Thu Aug 25 09:55:51 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.892884	100.900686	0.000000
0.748675	109.592135	0.005005
0.976147	96.525084	0.010010
0.990356	100.088557	0.015014
0.570494	104.840015	0.020019
1.000925	95.322547	0.025024
0.623518	86.336620	0.030029
0.506862	72.722390	0.035034
0.293065	67.520004	0.040038
-0.254332	54.438350	0.045043
-0.096367	45.539403	0.050048
-0.752565	35.897993	0.055053
-1.353261	21.372552	0.060058
-1.623579	15.812042	0.065062
-1.509716	19.654114	0.070067
-1.737530	5.617590	0.075072
-2.011382	4.768459	0.080077
-2.043799	3.185474	0.085082
-2.634501	-2.163480	0.090086
-2.941617	-0.795941	0.095091
-4.072569	-8.021769	0.100096
-4.549742	-1.603557	0.105101
-4.797879	-3.282455	0.110106
-4.217521	-8.049265	0.115110
-4.805366	-0.876560	0.120115
-4.587478	-9.579225	0.125120
-4.914191	5.692886	0.130125
-5.028475	-3.441790	0.135130
-5.787905	-1.879995	0.140134
-6.091166	-2.639097	0.145139
-6.114152	-4.432366	0.150144
-6.441815	-2.261179	0.155149
-6.464488	-1.251418	0.160154
-7.134102	7.193273	0.165158
-7.728453	5.742626	0.170163
-7.775809	8.743089	0.175168
-8.013789	-7.452670	0.180173
-7.914506	-1.684761	0.185178
-7.824159	-1.195744	0.190182
-8.139831	-0.706386	0.195187
-8.025096	0.740589	0.200192
-8.849355	4.647388	0.205197
-9.115716	-3.875002	0.210202
-9.602877	-1.678825	0.215206
-9.960661	1.151976	0.220211
-9.841813	-8.202722	0.225216
-10.142126	-6.697044	0.230221
-10.837944	-6.913749	0.235226
-11.217503	-4.902110	0.240230
-11.422815	-7.540005	0.245235
-11.469288	-12.091542	0.250240
-11.703918	0.606667	0.255245
-11.544261	-10.193928	0.260250
-11.133689	-8.344055	0.265254
-11.538614	-3.832247	0.270259
-11.979453	-0.589800	0.275264
-12.529129	-2.825727	0.280269
-12.838180	-4.631122	0.285274
-13.361154	-1.530830	0.290278
-13.985392	1.098112	0.295283
-13.973441	-5.829062	0.300288
-14.473966	-4.105353	0.305293
-14.110309	-7.259502	0.310298
-14.061748	0.053935	0.315302
-14.284952	-0.018523	0.320307
-14.320238	1.996122	0.325312
-15.162630	-2.149136	0.330317
-15.499878	0.358909	0.335322
-15.425215	-1.661631	0.340326
-16.037490	15.638899	0.345331
-16.211870	-5.549729	0.350336
-17.230331	-6.734607	0.355341
-17.106918	-2.720031	0.360346
-16.694626	-5.404075	0.365350
-17.184923	-0.970638	0.370355
-16.975266	-6.315279	0.375360
-17.479163	1.954749	0.380365
-17.792656	2.405801	0.385370
-17.901204	0.464587	0.390374
-18.273722	-1.931975	0.395379
-18.384243	-7.428928	0.400384
-18.823342	7.585546	0.405389
-19.653306	-2.727802	0.410394
-19.551526	-2.180465	0.415398
-19.868421	1.865136	0.420403
-19.937815	-6.571055	0.425408
-20.029012	2.232257	0.430413
-20.050303	-2.304245	0.435418
-20.751229	-6.595053	0.440422
-21.196918	-6.901569	0.445427
-20.957319	-2.471765	0.450432
-21.268612	2.164579	0.455437
-21.559511	-1.832972	0.460442
-22.098478	-9.142059	0.465446
-22.579491	-5.671856	0.470451
-22.604139	-6.923863	0.475456
-22.981900	3.113917	0.480461
-22.888726	0.078078	0.485466
-23.140130	-6.380727	0.490470
-23.189568	6.364399	0.495475
-23.388596	-16.101671	0.500480
-23.703421	-0.106933	0.505485
-24.091592	-0.969789	0.510490
-24.168386	-3.178569	0.515494
-24.987412	-0.810170	0.520499
-25.296620	0.741195	0.525504
-25.273534	-1.021328	0.530509
-25.211073	-6.295450	0.535514
-24.887833	0.607954	0.540518
-25.926831	0.935401	0.545523
-26.374208	9.174430	0.550528
-26.834355	-0.342651	0.555533
-26.855200	-2.984139	0.560538
-26.943645	5.679539	0.565542
-27.257879	-2.645524	0.570547
-27.092336	-1.234984	0.575552
-27.796422	-4.512898	0.580557
-28.190225	-5.241994	0.585562
-28.113300	-10.081784	0.590566
-28.789684	-4.451769	0.595571
-28.235295	-15.728659	0.600576
-28.461164	-5.293905	0.605581
-29.366149	-2.877237	0.610586
-29.546256	-3.798003	0.615590
-29.734972	-3.363337	0.620595
-29.808003	-8.375784	0.625600
-30.113646	1.922778	0.630605
-30.910448	-10.528124	0.635610
-31.161999	4.763844	0.640614
-31.384883	6.235245	0.645619
-31.162027	-0.889491	0.650624
-31.377402	9.356967	0.655629
-31.376757	-1.111835	0.660634
-31.201569	-4.423114	0.665638
-32.357884	-2.814950	0.670643
-32.538265	-2.324642	0.675648
-32.758868	4.445675	0.680653
-32.938903	-8.829528	0.685658
-33.149056	-10.096761	0.690662
-33.914839	-6.967916	0.695667
-34.050589	-1.640908	0.700672
-34.519830	3.637115	0.705677
-34.708024	-8.535826	0.710682
-34.174517	-8.948311	0.715686
-34.569811	1.047923	0.720691
-34.220327	-10.487929	0.725696
-35.070839	-4.220028	0.730701
-35.468669	-4.581498	0.735706
-35.571017	-9.684263	0.740710
-36.030888	-3.847727	0.745715
-35.785417	-2.842016	0.750720
-36.781631	2.271804	0.755725
-37.082795	-7.940896	0.760730
-36.736949	-3.850443	0.765734
-37.471157	-2.327398	0.770739
-37.167213	-12.600106	0.775744
-37.491349	-5.588944	0.780749
-38.205198	-5.125781	0.785754
-38.508124	-2.164370	0.790758
-39.134240	7.599115	0.795763
-39.133115	-6.185364	0.800768
-39.102357	1.140352	0.805773
-39.207972	-7.071863	0.810778
-39.015032	-3.890756	0.815782
-39.397081	4.926491	0.820787
-39.917248	-7.517136	0.825792
-40.727492	-4.574312	0.830797
-40.822895	2.157405	0.835802
-40.580385	-3.356899	0.840806
-40.506080	4.964902	0.845811
-41.079526	-13.010092	0.850816
-41.964731	-6.739919	0.855821
-41.953339	-6.763713	0.860826
-41.914793	-11.157728	0.865830
-42.337337	-1.929180	0.870835
-42.090915	-8.197067	0.875840
-42.086901	0.746349	0.880845
-43.096768	1.293859	0.885850
-42.975500	-10.152450	0.890854
-43.438234	8.304716	0.895859
-43.864922	-9.750224	0.900864
-44.150623	1.215926	0.905869
-44.609932	-3.891020	0.910874
-44.306557	-7.260349	0.915878
-44.860163	-2.095659	0.920883
-44.764269	-0.088913	0.925888
-45.217595	-0.011418	0.930893
-45.764058	5.876653	0.935898
-46.077114	-1.527943	0.940902
-46.139349	-3.900354	0.945907
-46.350382	-3.164799	0.950912
-46.272029	-2.085446	0.955917
-46.509922	-3.139526	0.960922
-46.752759	3.336883	0.965926
-47.563047	8.355134	0.970931
-47.596485	-3.816747	0.975936
-47.712273	-4.102186	0.980941
-47.990957	-4.801863	0.985946
-48.099772	-1.029310	0.990950
-48.849720	8.914930	0.995955
-49.189032	-8.549425	1.000960
-49.622851	1.829331	1.005965
-49.429794	6.038638	1.010970
-49.058630	-12.473504	1.015974
-49.368849	9.607561	1.020979
-49.513972	0.911153	1.025984
-50.276985	-0.940168	1.030989
-50.568189	5.404615	1.035994
-51.025352	-3.961068	1.040998
-51.327145	9.633516	1.046003
-50.758901	-6.334223	1.051008
-51.312511	-0.910104	1.056013
-52.161878	-0.852811	1.061018
-52.480028	-0.404192	1.066022
-52.227411	-0.443636	1.071027
-52.364682	-1.693816	1.076032
-52.522786	4.215661	1.081037
-52.518160	5.290747	1.086042
-53.141631	-0.432717	1.091046
-53.740624	3.615958	1.096051
-53.712584	0.084125	1.101056
-54.067742	3.613704	1.106061
-53.961465	-1.654628	1.111066
-54.454479	-7.670613	1.116070
-54.875750	-6.933753	1.121075
-55.696793	-5.412921	1.126080
-55.298446	-6.949504	1.131085
-55.260894	-1.001084	1.136090
-55.275288	-0.464018	1.141094
-56.075273	3.094131	1.146099
-56.204447	-5.557316	1.151104
-56.522647	-6.067303	1.156109
-56.765883	4.019001	1.161114
-56.798024	-2.812679	1.166118
-57.691695	-5.184527	1.171123
-57.904167	0.812561	1.176128
-58.461529	-2.289024	1.181133
-58.288343	3.710911	1.186138
-58.392556	-1.065696	1.191142
-58.532562	-0.480475	1.196147
-58.402663	-5.205179	1.201152
-58.778155	0.004370	1.206157
-59.162072	4.490742	1.211162
-59.238629	1.196761	1.216166
-59.591635	1.941907	1.221171
-59.654482	-3.698556	1.226176
-60.735114	-6.310027	1.231181
-61.095444	-5.054371	1.236186
-61.235789	-5.500477	1.241190
-61.421902	0.505136	1.246195
-61.159396	-7.546459	1.251200
-61.631995	0.721827	1.256205
-61.492808	6.135470	1.261210
-61.202656	-4.704554	1.266214
-62.254854	-3.944765	1.271219
-62.406120	-3.977873	1.276224
-62.850772	-2.307209	1.281229
-63.035289	-6.131600	1.286234
-62.927494	-5.873107	1.291238
-63.426475	10.163146	1.296243
-63.652311	-8.103596	1.301248
-63.898550	3.720073	1.306253
-64.044228	0.655221	1.311258
-64.831201	-9.522482	1.316262
-65.281964	-4.190409	1.321267
-65.257767	-2.181922	1.326272
-65.662335	-5.228353	1.331277
-65.922176	-0.055908	1.336282
-65.295917	-4.627433	1.341286
-65.682461	4.497400	1.346291
-65.881362	-6.772192	1.351296
-66.496146	-15.853743	1.356301
-67.066130	-3.090340	1.361306
-67.031621	-15.279185	1.366310
-67.143509	-8.554381	1.371315
-67.645417	-13.214886	1.376320
-68.008872	-3.755154	1.381325
-68.663415	-10.024236	1.386330
-68.241321	2.181927	1.391334
-68.731999	2.711364	1.396339
-68.556963	-2.077361	1.401344
-68.670602	-0.420598	1.406349
-69.336562	0.718433	1.411354
-69.656717	-5.267688	1.416358
-70.050133	-7.240194	1.421363
-70.135219	-7.827836	1.426368
-70.447071	2.585592	1.431373
-70.649420	0.579984	1.436378
-70.332452	-1.127347	1.441382
-70.965388	-7.735172	1.446387
-71.217725	-11.985531	1.451392
-71.791357	-5.185212	1.456397
-71.670357	-4.773765	1.461402
-71.340120	-11.377484	1.466406
-72.372346	-3.948489	1.471411
-72.422487	-2.203599	1.476416
-72.584809	-3.468835	1.481421
-73.074114	2.264747	1.486426
-73.318586	0.506183	1.491430
-74.203390	7.342610	1.496435
-73.764987	11.766574	1.501440
-74.106700	-1.875600	1.506445
-74.130405	5.072672	1.511450
-74.052116	1.542458	1.516454
-75.000795	-6.158006	1.521459
-75.285625	-6.056291	1.526464
-75.512482	-8.966052	1.531469
-75.851321	4.650150	1.536474
-75.850071	-4.024896	1.541478
-75.785010	-1.029396	1.546483
-76.095917	-2.559251	1.551488
-76.795506	8.886204	1.556493
-77.172850	-5.699507	1.561498
-76.909538	-7.692658	1.566502
-77.395060	-4.788057	1.571507
-76.931052	-3.800771	1.576512
-77.958472	0.719993	1.581517
-78.668121	-5.844174	1.586522
-78.774895	-13.834739	1.591526
-78.847797	2.577668	1.596531
-78.841289	0.529843	1.601536
-79.136377	-6.485258	1.606541
-79.018670	-2.067996	1.611546
-79.275375	2.869841	1.616550
-79.939202	-4.897401	1.621555
-80.110484	-2.374232	1.626560
-80.320779	2.534188	1.631565
-80.374932	3.305273	1.636570
-80.694658	-1.143336	1.641574
-81.233024	0.323714	1.646579
-81.357901	-4.671115	1.651584
-81.713773	-8.183918	1.656589
-82.020203	-4.076683	1.661594
-81.878933	-2.646523	1.666598
-82.388935	-0.899180	1.671603
-82.722426	0.545260	1.676608
-83.229894	5.800801	1.681613
-83.456941	5.646690	1.686618
-83.655130	9.490195	1.691622
-83.681414	4.884874	1.696627
-83.364349	6.796852	1.701632
-83.358592	2.822423	1.706637
-84.018091	-3.072561	1.711642
-84.155407	-9.115803	1.716646
-84.934767	2.503498	1.721651
-84.913831	-14.469963	1.726656
-85.656016	-4.552257	1.731661
-85.804631	0.004812	1.736666
-85.990351	-5.869496	1.741670
-86.204244	3.889507	1.746675
-86.062930	-1.631087	1.751680
-86.463626	10.381302	1.756685
-87.408445	6.657060	1.761690
-87.195550	-0.598991	1.766694
-87.548999	6.919803	1.771699
