Thu Aug 25 09:52:53 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.766610	102.368575	0.000000
1.685885	99.075218	0.005005
1.764041	106.709920	0.010010
1.788119	96.427205	0.015014
1.550659	91.854937	0.020019
1.256389	87.266260	0.025024
1.523491	81.071022	0.030029
1.187246	80.459445	0.035034
1.099887	65.135356	0.040038
0.829301	55.847960	0.045043
0.384235	47.752170	0.050048
0.173845	32.352473	0.055053
-0.051524	28.686323	0.060058
-0.557652	13.861326	0.065062
-0.844288	14.596062	0.070067
-1.303906	4.737200	0.075072
-1.576293	4.204205	0.080077
-1.906580	7.337573	0.085082
-2.642349	-0.586097	0.090086
-3.220118	2.244363	0.095091
-3.044223	2.856008	0.100096
-3.015323	7.799709	0.105101
-3.350663	5.394148	0.110106
-3.129199	2.771631	0.115110
-3.547272	1.600240	0.120115
-4.071904	-4.284256	0.125120
-4.389486	-2.538600	0.130125
-4.838121	0.815791	0.135130
-4.787160	1.943719	0.140134
-4.989009	10.425844	0.145139
-5.567973	9.229041	0.150144
-5.934363	2.680672	0.155149
-6.288201	5.548812	0.160154
-6.129310	-1.214736	0.165158
-6.705658	3.725720	0.170163
-6.689964	8.494321	0.175168
-6.751219	2.717553	0.180173
-6.425903	7.213014	0.185178
-6.981898	-3.465972	0.190182
-7.510466	6.687180	0.195187
-7.780398	0.832378	0.200192
-7.599821	-6.212975	0.205197
-8.482976	13.755895	0.210202
-8.584775	-2.265061	0.215206
-9.069103	8.390523	0.220211
-9.125886	1.603819	0.225216
-8.855970	4.333098	0.230221
-9.670949	4.375500	0.235226
-10.201599	2.842098	0.240230
-10.624453	13.193824	0.245235
-10.615474	8.880357	0.250240
-10.229889	9.667955	0.255245
-10.609318	9.278281	0.260250
-10.920017	-0.790571	0.265254
-11.302098	6.697900	0.270259
-12.079802	4.893161	0.275264
-11.995684	1.447444	0.280269
-12.275500	-4.779129	0.285274
-12.275921	-3.798173	0.290278
-12.300174	7.326324	0.295283
-12.926928	6.564115	0.300288
-13.092304	-0.642169	0.305293
-13.907676	0.222868	0.310298
-13.766006	0.874677	0.315302
-14.099099	1.945722	0.320307
-13.831648	12.375949	0.325312
-13.856655	-5.647033	0.330317
-14.557679	3.213856	0.335322
-14.991295	1.877222	0.340326
-14.860002	-3.303291	0.345331
-15.393868	1.839316	0.350336
-15.278432	0.286940	0.355341
-15.860803	5.108118	0.360346
-15.898342	-1.786002	0.365350
-16.105213	-2.319771	0.370355
-16.483863	1.330538	0.375360
-17.149552	-1.500987	0.380365
-17.387504	2.459470	0.385370
-17.469370	9.613003	0.390374
-17.254833	-4.483336	0.395379
-17.478431	3.787057	0.400384
-18.432960	-3.415800	0.405389
-19.226541	-1.924591	0.410394
-18.598150	-0.127839	0.415398
-18.968637	3.283910	0.420403
-19.399575	5.401668	0.425408
-19.354599	-8.734538	0.430413
-19.627903	6.981609	0.435418
-19.448104	-5.176237	0.440422
-19.760497	-1.109204	0.445427
-20.575983	-1.889296	0.450432
-20.365260	-4.076696	0.455437
-20.961496	0.420788	0.460442
-20.961335	-1.907626	0.465446
-21.635104	2.019877	0.470451
-22.092296	2.202372	0.475456
-22.200157	4.968696	0.480461
-22.704170	2.323811	0.485466
-22.557769	0.146489	0.490470
-22.413676	6.230071	0.495475
-22.134812	0.887230	0.500480
-22.561158	-4.022411	0.505485
-23.543232	6.613084	0.510490
-23.994864	-0.456598	0.515494
-23.808977	2.001109	0.520499
-24.282715	2.056482	0.525504
-24.039460	-9.893004	0.530509
-24.651303	0.330139	0.535514
-25.124094	-2.787872	0.540518
-25.625886	-5.999415	0.545523
-25.441723	2.260871	0.550528
-25.159719	3.276668	0.555533
-25.827083	6.212916	0.560538
-26.494137	4.460443	0.565542
-26.864832	7.460939	0.570547
-26.709354	2.988478	0.575552
-26.724122	-8.284668	0.580557
-27.140374	-1.205296	0.585562
-26.943986	-0.033716	0.590566
-27.501293	-7.324118	0.595571
-28.210139	-2.657131	0.600576
-28.160629	-8.498705	0.605581
-28.237553	3.355374	0.610586
-28.308176	-3.821462	0.615590
-28.645005	-11.950000	0.620595
-29.537099	-3.283802	0.625600
-29.840504	-2.581239	0.630605
-29.793754	1.382065	0.635610
-29.802212	-4.931317	0.640614
-29.910829	-3.218402	0.645619
-30.292082	-3.955800	0.650624
-30.694119	-7.284213	0.655629
-31.394402	0.434448	0.660634
-31.185265	7.181715	0.665638
-31.327824	1.965017	0.670643
-31.733785	7.774117	0.675648
-31.516323	2.159323	0.680653
-32.380204	4.376555	0.685658
-32.382752	5.107908	0.690662
-32.767471	5.310686	0.695667
-32.881884	10.688128	0.700672
-32.599596	-1.748368	0.705677
-33.732617	8.195774	0.710682
-34.016247	-2.772657	0.715686
-34.037215	6.288561	0.720691
-34.379580	5.608345	0.725696
-34.385214	3.508628	0.730701
-34.461480	5.048796	0.735706
-34.142920	-5.548917	0.740710
-34.953026	2.756426	0.745715
-35.615590	6.020952	0.750720
-35.539411	-4.931088	0.755725
-35.754538	-4.128462	0.760730
-36.212844	0.492942	0.765734
-36.695695	-3.670691	0.770739
-37.027356	5.331640	0.775744
-36.684220	-1.049488	0.780749
-37.263149	2.591074	0.785754
-37.030997	-4.978051	0.790758
-37.841634	0.340800	0.795763
-38.449671	0.037568	0.800768
-38.456886	-5.972288	0.805773
-38.504591	3.830270	0.810778
-38.558569	-0.830833	0.815782
-38.500992	2.482207	0.820787
-39.180714	6.647926	0.825792
-39.698533	8.554672	0.830797
-39.724348	6.303093	0.835802
-39.978094	-2.464887	0.840806
-40.021540	-3.321654	0.845811
-40.183112	4.420166	0.850816
-40.721266	5.415775	0.855821
-41.555313	11.497596	0.860826
-41.388235	2.021435	0.865830
-41.633556	-3.441751	0.870835
-42.238691	12.769317	0.875840
-41.767650	-5.714198	0.880845
-42.154672	6.419424	0.885850
-41.932873	6.255086	0.890854
-42.411281	9.525559	0.895859
-43.158800	5.906430	0.900864
-43.068091	4.044718	0.905869
-43.296768	4.738736	0.910874
-43.602309	4.182463	0.915878
-44.227972	0.370236	0.920883
-44.841305	9.843810	0.925888
-44.859452	-4.956384	0.930893
-45.027483	13.568495	0.935898
-45.361117	13.899310	0.940902
-44.761840	6.016394	0.945907
-45.639067	18.324909	0.950912
-44.766177	4.463931	0.955917
-45.650480	7.345587	0.960922
-46.165833	5.211843	0.965926
-46.043881	-0.618938	0.970931
-46.415334	17.691047	0.975936
-47.257446	-7.420405	0.980941
-47.399897	5.605036	0.985946
-48.154425	2.110392	0.990950
-47.549710	8.200892	0.995955
-48.090857	4.078030	1.000960
-48.138771	8.299775	1.005965
-48.292222	8.817492	1.010970
-48.573717	0.480965	1.015974
-49.347419	4.262777	1.020979
-49.741740	4.660048	1.025984
-49.574662	3.744985	1.030989
-50.163696	10.952674	1.035994
-49.661959	5.846992	1.040998
-49.769515	11.033535	1.046003
-50.364830	14.515316	1.051008
-50.575665	8.480413	1.056013
-50.981210	6.895774	1.061018
-51.183712	8.632892	1.066022
-51.018204	-0.292530	1.071027
-51.659100	12.263688	1.076032
-52.020729	7.302777	1.081037
-52.435051	8.487791	1.086042
-52.405484	15.940239	1.091046
-52.541448	8.068122	1.096051
-52.923791	12.816833	1.101056
-53.079410	0.743179	1.106061
-53.672963	10.365514	1.111066
-54.177840	5.971213	1.116070
-54.409529	5.001574	1.121075
-54.249820	11.955902	1.126080
-53.857462	4.595789	1.131085
-54.409856	1.569346	1.136090
-54.916429	2.499897	1.141094
-55.496339	5.425607	1.146099
-55.784625	7.264751	1.151104
-55.315629	-0.977398	1.156109
-55.658116	3.806193	1.161114
-56.279883	2.998915	1.166118
-56.789621	-3.020787	1.171123
-57.243962	10.063017	1.176128
-57.036356	5.025570	1.181133
-56.876993	8.167637	1.186138
-56.926775	9.700492	1.191142
-57.781775	5.313596	1.196147
-58.410335	8.031795	1.201152
-58.423143	0.991433	1.206157
-58.442008	9.710637	1.211162
-58.347210	11.230328	1.216166
-58.640877	5.834828	1.221171
-59.983223	12.056406	1.226176
-59.999784	10.379180	1.231181
-60.045986	3.897705	1.236186
-59.930484	4.518812	1.241190
-60.367113	4.482952	1.246195
-60.160861	9.221692	1.251200
-60.040890	5.618497	1.256205
-60.588969	7.286377	1.261210
-60.973555	8.621756	1.266214
-61.173739	1.243759	1.271219
-62.338789	5.276717	1.276224
-62.412774	4.636707	1.281229
-62.224960	4.664354	1.286234
-62.713691	3.390142	1.291238
-62.702461	10.646144	1.296243
-63.033627	13.175377	1.301248
-63.001746	8.494492	1.306253
-63.204013	4.429263	1.311258
-63.620569	6.057552	1.316262
-63.992998	10.096029	1.321267
-64.426692	4.209943	1.326272
-63.825066	5.871681	1.331277
-64.665877	8.319419	1.336282
-65.358868	8.557846	1.341286
-65.420843	12.405310	1.346291
-65.464235	14.022584	1.351296
-65.378723	6.887720	1.356301
-65.525336	7.689103	1.361306
-66.569500	1.053954	1.366310
-66.923024	6.731451	1.371315
-66.867111	8.424914	1.376320
-66.966457	3.426072	1.381325
-67.006821	12.705464	1.386330
-67.310371	9.314164	1.391334
-68.189899	-2.076581	1.396339
-68.315651	4.156846	1.401344
-68.615365	1.027537	1.406349
-68.701537	2.689479	1.411354
-68.769162	3.908754	1.416358
-68.851785	3.614945	1.421363
-68.765184	4.373458	1.426368
-69.288820	4.999799	1.431373
-69.884860	1.050056	1.436378
-70.460392	6.025187	1.441382
-70.015417	-0.539576	1.446387
-70.115708	7.284390	1.451392
-70.421969	3.108906	1.456397
-70.882704	6.110856	1.461402
-71.453846	3.169609	1.466406
-71.290652	2.482944	1.471411
-71.810002	-3.092325	1.476416
-72.380119	-15.578742	1.481421
-72.667812	-7.801348	1.486426
-72.834099	-0.862384	1.491430
-72.842807	-2.382652	1.496435
-72.944250	0.246624	1.501440
-73.413657	-2.758019	1.506445
-73.011545	2.661871	1.511450
-73.511755	5.967398	1.516454
-73.499821	-4.901805	1.521459
-74.039733	-0.631444	1.526464
-74.316551	-7.956300	1.531469
-75.072485	0.789806	1.536474
-75.549956	-2.365433	1.541478
-75.694413	-3.076658	1.546483
-76.101789	6.608251	1.551488
-75.945930	-5.564821	1.556493
-75.752327	1.077307	1.561498
-76.167226	-0.768455	1.566502
-75.950223	-1.707160	1.571507
-76.472746	9.378349	1.576512
-76.958972	-4.978339	1.581517
-77.240533	-0.235932	1.586522
-77.459008	8.425962	1.591526
-77.487156	-1.149319	1.596531
-78.439771	-3.224035	1.601536
-78.954059	-8.594451	1.606541
-78.634889	-3.199532	1.611546
-78.727045	-3.276712	1.616550
-78.798703	0.657687	1.621555
-79.023116	-6.662725	1.626560
-78.981168	-9.193837	1.631565
-80.339206	-7.522429	1.636570
-80.577782	4.701824	1.641574
-80.269206	-6.011380	1.646579
-80.607738	3.596300	1.651584
-80.707005	1.881415	1.656589
-80.680340	-0.087320	1.661594
-81.520824	1.211927	1.666598
-81.935149	-4.971417	1.671603
-81.957848	0.274592	1.676608
-81.884611	-3.542740	1.681613
-82.062519	-4.849834	1.686618
-82.176920	3.131364	1.691622
-82.832028	1.883224	1.696627
-83.535907	0.668036	1.701632
-83.687224	-1.525910	1.706637
-83.771742	4.985793	1.711642
-83.777198	6.606614	1.716646
-83.901040	1.111740	1.721651
-84.130071	-4.461562	1.726656
-84.204764	-2.168671	1.731661
-84.711908	7.133239	1.736666
-85.145976	5.518270	1.741670
-84.853398	2.141130	1.746675
-85.604933	6.672443	1.751680
-86.188301	8.127555	1.756685
-86.645136	-1.310950	1.761690
-86.902705	-5.092264	1.766694
-86.429306	-1.502699	1.771699
-86.678721	1.124453	1.776704
-86.443546	-0.392901	1.781709
-86.919565	9.679250	1.786714
-87.783388	11.421916	1.791718
-87.641614	5.540573	1.796723
-87.880624	11.791749	1.801728
-87.939505	4.322009	1.806733
-88.279103	5.371930	1.811738
-89.155305	1.023163	1.816742
-89.152055	2.376865	1.821747
-89.525721	13.704805	1.826752
-89.564523	7.440470	1.831757
-89.875715	5.689189	1.836762
-90.065875	3.181791	1.841766
-91.074446	9.208703	1.846771
-90.855300	7.807754	1.851776
-90.972421	9.240429	1.856781
-91.113151	11.812588	1.861786
-91.541553	6.824179	1.866790
-91.189950	0.460707	1.871795
-91.584446	6.094004	1.876800
-91.989121	-2.843310	1.881805
-92.340028	7.550920	1.886810
-92.626613	4.384753	1.891814
-92.676829	3.162053	1.896819
-92.859351	7.458674	1.901824
-93.216792	3.066586	1.906829
-93.977987	9.193940	1.911834
-94.194910	6.004203	1.916838
-94.107022	0.093340	1.921843
-94.387909	7.395111	1.926848
-94.567846	2.238057	1.931853
-94.444620	7.730120	1.936858
-94.951450	12.814711	1.941862
-95.274896	7.300493	1.946867
-95.767347	6.349569	1.951872
-95.851100	8.340161	1.956877
-96.037797	2.564073	1.961882
-96.132984	3.850941	1.966886
-96.564012	1.134514	1.971891
-97.247889	10.163563	1.976896
-97.402536	-3.780008	1.981901
-97.500594	11.823255	1.986906
-97.933948	6.051013	1.991910
-97.544224	9.568270	1.996915
-97.522558	7.318897	2.006912
-97.751184	5.657039	2.016909
-97.865317	7.388957	2.026906
-97.089163	14.429982	2.036902
-96.453663	10.751049	2.046899
-96.123437	18.748934	2.056896
-95.342318	11.369370	2.066893
-95.004461	6.897611	2.076890
-93.846878	5.981552	2.086886
-93.667919	8.820622	2.096883
-93.506410	4.930860	2.106880
-93.081285	11.326807	2.116877
-92.129450	8.222362	2.126874
-92.030387	10.351694	2.136870
-91.377297	3.499043	2.146867
-90.867776	4.404645	2.156864
-90.372772	0.443620	2.166861
-89.670902	2.044508	2.176858
-89.132770	5.391165	2.186854
-88.919067	5.056995	2.196851
-88.162887	3.836371	2.206848
-87.772392	4.624408	2.216845
-87.622379	0.993040	2.226842
-87.232277	1.496038	2.236838
-86.503833	2.760143	2.246835
-85.653907	10.625907	2.256832
-85.263639	3.294919	2.266829
-85.080045	0.314023	2.276826
-84.175449	3.356170	2.286822
-83.899478	4.244515	2.296819
-83.283172	7.065741	2.306816
-82.483982	7.422276	2.316813
-82.270551	13.654992	2.326810
-82.106147	6.140815	2.336806
-81.534193	5.832873	2.346803
-80.856132	5.973971	2.356800
-79.790931	7.587620	2.366797
-79.546015	5.148310	2.376794
-79.484006	7.793464	2.386790
-79.164054	-0.296279	2.396787
-78.225072	7.850136	2.406784
-77.988108	1.360461	2.416781
-77.384764	6.325149	2.426778
-76.394087	4.662303	2.436774
-76.299232	-0.227541	2.446771
-76.149662	8.416369	2.456768
-75.155304	6.486852	2.466765
-74.822855	7.321999	2.476762
-74.100887	8.111951	2.486758
-73.706818	11.465346	2.496755
-73.528410	18.663394	2.506752
-72.949412	1.957831	2.516749
-72.607010	10.793272	2.526746
-71.095957	4.306697	2.536742
-71.267972	8.461546	2.546739
-71.032605	15.270533	2.556736
-70.739531	16.539503	2.566733
-69.745542	8.321966	2.576730
-69.248686	14.928422	2.586726
-68.342801	9.103706	2.596723
-67.980361	11.571905	2.606720
-67.611005	9.008560	2.616717
-67.446777	8.096100	2.626714
-67.100007	9.286965	2.636710
-66.152285	6.509451	2.646707
-65.902610	6.819043	2.656704
-65.486728	12.291444	2.666701
-65.111461	7.788480	2.676698
-63.806172	15.918686	2.686694
-63.266033	7.240073	2.696691
-63.376128	12.015612	2.706688
-63.242613	10.512419	2.716685
-62.364458	13.419330	2.726682
-61.846524	11.387068	2.736678
-60.817011	16.338836	2.746675
-60.668983	16.718209	2.756672
-60.496983	8.854382	2.766669
-60.186823	13.114245	2.776666
-59.613149	14.861935	2.786662
-58.430449	10.061393	2.796659
-57.871126	11.332994	2.806656
-57.886729	12.976615	2.816653
-57.729226	7.072760	2.826650
-56.781811	13.155625	2.836646
-56.203068	5.858459	2.846643
-55.206265	2.677281	2.856640
-55.055994	7.161766	2.866637
-54.984145	8.170796	2.876634
-54.482308	5.320597	2.886630
-53.354860	5.065000	2.896627
-53.364287	9.808926	2.906624
-52.916838	11.437011	2.916621
-52.172309	6.543570	2.926618
-51.873482	2.160290	2.936614
-51.162414	14.403539	2.946611
-50.863491	11.762531	2.956608
-50.314175	10.986136	2.966605
-49.172517	12.191835	2.976602
-48.881669	6.390631	2.986598
-48.700535	10.971651	2.996595
-48.731969	5.642262	3.006592
-47.692939	2.001474	3.016589
-47.483690	5.301465	3.026586
-46.539328	8.362730	3.036582
-45.896896	5.743926	3.046579
-45.540937	14.605759	3.056576
-45.720675	6.904751	3.066573
-44.696917	9.801521	3.076570
-44.143716	7.944299	3.086566
-43.751138	6.460702	3.096563
-43.037825	8.265708	3.106560
-42.851421	14.337937	3.116557
-42.610939	6.691462	3.126554
-41.743374	3.277111	3.136550
-41.078224	3.119294	3.146547
-40.195978	6.199795	3.156544
-40.503308	4.052923	3.166541
-40.203369	1.988297	3.176538
-39.062294	7.483285	3.186534
-38.518423	4.141828	3.196531
-38.157069	9.968065	3.206528
-37.663608	10.863517	3.216525
-37.026789	11.159966	3.226522
-36.815278	8.668870	3.236518
-36.203988	13.667165	3.246515
-35.567373	13.307913	3.256512
-35.359318	14.941832	3.266509
-34.756868	10.583835	3.276506
-34.158193	11.849273	3.286502
-33.913779	7.737444	3.296499
-32.957728	13.093534	3.306496
-32.688607	10.013704	3.316493
-32.350364	16.147673	3.326490
-31.351229	8.547051	3.336486
-31.124608	2.679884	3.346483
-31.265233	10.311225	3.356480
-30.304890	9.901249	3.366477
-29.584431	9.747438	3.376474
-28.643560	7.300451	3.386470
-28.427121	9.782026	3.396467
-28.195036	2.653219	3.406464
-28.375803	0.841310	3.416461
-27.329634	8.470427	3.426458
-26.391282	6.790443	3.436454
-25.783145	5.494817	3.446451
-25.758677	4.908365	3.456448
-25.331535	7.996821	3.466445
-24.636365	4.580974	3.476442
-23.671909	-1.199062	3.486438
-23.587900	0.197701	3.496435
-23.434036	2.913994	3.506432
-22.587440	3.614731	3.516429
-21.977896	3.608180	3.526426
-21.737604	2.617279	3.536422
-21.467814	4.669177	3.546419
-20.745372	5.766336	3.556416
-20.122138	7.370048	3.566413
-18.950464	1.275611	3.576410
-19.017260	-2.030350	3.586406
-19.052671	3.588791	3.596403
-18.510807	6.089068	3.606400
-17.911125	1.360876	3.616397
-16.737864	8.219314	3.626394
-16.356724	5.467223	3.636390
-16.272982	2.251715	3.646387
-15.877802	8.341916	3.656384
-15.218882	3.648791	3.666381
-14.869459	10.240338	3.676378
-13.793293	-1.408123	3.686374
-13.509024	1.975150	3.696371
-13.277818	8.661247	3.706368
-12.957537	1.844904	3.716365
-12.151771	1.649218	3.726362
-11.744793	6.270880	3.736358
-11.059296	-3.247796	3.746355
-10.760709	-2.302803	3.756352
-10.096659	5.747318	3.766349
-9.069306	3.977363	3.776346
-9.337124	5.353225	3.786342
-9.164697	4.882973	3.796339
-8.077102	9.512036	3.806336
-7.499493	6.272998	3.816333
-6.785659	4.510986	3.826330
-6.396195	-0.038550	3.836326
-6.190929	-1.350245	3.846323
-6.250238	8.910298	3.856320
-5.391921	5.424539	3.866317
-4.367500	10.858618	3.876314
-3.807103	18.880637	3.886310
-3.556777	22.557502	3.896307
-3.467474	19.822625	3.906304
-3.037903	22.660449	3.916301
-2.642230	39.197996	3.926298
-1.949043	49.784152	3.936294
-1.487662	60.279922	3.946291
-1.472707	75.720906	3.956288
-0.832362	95.394316	3.966285
-0.421156	113.934726	3.976282
0.000000	128.355030	3.981286
0.297460	135.196078	3.986291
0.651696	159.916207	3.991296
1.080729	161.329760	3.996301
0.781756	176.012361	4.001306
1.038547	164.494073	4.006310
1.141096	171.368839	4.011315
0.917179	179.591907	4.016320
1.138510	171.027813	4.021325
0.864838	179.919906	4.026330
1.070256	175.952110	4.031334
1.116622	175.122391	4.036339
1.154637	186.708647	4.041344
1.044523	193.097882	4.046349
1.128736	198.048788	4.051354
1.543369	188.385040	4.056358
1.573047	197.349836	4.061363
1.382671	186.945645	4.066368
1.302210	176.264809	4.071373
1.241235	187.933015	4.076378
1.276363	178.493251	4.081382
1.062946	186.300223	4.086387
1.099225	191.065647	4.091392
1.552897	194.231240	4.096397
1.321128	187.070083	4.101402
1.368994	191.817873	4.106406
1.799854	191.725182	4.111411
1.399474	190.525695	4.116416
1.430914	195.320353	4.121421
1.512758	194.292084	4.126426
1.126116	187.057115	4.131430
1.282105	186.536089	4.136435
1.483635	200.206975	4.141440
1.682466	199.122411	4.146445
1.751838	196.450930	4.151450
1.619435	193.599090	4.156454
1.784744	205.098975	4.161459
1.668162	197.192095	4.166464
1.845401	180.329981	4.171469
1.384781	178.042102	4.176474
1.271536	178.256128	4.181478
1.200478	180.931291	4.186483
1.556127	188.677575	4.191488
1.876135	186.017445	4.196493
1.721494	197.197293	4.201498
1.577956	193.888450	4.206502
1.851947	189.353080	4.211507
1.368343	190.150323	4.216512
1.775026	182.879642	4.221517
1.539997	194.458064	4.226522
1.532835	196.057024	4.231526
1.423967	194.805534	4.236531
1.350274	207.038898	4.241536
1.199336	198.805204	4.246541
1.277548	199.251827	4.251546
1.581450	194.069522	4.256550
1.790830	214.338837	4.261555
1.691097	226.335847	4.266560
2.061287	217.438356	4.271565
1.849744	222.568488	4.276570
1.931454	221.378885	4.281574
2.181398	213.265873	4.286579
1.698683	204.565299	4.291584
1.626663	201.659704	4.296589
2.045992	218.839916	4.301594
1.921554	209.921850	4.306598
1.612183	208.948550	4.311603
1.744259	220.020212	4.316608
2.020675	216.208963	4.321613
2.050983	236.990420	4.326618
1.930337	233.567250	4.331622
2.253146	229.596868	4.336627
2.058958	230.889773	4.341632
2.027940	214.803746	4.346637
1.629863	213.714629	4.351642
2.175051	219.099520	4.356646
2.059333	229.833523	4.361651
1.927516	236.745034	4.366656
2.626559	229.447509	4.371661
1.919015	221.218757	4.376666
1.946532	217.993840	4.381670
2.208518	235.540409	4.386675
2.265333	224.534312	4.391680
1.925408	208.126528	4.396685
2.020648	230.261395	4.401690
2.024448	232.662242	4.406694
2.189277	231.614642	4.411699
1.949462	236.255656	4.416704
1.961932	229.464342	4.421709
1.830464	235.034353	4.426714
2.167461	232.273477	4.431718
2.298273	233.224393	4.436723
2.092893	230.314378	4.441728
2.101340	228.566772	4.446733
2.221671	223.675816	4.451738
2.275951	224.173645	4.456742
2.283493	226.380915	4.461747
2.244297	229.867350	4.466752
2.310655	221.216781	4.471757
2.222394	234.926771	4.476762
2.184368	229.643005	4.481766
2.662026	235.655420	4.486771
2.150813	238.494470	4.491776
2.454450	222.267416	4.496781
2.085308	232.345095	4.501786
2.241538	233.488182	4.506790
2.435312	222.577687	4.511795
2.284336	231.785943	4.516800
2.340175	224.019717	4.521805
2.311112	229.754017	4.526810
2.734205	233.405304	4.531814
2.363438	243.945157	4.536819
2.158748	246.944992	4.541824
2.291209	244.595817	4.546829
2.833389	256.644133	4.551834
2.306904	254.221029	4.556838
2.556665	254.621791	4.561843
2.374846	258.405829	4.566848
2.464491	250.137579	4.571853
2.547094	264.099234	4.576858
2.413328	251.968196	4.581862
2.506901	256.854376	4.586867
2.489510	262.615332	4.591872
2.898498	255.454992	4.596877
2.822250	263.363893	4.601882
2.603534	262.252998	4.606886
2.937164	258.511870	4.611891
3.221191	261.137737	4.616896
2.995576	255.171502	4.621901
2.715864	240.117849	4.626906
2.519162	232.286783	4.631910
2.814231	226.121915	4.636915
2.293644	225.194362	4.641920
2.861647	234.910071	4.646925
2.381016	245.837302	4.651930
2.615436	252.479463	4.656934
2.843235	244.274992	4.661939
2.528697	252.347776	4.666944
3.046841	257.793864	4.671949
2.482800	264.013798	4.676954
2.663678	257.670656	4.681958
2.979689	263.866597	4.686963
2.788392	262.378078	4.691968
3.144631	259.516106	4.696973
2.954479	260.669174	4.701978
2.698075	264.395295	4.706982
2.904863	248.041022	4.711987
2.780433	255.185503	4.716992
3.072364	252.080505	4.721997
3.105270	255.875191	4.727002
2.887911	257.412177	4.732006
3.069099	247.876724	4.737011
2.974551	244.569687	4.742016
3.109082	250.518809	4.747021
3.124440	258.533579	4.752026
3.172093	259.636732	4.757030
3.340893	254.507216	4.762035
2.964826	257.635145	4.767040
2.953421	261.284913	4.772045
2.981253	258.933147	4.777050
2.829787	254.540354	4.782054
2.816122	249.847557	4.787059
2.715315	262.490173	4.792064
3.168322	257.559738	4.797069
2.705147	260.375446	4.802074
3.066297	259.698885	4.807078
2.825965	254.864430	4.812083
2.896938	268.502040	4.817088
2.772242	272.748535	4.822093
2.647182	284.369897	4.827098
3.192310	273.372682	4.832102
3.364872	277.873164	4.837107
3.314609	288.913326	4.842112
3.569148	279.761838	4.847117
3.267371	279.034120	4.852122
3.436795	293.026487	4.857126
3.566582	272.656741	4.862131
3.422261	274.128500	4.867136
3.240419	275.169534	4.872141
3.785577	277.621610	4.877146
3.361191	279.399845	4.882150
3.960523	274.063660	4.887155
3.424475	261.169895	4.892160
3.345302	259.920075	4.897165
2.974604	258.741243	4.902170
2.989110	252.379877	4.907174
3.151630	262.598900	4.912179
3.272903	272.549141	4.917184
3.428758	284.521964	4.922189
3.205963	277.631450	4.927194
3.518025	281.005911	4.932198
3.746523	284.485216	4.937203
3.282597	284.725715	4.942208
3.430986	275.394705	4.947213
3.422298	285.403282	4.952218
3.364930	286.639952	4.957222
3.347567	282.482408	4.962227
3.613125	276.163957	4.967232
3.547531	277.987218	4.972237
3.710959	283.817926	4.977242
3.319552	285.461280	4.982246
3.484871	282.578597	4.987251
3.349795	281.426121	4.992256
3.257227	275.018248	4.997261
3.356058	284.184227	5.002266
3.861742	294.830398	5.007270
3.760098	287.063509	5.012275
3.614493	281.882006	5.017280
3.334653	278.018692	5.022285
3.400064	302.781109	5.027290
3.770298	306.665323	5.032294
3.882636	303.398627	5.037299
3.466668	317.071440	5.042304
3.825531	313.253580	5.047309
3.696381	318.902349	5.052314
3.848065	316.702015	5.057318
4.141412	308.196175	5.062323
3.856570	317.979115	5.067328
3.870279	312.997271	5.072333
3.837727	314.559090	5.077338
3.556855	309.114030	5.082342
4.111283	314.469028	5.087347
3.575057	312.221452	5.092352
3.706450	310.938636	5.097357
3.815570	314.965006	5.102362
3.930063	321.540561	5.107366
4.194641	307.749350	5.112371
3.891939	314.444054	5.117376
4.030859	317.617856	5.122381
4.068095	308.465599	5.127386
3.964386	319.406585	5.132390
4.068909	309.471817	5.137395
3.738109	320.046582	5.142400
3.437041	313.611251	5.147405
3.416973	319.581455	5.152410
3.977014	319.712137	5.157414
3.731626	307.620697	5.162419
3.587939	312.325765	5.167424
3.834435	322.047602	5.172429
3.841122	332.183512	5.177434
4.038967	331.573665	5.182438
4.302117	336.290926	5.187443
4.574291	338.184659	5.192448
4.460021	333.798674	5.197453
3.926265	321.464500	5.202458
3.783229	316.934327	5.207462
4.100774	324.569580	5.212467
3.900361	340.666913	5.217472
4.039435	329.382102	5.222477
3.948468	335.638672	5.227482
4.376254	333.556429	5.232486
4.374893	337.916495	5.237491
4.306523	345.934932	5.242496
4.498229	339.808367	5.247501
4.085775	339.161263	5.252506
4.316227	342.377677	5.257510
4.488509	341.866749	5.262515
4.429169	347.045836	5.267520
4.315837	338.426529	5.272525
4.530957	332.856291	5.277530
4.341168	332.636215	5.282534
4.533538	336.760280	5.287539
4.451859	342.237100	5.292544
4.513518	336.124584	5.297549
4.205234	325.893813	5.302554
3.746894	331.470775	5.307558
4.262864	330.121374	5.312563
4.127480	334.087980	5.317568
4.463396	330.495178	5.322573
4.524723	333.409054	5.327578
4.449585	343.383781	5.332582
4.572239	332.351482	5.337587
4.222661	347.032661	5.342592
4.268429	339.897561	5.347597
4.336184	343.677314	5.352602
4.565571	339.376690	5.357606
4.263795	338.857780	5.362611
4.213125	350.499167	5.367616
4.249067	345.219596	5.372621
4.306820	351.851509	5.377626
4.377372	365.046326	5.382630
4.721896	363.106842	5.387635
4.593345	374.418756	5.392640
4.369118	359.669526	5.397645
4.901200	366.837741	5.402650
4.739423	364.411263	5.407654
4.951990	367.807658	5.412659
4.661097	370.178765	5.417664
5.000699	360.504535	5.422669
4.982549	354.917055	5.427674
4.564304	349.553619	5.432678
4.397515	337.854810	5.437683
4.499965	354.793732	5.442688
4.608521	359.304263	5.447693
4.708791	364.736763	5.452698
4.914318	372.136483	5.457702
4.713282	363.749207	5.462707
4.768259	383.008340	5.467712
4.869778	364.072963	5.472717
4.836501	371.158916	5.477722
4.662393	373.239638	5.482726
4.902991	364.742036	5.487731
4.584929	368.278519	5.492736
4.507867	363.662066	5.497741
5.010695	370.806392	5.502746
4.980929	365.081521	5.507750
4.755884	362.902242	5.512755
4.644461	367.830064	5.517760
4.722687	362.031325	5.522765
5.014650	366.373914	5.527770
4.800782	367.998949	5.532774
4.776396	368.237020	5.537779
4.767920	372.677305	5.542784
5.110649	375.401561	5.547789
4.795475	363.725985	5.552794
4.407084	385.063608	5.557798
5.103222	392.598441	5.562803
4.894420	394.168900	5.567808
4.815213	393.627771	5.572813
4.959406	396.977935	5.577818
5.181174	392.479172	5.582822
5.269202	389.377623	5.587827
4.817197	392.140980	5.592832
4.718049	403.394521	5.597837
5.124300	399.145266	5.602842
5.294734	404.475034	5.607846
5.470302	395.247273	5.612851
5.523099	396.998211	5.617856
5.054338	394.464801	5.622861
5.273783	389.036241	5.627866
5.179607	394.420120	5.632870
5.287600	392.982775	5.637875
5.183075	393.976899	5.642880
5.234880	388.919461	5.647885
5.141657	393.040828	5.652890
5.096547	399.777463	5.657894
5.304149	398.954109	5.662899
5.454695	399.247031	5.667904
5.678644	389.745933	5.672909
5.172241	398.171553	5.677914
5.118917	397.107502	5.682918
5.395241	391.989574	5.687923
5.350057	402.092521	5.692928
5.306547	397.910573	5.697933
5.206975	390.070546	5.702938
5.273365	395.081249	5.707942
5.572559	393.322874	5.712947
5.298901	395.099651	5.717952
5.340342	395.118597	5.722957
5.296967	399.887066	5.727962
5.069019	400.511380	5.732966
5.630557	404.305529	5.737971
5.356005	407.870005	5.742976
5.618680	411.182625	5.747981
5.771695	414.686437	5.752986
5.344275	412.016831	5.757990
5.430031	410.029300	5.762995
5.586166	421.872454	5.768000
5.670213	420.299650	5.773005
6.148990	408.654673	5.778010
5.377761	396.335508	5.783014
5.762904	394.424458	5.788019
5.684150	407.342138	5.793024
5.621211	393.133932	5.798029
5.658734	396.700130	5.803034
5.696884	400.943288	5.808038
5.445236	398.793483	5.813043
5.273639	404.426782	5.818048
5.654106	415.083153	5.823053
6.074450	420.389588	5.828058
5.601208	409.662584	5.833062
5.490396	411.008879	5.838067
5.954019	420.665112	5.843072
6.021780	426.792438	5.848077
5.640541	419.455285	5.853082
5.882839	407.989733	5.858086
5.867896	397.276352	5.863091
5.763196	402.908660	5.868096
5.942075	400.568011	5.873101
5.594186	404.362280	5.878106
5.734475	410.592133	5.883110
5.994829	411.899256	5.888115
5.556521	421.573417	5.893120
5.983189	424.306676	5.898125
6.180713	433.134559	5.903130
5.955892	424.716179	5.908134
5.874340	412.997638	5.913139
6.025286	416.565052	5.918144
5.957769	412.798158	5.923149
6.165500	407.216400	5.928154
5.459077	402.508717	5.933158
6.137522	412.846311	5.938163
5.824450	431.270966	5.943168
6.127783	430.669898	5.948173
6.083833	429.727766	5.953178
5.889672	441.894743	5.958182
6.285143	430.908225	5.963187
5.960463	436.739530	5.968192
6.088859	426.873724	5.973197
6.041424	430.541827	5.978202
6.281324	429.447651	5.983206
6.144933	424.489293	5.988211
5.797577	423.787693	5.993216
5.942641	430.972279	5.998221
5.999620	430.147214	6.003226
5.925621	436.556187	6.008230
6.115377	428.759398	6.013235
6.001396	436.443329	6.018240
5.969365	434.388827	6.023245
6.088102	424.973798	6.028250
5.993634	435.226858	6.033254
6.340549	424.652921	6.038259
5.873918	433.078653	6.043264
6.100657	430.217962	6.048269
6.063404	426.386210	6.053274
6.024855	429.435976	6.058278
6.263629	419.445310	6.063283
6.112754	422.227929	6.068288
6.154489	426.375616	6.073293
6.119552	428.203580	6.078298
5.558482	433.182888	6.083302
5.925171	420.150729	6.088307
6.013530	429.036843	6.093312
5.875036	432.573678	6.098317
6.231674	430.426641	6.103322
5.692264	436.680741	6.108326
5.783023	430.259907	6.113331
6.084297	433.563319	6.118336
6.226966	424.312224	6.123341
6.157049	424.702966	6.128346
5.761936	436.749562	6.133350
6.084129	432.522961	6.138355
6.056072	433.884766	6.143360
6.047024	426.818332	6.148365
6.040984	428.315895	6.153370
6.076317	435.188638	6.158374
5.795872	429.955450	6.163379
6.064091	442.334725	6.168384
6.024601	449.197051	6.173389
6.467573	454.702436	6.178394
6.245343	452.250616	6.183398
6.218276	426.976029	6.188403
6.021670	435.884649	6.193408
5.920911	434.919779	6.198413
5.948329	434.469512	6.203418
5.754599	445.987841	6.208422
6.045655	440.567028	6.213427
5.949667	447.858993	6.218432
5.907070	444.423554	6.223437
6.082280	453.495393	6.228442
5.969608	458.562644	6.233446
6.286258	453.413069	6.238451
5.897671	451.123359	6.243456
6.012801	457.069262	6.248461
6.351892	450.777195	6.253466
6.203145	453.379148	6.258470
6.544580	455.265205	6.263475
6.165359	455.682263	6.268480
6.124360	448.193710	6.273485
6.187495	441.704433	6.278490
5.527592	446.661264	6.283494
6.066330	449.313691	6.288499
6.176810	458.126749	6.293504
6.111789	462.661339	6.298509
6.514286	461.209483	6.303514
5.984636	448.371529	6.308518
6.055702	449.603906	6.313523
6.086836	454.585347	6.318528
6.204264	450.574327	6.323533
6.437432	441.074921	6.328538
6.047654	439.664942	6.333542
5.913167	431.542460	6.338547
5.594280	435.224621	6.343552
5.946073	453.485014	6.348557
6.061871	454.878065	6.353562
5.814386	461.342704	6.358566
6.310082	463.245722	6.363571
6.468059	456.181581	6.368576
6.357109	456.945757	6.373581
6.308615	443.864734	6.378586
6.075444	438.636792	6.383590
6.224735	432.437746	6.388595
5.890946	441.478597	6.393600
6.157559	437.130987	6.398605
6.053485	430.791301	6.403610
6.012450	434.094562	6.408614
6.075381	430.800782	6.413619
6.005392	426.401508	6.418624
5.932285	425.239313	6.423629
6.468054	444.768038	6.428634
6.135334	448.240393	6.433638
6.240180	437.232966	6.438643
6.260168	432.556995	6.443648
5.954151	433.440321	6.448653
6.027300	432.865827	6.453658
6.375404	429.562168	6.458662
5.933569	433.852064	6.463667
5.538829	433.575512	6.468672
5.572636	447.361454	6.473677
6.132544	444.983245	6.478682
5.717793	462.003305	6.483686
6.395318	453.598558	6.488691
6.294588	456.006322	6.493696
6.489371	453.593570	6.498701
6.815450	449.957992	6.503706
6.102411	438.752838	6.508710
6.304730	434.987955	6.513715
6.413673	426.934904	6.518720
6.091319	433.047423	6.523725
6.371026	435.316482	6.528730
6.191125	438.904099	6.533734
5.976766	430.787804	6.538739
6.010541	428.985590	6.543744
5.944347	434.149957	6.548749
6.459055	424.831078	6.553754
5.798630	435.761284	6.558758
6.110249	438.958671	6.563763
6.062872	431.360391	6.568768
5.924816	434.235918	6.573773
6.179532	434.170827	6.578778
6.108078	439.563815	6.583782
6.126814	433.749064	6.588787
5.784702	432.635344	6.593792
5.673861	431.896686	6.598797
5.873036	437.421281	6.603802
5.703996	431.294258	6.608806
5.919822	427.745564	6.613811
5.995107	434.691143	6.618816
6.178897	449.760246	6.623821
6.475558	445.996398	6.628826
6.238828	435.665765	6.633830
6.194610	433.970684	6.638835
6.335973	435.264814	6.643840
5.782966	444.270409	6.648845
6.380663	444.575531	6.653850
6.001460	436.595796	6.658854
5.818544	436.779611	6.663859
5.913955	437.780378	6.668864
6.159696	434.223831	6.673869
6.357749	426.555460	6.678874
6.135063	438.309280	6.683878
5.820167	434.008490	6.688883
6.092730	431.697451	6.693888
6.321440	430.684123	6.698893
5.979924	419.588454	6.703898
6.193941	430.378483	6.708902
6.142728	429.380540	6.713907
6.242227	434.427196	6.718912
6.403502	439.207903	6.723917
6.128315	429.889395	6.728922
6.143850	432.835773	6.733926
6.130233	433.404359	6.738931
6.110151	435.328075	6.743936
6.068667	436.527464	6.748941
6.167600	432.842056	6.753946
5.984073	440.679257	6.758950
6.205995	430.944331	6.763955
5.977245	435.529878	6.768960
5.804188	438.293829	6.773965
6.263356	435.634006	6.778970
5.938632	438.124321	6.783974
6.049808	438.040590	6.788979
6.036922	430.073066	6.793984
5.954103	436.113254	6.798989
6.255362	435.588443	6.803994
5.933918	437.306271	6.808998
6.058553	438.179070	6.814003
6.056099	433.791360	6.819008
6.266019	431.977365	6.824013
6.126414	437.093122	6.829018
6.048331	437.304806	6.834022
6.091953	434.890430	6.839027
6.144788	427.988310	6.844032
5.943941	433.157955	6.849037
5.973507	442.132384	6.854042
6.002246	431.320387	6.859046
6.189794	428.794874	6.864051
6.389105	431.048054	6.869056
5.957227	436.864517	6.874061
6.180736	427.385614	6.879066
6.183147	439.638852	6.884070
6.089616	437.299750	6.889075
6.091602	432.822757	6.894080
6.058457	433.210901	6.899085
6.073597	430.728220	6.904090
5.992260	441.950520	6.909094
6.020924	428.499907	6.914099
6.271598	439.521485	6.919104
6.250966	443.185392	6.924109
6.460305	436.961116	6.929114
5.964336	439.952836	6.934118
6.191087	432.352734	6.939123
6.222937	433.755773	6.944128
6.230543	438.408695	6.949133
6.225895	434.334546	6.954138
6.131548	434.912618	6.959142
6.459276	432.479038	6.964147
6.664303	434.664882	6.969152
6.052262	432.660128	6.974157
6.610993	416.342308	6.979162
6.009845	416.139227	6.984166
6.146744	409.208124	6.989171
5.910501	406.264950	6.994176
6.192942	406.711217	6.999181
6.229821	412.852867	7.004186
5.987978	417.465772	7.009190
5.983339	411.872993	7.014195
6.130669	415.811140	7.019200
5.880305	413.667460	7.024205
6.125815	409.715477	7.029210
5.607547	415.925127	7.034214
5.995963	433.626093	7.039219
6.386507	434.422426	7.044224
6.215301	439.274211	7.049229
6.224928	424.016876	7.054234
5.851363	422.344926	7.059238
6.328871	425.459369	7.064243
6.063460	425.105605	7.069248
5.964342	417.430014	7.074253
6.060919	420.170699	7.079258
5.842574	418.955328	7.084262
6.040522	424.147911	7.089267
6.325401	431.509911	7.094272
6.077855	434.665192	7.099277
6.373883	419.945131	7.104282
6.069890	417.208727	7.109286
6.124278	423.923453	7.114291
6.320463	420.634107	7.119296
5.896755	415.043712	7.124301
5.914442	405.321817	7.129306
6.251453	410.695091	7.134310
6.225981	414.606527	7.139315
6.110875	414.678476	7.144320
5.958203	423.842803	7.149325
5.944290	409.781930	7.154330
5.761095	424.459250	7.159334
5.919559	420.710732	7.164339
6.169975	430.102978	7.169344
5.911758	439.375601	7.174349
6.484559	436.299332	7.179354
5.896702	430.098723	7.184358
6.181745	430.914750	7.189363
5.930532	428.109962	7.194368
6.193961	431.201000	7.199373
6.314183	433.608944	7.204378
5.829551	424.649129	7.209382
5.976621	432.754074	7.214387
6.214022	430.654193	7.219392
6.017322	440.822032	7.224397
6.060938	442.495317	7.229402
6.154414	450.795333	7.234406
6.573962	432.822478	7.239411
6.087463	422.663867	7.244416
6.087566	413.805282	7.249421
6.462448	412.262842	7.254426
6.222307	420.118396	7.259430
5.820765	415.650848	7.264435
6.108499	409.154865	7.269440
5.843716	408.617501	7.274445
5.932018	403.680893	7.279450
6.082303	408.143769	7.284454
5.761074	409.861561	7.289459
6.012899	425.011734	7.294464
6.345200	434.660077	7.299469
6.517274	427.062217	7.304474
6.003509	409.684881	7.309478
6.041295	403.721619	7.314483
6.007353	404.631917	7.319488
5.947860	417.192238	7.324493
6.187926	403.544002	7.329498
5.731072	417.504878	7.334502
6.301074	425.385362	7.339507
6.180469	422.730958	7.344512
5.998418	423.329098	7.349517
6.272918	407.280452	7.354522
5.833706	413.828899	7.359526
5.887794	418.357471	7.364531
6.434268	415.617531	7.369536
6.439813	425.677741	7.374541
6.304861	413.768246	7.379546
6.229523	419.424434	7.384550
5.847987	416.541989	7.389555
5.912325	402.712475	7.394560
5.503108	412.954726	7.399565
6.305640	420.833577	7.404570
6.012256	435.259246	7.409574
5.980288	428.791201	7.414579
5.973786	427.567949	7.419584
6.172776	437.322604	7.424589
6.388697	432.941808	7.429594
6.395481	419.083333	7.434598
5.746881	412.582193	7.439603
6.134746	419.807828	7.444608
6.227785	424.263858	7.449613
5.870506	412.319594	7.454618
6.009353	427.433686	7.459622
6.137108	434.288785	7.464627
5.915792	425.721156	7.469632
6.397868	435.352359	7.474637
6.249988	423.353132	7.479642
6.333721	423.909629	7.484646
5.984149	410.486655	7.489651
6.249124	411.774070	7.494656
6.119182	415.787299	7.499661
6.040294	412.677097	7.504666
5.866407	412.169785	7.509670
5.812070	417.851157	7.514675
6.217276	412.263767	7.519680
5.886367	411.901282	7.524685
6.148266	413.980135	7.529690
5.870492	428.919055	7.534694
6.356625	433.436886	7.539699
6.400882	419.246666	7.544704
5.997195	407.490015	7.549709
6.054061	407.319878	7.554714
5.925659	409.111864	7.559718
5.800790	416.917717	7.564723
6.438584	427.296490	7.569728
6.106173	426.076845	7.574733
6.074466	419.301872	7.579738
6.180253	417.561143	7.584742
5.862613	419.392271	7.589747
6.295739	424.861224	7.594752
5.935341	423.013199	7.599757
6.085895	424.793117	7.604762
6.075891	416.635318	7.609766
6.009202	415.930873	7.614771
6.358037	423.599231	7.619776
5.692791	424.231950	7.624781
6.361786	437.174864	7.629786
6.204662	425.224541	7.634790
5.949012	425.720316	7.639795
5.992491	413.086823	7.644800
6.017755	437.096400	7.649805
6.597087	426.748644	7.654810
6.074406	428.061394	7.659814
5.856948	415.851606	7.664819
6.182926	416.917488	7.669824
5.819224	409.884482	7.674829
6.026999	417.935615	7.679834
6.307280	426.345559	7.684838
6.364567	420.831662	7.689843
6.116819	422.031730	7.694848
5.611568	418.504267	7.699853
5.957006	421.816577	7.704858
6.013786	431.466957	7.709862
6.547527	437.040374	7.714867
6.213133	417.274714	7.719872
6.025558	409.837618	7.724877
5.910468	414.380041	7.729882
5.959146	416.005073	7.734886
6.268769	425.552558	7.739891
6.137973	414.335288	7.744896
5.826174	425.283633	7.749901
6.319629	422.232453	7.754906
6.460615	421.707444	7.759910
5.945965	415.106220	7.764915
6.231058	407.031906	7.769920
5.845368	417.602673	7.774925
6.094972	404.389550	7.779930
6.303203	413.029080	7.784934
5.918425	403.765722	7.789939
6.085226	406.498565	7.794944
6.049518	418.017427	7.799949
6.284972	411.877655	7.804954
5.825142	410.776054	7.809958
5.859948	407.341149	7.814963
6.303620	420.664211	7.819968
6.028992	420.735843	7.824973
5.682786	413.231849	7.829978
5.898268	422.591599	7.834982
6.547727	434.297353	7.839987
6.323779	433.782065	7.844992
6.220293	420.905833	7.849997
6.213393	417.689436	7.855002
5.942949	409.607250	7.860006
6.237408	403.812583	7.865011
6.094056	405.486685	7.870016
6.105448	410.284542	7.875021
6.156107	406.663652	7.880026
5.869353	406.971306	7.885030
6.164111	410.228278	7.890035
5.959092	399.728179	7.895040
6.059054	401.060431	7.900045
5.954493	413.488603	7.905050
6.170718	399.923201	7.910054
5.922447	401.955434	7.915059
6.338301	411.951348	7.920064
5.937951	413.248094	7.925069
6.268765	406.571352	7.930074
6.155640	406.968864	7.935078
6.263573	399.649989	7.940083
