	45.794191	0.060058
0.745359	35.929006	0.065062
0.514316	33.744382	0.070067
0.519347	26.008342	0.075072
0.070657	20.823780	0.080077
0.115599	12.818901	0.085082
0.136039	7.715862	0.090086
-0.588980	-4.679878	0.095091
-1.240525	-7.915414	0.100096
-1.532507	-2.722112	0.105101
-1.505230	-15.068039	0.110106
-2.182331	-18.217312	0.115110
-2.577955	-25.738692	0.120115
-2.253576	-21.603750	0.125120
-3.695797	-27.217918	0.130125
-4.065173	-13.467214	0.135130
-3.835056	-18.296216	0.140134
-4.191454	-16.348321	0.145139
-4.126338	-23.533770	0.150144
-4.458822	-8.732151	0.155149
-4.357234	-17.672870	0.160154
-3.910408	-13.993709	0.165158
-4.453517	-27.373386	0.170163
-4.907317	-17.810911	0.175168
-5.256126	-11.953812	0.180173
-5.550986	-16.431640	0.185178
-6.480928	-11.758476	0.190182
-7.181216	-11.813134	0.195187
-6.890010	-14.892664	0.200192
-7.079852	-13.265094	0.205197
-7.142460	-21.022152	0.210202
-7.222508	-17.057958	0.215206
-7.317699	-18.615293	0.220211
-7.083007	-21.236716	0.225216
-7.976565	-8.267579	0.230221
-8.631384	-12.622568	0.235226
-8.569182	-17.842874	0.240230
-8.950790	-8.769432	0.245235
-8.596380	-20.761651	0.250240
-9.288759	-8.529552	0.255245
-9.843960	-14.633883	0.260250
-9.750993	-15.344343	0.265254
-10.445302	-8.465001	0.270259
-10.003707	-10.647445	0.275264
-10.174832	-8.709596	0.280269
-10.233620	-14.028005	0.285274
-11.213013	-16.329484	0.290278
-11.619743	-11.247919	0.295283
-11.401358	-17.505097	0.300288
-11.770103	-14.634616	0.305293
-12.377350	-21.910868	0.310298
-12.754772	-15.191912	0.315302
-13.012632	-8.953594	0.320307
-12.662010	-18.743252	0.325312
-13.206056	-14.333033	0.330317
-13.335125	-18.242052	0.335322
-12.881244	-20.565625	0.340326
-13.603389	-17.813778	0.345331
-13.765343	-20.274975	0.350336
-14.464082	-9.221957	0.355341
-14.495226	-18.366504	0.360346
-14.607395	-18.766411	0.365350
-15.179906	-13.804404	0.370355
-15.559432	-23.878286	0.375360
-15.845785	-16.822424	0.380365
-16.077571	-9.335349	0.385370
-16.376220	-16.707411	0.390374
-16.122673	-13.750938	0.395379
-16.037576	-27.671969	0.400384
-16.763926	-25.704073	0.405389
-17.048296	-15.535396	0.410394
-17.072113	-22.178564	0.415398
-17.439311	-17.878313	0.420403
-17.681778	-29.549213	0.425408
-18.058787	-8.413128	0.430413
-18.369695	-17.203792	0.435418
-18.673774	-19.497188	0.440422
-18.889462	-16.539958	0.445427
-18.847439	-18.071337	0.450432
-19.294548	-7.674676	0.455437
-19.867123	-22.283600	0.460442
-19.912384	-17.556066	0.465446
-20.533551	-10.662876	0.470451
-20.383802	-14.311862	0.475456
-20.482452	-6.364757	0.480461
-20.455403	-16.113207	0.485466
-20.679879	-17.874911	0.490470
-21.380785	-17.233447	0.495475
-21.495001	-24.893831	0.500480
-22.066883	-8.071034	0.505485
-22.109203	-16.514641	0.510490
-22.135072	-13.479586	0.515494
-22.799194	-6.851746	0.520499
-22.666281	-17.141966	0.525504
-23.538484	-10.073399	0.530509
-23.316711	-13.483735	0.535514
-23.402744	-5.253869	0.540518
-23.792491	-3.215325	0.545523
-24.087422	-13.710591	0.550528
-24.480766	-5.119362	0.555533
-24.859058	-3.259783	0.560538
-24.661353	-8.276697	0.565542
-24.845607	-4.068383	0.570547
-24.903186	-8.365091	0.575552
-26.042920	8.075297	0.580557
-26.405420	-10.707901	0.585562
-26.145739	-15.329564	0.590566
-26.550208	-8.277338	0.595571
-26.326787	-12.845864	0.600576
-26.309911	-5.037082	0.605581
-26.944775	-3.083518	0.610586
-27.512617	-9.530717	0.615590
-28.116050	-4.396183	0.620595
-27.902512	-8.713225	0.625600
-28.058415	-8.887982	0.630605
-27.991625	-14.504476	0.635610
-28.715874	-2.713468	0.640614
-29.524016	0.206881	0.645619
-29.344069	-7.037694	0.650624
-29.397457	0.655550	0.655629
-29.296114	-10.180219	0.660634
-29.598835	-10.866644	0.665638
-30.013876	-4.309468	0.670643
-29.994371	-8.191148	0.675648
-30.711611	-10.188853	0.680653
-30.677769	-9.298683	0.685658
-30.788611	-7.617052	0.690662
-31.392278	-4.994498	0.695667
-32.063100	-9.128679	0.700672
-32.359965	-8.012684	0.705677
-32.391794	-13.635873	0.710682
-32.373651	-12.436360	0.715686
-32.512013	-6.308514	0.720691
-32.576342	-11.676675	0.725696
-32.640635	-5.756587	0.730701
-32.820503	-5.158797	0.735706
-33.251415	-5.008889	0.740710
-33.937284	-7.764482	0.745715
-33.913541	-18.407752	0.750720
-34.500175	-13.171449	0.755725
-34.859685	-7.031099	0.760730
-35.221770	-13.747816	0.765734
-35.591659	-11.500414	0.770739
-35.363545	-16.256335	0.775744
-35.374323	-10.597735	0.780749
-35.445699	-20.523748	0.785754
-35.879646	-23.081530	0.790758
-36.589815	-12.593034	0.795763
-36.291900	-19.530223	0.800768
-37.130873	-9.768187	0.805773
-37.222778	-17.438397	0.810778
-37.722797	-11.329816	0.815782
-38.117622	-8.724166	0.820787
-38.094790	-11.328212	0.825792
-38.390132	-5.093512	0.830797
-38.405948	-21.301942	0.835802
-38.651280	-16.897400	0.840806
-38.792774	-5.567864	0.845811
-38.919340	-17.661889	0.850816
-39.002251	-13.520077	0.855821
-39.373403	-15.163885	0.860826
-39.551804	-6.340582	0.865830
-39.990182	-6.448930	0.870835
-40.577660	-9.349653	0.875840
-41.154627	-14.188234	0.880845
-41.319951	-13.507302	0.885850
-41.277771	-14.504032	0.890854
-41.738420	-11.223682	0.895859
-41.345426	-10.889660	0.900864
-41.436031	-11.938350	0.905869
-41.638783	-10.147406	0.910874
-42.289885	-14.632686	0.915878
-42.949504	-12.798629	0.920883
-43.112201	-14.582667	0.925888
-42.842386	-6.930579	0.930893
-43.273684	-3.604206	0.935898
-43.760510	-20.849310	0.940902
-44.572475	-11.015577	0.945907
-44.055363	-21.609600	0.950912
-44.149506	-14.292791	0.955917
-44.576125	-9.385279	0.960922
-44.202374	-17.527084	0.965926
-45.259593	-17.753601	0.970931
-45.685355	-25.273418	0.975936
-46.069180	-14.193818	0.980941
-46.086627	-15.133749	0.985946
-45.633944	-11.784537	0.990950
-46.492142	-16.443011	0.995955
-46.353826	-21.276609	1.000960
-46.794821	-16.120074	1.005965
-46.959985	-10.174692	1.010970
-46.994636	-14.221891	1.015974
-47.482550	-16.410550	1.020979
-48.072318	-18.972390	1.025984
-48.374626	-18.067514	1.030989
-48.542135	-7.429928	1.035994
-48.345976	-15.407866	1.040998
-48.925175	-9.517830	1.046003
-48.674361	-10.828825	1.051008
-49.452437	-12.563896	1.056013
-50.149308	-15.067825	1.061018
-49.787409	-21.176646	1.066022
-50.094053	-16.955485	1.071027
-50.326100	-19.367733	1.076032
-50.182996	-18.349152	1.081037
-50.880820	-17.439250	1.086042
-51.120309	-19.543448	1.091046
-51.599725	-15.554642	1.096051
-51.630838	-16.384864	1.101056
-52.059568	-9.151667	1.106061
-52.593039	-19.666496	1.111066
-52.518560	-15.596802	1.116070
-52.887751	-11.679051	1.121075
-53.014911	-14.205810	1.126080
-53.294429	-13.848670	1.131085
-53.677261	-14.800950	1.136090
-53.274552	-13.579438	1.141094
-53.640161	-10.605044	1.146099
-53.758263	-19.457552	1.151104
-54.144587	-13.638868	1.156109
-54.619708	-14.364717	1.161114
-54.919412	-15.004157	1.166118
-56.168812	-14.251435	1.171123
-55.451817	-17.805806	1.176128
-56.197779	-18.761299	1.181133
-56.025065	-21.236969	1.186138
-56.135746	-17.059168	1.191142
-56.786922	-9.936649	1.196147
-56.217051	-13.787506	1.201152
-56.171969	-15.879347	1.206157
-57.041306	-13.813112	1.211162
-57.085507	-17.833503	1.216166
-57.519365	-13.611391	1.221171
-57.556866	-19.243179	1.226176
-58.379565	-12.903703	1.231181
-58.868550	-16.965131	1.236186
-58.836261	-15.764672	1.241190
-59.295661	-12.326329	1.246195
-59.248900	-16.705822	1.251200
-59.247411	-19.072405	1.256205
-59.355495	-12.155207	1.261210
-59.856679	-11.105274	1.266214
-60.381228	-12.411834	1.271219
-60.473153	-15.516752	1.276224
-60.569391	-11.496238	1.281229
-60.529228	-12.755243	1.286234
-61.193582	-15.473074	1.291238
-61.963538	-9.768283	1.296243
-62.159582	-15.134784	1.301248
-62.344368	-16.864741	1.306253
-62.338274	-7.649570	1.311258
-62.153531	-6.539437	1.316262
-62.543056	-11.432697	1.321267
-62.197305	-12.087854	1.326272
-63.031259	-13.209892	1.331277
-63.343609	-17.469839	1.336282
-63.580485	-8.691159	1.341286
-63.866563	-14.046717	1.346291
-64.719773	-13.511098	1.351296
-65.080982	-10.290620	1.356301
-64.995202	-9.326332	1.361306
-65.300408	-12.005526	1.366310
-65.342414	-15.482097	1.371315
-65.149262	-18.979696	1.376320
-65.047575	-12.743936	1.381325
-65.495461	-8.510133	1.386330
-66.238363	-19.153495	1.391334
-66.766239	-7.339477	1.396339
-66.618206	-12.987683	1.401344
-66.733089	-11.969806	1.406349
-66.629678	-7.256076	1.411354
-67.306480	-20.617962	1.416358
-67.948842	-11.756764	1.421363
-68.107250	-20.574480	1.426368
-67.799951	-17.012667	1.431373
-68.642728	-12.014636	1.436378
-68.784918	-12.754687	1.441382
-69.319965	-14.236772	1.446387
-69.245571	-12.796137	1.451392
-69.290635	-8.011686	1.456397
-69.606376	-15.542417	1.461402
-69.440025	-17.533037	1.466406
-70.625982	-11.652331	1.471411
-70.723721	-9.121706	1.476416
-70.840187	-9.647489	1.481421
-71.183811	-4.278418	1.486426
-70.808724	-16.264385	1.491430
-71.166299	-10.000953	1.496435
-71.530205	-12.721569	1.501440
-72.063633	-14.640504	1.506445
-72.541963	-5.858790	1.511450
-72.115877	-14.818715	1.516454
-72.357961	-8.035543	1.521459
-72.877419	-13.667742	1.526464
-73.862670	-15.401984	1.531469
-73.807391	-9.601876	1.536474
-73.812779	-14.934976	1.541478
-74.100877	-14.503724	1.546483
-74.327382	-12.724876	1.551488
-73.978793	-15.667866	1.556493
-74.544230	-4.569295	1.561498
-74.985556	-14.696766	1.566502
-75.641129	-7.655814	1.571507
-75.656061	-15.119784	1.576512
-75.460055	-9.768833	1.581517
-75.533870	-8.782701	1.586522
-75.931534	-15.348306	1.591526
-76.876052	0.722965	1.596531
-76.567086	-16.222889	1.601536
-76.780637	-10.981769	1.606541
-77.076820	-3.373871	1.611546
-77.261489	-6.809106	1.616550
-78.067667	-3.123435	1.621555
-78.217999	-10.284617	1.626560
-78.228873	1.356646	1.631565
-78.454301	-18.083925	1.636570
-78.381336	-16.364658	1.641574
-78.637372	-11.670536	1.646579
-79.035994	-6.232737	1.651584
-79.496567	-6.995665	1.656589
-79.871332	-7.044377	1.661594
-79.987161	-9.262865	1.666598
-80.243032	-7.466760	1.671603
-80.871835	-18.991701	1.676608
-81.275546	-12.369865	1.681613
-81.392858	-11.835661	1.686618
-81.359935	-15.339791	1.691622
-81.549704	-1.708976	1.696627
-81.298834	-4.288643	1.701632
-81.473914	-12.104006	1.706637
-81.842664	-6.813256	1.711642
-82.213086	-15.967910	1.716646
-82.803388	-7.817220	1.721651
-82.593661	-12.775904	1.726656
-83.348832	-12.249318	1.731661
-83.819852	-19.103982	1.736666
-83.934286	-17.462918	1.741670
-84.224842	-10.371596	1.746675
-84.146928	-17.483118	1.751680
-84.005830	-10.788463	1.756685
-84.856187	-13.850468	1.761690
-85.033319	-12.411550	1.766694
-85.709175	-14.248055	1.771699
-85.302834	-13.568115	1.776704
-85.400395	-7.519431	1.781709
-85.770650	-14.421524	1.786714
-85.984442	-14.033553	1.791718
-86.843336	-6.650694	1.796723
-87.400628	-14.551696	1.801728
-87.345027	-14.332487	1.806733
-87.323102	-9.561698	1.811738
-87.357038	-14.165826	1.816742
-88.029521	-11.586270	1.821747
-87.856382	-16.681589	1.826752
-87.997673	-22.834947	1.831757
-88.622357	-15.969680	1.836762
-88.904290	-22.252860	1.841766
-88.905597	-13.884419	1.846771
-88.648618	-12.839389	1.851776
-88.973644	-21.453825	1.856781
-89.879794	-3.547271	1.861786
-90.316965	-18.699419	1.866790
-90.506741	-9.966086	1.871795
-90.520054	-19.379174	1.876800
-90.770564	-16.274120	1.881805
-91.096558	-18.016750	1.886810
-91.416795	-24.841254	1.891814
-91.992619	-15.585526	1.896819
-92.147446	-14.162758	1.901824
-92.159518	-9.769455	1.906829
-92.805442	-7.121294	1.911834
-92.188103	-11.602849	1.916838
-92.111435	-13.870481	1.921843
-93.057861	-15.471599	1.926848
-92.884566	-20.889643	1.931853
-93.757783	-15.659053	1.936858
-93.360739	-20.637596	1.941862
-93.583868	-13.132898	1.946867
-94.239306	-21.667086	1.951872
-94.368321	-17.214332	1.956877
-94.570067	-16.467581	1.961882
-94.631217	-21.292069	1.966886
-95.379353	-12.879368	1.971891
-96.144936	-11.145762	1.976896
-96.211747	-17.937213	1.981901
-96.157348	-15.319697	1.986906
-96.167420	-23.926536	1.991910
-96.261605	-7.045720	1.996915
-96.212128	-16.684024	2.006912
-96.682348	-15.814962	2.016909
-96.578282	-16.721157	2.026906
-95.567300	-11.684124	2.036902
-94.926521	-20.540057	2.046899
-94.580606	-18.864381	2.056896
-94.200637	-15.122302	2.066893
-93.748292	-11.705175	2.076890
-92.934396	-17.629513	2.086886
-92.618626	-13.814018	2.096883
-92.334990	-21.052264	2.106880
-91.503092	-15.328269	2.116877
-91.129671	-15.430868	2.126874
-90.256145	-22.134323	2.136870
-89.800065	-12.005222	2.146867
-89.726253	-20.639266	2.156864
-89.206063	-18.335164	2.166861
-88.599065	-19.247306	2.176858
-88.231934	-15.129415	2.186854
-87.119898	-16.820777	2.196851
-86.965966	-14.437109	2.206848
-86.531728	-16.405566	2.216845
-85.538018	-15.993977	2.226842
-85.480773	-12.093622	2.236838
-85.248048	-17.068421	2.246835
-84.726739	-13.329481	2.256832
-84.118113	-15.537507	2.266829
-83.691809	-11.067758	2.276826
-82.854585	-15.063395	2.286822
-82.520028	-12.948782	2.296819
-82.218686	-16.081172	2.306816
-81.385270	-19.531350	2.316813
-81.261383	-17.782869	2.326810
-80.489925	-21.784039	2.336806
-79.733379	-10.976592	2.346803
-79.796913	-14.682199	2.356800
-79.046578	-12.480682	2.366797
-78.597660	-11.366005	2.376794
-77.438112	-14.613864	2.386790
-77.281659	-14.682465	2.396787
-77.193432	-13.935755	2.406784
-76.877934	-12.743152	2.416781
-75.921245	-14.378493	2.426778
-75.467812	-7.901442	2.436774
-75.076672	-12.688822	2.446771
-73.954550	-7.789576	2.456768
-73.921503	-2.488429	2.466765
-73.891194	-9.310017	2.476762
-72.845269	-11.466188	2.486758
-72.208244	-12.237315	2.496755
-72.147139	-9.180199	2.506752
-71.398580	-13.668790	2.516749
-70.895458	-13.829725	2.526746
-70.993797	-13.820388	2.536742
-69.923313	-15.270820	2.546739
-69.621974	-19.432742	2.556736
-68.457892	-20.267449	2.566733
-68.177252	-9.211199	2.576730
-68.187268	-8.997124	2.586726
-67.900509	-10.391275	2.596723
-67.126250	-11.304283	2.606720
-66.257851	-11.614320	2.616717
-65.677363	-10.016579	2.626714
-65.307081	-11.898987	2.636710
-64.990691	-9.445740	2.646707
-64.913427	-12.733086	2.656704
-63.749421	-8.420108	2.666701
-63.805726	-11.784727	2.676698
-62.855094	-10.406542	2.686694
-62.425024	-18.526208	2.696691
-61.996818	-13.473881	2.706688
-61.435601	-14.518231	2.716685
-60.880435	-10.109853	2.726682
-60.573709	-11.709872	2.736678
-59.509531	-7.732877	2.746675
-59.719716	-10.484174	2.756672
-59.012377	-10.993888	2.766669
-58.227767	-9.570681	2.776666
-58.005377	-10.980089	2.786662
-57.581741	-9.646039	2.796659
-56.473924	-8.343167	2.806656
-56.528397	-4.859293	2.816653
-56.334933	-4.436349	2.826650
-55.199210	-12.568385	2.836646
-54.998796	-13.378803	2.846643
-54.578371	-19.130613	2.856640
-53.506588	-21.281329	2.866637
-53.485763	-22.437407	2.876634
-53.380100	-13.827789	2.886630
-52.529505	-23.483204	2.896627
-52.026762	-13.988634	2.906624
-50.987015	-11.281265	2.916621
-50.583139	-16.114988	2.926618
-50.698918	-11.297370	2.936614
-50.098952	-16.364558	2.946611
-49.221143	-17.312796	2.956608
-48.921942	-18.423794	2.966605
-48.704208	-18.657219	2.976602
-48.043688	-18.392988	2.986598
-47.515854	-14.838801	2.996595
-46.605225	-21.731799	3.006592
-46.604887	-19.903770	3.016589
-45.947531	-10.506284	3.026586
-44.994983	-12.571793	3.036582
-45.061444	-18.817516	3.046579
-44.707650	-27.783699	3.056576
-43.909593	-17.936261	3.066573
-43.829182	-14.191590	3.076570
-42.411470	-18.823042	3.086566
-41.962093	-19.102266	3.096563
-42.380314	-13.236235	3.106560
-41.491965	-11.797603	3.116557
-40.761411	-14.385860	3.126554
-40.620800	-17.698971	3.136550
-39.469865	-15.287789	3.146547
-38.970022	-14.523212	3.156544
-38.948081	-15.546417	3.166541
-38.874500	-13.809059	3.176538
-37.963837	-17.252332	3.186534
-37.502809	-12.477576	3.196531
-36.427661	-12.154768	3.206528
-35.949038	-12.080614	3.216525
-35.931968	-12.805283	3.226522
-35.925405	-15.916826	3.236518
-34.962060	-9.852288	3.246515
-34.446583	-15.644334	3.256512
-33.400086	-6.928706	3.266509
-33.049575	-12.508005	3.276506
-32.979738	-15.727664	3.286502
-33.125090	-17.472257	3.296499
-31.920868	-15.715654	3.306496
-31.214000	-9.715466	3.316493
-30.421250	-11.895319	3.326490
-30.465004	-9.898822	3.336486
-29.979289	-10.025349	3.346483
-29.399984	-5.630253	3.356480
-28.779683	-7.444131	3.366477
-28.621595	-14.352265	3.376474
-27.596248	-8.139050	3.386470
-27.220926	-6.217721	3.396467
-27.073356	-14.628911	3.406464
-26.147162	-12.746381	3.416461
-25.583861	-14.101499	3.426458
-25.808807	-3.935368	3.436454
-25.143376	-10.330620	3.446451
-24.394206	-9.668463	3.456448
-24.094815	-14.302084	3.466445
-23.073613	-12.203190	3.476442
-22.533131	-10.409109	3.486438
-22.607523	-15.408646	3.496435
-21.831611	-12.393838	3.506432
-21.383722	-7.455463	3.516429
-20.889155	-13.003482	3.526426
-19.980462	-12.984041	3.536422
-19.843463	-11.836326	3.546419
-19.472021	-15.863515	3.556416
-18.707639	-11.877553	3.566413
-18.321963	-3.793308	3.576410
-18.348910	-11.800187	3.586406
-17.515532	-9.044639	3.596403
-16.574644	-10.265684	3.606400
-15.888590	-8.253659	3.616397
-15.473272	-12.639349	3.626394
-15.394065	-13.120330	3.636390
-15.171473	-13.763161	3.646387
-14.720066	-8.530732	3.656384
-13.861780	-10.046111	3.666381
-13.088792	-12.707540	3.676378
-12.500757	-11.285206	3.686374
-12.238004	-9.590158	3.696371
-12.030229	-13.870469	3.706368
-11.513597	-11.546795	3.716365
-10.859003	-9.909976	3.726362
-10.289285	-4.046684	3.736358
-9.552508	-10.687531	3.746355
-9.446470	-8.359711	3.756352
-9.036761	-9.659085	3.766349
-8.259150	-9.935885	3.776346
-7.921066	-8.819676	3.786342
-7.032154	-9.693622	3.796339
-6.578889	-16.511791	3.806336
-6.369052	-14.383968	3.816333
-6.023103	-13.319677	3.826330
-5.350806	-9.480843	3.836326
-5.023866	-6.462208	3.846323
-4.423304	0.653871	3.856320
-4.134495	-0.145055	3.866317
-3.562824	19.244457	3.876314
-3.273393	21.283786	3.886310
-2.956682	28.878341	3.896307
-2.116630	50.623865	3.906304
-1.685499	60.829789	3.916301
-1.251208	78.888236	3.926298
-1.206385	85.568736	3.936294
-0.336722	111.016041	3.946291
0.000000	120.117629	3.951296
-0.079949	131.383827	3.956301
0.445257	144.931210	3.961306
0.614317	136.998578	3.966310
0.447526	152.979767	3.971315
0.854001	155.684516	3.976320
1.054977	165.831035	3.981325
1.105977	163.937563	3.986330
1.325148	159.353840	3.991334
1.025551	158.113256	3.996339
1.060144	142.285918	4.001344
1.248984	141.968558	4.006349
0.782628	149.388049	4.011354
0.873319	148.307778	4.016358
0.860162	162.151501	4.021363
0.941320	164.056167	4.026368
1.374089	173.356444	4.031373
1.369367	173.547142	4.036378
1.578164	166.339104	4.041382
0.971185	153.728605	4.046387
1.011971	145.458560	4.051392
1.402696	144.283822	4.056397
0.749746	147.493090	4.061402
0.773289	144.332084	4.066406
0.839171	162.637002	4.071411
1.133475	161.531155	4.076416
1.234306	163.758608	4.081421
1.365030	173.745295	4.086426
1.486320	168.721321	4.091430
1.152968	173.019478	4.096435
1.427508	168.987066	4.101440
1.494914	172.020193	4.106445
1.235899	166.809033	4.111450
1.595099	165.642397	4.116454
1.578070	178.439527	4.121459
1.579823	168.682283	4.126464
1.128188	157.379392	4.131469
1.146515	158.003080	4.136474
1.545777	165.486267	4.141478
1.061856	171.579733	4.146483
1.182051	169.602651	4.151488
1.411488	172.790727	4.156493
1.111852	174.843644	4.161498
1.416583	172.397883	4.166502
1.543327	172.549000	4.171507
1.284541	169.239236	4.176512
1.315040	174.252346	4.181517
1.212992	178.681943	4.186522
1.336667	172.961562	4.191526
1.214550	172.711906	4.196531
1.298741	166.190950	4.201536
1.151929	170.947100	4.206541
1.177888	189.543042	4.211546
1.698575	190.692302	4.216550
1.772636	195.426507	4.221555
1.840691	194.159953	4.226560
1.775832	188.111600	4.231565
1.531422	179.851424	4.236570
1.312013	174.124687	4.241574
1.344970	192.662587	4.246579
1.915701	183.142055	4.251584
1.701202	189.465397	4.256589
1.805850	194.352998	4.261594
2.130343	188.838431	4.266598
1.415130	185.767859	4.271603
1.747254	175.712072	4.276608
1.690632	179.349933	4.281613
1.716017	184.727682	4.286618
1.441680	168.989855	4.291622
1.664551	191.101543	4.296627
1.764122	196.277845	4.301632
1.694051	199.794430	4.306637
1.603923	197.325112	4.311642
2.112348	191.050890	4.316646
1.974813	205.126108	4.321651
2.104852	193.969338	4.326656
1.781199	197.522491	4.331661
1.991776	198.549497	4.336666
2.406560	191.502165	4.341670
1.944441	183.364685	4.346675
2.083362	173.528998	4.351680
2.105577	181.814758	4.356685
1.653789	172.745512	4.361690
1.528815	172.635510	4.366694
1.392650	183.113276	4.371699
1.945093	191.085006	4.376704
2.110730	196.219318	4.381709
1.738503	203.000817	4.386714
1.813386	191.938113	4.391718
2.084928	199.049017	4.396723
1.970777	193.375385	4.401728
2.221402	196.433593	4.406733
1.927574	202.949705	4.411738
2.595196	191.781473	4.416742
2.298522	201.844634	4.421747
2.120074	198.680466	4.426752
2.020727	191.273924	4.431757
2.137359	186.130451	4.436762
2.352376	188.140697	4.441766
1.949067	191.041936	4.446771
1.918630	180.691773	4.451776
2.107922	190.836974	4.456781
2.124737	202.420253	4.461786
2.057109	192.901659	4.466790
1.962956	190.762006	4.471795
1.901046	186.105257	4.476800
2.118798	191.437048	4.481805
2.249972	202.455074	4.486810
2.074020	196.012833	4.491814
2.155599	196.218484	4.496819
2.201531	196.097522	4.501824
2.307086	199.814382	4.506829
1.841153	196.518087	4.511834
2.250911	186.443802	4.516838
1.942777	194.768674	4.521843
2.079217	195.468770	4.526848
2.484082	197.325884	4.531853
2.283006	205.105634	4.536858
2.608265	215.001751	4.541862
2.214760	216.734020	4.546867
2.275317	218.670393	4.551872
2.531600	222.635727	4.556877
2.647821	220.029669	4.561882
2.697530	196.916872	4.566886
2.476849	198.878327	4.571891
2.550861	204.568005	4.576896
2.662975	200.099123	4.581901
2.318982	198.656682	4.586906
2.453174	198.708555	4.591910
2.424200	196.153724	4.596915
2.619262	191.115021	4.601920
2.373892	197.851332	4.606925
2.006997	199.114353	4.611930
2.577378	221.820206	4.616934
2.355141	223.462365	4.621939
2.538000	222.671372	4.626944
2.696028	228.873083	4.631949
2.691428	227.532488	4.636954
2.777535	215.680227	4.641958
2.690330	230.949818	4.646963
2.913233	234.344575	4.651968
2.866012	227.755600	4.656973
2.554505	224.384483	4.661978
2.868678	220.428108	4.666982
2.512894	229.918409	4.671987
2.795279	225.637979	4.676992
2.911306	225.351009	4.681997
2.904990	213.503739	4.687002
2.724237	201.867308	4.692006
2.217993	209.286746	4.697011
2.445722	214.822628	4.702016
2.791664	219.805308	4.707021
2.679331	225.290070	4.712026
3.122853	220.383273	4.717030
2.686410	223.074571	4.722035
2.635477	227.556283	4.727040
2.938072	225.098194	4.732045
2.713464	234.055410	4.737050
2.965173	223.581920	4.742054
2.907183	227.381359	4.747059
2.539473	229.843586	4.752064
3.013797	223.157076	4.757069
2.862902	225.569513	4.762074
2.967808	216.432002	4.767078
2.634223	222.906894	4.772083
2.821921	222.304970	4.777088
2.773215	220.616942	4.782093
2.306511	227.008289	4.787098
2.938733	224.884535	4.792102
3.334491	247.532360	4.797107
3.035873	247.544479	4.802112
3.118421	226.084327	4.807117
2.833089	225.686235	4.812122
3.305388	222.622583	4.817126
2.959357	226.755058	4.822131
2.990836	224.235044	4.827136
3.245553	241.197483	4.832141
2.554204	231.561458	4.837146
2.772431	234.229275	4.842150
3.039830	233.545260	4.847155
3.253126	251.007750	4.852160
3.247615	247.844950	4.857165
3.184641	253.464358	4.862170
3.552315	249.724223	4.867174
3.523919	252.661642	4.872179
3.211491	252.631632	4.877184
3.243015	246.802278	4.882189
3.285842	255.894774	4.887194
3.365889	250.801308	4.892198
3.162065	251.640144	4.897203
3.203811	254.531772	4.902208
3.766836	240.064241	4.907213
3.055067	237.170292	4.912218
3.151862	235.462629	4.917222
3.345033	250.074531	4.922227
3.548107	250.457301	4.927232
3.465642	240.162713	4.932237
3.168642	228.360979	4.937242
3.264911	228.779466	4.942246
3.302946	240.378428	4.947251
3.350684	252.086610	4.952256
3.142074	244.054915	4.957261
3.171771	251.317630	4.962266
3.196416	252.171289	4.967270
3.408800	250.657487	4.972275
3.340018	249.880611	4.977280
3.560175	240.756668	4.982285
3.016080	245.176448	4.987290
3.607358	248.823541	4.992294
3.490276	253.084667	4.997299
3.395699	252.004944	5.002304
3.568995	252.329104	5.007309
3.286473	265.822802	5.012314
3.437978	260.411248	5.017318
3.332258	256.315010	5.022323
3.315289	256.555085	5.027328
3.842680	263.391806	5.032333
3.848338	261.692092	5.037338
3.452957	252.161544	5.042342
3.424344	257.677492	5.047347
3.789421	270.924190	5.052352
4.048146	274.727799	5.057357
3.697956	263.159005	5.062362
3.343676	255.485493	5.067366
3.518515	264.304205	5.072371
3.304341	280.909873	5.077376
4.211637	278.021667	5.082381
4.156278	294.570826	5.087386
3.983307	271.442202	5.092390
3.788605	265.828625	5.097395
3.743986	257.897782	5.102400
3.820342	250.966728	5.107405
3.475670	252.166159	5.112410
3.488273	250.727953	5.117414
3.739842	275.274536	5.122419
3.954877	278.110541	5.127424
3.964910	288.676196	5.132429
3.872928	290.339080	5.137434
4.317456	278.278756	5.142438
4.090016	263.947714	5.147443
3.669490	264.178254	5.152448
3.892466	262.498274	5.157453
3.725997	261.746195	5.162458
3.889961	264.653476	5.167462
4.000939	270.821445	5.172467
3.879579	281.277966	5.177472
4.224257	272.068056	5.182477
3.643143	284.263938	5.187482
4.095907	270.955790	5.192486
3.949250	275.825841	5.197491
4.043718	277.057708	5.202496
4.273345	267.865827	5.207501
4.075200	280.931858	5.212506
4.233283	273.516585	5.217510
4.126797	255.297273	5.222515
3.722280	256.746529	5.227520
4.136215	266.416807	5.232525
4.083923	283.908287	5.237530
4.079340	277.815657	5.242534
4.133482	280.360493	5.247539
3.601627	280.241475	5.252544
4.079928	276.113837	5.257549
4.123963	284.076682	5.262554
4.022818	277.477155	5.267558
4.087371	284.073187	5.272563
3.932098	280.228320	5.277568
4.198260	280.306972	5.282573
3.904482	286.718702	5.287578
4.219542	280.993610	5.292582
4.023062	288.586012	5.297587
4.387736	288.275901	5.302592
4.182056	278.456184	5.307597
3.934153	286.183194	5.312602
4.188250	302.456079	5.317606
4.270305	303.427297	5.322611
4.152790	311.339536	5.327616
4.429317	311.489332	5.332621
4.128173	316.121004	5.337626
4.145096	319.554378	5.342630
4.726792	318.783149	5.347635
4.202167	308.703336	5.352640
4.787034	303.948380	5.357645
4.724714	305.900852	5.362650
4.692977	310.588388	5.367654
4.699607	308.445585	5.372659
4.445753	298.908656	5.377664
4.596128	286.536905	5.382669
3.940482	289.974414	5.387674
4.581443	301.475782	5.392678
4.677686	303.232565	5.397683
4.634823	299.936401	5.402688
4.867810	297.533502	5.407693
4.546424	303.193415	5.412698
4.302179	287.305232	5.417702
4.688912	290.266199	5.422707
4.171957	286.076198	5.427712
4.624244	297.740006	5.432717
4.374378	296.953536	5.437722
4.695851	303.490337	5.442726
4.459495	307.418982	5.447731
4.230248	314.285690	5.452736
4.978644	307.983319	5.457741
4.398244	306.739265	5.462746
4.935192	306.690067	5.467750
4.431270	308.382696	5.472755
4.359378	311.466148	5.477760
4.622113	313.896046	5.482765
4.239204	328.310368	5.487770
4.689164	314.607151	5.492774
4.597883	311.865910	5.497779
4.432343	316.761077	5.502784
4.663837	327.636910	5.507789
4.397230	334.170952	5.512794
4.736205	326.505847	5.517798
4.948483	338.931800	5.522803
5.064175	339.745887	5.527808
4.970595	334.527739	5.532813
4.957254	347.238990	5.537818
5.057705	330.929758	5.542822
5.285755	334.114916	5.547827
4.678042	331.097078	5.552832
4.795529	319.100624	5.557837
4.817804	326.411989	5.562842
4.884194	330.191961	5.567846
4.870364	328.014396	5.572851
5.162913	335.362512	5.577856
5.279252	330.165259	5.582861
5.308435	341.028506	5.587866
5.361247	322.002705	5.592870
4.984402	312.491367	5.597875
4.754281	311.455025	5.602880
4.712122	309.538169	5.607885
4.718151	324.252221	5.612890
5.195877	327.711475	5.617894
5.412168	327.396138	5.622899
4.893078	339.050819	5.627904
5.371393	340.690792	5.632909
5.178416	340.417434	5.637914
5.633366	327.675224	5.642918
5.076579	317.154349	5.647923
4.922970	313.840733	5.652928
5.215349	312.308065	5.657933
4.694548	315.806709	5.662938
5.364649	316.208055	5.667942
5.513598	331.352144	5.672947
4.823438	322.323334	5.677952
5.368231	327.173646	5.682957
5.224691	334.384443	5.687962
4.928457	330.909670	5.692966
5.111541	340.609832	5.697971
4.868341	331.207260	5.702976
5.352258	331.723202	5.707981
5.358518	335.253164	5.712986
5.384347	342.317202	5.717990
5.318501	335.022412	5.722995
5.148912	345.227096	5.728000
5.579460	326.822324	5.733005
5.316926	333.570866	5.738010
5.546799	333.753283	5.743014
5.754034	335.037089	5.748019
5.491237	335.021449	5.753024
5.376820	327.946247	5.758029
5.419484	333.289696	5.763034
5.062275	334.468949	5.768038
5.541679	344.654204	5.773043
5.327718	329.523717	5.778048
5.838935	329.263412	5.783053
5.553739	332.443565	5.788058
5.403480	331.435838	5.793062
5.541976	343.895502	5.798067
5.346076	343.464412	5.803072
5.094825	329.149704	5.808077
5.198463	336.274316	5.813082
5.527465	335.261099	5.818086
5.592452	333.915921	5.823091
5.379353	343.007432	5.828096
5.595446	340.085146	5.833101
5.644149	336.996095	5.838106
5.870000	336.644458	5.843110
5.642568	336.876382	5.848115
5.461661	331.333390	5.853120
5.650430	337.811901	5.858125
5.340629	341.957709	5.863130
5.532083	336.419649	5.868134
5.333754	336.985540	5.873139
5.584277	359.339882	5.878144
5.885961	363.431014	5.883149
5.708558	365.031358	5.888154
6.067798	356.081720	5.893158
5.763258	359.565471	5.898163
5.697297	372.016060	5.903168
6.001322	360.059954	5.908173
5.894861	357.871588	5.913178
6.252399	349.539164	5.918182
5.706810	342.351177	5.923187
5.479997	340.058282	5.928192
6.256334	349.719280	5.933197
6.165596	349.322334	5.938202
5.950589	336.710400	5.943206
5.484819	335.644539	5.948211
5.559769	339.030859	5.953216
5.979143	349.624163	5.958221
6.125853	349.731024	5.963226
5.832974	346.192446	5.968230
5.940423	346.552236	5.973235
5.726984	356.108887	5.978240
5.960468	354.430416	5.983245
5.701815	359.634419	5.988250
5.562649	354.667022	5.993254
5.958702	364.726140	5.998259
5.516872	364.456972	6.003264
5.722111	351.934208	6.008269
5.738623	355.759967	6.013274
5.709826	355.853197	6.018278
5.817597	355.355543	6.023283
5.609701	360.045384	6.028288
5.755601	356.197604	6.033293
5.619722	363.739413	6.038298
5.857821	363.338399	6.043302
6.180834	362.512785	6.048307
5.836999	362.459221	6.053312
5.962872	355.779802	6.058317
5.530070	365.329699	6.063322
5.825701	359.009665	6.068326
6.068368	359.123638	6.073331
5.647749	358.458833	6.078336
6.096827	357.034489	6.083341
5.988447	368.333766	6.088346
5.835581	366.320353	6.093350
5.965295	359.463156	6.098355
5.297929	364.671087	6.103360
6.273663	371.810932	6.108365
6.053073	372.510028	6.113370
6.165216	371.632031	6.118374
6.388447	357.866228	6.123379
5.885102	362.042366	6.128384
6.165919	357.262268	6.133389
5.996406	358.949962	6.138394
5.832719	359.494607	6.143398
5.809501	360.007750	6.148403
6.161245	359.617405	6.153408
6.182808	361.490300	6.158413
5.855509	363.101476	6.163418
5.988302	361.451436	6.168422
5.920068	359.576626	6.173427
5.759285	363.319432	6.178432
6.151522	353.349041	6.183437
6.101062	360.099166	6.188442
6.112918	353.510380	6.193446
5.930959	356.073236	6.198451
5.868993	361.603933	6.203456
6.262853	353.749879	6.208461
5.830955	358.917751	6.213466
5.907532	355.406706	6.218470
5.934009	353.884059	6.223475
5.976721	359.774847	6.228480
6.140805	347.865987	6.233485
5.954495	342.406097	6.238490
5.425045	344.542499	6.243494
5.618551	338.545364	6.248499
5.697609	354.731826	6.253504
5.966102	354.227973	6.258509
5.847313	366.617231	6.263514
6.029096	367.341869	6.268518
5.921680	362.774463	6.273523
5.895669	366.730275	6.278528
6.135468	361.428246	6.283533
5.979877	355.643994	6.288538
6.073352	359.078036	6.293542
5.779809	359.010265	6.298547
5.938470	370.811878	6.303552
6.006367	360.430385	6.308557
5.926753	354.510840	6.313562
5.875485	357.303161	6.318566
6.047344	367.153794	6.323571
5.903164	358.703821	6.328576
5.845097	361.155515	6.333581
5.809384	358.139800	6.338586
5.501860	358.801896	6.343590
5.740646	363.029436	6.348595
5.879292	364.254387	6.353600
5.915228	362.255685	6.358605
5.924828	362.535892	6.363610
6.098836	367.232336	6.368614
6.371658	364.288502	6.373619
5.846145	357.477022	6.378624
6.226736	354.073370	6.383629
5.833512	349.655155	6.388634
5.654211	337.898182	6.393638
5.868076	344.578412	6.398643
5.831092	353.110813	6.403648
5.989819	351.700325	6.408653
5.839398	358.519896	6.413658
5.992100	362.510983	6.418662
6.314711	362.919320	6.423667
6.206957	345.304403	6.428672
6.076876	342.322459	6.433677
6.057793	337.782349	6.438682
5.611910	329.107574	6.443686
6.095162	326.880597	6.448691
6.065982	329.669453	6.453696
6.263420	329.534244	6.458701
5.676976	338.655775	6.463706
6.101315	334.814994	6.468710
6.018765	331.550354	6.473715
5.783600	338.671103	6.478720
5.816249	332.310025	6.483725
5.901611	340.604947	6.488730
5.945257	340.984225	6.493734
5.995745	325.964169	6.498739
5.644255	334.144036	6.503744
5.755985	332.377075	6.508749
5.674025	335.651936	6.513754
5.735243	325.761900	6.518758
6.081394	338.486422	6.523763
5.875944	341.714193	6.528768
6.103664	330.763500	6.533773
5.913620	341.347879	6.538778
5.710606	337.561101	6.543782
6.162351	331.659550	6.548787
5.546657	341.168486	6.553792
5.638736	337.531628	6.558797
5.868949	337.676026	6.563802
5.944888	335.655240	6.568806
5.944101	336.554017	6.573811
5.709159	344.513143	6.578816
5.978309	331.543774	6.583821
5.984908	326.676933	6.588826
5.528529	335.778084	6.593830
5.837986	345.335059	6.598835
5.657774	362.419545	6.603840
6.167206	364.228654	6.608845
5.990160	368.331521	6.613850
5.524476	355.727212	6.618854
6.383071	357.623984	6.623859
6.230112	350.434588	6.628864
5.784169	339.304698	6.633869
5.661774	341.323536	6.638874
5.844145	343.658460	6.643878
5.949106	343.635819	6.648883
5.743110	338.305567	6.653888
5.994321	339.772312	6.658893
5.812544	340.041375	6.663898
5.832007	347.400647	6.668902
6.116586	355.895321	6.673907
5.769965	360.556276	6.678912
5.691720	354.687137	6.683917
5.815088	363.523455	6.688922
5.734697	359.372603	6.693926
6.160845	367.996964	6.698931
6.025256	370.884758	6.703936
6.101490	363.127924	6.708941
5.798531	358.518390	6.713946
5.848219	368.043311	6.718950
6.056044	364.717348	6.723955
5.762440	355.765595	6.728960
5.991655	352.331877	6.733965
5.949357	365.917727	6.738970
5.560643	361.701286	6.743974
5.866759	361.859102	6.748979
5.869441	367.613794	6.753984
6.178930	370.890604	6.758989
5.735671	368.546196	6.763994
6.083308	373.367300	6.768998
6.061393	366.986284	6.774003
5.674094	359.295753	6.779008
6.186353	349.876045	6.784013
5.714961	352.762666	6.789018
6.042946	351.857178	6.794022
5.660532	351.980504	6.799027
5.915852	364.526284	6.804032
5.762504	366.050091	6.809037
5.993876	366.235438	6.814042
5.793176	362.752018	6.819046
6.018612	367.519499	6.824051
5.831874	362.486785	6.829056
5.915422	359.828877	6.834061
5.679226	361.504873	6.839066
5.573899	369.057716	6.844070
5.682852	363.409185	6.849075
5.777290	373.923700	6.854080
6.011600	369.090773	6.859085
6.003756	371.022062	6.864090
5.925913	364.349248	6.869094
6.292119	360.337232	6.874099
5.985865	363.390973	6.879104
6.024578	362.913631	6.884109
6.139024	364.291073	6.889114
5.674597	373.191020	6.894118
6.075979	368.945696	6.899123
6.200888	374.915361	6.904128
6.129541	360.610406	6.909133
5.670355	352.595777	6.914138
5.450510	349.017281	6.919142
5.925350	358.038976	6.924147
5.549035	369.981360	6.929152
5.515029	370.629075	6.934157
5.566013	372.842217	6.939162
5.636866	372.843903	6.944166
5.881700	370.337896	6.949171
5.773313	373.287868	6.954176
5.715621	364.267509	6.959181
5.939909	375.191957	6.964186
5.733387	371.342445	6.969190
5.892944	365.698639	6.974195
5.906238	367.598142	6.979200
6.200442	365.419764	6.984205
5.741098	372.515540	6.989210
6.146840	366.627513	6.994214
6.130365	366.307517	6.999219
5.994469	372.169346	7.004224
6.143481	363.597499	7.009229
6.069832	367.405749	7.014234
6.011105	368.819817	7.019238
5.976750	351.936890	7.024243
5.875223	367.113928	7.029248
5.780289	360.314077	7.034253
6.000861	367.518457	7.039258
5.977149	365.804353	7.044262
6.037678	364.368120	7.049267
5.731096	370.221890	7.054272
5.747999	365.331278	7.059277
5.895559	369.313680	7.064282
5.732806	370.348570	7.069286
5.779386	363.358863	7.074291
5.989206	369.552508	7.079296
6.456512	353.543286	7.084301
6.021141	364.156626	7.089306
5.930400	366.768468	7.094310
5.979374	362.065825	7.099315
6.219200	367.217036	7.104320
5.885014	363.947524	7.109325
6.310449	363.491847	7.114330
5.829374	360.011228	7.119334
6.100602	348.462074	7.124339
5.874760	346.371510	7.129344
5.478347	339.754948	7.134349
5.698633	345.386950	7.139354
5.642547	356.099048	7.144358
5.861236	363.423947	7.149363
5.778456	371.770540	7.154368
5.937991	366.171031	7.159373
6.265191	363.617318	7.164378
6.029451	368.241919	7.169382
6.270827	366.862773	7.174387
5.756822	359.337631	7.179392
5.959370	356.271929	7.184397
5.626917	353.397623	7.189402
5.777588	363.381291	7.194406
6.122722	369.132947	7.199411
6.028479	367.597576	7.204416
5.462991	361.826925	7.209421
5.923992	370.221195	7.214426
5.862254	369.721626	7.219430
5.870687	361.614742	7.224435
5.483479	368.968137	7.229440
5.721593	364.460489	7.234445
5.674142	358.975673	7.239450
5.865747	377.580659	7.244454
5.907919	365.469421	7.249459
6.001655	375.243714	7.254464
5.917887	371.843212	7.259469
6.108359	375.774599	7.264474
5.837375	370.903782	7.269478
5.882348	357.906242	7.274483
5.809360	364.039791	7.279488
6.163910	359.751187	7.284493
6.072551	363.169898	7.289498
5.932093	364.859368	7.294502
5.880553	370.768091	7.299507
5.725174	376.996813	7.304512
5.809528	365.435798	7.309517
5.967712	369.400717	7.314522
5.718113	373.223882	7.319526
5.660613	368.107640	7.324531
5.655967	372.006322	7.329536
5.649522	372.855366	7.334541
5.944469	374.122268	7.339546
5.652115	367.818428	7.344550
5.841395	364.697855	7.349555
5.808671	375.861894	7.354560
5.754188	362.996995	7.359565
5.679603	372.538226	7.364570
5.631579	385.568156	7.369574
6.052635	383.360410	7.374579
6.340780	392.658152	7.379584
6.063468	371.706636	7.384589
5.730413	371.752625	7.389594
5.778799	376.588979	7.394598
5.659766	362.234546	7.399603
5.697888	379.449356	7.404608
6.082915	385.185275	7.409613
6.535171	388.341641	7.414618
6.073157	375.259007	7.419622
5.976430	372.044038	7.424627
5.793525	365.349719	7.429632
6.063431	363.304866	7.434637
6.047494	366.411198	7.439642
5.971900	364.461608	7.444646
6.160069	360.347772	7.449651
5.961971	378.036200	7.454656
5.830494	362.835812	7.459661
5.879788	366.713386	7.464666
5.600447	372.338257	7.469670
5.792256	365.876298	7.474675
5.738407	366.539777	7.479680
5.892360	360.738660	7.484685
5.882889	371.927528	7.489690
5.408116	363.137037	7.494694
5.683871	362.688995	7.499699
6.108259	384.266302	7.504704
5.945144	380.235976	7.509709
5.548692	375.628431	7.514714
6.036354	388.381437	7.519718
6.359238	386.312461	7.524723
5.814397	378.703555	7.529728
5.778118	365.883259	7.534733
5.785916	373.200075	7.539738
5.423098	368.656866	7.544742
5.998305	371.863569	7.549747
6.076297	385.892503	7.554752
5.976882	394.700467	7.559757
6.353781	395.679278	7.564762
5.426302	383.742104	7.569766
6.007920	374.985408	7.574771
5.966922	389.830272	7.579776
6.085068	384.022103	7.584781
6.169965	362.798705	7.589786
5.999215	366.745558	7.594790
6.059427	368.517484	7.599795
5.886012	373.720791	7.604800
6.132299	371.309471	7.609805
6.282922	365.521530	7.614810
5.692809	366.756260	7.619814
6.055132	363.861680	7.624819
5.709343	373.935796	7.629824
5.623338	365.574782	7.634829
5.771532	363.786286	7.639834
5.559288	371.169217	7.644838
6.006873	361.791274	7.649843
5.708699	371.845274	7.654848
5.812235	377.457613	7.659853
5.700697	376.203367	7.664858
6.034589	391.144519	7.669862
5.959707	375.976382	7.674867
5.745017	381.815758	7.679872
5.942662	386.840704	7.684877
5.955703	380.454207	7.689882
5.582108	386.100179	7.694886
6.361335	376.898060	7.699891
5.878363	389.436147	7.704896
5.504171	372.258428	7.709901
5.863841	378.744979	7.714906
6.185181	388.126105	7.719910
6.007915	389.236038	7.724915
5.875767	376.022623	7.729920
5.890287	371.825258	7.734925
6.024545	359.310447	7.739930
5.477004	364.607173	7.744934
5.977498	377.642904	7.749939
6.125215	393.533900	7.754944
6.199038	386.739235	7.759949
6.010306	378.188663	7.764954
6.074204	380.950288	7.769958
6.111798	370.488113	7.774963
5.929456	374.246955	7.779968
5.783766	373.320769	7.784973
5.972821	374.727652	7.789978
5.817147	372.325528	7.794982
6.214439	365.967416	7.799987
6.290734	366.237174	7.804992
6.017792	375.787339	7.809997
6.115504	370.963160	7.815002
5.704865	372.214064	7.820006
6.190225	364.911991	7.825011
5.902449	376.255201	7.830016
6.164551	372.879603	7.835021
6.099488	370.665766	7.840026
5.932087	372.419571	7.845030
5.917983	367.571782	7.850035
5.795543	381.258787	7.855040
5.905721	366.941204	7.860045
6.089274	365.412927	7.865050
6.206297	371.500888	7.870054