-87.733536	-4.529209	1.776704
-87.694027	-0.795717	1.781709
-88.071744	-3.450887	1.786714
-87.798264	-2.452730	1.791718
-88.900409	-5.646118	1.796723
-89.066686	-0.472515	1.801728
-88.863193	-2.215849	1.806733
-89.371929	-2.319494	1.811738
-89.393969	-13.056810	1.816742
-90.123978	-2.600011	1.821747
-90.304280	-5.159564	1.826752
-90.593159	-5.484319	1.831757
-90.811622	-8.218225	1.836762
-90.458550	-10.845534	1.841766
-90.899707	-4.676574	1.846771
-90.841467	-11.835621	1.851776
-91.725063	-10.681470	1.856781
-92.321743	-1.805287	1.861786
-92.223452	-9.141452	1.866790
-92.398269	0.475384	1.871795
-92.639412	-3.605888	1.876800
-93.035644	-2.423699	1.881805
-94.029673	-5.371436	1.886810
-93.350206	-7.046983	1.891814
-93.929886	5.765400	1.896819
-93.787068	1.513233	1.901824
-94.279916	-0.772721	1.906829
-94.546789	-6.529908	1.911834
-93.972460	-5.778208	1.916838
-94.674371	0.371500	1.921843
-94.844687	1.847320	1.926848
-95.369272	-8.953622	1.931853
-95.205266	-2.446053	1.936858
-95.625812	0.663502	1.941862
-96.335830	7.611747	1.946867
-96.576648	0.104088	1.951872
-96.628209	-7.512317	1.956877
-96.838494	10.481347	1.961882
-96.674032	-1.924019	1.966886
-97.573325	8.179663	1.971891
-98.191083	-0.319295	1.976896
-97.882779	-6.859468	1.981901
-98.443459	4.406030	1.986906
-98.384983	-2.585378	1.991910
-98.601011	4.614490	1.996915
-98.458975	1.248673	2.006912
-98.531081	-2.503094	2.016909
-98.543631	4.218040	2.026906
-97.666003	0.574047	2.036902
-97.078763	-4.133171	2.046899
-97.058992	0.593522	2.056896
-96.132493	-0.371838	2.066893
-96.014689	1.165365	2.076890
-95.229377	-0.617338	2.086886
-94.808747	-3.781076	2.096883
-94.073225	-3.807354	2.106880
-93.340866	-6.300849	2.116877
-92.961211	0.618588	2.126874
-93.048889	-6.751528	2.136870
-92.148722	-6.075012	2.146867
-91.681918	-11.248030	2.156864
-90.907589	3.177425	2.166861
-90.585547	2.607719	2.176858
-90.393363	-3.431427	2.186854
-89.673270	-3.033971	2.196851
-88.721623	-3.372879	2.206848
-88.758625	1.185314	2.216845
-88.529171	-1.077325	2.226842
-87.566503	1.011738	2.236838
-87.111286	5.302739	2.246835
-86.282598	3.091923	2.256832
-86.140660	5.936812	2.266829
-86.235181	-0.412204	2.276826
-84.990927	-0.185577	2.286822
-84.782359	0.067118	2.296819
-83.487352	1.581421	2.306816
-83.859428	4.066528	2.316813
-83.273476	4.380467	2.326810
-82.940478	7.885998	2.336806
-82.136476	-0.488648	2.346803
-81.779504	0.561253	2.356800
-80.900252	-3.817921	2.366797
-80.777859	1.218976	2.376794
-79.872444	-5.483123	2.386790
-79.043581	-0.471393	2.396787
-79.022768	-5.121535	2.406784
-79.005560	-2.776621	2.416781
-78.247807	-1.871882	2.426778
-77.805631	-1.494233	2.436774
-77.170419	-2.464634	2.446771
-76.314634	1.294767	2.456768
-76.189215	-1.002255	2.466765
-75.657533	-5.181249	2.476762
-74.973014	-2.402371	2.486758
-74.574652	-2.356811	2.496755
-74.316218	-0.106715	2.506752
-73.571892	-3.853362	2.516749
-73.451395	0.908235	2.526746
-72.421390	-1.064862	2.536742
-72.050860	-0.704497	2.546739
-71.745674	1.173978	2.556736
-71.056574	0.182462	2.566733
-70.666772	4.490049	2.576730
-69.862847	1.735086	2.586726
-69.297981	-0.542095	2.596723
-69.180573	2.465028	2.606720
-68.937751	-1.383604	2.616717
-68.270169	6.561437	2.626714
-67.677685	4.203901	2.636710
-66.798193	0.546947	2.646707
-66.547564	3.406484	2.656704
-66.241361	2.839261	2.666701
-65.395607	0.793666	2.676698
-64.844157	1.768746	2.686694
-64.944090	6.650414	2.696691
-63.998341	-0.745418	2.706688
-63.627581	-4.889694	2.716685
-63.623246	-3.832055	2.726682
-62.299026	-5.955787	2.736678
-61.983372	-3.312346	2.746675
-61.254236	-6.841202	2.756672
-60.645410	-5.358762	2.766669
-60.587395	0.565703	2.776666
-60.490329	-4.229435	2.786662
-59.917449	-10.679856	2.796659
-59.068276	-8.348094	2.806656
-57.995930	0.426842	2.816653
-57.851578	-4.090604	2.826650
-57.907655	-2.165026	2.836646
-57.283251	-2.205568	2.846643
-56.515781	-0.608602	2.856640
-56.260550	-0.917582	2.866637
-55.189533	1.962296	2.876634
-54.652304	-1.393940	2.886630
-54.769683	-1.115514	2.896627
-54.512973	-1.158631	2.906624
-53.431347	3.056396	2.916621
-53.117100	-4.116942	2.926618
-51.997770	4.105775	2.936614
-51.913475	0.823675	2.946611
-51.829932	-1.596666	2.956608
-51.263583	-2.442234	2.966605
-50.637029	-0.946732	2.976602
-50.114961	-1.424233	2.986598
-49.168597	-4.112815	2.996595
-48.960891	-0.771382	3.006592
-48.846047	-2.914694	3.016589
-48.100713	-5.907562	3.026586
-47.501742	-7.809950	3.036582
-47.171283	-1.893327	3.046579
-46.293975	-5.717830	3.056576
-45.946429	-11.651438	3.066573
-45.656606	-6.434869	3.076570
-44.524426	-9.447168	3.086566
-44.483155	-3.073421	3.096563
-44.398339	-7.819122	3.106560
-43.058622	-8.054106	3.116557
-42.808044	-7.177601	3.126554
-42.977497	-4.274418	3.136550
-42.370387	-6.326967	3.146547
-41.543049	-4.596829	3.156544
-41.002633	-2.663345	3.166541
-40.065480	-8.087457	3.176538
-39.896693	-1.572131	3.186534
-39.693665	-7.955099	3.196531
-39.061705	-6.466778	3.206528
-38.376801	-9.564217	3.216525
-38.124617	-12.315089	3.226522
-37.074137	1.579267	3.236518
-36.944038	0.273031	3.246515
-37.043432	3.405991	3.256512
-36.348486	4.488469	3.266509
-35.472058	2.951253	3.276506
-34.429508	-0.959329	3.286502
-34.209791	5.003159	3.296499
-34.032596	4.798273	3.306496
-33.469114	1.634327	3.316493
-32.925847	1.774392	3.326490
-32.317331	3.196696	3.336486
-32.227297	3.262058	3.346483
-31.922745	3.312816	3.356480
-30.898080	2.588672	3.366477
-30.423606	2.973934	3.376474
-29.394889	4.891099	3.386470
-29.487816	-2.988216	3.396467
-29.429195	0.243529	3.406464
-28.681001	-2.524873	3.416461
-28.013177	3.928103	3.426458
-27.857754	2.209253	3.436454
-27.073582	-1.249030	3.446451
-26.443648	-0.561844	3.456448
-25.496473	3.943517	3.466445
-25.556694	-1.957882	3.476442
-25.579449	1.125056	3.486438
-24.473718	-1.122827	3.496435
-23.973414	-3.434239	3.506432
-22.856541	-11.420745	3.516429
-22.547804	-5.545068	3.526426
-22.460642	2.848882	3.536422
-22.111121	-5.232805	3.546419
-21.985788	-7.289061	3.556416
-21.129011	-4.594188	3.566413
-19.896366	3.376363	3.576410
-20.072320	3.572100	3.586406
-19.434722	-6.084770	3.596403
-19.210020	0.028990	3.606400
-18.245520	6.014167	3.616397
-18.265254	-5.959907	3.626394
-17.198197	-7.831098	3.636390
-16.628566	-3.234905	3.646387
-16.641007	-7.689770	3.656384
-16.246466	-9.848394	3.666381
-15.293760	-5.144330	3.676378
-15.068060	-3.161533	3.686374
-14.600080	-5.810002	3.696371
-13.626779	-8.366584	3.706368
-13.786018	-3.621344	3.716365
-12.755465	-10.349381	3.726362
-12.268798	-16.662747	3.736358
-11.943060	-8.480411	3.746355
-11.714404	-10.255083	3.756352
-10.914944	-12.391620	3.766349
-10.447254	-5.853435	3.776346
-9.725929	-7.325165	3.786342
-9.228094	-10.846286	3.796339
-9.186420	-2.258311	3.806336
-8.132670	-4.244624	3.816333
-7.841187	-6.957304	3.826330
-7.657639	-7.156850	3.836326
-7.004459	-8.617902	3.846323
-6.087655	-6.071816	3.856320
-5.850432	-4.790906	3.866317
-5.872141	-5.949812	3.876314
-4.946745	-7.269783	3.886310
-4.780814	3.516184	3.896307
-4.099336	13.736708	3.906304
-3.785301	17.235715	3.916301
-3.350306	29.094606	3.926298
-2.786500	40.055841	3.936294
-2.246935	52.924733	3.946291
-1.918333	70.439020	3.956288
-1.284406	80.476964	3.966285
-1.175088	95.665613	3.976282
-0.916441	116.146477	3.986278
0.000000	132.480964	3.991283
-0.057578	138.343099	3.996288
0.713863	149.966288	4.001293
0.639956	154.397797	4.006298
0.455788	156.612958	4.011302
0.668745	163.141398	4.016307
0.655743	162.387431	4.021312
1.179920	151.029747	4.026317
0.523130	173.222271	4.031322
0.682778	163.959167	4.036326
0.830730	155.792567	4.041331
0.640759	169.398229	4.046336
0.651552	177.650971	4.051341
0.884212	185.505119	4.056346
0.777293	183.288381	4.061350
0.752222	185.019870	4.066355
0.907902	192.696256	4.071360
0.676379	186.288048	4.076365
0.504842	198.612678	4.081370
0.917265	197.668665	4.086374
1.345271	196.000868	4.091379
0.728024	196.132519	4.096384
1.129675	194.652351	4.101389
0.900286	201.768973	4.106394
0.817199	197.121878	4.111398
1.264775	192.116390	4.116403
0.771669	191.788824	4.121408
0.889443	192.956926	4.126413
1.142838	206.290667	4.131418
1.217367	207.981243	4.136422
1.460872	200.365968	4.141427
1.286510	200.975561	4.146432
1.411424	200.940307	4.151437
1.027363	194.973616	4.156442
0.663667	195.442029	4.161446
1.255120	205.815288	4.166451
1.468974	211.837401	4.171456
1.190600	202.016478	4.176461
1.230452	201.244736	4.181466
1.691870	210.360204	4.186470
1.767773	195.367938	4.191475
1.268135	202.099793	4.196480
1.477921	195.679385	4.201485
1.137587	199.801470	4.206490
1.209491	194.949755	4.211494
1.122512	196.371403	4.216499
1.046778	199.955316	4.221504
1.335173	197.531104	4.226509
1.198400	194.778035	4.231514
1.367842	217.594138	4.236518
1.334974	212.837929	4.241523
1.114685	220.835829	4.246528
1.534291	218.175918	4.251533
1.654286	219.830897	4.256538
1.535391	223.984731	4.261542
1.762960	218.871336	4.266547
1.125253	222.404098	4.271552
1.373669	228.547352	4.276557
1.928587	231.602185	4.281562
1.747440	223.056842	4.286566
1.827819	208.544760	4.291571
1.317744	202.493405	4.296576
1.301358	204.647482	4.301581
1.762465	218.888332	4.306586
1.606800	223.693340	4.311590
1.586318	212.816429	4.316595
1.425607	220.637313	4.321600
1.853682	220.336259	4.326605
1.664807	233.891178	4.331610
1.658612	233.243710	4.336614
1.995058	232.045841	4.341619
1.442387	223.932036	4.346624
1.409023	204.733228	4.351629
1.478749	219.674485	4.356634
1.886185	221.632444	4.361638
2.207358	225.043442	4.366643
1.823723	216.934793	4.371648
1.691426	202.658519	4.376653
1.469323	208.707808	4.381658
1.686107	219.377062	4.386662
1.846744	231.504135	4.391667
1.710089	228.944033	4.396672
1.807863	227.451363	4.401677
1.683017	225.711996	4.406682
1.302807	233.051580	4.411686
1.400794	221.485379	4.416691
1.123435	232.358615	4.421696
1.571820	233.883048	4.426701
1.698811	231.193052	4.431706
1.951489	244.036547	4.436710
2.152291	239.506314	4.441715
1.978453	244.640045	4.446720
2.178773	229.925652	4.451725
1.925060	231.449358	4.456730
1.809973	231.632044	4.461734
1.990925	233.786844	4.466739
2.103703	235.085447	4.471744
1.737694	235.459310	4.476749
2.231564	236.698203	4.481754
1.815831	229.758852	4.486758
2.015838	228.962015	4.491763
1.907434	243.861599	4.496768
1.758590	246.814727	4.501773
2.106493	251.430109	4.506778
2.062160	257.169984	4.511782
2.286647	245.359317	4.516787
2.429559	265.927021	4.521792
2.320305	254.655864	4.526797
2.428212	227.322937	4.531802
2.374780	231.966395	4.536806
2.109574	233.751332	4.541811
2.167062	232.866093	4.546816
2.283673	229.070397	4.551821
1.949017	232.767652	4.556826
1.723857	238.285913	4.561830