6.281431	402.880741	7.945088
6.293483	410.219040	7.950093
6.556486	401.297122	7.955098
6.083319	403.070358	7.960102
6.265746	405.212282	7.965107
6.422067	396.316574	7.970112
6.027334	409.533704	7.975117
6.436199	406.922897	7.980122
6.176482	407.231666	7.985139
6.126016	408.221140	7.990157
6.155437	402.990741	7.995174
6.085139	416.483240	8.000192
6.245441	405.274280	8.005210
6.068333	413.601776	8.010227
6.158582	416.961260	8.015245
6.245562	406.110921	8.020262
6.269018	418.585204	8.025280
6.196326	409.277796	8.030298
6.017436	400.211090	8.035315
6.116354	407.618037	8.040333
6.199323	406.929836	8.045350
6.188307	422.476910	8.050368
6.232838	400.073716	8.055386
5.944126	402.561628	8.060403
5.962748	406.525614	8.065421
6.342525	417.457710	8.070438
6.180015	413.699558	8.075456
6.016508	415.571418	8.080474
6.253365	422.770570	8.085491
6.008799	413.957140	8.090509
6.449082	418.082275	8.095526
6.083354	423.826368	8.100544
6.156471	415.682674	8.105562
6.654303	412.925570	8.110579
6.292917	406.778121	8.115597
6.205426	412.096770	8.120614
5.652232	414.660837	8.125632
6.046770	402.487389	8.130650
6.045666	407.407500	8.135667
5.944756	407.912581	8.140685
6.411403	409.139762	8.145702
6.031569	403.317091	8.150720
5.809672	414.182514	8.155738
5.725980	415.110923	8.160755
6.055413	415.094148	8.165773
6.032675	419.225560	8.170790
6.484654	428.189785	8.175808
6.388589	424.351794	8.180826
6.649723	418.286680	8.185843
6.335729	405.466864	8.190861
6.743295	405.949079	8.195878
6.624877	409.603183	8.200896
6.094546	396.807802	8.205914
6.270835	402.814096	8.210931
5.893391	409.535147	8.215949
6.100340	394.853874	8.220966
6.321737	409.449355	8.225984
6.354848	402.826694	8.231002
6.434203	414.285532	8.236019
6.487848	410.225275	8.241037
6.534600	399.419111	8.246054
6.259394	401.627202	8.251072
6.463247	402.977608	8.256090
6.639648	391.649371	8.261107
6.266439	403.586203	8.266125
6.452520	408.186657	8.271142
6.114284	407.280435	8.276160
6.153692	406.457050	8.281178
6.383445	404.767569	8.286195
6.483297	415.866598	8.291213
6.436806	411.900923	8.296230
6.506115	406.238248	8.301248
6.251794	405.599738	8.306266
6.325397	412.736104	8.311283
6.323504	421.159224	8.316301
6.690084	416.355669	8.321318
6.589842	420.871603	8.326336
6.266658	414.027056	8.331354
6.598804	407.089301	8.336371
6.505057	410.591219	8.341389
6.417119	403.331128	8.346406
6.241228	409.010760	8.351424
6.555167	426.510823	8.356442
6.613413	422.228939	8.361459
6.458292	415.026705	8.366477
6.612630	410.827597	8.371494
6.393623	415.911238	8.376512
6.657362	416.611644	8.381530
6.776852	410.890613	8.386547
6.563315	411.662644	8.391565
6.509113	413.921314	8.396582
6.588936	415.035539	8.401600
6.240399	409.921161	8.406618
6.685719	411.031766	8.411635
6.366348	406.398804	8.416653
6.351259	412.555006	8.421670
6.292803	417.121195	8.426688
5.934693	420.888595	8.431706
6.261134	428.139983	8.436723
6.469440	430.635231	8.441741
6.875783	432.067519	8.446758
6.881144	447.154465	8.451776
6.516242	442.048953	8.456794
6.770957	439.411987	8.461811
6.596820	433.885275	8.466829
7.206997	439.126178	8.471846
6.642012	432.761316	8.476864
6.520164	425.310872	8.481882
6.472211	428.972874	8.486899
6.361632	440.688703	8.491917
6.512253	434.940696	8.496934
6.716579	436.414104	8.501952
6.947086	431.934817	8.506970
6.750935	435.790451	8.511987
6.499696	429.414301	8.517005
6.873998	424.565353	8.522022
6.860777	424.633824	8.527040
6.511850	423.293781	8.532058
6.619185	427.982317	8.537075
6.599475	437.392831	8.542093
6.769582	436.943436	8.547110
6.582904	432.545293	8.552128
6.760284	431.450986	8.557146
6.950532	429.000844	8.562163
6.696334	427.472393	8.567181
6.686768	432.636830	8.572199
6.583325	432.432264	8.577216
6.513480	436.463765	8.582234
6.847156	432.454299	8.587251
6.776222	437.167613	8.592269
7.066109	434.976409	8.597287
6.759983	430.158333	8.602304
6.588224	427.146385	8.607322
6.543610	428.620928	8.612339
6.791867	434.622268	8.617357
6.732293	432.867666	8.622375
6.868541	437.901962	8.627392
6.775686	432.775919	8.632410
7.127167	431.225150	8.637427
6.764869	440.373768	8.642445
6.774903	422.589663	8.647463
6.961615	423.576689	8.652480
7.093257	422.637868	8.657498
6.832548	409.323715	8.662515
6.770486	412.972145	8.667533
6.397065	402.449560	8.672551
6.452516	412.955952	8.677568
6.620365	427.929061	8.682586
7.060854	422.448061	8.687603
6.859037	436.137903	8.692621
6.691977	433.137841	8.697639
6.790112	436.764332	8.702656
6.786687	436.916473	8.707674
7.095617	426.365856	8.712691
6.856240	433.478686	8.717709
6.823299	427.219808	8.722727
7.041649	435.292852	8.727744
6.695693	435.495506	8.732762
6.809013	435.698783	8.737779
6.635297	446.010730	8.742797
6.882189	442.980520	8.747815
6.873928	440.400537	8.752832
6.537696	435.697627	8.757850
6.592600	432.539713	8.762867
6.601287	437.767562	8.767885
6.718633	441.040756	8.772903
6.936481	436.001727	8.777920
6.736185	448.574204	8.782938
6.927360	453.252766	8.787955
7.098230	460.900922	8.792973
6.994938	460.822562	8.797991
7.269773	455.373818	8.803008
6.933665	447.855952	8.808026
7.258808	435.677575	8.813043
6.813219	437.533675	8.818061
6.788660	441.671689	8.823079
6.647569	437.847061	8.828096
6.770999	459.962315	8.833114
6.624921	459.909594	8.838131
6.918061	461.264949	8.843149
7.186526	458.717343	8.848167
7.431292	462.077871	8.853184
7.336907	468.779839	8.858202
7.687741	459.970927	8.863219
7.210142	449.281603	8.868237
7.081940	437.429872	8.873255
7.333460	435.837962	8.878272
7.386511	441.734193	8.883290
7.036563	439.652707	8.888307
7.250655	437.208296	8.893325
7.238198	432.113836	8.898343
7.279919	437.358600	8.903360
7.218320	433.022909	8.908378
6.987896	433.564061	8.913395
7.083993	443.404550	8.918413
6.944346	441.826592	8.923431
6.967001	447.348897	8.928448
6.842189	439.195178	8.933466
6.980520	428.728093	8.938483
7.082312	425.897343	8.943501
7.293676	424.415865	8.948519
7.120439	430.562138	8.953536
7.138417	440.519005	8.958554
6.986762	434.297661	8.963571
6.576905	441.468762	8.968589
6.961877	455.700987	8.973607
7.223450	459.453351	8.978624
7.140605	465.957853	8.983642
7.347545	464.129932	8.988659
7.730071	467.431008	8.993677
7.054757	454.809778	8.998695
7.415059	457.218099	9.003712
7.077801	450.075947	9.008730
7.165818	456.613634	9.013747
7.301900	460.268897	9.018765
7.535072	457.092514	9.023783
7.374995	448.893825	9.028800
7.240879	454.002045	9.033818
7.211251	444.324959	9.038835
7.281072	439.564739	9.043853
6.903514	439.024431	9.048871
7.187685	450.833048	9.053888
6.838065	468.415030	9.058906
7.400528	465.360618	9.063923
7.243331	474.928391	9.068941
7.159430	474.562974	9.073959
7.466942	465.139162	9.078976
7.055896	468.056500	9.083994
6.913808	465.585843	9.089011
7.177728	461.221232	9.094029
7.054986	467.747764	9.099047
7.468974	459.667404	9.104064
7.058661	468.602657	9.109082
7.062550	468.457011	9.114099
7.522681	466.895528	9.119117
7.434590	470.633254	9.124135
7.432177	466.408200	9.129152
7.611075	462.492405	9.134170
7.541450	467.366465	9.139187
7.201169	471.402477	9.144205
7.382483	478.480968	9.149223
7.697408	473.265775	9.154240
7.313324	470.164012	9.159258
7.327970	460.694572	9.164275
7.326126	467.950077	9.169293
6.770866	466.942157	9.174311
7.404411	462.661641	9.179328
7.217032	478.056519	9.184346
7.662596	490.445781	9.189363
7.721967	487.763676	9.194381
7.506315	476.083410	9.199399
7.209605	471.465815	9.204416
7.411279	475.464250	9.209434
7.394989	478.890931	9.214451
7.550721	490.937446	9.219469
7.516796	491.353139	9.224487
7.999052	484.467573	9.229504
7.479365	474.330775	9.234522
7.414037	472.106862	9.239539
7.672023	466.780673	9.244557
6.973624	472.311822	9.249575
7.619867	486.477889	9.254592
7.906189	482.437962	9.259610
7.741312	472.075162	9.264627
7.726275	474.920986	9.269645
7.538840	470.324140	9.274663
7.525323	463.285890	9.279680
7.183198	467.372682	9.284698
7.316240	474.114756	9.289715
7.559500	477.494458	9.294733
7.667414	490.435234	9.299751
8.069680	483.985073	9.304768
7.650291	476.638031	9.309786
7.346986	472.378071	9.314803
7.642512	477.731400	9.319821
7.771667	476.635179	9.324839
7.416408	474.481938	9.329856
7.777696	488.607449	9.334874
7.410549	483.069937	9.339891
7.120620	477.722298	9.344909
7.656445	496.295336	9.349927
7.593081	498.056841	9.354944
7.500077	490.661811	9.359962
7.460860	496.313744	9.364979
7.849487	496.609583	9.369997
7.712788	502.178963	9.375015
7.833879	492.828526	9.380032
8.017450	494.324125	9.385050
7.658449	498.587136	9.390067
7.945332	501.764350	9.395085
7.644626	500.647117	9.400103
7.764838	503.320278	9.405120
7.745936	498.283613	9.410138
7.570555	499.305286	9.415155
7.490164	494.060509	9.420173
7.556241	495.290499	9.425191
7.637739	496.262457	9.430208
7.618610	500.232378	9.435226
7.289281	499.047047	9.440243
7.505736	495.084336	9.445261
7.820972	499.513101	9.450279
7.952734	498.763603	9.455296
8.034949	502.149608	9.460314
7.841612	505.506205	9.465331
7.862714	495.101630	9.470349
7.877034	503.178270	9.475367
8.025371	498.150115	9.480384
7.973788	496.239622	9.485402
7.653455	503.150572	9.490419
8.216005	495.223642	9.495437
8.090361	504.344680	9.500455
7.984654	499.473092	9.505472
8.048142	498.822653	9.510490
7.964405	514.169765	9.515507
7.860603	494.579391	9.520525
7.648773	497.282485	9.525543
7.928677	496.882157	9.530560
7.903681	498.044367	9.535578
7.938013	497.108166	9.540595
8.002987	494.983753	9.545613
7.525995	499.760706	9.550631
7.670759	492.896458	9.555648
7.621565	491.553628	9.560666
7.645869	501.477980	9.565683
7.920972	485.656191	9.570701
7.726631	493.588798	9.575719
7.934772	499.410256	9.580736
8.584565	509.691040	9.585754
7.732015	500.152328	9.590771
7.547422	491.155897	9.595789
7.763346	501.943307	9.600807
7.832966	511.059000	9.605824
8.015066	519.131450	9.610842
7.938572	527.477947	9.615859
8.170915	520.397997	9.620877
8.159557	519.093418	9.625895
8.256605	520.403763	9.630912
8.005523	517.347424	9.635930
8.283561	522.602523	9.640947
8.436093	514.746138	9.645965
7.938676	500.916745	9.650983
7.911798	502.634665	9.656000
7.894084	506.342437	9.661018
7.780649	525.051946	9.666035
7.995215	513.105434	9.671053
8.196278	522.819069	9.676071
7.811239	519.701668	9.681088
8.032166	526.044989	9.686106
8.058260	516.561103	9.691123
8.271327	518.948321	9.696141
8.235964	521.169339	9.701159
8.272961	515.972434	9.706176
8.412648	517.979835	9.711194
8.005675	521.729665	9.716211
8.077547	519.926057	9.721229
8.314430	519.377836	9.726247
8.427331	520.849797	9.731264
8.338193	522.829935	9.736282
8.108046	523.456253	9.741299
8.154383	525.244754	9.746317
8.057354	531.672608	9.751335
8.385292	528.878991	9.756352
8.255600	524.067958	9.761370
8.011995	532.576339	9.766387
8.510456	523.438155	9.771405
8.239849	528.419461	9.776423
7.793927	527.088297	9.781440
8.247913	524.558950	9.786458
8.409995	521.983823	9.791475
8.332381	522.945998	9.796493
8.200767	522.622770	9.801511
8.312204	525.095340	9.806528
8.376498	521.765526	9.811546
8.603889	528.227754	9.816563
8.608351	515.386365	9.821581
8.365580	526.501276	9.826599
8.310915	501.456339	9.831616
8.259148	495.850475	9.836634
8.086879	503.265239	9.841651
8.303850	515.381070	9.846669
8.599772	524.436066	9.851687
7.922576	523.485117	9.856704
8.331280	523.408586	9.861722
8.190321	525.949104	9.866739
8.219142	527.052392	9.871757
8.337698	520.848639	9.876775
8.316167	518.930279	9.881792
8.195763	517.573358	9.886810
8.139515	526.917062	9.891827
8.314063	526.356517	9.896845
8.028512	528.717721	9.901863
8.137999	529.530662	9.906880
8.070665	513.996028	9.911898
8.110220	538.330403	9.916915
8.640112	553.587715	9.921933
8.579398	547.270032	9.926951
8.370141	550.812167	9.931968
8.501329	543.940559	9.936986
8.645411	547.424175	9.942003
8.794565	554.236338	9.947021
8.713067	543.718423	9.952039
8.321917	528.439638	9.957056
8.767823	526.246069	9.962074
8.244212	528.445759	9.967091
8.211499	526.863662	9.972109
8.604470	546.061886	9.977127
8.517765	545.958836	9.982144
8.622050	548.621876	9.987162
8.657338	542.992890	9.992179
8.379642	540.764373	9.997197
8.492838	549.986866	10.002215
8.509515	537.310803	10.007232
8.574245	549.362149	10.012250
8.764564	554.687805	10.017267
8.693710	551.966136	10.022285
9.051658	552.244692	10.027303
8.313871	553.348176	10.032320
8.354293	551.353834	10.037338
8.376421	559.000091	10.042355
8.876873	557.003097	10.047373
8.836856	553.345643	10.052391
8.743355	556.140658	10.057408
8.848567	553.527100	10.062426
8.412358	544.529040	10.067443
8.231486	545.198130	10.072461
8.965343	540.696754	10.077479
8.303845	545.774024	10.082496
8.509648	538.095473	10.087514
8.470690	557.557042	10.092531
8.573867	551.529256	10.097549
8.475149	553.637130	10.102567
8.276424	546.167123	10.107584
8.887509	544.897559	10.112602
8.889434	551.672830	10.117619
8.448123	545.181253	10.122637
8.347110	544.392487	10.127655
8.803324	560.936281	10.132672
8.605172	567.291630	10.137690
9.022908	567.974226	10.142707
8.939652	571.237849	10.147725
9.157635	556.523157	10.152743
8.753924	560.162033	10.157760
8.602401	551.321334	10.162778
8.708736	549.029489	10.167795
8.487545	564.464452	10.172813
8.668398	565.837409	10.177831
8.748545	577.851644	10.182848
8.914546	576.206850	10.187866
9.000298	583.000556	10.192883
8.890176	576.476011	10.197901
9.335879	574.907312	10.202919
9.186503	571.181782	10.207936
8.539994	552.910285	10.212954
8.656897	559.635986	10.217971
9.035161	568.043793	10.222989
9.139396	568.242183	10.228007
8.986829	568.973110	10.233024
9.410106	561.569740	10.238042
9.191055	549.839466	10.243059
9.094414	538.594942	10.248077
9.007856	540.549432	10.253095
8.857171	547.569517	10.258112
8.896028	539.721464	10.263130
8.872551	539.343423	10.268147
8.626616	542.244370	10.273165
9.018509	534.088544	10.278183
8.697530	554.477914	10.283200
8.840135	566.690638	10.288218
8.903959	567.081550	10.293235
8.835878	570.790915	10.298253
9.159539	562.866672	10.303271
8.918257	569.506487	10.308288
9.007637	566.904876	10.313306
9.193221	569.937029	10.318323
9.031568	569.593260	10.323341
9.226272	566.362926	10.328359
9.002093	570.450196	10.333376
9.039211	565.224855	10.338394
9.284222	574.944256	10.343411
9.067370	572.289639	10.348429
9.317847	559.314998	10.353447
8.889290	571.582503	10.358464
9.072944	576.764044	10.363482
9.354478	576.101529	10.368499
9.257114	573.573356	10.373517
9.316581	570.916471	10.378535
9.371492	570.955333	10.383552
9.372874	575.821453	10.388570
9.087623	560.472400	10.393587
9.207609	568.945921	10.398605
9.003018	570.641199	10.403623
9.276050	572.012337	10.408640
9.111061	574.275762	10.413658
9.441111	568.543780	10.418675
9.193465	574.865862	10.423693
9.169691	572.941536	10.428711
8.973649	572.511637	10.433728
9.021573	577.326285	10.438746
9.250393	569.596777	10.443763
8.868959	580.865991	10.448781
8.902479	574.495664	10.453799
8.961354	576.443150	10.458816
9.046403	577.584967	10.463834
9.197205	570.836507	10.468851
9.057298	577.047036	10.473869
9.158019	566.734084	10.478887
9.186827	586.898273	10.483904
9.279498	580.922616	10.488922
9.407633	591.278870	10.493939
9.239645	595.477261	10.498957
9.288463	585.459607	10.503975
9.211699	591.350981	10.508992
9.480254	591.410017	10.514010
9.633953	588.277620	10.519027
9.119176	585.208937	10.524045
9.603219	590.154070	10.529063
9.554045	594.974469	10.534080
9.388434	595.701129	10.539098
9.834160	585.747518	10.544115
9.415210	596.123222	10.549133
9.696254	592.162992	10.554151
9.615678	580.653996	10.559168
9.328649	573.993069	10.564186
9.460578	573.123623	10.569203
9.225480	576.164887	10.574221
9.412103	577.120378	10.579239
9.571712	583.555377	10.584256
9.383512	584.121475	10.589274
9.918058	583.233127	10.594291
9.538817	580.916374	10.599309
9.708473	583.726966	10.604327
9.592043	578.055469	10.609344
9.441055	576.911617	10.614362
9.588556	563.078958	10.619379
9.242166	573.765169	10.624397
9.143622	574.241481	10.629415
9.366690	592.772106	10.634432
9.107634	587.053526	10.639450
9.464553	588.108566	10.644467
9.306212	589.266429	10.649485
9.465935	587.774094	10.654503
9.874131	595.776440	10.659520
9.806413	594.054655	10.664538
10.114649	597.948059	10.669555
9.726784	599.833001	10.674573
9.790240	590.482076	10.679591
9.656985	592.153557	10.684608
9.698023	592.563819	10.689626
9.273855	587.069923	10.694643
9.407978	594.859592	10.699661
9.522685	593.147094	10.704679
9.691595	594.026467	10.709696
9.479918	596.420286	10.714714
9.542655	593.851246	10.719731
9.242507	600.809564	10.724749
9.842400	609.097458	10.729767
10.092559	621.782514	10.734784
10.102460	608.542576	10.739802
9.663985	599.794150	10.744819
9.364558	602.315327	10.749837
9.561017	603.060996	10.754855
9.759164	609.199634	10.759872
9.802715	616.987726	10.764890
10.039091	618.314117	10.769907
9.753889	625.320595	10.774925
9.947715	618.499104	10.779943
9.721195	623.631318	10.784960
9.922182	619.383826	10.789978
10.052531	616.971447	10.794995
9.848035	619.973210	10.800013
9.834364	624.791209	10.805031
9.700859	628.460345	10.810048
9.896946	628.025810	10.815066
9.989153	627.042665	10.820083
9.962572	621.536956	10.825101
10.078663	626.041136	10.830119
9.951848	617.613097	10.835136
9.629043	628.393475	10.840154
9.893144	611.269959	10.845171
9.892248	618.553778	10.850189
10.209866	618.226433	10.855207
10.454018	627.955464	10.860224
10.300116	615.956163	10.865242
10.453387	598.925763	10.870259
10.171435	602.851680	10.875277
9.872231	595.302722	10.880295
9.976869	597.688006	10.885312
9.754752	602.141030	10.890330
9.625609	595.161870	10.895347
9.934445	613.253047	10.900365
9.693827	620.060034	10.905383
10.073570	626.798227	10.910400
10.410272	635.354588	10.915418
10.291992	622.901579	10.920435
10.099122	618.905145	10.925453
9.856878	604.369820	10.930471
10.057084	612.164922	10.935488
10.037152	614.320418	10.940506
9.953247	617.811368	10.945523
9.984926	622.395045	10.950541
10.109069	622.555602	10.955559
10.586062	626.207978	10.960576
10.071571	625.771169	10.965594
10.415973	624.701173	10.970611
9.834726	631.593093	10.975629
10.181328	629.118427	10.980647
9.966089	626.230021	10.985664
9.931539	634.522660	10.990682
10.324315	625.246350	10.995699
10.206801	627.944154	11.000717
10.117476	629.870685	11.005735
10.386610	623.214117	11.010752
10.048773	626.202060	11.015770
10.262425	621.435034	11.020787
10.129920	620.752184	11.025805
9.700679	626.256986	11.030823
9.782021	622.195496	11.035840
10.109136	630.463025	11.040858
10.693651	644.061380	11.045875
10.340658	631.591492	11.050893
10.129504	626.950985	11.055911
10.353389	632.728994	11.060928
10.349776	643.307892	11.065946
10.546898	645.722872	11.070963
10.478013	632.220707	11.075981
9.866440	628.760086	11.080999
10.481389	640.517002	11.086016
10.312404	644.141208	11.091034
10.418125	655.697055	11.096051
10.337706	655.422607	11.101069
10.442772	651.821295	11.106087
10.843248	644.897989	11.111104
10.539967	645.286462	11.116122
10.066333	638.629502	11.121139
10.450340	641.759966	11.126157
10.405594	649.271574	11.131175
10.614355	647.228755	11.136192
10.590452	654.118564	11.141210
10.656375	651.596354	11.146227
10.158670	652.873665	11.151245
10.549345	655.712754	11.156263
10.671098	643.973200	11.161280
10.684760	661.495296	11.166298
11.242054	639.286015	11.171315
10.801066	632.563982	11.176333
10.019375	626.933588	11.181351
10.321535	616.459659	11.186368
10.197442	638.519244	11.191386
10.383164	645.126897	11.196403
10.750065	651.030827	11.201421
10.452442	654.861381	11.206439
10.992249	650.513458	11.211456
10.645666	652.385626	11.216474
10.511337	647.651025	11.221491
10.784145	643.698386	11.226509
10.809643	654.228548	11.231527
10.849453	645.758609	11.236544
10.813942	648.916936	11.241562
10.600106	632.313250	11.246579
10.467218	640.308877	11.251597
10.498290	645.893040	11.256615
11.027712	644.352243	11.261632
10.693709	645.231521	11.266650
10.505293	644.516404	11.271667
10.616010	639.449923	11.276685
10.527169	640.192959	11.281703
11.055331	651.225026	11.286720
10.963193	652.574490	11.291738
11.033991	644.150189	11.296755
11.207341	637.436041	11.301773
10.699640	641.592996	11.306791
10.775453	627.203477	11.311808
10.698915	633.924801	11.316826
10.928322	637.000593	11.321843
10.809077	636.744852	11.326861
10.789282	642.690432	11.331879
11.060591	641.521435	11.336896
10.777404	646.634132	11.341914
10.727619	646.686242	11.346931
11.198631	647.332092	11.351949
10.661719	660.080534	11.356967
10.853000	651.293371	11.361984
11.175042	658.589724	11.367002
10.741077	653.435012	11.372019
10.756870	648.086757	11.377037
10.610356	647.617539	11.382055
10.764944	652.762631	11.387072
10.749678	651.786857	11.392090
11.126450	655.275061	11.397107
11.101777	650.015197	11.402125
10.723350	649.702235	11.407143
11.061620	645.073467	11.412160
10.974498	636.389892	11.417178
10.992945	641.348030	11.422195
11.000099	645.364358	11.427213
10.723223	641.276940	11.432231
10.885844	641.261056	11.437248
10.719188	641.511358	11.442266
10.961686	643.000893	11.447283
11.436023	647.477351	11.452301
11.096228	648.389094	11.457319
11.028522	639.371118	11.462336
11.172284	623.393061	11.467354
11.019354	638.536527	11.472371
10.897548	636.558127	11.477389
11.126349	655.176280	11.482407
11.444130	656.237457	11.487424
10.843692	653.598748	11.492442
11.032285	668.796026	11.497459
11.330682	667.988855	11.502477
11.360696	667.990593	11.507495
11.482220	661.202505	11.512512
11.294113	648.104015	11.517530
11.038848	644.208869	11.522547
11.306474	642.494497	11.527565
11.187670	658.036574	11.532583
11.448898	653.079050	11.537600
10.929882	645.646562	11.542618
10.944003	655.405338	11.547635
11.465891	657.813616	11.552653
11.407775	660.625194	11.557671
11.282709	666.236984	11.562688
11.185673	667.543035	11.567706
11.556060	661.132520	11.572723
11.827176	666.982035	11.577741
11.222010	656.902707	11.582759
10.937396	649.682799	11.587776
11.313448	664.875948	11.592794
11.299512	659.529192	11.597811
11.745797	655.309530	11.602829
11.293197	659.618801	11.607847
11.272989	663.181830	11.612864
11.233718	663.166021	11.617882
11.061033	664.351383	11.622899
11.499729	662.474506	11.627917
10.995033	666.823500	11.632935
11.273362	665.517702	11.637952
11.501289	664.497511	11.642970
11.228741	667.150184	11.647987
11.257087	658.511623	11.653005
11.325033	666.699855	11.658023
11.822515	673.864585	11.663040
11.245333	662.995076	11.668058
11.387992	674.889130	11.673075
11.370071	681.361447	11.678093
11.504579	684.748761	11.683111
11.614420	677.157769	11.688128
11.856871	689.651578	11.693146
12.046501	692.509550	11.698163
11.787024	674.581229	11.703181
11.436340	677.593284	11.708199
11.535411	677.641006	11.713216
11.603788	672.350776	11.718234
11.412094	674.766720	11.723251
11.894660	683.319185	11.728269
11.749280	682.505806	11.733287
11.884940	682.733987	11.738304
11.456271	672.544946	11.743322
11.435620	680.201113	11.748339
11.886211	688.970029	11.753357
11.924779	699.024800	11.758375
11.415334	686.563608	11.763392
11.775322	684.695905	11.768410
11.759927	696.169771	11.773427
12.072921	686.489364	11.778445
11.964805	688.141135	11.783463
11.538423	671.024763	11.788480
12.162403	680.984644	11.793498
11.645665	677.332430	11.798515
11.884066	661.781322	11.803533
11.766694	673.605665	11.808551
11.803357	676.348747	11.813568
11.738383	686.889947	11.818586
11.685574	692.133818	11.823603
12.055814	688.371031	11.828621
11.961982	692.892340	11.833639
11.900919	690.263789	11.838656
11.861359	696.386053	11.843674
11.854974	699.249492	11.848691
11.921091	692.703602	11.853709
12.197507	694.800053	11.858727
12.050246	687.694308	11.863744
11.962797	676.672319	11.868762
11.928841	683.134526	11.873779
12.313543	677.182508	11.878797
11.996332	675.269433	11.883815
11.689285	671.423420	11.888832
12.095977	660.841568	11.893850
11.757475	680.552176	11.898867
12.232813	678.540169	11.903885
12.179507	692.478337	11.908903
11.970135	687.689212	11.913920
12.114669	675.302286	11.918938
11.903979	686.838302	11.923955
12.367652	685.484528	11.928973
12.131859	685.417460	11.933991
11.986685	669.648735	11.939008
12.180289	673.541182	11.944026
11.818880	687.524464	11.949043
12.296626	686.897474	11.954061
12.350869	692.336010	11.959079
12.055484	692.969399	11.964096
12.679598	691.969182	11.969114
11.983517	685.987685	11.974131
12.040957	673.055831	11.979149
12.154740	685.598198	11.984167
11.751386	691.720656	11.989184
12.010988	689.587816	11.994202
11.846791	691.333581	11.999219
11.951588	685.277094	12.004237
12.071367	691.387014	12.009255
12.219626	699.995022	12.014272
12.279643	695.384593	12.019290
12.147836	691.804607	12.024307
12.118024	690.408233	12.029325
12.230412	695.689338	12.034343
12.097425	703.025445	12.039360
12.351619	716.842869	12.044378
12.437646	720.950997	12.049395
12.228493	718.503435	12.054413
12.186670	717.175213	12.059431
12.262509	724.762632	12.064448
12.365502	715.683158	12.069466
12.389996	720.738201	12.074483
12.482931	724.075231	12.079501
12.612205	717.828706	12.084519
12.657403	720.826077	12.089536
12.693787	718.567262	12.094554
12.677983	718.667696	12.099571
12.698434	707.426811	12.104589
12.306554	697.014241	12.109607
12.436948	695.797892	12.114624
12.944438	696.210811	12.119642
12.178376	699.515168	12.124659
12.165652	704.150005	12.129677
12.743933	707.770748	12.134695
12.486670	721.769297	12.139712
13.034891	721.137576	12.144730
12.727683	715.044647	12.149747
12.470663	705.030664	12.154765
12.448903	695.014539	12.159783
12.402871	713.224535	12.164800
12.646890	713.388401	12.169818
12.655085	722.166689	12.174835
12.714699	715.366189	12.179853
12.898486	719.648348	12.184871
12.870450	721.328601	12.189888
12.824604	705.588463	12.194906
12.480260	704.900931	12.199923
12.865327	702.925156	12.204941
12.760275	695.667627	12.209959
12.676815	700.190469	12.214976
12.514296	689.382205	12.219994
12.768887	707.112749	12.225011
12.506066	720.465229	12.230029
12.912067	712.979297	12.235047
12.671292	718.596609	12.240064
12.915114	716.160126	12.245082
12.909895	715.836025	12.250099
12.907555	711.465735	12.255117
12.848980	707.710170	12.260135
12.734221	728.420877	12.265152
12.895504	714.832093	12.270170
12.883955	714.335415	12.275187
12.816391	715.939810	12.280205
13.150518	712.330998	12.285223
12.659484	720.786718	12.290240
13.053790	714.877364	12.295258
12.640282	725.476352	12.300275
13.235121	711.384140	12.305293
12.824327	707.573309	12.310311
12.835757	715.227621	12.315328
12.737803	709.600524	12.320346
12.856195	718.487776	12.325363
12.818721	714.662632	12.330381
13.141878	716.098511	12.335399
12.788174	721.083422	12.340416
12.803967	714.239297	12.345434
12.679821	716.297525	12.350451
12.823611	719.512977	12.355469
12.969302	722.778626	12.360487
12.923739	739.196078	12.365504
13.177874	739.872757	12.370522
13.009329	744.538329	12.375539
13.197391	747.112533	12.380557
13.325866	737.331622	12.385575
13.101364	751.252478	12.390592
12.979923	741.482319	12.395610
13.316825	745.156669	12.400627
12.812752	740.552560	12.405645
13.065961	741.797428	12.410663
12.958707	746.642747	12.415680
13.186304	742.649833	12.420698
13.394497	752.444527	12.425715
13.235862	744.987090	12.430733
13.481388	739.785850	12.435751
13.304467	740.028293	12.440768
13.220000	740.148954	12.445786
13.159817	745.384528	12.450803
13.339506	740.537586	12.455821
13.243291	729.936660	12.460839
13.135927	748.260443	12.465856
13.182134	737.905441	12.470874
13.040338	744.037428	12.475891
13.064380	746.574214	12.480909
13.223915	727.497747	12.485927
12.918232	739.313768	12.490944
13.331400	756.634506	12.495962
13.447860	761.899213	12.500979
13.598998	754.484755	12.505997
13.588722	756.149606	12.511015
13.341413	761.786889	12.516032
13.616780	756.786096	12.521050
13.586163	756.999305	12.526067
13.960225	765.060725	12.531085
13.557512	741.019884	12.536103
13.376527	735.917029	12.541120
13.456299	723.663293	12.546138
13.351682	725.159885	12.551155
13.649362	743.972466	12.556173
14.110939	740.832830	12.561191
13.526376	737.440539	12.566208
13.484822	735.787225	12.571226
13.998521	731.272960	12.576243
13.638129	731.878665	12.581261
13.980885	728.767116	12.586279
13.475069	731.708812	12.591296
13.649616	733.082769	12.596314
13.981611	725.185551	12.601331
13.627490	733.354737	12.606349
13.850872	730.309228	12.611367
13.783307	743.463874	12.616384
13.746101	741.241833	12.621402
13.616186	738.153848	12.626419
13.954072	739.006752	12.631437
14.113383	729.577620	12.636455
13.954379	738.685069	12.641472
13.525508	722.260158	12.646490
13.898605	732.038471	12.651507
13.374207	731.293943	12.656525
13.894910	731.165150	12.661543
14.050075	733.021827	12.666560
13.588068	737.957440	12.671578
14.029287	733.612321	12.676595
13.863101	736.551297	12.681613
14.001699	727.485172	12.686631
13.888339	733.420196	12.691648
13.923867	736.936637	12.696666
14.274953	727.859311	12.701683
13.795772	733.349879	12.706701
14.108314	736.769269	12.711719
14.041507	741.778662	12.716736
13.891003	733.029231	12.721754
13.776095	737.784228	12.726771
13.779874	738.070943	12.731789
13.758397	739.466148	12.736807
13.477757	740.545352	12.741824
13.829085	745.312507	12.746842
14.183633	756.898861	12.751859
14.032542	762.798781	12.756877
14.413354	768.912010	12.761895
14.390075	773.911437	12.766912
13.869855	755.184442	12.771930
13.735724	762.025292	12.776947
14.062576	764.628245	12.781965
14.084459	765.066759	12.786983
14.106911	769.711880	12.792000
14.071352	763.554281	12.797018
14.304053	764.969622	12.802035
14.147039	762.397120	12.807053
14.436332	763.339691	12.812071
14.660484	765.598973	12.817088
14.438311	763.522675	12.822106
14.057954	758.290105	12.827123
14.388625	760.100352	12.832141
14.390627	762.444934	12.837159
14.160285	769.007370	12.842176
14.407286	769.625207	12.847194
14.459964	763.867194	12.852211
14.134086	766.663937	12.857229
14.683126	757.344140	12.862247
14.361763	761.162658	12.867264
13.873705	760.879494	12.872282
14.147731	755.355046	12.877299
14.178038	760.118855	12.882317
14.189219	747.740149	12.887335
14.231861	755.209707	12.892352
14.033673	756.493744	12.897370
14.537427	755.619680	12.902387
14.548358	760.424394	12.907405
14.716714	757.501111	12.912423
14.382419	770.713348	12.917440
14.160060	766.229194	12.922458
14.552272	759.594318	12.927475
13.898311	770.095307	12.932493
14.301724	779.553314	12.937511
14.899217	790.104389	12.942528
14.824393	787.193956	12.947546
14.509958	768.598807	12.952563
14.604134	766.678070	12.957581
14.550036	771.931634	12.962599
14.658141	774.874977	12.967616
14.705020	783.066563	12.972634
14.828244	784.215036	12.977651
14.558108	782.250393	12.982669
14.539158	788.000228	12.987687
14.810526	787.153106	12.992704
14.597930	790.945120	12.997722
14.907588	791.796139	13.002739
14.495538	797.333013	13.007757
14.756448	796.654787	13.012775
14.760459	794.981705	13.017792
14.573024	794.648282	13.022810
14.959699	785.186652	13.027827
14.681363	791.280088	13.032845
14.766123	801.346614	13.037863
14.716992	795.598231	13.042880
14.549039	793.301994	13.047898
14.655306	785.162405	13.052915
14.742212	787.301183	13.057933
15.148112	786.657045	13.062951
14.977155	783.310394	13.067968
14.872962	798.070817	13.072986
14.871960	788.243892	13.078003
14.943701	797.615020	13.083021
15.156086	794.321914	13.088039
15.066428	798.407094	13.093056
14.648639	799.596153	13.098074
15.255325	787.698474	13.103091
14.834977	792.507654	13.108109
14.974838	793.748195	13.113127
15.124809	795.299578	13.118144
14.844126	804.161037	13.123162
15.278022	786.878205	13.128179
14.800645	790.680148	13.133197
15.142803	798.178534	13.138215
14.836438	791.889786	13.143232
15.156476	795.932864	13.148250
15.462615	797.620725	13.153267
14.926108	796.704521	13.158285
15.112138	790.515350	13.163303
15.355215	797.486460	13.168320
15.206308	788.537935	13.173338
15.004802	787.045378	13.178355
15.156720	793.686786	13.183373
15.183200	798.189271	13.188391
15.221414	794.412212	13.193408
15.231659	800.160633	13.198426
15.424393	794.251278	13.203443
15.175021	798.449844	13.208461
14.949401	810.751987	13.213479
15.248026	810.784222	13.218496
15.310016	825.755317	13.223514
15.207744	820.419197	13.228531
15.814250	819.794120	13.233549
15.738774	822.463275	13.238567
15.767420	814.080213	13.243584
15.104324	800.708892	13.248602
15.057700	796.790490	13.253619
15.114539	813.292952	13.258637
15.276540	819.872830	13.263655
15.850044	817.880141	13.268672
15.406297	823.500885	13.273690
15.723945	814.362482	13.278707
15.236393	823.754983	13.283725
14.837820	826.077129	13.288743
14.839200	819.613920	13.293760
14.778639	823.678767	13.298778
15.182860	822.542583	13.303795
15.726226	832.489934	13.308813
15.917896	840.046631	13.313831
15.986351	844.438409	13.318848
15.782082	844.836618	13.323866
15.605289	829.205251	13.328883
15.833673	832.628378	13.333901
15.628276	829.078830	13.338919
15.612098	821.801013	13.343936
15.888413	839.720790	13.348954
16.177168	825.916288	13.353971
15.940764	827.061150	13.358989
15.652840	829.870892	13.364007
15.947782	812.890674	13.369024
15.709699	820.388464	13.374042
15.922077	807.915077	13.379059
15.971648	818.422629	13.384077
15.841550	816.981997	13.389095
15.860895	806.454438	13.394112
15.491278	813.742460	13.399130
15.998236	807.749153	13.404147
15.870677	812.566112	13.409165
16.083475	822.350656	13.414183
16.299995	816.566955	13.419200
15.770879	820.967148	13.424218
15.842962	815.111404	13.429235
15.889928	815.214628	13.434253
15.733472	817.085425	13.439271
15.745214	813.637559	13.444288
15.892338	822.810696	13.449306
15.982906	827.249498	13.454323
16.002284	835.476976	13.459341
15.984348	843.050737	13.464359
16.357228	832.739171	13.469376
15.643606	831.229018	13.474394
16.289217	835.167445	13.479411
15.839498	844.815962	13.484429
15.915761	855.836909	13.489447
16.405574	849.275070	13.494464
16.302002	851.885516	13.499482
16.271160	841.640356	13.504499
16.358934	836.053547	13.509517
16.244068	838.369113	13.514535
16.176429	813.814924	13.519552
15.986566	821.115810	13.524570
16.214968	834.555512	13.529587
16.278160	843.486189	13.534605
15.948742	843.304400	13.539623
16.358879	835.688382	13.544640
16.288977	837.687631	13.549658
16.261094	833.715792	13.554675
16.524070	835.325212	13.559693
16.104273	839.026624	13.564711
16.216428	831.946448	13.569728
16.335187	838.605691	13.574746
16.332800	848.016863	13.579763
16.003581	833.106812	13.584781
15.877103	836.831694	13.589799
15.800110	834.407590	13.594816
16.140899	856.836421	13.599834
16.299908	863.199031	13.604851
16.683525	860.289342	13.609869
16.391700	868.972696	13.614887
16.906194	856.682314	13.619904
16.470817	871.437883	13.624922
16.323110	871.849322	13.629939
16.482810	861.432285	13.634957
16.426723	865.531155	13.639975
16.669260	864.388742	13.644992
16.588066	867.156631	13.650010
16.429652	874.439988	13.655027
16.480626	863.105859	13.660045
16.593012	859.200399	13.665063
16.814567	866.017117	13.670080
17.008644	864.481508	13.675098
16.970896	873.181860	13.680115
16.919924	859.777703	13.685133
16.623389	866.546207	13.690151
16.766662	853.051660	13.695168
16.912845	858.759866	13.700186
16.735860	850.784549	13.705203
16.917675	853.883614	13.710221
17.142149	870.902666	13.715239
16.946111	863.391080	13.720256
16.989550	860.926012	13.725274
17.089553	856.119927	13.730291
16.968190	855.387984	13.735309
16.579173	866.822668	13.740327
16.977879	858.971743	13.745344
16.960624	861.546575	13.750362
16.994426	864.025044	13.755379
16.928105	855.442245	13.760397
16.917426	865.182931	13.765415
16.900186	855.749837	13.770432
17.073638	860.175661	13.775450
17.275242	862.410086	13.780467
16.915826	861.052718	13.785485
16.703726	865.131850	13.790503
16.826406	864.162853	13.795520
17.228526	866.381641	13.800538
17.057306	866.339169	13.805555
17.254959	856.156031	13.810573
17.021378	865.982135	13.815591
17.084300	859.199998	13.820608
17.221124	862.880475	13.825626
17.114840	859.365885	13.830643
16.905705	860.295036	13.835661
16.797596	857.007952	13.840679
17.195275	856.986798	13.845696
16.941136	860.450818	13.850714
17.190606	855.924273	13.855731
17.300409	864.882372	13.860749
17.281571	865.491371	13.865767
16.868465	853.453627	13.870784
17.155850	878.538592	13.875802
17.372702	877.223477	13.880819
17.511456	878.543093	13.885837
17.311610	883.993096	13.890855
17.308461	884.233562	13.895872
17.294736	873.973079	13.900890
17.162839	881.476348	13.905907
17.544919	879.504178	13.910925
17.236685	883.147093	13.915943
17.249314	882.630843	13.920960
17.305838	880.517176	13.925978
17.201534	874.752165	13.930995
17.545069	876.939108	13.936013
17.665720	881.313249	13.941031
17.583067	883.361839	13.946048
17.856122	880.646196	13.951066
17.236360	885.606567	13.956083
17.738866	871.844280	13.961101
17.404648	879.546507	13.966119
17.685648	879.117597	13.971136
17.894821	881.827369	13.976154
17.506524	890.749914	13.981171
17.540610	875.978565	13.986189
17.571982	877.971419	13.991207
17.618674	876.272707	13.996224
17.585298	884.353837	14.001242
17.684231	901.152745	14.006259
18.093261	901.745200	14.011277
18.180813	891.686591	14.016295
18.233014	887.525465	14.021312
17.965895	879.731516	14.026330
17.730543	877.057661	14.031347
18.033639	874.144807	14.036365
17.540611	871.164184	14.041383
17.626183	874.903187	14.046400
18.091716	882.902991	14.051418
17.892737	879.346116	14.056435
17.994837	873.769674	14.061453
18.076054	880.658879	14.066471
18.235791	875.089186	14.071488
17.861450	868.930982	14.076506
17.833600	876.440038	14.081523
18.033786	869.961440	14.086541
17.617886	867.360057	14.091559
17.809162	886.186304	14.096576
18.326632	901.742510	14.101594
17.833762	896.521216	14.106611
18.004478	902.358138	14.111629
18.396731	898.008028	14.116647
17.986451	900.846419	14.121664
18.232415	896.490828	14.126682
18.078170	897.143135	14.131699
18.213449	897.500768	14.136717
18.007551	906.069691	14.141735
18.475660	901.433138	14.146752
18.222077	900.999623	14.151770
18.070717	898.877500	14.156787
18.432341	898.893553	14.161805
18.271783	905.113742	14.166823
18.430928	903.081824	14.171840
18.112846	889.631133	14.176858
17.779207	901.095031	14.181875
18.068203	892.374492	14.186893
18.059925	900.521125	14.191911
18.172816	904.161179	14.196928
18.379886	898.246388	14.201946
18.566487	900.972323	14.206963
18.567678	897.668107	14.211981
18.347597	898.242365	14.216999
18.073562	896.152086	14.222016
18.502306	918.059124	14.227034
18.730817	924.016387	14.232051
18.568321	925.982816	14.237069
18.696359	922.002306	14.242087
18.502618	925.504213	14.247104
18.711920	918.762236	14.252122
18.472724	920.352514	14.257139
18.671363	916.755423	14.262157
18.743063	914.446868	14.267175
18.923661	929.607751	14.272192
18.813279	908.834514	14.277210
18.677046	902.121434	14.282227
18.858926	899.748281	14.287245
18.742598	885.521204	14.292263
18.597821	899.959863	14.297280
18.810651	905.837525	14.302298
18.827664	921.790900	14.307315
19.029938	907.501264	14.312333
19.492693	898.608328	14.317351
18.819261	896.258732	14.322368
18.872988	893.751022	14.327386
18.230713	892.185503	14.332403
18.370044	899.409596	14.337421
18.818980	907.456193	14.342439
18.833434	917.833605	14.347456
18.675131	920.184389	14.352474
18.461573	923.541077	14.357491
18.833290	919.415089	14.362509
19.020212	919.789877	14.367527
18.529581	917.572584	14.372544
18.988829	922.960358	14.377562
18.780870	924.100769	14.382579
19.344343	939.624554	14.387597
19.030326	940.286117	14.392615
19.197415	944.823414	14.397632
19.556296	928.514731	14.402650
19.290574	918.776548	14.407667
19.388752	912.919839	14.412685
19.512203	917.470278	14.417703
19.005630	913.769084	14.422720
19.060373	906.022525	14.427738
19.145876	921.236170	14.432755
19.252003	912.525338	14.437773
19.342577	916.743254	14.442791
19.318617	914.547518	14.447808
19.372738	915.315503	14.452826
19.305557	912.940344	14.457843
19.634694	913.772538	14.462861
19.430479	904.428674	14.467879
18.824609	915.174679	14.472896
19.296519	917.912719	14.477914
19.366405	933.346575	14.482931
19.712630	933.368197	14.487949
19.493163	916.459012	14.492967
19.523612	914.952192	14.497984
19.472284	911.668824	14.503002
19.585031	914.529411	14.508019
19.361064	910.897549	14.513037
19.244040	919.663994	14.518055
19.715663	927.467202	14.523072
19.995723	927.215165	14.528090
19.542742	928.400279	14.533107
19.597151	930.518919	14.538125
19.649791	929.756554	14.543143
19.411278	940.246198	14.548160
19.604779	938.584439	14.553178
19.531494	934.730145	14.558195
19.734230	936.629883	14.563213
19.943653	935.849265	14.568231
19.677590	943.474568	14.573248
19.848586	941.911010	14.578266
19.831276	945.662991	14.583283
19.653679	944.895674	14.588301
19.963981	934.420283	14.593319
20.010171	945.060985	14.598336
20.104233	925.192981	14.603354
19.521399	927.076945	14.608371
19.747072	938.282819	14.613389
20.238189	945.600137	14.618407
19.814596	942.119468	14.623424
19.838340	931.991938	14.628442
19.933778	939.314443	14.633459
19.819058	938.338456	14.638477
19.996715	937.995165	14.643495
20.211493	933.350959	14.648512
20.317827	932.996752	14.653530
20.116162	933.094750	14.658547
19.849725	940.827410	14.663565