6.077073	357.369522	7.875059
5.912022	353.137022	7.880064
5.671823	347.808963	7.885069
5.931347	351.947828	7.890074
6.050748	352.849921	7.895078
6.203169	347.754579	7.900083
5.843727	351.253258	7.905088
5.828423	349.018972	7.910093
6.021401	339.791667	7.915098
6.003720	355.607302	7.920102
5.716875	340.643253	7.925107
5.633008	346.019186	7.930112
5.576369	357.408427	7.935117
5.912945	361.190365	7.940122
5.897033	372.396061	7.945126
6.169751	367.300848	7.950131
6.108945	368.534896	7.955149
5.494197	360.457972	7.960166
5.731132	359.038765	7.965184
5.717435	368.656595	7.970202
6.087669	362.438705	7.975219
5.848477	370.674939	7.980237
5.958989	368.432955	7.985254
5.939356	364.898574	7.990272
5.989045	372.224872	7.995290
6.317174	367.443129	8.000307
5.689371	371.786106	8.005325
5.740001	371.671009	8.010342
5.990315	368.946382	8.015360
5.648403	373.014195	8.020378
5.971894	381.572517	8.025395
6.186605	367.921963	8.030413
6.289527	373.589467	8.035430
6.134186	368.334376	8.040448
5.895284	375.563885	8.045466
6.063625	368.885329	8.050483
5.944814	366.502555	8.055501
5.930012	371.699363	8.060518
6.324364	370.075612	8.065536
5.925918	376.203518	8.070554
6.249241	372.476546	8.075571
6.038841	375.744284	8.080589
5.807090	370.169813	8.085606
6.380754	369.038665	8.090624
6.071694	360.872819	8.095642
5.991227	354.094400	8.100659
5.786499	350.939311	8.105677
5.729210	357.051625	8.110694
6.170686	361.492142	8.115712
5.907772	369.476477	8.120730
6.135687	371.555248	8.125747
6.064764	379.910286	8.130765
6.155256	373.862452	8.135782
6.165680	363.257648	8.140800
6.097917	371.495424	8.145818
5.900542	376.948053	8.150835
6.265428	370.945588	8.155853
6.092080	365.772214	8.160870
6.425329	377.487906	8.165888
6.236432	371.329217	8.170906
5.880277	365.382927	8.175923
6.126748	367.136904	8.180941
6.143083	372.300431	8.185958
6.389557	366.136644	8.190976
6.128295	376.162490	8.195994
6.273041	374.325389	8.201011
6.248063	379.340760	8.206029
6.208239	372.981991	8.211046
6.144068	371.256518	8.216064
6.098560	368.780209	8.221082
5.832604	370.870091	8.226099
6.152496	368.658416	8.231117
5.950355	371.451497	8.236134
6.387360	364.942282	8.241152
6.271190	370.110792	8.246170
6.171567	364.641849	8.251187
6.241211	367.565912	8.256205
6.240937	382.846209	8.261222
6.095852	368.844938	8.266240
5.882145	370.387001	8.271258
6.071645	370.584655	8.276275
6.082465	371.163749	8.281293
6.129923	370.547386	8.286310
6.401737	357.336009	8.291328
6.175817	369.827261	8.296346
6.248328	370.866895	8.301363
6.023351	372.704208	8.306381
5.801812	380.069851	8.311398
6.100188	367.419183	8.316416
5.736897	371.039074	8.321434
6.134056	380.056059	8.326451
6.447603	387.969015	8.331469
5.932038	397.337298	8.336486
6.457983	393.042097	8.341504
6.536162	393.225636	8.346522
6.143386	401.059922	8.351539
6.386416	392.157474	8.356557
6.263579	398.040235	8.361574
6.500151	393.070864	8.366592
6.155132	393.939238	8.371610
6.210016	398.790626	8.376627
6.435832	392.021006	8.381645
6.322570	401.853267	8.386662
6.441388	391.127323	8.391680
6.245084	398.072460	8.396698
6.445103	398.192728	8.401715
6.722231	403.656224	8.406733
6.319247	406.881560	8.411750
6.420890	401.630375	8.416768
6.381279	402.545570	8.421786
6.416367	403.142953	8.426803
6.521190	396.023067	8.431821
5.978941	405.073648	8.436838
6.402457	402.870979	8.441856
6.275357	409.792654	8.446874
6.524001	408.485215	8.451891
6.861063	410.651029	8.456909
6.642978	401.268569	8.461926
6.496290	399.455038	8.466944
6.787476	402.470624	8.471962
6.363801	399.592824	8.476979
6.271864	383.244803	8.481997
6.140413	387.961284	8.487014
6.642143	396.163489	8.492032
6.611953	403.688505	8.497050
6.509616	396.377019	8.502067
6.392452	401.179626	8.507085
6.043579	404.623698	8.512102
6.078881	396.451216	8.517120
6.305525	402.140368	8.522138
6.313230	403.603561	8.527155
6.207362	399.716618	8.532173
6.222226	402.690294	8.537190
6.251983	407.959024	8.542208
6.489554	405.056510	8.547226
6.157844	403.691684	8.552243
6.576523	420.146580	8.557261
6.668818	430.811326	8.562279
6.918160	427.253723	8.567296
6.420468	410.925071	8.572314
6.279025	409.104406	8.577331
6.870769	413.735983	8.582349
6.787681	412.199659	8.587367
6.809289	401.899187	8.592384
6.612544	402.239410	8.597402
6.213438	408.616734	8.602419
6.902500	403.197771	8.607437
6.604598	414.636845	8.612455
6.435135	403.832988	8.617472
6.552668	405.089629	8.622490
6.463206	402.184708	8.627507
6.781220	399.667215	8.632525
6.731697	412.279179	8.637543
6.848866	405.065838	8.642560
7.046701	398.433142	8.647578
6.489257	402.578912	8.652595
6.686347	402.355662	8.657613
6.443225	403.905493	8.662631
6.747000	399.067598	8.667648
6.766994	399.692592	8.672666
6.497254	408.280762	8.677683
6.754161	399.003758	8.682701
6.647166	413.625473	8.687719
6.698246	404.055673	8.692736
6.717287	408.726490	8.697754
6.639932	410.269282	8.702771
6.622907	401.088845	8.707789
6.581598	403.689477	8.712807
6.682721	405.254796	8.717824
6.765615	398.788429	8.722842
6.481960	409.111287	8.727859
6.638856	420.832550	8.732877
6.865009	426.221989	8.737895
7.051935	423.226424	8.742912
6.765744	420.226094	8.747930
6.783487	411.239017	8.752947
6.760903	395.211472	8.757965
6.439612	409.153561	8.762983
6.785524	425.058140	8.768000
6.882720	435.333963	8.773018
6.515486	438.922927	8.778035
7.391799	424.326080	8.783053
6.802204	422.402065	8.788071
6.597730	411.250245	8.793088
6.730747	413.407005	8.798106
7.225059	422.333051	8.803123
6.819727	411.856476	8.808141
6.521991	415.478727	8.813159
7.097248	417.367382	8.818176
6.654171	416.932017	8.823194
6.783445	427.644615	8.828211
6.781206	428.462439	8.833229
6.680082	437.974086	8.838247
6.696861	426.636113	8.843264
6.819654	429.135298	8.848282
6.936340	433.582542	8.853299
7.023039	427.847705	8.858317
7.364771	432.865592	8.863335
7.160201	421.051072	8.868352
7.167680	414.410327	8.873370
6.282082	420.794455	8.878387
7.139258	420.300525	8.883405
6.874534	431.901666	8.888423
7.234080	431.877021	8.893440
6.910686	415.587326	8.898458
6.783857	418.545337	8.903475
6.949827	424.310273	8.908493
6.910243	422.391597	8.913511
7.194668	435.077482	8.918528
6.900469	422.213515	8.923546
6.950185	418.365305	8.928563
7.119119	415.634487	8.933581
7.034777	421.097821	8.938599
6.641938	414.939514	8.943616
6.994806	429.981487	8.948634
6.784956	438.778035	8.953651
7.396661	435.362466	8.958669
6.926617	440.094144	8.963687
6.807645	437.604091	8.968704
6.980235	430.770214	8.973722
6.726833	425.716661	8.978739
6.665716	423.444758	8.983757
6.870303	435.818110	8.988775
6.484278	426.512443	8.993792
6.639796	439.493080	8.998810
6.744323	436.387348	9.003827
6.979089	435.886799	9.008845
7.045761	454.807880	9.013863
6.978735	451.520746	9.018880
6.982207	450.327457	9.023898
7.032201	457.899891	9.028915
7.056771	451.941254	9.033933
7.258204	456.722359	9.038951
7.176723	459.244088	9.043968
7.446336	457.494709	9.048986
7.134488	455.542951	9.054003
7.392672	450.986737	9.059021
7.283013	443.130433	9.064039
6.720173	441.811285	9.069056
7.070816	448.897959	9.074074
7.225392	459.698128	9.079091
7.432547	454.960563	9.084109
7.188089	457.255367	9.089127
7.059795	462.501541	9.094144
7.334343	465.213636	9.099162
6.974938	461.912351	9.104179
7.537021	453.363819	9.109197
7.379698	450.147636	9.114215
6.988157	441.391927	9.119232
7.440143	445.991762	9.124250
7.092014	444.736801	9.129267
7.244083	429.537071	9.134285
6.931188	440.375761	9.139303
6.878574	450.826542	9.144320
7.456658	456.687860	9.149338
7.264330	465.304954	9.154355
6.974165	453.140911	9.159373
7.020262	459.738827	9.164391
7.236516	459.260113	9.169408
7.598373	448.199413	9.174426
7.108888	454.168043	9.179443
7.081370	452.925962	9.184461
7.464642	459.136537	9.189479
6.696689	464.435600	9.194496
7.300896	451.844250	9.199514
7.075289	462.426283	9.204531
6.981151	454.756887	9.209549
7.119142	452.311775	9.214567
6.838783	463.956411	9.219584
7.903717	464.177844	9.224602
7.453065	469.906868	9.229619
7.604629	455.717039	9.234637
7.514971	457.908693	9.239655
7.181875	460.810669	9.244672
7.685501	453.461018	9.249690
7.239412	449.636838	9.254707
7.377392	454.061816	9.259725
7.265774	456.966958	9.264743
7.226721	458.049323	9.269760
7.783674	453.130721	9.274778
7.771345	463.007160	9.279795
7.542038	461.736736	9.284813
7.978136	453.413069	9.289831
7.548709	459.896146	9.294848
8.038352	456.774250	9.299866
7.705126	454.586003	9.304883
8.064330	457.815001	9.309901
7.658215	448.474600	9.314919
7.134553	440.020456	9.319936
7.420205	436.353021	9.324954
7.078761	438.195967	9.329971
7.283834	443.825397	9.334989
7.681391	452.479444	9.340007
7.448348	463.813714	9.345024
7.729560	454.482380	9.350042
7.519540	462.976014	9.355059
7.287094	460.497425	9.360077
7.395529	451.931612	9.365095
7.238579	455.882101	9.370112
7.415906	459.682387	9.375130
7.662831	459.889979	9.380147
7.130429	462.072112	9.385165
7.542565	455.898115	9.390183
7.445734	457.036870	9.395200
7.414440	456.931454	9.400218
7.559083	470.488166	9.405235
7.452155	462.303226	9.410253
7.454399	448.594384	9.415271
7.342261	461.096273	9.420288
7.541582	455.558373	9.425306
7.466006	451.401587	9.430323
7.225398	457.548971	9.435341
7.835784	467.466696	9.440359
7.516253	477.672140	9.445376
7.716505	479.468083	9.450394
7.829195	484.635481	9.455411
7.994521	467.306655	9.460429
7.361680	456.906726	9.465447
7.527245	457.063950	9.470464
7.586532	459.314318	9.475482
7.517210	476.230731	9.480499
7.547709	472.959869	9.485517
7.656673	477.663951	9.490535
7.681647	484.372482	9.495552
7.698092	479.693194	9.500570
7.787580	480.572386	9.505587
7.759612	482.583967	9.510605
8.026328	483.637359	9.515623
7.754256	499.238050	9.520640
7.829776	485.703889	9.525658
7.766780	478.846947	9.530675
7.842044	481.653384	9.535693
7.653654	477.258652	9.540711
7.547727	481.188529	9.545728
8.095018	476.347173	9.550746
8.023556	486.422236	9.555763
7.713691	489.058647	9.560781
8.016128	482.620967	9.565799
7.437719	472.865742	9.570816
7.808794	479.087703	9.575834
7.870181	478.847846	9.580851
7.759488	500.652733	9.585869
7.843682	486.880529	9.590887
7.689815	491.297596	9.595904
7.600726	486.363446	9.600922
7.810055	483.266531	9.605939
7.205708	492.235369	9.610957
7.779637	469.619726	9.615975
7.640943	480.693074	9.620992
7.464337	480.537844	9.626010
7.724347	479.171815	9.631027
7.554347	486.980700	9.636045
8.231113	504.023234	9.641063
7.613086	499.711592	9.646080
8.313871	501.441735	9.651098
7.966021	495.134342	9.656115
7.635942	495.422875	9.661133
7.888959	495.209796	9.666151
8.282078	510.176103	9.671168
8.305898	492.029991	9.676186
7.763178	495.381378	9.681203
7.912750	491.593244	9.686221
8.211454	477.863175	9.691239
7.649506	483.953620	9.696256
7.577051	485.748113	9.701274
8.555673	497.113458	9.706291
8.239448	503.698734	9.711309
8.111555	496.378588	9.716327
7.735266	489.198350	9.721344
7.832420	483.944688	9.726362
8.265391	488.506489	9.731379
7.745637	485.495408	9.736397
7.828905	499.885413	9.741415
8.099050	502.206888	9.746432
8.302590	502.774725	9.751450
8.268287	496.923126	9.756467
8.462123	499.789882	9.761485
8.146490	489.150886	9.766503
7.988741	483.577406	9.771520
8.238276	471.294075	9.776538
8.384745	473.284635	9.781555
8.163417	481.294062	9.786573
8.557500	477.650655	9.791591
8.039923	486.325031	9.796608
7.733068	480.162697	9.801626
8.135494	486.565938	9.806643
7.612420	487.629471	9.811661
7.876001	480.834966	9.816679
7.815545	488.147012	9.821696
8.098259	496.986331	9.826714
8.400452	504.512958	9.831731
8.157349	505.166555	9.836749
8.570940	504.000521	9.841767
8.253859	498.824382	9.846784
7.866166	500.977534	9.851802
8.143483	497.510207	9.856819
8.449496	504.029545	9.861837
8.357789	493.421732	9.866855
8.216044	493.696534	9.871872
8.338136	505.300230	9.876890
8.350104	496.314015	9.881907
8.204737	491.855735	9.886925
8.242939	497.132635	9.891943
8.311043	507.842243	9.896960
8.341413	501.406159	9.901978
8.407698	487.308561	9.906995
7.976762	479.269053	9.912013
8.351417	496.513548	9.917031
8.168292	506.612430	9.922048
8.353391	502.569422	9.927066
8.450654	503.942853	9.932083
8.308490	510.403029	9.937101
8.482332	505.560219	9.942119
8.370236	507.711215	9.947136
8.222081	506.049380	9.952154
8.705678	500.905575	9.957171
7.886820	495.072764	9.962189
8.069560	504.088695	9.967207
8.151792	512.208361	9.972224
7.904360	501.202069	9.977242
8.173021	514.404871	9.982259
8.202920	516.823950	9.987277
8.657621	507.017287	9.992295
8.522580	501.800002	9.997312
8.029665	500.933791	10.002330
8.615420	509.855021	10.007347
7.971259	514.175348	10.012365
8.479615	497.584844	10.017383
8.716137	507.908306	10.022400
8.433308	518.925367	10.027418
8.116312	508.018332	10.032435
8.059023	521.830782	10.037453
8.426013	528.952795	10.042471
8.706927	537.757703	10.047488
8.851140	531.641439	10.052506
8.741495	522.046267	10.057523
8.648222	511.788978	10.062541
8.623810	515.030756	10.067559
8.654497	510.955136	10.072576
8.562061	513.140921	10.077594
8.557563	517.408361	10.082611
8.568385	517.129089	10.087629
8.499870	508.048182	10.092647
8.719658	509.702214	10.097664
8.483976	502.998550	10.102682
8.924158	510.894875	10.107699
8.456222	518.889310	10.112717
8.704832	509.739779	10.117735
8.750583	513.822621	10.122752
8.627235	511.314308	10.127770
8.906654	509.206786	10.132787
8.843137	509.166378	10.137805
8.431272	515.599387	10.142823
8.399666	510.129210	10.147840
8.240989	505.556248	10.152858
8.382269	502.738232	10.157875
8.304704	513.041482	10.162893
8.682208	526.299822	10.167911
8.942366	542.394665	10.172928
8.594446	533.871914	10.177946
8.779557	518.682710	10.182963
8.758941	529.945869	10.187981
8.523564	534.397808	10.192999
8.823009	539.722151	10.198016
8.504768	541.996968	10.203034
8.616835	540.925512	10.208051
8.260435	538.242273	10.213069
8.650483	540.314595	10.218087
8.708747	540.760030	10.223104
8.619532	546.129492	10.228122
8.771930	534.337860	10.233139
8.584515	537.832398	10.238157
8.616617	543.760358	10.243175
8.626609	537.011877	10.248192
8.517864	538.023116	10.253210
8.814928	528.645080	10.258227
8.358449	545.167788	10.263245
8.801786	560.441846	10.268263
9.180351	569.868937	10.273280
8.916893	557.757442	10.278298
9.135784	542.812231	10.283315
8.886113	542.911443	10.288333
8.637245	529.213482	10.293351
9.044267	538.620319	10.298368
8.542866	548.948972	10.303386
9.294907	546.350831	10.308403
9.148990	557.964997	10.313421
9.105303	546.497567	10.318439
9.171069	542.419600	10.323456
9.013402	544.593519	10.328474
9.071733	538.276117	10.333491
8.861963	540.063727	10.338509
9.029336	537.036493	10.343527
8.871301	532.248831	10.348544
8.821677	544.419095	10.353562
8.842599	538.912276	10.358579
8.787351	541.584539	10.363597
8.710353	543.480734	10.368615
8.984686	544.700193	10.373632
9.033091	561.229015	10.378650
9.132294	558.079915	10.383667
8.985377	559.715670	10.388685
9.148655	568.728371	10.393703
9.148464	542.993164	10.398720
8.961725	544.919176	10.403738
8.869053	544.368945	10.408755
8.782521	565.333844	10.413773
9.159472	560.664320	10.418791
9.280550	564.457663	10.423808
9.177242	567.639229	10.428826
9.572102	560.306577	10.433843
9.038679	552.971053	10.438861
8.923312	545.194493	10.443879
9.119514	547.606454	10.448896
9.092161	562.291551	10.453914
9.403842	560.043270	10.458931
9.198352	561.612463	10.463949
8.893298	543.072864	10.468967
9.280965	546.489920	10.473984
9.232169	555.933471	10.479002
9.434506	557.628111	10.484019
9.414362	547.412992	10.489037
8.814824	540.125703	10.494055
8.947707	544.049734	10.499072
9.180061	558.217613	10.504090
9.193025	557.076478	10.509107
9.150393	563.606284	10.514125
9.166949	552.713231	10.519143
9.513771	557.825030	10.524160
9.181228	563.462995	10.529178
9.049195	555.436579	10.534195
9.398424	554.451038	10.539213
9.363941	569.279268	10.544231
9.488919	560.994831	10.549248
9.327048	564.946115	10.554266
9.453676	568.334649	10.559283
9.299794	562.725825	10.564301
9.100777	568.674227	10.569319
9.491706	565.567779	10.574336
9.603571	566.184696	10.579354
9.629221	566.193432	10.584371
9.530587	561.311249	10.589389
8.945227	550.477794	10.594407
9.317322	553.168307	10.599424
9.643637	561.006756	10.604442
9.831746	558.645294	10.609459
9.829844	544.671943	10.614477
9.504573	549.882734	10.619495
9.340200	534.454788	10.624512
8.755245	540.993821	10.629530
8.991346	544.885901	10.634547
8.996678	547.245718	10.639565
9.133197	568.708999	10.644583
9.266541	570.215636	10.649600
9.066755	565.084216	10.654618
9.469008	556.866788	10.659635
9.614837	566.983590	10.664653
8.954722	569.412961	10.669671
9.165703	572.425364	10.674688
9.322164	586.945982	10.679706
9.220154	589.029136	10.684723
9.625912	590.057593	10.689741
9.558105	601.804714	10.694759
9.648020	595.630665	10.699776
9.577398	593.543265	10.704794
9.691297	588.381623	10.709811
9.734054	598.025445	10.714829
9.680000	594.243949	10.719847
9.727072	585.845476	10.724864
9.309249	592.001737	10.729882
9.497552	592.032325	10.734899
9.762512	579.061698	10.739917
9.214174	588.507798	10.744935
9.501901	595.452911	10.749952
9.726602	595.196931	10.754970
9.929567	596.919878	10.759987
9.747914	594.234497	10.765005
9.522892	598.934137	10.770023
9.725771	590.773180	10.775040
9.483234	595.425071	10.780058
9.651212	604.023646	10.785075
9.605942	589.946601	10.790093
9.353124	585.858581	10.795111
9.787661	583.871912	10.800128
9.549832	590.230343	10.805146
9.391730	590.065900	10.810163
9.403495	584.478452	10.815181
9.787612	601.626892	10.820199
9.908494	603.245937	10.825216
9.698750	595.998535	10.830234
9.536956	586.319981	10.835251
9.831438	598.792970	10.840269
10.107679	614.595026	10.845287
10.076870	598.117310	10.850304
9.860414	597.662211	10.855322
9.417792	585.398890	10.860339
9.676940	595.387500	10.865357
9.585487	615.712605	10.870375
10.115637	608.159921	10.875392
10.366376	616.786560	10.880410
9.829692	608.271260	10.885427
9.920409	594.289669	10.890445
9.660637	592.556952	10.895463
10.184262	602.330558	10.900480
10.112257	596.166100	10.905498
9.700427	593.542031	10.910515
9.753454	598.258065	10.915533
9.769683	609.837390	10.920551
9.967102	611.744244	10.925568
9.941881	612.751868	10.930586
10.140303	626.341297	10.935603
10.445499	611.183692	10.940621
9.847063	610.883116	10.945639
10.056247	600.382728	10.950656
10.196177	603.261102	10.955674
10.059310	601.480725	10.960691
9.880110	590.252250	10.965709
10.208011	599.412741	10.970727
10.059518	587.302148	10.975744
10.313773	584.835645	10.980762
9.750932	586.280952	10.985779
10.423970	583.202882	10.990797
10.143262	587.409475	10.995815
9.785204	580.762826	11.000832
10.099465	590.039058	11.005850
9.824787	601.222149	11.010867
10.119905	603.012709	11.015885
10.185820	621.523832	11.020903
10.232881	617.852720	11.025920
10.305935	612.889973	11.030938
10.182571	608.699614	11.035955
10.363298	598.216308	11.040973
10.109698	600.395798	11.045991
10.064355	586.678528	11.051008
10.408772	596.388692	11.056026
10.305331	600.049964	11.061043
10.345086	588.105533	11.066061
9.961923	586.966503	11.071079
10.310410	593.668567	11.076096
10.357774	585.970632	11.081114
9.889362	596.836939	11.086131
10.300679	599.369836	11.091149
10.242912	615.419885	11.096167
10.841727	609.784629	11.101184
10.166648	596.787710	11.106202
9.917738	598.357398	11.111219
10.458847	597.546916	11.116237
10.113589	610.647167	11.121255
10.337884	606.926196	11.126272
10.534864	616.555331	11.131290
10.384551	616.424381	11.136307
10.292344	604.248153	11.141325
10.426595	618.059068	11.146343
10.139728	600.573748	11.151360
10.457864	608.946828	11.156378
10.214892	615.536446	11.161395
10.492897	613.479626	11.166413
10.459233	622.605263	11.171431
10.491988	614.821243	11.176448
10.162839	612.386187	11.181466
10.242687	622.494423	11.186483
10.507758	610.801851	11.191501
10.573982	616.718177	11.196519
10.512792	612.448647	11.201536
10.647178	614.011929	11.206554
10.388477	615.056136	11.211571
10.575167	611.470444	11.216589
10.631198	612.746202	11.221607
10.791174	605.267299	11.226624
10.799045	607.680375	11.231642
10.393347	610.543257	11.236659
10.746682	608.834395	11.241677
10.473929	605.257575	11.246695
10.420790	603.710230	11.251712
10.736027	601.410894	11.256730
10.238420	614.626536	11.261747
10.527175	619.946266	11.266765
10.554390	611.692902	11.271783
10.403847	624.428140	11.276800
10.760060	610.976136	11.281818
10.501735	618.325549	11.286835
10.884020	615.400327	11.291853
10.754153	624.642024	11.296871
10.548819	621.619524	11.301888
10.705233	620.408572	11.306906
10.459314	626.260200	11.311923
10.619830	619.623802	11.316941
10.775488	624.415281	11.321959
10.634387	617.198140	11.326976
10.426103	620.077429	11.331994
10.674364	618.047359	11.337011
10.766551	614.173518	11.342029
10.442688	616.992021	11.347047
10.366690	615.176859	11.352064
11.013951	607.189262	11.357082
10.681934	620.325314	11.362099
10.737767	604.458863	11.367117
10.576597	611.499563	11.372135
10.536839	613.348905	11.377152
10.648079	619.280269	11.382170
10.655444	632.546190	11.387187
10.737430	632.391466	11.392205
10.674996	640.663244	11.397223
10.698760	644.017417	11.402240
10.963351	636.493707	11.407258
10.919474	647.864726	11.412275
11.195478	642.968002	11.417293
11.240361	636.381273	11.422311
10.992827	643.325065	11.427328
11.166028	644.472014	11.432346
10.783083	635.194157	11.437363
10.798978	624.127595	11.442381
11.078559	629.830616	11.447399
10.892426	634.177035	11.452416
11.315415	631.766138	11.457434
10.637273	636.442111	11.462451
11.090792	636.923448	11.467469
10.815885	634.445176	11.472487
10.681042	640.591829	11.477504
10.998393	628.076859	11.482522
10.817040	644.468189	11.487539
11.279952	635.575349	11.492557
11.255069	641.468089	11.497575
11.265663	638.651594	11.502592
11.393001	642.974146	11.507610
11.023774	636.417588	11.512627
11.352676	635.454163	11.517645
11.033560	633.481432	11.522663
11.149806	628.761222	11.527680
10.839948	624.316058	11.532698
10.913867	639.439784	11.537715
10.944762	640.937233	11.542733
11.050477	636.316500	11.547751
11.101886	639.565355	11.552768
11.137163	644.703902	11.557786
10.628129	648.687509	11.562803
10.860282	643.583062	11.567821
11.190373	645.800490	11.572839
11.182568	647.054695	11.577856
11.427006	643.049695	11.582874
11.000806	645.202585	11.587891
11.294308	636.112228	11.592909
11.459702	635.120773	11.597927
11.315592	636.487852	11.602944
11.401536	641.893015	11.607962
10.946887	642.765954	11.612979
11.287024	645.212181	11.617997
11.503075	641.940617	11.623015
11.182203	642.196152	11.628032
11.420085	641.035549	11.633050
10.819648	652.859847	11.638067
11.316026	653.394429	11.643085
11.722010	660.182182	11.648103
11.403743	655.441684	11.653120
11.681029	645.201997	11.658138
11.279581	644.908425	11.663155
11.291391	640.943030	11.668173
11.515524	643.751414	11.673191
11.134089	649.419157	11.678208
11.711329	646.510720	11.683226
11.291254	648.820441	11.688243
11.210763	650.000829	11.693261
11.482410	668.363002	11.698279
11.277719	670.257127	11.703296
11.596213	666.152156	11.708314
11.513140	673.351057	11.713331
11.582981	680.163084	11.718349
11.463047	668.682277	11.723367
11.731852	672.196876	11.728384
11.654575	660.532666	11.733402
11.332740	670.628127	11.738419
11.396169	669.513791	11.743437
11.494502	662.975483	11.748455
11.276800	680.836831	11.753472
11.696419	667.412719	11.758490
11.365810	668.108435	11.763507
11.575950	667.245667	11.768525
11.851744	674.536662	11.773543
11.203934	679.719133	11.778560
11.708869	671.482409	11.783578
11.540205	674.686857	11.788595
11.696321	675.782837	11.793613
11.552740	672.454008	11.798631
11.583958	684.428664	11.803648
11.447303	674.092873	11.808666
11.655494	672.211087	11.813683
11.735162	675.837373	11.818701
11.535885	670.323990	11.823719
11.486666	669.492392	11.828736
11.901649	680.741042	11.833754
11.685154	673.087568	11.838771
11.406853	677.394790	11.843789
11.789554	689.683607	11.848807
11.772020	697.134180	11.853824
12.089789	696.835214	11.858842
12.089130	705.400301	11.863859
11.729014	690.886514	11.868877
11.854162	689.109256	11.873895
11.736633	697.203501	11.878912
12.053506	696.983571	11.883930
11.870909	697.037560	11.888947
12.089250	693.465827	11.893965
12.338449	679.298392	11.898983
12.002503	675.905029	11.904000
12.134147	670.548079	11.909018
12.136118	670.645732	11.914035
12.158537	669.203307	11.919053
12.255012	676.434037	11.924071
12.201192	667.050946	11.929088
12.095564	667.597802	11.934106
12.258112	676.364520	11.939123
11.928948	669.460847	11.944141
12.029058	670.704457	11.949159
11.675704	676.247888	11.954176
11.988178	678.408120	11.959194
11.648245	674.434714	11.964211
11.682000	672.993669	11.969229
11.985877	677.162336	11.974247
11.681188	677.992847	11.979264
12.046018	672.334272	11.984282
11.998928	689.490400	11.989299
11.694417	696.165429	11.994317
12.089975	705.839238	11.999335
11.815034	711.982620	12.004352
12.097813	692.896325	12.009370
11.996063	700.445301	12.014387
12.141618	707.264410	12.019405
12.134412	699.622314	12.024423
12.248146	702.066153	12.029440
11.747386	699.547519	12.034458
12.011631	700.418276	12.039475
11.900606	697.428323	12.044493
12.415962	686.106741	12.049511
12.178231	692.477815	12.054528
12.426465	696.068226	12.059546
12.445367	705.081527	12.064563
11.975658	701.207345	12.069581
11.924946	697.371654	12.074599
12.112265	714.989695	12.079616
12.448118	711.462663	12.084634
12.311510	728.837982	12.089651
12.082000	725.181779	12.094669
12.777020	711.736574	12.099687
12.522645	724.014780	12.104704
12.217756	714.973960	12.109722
12.340965	715.579637	12.114739
12.329709	726.516404	12.119757
12.689404	725.784835	12.124775
12.422493	732.122626	12.129792
12.458189	715.034778	12.134810
12.444137	711.673023	12.139827
12.796710	708.073944	12.144845
12.691730	700.478725	12.149863
12.231890	695.687814	12.154880
12.378704	699.347765	12.159898
13.014019	694.729244	12.164915
12.244163	697.163203	12.169933
12.394017	693.674784	12.174951
12.479996	702.431422	12.179968
12.264530	700.846387	12.184986
12.907716	720.485304	12.190003
12.619239	722.897492	12.195021
12.646249	704.359344	12.200039
12.361186	705.716955	12.205056
12.614947	712.799980	12.210074
13.127244	720.432634	12.215091
12.343216	713.565499	12.220109
12.558517	708.801345	12.225127
12.566660	720.511397	12.230144
12.702390	714.468984	12.235162
12.791935	719.731594	12.240179
12.655721	729.902147	12.245197
12.749876	717.816562	12.250215
12.904772	722.851183	12.255232
12.687932	727.865156	12.260250
12.892967	711.549199	12.265267
12.592977	717.093748	12.270285
12.925917	720.891799	12.275303
12.814690	719.587075	12.280320
12.716423	713.754895	12.285338
12.713458	715.809921	12.290355
12.318481	729.306212	12.295373
12.814272	721.610542	12.300391
13.051528	728.336396	12.305408
12.746621	730.025322	12.310426
13.087842	726.030386	12.315443
12.617435	725.687657	12.320461
12.900764	729.887958	12.325479
12.828269	731.117591	12.330496
13.185807	721.439644	12.335514
12.959663	721.102824	12.340531
12.899689	725.953362	12.345549
12.823870	720.139753	12.350567
13.193615	727.971472	12.355584
13.009984	729.022858	12.360602
13.213306	727.470033	12.365619
13.024468	728.881997	12.370637
13.093136	729.912787	12.375655
12.627704	726.463963	12.380672
12.442018	729.914085	12.385690
12.996216	726.684198	12.390707
12.918254	726.226330	12.395725
13.047501	721.387293	12.400743
12.912561	733.072436	12.405760
12.597526	729.779927	12.410778
13.023907	727.649353	12.415795
12.928082	731.902751	12.420813
13.167645	733.373824	12.425831
13.112206	729.579893	12.430848
13.069741	723.581176	12.435866
12.716653	735.647639	12.440883
12.770833	746.829787	12.445901
13.166023	748.260698	12.450919
13.309218	750.176062	12.455936
13.172877	753.968753	12.460954
13.107812	746.540830	12.465971
12.987920	752.729361	12.470989
13.452804	756.585640	12.476007
13.311412	756.361773	12.481024
13.143312	754.371679	12.486042
13.166599	748.198549	12.491059
12.959221	754.820510	12.496077
13.136316	749.039848	12.501095
13.587705	746.520345	12.506112
13.330350	751.922525	12.511130
13.591929	757.060362	12.516147
13.192740	753.736853	12.521165
13.589827	744.532380	12.526183
13.589930	750.291853	12.531200
13.354691	756.807727	12.536218
13.494008	748.085455	12.541235
13.320440	752.751826	12.546253
13.377449	751.004173	12.551271
13.506717	748.475180	12.556288
13.321822	748.845110	12.561306
13.448763	748.831665	12.566323
13.116490	753.276750	12.571341
13.323155	756.160472	12.576359
13.356035	751.121931	12.581376
13.188383	751.871012	12.586394
13.663070	748.101313	12.591411
13.586465	773.804931	12.596429
13.838496	770.019620	12.601447
13.497295	753.388423	12.606464
13.338089	755.212313	12.611482
13.821593	758.406111	12.616499
13.513119	762.307825	12.621517
13.803825	761.596531	12.626535
13.830415	756.517949	12.631552
13.898758	756.914472	12.636570
13.785744	754.265650	12.641587
13.366199	754.435660	12.646605
13.451033	741.101818	12.651623
13.782854	754.411667	12.656640
13.229049	766.856739	12.661658
13.660349	766.656749	12.666675
13.734483	779.855513	12.671693
13.818159	774.824786	12.676711
14.066706	776.509051	12.681728
13.943324	770.639761	12.686746
14.117044	767.759817	12.691763
13.509865	767.384868	12.696781
13.460828	769.182030	12.701799
13.776215	771.512232	12.706816
13.924344	777.463115	12.711834
14.282657	773.727423	12.716851
14.016035	776.271893	12.721869
13.949828	775.405082	12.726887
13.690473	765.770119	12.731904
13.505176	780.205586	12.736922
13.895439	775.881061	12.741939
13.548964	786.482224	12.746957
13.921319	783.747880	12.751975
14.034481	775.146458	12.756992
13.516342	783.849467	12.762010
13.804060	780.342586	12.767027
13.756648	778.462968	12.772045
14.059932	780.829781	12.777063
14.182090	773.486122	12.782080
13.945688	773.984043	12.787098
14.128379	767.921631	12.792115
14.099725	771.517571	12.797133
13.861368	773.789368	12.802151
14.334557	771.733506	12.807168
14.154067	773.986769	12.812186
14.332706	776.029127	12.817203
13.723725	770.273793	12.822221
13.966576	773.511611	12.827239
14.162291	771.559186	12.832256
13.938923	777.006542	12.837274
14.134083	780.229743	12.842291
13.964128	790.503447	12.847309
14.131686	799.092715	12.852327
14.557026	800.332713	12.857344
14.797661	796.454508	12.862362
13.995378	783.518408	12.867379
14.142644	777.079689	12.872397
14.036850	787.368585	12.877415
13.895513	792.168773	12.882432
14.158562	804.848803	12.887450
14.158602	804.530191	12.892467
14.264831	812.359054	12.897485
14.162078	805.871135	12.902503
14.427982	804.071812	12.907520
14.088616	802.805983	12.912538
14.277943	792.027726	12.917555
14.161008	796.792533	12.922573
14.114894	810.710753	12.927591
14.065138	802.822814	12.932608
14.335532	822.845305	12.937626
14.630098	828.318822	12.942643
14.606314	821.105308	12.947661
14.455804	822.646975	12.952679
14.761988	827.771531	12.957696
14.551641	806.745806	12.962714
14.462216	805.686970	12.967731
14.531313	798.799741	12.972749
14.099036	800.047881	12.977767
14.759041	816.219178	12.982784
14.492508	824.147477	12.987802
14.776987	814.073826	12.992819
14.873219	830.989882	12.997837
14.432051	825.848869	13.002855
14.596526	823.279635	13.007872
14.794790	832.914998	13.012890
14.569572	821.740925	13.017907
14.749298	822.893175	13.022925
14.678254	830.415304	13.027943
15.128173	826.564262	13.032960
14.561229	825.709633	13.037978
14.755268	816.631612	13.042995
14.941781	816.615144	13.048013
14.550001	808.736610	13.053031
14.799605	815.154448	13.058048
14.781448	823.851722	13.063066
14.565889	821.165307	13.068083
14.842089	820.377389	13.073101
14.739098	825.487160	13.078119
15.398492	819.570946	13.083136
15.036148	818.696883	13.088154
15.120076	809.314225	13.093171
14.707168	805.831909	13.098189
14.471246	812.000769	13.103207
15.162607	805.246414	13.108224
14.640224	807.458575	13.113242
14.908368	817.010396	13.118259
15.061705	822.171523	13.123277
15.063134	825.920552	13.128295
15.068624	824.114691	13.133312
14.764553	817.494209	13.138330
15.507361	821.641474	13.143347
14.821824	806.430651	13.148365
14.789689	817.414927	13.153383
15.382682	821.311109	13.158400
15.248071	825.062518	13.163418
14.609552	819.769391	13.168435
15.032780	818.819579	13.173453
14.882455	821.702442	13.178471
14.922985	821.257564	13.183488
14.890562	822.124316	13.188506
14.965094	822.762871	13.193523
15.291549	817.078706	13.198541
14.961574	825.263100	13.203559
15.021774	832.108254	13.208576
14.994391	829.524899	13.213594
14.894769	823.831752	13.218611
14.878221	825.248286	13.223629
14.814809	842.318755	13.228647
15.171216	843.680011	13.233664
15.521861	861.272607	13.238682
15.470239	849.629499	13.243699
15.554202	847.448421	13.248717
15.258432	850.748556	13.253735
15.431174	851.968175	13.258752
15.526397	851.224391	13.263770
15.444653	844.212454	13.268787
15.471952	835.577119	13.273805
15.351729	835.151117	13.278823
15.300095	838.933709	13.283840
15.077725	848.584493	13.288858
15.197010	841.853487	13.293875
16.123840	847.789683	13.298893
15.825565	847.969094	13.303911
15.711077	834.789491	13.308928
15.493590	831.251303	13.313946
15.436437	824.254457	13.318963
15.320907	825.778019	13.323981
15.550607	833.076301	13.328999
15.619248	829.884605	13.334016
15.647331	845.135609	13.339034
15.547311	839.382558	13.344051
15.619378	845.165499	13.349069
15.466828	848.219130	13.354087
15.554500	850.171607	13.359104
15.380867	852.613155	13.364122
15.348091	857.822388	13.369139
15.356063	855.542761	13.374157
15.445575	854.670482	13.379175
15.872257	846.389134	13.384192
15.533557	854.054197	13.389210
15.268961	857.892252	13.394227
15.641926	848.596831	13.399245
15.398988	856.818095	13.404263
15.612055	851.180088	13.409280
15.812955	866.883719	13.414298
15.806630	865.606730	13.419315
16.173177	872.785756	13.424333
15.832095	871.952540	13.429351
16.135914	864.485705	13.434368
15.886167	860.655919	13.439386
15.750642	853.399939	13.444403
15.797177	848.431815	13.449421
15.576422	857.205030	13.454439
15.924992	861.622360	13.459456
16.356803	872.174213	13.464474
15.894604	872.511854	13.469491
15.925121	871.131261	13.474509
15.551268	872.098850	13.479527
15.868958	864.696114	13.484544
16.089871	865.400097	13.489562
15.999473	870.776154	13.494579
16.067511	870.285939	13.499597
15.965654	872.271271	13.504615
15.966359	875.329296	13.509632
15.787469	868.818569	13.514650
15.902806	863.994297	13.519667
16.487291	869.725361	13.524685
15.921547	871.597182	13.529703
16.142806	868.185905	13.534720
16.070782	876.598152	13.539738
15.821783	875.122497	13.544755
16.120749	872.014628	13.549773
16.006701	875.065386	13.554791
16.332829	864.906284	13.559808
16.461108	869.279237	13.564826
16.006604	877.539972	13.569843
16.359015	864.438671	13.574861
16.440214	876.771701	13.579879
16.091630	870.192888	13.584896
16.536394	880.720625	13.589914
16.378207	872.587709	13.594931
16.380408	865.594170	13.599949
16.158365	874.803101	13.604967
16.359652	885.883391	13.609984
16.654235	883.628281	13.615002
16.539115	887.540753	13.620019
16.671323	873.574534	13.625037
16.232477	866.132542	13.630055
16.251933	865.271239	13.635072
16.570981	866.919220	13.640090
16.528779	881.354439	13.645107
16.838738	884.496555	13.650125
16.813473	874.897440	13.655143
16.507894	866.797089	13.660160
16.471876	867.793796	13.665178
16.280196	863.547808	13.670195
16.657735	861.794104	13.675213
16.648594	884.542920	13.680231
16.729430	888.831791	13.685248
17.103356	878.475843	13.690266
16.519312	871.170210	13.695283
16.700548	865.669730	13.700301
16.628243	866.302891	13.705319
16.506013	872.242517	13.710336
16.908668	876.938558	13.715354
16.655959	882.239063	13.720371
17.224102	869.536306	13.725389
16.689404	867.493185	13.730407
16.692179	866.625028	13.735424
16.652024	861.137148	13.740442
16.594049	874.605992	13.745459
16.635941	881.062710	13.750477
16.970499	890.193906	13.755495
16.836806	891.893891	13.760512
17.177082	899.856536	13.765530
16.748071	891.778669	13.770547
16.919823	883.429950	13.775565
17.209866	886.833966	13.780583
16.864504	889.422347	13.785600
17.069441	890.636925	13.790618
16.846980	894.263256	13.795635
17.209729	893.215618	13.800653
16.853963	896.932265	13.805671
17.161845	891.825349	13.810688
16.947032	885.929322	13.815706
16.770538	885.105032	13.820723
16.839590	882.374014	13.825741
16.903364	879.934161	13.830759
16.663009	887.261933	13.835776
17.111596	876.673380	13.840794
16.482418	895.678709	13.845811
17.004815	885.271091	13.850829
16.974309	893.212933	13.855847
17.063972	897.386813	13.860864
17.404771	897.674378	13.865882
17.106335	903.947741	13.870899
17.238767	901.727503	13.875917
17.432393	905.029864	13.880935
17.214537	903.293704	13.885952
17.417845	907.768520	13.890970
17.114361	912.158640	13.895987
17.275801	911.814737	13.901005
17.809852	922.379003	13.906023
17.530518	908.843316	13.911040
17.768287	885.891652	13.916058
17.689405	886.844583	13.921075
17.414793	877.981974	13.926093
17.257448	892.974890	13.931111
17.091853	888.320862	13.936128
17.536538	890.028055	13.941146
17.253203	888.131742	13.946163
17.597462	887.487793	13.951181
17.359413	891.485799	13.956199
17.698782	886.506496	13.961216
17.614590	886.740728	13.966234
17.576072	895.946161	13.971251
17.553080	882.228317	13.976269
17.345702	879.644754	13.981287
17.258423	896.962014	13.986304
17.748623	908.173777	13.991322
17.748765	913.854401	13.996339
17.931016	912.743524	14.001357
17.552490	911.070408	14.006375
17.737293	908.491665	14.011392
17.876736	910.644323	14.016410
17.662398	904.653540	14.021427
17.821643	907.200730	14.026445
17.753939	910.181116	14.031463
17.593385	897.583047	14.036480
17.840558	909.725991	14.041498
17.606331	904.369492	14.046515
17.854950	907.202484	14.051533
18.038574	909.976232	14.056551
18.078367	910.793803	14.061568
18.116570	907.944538	14.066586
17.705117	901.325069	14.071603
18.148848	900.665534	14.076621
17.889620	892.690454	14.081639
17.458847	893.909962	14.086656
17.891316	897.591469	14.091674
17.519269	905.208129	14.096691
17.952877	907.040138	14.101709
18.093405	908.520431	14.106727
17.960040	916.835010	14.111744
18.109149	909.711137	14.116762
18.057843	911.338254	14.121779
18.391433	909.361055	14.126797
18.264380	905.265879	14.131815
17.921596	906.332744	14.136832
18.300889	909.631262	14.141850
18.039411	908.081819	14.146867
18.152923	897.072378	14.151885
18.166994	909.119300	14.156903
18.179061	910.199995	14.161920
18.522231	906.390908	14.166938
18.335558	904.533097	14.171955
18.787014	903.184378	14.176973
18.524402	903.045775	14.181991
18.149462	894.628071	14.187008
18.425668	894.051590	14.192026
18.117827	903.090939	14.197043
18.258659	896.691055	14.202061
18.511079	907.324686	14.207079
18.037012	918.554994	14.212096
18.351672	906.311655	14.217114
18.504679	912.993975	14.222131
18.307463	899.066727	14.227149
18.427146	904.592917	14.232167
18.469744	901.294834	14.237184
18.325835	904.602743	14.242202
18.464323	905.673097	14.247219
18.642659	909.397581	14.252237
18.343795	903.476847	14.257255
18.025719	907.316980	14.262272
18.418201	906.270994	14.267290
18.204795	910.605974	14.272307
17.928685	909.873031	14.277325
18.534866	919.495020	14.282343
18.301032	929.819839	14.287360
18.695177	940.636413	14.292378
18.441808	935.273436	14.297395
18.467940	936.033189	14.302413
18.776023	930.313997	14.307431
18.688662	941.805625	14.312448
18.731522	937.128390	14.317466
18.652474	935.203219	14.322483
18.433858	937.980034	14.327501
18.772999	932.177079	14.332519
18.398974	943.315988	14.337536
18.779142	936.739733	14.342554
18.832624	949.749352	14.347571
18.932534	953.325184	14.352589
18.979099	949.366899	14.357607
18.839929	950.253539	14.362624
19.202200	945.248541	14.367642
18.911927	937.757994	14.372659
18.797762	933.768090	14.377677
18.879070	944.602125	14.382695
18.874195	960.315988	14.387712
19.051050	956.308884	14.392730
19.005694	961.438066	14.397747
19.002734	963.054457	14.402765
19.268349	949.439667	14.407783
19.091532	953.749989	14.412800
19.041824	958.598981	14.417818
19.243974	958.974544	14.422835
19.194977	954.699867	14.427853
19.335715	955.975001	14.432871
19.123439	958.690865	14.437888
19.373079	948.363818	14.442906
19.698464	953.176129	14.447923
19.369681	947.196951	14.452941
19.252976	932.458634	14.457959
19.073021	928.071936	14.462976
19.350900	935.062906	14.467994
19.243784	918.899812	14.473011
18.977337	930.706675	14.478029
19.509930	933.930684	14.483047
19.689626	951.193543	14.488064
19.492069	934.523890	14.493082
19.602682	927.390262	14.498099
19.253465	931.263682	14.503117
19.685971	925.038996	14.508135
19.465479	925.149416	14.513152
19.304843	921.908420	14.518170
19.195937	926.438471	14.523187
19.657901	938.301625	14.528205
19.689990	937.627690	14.533223
19.545335	933.014551	14.538240
19.673262	926.544094	14.543258
19.549167	923.590866	14.548275
19.241332	926.410060	14.553293
19.507559	935.315298	14.558311
19.208875	944.217532	14.563328
19.825452	955.087627	14.568346
19.608256	954.809361	14.573363
19.449143	962.212799	14.578381
19.767133	952.083326	14.583399
19.816937	953.625176	14.588416
19.517065	949.503418	14.593434
19.402623	949.915963	14.598451
19.577993	947.168277	14.603469