1.897720	240.897410	4.566835
2.008350	261.713779	4.571840
2.218849	247.864656	4.576845
2.221143	256.821127	4.581850
2.108455	253.706767	4.586854
2.393911	254.804307	4.591859
2.275313	256.648535	4.596864
2.347172	251.673424	4.601869
1.937846	251.642782	4.606874
2.308452	267.236134	4.611878
2.457112	258.727686	4.616883
2.251609	271.665136	4.621888
2.624884	262.627941	4.626893
2.423813	263.700470	4.631898
2.482791	253.187576	4.636902
2.518953	251.220497	4.641907
2.240291	261.910456	4.646912
2.346304	256.588303	4.651917
2.235404	263.401643	4.656922
2.119821	267.361977	4.661926
2.487535	265.801698	4.666931
2.221115	265.084268	4.671936
2.411956	256.679945	4.676941
2.397141	260.409351	4.681946
2.405015	255.849230	4.686950
2.539740	259.988645	4.691955
2.481094	262.196808	4.696960
2.392517	259.951875	4.701965
2.547768	262.272058	4.706970
2.602147	265.031995	4.711974
2.942614	271.445582	4.716979
2.656856	265.669111	4.721984
2.785915	257.132097	4.726989
2.972131	257.549153	4.731994
2.737774	258.092216	4.736998
2.892326	251.091977	4.742003
2.627732	258.941810	4.747008
2.508544	257.891260	4.752013
2.452910	273.155928	4.757018
2.341748	262.701324	4.762022
2.486647	259.999025	4.767027
2.562840	271.225020	4.772032
2.999144	278.480983	4.777037
2.828102	279.735472	4.782042
2.583377	278.074995	4.787046
2.976215	275.147183	4.792051
2.539580	268.204764	4.797056
2.571149	279.709842	4.802061
2.895165	288.369145	4.807066
2.813371	290.995395	4.812070
3.014626	288.132401	4.817075
2.875971	297.076175	4.822080
2.655268	293.463032	4.827085
2.907340	299.159642	4.832090
3.107045	292.750271	4.837094
2.811452	293.138412	4.842099
2.604893	291.465626	4.847104
2.734839	290.157738	4.852109
2.726505	289.928224	4.857114
2.209971	299.149507	4.862118
2.917840	292.796559	4.867123
2.630909	299.871615	4.872128
2.732980	285.925555	4.877133
3.033064	295.284646	4.882138
3.012173	311.809423	4.887142
3.188082	313.974514	4.892147
2.865652	310.152676	4.897152
3.353256	307.637124	4.902157
3.187331	293.299608	4.907162
2.743576	290.518691	4.912166
3.140680	297.280923	4.917171
3.233947	323.668372	4.922176
3.011922	307.264179	4.927181
3.225859	306.908089	4.932186
3.243621	307.224987	4.937190
3.249785	296.435600	4.942195
2.935404	303.742752	4.947200
2.910569	307.144703	4.952205
3.386673	306.620984	4.957210
3.256835	314.221933	4.962214
2.973564	315.905304	4.967219
3.295520	317.107862	4.972224
3.480077	297.906448	4.977229
3.407816	321.554669	4.982234
3.389972	315.907050	4.987238
3.467372	308.213349	4.992243
3.055828	302.965946	4.997248
3.308360	299.379896	5.002253
3.177830	308.151558	5.007258
3.406952	306.581352	5.012262
3.351384	321.498033	5.017267
3.565674	319.578968	5.022272
3.214475	308.551332	5.027277
3.182558	315.184636	5.032282
3.277931	315.062260	5.037286
3.256106	315.233499	5.042291
3.273310	316.879282	5.047296
3.325254	313.362624	5.052301
3.357782	316.518303	5.057306
3.182997	318.399815	5.062310
3.481757	310.041833	5.067315
3.415170	319.771605	5.072320
3.073302	314.519609	5.077325
3.542570	313.519227	5.082330
3.236133	317.370268	5.087334
3.436708	305.363989	5.092339
3.369728	320.595673	5.097344
3.621155	323.938523	5.102349
3.782534	325.365561	5.107354
3.424210	322.368771	5.112358
3.474067	326.027945	5.117363
3.462223	315.238205	5.122368
4.188694	327.216575	5.127373
3.845537	326.685175	5.132378
3.566650	325.172417	5.137382
3.603285	315.827267	5.142387
3.308295	315.221880	5.147392
3.444912	315.365130	5.152397
3.770411	327.064634	5.157402
3.728663	335.993244	5.162406
3.795484	343.025546	5.167411
3.656725	347.888050	5.172416
3.873943	343.329908	5.177421
4.210425	340.781081	5.182426
3.405424	335.231479	5.187430
4.031345	322.133471	5.192435
3.860720	323.625184	5.197440
3.628586	312.215053	5.202445
3.454834	321.892013	5.207450
3.486279	342.221001	5.212454
4.095983	341.834539	5.217459
3.680674	333.610575	5.222464
4.054778	334.710050	5.227469
4.053062	337.323760	5.232474
3.861197	337.989884	5.237478
3.845509	334.888786	5.242483
3.326147	342.256545	5.247488
3.680606	337.411141	5.252493
3.745062	338.024449	5.257498
3.777793	339.275490	5.262502
3.780429	337.686983	5.267507
3.940369	334.276788	5.272512
3.780358	333.833753	5.277517
3.865809	335.763079	5.282522
3.415593	342.686562	5.287526
4.015171	355.906063	5.292531
4.026936	371.432342	5.297536
4.214490	367.033869	5.302541
4.247887	365.022917	5.307546
4.246727	367.810554	5.312550
4.074712	360.719068	5.317555
3.990614	367.952199	5.322560
4.102814	358.617334	5.327565
4.023894	363.426173	5.332570
3.746373	366.041972	5.337574
4.242826	359.981558	5.342579
3.839194	371.064492	5.347584
4.318997	367.006214	5.352589
4.561382	369.353888	5.357594
4.271174	370.329656	5.362598
4.407741	358.140378	5.367603
4.197050	369.446186	5.372608
4.372176	367.821160	5.377613
4.299955	355.800640	5.382618
4.356891	357.307322	5.387622
4.596579	359.905359	5.392627
4.521424	370.905189	5.397632
4.464840	353.766337	5.402637
4.084103	345.426217	5.407642
3.936477	359.446176	5.412646
4.004759	351.124287	5.417651
4.145363	363.017302	5.422656
4.313326	363.497333	5.427661
4.417551	366.040664	5.432666
4.033902	368.885066	5.437670
4.416148	357.777284	5.442675
4.540725	363.993774	5.447680
4.396494	363.934250	5.452685
4.001391	359.029110	5.457690
4.077251	356.774220	5.462694
4.233041	359.733421	5.467699
4.435650	366.171807	5.472704
4.602730	372.707513	5.477709
4.253963	372.888848	5.482714
4.444920	381.192551	5.487718
4.560515	384.578841	5.492723
4.332950	394.685059	5.497728
4.537879	387.907832	5.502733
4.509953	382.271263	5.507738
4.484337	385.306348	5.512742
5.113468	386.805639	5.517747
4.706795	394.747396	5.522752
4.846235	378.742092	5.527757
4.737167	383.391142	5.532762
4.653990	379.990556	5.537766
4.968762	363.625593	5.542771
4.653180	363.681504	5.547776
4.773383	367.927626	5.552781
4.499449	367.654303	5.557786
4.476565	366.939840	5.562790
4.876183	373.182843	5.567795
4.814016	380.074015	5.572800
4.767695	375.854555	5.577805
4.975488	368.279606	5.582810
4.451464	373.174006	5.587814
4.931571	372.368079	5.592819
4.865989	377.298222	5.597824
4.473178	366.308708	5.602829
4.947042	371.771271	5.607834
4.805384	396.578928	5.612838
5.141439	386.313614	5.617843
4.792661	390.373789	5.622848
4.759715	385.772573	5.627853
5.012621	387.663012	5.632858
5.008172	385.879455	5.637862
4.908937	382.009976	5.642867
4.957598	383.986201	5.647872
4.711776	390.305027	5.652877
5.080258	385.286568	5.657882
5.048890	389.964575	5.662886
5.126926	385.285858	5.667891
5.114426	379.453880	5.672896
4.757460	377.380701	5.677901
5.038829	376.583766	5.682906
5.262503	390.630996	5.687910
5.233083	371.687660	5.692915
4.922665	366.775577	5.697920
5.113455	365.122786	5.702925
5.152207	372.554974	5.707930
4.764072	379.867385	5.712934
5.195403	377.139173	5.717939
4.900175	397.585848	5.722944
4.978508	383.953485	5.727949
5.538138	396.255442	5.732954
5.052910	392.800786	5.737958
5.616146	389.529876	5.742963
5.105132	379.118870	5.747968
4.920660	373.358132	5.752973
5.293550	380.965765	5.757978
5.314366	373.030960	5.762982
5.228581	372.487707	5.767987
5.062375	386.149924	5.772992
5.081218	395.024777	5.777997
5.272885	393.976134	5.783002
5.220716	387.517606	5.788006
5.177299	394.424829	5.793011
5.149960	401.978118	5.798016
5.383585	384.331849	5.803021
5.063334	397.581603	5.808026
5.172134	399.766711	5.813030
5.457487	398.076954	5.818035
5.319802	392.425940	5.823040
4.864491	393.668029	5.828045
5.418573	388.123769	5.833050
5.470169	391.520088	5.838054
5.508019	383.604757	5.843059
5.363701	396.795308	5.848064
5.339869	399.690908	5.853069
5.290160	393.456623	5.858074
5.254011	399.549608	5.863078
5.402316	394.755473	5.868083
5.388051	391.166914	5.873088
5.298811	404.396298	5.878093
5.372611	401.974043	5.883098
5.389900	410.096158	5.888102
5.920830	407.766797	5.893107
5.588330	407.784229	5.898112
5.354354	400.268991	5.903117
5.409251	402.636555	5.908122
5.441328	412.914078	5.913126
5.647928	411.372703	5.918131
5.890241	420.086001	5.923136
5.530989	412.504964	5.928141
5.694837	420.575646	5.933146
5.687060	426.736963	5.938150
5.912683	416.305433	5.943155
5.515067	415.779399	5.948160
5.476033	414.349278	5.953165
5.767078	419.283667	5.958170
5.786905	423.833437	5.963174
5.619060	417.832793	5.968179
5.376798	420.670870	5.973184
5.627881	418.489761	5.978189
5.831379	414.148890	5.983194
5.747365	411.137580	5.988198
5.726318	412.536259	5.993203
5.983446	425.708226	5.998208
5.968612	423.043585	6.003213
5.778103	422.921708	6.008218
5.959086	427.379789	6.013222
5.845475	421.604769	6.018227
5.820181	419.277133	6.023232
5.587346	418.484831	6.028237
6.126571	407.713098	6.033242
5.661410	428.651516	6.038246
5.777391	424.191475	6.043251
5.883915	425.567003	6.048256
5.825303	414.414363	6.053261
6.246642	418.812636	6.058266
5.662474	409.783008	6.063270
5.913608	399.138678	6.068275
5.573130	397.316018	6.073280
5.600334	400.187803	6.078285
5.878029	401.596624	6.083290
5.422457	415.149174	6.088294
5.938664	412.679747	6.093299
5.746868	423.495400	6.098304
5.789092	421.410291	6.103309
5.803171	414.944537	6.108314
5.739059	414.575061	6.113318
6.121917	412.968104	6.118323
6.148113	412.068776	6.123328
5.504464	410.306271	6.128333
6.094129	392.983867	6.133338
5.662186	400.224055	6.138342
5.946455	394.272806	6.143347
5.777286	399.709576	6.148352
5.575844	392.299979	6.153357
5.722141	388.521745	6.158362
5.815583	404.699657	6.163366
5.978459	402.064125	6.168371
6.001161	399.577108	6.173376
5.986922	397.007293	6.178381
5.828246	396.681108	6.183386
5.872030	399.192784	6.188390
5.861305	404.174451	6.193395
5.771815	397.535101	6.198400
5.970149	397.519983	6.203405
5.811717	396.703368	6.208410
5.569993	397.181150	6.213414
5.917428	402.103536	6.218419
5.527000	402.636255	6.223424
5.836239	400.126490	6.228429
5.518050	392.959815	6.233434
5.042237	399.830382	6.238438
5.674342	402.458691	6.243443
5.692495	408.426110	6.248448
5.785481	408.579361	6.253453
5.964846	416.701395	6.258458
5.676119	413.855039	6.263462
5.618321	410.077140	6.268467
5.578656	418.913714	6.273472
5.605611	422.497401	6.278477
5.996744	419.775482	6.283482
5.723858	422.548753	6.288486
5.721863	415.000327	6.293491
5.847961	409.171934	6.298496
5.927461	413.788283	6.303501
5.950936	413.825872	6.308506
5.829747	422.349348	6.313510
5.979221	413.717309	6.318515
5.989696	413.817048	6.323520
5.884600	420.809876	6.328525
5.793875	417.714192	6.333530
5.925938	417.535447	6.338534
5.715599	404.337448	6.343539
5.560935	409.705508	6.348544
5.648660	411.805332	6.353549
5.879971	410.364491	6.358554
5.841600	428.404420	6.363558
5.882478	421.507349	6.368563
5.792381	419.085460	6.373568
5.884423	416.410403	6.378573
6.201637	412.529453	6.383578
5.863735	413.057106	6.388582