20.140201	938.137431	14.668583
19.693462	935.821739	14.673600
20.210950	931.461468	14.678618
19.878524	922.096656	14.683635
19.914794	934.398877	14.688653
20.011555	924.745910	14.693671
20.208215	940.721649	14.698688
20.355898	932.957360	14.703706
20.384333	948.738555	14.708723
20.144673	946.119014	14.713741
20.314483	948.210107	14.718759
20.042889	950.001127	14.723776
20.626094	949.594294	14.728794
20.695208	949.037633	14.733811
20.443437	950.749806	14.738829
20.660095	942.772732	14.743847
20.227673	931.924558	14.748864
20.413818	937.490827	14.753882
20.410380	940.877713	14.758899
20.209462	946.753941	14.763917
20.671648	939.003490	14.768935
20.441931	956.920619	14.773952
20.701986	960.534470	14.778970
20.586625	956.989725	14.783987
20.388062	951.526640	14.789005
20.617775	955.937361	14.794023
20.606153	955.585856	14.799040
20.565870	955.664881	14.804058
20.800876	958.260163	14.809075
20.449974	967.880640	14.814093
20.902172	955.937627	14.819111
20.745791	962.141402	14.824128
20.780940	961.072504	14.829146
20.805258	954.075470	14.834163
20.701282	964.547205	14.839181
20.747244	954.899025	14.844199
20.604586	967.450212	14.849216
20.802427	967.378317	14.854234
20.755787	961.563217	14.859251
20.516447	954.026818	14.864269
20.494177	952.301034	14.869287
20.798153	952.127302	14.874304
20.607220	958.352268	14.879322
20.944951	960.180365	14.884339
20.700700	961.395893	14.889357
20.477390	970.990069	14.894375
21.039112	973.556254	14.899392
20.976173	976.813612	14.904410
21.269761	968.758200	14.909427
21.084737	982.840310	14.914445
21.018785	980.572249	14.919463
20.890755	986.538058	14.924480
20.746704	976.638767	14.929498
21.018500	983.078424	14.934515
20.963969	981.496549	14.939533
21.015681	984.088995	14.944551
21.028749	983.976621	14.949568
21.381327	978.357746	14.954586
21.451826	984.440774	14.959603
21.202011	980.740362	14.964621
21.511540	979.088822	14.969639
21.444474	980.974033	14.974656
20.994572	979.845430	14.979674
21.517074	978.510821	14.984691
21.199939	980.908590	14.989709
21.583708	977.926274	14.994727
21.043670	990.669129	14.999744
21.417460	1001.656172	15.004762
22.038321	991.394026	15.009779
21.820362	986.221152	15.014797
21.649439	985.146669	15.019815
21.328528	984.401804	15.024832
21.314506	979.654577	15.029850
21.410354	974.394668	15.034867
21.287730	982.808567	15.039885
21.735240	993.291742	15.044903
21.836809	1003.753386	15.049920
21.568506	994.681452	15.054938
21.849783	994.138885	15.059955
21.630486	992.068421	15.064973
21.584365	994.840301	15.069991
21.325601	993.426126	15.075008
21.716819	1006.985617	15.080026
21.845682	1001.786801	15.085043
21.407841	1012.250912	15.090061
21.930952	1011.411674	15.095079
21.533715	1010.180142	15.100096
21.529415	1013.150604	15.105114
21.930793	1016.445674	15.110131
21.950057	1012.283368	15.115149
21.980162	1002.909050	15.120167
21.758268	1011.808738	15.125184
21.890831	1012.040565	15.130202
21.849756	994.667847	15.135219
21.725822	1005.915917	15.140237
21.974933	1001.477756	15.145255
21.860171	1006.785075	15.150272
21.994761	1019.646315	15.155290
22.578988	1021.271692	15.160307
22.271364	1014.269838	15.165325
22.277002	1011.908504	15.170343
21.877434	1015.123937	15.175360
21.576410	1004.119429	15.180378
22.257876	1013.167917	15.185395
22.123641	1034.964488	15.190413
22.338433	1029.654369	15.195431
22.245682	1030.079291	15.200448
22.219405	1032.090663	15.205466
22.746565	1036.416930	15.210483
22.508788	1031.524863	15.215501
22.554945	1020.844651	15.220519
22.390811	1007.047853	15.225536
22.034792	1008.931002	15.230554
22.364712	1003.072668	15.235571
22.564183	1022.629933	15.240589
22.524700	1021.534855	15.245607
22.509977	1010.062601	15.250624
22.151499	1011.087743	15.255642
22.577046	1019.516759	15.260659
22.597747	1027.239181	15.265677
22.812931	1022.642225	15.270695
22.509323	1010.388400	15.275712
22.409041	1021.383461	15.280730
22.597140	1023.689452	15.285747
22.686008	1022.552172	15.290765
22.826236	1031.196313	15.295783
22.745395	1021.277626	15.300800
22.714818	1021.405624	15.305818
22.816864	1020.433540	15.310835
22.670338	1026.175038	15.315853
22.726158	1031.887990	15.320871
22.870063	1032.108573	15.325888
22.554721	1035.623242	15.330906
22.871981	1027.709264	15.335923
22.320502	1033.810864	15.340941
22.473883	1024.919001	15.345959
22.719740	1021.216660	15.350976
22.424353	1031.873061	15.355994
22.649892	1027.526951	15.361011
22.461130	1046.302456	15.366029
22.658699	1049.986078	15.371047
22.954095	1054.361286	15.376064
22.798185	1060.262059	15.381082
23.162027	1047.304017	15.386099
22.888162	1046.570713	15.391117
22.738172	1062.875435	15.396135
22.964470	1052.520437	15.401152
22.960525	1058.416334	15.406170
23.402261	1049.870606	15.411187
23.244787	1061.679397	15.416205
22.651851	1054.233072	15.421223
22.977140	1061.702655	15.426240
23.321804	1075.338921	15.431258
23.461262	1075.257238	15.436275
23.237604	1076.561068	15.441293
23.271191	1086.957671	15.446311
23.989407	1077.914166	15.451328
23.463291	1075.632983	15.456346
23.435289	1057.778464	15.461363
23.512835	1056.614553	15.466381
23.502489	1056.919265	15.471399
23.320368	1052.359306	15.476416
23.029887	1057.268130	15.481434
23.490724	1063.776029	15.486451
23.585732	1075.384321	15.491469
23.685324	1078.893948	15.496487
23.999370	1075.272432	15.501504
23.548033	1071.868669	15.506522
23.725645	1055.581960	15.511539
23.112473	1059.730288	15.516557
23.137863	1070.052425	15.521575
23.783596	1066.735554	15.526592
23.575401	1074.755797	15.531610
23.904921	1077.402561	15.536627
23.932288	1078.209460	15.541645
23.794357	1081.516457	15.546663
23.681699	1076.197667	15.551680
23.777848	1083.384418	15.556698
23.794338	1075.788948	15.561715
23.619498	1083.614617	15.566733
23.788627	1073.599930	15.571751
23.703094	1069.854825	15.576768
23.447840	1080.236718	15.581786
23.810746	1077.708943	15.586803
24.010247	1080.953604	15.591821
23.506972	1076.623841	15.596839
23.890876	1088.565581	15.601856
24.065319	1094.657607	15.606874
24.255957	1101.084775	15.611891
24.348482	1099.265250	15.616909
24.114099	1101.268208	15.621927
24.235106	1089.967145	15.626944
23.979717	1092.916999	15.631962
24.446312	1094.759634	15.636979
24.149959	1101.569224	15.641997
24.112317	1099.359830	15.647015
24.289227	1096.454087	15.652032
24.242400	1100.851368	15.657050
24.241667	1105.885225	15.662067
24.474108	1104.848523	15.667085
24.372400	1100.515798	15.672103
24.700971	1096.936184	15.677120
24.518975	1103.459608	15.682138
24.416133	1092.196773	15.687155
24.551414	1087.852166	15.692173
24.757975	1084.250644	15.697191
24.100515	1067.460435	15.702208
24.303199	1091.716355	15.707226
24.496670	1089.268775	15.712243
24.543722	1092.414244	15.717261
24.605324	1098.757486	15.722279
24.752469	1096.992520	15.727296
24.354244	1099.863767	15.732314
24.192403	1104.575720	15.737331
24.645488	1093.228936	15.742349
24.453553	1096.102576	15.747367
24.706010	1099.095940	15.752384
24.247871	1103.305196	15.757402
24.271978	1102.291669	15.762419
24.732784	1112.504583	15.767437
24.506094	1119.653567	15.772455
25.144962	1115.744459	15.777472
24.846784	1124.277450	15.782490
24.791272	1128.505680	15.787507
25.018457	1133.705811	15.792525
24.638871	1130.524329	15.797543
25.193651	1137.374150	15.802560
24.635111	1133.845157	15.807578
24.960777	1127.734980	15.812595
25.206479	1127.769197	15.817613
24.969632	1131.703940	15.822631
25.184352	1131.891338	15.827648
25.178813	1132.633965	15.832666
24.794728	1130.324210	15.837683
25.211138	1123.243586	15.842701
25.142347	1122.588604	15.847719
25.539130	1125.890726	15.852736
25.312027	1127.018370	15.857754
24.854223	1121.785203	15.862771
25.091920	1118.794192	15.867789
25.256126	1123.546585	15.872807
25.367190	1118.871243	15.877824
25.480211	1117.768043	15.882842
25.232760	1121.950604	15.887859
25.429754	1121.228732	15.892877
25.344117	1121.753530	15.897895
25.435327	1119.785882	15.902912
25.297760	1124.500349	15.907930
25.143297	1119.374293	15.912947
25.705480	1121.687958	15.917965
25.505181	1121.397571	15.922983
25.695503	1112.417824	15.928000
25.482728	1120.180023	15.933018
25.230548	1109.224603	15.938035
25.419460	1141.776381	15.943053
25.580658	1151.263070	15.948071
25.839384	1141.934912	15.953088
25.637852	1139.189445	15.958106
25.567620	1147.191260	15.963123
25.430326	1145.799067	15.968141
25.318159	1144.200960	15.973159
25.547204	1146.323822	15.978176
25.817006	1150.349606	15.983194
25.567551	1140.570883	15.988211
25.910527	1140.053360	15.993229
25.586522	1149.761240	15.998247
26.102228	1160.331662	16.003264
25.959634	1161.625952	16.008282
26.381743	1167.107984	16.013299
26.200188	1157.561616	16.018317
25.770531	1148.858875	16.023335
25.922152	1157.393992	16.028352
25.839296	1161.553930	16.033370
25.603412	1163.774887	16.038387
26.343707	1167.698554	16.043405
26.111281	1174.337206	16.048423
26.225699	1170.655427	16.053440
26.652307	1167.783136	16.058458
26.355041	1173.844952	16.063475
26.152811	1173.993534	16.068493
25.977661	1178.584513	16.073511
25.982165	1172.931749	16.078528
26.424782	1172.688955	16.083546
26.102662	1170.069676	16.088563
26.579136	1161.789859	16.093581
26.589529	1176.226520	16.098599
26.425148	1168.476309	16.103616
26.486389	1170.622310	16.108634
26.412872	1169.579893	16.113651
26.183385	1173.762807	16.118669
26.730188	1170.054310	16.123687
26.860446	1168.058447	16.128704
26.801536	1170.311638	16.133722
26.262263	1169.518925	16.138739
26.758739	1165.723637	16.143757
26.512837	1165.733891	16.148775
26.467743	1173.078511	16.153792
26.669114	1165.103733	16.158810
26.408643	1176.714138	16.163827
26.529881	1185.272964	16.168845
26.933293	1192.004508	16.173863
27.191896	1192.551114	16.178880
27.345442	1193.603342	16.183898
26.634240	1181.612081	16.188915
26.999344	1174.059782	16.193933
27.226306	1167.305476	16.198951
27.172868	1163.747832	16.203968
26.912189	1168.715135	16.208986
26.984027	1162.499545	16.214003
26.719871	1148.967622	16.219021
26.915383	1164.688115	16.224039
26.867935	1172.036260	16.229056
27.042758	1177.588599	16.234074
26.858717	1181.780174	16.239091
27.329181	1181.245831	16.244109
27.311192	1183.148621	16.249127
27.393777	1177.256398	16.254144
27.266168	1179.163739	16.259162
27.252502	1185.465154	16.264179
27.597526	1177.436305	16.269197
27.019376	1178.249716	16.274215
27.553200	1175.691992	16.279232
27.550753	1170.251762	16.284250
27.635160	1182.104788	16.289267
27.458452	1176.335244	16.294285
27.163984	1180.648265	16.299303
27.250673	1181.947659	16.304320
27.358650	1181.738361	16.309338
27.197909	1187.668335	16.314355
27.169047	1191.210734	16.319373
27.074597	1191.181479	16.324391
27.257884	1180.874172	16.329408
27.282312	1188.416194	16.334426
27.247623	1204.040243	16.339443
27.363270	1199.184276	16.344461
27.800811	1203.325805	16.349479
27.487349	1207.982644	16.354496
27.977269	1209.392436	16.359514
27.578012	1205.759574	16.364531
27.773027	1209.213249	16.369549
27.957166	1216.455698	16.374567
27.634787	1212.422615	16.379584
28.049464	1205.399036	16.384602
27.594273	1215.673475	16.389619
28.082959	1217.626274	16.394637
27.950904	1215.804053	16.399655
27.638004	1214.417277	16.404672
28.224025	1216.339046	16.409690
28.362725	1218.637023	16.414707
28.286415	1215.262837	16.419725
28.070893	1213.756659	16.424743
28.467203	1214.808723	16.429760
28.028737	1211.522840	16.434778
27.722919	1218.643234	16.439795
28.365019	1226.258914	16.444813
28.612150	1237.133401	16.449831
28.138172	1225.303763	16.454848
28.493759	1231.443196	16.459866
28.215297	1237.751403	16.464883
28.714965	1226.296249	16.469901
28.199673	1218.597840	16.474919
28.431406	1220.912800	16.479936
28.530237	1226.590673	16.484954
28.199411	1235.387615	16.489971
28.569087	1228.749786	16.494989
28.850865	1231.716487	16.500007
28.628760	1230.113507	16.505024
28.733866	1229.658498	16.510042
28.611176	1231.779675	16.515059
28.698576	1225.883526	16.520077
28.870782	1231.966482	16.525095
28.442078	1226.264808	16.530112
29.037671	1218.244019	16.535130
28.883620	1224.693680	16.540147
28.639953	1202.691250	16.545165
28.559899	1211.082806	16.550183
28.304984	1224.623776	16.555200
28.680236	1232.287580	16.560218
28.614243	1238.010216	16.565235
29.017116	1239.840759	16.570253
28.937006	1237.009979	16.575271
28.673097	1238.165487	16.580288
29.249162	1229.630187	16.585306
28.958677	1230.464802	16.590323
28.792929	1232.504360	16.595341
28.910332	1228.629593	16.600359
28.757508	1229.631992	16.605376
28.754764	1223.074607	16.610394
29.060069	1246.576180	16.615411
29.103716	1248.406201	16.620429
29.226272	1255.188086	16.625447
29.344282	1256.302692	16.630464
29.517618	1251.358775	16.635482
29.018087	1256.407707	16.640499
29.058094	1255.893469	16.645517
29.412180	1255.626674	16.650535
28.906766	1261.320333	16.655552
29.450559	1260.651419	16.660570
29.613836	1260.638589	16.665587
29.319212	1255.206241	16.670605
29.208796	1261.866835	16.675623
29.291698	1257.694501	16.680640
29.274608	1262.289139	16.685658
29.130685	1267.093005	16.690675
29.420241	1281.669054	16.695693
29.577715	1271.444637	16.700711
29.630299	1280.213088	16.705728
29.684307	1288.056640	16.710746
29.684799	1285.935925	16.715763
30.039201	1278.836552	16.720781
30.241389	1282.708853	16.725799
30.055608	1286.525173	16.730816
30.029835	1271.482001	16.735834
29.872000	1274.164127	16.740851
29.993397	1285.402337	16.745869
30.138078	1280.017919	16.750887
30.385779	1277.994176	16.755904
30.198087	1272.156892	16.760922
30.284261	1276.413453	16.765939
30.220826	1255.417855	16.770957
30.070310	1253.513314	16.775975
29.876489	1258.009405	16.780992
30.187739	1268.129073	16.786010
30.256410	1272.956437	16.791027
30.089129	1275.706318	16.796045
30.410606	1264.515751	16.801063
30.017749	1278.659059	16.806080
30.804587	1269.311208	16.811098
30.285225	1273.804659	16.816115
30.165677	1277.124591	16.821133
30.084518	1283.449239	16.826151
29.969894	1280.772187	16.831168
29.910742	1284.789579	16.836186
29.852801	1271.200007	16.841203
29.778208	1281.932419	16.846221
30.060356	1292.290197	16.851239
30.119721	1307.173741	16.856256
30.488730	1296.101943	16.861274
30.391342	1298.092927	16.866291
30.567522	1294.521371	16.871309
30.828416	1296.484623	16.876327
30.473419	1305.061317	16.881344
30.666563	1301.143108	16.886362
30.769303	1299.217816	16.891379
30.891983	1303.187788	16.896397
30.911434	1290.311934	16.901415
30.697421	1303.748722	16.906432
30.743691	1293.488065	16.911450
30.999607	1302.199422	16.916467
30.809077	1312.303056	16.921485
31.114475	1311.456891	16.926503
31.091827	1319.681708	16.931520
30.966656	1310.934336	16.936538
31.021847	1300.798514	16.941555
31.251949	1314.509720	16.946573
31.499005	1306.291029	16.951591
30.995495	1299.184050	16.956608
31.222968	1292.912471	16.961626
31.506513	1294.493465	16.966643
30.936962	1298.190029	16.971661
31.129188	1295.038850	16.976679
31.355835	1306.247959	16.981696
31.552085	1309.594159	16.986714
31.204367	1308.531577	16.991731
31.163978	1315.234870	16.996749
31.536330	1305.607948	17.001767
31.411080	1313.485909	17.006784
31.534248	1307.495764	17.011802
31.538855	1309.764268	17.016819
31.378001	1316.341263	17.021837
31.327231	1306.376679	17.026855
31.314846	1311.614398	17.031872
31.332389	1308.970284	17.036890
31.114691	1309.670418	17.041907
31.386820	1313.762148	17.046925
31.348885	1324.968540	17.051943
31.422563	1335.826081	17.056960
31.781551	1330.468033	17.061978
32.202181	1335.940882	17.066995
31.769874	1343.633428	17.072013
32.318809	1335.477883	17.077031
32.106696	1340.191462	17.082048
31.881336	1332.043621	17.087066
32.239550	1334.439768	17.092083
31.779761	1329.080614	17.097101
32.012665	1325.424423	17.102119
31.712495	1333.856836	17.107136
32.342197	1331.003193	17.112154
32.139962	1318.528138	17.117171
31.944995	1328.948068	17.122189
32.295747	1325.948777	17.127207
32.493277	1326.094688	17.132224
32.366955	1327.560015	17.137242
32.684925	1327.882722	17.142259
32.108891	1331.706545	17.147277
32.315771	1334.754429	17.152295
32.210699	1326.874932	17.157312
32.520065	1333.709631	17.162330
32.686896	1327.665299	17.167347
32.197350	1333.476419	17.172365
32.563423	1327.214671	17.177383
31.688924	1325.862227	17.182400
32.453168	1338.827021	17.187418
32.624891	1341.820452	17.192435
32.530894	1355.210071	17.197453
33.078717	1351.419323	17.202471
32.894189	1353.581762	17.207488
32.306044	1342.268569	17.212506
32.924630	1353.949648	17.217523
32.358406	1355.048385	17.222541
32.817178	1351.400982	17.227559
32.884223	1352.851795	17.232576
33.015059	1351.206128	17.237594
32.819488	1348.715324	17.242611
32.577032	1348.450472	17.247629
32.866398	1346.947231	17.252647
32.901893	1350.324938	17.257664
32.878733	1358.502515	17.262682
33.046039	1344.877596	17.267699
32.657082	1358.054646	17.272717
32.874468	1354.637574	17.277735
33.222426	1369.848351	17.282752
33.147078	1374.600474	17.287770
33.325251	1370.469993	17.292787
33.322690	1381.513083	17.297805
33.291979	1374.205759	17.302823
33.191986	1381.833631	17.307840
33.642935	1383.997497	17.312858
33.656303	1388.634734	17.317875
33.445500	1381.529200	17.322893
33.738258	1380.303145	17.327911
33.397686	1382.265966	17.332928
33.019132	1377.844001	17.337946
33.667841	1374.416152	17.342963
33.718809	1381.070440	17.347981
33.942804	1377.911113	17.352999
33.922010	1370.876802	17.358016
33.650755	1377.941349	17.363034
33.813241	1371.389580	17.368051
33.626796	1373.533386	17.373069
33.979501	1374.762712	17.378087
33.856599	1376.016061	17.383104
33.596956	1379.534693	17.388122
33.768846	1375.351545	17.393139
33.513853	1383.473935	17.398157
33.677988	1369.773751	17.403175
33.691391	1378.832422	17.408192
33.550969	1374.701362	17.413210
34.327255	1383.277577	17.418227
33.919875	1380.892540	17.423245
33.844105	1385.417505	17.428263
34.326813	1396.577084	17.433280
34.298597	1397.970239	17.438298
34.455000	1396.740300	17.443315
34.516294	1402.206352	17.448333
34.673725	1394.645471	17.453351
34.370573	1380.371529	17.458368
34.141661	1380.391744	17.463386
34.377256	1371.145989	17.468403
34.248071	1387.747558	17.473421
34.198918	1383.315008	17.478439
34.485458	1385.116456	17.483456
34.153147	1400.285515	17.488474
34.456427	1393.418178	17.493491
34.507868	1399.769430	17.498509
34.372170	1386.829450	17.503527
34.982665	1401.658281	17.508544
34.627667	1398.886324	17.513562
35.078261	1391.926476	17.518579
34.934249	1397.541462	17.523597
34.916870	1393.943406	17.528615
35.217395	1388.525071	17.533632
35.054644	1389.478540	17.538650
35.122726	1389.925610	17.543667
34.877854	1395.556398	17.548685
35.036305	1404.134747	17.553703
35.088971	1393.061959	17.558720
34.748718	1391.600556	17.563738
34.905258	1388.174075	17.568755
34.802646	1393.337589	17.573773
34.959695	1389.746920	17.578791
35.092555	1389.404328	17.583808
34.979596	1387.667463	17.588826
35.350275	1381.616422	17.593843
35.035982	1390.477124	17.598861
34.966256	1381.632664	17.603879
35.116715	1398.708000	17.608896
34.993795	1413.901070	17.613914
35.185629	1408.973147	17.618931
35.266676	1411.510565	17.623949
35.407998	1409.216285	17.628967
35.400478	1412.638615	17.633984
35.549300	1414.808795	17.639002
35.424450	1416.961890	17.644019
35.116911	1420.443852	17.649037
35.361811	1415.905259	17.654055
35.269563	1431.996134	17.659072
35.490777	1449.805232	17.664090
36.086152	1438.839896	17.669107
35.995216	1449.098424	17.674125
35.474892	1441.157700	17.679143
35.826546	1442.784843	17.684160
35.563436	1443.820314	17.689178
35.854784	1438.362374	17.694195
35.753911	1444.538683	17.699213
35.907153	1437.442363	17.704231
35.594754	1442.086472	17.709248
35.890296	1447.275984	17.714266
36.483532	1460.056213	17.719283
36.432813	1449.772793	17.724301
36.190966	1439.509856	17.729319
36.369623	1437.197099	17.734336
36.492697	1432.898505	17.739354
36.284748	1435.692653	17.744371
36.478491	1430.158487	17.749389
36.316640	1439.149968	17.754407
36.656486	1428.672817	17.759424
36.146024	1436.939403	17.764442
36.416722	1431.074431	17.769459
36.389782	1436.759452	17.774477
36.433819	1456.635048	17.779495
36.791691	1455.881644	17.784512
36.447985	1465.169886	17.789530
36.926846	1463.075189	17.794547
36.907997	1459.635148	17.799565
36.664057	1452.702041	17.804583
36.849067	1460.143276	17.809600
36.767025	1464.164295	17.814618
37.145296	1459.617418	17.819635
36.770587	1454.121814	17.824653
36.883939	1454.722746	17.829671
37.063836	1458.058913	17.834688
36.997957	1457.561258	17.839706
37.035085	1458.742200	17.844723
37.146596	1462.811792	17.849741
37.116548	1464.445090	17.854759
36.983085	1441.042801	17.859776
36.921069	1453.995121	17.864794
36.769171	1450.992509	17.869811
37.376389	1449.931785	17.874829
37.442951	1450.211830	17.879847
37.463971	1448.744313	17.884864
37.369290	1456.437660	17.889882
37.040767	1452.471759	17.894899
37.158186	1456.060721	17.899917
37.294163	1454.833979	17.904935
37.259112	1451.500623	17.909952
37.415148	1451.009226	17.914970
37.532995	1447.541458	17.919987
37.458369	1441.863136	17.925005
37.141272	1448.411008	17.930023
37.246508	1453.908062	17.935040
37.819558	1464.930447	17.940058
37.974097	1469.573991	17.945075
37.872478	1468.684288	17.950093
37.842738	1472.053303	17.955111
37.639194	1473.735877	17.960128
37.424945	1469.449098	17.965146
38.033875	1464.541020	17.970163
37.888246	1468.035494	17.975181
37.514937	1475.352764	17.980199
37.879415	1471.871596	17.985216
37.829112	1472.946313	17.990234
37.962701	1462.807584	17.995251
38.005980	1462.595796	18.000269
37.945189	1463.899382	18.005287
38.176593	1489.994409	18.010304
38.015739	1502.551977	18.015322
38.259948	1488.921211	18.020339
38.518636	1495.101165	18.025357
38.141148	1494.516626	18.030375
38.374409	1484.602120	18.035392
38.427620	1492.976084	18.040410
38.254699	1490.093530	18.045427
38.436350	1498.052881	18.050445
38.027136	1493.114960	18.055463
38.371968	1491.495715	18.060480
38.493145	1493.774382	18.065498
38.620050	1487.591078	18.070515
38.444493	1500.248783	18.075533
38.193767	1506.454904	18.080551
38.783193	1517.885029	18.085568
38.840114	1508.787124	18.090586
38.936587	1511.704008	18.095603
38.616924	1509.904839	18.100621
38.636598	1519.470704	18.105639
39.397713	1513.724535	18.110656
39.252697	1514.280739	18.115674
39.300378	1513.607493	18.120691
39.457689	1510.142997	18.125709
39.117241	1519.752663	18.130727
39.347063	1514.149699	18.135744
39.232977	1513.167269	18.140762
39.012722	1504.204316	18.145779
39.378893	1511.673995	18.150797
39.100986	1509.783073	18.155815
39.242557	1509.776800	18.160832
39.176200	1507.237325	18.165850
39.077843	1513.511097	18.170867
38.969389	1510.675246	18.175885
39.202437	1517.657679	18.180903
39.500316	1528.025753	18.185920
39.785666	1535.217758	18.190938
39.712777	1545.527164	18.195955
40.431964	1534.447694	18.200973
39.690065	1525.790533	18.205991
39.952539	1511.140674	18.211008
39.706936	1514.584545	18.216026
39.908988	1504.204682	18.221043
40.122879	1501.160531	18.226061
39.755588	1509.909669	18.231079
40.237180	1504.077905	18.236096
40.238754	1495.941772	18.241114
39.751224	1507.736295	18.246131
40.148588	1501.807270	18.251149
40.029512	1510.590106	18.256167
40.276139	1506.887545	18.261184
40.229643	1496.710737	18.266202
40.110582	1501.397156	18.271219
39.815999	1499.701360	18.276237
39.466854	1517.505211	18.281255
40.116314	1510.690892	18.286272
40.113791	1526.793042	18.291290
40.117477	1534.111231	18.296307
40.551479	1522.072860	18.301325
40.253228	1530.277837	18.306343
40.407735	1523.436915	18.311360
40.603673	1522.077692	18.316378
40.500210	1529.579933	18.321395
40.719540	1522.719388	18.326413
40.329514	1523.244549	18.331431
40.567047	1522.115505	18.336448
41.014832	1543.903560	18.341466
40.943445	1535.807244	18.346483
41.079839	1524.339387	18.351501
40.813165	1535.913124	18.356519
40.850303	1526.594237	18.361536
41.032646	1529.109489	18.366554
41.225741	1546.913622	18.371571
40.879463	1532.453802	18.376589
40.835482	1536.711882	18.381607
41.184651	1542.685163	18.386624
41.170727	1558.060103	18.391642
41.129513	1555.071692	18.396659
41.270580	1547.734228	18.401677
41.696429	1546.231678	18.406695
41.407077	1543.051763	18.411712
41.620339	1551.750989	18.416730
41.098680	1553.723264	18.421747
41.487430	1548.130105	18.426765
41.340732	1542.207411	18.431783
41.324885	1549.235164	18.436800
41.226034	1544.302253	18.441818
41.316578	1545.178173	18.446835
41.413337	1547.097738	18.451853
41.245450	1544.195450	18.456871
41.329440	1549.194066	18.461888
41.584628	1551.903045	18.466906
41.481295	1570.908723	18.471923
41.757146	1568.653309	18.476941
41.707617	1567.323074	18.481959
41.738979	1564.209676	18.486976
41.857151	1563.733677	18.491994
42.173422	1561.282573	18.497011
42.019444	1555.373639	18.502029
41.916702	1563.570091	18.507047
41.926081	1561.429015	18.512064
42.118320	1557.416213	18.517082
42.145004	1584.408184	18.522099
42.538809	1587.316366	18.527117
42.078361	1572.745008	18.532135
42.431287	1579.336279	18.537152
42.455706	1592.890568	18.542170
42.164348	1591.153231	18.547187
42.543516	1583.765822	18.552205
42.036049	1591.785845	18.557223
42.142306	1593.107452	18.562240
42.306251	1586.217689	18.567258
42.276572	1592.247188	18.572275
42.740012	1590.218013	18.577293
42.661280	1590.179982	18.582311
42.506124	1590.905042	18.587328
42.766520	1594.537906	18.592346
42.641970	1604.637680	18.597363
42.910359	1608.969917	18.602381
43.051342	1608.648141	18.607399
43.207199	1610.021941	18.612416
42.741858	1590.900440	18.617434
42.860465	1601.104132	18.622451
42.945929	1598.878543	18.627469
43.228714	1605.007421	18.632487
43.189038	1609.211192	18.637504
43.676872	1611.233601	18.642522
43.157176	1610.766018	18.647539
43.255600	1599.733272	18.652557
43.201723	1599.823897	18.657575
43.314802	1596.486241	18.662592
43.479823	1600.282380	18.667610
43.544582	1601.818782	18.672627
43.822098	1602.229888	18.677645
43.686735	1597.163820	18.682663
43.493035	1598.396717	18.687680
43.520350	1591.613570	18.692698
43.602936	1607.336367	18.697715
43.591318	1599.274841	18.702733
43.640785	1593.962054	18.707751
43.710217	1598.988213	18.712768
43.916641	1603.828799	18.717786
44.025628	1609.959661	18.722803
44.092800	1606.884829	18.727821
43.960731	1599.722688	18.732839
44.142387	1609.181168	18.737856
44.097762	1595.046438	18.742874
43.878955	1603.923843	18.747891
44.051371	1596.354218	18.752909
44.028811	1605.254528	18.757927
43.959430	1608.333120	18.762944
44.420830	1606.970170	18.767962
44.017411	1618.439146	18.772979
44.202783	1619.180286	18.777997
44.716230	1624.313618	18.783015
44.649730	1623.339506	18.788032
44.565886	1614.273069	18.793050
44.469588	1625.195290	18.798067
44.513527	1618.961821	18.803085
44.550573	1614.105433	18.808103
44.464353	1616.637527	18.813120
44.909627	1612.020152	18.818138
44.600992	1617.449550	18.823155
44.701080	1609.506224	18.828173
44.777153	1621.786902	18.833191
44.776554	1608.156529	18.838208
44.548041	1614.842069	18.843226
44.505577	1624.619709	18.848243
44.754249	1632.455004	18.853261
44.951741	1641.257736	18.858279
45.088576	1634.902404	18.863296
45.311565	1630.786933	18.868314
44.957749	1647.218800	18.873331
45.312144	1629.278550	18.878349
45.685393	1634.383355	18.883367
45.336284	1635.836274	18.888384
45.501033	1632.907103	18.893402
45.520213	1628.489033	18.898419
45.605588	1627.298611	18.903437
45.356685	1631.339499	18.908455
45.643804	1634.153946	18.913472
45.503485	1629.372683	18.918490
45.352972	1625.940614	18.923507
45.418823	1619.946721	18.928525
45.715527	1626.695150	18.933543
45.937313	1625.843135	18.938560
45.488986	1619.311234	18.943578
45.696750	1634.951323	18.948595
45.747196	1640.946193	18.953613
45.870713	1650.959786	18.958631
45.913954	1649.545579	18.963648
46.260362	1651.861564	18.968666
46.144655	1661.597048	18.973683
46.088360	1659.251644	18.978701
46.213319	1652.478423	18.983719
46.011477	1656.085887	18.988736
46.020422	1649.892606	18.993754
46.072135	1654.208308	18.998771
45.883562	1656.519747	19.003789
46.504090	1644.082821	19.008807
46.400652	1651.313696	19.013824
46.287917	1644.410453	19.018842
46.457234	1656.304141	19.023859
46.711706	1670.725051	19.028877
46.802683	1672.664472	19.033895
46.381894	1658.541289	19.038912
46.520483	1667.290143	19.043930
46.741817	1669.909764	19.048947
46.707972	1671.007161	19.053965
47.129517	1676.852378	19.058983
46.612062	1671.669420	19.064000
46.748052	1678.130607	19.069018
46.985099	1671.999415	19.074035
47.182344	1675.954632	19.079053
47.273394	1671.758833	19.084071
47.069582	1671.816142	19.089088
47.167291	1675.051612	19.094106
47.161876	1674.689653	19.099123
47.094355	1680.463165	19.104141
46.918628	1663.925135	19.109159
47.549573	1684.138240	19.114176
47.507082	1684.984515	19.119194
47.450595	1690.721586	19.124211
47.559262	1692.790788	19.129229
47.586537	1691.865099	19.134247
47.643391	1683.972697	19.139264
47.846134	1689.981594	19.144282
47.400136	1691.831570	19.149299
47.865760	1691.234854	19.154317
48.125768	1683.465266	19.159335
47.695311	1686.104956	19.164352
47.777503	1689.144034	19.169370
47.690462	1690.745255	19.174387
47.627907	1692.146969	19.179405
47.680406	1686.335036	19.184423
47.904673	1684.804096	19.189440
47.917463	1687.819331	19.194458
47.931036	1693.548583	19.199475
48.195950	1711.903392	19.204493
48.400712	1704.461204	19.209511
48.040349	1720.070453	19.214528
48.153156	1717.925777	19.219546
48.260015	1709.492170	19.224563
48.581192	1711.796337	19.229581
48.442161	1715.769533	19.234599
48.292988	1713.931007	19.239616
48.562486	1711.140054	19.244634
48.370673	1714.152635	19.249651
48.624317	1713.122046	19.254669
48.492396	1707.367405	19.259687
48.663907	1718.727431	19.264704
48.861861	1730.465195	19.269722
49.085531	1732.696274	19.274739
49.014580	1742.762479	19.279757
49.086604	1733.195008	19.284775
49.129870	1744.565676	19.289792
49.274634	1732.840740	19.294810
49.254436	1717.979365	19.299827
48.853007	1711.970286	19.304845
49.157589	1714.952433	19.309863
49.120530	1728.036748	19.314880
49.393773	1732.090529	19.319898
49.776788	1727.302988	19.324915
49.394747	1725.298963	19.329933
49.475314	1734.798596	19.334951
49.162450	1731.559210	19.339968
49.426725	1732.584655	19.344986
49.497553	1722.843798	19.350003
49.384882	1723.937768	19.355021
49.546539	1725.272797	19.360039
49.566150	1729.407344	19.365056
49.680047	1716.740460	19.370074
49.614399	1728.604734	19.375091
49.611883	1739.130457	19.380109
50.146070	1746.665434	19.385127
50.137936	1757.517114	19.390144
50.238418	1759.486615	19.395162
50.120840	1748.790595	19.400179
50.340695	1755.232358	19.405197
50.270427	1748.742167	19.410215
50.060981	1755.143889	19.415232
50.176446	1746.399629	19.420250
50.420181	1746.367882	19.425267
50.100985	1742.312087	19.430285
50.670226	1738.139186	19.435303
50.145638	1751.482950	19.440320
49.962184	1738.843703	19.445338
50.491237	1736.968343	19.450355
50.237246	1741.972627	19.455373
50.199784	1754.795078	19.460391
50.457591	1771.967567	19.465408
50.300149	1773.829149	19.470426
50.852037	1769.068791	19.475443
50.782903	1771.860177	19.480461
50.780914	1766.785788	19.485479
50.790055	1777.742077	19.490496
51.117389	1785.495684	19.495514
51.431615	1779.462823	19.500531
51.151635	1784.461723	19.505549
51.358743	1786.240941	19.510567
51.194314	1786.244740	19.515584
51.346448	1797.216509	19.520602
51.677459	1795.050261	19.525619
51.531075	1790.623375	19.530637
51.632619	1783.411934	19.535655
51.370280	1772.381954	19.540672
51.397616	1789.944041	19.545690
51.421347	1785.196997	19.550707
51.482187	1789.015811	19.555725
51.317608	1785.469143	19.560743
51.422056	1788.706734	19.565760
51.534592	1797.374522	19.570778
51.530490	1789.680984	19.575795
51.848310	1799.351774	19.580813
52.161881	1810.033154	19.585831
52.130687	1805.610310	19.590848
52.208901	1796.288003	19.595866
52.356536	1793.585563	19.600883
52.123849	1783.358864	19.605901
52.198077	1782.220674	19.610919
52.464290	1782.374765	19.615936
52.357477	1784.155827	19.620954
52.238521	1774.286877	19.625971
52.288784	1787.067203	19.630989
52.359881	1796.255909	19.636007
52.578734	1795.937709	19.641024
52.804839	1805.929004	19.646042
52.687641	1802.169770	19.651059
52.601509	1806.655438	19.656077
52.554803	1808.657473	19.661095
53.019267	1808.909898	19.666112
52.740835	1813.589808	19.671130
52.947200	1803.164913	19.676147
52.801828	1811.046245	19.681165
52.670437	1810.214841	19.686183
52.495553	1808.667528	19.691200
52.574579	1806.704871	19.696218
52.823056	1799.760754	19.701235
52.828580	1815.811407	19.706253
53.052816	1821.627621	19.711271
52.965277	1822.083305	19.716288
52.967016	1831.156656	19.721306
53.176496	1822.845780	19.726323
53.162278	1823.192140	19.731341
53.206681	1834.215527	19.736359
53.258158	1848.419062	19.741376
53.156810	1857.666378	19.746394
53.865668	1853.866077	19.751411
53.643003	1863.381727	19.756429
53.671206	1854.395450	19.761447
53.626921	1853.266356	19.766464
54.289019	1855.283584	19.771482
54.064052	1850.364035	19.776499
53.781354	1851.165897	19.781517
53.929479	1858.180705	19.786535
54.172918	1854.472260	19.791552
53.900911	1857.850902	19.796570
53.983840	1857.708641	19.801587
54.100829	1866.672429	19.806605
54.236862	1877.763542	19.811623
54.651136	1889.199258	19.816640
54.117984	1884.138625	19.821658
54.728361	1877.080968	19.826675
54.484890	1883.923596	19.831693
54.426673	1876.645624	19.836711
54.410791	1879.889461	19.841728
54.328895	1879.539480	19.846746
54.944583	1875.337179	19.851763
54.728844	1876.131707	19.856781
54.834386	1872.694189	19.861799
54.723112	1868.634192	19.866816
54.478699	1871.800216	19.871834
55.336261	1892.975350	19.876851
55.083487	1899.172459	19.881869
55.236398	1904.958847	19.886887
54.964604	1895.716575	19.891904
54.981530	1901.369623	19.896922
55.645439	1895.496545	19.901939
55.223600	1903.970380	19.906957
55.255894	1899.638557	19.911975
55.781801	1892.104948	19.916992
55.522495	1893.821545	19.922010
55.770242	1893.694489	19.927027
55.543247	1888.974076	19.932045
55.566762	1893.644571	19.937063
55.673821	1892.734775	19.942080
55.475945	1900.583344	19.947098
56.056665	1891.453674	19.952115
55.660794	1890.774164	19.957133
55.585565	1882.649889	19.962151
55.971597	1888.324003	19.967168
55.690985	1893.935298	19.972186
55.694090	1895.143692	19.977203
55.775833	1909.995828	19.982221
56.285051	1908.890470	19.987239
56.472494	1912.572702	19.992256
55.838870	1913.779866	19.997274
56.462265	1908.291852	20.002291
56.217756	1910.148153	20.007309
56.713164	1920.832670	20.012327
56.770696	1912.447724	20.017344
56.620366	1910.984924	20.022362
56.614575	1918.004934	20.027379
56.674298	1910.585386	20.032397
56.775045	1909.679734	20.037415
57.037782	1917.866425	20.042432
56.661256	1914.857901	20.047450
56.806620	1918.628784	20.052467
56.613421	1912.201978	20.057485
56.775806	1917.655504	20.062503
56.991987	1924.830100	20.067520
57.003962	1924.342327	20.072538
57.462282	1921.499666	20.077555
57.269713	1929.429473	20.082573
57.303483	1926.637548	20.087591
57.279478	1930.084652	20.092608
56.920970	1931.684242	20.097626
57.066860	1926.274194	20.102643
57.185877	1925.409863	20.107661
56.958454	1936.731539	20.112679
57.570425	1944.257570	20.117696
57.169329	1949.101910	20.122714
57.664983	1946.890912	20.127731
57.657159	1953.699802	20.132749
57.835738	1947.517713	20.137767
57.690799	1953.454931	20.142784
57.871162	1968.733507	20.147802
57.844159	1968.333896	20.152819
57.994485	1969.670718	20.157837
57.735480	1969.282207	20.162855
58.100958	1975.855880	20.167872
57.946004	1970.590791	20.172890
58.306698	1972.188164	20.177907
58.580014	1966.707642	20.182925
58.162417	1973.530244	20.187943
58.783241	1972.558886	20.192960
58.845946	1990.620592	20.197978
58.991336	1972.737993	20.202995
59.177266	1977.525084	20.208013
58.887005	1969.052581	20.213031
59.005757	1960.803198	20.218048
58.831606	1964.409541	20.223066
59.030456	1958.331576	20.228083
58.747938	1960.256958	20.233101
58.826440	1953.784412	20.238119
59.448721	1962.523904	20.243136
59.313492	1960.591642	20.248154
58.921508	1957.471916	20.253171
59.256376	1970.292994	20.258189
59.130231	1978.000961	20.263207
59.588111	1971.128119	20.268224
59.487245	1973.201778	20.273242
59.714246	1977.995059	20.278259
59.811533	1971.604776	20.283277
59.581309	1969.056192	20.288295
59.903915	1965.758228	20.293312
59.855807	1976.550027	20.298330
59.831832	1972.877144	20.303347
59.938237	1969.215394	20.308365
59.830417	1973.429927	20.313383
59.969511	1970.706707	20.318400
59.943519	1974.703278	20.323418
59.761262	1973.769375	20.328435
59.536007	1970.907565	20.333453
59.483685	1969.378908	20.338471
59.879894	1970.973873	20.343488
60.300220	1987.227952	20.348506
60.305560	1997.872525	20.353523
60.550659	1992.999217	20.358541
60.480476	2000.663710	20.363559
60.506454	1990.996011	20.368576
60.248396	1994.482953	20.373594
60.433220	1993.355827	20.378611
60.884927	1993.487170	20.383629
60.345252	1995.449689	20.388647
60.840542	1997.193246	20.393664
60.785730	2005.991503	20.398682
60.810188	2026.745020	20.403699
61.187766	2020.683216	20.408717
61.198337	2014.233916	20.413735
61.483481	2012.488269	20.418752
60.719409	2022.344467	20.423770
60.672831	2020.878026	20.428787
61.233341	2019.467959	20.433805
60.936380	2022.247738	20.438823
61.128020	2026.958203	20.443840
61.129192	2043.158075	20.448858
61.336198	2047.512662	20.453875
61.450809	2035.997395	20.458893
61.370234	2043.054419	20.463911
62.026321	2035.112162	20.468928
61.725043	2034.544067	20.473946
61.619761	2045.234404	20.478963
61.783437	2047.686378	20.483981
61.787539	2067.010289	20.488999
62.149189	2062.431151	20.494016
61.993775	2067.704124	20.499034
62.267074	2075.747211	20.504051
62.333324	2063.617762	20.509069
62.583651	2069.900220	20.514087
62.641843	2062.121060	20.519104
62.554567	2067.175059	20.524122
62.377404	2064.390913	20.529139
62.644013	2058.646307	20.534157
62.592508	2058.689222	20.539175
62.734549	2061.627461	20.544192
62.715504	2063.710404	20.549210
62.740005	2064.483079	20.554227
62.937522	2058.727206	20.559245
62.683168	2066.351149	20.564263
62.626916	2067.117541	20.569280
63.006386	2081.452923	20.574298
63.057833	2080.318284	20.579315
63.294322	2086.467205	20.584333
62.905646	2086.771245	20.589351
63.384042	2073.112813	20.594368
63.192479	2081.156146	20.599386
63.182792	2079.497714	20.604403
63.537056	2081.351744	20.609421
63.402682	2082.408108	20.614439
63.339324	2072.142090	20.619456
63.443911	2089.234741	20.624474
63.653388	2102.773046	20.629491
63.594010	2095.242683	20.634509
63.764743	2094.922550	20.639527
63.786367	2102.948272	20.644544
64.036831	2105.538146	20.649562
63.874953	2100.419281	20.654579
64.236117	2098.743772	20.659597
64.364296	2109.085121	20.664615
64.191531	2096.645933	20.669632
64.216620	2098.384268	20.674650
63.799277	2098.683332	20.679667
64.211196	2099.253288	20.684685
64.141393	2121.773288	20.689703
64.422015	2124.374221	20.694720
64.542548	2121.341437	20.699738
64.466151	2126.671480	20.704755
64.921073	2117.397291	20.709773
64.502360	2121.502766	20.714791
64.630505	2126.993282	20.719808
64.673074	2123.720228	20.724826
64.826326	2141.250307	20.729843
65.440538	2144.344974	20.734861
64.975224	2151.373951	20.739879
65.067921	2146.467671	20.744896
65.577527	2142.707998	20.749914
65.224182	2134.592466	20.754931
65.399959	2144.509778	20.759949
65.209717	2137.927781	20.764967
65.420031	2138.456736	20.769984
65.118266	2143.560142	20.775002
65.329508	2160.203771	20.780019
65.507686	2159.756228	20.785037
65.712536	2159.875752	20.790055
65.993352	2161.665553	20.795072
66.432926	2160.845670	20.800090
65.942706	2152.862036	20.805107
66.245703	2159.066840	20.810125
66.126505	2156.081078	20.815143
65.881116	2161.169344	20.820160
66.050613	2165.892783	20.825178
66.341189	2155.009486	20.830195
66.208991	2153.420738	20.835213
66.233519	2161.843695	20.840231
66.135870	2152.984292	20.845248
66.407493	2170.808304	20.850266
66.378372	2176.355035	20.855283
66.880621	2182.396075	20.860301
66.732218	2181.983918	20.865319
66.992181	2177.348093	20.870336
66.947182	2176.998637	20.875354
66.822049	2173.903341	20.880371
67.132507	2176.098786	20.885389
67.071979	2176.215704	20.890407
66.786331	2176.033351	20.895424
67.258370	2180.027684	20.900442
67.216233	2195.347626	20.905459
67.370664	2194.692347	20.910477
67.312069	2199.928097	20.915495
67.346400	2213.560204	20.920512
67.576115	2201.821652	20.925530
67.467650	2198.332387	20.930547
67.744536	2204.778003	20.935565
67.453703	2200.417832	20.940583
67.568806	2203.543367	20.945600
67.886780	2198.623870	20.950618
67.625681	2197.478227	20.955635
67.723839	2207.537134	20.960653
68.074491	2220.482161	20.965671
68.326341	2220.524889	20.970688
68.441851	2214.065388	20.975706
68.179239	2219.364668	20.980723
68.631044	2215.699250	20.985741
68.292125	2212.735279	20.990759
68.887830	2212.648388	20.995776
68.623689	2207.955803	21.000794
68.705472	2213.327366	21.005811
68.765987	2210.105138	21.010829
69.216332	2212.357574	21.015847
68.980501	2219.716726	21.020864
69.007727	2217.396036	21.025882
68.913913	2222.470039	21.030899
69.301306	2214.352033	21.035917