19.788897	948.647015	14.608487
19.844565	957.070851	14.613504
19.804179	946.912325	14.618522
19.603096	953.549152	14.623539
19.434484	959.631777	14.628557
19.736373	970.153551	14.633575
19.725858	981.961373	14.638592
19.738005	967.054514	14.643610
19.839398	978.573397	14.648627
19.719303	979.169867	14.653645
20.191661	968.536508	14.658663
20.129497	977.976066	14.663680
19.996615	973.771332	14.668698
20.225117	974.493066	14.673715
19.591145	978.041878	14.678733
19.890819	970.105426	14.683751
19.999469	977.593150	14.688768
19.806571	973.208469	14.693786
19.976247	977.357208	14.698803
20.372573	993.229149	14.703821
20.906707	985.464242	14.708839
20.123141	979.537374	14.713856
20.283865	974.639688	14.718874
20.511215	961.194988	14.723891
20.025126	971.003925	14.728909
20.328574	965.790384	14.733927
20.122484	970.461908	14.738944
20.017238	969.594892	14.743962
20.589758	981.525961	14.748979
20.424340	990.202207	14.753997
20.260616	983.938374	14.759015
20.313794	982.371183	14.764032
20.729557	991.669591	14.769050
20.576163	994.691820	14.774067
20.423556	995.498515	14.779085
20.511288	981.507622	14.784103
20.134498	976.993960	14.789120
20.698904	982.052856	14.794138
20.957786	983.618755	14.799155
20.521773	975.412556	14.804173
20.506865	963.280777	14.809191
20.452128	970.699423	14.814208
20.670199	979.448123	14.819226
20.709107	986.741648	14.824243
20.506959	988.663810	14.829261
20.790993	990.834849	14.834279
20.888337	994.837133	14.839296
20.798194	986.437880	14.844314
20.669328	987.676363	14.849331
20.385593	992.773475	14.854349
20.506874	988.475265	14.859367
20.854033	992.523615	14.864384
20.401564	982.363362	14.869402
20.740695	982.575450	14.874419
20.961735	996.937957	14.879437
21.129201	984.547211	14.884455
20.780032	984.254908	14.889472
20.681964	989.995126	14.894490
21.208644	993.074903	14.899507
21.017554	989.349508	14.904525
21.010027	993.043170	14.909543
21.052857	985.004942	14.914560
20.543295	991.276700	14.919578
21.168415	992.984035	14.924595
21.222582	993.288110	14.929613
21.163827	994.626063	14.934631
21.488954	991.618217	14.939648
21.074156	996.379254	14.944666
21.211007	985.325075	14.949683
20.799979	995.384201	14.954701
21.072196	990.816185	14.959719
21.427550	984.893906	14.964736
21.308629	985.493348	14.969754
21.170354	983.302892	14.974771
21.043820	987.576941	14.979789
20.985839	984.158900	14.984807
21.083086	993.702879	14.989824
21.038362	1015.532771	14.994842
21.459911	1006.204410	14.999859
21.339565	1020.134423	15.004877
21.451836	1016.317310	15.009895
21.622465	1013.642941	15.014912
21.576647	1004.078535	15.019930
21.644780	1015.596342	15.024947
21.295783	1015.171465	15.029965
21.367658	1014.712204	15.034983
21.659514	1018.781848	15.040000
21.601048	1021.252712	15.045018
21.714800	1014.686612	15.050035
21.633963	1022.753164	15.055053
21.463091	1020.517317	15.060071
21.693975	1017.546324	15.065088
21.310667	1015.157567	15.070106
21.549245	1008.991641	15.075123
21.609367	1019.844820	15.080141
21.658745	1017.107396	15.085159
21.750152	1015.231250	15.090176
21.711343	1016.461936	15.095194
22.007785	1018.204993	15.100211
21.913252	1013.022237	15.105229
21.716185	1018.042659	15.110247
21.959175	1009.256679	15.115264
21.857845	1008.471099	15.120282
22.231757	1007.573188	15.125299
21.942443	1011.632902	15.130317
21.921796	1017.181114	15.135335
21.971268	1023.024459	15.140352
21.879610	1017.225858	15.145370
21.797928	1018.854588	15.150387
21.933752	1019.694989	15.155405
21.808438	1017.679226	15.160423
21.533936	1015.431214	15.165440
21.520454	1014.347843	15.170458
21.879967	1011.874258	15.175475
21.608781	1019.891737	15.180493
21.919586	1027.347808	15.185511
22.387514	1033.071942	15.190528
22.146760	1034.555181	15.195546
22.207316	1033.419182	15.200563
22.130157	1039.263438	15.205581
22.513279	1036.846112	15.210599
22.492332	1030.802894	15.215616
22.164807	1040.265126	15.220634
22.367792	1026.571726	15.225651
22.146753	1035.682750	15.230669
22.166241	1039.463709	15.235687
22.389832	1028.408536	15.240704
22.556866	1037.417731	15.245722
22.547955	1027.834906	15.250739
22.271359	1034.691882	15.255757
22.523109	1034.485308	15.260775
22.549898	1028.582937	15.265792
22.046726	1035.115645	15.270810
22.603790	1023.638991	15.275827
22.695278	1032.937735	15.280845
22.438978	1030.219802	15.285863
22.420376	1035.098656	15.290880
22.337001	1036.904381	15.295898
22.421364	1037.566650	15.300915
22.405728	1036.515174	15.305933
22.461066	1031.911700	15.310951
22.611064	1029.218471	15.315968
22.892887	1046.083560	15.320986
22.645792	1045.917277	15.326003
22.375416	1046.322697	15.331021
22.817368	1059.937417	15.336039
23.334750	1054.245354	15.341056
22.987935	1052.658775	15.346074
22.658266	1038.174649	15.351091
22.830853	1048.057153	15.356109
22.663682	1055.742764	15.361127
22.839727	1064.270868	15.366144
23.112840	1060.056152	15.371162
23.046907	1052.217975	15.376179
23.122602	1056.741227	15.381197
22.665531	1054.490256	15.386215
23.338070	1055.063524	15.391232
22.925488	1055.172483	15.396250
23.318371	1056.338689	15.401267
23.325381	1064.539822	15.406285
23.248207	1049.451225	15.411303
23.559856	1045.811152	15.416320
23.468713	1039.409694	15.421338
22.978056	1026.254173	15.426355
22.974362	1029.341316	15.431373
22.979123	1033.269750	15.436391
22.696315	1040.143481	15.441408
23.173950	1049.773059	15.446426
23.308335	1042.155970	15.451443
23.218741	1044.420271	15.456461
23.289009	1052.097080	15.461479
23.417309	1040.179500	15.466496
23.459348	1054.901467	15.471514
23.517990	1050.322717	15.476531
23.507568	1046.114559	15.481549
23.379050	1054.355857	15.486567
23.533411	1051.920721	15.491584
23.252598	1053.091496	15.496602
23.501801	1050.493176	15.501619
23.568141	1053.190646	15.506637
23.505203	1061.607868	15.511655
23.272922	1051.277374	15.516672
23.388289	1056.457141	15.521690
23.684637	1053.472729	15.526707
23.407993	1051.865689	15.531725
23.553605	1049.390899	15.536743
23.454086	1046.048783	15.541760
23.638472	1053.512050	15.546778
23.757001	1053.010763	15.551795
23.640055	1068.480344	15.556813
23.652354	1073.805656	15.561831
23.891973	1074.973786	15.566848
23.958614	1082.846841	15.571866
24.039000	1074.136800	15.576883
23.660514	1074.928396	15.581901
24.193526	1077.338152	15.586919
24.145301	1068.951227	15.591936
23.767874	1079.175552	15.596954
23.816232	1069.066168	15.601971
23.814691	1076.189339	15.606989
23.905290	1076.143717	15.612007
24.049054	1069.664415	15.617024
24.183992	1068.002353	15.622042
24.370291	1079.340738	15.627059
24.545582	1065.424424	15.632077
24.312988	1076.250916	15.637095
24.162846	1068.271288	15.642112
24.165668	1071.158598	15.647130
24.375332	1068.067843	15.652147
24.279440	1056.403134	15.657165
23.946265	1054.700807	15.662183
24.413584	1063.577757	15.667200
24.318602	1075.761802	15.672218
24.319848	1069.822392	15.677235
24.258976	1072.397784	15.682253
24.268929	1071.291802	15.687271
24.602325	1076.140762	15.692288
24.458958	1074.932568	15.697306
24.651153	1074.265101	15.702323
24.356447	1073.913769	15.707341
24.436973	1072.197115	15.712359
24.553336	1070.894576	15.717376
24.402799	1075.683658	15.722394
24.297325	1074.412721	15.727411
24.435614	1078.241347	15.732429
24.310976	1066.527486	15.737447
24.706825	1076.741105	15.742464
24.499410	1071.219405	15.747482
24.596360	1073.233571	15.752499
24.525866	1073.661323	15.757517
24.611933	1075.194346	15.762535
24.693017	1068.298823	15.767552
24.386402	1071.016862	15.772570
24.351763	1077.596098	15.777587
24.714631	1089.812558	15.782605
24.455573	1094.101085	15.787623
24.789724	1095.942385	15.792640
25.164688	1091.670677	15.797658
24.934683	1100.953556	15.802675
25.318760	1100.060359	15.807693
24.719618	1098.516467	15.812711
25.173712	1101.118476	15.817728
24.969839	1098.354448	15.822746
24.512004	1088.639952	15.827763
25.566539	1086.527684	15.832781
24.724859	1099.892268	15.837799
24.879188	1084.262429	15.842816
24.971890	1096.483354	15.847834
24.707269	1091.576539	15.852851
25.052618	1094.981397	15.857869
25.154894	1096.183672	15.862887
25.294435	1085.959004	15.867904
25.257973	1095.328323	15.872922
25.111266	1094.382589	15.877939
25.534560	1103.399003	15.882957
25.299342	1095.940789	15.887975
25.542583	1095.432584	15.892992
25.713919	1098.839462	15.898010
25.385097	1097.196410	15.903027
25.435290	1090.905335	15.908045
25.198285	1092.154457	15.913063
25.604235	1092.223530	15.918080
25.377256	1096.952009	15.923098
25.653884	1100.686380	15.928115
25.765765	1104.926257	15.933133
25.586398	1103.629026	15.938151
25.353312	1093.831975	15.943168
25.522036	1105.457158	15.948186
25.540484	1112.387859	15.953203
25.417724	1108.468692	15.958221
25.468102	1119.134105	15.963239
26.171641	1103.714850	15.968256
25.972934	1111.578999	15.973274
25.784115	1111.002788	15.978291
26.205833	1113.120711	15.983309
25.939836	1109.678433	15.988327
25.763535	1112.303474	15.993344
26.057650	1115.290321	15.998362
25.957200	1109.530938	16.003379
26.033296	1105.981411	16.008397
25.703841	1106.885249	16.013415
25.865865	1098.541110	16.018432
26.117717	1102.844264	16.023450
26.129071	1114.550916	16.028467
25.936086	1117.816059	16.033485
25.895961	1119.324676	16.038503
25.770307	1114.345587	16.043520
26.237021	1102.195057	16.048538
25.862421	1107.612558	16.053555
26.036584	1113.922401	16.058573
25.967481	1111.566453	16.063591
26.124340	1109.702133	16.068608
26.180053	1106.275722	16.073626
25.940855	1105.492805	16.078643
25.945275	1103.261041	16.083661
26.001786	1131.178676	16.088679
26.294650	1133.888005	16.093696
26.325439	1140.094086	16.098714
26.481022	1139.927826	16.103731
26.889527	1130.184868	16.108749
26.541550	1130.482525	16.113767
26.922347	1129.097524	16.118784
26.922116	1125.897631	16.123802
26.556855	1113.703876	16.128819
26.556506	1110.314651	16.133837
26.479531	1114.290625	16.138855
26.399188	1099.331873	16.143872
26.755441	1110.883495	16.148890
26.506666	1117.916028	16.153907
26.679582	1117.093786	16.158925
27.075342	1121.292345	16.163943
26.803847	1116.437094	16.168960
26.682584	1105.669441	16.173978
26.537324	1116.801017	16.178995
26.939320	1117.082154	16.184013
27.027876	1128.612613	16.189031
27.208284	1123.718114	16.194048
26.758651	1104.433704	16.199066
26.801645	1110.189728	16.204083
27.138342	1118.070980	16.209101
27.001871	1109.912462	16.214119
26.672172	1102.746766	16.219136
26.973252	1108.276155	16.224154
27.003889	1117.783299	16.229171
26.790891	1109.090805	16.234189
27.283390	1117.462053	16.239207
27.073003	1116.384281	16.244224
27.106021	1123.479964	16.249242
27.018097	1122.401939	16.254259
27.001558	1115.240820	16.259277
27.313645	1115.015325	16.264295
27.065307	1114.328516	16.269312
27.257124	1121.695970	16.274330
27.607404	1116.957897	16.279347
27.578301	1118.455319	16.284365
27.376504	1125.221713	16.289383
27.177742	1115.652807	16.294400
27.073916	1107.659593	16.299418
27.344909	1124.166685	16.304435
27.595424	1119.595725	16.309453
27.144711	1118.514580	16.314471
27.330339	1124.570161	16.319488
27.849165	1136.976818	16.324506
27.388730	1130.737331	16.329523
27.692368	1126.662987	16.334541
27.220283	1133.670554	16.339559
27.627684	1136.406119	16.344576
27.759678	1142.561630	16.349594
27.645326	1149.203875	16.354611
28.032494	1143.421731	16.359629
27.961826	1144.408103	16.364647
28.042685	1148.018519	16.369664
27.826548	1139.399087	16.374682
27.742705	1149.410191	16.379699
27.969498	1141.160027	16.384717
28.001764	1151.686283	16.389735
27.603369	1151.638381	16.394752
28.141607	1139.981561	16.399770
27.701717	1142.064068	16.404787
27.615286	1147.411183	16.409805
27.685004	1145.708839	16.414823
27.814854	1140.749670	16.419840
27.859357	1137.498584	16.424858
27.758652	1151.498208	16.429875
27.716423	1160.849529	16.434893
27.988346	1171.221479	16.439911
27.999376	1164.324272	16.444928
28.600116	1162.857469	16.449946
28.452853	1173.500232	16.454963
28.639687	1167.519088	16.459981
28.516210	1165.884883	16.464999
28.422948	1169.491026	16.470016
28.440019	1151.796593	16.475034
28.478968	1162.432264	16.480051
28.676603	1156.670344	16.485069
28.789648	1160.083210	16.490087
28.219339	1155.827047	16.495104
28.477383	1155.237624	16.500122
28.724674	1162.467012	16.505139
28.558434	1149.241634	16.510157
28.468813	1155.192025	16.515175
28.256113	1157.453538	16.520192
28.540714	1163.859707	16.525210
28.588939	1166.427486	16.530227
28.585077	1158.724707	16.535245
28.818322	1161.317146	16.540263
28.392161	1159.897628	16.545280
28.665418	1156.478149	16.550298
28.730976	1154.325165	16.555315
28.689166	1157.490888	16.560333
28.787563	1155.758802	16.565351
28.755097	1165.477834	16.570368
28.932006	1163.733446	16.575386
28.604384	1165.668975	16.580403
28.716400	1148.893811	16.585421
28.817380	1166.380655	16.590439
29.231845	1181.520913	16.595456
29.376326	1173.400399	16.600474
29.355989	1180.037394	16.605491
29.000803	1166.510239	16.610509
29.186947	1165.332464	16.615527
29.143293	1181.383966	16.620544
29.279259	1177.888161	16.625562
28.999983	1179.175471	16.630579
29.041032	1171.708654	16.635597
29.164973	1174.292973	16.640615
29.022637	1181.498208	16.645632
29.545691	1164.065320	16.650650
29.709282	1176.764355	16.655667
29.285163	1169.973196	16.660685
29.525119	1179.681112	16.665703
29.186058	1172.406398	16.670720
29.290284	1171.209898	16.675738
29.241754	1174.124206	16.680755
29.154496	1176.845761	16.685773
29.943493	1174.929728	16.690791
29.136867	1188.096375	16.695808
29.554249	1181.574162	16.700826
30.012974	1200.393579	16.705843
29.509256	1196.215337	16.710861
29.866086	1190.150745	16.715879
29.560336	1197.753985	16.720896
30.214356	1200.542441	16.725914
29.943152	1197.022064	16.730931
30.049209	1190.668550	16.735949
29.949704	1177.880831	16.740967
29.474223	1174.341971	16.745984
29.636102	1182.979653	16.751002
29.801246	1195.782602	16.756019
29.869973	1199.271850	16.761037
30.265589	1188.154911	16.766055
29.966214	1200.118593	16.771072
29.964054	1193.289715	16.776090
30.260042	1199.602592	16.781107
30.097160	1196.131517	16.786125
30.544652	1188.859794	16.791143
29.962915	1200.391178	16.796160
30.051563	1205.537304	16.801178
30.352687	1206.926187	16.806195
30.328766	1205.330030	16.811213
30.546115	1185.385591	16.816231
30.233992	1198.458987	16.821248
30.055959	1191.490403	16.826266
30.426401	1196.923744	16.831283
30.493705	1193.634360	16.836301
30.760830	1192.431271	16.841319
30.236013	1202.852332	16.846336
30.330517	1192.650440	16.851354
30.766189	1197.896831	16.856371
30.410055	1192.676113	16.861389
30.667242	1186.535613	16.866407
30.487754	1195.311995	16.871424
30.182735	1188.615781	16.876442
30.341199	1191.033743	16.881459
30.262950	1204.827914	16.886477
31.109310	1213.547718	16.891495
30.847241	1221.062070	16.896512
31.016267	1213.909709	16.901530
31.106695	1211.004873	16.906547
31.085291	1211.860450	16.911565
31.127176	1196.519538	16.916583
30.773005	1193.362465	16.921600
30.898558	1200.210145	16.926618
30.936468	1211.215248	16.931635
31.274601	1213.030690	16.936653
31.353971	1214.700478	16.941671
30.921893	1209.703099	16.946688
30.798070	1204.692138	16.951706
31.208540	1203.444497	16.956723
31.109709	1213.265475	16.961741
31.154925	1207.947154	16.966759
30.893997	1217.670451	16.971776
31.066140	1212.840341	16.976794
31.204867	1209.385124	16.981811
30.891029	1213.265684	16.986829
31.000708	1212.929886	16.991847
30.868842	1218.445092	16.996864
31.590282	1225.874779	17.001882
31.439014	1229.335383	17.006899
31.622758	1229.754863	17.011917
31.561875	1230.420961	17.016935
31.737398	1231.453974	17.021952
31.458104	1229.348700	17.026970
31.736342	1227.954514	17.031987
31.655526	1228.484875	17.037005
31.500787	1227.549860	17.042023
31.535072	1237.249005	17.047040
31.802641	1229.383743	17.052058
31.753639	1226.396607	17.057075
31.625837	1235.546775	17.062093
32.115129	1233.456781	17.067111
31.758709	1232.868954	17.072128
32.006625	1229.229364	17.077146
32.400250	1215.256634	17.082163
32.055742	1228.278319	17.087181
32.243770	1230.827359	17.092199
31.951013	1231.472981	17.097216
32.104803	1224.206234	17.102234
32.076848	1231.747028	17.107251
31.971018	1230.750698	17.112269
32.118275	1225.211251	17.117287
31.925954	1228.204903	17.122304
31.604486	1234.721837	17.127322
31.908469	1225.478056	17.132339
32.016668	1227.462074	17.137357
32.270199	1227.567654	17.142375
32.071345	1222.022474	17.147392
32.177384	1246.082337	17.152410
32.302174	1245.687364	17.157427
32.036880	1251.305539	17.162445
32.357606	1250.289714	17.167463
32.386649	1248.439094	17.172480
32.457971	1245.029147	17.177498
32.219460	1259.757368	17.182515
32.534442	1256.539623	17.187533
32.604906	1251.637068	17.192551
32.252635	1256.224268	17.197568
32.466210	1243.617829	17.202586
32.828623	1250.570432	17.207603
32.521575	1253.487387	17.212621
32.519151	1258.310117	17.217639
33.233209	1269.606959	17.222656
32.906408	1273.095075	17.227674
32.931783	1260.398187	17.232691
32.704128	1266.676365	17.237709
32.911912	1262.869481	17.242727
33.305750	1273.288662	17.247744
33.130744	1264.968849	17.252762
33.198108	1247.228570	17.257779
32.960562	1245.691127	17.262797
32.807481	1246.144447	17.267815
33.128218	1265.645136	17.272832
33.160045	1263.147118	17.277850
33.268982	1260.018462	17.282867
32.984143	1269.855991	17.287885
33.628970	1264.099711	17.292903
33.280024	1263.532804	17.297920
33.108200	1261.467494	17.302938
33.264398	1264.573809	17.307955
33.438091	1268.412708	17.312973
33.413578	1267.144852	17.317991
33.697088	1268.902584	17.323008
33.430783	1262.421189	17.328026
33.261721	1255.902469	17.333043
33.285921	1264.378719	17.338061
33.354036	1266.741419	17.343079
33.465256	1264.824271	17.348096
33.699054	1256.696037	17.353114
33.808386	1256.631700	17.358131
33.697866	1263.730994	17.363149
33.437969	1256.197681	17.368167
33.749731	1258.995590	17.373184
33.812831	1261.763030	17.378202
33.753258	1261.090821	17.383219
33.706979	1285.171445	17.388237
34.178082	1285.672140	17.393255
33.641386	1290.954141	17.398272
33.922468	1295.429494	17.403290
34.110984	1283.956768	17.408307
33.841640	1283.336361	17.413325
33.964989	1283.260360	17.418343
34.068635	1284.512928	17.423360
34.170503	1289.322481	17.428378
34.438194	1285.070691	17.433395
34.068828	1292.396751	17.438413
34.209589	1279.530287	17.443431
34.225348	1280.717726	17.448448
33.816596	1281.463578	17.453466
34.447693	1285.417013	17.458483
34.201857	1292.543831	17.463501
34.378529	1281.656806	17.468519
34.319493	1280.766754	17.473536
34.448614	1281.125364	17.478554
34.777769	1279.088859	17.483571
34.265065	1284.515428	17.488589
34.587717	1287.355817	17.493607
34.778201	1292.912061	17.498624
34.785509	1287.470263	17.503642
34.678326	1287.039050	17.508659
34.210746	1297.839375	17.513677
34.467102	1295.722753	17.518695
35.119641	1305.785829	17.523712
35.006145	1297.658341	17.528730
35.097050	1293.803489	17.533747
35.122651	1307.606715	17.538765
35.171989	1293.618437	17.543783
35.004177	1280.317466	17.548800
34.707270	1277.492244	17.553818
34.954930	1277.153761	17.558835
34.810577	1290.308238	17.563853
35.045813	1299.843384	17.568871
35.094971	1297.124888	17.573888
35.111228	1302.664250	17.578906
35.277467	1301.306542	17.583923
35.041587	1300.283246	17.588941
35.362767	1296.016761	17.593959
35.217988	1293.552721	17.598976
35.150353	1292.531468	17.603994
34.836095	1289.753146	17.609011
34.879299	1294.663413	17.614029
34.934606	1298.255772	17.619047
35.122862	1316.183540	17.624064
35.423758	1322.965923	17.629082
35.581189	1319.116422	17.634099
35.336507	1321.149428	17.639117
35.451495	1318.758297	17.644135
35.699518	1318.123101	17.649152
35.891246	1322.262155	17.654170
35.902022	1322.506760	17.659187
35.747282	1326.914701	17.664205
35.927364	1322.900698	17.669223
36.073907	1326.494547	17.674240
35.953370	1318.330282	17.679258
36.062315	1326.098983	17.684275
35.960507	1320.264002	17.689293
35.720403	1320.629969	17.694311
36.017020	1324.203460	17.699328
35.411081	1329.770887	17.704346
35.734034	1319.605714	17.709363
35.389894	1330.168960	17.714381
36.006343	1338.400967	17.719399
36.050137	1344.485157	17.724416
35.916016	1347.229860	17.729434
35.990903	1341.398748	17.734451
36.266841	1333.708861	17.739469
36.494413	1332.477245	17.744487
36.963148	1341.148978	17.749504
36.559175	1335.960961	17.754522
36.798670	1342.544681	17.759539
36.611173	1345.509194	17.764557
36.788008	1339.005678	17.769575
36.661264	1333.840498	17.774592
36.548942	1339.191727	17.779610
36.853075	1334.583909	17.784627
36.708785	1333.063406	17.789645
36.466374	1341.676143	17.794663
36.895029	1326.971977	17.799680
36.582381	1332.518699	17.804698
36.608967	1328.096384	17.809715
36.922052	1326.759849	17.814733
36.546408	1328.450445	17.819751
36.976010	1326.398197	17.824768
36.989119	1333.099438	17.829786
36.827616	1330.281395	17.834803
36.984290	1333.296126	17.839821
36.489208	1335.554565	17.844839
36.848396	1330.575192	17.849856
37.158896	1330.561389	17.854874
37.262796	1330.239119	17.859891
37.043013	1335.095925	17.864909
36.734499	1329.378539	17.869927
37.412311	1339.182045	17.874944
37.225279	1339.716429	17.879962
37.509470	1340.337932	17.884979
37.344734	1333.502913	17.889997
37.473868	1328.919360	17.895015
37.613242	1332.309199	17.900032
37.226716	1327.522407	17.905050
37.427801	1341.187706	17.910067
37.595913	1346.785343	17.915085
38.041142	1342.149104	17.920103
37.620387	1332.015240	17.925120
37.585413	1315.730025	17.930138
37.527794	1333.822572	17.935155
37.431108	1342.343047	17.940173
37.520067	1344.737206	17.945191
38.082877	1353.084925	17.950208
37.754397	1355.424566	17.955226
37.719792	1352.731809	17.960243
37.598378	1351.665328	17.965261
37.546991	1350.878220	17.970279
37.672849	1343.221312	17.975296
37.880522	1356.333305	17.980314
38.134092	1352.310938	17.985331
38.023491	1348.872668	17.990349
38.122902	1349.614645	17.995367
38.308800	1365.848105	18.000384
38.101431	1366.196320	18.005402
38.398021	1373.039359	18.010419
38.374986	1372.664390	18.015437
38.646379	1373.429916	18.020455
38.574091	1354.117672	18.025472
38.107900	1358.912103	18.030490
38.493137	1355.320401	18.035507
38.348991	1369.983434	18.040525
38.329125	1377.601920	18.045543
38.647197	1362.662577	18.050560
38.460376	1361.704177	18.055578
38.549084	1377.220702	18.060595
38.856991	1369.134456	18.065613
38.835402	1370.999965	18.070631
38.593543	1372.300360	18.075648
38.558456	1378.273840	18.080666
38.613521	1377.006131	18.085683
38.733312	1366.509833	18.090701
38.467277	1367.387967	18.095719
38.768513	1362.802687	18.100736
38.579253	1369.500934	18.105754
39.025844	1376.907474	18.110771
39.248299	1380.139132	18.115789
39.151171	1391.039267	18.120807
39.581900	1378.187262	18.125824
38.886723	1378.021749	18.130842
38.940418	1382.703171	18.135859
38.905073	1382.345910	18.140877
39.070931	1385.179323	18.145895
39.266170	1384.445094	18.150912
39.397656	1388.423181	18.155930
39.338003	1389.404685	18.160947
39.660102	1387.593344	18.165965
39.401199	1384.901011	18.170983
39.608701	1384.881255	18.176000
39.427843	1379.696137	18.181018
39.505756	1380.223725	18.186035
39.506364	1386.683939	18.191053
39.382985	1379.706718	18.196071
39.871302	1373.829754	18.201088
39.596236	1392.338296	18.206106
39.400082	1385.441906	18.211123
39.763797	1391.100431	18.216141
39.656031	1398.461289	18.221159
40.083807	1409.487483	18.226176
40.132412	1404.667209	18.231194
39.937111	1409.327688	18.236211
40.080450	1389.602909	18.241229
40.098768	1403.855491	18.246247
40.365166	1407.768262	18.251264
39.763822	1398.770385	18.256282
39.929801	1399.438816	18.261299
40.636677	1402.477810	18.266317
40.359558	1408.833218	18.271335
40.533202	1407.007264	18.276352
40.247253	1401.930128	18.281370
40.526390	1409.031546	18.286387
40.508800	1409.959121	18.291405
40.508615	1397.468120	18.296423
40.420843	1396.074461	18.301440
40.458381	1410.393467	18.306458
40.441667	1405.719132	18.311475
40.561628	1407.720263	18.316493
40.815056	1417.252622	18.321511
40.503351	1400.149119	18.326528
40.383018	1412.962239	18.331546
40.338737	1409.298963	18.336563
40.419891	1402.488511	18.341581
40.379054	1411.833434	18.346599
40.748919	1413.110573	18.351616
41.141610	1435.266936	18.356634
40.835387	1435.438129	18.361651
40.976182	1431.925739	18.366669
40.927358	1434.565569	18.371687
41.050639	1424.365348	18.376704
41.186871	1428.481561	18.381722
41.125629	1439.915767	18.386739
40.957551	1435.265140	18.391757
40.923173	1438.322446	18.396775
41.076894	1434.413539	18.401792
41.092730	1424.110227	18.406810
41.134507	1424.391003	18.411827
41.067865	1428.652617	18.416845
41.233139	1448.061095	18.421863
41.547950	1445.641795	18.426880
41.788690	1459.373559	18.431898
41.800523	1458.787989	18.436915
41.947739	1451.632637	18.441933
41.703766	1451.377493	18.446951
41.946406	1447.618760	18.451968
41.793946	1440.611357	18.456986
42.051196	1440.792098	18.462003
42.212321	1425.927788	18.467021
42.077371	1421.123645	18.472039
41.696460	1414.287751	18.477056
41.594816	1407.477534	18.482074
41.846836	1430.309208	18.487091
42.240740	1434.214631	18.492109
42.346251	1446.935582	18.497127
42.334306	1440.209133	18.502144
42.304354	1431.632975	18.507162
41.910195	1430.968999	18.512179
42.266816	1425.582887	18.517197
42.179651	1438.801099	18.522215
42.085006	1440.668593	18.527232
42.301488	1448.366848	18.532250
42.171657	1447.014490	18.537267
42.775817	1446.282463	18.542285
42.289414	1455.327976	18.547303
42.475498	1447.450139	18.552320
42.360807	1445.126537	18.557338
42.174414	1446.727529	18.562355
42.612322	1445.201007	18.567373
42.263945	1452.448101	18.572391
42.392283	1438.340030	18.577408
42.684478	1442.864174	18.582426
42.241358	1462.251222	18.587443
42.261818	1449.545502	18.592461
42.300639	1454.667948	18.597479
42.141857	1459.234352	18.602496
42.467293	1474.502422	18.607514
42.523184	1482.708712	18.612531
43.622795	1482.198871	18.617549
42.704792	1490.179041	18.622567
42.954701	1489.852826	18.627584
43.203123	1480.737546	18.632602
42.959861	1494.674564	18.637619
43.323895	1469.758306	18.642637
43.330787	1478.625551	18.647655
43.336722	1485.343753	18.652672
43.103982	1476.950831	18.657690
43.442669	1499.093643	18.662707
43.725439	1485.889186	18.667725
43.654375	1491.934615	18.672743
43.678985	1489.112634	18.677760
43.803352	1478.669204	18.682778
43.538092	1491.246300	18.687795
43.693420	1489.476858	18.692813
43.898496	1502.235901	18.697831
44.225559	1508.051692	18.702848
44.154250	1492.551527	18.707866
43.488840	1480.313025	18.712883
43.680905	1483.151816	18.717901
44.110022	1494.509227	18.722919
44.150914	1508.325991	18.727936
44.220423	1502.773392	18.732954
44.249279	1501.086884	18.737971
44.216562	1492.691019	18.742989
44.049941	1489.829569	18.748007
44.150208	1498.278233	18.753024
44.416827	1500.048103	18.758042
44.362061	1503.020248	18.763059
44.333217	1487.734351	18.768077
44.565104	1490.727857	18.773095
44.514977	1494.261031	18.778112
44.463061	1495.597950	18.783130
44.505820	1504.825678	18.788147
44.690491	1497.209984	18.793165
44.469854	1496.484103	18.798183
44.350788	1494.779745	18.803200
44.624723	1494.541288	18.808218
44.251686	1498.260763	18.813235
45.120037	1501.839389	18.818253
44.675433	1489.743017	18.823271
44.743404	1506.522124	18.828288
44.796325	1497.563704	18.833306
44.541510	1505.080195	18.838323
45.002095	1511.266404	18.843341
45.107277	1514.592204	18.848359
44.882852	1530.211574	18.853376
44.929777	1521.266706	18.858394
45.040399	1533.822809	18.863411
44.934879	1525.990626	18.868429
45.220051	1527.880675	18.873447
45.336225	1526.338281	18.878464
45.305049	1514.218144	18.883482
45.247983	1523.928602	18.888499
45.338482	1517.684712	18.893517
45.244566	1524.080887	18.898535
45.565604	1536.818629	18.903552
45.956373	1535.028075	18.908570
45.397055	1539.496301	18.913587
45.595172	1539.433833	18.918605
45.814210	1542.243159	18.923623
45.732079	1544.749362	18.928640
45.689313	1543.402291	18.933658
45.923834	1539.417582	18.938675
45.925204	1542.642883	18.943693
45.906521	1540.408372	18.948711
45.772708	1548.941075	18.953728
46.228308	1543.709840	18.958746
45.808182	1542.551288	18.963763
46.182674	1541.012603	18.968781
46.063378	1536.556287	18.973799
45.981060	1543.928997	18.978816
46.134534	1542.235584	18.983834
45.957209	1538.741457	18.988851
46.221329	1533.107861	18.993869
46.236546	1532.600657	18.998887
46.024667	1559.065092	19.003904
46.431422	1558.894192	19.008922
46.333868	1567.216084	19.013939
46.405138	1557.074432	19.018957
46.640191	1558.445292	19.023975
46.149304	1563.818030	19.028992
46.751843	1566.138063	19.034010
46.794319	1571.869070	19.039027
47.087757	1565.148377	19.044045
46.930687	1555.159272	19.049063
46.671701	1564.166052	19.054080
46.613781	1559.324555	19.059098
47.022841	1577.006541	19.064115
47.272070	1582.118149	19.069133
47.390388	1582.279632	19.074151
47.308387	1576.608730	19.079168
47.549055	1575.097322	19.084186
47.036252	1563.327182	19.089203
47.194512	1570.886282	19.094221
47.256451	1573.417255	19.099239
47.006835	1584.862132	19.104256
47.522331	1581.357280	19.109274
47.338993	1575.127872	19.114291
47.272727	1581.630194	19.119309
47.523215	1576.093399	19.124327
47.069091	1583.881003	19.129344
47.430470	1577.339018	19.134362
47.552186	1583.114421	19.139379
47.914731	1591.783980	19.144397
47.454918	1595.116263	19.149415
47.902884	1604.305802	19.154432
47.996622	1607.418807	19.159450
47.998081	1602.123004	19.164467
48.086221	1595.466026	19.169485
48.136203	1603.726948	19.174503
48.198114	1605.459472	19.179520
48.508172	1594.598697	19.184538
48.518696	1594.704483	19.189555
48.319036	1586.031758	19.194573
48.218072	1590.690127	19.199591
48.517927	1600.019640	19.204608
48.475726	1592.833947	19.209626
48.420856	1589.380587	19.214643
48.596195	1586.317213	19.219661
48.664438	1582.872969	19.224679
48.323025	1574.244551	19.229696
48.693395	1582.673027	19.234714
48.831955	1581.928735	19.239731
48.639194	1590.477005	19.244749
48.658405	1591.181063	19.249767
48.645667	1597.592948	19.254784
48.932563	1583.851259	19.259802
48.826503	1583.511386	19.264819
48.695375	1590.307909	19.269837
48.405573	1590.129374	19.274855
48.806139	1595.927366	19.279872
48.984583	1583.446119	19.284890
49.233119	1590.804881	19.289907
48.843071	1588.095193	19.294925
48.798042	1587.849903	19.299943
48.563383	1607.242317	19.304960
49.031042	1606.787305	19.309978
49.402744	1611.482081	19.314995
49.264465	1614.394742	19.320013
49.490433	1616.615985	19.325031
49.198724	1623.885828	19.330048
49.433579	1615.820386	19.335066
49.343541	1611.675063	19.340083
49.366169	1622.231510	19.345101
49.757107	1630.388529	19.350119
49.783481	1629.387243	19.355136
49.936714	1631.174892	19.360154
49.865423	1632.751555	19.365171
49.534276	1637.174587	19.370189
50.276332	1623.191132	19.375207
50.072181	1636.547746	19.380224
50.476736	1638.438038	19.385242
50.598082	1638.109872	19.390259
50.219952	1643.007351	19.395277
50.276024	1627.963663	19.400295
50.240482	1631.207387	19.405312
50.340130	1634.909637	19.410330
50.487178	1626.605470	19.415347
50.211278	1630.495954	19.420365
50.169548	1630.710918	19.425383
50.218700	1631.006322	19.430400
50.515679	1634.971160	19.435418
50.861125	1635.491554	19.440435
50.543212	1637.403518	19.445453
50.313900	1629.625401	19.450471
50.562745	1639.363735	19.455488
50.703900	1651.403870	19.460506
50.702289	1660.165234	19.465523
50.370881	1658.045981	19.470541
50.812886	1659.703178	19.475559
50.678793	1657.022807	19.480576
50.811255	1659.277641	19.485594
51.010588	1654.013940	19.490611
50.709884	1663.440737	19.495629
50.870715	1669.074332	19.500647
51.052221	1674.647882	19.505664
51.373433	1676.358721	19.510682
51.499992	1679.939993	19.515699
51.592083	1686.991929	19.520717
51.839476	1681.667038	19.525735
51.733594	1677.972331	19.530752
51.462191	1668.584932	19.535770
51.790768	1669.259457	19.540787
52.034446	1680.137930	19.545805
51.934640	1668.782720	19.550823
51.632208	1671.607495	19.555840
51.759485	1670.328451	19.560858
51.583290	1675.689788	19.565875
51.719564	1678.881352	19.570893
51.906477	1673.215626	19.575911
51.761620	1673.020692	19.580928
51.846856	1679.663423	19.585946
52.183941	1678.727067	19.590963
51.967578	1676.709714	19.595981
52.225344	1662.833666	19.600999
52.333318	1672.991743	19.606016
52.195233	1670.378271	19.611034
52.441465	1673.795617	19.616051
52.274470	1696.911045	19.621069
52.554044	1691.192923	19.626087
52.501529	1702.707985	19.631104
52.534636	1695.087550	19.636122
52.649165	1696.843399	19.641139
52.365560	1698.166138	19.646157
52.956132	1688.302829	19.651175
52.426754	1693.609048	19.656192
52.495613	1687.437921	19.661210
52.798167	1689.457815	19.666227
52.611170	1695.455202	19.671245
52.877036	1690.626058	19.676263
52.861396	1702.842282	19.681280
52.905646	1724.280382	19.686298
53.407859	1720.203196	19.691315
53.160379	1717.518489	19.696333
53.242283	1724.407925	19.701351
53.453145	1730.535502	19.706368
53.283536	1712.453173	19.711386
53.629436	1713.358529	19.716403
53.430584	1711.830762	19.721421
53.464601	1715.868378	19.726439
53.604558	1717.045855	19.731456
53.472787	1717.846161	19.736474
53.539672	1709.633415	19.741491
53.780513	1713.780645	19.746509
53.382396	1712.643880	19.751527
53.568554	1710.415126	19.756544
53.422617	1731.848317	19.761562
53.648648	1733.738187	19.766579
53.880650	1740.373725	19.771597
53.834382	1739.607889	19.776615
54.148567	1739.978541	19.781632
54.316056	1738.077775	19.786650
54.485865	1736.460685	19.791667
54.115944	1732.838896	19.796685
54.610510	1732.294454	19.801703
54.602189	1735.862154	19.806720
54.593658	1733.004299	19.811738
54.857366	1726.505968	19.816755
54.388564	1733.876190	19.821773
54.747218	1724.683551	19.826791
54.272172	1730.852320	19.831808
54.475056	1732.398657	19.836826
54.740005	1724.700857	19.841843
54.593125	1751.868646	19.846861
54.834527	1742.274622	19.851879
54.900666	1753.310352	19.856896
55.093350	1756.433128	19.861914
55.396347	1752.870015	19.866931
55.281523	1754.860631	19.871949
55.224972	1742.356128	19.876967
55.338709	1743.985866	19.881984
55.311957	1746.975754	19.887002
55.305861	1743.953405	19.892019
55.339277	1753.902290	19.897037
55.521356	1741.436143	19.902055
55.910570	1737.020032	19.907072
55.755624	1744.375799	19.912090
55.610625	1724.992490	19.917107
55.672700	1729.609570	19.922125
55.539620	1722.971425	19.927143
55.640936	1728.478657	19.932160
55.410750	1739.765945	19.937178
55.791567	1739.949422	19.942195
55.495160	1748.681274	19.947213
55.741609	1739.477804	19.952231
55.578225	1739.961153	19.957248
55.624979	1735.428274	19.962266
55.953139	1746.151532	19.967283
55.932255	1755.802795	19.972301
56.332624	1758.817288	19.977319
55.973589	1765.507566	19.982336
56.123156	1763.940985	19.987354
56.220901	1763.969986	19.992371
56.018616	1767.375567	19.997389
56.170858	1765.593959	20.002407
55.770842	1768.670737	20.007424
55.739862	1787.605375	20.012442
56.069267	1782.144521	20.017459
56.672332	1802.302194	20.022477
56.683467	1809.530975	20.027495
57.001321	1808.562910	20.032512
57.162323	1808.944940	20.037530
57.163392	1805.498554	20.042547
56.840024	1815.733762	20.047565
57.141918	1810.744298	20.052583
57.562928	1811.846186	20.057600
57.572843	1811.888949	20.062618
57.447386	1794.708547	20.067635
57.017403	1798.238177	20.072653
57.182520	1796.167353	20.077671
57.304781	1807.923358	20.082688
57.233126	1809.578993	20.087706
57.672620	1810.084657	20.092723
57.459224	1807.681793	20.097741
57.347082	1804.736012	20.102759
57.631136	1802.908500	20.107776
57.567180	1801.788805	20.112794
57.428358	1808.128997	20.117811
57.548562	1820.791105	20.122829
57.671861	1828.545152	20.127847
57.920657	1828.345347	20.132864
57.969989	1821.653337	20.137882
58.073618	1821.681417	20.142899
57.986861	1828.294343	20.147917
58.049892	1827.151594	20.152935
58.411547	1828.228068	20.157952
58.178029	1829.912221	20.162970
58.071692	1831.399711	20.167987
58.234821	1846.999663	20.173005
58.350823	1852.662432	20.178023
58.633608	1850.595258	20.183040
58.381996	1860.011310	20.188058
58.373699	1846.842724	20.193075
58.673731	1849.219661	20.198093
58.526481	1848.453862	20.203111
59.058558	1851.854861	20.208128
59.068269	1846.955349	20.213146
59.175327	1842.908489	20.218163
59.048767	1851.894663	20.223181
59.150696	1845.266992	20.228199
59.065199	1845.296300	20.233216
59.001523	1853.029156	20.238234
59.231126	1850.140284	20.243251
59.526869	1863.879522	20.248269
59.283294	1855.510211	20.253287
59.362676	1863.810832	20.258304
59.507637	1869.535345	20.263322
59.696649	1867.173571	20.268339
59.536945	1869.278536	20.273357
59.729445	1867.642099	20.278375
59.586348	1863.274642	20.283392
59.698375	1864.907815	20.288410
59.620062	1864.901281	20.293427
59.418199	1866.387961	20.298445
59.406528	1864.887661	20.303463
59.728312	1862.060089	20.308480
59.955620	1877.028279	20.313498
60.146974	1886.456998	20.318515
60.269199	1885.879366	20.323533
60.238384	1885.227875	20.328551
60.283704	1875.434114	20.333568
60.354273	1884.462007	20.338586
60.302600	1885.303423	20.343603
60.564056	1883.965469	20.348621
60.795943	1885.927026	20.353639
60.801612	1883.979010	20.358656
60.875455	1887.312946	20.363674
60.716449	1883.525528	20.368691
60.782470	1881.325043	20.373709
60.643199	1884.493540	20.378727
61.169165	1884.297649	20.383744
60.655661	1877.921035	20.388762
60.619248	1865.785701	20.393779
60.602536	1877.790759	20.398797
60.893801	1894.497372	20.403815
61.347801	1898.740645	20.408832
60.938809	1900.067263	20.413850
61.113079	1901.091044	20.418867
61.150830	1904.509539	20.423885
61.102182	1905.079064	20.428903
61.308174	1909.837755	20.433920
61.453758	1918.383666	20.438938
61.526139	1925.072686	20.443955
61.776793	1918.598423	20.448973
61.251486	1918.709263	20.453991
61.532204	1925.491883	20.459008
61.464749	1922.381280	20.464026
61.495914	1928.060521	20.469043
61.898916	1944.017478	20.474061
62.011296	1946.231311	20.479079
62.394069	1931.401287	20.484096
62.365297	1947.201819	20.489114
62.239369	1938.444781	20.494131
62.811919	1934.946704	20.499149
62.756211	1949.634226	20.504167
62.880118	1944.625271	20.509184
62.747409	1942.156094	20.514202
62.954503	1931.664723	20.519219
62.520133	1918.698549	20.524237
62.446301	1922.992967	20.529255
62.736570	1924.156376	20.534272
62.638999	1942.552463	20.539290
62.615380	1939.274032	20.544307
62.529742	1933.376353	20.549325
62.665014	1936.018974	20.554343
62.783624	1937.326051	20.559360
62.473097	1946.678791	20.564378
62.715677	1955.714486	20.569395
62.814354	1961.159082	20.574413
63.081876	1960.104215	20.579431
63.505877	1953.325050	20.584448
63.061534	1956.023770	20.589466
63.576675	1964.439213	20.594483
63.522215	1982.405678	20.599501
63.969316	1973.502034	20.604519
64.073767	1972.321227	20.609536
63.808435	1965.946727	20.614554
63.641506	1950.186573	20.619571
64.026077	1946.317130	20.624589
63.531259	1961.603674	20.629607
64.233615	1969.361737	20.634624
64.274119	1978.615310	20.639642
64.041772	1982.865146	20.644659
64.218532	1982.124321	20.649677
64.437708	1981.701921	20.654695
64.460684	1968.673523	20.659712
64.264998	1972.772435	20.664730
64.446338	1973.782489	20.669747
64.316530	1965.508918	20.674765
64.177260	1975.516543	20.679783
64.375154	1973.800350	20.684800
63.811644	1973.708878	20.689818
63.821675	1981.221944	20.694835
64.613340	1987.514249	20.699853
64.612017	1996.768073	20.704871
64.768487	1991.678258	20.709888
64.494742	1998.705579	20.714906
64.943162	2006.850609	20.719923
64.973951	2009.859930	20.724941
64.707376	2021.588629	20.729959
65.291100	2010.306002	20.734976
65.482744	2009.108375	20.739994
65.586907	2013.425423	20.745011
65.469338	2013.620713	20.750029
65.735948	2009.905449	20.755047
65.786979	2013.511246	20.760064
65.632866	2013.623893	20.765082
65.699092	2019.786855	20.770099
66.186450	2020.237687	20.775117
65.970478	2011.630431	20.780135
66.220455	2008.662598	20.785152
65.603705	2008.920318	20.790170
66.047838	2014.304493	20.795187
66.357311	2030.986290	20.800205
66.467710	2034.598569	20.805223
66.139692	2028.000322	20.810240
66.762014	2034.524318	20.815258
66.422751	2028.379146	20.820275
66.738470	2024.653028	20.825293
66.199862	2031.226362	20.830311
66.858813	2039.805515	20.835328
66.530780	2036.230753	20.840346
66.671707	2038.051932	20.845363
66.830208	2018.207313	20.850381
66.828869	2040.757547	20.855399
66.891177	2026.088117	20.860416
66.656726	2039.673857	20.865434
66.661071	2031.174094	20.870451
67.281942	2025.626472	20.875469
67.208009	2032.044946	20.880487
67.060414	2030.458623	20.885504
67.092294	2036.421830	20.890522
67.641187	2062.079794	20.895539
67.653364	2054.389897	20.900557
67.503593	2066.567419	20.905575
67.633885	2054.358497	20.910592
67.668241	2050.449222	20.915610
67.745705	2056.818735	20.920627
68.023764	2048.184555	20.925645
67.713207	2053.728013	20.930663
68.203134	2048.409199	20.935680
68.117040	2054.971608	20.940698
67.880557	2061.279849	20.945715
68.062579	2053.017346	20.950733
68.235845	2065.261028	20.955751
68.293266	2056.516235	20.960768
68.154976	2042.522053	20.965786
68.100859	2052.311236	20.970803
68.157851	2040.145368	20.975821
67.885786	2054.715385	20.980839