5.790407	397.676756	6.393587
5.363584	409.044927	6.398592
5.608367	411.958555	6.403597
5.794735	409.075727	6.408602
5.812154	426.372906	6.413606
5.816879	417.605354	6.418611
5.951386	407.608893	6.423616
5.903994	407.458265	6.428621
5.872047	410.934118	6.433626
5.448822	403.742766	6.438630
5.379622	398.758078	6.443635
5.740784	411.170236	6.448640
5.781472	413.014833	6.453645
6.056611	418.033974	6.458650
6.083113	429.169775	6.463654
6.234116	415.551312	6.468659
5.969220	417.136898	6.473664
5.845111	404.273409	6.478669
5.753540	405.869803	6.483674
6.019805	415.987246	6.488678
6.025010	407.760636	6.493683
5.672679	402.203364	6.498688
5.655485	406.401418	6.503693
5.823198	407.599676	6.508698
5.447151	404.453785	6.513702
5.511828	404.627290	6.518707
5.816062	411.056097	6.523712
5.609040	406.659324	6.528717
5.719629	397.761297	6.533722
5.629523	413.363686	6.538726
5.946505	411.447505	6.543731
5.793931	409.206253	6.548736
5.770681	404.720575	6.553741
5.513879	401.695208	6.558746
5.612617	420.574206	6.563750
5.847786	424.065157	6.568755
6.007248	425.043242	6.573760
5.987572	424.559233	6.578765
6.174988	418.509254	6.583770
5.420478	415.080966	6.588774
5.664215	405.080048	6.593779
5.851358	402.791897	6.598784
5.443022	415.773887	6.603789
5.842330	421.997972	6.608794
5.894530	422.901112	6.613798
5.841576	425.513371	6.618803
5.751991	416.706811	6.623808
5.490524	417.867908	6.628813
5.815943	419.870378	6.633818
5.719054	426.744862	6.638822
5.679062	418.655046	6.643827
5.679246	421.113443	6.648832
5.330096	424.202391	6.653837
5.626047	417.395072	6.658842
5.270111	420.336383	6.663846
5.404392	420.008590	6.668851
5.590251	421.143893	6.673856
5.332186	429.650853	6.678861
5.756622	426.135922	6.683866
5.809990	450.429032	6.688870
6.088592	442.520247	6.693875
6.047233	436.091646	6.698880
5.897676	427.816508	6.703885
6.128008	425.546898	6.708890
5.815660	419.989683	6.713894
6.024245	418.552402	6.718899
5.796945	424.482352	6.723904
5.887821	424.139214	6.728909
5.990468	432.197343	6.733914
5.842435	423.447395	6.738918
5.836051	416.744396	6.743923
6.203740	423.394224	6.748928
5.947418	419.622118	6.753933
5.993963	420.687498	6.758938
5.947481	419.574925	6.763942
6.169486	412.092646	6.768947
6.228590	418.695907	6.773952
5.992724	410.671586	6.778957
5.867250	403.753128	6.783962
5.634407	408.551295	6.788966
5.851880	402.414353	6.793971
5.771434	404.913856	6.798976
5.638067	411.423882	6.803981
5.703176	405.158948	6.808986
5.759577	408.807623	6.813990
5.704959	401.672416	6.818995
5.695245	402.702316	6.824000
5.651244	404.775321	6.829005
5.553779	403.367011	6.834010
5.908440	426.423286	6.839014
5.963975	415.724170	6.844019
5.736543	401.981509	6.849024
5.631791	404.858151	6.854029
5.801015	407.106560	6.859034
5.332549	414.504339	6.864038
5.788882	414.300097	6.869043
5.874379	420.212675	6.874048
5.826405	418.869378	6.879053
6.167046	421.514882	6.884058
5.892613	417.520983	6.889062
5.544881	407.483018	6.894067
6.039624	413.853503	6.899072
5.641555	409.303161	6.904077
5.682752	405.841953	6.909082
5.527464	415.459122	6.914086
5.861098	417.327424	6.919091
5.964964	424.018589	6.924096
5.725715	425.549536	6.929101
6.090630	419.522367	6.934106
5.633423	413.405707	6.939110
5.726675	418.602046	6.944115
5.677270	416.689485	6.949120
5.688641	424.429711	6.954125
6.249283	426.347870	6.959130
6.113970	417.241584	6.964134
6.073385	411.837947	6.969139
5.743108	402.477472	6.974144
5.627368	402.030662	6.979149
5.690838	403.976095	6.984154
5.796527	411.739504	6.989158
5.630773	405.415827	6.994163
6.037507	401.505034	6.999168
5.710766	411.870414	7.004173
5.897853	404.333496	7.009178
5.635683	403.896974	7.014182
5.543936	402.630140	7.019187
5.440764	409.635318	7.024192
5.662427	418.915011	7.029197
6.079312	424.073300	7.034202
6.035747	426.345560	7.039206
5.601949	411.357042	7.044211
5.703056	414.134990	7.049216
6.000496	416.572123	7.054221
6.008694	412.005584	7.059226
5.590563	408.989675	7.064230
5.985391	408.738121	7.069235
5.785352	410.313544	7.074240
5.881621	410.118261	7.079245
5.940834	401.066927	7.084250
5.797528	409.445162	7.089254
5.623712	401.452253	7.094259
5.562307	404.246172	7.099264
5.756431	402.573872	7.104269
5.801950	399.472664	7.109274
5.830237	409.181291	7.114278
5.730061	402.692313	7.119283
5.633395	404.188264	7.124288
5.809607	410.254307	7.129293
5.959126	406.678049	7.134298
5.580094	406.930566	7.139302
5.786564	411.008155	7.144307
5.904016	414.754835	7.149312
5.530438	415.674064	7.154317
5.664255	409.629322	7.159322
5.640178	424.164660	7.164326
5.515658	418.125590	7.169331
5.738054	423.580111	7.174336
5.844049	424.085672	7.179341
6.016200	423.910137	7.184346
5.976374	426.637401	7.189350
5.827710	430.511204	7.194355
5.981675	425.118211	7.199360
5.941434	429.316718	7.204365
5.699329	413.190826	7.209370
5.574435	410.473828	7.214374
5.708171	413.594684	7.219379
5.637567	419.563358	7.224384
5.719662	423.062474	7.229389
6.103291	420.126591	7.234394
6.126283	423.919711	7.239398
5.780602	417.282529	7.244403
5.711634	413.547509	7.249408
5.634430	420.713141	7.254413
5.754290	418.141295	7.259418
6.027948	430.839266	7.264422
5.869640	418.626544	7.269427
5.970608	409.891374	7.274432
5.332922	409.713009	7.279437
5.733498	407.182604	7.284442
5.739380	419.254957	7.289446
5.571456	421.559356	7.294451
5.867101	427.584546	7.299456
5.617883	429.113891	7.304461
5.749909	423.863544	7.309466
5.977253	432.715239	7.314470
6.022993	430.031615	7.319475
6.179130	426.511265	7.324480
5.656163	412.776935	7.329485
5.651758	408.762876	7.334490
5.604332	419.400879	7.339494
5.539471	427.820618	7.344499
5.753788	420.706542	7.349504
5.823631	428.127554	7.354509
6.083489	420.402053	7.359514
5.911035	434.982795	7.364518
5.825316	428.304876	7.369523
5.967374	406.635895	7.374528
5.757606	413.518568	7.379533
5.778119	408.548295	7.384538
5.731092	410.026977	7.389542
5.400291	409.006410	7.394547
5.387814	411.058657	7.399552
5.410942	424.226156	7.404557
5.908932	420.674392	7.409562
5.817111	427.487969	7.414566
6.070553	423.161418	7.419571
6.143539	418.508794	7.424576
5.909057	431.083897	7.429581
5.805474	419.830729	7.434586
5.507012	426.164144	7.439590
5.650647	425.350821	7.444595
5.839411	420.034637	7.449600
6.017388	426.002330	7.454605
5.978740	428.302294	7.459610
5.853721	424.332440	7.464614
5.902776	419.519047	7.469619
6.038856	401.229970	7.474624
5.692980	409.133733	7.479629
5.786301	407.543667	7.484634
5.663717	406.851152	7.489638
5.626008	408.989612	7.494643
5.649954	416.661424	7.499648
5.739163	428.657451	7.504653
5.899203	425.905298	7.509658
5.903492	431.944501	7.514662
5.837557	425.361563	7.519667
5.900067	420.865607	7.524672
5.656050	426.358406	7.529677
5.869715	423.335254	7.534682
5.616780	426.510369	7.539686
5.732465	428.001524	7.544691
6.329403	426.361024	7.549696
5.851083	419.592759	7.554701
5.827896	411.766074	7.559706
5.623884	409.282940	7.564710
5.904279	413.007253	7.569715
5.955339	411.686405	7.574720
5.610084	405.912883	7.579725
5.867236	403.385968	7.584730
6.002995	408.676886	7.589734
5.554573	402.356370	7.594739
5.972121	414.120604	7.599744
5.515666	409.288339	7.604749
5.613951	400.771897	7.609754
5.833148	418.198809	7.614758
5.787060	411.369152	7.619763
5.888729	418.168229	7.624768
5.673897	411.595969	7.629773
6.005599	411.325832	7.634778
5.489066	409.378892	7.639782
5.609252	408.300319	7.644787
5.840523	416.157951	7.649792
5.630001	429.909404	7.654797
5.899461	422.489289	7.659802
5.822702	434.979569	7.664806
5.904457	429.082186	7.669811
5.861651	422.976526	7.674816
5.635193	417.576700	7.679821
5.821892	416.604767	7.684826
5.747467	416.066061	7.689830
5.848157	421.178975	7.694835
6.016301	414.654280	7.699840
6.010383	412.380558	7.704845
5.880393	406.560652	7.709850
5.869217	414.158871	7.714854
5.679486	396.620052	7.719859
5.539786	400.359563	7.724864
5.805058	411.391502	7.729869
5.768404	414.849110	7.734874
5.937927	409.425210	7.739878
5.815378	415.522246	7.744883
5.504548	403.501115	7.749888
5.649025	413.223178	7.754893
5.780048	416.410900	7.759898
6.071902	419.728451	7.764902
5.986940	420.112067	7.769907
5.936411	407.800206	7.774912
5.897899	402.538620	7.779917
5.961982	404.544069	7.784922
5.869763	411.724706	7.789926
5.784193	410.324023	7.794931
5.830283	413.370025	7.799936
5.292151	406.386505	7.804941
5.180568	406.847060	7.809946
5.640719	420.227663	7.814950
6.112379	423.672070	7.819955
5.901642	414.270712	7.824960
5.686018	419.145279	7.829965
5.647474	410.732530	7.834970
5.885532	419.595194	7.839974
5.898348	421.013879	7.844979
5.980898	418.672510	7.849984
5.727434	417.760051	7.854989
5.665240	410.126144	7.859994
5.629180	413.254621	7.864998
5.538633	414.303514	7.870003
5.779546	416.382501	7.875008
5.998221	435.068712	7.880013
5.954950	427.105958	7.885018
5.852174	421.528562	7.890022
5.611900	414.390801	7.895027
5.675560	415.311127	7.900032
5.717607	431.373726	7.905037
5.677311	425.394225	7.910042
5.911631	427.581816	7.915046
6.156646	426.819049	7.920051
6.063476	421.964662	7.925056
5.667556	419.761537	7.930061
5.590549	424.174616	7.935066
5.777368	411.600933	7.940070
5.492947	408.931077	7.945075
5.582457	408.961483	7.950080
5.221662	427.194300	7.955085
5.593349	427.560154	7.960090
5.872213	416.338817	7.965094
5.659356	423.611128	7.970099
5.738729	422.048557	7.975104
5.578888	431.555714	7.980109
5.934225	422.173228	7.985114
5.573593	421.856539	7.990118
5.988135	428.235107	7.995136
5.892064	430.323627	8.000154
6.111944	436.035939	8.005171
6.174525	433.236586	8.010189
5.945832	430.277747	8.015206
5.977129	432.737623	8.020224
5.849360	429.365346	8.025242
5.877161	436.679318	8.030259
5.780488	427.782758	8.035277
5.582820	435.264598	8.040294
5.830442	433.607037	8.045312
5.775172	428.935854	8.050330
5.797736	430.687054	8.055347
6.171581	432.761906	8.060365
6.112024	435.381183	8.065382
6.106401	422.083864	8.070400
5.961357	416.909207	8.075418
5.490277	414.168226	8.080435
5.719945	414.630987	8.085453
5.785164	423.876721	8.090470
5.778342	429.656108	8.095488
5.803742	422.100554	8.100506
5.399740	428.260902	8.105523
5.516958	426.099919	8.110541
6.090298	438.469135	8.115558
5.550451	435.764171	8.120576
6.073147	423.684244	8.125594
5.610783	435.373148	8.130611
5.783758	434.389990	8.135629
5.846488	428.513756	8.140646
5.498727	432.746597	8.145664
5.883272	426.677933	8.150682
5.911589	457.123504	8.155699
6.085673	449.219599	8.160717
5.900132	441.428848	8.165734
6.167354	448.471786	8.170752
5.831129	430.486316	8.175770
6.103436	447.885638	8.180787
6.040777	440.672072	8.185805
6.009304	436.306422	8.190822
5.854566	434.696125	8.195840
6.045394	438.210274	8.200858
5.895038	435.321210	8.205875
6.229304	444.490086	8.210893
6.317361	430.941401	8.215910