69.452034	2214.473726	21.040935
69.228790	2212.488949	21.045952
69.424595	2208.885733	21.050970
69.268587	2213.410855	21.055987
69.395948	2208.495971	21.061005
69.128073	2205.707079	21.066023
69.147241	2210.302591	21.071040
69.122512	2205.780797	21.076058
69.180036	2201.908890	21.081075
69.446447	2216.688162	21.086093
69.556573	2220.998005	21.091111
69.575055	2235.951849	21.096128
69.681518	2219.990838	21.101146
69.835556	2236.810772	21.106163
69.694043	2228.605199	21.111181
69.770835	2240.750478	21.116199
69.797947	2249.782192	21.121216
69.809910	2248.893591	21.126234
69.989763	2247.672545	21.131251
70.422090	2263.931309	21.136269
70.574742	2273.041204	21.141287
70.415775	2269.149548	21.146304
70.680753	2267.757361	21.151322
70.643975	2274.498319	21.156339
70.872510	2276.463595	21.161357
70.816206	2273.692041	21.166375
70.771167	2273.421492	21.171392
70.906077	2266.245659	21.176410
71.007574	2277.544419	21.181427
70.656520	2271.887050	21.186445
71.475902	2274.794948	21.191463
71.214499	2281.946675	21.196480
71.262017	2281.402826	21.201498
71.201829	2291.104703	21.206515
71.406394	2293.518744	21.211533
71.321570	2288.312006	21.216551
71.208170	2285.918657	21.221568
71.752103	2281.140476	21.226586
71.367909	2296.621403	21.231603
71.444467	2303.887461	21.236621
72.033154	2306.945128	21.241639
71.804376	2316.449351	21.246656
72.583833	2312.571618	21.251674
72.361741	2308.061783	21.256691
72.396283	2304.373352	21.261709
72.464308	2302.178814	21.266727
72.512674	2296.944894	21.271744
72.392328	2294.107625	21.276762
72.623700	2301.955394	21.281779
72.754523	2301.673071	21.286797
72.921815	2299.478761	21.291815
72.957041	2303.194391	21.296832
72.857314	2295.061143	21.301850
72.822833	2298.917093	21.306867
73.250976	2296.814470	21.311885
73.318694	2289.030563	21.316903
72.969134	2275.028286	21.321920
73.010652	2269.369377	21.326938
72.709429	2287.056017	21.331955
72.585406	2293.498200	21.336973
73.240576	2283.829603	21.341991
72.857055	2297.101170	21.347008
72.891945	2287.583407	21.352026
73.324834	2302.731177	21.357043
73.333640	2307.514547	21.362061
73.387216	2307.048650	21.367079
73.481181	2321.006040	21.372096
73.323099	2313.415305	21.377114
73.784830	2324.578754	21.382131
73.941132	2336.878913	21.387149
73.959388	2338.807708	21.392167
73.785174	2344.222575	21.397184
74.378617	2336.712918	21.402202
74.377231	2340.058717	21.407219
74.451165	2330.967198	21.412237
74.977210	2333.744324	21.417255
74.578563	2338.752500	21.422272
74.660675	2330.634931	21.427290
74.502918	2332.016894	21.432307
74.526359	2337.053622	21.437325
74.537373	2336.136759	21.442343
74.728118	2337.315785	21.447360
75.080634	2349.127578	21.452378
75.526994	2356.383060	21.457395
75.305433	2352.516973	21.462413
75.528671	2327.861479	21.467431
75.022683	2331.684002	21.472448
75.385946	2335.480800	21.477466
75.166700	2347.735655	21.482483
74.798608	2354.317093	21.487501
75.367341	2345.741389	21.492519
75.221288	2352.597336	21.497536
75.761031	2351.730190	21.502554
75.572329	2352.315355	21.507571
75.721290	2361.116578	21.512589
75.909342	2364.259116	21.517607
75.994958	2375.664578	21.522624
75.827113	2371.976281	21.527642
75.531522	2371.757609	21.532659
75.594197	2374.061336	21.537677
76.049824	2378.190841	21.542695
76.049647	2399.014926	21.547712
76.243462	2391.488956	21.552730
76.363133	2393.405023	21.557747
76.287218	2405.034646	21.562765
76.628927	2390.756701	21.567783
76.792604	2412.271563	21.572800
76.965810	2424.572291	21.577818
76.952548	2420.219075	21.582835
77.045890	2427.725574	21.587853
76.743075	2421.413597	21.592871
76.789032	2418.644936	21.597888
77.424699	2414.635062	21.602906
77.508805	2419.005839	21.607923
77.569648	2425.188709	21.612941
77.492065	2420.899225	21.617959
77.323406	2414.342149	21.622976
77.136403	2418.588128	21.627994
77.433508	2415.859021	21.633011
77.360155	2432.421248	21.638029
78.167536	2432.001364	21.643047
77.648784	2435.879562	21.648064
77.664548	2440.867024	21.653082
78.007651	2443.060545	21.658099
77.997662	2441.575713	21.663117
78.437160	2435.825993	21.668135
78.309460	2439.131635	21.673152
78.278168	2437.463930	21.678170
78.670600	2437.705561	21.683187
77.793524	2440.020818	21.688205
78.103055	2435.976821	21.693223
78.518559	2454.895835	21.698240
78.668488	2459.625574	21.703258
78.745517	2461.892345	21.708275
78.955422	2455.780921	21.713293
79.145637	2456.530807	21.718311
78.901847	2456.891054	21.723328
79.001719	2455.190173	21.728346
79.383038	2453.912301	21.733363
79.016170	2452.467601	21.738381
79.559487	2445.114090	21.743399
79.036588	2459.417567	21.748416
79.731654	2467.129638	21.753434
79.986174	2469.564281	21.758451
79.820156	2475.265110	21.763469
79.886373	2482.040507	21.768487
79.686358	2478.502409	21.773504
79.835334	2473.372607	21.778522
80.000989	2471.468895	21.783539
79.767019	2474.223093	21.788557
79.780296	2471.134464	21.793575
79.953075	2475.308308	21.798592
80.258645	2486.038689	21.803610
80.219128	2499.537402	21.808627
80.442714	2495.162841	21.813645
80.742240	2494.020869	21.818663
80.315993	2491.518702	21.823680
80.303993	2487.424074	21.828698
80.667356	2492.966221	21.833715
80.235310	2499.279993	21.838733
80.721357	2504.850264	21.843751
80.759627	2521.521330	21.848768
80.769583	2516.302832	21.853786
81.308013	2525.794272	21.858803
81.079054	2516.384005	21.863821
81.435321	2522.214479	21.868839
81.246322	2522.313654	21.873856
81.684383	2528.225999	21.878874
81.702930	2535.349746	21.883891
81.488116	2534.020086	21.888909
81.796542	2530.058301	21.893927
81.769721	2529.930074	21.898944
81.583965	2528.892537	21.903962
81.919595	2527.432451	21.908979
81.704575	2526.727735	21.913997
82.088500	2524.098630	21.919015
82.352856	2540.027320	21.924032
82.185380	2549.711429	21.929050
82.483793	2538.391128	21.934067
82.343649	2544.116329	21.939085
82.700491	2546.446581	21.944103
82.608347	2543.888904	21.949120
82.851783	2546.034931	21.954138
82.985835	2538.022751	21.959155
83.090031	2544.580761	21.964173
83.348172	2532.935380	21.969191
83.127561	2541.911370	21.974208
83.040991	2543.825049	21.979226
83.262205	2541.205653	21.984243
83.188908	2535.615147	21.989261
83.194367	2538.748450	21.994279
83.170116	2534.122346	21.999296
83.078599	2552.133033	22.004314
83.323833	2557.314973	22.009331
83.418483	2570.985244	22.014349
83.691877	2557.503746	22.019367
83.981522	2563.938024	22.024384
83.792109	2565.716324	22.029402
84.143062	2559.933096	22.034419
83.808862	2577.429508	22.039437
83.846573	2586.021029	22.044455
84.233992	2595.668724	22.049472
84.092112	2589.457719	22.054490
84.497746	2586.424375	22.059507
84.271203	2592.071600	22.064525
84.602020	2585.483549	22.069543
84.582421	2595.087703	22.074560
84.547195	2611.770367	22.079578
84.647309	2614.298657	22.084595
84.549870	2605.640990	22.089613
84.636439	2606.590177	22.094631
85.042078	2611.251488	22.099648
84.874290	2630.539814	22.104666
85.148648	2627.542812	22.109683
85.114859	2634.504366	22.114701
85.514768	2630.086366	22.119719
85.608106	2630.977684	22.124736
85.289212	2629.411831	22.129754
85.397749	2624.720713	22.134771
85.695448	2653.136280	22.139789
85.827807	2654.718993	22.144807
85.820285	2656.001694	22.149824
85.742600	2659.397381	22.154842
86.015863	2654.528952	22.159859
86.210062	2653.529719	22.164877
86.390805	2657.191062	22.169895
86.532730	2665.103503	22.174912
86.284035	2679.320008	22.179930
86.863641	2671.531484	22.184947
86.793784	2679.382428	22.189965
86.719202	2672.078292	22.194983
86.690229	2671.331797	22.200000
86.957720	2681.004639	22.205018
87.068103	2671.342286	22.210035
87.132496	2670.218207	22.215053
87.426333	2672.129110	22.220071
87.482751	2664.703456	22.225088
87.374017	2674.782415	22.230106
87.313800	2663.139486	22.235123
87.605558	2668.781279	22.240141
87.791758	2675.225492	22.245159
87.781132	2686.352709	22.250176
87.589380	2701.573433	22.255194
88.085724	2690.436645	22.260211
87.603730	2696.272264	22.265229
88.025039	2685.222982	22.270247
87.862570	2688.947573	22.275264
87.802812	2690.506734	22.280282
88.177094	2689.643404	22.285299
88.307177	2705.195603	22.290317
88.303655	2707.677019	22.295335
88.646190	2711.259371	22.300352
88.529293	2714.983139	22.305370
88.883065	2709.568692	22.310387
88.729843	2710.416582	22.315405
88.384195	2710.571862	22.320423
88.822056	2717.342775	22.325440
88.924096	2734.423816	22.330458
88.905209	2735.970265	22.335475
88.782563	2733.862358	22.340493
89.181166	2742.343758	22.345511
89.435236	2737.999080	22.350528
89.269587	2743.374851	22.355546
89.481596	2748.483148	22.360563
89.804549	2758.283057	22.365581
89.660668	2760.559228	22.370599
90.003509	2756.257448	22.375616
89.689677	2763.808944	22.380634
90.064476	2753.360266	22.385651
90.445574	2754.919798	22.390669
90.346536	2762.292457	22.395687
90.529752	2761.228659	22.400704
90.357805	2762.937962	22.405722
90.650845	2755.970716	22.410739
90.439930	2755.167507	22.415757
90.584222	2765.412025	22.420775
91.359906	2773.509276	22.425792
90.920990	2773.404581	22.430810
91.298045	2772.357756	22.435827
91.114050	2764.568894	22.440845
90.936867	2779.102514	22.445863
91.483431	2773.023454	22.450880
90.837488	2781.737959	22.455898
90.882482	2781.756288	22.460915
91.029453	2786.859005	22.465933
91.428381	2793.200496	22.470951
91.807084	2792.068195	22.475968
91.683167	2809.828567	22.480986
91.862317	2810.908444	22.486003
91.984172	2810.614894	22.491021
91.661267	2800.360718	22.496039
91.932392	2800.425678	22.501056
91.899157	2812.266653	22.506074
92.252103	2816.219823	22.511091
92.318702	2826.520734	22.516109
92.204282	2835.341361	22.521127
92.557450	2825.801853	22.526144
92.430378	2827.832373	22.531162
92.553432	2836.909319	22.536179
92.910124	2847.066951	22.541197
92.848530	2852.723132	22.546215
93.171196	2850.911561	22.551232
93.385117	2846.427963	22.556250
93.227722	2848.340146	22.561267
93.058970	2839.160145	22.566285
93.069337	2848.526183	22.571303
93.502139	2857.734512	22.576320
93.579802	2860.029640	22.581338
94.002356	2863.634204	22.586355
94.122134	2869.208319	22.591373
93.976923	2867.719388	22.596391
93.447964	2868.604060	22.601408
93.780592	2866.768832	22.606426
94.144972	2857.063430	22.611443
94.328435	2871.559558	22.616461
94.431402	2885.295044	22.621479
94.619803	2886.922652	22.626496
94.811580	2887.359850	22.631514
94.153657	2880.857164	22.636531
94.770064	2887.237209	22.641549
94.461669	2881.973796	22.646567
94.820376	2887.680918	22.651584
94.742465	2897.297525	22.656602
95.145390	2901.009326	22.661619
95.149439	2905.253893	22.666637
95.325446	2906.848726	22.671655
95.785060	2901.386078	22.676672
95.682988	2905.833486	22.681690
95.387011	2913.603179	22.686707
95.750964	2903.042492	22.691725
95.790638	2906.429306	22.696743
95.861500	2897.293796	22.701760
95.544210	2897.621380	22.706778
95.715374	2891.358069	22.711795
95.868524	2903.794827	22.716813
95.684698	2916.199171	22.721831
96.101453	2914.508568	22.726848
96.143426	2927.631873	22.731866
95.944116	2924.576473	22.736883
96.435880	2946.390911	22.741901
96.685103	2949.407190	22.746919
96.875701	2947.499521	22.751936
96.730830	2942.545028	22.756954
96.850085	2947.885692	22.761971
96.905962	2942.615690	22.766989
96.392688	2968.173052	22.772007
97.207581	2961.019813	22.777024
97.144043	2970.346993	22.782042
97.276448	2974.208503	22.787059
97.749508	2964.968915	22.792077
97.665313	2979.664874	22.797095
97.555721	2982.674252	22.802112
98.040738	2991.461007	22.807130
98.141522	2991.593687	22.812147
97.967885	2991.106559	22.817165
98.457999	2993.551707	22.822183
98.243351	2988.002142	22.827200
98.626091	2981.175410	22.832218
98.545225	2991.991888	22.837235
98.647227	2982.627365	22.842253
98.501847	2978.259995	22.847271
98.697236	2986.246263	22.852288
98.249950	3003.489371	22.857306
98.462307	2999.577254	22.862323
98.879757	2999.931756	22.867341
98.276326	3014.721718	22.872359
98.911714	3025.959398	22.877376
98.988104	3031.660297	22.882394
99.098580	3034.875077	22.887411
99.529020	3047.337927	22.892429
99.645723	3054.361283	22.897447
99.874357	3064.116169	22.902464
99.943315	3056.865138	22.907482
99.654927	3052.438093	22.912499
100.414394	3054.743207	22.917517
100.642025	3063.721822	22.922535
100.462826	3047.820613	22.927552
100.560594	3053.133113	22.932570
100.198631	3054.635496	22.937587
100.524324	3046.795064	22.942605
100.568398	3065.346827	22.947623
100.926834	3081.889345	22.952640
100.591140	3077.498112	22.957658
100.761845	3081.577736	22.962675
100.938676	3074.688542	22.967693
100.808583	3078.471264	22.972711
100.887463	3078.979811	22.977728
101.489089	3094.638373	22.982746
101.123733	3106.989227	22.987763
101.510920	3101.550492	22.992781
101.672524	3104.788835	22.997799
101.826580	3100.873206	23.002816
101.762747	3106.722347	23.007834
101.581249	3108.041806	23.012851
102.177932	3116.899503	23.017869
102.204214	3119.685617	23.022887
102.116117	3126.346560	23.027904
102.248404	3125.101347	23.032922
101.976698	3127.100905	23.037939
102.216312	3127.738925	23.042957
102.237665	3124.118673	23.047975
102.794094	3137.960056	23.052992
102.971949	3139.725058	23.058010
102.627147	3147.549844	23.063027
102.793222	3148.268823	23.068045
102.496618	3151.064498	23.073063
102.866045	3146.060936	23.078080
103.287116	3166.580037	23.083098
103.046851	3171.383722	23.088115
103.585561	3160.969098	23.093133
103.454578	3171.664130	23.098151
103.665876	3170.094068	23.103168
103.646054	3185.490262	23.108186
103.670612	3203.492883	23.113203
104.129627	3182.577301	23.118221
104.008185	3195.372905	23.123239
104.203207	3201.749644	23.128256
104.493822	3197.105602	23.133274
104.391470	3203.816150	23.138291
104.672035	3210.072178	23.143309
104.354101	3209.304651	23.148327
104.678683	3213.114010	23.153344
104.931602	3207.689967	23.158362
104.703578	3214.540145	23.163379
104.631433	3215.185981	23.168397
104.842898	3238.105185	23.173415
105.751341	3223.232793	23.178432
105.458815	3228.562305	23.183450
105.512784	3229.254664	23.188467
105.625822	3232.917265	23.193485
105.542480	3230.279205	23.198503
105.667962	3245.857842	23.203520
106.007477	3250.832681	23.208538
106.396404	3264.185935	23.213555
106.522589	3256.534482	23.218573
106.650380	3250.164218	23.223591
106.288401	3246.326248	23.228608
106.338703	3240.870814	23.233626
106.944967	3249.641857	23.238643
107.040459	3235.332384	23.243661
107.049952	3244.951264	23.248679
107.091759	3238.512412	23.253696
107.047389	3240.952958	23.258714
107.135972	3246.238547	23.263731
107.197437	3246.702483	23.268749
107.418045	3261.827512	23.273767
107.616032	3262.068059	23.278784
107.790005	3256.842588	23.283802
107.419709	3272.842954	23.288819
107.564337	3266.179670	23.293837
107.657831	3271.701216	23.298855
107.762295	3266.196257	23.303872
107.986190	3277.100877	23.308890
108.056800	3286.451391	23.313907
108.337917	3292.685268	23.318925
108.155469	3283.267311	23.323943
108.162624	3295.206431	23.328960
108.448580	3291.547846	23.333978
108.312800	3311.403167	23.338995
108.523123	3305.588079	23.344013
108.654438	3306.722825	23.349031
108.666923	3315.492240	23.354048
109.100167	3323.674956	23.359066
109.110123	3336.645762	23.364083
109.405885	3329.854621	23.369101
109.499590	3341.587679	23.374119
109.563335	3334.498322	23.379136
109.904743	3329.069848	23.384154
109.512944	3328.796796	23.389171
109.645125	3334.192362	23.394189
109.830348	3336.211886	23.399207
110.257756	3348.369264	23.404224
110.306669	3349.759955	23.409242
109.972189	3362.806836	23.414259
110.217090	3342.618994	23.419277
110.753554	3347.218972	23.424295
110.517117	3361.039558	23.429312
110.647285	3358.052402	23.434330
110.718517	3362.308644	23.439347
111.155577	3366.719043	23.444365
111.277904	3378.558111	23.449383
111.356045	3377.343458	23.454400
111.494394	3372.972572	23.459418
111.547532	3379.822950	23.464435
111.626693	3377.209910	23.469453
111.595182	3372.117600	23.474471
111.805211	3389.365406	23.479488
111.851721	3386.577572	23.484506
112.012102	3388.001303	23.489523
111.900023	3387.409831	23.494541
112.533133	3391.739020	23.499559
112.191699	3396.861616	23.504576
112.397171	3383.424864	23.509594
112.200958	3403.668507	23.514611
112.397129	3404.127124	23.519629
112.471969	3403.951401	23.524647
112.854683	3413.066863	23.529664
112.944218	3417.736880	23.534682
113.176058	3437.373773	23.539699
113.501761	3430.199150	23.544717
113.539700	3429.574704	23.549735
113.491588	3432.432491	23.554752
113.484220	3424.846078	23.559770
113.337863	3432.251674	23.564787
113.954144	3436.867576	23.569805
114.038078	3442.898834	23.574823
113.833433	3460.959715	23.579840
114.288295	3456.100497	23.584858
114.087447	3458.436180	23.589875
114.296471	3457.371456	23.594893
114.298881	3457.832024	23.599911
114.329899	3461.848400	23.604928
114.535265	3463.820595	23.609946
114.592079	3476.803098	23.614963
114.649649	3480.569128	23.619981
115.020300	3484.503892	23.624999
114.972861	3495.002961	23.630016
115.341408	3501.005428	23.635034
115.418568	3502.398018	23.640051
115.663003	3503.483492	23.645069
115.571249	3506.105093	23.650087
115.735782	3511.643990	23.655104
115.833233	3502.838574	23.660122
115.567213	3512.901611	23.665139
115.923886	3528.318020	23.670157
116.328162	3527.705615	23.675175
116.154261	3526.000182	23.680192
116.033346	3525.959285	23.685210
116.450097	3533.563923	23.690227
116.602221	3538.028474	23.695245
117.123376	3542.469929	23.700263
116.805921	3546.051693	23.705280
117.049120	3533.136021	23.710298
117.155138	3539.296415	23.715315
117.288691	3538.107790	23.720333
117.961951	3540.918859	23.725351
117.230970	3544.063557	23.730368
117.456500	3541.664284	23.735386
117.220685	3548.660999	23.740403
117.566676	3552.066226	23.745421
117.747189	3560.954626	23.750439
117.457412	3557.966948	23.755456
118.031661	3565.572175	23.760474
118.122472	3587.598555	23.765491
118.067803	3580.458214	23.770509
118.438398	3583.660746	23.775527
118.474197	3593.951141	23.780544
118.343248	3590.436720	23.785562
118.768841	3604.762940	23.790579
119.034550	3605.037071	23.795597
119.177733	3609.196878	23.800615
118.662747	3608.962059	23.805632
119.175035	3613.171354	23.810650
119.508461	3631.015540	23.815667
119.418860	3638.529112	23.820685
119.804120	3627.601689	23.825703
119.947797	3632.487377	23.830720
119.986362	3632.538278	23.835738
120.392806	3634.882997	23.840755
120.457644	3637.170766	23.845773
120.479668	3644.411190	23.850791
120.426299	3645.795834	23.855808
120.661914	3645.276133	23.860826
120.609516	3648.144094	23.865843
120.576594	3652.931202	23.870861
120.948334	3646.794023	23.875879
121.042184	3647.764219	23.880896
121.169565	3658.709441	23.885914
121.278630	3671.406142	23.890931
121.443410	3669.398285	23.895949
121.227952	3673.118753	23.900967
121.138626	3671.949256	23.905984
121.447091	3686.224451	23.911002
121.898841	3695.969975	23.916019
121.669912	3699.241205	23.921037
121.958787	3699.199232	23.926055
121.926660	3704.750060	23.931072
121.914207	3716.534714	23.936090
121.890919	3729.230097	23.941107
122.061563	3734.326218	23.946125
122.617518	3738.743333	23.951143
122.638727	3747.615750	23.956160
123.077432	3741.086131	23.961178
123.302250	3745.902323	23.966195
123.227029	3752.473102	23.971213
123.259566	3755.592905	23.976231
123.877246	3770.956005	23.981248
123.692735	3768.845043	23.986266
123.781362	3761.218199	23.991283
123.590847	3771.970257	23.996301
124.149254	3765.930046	24.001319
123.596259	3764.432330	24.006336
124.037388	3786.015838	24.011354
124.495022	3794.491645	24.016371
124.641123	3787.689060	24.021389
125.030967	3786.018378	24.026407
124.825960	3787.874991	24.031424
124.921131	3790.486286	24.036442
124.835454	3781.800960	24.041459
125.015024	3790.879001	24.046477
125.121051	3786.544643	24.051495
125.343972	3788.097487	24.056512
125.149526	3794.939467	24.061530
125.326432	3804.636576	24.066547
125.335149	3825.009556	24.071565
125.728694	3814.014441	24.076583
125.702444	3815.085527	24.081600
125.362789	3828.158804	24.086618
125.725887	3831.403588	24.091635
125.862398	3827.948222	24.096653
126.221900	3837.746152	24.101671
126.336900	3864.045935	24.106688
126.386662	3851.548574	24.111706
126.586646	3858.319313	24.116723
126.264566	3867.696931	24.121741
126.646499	3883.778834	24.126759
127.076609	3887.183573	24.131776
127.154415	3883.011431	24.136794
127.356983	3896.814148	24.141811
127.421592	3908.552134	24.146829
127.489485	3908.585815	24.151847
127.691854	3902.670779	24.156864
127.539240	3904.165682	24.161882
128.329165	3915.111420	24.166899
128.464540	3930.622814	24.171917
128.375689	3921.221423	24.176935
128.391520	3916.667594	24.181952
128.404239	3923.474009	24.186970
128.643845	3920.554838	24.191987
128.549500	3934.337817	24.197005
129.168582	3936.232623	24.202023
129.414875	3935.348259	24.207040
129.127086	3950.392540	24.212058
129.584781	3938.225756	24.217075
129.647260	3936.464312	24.222093
129.506479	3931.196425	24.227111
129.741672	3951.871798	24.232128
129.615743	3962.910549	24.237146
129.898678	3962.361331	24.242163
130.133334	3964.423684	24.247181
130.151792	3964.032687	24.252199
130.412822	3969.414570	24.257216
130.388171	3974.992717	24.262234
130.899255	3969.903609	24.267251
130.690050	3983.354263	24.272269
131.015114	3979.869328	24.277287
130.982313	3986.764965	24.282304
130.865716	4001.394234	24.287322
131.290914	3999.446545	24.292339
131.626987	3997.272936	24.297357
131.681040	3995.029880	24.302375
131.802975	3999.546622	24.307392
131.539642	4005.048542	24.312410
131.622703	4020.116847	24.317427
131.633357	4029.770683	24.322445
132.253387	4021.656459	24.327463
132.103488	4033.551231	24.332480
132.348678	4048.789855	24.337498
132.586656	4041.433039	24.342515
132.774439	4045.011498	24.347533
133.124780	4041.913983	24.352551
132.709404	4049.324100	24.357568
133.399021	4065.541032	24.362586
133.775242	4067.824260	24.367603
133.147286	4073.452767	24.372621
133.580150	4070.092964	24.377639
133.593931	4069.213457	24.382656
133.559500	4068.455133	24.387674
133.545165	4061.103118	24.392691
133.902714	4074.193598	24.397709
134.188317	4084.584016	24.402727
134.501602	4097.179581	24.407744
134.125573	4097.368033	24.412762
134.509843	4084.625565	24.417779
134.577809	4089.226537	24.422797
134.661946	4099.579087	24.427815
135.065761	4105.958157	24.432832
134.909237	4117.402657	24.437850
135.268144	4107.451247	24.442867
135.377691	4110.641114	24.447885
135.294599	4117.749845	24.452903
135.610846	4126.778235	24.457920
135.442452	4136.494899	24.462938
135.861180	4133.168863	24.467955
135.662516	4131.732389	24.472973
135.875605	4149.122480	24.477991
136.340258	4150.252404	24.483008
136.339892	4170.816580	24.488026
136.879998	4163.144087	24.493043
136.462146	4172.066561	24.498061
136.788433	4174.928937	24.503079
137.048418	4174.073980	24.508096
136.863097	4183.187291	24.513114
137.273001	4188.526977	24.518131
137.518217	4197.951614	24.523149
137.580559	4202.244167	24.528167
137.577417	4202.895009	24.533184
137.691520	4203.609550	24.538202
138.011594	4202.852497	24.543219
138.302131	4222.648339	24.548237
138.289764	4221.419402	24.553255
137.871856	4227.665270	24.558272
138.289707	4229.954623	24.563290
138.763896	4238.560616	24.568307
138.637244	4246.111808	24.573325
138.695892	4253.728665	24.578343
139.056881	4242.839398	24.583360
138.862559	4248.977646	24.588378
139.250944	4271.040305	24.593395
139.613439	4272.334593	24.598413
139.467747	4277.089031	24.603431
139.950307	4274.523137	24.608448
139.900722	4287.377696	24.613466
140.415033	4285.728503	24.618483
140.440463	4284.023333	24.623501
139.941527	4287.097079	24.628519
140.502477	4289.547095	24.633536
140.272864	4294.355718	24.638554
141.030422	4301.014019	24.643571
140.697203	4313.360657	24.648589
141.051120	4313.838775	24.653607
141.678647	4307.269904	24.658624
141.632154	4306.021056	24.663642
142.020833	4301.610729	24.668659
141.839141	4301.958122	24.673677
141.805033	4302.263456	24.678695
142.090448	4301.710684	24.683712
141.977900	4317.646336	24.688730
142.517409	4317.404120	24.693747
142.511617	4323.569673	24.698765
142.707941	4327.421460	24.703783
142.898917	4309.867145	24.708800
142.684632	4318.685200	24.713818
142.832158	4309.915738	24.718835
142.862637	4320.797633	24.723853
142.946665	4333.514503	24.728871
142.915937	4337.332422	24.733888
143.321022	4337.354311	24.738906
143.302862	4334.440737	24.743923
143.544150	4352.590464	24.748941
143.849877	4362.356071	24.753959
143.677609	4360.972259	24.758976
144.022524	4361.489667	24.763994
144.098887	4368.993321	24.769011
144.307082	4382.707148	24.774029
144.189300	4394.982212	24.779047
144.526808	4387.628602	24.784064
144.459337	4406.076114	24.789082
144.735785	4407.200819	24.794099
144.987506	4416.046920	24.799117
144.906049	4424.585387	24.804135
145.472505	4431.674546	24.809152
145.405286	4439.986682	24.814170
145.309514	4446.336822	24.819187
145.671488	4452.763605	24.824205
145.919836	4472.209650	24.829223
146.228589	4468.439940	24.834240
146.190645	4478.767642	24.839258
146.377934	4470.092880	24.844275
146.392826	4480.475435	24.849293
146.539460	4491.045682	24.854311
146.923244	4486.172077	24.859328
146.719268	4501.115302	24.864346
147.183506	4501.844443	24.869363
147.391150	4511.956926	24.874381
147.301784	4518.119856	24.879399
147.873009	4511.834345	24.884416
147.934498	4512.490856	24.889434
148.052071	4517.620765	24.894451
147.921894	4528.786783	24.899469
148.182659	4531.110256	24.904487
148.464986	4522.840391	24.909504
148.815614	4521.794457	24.914522
148.625082	4529.106412	24.919539
148.983249	4549.150847	24.924557
148.869992	4566.712413	24.929575
149.368037	4550.343941	24.934592
148.835783	4555.802933	24.939610
149.263727	4570.700875	24.944627
149.365227	4572.664214	24.949645
149.347549	4576.704249	24.954663
149.572014	4583.787074	24.959680
149.948070	4594.166771	24.964698
150.075696	4593.534548	24.969715
149.900841	4597.741253	24.974733
149.985637	4618.346255	24.979751
150.190395	4623.538291	24.984768
150.341492	4632.892674	24.989786
150.880729	4633.670044	24.994803
151.238292	4643.159381	24.999821
151.218214	4655.851752	25.004839
151.598100	4654.299345	25.009856
151.726516	4649.734006	25.014874
151.799302	4666.322730	25.019891
151.919225	4666.114682	25.024909
152.134002	4679.310037	25.029927
152.170862	4676.577177	25.034944
152.310838	4675.217022	25.039962
152.244973	4670.543230	25.044979
152.405160	4670.925450	25.049997
152.198502	4695.714367	25.055015
152.829237	4683.444222	25.060032
152.670891	4692.938654	25.065050
152.567330	4698.166388	25.070067
153.443605	4717.684773	25.075085
153.088342	4723.564309	25.080103
153.573875	4720.900038	25.085120
153.402614	4738.887516	25.090138
153.631077	4742.693322	25.095155
153.868971	4741.548247	25.100173
153.754346	4755.202452	25.105191
153.940430	4766.716789	25.110208
154.257102	4758.050030	25.115226
153.951145	4780.461984	25.120243
154.612705	4790.023719	25.125261
154.578925	4799.085188	25.130279
154.999117	4805.540854	25.135296
155.017400	4815.563225	25.140314
155.401271	4815.045519	25.145331
155.544672	4816.472025	25.150349
155.603571	4830.660962	25.155367
155.911486	4836.300907	25.160384
156.284572	4845.156613	25.165402
156.202212	4848.215692	25.170419
156.392042	4844.107850	25.175437
156.416336	4858.804118	25.180455
156.352186	4850.698865	25.185472
157.067420	4856.947344	25.190490
157.035366	4861.485269	25.195507
157.337612	4869.907014	25.200525
157.312447	4881.214624	25.205543
157.808861	4885.275196	25.210560
157.840575	4887.056953	25.215578
157.946425	4884.824613	25.220595
158.097921	4878.197542	25.225613
158.100838	4888.133978	25.230631
158.255371	4892.983585	25.235648
158.485424	4902.395182	25.240666
158.513528	4898.555717	25.245683
158.493498	4910.721117	25.250701
158.625886	4922.834238	25.255719
158.925865	4922.954668	25.260736
159.119521	4937.955904	25.265754
159.278194	4945.655233	25.270771
159.571015	4945.325398	25.275789
159.819207	4959.342736	25.280807
159.689387	4949.445340	25.285824
159.873658	4961.600863	25.290842
160.027976	4964.313541	25.295859
160.560131	4968.393785	25.300877
160.382226	4980.823864	25.305895
160.527437	4991.265207	25.310912
161.042325	4987.930267	25.315930
161.187767	4989.350154	25.320947
161.562793	4988.994813	25.325965
161.480727	4987.820936	25.330983
161.614442	5011.411130	25.336000
161.864952	5011.807617	25.341018
161.830531	5014.016414	25.346035
162.311527	5010.409002	25.351053
162.259422	5019.517643	25.356071
162.236340	5014.884408	25.361088
162.681622	5027.273704	25.366106
162.491634	5045.456968	25.371123
162.631468	5039.687094	25.376141
162.447586	5045.874479	25.381159
162.786831	5053.302510	25.386176
163.116921	5059.993343	25.391194
163.072397	5063.785167	25.396211
163.401805	5064.563865	25.401229
163.536501	5076.348445	25.406247
163.449992	5089.196728	25.411264
164.023832	5086.979429	25.416282
163.859650	5098.283700	25.421299
164.403458	5115.679724	25.426317
164.305906	5114.653467	25.431335
164.438760	5110.646031	25.436352
164.812947	5118.403212	25.441370
164.794302	5130.795816	25.446387
165.117044	5128.216966	25.451405
165.401202	5134.315273	25.456423
165.525230	5138.756213	25.461440
165.779656	5143.959557	25.466458
165.931795	5163.670785	25.471475
166.074685	5156.502030	25.476493
166.100689	5156.008815	25.481511
165.955805	5155.040476	25.486528
166.108532	5165.439706	25.491546
166.481331	5182.401725	25.496563
166.730933	5178.420177	25.501581
166.622059	5201.534099	25.506599
166.814296	5203.334932	25.511616
167.469735	5202.967224	25.516634
167.528432	5232.551192	25.521651
167.820933	5223.253524	25.526669
167.818758	5230.318447	25.531687
167.921511	5232.363733	25.536704
167.819561	5249.977847	25.541722
168.259496	5261.954628	25.546739
168.468482	5255.731929	25.551757
168.439397	5272.308756	25.556775
168.694404	5279.355502	25.561792
168.887182	5276.225647	25.566810
169.041475	5295.270638	25.571827
169.491000	5298.776775	25.576845
169.682302	5303.952175	25.581863
169.600993	5306.180978	25.586880
169.645722	5313.188079	25.591898
169.623849	5325.401394	25.596915
170.059517	5325.585798	25.601933
169.993493	5335.558531	25.606951
170.230988	5339.318856	25.611968
170.618908	5340.394592	25.616986
170.639663	5359.176475	25.622003
171.524069	5370.733311	25.627021
171.574131	5366.432598	25.632039
171.718159	5365.557877	25.637056
171.976849	5364.819866	25.642074
171.751765	5376.976666	25.647091
171.921000	5384.551420	25.652109
171.880015	5393.248144	25.657127
172.245795	5400.296523	25.662144
172.303322	5395.407502	25.667162
172.516392	5415.273601	25.672180
172.837838	5415.955708	25.677197
172.604157	5420.904155	25.682215
172.870183	5439.527743	25.687232
173.413041	5441.109526	25.692250
173.147972	5455.535946	25.697268
173.614849	5448.328946	25.702285
173.791488	5465.287237	25.707303
173.996666	5475.255439	25.712320
174.466284	5477.126483	25.717338
174.219279	5478.323793	25.722356
174.515239	5481.607807	25.727373
174.487039	5491.918773	25.732391
174.614671	5494.086457	25.737408
175.056837	5492.429525	25.742426
174.857873	5514.844558	25.747444
175.059221	5516.634525	25.752461
175.336500	5521.108370	25.757479
175.607629	5525.895687	25.762496
175.759278	5533.972007	25.767514
175.600987	5547.387427	25.772532
176.073005	5552.174846	25.777549
175.967941	5555.673218	25.782567
176.210329	5570.209627	25.787584
176.523765	5569.156836	25.792602
176.302852	5581.524614	25.797620
176.630633	5584.532189	25.802637
176.900273	5596.797873	25.807655
177.218371	5607.613380	25.812672
177.614733	5612.384257	25.817690
178.108833	5626.742385	25.822708
178.358534	5626.873854	25.827725
178.697333	5628.402393	25.832743
178.575065	5630.558736	25.837760
178.699555	5619.323746	25.842778
178.467722	5634.688941	25.847796
178.992267	5641.248512	25.852813
179.174015	5653.351230	25.857831
179.246117	5653.564187	25.862848
179.448900	5653.778767	25.867866
179.509131	5664.890397	25.872884
179.833091	5670.629102	25.877901
180.059761	5671.660674	25.882919
180.066019	5679.409446	25.887936
180.581706	5687.425647	25.892954
180.575657	5700.738413	25.897972
180.559499	5699.806697	25.902989
181.086332	5707.151946	25.908007
181.176230	5716.942626	25.913024
181.610550	5714.096838	25.918042
181.803336	5723.820897	25.923060
181.716784	5715.548307	25.928077
181.742354	5718.281269	25.933095
181.683318	5735.033668	25.938112
182.221484	5733.633151	25.943130
182.162416	5744.028013	25.948148
182.405163	5760.433273	25.953165
182.817172	5771.818153	25.958183
182.717099	5786.518869	25.963200
182.959666	5773.532264	25.968218
183.089433	5796.915752	25.973236
183.466745	5802.775566	25.978253
183.392149	5799.488638	25.983271
183.594982	5817.377534	25.988288
184.108723	5819.885668	25.993306
183.808705	5827.117437	25.998324
183.989951	5845.584261	26.003341
184.808645	5847.406971	26.008359
184.407283	5859.746385	26.013376
184.635441	5872.369147	26.018394
185.053435	5884.425538	26.023412
185.274342	5880.726124	26.028429
185.569779	5883.805107	26.033447
185.469058	5907.720448	26.038464
185.679705	5899.069761	26.043482
185.571919	5903.506168	26.048500
185.781714	5918.821354	26.053517
186.226199	5926.492108	26.058535
185.974265	5930.666999	26.063552
186.603800	5943.706750	26.068570
186.793816	5948.920417	26.073588
186.810662	5957.971372	26.078605
186.863276	5971.906488	26.083623
186.890297	5982.228020	26.088640
187.239563	5995.390634	26.093658
188.068386	6002.458252	26.098676
187.814068	6011.823193	26.103693
188.294328	6007.249747	26.108711
188.269844	6033.457719	26.113728
188.377731	6019.264072	26.118746
188.856191	6025.142836	26.123764
188.662255	6041.111683	26.128781
189.308593	6040.685412	26.133799
189.227607	6055.736908	26.138816
189.083558	6049.853353	26.143834
189.352768	6072.003161	26.148852
189.745250	6078.589895	26.153869
190.067929	6095.058695	26.158887
190.189687	6101.290099	26.163904
190.520953	6104.224610	26.168922
190.347146	6104.337200	26.173940
190.604767	6109.638180	26.178957
190.748906	6124.626054	26.183975
191.153777	6131.700161	26.188992
191.226968	6141.518940	26.194010
191.737971	6152.541308	26.199028
191.837675	6157.712361	26.204045
192.112615	6171.836929	26.209063
192.199144	6181.738872	26.214080
192.478433	6176.035183	26.219098
192.439264	6173.598119	26.224116
192.649333	6194.804001	26.229133
193.026275	6192.238611	26.234151
192.720893	6208.458663	26.239168
193.621824	6219.066427	26.244186
193.498445	6225.137401	26.249204
193.467472	6233.069019	26.254221
194.117747	6239.356569	26.259239
194.027027	6255.249454	26.264256
194.352543	6259.637006	26.269274
194.592019	6268.485929	26.274292
194.938452	6276.424733	26.279309
195.190510	6281.947609	26.284327
195.062707	6282.094030	26.289344
195.338261	6283.225311	26.294362
195.659559	6293.270472	26.299380
195.295212	6301.109134	26.304397
195.657604	6308.815007	26.309415
195.791801	6329.565729	26.314432
196.221966	6332.955144	26.319450
196.355656	6339.948702	26.324468
196.419809	6349.222885	26.329485
196.689093	6354.335859	26.334503
196.478123	6371.390440	26.339520
197.204680	6370.705367	26.344538
197.595081	6386.838672	26.349556
197.997168	6406.145896	26.354573
198.256568	6396.991721	26.359591
198.324414	6405.091026	26.364608
198.568089	6402.982123	26.369626
199.085538	6409.928215	26.374644
198.875527	6429.770151	26.379661
198.849951	6419.413673	26.384679
198.999640	6416.890168	26.389696
198.792597	6425.872254	26.394714
199.433993	6435.396984	26.399732
199.485118	6443.969290	26.404749
199.996779	6451.793895	26.409767
200.648272	6464.038223	26.414784
200.599655	6455.661495	26.419802
200.714847	6456.843163	26.424820
200.569004	6461.806539	26.429837
200.703869	6449.758116	26.434855
200.663596	6462.158167	26.439872
200.916493	6471.582781	26.444890
201.341530	6474.976184	26.449908
201.166008	6485.134008	26.454925
201.642917	6493.964784	26.459943
201.859988	6506.753876	26.464960
202.221017	6530.269383	26.469978
202.217268	6521.427857	26.474996
202.041781	6530.016762	26.480013
202.833523	6540.941719	26.485031
202.907260	6546.893528	26.490048
202.956639	6556.391108	26.495066
203.295904	6568.848574	26.500084
203.003320	6576.354115	26.505101
203.267892	6597.116283	26.510119
203.526817	6607.124036	26.515136
204.041889	6616.283518	26.520154
204.091479	6637.562406	26.525172
204.084233	6647.488762	26.530189
204.650968	6653.729566	26.535207
205.306355	6662.286231	26.540224
205.462545	6678.671150	26.545242
205.552920	6679.181157	26.550260
205.540764	6685.440053	26.555277
205.844409	6690.576150	26.560295
206.215934	6700.395845	26.565312
206.289637	6697.426463	26.570330
206.780771	6702.239605	26.575348
207.248696	6718.575724	26.580365
207.202409	6738.076659	26.585383
207.606259	6738.057717	26.590400
207.360104	6736.398021	26.595418
207.445747	6733.742448	26.600436
207.570754	6753.409132	26.605453
207.682440	6747.693641	26.610471
207.803934	6757.473615	26.615488
208.116552	6779.566970	26.620506
208.866164	6773.110692	26.625524
208.622581	6805.055378	26.630541
208.976897	6802.843862	26.635559
209.105951	6819.128981	26.640576
208.858758	6833.244308	26.645594
209.208906	6825.669923	26.650612
209.454909	6852.973164	26.655629
209.752964	6860.954528	26.660647
209.879205	6877.085452	26.665664
210.280014	6886.155637	26.670682
210.493966	6900.277694	26.675700
210.854832	6908.738556	26.680717
211.444621	6910.445711	26.685735
211.406433	6912.888936	26.690752
211.269330	6933.755450	26.695770
211.640086	6930.360669	26.700788
211.702219	6943.044905	26.705805
211.846433	6954.917598	26.710823
212.265937	6969.853555	26.715840
212.559552	6976.872812	26.720858
212.756156	6983.307461	26.725876
213.082031	6990.252218	26.730893
213.470967	7000.173524	26.735911
213.463076	7009.247815	26.740928
213.627576	7007.100737	26.745946
213.826100	7021.256874	26.750964
213.795288	7031.641724	26.755981
213.973652	7038.161328	26.760999
214.343621	7038.065616	26.766016
214.332461	7056.888964	26.771034
214.562208	7058.485222	26.776052
215.160363	7077.096332	26.781069
215.031214	7082.906468	26.786087
215.466730	7081.888139	26.791104
215.430609	7093.899665	26.796122
215.717596	7110.119262	26.801140
215.720898	7116.290646	26.806157
216.264069	7135.901701	26.811175
216.402874	7135.690670	26.816192
216.878090	7152.265960	26.821210
217.148260	7159.090074	26.826228
217.288900	7167.841267	26.831245
217.070788	7173.873726	26.836263
217.485112	7181.849643	26.841280
217.358434	7189.351539	26.846298
217.931385	7203.363923	26.851316
218.132096	7211.016584	26.856333
218.309321	7224.317528	26.861351
218.936228	7237.901612	26.866368
218.706424	7248.046261	26.871386
219.199216	7260.953689	26.876404
219.762500	7268.833699	26.881421
219.478781	7272.259361	26.886439
219.905574	7279.074769	26.891456
220.085588	7293.439217	26.896474
220.343209	7296.252869	26.901492
220.516884	7309.592314	26.906509
220.429581	7309.208344	26.911527
220.869195	7320.144736	26.916544
220.955469	7345.143901	26.921562
221.406675	7341.676459	26.926580
221.520194	7356.505975	26.931597
221.771640	7362.679609	26.936615
222.281792	7376.424150	26.941632
221.847570	7395.449870	26.946650
222.713186	7397.315910	26.951668
222.775612	7401.713383	26.956685
222.707516	7418.364557	26.961703
223.121619	7428.522083	26.966720
223.267544	7433.777808	26.971738
223.725339	7435.130014	26.976756
224.182743	7451.610499	26.981773
224.477858	7471.724849	26.986791
224.706761	7464.971070	26.991808
224.828557	7461.750944	26.996826
224.785490	7476.516691	27.001844
225.484707	7476.558817	27.006861
225.342509	7479.119434	27.011879
225.332251	7498.280889	27.016896
225.477977	7504.366952	27.021914
225.862300	7508.792949	27.026932
226.176400	7523.916346	27.031949
226.035665	7536.610674	27.036967
226.702858	7541.188098	27.041984
227.084223	7558.813952	27.047002
227.139422	7559.039050	27.052020
227.449079	7568.707897	27.057037
227.230680	7584.284133	27.062055
227.955634	7581.256784	27.067072
227.898249	7587.188430	27.072090
227.999667	7604.817142	27.077108
228.225305	7614.663340	27.082125
228.551066	7633.664958	27.087143
229.278302	7629.295516	27.092160
229.267825	7640.331023	27.097178
229.358169	7642.422723	27.102196
229.444508	7647.602605	27.107213
229.269174	7657.120171	27.112231
229.491650	7654.881854	27.117248
229.968678	7683.315073	27.122266
230.436948	7689.868419	27.127284
230.652906	7689.534800	27.132301
230.237044	7711.415068	27.137319
230.394563	7713.193178	27.142336
231.031932	7741.689766	27.147354
231.143535	7743.876015	27.152372
231.791155	7766.435829	27.157389
231.481646	7771.305228	27.162407
232.238171	7782.034399	27.167424
232.424577	7789.635873	27.172442
232.830088	7799.460305	27.177460
233.158423	7815.898196	27.182477
232.738235	7826.079300	27.187495
233.249601	7833.601472	27.192512
233.455389	7837.982906	27.197530
233.887721	7855.620001	27.202548
234.216446	7860.364184	27.207565
234.001732	7870.696232	27.212583
234.481209	7874.554929	27.217600
234.702856	7888.117743	27.222618
235.234088	7902.594969	27.227636
235.608014	7909.437837	27.232653
235.495377	7919.668682	27.237671
236.013821	7929.320796	27.242688
235.889049	7936.412280	27.247706
235.970352	7936.680650	27.252724