68.264307	2055.473627	20.985856
68.286721	2065.392848	20.990874
68.369577	2063.331726	20.995891
68.684927	2057.140789	21.000909
68.362427	2064.317796	21.005927
68.407770	2062.183651	21.010944
68.816944	2084.439231	21.015962
68.725367	2092.126065	21.020979
68.942721	2079.524759	21.025997
68.967151	2081.563026	21.031015
69.021865	2093.850551	21.036032
69.073329	2089.316845	21.041050
68.942031	2111.616110	21.046067
69.218630	2115.104528	21.051085
69.785428	2115.022169	21.056103
69.526380	2101.198351	21.061120
69.500867	2109.408214	21.066138
69.529462	2114.027484	21.071155
69.877420	2099.537318	21.076173
69.489468	2115.230158	21.081191
69.726422	2118.847875	21.086208
69.961033	2129.718574	21.091226
69.756530	2124.265523	21.096243
70.144175	2129.892132	21.101261
69.944756	2130.747239	21.106279
70.293178	2136.724006	21.111296
70.341918	2132.077098	21.116314
70.481708	2131.256846	21.121331
70.783095	2125.184848	21.126349
70.738554	2129.515754	21.131367
70.686447	2130.148950	21.136384
70.540201	2123.077183	21.141402
70.899362	2139.672395	21.146419
71.214952	2147.772023	21.151437
71.064755	2153.735392	21.156455
71.008435	2151.456205	21.161472
71.323134	2152.779917	21.166490
71.196917	2158.281901	21.171507
71.164062	2151.649986	21.176525
71.144980	2155.127930	21.181543
71.380345	2146.737097	21.186560
71.627070	2150.927692	21.191578
71.526162	2142.826251	21.196595
71.776761	2140.981855	21.201613
71.579842	2148.600004	21.206631
71.535897	2153.022348	21.211648
71.651417	2139.767871	21.216666
71.683213	2138.197617	21.221683
72.027886	2137.345264	21.226701
71.526686	2146.955218	21.231719
71.941693	2155.632613	21.236736
72.100234	2160.105292	21.241754
72.326508	2164.548424	21.246771
72.482140	2160.717962	21.251789
72.220241	2166.282235	21.256807
72.208238	2161.594340	21.261824
72.545807	2161.042926	21.266842
72.345977	2161.645614	21.271859
72.329897	2159.760940	21.276877
72.354357	2169.654651	21.281895
72.595184	2174.733029	21.286912
72.849641	2189.138603	21.291930
72.991707	2188.049727	21.296947
73.013615	2186.572543	21.301965
72.854420	2184.640857	21.306983
72.761376	2184.346273	21.312000
73.215351	2182.062876	21.317018
73.213275	2186.832148	21.322035
72.993876	2180.141080	21.327053
73.117490	2183.006488	21.332071
73.856103	2196.629253	21.337088
74.162996	2197.313510	21.342106
73.659463	2193.390641	21.347123
73.664370	2185.477746	21.352141
73.802064	2186.715575	21.357159
73.761568	2198.147014	21.362176
74.075442	2212.041482	21.367194
73.607977	2215.577065	21.372211
73.666761	2212.667558	21.377229
73.973301	2208.280066	21.382247
73.870576	2205.522108	21.387264
74.408691	2208.698150	21.392282
73.890686	2213.608229	21.397299
74.159007	2217.833329	21.402317
74.317212	2227.261110	21.407335
74.295764	2239.320805	21.412352
74.644148	2227.203839	21.417370
74.421231	2234.608329	21.422387
74.757676	2239.949479	21.427405
74.769529	2250.025105	21.432423
74.957735	2248.449272	21.437440
74.804689	2255.183203	21.442458
74.828359	2256.603018	21.447475
75.229416	2257.461889	21.452493
74.896965	2250.927374	21.457511
74.829479	2253.860608	21.462528
75.446304	2262.235012	21.467546
75.923314	2256.043928	21.472563
75.608153	2275.478080	21.477581
75.665778	2269.324294	21.482599
75.794004	2268.960323	21.487616
75.689980	2269.011470	21.492634
75.612616	2273.940897	21.497651
75.770352	2263.554905	21.502669
75.898327	2266.261839	21.507687
75.661066	2270.042255	21.512704
76.454960	2269.618175	21.517722
76.635050	2281.924058	21.522739
76.425004	2287.117295	21.527757
76.602340	2283.961964	21.532775
76.918487	2286.046076	21.537792
77.149030	2271.905557	21.542810
76.663049	2260.465296	21.547827
76.476858	2255.176607	21.552845
76.714274	2259.384467	21.557863
76.900227	2275.584029	21.562880
76.909366	2287.664213	21.567898
76.530121	2281.209608	21.572915
77.258728	2281.919322	21.577933
77.071655	2284.814488	21.582951
76.806208	2283.981974	21.587968
76.899148	2275.026364	21.592986
77.405629	2295.272318	21.598003
77.278462	2299.243793	21.603021
77.660383	2303.507925	21.608039
77.406545	2312.836192	21.613056
77.694405	2306.450644	21.618074
77.474840	2302.221304	21.623091
77.772066	2306.845876	21.628109
77.692947	2299.451069	21.633127
77.714152	2300.451514	21.638144
77.955189	2295.278931	21.643162
77.780185	2315.328696	21.648179
77.823457	2323.332202	21.653197
78.105057	2325.832023	21.658215
78.040761	2320.884012	21.663232
78.450380	2320.895713	21.668250
78.414367	2320.147182	21.673267
78.534600	2343.262625	21.678285
78.647033	2340.897009	21.683303
78.628732	2343.453288	21.688320
78.801221	2341.008827	21.693338
79.110649	2341.989366	21.698355
78.808277	2349.529439	21.703373
79.274446	2344.495154	21.708391
78.944435	2342.053677	21.713408
79.146066	2337.171304	21.718426
79.225858	2347.880183	21.723443
78.970784	2350.902789	21.728461
79.095546	2358.328603	21.733479
79.428629	2367.201990	21.738496
79.725560	2362.150030	21.743514
79.645938	2362.607647	21.748531
79.439218	2369.271128	21.753549
79.579234	2373.790948	21.758567
79.781825	2384.963493	21.763584
80.379080	2386.934139	21.768602
80.224156	2391.853658	21.773619
80.376997	2390.835671	21.778637
80.519308	2380.066984	21.783655
80.330601	2386.222672	21.788672
80.477439	2392.291074	21.793690
80.430948	2389.177106	21.798707
80.461284	2383.469411	21.803725
80.874909	2379.330213	21.808743
80.896724	2378.683083	21.813760
81.077365	2378.983147	21.818778
81.033238	2372.636965	21.823795
80.654904	2376.969731	21.828813
81.145963	2374.800433	21.833831
80.740673	2375.485816	21.838848
81.096952	2393.176881	21.843866
81.081893	2398.450064	21.848883
81.104934	2409.259398	21.853901
81.334737	2406.023235	21.858919
81.285153	2402.246967	21.863936
81.259777	2406.543377	21.868954
81.454197	2412.023607	21.873971
81.573825	2414.741340	21.878989
81.878481	2421.848634	21.884007
81.905697	2426.020032	21.889024
82.107813	2427.449775	21.894042
82.110112	2431.170599	21.899059
81.965408	2430.839919	21.904077
82.424685	2433.400288	21.909095
82.402556	2447.678975	21.914112
82.614688	2448.333903	21.919130
82.727757	2445.983954	21.924147
82.221865	2445.236446	21.929165
82.503557	2446.281302	21.934183
82.336414	2449.959243	21.939200
82.819604	2447.917413	21.944218
82.817672	2442.770231	21.949235
82.842825	2453.206839	21.954253
83.171921	2459.581257	21.959271
83.239507	2470.314214	21.964288
83.582910	2467.760900	21.969306
83.740601	2469.674181	21.974323
83.589476	2470.414429	21.979341
83.429883	2458.563106	21.984359
83.695969	2466.642231	21.989376
83.416381	2460.910478	21.994394
83.452293	2463.950634	21.999411
83.304325	2462.443234	22.004429
83.561153	2457.798357	22.009447
83.703100	2464.025355	22.014464
83.552485	2476.796636	22.019482
83.983036	2481.611825	22.024499
83.881454	2484.474691	22.029517
84.478481	2486.284423	22.034535
84.239578	2486.265175	22.039552
84.378990	2501.629549	22.044570
84.621322	2512.499271	22.049587
84.352031	2520.192038	22.054605
85.071752	2511.987107	22.059623
84.958713	2509.088692	22.064640
85.009672	2509.424857	22.069658
84.870488	2505.324901	22.074675
84.704981	2519.206344	22.079693
84.852389	2509.377306	22.084711
85.234300	2529.740882	22.089728
85.349525	2533.567123	22.094746
85.497103	2536.236309	22.099763
85.376678	2537.625068	22.104781
85.684760	2528.051742	22.109799
85.666028	2533.180358	22.114816
85.485611	2528.951142	22.119834
85.850215	2535.787130	22.124851
85.464493	2538.612463	22.129869
85.737083	2542.679166	22.134887
86.182796	2549.060593	22.139904
86.277700	2555.443332	22.144922
86.273751	2550.690951	22.149939
85.921205	2556.279014	22.154957
86.206931	2543.486773	22.159975
86.406356	2556.512568	22.164992
86.162504	2577.943173	22.170010
86.966780	2575.671123	22.175027
86.489979	2574.707590	22.180045
86.565200	2569.529347	22.185063
87.044020	2574.324374	22.190080
87.244155	2590.209540	22.195098
87.148656	2585.395746	22.200115
87.043714	2592.406318	22.205133
87.229491	2583.944147	22.210151
87.385273	2590.964368	22.215168
87.375211	2588.810436	22.220186
87.428428	2588.483460	22.225203
87.561135	2599.929048	22.230221
87.975424	2599.412943	22.235239
88.128742	2600.664134	22.240256
88.254020	2616.911383	22.245274
88.245027	2608.766926	22.250291
87.968745	2616.309334	22.255309
88.077223	2618.653264	22.260327
88.266311	2612.343050	22.265344
88.659279	2615.955362	22.270362
88.763953	2604.084632	22.275379
88.437637	2608.983720	22.280397
88.736942	2605.417863	22.285415
88.704521	2611.605953	22.290432
88.620612	2605.221736	22.295450
88.778979	2601.510686	22.300467
88.621881	2603.063002	22.305485
88.938695	2610.269462	22.310503
89.314474	2617.450906	22.315520
89.520560	2622.509607	22.320538
89.725806	2622.616452	22.325555
89.553416	2630.571825	22.330573
89.721999	2626.543555	22.335591
89.809389	2623.348603	22.340608
89.525858	2622.275883	22.345626
89.854976	2610.442575	22.350643
89.443540	2624.239541	22.355661
89.840597	2613.045752	22.360679
89.844923	2615.494372	22.365696
89.781605	2628.056402	22.370714
89.820914	2630.297550	22.375731
89.964972	2646.005339	22.380749
90.329619	2644.427077	22.385767
90.054106	2642.721871	22.390784
90.030026	2647.204347	22.395802
90.655975	2660.538974	22.400819
90.484017	2671.691476	22.405837
90.597336	2676.767882	22.410855
90.442352	2675.372028	22.415872
90.552314	2688.446654	22.420890
91.102042	2692.242727	22.425907
91.204020	2706.521112	22.430925
91.225576	2693.126297	22.435943
91.407204	2695.752299	22.440960
91.206793	2704.324388	22.445978
91.665856	2696.015030	22.450995
91.709604	2695.156146	22.456013
92.044963	2705.512738	22.461031
91.792034	2704.854987	22.466048
91.811956	2709.065468	22.471066
92.167818	2712.440589	22.476083
92.226718	2722.575388	22.481101
92.261346	2708.929177	22.486119
92.114913	2701.128139	22.491136
91.628697	2708.056465	22.496154
92.214394	2704.969640	22.501171
92.523081	2719.029436	22.506189
92.757102	2726.214196	22.511207
92.959855	2726.605488	22.516224
92.693588	2733.363648	22.521242
93.304301	2731.607956	22.526259
93.214199	2738.032370	22.531277
92.935481	2722.828755	22.536295
93.264265	2718.308253	22.541312
93.540235	2732.111223	22.546330
93.819083	2741.230007	22.551347
93.626836	2742.885683	22.556365
93.904821	2747.096771	22.561383
94.244210	2755.391786	22.566400
94.033995	2730.926712	22.571418
93.901425	2723.215021	22.576435
94.025996	2737.887567	22.581453
93.958454	2742.203287	22.586471
94.657501	2731.978396	22.591488
94.265818	2744.980162	22.596506
94.170173	2744.944781	22.601523
93.952046	2745.932249	22.606541
94.247580	2744.790890	22.611559
94.468402	2742.856414	22.616576
94.435358	2763.342080	22.621594
94.460106	2761.539320	22.626611
94.674185	2765.387997	22.631629
94.780302	2761.978623	22.636647
95.185021	2766.081487	22.641664
94.988747	2773.005442	22.646682
95.032432	2773.557371	22.651699
95.236302	2790.979184	22.656717
95.144094	2788.134272	22.661735
95.465682	2792.449005	22.666752
95.392563	2783.310852	22.671770
95.603981	2782.854934	22.676787
95.463817	2795.034598	22.681805
95.527679	2810.228015	22.686823
95.865484	2815.704841	22.691840
95.571966	2815.757273	22.696858
96.118620	2819.310830	22.701875
96.195055	2830.541292	22.706893
96.398760	2832.674648	22.711911
96.568470	2840.099931	22.716928
96.714166	2838.205622	22.721946
96.819508	2842.980331	22.726963
96.696593	2830.933645	22.731981
97.015654	2834.958416	22.736999
96.716337	2818.785844	22.742016
96.735221	2838.982560	22.747034
97.362135	2844.650813	22.752051
97.458646	2849.969772	22.757069
97.536003	2855.080269	22.762087
97.440139	2851.412155	22.767104
97.626615	2852.699199	22.772122
97.567552	2852.036318	22.777139
97.753956	2851.969372	22.782157
97.868332	2849.376139	22.787175
98.049166	2858.308342	22.792192
97.966819	2868.907219	22.797210
98.415282	2865.996522	22.802227
98.050156	2873.587676	22.807245
98.488193	2866.064268	22.812263
98.372718	2873.584746	22.817280
98.299229	2878.665228	22.822298
98.497115	2876.390307	22.827315
98.365105	2892.375122	22.832333
98.662925	2894.806203	22.837351
99.030215	2889.257020	22.842368
98.754675	2892.289233	22.847386
98.678075	2895.031471	22.852403
98.907131	2908.523152	22.857421
99.455670	2911.107481	22.862439
99.529438	2917.405287	22.867456
99.188692	2919.456676	22.872474
99.576618	2913.298264	22.877491
99.531357	2910.281854	22.882509
99.588919	2923.525826	22.887527
99.997029	2928.142656	22.892544
100.256266	2931.993763	22.897562
100.015797	2936.993112	22.902579
100.228918	2933.355476	22.907597
100.176308	2932.839922	22.912615
100.544289	2929.982855	22.917632
100.611506	2945.958597	22.922650
101.116638	2950.197269	22.927667
100.993192	2952.044182	22.932685
101.245100	2956.218374	22.937703
101.503088	2937.531262	22.942720
101.517632	2930.888477	22.947738
101.569947	2921.244547	22.952755
101.466202	2917.927992	22.957773
101.659188	2920.325002	22.962791
101.299573	2910.035473	22.967808
101.614626	2924.874013	22.972826
101.580217	2939.527445	22.977843
101.690099	2937.367303	22.982861
101.646688	2941.991754	22.987879
102.232516	2941.486640	22.992896
102.001278	2950.275141	22.997914
102.079921	2942.972132	23.002931
102.355695	2943.282552	23.007949
102.147693	2944.546190	23.012967
102.399040	2927.160482	23.017984
102.090094	2944.138860	23.023002
102.042607	2957.557126	23.028019
102.678153	2956.482419	23.033037
102.429357	2966.788655	23.038055
102.654127	2970.888198	23.043072
102.649536	2987.749496	23.048090
102.978991	2991.763205	23.053107
102.947541	2984.019778	23.058125
102.890203	2996.167665	23.063143
103.057190	3000.705512	23.068160
103.176277	3023.578982	23.073178
102.901378	3032.806764	23.078195
103.507520	3025.919758	23.083213
103.711304	3040.106708	23.088231
103.597709	3041.295594	23.093248
103.852832	3044.607656	23.098266
104.091006	3047.366881	23.103283
103.854553	3053.741743	23.108301
104.185235	3065.150297	23.113319
104.556631	3063.608818	23.118336
104.241148	3071.826676	23.123354
104.643364	3061.502920	23.128371
104.602106	3068.238577	23.133389
104.881573	3084.496810	23.138407
104.710961	3076.885614	23.143424
105.110905	3086.086599	23.148442
105.352983	3085.748963	23.153459
105.238271	3084.675014	23.158477
105.522206	3096.065662	23.163495
105.738625	3101.892998	23.168512
106.084399	3111.800010	23.173530
105.717041	3109.916617	23.178547
105.762446	3099.115340	23.183565
105.721515	3109.477465	23.188583
105.699665	3102.650945	23.193600
105.844315	3109.922455	23.198618
106.325463	3121.070754	23.203635
106.828206	3124.981594	23.208653
106.628664	3135.422240	23.213671
106.979756	3128.704561	23.218688
106.675865	3129.992703	23.223706
106.533272	3138.028849	23.228723
106.939736	3129.061569	23.233741
106.758164	3133.521497	23.238759
107.175208	3139.775067	23.243776
107.304275	3137.343616	23.248794
107.631936	3144.532812	23.253811
107.884874	3146.450180	23.258829
107.459261	3152.359185	23.263847
107.738567	3149.474946	23.268864
108.249768	3151.241384	23.273882
107.918152	3145.063065	23.278899
108.405160	3150.705993	23.283917
108.200590	3145.520920	23.288935
108.347029	3144.939456	23.293952
108.289084	3139.680913	23.298970
108.274741	3139.023639	23.303987
108.690774	3157.791842	23.309005
108.612243	3165.243527	23.314023
108.580001	3167.644295	23.319040
108.662397	3162.041822	23.324058
108.659946	3170.128619	23.329075
108.907533	3166.700161	23.334093
108.852659	3179.052940	23.339111
109.169346	3181.231762	23.344128
109.253462	3185.886795	23.349146
109.112766	3188.841119	23.354163
109.448216	3193.298965	23.359181
109.207986	3199.081096	23.364199
109.520836	3203.586673	23.369216
110.029541	3215.705993	23.374234
109.912976	3220.686007	23.379251
109.803480	3212.812678	23.384269
109.795959	3220.767730	23.389287
109.955476	3224.849148	23.394304
110.303143	3232.483431	23.399322
110.477410	3240.877135	23.404339
110.920272	3237.882039	23.409357
110.836504	3236.118327	23.414375
110.794995	3227.947121	23.419392
111.392466	3242.302957	23.424410
111.117761	3256.470356	23.429427
111.285799	3265.767736	23.434445
111.505264	3257.170566	23.439463
111.486079	3256.138453	23.444480
111.759999	3253.551729	23.449498
111.698126	3256.790402	23.454515
111.982888	3245.787411	23.459533
111.498531	3253.605716	23.464551
111.863922	3266.883774	23.469568
111.802691	3265.413216	23.474586
112.129104	3279.824174	23.479603
112.239581	3268.138318	23.484621
112.340756	3279.980654	23.489639
112.583119	3294.714105	23.494656
113.123448	3292.394951	23.499674
113.133450	3297.617127	23.504691
113.220093	3292.727262	23.509709
113.049869	3299.947181	23.514727
113.159329	3302.066953	23.519744
113.613099	3295.888627	23.524762
112.952864	3296.569795	23.529779
113.330283	3301.207313	23.534797
113.490150	3322.998488	23.539815
113.534317	3321.953290	23.544832
113.689091	3313.912262	23.549850
113.951604	3312.744480	23.554867
113.951938	3316.118605	23.559885
114.055827	3326.600197	23.564903
114.129691	3337.424220	23.569920
114.724895	3334.720868	23.574938
114.559917	3344.928968	23.579955
114.859825	3339.166111	23.584973
114.661632	3341.971654	23.589991
114.845763	3339.847176	23.595008
114.770482	3349.141689	23.600026
115.227212	3359.946772	23.605043
115.254341	3359.380838	23.610061
115.209536	3361.651036	23.615079
115.378209	3356.846147	23.620096
115.412751	3353.649878	23.625114
115.252827	3371.511158	23.630131
115.475143	3368.133966	23.635149
115.382089	3372.311802	23.640167
115.469782	3380.946387	23.645184
115.797427	3385.414973	23.650202
115.926558	3403.837003	23.655219
115.915972	3402.942411	23.660237
116.373516	3409.129761	23.665255
116.283166	3412.606488	23.670272
116.931750	3420.218956	23.675290
116.444074	3423.095116	23.680307
116.802788	3415.934257	23.685325
117.331040	3419.386663	23.690343
117.082195	3422.477907	23.695360
117.087799	3424.942217	23.700378
117.119180	3427.213113	23.705395
117.594476	3431.930018	23.710413
117.626146	3441.971644	23.715431
117.795650	3436.791005	23.720448
118.157331	3436.327311	23.725466
117.710860	3449.025693	23.730483
118.432589	3443.256685	23.735501
117.678448	3439.751554	23.740519
118.245141	3460.705868	23.745536
118.622848	3458.582612	23.750554
118.451897	3459.755260	23.755571
118.489418	3461.517035	23.760589
118.368104	3455.656008	23.765607
118.530658	3464.376749	23.770624
118.989643	3478.183183	23.775642
119.032121	3489.933851	23.780659
119.099878	3487.723431	23.785677
119.137427	3485.792341	23.790695
119.221234	3503.271530	23.795712
119.578939	3511.835468	23.800730
119.776263	3515.222956	23.805747
119.563259	3508.476732	23.810765
119.800086	3521.244863	23.815783
119.767978	3532.789460	23.820800
120.087566	3530.271294	23.825818
119.843805	3543.947999	23.830835
120.103447	3540.192484	23.835853
120.849033	3552.429578	23.840871
120.894741	3560.717321	23.845888
121.085293	3556.679090	23.850906
120.885903	3562.293967	23.855923
120.931310	3558.556231	23.860941
121.405758	3554.931186	23.865959
121.171331	3565.342826	23.870976
121.442480	3579.667993	23.875994
121.320728	3582.168060	23.881011
121.373371	3577.015159	23.886029
121.731768	3580.992905	23.891047
121.562120	3599.029530	23.896064
121.971792	3598.905508	23.901082
121.692838	3606.129958	23.906099
121.926182	3600.617328	23.911117
122.604836	3611.261541	23.916135
122.383680	3631.512533	23.921152
122.674132	3622.215991	23.926170
122.836161	3626.644302	23.931187
122.779552	3619.561058	23.936205
123.294809	3621.001809	23.941223
123.300843	3625.388277	23.946240
123.620980	3627.348828	23.951258
123.434080	3645.429234	23.956275
123.786172	3635.914711	23.961293
124.066660	3640.772664	23.966311
123.634262	3638.994093	23.971328
124.100367	3638.154214	23.976346
123.935241	3639.654219	23.981363
123.899594	3643.078231	23.986381
124.207108	3646.104441	23.991399
123.809136	3665.145895	23.996416
124.556118	3670.552565	24.001434
124.701140	3671.546314	24.006451
124.683496	3671.710183	24.011469
124.462633	3666.972554	24.016487
124.695508	3678.027531	24.021504
124.976369	3687.705150	24.026522
125.007790	3694.821038	24.031539
125.519785	3695.949830	24.036557
125.346545	3698.691548	24.041575
125.077417	3700.810710	24.046592
125.250839	3708.781816	24.051610
125.463558	3716.276476	24.056627
125.753696	3714.037500	24.061645
125.953174	3721.903527	24.066663
126.192488	3733.352071	24.071680
126.413267	3737.569200	24.076698
126.427394	3735.401871	24.081715
126.948475	3736.128388	24.086733
126.740121	3746.602329	24.091751
126.605045	3745.140144	24.096768
127.247673	3743.117385	24.101786
127.069906	3752.557572	24.106803
127.449612	3752.889601	24.111821
127.615148	3755.448841	24.116839
127.287345	3760.196966	24.121856
127.368202	3755.118503	24.126874
127.943156	3758.112302	24.131891
127.758540	3767.979675	24.136909
128.215364	3774.808003	24.141927
128.238746	3768.255059	24.146944
128.297348	3774.514508	24.151962
128.126909	3770.794763	24.156979
128.305037	3769.359259	24.161997
128.489634	3779.171950	24.167015
128.453296	3798.103228	24.172032
128.793884	3793.637426	24.177050
129.019603	3803.390030	24.182067
128.792174	3811.345074	24.187085
129.369570	3808.821200	24.192103
129.636486	3817.509979	24.197120
129.583450	3808.412350	24.202138
129.729477	3814.680210	24.207155
129.927536	3815.763504	24.212173
129.928951	3818.686195	24.217191
130.108970	3839.370114	24.222208
130.267798	3831.807989	24.227226
130.388232	3835.756789	24.232243
130.276293	3837.239008	24.237261
130.906993	3829.991186	24.242279
130.435149	3843.078892	24.247296
130.953563	3853.871453	24.252314
130.724021	3867.760806	24.257331
130.832655	3866.203615	24.262349
131.310887	3857.410959	24.267367
131.695254	3868.985213	24.272384
131.794013	3880.329616	24.277402
131.432622	3892.311108	24.282419
131.852810	3894.953570	24.287437
131.978631	3889.628142	24.292455
132.031683	3887.729300	24.297472
131.966335	3889.557736	24.302490
132.070339	3900.042799	24.307507
132.122777	3909.216586	24.312525
132.407814	3902.859328	24.317543
132.041952	3915.434933	24.322560
132.574789	3923.286697	24.327578
132.781656	3928.588685	24.332595
132.948109	3936.387383	24.337613
132.994902	3928.385096	24.342631
133.053516	3941.045721	24.347648
133.393454	3955.445632	24.352666
133.584505	3962.205197	24.357683
133.446015	3951.722608	24.362701
133.756655	3955.802611	24.367719
133.895613	3959.521278	24.372736
133.766814	3973.959920	24.377754
134.178265	3988.948366	24.382771
134.488881	3984.518778	24.387789
134.440524	3981.897221	24.392807
134.079756	3987.272376	24.397824
134.276490	3997.862910	24.402842
134.452732	4005.776891	24.407859
134.983493	4014.796883	24.412877
135.040708	4029.187488	24.417895
135.292758	4034.021596	24.422912
135.368320	4026.270426	24.427930
135.845732	4023.850566	24.432947
135.297719	4026.805711	24.437965
136.045661	4039.585669	24.442983
135.980622	4053.635618	24.448000
136.557011	4041.181863	24.453018
136.541809	4044.593279	24.458035
136.568509	4040.609019	24.463053
137.060661	4041.245390	24.468071
136.764582	4045.010137	24.473088
137.126665	4037.605465	24.478106
137.290325	4042.008372	24.483123
136.978571	4036.669389	24.488141
137.355731	4046.414180	24.493159
137.254039	4049.438285	24.498176
137.388201	4065.322463	24.503194
137.587993	4063.596310	24.508211
137.707279	4078.627448	24.513229
137.875930	4078.184513	24.518247
137.989890	4086.101974	24.523264
137.838924	4070.814078	24.528282
138.474709	4074.205575	24.533299
138.545133	4089.575799	24.538317
138.574060	4092.266963	24.543335
138.765856	4104.824771	24.548352
138.383042	4094.989563	24.553370
138.831075	4102.968323	24.558387
138.888267	4124.470381	24.563405
139.398277	4128.143576	24.568423
139.580157	4131.211647	24.573440
139.431269	4129.316011	24.578458
139.789897	4131.614635	24.583475
139.824985	4136.539577	24.588493
139.990951	4137.403814	24.593511
140.050109	4145.557149	24.598528
140.523519	4152.875422	24.603546
140.611633	4149.989417	24.608563
140.423912	4171.179539	24.613581
140.915195	4171.648762	24.618599
140.831727	4159.411936	24.623616
140.587794	4166.959388	24.628634
141.330902	4178.749089	24.633651
141.091489	4192.665488	24.638669
141.325322	4186.432941	24.643687
141.086086	4198.070385	24.648704
141.385320	4201.656673	24.653722
141.867757	4215.327429	24.658739
141.455513	4221.960660	24.663757
141.977318	4215.755584	24.668775
141.907514	4225.848263	24.673792
142.321663	4236.117640	24.678810
142.113242	4240.058079	24.683827
142.438758	4241.812688	24.688845
142.607223	4259.301439	24.693863
143.016789	4271.891530	24.698880
143.017519	4273.188841	24.703898
143.154164	4269.774402	24.708915
143.282322	4263.214334	24.713933
143.408329	4262.026846	24.718951
143.807158	4278.542065	24.723968
143.797579	4281.409739	24.728986
143.678903	4278.584518	24.734003
143.612588	4281.053900	24.739021
144.016965	4301.671633	24.744039
144.586040	4304.322396	24.749056
144.403209	4315.083058	24.754074
144.891688	4312.405756	24.759091
144.785561	4312.735002	24.764109
145.021510	4315.122312	24.769127
145.049919	4324.631500	24.774144
145.266634	4330.812711	24.779162
145.062609	4337.299729	24.784179
145.254948	4337.440176	24.789197
145.638821	4343.850874	24.794215
145.774212	4360.069701	24.799232
145.843804	4364.695749	24.804250
146.079883	4360.618644	24.809267
146.100172	4368.175287	24.814285
146.399134	4369.754152	24.819303
146.466856	4376.836213	24.824320
146.592740	4383.817627	24.829338
146.920797	4381.146510	24.834355
146.859957	4400.274798	24.839373
147.075729	4408.561537	24.844391
147.354791	4408.846220	24.849408
147.364597	4410.186309	24.854426
147.654210	4409.276200	24.859443
147.628188	4430.043577	24.864461
147.849123	4435.498177	24.869479
147.877069	4427.097752	24.874496
147.753444	4433.524862	24.879514
148.133835	4440.488520	24.884531
148.015355	4454.389330	24.889549
148.288486	4451.985637	24.894567
148.896697	4467.142511	24.899584
148.717976	4481.021214	24.904602
149.233818	4465.805279	24.909619
149.045970	4473.318819	24.914637
149.060465	4487.754358	24.919655
149.404919	4497.034204	24.924672
149.285573	4499.395134	24.929690
149.685827	4503.669549	24.934707
149.912332	4512.541758	24.939725
150.199115	4510.236926	24.944743
150.392859	4518.277805	24.949760
150.440925	4518.870137	24.954778
150.596585	4524.098255	24.959795
150.585037	4539.248122	24.964813
151.106955	4530.726069	24.969831
150.973070	4531.769875	24.974848
150.811063	4543.679523	24.979866
151.136401	4553.309604	24.984883
151.347330	4560.590255	24.989901
151.707748	4562.563538	24.994919
151.739619	4560.655319	24.999936
151.920551	4585.121411	25.004954
152.130030	4585.454877	25.009971
152.451997	4587.491004	25.014989
152.603748	4588.982475	25.020007
152.796086	4582.503775	25.025024
152.707612	4591.611602	25.030042
152.830810	4582.997323	25.035059
152.878933	4589.470180	25.040077
152.961349	4603.557427	25.045095
153.162806	4607.736753	25.050112
153.143850	4620.365814	25.055130
153.301282	4616.275722	25.060147
153.543965	4630.473610	25.065165
153.607061	4642.745774	25.070183
153.480661	4634.808188	25.075200
153.699401	4654.296973	25.080218
154.257526	4651.293062	25.085235
154.279942	4657.378565	25.090253
154.707699	4674.520913	25.095271
154.752148	4678.709071	25.100288
154.592994	4693.468690	25.105306
154.601154	4687.397589	25.110323
154.593621	4698.370907	25.115341
155.172257	4709.359720	25.120359
155.340343	4713.717906	25.125376
155.610748	4734.338182	25.130394
155.848550	4740.323682	25.135411
156.062366	4742.910221	25.140429
156.295186	4739.382776	25.145447
156.009654	4750.248167	25.150464
156.006872	4759.424722	25.155482
156.441375	4763.725399	25.160499
156.783234	4787.210126	25.165517
156.803462	4789.539758	25.170535
157.159153	4787.716514	25.175552
156.813849	4792.473959	25.180570
157.264713	4803.656456	25.185587
157.644604	4814.439730	25.190605
157.519821	4816.962536	25.195623
157.751314	4827.437632	25.200640
157.872404	4842.952068	25.205658
158.204321	4839.235470	25.210675
158.134827	4851.478043	25.215693
158.389834	4852.814471	25.220711
158.755391	4849.888046	25.225728
158.636839	4849.793116	25.230746
159.153229	4854.939563	25.235763
159.935445	4864.861234	25.240781
159.818672	4860.564680	25.245799
160.208213	4858.909735	25.250816
160.091706	4863.498779	25.255834
160.160023	4855.060267	25.260851
160.095817	4858.438478	25.265869
160.119398	4866.903894	25.270887
160.453111	4857.675703	25.275904
160.386458	4877.506153	25.280922
160.700255	4881.996223	25.285939
160.845420	4887.039854	25.290957
160.842226	4886.980512	25.295975
161.324226	4893.489669	25.300992
161.537140	4907.310496	25.306010
161.568539	4906.563922	25.311027
161.803434	4906.820813	25.316045
161.628058	4908.631866	25.321063
161.892753	4908.795704	25.326080
161.937209	4928.813979	25.331098
161.967990	4931.230358	25.336115
162.227573	4938.408842	25.341133
162.870859	4948.364951	25.346151
163.160765	4950.769146	25.351168
163.008522	4956.402317	25.356186
163.046511	4956.604830	25.361203
163.165401	4957.902617	25.366221
163.261544	4956.533527	25.371239
163.794191	4958.088461	25.376256
163.560726	4971.613110	25.381274
163.792649	4974.177907	25.386291
163.974629	4983.515022	25.391309
163.756044	4990.825257	25.396327
164.508901	4990.574867	25.401344
164.269453	5008.999455	25.406362
164.678680	5006.520708	25.411379
164.106675	5004.852252	25.416397
164.480575	5017.369536	25.421415
165.207850	5019.910396	25.426432
164.758738	5028.898174	25.431450
165.138726	5050.862120	25.436467
165.348817	5058.136789	25.441485
165.576595	5056.579770	25.446503
165.612599	5077.663295	25.451520
165.840571	5083.426333	25.456538
166.101477	5086.898854	25.461555
166.437676	5094.554665	25.466573
166.825523	5099.096319	25.471591
166.970623	5108.559226	25.476608
166.759854	5105.154868	25.481626
166.824064	5114.352672	25.486643
167.253011	5128.742730	25.491661
167.022451	5142.443819	25.496679
167.561326	5145.263583	25.501696
167.857442	5153.885299	25.506714
167.735772	5155.735312	25.511731
168.073118	5157.033611	25.516749
168.373186	5185.367601	25.521767
168.588374	5189.519658	25.526784
168.618426	5179.694935	25.531802
168.343317	5182.522278	25.536819
168.973786	5198.888409	25.541837
169.058963	5199.976848	25.546855
168.991124	5203.977540	25.551872
168.948059	5218.798312	25.556890
169.054507	5229.362675	25.561907
169.778768	5234.325148	25.566925
170.001947	5248.400312	25.571943
170.355791	5254.601391	25.576960
170.400149	5258.764444	25.581978
170.763331	5266.627593	25.586995
170.979626	5280.344006	25.592013
170.903765	5278.553602	25.597031
171.409878	5269.642265	25.602048
171.628899	5281.761011	25.607066
171.446472	5298.513428	25.612083
171.461749	5301.756160	25.617101
171.705033	5305.809144	25.622119
172.151545	5296.436796	25.627136
171.922696	5301.567548	25.632154
172.196424	5314.305910	25.637171
172.558349	5318.053058	25.642189
172.312655	5315.556923	25.647207
172.837280	5324.000874	25.652224
173.111929	5343.033400	25.657242
173.210339	5350.410911	25.662259
173.547757	5344.736247	25.667277
173.260464	5345.586325	25.672295
173.474808	5358.501323	25.677312
173.686964	5367.871788	25.682330
173.870035	5376.542887	25.687348
174.414422	5375.655951	25.692365
174.083511	5394.808654	25.697383
174.394417	5392.067477	25.702400
174.742399	5390.526322	25.707418
174.655570	5399.751089	25.712436
175.197194	5408.034585	25.717453
175.008850	5414.137577	25.722471
175.206483	5423.229405	25.727488
175.191107	5420.987582	25.732506
175.468028	5430.774078	25.737524
176.017650	5428.203835	25.742541
175.786315	5441.292883	25.747559
175.927491	5449.200362	25.752576
176.316727	5457.211031	25.757594
176.505311	5474.555751	25.762612
176.626905	5474.530520	25.767629
176.704752	5487.501717	25.772647
177.100999	5497.547339	25.777664
177.080158	5492.964134	25.782682
177.102704	5497.083309	25.787700
177.687936	5506.149179	25.792717
177.554072	5523.598125	25.797735
177.920753	5521.492147	25.802752
177.900269	5536.959909	25.807770
178.086721	5544.658311	25.812788
178.412802	5544.118077	25.817805
178.333699	5546.665392	25.822823
178.779032	5555.737421	25.827840
178.612726	5563.784665	25.832858
178.692445	5580.720392	25.837876
179.315668	5573.113202	25.842893
179.722009	5587.387211	25.847911
179.882779	5586.724512	25.852928
180.355069	5603.759749	25.857946
180.425253	5602.303135	25.862964
180.300402	5605.788841	25.867981
180.325087	5606.915190	25.872999
180.561282	5618.318065	25.878016
180.885949	5615.476843	25.883034
180.809779	5627.354809	25.888052
181.162789	5636.763323	25.893069
181.558779	5644.558363	25.898087
181.359730	5647.440151	25.903104
181.703660	5659.381747	25.908122
181.972938	5663.708525	25.913140
182.115882	5676.650718	25.918157
182.258108	5687.818981	25.923175
182.180411	5689.905221	25.928192
182.516092	5692.229742	25.933210
182.688469	5706.035430	25.938228
183.178984	5722.815389	25.943245
183.149715	5721.598471	25.948263
183.212152	5729.000712	25.953280
183.917109	5725.152890	25.958298
183.929087	5737.351727	25.963316
184.034454	5743.030011	25.968333
184.151530	5738.349378	25.973351
184.417669	5755.167675	25.978368
184.683101	5753.064907	25.983386
184.921667	5756.095965	25.988404
184.932762	5755.930211	25.993421
185.172617	5765.590113	25.998439
185.517683	5784.694143	26.003456
185.569020	5783.685561	26.008474
185.440182	5780.580752	26.013492
185.990622	5784.352128	26.018509
185.883368	5795.881524	26.023527
185.940558	5808.426874	26.028544
186.395952	5802.979809	26.033562
186.240913	5824.444520	26.038580
186.843235	5830.215438	26.043597
187.058234	5834.572859	26.048615
187.155614	5834.175774	26.053632
187.445139	5832.492221	26.058650
187.421265	5849.813761	26.063668
187.476739	5862.154232	26.068685
187.567459	5856.240269	26.073703
187.644613	5857.333161	26.078720
187.901328	5873.528017	26.083738
187.734998	5884.817344	26.088756
188.515429	5895.544825	26.093773
188.915830	5903.755972	26.098791
188.373000	5915.524145	26.103808
189.020391	5918.090279	26.108826
189.011064	5933.935434	26.113844
189.169088	5934.497960	26.118861
189.680189	5953.598252	26.123879
189.491758	5969.051652	26.128896
190.112231	5956.738060	26.133914
190.055071	5981.543217	26.138932
190.300771	5971.820023	26.143949
190.377510	5988.731342	26.148967
190.814119	5999.250741	26.153984
191.315131	6005.782576	26.159002
190.738459	6015.213820	26.164020
191.746113	6027.534657	26.169037
191.625726	6035.565443	26.174055
191.211209	6031.760357	26.179072
191.880121	6041.400539	26.184090
192.104757	6057.537448	26.189108
192.546567	6060.019011	26.194125
192.565029	6066.957923	26.199143
192.838918	6080.504923	26.204160
192.931852	6077.873556	26.209178
192.828624	6082.842790	26.214196
193.377365	6097.760965	26.219213
193.703584	6118.620291	26.224231
193.256192	6107.765005	26.229248
193.853453	6118.991671	26.234266
193.732857	6130.434978	26.239284
193.849811	6140.354246	26.244301
194.480760	6159.568562	26.249319
194.282571	6175.475082	26.254336
194.825008	6178.818476	26.259354
194.900273	6184.552121	26.264372
195.411424	6197.373864	26.269389
195.714635	6207.949007	26.274407
195.680080	6212.162521	26.279424
196.122756	6210.145578	26.284442
196.270176	6224.006076	26.289460
196.589128	6223.012367	26.294477
196.514167	6226.253617	26.299495
196.841449	6235.578081	26.304512
196.918520	6241.554533	26.309530
197.259533	6248.468237	26.314548
197.455969	6264.710764	26.319565
197.524901	6261.915822	26.324583
197.950052	6273.119038	26.329600
198.035180	6281.395531	26.334618
198.257724	6283.747324	26.339636
197.902188	6280.561144	26.344653
198.292314	6294.374202	26.349671
198.381433	6311.369113	26.354688
199.157523	6319.089113	26.359706
199.051991	6326.947232	26.364724
198.977138	6325.901568	26.369741
199.292522	6333.551693	26.374759
199.392133	6344.764916	26.379776
199.738300	6342.450556	26.384794
199.445078	6356.579064	26.389812
200.000999	6367.023162	26.394829
200.163913	6383.517277	26.399847
200.082569	6378.539259	26.404864
200.392641	6397.460005	26.409882
200.489530	6405.766279	26.414900
200.971400	6418.517002	26.419917
200.944625	6433.288853	26.424935
200.808825	6438.522144	26.429952
201.337272	6451.467628	26.434970
201.840792	6462.030479	26.439988
201.996756	6471.659702	26.445005
202.320413	6478.831914	26.450023
202.716236	6497.969777	26.455040
203.059749	6496.905913	26.460058
203.061339	6506.332049	26.465076
203.432702	6512.303524	26.470093
203.299267	6514.941562	26.475111
203.960674	6527.471668	26.480128
203.599975	6526.669653	26.485146
203.757978	6534.578123	26.490164
203.780579	6556.792439	26.495181
203.958139	6554.277176	26.500199
204.174976	6571.697432	26.505216
204.679096	6581.931948	26.510234
204.922901	6600.869599	26.515252
205.294668	6608.394204	26.520269
205.540650	6607.137263	26.525287
205.475926	6617.943910	26.530304
205.950272	6628.426193	26.535322
206.017036	6631.686350	26.540340
206.257741	6637.987706	26.545357
206.650501	6648.921583	26.550375
206.693884	6653.981650	26.555392
207.014085	6664.229241	26.560410
207.166151	6674.597883	26.565428
207.039760	6677.061215	26.570445
207.683157	6695.232386	26.575463
207.737669	6705.442703	26.580480
208.122870	6708.163675	26.585498
208.029450	6719.622032	26.590516
208.324967	6740.916210	26.595533
208.639405	6723.940022	26.600551
208.911043	6742.892401	26.605568
208.904369	6747.006964	26.610586
209.601847	6750.597667	26.615604
209.645725	6758.309446	26.620621
209.856407	6780.557705	26.625639
209.709748	6790.581761	26.630656
210.262325	6782.508457	26.635674
210.253446	6798.742584	26.640692
209.959311	6805.459257	26.645709
210.692485	6812.175993	26.650727
210.527304	6830.979072	26.655744
211.097946	6835.385193	26.660762
210.772453	6852.357167	26.665780
210.921084	6865.318251	26.670797
211.544023	6873.476032	26.675815
212.020874	6887.326463	26.680832
212.102179	6892.342772	26.685850
212.501866	6907.648002	26.690868
212.556518	6914.796234	26.695885
213.061183	6915.847470	26.700903
213.189928	6936.467173	26.705920
213.183523	6934.690979	26.710938
213.299301	6946.344001	26.715956
213.445754	6954.674329	26.720973
214.039920	6956.586006	26.725991
214.115771	6969.299701	26.731008
214.301545	6967.717536	26.736026
214.162079	6977.907882	26.741044
214.290940	6993.587087	26.746061
214.702294	6997.986634	26.751079
215.062889	7016.117192	26.756096
215.095458	7020.541359	26.761114
215.350354	7028.886301	26.766132
215.258678	7039.634281	26.771149
215.809203	7045.120112	26.776167
215.998001	7063.830090	26.781184
216.489837	7059.939621	26.786202
216.472632	7073.555058	26.791220
216.682970	7092.653148	26.796237
216.980759	7095.725663	26.801255
217.112137	7107.445796	26.806272
217.214827	7111.877942	26.811290
217.597764	7130.298706	26.816308
217.660728	7144.593002	26.821325
218.541162	7151.908710	26.826343
218.103113	7155.652132	26.831360
218.277834	7164.836811	26.836378
218.645196	7169.445335	26.841396
218.559124	7181.401624	26.846413
219.083529	7187.756590	26.851431
219.377645	7196.256467	26.856448
219.274050	7219.488945	26.861466
219.612684	7230.598968	26.866484
219.901796	7243.326796	26.871501
220.010306	7239.976197	26.876519
220.203258	7265.804637	26.881536
220.846552	7259.648967	26.886554
221.377385	7276.070461	26.891572
221.235785	7291.375573	26.896589
221.581799	7290.087130	26.901607
221.985964	7299.687376	26.906624
221.931506	7307.938846	26.911642
222.350857	7314.578655	26.916660
222.643402	7312.739807	26.921677
222.525381	7327.349881	26.926695
222.716369	7332.488034	26.931712
222.496306	7332.986714	26.936730
222.999127	7350.198745	26.941748
223.275262	7363.197031	26.946765
223.576616	7370.294164	26.951783
224.020356	7383.193597	26.956800
224.525112	7395.044838	26.961818
224.591073	7408.274971	26.966836
224.947707	7419.590648	26.971853
224.725912	7410.915438	26.976871
224.970970	7427.186105	26.981888
225.099138	7436.987510	26.986906
225.781582	7442.496992	26.991924
225.732383	7457.358417	26.996941
226.266314	7462.259776	27.001959
226.557865	7458.567922	27.006976
226.658178	7468.619951	27.011994
226.798818	7478.744594	27.017012
226.680520	7492.833940	27.022029
227.041379	7495.492548	27.027047
227.215905	7514.505135	27.032064
227.202495	7517.746440	27.037082
227.573138	7521.824165	27.042100
227.408853	7545.016049	27.047117
228.035891	7559.001310	27.052135
227.863531	7572.862412	27.057152
228.302363	7582.962496	27.062170
228.595449	7595.263750	27.067188
228.736296	7605.407372	27.072205
229.432055	7611.508338	27.077223
229.694277	7626.441078	27.082240
229.810725	7625.854706	27.087258
230.274929	7630.830174	27.092276
230.017339	7652.189959	27.097293
230.593090	7644.996616	27.102311
230.512075	7645.757652	27.107328
230.644682	7667.671944	27.112346
230.867861	7669.900694	27.117364
231.014296	7689.640819	27.122381
231.296291	7688.586528	27.127399
231.863127	7705.867790	27.132416
231.910131	7727.467233	27.137434
232.381324	7726.399086	27.142452
232.418399	7736.164408	27.147469
232.595425	7740.979689	27.152487
232.719251	7756.903423	27.157504
233.122061	7769.904252	27.162522
233.526444	7771.624758	27.167540
233.472522	7791.431107	27.172557
233.732938	7797.994965	27.177575
234.113643	7815.166580	27.182592
234.457117	7819.431737	27.187610
234.672341	7823.660159	27.192628
234.849416	7836.519604	27.197645
235.164837	7840.789161	27.202663
235.637329	7854.483154	27.207680