6.117363	437.309626	8.220928
6.156294	430.916421	8.225946
5.873392	439.506663	8.230963
6.051088	427.158901	8.235981
6.146069	429.056543	8.240998
5.917605	432.910937	8.246016
6.402771	427.463968	8.251034
6.165099	428.990860	8.256051
5.882513	430.960282	8.261069
5.767820	427.311406	8.266086
5.656257	437.503169	8.271104
6.064524	438.733198	8.276122
6.289002	451.715652	8.281139
6.395723	444.462922	8.286157
6.187546	425.488579	8.291174
6.076798	433.408071	8.296192
6.232042	428.542961	8.301210
5.934903	431.391963	8.306227
6.106199	436.335572	8.311245
6.191516	428.480298	8.316262
6.074247	428.271595	8.321280
6.247730	429.910788	8.326298
5.975981	433.727784	8.331315
5.799681	430.763891	8.336333
6.286182	433.767818	8.341350
6.007946	440.937241	8.346368
6.003345	442.487574	8.351386
6.393430	456.135194	8.356403
6.555128	443.067260	8.361421
6.405674	428.962508	8.366438
6.151064	428.011633	8.371456
6.271839	426.437062	8.376474
6.195832	437.364856	8.381491
5.875004	431.993678	8.386509
6.162579	429.979569	8.391526
6.360572	435.414448	8.396544
6.234644	428.788302	8.401562
6.173716	432.225133	8.406579
6.244672	428.714424	8.411597
5.987146	433.810426	8.416614
5.882398	437.001663	8.421632
6.229045	442.791944	8.426650
6.345266	455.671444	8.431667
6.489723	446.292132	8.436685
6.703244	439.918905	8.441702
6.428036	445.308010	8.446720
6.446671	433.745703	8.451738
6.114765	430.430657	8.456755
5.903500	431.104513	8.461773
5.875414	424.671319	8.466790
5.901816	445.047171	8.471808
6.483096	447.098990	8.476826
6.447280	459.544730	8.481843
6.183449	458.860381	8.486861
6.918183	446.964963	8.491878
6.318872	445.143458	8.496896
5.962429	435.091565	8.501914
6.114863	452.310861	8.506931
6.252238	446.403991	8.511949
6.542432	450.697824	8.516966
6.372795	457.714540	8.521984
6.672165	443.015600	8.527002
6.121693	441.243247	8.532019
6.048786	444.688269	8.537037
6.328005	456.819563	8.542054
6.194464	455.366886	8.547072
6.226908	461.307386	8.552090
6.462360	455.337810	8.557107
6.569669	455.033961	8.562125
6.566931	455.211250	8.567143
6.085882	460.216051	8.572160
6.318617	455.616499	8.577178
6.411864	458.631553	8.582195
6.329930	465.375760	8.587213
6.456135	449.946563	8.592231
6.387069	459.396389	8.597248
6.416720	449.110428	8.602266
6.785198	454.436551	8.607283
6.513230	454.627621	8.612301
6.809972	449.677221	8.617319
6.418729	454.693196	8.622336
6.458993	458.893649	8.627354
6.482043	460.954040	8.632371
6.558899	457.833715	8.637389
6.526564	456.901659	8.642407
6.459717	453.788072	8.647424
6.503718	460.992220	8.652442
6.521544	469.011502	8.657459
6.478416	457.376806	8.662477
6.099076	461.895464	8.667495
6.152579	454.158771	8.672512
6.136758	456.553451	8.677530
6.081377	457.663625	8.682547
5.976333	452.678347	8.687565
6.231329	458.940577	8.692583
6.235468	477.439124	8.697600
6.490096	481.871079	8.702618
6.588039	484.049125	8.707635
6.398881	493.754467	8.712653
6.812808	488.586882	8.717671
6.668666	487.808041	8.722688
7.054988	486.529525	8.727706
6.463674	471.279003	8.732723
6.407127	463.389137	8.737741
6.661820	471.112535	8.742759
6.378549	481.722541	8.747776
6.822816	479.169486	8.752794
6.735340	474.118335	8.757811
6.907764	477.875214	8.762829
6.549732	456.456512	8.767847
6.196844	455.757715	8.772864
6.680258	463.227526	8.777882
7.148038	473.738786	8.782899
6.738622	466.557449	8.787917
6.707081	461.686883	8.792935
6.427307	463.592753	8.797952
6.631083	457.249448	8.802970
6.716078	448.112979	8.807987
6.382528	458.563593	8.813005
6.440892	459.495002	8.818023
6.679573	484.060042	8.823040
6.875865	477.503311	8.828058
6.839389	472.879665	8.833075
7.027362	473.124902	8.838093
6.901377	462.333150	8.843111
6.521795	460.707587	8.848128
6.486900	459.977900	8.853146
6.907988	469.783273	8.858163
6.550611	468.012220	8.863181
7.178355	465.241075	8.868199
6.813590	461.991131	8.873216
6.510221	461.903103	8.878234
6.497788	462.653103	8.883251
6.382474	474.145647	8.888269
6.985996	470.633537	8.893287
7.078375	483.510481	8.898304
7.095125	469.518510	8.903322
6.723876	460.847989	8.908339
6.459117	461.804779	8.913357
6.716428	466.217375	8.918375
6.936383	475.202209	8.923392
7.011101	476.998891	8.928410
6.786890	467.424871	8.933427
6.914923	478.920315	8.938445
7.062345	466.820263	8.943463
7.044069	460.650602	8.948480
6.919523	464.091095	8.953498
6.659138	455.655666	8.958515
6.911208	461.571223	8.963533
7.049725	464.285700	8.968551
6.993026	463.114468	8.973568
6.782528	458.619075	8.978586
6.871256	454.206186	8.983603
6.350890	462.571717	8.988621
6.782947	469.898101	8.993639
6.772262	475.491919	8.998656
6.771173	479.001432	9.003674
6.798936	477.839056	9.008691
6.657687	489.663873	9.013709
6.727828	485.004583	9.018727
6.826936	491.480595	9.023744
6.795926	487.686054	9.028762
7.023596	482.525563	9.033779
6.746831	485.040026	9.038797
6.977847	485.802376	9.043815
6.835607	485.070573	9.048832
6.826454	487.385318	9.053850
7.094921	487.450688	9.058867
6.921596	491.362726	9.063885
7.064865	480.512998	9.068903
7.082621	480.330475	9.073920
6.953505	477.513814	9.078938
7.199609	471.624613	9.083955
7.080028	485.875967	9.088973
6.997705	476.289179	9.093991
6.731701	473.105808	9.099008
6.620611	480.640372	9.104026
6.916334	478.795392	9.109043
6.784228	487.945846	9.114061
6.580843	479.488852	9.119079
7.208102	492.442941	9.124096
7.119988	495.508507	9.129114
7.383600	490.528573	9.134131
7.124320	480.953729	9.139149
7.091069	482.495932	9.144167
7.163654	482.143875	9.149184
6.952328	480.372028	9.154202
7.126926	473.152832	9.159219
6.911118	480.773231	9.164237
6.914388	479.841907	9.169255
7.284985	489.699382	9.174272
7.375314	497.268665	9.179290
7.373612	479.764057	9.184307
7.125177	493.404453	9.189325
6.974818	485.813295	9.194343
7.095529	481.373298	9.199360
6.929839	481.137468	9.204378
7.384346	489.113585	9.209395
7.352200	494.007036	9.214413
7.189339	487.683297	9.219431
6.783600	487.475611	9.224448
6.951450	493.110887	9.229466
7.451066	495.336452	9.234483
7.218915	505.278908	9.239501
7.402445	502.220755	9.244519
7.371268	491.275278	9.249536
7.074102	496.528985	9.254554
7.141226	484.643471	9.259571
7.296188	490.394374	9.264589
7.280612	498.500952	9.269607
7.342447	490.993308	9.274624
7.320064	485.127235	9.279642
7.064598	473.270183	9.284659
7.028346	489.796409	9.289677
7.336933	494.942583	9.294695
7.556292	496.568283	9.299712
7.248518	498.658422	9.304730
7.308582	491.270974	9.309747
7.056531	494.182348	9.314765
7.211623	502.025505	9.319783
7.444016	503.671254	9.324800
7.339814	510.898642	9.329818
7.984256	505.316243	9.334835
7.659357	490.762411	9.339853
7.592043	494.995507	9.344871
7.615084	486.168522	9.349888
7.151760	487.153269	9.354906
7.183449	471.082465	9.359923
6.997848	472.604357	9.364941
7.287407	489.716998	9.369959
7.330964	484.339205	9.374976
6.759368	491.235880	9.379994
7.093229	486.891871	9.385011
7.304348	509.274321	9.390029
7.209123	506.032629	9.395047
7.606220	506.727933	9.400064
7.516896	513.924590	9.405082
7.443913	504.049148	9.410099
7.496747	510.267333	9.415117
7.287838	511.360540	9.420135
7.742344	509.717894	9.425152
7.113444	508.478524	9.430170
7.766968	507.824008	9.435187
7.525872	512.560857	9.440205
7.333954	507.469256	9.445223
7.662059	503.732052	9.450240
7.320107	508.743475	9.455258
7.618988	515.554264	9.460275
7.582280	510.110144	9.465293
7.392582	509.133315	9.470311
7.542378	503.192922	9.475328
7.391050	511.011511	9.480346
7.524384	513.401764	9.485363
7.674720	522.631057	9.490381
7.357818	508.549322	9.495399
7.564291	505.367656	9.500416
7.628414	508.895360	9.505434
7.541091	511.446415	9.510451
7.541709	518.812016	9.515469
7.640039	517.651204	9.520487
7.718329	506.316185	9.525504
7.877195	512.385216	9.530522
7.516568	513.688385	9.535539
7.538788	508.001506	9.540557
7.568884	509.656861	9.545575
7.441498	514.924998	9.550592
7.366433	515.201981	9.555610
7.573893	502.776922	9.560627
7.728137	513.384667	9.565645
7.683096	511.990701	9.570663
7.716368	521.194154	9.575680
7.775863	522.857528	9.580698
7.970745	522.972296	9.585715
7.856678	519.351706	9.590733
7.638591	510.786549	9.595751
7.498028	507.340524	9.600768
7.168968	513.296657	9.605786
7.678089	518.111620	9.610803
7.540893	520.762008	9.615821
7.446004	517.703296	9.620839
7.983113	513.374772	9.625856
7.685706	519.108200	9.630874
8.021813	508.562752	9.635891
7.734205	509.879726	9.640909
7.460320	508.556330	9.645927
7.841352	515.723472	9.650944
7.685064	518.279023	9.655962
7.664193	511.099905	9.660979
7.748331	515.867847	9.665997
7.759066	520.533682	9.671015
7.958953	515.342822	9.676032
7.660759	510.674966	9.681050
7.460535	506.585045	9.686067
7.357969	510.542804	9.691085
7.331070	518.840512	9.696103
7.949803	518.914117	9.701120
7.701827	531.636143	9.706138
7.802601	528.792922	9.711155
8.297569	533.689000	9.716173
7.918090	523.511280	9.721191
7.860829	515.552076	9.726208
7.752607	508.153119	9.731226
7.693566	515.726879	9.736243
7.713379	513.142495	9.741261
7.940758	523.107634	9.746279
8.173905	523.673994	9.751296
7.902538	521.163633	9.756314
7.797027	517.323955	9.761331
8.003121	508.701805	9.766349
7.760222	515.973017	9.771367
7.991128	516.104232	9.776384
7.907988	526.970082	9.781402
8.165279	514.745488	9.786419
7.968049	516.856178	9.791437
7.671491	514.690588	9.796455
8.007897	520.441474	9.801472
8.324967	531.717987	9.806490
8.135022	519.686537	9.811507
8.184978	510.918439	9.816525
8.118039	508.413919	9.821543
7.871527	500.244536	9.826560
7.942514	514.851058	9.831578
7.988216	505.181079	9.836595
8.029023	510.220892	9.841613
8.266594	516.053533	9.846631
8.256327	505.199444	9.851648
7.817601	516.648015	9.856666
7.872288	505.045299	9.861683
8.154199	506.878947	9.866701
7.760835	514.849068	9.871719
8.216198	499.519732	9.876736
7.925510	521.324423	9.881754
8.006542	509.424090	9.886771
8.208619	510.118392	9.891789
7.666076	520.491337	9.896807
7.929649	522.005971	9.901824
8.364470	530.439622	9.906842
8.445000	532.588845	9.911859
8.326983	514.199876	9.916877
7.990528	514.842859	9.921895
8.006255	512.732480	9.926912
8.056028	523.148319	9.931930
8.117067	528.781408	9.936947
8.313817	528.154278	9.941965
8.287487	532.961623	9.946983
7.984871	522.809729	9.952000
7.895152	533.361037	9.957018
8.085593	537.440150	9.962035
8.224420	542.530886	9.967053
8.095240	545.186333	9.972071
8.368528	529.408978	9.977088
8.231906	543.527350	9.982106
7.989164	553.263210	9.987123
8.433832	537.727237	9.992141
7.964415	541.272272	9.997159
8.349405	543.089773	10.002176
8.303884	544.794849	10.007194
8.190418	536.976984	10.012211
8.435957	539.277077	10.017229
8.093116	538.579858	10.022247
8.263984	549.942405	10.027264
8.187243	546.726211	10.032282
8.250004	543.355618	10.037299
7.983383	538.622848	10.042317