236.526451	7954.961435	27.257741
236.552199	7963.349000	27.262759
237.050971	7978.308088	27.267776
236.760735	7987.436562	27.272794
237.379230	7998.910453	27.277812
237.577730	8009.098919	27.282829
237.684799	8012.864445	27.287847
238.294258	8021.432103	27.292864
238.210121	8033.113956	27.297882
238.938816	8060.586467	27.302900
239.172514	8066.330599	27.307917
239.165188	8068.279794	27.312935
239.695416	8070.659382	27.317952
240.015823	8085.848553	27.322970
240.194005	8087.213042	27.327988
240.455003	8086.967073	27.333005
240.600463	8099.604325	27.338023
240.897764	8109.190151	27.343040
241.286367	8107.686614	27.348058
241.483964	8108.981764	27.353076
241.747351	8112.953291	27.358093
241.605628	8129.957606	27.363111
241.842333	8131.622325	27.368128
241.922662	8135.770917	27.373146
242.132205	8148.290822	27.378164
242.408163	8151.319573	27.383181
242.476356	8171.817517	27.388199
242.936099	8170.435429	27.393216
243.206137	8187.659431	27.398234
243.184111	8193.099539	27.403252
243.799178	8209.114011	27.408269
243.634610	8224.483454	27.413287
244.410438	8235.247754	27.418304
244.521107	8241.885733	27.423322
244.626270	8254.611488	27.428340
245.239391	8253.757861	27.433357
245.461875	8269.312963	27.438375
245.413553	8271.454871	27.443392
245.803027	8275.507708	27.448410
245.973200	8278.341526	27.453428
246.289826	8273.919448	27.458445
246.296555	8305.145579	27.463463
246.688564	8298.779528	27.468480
246.425932	8309.630781	27.473498
246.741387	8318.686633	27.478516
247.221020	8334.075221	27.483533
247.398799	8349.751050	27.488551
247.343011	8351.622624	27.493568
247.738638	8370.999228	27.498586
247.898901	8377.383230	27.503604
248.216456	8392.737272	27.508621
248.583666	8418.846235	27.513639
248.750083	8430.053402	27.518656
249.248656	8438.193470	27.523674
249.229615	8464.640835	27.528692
249.390016	8467.539356	27.533709
249.521494	8492.308835	27.538727
249.757713	8500.531072	27.543744
250.299603	8509.624161	27.548762
250.226528	8525.080549	27.553780
250.888271	8538.799057	27.558797
250.779956	8557.711770	27.563815
251.354692	8565.786292	27.568832
251.575576	8592.691929	27.573850
251.724372	8598.888374	27.578868
252.169695	8613.755322	27.583885
252.405618	8631.142941	27.588903
252.885397	8645.625656	27.593920
253.238435	8652.986695	27.598938
253.053139	8668.896474	27.603956
253.710699	8669.156669	27.608973
253.761145	8685.755684	27.613991
254.339979	8689.292743	27.619008
254.193673	8703.668366	27.624026
254.643786	8720.959371	27.629044
254.632048	8727.234680	27.634061
254.898939	8746.290868	27.639079
255.210097	8749.194231	27.644096
255.576603	8770.526964	27.649114
256.165997	8778.438265	27.654132
256.376316	8790.295471	27.659149
256.695155	8804.181554	27.664167
256.562153	8802.652330	27.669184
257.107732	8817.680541	27.674202
257.306154	8831.920173	27.679220
257.441315	8837.771541	27.684237
257.566641	8841.452289	27.689255
257.743487	8852.588620	27.694272
258.169304	8872.876613	27.699290
258.253103	8890.443010	27.704308
258.737146	8901.565976	27.709325
258.873622	8915.925879	27.714343
259.214050	8928.826776	27.719360
259.670863	8933.383839	27.724378
259.560774	8949.196831	27.729396
260.047305	8957.279029	27.734413
260.241819	8962.208698	27.739431
260.610764	8979.541076	27.744448
260.794470	8984.674508	27.749466
260.903108	9008.886267	27.754484
261.160233	9006.162462	27.759501
261.484958	9025.636105	27.764519
261.968489	9037.586432	27.769536
262.120504	9049.140370	27.774554
262.309657	9063.940464	27.779572
262.854971	9063.043755	27.784589
262.853231	9073.734607	27.789607
263.066212	9092.916415	27.794624
263.421662	9084.569912	27.799642
263.667767	9106.891171	27.804660
263.650911	9112.908516	27.809677
263.634890	9119.396164	27.814695
263.839342	9133.152022	27.819712
264.134583	9145.005624	27.824730
263.983080	9173.400680	27.829748
265.021460	9185.823020	27.834765
264.938924	9209.913440	27.839783
264.968253	9223.996740	27.844800
265.314876	9239.735276	27.849818
265.914896	9256.649684	27.854836
266.381391	9271.213904	27.859853
266.445980	9294.441548	27.864871
266.988688	9305.419804	27.869888
267.731191	9303.573423	27.874906
267.378183	9327.437995	27.879924
267.737298	9333.835379	27.884941
268.255755	9353.702096	27.889959
268.434187	9354.836159	27.894976
268.428956	9362.657740	27.899994
268.684945	9391.993316	27.905012
269.279364	9391.862440	27.910029
269.856083	9397.366971	27.915047
270.117683	9410.987790	27.920064
270.221344	9424.604945	27.925082
270.358967	9436.688650	27.930100
270.941220	9433.702311	27.935117
271.283896	9452.431622	27.940135
271.226654	9464.476410	27.945152
271.519180	9467.433324	27.950170
271.651755	9480.405055	27.955188
272.136262	9489.384482	27.960205
272.310764	9509.519946	27.965223
272.705366	9514.778354	27.970240
272.821923	9531.945560	27.975258
273.057544	9533.926311	27.980276
273.453656	9550.730852	27.985293
273.550258	9561.337118	27.990311
273.749657	9571.516832	27.995328
274.275525	9578.093406	28.000346
274.700656	9605.183215	28.005364
274.733418	9605.336078	28.010381
275.141056	9607.874000	28.015399
274.899052	9624.724894	28.020416
275.685663	9635.807220	28.025434
276.035407	9653.266373	28.030452
276.500340	9655.157542	28.035469
276.594461	9657.236249	28.040487
276.786749	9675.433651	28.045504
277.458270	9681.343344	28.050522
277.491120	9699.739400	28.055540
277.765560	9708.903395	28.060557
277.950691	9704.580514	28.065575
278.148087	9721.558420	28.070592
278.882302	9716.669603	28.075610
279.065606	9726.068898	28.080628
279.503782	9739.510745	28.085645
279.828958	9735.873168	28.090663
279.641085	9739.325311	28.095680
280.248209	9745.977622	28.100698
280.234358	9755.189959	28.105716
280.544841	9761.238327	28.110733
280.911573	9777.937168	28.115751
280.759377	9786.492358	28.120768
281.311768	9790.179015	28.125786
281.052552	9797.317526	28.130804
281.015410	9807.281835	28.135821
281.359292	9828.774041	28.140839
281.559642	9843.064665	28.145856
281.980510	9856.010441	28.150874
282.079253	9871.980945	28.155892
282.698874	9897.345197	28.160909
283.006181	9905.256971	28.165927
282.755430	9930.157707	28.170944
283.501423	9950.365150	28.175962
283.751400	9963.710344	28.180980
283.922489	9980.200052	28.185997
284.423984	9997.885192	28.191015
284.684395	10012.640149	28.196032
284.890651	10021.979165	28.201050
285.072296	10053.553407	28.206068
285.662780	10066.962159	28.211085
285.858171	10079.400336	28.216103
286.106639	10105.836545	28.221120
286.394870	10114.430244	28.226138
287.137596	10125.137691	28.231156
287.209626	10137.140560	28.236173
287.580439	10149.557619	28.241191
287.658927	10159.355602	28.246208
288.303807	10171.505565	28.251226
288.189061	10177.968000	28.256244
288.290289	10195.614992	28.261261
289.310133	10214.317929	28.266279
289.059254	10231.107611	28.271296
289.924161	10240.779288	28.276314
290.231245	10257.513163	28.281332
290.421221	10269.652357	28.286349
290.710450	10268.337881	28.291367
291.041683	10281.326412	28.296384
291.412119	10292.799546	28.301402
291.429079	10304.643805	28.306420
291.708994	10320.889430	28.311437
292.218592	10327.550915	28.316455
292.087493	10349.793825	28.321472
292.862779	10356.896794	28.326490
293.099562	10367.525764	28.331508
293.011418	10385.890930	28.336525
293.578367	10379.594654	28.341543
293.576541	10401.166935	28.346560
293.834211	10409.434023	28.351578
294.123538	10426.353965	28.356596
294.316903	10447.144243	28.361613
294.791214	10457.568709	28.366631
294.767913	10487.180258	28.371648
295.443849	10495.738659	28.376666
295.561969	10513.879033	28.381684
295.678889	10530.137742	28.386701
296.179818	10552.872340	28.391719
296.543634	10576.534648	28.396736
296.801001	10576.848101	28.401754
296.900068	10592.831801	28.406772
296.994029	10608.102718	28.411789
297.722100	10622.712276	28.416807
298.046092	10646.137782	28.421824
298.454452	10661.896270	28.426842
298.623858	10673.426390	28.431860
298.973428	10693.033662	28.436877
299.252241	10699.939830	28.441895
299.577409	10725.515527	28.446912
299.821730	10735.221527	28.451930
300.387744	10746.686407	28.456948
300.362600	10769.058464	28.461965
300.768908	10766.655209	28.466983
301.015846	10781.198172	28.472000
301.533015	10790.975131	28.477018
301.446650	10806.201834	28.482036
302.098307	10812.174998	28.487053
302.464990	10817.703386	28.492071
302.684367	10846.889110	28.497088
303.125660	10839.213571	28.502106
303.212751	10855.594066	28.507124
303.272374	10874.217585	28.512141
303.846035	10884.759345	28.517159
303.885861	10904.636389	28.522176
304.207933	10909.218209	28.527194
304.594507	10923.808876	28.532212
304.923998	10947.824363	28.537229
305.417535	10942.126709	28.542247
305.419276	10981.627778	28.547264
305.698398	10989.219199	28.552282
306.114051	11007.774450	28.557300
306.344856	11019.683547	28.562317
306.760162	11021.159519	28.567335
306.810476	11048.550116	28.572352
306.945104	11059.179695	28.577370
307.410770	11089.741816	28.582388
307.816253	11104.440178	28.587405
308.188097	11123.873902	28.592423
308.323182	11133.590905	28.597440
308.679001	11162.799955	28.602458
309.327617	11171.047188	28.607476
309.639148	11193.515420	28.612493
310.142391	11199.275139	28.617511
310.452951	11219.189046	28.622528
310.765723	11222.900899	28.627546
311.109226	11234.337783	28.632564
311.212744	11246.573253	28.637581
311.577907	11268.029050	28.642599
311.943031	11285.493638	28.647616
312.450487	11294.192476	28.652634
312.586747	11302.851579	28.657652
312.921798	11322.202859	28.662669
313.163670	11327.845679	28.667687
314.025645	11350.669943	28.672704
314.014231	11351.578101	28.677722
314.231626	11364.834673	28.682740
314.277544	11370.820808	28.687757
314.697217	11387.159142	28.692775
315.033196	11411.729953	28.697792
315.601384	11422.149728	28.702810
315.259544	11435.718145	28.707828
315.726453	11447.126356	28.712845
316.148771	11454.752373	28.717863
316.192218	11478.106034	28.722880
316.647903	11500.400485	28.727898
317.119952	11510.961676	28.732916
317.369451	11528.564595	28.737933
317.709067	11542.016867	28.742951
317.811004	11568.989641	28.747968
318.107931	11575.710151	28.752986
318.677618	11594.503942	28.758004
319.141547	11615.316287	28.763021
320.059999	11632.561900	28.768039
319.928449	11644.105027	28.773056
320.199461	11645.253151	28.778074
320.901991	11661.212701	28.783092
320.970480	11662.758842	28.788109
321.639282	11675.916503	28.793127
321.738041	11683.545933	28.798144
321.831951	11688.233155	28.803162
322.249348	11698.231471	28.808180
322.573902	11710.764178	28.813197
323.361226	11712.030362	28.818215
323.086610	11725.651611	28.823232
323.053689	11744.082082	28.828250
323.357533	11743.624113	28.833268
323.859956	11764.376914	28.838285
324.414330	11775.698997	28.843303
324.308461	11794.140943	28.848320
324.773762	11806.241164	28.853338
325.045701	11819.259000	28.858356
325.347121	11835.009968	28.863373
325.749592	11842.528733	28.868391
325.940665	11860.687401	28.873408
326.245316	11880.261903	28.878426
326.533844	11883.241936	28.883444
326.707746	11910.036566	28.888461
327.348475	11924.111384	28.893479
327.710078	11934.971154	28.898496
328.134957	11958.736165	28.903514
328.604899	11969.711610	28.908532
328.408990	11995.781172	28.913549
328.891165	12005.428468	28.918567
328.837499	12026.786538	28.923584
329.428428	12057.359035	28.928602
330.071026	12066.858081	28.933620
330.313934	12092.751675	28.938637
330.519633	12105.874818	28.943655
331.076222	12119.874546	28.948672
331.162200	12143.648669	28.953690
331.382473	12147.978331	28.958708
331.646893	12168.768861	28.963725
332.451337	12193.068373	28.968743
332.713086	12202.923978	28.973760
332.901655	12226.318990	28.978778
333.656470	12247.058051	28.983796
333.887921	12260.313053	28.988813
334.298311	12268.310733	28.993831
334.438605	12294.855394	28.998848
334.444199	12313.589852	29.003866
334.950874	12320.754603	29.008884
335.412543	12345.310104	29.013901
335.903100	12363.937068	29.018919
336.409248	12375.377592	29.023936
336.418121	12397.193640	29.028954
336.763048	12405.018480	29.033972
336.909372	12428.505622	29.038989
337.138048	12446.248448	29.044007
337.114601	12471.862188	29.049024
337.910835	12493.561327	29.054042
338.300107	12508.250699	29.059060
338.464592	12536.121356	29.064077
338.702552	12552.223912	29.069095
339.343203	12567.606571	29.074112
339.578543	12582.954840	29.079130
340.261904	12594.333002	29.084148
340.609437	12615.171004	29.089165
341.043677	12631.413405	29.094183
340.928622	12652.143913	29.099200
341.414002	12667.869920	29.104218
342.281457	12679.134034	29.109236
342.394882	12701.155106	29.114253
342.957923	12715.176373	29.119271
343.176492	12719.512750	29.124288
343.154257	12736.060428	29.129306
343.638957	12748.230849	29.134324
343.674487	12767.936850	29.139341
344.091056	12784.829516	29.144359
344.740112	12802.077356	29.149376
345.008970	12803.961676	29.154394
345.538084	12819.008331	29.159412
345.719382	12828.478973	29.164429
345.793669	12851.011611	29.169447
346.010316	12852.342011	29.174464
346.565138	12867.397309	29.179482
347.107570	12884.952453	29.184500
346.966877	12905.106201	29.189517
347.449169	12926.182386	29.194535
348.104342	12939.362019	29.199552
347.788248	12961.955941	29.204570
348.787403	12982.610171	29.209588
349.112247	12999.365818	29.214605
349.400355	13012.467210	29.219623
349.613193	13026.995149	29.224640
349.905473	13055.320242	29.229658
350.200135	13065.815359	29.234676
350.311198	13080.788760	29.239693
350.644636	13106.499035	29.244711
351.297510	13122.584453	29.249728
351.694100	13147.760675	29.254746
352.145606	13167.228246	29.259764
352.416221	13182.331473	29.264781
352.791203	13208.092222	29.269799
353.347421	13212.893726	29.274816
353.496205	13235.345678	29.279834
353.924702	13257.990688	29.284852
354.333786	13275.971303	29.289869
354.680975	13294.334269	29.294887
355.362568	13313.642789	29.299904
355.433795	13335.235410	29.304922
355.498812	13351.893118	29.309940
355.807807	13367.161011	29.314957
356.278542	13391.899618	29.319975
356.916723	13397.130448	29.324992
356.827080	13427.009646	29.330010
357.646514	13440.397591	29.335028
357.964013	13463.732885	29.340045
358.021492	13487.971071	29.345063
358.559300	13506.484391	29.350080
359.031652	13516.219270	29.355098
359.966673	13537.133638	29.360116
360.171444	13551.963254	29.365133
360.343621	13575.204603	29.370151
360.846724	13580.437695	29.375168
361.238771	13601.456136	29.380186
361.546020	13607.594684	29.385204
361.714982	13619.054046	29.390221
361.870459	13638.846378	29.395239
362.275793	13652.577246	29.400256
362.215449	13679.562662	29.405274
362.668193	13696.605221	29.410292
363.168650	13717.856293	29.415309
363.415379	13732.982649	29.420327
364.242429	13746.407516	29.425344
364.395830	13776.997649	29.430362
364.875475	13786.744158	29.435380
365.287445	13814.641092	29.440397
365.572319	13829.117308	29.445415
366.263915	13840.068600	29.450432
366.267640	13869.829653	29.455450
366.472517	13881.889894	29.460468
367.225167	13898.869867	29.465485
367.192813	13918.297155	29.470503
367.940980	13937.820108	29.475520
368.199320	13955.449171	29.480538
367.992129	13956.012311	29.485556
368.311703	13982.303873	29.490573
368.665653	14002.839225	29.495591
369.529401	14019.407144	29.500608
369.737929	14037.672544	29.505626
370.549027	14057.128918	29.510644
370.663233	14068.199208	29.515661
370.696937	14089.425909	29.520679
371.503776	14095.126338	29.525696
371.495289	14116.100713	29.530714
371.781922	14138.219489	29.535732
372.129433	14154.290457	29.540749
372.209613	14180.916656	29.545767
372.428264	14205.083138	29.550784
373.388930	14229.907159	29.555802
373.950522	14257.509709	29.560820
374.264281	14271.880679	29.565837
374.390465	14293.497361	29.570855
374.857688	14316.781829	29.575872
375.303294	14351.805345	29.580890
375.939156	14358.157947	29.585908
376.152168	14377.326199	29.590925
376.286166	14399.601829	29.595943
377.067594	14421.242345	29.600960
377.239240	14441.291948	29.605978
377.656798	14461.925209	29.610996
378.123411	14475.947100	29.616013
378.640528	14501.030444	29.621031
379.152783	14516.769573	29.626048
379.285007	14523.955922	29.631066
379.670412	14530.262544	29.636084
379.732050	14555.625746	29.641101
380.078552	14572.673101	29.646119
381.027312	14592.459019	29.651136
381.215917	14613.952593	29.656154
381.705599	14640.995333	29.661172
382.246396	14652.810796	29.666189
382.436430	14677.020258	29.671207
383.069131	14690.384654	29.676224
383.547139	14708.643228	29.681242
383.934434	14726.615999	29.686260
383.971183	14736.403950	29.691277
383.992470	14763.400221	29.696295
385.276029	14782.840183	29.701312
385.792485	14797.928295	29.706330
385.751702	14815.778712	29.711348
386.254132	14820.563791	29.716365
386.610564	14845.846462	29.721383
386.834363	14841.750066	29.726400
387.120909	14867.305844	29.731418
387.589402	14885.540812	29.736436
388.234538	14898.069635	29.741453
388.179584	14929.477495	29.746471
388.895631	14941.619410	29.751488
389.274348	14950.627511	29.756506
389.321969	14957.530402	29.761524
390.119033	14988.508026	29.766541
390.806363	15003.882203	29.771559
390.935540	15004.320043	29.776576
391.244631	15027.229054	29.781594
391.898147	15044.664581	29.786612
392.160984	15056.151161	29.791629
392.398303	15073.244492	29.796647
392.499957	15081.373843	29.801664
392.889584	15107.147507	29.806682
393.396462	15126.216791	29.811700
393.753103	15138.250899	29.816717
393.873454	15172.846816	29.821735
394.083782	15178.565215	29.826752
394.708020	15205.076039	29.831770
394.950453	15219.019896	29.836788
395.351187	15235.449803	29.841805
395.539491	15262.932260	29.846823
395.953874	15269.853615	29.851840
396.300484	15292.744433	29.856858
396.802149	15317.543870	29.861876
397.302221	15338.673642	29.866893
397.481689	15374.833497	29.871911
398.053448	15383.745242	29.876928
398.368323	15410.323759	29.881946
398.843450	15428.634008	29.886964
399.852681	15445.316196	29.891981
399.267795	15476.220513	29.896999
399.807711	15488.181918	29.902016
400.185058	15519.260890	29.907034
400.844031	15546.846897	29.912052
401.338019	15563.878354	29.917069
401.605220	15589.166511	29.922087
401.883182	15619.076834	29.927104
402.142691	15644.748429	29.932122
402.534124	15670.380444	29.937140
402.782525	15690.624629	29.942157
403.184217	15721.886459	29.947175
403.980616	15746.810837	29.952192
404.227659	15765.273995	29.957210
404.522973	15804.849664	29.962228
405.702652	15823.375246	29.967245
406.267961	15848.664426	29.972263
406.977211	15858.890854	29.977280
407.312782	15871.326682	29.982298
407.707531	15887.132725	29.987316
408.210880	15893.838235	29.992333
408.432977	15914.626862	29.997351
409.238235	15939.878579	30.002368
409.826143	15945.923390	30.007386
409.751337	15963.233802	30.012404
410.182388	15976.741233	30.017421
410.539058	15996.924565	30.022439
410.347947	16010.456830	30.027456
411.067813	16030.984427	30.032474
411.000270	16053.056671	30.037492
411.334802	16073.155115	30.042509
411.682224	16106.479047	30.047527
412.098834	16139.877477	30.052544
412.751484	16162.190782	30.057562
413.346503	16187.469440	30.062580
413.692007	16202.348560	30.067597
414.248838	16219.566581	30.072615
414.746255	16249.099242	30.077632
414.943102	16256.323498	30.082650
415.336428	16292.369465	30.087668
415.872260	16302.945458	30.092685
416.974435	16324.879013	30.097703
417.207574	16346.323338	30.102720
417.554745	16362.813139	30.107738
417.562378	16383.481101	30.112756
418.208858	16397.811032	30.117773
418.569060	16423.603712	30.122791
418.760615	16441.848802	30.127808
419.276028	16463.277470	30.132826
419.740257	16486.985132	30.137844
419.771613	16501.357796	30.142861
420.318917	16526.521194	30.147879
420.430655	16552.877275	30.152896
421.306448	16572.828293	30.157914
421.594837	16602.520578	30.162932
422.144402	16630.245307	30.167949
422.527834	16640.456862	30.172967
422.772412	16662.398793	30.177984
423.579319	16684.903325	30.183002
423.713356	16705.457077	30.188020
424.417906	16720.713078	30.193037
424.821891	16743.839849	30.198055
424.817086	16760.451453	30.203072
425.616109	16776.665528	30.208090
425.832356	16795.264000	30.213108
426.093301	16812.986890	30.218125
425.822257	16834.823428	30.223143
426.582644	16860.159192	30.228160
426.911436	16889.223356	30.233178
427.623752	16924.762552	30.238196
427.964621	16948.322703	30.243213
428.450605	16979.361753	30.248231
428.654950	17005.053281	30.253248
429.288659	17031.069255	30.258266
429.929145	17059.396284	30.263284
430.510277	17095.837588	30.268301
431.088446	17109.701805	30.273319
431.501451	17130.250218	30.278336
432.383022	17150.965313	30.283354
432.780416	17171.446726	30.288372
433.350460	17187.643320	30.293389
433.617203	17211.796586	30.298407
434.247188	17226.644574	30.303424
434.329221	17240.194930	30.308442
434.450746	17268.641457	30.313460
435.074869	17274.001918	30.318477
435.661365	17302.748382	30.323495
435.813682	17319.983373	30.328512
436.657130	17346.465984	30.333530
437.099825	17376.245844	30.338548
436.956679	17394.967518	30.343565
437.431799	17416.700472	30.348583
437.876937	17452.317236	30.353600
438.465013	17464.632421	30.358618
439.005238	17500.417581	30.363636
439.357298	17525.644453	30.368653
439.814275	17542.522375	30.373671
440.142408	17571.448689	30.378688
440.672961	17591.435891	30.383706
441.361043	17618.745513	30.388724
441.858235	17634.511680	30.393741
442.376930	17664.292715	30.398759
442.380785	17684.375146	30.403776
442.953969	17700.350572	30.408794
443.065814	17734.023769	30.413812
443.018465	17759.629376	30.418829
443.782876	17781.557489	30.423847
444.685844	17812.965309	30.428864
445.217361	17839.623805	30.433882
445.814788	17864.364150	30.438900
446.099594	17884.364878	30.443917
446.750707	17906.342467	30.448935
446.938342	17931.197623	30.453952
447.339744	17953.372315	30.458970
448.073435	17984.686897	30.463988
448.806260	17996.518575	30.469005
449.271217	18024.918739	30.474023
449.394682	18037.717700	30.479040
450.056961	18055.821093	30.484058
450.470600	18084.185159	30.489076
450.502030	18108.711230	30.494093
451.131812	18121.936343	30.499111
451.497176	18140.534865	30.504128
452.322471	18160.805002	30.509146
452.332121	18174.228362	30.514164
452.628531	18195.693261	30.519181
453.082281	18205.799871	30.524199
453.146143	18229.126999	30.529216
453.961203	18258.521381	30.534234
454.448973	18280.335454	30.539252
454.636563	18311.300189	30.544269
455.466541	18331.449738	30.549287
455.163280	18353.116136	30.554304
455.918971	18379.506512	30.559322
456.375743	18407.592639	30.564340
457.013969	18437.406682	30.569357
457.275930	18459.401630	30.574375
457.651114	18502.757735	30.579392
458.479565	18527.058413	30.584410
458.450987	18552.630537	30.589428
459.000941	18589.869247	30.594445
459.801266	18611.053511	30.599463
460.038559	18647.020909	30.604480
460.622218	18677.096574	30.609498
461.082420	18700.058939	30.614516
461.433240	18719.917517	30.619533
462.232373	18748.866581	30.624551
462.668214	18785.403319	30.629568
462.833981	18798.290922	30.634586
463.450747	18833.769623	30.639604
463.978955	18861.365068	30.644621
464.481827	18889.899550	30.649639
465.126386	18923.181798	30.654656
466.097489	18946.077067	30.659674
466.576592	18961.708159	30.664692
467.238570	18986.104984	30.669709
467.736454	18998.264696	30.674727
467.884033	19028.459751	30.679744
467.985120	19039.948774	30.684762
468.418661	19062.675667	30.689780
468.785536	19088.180235	30.694797
469.614598	19114.572756	30.699815
469.912597	19146.848273	30.704832
470.785361	19162.379960	30.709850
471.138230	19187.179253	30.714868
471.107337	19212.234540	30.719885
471.953075	19232.091937	30.724903
472.074680	19259.789541	30.729920
472.853518	19278.823504	30.734938
473.331219	19312.941244	30.739956
473.398942	19339.282734	30.744973
474.048205	19355.070710	30.749991
474.316842	19393.346932	30.755008
475.170577	19423.179276	30.760026
475.495921	19446.877573	30.765044
475.977456	19471.625485	30.770061
476.561641	19493.672219	30.775079
476.956467	19535.555462	30.780096
477.353810	19558.471825	30.785114
477.962128	19578.998561	30.790132
478.323450	19610.930074	30.795149
479.091668	19640.536062	30.800167
479.025929	19675.680936	30.805184
479.783673	19691.723869	30.810202
480.252329	19717.383906	30.815220
480.852728	19745.190428	30.820237
481.274090	19771.110664	30.825255
481.564530	19804.178207	30.830272
482.393422	19824.803333	30.835290
482.823914	19852.194356	30.840308
483.151524	19870.313954	30.845325
483.739783	19889.188823	30.850343
484.263163	19916.262119	30.855360
484.771014	19931.946351	30.860378
485.736207	19957.857473	30.865396
486.126585	19976.517015	30.870413
486.493192	19985.475670	30.875431
486.756328	20008.205083	30.880448
486.795364	20029.326910	30.885466
487.387002	20044.037753	30.890484
487.790319	20077.347121	30.895501
488.274010	20100.206368	30.900519
488.864642	20129.588188	30.905536
489.914616	20142.704641	30.910554
490.384157	20159.140600	30.915572
490.474783	20194.148186	30.920589
491.193453	20210.172395	30.925607
491.665196	20235.289264	30.930624
492.059807	20255.584822	30.935642
492.846315	20285.384789	30.940660
492.796342	20306.356581	30.945677
493.909840	20328.188672	30.950695
494.166671	20347.254896	30.955712
494.475256	20373.231504	30.960730
494.852612	20393.315087	30.965748
495.163459	20433.210521	30.970765
495.918066	20449.008159	30.975783
496.248312	20474.122224	30.980800
497.036286	20505.956781	30.985818
497.546574	20537.203054	30.990836
498.070528	20561.490786	30.995853
498.902388	20579.968027	31.000871
498.910316	20604.349272	31.005888
499.472008	20626.925230	31.010906
500.156878	20657.443017	31.015924
500.380217	20684.760239	31.020941
500.993167	20709.463862	31.025959
501.378617	20733.324898	31.030976
501.738014	20777.130808	31.035994
502.709863	20790.759088	31.041012
502.886794	20834.138781	31.046029
503.662026	20850.559034	31.051047
503.858103	20875.802040	31.056064
504.394921	20910.203952	31.061082
505.122351	20931.541167	31.066100
505.337110	20968.312484	31.071117
505.639298	20992.540708	31.076135
506.303070	21020.054787	31.081152
506.807842	21052.092549	31.086170
507.915351	21077.275200	31.091188
508.424564	21095.721323	31.096205
508.985456	21123.384349	31.101223
509.420462	21150.018261	31.106240
510.048271	21168.433240	31.111258
510.937051	21193.681892	31.116276
511.667654	21220.945683	31.121293
511.932027	21222.616721	31.126311
512.096036	21244.257352	31.131328
512.785097	21265.626215	31.136346
513.572690	21277.988399	31.141364
513.770600	21300.445191	31.146381
514.573724	21318.207318	31.151399
514.603099	21344.728107	31.156416
514.940933	21366.954547	31.161434
515.737361	21387.182023	31.166452
516.021490	21417.542608	31.171469
516.331914	21437.340770	31.176487
516.589413	21465.854256	31.181504
517.053192	21494.588219	31.186522
517.685181	21512.200405	31.191540
518.348748	21543.853937	31.196557
518.625694	21566.930515	31.201575
519.086609	21591.324175	31.206592
519.389680	21626.054607	31.211610
520.221616	21645.208937	31.216628
520.388354	21679.847081	31.221645
520.929235	21701.498692	31.226663
521.296066	21735.018783	31.231680
521.941435	21767.926623	31.236698
522.398334	21796.080784	31.241716
523.035491	21835.984821	31.246733
523.882079	21862.751113	31.251751
523.996783	21887.597444	31.256768
524.245773	21913.421132	31.261786
524.637115	21952.826813	31.266804
525.510621	21987.316887	31.271821
526.164254	22010.587736	31.276839
526.956297	22049.545407	31.281856
527.749447	22094.872321	31.286874
528.365078	22114.174725	31.291892
528.551263	22145.316344	31.296909
528.992184	22177.365936	31.301927
529.505222	22199.426859	31.306944
530.179772	22230.643774	31.311962
530.710421	22270.243110	31.316980
531.691044	22296.211781	31.321997
531.640030	22320.964551	31.327015
532.306147	22359.626613	31.332032
532.807462	22391.212134	31.337050
533.358204	22419.377760	31.342068
533.551761	22458.303595	31.347085
534.267165	22486.329787	31.352103
534.938572	22524.296261	31.357120
535.606644	22559.072266	31.362138
536.106135	22586.816470	31.367156
536.264686	22621.988335	31.372173
537.226189	22658.374124	31.377191
538.084407	22683.882235	31.382208
538.138117	22716.859046	31.387226
539.296851	22748.038858	31.392244
539.313132	22784.244332	31.397261
540.036826	22818.683493	31.402279
540.450289	22844.154046	31.407296
541.000189	22871.044003	31.412314
541.512542	22897.541777	31.417332
541.943270	22930.308235	31.422349
542.377532	22966.947783	31.427367
543.033964	22996.961803	31.432384
543.491205	23030.754285	31.437402
544.223244	23054.108869	31.442420
544.726963	23106.257501	31.447437
545.464100	23134.224334	31.452455
546.128800	23171.314740	31.457472
546.352743	23198.180362	31.462490
547.137269	23221.242562	31.467508
547.632334	23263.478219	31.472525
548.229387	23284.465573	31.477543
549.505416	23310.231332	31.482560
549.722060	23340.978265	31.487578
550.571449	23362.166310	31.492596
550.871870	23401.228915	31.497613
551.425821	23411.284611	31.502631
551.942703	23441.864612	31.507648
552.372782	23460.963582	31.512666
552.916662	23486.237594	31.517684
553.347898	23523.403137	31.522701
553.765680	23548.229353	31.527719
554.445537	23572.009792	31.532736
554.774152	23601.235606	31.537754
555.038202	23625.334003	31.542772
555.220450	23662.045897	31.547789
555.607924	23693.878815	31.552807
556.248838	23730.784410	31.557824
556.858112	23773.496168	31.562842
557.826129	23798.350266	31.567860
557.794339	23828.827213	31.572877
558.548801	23869.216197	31.577895
559.380371	23906.174408	31.582912
559.964437	23944.631229	31.587930
560.452062	23965.352069	31.592948
561.196115	24006.633994	31.597965
561.781808	24033.696861	31.602983
562.373349	24056.145677	31.608000
562.985573	24098.143574	31.613018
563.550513	24138.196258	31.618036
564.074031	24160.504179	31.623053
564.889596	24199.493983	31.628071
565.810433	24232.779854	31.633088
565.965231	24263.070253	31.638106
566.822327	24287.007052	31.643124
567.232838	24320.429870	31.648141
567.545203	24344.666916	31.653159
568.353442	24379.032343	31.658176
569.018506	24416.630571	31.663194
569.385062	24437.592048	31.668212
570.216373	24474.090026	31.673229
570.625311	24507.886258	31.678247
571.224739	24538.638279	31.683264
571.700164	24575.666149	31.688282
572.396256	24601.208436	31.693300
572.975920	24642.757566	31.698317
572.852071	24674.602612	31.703335
573.598194	24708.839303	31.708352
574.776723	24743.760366	31.713370
574.779179	24776.742284	31.718388
575.192764	24820.997323	31.723405
575.628105	24856.919731	31.728423
576.984052	24890.953789	31.733440
577.695243	24929.234601	31.738458
578.250266	24957.466346	31.743476
578.680189	24992.441891	31.748493
579.409635	25028.546054	31.753511
579.915273	25064.394627	31.758528
580.514615	25089.371274	31.763546
581.038084	25115.516350	31.768564
581.848923	25147.373750	31.773581
582.750953	25185.618843	31.778599
583.222940	25204.055662	31.783616
583.847023	25250.787631	31.788634
584.388887	25266.546612	31.793652
584.894287	25296.031604	31.798669
585.183422	25323.673526	31.803687
586.115487	25348.857500	31.808704
586.591838	25375.958268	31.813722
587.137472	25407.788099	31.818740
587.733928	25436.437458	31.823757
588.127980	25456.751070	31.828775
588.724230	25490.968330	31.833792
589.233858	25522.747104	31.838810
590.296922	25551.538425	31.843828
590.494337	25587.164448	31.848845
590.920601	25608.705548	31.853863
591.936485	25640.493699	31.858880
592.269927	25673.715966	31.863898
592.819205	25716.308544	31.868916
593.278912	25736.403598	31.873933
593.955428	25768.434700	31.878951
594.477593	25783.318700	31.883968
595.500803	25821.729306	31.888986
595.496291	25846.340111	31.894004
596.028970	25872.813369	31.899021
596.403670	25904.405318	31.904039
596.997191	25935.122485	31.909056
597.598626	25970.395190	31.914074
598.381470	26009.899243	31.919092
599.091032	26036.155412	31.924109
599.969223	26073.331524	31.929127
600.295078	26094.294784	31.934144
600.884611	26132.584303	31.939162
601.855422	26166.668210	31.944180
602.723171	26186.996852	31.949197
602.841121	26225.189760	31.954215
603.369672	26245.584225	31.959232
603.239813	26288.556140	31.964250
604.221638	26327.239637	31.969268
604.917060	26365.513013	31.974285
605.348742	26418.977172	31.979303
606.409174	26457.288359	31.984320
606.874352	26482.382552	31.989338
607.333581	26532.461404	31.994356
608.093777	26553.199112	31.999373
608.742808	26594.823572	32.004391
609.839068	26624.590865	32.009408
610.183331	26662.407863	32.014426
610.793125	26696.707212	32.019444
611.335847	26728.065566	32.024461
612.082886	26770.427149	32.029479
612.836514	26792.967408	32.034496
613.180707	26834.368331	32.039514
613.438925	26866.220197	32.044532
614.467333	26898.943779	32.049549
615.016455	26946.272883	32.054567
615.747199	26973.626692	32.059584
616.211163	27009.346202	32.064602
617.087201	27046.480201	32.069620
617.784893	27080.311369	32.074637
618.546249	27120.693169	32.079655
619.266975	27156.524416	32.084672
619.787127	27178.577079	32.089690
620.617103	27209.176987	32.094708
621.626541	27224.137429	32.099725
622.099117	27257.252021	32.104743
622.913354	27279.871817	32.109760
623.333997	27306.579395	32.114778
623.778811	27339.015862	32.119796
624.511957	27366.350864	32.124813
624.856967	27403.587645	32.129831
625.044138	27430.382514	32.134848
626.035707	27461.817080	32.139866
626.668597	27502.162876	32.144884
627.431034	27533.589195	32.149901
627.682602	27564.191738	32.154919
628.655083	27593.922961	32.159936
629.601265	27633.777516	32.164954
629.471088	27655.041352	32.169972
629.886638	27688.961967	32.174989
630.364287	27729.136588	32.180007
631.492673	27762.914085	32.185024
632.027443	27796.563384	32.190042
632.816455	27840.968499	32.195060
633.230881	27864.707104	32.200077
633.678568	27906.890400	32.205095
634.230590	27947.243422	32.210112
634.797214	27981.140863	32.215130
635.382549	28011.521149	32.220148
636.172473	28048.980182	32.225165
636.803705	28088.847030	32.230183
637.301905	28116.706529	32.235200
638.033459	28152.480951	32.240218
638.801442	28184.065426	32.245236
639.303142	28225.962811	32.250253
639.887267	28263.081546	32.255271
640.698961	28297.377263	32.260288
641.548084	28331.920006	32.265306
641.498203	28368.954923	32.270324
642.570005	28392.869306	32.275341
642.896156	28434.845179	32.280359
643.732742	28470.022197	32.285376
644.492396	28511.443637	32.290394
644.515973	28547.898501	32.295412
645.918104	28589.244763	32.300429
646.232180	28620.193066	32.305447
647.273833	28663.688131	32.310464
648.387652	28694.612434	32.315482
648.459134	28741.691830	32.320500
649.316520	28762.783192	32.325517
649.893286	28805.668710	32.330535
650.619402	28838.682956	32.335552
651.282245	28872.933423	32.340570
651.992816	28912.587185	32.345588
652.655585	28954.719998	32.350605
653.569282	28991.118422	32.355623
653.814469	29017.817794	32.360640
654.696392	29053.399581	32.365658
655.070701	29095.666352	32.370676
655.795663	29128.883520	32.375693
656.488375	29176.821094	32.380711
657.183269	29209.670162	32.385728
657.571208	29250.437036	32.390746
658.085308	29296.392775	32.395764
658.814404	29335.955961	32.400781
659.617662	29392.005608	32.405799
660.058591	29430.665944	32.410816
660.919995	29469.146724	32.415834
661.532579	29508.279691	32.420852
662.373079	29540.512302	32.425869
662.854976	29589.097003	32.430887
663.774238	29629.914165	32.435904
664.342120	29667.910310	32.440922
664.764072	29720.942165	32.445940
665.850683	29755.412193	32.450957
666.368707	29799.573225	32.455975
666.874726	29831.694324	32.460992
667.753311	29874.073360	32.466010
668.405728	29922.429864	32.471028
669.165588	29962.779595	32.476045
669.667955	30004.794294	32.481063
670.842595	30046.533122	32.486080
671.234590	30078.817853	32.491098
671.729320	30118.520390	32.496116
672.940867	30150.424034	32.501133
673.091383	30181.096882	32.506151
673.969126	30226.934537	32.511168
674.678338	30262.608681	32.516186
675.613334	30306.838248	32.521204
675.948547	30341.540720	32.526221
676.608884	30387.419100	32.531239
677.331627	30419.658889	32.536256
677.969271	30457.708780	32.541274
678.529232	30505.196135	32.546292
679.225342	30537.920707	32.551309
679.817279	30573.398827	32.556327
680.223869	30609.152571	32.561344
681.255277	30636.596954	32.566362
681.611452	30674.893611	32.571380
682.080253	30703.842200	32.576397
682.733336	30752.680979	32.581415
683.329059	30792.198316	32.586432
684.320345	30826.520710	32.591450
684.720603	30872.384004	32.596468
685.434678	30912.148539	32.601485
686.225430	30957.381929	32.606503
687.118478	31008.788213	32.611520
687.756191	31045.909906	32.616538
688.857978	31090.209855	32.621556
688.965849	31126.788831	32.626573
690.305403	31157.011408	32.631591
690.379591	31195.283650	32.636608
691.453636	31229.852942	32.641626
692.234533	31279.823486	32.646644
693.181701	31311.473216	32.651661
694.167565	31353.737345	32.656679
694.322879	31386.010610	32.661696
695.495518	31425.615815	32.666714
696.003329	31465.470611	32.671732
697.009135	31499.216574	32.676749
697.774849	31518.213674	32.681767
698.444047	31562.405372	32.686784
699.206935	31582.774792	32.691802
699.647294	31629.202436	32.696820
700.488376	31649.445884	32.701837
701.105483	31676.785846	32.706855
701.633508	31724.748809	32.711872
702.340917	31759.085601	32.716890
703.237392	31802.072684	32.721908
703.738740	31840.298185	32.726925
704.647095	31873.276114	32.731943
705.033567	31917.177786	32.736960
705.525256	31957.130877	32.741978
706.555919	31997.499068	32.746996
707.642280	32039.812076	32.752013
708.045730	32069.518789	32.757031
708.496239	32101.266471	32.762048
709.311215	32141.175610	32.767066
709.671470	32193.313102	32.772084
710.413643	32232.020006	32.777101
711.523439	32281.170177	32.782119
711.897317	32314.226185	32.787136
713.006902	32356.947130	32.792154
713.548804	32408.133703	32.797172
714.218438	32446.846045	32.802189
714.858142	32481.883731	32.807207
715.754560	32518.664086	32.812224
716.470687	32560.568304	32.817242
717.117150	32612.156258	32.822260
717.849683	32647.445212	32.827277
718.827385	32691.692149	32.832295
718.972903	32732.440620	32.837312
720.349908	32765.883952	32.842330
720.531661	32817.450356	32.847348
721.440724	32843.159278	32.852365
722.075127	32897.006823	32.857383
722.927178	32943.164291	32.862400
723.813305	32977.418205	32.867418
724.648924	33015.669378	32.872436
725.092295	33063.490622	32.877453
725.980985	33095.645362	32.882471
726.685246	33136.028942	32.887488
727.527552	33173.381602	32.892506
728.130315	33204.683530	32.897524
728.451479	33238.906224	32.902541
729.687791	33273.086817	32.907559
729.991629	33307.192214	32.912576
730.663075	33341.107330	32.917594
731.185882	33378.636836	32.922612
731.860019	33417.483039	32.927629
732.622980	33449.133261	32.932647
733.032815	33508.252416	32.937664
734.231523	33545.138977	32.942682
734.722722	33595.242630	32.947700
735.162854	33631.988921	32.952717
736.281140	33671.746007	32.957735
736.667773	33731.773524	32.962752
737.690478	33773.366620	32.967770
738.705228	33815.852506	32.972788
739.496180	33861.989955	32.977805
740.226763	33897.060037	32.982823
740.779638	33948.356138	32.987840
741.495438	33986.381272	32.992858
742.410612	34035.705142	32.997876
743.203092	34073.237917	33.002893
744.082655	34114.367273	33.007911
744.416842	34168.113354	33.012928
745.176641	34201.895897	33.017946
746.142682	34250.421988	33.022964
746.993230	34286.921799	33.027981
747.861130	34329.513913	33.032999
748.617312	34380.431487	33.038016
749.840640	34414.647592	33.043034
750.674868	34453.761481	33.048052
750.955119	34502.477741	33.053069
751.945684	34538.083539	33.058087
752.739605	34583.975524	33.063104
753.357000	34624.388215	33.068122
754.366187	34657.127133	33.073140
754.887902	34697.833145	33.078157
755.843643	34729.271750	33.083175
756.215438	34784.707993	33.088192
757.044526	34821.275318	33.093210
757.882843	34870.309688	33.098228
758.730603	34912.918782	33.103245
759.651802	34951.216985	33.108263
760.181595	34997.265041	33.113280
760.916363	35034.429200	33.118298
761.891536	35079.452949	33.123316
762.348188	35115.061135	33.128333
763.294816	35156.213638	33.133351
763.850479	35208.941323	33.138368
764.621030	35249.286966	33.143386
765.474150	35295.405172	33.148404
766.040723	35349.086249	33.153421
766.773159	35388.812162	33.158439
767.449647	35441.673254	33.163456
768.152018	35496.452593	33.168474
769.436262	35530.610390	33.173492
769.980802	35579.856805	33.178509
770.504773	35619.141574	33.183527
771.537089	35665.921727	33.188544
772.422288	35702.911753	33.193562
773.514737	35750.118962	33.198580
774.087289	35793.177596	33.203597
775.049941	35829.023895	33.208615
775.398715	35873.464538	33.213632
776.179834	35917.673172	33.218650
777.285178	35970.911039	33.223668
777.952248	36009.187723	33.228685
778.867695	36040.710468	33.233703
779.518275	36080.627541	33.238720
780.316784	36112.851599	33.243738
780.846161	36147.824143	33.248756
781.687344	36193.914557	33.253773
782.656086	36225.384968	33.258791
783.206141	36261.960539	33.263808