235.643820	7857.749814	27.212698
235.903824	7869.854384	27.217716
235.986078	7879.416967	27.222733
236.395050	7892.527414	27.227751
236.635997	7897.136985	27.232768
236.535448	7915.760562	27.237786
237.058053	7911.252628	27.242804
237.167060	7936.905737	27.247821
237.495376	7938.092004	27.252839
237.788365	7946.333528	27.257856
237.888429	7959.037798	27.262874
238.161751	7960.144284	27.267892
238.271155	7982.220438	27.272909
238.351854	7993.181906	27.277927
238.807523	8003.705789	27.282944
239.268648	8012.100955	27.287962
239.327345	8019.526805	27.292980
239.084453	8040.591127	27.297997
239.212883	8047.103139	27.303015
240.024275	8066.354332	27.308032
240.408911	8074.190077	27.313050
240.804347	8094.475688	27.318068
241.201030	8091.711209	27.323085
241.156976	8106.127200	27.328103
241.577560	8117.022867	27.333120
241.730566	8124.067762	27.338138
242.051447	8122.151783	27.343156
242.271042	8148.062528	27.348173
242.631189	8153.704803	27.353191
242.541227	8149.864211	27.358208
242.811445	8173.039328	27.363226
242.973830	8162.185163	27.368244
243.274489	8178.873992	27.373261
243.465437	8195.052786	27.378279
243.704839	8194.633405	27.383296
243.929767	8213.095794	27.388314
244.174121	8222.472148	27.393332
244.215793	8229.689223	27.398349
244.576364	8244.982754	27.403367
244.999283	8250.580497	27.408384
244.522872	8258.544896	27.413402
245.650692	8275.018989	27.418420
245.516413	8278.001535	27.423437
245.871709	8294.214656	27.428455
246.388288	8294.099134	27.433472
246.399057	8301.017994	27.438490
246.661564	8325.706772	27.443508
246.759778	8329.057018	27.448525
247.046157	8330.843422	27.453543
247.483264	8343.198386	27.458560
247.139823	8356.970061	27.463578
247.538523	8362.404305	27.468596
247.759234	8376.674843	27.473613
248.087593	8394.944411	27.478631
248.377046	8400.654666	27.483648
248.595058	8421.824017	27.488666
249.006405	8423.600325	27.493684
249.014743	8443.517590	27.498701
249.609792	8446.455366	27.503719
249.997028	8453.198493	27.508736
250.128945	8468.168114	27.513754
250.258484	8472.476410	27.518772
250.713346	8480.175041	27.523789
250.767108	8504.331629	27.528807
251.250693	8516.262683	27.533824
251.207118	8523.505856	27.538842
251.574520	8524.521867	27.543860
251.623275	8549.055000	27.548877
251.990696	8553.247120	27.553895
252.134027	8562.955190	27.558912
252.175469	8585.838318	27.563930
252.779990	8596.620211	27.568948
253.271872	8617.238577	27.573965
253.857014	8621.169289	27.578983
253.941882	8625.948724	27.584000
253.822891	8630.469635	27.589018
254.377776	8632.166648	27.594036
254.684973	8657.660264	27.599053
254.551461	8667.879022	27.604071
255.206170	8671.246339	27.609088
255.134006	8688.335009	27.614106
255.532962	8698.432483	27.619124
255.504498	8697.508860	27.624141
256.016216	8719.374481	27.629159
256.288110	8728.102711	27.634176
256.322730	8747.927784	27.639194
256.450289	8753.635095	27.644212
256.684770	8766.299920	27.649229
257.051495	8776.614018	27.654247
257.505267	8788.237356	27.659264
257.404517	8802.959548	27.664282
257.968710	8817.331322	27.669300
258.299530	8829.643276	27.674317
258.832554	8839.966088	27.679335
259.189663	8849.391399	27.684352
259.182085	8866.018633	27.689370
259.874336	8859.226486	27.694388
259.637721	8869.401519	27.699405
259.684970	8878.319715	27.704423
259.861973	8887.729059	27.709440
259.978292	8910.780820	27.714458
260.598552	8927.398157	27.719476
260.883636	8930.747653	27.724493
260.723507	8949.858344	27.729511
261.056847	8959.710504	27.734528
261.580788	8990.569499	27.739546
261.808875	8996.333754	27.744564
261.871287	8995.272747	27.749581
262.167204	9003.088058	27.754599
262.638855	9012.173470	27.759616
262.902229	9037.958627	27.764634
262.942934	9032.553486	27.769652
263.617385	9047.037614	27.774669
263.450703	9061.902944	27.779687
264.379584	9065.268429	27.784704
264.407081	9089.919268	27.789722
264.385957	9092.732670	27.794740
264.569106	9089.859421	27.799757
264.706651	9105.374881	27.804775
265.068208	9116.634000	27.809792
265.178526	9143.554638	27.814810
265.560997	9159.249626	27.819828
265.866253	9173.027629	27.824845
266.304924	9187.908733	27.829863
266.563951	9196.484493	27.834880
266.364241	9208.649328	27.839898
266.513861	9216.724443	27.844916
267.345847	9230.145291	27.849933
267.528748	9247.049284	27.854951
268.136167	9264.126742	27.859968
267.873716	9283.973667	27.864986
267.907134	9289.503296	27.870004
268.607797	9307.071355	27.875021
268.404548	9322.668799	27.880039
269.380103	9325.045102	27.885056
269.643224	9349.214194	27.890074
269.852724	9362.827373	27.895092
270.414252	9366.540935	27.900109
270.113958	9392.459088	27.905127
270.595883	9395.601023	27.910144
270.930137	9404.730254	27.915162
271.768231	9425.465781	27.920180
271.984226	9428.235773	27.925197
271.740061	9434.418292	27.930215
272.082922	9437.904066	27.935232
272.466510	9457.602611	27.940250
272.546218	9476.786777	27.945268
272.951639	9486.662657	27.950285
273.295207	9490.666132	27.955303
273.163735	9503.846601	27.960320
273.501209	9516.827324	27.965338
273.892834	9530.952000	27.970356
274.025106	9539.250986	27.975373
274.187489	9567.003931	27.980391
275.239702	9569.264067	27.985408
275.174888	9587.918453	27.990426
275.232042	9596.311323	27.995444
275.572207	9614.624448	28.000461
275.639719	9619.864674	28.005479
275.877856	9639.832471	28.010496
276.037770	9646.182246	28.015514
276.344240	9661.207577	28.020532
276.975989	9680.655940	28.025549
276.844396	9695.787811	28.030567
277.479698	9704.494304	28.035584
277.726967	9727.191882	28.040602
277.925642	9742.982462	28.045620
278.215875	9756.431728	28.050637
278.712534	9777.268498	28.055655
279.039896	9765.298261	28.060672
279.156539	9798.650425	28.065690
279.545731	9812.096859	28.070708
279.965069	9816.871566	28.075725
279.830010	9829.936004	28.080743
280.485233	9844.013310	28.085760
280.833131	9852.449156	28.090778
280.761339	9860.638171	28.095796
281.162501	9872.213600	28.100813
281.331743	9885.618766	28.105831
281.609960	9892.695238	28.110848
281.904934	9903.314843	28.115866
281.911793	9917.844244	28.120884
282.550864	9928.040544	28.125901
282.357035	9943.621244	28.130919
283.116373	9965.178009	28.135936
283.199092	9972.995553	28.140954
283.080332	9985.801797	28.145972
283.607017	9991.162798	28.150989
283.899525	10017.001583	28.156007
284.498708	10021.523993	28.161024
284.500226	10047.806240	28.166042
284.844116	10060.846329	28.171060
285.578342	10071.173043	28.176077
285.962486	10088.958771	28.181095
286.072203	10098.903403	28.186112
286.121666	10096.338269	28.191130
286.632794	10120.194816	28.196148
286.871020	10136.582603	28.201165
287.077057	10153.947938	28.206183
287.474489	10158.230448	28.211200
287.424784	10168.721068	28.216218
287.563082	10193.261287	28.221236
288.369443	10197.928103	28.226253
288.174249	10217.724436	28.231271
288.650816	10224.391069	28.236288
289.009715	10257.977645	28.241306
289.138457	10258.150214	28.246324
289.622852	10265.443969	28.251341
289.707291	10289.105505	28.256359
290.170728	10304.687740	28.261376
290.788293	10322.181370	28.266394
290.266391	10342.076376	28.271412
290.715413	10350.291372	28.276429
291.240828	10374.515431	28.281447
291.755917	10389.404473	28.286464
292.177498	10409.669578	28.291482
292.227907	10426.636444	28.296500
292.513012	10436.462214	28.301517
292.713087	10451.842701	28.306535
292.923938	10465.589090	28.311552
293.678957	10479.591254	28.316570
293.688196	10498.143380	28.321588
294.292564	10503.069258	28.326605
294.118716	10519.790321	28.331623
294.489921	10528.573307	28.336640
294.946897	10546.392267	28.341658
295.067904	10563.755516	28.346676
295.515550	10571.961354	28.351693
295.882058	10590.785987	28.356711
295.922084	10607.101037	28.361728
296.626296	10617.991640	28.366746
296.770234	10640.690730	28.371764
297.320322	10636.379928	28.376781
297.626783	10659.419854	28.381799
298.147821	10672.300005	28.386816
298.270328	10678.526534	28.391834
298.134707	10695.045999	28.396852
298.665333	10697.106971	28.401869
299.060771	10720.849794	28.406887
299.333999	10724.675104	28.411904
299.749814	10735.083645	28.416922
299.547828	10748.307612	28.421940
300.241354	10755.748780	28.426957
300.485874	10773.080245	28.431975
300.845521	10769.872810	28.436992
300.888106	10781.928088	28.442010
301.330062	10801.113704	28.447028
301.374590	10803.070856	28.452045
301.951342	10816.577047	28.457063
301.954431	10823.226498	28.462080
302.391579	10845.175771	28.467098
302.501860	10860.652758	28.472116
302.997266	10863.129749	28.477133
303.100435	10886.189170	28.482151
303.083103	10894.477462	28.487168
303.098381	10913.164829	28.492186
303.622791	10936.897196	28.497204
304.022371	10955.802271	28.502221
304.410798	10977.307798	28.507239
304.703751	10990.969088	28.512256
305.288893	11007.423283	28.517274
305.520132	11030.551232	28.522292
305.771327	11035.832548	28.527309
305.787576	11057.933260	28.532327
306.449366	11077.264706	28.537344
306.886675	11094.629420	28.542362
307.006480	11115.911948	28.547380
307.497221	11128.171956	28.552397
307.830711	11143.671048	28.557415
308.200133	11165.928122	28.562432
308.611951	11181.370768	28.567450
308.473178	11195.396653	28.572468
308.971242	11212.082545	28.577485
309.423694	11234.734026	28.582503
309.582918	11238.450997	28.587520
309.897451	11255.026742	28.592538
310.027003	11278.669831	28.597556
310.325239	11292.279991	28.602573
310.686991	11324.958639	28.607591
311.033452	11338.949668	28.612608
311.316263	11350.850847	28.617626
311.524018	11364.835206	28.622644
312.130670	11386.941705	28.627661
312.309649	11399.566493	28.632679
312.214945	11413.282503	28.637696
313.042504	11440.457225	28.642714
313.118017	11454.572883	28.647732
313.840752	11458.536336	28.652749
313.898710	11486.769507	28.657767
314.416321	11506.591317	28.662784
314.785381	11528.956239	28.667802
315.507113	11550.577570	28.672820
315.501344	11561.232600	28.677837
316.073783	11570.597144	28.682855
315.842909	11589.933175	28.687872
316.601290	11602.318926	28.692890
316.913103	11624.572939	28.697908
317.289475	11620.968031	28.702925
317.383098	11650.496828	28.707943
317.971729	11654.696053	28.712960
318.533360	11660.841491	28.717978
318.331623	11681.025628	28.722996
318.709853	11692.135284	28.728013
319.010458	11704.248625	28.733031
319.154286	11722.705094	28.738048
319.891740	11735.624706	28.743066
319.761520	11755.879821	28.748084
320.268019	11765.182165	28.753101
320.344832	11783.131327	28.758119
320.767792	11794.338241	28.763136
320.876645	11803.267130	28.768154
321.156405	11824.298048	28.773172
321.316150	11835.776733	28.778189
322.102306	11842.787010	28.783207
322.239912	11865.122278	28.788224
322.495353	11885.092920	28.793242
322.645333	11900.678223	28.798260
323.168187	11909.848610	28.803277
323.320646	11933.760500	28.808295
323.535844	11952.594416	28.813312
323.962530	11966.219680	28.818330
323.932469	11981.965879	28.823348
324.321086	12003.816749	28.828365
324.885541	12027.061088	28.833383
325.211643	12049.685981	28.838400
325.737420	12060.738007	28.843418
325.560129	12085.791171	28.848436
325.937835	12105.689213	28.853453
326.739330	12126.622952	28.858471
327.038340	12154.377276	28.863488
327.416200	12173.116461	28.868506
327.485323	12194.240786	28.873524
327.856471	12206.052884	28.878541
328.657257	12223.494334	28.883559
328.685807	12243.065123	28.888576
329.590995	12252.671560	28.893594
329.757364	12257.770727	28.898612
330.119258	12281.457625	28.903629
330.142570	12299.080933	28.908647
330.594213	12307.170071	28.913664
330.849020	12313.862721	28.918682
331.394769	12341.777612	28.923700
331.356739	12357.607476	28.928717
332.148794	12362.330772	28.933735
332.251991	12385.155191	28.938752
332.469921	12397.474556	28.943770
332.815315	12408.324524	28.948788
333.444176	12432.427676	28.953805
334.012126	12433.952488	28.958823
334.087418	12464.596985	28.963840
334.479095	12467.298861	28.968858
334.568440	12484.836210	28.973876
334.722582	12499.186645	28.978893
335.570132	12504.144439	28.983911
335.645282	12527.147104	28.988928
336.138849	12548.041130	28.993946
336.197060	12555.430966	28.998964
336.605303	12575.574191	29.003981
337.272029	12597.890599	29.008999
337.332510	12619.379907	29.014016
337.535554	12628.916529	29.019034
338.157222	12647.940097	29.024052
338.350099	12653.388900	29.029069
338.868727	12674.525454	29.034087
338.926198	12681.040727	29.039104
339.347291	12706.133609	29.044122
339.691850	12713.964963	29.049140
339.959217	12731.986231	29.054157
340.439133	12743.352158	29.059175
340.628595	12772.776121	29.064192
341.107174	12784.464386	29.069210
341.255808	12803.413790	29.074228
341.580731	12825.455590	29.079245
341.949159	12833.763255	29.084263
341.948623	12861.805542	29.089280
342.518042	12884.011217	29.094298
342.908066	12900.554483	29.099316
343.129956	12914.619884	29.104333
343.787690	12926.684385	29.109351
343.720748	12952.125622	29.114368
344.192707	12958.212904	29.119386
344.558497	12980.377958	29.124404
344.777443	13001.621823	29.129421
345.611940	13020.561903	29.134439
345.647770	13036.721820	29.139456
345.839854	13049.127766	29.144474
346.451708	13058.695305	29.149492
346.345360	13080.669169	29.154509
347.128062	13092.436304	29.159527
347.381454	13115.929665	29.164544
347.565861	13131.052691	29.169562
347.978972	13149.436795	29.174580
348.106484	13171.860455	29.179597
349.051191	13179.746416	29.184615
349.000209	13200.691730	29.189632
349.916566	13220.077090	29.194650
350.159837	13229.108758	29.199668
350.402169	13247.734451	29.204685
350.820902	13258.314468	29.209703
350.671912	13275.147764	29.214720
351.222656	13299.829538	29.219738
351.323048	13307.503594	29.224756
351.640020	13336.267391	29.229773
352.155218	13349.980848	29.234791
352.497533	13378.630211	29.239808
352.844999	13397.621697	29.244826
353.571891	13412.855767	29.249844
354.072584	13435.878143	29.254861
354.569679	13438.885763	29.259879
354.573059	13463.381905	29.264896
354.690589	13472.566022	29.269914
355.309389	13488.439210	29.274932
355.450356	13511.603293	29.279949
356.128369	13521.334396	29.284967
356.177193	13540.653869	29.289984
356.585670	13557.630625	29.295002
357.157648	13583.376850	29.300020
357.581575	13597.527958	29.305037
357.976635	13608.989809	29.310055
357.990002	13624.013702	29.315072
358.477325	13651.298604	29.320090
359.053791	13657.796077	29.325108
359.142573	13680.125347	29.330125
359.854754	13694.616654	29.335143
359.908794	13713.149136	29.340160
359.945173	13725.646234	29.345178
360.868160	13741.304610	29.350196
361.051142	13762.731813	29.355213
361.744445	13780.065224	29.360231
361.787820	13801.713296	29.365248
362.070430	13812.453902	29.370266
362.655670	13830.139040	29.375284
363.015531	13850.733331	29.380301
363.233710	13861.771441	29.385319
363.899887	13876.800648	29.390336
364.279755	13895.743346	29.395354
364.678184	13915.280030	29.400372
364.734599	13938.707367	29.405389
365.383733	13944.119812	29.410407
365.610331	13958.466320	29.415424
365.833268	13970.065885	29.420442
366.324050	13977.830648	29.425460
366.362484	14003.793661	29.430477
367.124400	14016.796284	29.435495
367.339904	14029.549751	29.440512
367.587400	14043.034050	29.445530
367.991446	14060.994118	29.450548
368.375512	14083.129178	29.455565
368.416241	14092.287728	29.460583
368.493171	14096.545558	29.465600
369.417436	14128.588279	29.470618
370.052066	14135.395776	29.475636
369.867531	14162.432948	29.480653
370.083300	14181.518486	29.485671
370.221008	14194.082131	29.490688
370.481367	14225.777401	29.495706
371.079333	14241.847131	29.500724
371.414281	14267.514565	29.505741
371.778136	14277.371065	29.510759
372.216796	14308.621671	29.515776
372.563025	14336.589710	29.520794
372.969839	14359.962677	29.525812
373.388188	14379.127216	29.530829
374.104428	14402.107528	29.535847
374.250188	14419.786263	29.540864
374.838728	14446.589047	29.545882
375.133494	14456.415407	29.550900
375.009989	14486.102646	29.555917
375.930085	14502.545333	29.560935
376.394110	14536.233602	29.565952
376.757784	14549.469515	29.570970
377.307244	14579.872611	29.575988
377.381829	14593.112782	29.581005
378.140280	14603.706662	29.586023
378.346802	14622.876204	29.591040
378.638975	14645.828492	29.596058
379.321396	14651.621227	29.601076
379.862378	14667.065448	29.606093
380.425912	14680.696503	29.611111
380.979207	14697.664229	29.616128
381.283054	14712.491885	29.621146
381.476932	14719.668663	29.626164
382.067658	14732.929145	29.631181
382.462075	14755.208643	29.636199
382.476213	14764.621180	29.641216
382.869884	14774.893310	29.646234
383.362768	14790.544133	29.651252
383.303902	14818.667924	29.656269
383.748043	14830.227048	29.661287
384.126176	14855.291606	29.666304
384.345110	14870.009515	29.671322
384.834878	14887.186329	29.676340
385.012535	14910.523228	29.681357
385.450652	14931.352775	29.686375
385.779437	14959.109701	29.691392
385.855675	14983.839569	29.696410
386.615005	15009.027797	29.701428
387.076053	15038.649595	29.706445
386.995634	15049.659369	29.711463
387.637373	15072.582681	29.716480
387.964216	15106.375561	29.721498
388.511797	15131.173911	29.726516
388.569300	15155.442670	29.731533
389.157246	15182.237109	29.736551
389.760531	15201.502997	29.741568
389.919356	15223.725197	29.746586
390.628439	15246.783451	29.751604
390.922700	15278.670974	29.756621
391.076714	15289.299910	29.761639
391.849498	15307.983495	29.766656
392.102707	15333.251430	29.771674
392.863579	15346.191967	29.776692
393.295456	15376.535794	29.781709
393.665515	15393.141212	29.786727
394.008181	15408.383384	29.791744
394.214601	15419.648480	29.796762
394.825997	15433.654735	29.801780
395.033109	15443.324786	29.806797
395.200849	15459.083939	29.811815
395.710083	15478.746996	29.816832
395.869414	15510.469700	29.821850
396.423906	15524.061719	29.826868
397.016491	15548.272428	29.831885
397.184898	15563.557811	29.836903
397.772993	15577.248830	29.841920
397.831256	15599.575652	29.846938
398.332084	15618.062106	29.851956
398.731775	15640.363920	29.856973
399.043759	15660.835018	29.861991
399.410274	15682.620948	29.867008
399.540740	15708.211807	29.872026
400.331783	15727.095080	29.877044
400.503977	15760.104796	29.882061
401.091137	15774.614121	29.887079
401.501893	15794.299246	29.892096
401.899560	15813.803255	29.897114
401.974118	15839.977873	29.902132
403.000960	15870.162962	29.907149
403.119172	15890.260383	29.912167
403.514152	15907.857239	29.917184
404.041768	15938.168010	29.922202
404.539446	15955.486675	29.927220
404.537743	15983.726398	29.932237
405.373458	16009.112436	29.937255
405.796411	16023.284454	29.942272
406.023542	16055.095349	29.947290
406.550301	16070.201827	29.952308
407.362279	16091.425732	29.957325
407.551087	16106.866275	29.962343
408.478605	16120.138138	29.967360
408.763185	16148.083743	29.972378
408.892847	16155.362715	29.977396
409.401844	16178.573456	29.982413
409.591048	16202.443898	29.987431
410.247629	16210.625790	29.992448
409.649335	16235.848261	29.997466
410.322028	16256.604607	30.002484
410.772742	16286.220480	30.007501
411.289811	16309.802814	30.012519
411.760167	16331.004693	30.017536
412.287233	16368.463843	30.022554
412.648423	16395.807173	30.027572
413.107099	16419.370362	30.032589
413.415721	16440.398711	30.037607
414.023488	16467.574023	30.042624
414.161817	16490.963225	30.047642
414.848013	16507.036841	30.052660
415.261859	16536.892604	30.057677
415.368792	16555.988084	30.062695
416.127425	16579.378145	30.067712
416.448185	16604.217091	30.072730
417.215606	16630.189500	30.077748
417.525225	16647.522456	30.082765
417.940484	16671.563375	30.087783
418.643504	16682.309234	30.092800
418.692588	16710.147251	30.097818
419.021338	16723.946044	30.102836
419.321632	16746.646896	30.107853
419.992300	16765.948026	30.112871
420.354950	16798.547509	30.117888
420.589068	16823.280284	30.122906
421.123850	16840.641317	30.127924
421.545716	16862.201976	30.132941
421.483822	16887.789791	30.137959
422.362289	16901.771083	30.142976
422.727209	16920.409584	30.147994
423.046062	16936.440026	30.153012
423.238627	16959.619154	30.158029
423.520339	16980.270121	30.163047
424.387451	16996.615874	30.168064
424.570814	17027.054934	30.173082
425.256242	17051.597284	30.178100
425.764755	17076.723290	30.183117
425.767176	17091.359950	30.188135
426.676731	17116.726415	30.193152
426.988884	17136.096708	30.198170
427.471306	17157.038604	30.203188
428.198144	17168.877041	30.208205
428.156619	17186.521332	30.213223
428.771909	17211.820305	30.218240
429.043634	17231.241247	30.223258
429.368473	17259.971813	30.228276
430.234967	17280.822097	30.233293
430.224888	17311.670940	30.238311
430.952487	17326.510052	30.243328
431.329753	17352.642468	30.248346
431.614134	17370.336953	30.253364
431.762138	17397.983583	30.258381
432.304858	17420.110286	30.263399
433.114281	17444.734794	30.268416
433.391697	17472.291769	30.273434
434.073883	17495.666492	30.278452
434.266353	17504.695509	30.283469
434.631385	17530.229936	30.288487
435.763915	17562.037323	30.293504
436.156155	17583.107519	30.298522
436.479705	17599.437851	30.303540
436.919289	17605.996029	30.308557
437.357143	17621.803087	30.313575
438.074495	17635.968087	30.318592
438.248327	17660.844044	30.323610
438.297539	17673.433305	30.328628
438.839176	17703.551982	30.333645
439.439896	17720.331757	30.338663
439.873980	17738.116844	30.343680
439.848323	17768.823555	30.348698
440.318456	17793.615366	30.353716
441.234653	17816.770620	30.358733
441.416269	17844.949604	30.363751
442.000295	17863.835823	30.368768
442.464251	17888.774025	30.373786
442.727055	17920.073854	30.378804
443.167544	17937.712820	30.383821
443.684882	17962.863867	30.388839
444.059622	17986.382104	30.393856
444.539908	18011.469526	30.398874
445.084081	18041.695729	30.403892
445.535791	18054.696005	30.408909
445.982854	18078.493631	30.413927
446.469233	18096.763622	30.418944
446.983484	18133.893380	30.423962
447.043191	18143.935341	30.428980
447.971845	18174.613249	30.433997
447.987048	18195.844250	30.439015
448.547843	18222.644024	30.444032
448.856385	18247.164803	30.449050
449.211403	18273.061880	30.454068
449.882397	18294.493513	30.459085
450.276435	18306.024679	30.464103
450.665037	18337.646627	30.469120
451.209160	18366.079149	30.474138
451.445310	18380.181082	30.479156
451.955609	18404.019744	30.484173
452.320490	18428.639326	30.489191
452.597286	18438.843283	30.494208
452.987697	18470.717869	30.499226
453.678618	18505.704258	30.504244
454.293761	18516.670236	30.509261
454.473250	18540.769363	30.514279
454.690441	18569.000685	30.519296
455.270283	18594.193303	30.524314
455.907241	18624.570142	30.529332
456.346331	18646.783976	30.534349
456.606100	18676.474489	30.539367
457.389644	18705.470188	30.544384
457.618475	18731.867788	30.549402
458.186263	18753.316095	30.554420
458.642474	18784.176371	30.559437
459.286331	18809.782530	30.564455
459.624963	18828.183755	30.569472
460.692850	18860.085537	30.574490
460.701754	18884.698278	30.579508
461.759642	18912.596249	30.584525
461.862079	18924.659927	30.589543
461.946424	18948.894500	30.594560
462.876004	18970.576998	30.599578
463.370597	18990.299638	30.604596
464.239825	19010.064703	30.609613
464.270612	19041.939694	30.614631
464.532831	19057.105747	30.619648
464.700561	19078.585486	30.624666
465.449742	19112.698302	30.629684
466.218552	19129.212894	30.634701
466.676556	19158.241307	30.639719
467.046906	19176.909562	30.644736
467.197205	19202.170250	30.649754
467.545695	19231.114838	30.654772
468.349705	19248.856006	30.659789
468.489896	19282.969739	30.664807
469.110142	19309.553211	30.669824
469.566966	19340.742804	30.674842
469.910012	19362.359662	30.679860
470.389430	19396.603679	30.684877
470.886534	19426.352929	30.689895
471.419320	19459.994812	30.694912
471.799461	19475.610249	30.699930
472.246735	19508.330552	30.704948
473.137248	19534.063299	30.709965
473.663233	19567.384215	30.714983
473.878115	19592.989099	30.720000
474.665206	19613.746935	30.725018
474.708983	19638.942737	30.730036
475.441689	19653.125768	30.735053
475.661448	19692.566476	30.740071
476.252013	19716.381538	30.745088
476.926268	19748.422251	30.750106
477.371219	19778.736196	30.755124
477.847748	19797.356824	30.760141
478.341805	19831.523494	30.765159
478.476209	19850.425211	30.770176
479.165245	19869.644431	30.775194
479.384125	19905.920346	30.780212
479.778706	19923.991620	30.785229
480.211365	19966.040499	30.790247
480.848345	19990.322485	30.795264
481.335388	20027.384297	30.800282
481.665995	20057.198495	30.805300
482.318891	20077.535575	30.810317
483.019156	20114.204019	30.815335
483.525233	20137.438922	30.820352
484.033299	20154.766044	30.825370
484.226257	20185.221179	30.830388
484.613973	20203.748696	30.835405
485.248527	20232.270870	30.840423
485.781793	20257.314981	30.845440
486.238006	20279.730177	30.850458
486.608112	20313.114689	30.855476
487.119256	20323.017563	30.860493
487.568235	20361.836120	30.865511
487.920845	20388.835759	30.870528
488.353475	20411.254800	30.875546
488.887229	20442.844788	30.880564
489.257345	20475.363972	30.885581
489.859876	20509.426380	30.890599
490.348061	20536.746175	30.895616
491.261367	20561.876470	30.900634
491.282532	20602.929692	30.905652
491.886543	20628.468661	30.910669
492.332025	20672.589459	30.915687
492.967879	20696.632401	30.920704
493.774065	20717.527426	30.925722
493.783376	20741.763333	30.930740
494.280128	20770.623793	30.935757
495.206773	20807.068526	30.940775
495.829319	20837.804898	30.945792
496.431043	20860.229560	30.950810
496.828776	20890.293565	30.955828
497.386600	20905.958135	30.960845
497.705188	20939.926759	30.965863
497.989226	20969.661179	30.970880
498.699546	20992.125848	30.975898
498.976157	21026.638264	30.980916
500.070927	21051.532257	30.985933
500.097975	21082.968857	30.990951
500.647266	21107.784079	30.995968
501.475568	21129.971368	31.000986
501.536008	21164.315692	31.006004
502.435414	21190.978050	31.011021
502.943837	21217.771187	31.016039
503.308832	21241.933044	31.021056
504.031720	21261.818095	31.026074
504.069886	21309.618319	31.031092
504.491201	21333.082745	31.036109
504.983065	21357.622942	31.041127
505.505161	21391.396187	31.046144
505.956121	21411.759963	31.051162
506.659897	21456.808806	31.056180
507.314667	21482.574724	31.061197
507.789510	21522.301400	31.066215
508.220077	21548.077246	31.071232
509.214090	21574.087126	31.076250
509.652544	21600.392571	31.081268
510.010110	21619.279990	31.086285
510.815013	21651.890986	31.091303
510.998376	21682.507907	31.096320
511.584337	21704.386277	31.101338
512.137830	21733.087614	31.106356
512.611075	21768.101298	31.111373
513.343737	21788.452935	31.116391
513.562664	21813.567220	31.121408
514.165042	21835.651682	31.126426
514.697753	21860.470450	31.131444
515.093717	21891.364013	31.136461
515.588329	21921.186943	31.141479
515.744837	21944.402911	31.146496
516.792639	21973.140913	31.151514
517.121025	22006.667525	31.156532
517.718538	22025.422971	31.161549
518.273150	22050.636631	31.166567
517.963780	22067.587972	31.171584
518.779121	22093.974058	31.176602
519.329304	22130.410701	31.181620
519.548438	22153.623424	31.186637
520.412295	22187.003286	31.191655
520.447605	22212.860864	31.196672
521.069037	22251.352830	31.201690
521.912197	22282.176961	31.206708
522.400437	22311.268491	31.211725
522.868357	22339.826141	31.216743
523.348198	22375.642365	31.221760
524.244863	22400.272111	31.226778
524.629027	22428.425960	31.231796
524.588652	22457.676326	31.236813
525.689273	22495.183790	31.241831
525.899221	22528.849896	31.246848
526.695798	22557.015161	31.251866
527.481230	22587.103174	31.256884
527.894483	22625.938104	31.261901
528.252003	22656.996857	31.266919
528.549456	22687.230960	31.271936
529.156710	22713.814760	31.276954
529.666263	22753.506877	31.281972
530.772337	22784.454907	31.286989
531.250808	22812.114285	31.292007
531.532488	22842.591219	31.297024
532.094763	22869.289695	31.302042
532.644465	22900.761063	31.307060
533.614687	22935.572592	31.312077
534.023397	22961.859231	31.317095
534.502323	23000.204356	31.322112
535.111090	23028.090072	31.327130
535.653213	23053.932557	31.332148
536.235578	23097.740333	31.337165
536.647051	23115.293724	31.342183
536.941405	23148.966618	31.347200
537.702694	23172.304150	31.352218
538.276645	23210.647437	31.357236
538.642903	23241.857395	31.362253
539.253428	23276.334073	31.367271
539.412463	23310.407585	31.372288
540.287452	23344.438531	31.377306
540.656808	23376.539222	31.382324
541.187869	23409.954312	31.387341
541.816818	23440.200832	31.392359
541.952361	23475.365212	31.397376
542.927337	23506.341223	31.402394
543.453757	23544.332400	31.407412
544.024498	23581.406733	31.412429
544.555188	23613.653158	31.417447
545.280459	23651.177364	31.422464
545.834602	23676.848155	31.427482
546.470918	23712.124099	31.432500
547.106030	23741.662350	31.437517
547.654350	23772.124222	31.442535
548.044348	23800.076882	31.447552
548.667130	23815.032143	31.452570
549.072350	23855.014531	31.457588
549.931940	23887.115095	31.462605
550.434394	23908.301211	31.467623
550.935709	23938.631674	31.472640
551.606414	23966.294146	31.477658
552.246826	23992.988214	31.482676
552.803003	24024.283401	31.487693
553.298705	24040.541577	31.492711
553.996947	24077.710613	31.497728
554.394591	24087.393024	31.502746
554.610460	24110.355764	31.507764
555.244825	24125.998265	31.512781
556.048635	24162.038703	31.517799
556.622240	24189.388081	31.522816
556.816333	24217.940761	31.527834
557.255362	24236.672567	31.532852
557.600844	24265.751399	31.537869
558.305870	24296.031541	31.542887
558.590400	24328.614692	31.547904
559.539729	24357.858183	31.552922
559.998835	24393.074613	31.557940
560.242533	24426.030850	31.562957
561.465305	24450.239216	31.567975
561.681809	24485.677072	31.572992
562.227917	24515.717016	31.578010
562.662416	24539.669777	31.583028
563.096530	24580.483273	31.588045
563.791333	24611.302659	31.593063
564.337938	24645.507333	31.598080
564.804711	24675.926479	31.603098
566.233062	24713.974529	31.608116
566.340544	24750.813927	31.613133
567.155576	24770.296257	31.618151
567.491521	24809.476168	31.623168
568.212464	24834.168056	31.628186
568.691843	24856.123472	31.633204
569.407884	24896.634350	31.638221
570.272585	24932.426493	31.643239
570.742159	24949.548980	31.648256
570.711367	24978.713058	31.653274
571.838068	25016.075842	31.658292
572.070696	25048.251190	31.663309
572.992782	25074.624519	31.668327
573.485176	25110.475291	31.673344
573.836068	25138.018842	31.678362
574.539091	25172.212556	31.683380
574.934599	25203.199804	31.688397
575.538409	25226.242099	31.693415
575.709761	25265.139008	31.698432
576.553215	25294.356213	31.703450
577.672009	25333.231261	31.708468
577.655675	25365.224915	31.713485
578.457677	25396.704942	31.718503
579.228660	25434.023100	31.723520
579.484595	25467.655355	31.728538
580.496300	25501.927683	31.733556
580.598856	25531.261272	31.738573
581.568988	25564.598556	31.743591
581.951723	25607.217035	31.748608
582.513896	25641.926562	31.753626
583.372146	25666.926608	31.758644
583.630365	25696.431975	31.763661
584.210098	25738.937721	31.768679
584.822504	25773.595368	31.773696
585.612505	25804.249998	31.778714
586.095798	25843.996604	31.783732
586.390784	25877.636066	31.788749
587.203532	25895.849533	31.793767
587.627016	25936.585288	31.798784
588.481053	25974.561362	31.803802
589.513290	26003.263391	31.808820
590.009251	26047.299715	31.813837
590.683938	26064.700712	31.818855
591.150807	26093.769499	31.823872
591.705171	26122.913106	31.828890
592.638988	26144.893559	31.833908
593.016218	26179.045210	31.838925
593.489778	26189.165476	31.843943
593.507641	26220.346157	31.848960
594.385079	26246.114971	31.853978
594.943718	26276.168225	31.858996
595.300848	26293.461153	31.864013
595.945087	26329.100708	31.869031
596.319789	26357.166769	31.874048
597.105193	26395.824322	31.879066
597.614180	26424.362416	31.884084
597.822418	26466.978440	31.889101
598.566751	26495.966429	31.894119
599.254292	26539.423965	31.899136
599.462291	26567.933559	31.904154
600.509715	26611.650897	31.909172
600.919023	26655.910686	31.914189
601.754026	26679.512539	31.919207
602.309384	26719.173737	31.924224
602.805439	26758.585170	31.929242
603.506756	26789.539601	31.934260
603.943787	26840.159970	31.939277
604.443981	26873.016835	31.944295
605.376953	26916.120726	31.949312
606.030262	26952.998742	31.954330
606.769638	26986.387161	31.959348
607.096598	27036.601796	31.964365
608.267724	27074.587162	31.969383
608.600776	27097.604480	31.974400
609.139758	27137.446032	31.979418
609.969855	27165.783191	31.984436
610.385801	27218.266001	31.989453
611.123529	27237.819719	31.994471
611.782601	27277.370960	31.999488
612.431626	27312.562747	32.004506
613.146780	27345.955552	32.009524
613.479511	27390.228935	32.014541
614.265644	27418.560693	32.019559
614.882186	27464.666970	32.024576
615.500550	27498.549221	32.029594
616.147641	27537.205333	32.034612
616.737765	27585.092083	32.039629
617.211656	27614.408454	32.044647
618.219915	27644.816798	32.049664
618.742981	27689.509782	32.054682
619.348904	27717.832258	32.059700
619.729988	27770.132334	32.064717
620.673055	27787.189398	32.069735
621.025271	27822.561286	32.074752
621.581865	27870.593012	32.079770
622.406399	27910.593617	32.084788
622.916728	27946.023125	32.089805
623.800441	27981.830341	32.094823
624.640866	28018.390238	32.099840
624.850455	28050.643492	32.104858
625.838244	28085.593943	32.109876
626.337643	28127.883416	32.114893
626.834450	28152.184664	32.119911
627.281815	28187.396908	32.124928
628.040209	28218.964010	32.129946
628.856485	28260.515172	32.134964
629.686797	28300.180639	32.139981
630.163322	28327.298005	32.144999
630.623569	28351.782198	32.150016
631.217733	28395.542763	32.155034
632.269006	28431.912362	32.160052
632.876936	28473.471305	32.165069
633.413600	28493.626596	32.170087
634.154658	28525.152642	32.175104
634.239768	28557.040621	32.180122
634.846286	28580.408678	32.185140
635.935301	28611.286205	32.190157
636.623078	28637.378526	32.195175
637.598017	28663.387982	32.200192
637.726651	28683.765384	32.205210
638.263214	28705.437908	32.210228
638.674235	28739.146107	32.215245
639.462926	28766.859897	32.220263
639.941120	28806.139032	32.225280
640.146905	28837.452308	32.230298
640.935304	28867.909557	32.235316
641.520767	28925.705068	32.240333
641.814750	28964.318052	32.245351
642.744694	28999.253846	32.250368
643.535437	29048.648604	32.255386
644.202446	29071.268195	32.260404
644.726956	29111.501451	32.265421
645.340565	29159.381894	32.270439
646.213522	29188.151310	32.275456
646.983389	29239.414498	32.280474
647.409517	29272.558636	32.285492
648.387541	29306.672010	32.290509
648.392214	29347.511789	32.295527
649.481816	29394.110910	32.300544
650.325678	29441.191100	32.305562
650.837617	29470.978259	32.310580
651.666545	29509.312536	32.315597
652.132182	29549.732862	32.320615
653.168700	29576.353309	32.325632
653.263749	29637.742181	32.330650
654.113159	29662.173317	32.335668
654.410095	29702.645649	32.340685
655.634202	29745.128381	32.345703
656.455958	29781.536326	32.350720
657.030668	29827.028683	32.355738
657.765406	29858.071039	32.360756
658.484223	29895.209606	32.365773
658.668028	29936.186849	32.370791
659.636477	29973.254856	32.375808
660.188955	30012.581556	32.380826
661.320250	30053.619248	32.385844
661.885821	30098.102230	32.390861
662.530481	30122.622872	32.395879
663.022102	30159.203293	32.400896
663.957811	30198.268048	32.405914
664.445188	30230.038730	32.410932
665.009446	30274.591833	32.415949
665.651855	30305.352220	32.420967
666.533764	30348.597785	32.425984
667.109050	30393.857412	32.431002
667.516092	30431.355521	32.436020
668.284479	30473.734131	32.441037
669.467129	30510.453489	32.446055
669.981855	30542.498512	32.451072
670.361093	30583.250468	32.456090
671.063995	30618.401576	32.461108
671.612308	30661.832792	32.466125
671.935857	30701.076549	32.471143
673.287009	30733.939099	32.476160
673.560699	30783.621286	32.481178
674.295014	30833.237775	32.486196
675.142894	30862.632974	32.491213
675.470265	30907.123394	32.496231
676.253394	30933.816892	32.501248
676.830354	30983.085412	32.506266
678.041939	31021.710264	32.511284
678.295815	31054.802063	32.516301
678.896578	31091.676802	32.521319
680.018201	31122.660474	32.526336
680.599961	31159.348660	32.531354
681.359782	31182.474414	32.536372
681.843447	31209.739863	32.541389
682.073027	31243.784015	32.546407
683.039848	31275.759372	32.551424
683.742482	31314.976533	32.556442
684.165552	31347.536568	32.561460
684.739828	31391.919824	32.566477
685.256651	31440.029335	32.571495
685.803661	31471.982237	32.576512
686.696874	31525.001869	32.581530
687.471421	31557.361791	32.586548
688.360454	31604.591566	32.591565
688.458459	31651.098211	32.596583
689.604551	31684.342088	32.601600
690.362094	31739.570852	32.606618
691.065956	31770.804253	32.611636
691.768792	31812.253920	32.616653
692.477045	31860.043620	32.621671
693.482978	31911.352335	32.626688
693.937630	31952.057238	32.631706
694.783061	31989.527442	32.636724
695.434580	32025.024044	32.641741
695.933865	32071.348668	32.646759
696.998371	32115.877963	32.651776
697.457158	32159.920595	32.656794
697.921129	32206.478640	32.661812
698.993562	32239.899314	32.666829
699.117210	32287.079811	32.671847
700.150487	32330.994904	32.676864
700.812644	32384.748330	32.681882
701.351086	32426.629573	32.686900
702.570909	32479.998778	32.691917
703.474734	32520.969516	32.696935
704.101909	32562.280796	32.701952
704.608691	32597.522870	32.706970
705.510546	32637.729178	32.711988
706.502765	32686.980957	32.717005
706.854914	32724.959637	32.722023
707.701483	32766.281217	32.727040
708.685899	32805.400160	32.732058
709.360098	32840.711258	32.737076
710.103726	32879.280090	32.742093
710.568290	32923.854489	32.747111
711.167136	32952.747945	32.752128
712.030367	33005.434645	32.757146
712.712473	33047.281989	32.762164
713.432847	33084.729492	32.767181
713.986055	33127.634025	32.772199
715.303322	33158.874601	32.777216
715.911829	33190.801542	32.782234
716.802638	33224.441907	32.787252
717.664401	33262.512456	32.792269
718.421961	33298.184285	32.797287
718.999670	33334.624048	32.802304
719.641182	33376.130682	32.807322
720.377079	33410.920975	32.812340
721.087167	33441.087435	32.817357
721.529340	33478.547598	32.822375
722.586225	33510.695637	32.827392
722.902922	33544.072374	32.832410
723.728467	33590.229146	32.837428
724.415753	33620.943159	32.842445
725.285060	33660.739256	32.847463
725.702477	33696.205814	32.852480
726.636930	33745.696739	32.857498
727.350177	33776.033892	32.862516
727.850334	33808.332797	32.867533
728.520484	33848.015023	32.872551
729.065948	33879.017166	32.877568
729.525436	33915.375291	32.882586
729.804731	33954.878674	32.887604
730.785706	34002.396632	32.892621
731.140055	34047.660861	32.897639
731.932032	34095.758684	32.902656
732.845129	34137.786997	32.907674
733.656280	34180.185420	32.912692
734.134148	34224.033404	32.917709
735.143910	34270.700239	32.922727
736.018154	34314.890983	32.927744
736.996805	34367.120447	32.932762
737.467791	34416.160756	32.937780
738.150669	34459.654672	32.942797
738.654553	34515.474229	32.947815
739.474280	34555.368302	32.952832
740.453607	34606.283143	32.957850
741.423555	34649.340490	32.962868
742.461379	34686.766428	32.967885
742.740691	34744.739858	32.972903
743.613322	34783.209792	32.977920
744.254329	34829.328632	32.982938
744.929744	34888.226771	32.987956
746.156348	34925.155686	32.992973
746.346344	34983.567382	32.997991
747.279886	35023.918725	33.003008
748.343142	35067.657820	33.008026
748.745929	35114.023239	33.013044
749.612732	35168.497832	33.018061
750.065652	35218.522869	33.023079
751.065819	35264.795067	33.028096
752.097574	35304.587800	33.033114
752.893554	35361.173173	33.038132
753.928985	35400.073984	33.043149
754.495077	35444.075078	33.048167
755.453665	35482.083897	33.053184
756.082751	35542.249372	33.058202
756.919878	35576.268637	33.063220
758.093332	35623.456602	33.068237
758.630641	35664.067229	33.073255
759.297532	35713.920821	33.078272
760.064564	35746.010178	33.083290
760.818306	35796.526924	33.088308
761.926669	35824.497249	33.093325
762.491962	35871.003271	33.098343
762.818350	35920.347920	33.103360
764.107555	35958.135097	33.108378
763.947399	36003.996247	33.113396
765.337198	36046.320444	33.118413
766.097480	36094.105299	33.123431
767.127646	36130.365219	33.128448
768.113557	36183.856331	33.133466
768.315842	36214.302297	33.138484
769.402339	36260.322871	33.143501
770.091216	36298.489206	33.148519
770.898708	36336.927902	33.153536
771.582944	36387.393705	33.158554
772.444348	36421.524342	33.163572
773.105799	36469.900929	33.168589
773.994216	36517.445357	33.173607
774.554879	36555.676494	33.178624
775.544331	36585.841641	33.183642
776.044091	36642.811946	33.188660
777.279938	36673.678454	33.193677
777.981083	36715.283479	33.198695
778.664203	36746.559137	33.203712
779.341225	36786.599900	33.208730
779.836682	36824.278956	33.213748
780.704600	36859.629676	33.218765