8.083024	547.882187	10.047335
8.389011	539.200191	10.052352
8.344769	548.611461	10.057370
8.116160	549.114472	10.062387
8.396380	540.644793	10.067405
8.150050	548.361519	10.072423
8.210520	544.868210	10.077440
8.375491	545.571483	10.082458
8.215951	549.711745	10.087475
8.452449	541.226826	10.092493
8.103971	547.738273	10.097511
8.771401	556.274345	10.102528
8.760135	544.211728	10.107546
8.715151	543.344765	10.112563
8.538884	544.587492	10.117581
8.497097	542.672312	10.122599
8.313644	541.606141	10.127616
8.394519	541.353768	10.132634
8.194671	546.989870	10.137651
8.722678	535.634863	10.142669
8.414136	545.245331	10.147687
8.376417	541.824210	10.152704
8.561182	543.998127	10.157722
8.552693	551.614475	10.162739
8.545309	541.839186	10.167757
8.268103	554.212361	10.172775
8.445847	539.207353	10.177792
8.527606	540.393874	10.182810
8.186934	545.193669	10.187827
8.618073	550.301723	10.192845
8.557934	567.128406	10.197863
8.845500	559.364461	10.202880
8.319051	552.728440	10.207898
8.517183	560.457584	10.212915
8.811678	554.873195	10.217933
8.802726	555.291298	10.222951
8.565797	547.199286	10.227968
8.664461	547.079825	10.232986
8.086761	543.512937	10.238003
8.587467	553.400554	10.243021
8.786230	560.507911	10.248039
8.699267	568.329063	10.253056
8.528155	569.952834	10.258074
8.262394	564.355239	10.263091
8.703350	566.293361	10.268109
8.898533	575.215856	10.273127
8.797866	575.373776	10.278144
8.751537	565.008135	10.283162
8.818815	576.768779	10.288179
8.745664	569.793487	10.293197
8.854741	570.234123	10.298215
8.797755	569.848717	10.303232
9.069358	556.801349	10.308250
8.517073	567.623967	10.313267
8.584912	553.882699	10.318285
8.617633	565.472026	10.323303
8.474909	564.847592	10.328320
9.149370	568.090333	10.333338
8.913444	567.401607	10.338355
9.100047	567.183161	10.343373
8.864195	560.785626	10.348391
8.571241	543.497001	10.353408
8.712164	550.597637	10.358426
8.807690	563.382628	10.363443
9.080412	569.269739	10.368461
9.189616	557.052539	10.373479
9.016713	550.496823	10.378496
9.114198	543.968172	10.383514
8.757111	545.030950	10.388531
9.081690	539.795299	10.393549
8.996883	543.302164	10.398567
9.047203	544.285330	10.403584
8.890412	539.932979	10.408602
9.139952	549.844168	10.413619
8.926946	546.510470	10.418637
8.631527	546.553739	10.423655
8.543151	547.362978	10.428672
8.490116	549.981249	10.433690
8.701192	544.652929	10.438707
8.733261	542.148671	10.443725
9.076366	555.033719	10.448743
8.970763	558.433393	10.453760
9.025246	564.348384	10.458778
8.468182	565.694958	10.463795
8.913890	564.119957	10.468813
8.963326	566.015282	10.473831
9.055273	570.349673	10.478848
9.051470	574.153118	10.483866
8.973201	579.981617	10.488883
9.330846	566.567314	10.493901
9.129236	567.599421	10.498919
9.094756	569.460558	10.503936
9.198707	568.390379	10.508954
8.920754	568.143736	10.513971
9.086426	564.665497	10.518989
9.289429	570.566687	10.524007
9.096960	569.997384	10.529024
9.307462	566.458472	10.534042
8.958330	559.308677	10.539059
9.148052	559.907088	10.544077
8.933368	559.931396	10.549095
9.079700	563.698692	10.554112
9.041835	560.141892	10.559130
9.077164	559.884033	10.564147
8.972128	558.515242	10.569165
8.807882	560.948971	10.574183
8.488682	564.502031	10.579200
9.055045	561.759424	10.584218
9.028693	564.045316	10.589235
8.796816	557.823883	10.594253
9.000960	573.845467	10.599271
8.839049	585.720921	10.604288
9.248105	578.969872	10.609306
9.157747	592.509837	10.614323
9.464275	591.303777	10.619341
9.445586	583.395303	10.624359
9.463508	595.498205	10.629376
9.566887	572.905701	10.634394
9.274563	568.681875	10.639411
9.167103	568.954468	10.644429
9.085053	566.947764	10.649447
9.095855	576.183168	10.654464
9.319057	583.599127	10.659482
9.395821	591.997391	10.664499
9.212439	580.738038	10.669517
9.805708	591.759877	10.674535
9.100116	588.001581	10.679552
9.330182	583.828445	10.684570
9.564843	590.778712	10.689587
9.564232	574.728654	10.694605
9.459554	577.774740	10.699623
8.981696	576.170875	10.704640
9.269740	578.571610	10.709658
8.957104	588.883325	10.714675
9.053185	593.504250	10.719693
9.563488	595.750243	10.724711
9.434902	600.636743	10.729728
9.472753	592.769899	10.734746
9.226768	606.637214	10.739763
9.523734	599.534494	10.744781
9.321049	597.369964	10.749799
9.639595	608.267601	10.754816
9.523816	589.464797	10.759834
9.555205	595.162512	10.764851
9.329337	604.081565	10.769869
9.701599	593.082282	10.774887
9.433026	604.011946	10.779904
9.378254	588.077659	10.784922
9.510580	595.908646	10.789939
9.206250	588.111196	10.794957
9.611439	601.071756	10.799975
9.429804	600.857358	10.804992
9.572310	596.240349	10.810010
9.228874	596.729795	10.815027
9.320398	594.639089	10.820045
9.672848	586.483116	10.825063
9.261720	594.478146	10.830080
9.558647	587.880361	10.835098
9.757691	614.316857	10.840115
9.681463	610.930158	10.845133
9.540030	599.597949	10.850151
9.708425	600.512126	10.855168
9.762328	597.963414	10.860186
9.422322	601.213631	10.865203
9.676164	617.918584	10.870221
10.094809	614.874067	10.875239
9.589074	598.025824	10.880256
9.740997	597.241615	10.885274
9.842987	581.276461	10.890291
9.603391	591.775548	10.895309
9.692530	601.298490	10.900327
9.415589	608.007032	10.905344
9.821244	607.845782	10.910362
9.779339	616.859094	10.915379
10.028307	614.658510	10.920397
9.625798	608.621583	10.925415
9.539182	619.380738	10.930432
9.802399	621.826394	10.935450
9.822135	611.485088	10.940467
9.992365	616.854945	10.945485
10.248311	607.540132	10.950503
9.906245	601.651526	10.955520
9.628968	593.420649	10.960538
9.589857	594.708161	10.965555
9.514844	607.709251	10.970573
9.925523	605.413905	10.975591
9.477910	616.450524	10.980608
9.838139	616.047085	10.985626
9.692103	624.183628	10.990643
9.811642	612.681134	10.995661
9.785450	612.723245	11.000679
9.742482	624.289756	11.005696
9.605127	613.139935	11.010714
10.164548	624.501611	11.015731
9.775061	617.654759	11.020749
9.638221	617.663714	11.025767
9.497794	623.565082	11.030784
9.681282	639.842425	11.035802
9.957665	649.743153	11.040819
9.950252	642.804870	11.045837
10.401499	641.276331	11.050855
10.074029	650.460633	11.055872
10.226338	640.136409	11.060890
9.988910	626.196763	11.065907
9.815830	628.546678	11.070925
10.275610	633.047513	11.075943
10.047413	641.061238	11.080960
10.125062	626.305369	11.085978
10.298279	620.998737	11.090995
9.861234	616.030718	11.096013
10.270968	625.462417	11.101031
10.038609	621.273364	11.106048
10.344746	614.648879	11.111066
10.457613	613.069220	11.116083
10.034278	620.027920	11.121101
10.228005	615.185132	11.126119
10.012466	617.772071	11.131136
10.273543	617.440971	11.136154
10.246486	616.432341	11.141171
10.403425	617.805902	11.146189
10.412249	616.671731	11.151207
10.258159	620.814311	11.156224
10.246168	611.913859	11.161242
10.394450	615.204337	11.166259
10.175020	617.873936	11.171277
10.125021	621.476347	11.176295
10.282558	624.434019	11.181312
10.427539	620.854870	11.186330
10.343366	626.728491	11.191347
10.263511	632.519387	11.196365
10.506959	619.545812	11.201383
10.238253	622.614450	11.206400
10.458633	621.349302	11.211418
10.777436	609.067668	11.216435
10.630891	623.566351	11.221453
10.498981	619.061760	11.226471
10.427145	617.583623	11.231488
10.425671	614.592308	11.236506
10.437489	603.191904	11.241523
10.270952	596.733003	11.246541
10.314572	601.920723	11.251559
10.000903	607.025571	11.256576
10.064243	621.314643	11.261594
10.635431	612.780407	11.266611
10.258945	616.067900	11.271629
10.280027	615.222140	11.276647
10.353194	612.424256	11.281664
10.200427	622.903445	11.286682
10.484808	620.444850	11.291699
10.327551	619.589163	11.296717
10.222795	610.816854	11.301735
10.269019	621.274331	11.306752
10.573736	613.640219	11.311770
10.426558	613.369929	11.316787
10.287506	624.004759	11.321805
10.370903	627.049787	11.326823
10.117264	621.368225	11.331840
9.992146	634.500260	11.336858
10.542103	643.408229	11.341875
10.725670	649.691185	11.346893
10.679888	649.991985	11.351911
10.452327	650.103516	11.356928
10.725526	643.279055	11.361946
10.884704	645.308672	11.366963
10.643663	650.995441	11.371981
10.320779	641.597733	11.376999
10.408077	646.892232	11.382016
10.396210	636.458033	11.387034
10.711996	640.261912	11.392051
10.559810	647.225475	11.397069
10.613817	643.401801	11.402087
10.469640	639.479792	11.407104
10.530911	641.228105	11.412122
10.639627	646.241537	11.417139
10.517108	644.338995	11.422157
10.774592	643.923251	11.427175
10.708440	644.119945	11.432192
10.560208	644.673481	11.437210
10.656941	635.803319	11.442227
10.405059	641.147802	11.447245
10.460986	642.250015	11.452263
10.844839	656.615130	11.457280
10.538233	665.341737	11.462298
10.762296	667.616809	11.467315
10.800728	675.481477	11.472333
11.038002	665.020849	11.477351
11.260278	661.675734	11.482368
10.780634	659.358932	11.487386
10.795910	654.515691	11.492403
10.885423	669.280382	11.497421
11.045967	669.217496	11.502439
10.689359	657.126860	11.507456
10.786155	653.047172	11.512474
10.921762	659.448099	11.517491
10.699467	663.569818	11.522509
10.949787	662.943758	11.527527
10.983257	667.688121	11.532544
10.741234	660.584619	11.537562
10.723796	667.495520	11.542579
10.847718	670.537362	11.547597
11.063859	665.776255	11.552615
11.076021	672.505796	11.557632
10.760858	670.759667	11.562650
10.858399	662.624665	11.567667
11.115404	668.088239	11.572685
11.249656	665.012533	11.577703
11.415065	671.686505	11.582720
10.978775	670.549488	11.587738
10.954525	672.267022	11.592755
10.869717	668.502961	11.597773
10.792950	671.326940	11.602791
11.030633	673.306390	11.607808
10.932144	664.185935	11.612826
11.173271	665.480038	11.617843
11.006923	666.124775	11.622861
11.052405	669.942609	11.627879
11.236770	669.711889	11.632896
10.789689	673.692105	11.637914
11.033330	669.529446	11.642931
11.008322	674.046288	11.647949
11.254229	671.552689	11.652967
11.081955	663.949109	11.657984
10.993230	669.517345	11.663002
11.081220	683.477558	11.668019
11.330464	694.625947	11.673037
11.377444	697.585175	11.678055
11.239184	682.897802	11.683072
10.716334	690.437009	11.688090
11.602304	688.953962	11.693107
11.483617	696.922152	11.698125
11.477123	697.769061	11.703143
11.213594	683.423206	11.708160
11.296375	697.750320	11.713178
11.430849	685.677395	11.718195
10.977435	689.705944	11.723213
11.146924	695.277912	11.728231
11.515056	688.908774	11.733248
11.399536	693.963665	11.738266
11.651002	696.606832	11.743283
11.397790	698.407579	11.748301
11.431487	689.654564	11.753319
11.210962	687.669544	11.758336
10.941380	692.272047	11.763354
11.373377	691.611209	11.768371
11.511448	699.075269	11.773389
11.394332	696.629077	11.778407
11.387877	694.831421	11.783424
11.684106	694.983961	11.788442