783.769559	36303.592606	33.268826
784.327417	36334.444621	33.273844
785.488547	36376.267775	33.278861
786.083727	36416.662070	33.283879
786.644030	36458.528886	33.288896
787.602543	36510.937467	33.293914
788.363922	36546.196820	33.298932
789.162869	36598.662220	33.303949
789.929117	36650.823029	33.308967
790.712499	36695.349088	33.313984
791.071753	36739.075365	33.319002
792.056377	36782.684832	33.324020
792.831968	36831.645030	33.329037
793.650039	36885.410744	33.334055
794.594421	36935.230014	33.339072
795.556769	36973.177642	33.344090
796.484065	37027.982611	33.349108
797.063367	37085.599212	33.354125
798.230434	37123.432845	33.359143
798.926824	37174.511925	33.364160
799.478608	37223.615566	33.369178
800.575736	37253.613005	33.374196
801.386677	37313.116272	33.379213
802.331181	37353.318521	33.384231
803.229016	37406.124533	33.389248
804.016305	37451.536844	33.394266
804.878824	37494.673654	33.399284
805.569639	37549.219784	33.404301
806.646703	37587.201128	33.409319
807.461796	37638.882433	33.414336
808.109192	37684.506851	33.419354
808.823776	37718.599284	33.424372
809.664300	37770.978843	33.429389
810.594846	37818.563786	33.434407
811.439914	37852.851002	33.439424
812.387006	37894.419764	33.444442
813.264280	37939.047534	33.449460
813.904949	37989.574477	33.454477
814.994406	38027.345981	33.459495
815.608831	38076.682065	33.464512
816.575167	38117.603230	33.469530
817.869375	38162.115587	33.474548
818.311824	38203.207483	33.479565
819.285087	38228.154065	33.484583
819.736902	38275.005548	33.489600
820.582450	38312.708245	33.494618
821.777625	38351.311148	33.499636
822.170503	38391.051556	33.504653
823.080364	38430.730055	33.509671
823.851517	38477.652125	33.514688
824.674003	38527.152700	33.519706
825.475949	38575.214771	33.524724
826.290124	38613.858835	33.529741
826.942602	38653.742468	33.534759
827.909686	38695.429803	33.539776
828.896667	38751.456659	33.544794
829.881569	38792.319287	33.549812
830.118916	38835.594629	33.554829
830.883636	38878.686294	33.559847
831.860157	38930.750157	33.564864
832.266604	38982.056004	33.569882
833.308878	39028.487818	33.574900
833.930731	39073.398248	33.579917
834.541999	39114.996660	33.584935
835.121084	39173.712937	33.589952
836.191987	39219.192078	33.594970
837.302902	39260.263524	33.599988
837.807340	39304.623658	33.605005
838.698561	39344.357349	33.610023
839.688223	39392.986308	33.615040
840.498558	39447.594418	33.620058
841.103210	39490.010393	33.625076
841.696344	39548.162641	33.630093
843.186018	39594.291621	33.635111
843.886299	39649.518265	33.640128
844.685727	39701.491556	33.645146
845.734289	39752.237015	33.650164
846.864617	39806.574577	33.655181
847.448860	39846.888492	33.660199
848.767954	39901.329541	33.665216
849.492718	39953.599717	33.670234
850.427363	39983.063558	33.675252
851.043017	40044.350431	33.680269
852.002355	40086.307281	33.685287
852.776501	40139.506163	33.690304
853.830812	40185.287173	33.695322
854.790432	40221.982426	33.700340
855.988310	40271.927831	33.705357
856.984590	40320.817132	33.710375
857.933172	40355.130064	33.715392
858.821128	40388.693621	33.720410
859.598407	40437.402449	33.725428
860.262474	40467.225536	33.730445
861.186168	40519.554464	33.735463
862.244965	40555.165928	33.740480
862.897403	40597.095929	33.745498
863.275101	40635.147884	33.750516
864.356288	40687.439906	33.755533
865.222287	40734.902241	33.760551
865.897826	40784.355089	33.765568
866.726442	40829.262072	33.770586
867.887637	40881.832959	33.775604
868.068041	40929.535886	33.780621
869.408855	40979.915900	33.785639
869.918559	41037.547606	33.790656
870.403643	41099.737003	33.795674
872.010354	41145.534729	33.800692
872.760322	41207.727228	33.805709
873.667972	41266.486247	33.810727
874.415438	41301.040874	33.815744
875.225554	41359.821742	33.820762
876.250921	41415.615449	33.825780
877.181255	41472.866204	33.830797
877.857333	41525.622121	33.835815
878.588050	41576.092718	33.840832
879.676831	41637.430147	33.845850
880.761085	41686.353006	33.850868
881.238797	41749.165223	33.855885
882.441060	41798.835150	33.860903
883.543664	41843.315503	33.865920
884.471557	41897.354763	33.870938
885.217056	41944.092265	33.875956
885.817669	42009.049064	33.880973
886.845240	42060.549513	33.885991
888.114711	42108.647383	33.891008
889.139452	42163.254019	33.896026
889.917951	42206.331138	33.901044
890.957538	42256.615789	33.906061
892.006445	42302.022590	33.911079
892.359189	42338.968227	33.916096
893.548690	42380.785923	33.921114
894.362013	42415.268746	33.926132
895.351517	42449.319239	33.931149
895.946255	42498.162435	33.936167
896.846168	42522.771251	33.941184
897.436900	42580.495518	33.946202
898.597421	42614.589064	33.951220
899.265782	42662.307896	33.956237
900.275948	42703.641962	33.961255
901.027285	42748.710454	33.966272
901.763161	42804.508745	33.971290
902.817056	42848.650884	33.976308
903.548572	42898.144006	33.981325
904.519731	42948.352401	33.986343
905.334728	42989.894667	33.991360
905.887060	43056.146107	33.996378
907.213142	43104.287893	34.001396
908.248693	43160.255214	34.006413
909.355676	43206.584586	34.011431
910.069748	43262.653104	34.016448
910.987213	43320.619103	34.021466
912.213006	43364.855538	34.026484
912.975783	43418.937036	34.031501
913.747181	43473.403155	34.036519
914.810136	43524.053902	34.041536
915.837491	43575.007628	34.046554
916.799251	43623.081086	34.051572
917.716668	43679.915807	34.056589
918.484978	43735.869500	34.061607
920.027739	43786.167406	34.066624
920.875909	43836.700691	34.071642
921.483102	43875.835576	34.076660
922.551052	43931.192539	34.081677
923.538779	43978.111484	34.086695
924.709848	44024.084637	34.091712
925.597273	44078.236781	34.096730
926.183128	44127.844014	34.101748
926.793464	44180.926519	34.106765
927.723345	44233.130481	34.111783
928.958188	44283.117178	34.116800
929.720100	44342.501807	34.121818
930.977188	44387.133892	34.126836
932.058054	44440.402686	34.131853
932.730762	44502.869587	34.136871
933.927625	44540.344579	34.141888
934.685172	44603.772614	34.146906
935.563150	44653.702161	34.151924
936.647907	44698.810971	34.156941
937.529690	44754.040993	34.161959
938.751599	44805.953875	34.166976
939.727136	44845.184605	34.171994
940.439855	44897.310266	34.177012
941.726011	44948.416389	34.182029
942.330790	45015.291696	34.187047
943.633981	45059.430834	34.192064
944.318014	45102.768755	34.197082
945.374786	45153.658237	34.202100
946.227186	45201.973633	34.207117
947.142375	45254.954028	34.212135
947.889061	45289.919866	34.217152
948.690027	45353.014290	34.222170
949.362716	45412.200660	34.227188
950.257865	45465.747688	34.232205
951.186036	45521.168442	34.237223
952.328473	45578.320694	34.242240
953.442085	45634.250390	34.247258
954.433611	45686.353212	34.252276
955.315705	45736.398400	34.257293
956.107591	45788.918599	34.262311
957.280135	45829.758620	34.267328
957.439581	45878.728004	34.272346
958.391999	45932.577150	34.277364
959.662311	45983.371824	34.282381
960.216382	46038.302074	34.287399
961.239596	46089.856839	34.292416
962.467320	46136.458076	34.297434
963.568361	46196.585277	34.302452
964.322490	46252.901754	34.307469
965.130300	46309.754006	34.312487
966.308078	46353.991249	34.317504
967.035338	46423.230170	34.322522
968.255804	46482.700503	34.327540
969.568133	46536.425157	34.332557
970.077198	46597.171184	34.337575
970.982523	46641.736328	34.342592
971.836755	46708.969838	34.347610
973.409938	46773.212571	34.352628
974.708183	46827.661308	34.357645
975.866307	46885.099107	34.362663
976.985818	46930.365126	34.367680
977.898753	46979.117702	34.372698
978.689991	47032.691058	34.377716
979.767914	47075.186657	34.382733
980.526012	47137.021218	34.387751
981.773507	47183.444393	34.392768
982.852236	47230.811402	34.397786
983.642191	47294.729086	34.402804
984.871623	47343.356977	34.407821
985.784611	47392.508996	34.412839
986.534241	47444.672742	34.417856
987.517308	47498.128596	34.422874
988.494666	47559.145509	34.427892
989.375072	47609.011656	34.432909
990.505809	47666.373486	34.437927
991.255911	47721.068362	34.442944
992.273923	47783.787653	34.447962
993.253204	47846.165225	34.452980
994.475813	47900.394312	34.457997
995.313546	47963.863546	34.463015
996.728297	48018.613237	34.468032
997.359063	48073.422545	34.473050
998.328874	48124.699297	34.478068
999.441530	48195.540851	34.483085
1000.597604	48253.937757	34.488103
1002.003698	48292.544023	34.493120
1002.967125	48357.063869	34.498138
1003.696343	48412.782266	34.503156
1005.496904	48454.446074	34.508173
1006.527163	48506.580974	34.513191
1007.649085	48548.667543	34.518208
1008.272784	48603.498214	34.523226
1009.374237	48648.277013	34.528244
1010.467332	48690.437953	34.533261
1011.422256	48740.231648	34.538279
1012.380390	48793.934871	34.543296
1013.390301	48840.404966	34.548314
1014.164780	48895.971942	34.553332
1015.527827	48929.284204	34.558349
1016.316202	48993.194255	34.563367
1017.182338	49031.437117	34.568384
1018.174824	49086.578162	34.573402
1018.703815	49136.546965	34.578420
1019.877492	49193.077108	34.583437
1020.931200	49243.185429	34.588455
1021.984217	49295.546336	34.593472
1022.858408	49350.409175	34.598490
1023.828713	49395.361820	34.603508
1025.082451	49441.465965	34.608525
1025.707871	49489.528694	34.613543
1026.730652	49527.165782	34.618560
1028.136249	49569.722305	34.623578
1029.083086	49629.844789	34.628596
1030.191737	49663.906577	34.633613
1031.011162	49714.856139	34.638631
1032.465154	49749.262586	34.643648
1033.078426	49801.459401	34.648666
1034.132875	49863.558659	34.653684
1034.869827	49910.927817	34.658701
1036.136970	49954.873375	34.663719
1036.578623	50018.796283	34.668736
1038.178163	50075.666861	34.673754
1038.702257	50125.651240	34.678772
1039.828295	50176.218484	34.683789
1040.814397	50235.330394	34.688807
1041.783174	50299.000717	34.693824
1043.169710	50353.665522	34.698842
1044.072969	50428.419001	34.703860
1045.356796	50483.840478	34.708877
1046.377871	50544.447253	34.713895
1047.255624	50604.880482	34.718912
1048.870577	50657.763932	34.723930
1049.801817	50720.042973	34.728948
1050.919557	50776.155519	34.733965
1051.870381	50841.861209	34.738983
1052.976612	50897.362104	34.744000
1053.876126	50956.046508	34.749018
1054.992581	51021.657176	34.754036
1056.354210	51070.417841	34.759053
1057.281356	51143.967697	34.764071
1058.407892	51199.345919	34.769088
1059.592837	51247.584137	34.774106
1060.580832	51309.134555	34.779124
1061.642258	51371.344349	34.784141
1062.742182	51436.560153	34.789159
1063.440230	51485.836873	34.794176
1064.550009	51551.146369	34.799194
1065.538821	51608.964235	34.804212
1066.865254	51671.063740	34.809229
1067.681853	51742.171395	34.814247
1068.630723	51793.029349	34.819264
1070.318093	51859.704621	34.824282
1071.196956	51919.426093	34.829300
1072.557234	51977.566374	34.834317
1073.663991	52032.253647	34.839335
1074.573309	52096.900024	34.844352
1076.098114	52158.064922	34.849370
1076.937277	52214.661177	34.854388
1078.046260	52269.677698	34.859405
1079.208297	52328.273850	34.864423
1080.385361	52385.216263	34.869440
1081.437231	52437.078262	34.874458
1082.418109	52501.474105	34.879476
1083.766064	52542.267047	34.884493
1084.690909	52604.343331	34.889511
1085.513009	52652.128728	34.894528
1086.663912	52701.685153	34.899546
1087.829960	52773.867596	34.904564
1088.888599	52820.875950	34.909581
1090.243496	52880.563323	34.914599
1091.492264	52936.603630	34.919616
1092.358758	52979.965897	34.924634
1093.265538	53045.564483	34.929652
1094.196078	53101.072840	34.934669
1095.322490	53150.248049	34.939687
1096.221712	53197.870618	34.944704
1097.584222	53245.446063	34.949722
1098.327835	53292.454063	34.954740
1099.311770	53342.734065	34.959757
1100.185783	53383.602681	34.964775
1101.248807	53442.191819	34.969792
1102.714542	53474.804831	34.974810
1103.533643	53543.797698	34.979828
1104.538903	53591.917038	34.984845
1105.611614	53651.397437	34.989863
1106.711932	53714.607229	34.994880
1107.798701	53770.086384	34.999898
1109.320955	53832.572314	35.004916
1110.363829	53890.267135	35.009933
1111.379451	53940.961114	35.014951
1112.213084	54007.636970	35.019968
1113.570135	54063.340284	35.024986
1114.793498	54125.323237	35.030004
1115.791186	54189.562884	35.035021
1116.889277	54236.264149	35.040039
1117.909689	54300.677732	35.045056
1119.444160	54361.688679	35.050074
1120.301419	54434.095437	35.055092
1121.480491	54477.626697	35.060109
1122.903047	54549.147943	35.065127
1124.297608	54612.579870	35.070144
1125.215073	54666.144850	35.075162
1126.525173	54723.008833	35.080180
1127.384347	54781.323132	35.085197
1128.962635	54836.158296	35.090215
1129.870076	54904.223701	35.095232
1131.002260	54957.325394	35.100250
1132.016223	55018.868849	35.105268
1133.547376	55070.389513	35.110285
1134.686053	55127.325606	35.115303
1135.811313	55188.307830	35.120320
1136.919107	55247.666524	35.125338
1138.395056	55309.429517	35.130356
1139.171970	55361.138510	35.135373
1140.834508	55412.443167	35.140391
1141.860015	55478.105882	35.145408
1143.017686	55527.268508	35.150426
1144.244809	55579.091022	35.155444
1145.197781	55625.937999	35.160461
1146.608127	55683.934073	35.165479
1147.527521	55742.026137	35.170496
1148.647266	55786.220944	35.175514
1150.149842	55842.234763	35.180532
1151.250460	55894.166372	35.185549
1152.547151	55945.497817	35.190567
1153.424721	56007.698057	35.195584
1155.175415	56043.852064	35.200602
1156.277535	56088.531176	35.205620
1157.891806	56127.371055	35.210637
1158.612242	56174.299820	35.215655
1159.336863	56218.886386	35.220672
1161.019782	56269.354315	35.225690
1161.865557	56325.086045	35.230708
1162.903962	56371.629994	35.235725
1164.192504	56419.622141	35.240743
1164.986036	56482.621549	35.245760
1166.505890	56529.716987	35.250778
1167.398540	56584.688854	35.255796
1168.436392	56629.385371	35.260813
1169.846069	56684.751190	35.265831
1170.579558	56752.564321	35.270848
1171.708592	56788.772486	35.275866
1172.593825	56854.321720	35.280884
1173.549596	56898.430344	35.285901
1174.382914	56944.760690	35.290919
1175.878594	57007.214860	35.295936
1176.994484	57059.444078	35.300954
1177.869629	57112.084509	35.305972
1179.134577	57170.024690	35.310989
1180.430138	57223.555227	35.316007
1180.948228	57291.928913	35.321024
1182.599178	57348.182535	35.326042
1183.833391	57410.849576	35.331060
1185.079254	57465.293489	35.336077
1185.920629	57533.478011	35.341095
1187.457985	57585.484167	35.346112
1188.413862	57650.182746	35.351130
1189.695718	57717.045664	35.356148
1190.734823	57777.978378	35.361165
1192.053141	57835.209274	35.366183
1193.187258	57912.709886	35.371200
1194.411509	57970.044438	35.376218
1195.642151	58043.878409	35.381236
1196.808537	58099.057732	35.386253
1197.941903	58168.647737	35.391271
1199.418359	58240.646320	35.396288
1200.389700	58306.382241	35.401306
1201.667416	58378.241457	35.406324
1202.902739	58450.120181	35.411341
1204.314191	58514.053531	35.416359
1205.697934	58580.061091	35.421376
1207.271658	58643.994699	35.426394
1208.568806	58705.484321	35.431412
1209.285779	58772.628481	35.436429
1210.804913	58826.583303	35.441447
1212.321970	58897.628075	35.446464
1213.612110	58957.707969	35.451482
1215.084649	59019.272203	35.456500
1216.000409	59085.284779	35.461517
1217.682568	59136.955143	35.466535
1218.618526	59197.888598	35.471552
1219.634987	59258.366535	35.476570
1220.824065	59308.475105	35.481588
1222.102266	59379.634637	35.486605
1223.567563	59441.606171	35.491623
1224.569433	59503.770674	35.496640
1225.765499	59561.486860	35.501658
1227.614798	59627.253492	35.506676
1228.330682	59679.930784	35.511693
1229.825711	59739.777991	35.516711
1230.887444	59791.610175	35.521728
1231.921941	59856.175749	35.526746
1233.439679	59914.994422	35.531764
1234.682286	59983.040744	35.536781
1236.003835	60038.706575	35.541799
1237.057705	60096.433631	35.546816
1238.509262	60160.282757	35.551834
1239.640285	60208.357753	35.556852
1240.686900	60275.897542	35.561869
1241.956284	60325.780424	35.566887
1243.441705	60395.581224	35.571904
1244.331100	60459.493818	35.576922
1245.661578	60520.678983	35.581940
1246.727233	60591.096753	35.586957
1248.299923	60640.540344	35.591975
1249.671473	60705.295935	35.596992
1250.482399	60761.764962	35.602010
1252.015183	60819.621312	35.607028
1253.318280	60887.027688	35.612045
1254.205301	60930.382171	35.617063
1255.182333	60997.770266	35.622080
1256.339369	61056.432936	35.627098
1257.687765	61110.786696	35.632116
1258.622996	61172.700017	35.637133
1260.130318	61228.225535	35.642151
1261.645782	61286.864297	35.647168
1262.815170	61343.284876	35.652186
1263.945669	61401.300527	35.657204
1264.823194	61458.577313	35.662221
1266.244699	61511.907699	35.667239
1267.402352	61575.926799	35.672256
1268.474380	61641.586319	35.677274
1269.990285	61707.220840	35.682292
1271.368141	61776.029581	35.687309
1272.633103	61827.834262	35.692327
1274.018432	61894.217695	35.697344
1275.598777	61960.216286	35.702362
1276.572115	62015.403049	35.707380
1277.738114	62089.544251	35.712397
1279.039721	62146.496707	35.717415
1280.489105	62221.771378	35.722432
1281.798387	62288.813468	35.727450
1283.266134	62350.652717	35.732468
1284.561782	62415.722221	35.737485
1286.253525	62482.116242	35.742503
1287.354492	62542.202901	35.747520
1288.897383	62598.074114	35.752538
1290.205643	62662.104106	35.757556
1291.753879	62730.578644	35.762573
1293.115814	62787.187620	35.767591
1294.351355	62835.681866	35.772608
1295.584172	62896.096919	35.777626
1297.158880	62945.728418	35.782644
1298.275173	63013.176180	35.787661
1299.474178	63077.110398	35.792679
1300.543810	63138.874666	35.797696
1301.434842	63208.219397	35.802714
1302.976851	63266.934677	35.807732
1304.438886	63340.944652	35.812749
1305.661897	63396.988022	35.817767
1307.309807	63463.138309	35.822784
1308.456448	63535.457314	35.827802
1310.045381	63592.583358	35.832820
1310.773519	63661.410413	35.837837
1312.738512	63722.162337	35.842855
1314.162879	63783.809368	35.847872
1315.167780	63847.307477	35.852890
1316.730314	63913.415349	35.857908
1317.582351	63979.514332	35.862925
1318.881839	64041.232193	35.867943
1320.793331	64102.354273	35.872960
1321.818479	64157.721279	35.877978
1323.488064	64232.897933	35.882996
1324.474586	64297.077458	35.888013
1325.980800	64352.382251	35.893031
1327.116370	64413.474614	35.898048
1328.476254	64483.718114	35.903066
1329.849037	64537.657741	35.908084
1331.286627	64606.699216	35.913101
1332.427103	64664.929853	35.918119
1333.896366	64730.522688	35.923136
1335.074751	64802.542833	35.928154
1336.546660	64855.131794	35.933172
1337.504966	64920.748131	35.938189
1339.033870	64985.996755	35.943207
1340.536979	65051.179946	35.948224
1341.801334	65119.730805	35.953242
1343.062354	65176.449634	35.958260
1344.227482	65244.946725	35.963277
1345.566804	65298.842577	35.968295
1346.823273	65348.345073	35.973312
1348.042083	65409.008974	35.978330
1349.420321	65457.049129	35.983348
1350.668325	65516.638760	35.988365
1351.854559	65567.564525	35.993383
1353.204692	65628.797196	35.998400
1354.223203	65687.872344	36.003418
1355.843200	65740.889492	36.008436
1357.222968	65823.447796	36.013453
1358.046474	65877.621897	36.018471
1359.890888	65947.888608	36.023488
1361.137778	66024.915868	36.028506
1362.667805	66078.808862	36.033524
1364.002772	66155.449186	36.038541
1365.274632	66217.043756	36.043559
1366.877751	66280.739275	36.048576
1368.060582	66347.280203	36.053594
1369.472831	66416.305275	36.058612
1370.967971	66485.830402	36.063629
1372.722475	66554.821272	36.068647
1374.019581	66612.987567	36.073664
1375.337940	66684.661934	36.078682
1377.153674	66750.155134	36.083700
1377.987092	66819.132616	36.088717
1379.366543	66887.562614	36.093735
1380.910528	66957.758856	36.098752
1382.212196	67032.754519	36.103770
1383.769337	67092.622375	36.108788
1385.433281	67174.532764	36.113805
1386.967237	67230.422029	36.118823
1388.383514	67300.278305	36.123840
1389.076615	67370.849475	36.128858
1391.102057	67431.581901	36.133876
1392.453464	67505.019922	36.138893
1393.463193	67573.022099	36.143911
1395.480107	67632.806592	36.148928
1396.429850	67713.545177	36.153946
1398.342219	67775.271200	36.158964
1399.611871	67851.635596	36.163981
1401.091110	67920.679585	36.168999
1402.925390	67976.263874	36.174016
1404.241916	68046.821634	36.179034
1405.549533	68101.614850	36.184052
1406.921334	68171.081565	36.189069
1408.354392	68239.975350	36.194087
1409.900627	68300.094685	36.199104
1411.080224	68369.743988	36.204122
1412.762641	68425.080753	36.209140
1414.004035	68503.863951	36.214157
1415.318846	68557.320988	36.219175
1416.813655	68621.311579	36.224192
1417.926989	68692.599428	36.229210
1419.567461	68751.805937	36.234228
1421.165524	68817.876727	36.239245
1422.132041	68889.447712	36.244263
1423.694741	68953.903401	36.249280
1424.947186	69024.081290	36.254298
1426.918812	69089.340794	36.259316
1428.324982	69158.443872	36.264333
1429.489931	69227.021339	36.269351
1431.207588	69281.987174	36.274368
1432.367625	69350.945664	36.279386
1433.894856	69414.546892	36.284404
1435.289953	69479.182099	36.289421
1436.621038	69543.029638	36.294439
1438.401160	69601.158774	36.299456
1439.589426	69664.155131	36.304474
1440.784307	69722.122859	36.309492
1441.935775	69776.013250	36.314509
1443.520486	69827.784306	36.319527
1444.580715	69884.937624	36.324544
1445.858187	69947.553438	36.329562
1447.482788	70003.630851	36.334580
1448.804755	70073.382776	36.339597
1450.502545	70133.514326	36.344615
1451.819701	70196.124529	36.349632
1453.113270	70271.453846	36.354650
1454.452143	70335.048825	36.359668
1456.121759	70393.450330	36.364685
1457.363192	70465.812172	36.369703
1458.897817	70537.419098	36.374720
1459.961477	70621.486095	36.379738
1461.610804	70682.639685	36.384756
1463.296055	70766.343894	36.389773
1464.655058	70838.080453	36.394791
1466.553669	70905.363349	36.399808
1468.005591	70986.090534	36.404826
1469.391286	71050.617136	36.409844
1470.744348	71123.115308	36.414861
1472.134889	71212.034406	36.419879
1474.218986	71270.056374	36.424896
1475.436565	71336.053817	36.429914
1476.948963	71410.161646	36.434932
1478.615950	71491.008707	36.439949
1480.240689	71560.273934	36.444967
1481.819303	71622.694652	36.449984
1483.001657	71708.380380	36.455002
1484.149296	71775.162458	36.460020
1486.062398	71855.642822	36.465037
1487.660891	71934.424847	36.470055
1489.048453	71998.079577	36.475072
1490.934888	72072.080068	36.480090
1492.187289	72144.926121	36.485108
1493.842292	72230.602898	36.490125
1495.347681	72309.096644	36.495143
1496.940611	72367.261250	36.500160
1498.341088	72447.456358	36.505178
1499.727192	72516.330822	36.510196
1501.501212	72586.930618	36.515213
1502.696012	72668.653146	36.520231
1504.706073	72731.857574	36.525248
1506.259806	72815.981543	36.530266
1507.754896	72885.523867	36.535284
1509.208527	72955.680827	36.540301
1510.869998	73026.983375	36.545319
1512.734921	73088.387478	36.550336
1513.602527	73157.826075	36.555354
1515.461027	73229.541640	36.560372
1516.938610	73291.994793	36.565389
1518.451428	73359.433020	36.570407
1520.479262	73431.806599	36.575424
1522.052057	73495.727267	36.580442
1523.668045	73564.239157	36.585460
1525.002682	73614.847221	36.590477
1526.384198	73684.219424	36.595495
1527.756771	73738.305005	36.600512
1529.343433	73805.644145	36.605530
1530.998315	73882.269875	36.610548
1532.294743	73939.990360	36.615565
1533.801809	74013.992332	36.620583
1535.541679	74068.578419	36.625600
1537.090088	74131.934445	36.630618
1538.606575	74196.220272	36.635636
1539.957736	74268.727374	36.640653
1541.281939	74336.539597	36.645671
1542.532420	74387.998296	36.650688
1543.922103	74457.662566	36.655706
1545.279658	74516.160061	36.660724
1547.086321	74572.294724	36.665741
1547.848803	74630.695607	36.670759
1549.447473	74695.463775	36.675776
1550.956842	74766.845460	36.680794
1552.318794	74837.338398	36.685812
1554.096672	74907.627089	36.690829
1555.537650	74993.852946	36.695847
1557.004635	75055.678547	36.700864
1558.578341	75135.601304	36.705882
1559.827060	75213.649783	36.710900
1561.734985	75288.263890	36.715917
1563.324789	75368.400158	36.720935
1564.677242	75457.200100	36.725952
1566.345911	75525.810112	36.730970
1567.737876	75615.820436	36.735988
1569.752886	75689.836207	36.741005
1570.870426	75784.196892	36.746023
1572.636124	75857.188095	36.751040
1574.747808	75941.031901	36.756058
1576.188255	76023.017585	36.761076
1578.060139	76107.507473	36.766093
1579.672195	76194.711120	36.771111
1581.086391	76274.510208	36.776128
1582.979391	76354.804631	36.781146
1584.761523	76436.535410	36.786164
1586.464981	76498.859348	36.791181
1587.777649	76582.171484	36.796199
1589.146178	76658.989295	36.801216
1590.965200	76745.959640	36.806234
1592.525401	76818.504228	36.811252
1594.219780	76892.218778	36.816269
1596.095735	76980.549082	36.821287
1597.776638	77056.698405	36.826304
1599.249497	77134.996037	36.831322
1601.025602	77214.411880	36.836340
1602.406328	77300.223809	36.841357
1604.144044	77375.402367	36.846375
1606.050502	77453.367024	36.851392
1607.845118	77525.636115	36.856410
1609.620445	77598.136443	36.861428
1611.200910	77663.218609	36.866445
1613.189695	77741.829947	36.871463
1614.461422	77814.663032	36.876480
1616.225437	77890.497639	36.881498
1617.618235	77954.963792	36.886516
1619.534782	78027.240465	36.891533
1620.981097	78092.534673	36.896551
1622.857308	78158.863901	36.901568
1624.528219	78229.139948	36.906586
1625.936307	78298.076453	36.911604
1627.688668	78371.545226	36.916621
1629.337676	78446.461908	36.921639
1630.776017	78518.789384	36.926656
1631.963021	78585.759588	36.931674
1633.826006	78660.630697	36.936692
1635.835443	78734.617625	36.941709
1637.121081	78812.695984	36.946727
1638.666005	78886.325285	36.951744
1640.474378	78957.113766	36.956762
1642.152695	79031.850094	36.961780
1643.739006	79091.360487	36.966797
1645.210712	79167.903148	36.971815
1646.991962	79240.001488	36.976832
1648.544421	79311.223665	36.981850
1650.210823	79386.203526	36.986868
1651.561665	79449.222825	36.991885
1652.655452	79513.954801	36.996903
1654.048450	79575.080112	37.001920
1655.914233	79648.217814	37.006938
1657.220834	79720.429700	37.011956
1658.850976	79793.452635	37.016973
1660.469781	79865.451339	37.021991
1662.003705	79944.621588	37.027008
1663.766230	80025.137229	37.032026
1665.283703	80094.555201	37.037044
1666.690692	80178.344912	37.042061
1668.188812	80256.318073	37.047079
1669.867443	80359.361170	37.052096
1671.777613	80435.902057	37.057114
1673.672626	80531.576354	37.062132
1675.145257	80611.885674	37.067149
1676.894760	80702.287494	37.072167
1678.416582	80796.424748	37.077184
1680.509228	80873.989852	37.082202
1681.935415	80967.483830	37.087220
1683.789232	81060.759159	37.092237
1685.903961	81152.942381	37.097255
1687.509370	81244.838192	37.102272
1689.431476	81329.767037	37.107290
1690.849248	81411.746980	37.112308
1692.747242	81494.918993	37.117325
1694.600159	81582.431414	37.122343
1696.522833	81675.419274	37.127360
1698.418438	81758.301033	37.132378
1699.996936	81849.430166	37.137396
1701.970138	81926.459398	37.142413
1703.785133	82015.347467	37.147431
1705.636808	82097.780978	37.152448
1707.402241	82177.998278	37.157466
1708.867790	82263.913649	37.162484
1710.812976	82350.983233	37.167501
1712.659474	82433.114449	37.172519
1714.184098	82508.821745	37.177536
1715.822003	82587.957850	37.182554
1717.529686	82668.654385	37.187572
1719.200569	82737.117283	37.192589
1721.220528	82836.644355	37.197607
1722.718970	82919.110203	37.202624
1724.970175	82988.559883	37.207642
1726.514112	83086.667206	37.212660
1728.267326	83172.274232	37.217677
1730.139032	83247.029570	37.222695
1731.573845	83322.258940	37.227712
1733.431238	83401.971161	37.232730
1734.848372	83489.304272	37.237748
1736.750872	83561.711530	37.242765
1738.893455	83658.422048	37.247783
1739.912306	83732.019706	37.252800
1742.144124	83817.325698	37.257818
1743.800312	83911.274912	37.262836
1745.406291	83986.567945	37.267853
1747.166004	84072.886236	37.272871
1748.697911	84168.211542	37.277888
1750.686948	84246.030206	37.282906
1752.194953	84330.526016	37.287924
1753.639148	84423.990573	37.292941
1755.841143	84518.756017	37.297959
1757.342232	84596.449257	37.302976
1759.162696	84679.287948	37.307994
1761.050765	84760.735126	37.313012
1763.006515	84856.604613	37.318029
1764.408158	84938.229788	37.323047
1765.886804	85024.683629	37.328064
1767.673718	85098.823511	37.333082
1769.340139	85172.729010	37.338100
1770.953390	85244.678934	37.343117
1772.845250	85319.195778	37.348135
1774.107490	85399.665620	37.353152
1775.845467	85472.559635	37.358170
1777.461897	85565.012556	37.363188
1779.117817	85651.884042	37.368205
1780.948340	85739.602816	37.373223
1782.726132	85828.369193	37.378240
1784.752743	85918.034619	37.383258
1786.325027	86011.306870	37.388276
1787.817747	86109.647960	37.393293
1789.795126	86200.766562	37.398311
1791.622012	86308.471285	37.403328
1793.744699	86397.375510	37.408346
1795.441249	86493.899247	37.413364
1797.330689	86587.529221	37.418381
1799.043465	86679.717173	37.423399
1800.849942	86778.340898	37.428416
1802.851113	86868.317371	37.433434
1805.003173	86972.957673	37.438452
1806.860776	87073.031706	37.443469
1808.397526	87161.320306	37.448487
1810.260714	87273.597634	37.453504
1812.751467	87361.889617	37.458522
1814.170107	87462.882729	37.463540
1815.856333	87557.523395	37.468557
1817.750981	87645.440634	37.473575
1819.689905	87748.875152	37.478592
1821.883353	87852.688402	37.483610
1823.960411	87935.927102	37.488628
1825.693413	88028.699080	37.493645
1828.062914	88125.465052	37.498663
1829.493678	88210.630546	37.503680
1831.239742	88295.075286	37.508698
1833.331533	88387.031876	37.513716
1835.210436	88484.750230	37.518733
1837.436559	88567.156322	37.523751
1839.008271	88654.632866	37.528768
1841.492308	88741.092463	37.533786
1842.982892	88834.171043	37.538804
1844.843617	88924.822121	37.543821
1846.241369	89009.766969	37.548839
1847.945201	89102.115997	37.553856
1850.018822	89189.312807	37.558874
1851.863672	89284.643891	37.563892
1853.855726	89373.146679	37.568909
1855.642540	89460.275108	37.573927
1857.664048	89564.640886	37.578944
1859.388725	89647.876185	37.583962
1861.345399	89734.319818	37.588980
1863.062209	89837.238763	37.593997
1864.837579	89924.535097	37.599015
1866.451133	90020.728511	37.604032
1868.866530	90115.174536	37.609050
1870.453628	90216.847726	37.614068
1872.082105	90307.032411	37.619085
1874.228457	90394.348106	37.624103
1875.853640	90499.818417	37.629120
1877.949016	90592.009399	37.634138
1879.574113	90689.077647	37.639156
1881.417532	90798.177602	37.644173
1883.180490	90880.827343	37.649191
1885.091349	90984.226820	37.654208
1886.821178	91075.335829	37.659226
1888.638038	91181.982571	37.664244
1890.666084	91272.639940	37.669261
1892.517466	91356.519212	37.674279
1894.385573	91444.984153	37.679296
1896.044928	91525.193084	37.684314
1897.545319	91609.837740	37.689332
1899.444934	91703.178092	37.694349
1900.925334	91783.808615	37.699367
1902.837107	91884.422684	37.704384
1904.714856	91974.091728	37.709402
1906.415981	92084.942318	37.714420
1908.099338	92185.580454	37.719437
1910.292633	92279.104765	37.724455
1912.103698	92388.266220	37.729472
1913.707567	92500.705190	37.734490
1915.698123	92626.683983	37.739508
1917.668683	92739.573441	37.744525
1919.687044	92844.141193	37.749543
1921.644620	92961.482344	37.754560
1923.688793	93074.108023	37.759578
1925.408861	93191.018250	37.764596
1927.403394	93321.803074	37.769613
1929.557734	93435.350790	37.774631
1931.275753	93555.165301	37.779648
1933.431627	93669.182619	37.784666
1935.236187	93784.865076	37.789684
1937.120911	93912.158581	37.794701
1939.660470	94036.409485	37.799719
1941.503222	94154.432276	37.804736
1943.838243	94265.432400	37.809754
1946.019564	94377.204822	37.814772
1947.982124	94490.710388	37.819789
1950.000550	94599.213489	37.824807
1951.764950	94716.033838	37.829824
1954.273533	94819.238696	37.834842
1956.032472	94938.418394	37.839860
1957.485124	95064.149094	37.844877
1959.404232	95167.155807	37.849895
1961.756842	95294.800083	37.854912
1963.815926	95408.661501	37.859930
1965.582302	95520.046641	37.864948
1967.502732	95644.324818	37.869965
1969.424009	95760.465395	37.874983
1971.545592	95894.638364	37.880000
1973.582307	96005.919556	37.885018
1975.739459	96126.068243	37.890036
1977.474964	96246.701680	37.895053
1979.661575	96361.586059	37.900071
1981.683965	96491.746077	37.905088
1983.525922	96612.567082	37.910106
1985.693653	96729.052973	37.915124
1987.660414	96856.966817	37.920141
1989.283613	96982.513737	37.925159
1991.074193	97099.516363	37.930176
1993.401924	97221.062309	37.935194
1995.163063	97347.768014	37.940212
1996.824381	97476.264575	37.945229
1999.083041	97615.544794	37.950247
2001.069250	97743.712715	37.955264
2002.949072	97864.773440	37.960282
2005.274679	97992.141327	37.965300
2006.897197	98119.771860	37.970317
2008.907353	98255.075189	37.975335
2011.134087	98387.619649	37.980352
2013.077598	98511.981566	37.985370
2015.058432	98647.291146	37.990388
2016.987577	98777.994901	37.995405
2019.179718	98898.237373	38.000423
2021.262155	99027.067286	38.005440
2022.816305	99152.557506	38.010458
2025.036041	99263.973629	38.015476
2026.557111	99375.740330	38.020493
2028.763383	99497.313963	38.025511
2030.624998	99620.742187	38.030528
2032.363400	99733.515678	38.035546
2034.362364	99859.306700	38.040564
2036.326797	99982.035629	38.045581
2037.986830	100102.124985	38.050599
2039.672683	100238.450916	38.055616
2041.916305	100386.734043	38.060634
2043.330867	100512.555656	38.065652
2045.604064	100659.681719	38.070669
2047.621020	100805.073629	38.075687
2049.926476	100951.739560	38.080704
2051.625626	101100.136489	38.085722
2053.649912	101239.633890	38.090740
2055.869638	101402.315051	38.095757
2058.226677	101547.137249	38.100775
2060.242289	101701.091170	38.105792
2062.405353	101854.071866	38.110810
2064.554252	102006.903349	38.115828
2066.846865	102168.410491	38.120845
2069.122917	102308.202686	38.125863
2070.710638	102458.930686	38.130880
2073.179215	102611.829066	38.135898
2075.350115	102764.115436	38.140916
2077.888546	102923.077426	38.145933
2079.765210	103066.599484	38.150951
2081.902835	103225.498849	38.155968
2084.046999	103370.501832	38.160986
2086.451314	103516.529780	38.166004
2088.718930	103681.420827	38.171021
2090.656427	103826.673677	38.176039
2092.526430	103977.275649	38.181056
2094.861732	104134.018318	38.186074
2097.303110	104274.477604	38.191092
2099.026458	104447.483573	38.196109
2101.053402	104589.112124	38.201127
2103.312272	104742.002377	38.206144
2105.438454	104900.518432	38.211162
2107.356980	105039.515825	38.216180
2109.824493	105207.984101	38.221197
2111.538007	105359.377529	38.226215
2113.466163	105524.191262	38.231232
2115.777383	105682.466479	38.236250
2118.032087	105834.943900	38.241268
2120.280257	106002.702337	38.246285
2122.512054	106160.459653	38.251303
2124.897125	106317.800638	38.256320
2126.897036	106475.113851	38.261338
2129.181087	106614.111225	38.266356
2131.516784	106777.840175	38.271373
2133.681100	106930.729728	38.276391
2135.913455	107072.970525	38.281408
2138.121750	107225.334619	38.286426
2140.544750	107360.369686	38.291444
2142.201187	107528.304272	38.296461
2144.041514	107673.512724	38.301479
2146.449736	107825.708710	38.306496
2148.578661	107987.878019	38.311514
2150.752429	108125.262958	38.316532
2152.737355	108288.419940	38.321549
2154.721869	108438.174121	38.326567
2156.882407	108593.937506	38.331584
2158.687766	108753.574121	38.336602
2160.905798	108919.829788	38.341620
2162.700107	109077.427975	38.346637
2164.874345	109232.773598	38.351655
2166.575216	109375.817154	38.356672
2168.333337	109531.952036	38.361690
2170.569137	109677.157706	38.366708
2172.591107	109840.569775	38.371725
2174.361212	109988.842389	38.376743
2176.207643	110149.683675	38.381760
2178.191533	110319.749002	38.386778
2180.478125	110491.593935	38.391796
2182.713626	110662.750207	38.396813
2184.520167	110845.146988	38.401831
2186.794937	111008.347366	38.406848
2188.962129	111195.178859	38.411866
2190.776891	111380.709510	38.416884
2192.918543	111570.704757	38.421901
2195.094389	111763.282796	38.426919
2197.272271	111948.810315	38.431936
2199.140041	112160.385726	38.436954
2201.506543	112349.348035	38.441972
2203.771927	112556.361380	38.446989
2205.885536	112768.992585	38.452007
2208.260097	112973.137708	38.457024
2210.684103	113177.060645	38.462042
2212.904945	113376.488832	38.467060
2214.989092	113589.852375	38.472077
2217.615828	113797.640658	38.477095
2220.002230	114000.445337	38.482112
2221.730530	114208.959934	38.487130
2224.753529	114406.416562	38.492148
2227.367097	114617.876943	38.497165
2229.397463	114819.295999	38.502183
2231.878950	115026.429098	38.507200
2233.983829	115231.605649	38.512218
2236.233177	115420.399290	38.517236
2238.788321	115635.679642	38.522253
2240.870045	115835.840557	38.527271
2243.706757	116037.901110	38.532288
2245.609381	116233.868583	38.537306
2248.251441	116429.125272	38.542324
2250.547834	116640.951244	38.547341
2252.762075	116828.527210	38.552359
2255.063870	117040.468752	38.557376
2257.559157	117240.547131	38.562394
2259.736783	117440.511381	38.567412
2262.042683	117642.245073	38.572429
2263.986764	117844.772129	38.577447
2266.798889	118040.860429	38.582464
2268.896224	118245.433172	38.587482
2271.098368	118437.280942	38.592500
2273.293051	118639.773036	38.597517
2275.347113	118845.801797	38.602535
2278.157038	119031.900215	38.607552
2280.278245	119240.457500	38.612570
2282.571502	119442.431044	38.617588
2284.576343	119647.583895	38.622605
2286.712486	119858.425448	38.627623
2289.447829	120049.931503	38.632640
2291.419554	120274.297723	38.637658
2293.752540	120470.625653	38.642676
2296.015198	120678.293325	38.647693
2298.173171	120890.291423	38.652711
2300.259076	121099.790283	38.657728
2302.288275	121303.755685	38.662746
2304.334090	121522.992674	38.667764
2306.721732	121747.048603	38.672781
2308.964935	121970.126256	38.677799
2311.417993	122184.190984	38.682816
2313.873170	122414.849315	38.687834
2315.845612	122603.227045	38.692852
2318.491911	122805.289640	38.697869
2320.504146	123003.748207	38.702887
2322.576217	123196.819600	38.707904
2324.503074	123397.348596	38.712922
2326.665281	123594.581483	38.717940
2328.580609	123807.863758	38.722957
2330.943215	124020.265283	38.727975
2333.319056	124233.084506	38.732992
2335.561431	124457.127696	38.738010
2338.112191	124676.823223	38.743028
2340.512833	124894.741961	38.748045
2342.235853	125124.617035	38.753063
2344.381303	125357.484779	38.758080
2346.855221	125592.598747	38.763098
2349.742012	125816.548634	38.768116
2351.340998	126062.243317	38.773133
2353.270595	126308.065366	38.778151
2355.600898	126556.668065	38.783168
2358.038508	126811.015368	38.788186
2360.327187	127064.207639	38.793204
2363.052970	127318.411485	38.798221
2364.795959	127583.199528	38.803239
2367.382872	127845.180211	38.808256
2369.708463	128112.202247	38.813274
2372.036625	128381.496638	38.818292
2374.722140	128640.815195	38.823309
2377.128787	128912.549406	38.828327
2379.806517	129177.188594	38.833344
2382.109210	129442.256052	38.838362
2384.721206	129718.162965	38.843380
2386.894148	129994.381419	38.848397
2389.214517	130258.030140	38.853415
2391.678168	130531.262963	38.858432
2394.385308	130806.743307	38.863450
2396.764905	131093.239315	38.868468
2399.303674	131355.820160	38.873485
2401.865491	131636.441933	38.878503
2404.101915	131902.968734	38.883520
2406.584757	132181.487394	38.888538
2409.055416	132458.461717	38.893556
2411.787711	132733.468171	38.898573
2414.090058	133019.037264	38.903591
2416.659374	133296.305961	38.908608
2418.966408	133571.752145	38.913626
2421.445989	133849.380943	38.918644
2424.569083	134113.790233	38.923661
2426.927644	134385.084040	38.928679
2429.658919	134651.372362	38.933696
2432.186203	134916.996258	38.938714
2434.712003	135178.726295	38.943732
2437.546028	135431.108219	38.948749
2439.654660	135705.507248	38.953767
2442.474674	135960.939813	38.958784
2444.426096	136215.596024	38.963802
2446.759469	136483.188262	38.968820
2449.524031	136748.405054	38.973837
2451.969917	137030.982321	38.978855
2454.577168	137292.267587	38.983872
2456.638683	137563.411075	38.988890
2458.815274	137839.144677	38.993908
2460.985313	138105.515533	38.998925
2462.949463	138388.785553	39.003943
2465.659877	138663.158791	39.008960
2467.825605	138941.768619	39.013978
2470.381710	139237.349746	39.018996
2472.747077	139507.403629	39.024013
2475.122645	139796.087399	39.029031
2477.704085	140068.039652	39.034048
2479.642101	140329.433793	39.039066
2482.035065	140598.220449	39.044084
2484.262601	140855.790273	39.049101
2486.783036	141129.598275	39.054119
2488.906175	141399.446887	39.059136
2490.802724	141683.368906	39.064154
2493.297597	141966.894394	39.069172
2495.553745	142256.715703	39.074189
2497.712319	142540.779390	39.079207
2499.886741	142843.435277	39.084224