781.206387	36902.695357	33.223783
781.805648	36942.369189	33.228800
782.851453	36987.891839	33.233818
783.645554	37030.456720	33.238836
784.511680	37069.855034	33.243853
785.209582	37112.416172	33.248871
785.874680	37144.997858	33.253888
786.878270	37196.825687	33.258906
787.326952	37240.045802	33.263924
788.183057	37267.305043	33.268941
788.987833	37323.356760	33.273959
789.618525	37369.368901	33.278976
790.413749	37413.610091	33.283994
791.049055	37469.302995	33.289012
791.572659	37507.876785	33.294029
792.437159	37562.193453	33.299047
793.602461	37617.531835	33.304064
794.450939	37670.839519	33.309082
794.742906	37723.855067	33.314100
795.923831	37767.303052	33.319117
797.035550	37829.340739	33.324135
797.532301	37872.257391	33.329152
798.565847	37912.832529	33.334170
799.471187	37974.877660	33.339188
800.223097	38019.063645	33.344205
801.442545	38077.025382	33.349223
801.942652	38114.111550	33.354240
802.696969	38159.087909	33.359258
803.739461	38208.458492	33.364276
804.591067	38256.461533	33.369293
805.577049	38303.754349	33.374311
806.225717	38346.572273	33.379328
807.029133	38387.026250	33.384346
807.795715	38433.284989	33.389364
808.849626	38480.491671	33.394381
809.549944	38535.152699	33.399399
810.053814	38580.219747	33.404416
811.095258	38632.626909	33.409434
811.816161	38680.069568	33.414452
812.292598	38728.897598	33.419469
813.653412	38775.765970	33.424487
814.201925	38830.799333	33.429504
815.492224	38866.226347	33.434522
815.997656	38922.379699	33.439540
816.523244	38968.721593	33.444557
817.578772	39017.516509	33.449575
818.389418	39057.780895	33.454592
819.434061	39106.887593	33.459610
820.165140	39156.808710	33.464628
821.100723	39204.111394	33.469645
821.872570	39249.833518	33.474663
822.544189	39297.980894	33.479680
823.676537	39336.253941	33.484698
824.250603	39386.636535	33.489716
825.343512	39436.362507	33.494733
826.003465	39477.365894	33.499751
826.701675	39531.644001	33.504768
827.656579	39570.868571	33.509786
828.672081	39611.342225	33.514804
829.572798	39663.160483	33.519821
830.214466	39702.529204	33.524839
831.054250	39755.508222	33.529856
831.887910	39789.382946	33.534874
832.743677	39837.047343	33.539892
833.600553	39879.494193	33.544909
834.228468	39922.337460	33.549927
834.877369	39958.872260	33.554944
835.456907	39986.779061	33.559962
836.095062	40044.811810	33.564980
837.122591	40084.089179	33.569997
837.888153	40135.208761	33.575015
838.647509	40176.836657	33.580032
839.501984	40219.841087	33.585050
840.298215	40272.796566	33.590068
841.186560	40327.129105	33.595085
841.915178	40376.553790	33.600103
842.288766	40428.880151	33.605120
843.591114	40467.653500	33.610138
844.098992	40530.236204	33.615156
845.403842	40579.065165	33.620173
846.017924	40634.187698	33.625191
847.059997	40693.461759	33.630208
848.209546	40737.148318	33.635226
848.817706	40792.531481	33.640244
849.858811	40840.023591	33.645261
850.742637	40883.290364	33.650279
851.753924	40944.467281	33.655296
852.730999	40989.009865	33.660314
853.182959	41041.458236	33.665332
854.549702	41095.091646	33.670349
855.241918	41141.374131	33.675367
855.917542	41192.921374	33.680384
856.843499	41240.489308	33.685402
857.804455	41296.267551	33.690420
858.770937	41342.292476	33.695437
859.566972	41397.951337	33.700455
860.248545	41445.791997	33.705472
861.272746	41492.415369	33.710490
861.673217	41542.185011	33.715508
862.807398	41600.884214	33.720525
863.974930	41651.330906	33.725543
864.510340	41705.798037	33.730560
865.538643	41756.292071	33.735578
866.723762	41808.551577	33.740596
867.263463	41863.043725	33.745613
868.436302	41920.118583	33.750631
869.201835	41975.416847	33.755648
870.422199	42010.081996	33.760666
870.928912	42061.822177	33.765684
871.593156	42119.483181	33.770701
873.361851	42168.274688	33.775719
873.926165	42213.112092	33.780736
874.553907	42259.577805	33.785754
876.193129	42303.532363	33.790772
876.406103	42352.801908	33.795789
877.647588	42396.452087	33.800807
878.417897	42438.405146	33.805824
879.321030	42481.564530	33.810842
880.138600	42525.262369	33.815860
881.098611	42579.728427	33.820877
881.993818	42615.988749	33.825895
882.351693	42659.512162	33.830912
883.665087	42705.523577	33.835930
884.477442	42766.135846	33.840948
885.301336	42815.279136	33.845965
886.183958	42864.716944	33.850983
886.969539	42912.291506	33.856000
887.911144	42961.954324	33.861018
888.802229	43016.406953	33.866036
889.583386	43065.974952	33.871053
890.509129	43113.009338	33.876071
891.027083	43162.144380	33.881088
892.262659	43213.931263	33.886106
892.958773	43256.561640	33.891124
893.441814	43301.192600	33.896141
894.693751	43342.205410	33.901159
895.624366	43380.833400	33.906176
896.351636	43423.920962	33.911194
897.138537	43471.945614	33.916212
897.984392	43512.946425	33.921229
898.657624	43557.978239	33.926247
899.645352	43620.798211	33.931264
900.440364	43668.961176	33.936282
901.715296	43725.101230	33.941300
902.351547	43777.938402	33.946317
903.141888	43829.448550	33.951335
904.340208	43883.703397	33.956352
905.012282	43938.401324	33.961370
905.903970	43994.387006	33.966388
906.615784	44050.843774	33.971405
907.674731	44104.108917	33.976423
908.260665	44169.947332	33.981440
909.554795	44228.622158	33.986458
910.229799	44283.516565	33.991476
910.900660	44339.822341	33.996493
912.346254	44406.766645	34.001511
913.254902	44466.293147	34.006528
913.788494	44524.676682	34.011546
915.016603	44582.666969	34.016564
915.582605	44645.865826	34.021581
917.125013	44700.625440	34.026599
918.199039	44767.685941	34.031616
919.324604	44818.500675	34.036634
920.272138	44881.982043	34.041652
921.018194	44935.823198	34.046669
922.632853	44983.702527	34.051687
923.086548	45040.758877	34.056704
924.006967	45088.019681	34.061722
925.144669	45142.135271	34.066740
926.364198	45186.483896	34.071757
927.583619	45234.931711	34.076775
928.504965	45276.942399	34.081792
929.565229	45321.796989	34.086810
930.506959	45371.199492	34.091828
931.437988	45419.231081	34.096845
932.488477	45454.440626	34.101863
933.303402	45497.436241	34.106880
933.861316	45539.099476	34.111898
935.007589	45589.514196	34.116916
935.670693	45634.001443	34.121933
936.420386	45678.108319	34.126951
937.696378	45736.903820	34.131968
938.284749	45788.171776	34.136986
939.586881	45828.668920	34.142004
940.301868	45888.058732	34.147021
941.334196	45935.183610	34.152039
941.982993	45982.539441	34.157056
943.297485	46043.929688	34.162074
944.074470	46088.532849	34.167092
944.701025	46140.845745	34.172109
945.611640	46187.718193	34.177127
946.839727	46247.876302	34.182144
947.593445	46296.487898	34.187162
948.562072	46358.040701	34.192180
949.156401	46412.933983	34.197197
950.535631	46458.430448	34.202215
951.630954	46521.962907	34.207232
952.496067	46568.343510	34.212250
953.120374	46617.899677	34.217268
953.705796	46673.010075	34.222285
954.890522	46729.292003	34.227303
956.358111	46773.971849	34.232320
956.789884	46832.478548	34.237338
957.645091	46861.318771	34.242356
958.417830	46917.539153	34.247373
959.657739	46967.543753	34.252391
960.438256	47016.823287	34.257408
961.136765	47069.348489	34.262426
961.965883	47125.041806	34.267444
963.435104	47191.067095	34.272461
964.443677	47241.671565	34.277479
965.478156	47291.633133	34.282496
966.264309	47346.454364	34.287514
966.954758	47401.815800	34.292532
967.767063	47459.372521	34.297549
968.893001	47515.178483	34.302567
970.237920	47566.382633	34.307584
970.913615	47632.362645	34.312602
972.110420	47681.034373	34.317620
973.196699	47746.564517	34.322637
974.375537	47793.366670	34.327655
975.374457	47846.194591	34.332672
976.332764	47903.305705	34.337690
977.785424	47958.390993	34.342708
978.463038	48000.811865	34.347725
979.761333	48064.139734	34.352743
980.553695	48111.819180	34.357760
981.103241	48170.494360	34.362778
982.271306	48222.600751	34.367796
983.199042	48281.160062	34.372813
984.325070	48327.509745	34.377831
985.452760	48384.734732	34.382848
985.855688	48446.464035	34.387866
987.084357	48502.964925	34.392884
988.223747	48573.797206	34.397901
989.208203	48623.022991	34.402919
990.489574	48682.938817	34.407936
991.425020	48739.486205	34.412954
992.414248	48797.689245	34.417972
993.107303	48864.366051	34.422989
994.239407	48912.867072	34.428007
995.684872	48976.161781	34.433024
996.104991	49035.371919	34.438042
997.298876	49088.906108	34.443060
998.113258	49139.557864	34.448077
999.266969	49190.049045	34.453095
1000.523211	49255.639168	34.458112
1001.566086	49318.864998	34.463130
1002.710235	49365.302530	34.468148
1003.543735	49426.353351	34.473165
1004.373128	49483.583510	34.478183
1005.348032	49540.898588	34.483200
1006.719352	49598.284607	34.488218
1007.768523	49653.715558	34.493236
1008.694185	49717.530268	34.498253
1009.564312	49761.708482	34.503271
1010.422212	49815.296977	34.508288
1011.570376	49881.759963	34.513306
1012.868238	49930.920512	34.518324
1014.037484	49990.509332	34.523341
1015.041765	50033.888837	34.528359
1015.785458	50082.446825	34.533376
1016.522170	50152.284087	34.538394
1017.629114	50196.337480	34.543412
1018.793118	50253.567785	34.548429
1019.830420	50320.397390	34.553447
1020.646408	50369.748215	34.558464
1021.469718	50425.962999	34.563482
1022.687543	50483.103195	34.568500
1023.634286	50524.683054	34.573517
1024.999980	50576.377905	34.578535
1025.880448	50615.500684	34.583552
1026.650669	50669.142859	34.588570
1027.852986	50704.469663	34.593588
1028.945057	50754.746157	34.598605
1029.951686	50793.583741	34.603623
1030.207928	50842.263942	34.608640
1031.083181	50903.476655	34.613658
1032.475180	50947.391945	34.618676
1033.566208	51007.976382	34.623693
1034.377028	51064.770467	34.628711
1035.854654	51115.088619	34.633728
1036.576797	51187.987419	34.638746
1038.152611	51234.626895	34.643764
1039.406935	51282.626578	34.648781
1039.954537	51342.094764	34.653799
1041.251453	51386.215600	34.658816
1041.863721	51453.551626	34.663834
1043.373709	51502.479839	34.668852
1044.172336	51563.529126	34.673869
1045.049188	51611.348146	34.678887
1046.219395	51671.554928	34.683904
1047.397313	51732.266862	34.688922
1048.644210	51794.379202	34.693940
1049.545533	51856.090228	34.698957
1050.617068	51915.427230	34.703975
1051.931085	51961.185333	34.708992
1053.022031	52029.036548	34.714010
1053.972553	52079.268480	34.719028
1054.928077	52137.997777	34.724045
1055.810853	52201.591938	34.729063
1057.052697	52263.598753	34.734080
1058.196496	52316.983765	34.739098
1059.485432	52377.306668	34.744116
1060.816525	52435.054066	34.749133
1061.566957	52492.854553	34.754151
1062.869655	52538.172623	34.759168
1063.561030	52594.533550	34.764186
1064.991996	52657.752049	34.769204
1065.762816	52719.973037	34.774221
1067.029957	52775.383673	34.779239
1068.323141	52828.189619	34.784256
1069.146265	52882.176655	34.789274
1070.283257	52941.145334	34.794292
1071.050228	52992.179971	34.799309
1072.469496	53056.110105	34.804327
1073.123317	53108.073929	34.809344
1074.355749	53176.222725	34.814362
1075.204098	53241.748802	34.819380
1076.673636	53297.249218	34.824397
1077.675025	53357.385539	34.829415
1078.976761	53417.316791	34.834432
1080.003534	53471.444158	34.839450
1081.242867	53522.007330	34.844468
1082.355880	53578.747575	34.849485
1083.218004	53632.711251	34.854503
1084.625121	53685.849340	34.859520
1085.294870	53746.475219	34.864538
1086.754823	53805.382854	34.869556
1087.752956	53856.648962	34.874573
1088.424478	53916.332112	34.879591
1089.680861	53961.293161	34.884608
1090.949378	54033.621706	34.889626
1092.190891	54079.534536	34.894644
1092.833452	54142.108442	34.899661
1094.014483	54196.301923	34.904679
1095.469946	54249.693177	34.909696
1096.130150	54300.234787	34.914714
1097.178376	54343.900229	34.919732
1097.846729	54389.340185	34.924749
1098.877265	54437.862349	34.929767
1100.251479	54497.664773	34.934784
1101.015303	54554.803772	34.939802
1102.114571	54602.695340	34.944820
1103.543764	54659.274781	34.949837
1104.222804	54716.509713	34.954855
1105.727990	54771.273945	34.959872
1105.966886	54841.525927	34.964890
1107.280470	54906.104153	34.969908
1108.480149	54955.872909	34.974925
1109.450741	55028.029652	34.979943
1110.793580	55088.351088	34.984960
1111.969340	55150.293610	34.989978
1113.372474	55207.941628	34.994996
1114.680037	55267.022332	35.000013
1115.745804	55332.165784	35.005031
1116.629575	55393.901516	35.010048
1117.704999	55455.670689	35.015066
1118.829861	55523.982347	35.020084
1120.417497	55589.608044	35.025101
1121.476367	55653.120683	35.030119
1122.749510	55704.138903	35.035136
1123.907970	55760.813994	35.040154
1125.148342	55821.045751	35.045172
1126.788903	55879.879660	35.050189
1127.646876	55936.950292	35.055207
1128.696719	55988.048383	35.060224
1129.955929	56048.954938	35.065242
1131.372528	56098.432657	35.070260
1132.457415	56150.044564	35.075277
1133.235531	56196.496054	35.080295
1134.856303	56254.169500	35.085312
1136.095026	56312.244653	35.090330
1137.037663	56372.176337	35.095348
1138.694645	56412.997266	35.100365
1139.266560	56469.164638	35.105383
1140.404644	56518.598231	35.110400
1141.525239	56583.660581	35.115418
1142.761245	56635.635941	35.120436
1143.869613	56682.580956	35.125453
1144.575406	56742.101298	35.130471
1145.782415	56812.954335	35.135488
1147.282008	56869.217909	35.140506
1147.989023	56926.320869	35.145524
1149.621742	56974.975457	35.150541
1150.593399	57043.264824	35.155559
1151.620032	57096.710641	35.160576
1153.324060	57156.423826	35.165594
1154.230395	57218.129103	35.170612
1155.484350	57261.906944	35.175629
1156.533954	57327.121668	35.180647
1157.716590	57379.739906	35.185664
1159.047650	57437.176760	35.190682
1159.934503	57494.866840	35.195700
1160.918709	57545.048162	35.200717
1162.231271	57611.551602	35.205735
1163.726720	57681.089895	35.210752
1164.518517	57725.390305	35.215770
1166.070539	57781.654145	35.220788
1167.062212	57835.037460	35.225805
1168.086756	57897.137371	35.230823
1169.430341	57956.776067	35.235840
1170.219995	58016.596569	35.240858
1171.342894	58073.953610	35.245876
1172.455967	58118.267738	35.250893
1173.488701	58182.120304	35.255911
1174.734095	58217.875721	35.260928
1175.617266	58268.441468	35.265946
1176.756060	58320.321772	35.270964
1178.141424	58365.808954	35.275981
1179.012635	58433.440756	35.280999
1180.194789	58470.079897	35.286016
1180.913455	58538.121963	35.291034
1182.069021	58600.848768	35.296052
1183.184373	58656.651349	35.301069
1184.526744	58729.254740	35.306087
1185.861848	58791.447580	35.311104
1187.319822	58859.691279	35.316122
1188.470102	58926.609849	35.321140
1189.870926	58987.824498	35.326157
1190.732682	59046.066549	35.331175
1192.454139	59109.478279	35.336192
1193.313080	59163.904362	35.341210
1194.533849	59228.072045	35.346228
1196.120652	59284.542822	35.351245
1196.921979	59356.960626	35.356263
1197.959234	59421.499347	35.361280
1199.097249	59486.389582	35.366298
1200.377612	59550.662721	35.371316
1201.937050	59614.613836	35.376333
1202.847968	59677.508320	35.381351
1204.163001	59749.536716	35.386368
1205.759095	59806.519957	35.391386
1207.317800	59882.783141	35.396404
1208.541530	59931.305182	35.401421
1209.789711	59999.376048	35.406439
1210.634296	60052.540419	35.411456
1212.127865	60118.832521	35.416474
1213.176440	60186.719946	35.421492
1214.638389	60248.713096	35.426509
1215.801740	60308.752927	35.431527
1216.807240	60366.412280	35.436544
1218.143155	60427.855931	35.441562
1219.147756	60485.186553	35.446580
1220.652037	60541.806096	35.451597
1221.855472	60609.132412	35.456615
1222.999212	60675.765637	35.461632
1224.469125	60737.043500	35.466650
1225.648098	60808.140500	35.471668
1226.908910	60862.361872	35.476685
1228.350680	60930.050546	35.481703
1229.417632	60990.202090	35.486720
1230.848907	61052.657840	35.491738
1231.661563	61108.304537	35.496756
1232.941537	61168.619400	35.501773
1233.659923	61228.148781	35.506791
1235.656876	61303.531212	35.511808
1236.960715	61363.089538	35.516826
1237.759646	61428.588730	35.521844
1239.364577	61489.537162	35.526861
1240.701903	61557.940232	35.531879
1242.048036	61605.300678	35.536896
1243.373213	61656.709471	35.541914
1244.708118	61720.536662	35.546932
1246.089919	61769.373104	35.551949
1247.034824	61830.147178	35.556967
1248.451788	61899.956697	35.561984
1249.610370	61942.814712	35.567002
1251.223401	62005.409017	35.572020
1252.503067	62055.401461	35.577037
1253.296318	62114.307225	35.582055
1254.371750	62169.396099	35.587072
1255.833965	62225.874187	35.592090
1257.023654	62273.336373	35.597108
1258.168923	62308.910908	35.602125
1258.980020	62364.028935	35.607143
1260.158195	62418.197040	35.612160
1261.232587	62463.386051	35.617178
1262.251772	62526.865940	35.622196
1263.410970	62572.098847	35.627213
1264.649812	62640.178492	35.632231
1265.884911	62694.661142	35.637248
1267.189715	62771.207269	35.642266
1268.131881	62832.066529	35.647284
1269.535787	62891.271035	35.652301
1271.184042	62965.978802	35.657319
1272.062931	63038.901748	35.662336
1273.716203	63102.758636	35.667354
1274.787163	63171.321817	35.672372
1276.408264	63232.398633	35.677389
1277.718789	63306.685502	35.682407
1279.054821	63363.128962	35.687424
1280.052710	63430.634425	35.692442
1281.621130	63498.987692	35.697460
1282.905887	63571.057331	35.702477
1284.317802	63642.442552	35.707495
1285.664550	63699.935989	35.712512
1287.155028	63755.039378	35.717530
1288.622696	63831.240406	35.722548
1289.714101	63883.190545	35.727565
1291.217442	63951.814802	35.732583
1292.160765	64017.051324	35.737600
1293.873231	64081.705465	35.742618
1294.682100	64155.788508	35.747636
1296.439990	64203.703554	35.752653
1297.805549	64272.831404	35.757671
1298.734097	64337.539284	35.762688
1300.203740	64398.338787	35.767706
1301.662724	64477.461670	35.772724
1303.356229	64548.336912	35.777741
1304.733687	64606.682301	35.782759
1306.220558	64661.965522	35.787776
1307.630431	64720.977181	35.792794
1308.701223	64784.220492	35.797812
1309.988170	64833.318386	35.802829
1311.499448	64885.515097	35.807847
1312.624264	64944.540251	35.812864
1314.366382	65007.520759	35.817882
1315.104418	65076.160271	35.822900
1316.600105	65133.779303	35.827917
1317.732590	65190.872865	35.832935
1318.908766	65248.023028	35.837952
1320.552712	65311.937673	35.842970
1321.757419	65380.106101	35.847988
1322.936458	65430.716197	35.853005
1324.079628	65497.090205	35.858023
1325.391857	65571.193587	35.863040
1327.063222	65632.059467	35.868058
1328.603217	65703.316544	35.873076
1329.833049	65757.509129	35.878093
1331.196839	65824.609207	35.883111
1332.452361	65884.306203	35.888128
1333.337778	65933.101887	35.893146
1334.831755	66019.397442	35.898164
1336.236192	66083.231240	35.903181
1337.969266	66149.641245	35.908199
1338.676946	66205.955207	35.913216
1340.205936	66266.237096	35.918234
1341.483218	66329.046750	35.923252
1342.557246	66390.495477	35.928269
1344.139995	66458.322722	35.933287
1345.216067	66514.851951	35.938304
1346.603893	66570.705695	35.943322
1347.986187	66633.765584	35.948340
1349.178465	66678.886765	35.953357
1350.368944	66734.942712	35.958375
1351.335542	66795.123951	35.963392
1352.630328	66855.804797	35.968410
1354.212067	66911.166739	35.973428
1355.563599	66976.847200	35.978445
1356.849187	67042.626794	35.983463
1358.047979	67113.162467	35.988480
1359.448052	67173.131120	35.993498
1361.047059	67247.479428	35.998516
1362.365888	67324.385453	36.003533
1363.587838	67387.440651	36.008551
1364.815703	67461.512104	36.013568
1366.375212	67521.899833	36.018586
1367.617044	67605.118738	36.023604
1369.010753	67674.074193	36.028621
1370.545302	67745.679762	36.033639
1371.705642	67826.949318	36.038656
1373.124596	67886.397490	36.043674
1375.179476	67983.154230	36.048692
1376.308694	68047.890823	36.053709
1378.292779	68113.557503	36.058727
1379.454474	68185.748205	36.063744
1381.010687	68250.804711	36.068762
1382.327751	68316.861256	36.073780
1383.836640	68384.420252	36.078797
1385.344379	68455.164536	36.083815
1386.626461	68514.129039	36.088832
1388.112283	68584.807460	36.093850
1389.291387	68659.345903	36.098868
1390.853595	68726.352906	36.103885
1392.239557	68793.039415	36.108903
1393.543502	68874.283472	36.113920
1395.157993	68934.589940	36.118938
1396.700166	69006.432115	36.123956
1397.677285	69072.309527	36.128973
1399.143616	69139.484582	36.133991
1400.408060	69215.378992	36.139008
1402.188889	69290.375957	36.144026
1403.250925	69357.519882	36.149044
1405.026759	69425.324767	36.154061
1406.606180	69501.240366	36.159079
1407.921425	69559.644842	36.164096
1409.374310	69629.305473	36.169114
1410.613033	69696.023694	36.174132
1411.915805	69773.395469	36.179149
1413.606233	69836.377006	36.184167
1414.945074	69921.361223	36.189184
1416.533364	69981.851539	36.194202
1418.287199	70044.342407	36.199220
1419.271752	70115.388429	36.204237
1420.378094	70169.508368	36.209255
1422.002855	70238.580158	36.214272
1423.260681	70315.510990	36.219290
1424.861367	70386.246010	36.224308
1426.511126	70454.085986	36.229325
1428.276321	70511.700286	36.234343
1429.497864	70594.488732	36.239360
1430.867405	70651.038107	36.244378
1432.457706	70718.102860	36.249396
1433.509568	70784.808796	36.254413
1435.197108	70840.143637	36.259431
1436.811678	70906.571831	36.264448
1438.505433	70965.046868	36.269466
1440.033607	71020.318382	36.274484
1441.258145	71073.129868	36.279501
1442.734660	71118.429648	36.284519
1443.980778	71161.295884	36.289536
1444.975672	71206.316581	36.294554
1446.062749	71255.730383	36.299572
1447.097889	71312.067566	36.304589
1448.994390	71372.031596	36.309607
1450.020735	71442.542752	36.314624
1451.298646	71504.655673	36.319642
1452.648459	71574.242651	36.324660
1454.185054	71637.885888	36.329677
1456.098597	71705.700494	36.334695
1456.824036	71779.071353	36.339712
1458.832237	71855.002687	36.344730
1460.333170	71921.539903	36.349748
1461.634418	71990.552977	36.354765
1463.519861	72062.134543	36.359783
1464.941626	72128.912655	36.364800
1466.261662	72205.231357	36.369818
1468.090814	72280.875308	36.374836
1469.179787	72352.177031	36.379853
1470.720754	72411.211169	36.384871
1472.129632	72505.590732	36.389888
1473.474631	72576.903651	36.394906
1475.180288	72647.539687	36.399924
1476.777708	72735.557676	36.404941
1477.949838	72796.664272	36.409959
1479.376540	72871.017663	36.414976
1480.819348	72949.814477	36.419994
1482.196682	73033.726153	36.425012
1484.098209	73118.354003	36.430029
1485.841283	73193.216082	36.435047
1487.503022	73281.643797	36.440064
1488.685698	73351.527611	36.445082
1490.563763	73422.430050	36.450100
1492.434217	73499.970946	36.455117
1493.744483	73563.008278	36.460135
1495.274616	73654.003739	36.465152
1496.664826	73714.090347	36.470170
1497.946368	73784.200482	36.475188
1499.491251	73869.899855	36.480205
1501.587602	73936.348945	36.485223
1502.754094	74006.870332	36.490240
1503.968433	74079.563046	36.495258
1505.820393	74157.704076	36.500276
1507.374100	74233.637378	36.505293
1509.154352	74299.642856	36.510311
1510.500680	74373.975031	36.515328
1512.177609	74443.645016	36.520346
1513.689024	74509.857759	36.525364
1514.865368	74589.271132	36.530381
1516.703259	74653.507794	36.535399
1518.434233	74725.551398	36.540416
1519.581922	74802.841875	36.545434
1521.322972	74865.992195	36.550452
1523.189921	74942.929828	36.555469
1524.612870	75005.180250	36.560487
1526.047811	75078.385824	36.565504
1527.448558	75141.108713	36.570522
1529.045574	75217.848712	36.575540
1530.195843	75287.945334	36.580557
1531.761353	75345.829446	36.585575
1533.148497	75424.629611	36.590592
1534.620441	75500.693304	36.595610
1536.356421	75572.953741	36.600628
1537.909458	75646.826404	36.605645
1539.860501	75714.113356	36.610663
1541.155447	75775.650898	36.615680
1542.415434	75839.005474	36.620698
1543.728553	75893.117417	36.625716
1545.048147	75955.424217	36.630733
1546.689673	76013.272532	36.635751
1547.858853	76074.640431	36.640768
1548.879948	76148.496386	36.645786
1550.639708	76219.146070	36.650804
1551.732580	76296.500079	36.655821
1553.881198	76370.750202	36.660839
1555.001163	76444.832173	36.665856
1557.209203	76523.190370	36.670874
1558.644270	76584.112445	36.675892
1560.193088	76663.321616	36.680909
1561.790925	76741.965968	36.685927
1563.185809	76818.210108	36.690944
1564.594551	76901.685590	36.695962
1566.628197	76979.350338	36.700980
1567.817155	77056.590130	36.705997
1569.522236	77142.502866	36.711015
1570.854357	77222.786350	36.716032
1572.302300	77306.446955	36.721050
1574.344266	77391.344983	36.726068
1575.848718	77479.760442	36.731085
1577.586612	77559.259328	36.736103
1579.341239	77639.389232	36.741120
1580.607635	77730.946451	36.746138
1582.607991	77800.916515	36.751156
1584.638839	77901.792460	36.756173
1586.266789	77974.937641	36.761191
1587.711643	78039.991296	36.766208
1589.284735	78126.738556	36.771226
1591.011493	78202.871278	36.776244
1592.694147	78287.460943	36.781261
1594.591855	78364.162773	36.786279
1596.461429	78434.205599	36.791296
1597.900675	78500.705431	36.796314
1599.476113	78580.764786	36.801332
1600.743752	78661.898704	36.806349
1602.523061	78735.769671	36.811367
1604.254794	78806.924523	36.816384
1605.680365	78886.653501	36.821402
1607.597513	78958.362485	36.826420
1609.322998	79040.376013	36.831437
1610.552191	79117.881356	36.836455
1612.164754	79190.740801	36.841472
1613.849515	79277.512216	36.846490
1615.360998	79352.465601	36.851508
1616.916010	79433.113397	36.856525
1618.830269	79512.539656	36.861543
1620.403766	79602.851481	36.866560
1621.773658	79673.406410	36.871578
1623.767754	79751.110538	36.876596
1625.659095	79837.686680	36.881613
1626.972214	79911.874470	36.886631
1628.670023	79982.720931	36.891648
1630.181109	80056.105302	36.896666
1631.970357	80136.933862	36.901684
1633.279377	80214.657824	36.906701
1635.214025	80288.990062	36.911719
1636.744798	80369.251623	36.916736
1638.265152	80454.418103	36.921754
1640.272016	80522.012212	36.926772
1641.877275	80595.725342	36.931789
1643.363287	80676.754962	36.936807
1645.048707	80749.366375	36.941824
1646.251586	80832.923989	36.946842
1648.011399	80911.656255	36.951860
1649.629327	80977.411898	36.956877
1650.857114	81049.601599	36.961895
1652.683483	81115.223587	36.966912
1653.729620	81184.515365	36.971930
1655.722984	81250.086195	36.976948
1657.067807	81317.342403	36.981965
1658.710885	81398.083465	36.986983
1660.207496	81470.244846	36.992000
1661.523224	81558.652188	36.997018
1662.938620	81639.277538	37.002036
1665.381530	81720.933284	37.007053
1666.409767	81801.138232	37.012071
1668.227195	81889.240033	37.017088
1669.541684	81981.525931	37.022106
1671.742517	82069.923056	37.027124
1673.469190	82162.322418	37.032141
1674.673619	82249.165573	37.037159
1676.566030	82327.665665	37.042176
1678.131659	82430.746785	37.047194
1680.159514	82521.440378	37.052212
1681.918465	82611.986292	37.057229
1683.982703	82702.902839	37.062247
1685.967271	82790.550502	37.067264
1687.571721	82881.286172	37.072282
1689.108446	82961.237442	37.077300
1690.913796	83051.042607	37.082317
1692.687697	83134.745746	37.087335
1694.574068	83226.528071	37.092352
1696.390553	83325.657955	37.097370
1698.205636	83394.404008	37.102388
1700.009421	83471.970838	37.107405
1701.540426	83565.710485	37.112423
1703.297457	83655.727854	37.117440
1704.782249	83745.293949	37.122458
1706.670145	83824.331067	37.127476
1708.817987	83918.989012	37.132493
1710.359750	84001.704683	37.137511
1712.166495	84081.768893	37.142528
1713.709213	84175.572064	37.147546
1715.631400	84256.961831	37.152564
1717.339583	84342.655494	37.157581
1718.928540	84434.247497	37.162599
1720.955138	84511.452830	37.167616
1722.663533	84598.971881	37.172634
1724.496276	84679.908012	37.177652
1725.945185	84756.976331	37.182669
1727.895976	84850.869903	37.187687
1729.573748	84927.687450	37.192704
1731.406596	85021.485994	37.197722
1733.279027	85101.314686	37.202740
1735.296504	85187.988856	37.207757
1736.617880	85269.551549	37.212775
1738.290071	85348.183123	37.217792
1740.226895	85432.272977	37.222810
1742.099048	85514.548479	37.227828
1743.731977	85600.587129	37.232845
1745.579380	85677.620891	37.237863
1747.119642	85754.411474	37.242880
1748.578442	85836.195024	37.247898
1750.517916	85919.500230	37.252916
1752.472057	86008.898547	37.257933
1753.882502	86096.405410	37.262951
1756.102539	86181.910391	37.267968
1757.254419	86266.961860	37.272986
1759.290107	86340.140981	37.278004
1761.260485	86427.016316	37.283021
1762.627139	86518.066803	37.288039
1764.263893	86598.950277	37.293056
1766.111206	86686.897433	37.298074
1767.966281	86753.744437	37.303092
1769.667779	86817.447575	37.308109
1771.153974	86890.954848	37.313127
1772.459256	86962.450382	37.318144
1774.010543	87035.301545	37.323162
1775.508098	87119.388998	37.328180
1777.443994	87208.210928	37.333197
1779.102283	87300.219333	37.338215
1781.048611	87379.903334	37.343232
1782.465801	87474.180369	37.348250
1784.341220	87562.797407	37.353268
1785.739293	87655.646019	37.358285
1787.667836	87760.666334	37.363303
1789.700899	87850.932358	37.368320
1791.388934	87954.014067	37.373338
1792.933439	88045.472342	37.378356
1794.546062	88142.306175	37.383373
1796.026229	88262.339667	37.388391
1798.461564	88357.626101	37.393408
1800.534490	88466.377510	37.398426
1802.437059	88574.420947	37.403444
1804.684833	88679.774769	37.408461
1806.312144	88781.094646	37.413479
1807.936958	88873.620127	37.418496
1809.965115	88978.857304	37.423514
1811.735504	89082.487679	37.428532
1813.752665	89167.919061	37.433549
1815.603950	89276.898230	37.438567
1817.485386	89380.436227	37.443584
1819.416904	89475.805105	37.448602
1821.345877	89580.616369	37.453620
1823.623973	89674.968471	37.458637
1825.019581	89780.206086	37.463655
1827.276998	89873.687583	37.468672
1828.905855	89966.241178	37.473690
1830.636652	90066.928234	37.478708
1832.862556	90162.684144	37.483725
1834.977211	90278.063970	37.488743
1836.888923	90365.454364	37.493760
1838.726526	90461.208626	37.498778
1840.563338	90548.649297	37.503796
1842.388061	90634.393820	37.508813
1844.302259	90743.292450	37.513831
1846.140632	90830.302786	37.518848
1848.062287	90924.359740	37.523866
1849.814931	91008.887237	37.528884
1851.311692	91096.129236	37.533901
1852.907880	91207.778882	37.538919
1854.867133	91298.016220	37.543936
1856.879927	91395.203565	37.548954
1858.528736	91507.492467	37.553972
1861.232748	91601.948750	37.558989
1862.824353	91694.855703	37.564007
1864.592771	91789.547701	37.569024
1866.492396	91887.857006	37.574042
1868.534739	91988.362319	37.579060
1870.464686	92064.537939	37.584077
1871.805866	92173.924305	37.589095
1873.842743	92267.333685	37.594112
1875.676772	92360.116017	37.599130
1877.765226	92476.116728	37.604148
1879.634428	92564.698883	37.609165
1881.373808	92670.691288	37.614183
1883.037820	92760.320097	37.619200
1884.850362	92863.424559	37.624218
1886.608717	92960.061017	37.629236
1888.532906	93057.166150	37.634253
1890.517274	93165.669582	37.639271
1892.391761	93245.215684	37.644288
1893.942646	93335.408903	37.649306
1895.600628	93420.464928	37.654324
1897.459241	93502.916760	37.659341
1898.716943	93595.640930	37.664359
1900.326801	93696.257572	37.669376
1902.566662	93807.968127	37.674394
1904.157096	93909.488443	37.679412
1906.330975	94003.806981	37.684429
1908.171888	94109.332163	37.689447
1909.848674	94217.912794	37.694464
1911.606066	94332.463970	37.699482
1913.787586	94446.214029	37.704500
1915.881956	94546.859033	37.709517
1917.452942	94670.643020	37.714535
1919.382226	94779.312865	37.719552
1921.358540	94895.897986	37.724570
1923.278528	95008.550230	37.729588
1925.551630	95124.696823	37.734605
1927.340182	95242.859062	37.739623
1929.307464	95353.908013	37.744640
1931.317043	95481.480040	37.749658
1933.063378	95596.924921	37.754676
1935.221961	95722.459150	37.759693
1937.311844	95839.435663	37.764711
1939.265593	95953.125470	37.769728
1941.298075	96083.041436	37.774746
1943.454399	96205.928657	37.779764
1945.680728	96324.064511	37.784781
1947.326939	96434.812608	37.789799
1949.487508	96557.117434	37.794816
1951.391782	96679.272694	37.799834
1953.067002	96803.378404	37.804852
1955.017803	96917.224279	37.809869
1957.037529	97043.596812	37.814887
1958.779225	97169.202059	37.819904
1961.067667	97289.169911	37.824922
1963.047759	97424.081503	37.829940
1965.105687	97544.200482	37.834957
1967.221026	97675.263624	37.839975
1969.183220	97798.567729	37.844992
1971.469931	97929.148740	37.850010
1973.035468	98053.048326	37.855028
1975.225024	98173.668842	37.860045
1977.491531	98302.454423	37.865063
1979.261002	98419.097646	37.870080
1981.060732	98542.658241	37.875098
1982.879201	98674.570604	37.880116
1985.550191	98791.302309	37.885133
1987.733430	98914.893073	37.890151
1989.580273	99034.683061	37.895168
1991.888568	99146.325844	37.900186
1993.876370	99264.269101	37.905204
1996.028032	99372.552327	37.910221
1997.663915	99504.788255	37.915239
1999.512841	99621.030417	37.920256
2001.302086	99728.331994	37.925274
2003.087471	99861.965877	37.930292
2005.007392	99981.507081	37.935309
2007.041638	100118.310526	37.940327
2009.009491	100244.906678	37.945344
2010.861512	100374.614830	37.950362
2012.629098	100513.769027	37.955380
2014.667304	100625.953629	37.960397
2017.068786	100765.275953	37.965415
2018.769567	100889.494920	37.970432
2020.808088	101021.052812	37.975450
2022.555630	101146.888233	37.980468
2024.852752	101273.424190	37.985485
2026.750687	101389.386100	37.990503
2028.221306	101499.583298	37.995520
2029.959477	101613.605876	38.000538
2032.084444	101735.428885	38.005556
2034.199138	101858.395008	38.010573
2035.710774	101992.549564	38.015591
2037.625751	102119.148583	38.020608
2039.773620	102253.242687	38.025626
2041.360126	102398.949995	38.030644
2043.592787	102545.495060	38.035661
2045.418027	102694.399367	38.040679
2047.328036	102830.688411	38.045696
2049.607933	102976.682811	38.050714
2051.048954	103132.584507	38.055732
2053.682279	103291.875829	38.060749
2055.756620	103440.681115	38.065767
2057.959218	103591.051877	38.070784
2060.162785	103734.779327	38.075802
2061.945361	103891.949760	38.080820
2064.178480	104049.709754	38.085837
2066.145463	104202.947601	38.090855
2068.400610	104369.048608	38.095872
2070.694555	104526.332196	38.100890
2072.401120	104681.831868	38.105908
2074.830580	104841.796450	38.110925
2076.841261	105010.297263	38.115943
2079.168488	105168.212622	38.120960
2081.159640	105323.987719	38.125978
2083.316338	105485.887305	38.130996
2085.412553	105652.514015	38.136013
2087.422037	105806.766888	38.141031
2089.361846	105978.504296	38.146048
2091.900144	106133.030947	38.151066
2093.877239	106308.530141	38.156084
2096.050682	106471.801250	38.161101
2098.358276	106630.956455	38.166119
2100.345720	106795.830555	38.171136
2102.559922	106966.350740	38.176154
2104.822088	107136.534578	38.181172
2106.577769	107297.719329	38.186189
2108.964064	107469.191476	38.191207
2111.128516	107620.511775	38.196224
2113.481180	107798.394491	38.201242
2115.747378	107962.926237	38.206260
2117.527475	108114.384921	38.211277
2119.845675	108293.036417	38.216295
2121.787651	108462.807704	38.221312
2124.113759	108622.717384	38.226330
2126.346283	108790.847021	38.231348
2128.312963	108955.874171	38.236365
2130.551626	109120.035276	38.241383
2132.343883	109286.790545	38.246400
2134.661357	109452.107544	38.251418
2136.656810	109626.339907	38.256436
2138.671297	109800.164354	38.261453
2140.879338	109966.566130	38.266471
2143.108386	110130.784198	38.271488
2145.417667	110301.927259	38.276506
2147.222966	110477.030563	38.281524
2149.436607	110651.880620	38.286541
2151.590195	110814.566514	38.291559
2153.199273	111004.718246	38.296576
2155.764306	111171.399564	38.301594
2157.983101	111343.918770	38.306612
2159.300307	111525.913779	38.311629
2162.288117	111695.651161	38.316647
2164.083820	111872.956825	38.321664
2166.374309	112032.874857	38.326682
2168.443635	112187.146590	38.331700
2170.365974	112338.334839	38.336717
2172.299108	112499.972235	38.341735
2174.212008	112656.274257	38.346752
2176.129737	112822.848942	38.351770
2177.968688	112995.651123	38.356788
2180.173784	113163.197013	38.361805
2182.120501	113340.676512	38.366823
2183.825013	113536.381683	38.371840
2186.581399	113713.419260	38.376858
2188.579806	113906.150734	38.381876
2190.640132	114095.753559	38.386893
2193.417781	114291.003179	38.391911
2194.919816	114489.624161	38.396928
2197.247126	114677.387246	38.401946
2199.582982	114883.147285	38.406964
2201.923195	115079.382724	38.411981
2203.714090	115270.923567	38.416999
2206.223463	115477.129055	38.422016
2208.438404	115674.490704	38.427034
2211.011208	115867.713344	38.432052
2213.443202	116074.441600	38.437069
2216.494928	116264.166824	38.442087
2218.768487	116446.607513	38.447104
2220.868673	116627.630275	38.452122
2223.219660	116818.393862	38.457140
2225.952056	117011.622833	38.462157
2228.404345	117192.402981	38.467175
2230.555293	117386.308308	38.472192
2232.970066	117573.450824	38.477210
2235.246565	117760.336851	38.482228
2237.155915	117950.046389	38.487245
2239.222409	118132.223238	38.492263
2241.721021	118319.318276	38.497280
2243.806610	118513.582083	38.502298
2246.131714	118712.096739	38.507316
2248.192744	118901.926828	38.512333
2250.700640	119091.446941	38.517351
2252.658743	119293.840082	38.522368
2255.047095	119481.148337	38.527386
2257.317458	119686.006256	38.532404
2259.358117	119889.556613	38.537421
2261.453604	120082.571034	38.542439
2263.661963	120288.279053	38.547456
2265.801242	120490.282269	38.552474
2267.946113	120704.514060	38.557492
2270.636286	120899.913101	38.562509
2272.788550	121113.308768	38.567527
2274.912386	121322.600024	38.572544
2277.085429	121532.176464	38.577562
2279.527121	121753.585529	38.582580
2281.618234	121953.180942	38.587597
2284.066802	122162.248278	38.592615
2286.211262	122379.863652	38.597632
2288.247275	122594.173545	38.602650
2290.307002	122820.380113	38.607668
2292.801511	123030.814913	38.612685
2294.908608	123249.354283	38.617703
2297.169856	123477.689661	38.622720
2299.481087	123700.880685	38.627738
2302.037557	123914.849856	38.632756
2303.980050	124149.924506	38.637773
2306.222826	124368.245779	38.642791
2308.426275	124598.195041	38.647808
2310.693602	124827.234885	38.652826
2312.907816	125043.978481	38.657844
2314.706178	125274.553160	38.662861
2317.272418	125487.120930	38.667879
2319.171430	125699.540460	38.672896
2321.937852	125912.180622	38.677914
2324.402786	126118.081629	38.682932
2326.125961	126330.455821	38.687949
2328.634576	126549.939771	38.692967
2330.599817	126762.988792	38.697984
2332.564844	126984.729570	38.703002
2335.062720	127212.871290	38.708020
2337.076093	127443.183447	38.713037
2339.471710	127673.399019	38.718055
2341.708716	127915.325703	38.723072
2343.941898	128158.459689	38.728090
2346.357408	128392.774143	38.733108
2348.614499	128642.733056	38.738125
2351.095638	128876.621250	38.743143
2353.953774	129138.732629	38.748160
2356.606627	129374.309555	38.753178
2358.967389	129612.382237	38.758196
2360.846300	129863.650931	38.763213
2363.832179	130104.305719	38.768231
2365.984878	130359.569278	38.773248
2367.763950	130611.530451	38.778266
2370.366752	130863.605312	38.783284
2372.642412	131125.033336	38.788301
2374.533653	131385.672958	38.793319
2377.228917	131641.747415	38.798336
2379.625668	131911.370655	38.803354
2381.972107	132174.316546	38.808372
2383.991431	132457.769326	38.813389
2386.930379	132723.721862	38.818407
2389.705599	132997.720958	38.823424
2391.705870	133270.954764	38.828442
2394.090995	133539.942686	38.833460
2396.791510	133823.284984	38.838477
2399.539925	134085.367282	38.843495
2401.730129	134360.798673	38.848512
2403.999176	134637.919788	38.853530
2406.686102	134902.820824	38.858548
2408.884304	135177.139303	38.863565
2411.347933	135457.534275	38.868583
2413.962293	135739.607809	38.873600
2416.394331	136006.242894	38.878618
2418.636403	136278.771921	38.883636
2420.981705	136568.316174	38.888653
2423.582941	136847.454559	38.893671
2426.474347	137129.138002	38.898688
2428.740637	137401.961767	38.903706
2431.302980	137676.822008	38.908724
2433.751671	137960.813225	38.913741
2436.587118	138242.994411	38.918759
2438.787105	138522.218327	38.923776
2440.955289	138807.070743	38.928794
2443.596747	139078.183160	38.933812
2445.953558	139357.438256	38.938829
2448.522530	139626.420443	38.943847
2450.683802	139921.851971	38.948864
2453.060932	140211.743745	38.953882
2455.533582	140488.208058	38.958900
2457.713928	140779.428517	38.963917
2460.010747	141056.888115	38.968935
2462.641693	141346.074391	38.973952
2464.668837	141632.044443	38.978970
2467.106779	141920.185574	38.983988
2469.740930	142214.414936	38.989005
2472.373155	142505.638500	38.994023
2474.492949	142812.668705	38.999040
2476.832549	143100.248330	39.004058
2479.080779	143379.188216	39.009076
2481.299287	143650.925424	39.014093
2483.501747	143918.427568	39.019111
2486.131621	144200.866043	39.024128
2488.297362	144493.405326	39.029146
2490.810564	144764.163261	39.034164
2493.125155	145062.305105	39.039181