11.751720	690.675307	11.793459
11.777647	694.896997	11.798477
11.449949	697.261679	11.803495
11.751947	687.156971	11.808512
11.407610	689.868241	11.813530
11.644545	685.646668	11.818547
11.450763	673.798752	11.823565
11.457133	681.207700	11.828583
11.846783	686.334917	11.833600
11.320468	681.128403	11.838618
11.707532	686.508488	11.843635
11.685212	688.213098	11.848653
11.641995	673.760149	11.853671
11.649159	667.393927	11.858688
11.277102	680.851864	11.863706
11.632410	690.721314	11.868723
11.311539	693.760267	11.873741
11.458166	698.439571	11.878759
11.655898	694.356683	11.883776
11.480200	697.022597	11.888794
11.719763	696.313014	11.893811
11.731960	699.552247	11.898829
11.538897	698.241419	11.903847
11.630194	697.674987	11.908864
11.635037	699.798219	11.913882
11.882287	700.182495	11.918899
11.801011	703.682526	11.923917
11.653158	694.279457	11.928935
12.329239	696.228091	11.933952
11.696366	706.328117	11.938970
11.862593	692.549236	11.943987
11.847028	700.419220	11.949005
11.687572	707.806823	11.954023
11.813980	693.475604	11.959040
11.212854	696.539533	11.964058
11.263968	693.154957	11.969075
11.798437	698.830687	11.974093
11.916173	708.472282	11.979111
12.029534	706.119366	11.984128
12.099353	700.396566	11.989146
12.126951	703.627075	11.994163
11.968438	706.350258	11.999181
12.251089	696.235953	12.004199
11.916804	691.245500	12.009216
12.404635	698.459099	12.014234
11.989682	691.212267	12.019251
12.107398	700.465698	12.024269
12.096035	696.295649	12.029287
12.088080	691.938876	12.034304
12.046316	709.008966	12.039322
12.094289	703.138109	12.044339
12.055585	707.032258	12.049357
12.168951	706.809506	12.054375
12.096947	700.960604	12.059392
11.750601	707.900964	12.064410
11.812071	704.975511	12.069427
12.233564	711.640932	12.074445
11.977326	706.019711	12.079463
12.131447	695.070322	12.084480
12.222663	701.938967	12.089498
12.010088	701.798842	12.094515
11.860703	705.085483	12.099533
11.843457	710.326952	12.104551
11.679285	700.418352	12.109568
11.593372	717.470121	12.114586
12.183567	729.095286	12.119603
11.877800	721.168615	12.124621
12.065086	721.514949	12.129639
12.161105	723.481887	12.134656
12.220863	717.135809	12.139674
12.590636	720.322176	12.144691
12.446793	718.082141	12.149709
12.214659	719.210557	12.154727
12.585579	718.603469	12.159744
12.394377	724.260362	12.164762
12.600621	711.068488	12.169779
12.290285	719.123520	12.174797
12.367011	718.404736	12.179815
12.911259	722.917606	12.184832
12.285945	719.392856	12.189850
12.002901	707.508410	12.194867
12.243208	707.877995	12.199885
12.234654	713.058143	12.204903
12.573506	718.209107	12.209920
12.749396	727.017936	12.214938
12.450720	721.589551	12.219955
12.415483	723.895791	12.224973
12.579724	728.632304	12.229991
12.607674	715.121224	12.235008
12.058962	714.285840	12.240026
12.555065	716.291077	12.245043
12.633601	712.166900	12.250061
12.296298	727.108965	12.255079
12.519469	718.342028	12.260096
12.284975	722.052261	12.265114
12.224370	730.399529	12.270131
12.388495	724.674569	12.275149
12.004704	726.956526	12.280167
12.132246	716.557242	12.285184
12.143539	728.235240	12.290202
12.449738	740.097412	12.295219
13.095682	745.014077	12.300237
12.451827	742.429502	12.305255
12.676584	738.402329	12.310272
12.743483	751.564326	12.315290
12.812496	745.314618	12.320307
12.732069	740.700944	12.325325
12.012541	739.346367	12.330343
12.681860	741.135120	12.335360
12.938408	746.018121	12.340378
12.592694	752.122110	12.345395
13.270613	740.134415	12.350413
12.993453	753.473396	12.355431
12.617378	736.683601	12.360448
12.629047	731.784100	12.365466
12.716306	740.793016	12.370483
12.699341	742.695607	12.375501
12.724910	751.695259	12.380519
12.765214	748.760492	12.385536
12.709398	757.794988	12.390554
12.729922	749.940257	12.395571
13.021462	744.719192	12.400589
12.902154	748.152607	12.405607
12.914256	744.524825	12.410624
12.878446	744.555820	12.415642
12.534198	744.518376	12.420659
13.006596	744.965207	12.425677
12.692886	752.922952	12.430695
13.001086	746.244448	12.435712
12.989628	751.459776	12.440730
12.962467	744.240525	12.445747
13.013341	742.834669	12.450765
12.792230	752.923855	12.455783
12.838607	751.102136	12.460800
12.890650	746.073229	12.465818
12.991659	752.388092	12.470835
13.030002	743.754243	12.475853
12.808340	747.459315	12.480871
12.902709	751.443076	12.485888
13.141981	751.320518	12.490906
12.886636	745.834843	12.495923
12.992110	740.866994	12.500941
13.096336	755.077184	12.505959
12.727281	742.423550	12.510976
13.223392	752.756968	12.515994
13.224365	761.978229	12.521011
13.445034	768.268037	12.526029
13.042918	762.713835	12.531047
13.484514	748.424706	12.536064
12.942888	747.099060	12.541082
13.132934	749.625626	12.546099
13.475665	754.504594	12.551117
13.517072	753.428424	12.556135
12.810519	742.370861	12.561152
13.161237	750.306553	12.566170
13.188627	759.728802	12.571187
13.528913	759.448405	12.576205
13.242876	763.381317	12.581223
13.348293	761.736540	12.586240
13.247133	756.674829	12.591258
13.015798	760.693845	12.596275
13.820648	763.865700	12.601293
13.617660	760.801792	12.606311
13.296591	752.896439	12.611328
13.331482	751.379478	12.616346
13.274610	765.305648	12.621363
13.639576	762.711331	12.626381
13.672539	769.112601	12.631399
13.511867	751.130860	12.636416
13.406364	746.843005	12.641434
13.458990	754.976884	12.646451
13.519529	748.567556	12.651469
13.463052	758.709846	12.656487
13.433346	743.323759	12.661504
13.373626	740.919062	12.666522
13.683510	759.101752	12.671539
13.334711	758.326561	12.676557
13.196212	764.429646	12.681575
13.268553	764.355333	12.686592
13.423351	764.028259	12.691610
13.691827	769.010384	12.696627
13.875032	762.764869	12.701645
13.534610	766.832535	12.706663
13.298989	768.090890	12.711680
13.875409	769.423985	12.716698
13.314751	763.392848	12.721715
13.570609	758.966322	12.726733
13.457398	764.106078	12.731751
13.933535	761.570082	12.736768
13.873982	758.404806	12.741786
13.523094	773.355350	12.746803
13.731422	768.185184	12.751821
13.937505	769.860327	12.756839
14.019331	765.571520	12.761856
13.919079	760.616963	12.766874
13.845499	770.108686	12.771891
13.827759	765.646130	12.776909
13.564926	777.060996	12.781927
13.938186	770.924556	12.786944
13.750546	769.455082	12.791962
13.992999	774.090990	12.796979
14.036285	763.695414	12.801997
14.335716	768.357107	12.807015
14.210466	760.149670	12.812032
14.243208	764.427112	12.817050
13.859188	763.524896	12.822067
13.835234	759.514596	12.827085
13.805503	763.852320	12.832103
13.860822	771.092690	12.837120
14.001160	764.828644	12.842138
13.696624	766.839411	12.847155
14.180660	762.620130	12.852173
14.039278	765.507896	12.857191
13.819622	766.053691	12.862208
14.245605	757.974482	12.867226
13.923951	760.003710	12.872243
14.284501	759.186806	12.877261
14.084606	766.189450	12.882279
13.886695	758.744481	12.887296
14.143692	760.168648	12.892314
13.803412	773.788934	12.897331
14.186811	765.337697	12.902349
13.815534	757.553818	12.907367
14.095464	770.849709	12.912384
13.922958	763.703715	12.917402
14.038135	770.552853	12.922419
14.096943	770.600581	12.927437
13.713690	767.094700	12.932455
13.826502	774.824681	12.937472
14.591402	776.213452	12.942490
14.296717	788.245544	12.947507
14.297976	780.428532	12.952525
14.321383	775.577673	12.957543
14.088474	772.477425	12.962560
14.640225	780.384789	12.967578
14.265215	781.775437	12.972595
13.873943	768.430986	12.977613
14.087379	786.193313	12.982631
14.266983	792.281281	12.987648
14.371771	785.694593	12.992666
14.401530	797.221419	12.997683
14.766308	789.659872	13.002701
14.541008	787.808133	13.007719
14.131908	792.369405	13.012736
14.332311	785.729867	13.017754
14.249241	795.595476	13.022771
14.311460	797.804405	13.027789
14.493305	801.765004	13.032807
14.597710	796.797306	13.037824
14.725844	793.987626	13.042842
14.626266	793.242814	13.047859
14.820175	801.304084	13.052877
14.586368	798.289180	13.057895
14.654148	794.292902	13.062912
14.691008	793.327896	13.067930
14.256238	799.616268	13.072947
14.409164	795.764440	13.077965
14.676574	789.407892	13.082983
14.549129	789.011430	13.088000
14.765925	790.647027	13.093018
14.766172	796.188739	13.098035
14.437822	788.300290	13.103053
14.655759	793.211444	13.108071
14.294255	794.748300	13.113088
14.393199	791.722287	13.118106
14.870514	795.816472	13.123123
14.488966	790.394738	13.128141
14.866110	789.537364	13.133159
14.887697	789.180668	13.138176
14.553905	792.603516	13.143194
14.329093	791.272409	13.148211
14.621934	791.791555	13.153229
15.046902	806.702617	13.158247
14.896305	811.551597	13.163264
14.865741	813.491041	13.168282
14.746773	817.527177	13.173299
14.943012	816.865404	13.178317
14.812346	815.213430	13.183335
14.559949	822.432605	13.188352
15.126124	816.890777	13.193370
14.910561	819.086426	13.198387
15.001840	823.906980	13.203405
15.416132	812.910444	13.208423
15.123028	813.650786	13.213440
15.163013	797.884502	13.218458
14.904790	800.929436	13.223475
14.983478	790.515674	13.228493
14.996252	796.664496	13.233511
15.162690	813.048810	13.238528
15.322191	807.595949	13.243546
15.034143	798.438853	13.248563
14.562569	793.864360	13.253581
15.138610	803.661418	13.258599
15.064751	816.488909	13.263616
15.025354	816.422636	13.268634
15.127443	815.232813	13.273651
15.074009	816.080771	13.278669
14.995096	818.699980	13.283687
14.647947	824.031042	13.288704
14.969164	813.563488	13.293722
14.954149	818.192410	13.298739
15.086447	812.399825	13.303757
15.166676	815.369642	13.308775
14.982863	818.005287	13.313792
15.459003	824.024714	13.318810
15.625148	827.523873	13.323827
15.434366	826.562974	13.328845
15.261938	814.768423	13.333863
15.152635	821.712712	13.338880
15.288072	813.063617	13.343898
15.798806	827.737195	13.348915
15.445940	825.466779	13.353933
15.603435	808.628030	13.358951
15.125595	823.424937	13.363968
15.324144	809.590409	13.368986
15.172449	815.351594	13.374003
15.341474	823.142216	13.379021
15.649669	828.241211	13.384039
15.688160	838.343420	13.389056
15.661649	830.253025	13.394074
15.484998	821.343553	13.399091
15.347850	822.605417	13.404109
15.829898	819.803398	13.409127
15.573019	817.379087	13.414144
15.465393	813.056836	13.419162
15.309804	824.896743	13.424179
15.245970	838.416960	13.429197
15.418389	836.638601	13.434215
15.729594	834.863744	13.439232
15.597946	824.268321	13.444250
15.538762	833.836718	13.449267
15.506335	836.294011	13.454285
16.105512	831.476003	13.459303
15.897298	836.078395	13.464320
15.851777	831.149958	13.469338
16.077622	836.716296	13.474355
16.021204	836.046772	13.479373
15.778931	829.217798	13.484391
15.581156	839.246571	13.489408
16.070502	831.472985	13.494426
16.049003	834.316732	13.499443