2502.459440	143161.247918	39.089242
2504.595595	143461.717925	39.094260
2507.404951	143773.253166	39.099277
2509.640231	144093.015601	39.104295
2511.931860	144411.882825	39.109312
2514.631550	144738.519187	39.114330
2516.634021	145065.799785	39.119348
2519.146369	145398.206511	39.124365
2521.934531	145739.558356	39.129383
2524.370028	146078.530716	39.134400
2526.746108	146426.373895	39.139418
2529.364707	146771.795292	39.144436
2531.768015	147131.151024	39.149453
2534.123155	147476.009062	39.154471
2536.867360	147828.601851	39.159488
2539.989050	148182.661094	39.164506
2542.369290	148541.636607	39.169524
2545.670209	148893.514771	39.174541
2548.022492	149250.493943	39.179559
2550.994279	149600.600440	39.184576
2553.425561	149953.941683	39.189594
2556.269653	150300.531279	39.194612
2558.753016	150642.559111	39.199629
2561.493968	151008.425237	39.204647
2564.095284	151355.567241	39.209664
2566.681949	151706.953400	39.214682
2569.126167	152059.087610	39.219700
2571.929553	152397.433167	39.224717
2574.737664	152759.339881	39.229735
2577.626080	153112.363281	39.234752
2580.182919	153456.174099	39.239770
2582.967204	153810.512930	39.244788
2585.687394	154148.399613	39.249805
2588.116360	154506.390792	39.254823
2590.393367	154859.850690	39.259840
2593.189377	155218.766336	39.264858
2595.054645	155583.796199	39.269876
2597.581740	155938.162918	39.274893
2600.025900	156315.471311	39.279911
2602.718013	156683.996645	39.284928
2605.157147	157049.821751	39.289946
2607.155553	157428.755698	39.294964
2609.805240	157802.601032	39.299981
2611.729994	158191.999266	39.304999
2614.247044	158592.034746	39.310016
2617.071894	158982.376322	39.315034
2619.690883	159383.226205	39.320052
2622.323289	159770.314779	39.325069
2625.035902	160174.747922	39.330087
2627.896145	160570.032480	39.335104
2630.760225	160963.795441	39.340122
2632.852515	161359.205049	39.345140
2635.943360	161756.390678	39.350157
2638.283035	162155.562548	39.355175
2640.580269	162552.128155	39.360192
2643.654644	162949.564914	39.365210
2645.842984	163364.675988	39.370228
2648.907196	163746.198247	39.375245
2650.874079	164135.372428	39.380263
2653.224835	164518.826274	39.385280
2656.131894	164891.543023	39.390298
2658.498560	165277.982352	39.395316
2661.179073	165657.493265	39.400333
2663.861398	166044.725534	39.405351
2666.448374	166433.739732	39.410368
2669.340584	166828.752021	39.415386
2671.692318	167232.383345	39.420404
2674.466673	167625.717187	39.425421
2676.773810	168032.839012	39.430439
2679.074429	168437.450167	39.435456
2682.288960	168841.920656	39.440474
2684.358807	169269.503555	39.445492
2686.626327	169687.611284	39.450509
2689.433153	170119.616799	39.455527
2691.426067	170554.697935	39.460544
2694.120588	170995.563500	39.465562
2696.513355	171443.475195	39.470580
2699.424077	171891.689452	39.475597
2702.497429	172349.429571	39.480615
2704.661489	172805.816288	39.485632
2707.442206	173262.833008	39.490650
2710.305169	173745.336963	39.495668
2712.710773	174207.014472	39.500685
2715.608988	174674.674580	39.505703
2718.209706	175165.964398	39.510720
2720.994459	175644.796825	39.515738
2723.463434	176132.633729	39.520756
2726.407014	176611.358021	39.525773
2729.167884	177100.043806	39.530791
2731.665678	177589.433876	39.535808
2734.914351	178073.960026	39.540826
2737.735900	178574.225846	39.545844
2740.084431	179072.714492	39.550861
2742.644514	179576.582552	39.555879
2745.322586	180072.637883	39.560896
2748.444057	180583.077993	39.565914
2751.112006	181090.874294	39.570932
2753.993646	181604.151366	39.575949
2756.574102	182111.027184	39.580967
2759.543400	182615.686032	39.585984
2762.567427	183200.928728	39.591002
2764.839335	183724.065638	39.596020
2767.424457	184237.530169	39.601037
2770.322558	184757.425141	39.606055
2772.568744	185293.172218	39.611072
2775.461468	185820.515420	39.616090
2778.233320	186345.949856	39.621108
2780.813523	186888.713971	39.626125
2783.591516	187421.112256	39.631143
2786.107120	187967.447883	39.636160
2789.575715	188505.001217	39.641178
2792.119850	189051.693344	39.646196
2794.977496	189591.684246	39.651213
2797.843667	190136.400808	39.656231
2800.811131	190685.955551	39.661248
2803.968808	191223.875068	39.666266
2806.581486	191764.879504	39.671284
2809.554605	192306.007771	39.676301
2812.260084	192848.094685	39.681319
2815.281742	193390.363087	39.686336
2818.131954	193913.838417	39.691354
2821.047894	194463.849771	39.696372
2823.605756	195002.184023	39.701389
2826.611175	195551.271402	39.706407
2829.126037	196095.941633	39.711424
2831.771951	196615.445945	39.716442
2834.235089	197150.043907	39.721460
2837.549336	197660.556886	39.726477
2840.756871	198172.891843	39.731495
2843.357780	198689.895755	39.736512
2845.969840	199190.743993	39.741530
2848.518898	199720.485837	39.746548
2851.123315	200240.237726	39.751565
2853.928577	200749.722757	39.756583
2856.352485	201295.695898	39.761600
2859.296182	201833.054288	39.766618
2861.748406	202385.885092	39.771636
2864.332601	202927.367426	39.776653
2867.563089	203477.158553	39.781671
2870.093340	204045.985810	39.786688
2872.710107	204603.268354	39.791706
2875.604128	205177.147966	39.796724
2877.735351	205750.183177	39.801741
2881.261145	206329.479614	39.806759
2884.217496	206913.490013	39.811776
2886.822680	207496.947184	39.816794
2889.800960	208091.956734	39.821812
2891.954163	208690.805676	39.826829
2895.160781	209297.112313	39.831847
2897.536856	209912.085801	39.836864
2900.462079	210527.635312	39.841882
2903.511458	211146.672447	39.846900
2906.353222	211765.286106	39.851917
2909.583332	212380.664843	39.856935
2912.512653	213011.842058	39.861952
2915.276432	213641.750763	39.866970
2918.368421	214279.357397	39.871988
2921.150905	214905.022946	39.877005
2924.348790	215543.707474	39.882023
2926.879369	216185.520382	39.887040
2929.589619	216835.257511	39.892058
2932.558634	217497.072700	39.897076
2935.468961	218155.696997	39.902093
2938.742054	218805.069076	39.907111
2941.819908	219467.402977	39.912128
2944.667748	220121.949030	39.917146
2947.623540	220783.795093	39.922164
2950.573002	221447.979792	39.927181
2953.620457	222112.479824	39.932199
2956.647534	222771.826350	39.937216
2960.581278	223419.447085	39.942234
2963.793436	224077.850564	39.947252
2966.821419	224716.620200	39.952269
2970.542023	225362.902796	39.957287
2973.670670	226008.947695	39.962304
2976.860290	226648.631955	39.967322
2979.767159	227295.625852	39.972340
2982.556819	227947.032767	39.977357
2985.506986	228585.763078	39.982375
2988.411424	229226.608737	39.987392
2991.011624	229876.875651	39.992410
2993.714034	230533.807349	39.997428
2996.928021	231180.166639	40.002445
2999.666580	231834.449487	40.007463
3002.595194	232494.265377	40.012480
3005.653123	233156.930907	40.017498
3008.354232	233816.907764	40.022516
3010.933081	234487.013542	40.027533
3014.107809	235148.235406	40.032551
3017.012270	235823.826178	40.037568
3019.832580	236493.255825	40.042586
3023.364474	237169.101692	40.047604
3026.174976	237840.105330	40.052621
3029.215476	238497.607732	40.057639
3032.015687	239140.742528	40.062656
3035.063033	239771.719830	40.067674
3038.207644	240414.112017	40.072692
3040.632994	241055.954657	40.077709
3043.711314	241701.707300	40.082727
3046.710982	242351.128614	40.087744
3048.987026	243013.870928	40.092762
3051.993870	243670.832171	40.097780
3054.785033	244338.850069	40.102797
3058.196855	245016.447313	40.107815
3060.803958	245708.800168	40.112832
3063.718908	246379.688008	40.117850
3067.154655	247067.969063	40.122868
3070.152656	247758.856285	40.127885
3073.098434	248451.781228	40.132903
3075.472626	249161.278915	40.137920
3078.499452	249869.503092	40.142938
3082.020924	250580.618933	40.147956
3085.043124	251307.000082	40.152973
3087.955767	252033.674410	40.157991
3091.464683	252756.365563	40.163008
3094.710804	253479.170489	40.168026
3097.841873	254210.651690	40.173044
3100.496898	254938.647342	40.178061
3103.572153	255681.179114	40.183079
3106.375591	256420.955157	40.188096
3109.627666	257174.093944	40.193114
3112.684786	257916.717460	40.198132
3116.018567	258676.972118	40.203149
3119.354295	259422.159267	40.208167
3122.370843	260188.042103	40.213184
3125.690112	260955.955386	40.218202
3128.606498	261719.049715	40.223220
3131.437171	262490.305564	40.228237
3134.631059	263263.404153	40.233255
3137.380855	264048.885321	40.238272
3140.556689	264840.059619	40.243290
3143.712720	265618.810821	40.248308
3147.015989	266409.089455	40.253325
3150.534705	267203.976041	40.258343
3153.770643	267992.728533	40.263360
3157.222618	268773.618081	40.268378
3160.690335	269550.968342	40.273396
3163.824026	270349.038039	40.278413
3167.094302	271128.691525	40.283431
3170.650664	271908.166451	40.288448
3173.618762	272700.551932	40.293466
3177.018664	273500.303861	40.298484
3180.079666	274280.926784	40.303501
3183.292066	275067.410662	40.308519
3187.017717	275858.352633	40.313536
3190.381710	276642.638882	40.318554
3193.430588	277425.366728	40.323572
3196.284125	278223.379883	40.328589
3199.259174	279010.547462	40.333607
3202.471770	279802.545533	40.338624
3205.553616	280604.942026	40.343642
3209.000979	281389.217302	40.348660
3212.312156	282189.554405	40.353677
3215.846564	282976.465176	40.358695
3218.688883	283777.644924	40.363712
3221.555372	284580.132124	40.368730
3224.860988	285378.148332	40.373748
3228.120371	286187.030378	40.378765
3231.206198	286977.139542	40.383783
3234.267334	287782.833750	40.388800
3237.384882	288601.001845	40.393818
3240.364675	289393.104245	40.398836
3243.940510	290178.248018	40.403853
3246.743783	290948.014476	40.408871
3250.098699	291728.349070	40.413888
3253.150660	292504.354023	40.418906
3256.262890	293275.566359	40.423924
3259.173732	294070.564686	40.428941
3262.121985	294859.529301	40.433959
3265.122943	295659.696833	40.438976
3268.469074	296460.027830	40.443994
3271.585400	297256.626153	40.449012
3274.628039	298078.967792	40.454029
3277.997078	298903.404227	40.459047
3281.439557	299717.611395	40.464064
3284.561046	300552.165789	40.469082
3287.975901	301381.000359	40.474100
3290.628260	302224.411134	40.479117
3293.626415	303074.633807	40.484135
3296.554220	303928.255243	40.489152
3299.501104	304799.476396	40.494170
3303.428769	305661.670386	40.499188
3306.923969	306540.137391	40.504205
3309.988528	307416.397240	40.509223
3313.364916	308295.308793	40.514240
3316.509962	309182.160006	40.519258
3320.314615	310058.891502	40.524276
3323.639411	310958.753555	40.529293
3326.877818	311833.205960	40.534311
3331.100151	312742.208478	40.539328
3334.492994	313628.151216	40.544346
3338.062999	314510.445369	40.549364
3341.553897	315399.739378	40.554381
3345.175310	316285.620167	40.559399
3348.482252	317180.364051	40.564416
3352.026504	318073.834655	40.569434
3355.828332	318966.409361	40.574452
3358.859184	319850.889756	40.579469
3362.141893	320739.804103	40.584487
3365.661256	321638.356236	40.589504
3368.937593	322541.139442	40.594522
3372.268262	323446.736579	40.599540
3375.533720	324351.512182	40.604557
3378.769303	325243.078599	40.609575
3382.285281	326147.318599	40.614592
3385.510326	327066.299477	40.619610
3389.166472	327970.628749	40.624628
3392.548622	328889.745941	40.629645
3395.915687	329794.788976	40.634663
3399.660681	330708.047703	40.639680
3402.982222	331620.006475	40.644698
3406.630184	332534.454673	40.649716
3410.005358	333446.437449	40.654733
3413.082754	334363.264405	40.659751
3416.715381	335277.470747	40.664768
3420.188309	336197.082366	40.669786
3423.609742	337108.435314	40.674804
3426.847470	338040.111101	40.679821
3430.068021	338972.323520	40.684839
3433.720618	339894.273476	40.689856
3436.843180	340824.296896	40.694874
3440.467233	341740.953105	40.699892
3443.864189	342678.543712	40.704909
3446.735179	343620.350288	40.709927
3450.628311	344557.127538	40.714944
3453.946280	345485.980859	40.719962
3457.617686	346425.251782	40.724980
3460.862111	347363.067071	40.729997
3464.165284	348297.525007	40.735015
3467.599170	349228.469547	40.740020
3470.644249	350129.692036	40.745024
3473.985763	350981.808665	40.750029
3477.063436	351788.393148	40.755034
3480.269165	352525.722905	40.760039
3483.350836	353213.693442	40.765044
3486.244925	353863.272714	40.770048
3489.151002	354442.711480	40.775053
3491.850500	354981.581725	40.780058
3494.262507	355459.285681	40.785063
3496.790181	355895.104499	40.790068
3498.794536	356277.957015	40.795072
3500.838732	356602.114962	40.800077
3502.638650	356880.738712	40.805082
3504.427575	357142.105057	40.810087
3506.230022	357342.421314	40.815092
3507.948620	357515.835498	40.820096
3509.343040	357628.050880	40.825101
3510.552691	357732.772118	40.830106
3511.849685	357791.123866	40.835111
3513.465745	357815.345215	40.840116
3514.198591	357825.472688	40.845120
3515.482816	357788.955162	40.850125
3516.181490	357739.135831	40.855130
3516.916160	357656.602583	40.860135
3517.876548	357565.164204	40.865140
3518.323942	357447.959229	40.870144
3518.931556	357300.968265	40.875149
3519.545388	357157.254129	40.880154
3520.088173	356978.452507	40.885159
3521.008775	356805.131259	40.890164
3521.155871	356606.845194	40.895168
3521.298424	356403.678824	40.900173
3521.667679	356198.366194	40.905178
3521.871622	355972.796329	40.910183
3522.302368	355729.169506	40.915188
3522.336256	355497.192561	40.920192
3522.781585	355225.271408	40.925197
3522.533706	354980.753607	40.930202
3522.713589	354715.147403	40.935207
3523.162409	354442.354750	40.940212
3523.323157	354169.630188	40.945216
3523.037066	353899.413196	40.950221
3523.223837	353608.684214	40.955226
3523.410563	353316.300414	40.960231
3523.385635	353026.514239	40.965236
3523.090802	352731.887307	40.970240
3523.171347	352445.002463	40.975245
3523.343729	352148.136530	40.980250
3523.172358	351844.000914	40.985255
3523.572410	351537.815802	40.990260
3523.388329	351248.623068	40.995264
3523.432679	350930.261025	41.000269
3522.969129	350632.667119	41.005274
3522.982020	350340.563023	41.010279
3523.052358	350022.594737	41.015284
3522.662465	349726.074101	41.020288
3522.486861	349422.551944	41.025293
3522.507004	349118.564214	41.030298
3522.227398	348811.824180	41.035303
3522.326448	348520.224220	41.040308
3521.953192	348221.857049	41.045312
3521.934646	347924.550304	41.050317
3521.734391	347628.438728	41.055322
3521.304086	347333.326537	41.060327
3521.693349	347030.380511	41.065332
3521.499032	346745.090253	41.070336
3521.380497	346453.124841	41.075341
3521.066063	346166.297623	41.080346
3520.622908	345871.581336	41.085351
3521.052684	345586.234523	41.090356
3520.394302	345302.148657	41.095360
3520.435733	345013.196665	41.100365
3520.432495	344735.029182	41.105370
3519.710886	344463.938099	41.110375
3520.114701	344176.396988	41.115380
3519.764375	343899.395656	41.120384
3519.596613	343628.211366	41.125389
3519.592012	343353.643263	41.130394
3519.386969	343083.706363	41.135399
3519.353215	342802.858286	41.140404
3519.047340	342545.188234	41.145408
3518.928428	342271.443047	41.150413
3518.438178	342016.823630	41.155418
3518.279081	341764.972942	41.160423
3518.632020	341504.115562	41.165428
3517.900164	341250.926813	41.170432
3518.423762	340995.251511	41.175437
3518.231352	340739.330308	41.180442
3517.776810	340482.253130	41.185447
3517.785896	340221.338287	41.190452
3517.571576	339991.783697	41.195456
3517.561635	339729.647668	41.200461
3517.523624	339489.611304	41.205466
3516.972102	339254.561301	41.210471
3516.811501	339004.852590	41.215476
3516.972728	338776.553751	41.220480
3516.893695	338525.176072	41.225485
3516.524842	338291.362641	41.230490
3516.277940	338064.140250	41.235495
3516.311704	337832.422390	41.240500
3516.110934	337604.579589	41.245504
3515.731408	337376.407285	41.250509
3515.867649	337150.950209	41.255514
3515.404357	336927.975897	41.260519
3515.434765	336716.061495	41.265524
3515.213941	336491.673376	41.270528
3515.372520	336277.396795	41.275533
3515.462054	336051.965672	41.280538
3515.493231	335842.004261	41.285543
3515.214498	335618.230199	41.290548
3514.682399	335416.797527	41.295552
3514.894131	335204.439163	41.300557
3514.713351	334991.606885	41.305562
3514.261130	334789.268211	41.310567
3514.188762	334578.680030	41.315572
3514.210873	334369.398346	41.320576
3514.095084	334183.687094	41.325581
3514.050194	333977.490963	41.330586
3513.983448	333780.096683	41.335591
3513.863128	333574.647666	41.340596
3513.508274	333388.791824	41.345600
3513.346789	333194.105129	41.350605
3513.309598	333003.060322	41.355610
3512.929812	332818.197446	41.360615
3513.088873	332628.264546	41.365620
3512.611707	332449.646195	41.370624
3512.840165	332266.669327	41.375629
3512.458273	332094.748804	41.380634
3512.502422	331911.214075	41.385639
3512.308506	331727.283311	41.390644
3512.139045	331566.009331	41.395648
3512.267090	331390.979300	41.400653
3512.592667	331222.352391	41.405658
3511.931529	331042.509957	41.410663
3511.973234	330865.608909	41.415668
3511.940595	330708.226811	41.420672
3511.784348	330533.618844	41.425677
3511.712083	330369.959255	41.430682
3511.465138	330203.070647	41.435687
3511.375326	330036.105885	41.440692
3511.283209	329886.843442	41.445696
3510.877892	329732.110002	41.450701
3511.305877	329569.869500	41.455706
3510.968438	329412.911331	41.460711
3511.011903	329255.180794	41.465716
3510.432667	329100.065077	41.470720
3510.916654	328954.982151	41.475725
3510.457748	328801.830410	41.480730
3510.682408	328656.990413	41.485735
3510.633934	328510.335774	41.490740
3510.520784	328363.868752	41.495744
3510.348325	328215.579071	41.500749
3510.227074	328057.386203	41.505754
3509.865814	327924.513760	41.510759
3509.909550	327777.587627	41.515764
3509.860464	327645.250477	41.520768
3509.763711	327502.644031	41.525773
3509.931987	327374.570753	41.530778
3509.473888	327236.394923	41.535783
3509.640550	327092.346816	41.540788
3509.719248	326969.755129	41.545792
3509.491582	326834.136431	41.550797
3509.604543	326701.491016	41.555802
3508.985832	326567.738575	41.560807
3509.349843	326433.068938	41.565812
3509.024332	326310.741930	41.570816
3509.158060	326186.307774	41.575821
3509.175161	326066.470186	41.580826
3508.315901	325942.546644	41.585831
3508.825970	325808.996775	41.590836
3508.204591	325697.168969	41.595840
3508.518039	325575.477531	41.600845
3508.321075	325461.369648	41.605850
3508.315987	325347.511263	41.610855
3508.161002	325237.593422	41.615860
3508.189809	325123.144040	41.620864
3507.944718	325004.056569	41.625869
3508.233741	324891.066696	41.630874
3507.620480	324782.211359	41.635879
3508.000229	324676.278507	41.640884
3508.058385	324574.694724	41.645888
3507.773284	324471.917877	41.650893
3507.990417	324347.363309	41.655898
3507.814112	324253.904797	41.660903
3507.409902	324137.129144	41.665908
3507.459715	324029.541827	41.670912
3507.277958	323936.515903	41.675917
3507.071902	323834.488266	41.680922
3506.957747	323732.802151	41.685927
3507.209333	323634.467412	41.690932
3506.815748	323550.555399	41.695936
3506.867284	323457.848069	41.700941
3507.176674	323366.957268	41.705946
3506.882767	323268.706943	41.710951
3507.003895	323172.960850	41.715956
3506.569325	323076.767192	41.720960
3506.728278	322983.914817	41.725965
3507.061777	322891.060386	41.730970
3506.998915	322809.842616	41.735975
3506.931942	322722.011090	41.740980
3506.756035	322627.760230	41.745984
3506.528746	322527.182753	41.750989
3506.748543	322438.313656	41.755994
3506.668672	322356.207280	41.760999
3506.516375	322257.499964	41.766004
3506.141522	322179.764104	41.771008
3505.817959	322096.321573	41.776013
3506.285003	322020.005622	41.781018
3505.901008	321932.629043	41.786023
3506.131613	321855.306725	41.791028
3506.361915	321782.080146	41.796032
3506.388378	321684.539217	41.801037
3506.031616	321610.768121	41.806042
3505.821926	321538.703831	41.811047
3506.070331	321449.344815	41.816052
3505.539299	321384.631826	41.821056
3505.511659	321306.280390	41.826061
3505.222438	321221.355227	41.831066
3505.344603	321161.933120	41.836071
3505.528148	321088.839855	41.841076
3505.445360	321016.932921	41.846080
3505.678857	320943.424550	41.851085
3505.671922	320874.278527	41.856090
3505.337496	320809.075994	41.861095
3505.367603	320733.919984	41.866100
3505.479355	320670.886257	41.871104
3505.213736	320602.467133	41.876109
3505.368840	320529.529999	41.881114
3505.079989	320455.212026	41.886119
3505.084499	320396.341503	41.891124
3504.692452	320335.548513	41.896128
3504.733209	320274.000868	41.901133
3505.302901	320211.429129	41.906138
3504.405923	320155.141539	41.911143
3504.757928	320088.100608	41.916148
3504.871597	320031.705734	41.921152
3504.606484	319981.475854	41.926157
3504.650929	319915.169645	41.931162
3504.657565	319858.155251	41.936167
3504.610293	319792.015838	41.941172
3504.456238	319743.956256	41.946176
3504.814058	319680.119370	41.951181
3504.914179	319622.021517	41.956186
3504.170129	319567.948079	41.961191
3504.276392	319511.528241	41.966196
3504.563839	319468.004206	41.971200
3504.091226	319412.132683	41.976205
3504.278489	319352.545245	41.981210
3504.180814	319303.433262	41.986215
3504.323711	319250.543716	41.991220
3504.192751	319203.421257	41.996224
3504.059737	319162.150617	42.001229
3504.221263	319110.402857	42.006234
3504.208718	319066.441929	42.011239
3504.210402	319009.732490	42.016244
3504.459771	318952.475421	42.021248
3504.244610	318895.723409	42.026253
3504.538446	318842.911537	42.031258
3504.008058	318796.995960	42.036263
3504.153277	318735.099051	42.041268
3503.868715	318694.971098	42.046272
3504.331917	318644.651245	42.051277
3503.994129	318604.506088	42.056282
3503.954670	318548.921922	42.061287
3504.000134	318489.304587	42.066292
3503.604336	318452.603018	42.071296
3504.091742	318401.872030	42.076301
3503.657503	318359.146647	42.081306
3503.651232	318317.473762	42.086311
3503.800787	318260.867442	42.091316
3503.629895	318227.285335	42.096320
3503.436429	318185.616149	42.101325
3503.536412	318142.628940	42.106330
3503.181789	318111.721449	42.111335
3503.954481	318065.525054	42.116340
3503.626891	318018.075865	42.121344
3503.855398	317988.578210	42.126349
3503.640948	317944.367855	42.131354
3503.389592	317912.884350	42.136359
3503.792576	317863.438051	42.141364
3503.890401	317814.293828	42.146368
3503.860972	317774.430452	42.151373
3503.554080	317725.731038	42.156378
3503.480889	317686.993888	42.161383
3503.587861	317648.355750	42.166388
3503.545574	317608.901313	42.171392
3503.243869	317566.408862	42.176397
3503.437966	317534.168498	42.181402
3503.197234	317496.271533	42.186407
3503.788148	317459.313102	42.191412
3503.634972	317423.463229	42.196416
3503.333247	317387.992746	42.201421
3503.231775	317353.457745	42.206426
3503.343100	317309.602904	42.211431
3503.950242	317262.006766	42.216436
3503.341353	317222.996763	42.221440
3503.361289	317186.509010	42.226445
3503.482755	317145.934525	42.231450
3503.147681	317109.095127	42.236455
3503.753011	317072.973730	42.241460
3503.313088	317032.893992	42.246464
3503.188556	316996.479554	42.251469
3503.095593	316958.889783	42.256474
3503.164681	316927.075606	42.261479
3503.307161	316887.235441	42.266484
3503.277146	316859.889206	42.271488
3503.101137	316826.942905	42.276493
3503.300443	316791.266400	42.281498
3503.130212	316758.980660	42.286503
3503.254475	316726.776071	42.291508
3503.249172	316683.167831	42.296512
3503.106337	316658.052647	42.301517
3503.385674	316621.142231	42.306522
3502.924228	316583.965953	42.311527
3503.194582	316550.186373	42.316532
3502.638945	316525.110208	42.321536
3503.077318	316497.385207	42.326541
3503.275385	316454.584570	42.331546
3502.851003	316425.315163	42.336551
3503.044067	316397.755667	42.341556
3503.090165	316370.906095	42.346560
3502.829566	316338.710508	42.351565
3503.042649	316301.657528	42.356570
3502.959311	316284.089453	42.361575
3503.048606	316238.913956	42.366580
3503.154503	316215.515217	42.371584
3502.975099	316178.014632	42.376589
3503.039389	316134.852955	42.381594
3502.746971	316113.933546	42.386599
3502.678636	316087.305241	42.391604
3502.890378	316063.406453	42.396608
3502.619385	316034.545345	42.401613
3502.913421	316001.397732	42.406618
3502.314335	315975.081327	42.411623
3502.480404	315952.639892	42.416628
3502.447629	315922.087651	42.421632
3502.499982	315908.034844	42.426637
3502.735133	315880.951875	42.431642
3502.399680	315853.601890	42.436647
3502.696187	315833.837005	42.441652
3502.597295	315810.724507	42.446656
3502.349867	315790.586660	42.451661
3502.866126	315755.444978	42.456666
3502.579071	315739.511477	42.461671
3502.920949	315711.037772	42.466676
3502.739137	315686.208015	42.471680
3502.685918	315652.910887	42.476685
3502.921446	315618.092866	42.481690
3502.972879	315596.279821	42.486695
3502.793247	315559.236739	42.491700
3502.561310	315536.043125	42.496704
3502.847101	315519.383898	42.501709
3502.631238	315488.478332	42.506714
3502.683455	315466.843207	42.511719
3502.497982	315435.373094	42.516724
3502.636576	315407.668846	42.521728
3502.463041	315385.483771	42.526733
3502.656075	315351.002956	42.531738
3502.639582	315336.757185	42.536743
3502.673726	315314.615938	42.541748
3502.662763	315288.436178	42.546752
3502.337945	315268.615522	42.551757
3502.415598	315240.615374	42.556762
3502.677887	315226.453202	42.561767
3502.555771	315199.171242	42.566772
3502.585949	315185.834104	42.571776
3502.127920	315151.429479	42.576781
3502.688107	315127.043175	42.581786
3502.492854	315109.899240	42.586791
3502.530124	315086.739639	42.591796
3502.508485	315060.968519	42.596800
3502.553914	315042.438404	42.601805
3502.501811	315012.143008	42.606810
3502.350503	314989.140060	42.611815
3502.472855	314974.719804	42.616820
3502.220749	314941.249695	42.621824
3502.058881	314924.533017	42.626829
3502.261803	314897.327279	42.631834
3502.232076	314879.877494	42.636839
3502.278536	314874.120021	42.641844
3502.417859	314851.936661	42.646848
3502.376338	314825.786856	42.651853
3502.489524	314805.261420	42.656858
3502.363650	314781.134853	42.661863
3502.206787	314752.662188	42.666868
3502.175549	314741.726261	42.671872
3502.476791	314715.980798	42.676877
3502.294491	314693.873087	42.681882
3502.130011	314681.507664	42.686887
3502.357243	314654.552421	42.691892
3502.389714	314646.227253	42.696896
3502.099470	314622.711514	42.701901
3502.510585	314598.882560	42.706906
3502.281012	314578.817715	42.711911
3502.018769	314560.386394	42.716916
3502.150960	314533.267829	42.721920
3501.861658	314522.702969	42.726925
3501.998014	314511.689896	42.731930
3501.940661	314492.768520	42.736935
3501.873461	314476.087765	42.741940
3501.957763	314477.550477	42.746944
3502.371260	314458.555474	42.751949
3502.882301	314427.739096	42.756954
3502.543394	314411.660569	42.761959
3502.404848	314386.696115	42.766964
3502.145537	314360.656425	42.771968
3502.385429	314349.398129	42.776973
3502.156666	314320.732880	42.781978
3502.165009	314312.665866	42.786983
3502.147540	314295.137608	42.791988
3502.063022	314274.693731	42.796993
3502.210430	314249.430054	42.801997
3501.939665	314227.972056	42.807002
3502.233161	314221.208995	42.812007
3501.945440	314202.247181	42.817012
3502.203227	314183.123742	42.822017
3502.075824	314173.398598	42.827021
3502.254681	314148.944168	42.832026
3502.120023	314144.130916	42.837031
3502.404065	314115.258146	42.842036
3501.994923	314100.895264	42.847041
3501.742944	314087.245695	42.852045
3502.294238	314060.570216	42.857050
3501.848474	314047.892376	42.862055
3501.651509	314041.155077	42.867060
3501.855397	314029.469776	42.872065
3502.082758	314005.745575	42.877069
3501.868796	313998.094928	42.882074
3501.764230	313995.058068	42.887079
3502.049104	313971.502970	42.892084
3502.095897	313959.842211	42.897089
3502.049662	313947.483547	42.902093
3501.737049	313932.927410	42.907098
3502.130529	313926.912009	42.912103
3501.979077	313905.944097	42.917108
3501.999368	313880.089422	42.922113
3502.080093	313876.489251	42.927117
3501.966517	313855.693507	42.932122
3501.971320	313836.380474	42.937127
3501.895645	313824.433493	42.942132
3501.920491	313821.758058	42.947137
3501.675111	313805.384805	42.952141
3501.802399	313787.197608	42.957146
3501.948997	313787.989044	42.962151
3501.830774	313766.888651	42.967156
3502.121155	313752.390852	42.972161
3502.019029	313740.982321	42.977165
3502.392162	313716.319176	42.982170
3501.675486	313709.637636	42.987175
3501.793459	313691.757193	42.992180
3501.784775	313667.128270	42.997185
3501.740785	313657.262752	43.002189
3501.937632	313652.677513	43.007194
3501.849645	313648.772920	43.012199
3501.655410	313623.485977	43.017204
3501.856135	313616.381106	43.022209
3502.016468	313608.900878	43.027213
3502.081685	313583.955021	43.032218
3502.196991	313575.769376	43.037223
3501.615508	313561.382380	43.042228
3501.853762	313536.816560	43.047233
3501.972773	313533.439379	43.052237
3502.027166	313522.286216	43.057242
3501.705896	313511.955122	43.062247
3501.520589	313482.773662	43.067252
3501.535219	313476.970101	43.072257
3501.695277	313477.021540	43.077261
3501.500214	313479.571194	43.082266
3501.550167	313468.571380	43.087271
3501.963582	313448.863522	43.092276
3501.916952	313439.914382	43.097281
3501.879487	313434.449742	43.102285
3501.763069	313412.356558	43.107290
3501.618861	313410.063756	43.112295
3501.725613	313403.278881	43.117300
3501.807092	313390.314871	43.122305
3501.951300	313384.541930	43.127309
3502.031360	313355.217123	43.132314
3501.388529	313352.696935	43.137319
3501.734857	313338.877270	43.142324
3502.083056	313323.937736	43.147329
3501.740385	313315.391082	43.152333
3501.986122	313305.531084	43.157338
3502.088991	313294.293952	43.162343
3501.754078	313278.087179	43.167348
3502.002484	313259.397387	43.172353
3501.642482	313241.006264	43.177357
3502.107930	313224.572564	43.182362
3502.190380	313227.994862	43.187367
3502.212189	313217.431952	43.192372
3502.079153	313181.448343	43.197377
3501.870423	313175.552439	43.202381
3501.611537	313149.537442	43.207386
3501.748503	313146.030201	43.212391
3501.841900	313140.646847	43.217396
3501.972982	313127.089775	43.222401
3501.627086	313114.523288	43.227405
3501.921180	313095.215608	43.232410
3501.885931	313091.429948	43.237415
3502.104672	313080.581769	43.242420
3502.267388	313054.373580	43.247425
3502.079872	313045.319165	43.252429
3501.845902	313017.468159	43.257434
3501.865109	313016.472929	43.262439
3502.111325	312998.673950	43.267444
3501.797648	312978.392549	43.272449
3501.764178	312973.665135	43.277453
3501.967743	312955.643802	43.282458
3502.111131	312938.420666	43.287463
3501.899300	312930.871288	43.292468
3501.941010	312925.012534	43.297473
3501.839425	312910.779312	43.302477
3502.060179	312890.668771	43.307482
3501.902937	312883.899648	43.312487
3501.732704	312864.715356	43.317492
3501.928789	312844.201530	43.322497
3501.803046	312838.139939	43.327501
3502.087991	312831.021780	43.332506
3501.873600	312810.266772	43.337511
3502.011866	312798.922207	43.342516
3502.283738	312790.024928	43.347521
3501.972433	312771.982237	43.352525
3501.852161	312754.978370	43.357530
3501.774212	312739.723595	43.362535
3501.908896	312725.071701	43.367540
3502.269071	312710.613557	43.372545
3502.128451	312709.872314	43.377549
3502.031798	312684.900390	43.382554
3501.953949	312689.518267	43.387559
3501.886060	312655.890468	43.392564
3501.871993	312638.539167	43.397569
3501.704433	312634.952271	43.402573
3501.946863	312620.359835	43.407578
3501.847554	312595.464614	43.412583
3501.741602	312595.201409	43.417588
3501.919084	312582.222165	43.422593
3501.986035	312569.514650	43.427597
3501.992317	312559.462923	43.432602
3501.997027	312556.917789	43.437607
3501.774208	312531.202150	43.442612
3502.192262	312512.689098	43.447617
3501.932122	312510.999617	43.452621
3501.811549	312486.743794	43.457626
3501.837215	312480.683930	43.462631
3501.678924	312471.650280	43.467636
3501.679784	312460.225333	43.472641
3501.550481	312441.212584	43.477645
3501.944615	312420.794836	43.482650
3501.668550	312428.268159	43.487655
3501.552943	312418.515356	43.492660
3501.728419	312407.801011	43.497665
3501.688982	312385.339070	43.502669
3501.547721	312385.005047	43.507674
3501.958659	312385.958744	43.512679
3501.605695	312368.329535	43.517684
3501.623668	312346.240280	43.522689
3501.418452	312345.534576	43.527693
3501.438637	312330.366106	43.532698
3501.784303	312326.597168	43.537703
3501.760117	312319.883497	43.542708
3501.783688	312286.597369	43.547713
3501.815621	312295.930966	43.552717
3501.724580	312283.298964	43.557722
3501.899698	312275.917993	43.562727
3501.685095	312250.353587	43.567732
3501.940263	312246.064437	43.572737
3501.471783	312250.896100	43.577741
3501.900063	312240.727439	43.582746
3502.014392	312223.152347	43.587751
3501.918396	312213.447326	43.592756
3501.897996	312203.526921	43.597761
3501.771401	312175.607734	43.602765
3502.084855	312157.721586	43.607770
3501.960078	312161.074578	43.612775
3501.638792	312135.068769	43.617780
3501.726741	312128.362985	43.622785
3501.553205	312122.766791	43.627789
3501.816352	312114.735895	43.632794
3501.901729	312086.121932	43.637799
3501.814709	312089.011007	43.642804
3501.845767	312077.403127	43.647809
3501.878079	312058.924757	43.652813
3501.381146	312042.997339	43.657818
3501.510021	312035.598114	43.662823
3501.605999	312036.397494	43.667828
3502.092006	312028.586197	43.672833
3501.628398	312011.457617	43.677837
3501.527639	311998.190919	43.682842
3501.531533	311999.895291	43.687847
3501.357905	311984.884238	43.692852
3501.951391	311983.773758	43.697857
3501.489783	311974.863769	43.702861
3501.664936	311957.813425	43.707866
3501.787640	311956.649319	43.712871
3501.571556	311950.627181	43.717876
3501.502412	311941.325035	43.722881
3501.351631	311929.491092	43.727885
3501.760353	311905.203109	43.732890
3501.520159	311906.385841	43.737895
3501.814477	311909.317092	43.742900
3501.772716	311898.483920	43.747905
3501.487224	311883.795671	43.752909
3501.692144	311864.806773	43.757914
3501.621246	311865.123333	43.762919
3501.808681	311856.671654	43.767924
3501.835441	311848.423212	43.772929
3501.495159	311836.847882	43.777933
3501.974097	311823.973973	43.782938
3502.026993	311825.416233	43.787943
3501.916144	311800.038926	43.792948
3502.000084	311780.407321	43.797953
3502.112497	311779.753733	43.802957
3502.028861	311752.311046	43.807962
3502.039205	311752.462231	43.812967
3501.813437	311736.136074	43.817972
3502.293614	311712.930987	43.822977
3501.796742	311708.225002	43.827981
3502.156350	311690.535027	43.832986
3501.894928	311665.232079	43.837991
3501.254654	311662.838625	43.842996
3501.554554	311653.733184	43.848001
3501.586075	311656.909102	43.853005
3501.752240	311627.289846	43.858010
3502.023604	311616.789342	43.863015
3501.924693	311609.425662	43.868020
3502.332242	311592.720540	43.873025
3501.851647	311573.787806	43.878029
3501.919599	311566.932394	43.883034
3501.849493	311551.701452	43.888039
3502.074556	311530.826282	43.893044
3502.389155	311528.105416	43.898049
3502.042357	311514.724372	43.903053
3502.329608	311497.758120	43.908058
3501.993332	311480.787561	43.913063
3502.007717	311457.146253	43.918068
3501.866250	311447.626304	43.923073
3501.684245	311436.280589	43.928077
3501.900983	311422.455174	43.933082
3502.250810	311410.364714	43.938087
3501.974792	311399.415376	43.943092
3501.940880	311375.501674	43.948097
3501.695694	311370.959873	43.953101
3502.151632	311357.834974	43.958106
3501.801412	311336.464402	43.963111
3501.959453	311327.457414	43.968116
3502.054742	311317.416952	43.973121
3502.017345	311297.855007	43.978125
3501.717056	311280.471615	43.983130
3501.921593	311282.322765	43.988135
3502.096610	311257.689299	43.993140
3502.004703	311249.408414	43.998145
3502.077019	311242.552272	44.003149
3501.937374	311218.044317	44.008154
3501.756343	311206.494827	44.013159
3501.875081	311205.407660	44.018164
3501.960244	311180.711864	44.023169
3501.755144	311171.049131	44.028173
3501.801162	311158.319062	44.033178
3501.926695	311149.749705	44.038183
3502.033920	311130.674002	44.043188
3501.971430	311116.790369	44.048193
3502.160461	311103.401776	44.053197
3502.080243	311085.703999	44.058202
3501.853908	311077.494992	44.063207
3501.412077	311062.194778	44.068212
3501.903746	311040.437991	44.073217
3501.654203	311031.520114	44.078221
3501.633835	311032.006902	44.083226
3501.790518	311035.315970	44.088231
3501.564562	311016.750340	44.093236
3501.784215	310994.476245	44.098241
3501.922903	311000.612645	44.103245
3501.582453	310988.502765	44.108250
3501.850638	310970.394231	44.113255
3501.465869	310957.909580	44.118260
3501.905452	310944.329095	44.123265
3501.515462	310950.141017	44.128269
3501.620871	310926.841460	44.133274
3501.562948	310921.277940	44.138279
3501.741674	310902.318198	44.143284
3501.842732	310902.556988	44.148289
3501.822589	310907.827617	44.153293
3501.600249	310885.520787	44.158298
3501.516345	310869.960984	44.163303
3501.540737	310869.066683	44.168308
3501.791497	310866.610221	44.173313
3501.428639	310863.537200	44.178317
3501.528408	310833.189890	44.183322
3501.772072	310830.963552	44.188327
3501.694893	310827.260604	44.193332
3501.993949	310812.862327	44.198337
3501.039239	310803.164036	44.203341
3501.703110	310793.925188	44.208346
3501.789961	310782.435499	44.213351
3501.711459	310781.379159	44.218356
3501.894586	310777.177479	44.223361
3501.492421	310766.324055	44.228365
3501.866773	310745.323414	44.233370
3501.686532	310744.410211	44.238375
3501.806755	310739.480421	44.243380
3501.691941	310722.907552	44.248385
3501.532914	310706.621499	44.253389
3501.471873	310701.185672	44.258394
3501.749039	310700.022833	44.263399
3501.588050	310699.004834	44.268404
3501.874302	310670.943875	44.273409
3501.580968	310664.959097	44.278413
3501.534193	310658.045151	44.283418
3501.763938	310657.474989	44.288423
3501.617506	310648.286457	44.293428
3501.718173	310626.616057	44.298433
3501.597746	310617.779702	44.303437
3501.667534	310608.124771	44.308442
3501.711530	310605.547945	44.313447
3501.586009	310599.918617	44.318452
3501.706904	310581.425822	44.323457
3501.670428	310581.838794	44.328461
3501.418573	310572.310481	44.333466
3501.701943	310560.484658	44.338471
3501.454114	310555.994085	44.343476
3502.091214	310540.957611	44.348481
3501.632794	310538.764684	44.353485
3501.632772	310534.337152	44.358490
3501.799692	310512.809021	44.363495
3501.481205	310507.387974	44.368500
3501.856889	310491.578071	44.373505
3501.409700	310489.612403	44.378509
3501.558962	310489.436518	44.383514
3501.934983	310468.588173	44.388519
3501.331514	310461.532215	44.393524
3501.763759	310439.937123	44.398529
3501.469770	310439.626964	44.403533
3501.777895	310441.996327	44.408538
3501.729021	310421.825104	44.413543
3501.958856	310406.241546	44.418548
3502.016845	310404.476805	44.423553
3501.551317	310378.976064	44.428557
3501.568663	310363.374819	44.433562
3501.544770	310356.075556	44.438567
3501.674385	310359.414350	44.443572
3501.872996	310350.426281	44.448577
3501.787901	310335.502651	44.453581
3501.791551	310319.369158	44.458586
3502.030073	310321.316819	44.463591
3501.758895	310310.290133	44.468596
3501.913559	310280.112016	44.473601
3501.660545	310281.627595	44.478605
3501.653866	310266.080968	44.483610
3502.051514	310269.174292	44.488615
3501.633226	310248.679053	44.493620
3501.763085	310231.457046	44.498625
3501.380258	310231.669704	44.503629
3501.766550	310223.441111	44.508634
3501.838825	310207.067833	44.513639
3501.601100	310203.313596	44.518644
3501.576670	310193.596972	44.523649
3501.573897	310193.801106	44.528653
3501.422746	310185.325726	44.533658
3501.723786	310166.957286	44.538663
3501.704898	310156.629072	44.543668
3501.503985	310153.428900	44.548673
3501.724016	310144.361105	44.553677
3501.590330	310138.478533	44.558682
3501.751467	310124.152505	44.563687
3501.492075	310113.989115	44.568692
3501.705292	310108.077752	44.573697
3501.539648	310105.024741	44.578701
3502.115944	310088.547178	44.583706
3502.078899	310084.863344	44.588711
3501.788532	310076.435155	44.593716
3501.968203	310056.457067	44.598721
3501.858311	310041.384542	44.603725
3501.740058	310030.817370	44.608730
3501.899954	310023.336643	44.613735
3501.609970	310005.416794	44.618740
3501.812178	309988.361516	44.623745
3501.782562	309987.272069	44.628749
3501.553018	309975.882545	44.633754
3501.265543	309950.328292	44.638759
3501.435087	309954.093464	44.643764
3501.534760	309945.756954	44.648769
3501.481227	309940.141741	44.653773
3501.513639	309938.915362	44.658778
3501.712826	309944.482614	44.663783
3501.766008	309932.260032	44.668788
3501.643912	309914.542922	44.673793
3501.428001	309912.541072	44.678797
3501.523782	309900.642628	44.683802
3501.788986	309902.458902	44.688807
3501.372331	309894.406679	44.693812
3501.563258	309880.712088	44.698817
3501.407737	309876.614166	44.703821
3501.287953	309868.235613	44.708826
3501.639536	309864.847257	44.713831
3501.697809	309869.495020	44.718836
3501.761114	309862.334730	44.723841