2495.703181	145362.070159	39.044199
2497.831204	145647.095557	39.049216
2500.318985	145954.214300	39.054234
2502.610269	146259.347530	39.059252
2504.665645	146563.339070	39.064269
2507.368715	146879.288963	39.069287
2510.008967	147187.533509	39.074304
2512.145538	147514.694577	39.079322
2515.024989	147828.972581	39.084340
2517.485055	148159.907579	39.089357
2519.505760	148486.775491	39.094375
2522.262921	148813.657143	39.099392
2524.353313	149154.607461	39.104410
2527.236845	149484.481704	39.109428
2529.416456	149831.654694	39.114445
2531.686160	150177.178386	39.119463
2534.470440	150522.953811	39.124480
2536.828941	150882.494274	39.129498
2539.739615	151246.837738	39.134516
2541.941969	151609.466526	39.139533
2544.525966	151957.516386	39.144551
2547.187244	152319.176771	39.149568
2549.624535	152682.626287	39.154586
2552.578501	153051.760390	39.159604
2554.919827	153403.639987	39.164621
2557.519715	153768.784754	39.169639
2560.728496	154142.405198	39.174656
2562.842841	154508.227262	39.179674
2565.877623	154871.254549	39.184692
2568.294013	155253.587531	39.189709
2570.789462	155620.854948	39.194727
2573.063909	155989.949176	39.199744
2575.836240	156366.889319	39.204762
2578.680161	156735.924522	39.209780
2581.726779	157112.179061	39.214797
2584.240912	157489.230173	39.219815
2586.733666	157864.039976	39.224832
2589.474103	158242.761526	39.229850
2592.490030	158610.537200	39.234868
2594.662561	158988.108080	39.239885
2597.311783	159360.541283	39.244903
2599.757019	159720.656023	39.249920
2602.665610	160113.607003	39.254938
2605.200331	160477.774661	39.259956
2607.679260	160850.446515	39.264973
2610.196963	161223.647715	39.269991
2613.043456	161592.026066	39.275008
2615.830979	161979.611861	39.280026
2618.328345	162350.359810	39.285044
2620.926533	162737.103742	39.290061
2623.390538	163117.497532	39.295079
2626.111981	163491.048131	39.300096
2628.565541	163881.198593	39.305114
2631.072758	164261.185928	39.310132
2633.602057	164653.423944	39.315149
2635.893199	165039.188231	39.320167
2638.567015	165432.931738	39.325184
2640.716694	165827.800619	39.330202
2643.273706	166234.225485	39.335220
2645.958985	166616.521612	39.340237
2648.392251	167017.434654	39.345255
2651.363117	167396.554274	39.350272
2653.468539	167775.328816	39.355290
2656.148386	168145.368880	39.360308
2658.152347	168533.838429	39.365325
2660.546966	168926.527901	39.370343
2663.235808	169316.926077	39.375360
2665.420996	169716.775700	39.380378
2667.852692	170125.667532	39.385396
2670.387176	170540.602207	39.390413
2672.642707	170952.535426	39.395431
2675.341284	171378.432390	39.400448
2677.662636	171812.314064	39.405466
2680.142939	172249.169993	39.410484
2682.784978	172692.110726	39.415501
2685.016540	173149.682605	39.420519
2687.188766	173608.053705	39.425536
2690.183676	174069.498676	39.430554
2692.917526	174523.342918	39.435572
2695.835052	174998.392263	39.440589
2698.523850	175459.258170	39.445607
2701.642197	175930.002230	39.450624
2704.375123	176404.237804	39.455642
2707.338167	176872.725785	39.460660
2710.491167	177349.034322	39.465677
2713.032199	177832.679416	39.470695
2715.947336	178292.319094	39.475712
2718.618753	178776.380819	39.480730
2721.504611	179247.052565	39.485748
2724.178138	179727.055563	39.490765
2726.452959	180203.186827	39.495783
2729.473007	180692.791928	39.500800
2731.763955	181182.767660	39.505818
2734.893055	181671.268783	39.510836
2737.682366	182153.399816	39.515853
2740.716087	182713.163611	39.520871
2743.761251	183211.108625	39.525888
2746.158914	183719.596348	39.530906
2748.852149	184199.060352	39.535924
2752.061529	184701.914609	39.540941
2754.736246	185198.632213	39.545959
2757.661679	185691.020549	39.550976
2759.876793	186185.909868	39.555994
2762.591605	186695.480473	39.561012
2765.478428	187200.276897	39.566029
2768.169736	187711.913399	39.571047
2771.359348	188210.723645	39.576064
2773.810711	188728.777779	39.581082
2776.908704	189224.508110	39.586100
2779.769326	189731.834815	39.591117
2782.383667	190246.873164	39.596135
2785.099986	190750.620052	39.601152
2787.916017	191271.905242	39.606170
2790.609074	191778.962173	39.611188
2793.486018	192292.241026	39.616205
2796.234407	192812.857548	39.621223
2799.225023	193321.068079	39.626240
2801.831249	193841.609446	39.631258
2804.467390	194354.451669	39.636276
2807.528530	194878.050334	39.641293
2810.052951	195399.321851	39.646311
2813.144844	195917.128208	39.651328
2816.249964	196427.669584	39.656346
2819.448910	196936.343804	39.661364
2822.159326	197445.172425	39.666381
2825.102123	197963.949364	39.671399
2827.797940	198470.904049	39.676416
2830.568641	198999.110143	39.681434
2833.015650	199497.953085	39.686452
2835.825081	199987.037301	39.691469
2838.143659	200475.615511	39.696487
2840.474981	200971.737645	39.701504
2843.336148	201472.122174	39.706522
2845.759109	201974.278652	39.711540
2848.763764	202482.899431	39.716557
2850.892627	202997.170974	39.721575
2853.884934	203511.562941	39.726592
2856.553450	204038.378067	39.731610
2858.823676	204572.115668	39.736628
2861.675725	205108.659635	39.741645
2864.013669	205666.776279	39.746663
2866.967450	206209.175270	39.751680
2869.498279	206773.945640	39.756698
2871.760857	207330.249362	39.761716
2875.129053	207898.092381	39.766733
2877.300117	208502.171163	39.771751
2880.665888	209071.592333	39.776768
2883.430944	209659.551555	39.781786
2885.807180	210269.241997	39.786804
2888.474693	210865.830867	39.791821
2891.071072	211475.438704	39.796839
2894.000774	212075.545535	39.801856
2897.027223	212706.198929	39.806874
2899.933811	213331.893165	39.811892
2902.913598	213948.431759	39.816909
2905.733283	214597.081360	39.821927
2908.934090	215224.028425	39.826944
2911.853213	215850.207578	39.831962
2914.442023	216490.386001	39.836980
2917.861818	217120.654840	39.841997
2921.345267	217780.001996	39.847015
2923.945312	218417.081812	39.852032
2927.239834	219060.379280	39.857050
2929.830972	219705.895901	39.862068
2933.136192	220352.317567	39.867085
2936.110277	221009.994691	39.872103
2939.180331	221648.604211	39.877120
2941.978935	222297.138715	39.882138
2944.744396	222965.163622	39.887156
2948.340713	223611.643196	39.892173
2950.746829	224264.024981	39.897191
2954.658903	224917.390746	39.902208
2957.809243	225565.362976	39.907226
2960.754565	226203.230997	39.912244
2964.034605	226852.503812	39.917261
2966.815186	227508.332600	39.922279
2969.813290	228149.468981	39.927296
2973.186440	228800.403183	39.932314
2975.730624	229447.376597	39.937332
2978.987464	230098.429787	39.942349
2981.419183	230761.221126	39.947367
2984.246856	231412.848410	39.952384
2987.469843	232060.704250	39.957402
2989.859848	232735.948043	39.962420
2992.877606	233394.986764	39.967437
2995.717736	234065.484118	39.972455
2998.434023	234737.117628	39.977472
3001.535043	235407.953208	39.982490
3004.323577	236085.517706	39.987508
3007.951183	236765.540936	39.992525
3010.591848	237441.144541	39.997543
3013.736475	238109.427949	40.002560
3017.081164	238782.429114	40.007578
3019.942416	239467.901255	40.012596
3023.224848	240132.754544	40.017613
3026.356474	240810.102831	40.022631
3028.867656	241467.274584	40.027648
3032.271070	242109.368008	40.032666
3034.688346	242763.426388	40.037684
3037.630008	243399.822010	40.042701
3040.608372	244054.982888	40.047719
3043.313640	244691.818189	40.052736
3046.610615	245351.878814	40.057754
3049.657922	246001.484999	40.062772
3052.678639	246662.676800	40.067789
3055.721802	247319.036303	40.072807
3058.744984	247992.873495	40.077824
3061.356231	248652.369421	40.082842
3064.277228	249332.695081	40.087860
3067.142724	250005.101204	40.092877
3070.133227	250700.372290	40.097895
3073.562092	251389.526142	40.102912
3076.791287	252082.848668	40.107930
3079.495664	252782.498917	40.112948
3082.142326	253476.896752	40.117965
3085.215993	254194.873244	40.122983
3088.341842	254902.423364	40.128000
3091.521554	255617.911994	40.133018
3094.734110	256340.808785	40.138036
3098.199002	257051.799895	40.143053
3101.118255	257775.039358	40.148071
3104.175968	258498.634003	40.153088
3107.116862	259223.969876	40.158106
3110.528640	259966.931757	40.163124
3113.592080	260682.866828	40.168141
3116.468643	261426.817471	40.173159
3119.497164	262177.165597	40.178176
3122.866597	262922.730975	40.183194
3126.036524	263674.646882	40.188212
3129.325193	264419.477885	40.193229
3132.566062	265173.124523	40.198247
3135.634477	265923.312911	40.203264
3138.765427	266683.239017	40.208282
3141.542353	267455.202718	40.213300
3144.767836	268208.777914	40.218317
3147.950598	268974.036942	40.223335
3150.684197	269746.903102	40.228352
3154.442126	270507.538664	40.233370
3157.498459	271292.201933	40.238388
3160.709121	272061.214805	40.243405
3163.704502	272844.578471	40.248423
3166.717316	273634.027475	40.253440
3169.755123	274418.792208	40.258458
3172.753543	275209.422218	40.263476
3176.103316	275998.034131	40.268493
3178.968473	276802.459477	40.273511
3182.422622	277598.124661	40.278528
3185.861742	278401.377254	40.283546
3188.656732	279202.157255	40.288564
3191.957056	280003.332254	40.293581
3195.217059	280804.428751	40.298599
3198.436702	281617.686627	40.303616
3202.261358	282410.271696	40.308634
3205.211181	283214.868958	40.313652
3208.258839	284022.108016	40.318669
3211.338468	284833.319384	40.323687
3214.730869	285645.919612	40.328704
3217.968639	286451.449750	40.333722
3221.103887	287271.738987	40.338740
3224.047950	288074.578331	40.343757
3227.087223	288901.844837	40.348775
3230.516677	289708.752128	40.353792
3233.771262	290537.741077	40.358810
3237.095913	291342.358601	40.363828
3240.118578	292148.510861	40.368845
3243.354163	292949.769710	40.373863
3246.395561	293729.974995	40.378880
3249.715031	294509.771124	40.383898
3252.754814	295305.595593	40.388916
3256.659199	296078.398991	40.393933
3259.279794	296854.566252	40.398951
3263.119094	297638.681846	40.403968
3266.660152	298418.542675	40.408986
3269.746108	299202.601831	40.414004
3272.945175	299994.476629	40.419021
3275.936582	300779.137294	40.424039
3278.757781	301583.411105	40.429056
3282.442410	302386.344675	40.434074
3285.385628	303196.388267	40.439092
3288.528514	304013.343512	40.444109
3291.839030	304835.209594	40.449127
3295.234800	305663.242834	40.454144
3298.531100	306478.129424	40.459162
3301.588299	307321.672309	40.464180
3304.678878	308157.707752	40.469197
3307.993959	309008.440948	40.474215
3310.973582	309855.252154	40.479232
3314.238648	310708.831418	40.484250
3317.439195	311572.405550	40.489268
3320.501991	312439.335630	40.494285
3323.993553	313309.126656	40.499303
3327.449842	314181.749339	40.504320
3331.080974	315059.733776	40.509338
3333.966204	315947.360140	40.514356
3337.481501	316832.840212	40.519373
3340.845419	317721.092460	40.524391
3343.818236	318624.385710	40.529408
3347.453587	319518.954063	40.534426
3350.981670	320412.454873	40.539444
3354.131985	321321.272045	40.544461
3358.280116	322214.688843	40.549479
3361.971253	323106.153511	40.554496
3365.722351	324002.258464	40.559514
3369.070589	324896.833787	40.564532
3372.262290	325797.478048	40.569549
3375.627076	326688.789049	40.574567
3379.164814	327594.540318	40.579584
3382.535219	328480.964505	40.584602
3386.219342	329397.890939	40.589620
3389.581708	330304.140148	40.594637
3393.467539	331193.847124	40.599655
3396.456101	332102.243539	40.604672
3400.190403	332999.441282	40.609690
3403.683489	333914.539377	40.614708
3407.012448	334814.293923	40.619725
3410.487289	335713.065316	40.624743
3413.271039	336625.265054	40.629760
3416.866845	337532.115270	40.634778
3420.206747	338448.773368	40.639796
3423.648341	339357.986036	40.644813
3426.942163	340274.807481	40.649831
3430.012014	341197.574932	40.654848
3433.616166	342112.778284	40.659866
3436.546067	343045.004044	40.664884
3439.793878	343985.574511	40.669901
3443.586206	344909.524999	40.674919
3446.785871	345849.164035	40.679936
3450.346125	346778.856220	40.684954
3453.800469	347732.501836	40.689972
3457.003724	348666.203644	40.694989
3460.660612	349610.203991	40.700007
3463.992433	350556.864835	40.705024
3467.508756	351476.055418	40.710029
3471.144455	352369.649331	40.715034
3474.014206	353213.900207	40.720039
3477.678117	354003.331955	40.725044
3480.919757	354755.091646	40.730048
3484.205895	355428.443122	40.735053
3486.912655	356064.077658	40.740058
3489.976710	356638.926615	40.745063
3492.574564	357153.020410	40.750068
3495.360069	357614.824456	40.755072
3498.075037	358027.507368	40.760077
3499.991839	358395.657679	40.765082
3501.979041	358704.223520	40.770087
3504.005552	358961.267543	40.775092
3505.716408	359183.669973	40.780096
3507.494183	359349.948701	40.785101
3508.920909	359506.090884	40.790106
3510.115431	359615.153515	40.795111
3511.457559	359680.406778	40.800116
3512.670181	359726.239534	40.805120
3514.029622	359729.839019	40.810125
3515.181555	359712.022731	40.815130
3515.733488	359673.029883	40.820135
3516.395680	359600.322555	40.825140
3517.063796	359518.389301	40.830144
3518.471066	359401.067260	40.835149
3518.898848	359269.082149	40.840154
3519.509983	359122.175739	40.845159
3520.237441	358964.348169	40.850164
3520.270228	358782.612767	40.855168
3521.047777	358581.343916	40.860173
3521.547101	358382.226572	40.865178
3521.710333	358159.576404	40.870183
3522.067532	357940.935127	40.875188
3522.279241	357695.528414	40.880192
3522.319747	357443.360842	40.885197
3522.736802	357197.536834	40.890202
3522.889818	356936.833608	40.895207
3523.048130	356664.665140	40.900212
3522.854363	356400.936382	40.905216
3523.279883	356119.851403	40.910221
3523.750720	355840.662982	40.915226
3523.435164	355544.667931	40.920231
3523.072267	355254.319886	40.925236
3523.356320	354966.358820	40.930240
3523.678775	354666.189073	40.935245
3523.077239	354371.269728	40.940250
3522.922474	354072.312688	40.945255
3523.118703	353778.432270	40.950260
3522.986314	353488.845255	40.955264
3522.785420	353175.653047	40.960269
3522.938495	352882.533616	40.965274
3522.385824	352578.058121	40.970279
3522.408001	352278.751515	40.975284
3522.681525	351980.419572	40.980288
3522.637396	351678.423327	40.985293
3522.433099	351380.770580	40.990298
3522.168208	351077.735604	40.995303
3522.361292	350773.558555	41.000308
3522.004119	350477.014441	41.005312
3521.707740	350181.093624	41.010317
3521.746392	349880.262416	41.015322
3521.315702	349593.712023	41.020327
3521.456198	349287.343130	41.025332
3520.985462	349009.309919	41.030336
3521.242329	348711.992839	41.035341
3521.153557	348425.963494	41.040346
3520.927050	348139.571876	41.045351
3520.550016	347841.735943	41.050356
3520.272889	347562.312911	41.055360
3520.161262	347281.844755	41.060365
3520.520921	346996.292278	41.065370
3520.096166	346719.707191	41.070375
3520.260165	346433.544928	41.075380
3519.652373	346156.424501	41.080384
3519.578045	345875.557391	41.085389
3519.883191	345598.645579	41.090394
3519.201297	345327.453675	41.095399
3519.421598	345050.016737	41.100404
3518.968927	344787.378067	41.105408
3518.616681	344513.306013	41.110413
3518.369105	344253.351597	41.115418
3518.360101	343995.468184	41.120423
3518.239707	343740.397018	41.125428
3517.848537	343480.459190	41.130432
3518.578467	343221.615406	41.135437
3517.792189	342961.938842	41.140442
3516.965981	342710.555433	41.145447
3517.278402	342465.348724	41.150452
3517.227194	342228.155571	41.155456
3516.882145	341986.836796	41.160461
3517.006014	341741.654466	41.165466
3516.566818	341505.330707	41.170471
3516.790296	341268.672908	41.175476
3516.615814	341028.388788	41.180480
3516.426594	340790.520929	41.185485
3516.439912	340563.935048	41.190490
3516.214532	340328.561624	41.195495
3515.975406	340093.621055	41.200500
3515.730715	339878.539085	41.205504
3515.804652	339638.079532	41.210509
3515.726384	339417.476265	41.215514
3515.576551	339186.380850	41.220519
3515.574412	338963.652310	41.225524
3515.230984	338754.020727	41.230528
3515.047998	338531.622921	41.235533
3514.975493	338317.826941	41.240538
3514.645331	338108.723530	41.245543
3514.662659	337891.579742	41.250548
3514.353742	337684.504907	41.255552
3514.349713	337470.794924	41.260557
3514.260785	337274.134965	41.265562
3514.505093	337069.131665	41.270567
3514.094633	336863.517533	41.275572
3513.810068	336663.604373	41.280576
3513.876913	336460.024060	41.285581
3513.750819	336251.284943	41.290586
3513.665992	336063.009907	41.295591
3513.716433	335873.034323	41.300596
3513.464970	335676.747218	41.305600
3512.956804	335487.619908	41.310605
3513.231411	335296.207596	41.315610
3512.808821	335113.117623	41.320615
3512.731163	334922.724846	41.325620
3512.555396	334738.271997	41.330624
3512.839873	334551.559149	41.335629
3512.616684	334379.904101	41.340634
3512.227071	334209.418721	41.345639
3512.649931	334020.011222	41.350644
3512.306109	333846.973821	41.355648
3511.793839	333675.665922	41.360653
3511.790469	333498.173891	41.365658
3511.900339	333327.250355	41.370663
3512.103646	333144.892159	41.375668
3511.617286	332976.756114	41.380672
3511.718666	332818.446272	41.385677
3511.783952	332646.789074	41.390682
3511.520768	332480.065615	41.395687
3511.145769	332311.782043	41.400692
3510.950386	332160.459129	41.405696
3511.045344	332003.647463	41.410701
3510.968626	331844.547538	41.415706
3510.345702	331684.209793	41.420711
3510.613337	331529.429312	41.425716
3510.421742	331388.861234	41.430720
3510.108699	331237.196987	41.435725
3510.156978	331089.952047	41.440730
3509.703706	330942.937561	41.445735
3510.260742	330790.652277	41.450740
3509.955222	330657.983961	41.455744
3509.932695	330499.607590	41.460749
3510.020151	330365.655979	41.465754
3509.770056	330237.352297	41.470759
3509.499647	330096.435747	41.475764
3509.149673	329962.780046	41.480768
3509.154287	329824.312123	41.485773
3509.449800	329687.960203	41.490778
3509.205859	329563.061621	41.495783
3509.346346	329429.530892	41.500788
3509.289927	329305.772188	41.505792
3509.033110	329166.478007	41.510797
3508.969723	329034.834584	41.515802
3508.361562	328915.688410	41.520807
3508.551243	328791.126542	41.525812
3508.685357	328675.577185	41.530816
3508.782369	328547.824144	41.535821
3508.427444	328424.948712	41.540826
3508.486489	328300.685512	41.545831
3508.374018	328177.313559	41.550836
3508.542954	328063.690101	41.555840
3508.199946	327941.421768	41.560845
3507.823158	327834.343744	41.565850
3507.995535	327723.440445	41.570855
3507.808986	327611.193953	41.575860
3508.181531	327499.699138	41.580864
3508.144457	327386.131387	41.585869
3508.275184	327281.719669	41.590874
3507.888346	327163.322150	41.595879
3507.962762	327053.704135	41.600884
3507.783280	326950.891689	41.605888
3507.556568	326836.054748	41.610893
3507.431967	326720.362097	41.615898
3507.122967	326626.090425	41.620903
3507.562445	326523.866914	41.625908
3507.350872	326418.031115	41.630912
3507.429167	326317.237149	41.635917
3507.234927	326206.412403	41.640922
3506.962028	326115.873162	41.645927
3507.071352	326004.517094	41.650932
3506.555437	325913.862770	41.655936
3506.614900	325809.712745	41.660941
3506.895697	325721.985929	41.665946
3506.911313	325629.594430	41.670951
3507.020468	325531.668129	41.675956
3506.762743	325446.568675	41.680960
3506.593980	325357.232468	41.685965
3506.597855	325268.250642	41.690970
3506.391620	325175.307725	41.695975
3506.599446	325079.908697	41.700980
3506.573196	324985.716189	41.705984
3506.187179	324898.854989	41.710989
3506.476374	324811.786290	41.715994
3505.995587	324727.686856	41.720999
3506.592875	324637.135468	41.726004
3506.053436	324557.750922	41.731008
3505.705362	324467.448711	41.736013
3506.181709	324380.502466	41.741018
3506.159015	324311.491820	41.746023
3506.223717	324218.682442	41.751028
3505.851828	324147.207705	41.756032
3505.813660	324065.505251	41.761037
3506.061905	323983.528909	41.766042
3505.740405	323913.394135	41.771047
3505.665111	323819.537322	41.776052
3505.072134	323742.499933	41.781056
3505.419880	323676.228572	41.786061
3505.438115	323614.384100	41.791066
3505.449819	323533.308766	41.796071
3505.546518	323462.039413	41.801076
3505.457265	323386.499823	41.806080
3505.195259	323309.969542	41.811085
3505.462540	323233.559885	41.816090
3505.064482	323170.787711	41.821095
3505.416445	323097.824283	41.826100
3505.095986	323027.357138	41.831104
3505.008110	322955.174522	41.836109
3504.827893	322883.515003	41.841114
3505.074655	322836.795453	41.846119
3504.999547	322760.896366	41.851124
3504.789155	322698.094141	41.856128
3504.843550	322638.990020	41.861133
3504.883741	322572.510591	41.866138
3504.707420	322507.896551	41.871143
3504.602097	322434.825381	41.876148
3504.417906	322378.098631	41.881152
3504.643126	322319.476145	41.886157
3504.474989	322262.059858	41.891162
3504.687749	322212.648325	41.896167
3504.306461	322150.380790	41.901172
3504.395888	322091.906415	41.906176
3504.284949	322037.050294	41.911181
3504.232043	321976.969864	41.916186
3504.198574	321926.019221	41.921191
3504.634520	321869.245712	41.926196
3504.443067	321810.458700	41.931200
3504.146817	321753.545108	41.936205
3504.213534	321708.200770	41.941210
3504.065161	321649.661199	41.946215
3504.416464	321595.469997	41.951220
3504.213721	321546.173524	41.956224
3504.113916	321492.612399	41.961229
3504.234523	321431.130299	41.966234
3503.796960	321376.680547	41.971239
3503.954119	321328.497801	41.976244
3503.945457	321282.045422	41.981248
3503.874130	321232.626276	41.986253
3504.111782	321184.049178	41.991258
3503.751627	321131.011666	41.996263
3503.944633	321081.830863	42.001268
3503.541442	321029.334199	42.006272
3503.761346	320987.450475	42.011277
3503.629485	320943.891755	42.016282
3503.712217	320900.553845	42.021287
3503.854213	320848.658616	42.026292
3503.951597	320806.564905	42.031296
3503.793234	320758.405402	42.036301
3503.997142	320710.112885	42.041306
3503.791235	320670.635956	42.046311
3504.235273	320612.511150	42.051316
3504.001696	320568.153847	42.056320
3503.621726	320512.854443	42.061325
3503.675471	320471.632208	42.066330
3503.301499	320425.286889	42.071335
3503.695575	320392.025208	42.076340
3503.527606	320336.895958	42.081344
3502.796234	320291.420475	42.086349
3503.304917	320248.880300	42.091354
3502.975241	320222.168177	42.096359
3503.268547	320184.469936	42.101364
3503.189178	320156.370271	42.106368
3502.933790	320122.472132	42.111373
3503.242926	320071.440263	42.116378
3503.523279	320044.810745	42.121383
3503.362687	320002.858340	42.126388
3503.512079	319965.843873	42.131392
3503.213869	319914.601478	42.136397
3503.377350	319876.465325	42.141402
3503.376873	319845.936221	42.146407
3503.312438	319793.206991	42.151412
3503.271516	319757.163420	42.156416
3503.108727	319717.856960	42.161421
3503.200394	319680.215243	42.166426
3503.284300	319646.747067	42.171431
3503.223071	319607.679041	42.176436
3503.255628	319564.322185	42.181440
3503.073034	319527.969836	42.186445
3503.429226	319493.670292	42.191450
3503.420882	319460.547131	42.196455
3503.331440	319427.283975	42.201460
3503.419854	319383.053198	42.206464
3503.211249	319348.104040	42.211469
3503.401683	319309.301696	42.216474
3503.125375	319267.493874	42.221479
3502.975351	319226.225980	42.226484
3502.977186	319190.200694	42.231488
3503.222008	319157.826408	42.236493
3503.256351	319120.498464	42.241498
3503.218906	319078.373259	42.246503
3503.304654	319037.729806	42.251508
3503.097942	319006.850728	42.256512
3502.953931	318972.756182	42.261517
3502.984305	318932.019521	42.266522
3502.693057	318893.037696	42.271527
3502.819714	318863.963639	42.276532
3502.903396	318840.544337	42.281536
3502.294352	318808.761235	42.286541
3502.583138	318776.608767	42.291546
3502.284092	318755.844312	42.296551
3502.377260	318712.578896	42.301556
3502.652767	318699.128141	42.306560
3502.510301	318671.546212	42.311565
3502.836989	318644.755938	42.316570
3502.562919	318617.677944	42.321575
3502.926926	318574.726234	42.326580
3502.622711	318543.353234	42.331584
3502.449259	318524.502615	42.336589
3502.578318	318495.860449	42.341594
3502.599237	318470.542619	42.346599
3502.930246	318436.856786	42.351604
3502.954590	318416.906636	42.356608
3502.753931	318390.503956	42.361613
3503.086661	318345.521554	42.366618
3502.499952	318322.308551	42.371623
3502.522140	318282.234055	42.376628
3502.453851	318257.286237	42.381632
3502.411569	318223.963905	42.386637
3502.413743	318200.353467	42.391642
3502.517189	318179.296833	42.396647
3502.689555	318161.791306	42.401652
3502.546003	318126.780113	42.406656
3502.293037	318102.878764	42.411661
3502.814233	318074.582090	42.416666
3502.267803	318051.108224	42.421671
3502.510744	318025.984406	42.426676
3502.745186	318000.403943	42.431680
3502.407546	317968.679566	42.436685
3502.859935	317941.843769	42.441690
3502.288037	317926.540769	42.446695
3502.543265	317882.078854	42.451700
3502.812671	317859.011625	42.456704
3502.106213	317840.523907	42.461709
3502.614831	317806.835265	42.466714
3502.432960	317790.860625	42.471719
3502.576508	317755.931462	42.476724
3502.656899	317728.619406	42.481728
3502.293746	317700.791502	42.486733
3502.621347	317677.409771	42.491738
3502.547484	317660.120637	42.496743
3502.520317	317622.750148	42.501748
3502.144301	317594.466225	42.506752
3502.329541	317571.284792	42.511757
3502.752721	317551.373664	42.516762
3502.693017	317534.565674	42.521767
3502.381345	317497.163231	42.526772
3502.656637	317470.176738	42.531776
3502.309228	317444.025414	42.536781
3502.275990	317415.306148	42.541786
3502.205100	317402.545217	42.546791
3502.469973	317385.050362	42.551796
3502.380273	317345.323258	42.556800
3502.381996	317315.631645	42.561805
3502.281655	317298.931688	42.566810
3502.561751	317281.536183	42.571815
3502.443419	317257.180801	42.576820
3502.494105	317237.785736	42.581824
3502.338676	317207.329898	42.586829
3502.661016	317181.379022	42.591834
3502.008099	317154.435682	42.596839
3502.216482	317131.224958	42.601844
3502.703413	317107.741689	42.606848
3502.180042	317085.281412	42.611853
3502.345246	317059.405916	42.616858
3502.324932	317041.497543	42.621863
3502.457141	317017.026532	42.626868
3502.428964	316986.041792	42.631872
3502.297854	316968.913995	42.636877
3502.582171	316939.585033	42.641882
3502.191602	316920.335143	42.646887
3502.451555	316893.477912	42.651892
3502.143683	316867.676266	42.656896
3502.065390	316838.302157	42.661901
3502.358942	316821.922082	42.666906
3501.963587	316800.026831	42.671911
3502.185742	316779.816029	42.676916
3502.270105	316759.397775	42.681920
3502.116337	316747.438341	42.686925
3502.258112	316726.527681	42.691930
3502.095343	316710.753208	42.696935
3502.037489	316699.847370	42.701940
3502.187984	316668.478274	42.706944
3501.943471	316648.620244	42.711949
3502.393368	316630.256548	42.716954
3502.060088	316600.286072	42.721959
3502.014700	316589.759903	42.726964
3502.026104	316569.505626	42.731968
3502.052864	316549.961343	42.736973
3502.233882	316521.258888	42.741978
3501.834913	316506.589878	42.746983
3501.630934	316483.341513	42.751988
3501.579170	316470.729982	42.756992
3501.471360	316454.132648	42.761997
3501.756328	316444.445303	42.767002
3501.660160	316442.094264	42.772007
3501.812962	316424.438452	42.777012
3501.985531	316403.904472	42.782016
3501.947299	316394.776508	42.787021
3502.315017	316367.087933	42.792026
3501.899963	316357.535454	42.797031
3501.729125	316334.332717	42.802036
3501.821947	316319.688531	42.807041
3501.674456	316313.503593	42.812045
3502.041558	316291.412560	42.817050
3502.215167	316276.653956	42.822055
3502.141095	316252.799969	42.827060
3502.350942	316232.768947	42.832065
3501.812040	316221.302119	42.837069
3502.222509	316186.660754	42.842074
3502.350332	316174.453597	42.847079
3502.248174	316147.423541	42.852084
3502.285714	316144.720820	42.857089
3502.175463	316110.313465	42.862093
3502.168920	316098.025522	42.867098
3502.242676	316070.891587	42.872103
3501.687015	316054.542225	42.877108
3502.308474	316033.429030	42.882113
3502.104020	316027.710939	42.887117
3502.133856	315998.522919	42.892122
3502.045278	315982.736590	42.897127
3502.180184	315952.870586	42.902132
3502.262962	315942.604104	42.907137
3501.880056	315920.248494	42.912141
3501.942827	315890.648161	42.917146
3502.093041	315891.260893	42.922151
3501.671545	315867.537348	42.927156
3501.689575	315850.614795	42.932161
3501.738403	315846.281913	42.937165
3502.065010	315816.156858	42.942170
3501.945351	315813.656797	42.947175
3502.145660	315784.772751	42.952180
3502.084673	315759.186301	42.957185
3501.585139	315756.262202	42.962189
3502.103448	315731.984559	42.967194
3501.676857	315722.815401	42.972199
3501.692664	315702.483713	42.977204
3501.824744	315683.507788	42.982209
3501.561572	315681.768018	42.987213
3501.939377	315665.323462	42.992218
3502.127893	315648.679503	42.997223
3502.236614	315630.165190	43.002228
3502.278067	315603.926548	43.007233
3502.000330	315597.278447	43.012237
3502.309796	315571.761192	43.017242
3502.066848	315560.120706	43.022247
3502.078202	315531.240596	43.027252
3502.023134	315506.034731	43.032257
3502.206392	315499.034663	43.037261
3501.980746	315472.863147	43.042266
3502.030506	315467.537781	43.047271
3501.931844	315441.371838	43.052276
3501.759482	315418.601408	43.057281
3501.694533	315414.031835	43.062285
3501.750958	315389.266460	43.067290
3501.960949	315369.820236	43.072295
3501.794592	315361.220967	43.077300
3501.890999	315344.642183	43.082305
3502.098813	315340.895044	43.087309
3501.463602	315316.950184	43.092314
3501.139180	315298.070910	43.097319
3501.766121	315292.171856	43.102324
3502.029240	315290.400678	43.107329
3501.772840	315267.261654	43.112333
3502.000192	315252.367095	43.117338
3501.750731	315242.406833	43.122343
3501.812226	315223.212756	43.127348
3502.059782	315211.546383	43.132353
3501.682475	315189.342197	43.137357
3501.836066	315170.108256	43.142362
3501.448030	315165.869052	43.147367
3501.756392	315146.051139	43.152372
3501.726956	315126.311473	43.157377
3501.888398	315126.286365	43.162381
3501.557609	315113.158312	43.167386
3501.598249	315094.654425	43.172391
3501.511896	315077.035474	43.177396
3501.527107	315072.733217	43.182401
3501.293427	315078.342085	43.187405
3501.616202	315049.769194	43.192410
3501.179276	315036.835819	43.197415
3501.363647	315029.352072	43.202420
3501.103167	315017.866851	43.207425
3501.355582	315025.282576	43.212429
3501.515694	315014.825685	43.217434
3501.249016	315000.898816	43.222439
3501.508689	314983.327507	43.227444
3501.913855	314977.615748	43.232449
3501.508948	314983.556725	43.237453
3501.476396	314967.430510	43.242458
3501.470505	314957.330330	43.247463
3501.613136	314944.306321	43.252468
3501.607888	314928.557483	43.257473
3501.579353	314920.979784	43.262477
3501.577323	314901.413844	43.267482
3501.976951	314897.178690	43.272487
3501.833161	314888.830242	43.277492
3502.019258	314870.914177	43.282497
3501.613998	314858.357460	43.287501
3501.723626	314838.901256	43.292506
3501.927723	314819.023170	43.297511
3501.582929	314817.321572	43.302516
3501.771881	314791.949939	43.307521
3501.714469	314779.287930	43.312525
3501.760515	314761.317385	43.317530
3501.681545	314767.334652	43.322535
3501.847556	314746.826389	43.327540
3501.951395	314727.600038	43.332545
3501.887133	314712.929002	43.337549
3501.981378	314689.327758	43.342554
3502.022789	314679.754446	43.347559
3501.943128	314660.098763	43.352564
3502.056634	314646.850225	43.357569
3501.475197	314620.962838	43.362573
3502.025955	314608.587361	43.367578
3501.798688	314607.478039	43.372583
3501.635498	314580.329367	43.377588
3501.890203	314565.710192	43.382593
3501.685119	314559.508574	43.387597
3501.868485	314556.655739	43.392602
3501.742911	314528.457945	43.397607
3501.765341	314516.699370	43.402612
3502.238575	314511.002356	43.407617
3501.692275	314497.755153	43.412621
3501.736693	314471.693502	43.417626
3501.863214	314461.216292	43.422631
3501.487105	314433.999044	43.427636
3501.924139	314433.498298	43.432641
3501.759735	314419.249931	43.437645
3502.012150	314391.756284	43.442650
3502.003799	314388.322750	43.447655
3501.976198	314368.404359	43.452660
3501.682522	314353.489187	43.457665
3501.492126	314344.969817	43.462669
3501.565946	314317.707601	43.467674
3501.994408	314309.040582	43.472679
3501.634282	314305.712927	43.477684
3501.958224	314282.660781	43.482689
3501.761956	314272.793768	43.487693
3501.758993	314262.947419	43.492698
3501.579704	314229.592645	43.497703
3501.823269	314226.781267	43.502708
3502.116739	314221.035989	43.507713
3501.874336	314204.815092	43.512717
3501.952551	314193.200377	43.517722
3501.777780	314176.994341	43.522727
3501.921387	314152.418218	43.527732
3501.602249	314141.298167	43.532737
3501.752026	314133.183573	43.537741
3501.746718	314109.699372	43.542746
3501.585184	314100.183112	43.547751
3501.562821	314088.991206	43.552756
3501.926369	314067.891978	43.557761
3501.609115	314061.733273	43.562765
3501.890182	314049.374365	43.567770
3501.851633	314038.261311	43.572775
3501.701191	314020.524750	43.577780
3502.019332	314009.076035	43.582785
3501.453876	313997.485570	43.587789
3501.772827	313980.922386	43.592794
3501.469560	313982.572931	43.597799
3501.504680	313963.764115	43.602804
3501.701480	313942.767233	43.607809
3501.094010	313933.167989	43.612813
3501.444162	313927.515591	43.617818
3501.699317	313927.704832	43.622823
3501.376213	313901.827538	43.627828
3501.825653	313891.350602	43.632833
3501.396561	313890.679927	43.637837
3501.598380	313884.083823	43.642842
3501.542219	313861.065446	43.647847
3501.153016	313847.818938	43.652852
3501.414396	313845.157418	43.657857
3501.459776	313838.992878	43.662861
3501.443322	313829.072212	43.667866
3501.428963	313807.981058	43.672871
3501.214703	313801.806216	43.677876
3501.425399	313794.038261	43.682881
3501.043868	313800.357403	43.687885
3501.448144	313793.805967	43.692890
3501.437019	313795.919737	43.697895
3501.286290	313785.740164	43.702900
3501.242397	313759.132134	43.707905
3501.338459	313754.588112	43.712909
3501.335952	313749.067160	43.717914
3501.295482	313750.523960	43.722919
3501.349869	313752.525711	43.727924
3501.708968	313732.470254	43.732929
3501.125861	313723.019824	43.737933
3501.447261	313705.921823	43.742938
3501.742333	313714.425210	43.747943
3501.564143	313699.822550	43.752948
3501.887149	313683.004180	43.757953
3501.596137	313672.363066	43.762957
3501.779040	313660.833629	43.767962
3501.819960	313641.769328	43.772967
3501.420119	313634.961916	43.777972
3501.690768	313620.747063	43.782977
3501.658313	313614.899997	43.787981
3501.464830	313593.353301	43.792986
3501.841956	313577.391550	43.797991
3501.637193	313582.767077	43.802996
3501.741130	313547.637290	43.808001
3501.762916	313544.148092	43.813005
3501.544714	313531.892546	43.818010
3501.800642	313520.936886	43.823015
3501.721113	313499.270551	43.828020
3501.792459	313490.048538	43.833025
3501.244459	313489.803563	43.838029
3501.608355	313460.154573	43.843034
3501.557478	313444.895809	43.848039
3501.589965	313454.916094	43.853044
3501.441701	313447.662206	43.858049
3501.513782	313433.478340	43.863053
3501.783099	313411.452088	43.868058
3501.493685	313401.981121	43.873063
3501.483156	313405.519723	43.878068
3501.740019	313379.602353	43.883073
3501.352592	313373.276412	43.888077
3501.885637	313361.412266	43.893082
3501.696748	313356.861865	43.898087
3501.439983	313340.566573	43.903092
3501.759874	313324.740907	43.908097
3501.717245	313322.661228	43.913101
3501.285464	313311.660367	43.918106
3501.391182	313296.529740	43.923111
3501.233445	313289.022861	43.928116
3501.030265	313283.380558	43.933121
3501.149089	313294.405173	43.938125
3501.235727	313289.506351	43.943130
3501.353447	313288.775622	43.948135
3501.551811	313284.724457	43.953140
3501.494627	313248.042052	43.958145
3501.396824	313244.596973	43.963149
3501.438781	313245.277556	43.968154
3501.459414	313244.969124	43.973159
3501.451783	313224.385549	43.978164
3501.623912	313209.091842	43.983169
3501.583600	313208.487599	43.988173
3501.433979	313204.821614	43.993178
3501.366202	313178.853107	43.998183
3501.513356	313161.146023	44.003188
3501.322402	313157.232047	44.008193
3501.279766	313162.149713	44.013197
3501.485546	313145.883817	44.018202
3501.524368	313137.124827	44.023207
3501.253932	313126.353145	44.028212
3501.766122	313115.179210	44.033217
3501.614502	313115.508385	44.038221
3501.519833	313106.668479	44.043226
3501.381733	313084.324095	44.048231
3501.457630	313073.854484	44.053236
3501.658061	313061.304359	44.058241
3501.682831	313064.939248	44.063245
3501.424959	313044.750946	44.068250
3501.440403	313032.127955	44.073255
3501.221451	313038.828902	44.078260
3501.380404	313021.959605	44.083265
3501.354258	313026.187691	44.088269
3501.613513	313010.320508	44.093274
3501.070114	312996.512627	44.098279
3501.297880	312997.367725	44.103284
3501.187081	312989.370003	44.108289
3501.527760	312986.950487	44.113293
3501.514004	312980.362513	44.118298
3501.704043	312957.177970	44.123303
3501.389492	312946.489478	44.128308
3501.324294	312940.672891	44.133313
3501.427446	312949.002865	44.138317
3501.134092	312939.557864	44.143322
3501.255807	312913.381468	44.148327
3501.032593	312902.424236	44.153332
3501.241705	312899.567274	44.158337
3501.410857	312907.683376	44.163341
3501.145150	312897.928704	44.168346
3501.377271	312899.673699	44.173351
3500.965026	312900.221737	44.178356
3501.282967	312902.258656	44.183361
3501.303114	312890.703583	44.188365
3501.213716	312863.466026	44.193370
3501.279783	312862.183575	44.198375
3501.173558	312864.235920	44.203380
3501.211636	312852.601699	44.208385
3501.329078	312855.916775	44.213389
3501.532855	312862.856998	44.218394
3501.896641	312840.408585	44.223399
3501.546003	312828.580680	44.228404
3501.619182	312804.345637	44.233409
3501.424116	312816.513579	44.238413
3501.395775	312794.584461	44.243418
3501.634323	312780.857826	44.248423
3501.426682	312773.664007	44.253428
3501.543652	312763.086124	44.258433
3501.095657	312751.349755	44.263437
3501.416749	312731.376143	44.268442
3501.217415	312736.369241	44.273447
3501.400830	312724.686821	44.278452
3501.551289	312723.060385	44.283457
3501.293203	312732.973583	44.288461
3501.429395	312724.097511	44.293466
3501.062091	312701.966893	44.298471
3501.195735	312697.315111	44.303476
3501.397292	312686.876657	44.308481
3501.268363	312695.064844	44.313485
3501.355384	312686.781692	44.318490
3501.105420	312681.324746	44.323495
3501.164244	312682.308043	44.328500
3501.514053	312654.645465	44.333505
3501.460346	312649.412285	44.338509
3501.037190	312643.855186	44.343514
3501.356055	312645.790191	44.348519
3501.195366	312644.186952	44.353524
3501.324988	312650.197329	44.358529
3501.063711	312643.800675	44.363533
3501.318635	312620.885718	44.368538
3501.502650	312602.765536	44.373543
3501.367530	312612.863096	44.378548
3501.738623	312608.962984	44.383553
3501.437749	312614.557210	44.388557
3501.662196	312584.522341	44.393562
3501.731746	312564.053634	44.398567
3501.548485	312566.576050	44.403572
3501.658734	312548.492825	44.408577
3501.637961	312534.119638	44.413581
3501.818933	312521.216177	44.418586
3501.663148	312522.894606	44.423591
3501.447170	312505.320382	44.428596
3501.591281	312487.588073	44.433601
3501.354976	312482.739655	44.438605
3501.528814	312482.356374	44.443610
3501.351751	312461.137374	44.448615
3501.175947	312437.399082	44.453620
3501.666782	312433.149446	44.458625
3501.364405	312444.367340	44.463629
3501.516381	312443.198673	44.468634
3501.460181	312431.604531	44.473639
3500.820900	312411.450139	44.478644
3501.552073	312399.554774	44.483649
3501.247022	312395.175111	44.488653
3501.009301	312392.286195	44.493658
3501.328874	312400.658767	44.498663
3501.282338	312391.556747	44.503668
3501.254529	312391.255882	44.508673
3501.289269	312376.695851	44.513677
3501.184519	312363.582564	44.518682
3501.169372	312358.903119	44.523687
3501.002598	312351.143047	44.528692
3501.307870	312353.207417	44.533697
3501.134046	312353.438287	44.538701
3501.076551	312347.925766	44.543706
3501.062387	312350.879773	44.548711
3501.391866	312343.805475	44.553716
3501.287432	312323.949107	44.558721
3500.977372	312315.626187	44.563725
3500.851054	312313.355984	44.568730
3501.139578	312313.132890	44.573735
3501.056587	312312.357190	44.578740
3501.392968	312313.297101	44.583745
3501.245711	312318.867345	44.588749
3501.081030	312302.557293	44.593754
3501.133871	312294.559314	44.598759
3500.920724	312310.597912	44.603764
3501.205327	312305.998826	44.608769
3501.346223	312304.297535	44.613773
3501.187526	312276.892353	44.618778
3501.326446	312269.542492	44.623783
3501.356493	312261.751634	44.628788
3501.487093	312259.695715	44.633793
3501.267890	312267.770863	44.638797
3501.246770	312253.219527	44.643802
3501.498317	312238.803675	44.648807
3501.478239	312224.786521	44.653812
3501.464021	312218.249402	44.658817
3501.348154	312219.514474	44.663821
3501.309156	312217.154278	44.668826
3501.127838	312188.734764	44.673831
3501.168333	312180.993150	44.678836
3501.464119	312174.102213	44.683841