3501.399925	309838.471424	44.728845
3501.498596	309833.010529	44.733850
3501.892002	309816.663253	44.738855
3501.434569	309816.862130	44.743860
3501.690590	309814.353899	44.748865
3501.608300	309792.075558	44.753869
3501.611300	309785.968000	44.758874
3501.628088	309777.593526	44.763879
3501.393369	309777.426776	44.768884
3501.667223	309773.287164	44.773889
3501.737889	309761.876101	44.778893
3501.594302	309751.363721	44.783898
3501.991722	309743.565902	44.788903
3501.586878	309745.054342	44.793908
3501.787693	309717.693246	44.798913
3501.219107	309707.196408	44.803917
3501.696249	309695.289185	44.808922
3501.799275	309684.611002	44.813927
3501.399469	309690.857205	44.818932
3501.425766	309685.280375	44.823937
3501.513769	309658.394926	44.828941
3501.823226	309648.498758	44.833946
3501.719434	309643.044049	44.838951
3501.280674	309648.660177	44.843956
3501.195654	309651.040151	44.848961
3501.412265	309649.683180	44.853965
3501.523192	309638.036772	44.858970
3501.668269	309620.048763	44.863975
3501.496484	309615.317191	44.868980
3501.729533	309607.265133	44.873985
3501.641962	309604.276226	44.878989
3501.460804	309601.709099	44.883994
3501.863434	309581.746850	44.888999
3501.661843	309570.301966	44.894004
3501.798363	309567.685172	44.899009
3501.634196	309567.787306	44.904013
3501.691955	309545.537849	44.909018
3502.014373	309535.028908	44.914023
3501.707775	309536.374760	44.919028
3501.857402	309519.760133	44.924033
3501.381078	309505.380900	44.929037
3501.746967	309495.195963	44.934042
3501.763869	309486.592399	44.939047
3501.949538	309497.378429	44.944052
3501.881663	309463.722921	44.949057
3501.948421	309441.802819	44.954061
3501.965112	309440.604333	44.959066
3501.946077	309413.989951	44.964071
3501.602983	309410.659276	44.969076
3502.041905	309404.508965	44.974081
3501.629555	309394.827381	44.979085
3501.428326	309380.914041	44.984090
3501.829961	309368.178795	44.989095
3501.357716	309370.950131	44.994100
3501.494656	309358.765203	44.999105
3501.641248	309358.691519	45.004109
3501.429493	309341.395367	45.009114
3501.228459	309336.693788	45.014119
3500.956432	309330.858193	45.019124
3501.546543	309319.035005	45.024129
3501.229724	309319.008324	45.029133
3501.383257	309309.416382	45.034138
3501.422460	309308.570630	45.039143
3501.310372	309304.873021	45.044148
3501.666729	309307.642053	45.049153
3501.590266	309297.271762	45.054157
3501.879134	309286.666224	45.059162
3501.577329	309271.445333	45.064167
3501.560242	309282.822944	45.069172
3501.753850	309280.349892	45.074177
3501.797616	309257.288186	45.079181
3501.658763	309243.415949	45.084186
3501.825841	309246.876198	45.089191
3501.591432	309232.128252	45.094196
3501.601552	309201.310435	45.099201
3501.840038	309204.199688	45.104205
3501.645865	309195.374601	45.109210
3501.531442	309185.875421	45.114215
3501.353375	309185.852494	45.119220
3501.576655	309162.431866	45.124225
3501.537115	309157.628680	45.129229
3501.385638	309148.058944	45.134234
3502.100073	309144.155764	45.139239
3501.628051	309142.117580	45.144244
3501.586303	309116.422681	45.149249
3501.618655	309110.081425	45.154253
3501.517863	309103.862773	45.159258
3501.575692	309106.780276	45.164263
3501.353534	309102.438235	45.169268
3501.806251	309093.130289	45.174273
3501.541461	309078.056232	45.179277
3501.705844	309075.562291	45.184282
3501.619205	309065.473460	45.189287
3501.474089	309075.471544	45.194292
3501.708872	309049.987848	45.199297
3501.122077	309048.858254	45.204301
3501.604822	309032.725770	45.209306
3501.629420	309028.803194	45.214311
3501.388197	309023.319006	45.219316
3501.334962	309024.090871	45.224321
3501.215008	309017.798862	45.229325
3501.300145	309022.824214	45.234330
3501.708504	309015.838877	45.239335
3501.635349	308998.851747	45.244340
3501.445481	308982.290014	45.249345
3501.375770	308981.105024	45.254349
3501.426282	308977.712782	45.259354
3501.421443	308975.067162	45.264359
3501.417440	308984.712390	45.269364
3501.549408	308953.671789	45.274369
3501.687629	308946.779570	45.279373
3501.545019	308945.656871	45.284378
3501.543335	308936.699854	45.289383
3501.388558	308935.477268	45.294388
3501.529081	308932.707131	45.299393
3501.611535	308910.809783	45.304397
3501.600602	308902.897541	45.309402
3502.095602	308891.928877	45.314407
3501.597783	308898.724897	45.319412
3501.727398	308884.607007	45.324417
3501.513003	308870.848264	45.329421
3501.784168	308862.484756	45.334426
3501.841544	308858.455253	45.339431
3501.654581	308843.063590	45.344436
3501.563047	308828.802129	45.349441
3501.563390	308816.663868	45.354445
3501.527719	308818.959825	45.359450
3501.714509	308816.157000	45.364455
3501.660414	308802.067809	45.369460
3501.672189	308780.156005	45.374465
3501.908417	308768.362563	45.379469
3501.555634	308767.832558	45.384474
3501.571789	308761.595578	45.389479
3501.484595	308750.870586	45.394484
3501.311437	308740.159032	45.399489
3501.221297	308739.689754	45.404493
3501.311625	308736.952901	45.409498
3501.730991	308726.275945	45.414503
3501.236601	308724.470266	45.419508
3501.513095	308725.521401	45.424513
3501.308059	308724.459350	45.429517
3501.432181	308707.364935	45.434522
3501.487242	308699.238764	45.439527
3501.448950	308698.048856	45.444532
3501.380883	308690.959826	45.449537
3501.252807	308700.039219	45.454541
3501.594490	308692.886130	45.459546
3501.789335	308680.081244	45.464551
3501.491693	308662.645594	45.469556
3501.563868	308649.961668	45.474561
3501.579725	308646.065875	45.479565
3501.484132	308639.922692	45.484570
3501.596887	308632.474569	45.489575
3501.481556	308623.916972	45.494580
3501.502860	308609.128859	45.499585
3501.640859	308604.425099	45.504589
3501.073393	308594.309553	45.509594
3501.345027	308593.732819	45.514599
3501.328705	308594.855183	45.519604
3501.317461	308598.037989	45.524609
3501.476600	308593.814423	45.529613
3501.496562	308589.561720	45.534618
3501.593441	308570.232148	45.539623
3501.613139	308561.271720	45.544628
3501.493178	308553.249230	45.549633
3501.139396	308552.973852	45.554637
3501.246464	308560.387877	45.559642
3501.486245	308544.980298	45.564647
3501.300405	308551.778485	45.569652
3501.709250	308550.798588	45.574657
3501.577161	308539.978780	45.579661
3501.497904	308527.343944	45.584666
3501.289321	308522.032728	45.589671
3501.334579	308526.529970	45.594676
3501.450582	308528.293280	45.599681
3501.567951	308519.470259	45.604685
3501.203976	308509.908172	45.609690
3501.539184	308489.523411	45.614695
3501.374549	308487.946091	45.619700
3501.525406	308488.940531	45.624705
3501.828742	308476.449447	45.629709
3501.484541	308477.953890	45.634714
3501.511546	308472.707627	45.639719
3501.523314	308449.065251	45.644724
3501.117730	308436.328725	45.649729
3501.381516	308440.104729	45.654733
3501.237587	308448.601357	45.659738
3501.932388	308442.945318	45.664743
3501.656607	308447.238284	45.669748
3501.850330	308427.079197	45.674753
3501.406107	308415.697421	45.679757
3501.299234	308398.079168	45.684762
3501.299517	308401.769134	45.689767
3501.154779	308397.923876	45.694772
3501.521800	308397.688492	45.699777
3501.311149	308406.984430	45.704781
3501.267065	308392.944450	45.709786
3501.336099	308390.032774	45.714791
3501.234159	308376.510784	45.719796
3501.251087	308353.020239	45.724801
3501.618029	308352.072338	45.729805
3501.444171	308348.867816	45.734810
3501.332733	308349.979608	45.739815
3501.347522	308354.328945	45.744820
3501.485817	308328.961748	45.749825
3501.779595	308272.753281	45.754829
3501.448514	308176.460728	45.759834
3501.705041	308026.330698	45.764839
3501.317844	307827.593862	45.769844
3501.139789	307582.330262	45.774849
3500.754250	307293.887143	45.779853
3500.698767	306962.306960	45.784858
3500.804493	306570.106759	45.789863
3499.858149	306133.558348	45.794868
3499.485284	305643.499346	45.799873
3499.325577	305124.186690	45.804877
3498.498196	304545.726927	45.809882
3498.253891	303932.074344	45.814887
3497.602554	303262.462606	45.819892
3496.909551	302549.659505	45.824897
3496.415856	301785.557805	45.829901
3496.098130	300983.673607	45.834906
3495.620947	300113.261418	45.839911
3494.566556	299216.608234	45.844916
3493.609408	298258.126855	45.849921
3493.206196	297261.617680	45.854925
3492.063996	296216.896119	45.859930
3491.336030	295122.964980	45.864935
3490.136637	293985.865663	45.869940
3489.681888	292785.322063	45.874945
3488.624440	291555.473393	45.879949
3487.478733	290280.531648	45.884954
3486.583753	288941.323825	45.889959
3485.180109	287578.492591	45.894964
3484.161803	286162.264823	45.899969
3483.048940	284702.208662	45.904973
3481.874800	283202.441123	45.909978
3480.823096	281643.684651	45.914983
3479.371402	280056.034942	45.919988
3477.734243	278419.674971	45.924993
3476.732860	276745.549686	45.929997
3474.951654	275030.925617	45.935002
3473.605951	273255.903930	45.940007
3471.954696	271462.967410	45.945012
3470.288739	269619.223748	45.950017
3468.884125	267741.434051	45.955021
3467.075853	265819.490846	45.960026
3465.602431	263866.544760	45.965031
3463.300307	261877.659335	45.970036
3461.681677	259847.963404	45.975041
3460.043450	257780.749989	45.980045
3458.107716	255675.247870	45.985050
3456.097399	253534.045663	45.990055
3453.955518	251369.911950	45.995060
3452.444275	249160.674402	46.000065
3450.048469	246928.803918	46.005069
3447.510338	244659.796971	46.010074
3445.608353	242351.215828	46.015079
3443.233645	240023.381120	46.020084
3440.870912	237658.620838	46.025089
3438.796758	235264.611119	46.030093
3436.582329	232846.821188	46.035098
3434.030790	230390.716645	46.040103
3430.979396	227925.258936	46.045108
3428.505984	225410.857031	46.050113
3426.100354	222893.591544	46.055117
3423.122470	220337.375010	46.060122
3420.803950	217764.762931	46.065127
3417.792354	215176.837045	46.070132
3415.270686	212545.910824	46.075137
3412.696808	209912.263457	46.080141
3409.565129	207254.483482	46.085146
3406.490782	204551.112657	46.090151
3403.452368	201856.279064	46.095156
3400.212834	199128.691303	46.100161
3397.277513	196387.606011	46.105165
3393.964101	193639.833197	46.110170
3390.986474	190867.721063	46.115175
3387.334204	188086.484119	46.120180
3383.888947	185295.175603	46.125185
3380.854364	182499.753686	46.130189
3376.848090	179681.648772	46.135194
3373.404774	176853.079298	46.140199
3369.661498	174031.742053	46.145204
3365.566949	171201.724589	46.150209
3362.130360	168362.111846	46.155213
3358.006969	165531.870614	46.160218
3354.463375	162689.627132	46.165223
3350.068041	159844.089158	46.170228
3345.810152	157012.519102	46.175233
3342.008957	154177.091487	46.180237
3337.381673	151354.340568	46.185242
3332.512556	148530.906051	46.190247
3327.627308	145736.597752	46.195252
3322.588848	142954.438522	46.200257
3317.156190	140202.714557	46.205261
3311.511220	137391.410768	46.210266
3305.702444	134691.134648	46.215271
3299.140131	132048.993210	46.220276
3293.134327	129430.850857	46.225281
3286.899563	126857.143488	46.230285
3280.054137	124361.898535	46.235290
3273.063903	121895.420004	46.240295
3265.667003	119503.058429	46.245300
3258.412511	117166.368006	46.250305
3250.644599	114895.197088	46.255309
3242.685554	112717.725919	46.260314
3234.179929	110625.223202	46.265319
3225.229845	108611.341865	46.270324
3216.359189	106700.841847	46.275329
3207.705296	104880.364143	46.280333
3198.014229	103173.315566	46.285338
3188.878649	101560.098030	46.290343
3179.784425	100052.320089	46.295348
3171.086328	98638.079923	46.300353
3162.294860	97331.244568	46.305357
3153.408992	96133.008909	46.310362
3145.452431	95008.583983	46.315367
3137.514165	93980.584611	46.320372
3130.349848	93033.761621	46.325377
3123.325869	92162.069368	46.330381
3115.924608	91367.984112	46.335386
3109.835264	90638.567548	46.340391
3103.551060	89959.667467	46.345396
3097.944561	89352.807453	46.350401
3092.720840	88783.457484	46.355405
3087.560730	88263.900598	46.360410
3082.654117	87775.656689	46.365415
3077.841997	87325.025333	46.370420
3073.284411	86904.445890	46.375425
3068.993363	86516.862672	46.380429
3065.519829	86145.875752	46.385434
3061.314903	85778.768382	46.390439
3057.618477	85439.458921	46.395444
3054.008474	85111.116135	46.400449
3050.365255	84786.656931	46.405453
3046.264274	84476.907599	46.410458
3043.406171	84170.219343	46.415463
3040.328730	83865.321728	46.420468
3036.886795	83565.298896	46.425473
3033.827322	83272.536412	46.430477
3030.324243	82980.125767	46.435482
3027.232181	82681.365915	46.440487
3024.161086	82393.860564	46.445492
3020.715998	82097.207204	46.450497
3017.490173	81801.678588	46.455501
3014.107328	81508.705387	46.460506
3010.820267	81194.863191	46.465511
3007.455927	80914.709818	46.470516
3004.006181	80614.884548	46.475521
3001.096476	80315.994175	46.480525
2997.178643	80018.750750	46.485530
2993.843484	79709.403699	46.490535
2990.429382	79417.943318	46.495540
2986.819361	79122.477624	46.500545
2983.461826	78822.542891	46.505549
2979.786438	78545.802363	46.510554
2976.478560	78245.116766	46.515559
2972.894344	77956.835489	46.520564
2969.223055	77664.443151	46.525569
2965.907189	77369.636053	46.530573
2961.963688	77085.916079	46.535578
2958.657925	76792.891660	46.540583
2955.251481	76505.563065	46.545588
2951.658448	76238.269098	46.550593
2948.113298	75945.811925	46.555597
2944.257411	75670.258980	46.560602
2940.868552	75386.520784	46.565607
2936.853311	75127.177531	46.570612
2933.212150	74854.990067	46.575617
2929.611469	74576.792314	46.580621
2926.197931	74312.448229	46.585626
2922.498568	74054.386622	46.590631
2918.870748	73793.433685	46.595636
2914.813381	73543.509437	46.600641
2911.706160	73278.581617	46.605645
2907.997724	73027.007623	46.610650
2904.498865	72766.133462	46.615655
2900.249364	72537.429512	46.620660
2896.834796	72282.210329	46.625665
2893.278210	72042.354960	46.630669
2889.740003	71807.616131	46.635674
2886.444504	71560.765881	46.640679
2882.496960	71337.751783	46.645684
2879.258923	71087.544812	46.650689
2875.815718	70853.764647	46.655693
2872.072047	70625.239446	46.660698
2868.485950	70389.593878	46.665703
2864.426566	70169.159355	46.670708
2861.061142	69936.860782	46.675713
2857.870174	69707.990537	46.680717
2854.093429	69490.602888	46.685722
2850.654743	69261.667395	46.690727
2847.116674	69043.763691	46.695732
2843.804774	68811.949278	46.700737
2840.555331	68582.291891	46.705741
2836.811713	68363.632551	46.710746
2833.571834	68132.460480	46.715751
2829.874759	67910.534819	46.720756
2826.365126	67685.166575	46.725761
2822.903109	67455.120833	46.730765
2819.364178	67237.283333	46.735770
2815.973819	67008.499959	46.740775
2812.587608	66790.661422	46.745780
2809.053633	66571.089557	46.750785
2805.678204	66335.390945	46.755789
2802.092048	66118.687559	46.760794
2798.825174	65878.259988	46.765799
2795.214370	65651.097462	46.770804
2791.761485	65429.047292	46.775809
2788.245303	65188.512921	46.780813
2784.723494	64976.741098	46.785818
2781.391553	64747.023225	46.790823
2777.475692	64518.541259	46.795828
2773.775025	64297.111053	46.800833
2770.685327	64066.618897	46.805837
2766.968671	63839.159217	46.810842
2763.283904	63621.077345	46.815847
2760.238890	63398.029279	46.820852
2756.556904	63172.886838	46.825857
2753.191893	62942.416369	46.830861
2749.275907	62721.338441	46.835866
2746.216144	62492.563385	46.840871
2742.674739	62273.607746	46.845876
2739.447154	62039.938175	46.850881
2735.824454	61816.049020	46.855885
2732.204961	61594.566674	46.860890
2728.989976	61363.839900	46.865895
2725.445155	61121.020106	46.870900
2721.743398	60901.029194	46.875905
2718.324469	60667.415238	46.880909
2714.515988	60447.324505	46.885914
2711.004007	60216.673986	46.890919
2707.561037	59994.131354	46.895924
2704.390010	59763.171595	46.900929
2700.726639	59536.688711	46.905933
2697.074740	59304.774130	46.910938
2693.776415	59074.976698	46.915943
2690.093954	58854.030294	46.920948
2686.347284	58634.758499	46.925953
2683.312816	58391.168952	46.930957
2679.728812	58180.499449	46.935962
2676.461823	57942.465034	46.940967
2672.779869	57710.697312	46.945972
2669.220537	57487.548628	46.950977
2665.866202	57256.838115	46.955981
2662.746484	57022.742850	46.960986
2659.143103	56788.116384	46.965991
2656.091271	56561.819522	46.970996
2652.077056	56326.278351	46.976001
2648.427407	56090.726894	46.981005
2644.724421	55860.325470	46.986010
2641.217992	55626.177454	46.991015
2637.744584	55396.480607	46.996020
2634.160150	55167.412438	47.001025
2631.113728	54931.911329	47.006029
2627.409715	54702.453951	47.011034
2624.232952	54465.474195	47.016039
2620.832460	54232.129119	47.021044
2617.038118	53997.794784	47.026049
2613.746267	53750.682819	47.031053
2610.183571	53524.152215	47.036058
2606.690757	53279.595307	47.041063
2603.213230	53049.756968	47.046068
2599.017210	52822.012623	47.051073
2596.036371	52577.141882	47.056077
2592.175905	52343.075480	47.061082
2588.691504	52110.976303	47.066087
2585.047489	51877.711763	47.071092
2581.655595	51652.796582	47.076097
2578.352506	51405.857036	47.081101
2575.000517	51188.209989	47.086106
2571.358006	50940.269102	47.091111
2567.928979	50707.566296	47.096116
2564.669944	50476.317264	47.101121
2561.185871	50234.949995	47.106125
2557.251624	49999.516891	47.111130
2554.168887	49772.085047	47.116135
2550.854549	49526.829263	47.121140
2546.940926	49293.969148	47.126145
2543.418932	49047.418912	47.131149
2539.760173	48816.604303	47.136154
2536.426019	48586.267709	47.141159
2533.382916	48340.988532	47.146164
2529.528190	48099.549481	47.151169
2526.265818	47855.369072	47.156173
2522.366389	47628.060921	47.161178
2519.095206	47380.893251	47.166183
2515.321162	47139.267845	47.171188
2511.914683	46905.039905	47.176193
2508.472085	46666.754568	47.181197
2504.899302	46428.479423	47.186202
2501.769696	46188.716802	47.191207
2498.137050	45941.037922	47.196212
2494.471196	45711.283453	47.201217
2491.237584	45464.543113	47.206221
2487.645295	45221.609706	47.211226
2484.254440	44977.030232	47.216231
2480.989240	44733.023566	47.221236
2476.934819	44494.482800	47.226241
2473.560175	44246.490566	47.231245
2470.085590	44013.584461	47.236250
2466.383572	43765.154149	47.241255
2463.332681	43525.414079	47.246260
2459.484511	43276.993065	47.251265
2455.996422	43042.932427	47.256269
2452.882511	42807.154311	47.261274
2448.904807	42555.185169	47.266279
2445.612912	42320.575166	47.271284
2442.176544	42077.296625	47.276289
2438.611774	41831.409334	47.281293
2434.978944	41592.440733	47.286298
2431.688451	41333.783480	47.291303
2428.207091	41099.374666	47.296308
2424.557237	40852.300561	47.301313
2421.441612	40601.829508	47.306317
2417.475295	40364.340447	47.311322
2414.027019	40123.704118	47.316327
2410.462115	39871.270087	47.321332
2406.817799	39628.514147	47.326337
2403.436143	39380.406651	47.331341
2400.020083	39146.547550	47.336346
2396.497210	38898.195033	47.341351
2393.185267	38651.156469	47.346356
2389.680253	38400.302538	47.351361
2386.164599	38162.171129	47.356365
2382.589264	37916.399451	47.361370
2378.970415	37662.332240	47.366375
2376.004026	37419.812050	47.371380
2372.217489	37172.496986	47.376385
2369.255984	36924.745067	47.381389
2365.131736	36678.052768	47.386394
2361.806768	36422.090463	47.391399
2358.218853	36168.074172	47.396404
2354.582555	35932.864477	47.401409
2351.552759	35669.517786	47.406413
2347.956524	35417.324768	47.411418
2344.427545	35170.430023	47.416423
2341.043065	34910.552308	47.421428
2337.496558	34656.446184	47.426433
2334.446361	34400.154636	47.431437
2330.718106	34144.980137	47.436442
2327.374965	33891.377520	47.441447
2323.794427	33630.779239	47.446452
2319.798973	33375.592480	47.451457
2316.426682	33127.302647	47.456461
2312.657768	32867.370817	47.461466
2309.468624	32616.053996	47.466471
2306.332488	32351.206131	47.471476
2302.457983	32091.186377	47.476481
2299.322342	31832.943014	47.481485
2295.620101	31584.729458	47.486490
2292.174771	31311.596038	47.491495
2289.037612	31066.253730	47.496500
2285.500358	30798.522258	47.501505
2281.895545	30523.358056	47.506509
2277.837865	30268.966914	47.511514
2274.618767	30004.085885	47.516519
2271.393637	29741.401947	47.521524
2267.704526	29483.572305	47.526529
2264.585169	29212.069659	47.531533
2260.875716	28954.851868	47.536538
2257.242179	28688.595053	47.541543
2254.105922	28425.641528	47.546548
2250.265253	28161.977785	47.551553
2246.967855	27891.128832	47.556557
2243.320642	27620.648702	47.561562
2239.934494	27356.702464	47.566567
2236.149882	27088.563790	47.571572
2232.413833	26824.894641	47.576577
2229.504226	26554.687139	47.581581
2226.123619	26293.136354	47.586586
2222.521621	26019.698716	47.591591
2219.176863	25746.515994	47.596596
2215.527088	25486.082242	47.601601
2212.119760	25212.555381	47.606605
2208.695313	24940.872334	47.611610
2204.911324	24665.739151	47.616615
2201.544884	24397.501078	47.621620
2198.139394	24119.046919	47.626625
2195.126684	23842.353492	47.631629
2191.220130	23575.326001	47.636634
2187.893987	23297.181311	47.641639
2184.596914	23008.259561	47.646644
2180.824892	22741.754355	47.651649
2177.480456	22462.838610	47.656653
2174.102698	22183.064091	47.661658
2170.665240	21891.475469	47.666663
2166.897367	21617.205382	47.671668
2163.152895	21336.581642	47.676673
2159.554316	21059.898254	47.681677
2156.299987	20783.519626	47.686682
2152.290024	20508.574351	47.691687
2148.991748	20228.884763	47.696692
2145.314752	19964.802905	47.701697
2141.822529	19684.074589	47.706701
2137.838086	19426.711733	47.711706
2134.170890	19175.079325	47.716711
2130.405805	18906.585336	47.721716
2126.459439	18651.525991	47.726721
2122.912217	18396.527881	47.731725
2118.918838	18154.327451	47.736730
2115.073963	17912.531166	47.741735
2111.460743	17675.109841	47.746740
2107.281643	17453.835475	47.751745
2103.637082	17231.282982	47.756749
2099.505067	17016.251058	47.761754
2095.249201	16811.225398	47.766759
2091.547265	16600.741481	47.771764
2087.630917	16414.989696	47.776769
2084.351097	16216.220520	47.781773
2080.686322	16031.896030	47.786778
2076.753091	15839.173417	47.791783
2073.836895	15645.666647	47.796788
2070.162532	15464.002623	47.801793
2066.643898	15282.062644	47.806797
2063.338561	15102.089010	47.811802
2059.688267	14908.625397	47.816807
2056.559375	14727.310486	47.821812
2052.831512	14548.446739	47.826817
2049.695543	14359.407522	47.831821
2045.776444	14176.014619	47.836826
2042.469163	13984.156330	47.841831
2039.033793	13802.553066	47.846836
2035.033512	13627.305719	47.851841
2031.725022	13430.422223	47.856845
2028.232144	13260.250130	47.861850
2025.005494	13081.391436	47.866855
2021.690906	12894.003115	47.871860
2017.896383	12719.814757	47.876865
2015.035856	12536.224606	47.881869
2011.379945	12350.550882	47.886874
2007.803573	12167.905800	47.891879
2004.441929	11978.621735	47.896884
2000.741737	11801.777280	47.901889
1997.200449	11614.304190	47.906893
1993.879134	11431.328768	47.911898
1990.362871	11247.312449	47.916903
1987.169088	11064.130708	47.921908
1983.688783	10888.979433	47.926913
1980.002571	10689.268105	47.931917
1976.316891	10510.711453	47.936922
1973.002959	10330.116683	47.941927
1969.648180	10133.898554	47.946932
1965.813665	9954.189768	47.951937
1962.258685	9765.888988	47.956941
1958.632435	9590.791729	47.961946
1955.108102	9408.130625	47.966951
1952.140438	9225.859018	47.971956
1948.472707	9051.393753	47.976961
1945.262790	8858.521698	47.981965
1941.903443	8674.534713	47.986970
1938.240609	8481.990674	47.991975
1934.905872	8296.212055	47.996980
1931.303685	8115.538322	48.001985
1928.244409	7917.189354	48.006989
1924.415393	7735.421704	48.011994
1920.530790	7541.162358	48.016999
1917.246044	7351.229641	48.022004
1913.193780	7167.904166	48.027009
1909.963050	6981.862983	48.032013
1906.162569	6796.533177	48.037018
1902.948119	6608.894908	48.042023
1899.686215	6427.098928	48.047028
1896.018342	6248.776864	48.052033
1892.936815	6050.999033	48.057037
1889.665632	5872.074209	48.062042
1885.845877	5680.182217	48.067047
1882.533183	5478.902184	48.072052
1878.675931	5291.295735	48.077057
1875.101257	5103.931821	48.082061
1871.502616	4919.617987	48.087066
1868.192705	4732.725972	48.092071
1865.157594	4541.223203	48.097076
1861.367876	4355.546241	48.102081
1858.173333	4168.056538	48.107085
1854.256447	3968.666228	48.112090
1851.151165	3777.286930	48.117095
1847.431859	3594.556025	48.122100
1843.620176	3402.417855	48.127105
1840.121175	3202.575046	48.132109
1836.323110	3018.530101	48.137114
1832.837124	2835.321036	48.142119
1829.106163	2638.071205	48.147124
1825.449846	2457.832235	48.152129
1822.366820	2274.765161	48.157133
1819.028366	2094.239615	48.162138
1815.343609	1908.511288	48.167143
1811.666120	1719.632304	48.172148
1808.383486	1542.913146	48.177153
1804.652600	1353.786923	48.182157
1801.063777	1180.501615	48.187162
1797.133193	1005.990062	48.192167
1793.713671	830.533317	48.197172
1790.459531	654.957498	48.202177
1786.541442	483.128939	48.207181
1782.822113	320.158195	48.212186
1778.248237	163.248520	48.217191
1774.212608	23.656891	48.222196
1764.794619	24.719619	48.227201
1755.942352	48.387771	48.232205
1751.016780	59.279758	48.237210
1747.753626	65.311410	48.242215
1745.294636	57.011724	48.247220
1742.816125	64.888467	48.252225
1740.514394	54.903174	48.257229
1737.670281	53.187529	48.262234
1734.079888	57.125337	48.267239
1730.267404	53.400367	48.272244
1726.821553	64.769481	48.277249
1724.059254	52.037323	48.282253
1720.975854	60.527599	48.287258
1717.225354	61.326665	48.292263
1714.431806	55.556607	48.297268
1710.743164	53.099932	48.302273
1706.693132	53.945879	48.307277
1703.254989	52.405472	48.312282
1700.277850	53.966211	48.317287
1697.117054	56.220092	48.322292
1693.191412	60.055355	48.327297
1690.134525	53.620991	48.332301
1686.292774	53.820572	48.337306
1682.741420	55.822366	48.342311
1679.476082	57.111835	48.347316
1676.286433	57.598509	48.352321
1673.031078	57.718974	48.357325
1669.733023	55.565022	48.362330
1665.570308	57.671996	48.367335
1662.580765	67.390973	48.372340
1658.622458	61.328654	48.377345
1655.588396	61.708725	48.382349
1651.981799	53.319756	48.387354
1648.213898	62.005766	48.392359
1644.847760	55.433154	48.397364
1641.351650	60.330686	48.402369
1638.306794	53.404069	48.407373
1634.716412	57.281793	48.412378
1631.081111	56.015881	48.417383
1627.766421	49.555450	48.422388
1623.836179	54.397544	48.427393
1620.648752	49.552883	48.432397
1617.388897	54.793100	48.437402
1613.837303	51.843606	48.442407
1610.652743	48.918927	48.447412
1606.684006	50.998727	48.452417
1602.759232	52.185783	48.457421
1599.689796	52.327794	48.462426
1596.324876	56.132277	48.467431
1593.136182	43.859224	48.472436
1589.568850	51.172403	48.477441
1585.898236	50.367622	48.482445
1582.652413	54.564762	48.487450
1578.874071	52.498669	48.492455
1575.452202	41.220752	48.497460
1571.651629	49.737883	48.502465
1568.440645	52.553322	48.507469
1564.891676	47.325501	48.512474
1561.538377	46.733659	48.517479
1558.262813	47.217997	48.522484
1554.559912	52.891412	48.527489
1550.941021	51.429969	48.532493
1547.439812	48.510580	48.537498
1543.994086	66.539514	48.542503
1541.067337	53.981864	48.547508
1536.791163	56.552741	48.552513
1533.585990	55.741568	48.557517
1530.049169	59.819754	48.562522
1526.684419	59.925751	48.567527
1523.428828	66.070176	48.572532
1519.704109	60.021979	48.577537
1515.934270	53.183571	48.582541
1512.461854	52.623044	48.587546
1508.733275	56.851475	48.592551
1505.561161	56.892525	48.597556
1502.490625	51.744868	48.602561
1498.953218	67.130572	48.607565
1495.039250	59.855979	48.612570
1491.646914	60.111840	48.617575
1488.218436	57.595545	48.622580
1484.766164	62.173046	48.627585
1481.130322	65.520092	48.632589
1477.849435	57.595913	48.637594
1473.861805	60.216566	48.642599
1470.655917	57.602160	48.647604
1466.897220	53.596792	48.652609
1463.778701	63.927627	48.657613
1460.607892	65.332084	48.662618
1456.778885	62.796234	48.667623
1453.321136	50.872238	48.672628
1449.651750	55.898191	48.677633
1446.130543	66.605279	48.682637
1442.776392	55.588898	48.687642
1438.960288	60.735899	48.692647
1435.924422	55.174707	48.697652
1431.777585	62.986776	48.702657
1428.810469	51.859199	48.707661
1425.309163	57.592851	48.712666
1421.634112	58.968681	48.717671
1418.516361	56.606255	48.722676
1414.882327	59.535418	48.727681
1411.671144	68.915814	48.732685
1407.861997	64.753847	48.737690
1403.894584	50.805727	48.742695
1400.444077	46.470569	48.747700
1396.916616	57.115368	48.752705
1393.738935	48.842873	48.757709
1390.850377	57.441930	48.762714
1387.365041	52.387718	48.767719
1383.903617	52.306413	48.772724
1379.615470	54.679909	48.777729
1375.954664	53.807231	48.782733
1372.684415	49.981710	48.787738
1369.140763	53.374472	48.792743
1365.597736	52.619404	48.797748
1362.085188	53.628127	48.802753
1358.733699	54.279441	48.807757
1355.483147	47.008636	48.812762
1351.642956	52.191073	48.817767
1348.403273	55.355923	48.822772
1344.859680	52.560304	48.827777
1341.248748	58.513626	48.832781
1337.831103	47.108596	48.837786
1333.980960	55.589269	48.842791
1330.884168	51.524636	48.847796
1327.016313	49.931406	48.852801
1323.815900	52.599728	48.857805
1320.616624	54.388338	48.862810
1316.646088	60.420107	48.867815
1313.427683	50.189303	48.872820
1309.912576	59.398995	48.877825
1306.299888	42.468895	48.882829
1303.035080	46.814620	48.887834
1299.380707	56.527011	48.892839
1295.847140	48.322922	48.897844
1292.127932	48.557253	48.902849
1288.905931	51.469413	48.907853
1285.190570	42.964756	48.912858
1281.331740	55.689448	48.917863
1278.115501	54.753539	48.922868
1274.996627	54.251648	48.927873
1271.453144	57.229959	48.932877
1267.693624	63.886782	48.937882
1264.266719	50.157845	48.942887
1260.767012	47.083304	48.947892
1256.881393	52.598755	48.952897
1253.707341	50.906432	48.957901
1250.608504	49.911025	48.962906
1246.460244	54.240046	48.967911
1243.086837	53.319262	48.972916
1240.010528	52.462702	48.977921
1236.311897	43.344836	48.982925
1232.843343	42.347202	48.987930
1228.945569	49.073132	48.992935
1225.971553	46.406694	48.997940
1222.235703	54.423416	49.002945
1218.738488	56.432709	49.007949
1215.791946	50.025537	49.012954
1211.688823	53.936213	49.017959
1208.563062	37.743033	49.022964
1205.018745	56.771394	49.027969
1200.913181	48.742316	49.032973
1197.475795	45.281552	49.037978
1194.036979	50.834645	49.042983
1190.594285	47.868265	49.047988
1186.968108	58.693092	49.052993
1183.408735	54.232689	49.057997
1180.272642	60.004154	49.063002
1176.465208	61.457746	49.068007
1173.055209	51.064004	49.073012
1169.786046	53.281223	49.078017
1166.436938	61.509503	49.083021
1162.978227	53.553180	49.088026
1159.102371	56.637350	49.093031
1155.638133	56.104144	49.098036
1152.262960	57.407812	49.103041
1148.333666	58.659027	49.108045
1145.663967	56.957383	49.113050
1141.959596	60.160246	49.118055
1138.098863	51.909367	49.123060
1134.649121	57.169959	49.128065
1130.984455	61.144901	49.133069
1127.775238	45.300179	49.138074
1124.146585	60.725557	49.143079
1120.602843	53.937348	49.148084
1117.199174	62.946149	49.153089
1113.603319	56.273670	49.158093
1110.321027	50.437963	49.163098
1106.626092	55.891976	49.168103
1103.385882	57.528874	49.173108
1099.502703	55.539498	49.178113
1095.979210	61.719657	49.183117
1092.613350	51.983435	49.188122
1088.890895	60.089853	49.193127
1085.942171	47.583290	49.198132
1082.452662	54.817997	49.203137
1078.744705	67.927262	49.208141
1075.555053	57.723690	49.213146
1071.511992	64.861572	49.218151
1067.750024	62.663404	49.223156
1064.507358	52.347915	49.228161
1060.792194	59.836263	49.233165
1057.789745	51.273871	49.238170
1054.229104	64.224032	49.243175
1051.211216	56.989684	49.248180
1047.248478	54.895727	49.253185
1043.682763	46.465826	49.258189
1040.347354	48.263184	49.263194
1036.261095	50.526119	49.268199
1033.284008	49.296584	49.273204
1029.497566	51.778338	49.278209
1025.773383	59.192178	49.283213
1022.760879	47.211324	49.288218
1018.906748	60.903477	49.293223
1015.781832	56.726298	49.298228
1012.001015	49.905653	49.303233
1008.397793	55.240935	49.308237
1005.106412	49.014384	49.313242
1001.950449	49.606731	49.318247
998.375160	50.286881	49.323252
994.834002	47.044925	49.328257
990.903220	54.788518	49.333261
987.854428	52.646399	49.338266
983.858664	46.261225	49.343271
980.625071	49.368285	49.348276
977.120012	54.270588	49.353281
973.425338	54.150020	49.358285
969.976345	50.589920	49.363290
966.306538	45.378101	49.368295
963.221219	49.816049	49.373300
959.432343	49.881081	49.378305
955.580327	52.275053	49.383309
952.692313	47.197093	49.388314
948.869863	53.193150	49.393319
946.101734	46.368996	49.398324
942.322763	50.532744	49.403329
938.584789	53.411908	49.408333
934.981706	52.039975	49.413338
931.429473	54.649611	49.418343
927.596139	56.509153	49.423348
924.496636	58.187354	49.428353
921.055503	53.506062	49.433357
917.545393	49.041220	49.438362
913.767319	58.513664	49.443367
910.741304	60.537870	49.448372
907.356873	45.878632	49.453377
903.376499	53.690132	49.458381
900.383367	44.968157	49.463386
896.359904	57.392872	49.468391
893.275234	51.902795	49.473396
889.654442	50.530490	49.478401
886.001757	49.324533	49.483405
882.379683	45.177798	49.488410
878.475657	49.446573	49.493415
875.491981	45.813649	49.498420
871.931572	49.215529	49.503425
868.537700	46.994609	49.508429
865.192606	47.683056	49.513434
861.471305	55.827330	49.518439
857.871398	56.467094	49.523444
854.366067	53.697315	49.528449
850.589439	57.050803	49.533453
847.466190	48.304930	49.538458
844.160497	59.604858	49.543463
840.529731	54.111728	49.548468
836.862363	51.762802	49.553473
833.530742	50.243996	49.558477
830.079066	57.279867	49.563482
826.062047	52.309140	49.568487
822.939500	51.535889	49.573492
819.763373	55.542007	49.578497
816.020546	58.045487	49.583501
812.666024	54.366250	49.588506
808.972507	60.127031	49.593511
805.600553	48.923898	49.598516
801.786831	46.069554	49.603521
797.997523	48.349363	49.608525
795.029725	54.104072	49.613530
791.138997	57.994310	49.618535
788.006144	51.369695	49.623540
784.601402	59.954809	49.628545
780.699841	56.642825	49.633549
777.593795	55.278542	49.638554
773.923900	59.858711	49.643559
770.334105	58.918200	49.648564
766.936756	61.497313	49.653569
763.276535	54.009322	49.658573
760.232995	43.966511	49.663578
756.305281	58.616230	49.668583
752.962488	48.117241	49.673588
749.614060	49.432679	49.678593
745.825102	55.141987	49.683597
742.356316	48.630110	49.688602
738.571092	52.310856	49.693607
735.018673	45.030628	49.698612
731.962319	50.720126	49.703617
728.576498	48.333482	49.708621
725.177668	42.383303	49.713626
721.253006	52.736146	49.718631
718.045399	53.210123	49.723636
714.434159	61.447944	49.728641
710.782784	53.256234	49.733645
707.579241	51.533919	49.738650
703.836880	51.711994	49.743655
700.197051	47.068239	49.748660
697.227478	45.935715	49.753665
693.376547	47.193825	49.758669
689.785055	50.822102	49.763674
686.003905	45.767049	49.768679
682.446452	43.976782	49.773684
679.385233	41.213454	49.778689
675.750940	54.358743	49.783693
672.629440	43.284132	49.788698
669.234088	47.777047	49.793703
665.172231	41.288484	49.798708
661.685057	48.978537	49.803713
657.843992	46.508191	49.808717
654.661846	47.579320	49.813722
651.276499	52.035873	49.818727
647.982013	55.576523	49.823732
644.765026	44.475749	49.828737
640.960742	59.008096	49.833741
637.322962	50.845930	49.838746
633.420557	54.987996	49.843751
630.341415	45.703792	49.848756
626.625048	43.255061	49.853761
622.980545	50.786267	49.858765
620.064204	43.570990	49.863770
616.261006	48.488467	49.868775
612.860183	55.525931	49.873780
608.879744	43.136864	49.878785
605.604522	44.181457	49.883789
602.096731	40.782577	49.888794
598.740530	48.955177	49.893799
595.680992	43.043663	49.898804
592.374794	47.766250	49.903809
588.004320	46.419731	49.908813
584.823295	40.176072	49.913818
580.669717	42.535163	49.918823
577.809660	54.306366	49.923828
574.440726	41.672848	49.928833
570.343815	51.546515	49.933837
567.053485	42.795292	49.938842
563.103640	48.896860	49.943847
560.294483	40.218976	49.948852
557.181242	40.558007	49.953857
553.447703	44.882463	49.958861
549.660439	41.555850	49.963866
545.984748	47.424660	49.968871
542.533639	43.713204	49.973876
538.930061	41.708756	49.978881
535.799748	45.261693	49.983885
532.800846	35.471420	49.988890
528.606496	43.734183	49.993895
524.810560	40.431086	49.998900
521.499189	43.031617	50.003905
517.933882	42.425897	50.008909
515.145509	46.130929	50.013914
511.389513	51.597876	50.018919
507.822433	48.882203	50.023924
504.282068	47.465819	50.028929
500.595472	48.242687	50.033933
496.902804	39.162206	50.038938
493.338946	49.657929	50.043943
489.893734	45.875968	50.048948
486.355575	41.763717	50.053953
482.843721	52.871399	50.058957
479.552722	43.215481	50.063962
475.902073	48.030022	50.068967
472.832617	46.631643	50.073972
469.579519	43.819350	50.078977
465.388466	51.825361	50.083981
462.146370	36.710622	50.088986
458.429209	46.683035	50.093991
455.331903	43.504660	50.098996
451.813220	42.512011	50.104001
447.942224	42.074422	50.109005
444.671197	44.785720	50.114010
440.737184	49.040380	50.119015
437.501868	41.593561	50.124020
434.273490	24.243080	50.129025
430.727809	33.305946	50.134029
427.210543	33.151483	50.139034
423.291386	36.109841	50.144039
419.913896	30.184928	50.149044
416.561321	36.854221	50.154049
412.696273	32.783716	50.159053
409.837034	35.313465	50.164058
406.098200	37.534901	50.169063
402.496894	34.470294	50.174068
398.556426	30.977923	50.179073
395.490051	31.198937	50.184077
392.138376	39.693589	50.189082
388.186212	39.170664	50.194087
384.869760	45.350257	50.199092
381.756064	43.759522	50.204097
377.757073	49.878352	50.209101
374.864248	46.914749	50.214106
371.323366	39.927113	50.219111
367.211711	38.524344	50.224116
363.866265	30.155175	50.229121
360.205813	47.050541	50.234125
357.406003	39.215998	50.239130
353.699866	42.046104	50.244135
349.790473	40.219354	50.249140
346.428166	42.970294	50.254145
342.733678	44.397033	50.259149
339.639310	36.842758	50.264154
335.781288	43.869666	50.269159
332.597971	43.909702	50.274164
329.331762	47.695965	50.279169
325.948889	43.100713	50.284173
322.303109	37.863274	50.289178
318.337861	51.503433	50.294183
314.726551	41.603537	50.299188
311.431897	41.028269	50.304193
307.581890	46.449906	50.309197
304.401423	45.572015	50.314202
301.103802	47.199194	50.319207
297.631037	49.866216	50.324212
293.716496	38.026989	50.329217
290.539896	49.192940	50.334221
286.921971	38.303837	50.339226
283.848381	48.289388	50.344231
279.386414	44.584535	50.349236
276.453422	37.906677	50.354241
273.031659	43.789590	50.359245
270.053478	42.661723	50.364250
265.830839	49.353472	50.369255
262.217476	42.064027	50.374260
258.719116	44.491462	50.379265
255.162936	49.117280	50.384269
251.624436	44.059219	50.389274
248.515594	43.005612	50.394279
245.030498	43.222669	50.399284
241.283886	44.103957	50.404289
237.628063	54.813486	50.409293
234.318961	46.666465	50.414298
230.487136	44.302433	50.419303
227.333195	47.618725	50.424308
223.662655	42.992651	50.429313
220.397096	55.770259	50.434317
216.801947	45.719180	50.439322
213.489374	49.512746	50.444327
209.899568	42.551830	50.449332
206.460474	46.365219	50.454337
202.794679	51.065176	50.459341
199.666141	48.467593	50.464346
196.098177	50.700313	50.469351
192.392469	42.688211	50.474356
188.753915	45.798862	50.479361
185.054656	52.639606	50.484365
181.911279	46.383885	50.489370
178.579545	52.132505	50.494375
174.720044	54.739937	50.499380
171.453378	48.405458	50.504385
167.368159	46.742378	50.509389
164.225604	43.922379	50.514394
160.741874	46.565858	50.519399
157.085128	49.264919	50.524404
153.762599	46.251656	50.529409
150.466030	48.290014	50.534413
147.143242	36.579625	50.539418
143.432741	42.811538	50.544423
139.576452	53.476574	50.549428
136.231013	45.389075	50.554433
132.456801	54.380282	50.559437
129.173538	38.895671	50.564442
125.627660	43.735056	50.569447
122.178237	45.012760	50.574452
118.572181	39.386377	50.579457
115.380982	49.621353	50.584461
111.898310	39.245824	50.589466
108.807206	46.007133	50.594471
104.904818	46.849609	50.599476
101.131937	40.236968	50.604481
97.516128	45.890915	50.609485
94.323285	37.368242	50.614490
90.753990	44.198148	50.619495
87.003923	43.988546	50.624500
83.400854	34.555714	50.629505
80.230628	44.752610	50.634509
76.532458	38.745209	50.639514
73.404850	47.793316	50.644519
69.742048	44.232287	50.649524
66.154631	51.106172	50.654529
62.719069	43.289091	50.659533
59.181901	41.287097	50.664538
55.980189	39.330624	50.669543
52.252609	44.818601	50.674548
48.674487	36.751783	50.679553
44.869996	44.086790	50.684557
41.605426	37.078163	50.689562
38.752639	43.789498	50.694567
34.816082	48.459175	50.699572
31.114407	42.620023	50.704577
27.340919	40.958790	50.709581
23.891992	43.454499	50.714586
20.398269	47.969378	50.719591
16.876455	45.753024	50.724596
13.888692	42.478560	50.729601
10.065325	44.764024	50.734605
6.571582	39.313085	50.739610
3.505915	36.724711	50.744615