3501.567946	312181.083610	44.688845
3501.369292	312174.244528	44.693850
3501.160505	312171.961766	44.698855
3501.236887	312164.010975	44.703860
3501.151742	312140.487368	44.708865
3501.260595	312137.417025	44.713869
3501.121356	312130.441421	44.718874
3501.428560	312125.151757	44.723879
3501.179757	312135.699766	44.728884
3501.464150	312127.156648	44.733889
3500.960198	312133.953172	44.738893
3501.152004	312109.851896	44.743898
3501.120934	312097.744834	44.748903
3501.079207	312096.479214	44.753908
3501.289008	312087.006267	44.758913
3500.966646	312083.214527	44.763917
3500.705397	312082.873820	44.768922
3501.304589	312090.566595	44.773927
3501.242726	312092.917384	44.778932
3501.253851	312084.569654	44.783937
3501.147982	312088.530389	44.788941
3501.251311	312081.669527	44.793946
3501.465060	312073.900809	44.798951
3501.100444	312049.886494	44.803956
3501.453355	312038.711759	44.808961
3501.130651	312039.093134	44.813965
3501.249676	312037.497035	44.818970
3501.131514	312042.477516	44.823975
3501.099568	312038.233241	44.828980
3501.338798	312030.994887	44.833985
3501.280384	312026.449402	44.838989
3501.182711	312008.780159	44.843994
3501.483333	311998.326064	44.848999
3501.176788	312010.028179	44.854004
3501.362337	312008.039995	44.859009
3501.236363	312013.810513	44.864013
3501.249825	311999.915276	44.869018
3501.068643	311979.078384	44.874023
3501.197842	311973.714750	44.879028
3501.119812	311956.907564	44.884033
3501.009321	311960.512795	44.889037
3501.139177	311955.581630	44.894042
3501.466717	311960.237984	44.899047
3501.451428	311961.080209	44.904052
3501.332797	311955.653537	44.909057
3501.480622	311950.566889	44.914061
3501.652624	311935.527241	44.919066
3501.546160	311935.442235	44.924071
3501.238873	311930.299510	44.929076
3501.701647	311922.822627	44.934081
3501.527187	311898.142365	44.939085
3501.144268	311897.642559	44.944090
3501.195083	311892.825528	44.949095
3501.373442	311881.652600	44.954100
3501.096862	311883.171818	44.959105
3500.811779	311883.369193	44.964109
3500.675352	311882.118373	44.969114
3501.179336	311879.495151	44.974119
3501.026010	311888.476107	44.979124
3501.189827	311871.478407	44.984129
3501.148058	311851.968280	44.989133
3501.186965	311850.893612	44.994138
3501.357330	311840.001827	44.999143
3501.268678	311839.201558	45.004148
3501.554683	311826.561387	45.009153
3501.600336	311832.941235	45.014157
3501.348073	311806.771797	45.019162
3501.704367	311808.904550	45.024167
3501.450849	311800.954384	45.029172
3501.286546	311800.471290	45.034177
3501.214696	311793.994013	45.039181
3501.332234	311775.298655	45.044186
3501.413635	311761.672628	45.049191
3501.212572	311752.670979	45.054196
3501.806931	311752.578188	45.059201
3501.831361	311749.037551	45.064205
3501.607155	311731.337094	45.069210
3501.464290	311716.779180	45.074215
3501.414772	311721.494507	45.079220
3501.691070	311710.815141	45.084225
3501.452287	311688.231372	45.089229
3501.172240	311674.865395	45.094234
3500.693499	311681.861608	45.099239
3501.245897	311673.174725	45.104244
3501.533111	311666.844860	45.109249
3501.575016	311670.248167	45.114253
3501.480641	311649.473895	45.119258
3501.730493	311634.956340	45.124263
3501.465715	311640.799496	45.129268
3501.545311	311628.166096	45.134273
3501.491575	311604.662756	45.139277
3501.534839	311601.857090	45.144282
3501.622408	311592.479492	45.149287
3501.331456	311600.922212	45.154292
3501.374509	311588.065503	45.159297
3501.337716	311564.712168	45.164301
3501.410524	311555.184195	45.169306
3501.184927	311548.120223	45.174311
3501.221936	311556.079099	45.179316
3501.561889	311555.110034	45.184321
3501.734781	311538.288916	45.189325
3501.467318	311517.210851	45.194330
3501.701838	311515.902027	45.199335
3501.341349	311516.798229	45.204340
3501.488592	311490.184468	45.209345
3501.597737	311477.800867	45.214349
3501.554138	311474.169062	45.219354
3501.500697	311471.022266	45.224359
3501.131653	311455.863486	45.229364
3501.216695	311432.338364	45.234369
3501.703596	311429.845017	45.239373
3501.662415	311430.106045	45.244378
3501.443469	311426.323529	45.249383
3501.172066	311420.106412	45.254388
3501.141678	311393.545814	45.259393
3501.178560	311390.410337	45.264397
3501.243843	311380.221913	45.269402
3501.562960	311384.268939	45.274407
3501.452574	311379.807855	45.279412
3501.814018	311370.769082	45.284417
3501.740602	311361.314823	45.289421
3501.488728	311344.839949	45.294426
3501.549988	311339.206959	45.299431
3501.487757	311339.674846	45.304436
3501.414132	311308.820603	45.309441
3501.485047	311303.949478	45.314445
3501.392649	311297.551683	45.319450
3501.261957	311307.521602	45.324455
3501.312534	311295.325231	45.329460
3501.220863	311282.235042	45.334465
3501.463217	311273.113086	45.339469
3501.298871	311280.569124	45.344474
3501.598877	311273.092140	45.349479
3501.192253	311272.875938	45.354484
3501.355911	311251.832136	45.359489
3501.357023	311234.706969	45.364493
3501.417519	311230.600844	45.369498
3501.585134	311227.826607	45.374503
3501.316357	311223.339378	45.379508
3501.236606	311209.102238	45.384513
3501.203843	311203.000459	45.389517
3501.076574	311188.668957	45.394522
3501.578821	311185.155360	45.399527
3501.382655	311186.433013	45.404532
3501.302179	311188.481405	45.409537
3501.478475	311177.944783	45.414541
3501.576347	311170.652061	45.419546
3501.717428	311161.596808	45.424551
3501.610927	311150.239229	45.429556
3501.413410	311142.000290	45.434561
3501.391302	311121.570732	45.439565
3500.984324	311116.825193	45.444570
3501.267232	311103.396487	45.449575
3501.161327	311110.919753	45.454580
3501.236492	311106.276957	45.459585
3501.383260	311112.030390	45.464589
3501.404162	311099.838608	45.469594
3501.548809	311069.688019	45.474599
3501.337855	311079.594195	45.479604
3501.564056	311057.395458	45.484609
3501.701992	311059.867737	45.489613
3501.203249	311048.393335	45.494618
3501.558180	311038.414014	45.499623
3501.452779	311029.219149	45.504628
3501.317190	311020.181679	45.509633
3501.368157	311023.787184	45.514637
3501.599333	311009.094236	45.519642
3501.555938	310987.599212	45.524647
3501.450145	310985.300290	45.529652
3501.796794	310980.538699	45.534657
3501.552043	310963.782672	45.539661
3501.154751	310966.720326	45.544666
3501.414381	310945.737723	45.549671
3501.656654	310944.631240	45.554676
3501.411712	310936.984940	45.559681
3501.484605	310917.685517	45.564685
3501.445695	310909.040048	45.569690
3501.636839	310903.717501	45.574695
3501.560544	310907.877280	45.579700
3501.604176	310889.498481	45.584705
3501.514422	310865.593267	45.589709
3501.496726	310865.138134	45.594714
3501.255883	310855.404595	45.599719
3501.094367	310858.076379	45.604724
3501.124334	310864.407918	45.609729
3501.471944	310835.904896	45.614733
3501.383913	310830.371525	45.619738
3501.624179	310819.315900	45.624743
3501.375743	310816.912039	45.629748
3501.753819	310810.389732	45.634753
3501.585462	310792.705638	45.639757
3501.569081	310781.766467	45.644762
3501.518837	310773.097300	45.649767
3501.572980	310772.096564	45.654772
3501.174547	310745.898499	45.659777
3501.440131	310739.190200	45.664781
3501.385590	310731.259637	45.669786
3501.321261	310727.198429	45.674791
3501.265477	310731.355017	45.679796
3501.614104	310712.165079	45.684801
3501.458350	310697.201727	45.689805
3501.176186	310698.543731	45.694810
3501.039588	310684.544337	45.699815
3501.417013	310688.047936	45.704820
3501.531861	310691.312678	45.709825
3501.512293	310667.549069	45.714829
3500.851548	310651.926712	45.719834
3501.413978	310595.246381	45.724839
3501.154902	310507.649890	45.729844
3501.047863	310349.873718	45.734849
3500.765148	310151.588182	45.739853
3500.438303	309920.253532	45.744858
3500.434552	309623.977932	45.749863
3499.986582	309292.780371	45.754868
3499.562588	308922.362712	45.759873
3499.222190	308492.102356	45.764877
3499.069126	308014.450874	45.769882
3498.538477	307492.548984	45.774887
3497.950735	306930.366026	45.779892
3497.638579	306313.597497	45.784897
3497.291578	305642.595360	45.789901
3496.445702	304934.302908	45.794906
3495.973984	304179.369427	45.799911
3495.369340	303376.116201	45.804916
3494.768358	302514.059648	45.809921
3493.818327	301624.022228	45.814925
3493.127811	300695.828861	45.819930
3492.420703	299698.724347	45.824935
3491.321815	298663.993670	45.829940
3490.545757	297570.066629	45.834945
3489.719703	296442.629758	45.839949
3488.858455	295258.185307	45.844954
3487.743682	294029.287814	45.849959
3486.663779	292760.344446	45.854964
3485.872252	291446.120633	45.859969
3484.596662	290079.047087	45.864973
3482.971486	288675.544812	45.869978
3482.205195	287221.039906	45.874983
3480.997301	285736.124585	45.879988
3479.639968	284197.584991	45.884993
3478.119154	282619.550201	45.889997
3477.029464	280999.557829	45.895002
3475.954076	279324.814012	45.900007
3474.099468	277639.639643	45.905012
3472.600639	275883.438744	45.910017
3470.886092	274087.538646	45.915021
3469.147096	272271.666873	45.920026
3467.952106	270403.549926	45.925031
3465.758126	268495.216801	45.930036
3464.337594	266564.366962	45.935041
3462.614447	264583.540401	45.940045
3460.445215	262577.077293	45.945050
3458.716013	260525.613430	45.950055
3456.698655	258451.137262	45.955060
3454.906505	256322.424559	45.960065
3452.940153	254171.395905	45.965069
3450.756095	251991.718239	45.970074
3448.782887	249761.220308	45.975079
3446.311226	247520.939856	45.980084
3444.577744	245231.669243	45.985089
3441.987836	242921.877596	45.990093
3439.477414	240583.220140	45.995098
3436.758922	238209.809974	46.000103
3434.789696	235815.762296	46.005108
3432.145732	233391.242478	46.010113
3429.885693	230939.602685	46.015117
3426.938932	228466.693161	46.020122
3424.477159	225963.420060	46.025127
3421.803279	223450.958996	46.030132
3419.101546	220898.391138	46.035137
3416.740797	218330.393426	46.040141
3413.797684	215744.491237	46.045146
3410.933172	213115.804769	46.050151
3407.811777	210486.440117	46.055156
3404.738209	207834.858997	46.060161
3402.039592	205154.826828	46.065165
3398.782308	202449.755164	46.070170
3395.521689	199738.459638	46.075175
3392.029495	197004.733413	46.080180
3388.949598	194269.007699	46.085185
3385.841234	191522.367193	46.090189
3382.201154	188763.215673	46.095194
3378.678138	185989.038625	46.100199
3375.273242	183214.280122	46.105204
3371.573976	180434.630327	46.110209
3368.103773	177623.481640	46.115213
3364.166477	174835.527401	46.120218
3360.433982	172021.005241	46.125223
3356.449298	169217.585618	46.130228
3352.526395	166414.671122	46.135233
3349.061267	163598.852830	46.140237
3344.796281	160778.734995	46.145242
3340.476785	157960.685465	46.150247
3336.173132	155168.777779	46.155252
3331.211855	152381.229680	46.160257
3326.507112	149603.158630	46.165261
3321.427434	146842.149499	46.170266
3316.359520	144108.540118	46.175271
3310.499149	141393.779375	46.180276
3304.860947	138637.849240	46.185281
3299.449328	135995.755175	46.190285
3292.863290	133397.491741	46.195290
3286.830054	130834.199192	46.200295
3279.540156	128327.807822	46.205300
3272.461321	125876.657495	46.210305
3265.542920	123479.986899	46.215309
3258.142715	121145.558990	46.220314
3250.746355	118878.160602	46.225319
3243.363918	116678.544271	46.230324
3235.191517	114564.259507	46.235329
3226.471126	112544.703398	46.240333
3217.830299	110605.587939	46.245338
3209.114378	108763.466272	46.250343
3200.189947	107006.395603	46.255348
3191.791788	105359.762840	46.260353
3182.914780	103813.528334	46.265357
3173.771433	102360.032085	46.270362
3165.110749	101002.145309	46.275367
3156.897121	99736.913652	46.280372
3148.223920	98563.223072	46.285377
3140.169114	97469.508047	46.290381
3132.635586	96475.665060	46.295386
3125.713504	95554.513073	46.300391
3118.466134	94716.625673	46.305396
3111.692544	93935.769718	46.310401
3105.885066	93225.994682	46.315405
3099.995907	92571.944168	46.320410
3094.538534	91961.996532	46.325415
3089.066206	91391.835254	46.330420
3084.231606	90872.613985	46.335425
3079.600497	90382.860969	46.340429
3074.449055	89930.095618	46.345434
3070.433310	89501.249804	46.350439
3065.945165	89100.576284	46.355444
3061.962029	88718.290304	46.360449
3058.322104	88354.060719	46.365453
3054.550322	88010.781729	46.370458
3050.864301	87660.657980	46.375463
3047.296627	87329.920307	46.380468
3043.925802	87016.510317	46.385473
3040.605815	86698.166314	46.390477
3037.126752	86397.751326	46.395482
3033.814608	86078.739495	46.400487
3030.351204	85777.705925	46.405492
3027.175996	85473.174877	46.410497
3023.977557	85170.810335	46.415501
3020.416416	84865.380520	46.420506
3017.305246	84568.001248	46.425511
3013.961195	84270.801200	46.430516
3010.895430	83966.370539	46.435521
3007.712912	83664.883129	46.440525
3004.231677	83355.137713	46.445530
3000.845836	83044.466116	46.450535
2997.411834	82750.154097	46.455540
2993.844951	82433.636016	46.460545
2990.675472	82131.845197	46.465549
2987.040525	81827.234210	46.470554
2983.914191	81524.655559	46.475559
2980.112094	81220.394817	46.480564
2976.885793	80919.540395	46.485569
2972.958317	80605.220446	46.490573
2969.244457	80308.513453	46.495578
2966.019570	80024.320521	46.500583
2962.506142	79722.952279	46.505588
2959.318337	79430.071732	46.510593
2955.723719	79125.979142	46.515597
2951.807363	78837.219694	46.520602
2948.109571	78537.861825	46.525607
2944.729214	78250.282082	46.530612
2940.794920	77956.924220	46.535617
2937.046252	77678.793908	46.540621
2933.512382	77396.682965	46.545626
2929.791936	77121.538507	46.550631
2926.110199	76852.639284	46.555636
2922.272396	76587.132651	46.560641
2918.937592	76318.057439	46.565645
2914.919868	76061.169276	46.570650
2911.314571	75805.222325	46.575655
2908.013495	75548.214241	46.580660
2904.124985	75289.967021	46.585665
2900.595703	75038.091986	46.590669
2896.917290	74798.383142	46.595674
2893.687629	74531.239546	46.600679
2889.945742	74294.326241	46.605684
2886.091619	74045.406693	46.610689
2882.685529	73795.682857	46.615693
2879.040945	73568.983302	46.620698
2875.127129	73323.292589	46.625703
2871.843179	73094.953339	46.630708
2868.354873	72857.911532	46.635713
2865.098313	72623.718099	46.640717
2861.195204	72389.323099	46.645722
2857.733145	72147.115398	46.650727
2854.274434	71928.768778	46.655732
2850.770819	71688.146327	46.660737
2847.540036	71458.619280	46.665741
2843.849404	71247.844312	46.670746
2840.292969	71008.848929	46.675751
2836.553396	70776.194958	46.680756
2832.966160	70546.871304	46.685761
2829.853615	70332.762787	46.690765
2826.421292	70106.923180	46.695770
2822.917682	69862.019542	46.700775
2819.891615	69635.269789	46.705780
2815.746003	69405.814962	46.710785
2812.285225	69168.656146	46.715789
2808.924774	68951.836259	46.720794
2805.727136	68720.810878	46.725799
2802.134272	68491.639549	46.730804
2798.345586	68264.678271	46.735809
2794.916725	68031.225829	46.740813
2791.525616	67805.856898	46.745818
2788.202008	67571.674846	46.750823
2784.551111	67338.320559	46.755828
2781.309951	67109.887325	46.760833
2777.639303	66889.324668	46.765837
2774.262437	66658.644205	46.770842
2770.968644	66424.512426	46.775847
2766.998033	66193.040378	46.780852
2764.030082	65959.515713	46.785857
2759.999861	65718.859783	46.790861
2756.638914	65503.865491	46.795866
2753.323879	65267.576898	46.800871
2749.771833	65034.228285	46.805876
2746.076193	64801.310511	46.810881
2742.734544	64572.515950	46.815885
2738.843805	64344.945482	46.820890
2735.721843	64113.397833	46.825895
2732.209060	63884.712466	46.830900
2728.903828	63653.946667	46.835905
2725.562150	63413.598588	46.840909
2721.946792	63185.272043	46.845914
2717.865069	62949.302892	46.850919
2714.499497	62717.990323	46.855924
2710.967376	62487.854695	46.860929
2707.791394	62258.287459	46.865933
2704.396997	62032.805583	46.870938
2700.970016	61784.820000	46.875943
2697.277668	61561.845094	46.880948
2693.750117	61318.817409	46.885953
2690.644896	61086.451251	46.890957
2686.906195	60867.037444	46.895962
2682.961780	60625.516051	46.900967
2679.862545	60388.459402	46.905972
2676.276227	60154.064065	46.910977
2672.979424	59918.673793	46.915981
2669.047793	59685.142900	46.920986
2665.730013	59453.701197	46.925991
2662.426595	59217.976041	46.930996
2658.839064	58985.749680	46.936001
2655.761206	58748.381978	46.941005
2652.311804	58519.063824	46.946010
2648.815689	58269.455766	46.951015
2644.975740	58024.663167	46.956020
2641.357670	57789.826019	46.961025
2637.744021	57550.618520	46.966029
2633.923149	57316.744124	46.971034
2630.544939	57073.500663	46.976039
2627.507330	56850.326895	46.981044
2623.729047	56617.670916	46.986049
2620.421141	56376.644308	46.991053
2616.834352	56151.354880	46.996058
2613.264066	55906.218095	47.001063
2609.706664	55662.369818	47.006068
2606.186507	55443.193093	47.011073
2602.792365	55194.508375	47.016077
2599.518123	54965.888358	47.021082
2596.047828	54721.179581	47.026087
2592.567374	54484.748193	47.031092
2589.106348	54253.880233	47.036097
2585.852836	54003.352466	47.041101
2582.332608	53759.949363	47.046106
2578.418980	53521.685735	47.051111
2575.122442	53276.768078	47.056116
2571.426193	53029.644295	47.061121
2567.921530	52783.406696	47.066125
2564.526672	52553.065296	47.071130
2560.794237	52315.293106	47.076135
2557.398859	52075.808516	47.081140
2554.056728	51836.774810	47.086145
2550.598299	51597.679281	47.091149
2546.834480	51361.520362	47.096154
2543.566164	51110.689651	47.101159
2539.672568	50871.193903	47.106164
2536.437313	50637.845993	47.111169
2532.958383	50391.718483	47.116173
2529.252117	50154.871436	47.121178
2526.083195	49904.691622	47.126183
2522.376421	49678.664870	47.131188
2519.104973	49419.257939	47.136193
2515.769298	49187.678447	47.141197
2511.860429	48930.292370	47.146202
2508.307592	48693.017754	47.151207
2504.933759	48454.747136	47.156212
2501.336102	48210.101419	47.161217
2498.308112	47960.269636	47.166221
2494.832029	47722.783792	47.171226
2491.055478	47465.526737	47.176231
2487.226541	47233.302157	47.181236
2484.186706	46982.404740	47.186241
2480.991866	46729.041781	47.191245
2476.990837	46488.010445	47.196250
2473.632376	46237.405802	47.201255
2470.275907	45992.479908	47.206260
2466.843964	45747.549457	47.211265
2462.962040	45497.193494	47.216269
2459.238272	45256.233450	47.221274
2456.208170	45008.419669	47.226279
2452.837031	44756.951991	47.231284
2448.994882	44515.263760	47.236289
2445.519121	44261.465222	47.241293
2441.912139	44018.483584	47.246298
2438.531701	43769.596856	47.251303
2435.049195	43519.232285	47.256308
2431.369915	43277.126163	47.261313
2428.094091	43028.561130	47.266317
2424.702120	42779.769746	47.271322
2421.192045	42519.052771	47.276327
2417.919610	42279.665033	47.281332
2414.336921	42029.878324	47.286337
2410.586224	41773.392922	47.291341
2407.209973	41529.337236	47.296346
2403.627782	41278.500049	47.301351
2400.653640	41024.596777	47.306356
2396.797289	40766.427660	47.311361
2393.249088	40510.470655	47.316365
2389.859723	40266.754465	47.321370
2386.557738	40008.076431	47.326375
2382.469666	39750.031679	47.331380
2379.212420	39504.521693	47.336385
2375.678017	39245.020466	47.341389
2372.305207	39001.328549	47.346394
2368.853495	38740.698209	47.351399
2365.461674	38494.472583	47.356404
2361.263066	38237.946709	47.361409
2358.209338	37977.871951	47.366413
2354.970657	37724.657262	47.371418
2351.333782	37470.512507	47.376423
2348.107246	37215.355613	47.381428
2344.247629	36966.164931	47.386433
2341.244390	36696.740525	47.391437
2337.445022	36441.409867	47.396442
2334.079764	36178.261293	47.401447
2330.739969	35915.923412	47.406452
2327.071220	35659.168023	47.411457
2323.967575	35399.335251	47.416461
2320.045500	35135.874631	47.421466
2316.633643	34871.513396	47.426471
2313.151183	34606.196654	47.431476
2309.482880	34350.927662	47.436481
2306.354489	34079.977623	47.441485
2302.698800	33819.249089	47.446490
2298.910878	33552.028400	47.451495
2295.962387	33286.384838	47.456500
2292.413666	33025.059934	47.461505
2288.942743	32753.996747	47.466509
2285.449588	32496.726282	47.471514
2282.045418	32218.174094	47.476519
2278.300038	31953.394661	47.481524
2274.486829	31686.499627	47.486529
2271.341060	31410.643148	47.491533
2267.576232	31147.429804	47.496538
2263.996715	30871.515246	47.501543
2261.468053	30607.259752	47.506548
2257.418754	30333.998954	47.511553
2254.294878	30059.563966	47.516557
2250.684905	29790.836329	47.521562
2247.309394	29514.267879	47.526567
2243.806513	29238.014586	47.531572
2240.045097	28952.540480	47.536577
2236.917718	28683.061054	47.541581
2232.903178	28408.920506	47.546586
2229.589720	28128.958026	47.551591
2226.189006	27855.818808	47.556596
2222.761387	27575.907114	47.561601
2219.591763	27280.034835	47.566605
2215.758371	27013.697806	47.571610
2212.380288	26728.289857	47.576615
2208.966520	26444.133441	47.581620
2205.385557	26168.022618	47.586625
2202.246725	25874.858936	47.591629
2198.411219	25598.244466	47.596634
2195.332830	25299.301113	47.601639
2191.679355	25019.580444	47.606644
2188.275135	24733.083292	47.611649
2184.869329	24430.801701	47.616653
2181.632724	24147.004736	47.621658
2177.959658	23848.017620	47.626663
2174.380967	23556.350386	47.631668
2170.506703	23260.799365	47.636673
2166.953833	22969.776541	47.641677
2163.734297	22679.738458	47.646682
2160.354013	22379.713909	47.651687
2157.112396	22091.144950	47.656692
2153.393349	21805.714670	47.661697
2150.126212	21499.933597	47.666701
2147.005273	21200.494471	47.671706
2143.394939	20893.490525	47.676711
2140.040743	20585.767154	47.681716
2136.716685	20291.992360	47.686721
2132.939943	19979.270687	47.691725
2129.694925	19680.209822	47.696730
2126.296875	19366.621549	47.701735
2122.521693	19054.649156	47.706740
2119.239651	18742.009195	47.711745
2115.669928	18428.912549	47.716749
2112.119335	18121.454991	47.721754
2108.721022	17814.637170	47.726759
2105.217464	17507.827998	47.731764
2101.568557	17199.349058	47.736769
2098.186803	16875.379844	47.741773
2094.446065	16569.699327	47.746778
2090.824965	16254.103052	47.751783
2087.351259	15940.661120	47.756788
2083.553163	15636.590818	47.761793
2080.184287	15330.387331	47.766797
2076.494791	15032.962261	47.771802
2072.516740	14726.578769	47.776807
2068.643201	14444.421675	47.781812
2064.283341	14152.887321	47.786817
2060.349659	13876.098978	47.791821
2055.772404	13611.183900	47.796826
2051.903329	13367.108607	47.801831
2048.062720	13109.139344	47.806836
2043.224654	12889.017919	47.811841
2039.361844	12665.821093	47.816845
2035.338851	12462.075046	47.821850
2031.075883	12258.479559	47.826855
2027.013626	12059.951933	47.831860
2023.153647	11874.599503	47.836865
2019.461788	11692.312433	47.841869
2015.867972	11513.323205	47.846874
2012.765050	11331.998521	47.851879
2009.566223	11155.033974	47.856884
2005.516266	10980.850803	47.861889
2002.344139	10802.691939	47.866893
1998.877027	10630.769754	47.871898
1995.810727	10464.215456	47.876903
1992.490068	10276.360093	47.881908
1989.235325	10101.437070	47.886913
1985.835733	9929.181565	47.891917
1982.354691	9751.043087	47.896922
1978.980177	9566.109230	47.901927
1975.646652	9383.756952	47.906932
1971.838276	9204.997526	47.911937
1968.489494	9017.019993	47.916941
1964.975914	8840.034875	47.921946
1961.057164	8665.045685	47.926951
1958.145593	8482.044331	47.931956
1954.558319	8310.779631	47.936961
1951.208985	8127.517936	47.941965
1947.882746	7945.371753	47.946970
1944.724534	7769.784594	47.951975
1941.022882	7574.457822	47.956980
1937.459969	7397.079616	47.961985
1933.972613	7203.372258	47.966989
1930.508380	7030.213829	47.971994
1927.164304	6850.660763	47.976999
1923.851426	6656.447621	47.982004
1920.375835	6478.650009	47.987009
1916.874520	6286.179340	47.992013
1913.421768	6106.669553	47.997018
1909.590312	5913.219557	48.002023
1906.377441	5735.600095	48.007028
1902.817899	5552.279888	48.012033
1899.148971	5356.689956	48.017037
1895.815841	5176.638917	48.022042
1892.495850	4988.603125	48.027047
1888.947037	4799.035420	48.032052
1885.402498	4616.630534	48.037057
1881.940362	4429.271513	48.042061
1878.558585	4236.278455	48.047066
1874.849771	4049.930305	48.052071
1871.675242	3858.642986	48.057076
1867.634188	3667.436329	48.062081
1864.114518	3486.257238	48.067085
1860.187507	3298.827604	48.072090
1856.736125	3118.100355	48.077095
1853.350164	2936.060981	48.082100
1850.068443	2751.235217	48.087105
1846.560713	2559.346137	48.092109
1843.333984	2378.148158	48.097114
1839.926974	2204.039522	48.102119
1836.305543	2016.600728	48.107124
1832.406963	1842.208651	48.112129
1828.885793	1656.615271	48.117133
1825.017384	1477.994791	48.122138
1821.453296	1305.365441	48.127143
1817.991574	1118.964668	48.132148
1814.392219	954.374456	48.137153
1811.006812	783.481353	48.142157
1806.892664	618.889374	48.147162
1802.892648	458.558624	48.152167
1799.415958	298.843469	48.157172
1794.881694	152.428297	48.162177
1790.103344	37.057815	48.167181
1782.006300	28.340146	48.172186
1773.936649	43.337250	48.177191
1769.604096	44.496322	48.182196
1765.188155	49.945915	48.187201
1762.589599	41.772474	48.192205
1760.008844	42.619428	48.197210
1757.131544	51.741855	48.202215
1754.619534	47.607709	48.207220
1751.365603	53.106410	48.212225
1748.196420	46.237178	48.217229
1745.529500	42.412022	48.222234
1741.983448	48.896093	48.227239
1738.253215	44.936787	48.232244
1734.206748	48.537853	48.237249
1731.089751	52.009275	48.242253
1727.673540	56.229891	48.247258
1724.760662	45.697995	48.252263
1721.169646	45.064217	48.257268
1717.053009	54.285701	48.262273
1713.794405	46.509808	48.267277
1710.627793	45.154704	48.272282
1707.260945	48.196991	48.277287
1703.686960	49.566406	48.282292
1700.345530	52.164949	48.287297
1697.167829	48.312176	48.292301
1693.490541	51.206898	48.297306
1690.056272	45.201766	48.302311
1686.667860	41.438925	48.307316
1683.094662	48.857419	48.312321
1679.890732	46.527385	48.317325
1676.220517	44.536090	48.322330
1672.359114	42.350088	48.327335
1669.278759	47.464134	48.332340
1665.586733	55.306200	48.337345
1662.299621	44.753804	48.342349
1659.318205	50.757216	48.347354
1655.768913	55.403649	48.352359
1652.228665	46.839780	48.357364
1648.056627	54.136872	48.362369
1644.891618	53.300401	48.367373
1641.706531	52.074762	48.372378
1637.675771	47.890445	48.377383
1634.281257	42.470745	48.382388
1630.788319	45.077201	48.387393
1628.093870	42.676936	48.392397
1624.358545	44.327898	48.397402
1620.420497	46.045391	48.402407
1616.963790	49.715548	48.407412
1613.599235	41.253915	48.412417
1610.191328	49.573554	48.417421
1606.716138	47.320802	48.422426
1603.376813	50.978919	48.427431
1599.971663	46.769468	48.432436
1596.427040	53.180591	48.437441
1593.034722	49.038737	48.442445
1589.452272	41.860921	48.447450
1585.484606	51.834261	48.452455
1582.405868	42.018090	48.457460
1578.642363	46.346891	48.462465
1575.337444	45.633583	48.467469
1571.816825	41.613063	48.472474
1567.954191	51.816745	48.477479
1564.702967	37.841870	48.482484
1561.465974	41.319463	48.487489
1557.636035	43.133955	48.492493
1554.503628	47.269071	48.497498
1551.006881	48.072783	48.502503
1547.323650	46.842886	48.507508
1543.621425	60.827527	48.512513
1540.488745	50.804672	48.517517
1537.085194	47.623230	48.522522
1533.359492	47.994542	48.527527
1530.327154	43.293324	48.532532
1526.268555	39.910692	48.537537
1522.968257	41.563201	48.542541
1519.615811	44.343859	48.547546
1515.826913	60.253009	48.552551
1512.206556	50.325481	48.557556
1508.853232	40.087241	48.562561
1505.821023	49.673734	48.567565
1502.119853	53.091122	48.572570
1498.218745	49.079563	48.577575
1495.135245	44.902064	48.582580
1491.251258	50.550076	48.587585
1487.872854	42.331110	48.592589
1484.585177	45.455986	48.597594
1481.224130	44.213649	48.602599
1477.852546	37.803316	48.607604
1473.770277	44.507439	48.612609
1470.354710	42.065069	48.617613
1467.022483	32.032360	48.622618
1463.630382	44.655489	48.627623
1460.384518	45.274427	48.632628
1456.433829	41.783184	48.637633
1452.931035	38.987473	48.642637
1449.560076	34.412058	48.647642
1446.046444	37.977279	48.652647
1442.643624	36.010658	48.657652
1439.146300	38.295155	48.662657
1435.843325	39.011627	48.667661
1432.079311	36.725056	48.672666
1428.320832	42.511630	48.677671
1424.671061	38.767651	48.682676
1421.448491	41.534337	48.687681
1418.523511	39.625806	48.692685
1415.027168	36.012840	48.697690
1411.330100	45.709752	48.702695
1407.945540	40.759987	48.707700
1404.127653	47.476535	48.712705
1400.750566	44.230890	48.717709
1396.797631	34.561131	48.722714
1393.116016	34.299162	48.727719
1389.926109	35.342802	48.732724
1386.699232	43.491789	48.737729
1383.139384	41.015088	48.742733
1379.691288	35.385574	48.747738
1375.970947	50.575327	48.752743
1372.820361	35.689431	48.757748
1369.031147	39.041549	48.762753
1365.549519	31.430428	48.767757
1362.072524	39.283210	48.772762
1358.584137	44.562450	48.777767
1355.043247	37.957203	48.782772
1351.465121	38.593386	48.787777
1347.888699	31.196430	48.792781
1344.222954	37.645566	48.797786
1341.097970	44.630157	48.802791
1337.873185	32.856415	48.807796
1334.182429	38.739987	48.812801
1330.658602	25.187556	48.817805
1327.104934	32.150668	48.822810
1323.909573	37.086649	48.827815
1320.242150	29.615365	48.832820
1316.492567	39.390125	48.837825
1313.194988	34.116731	48.842829
1309.623476	29.889144	48.847834
1305.825322	38.776158	48.852839
1302.607762	33.952155	48.857844
1299.194122	41.969047	48.862849
1295.784476	40.386366	48.867853
1292.215637	39.189280	48.872858
1288.570742	37.434619	48.877863
1285.118075	33.333971	48.882868
1281.488870	28.074540	48.887873
1278.044878	28.442975	48.892877
1274.735882	41.198671	48.897882
1270.995828	41.347697	48.902887
1267.489457	34.762394	48.907892
1264.094674	34.287890	48.912897
1260.240120	35.097095	48.917901
1256.865508	36.381667	48.922906
1253.569425	34.354112	48.927911
1250.427092	34.346298	48.932916
1246.533990	40.267904	48.937921
1243.169462	36.077542	48.942925
1239.626628	26.995403	48.947930
1235.949025	36.433047	48.952935
1232.725000	34.223374	48.957940
1228.967546	30.578592	48.962945
1225.612147	35.030285	48.967949
1222.037387	34.748488	48.972954
1218.265647	34.181152	48.977959
1215.266016	29.449616	48.982964
1211.854196	28.971470	48.987969
1207.842971	40.916455	48.992973
1204.155961	34.501829	48.997978
1200.644757	39.015888	49.002983
1197.723964	35.031324	49.007988
1194.305200	35.221831	49.012993
1190.420354	39.712130	49.017997
1186.844080	35.061389	49.023002
1183.466945	42.091824	49.028007
1180.166157	34.155072	49.033012
1176.633252	35.012031	49.038017
1173.368938	35.017011	49.043021
1169.925603	27.795452	49.048026
1165.813964	44.217114	49.053031
1162.528409	39.169687	49.058036
1158.923330	46.093447	49.063041
1155.305357	45.717198	49.068045
1152.033244	39.572998	49.073050
1148.252589	36.564640	49.078055
1144.796817	35.656795	49.083060
1141.537947	39.166412	49.088065
1138.191439	35.178916	49.093069
1134.965506	35.563882	49.098074
1130.937910	38.418727	49.103079
1127.828302	33.239363	49.108084
1124.163472	34.958563	49.113089
1120.072610	40.566322	49.118093
1117.196421	33.350902	49.123098
1113.252078	36.436331	49.128103
1110.039216	27.425976	49.133108
1106.453808	38.263437	49.138113
1103.033344	44.057311	49.143117
1099.883084	24.871909	49.148122
1095.967240	36.314770	49.153127
1092.191470	39.421271	49.158132
1088.651029	34.689030	49.163137
1085.599863	34.224065	49.168141
1082.044748	23.713890	49.173146
1078.112290	41.044000	49.178151
1075.057940	34.327894	49.183156
1071.538091	43.769365	49.188161
1067.901160	38.716877	49.193165
1064.526323	41.216444	49.198170
1060.990157	40.109243	49.203175
1057.725115	29.762469	49.208180
1053.988818	35.536202	49.213185
1050.203020	30.943634	49.218189
1046.801009	36.646048	49.223194
1042.929800	33.291241	49.228199
1039.860716	32.101426	49.233204
1036.124635	36.375498	49.238209
1033.166325	34.991169	49.243213
1030.010992	32.008340	49.248218
1026.044691	37.998432	49.253223
1022.312032	37.232063	49.258228
1018.593185	39.152751	49.263233
1015.081961	42.353903	49.268237
1012.141416	38.381986	49.273242
1008.603169	41.112803	49.278247
1004.890208	32.626885	49.283252
1001.204547	30.881885	49.288257
997.998850	39.976791	49.293261
994.321049	29.659871	49.298266
990.942828	40.515546	49.303271
987.631793	30.463907	49.308276
984.113546	34.131244	49.313281
980.358566	44.217005	49.318285
977.076631	35.353558	49.323290
973.191589	38.629075	49.328295
969.909835	34.378402	49.333300
966.355346	37.456629	49.338305
962.916936	45.085188	49.343309
959.296600	35.312945	49.348314
955.984483	38.375372	49.353319
952.725077	33.940871	49.358324
948.809687	43.263976	49.363329
945.180248	38.416013	49.368333
941.969423	41.873876	49.373338
938.278651	39.721572	49.378343
934.638272	39.899415	49.383348
931.311603	44.868727	49.388353
927.892878	44.480350	49.393357
924.554590	45.765676	49.398362
920.992722	40.641384	49.403367
917.611284	32.378845	49.408372
913.936988	37.804394	49.413377
909.932131	42.743864	49.418381
906.745241	38.228421	49.423386
903.194129	42.812103	49.428391
899.828460	34.626196	49.433396
896.699288	33.464821	49.438401
892.774936	30.577150	49.443405
889.085304	32.256028	49.448410
885.462246	34.892599	49.453415
882.099594	32.467475	49.458420
878.684537	37.184885	49.463425
875.418219	36.585999	49.468429
871.988196	30.109134	49.473434
868.325647	37.396326	49.478439
865.082726	38.151041	49.483444
861.081934	31.735083	49.488449
857.640669	31.435684	49.493453
854.464412	29.278779	49.498458
850.654662	41.749153	49.503463
847.420966	24.623910	49.508468
843.624442	28.996100	49.513473
840.321643	28.855360	49.518477
837.183472	31.178736	49.523482
833.089486	40.001494	49.528487
829.631192	30.792403	49.533492
826.535593	29.698562	49.538497
822.312532	37.864487	49.543501
819.214949	30.626899	49.548506
815.729807	30.378679	49.553511
812.101620	32.139714	49.558516
808.348131	35.745873	49.563521
805.224803	39.095163	49.568525
802.038643	31.276662	49.573530
798.349491	37.052593	49.578535
795.010200	32.159260	49.583540
791.421751	31.835477	49.588545
787.734112	36.696843	49.593549
784.368913	33.171160	49.598554
780.312967	44.705668	49.603559
777.097624	32.326413	49.608564
773.925784	45.415094	49.613569
770.244524	40.315891	49.618573
766.984147	37.393900	49.623578
763.458651	37.876524	49.628583
759.733457	30.626512	49.633588
755.932989	24.682278	49.638593
752.468291	34.823887	49.643597
749.095292	32.587097	49.648602
745.548026	27.735846	49.653607
742.055398	24.793290	49.658612
738.401535	28.491440	49.663617
734.957157	33.466589	49.668621
731.862151	33.682491	49.673626
728.556124	38.949191	49.678631
724.534309	30.106812	49.683636
721.365752	28.394841	49.688641
717.778356	29.035874	49.693645
714.619874	29.337653	49.698650
710.411985	26.943725	49.703655
706.923030	34.238584	49.708660
703.392958	31.789127	49.713665
699.925759	31.107868	49.718669
696.873107	32.914855	49.723674
693.167430	36.886895	49.728679
689.957219	19.207561	49.733684
686.245301	35.917935	49.738689
682.527318	28.749089	49.743693
679.427028	35.995744	49.748698
675.658660	27.436404	49.753703
672.105130	32.561547	49.758708
668.693112	29.321655	49.763713
664.653904	27.562560	49.768717
661.732944	19.215369	49.773722
658.163968	26.468989	49.778727
654.653938	25.250286	49.783732
651.292088	26.827300	49.788737
647.205528	31.846104	49.793741
643.942913	26.665577	49.798746
640.179566	26.619184	49.803751
637.367827	16.954587	49.808756
633.378469	30.778769	49.813761
630.090448	42.446160	49.818765
626.750909	21.743559	49.823770
623.055998	30.453267	49.828775
619.893353	23.156350	49.833780
616.472608	20.664498	49.838785
612.860539	33.562725	49.843789
609.278802	24.214884	49.848794
605.287061	30.595096	49.853799
602.122904	35.491600	49.858804
598.490119	30.337429	49.863809
594.697722	32.687416	49.868813
591.577173	27.054387	49.873818
587.849552	29.153784	49.878823
584.654398	24.769479	49.883828
580.743238	28.182116	49.888833
577.261477	32.299463	49.893837
573.705907	25.450083	49.898842
570.420297	25.022009	49.903847
567.005447	27.714674	49.908852
563.635107	26.015382	49.913857
560.056840	36.450083	49.918861
556.812828	28.109233	49.923866
552.821081	36.178921	49.928871
549.207318	26.181222	49.933876
546.135784	26.301761	49.938881
541.911066	27.928538	49.943885
539.272913	23.703784	49.948890
535.658718	29.686365	49.953895
532.241506	31.205654	49.958900
528.787902	40.051611	49.963905
524.844399	32.740989	49.968909
521.864967	33.229926	49.973914
517.755925	35.866822	49.978919
514.029546	35.251540	49.983924
510.744861	34.737920	49.988929
507.151895	30.260927	49.993933
504.022114	28.653694	49.998938
500.652268	34.775188	50.003943
497.067666	27.477971	50.008948
493.641829	41.777093	50.013953
489.722767	44.165945	50.018957
486.268033	31.606020	50.023962
482.778066	32.241376	50.028967
479.517915	34.210648	50.033972
475.930248	37.037983	50.038977
472.622510	34.462047	50.043981
468.809015	28.374453	50.048986
465.153484	30.835932	50.053991
461.861209	34.664211	50.058996
458.634383	37.517290	50.064001
455.008258	39.572370	50.069005
451.519211	32.595564	50.074010
447.730942	38.336524	50.079015
444.347888	29.381583	50.084020
440.981115	31.608016	50.089025
437.262347	28.337173	50.094029
433.946549	25.772007	50.099034
430.213532	27.840674	50.104039
426.658125	29.612603	50.109044
423.449692	24.123122	50.114049
419.796303	30.643396	50.119053
416.580513	31.925532	50.124058
412.636602	31.635432	50.129063
409.232719	29.447907	50.134068
406.011248	31.907857	50.139073
402.316654	36.830564	50.144077
398.799787	27.630849	50.149082
395.238029	31.422267	50.154087
391.740310	24.358265	50.159092
388.263746	24.308184	50.164097
384.755878	31.988924	50.169101
381.656770	35.872394	50.174106
377.847215	35.096190	50.179111
374.135397	34.921613	50.184116
371.000445	25.753838	50.189121
367.299283	30.089124	50.194125
363.928616	25.767200	50.199130
360.309754	28.599464	50.204135
357.115020	31.602574	50.209140
353.355735	32.628181	50.214145
349.577407	31.071976	50.219149
346.389849	26.730866	50.224154
342.753325	36.320544	50.229159
339.227028	30.074127	50.234164
335.807501	22.839714	50.239169
332.019863	34.136188	50.244173
328.920002	26.367645	50.249178
325.243721	21.185612	50.254183
321.456094	28.356537	50.259188
317.936046	25.842396	50.264193
314.685178	36.184757	50.269197
311.676328	24.766799	50.274202
307.875713	35.242735	50.279207
304.229774	33.520278	50.284212
301.128217	28.305170	50.289217
297.255829	25.757647	50.294221
293.999970	20.351580	50.299226
290.073656	27.158263	50.304231
286.041042	27.261768	50.309236
283.046472	30.682801	50.314241
279.410541	39.715585	50.319245
276.590398	17.859301	50.324250
272.955874	37.632839	50.329255
269.167091	29.810891	50.334260
265.619515	24.972555	50.339265
261.679128	40.450168	50.344269
258.165554	36.153837	50.349274
255.491641	37.635879	50.354279
251.940238	34.291443	50.359284
248.166864	32.965461	50.364289
244.879725	39.371477	50.369293
241.349683	28.256660	50.374298
237.313624	33.824545	50.379303
234.140662	34.002210	50.384308
230.483073	35.575086	50.389313
227.255817	32.075476	50.394317
223.858801	39.121973	50.399322
220.278529	32.842936	50.404327
216.781405	37.279195	50.409332
213.406099	29.604472	50.414337
209.446609	28.937253	50.419341
206.055598	27.380546	50.424346
202.483678	31.455203	50.429351
199.282337	32.001159	50.434356
195.935996	33.968215	50.439361
192.072508	29.808991	50.444365
188.445831	27.150257	50.449370
184.819384	34.469990	50.454375
181.576960	33.845470	50.459380
178.137894	33.223284	50.464385
174.427352	31.631227	50.469389
171.181270	24.505756	50.474394
167.750650	29.675096	50.479399
164.531766	24.816948	50.484404
160.531769	27.534993	50.489409
156.815380	33.587505	50.494413
153.476782	24.530824	50.499418
149.946112	32.363912	50.504423
146.733545	25.973520	50.509428
143.438721	29.710557	50.514433
139.828776	27.371927	50.519437
136.264576	29.376300	50.524442
132.255229	21.272605	50.529447
128.911415	28.858124	50.534452
125.442591	20.954487	50.539457
122.065860	30.883183	50.544461
118.933563	26.005160	50.549466
115.113065	30.963518	50.554471
111.623155	26.894501	50.559476
108.302474	16.382873	50.564481
104.444788	33.492727	50.569485
100.588725	16.617243	50.574490
97.335293	20.651530	50.579495
93.569434	23.158914	50.584500
90.133662	31.502337	50.589505
86.871719	29.957094	50.594509
83.793893	23.026764	50.599514
80.170270	25.809262	50.604519
76.664655	25.662617	50.609524
72.877176	25.022296	50.614529
69.392015	28.630991	50.619533
66.338878	18.137576	50.624538
62.667222	24.334972	50.629543
59.119516	20.420567	50.634548
55.583817	31.658676	50.639553
52.047452	29.343357	50.644557
48.697941	24.701876	50.649562
44.862083	28.833765	50.654567
41.005899	31.731811	50.659572
38.111098	22.865078	50.664577
34.676141	33.043371	50.669581
31.184762	29.661153	50.674586
27.399204	29.745052	50.679591
24.229009	33.813780	50.684596
20.975826	19.969672	50.689601
16.798511	37.351099	50.694605
13.558210	20.081791	50.699610
10.230214	26.494280	50.704615
6.048447	31.154947	50.709620
2.614678	23.157288	50.714625