15.776345	834.365901	13.504461
15.805725	825.480951	13.509479
16.122797	834.640100	13.514496
15.991940	817.543563	13.519514
15.580997	826.214012	13.524531
15.957872	822.263973	13.529549
15.876064	825.969239	13.534567
16.115570	831.798525	13.539584
15.780082	833.476476	13.544602
15.955245	820.652311	13.549619
15.541150	829.850277	13.554637
15.830435	835.775907	13.559655
16.084429	840.643555	13.564672
16.090746	842.599314	13.569690
16.053968	833.229261	13.574707
16.048225	840.700134	13.579725
16.191072	831.775312	13.584743
16.107688	842.695041	13.589760
16.225685	834.925987	13.594778
16.389254	830.747434	13.599795
16.140395	836.659550	13.604813
16.346873	833.272697	13.609831
16.488859	828.848215	13.614848
16.147116	831.060480	13.619866
16.136627	829.418078	13.624883
16.196837	825.593393	13.629901
16.371252	834.153196	13.634919
16.197149	832.978244	13.639936
16.233825	836.018005	13.644954
16.238049	825.050997	13.649971
16.443405	838.235546	13.654989
16.206659	832.112609	13.660007
16.512164	836.180074	13.665024
16.186086	831.440762	13.670042
16.069105	820.593734	13.675059
16.080843	823.040950	13.680077
16.065007	822.469209	13.685095
16.177699	827.447356	13.690112
16.556609	835.681629	13.695130
16.395049	830.591490	13.700147
15.991171	839.030463	13.705165
16.242114	832.465040	13.710183
16.206786	838.586699	13.715200
16.414577	843.691962	13.720218
16.636148	858.663338	13.725235
16.487322	866.383859	13.730253
16.733624	851.781262	13.735271
16.516563	849.697849	13.740288
16.801568	860.764999	13.745306
16.830209	835.179526	13.750323
16.320866	840.696953	13.755341
16.656057	835.219711	13.760359
16.530174	842.602110	13.765376
16.513314	848.998592	13.770394
16.664186	847.119465	13.775411
16.460227	864.382375	13.780429
16.835592	858.535912	13.785447
16.517412	864.730299	13.790464
16.619767	860.444565	13.795482
16.671306	856.214130	13.800499
16.720933	854.950473	13.805517
16.750316	855.255278	13.810535
16.695312	863.305083	13.815552
16.726832	859.333406	13.820570
16.895326	854.074783	13.825587
16.671266	865.347929	13.830605
16.834589	858.240799	13.835623
16.966144	856.503555	13.840640
16.697093	857.035001	13.845658
16.994871	851.323773	13.850675
16.540986	856.056182	13.855693
16.721692	851.606693	13.860711
16.974846	854.306424	13.865728
16.376121	853.393662	13.870746
17.128135	859.830627	13.875763
16.635060	879.429981	13.880781
16.905608	867.231472	13.885799
17.130339	876.310435	13.890816
16.892875	892.578224	13.895834
16.948835	878.008584	13.900851
17.052611	885.850483	13.905869
17.106408	877.744327	13.910887
16.931588	885.273268	13.915904
16.928768	884.544850	13.920922
17.671293	884.731609	13.925939
17.424251	886.152708	13.930957
17.357789	879.693804	13.935975
17.434832	882.193912	13.940992
17.256181	881.130123	13.946010
17.433572	877.324937	13.951027
17.316098	888.846488	13.956045
17.207999	880.336504	13.961063
17.132423	880.130731	13.966080
16.954858	877.965387	13.971098
17.217870	871.858810	13.976115
16.877979	879.773376	13.981133
17.124505	886.961743	13.986151
16.886269	890.233937	13.991168
16.901716	883.765353	13.996186
17.011045	893.332626	14.001203
17.432867	913.691240	14.006221
17.269098	904.249527	14.011239
17.677571	905.113481	14.016256
17.702743	914.053316	14.021274
17.663651	903.538020	14.026291
17.627221	915.498175	14.031309
17.599740	904.854825	14.036327
17.770400	902.537087	14.041344
17.188708	909.252464	14.046362
17.613713	904.853049	14.051379
17.689353	902.461836	14.056397
17.782127	905.148833	14.061415
18.071606	900.641264	14.066432
17.746735	898.401166	14.071450
17.764085	878.078178	14.076467
17.524522	888.918263	14.081485
17.517625	883.513541	14.086503
17.749494	885.803198	14.091520
17.681331	894.508335	14.096538
17.812797	889.315464	14.101555
17.644556	893.734882	14.106573
17.703094	905.017425	14.111591
18.048516	906.667593	14.116608
18.125088	902.840328	14.121626
17.871707	876.519492	14.126643
17.565007	877.287213	14.131661
17.535048	888.280651	14.136679
17.931095	896.035736	14.141696
17.844087	906.290191	14.146714
17.932180	914.061976	14.151731
17.807576	907.766807	14.156749
17.966295	894.686387	14.161767
17.871952	897.156545	14.166784
17.880150	905.401596	14.171802
17.897411	901.293287	14.176819
18.066614	894.617571	14.181837
18.044533	901.832250	14.186855
18.331024	903.087705	14.191872
17.996835	899.593044	14.196890
18.109167	898.237508	14.201907
18.245332	900.968200	14.206925
18.465617	904.828124	14.211943
18.018086	899.410383	14.216960
18.030911	911.018832	14.221978
18.133398	907.111765	14.226995
18.091533	914.118109	14.232013
18.301083	902.238404	14.237031
18.364771	902.364264	14.242048
17.841929	899.372538	14.247066
18.310441	892.432174	14.252083
18.130030	896.386436	14.257101
18.129967	900.836310	14.262119
18.404593	890.322362	14.267136
18.084587	893.320187	14.272154
18.286274	893.531724	14.277171
18.399617	889.512506	14.282189
18.523087	894.750917	14.287207
18.693096	892.237621	14.292224
18.179657	901.659474	14.297242
18.120474	896.253472	14.302259
18.379227	900.164173	14.307277
18.273172	893.124482	14.312295
18.419071	903.759014	14.317312
18.012536	898.470552	14.322330
18.219488	917.449022	14.327347
18.531474	920.963219	14.332365
18.528866	922.592178	14.337383
18.687680	913.598541	14.342400
18.635825	915.348826	14.347418
18.474918	917.930403	14.352435
18.344140	927.831963	14.357453
18.512535	922.131518	14.362471
18.628510	922.258653	14.367488
18.264377	921.766727	14.372506
18.372562	921.434331	14.377523
18.771482	924.300584	14.382541
18.361566	924.061987	14.387559
18.945211	927.227506	14.392576
18.811746	934.803637	14.397594
18.912447	925.702333	14.402611
18.631352	929.359949	14.407629
18.864124	928.348461	14.412647
19.359222	935.819798	14.417664
18.638924	928.901579	14.422682
18.979938	922.050609	14.427699
18.613376	928.555559	14.432717
18.689808	939.977333	14.437735
19.118075	942.532875	14.442752
18.880009	952.728973	14.447770
19.075870	948.340203	14.452787
19.186547	944.094170	14.457805
19.144815	948.907195	14.462823
19.333238	939.078919	14.467840
19.135903	933.252734	14.472858
18.960462	922.130778	14.477875
18.787699	928.750533	14.482893
19.187842	930.029208	14.487911
19.483995	924.794744	14.492928
18.807295	922.849612	14.497946
19.218189	932.565318	14.502963
19.441873	942.032648	14.507981
19.242914	935.603951	14.512999
19.238999	921.453915	14.518016
18.902682	930.554539	14.523034
19.004381	939.772734	14.528051
18.987476	941.981454	14.533069
18.937300	951.920892	14.538087
19.382724	952.242565	14.543104
19.154557	951.407439	14.548122
19.160359	956.746357	14.553139
19.237092	946.181330	14.558157
19.388337	951.257613	14.563175
19.485374	951.195210	14.568192
19.293104	944.219500	14.573210
19.581177	944.026178	14.578227
19.379908	954.835057	14.583245
19.221162	945.181094	14.588263
19.361629	953.850417	14.593280
19.313152	957.184410	14.598298
19.117718	947.129091	14.603315
19.509749	957.788208	14.608333
19.537122	960.403409	14.613351
19.809809	970.664660	14.618368
19.684950	973.644546	14.623386
19.592704	975.981841	14.628403
19.744086	972.231204	14.633421
19.575665	966.744465	14.638439
19.921491	964.172053	14.643456
19.671493	962.305230	14.648474
19.724905	963.095428	14.653491
19.610126	970.722296	14.658509
19.392683	983.727040	14.663527
19.712081	971.779585	14.668544
19.704554	970.414420	14.673562
19.820416	974.404331	14.678579
20.054178	976.548535	14.683597
19.427038	968.504845	14.688615
19.930364	966.365354	14.693632
19.691904	972.856561	14.698650
19.552326	975.122376	14.703667
19.671142	968.713306	14.708685
19.724097	970.204175	14.713703
19.716870	978.076129	14.718720
20.014007	983.066447	14.723738
20.261027	986.496161	14.728755
20.271094	969.617243	14.733773
19.906256	974.379912	14.738791
19.982599	971.224864	14.743808
19.989255	979.558554	14.748826
19.771124	987.094323	14.753843
20.216439	987.422326	14.758861
20.007965	1001.520758	14.763879
20.390706	999.327571	14.768896
20.517184	998.339046	14.773914
20.138151	999.626197	14.778931
20.019970	989.249476	14.783949
19.872511	996.155630	14.788967
20.381653	995.858241	14.793984
20.131847	987.831163	14.799002
20.261960	988.341098	14.804019
20.519260	990.670966	14.809037
20.286188	997.934521	14.814055
20.551602	991.950605	14.819072
20.568719	994.759925	14.824090
20.447239	987.132469	14.829107
20.494693	988.718876	14.834125
20.593580	991.802566	14.839143
20.774773	986.384122	14.844160
20.411312	988.391522	14.849178
20.484682	992.466991	14.854195
20.890218	987.884411	14.859213
20.315369	981.110643	14.864231
20.624996	971.171839	14.869248
20.373277	976.806735	14.874266
20.463245	986.392870	14.879283
20.630014	974.109561	14.884301
20.434708	983.468988	14.889319
20.732719	990.134927	14.894336
20.453487	998.829004	14.899354
20.533373	992.009453	14.904371
20.522124	991.673677	14.909389
20.544990	993.036716	14.914407
20.852458	986.348770	14.919424
20.581958	992.762952	14.924442
20.567209	996.858540	14.929459
20.565930	990.910098	14.934477
20.230929	992.455442	14.939495
20.327877	997.063712	14.944512
20.651782	1003.050247	14.949530
20.640074	1018.815712	14.954547
20.680782	1019.566877	14.959565
20.609248	1029.452899	14.964583
20.983300	1024.537566	14.969600
21.066544	1025.117962	14.974618
20.870651	1028.806431	14.979635
21.246520	1019.188587	14.984653
21.199324	1012.903344	14.989671
21.155257	1015.756968	14.994688
20.871104	1016.543252	14.999706
21.091056	1025.780834	15.004723
21.402853	1015.567107	15.009741
20.950732	1022.953357	15.014759
21.027380	1019.189172	15.019776
21.002225	1019.291083	15.024794
20.832954	1024.054682	15.029811
21.581975	1031.378975	15.034829
21.531910	1024.844865	15.039847
21.482386	1019.364728	15.044864
21.366204	1027.017086	15.049882
21.205300	1022.958755	15.054899
21.601708	1020.596165	15.059917
21.054979	1024.087133	15.064935
21.030007	1015.696606	15.069952
21.425447	1011.633162	15.074970
21.081588	1020.413116	15.079987
21.198227	1032.472444	15.085005
21.431040	1042.291853	15.090023
21.306867	1040.689334	15.095040
21.316983	1040.179794	15.100058
21.406729	1044.650347	15.105075
21.576810	1037.507373	15.110093
21.588478	1045.228072	15.115111
21.796748	1034.418317	15.120128
21.920495	1042.528560	15.125146
21.781587	1041.739406	15.130163
21.809181	1037.711499	15.135181
22.068749	1030.163180	15.140199
21.775999	1033.383979	15.145216
21.749121	1025.170475	15.150234
21.496013	1022.887559	15.155251
21.657732	1021.776744	15.160269
21.856510	1037.007465	15.165287
21.594937	1038.396138	15.170304
21.798853	1034.798206	15.175322
21.782739	1040.342557	15.180339
22.241437	1038.721299	15.185357
22.267266	1030.736224	15.190375
22.145888	1020.549337	15.195392
21.829798	1010.784289	15.200410
21.378917	1011.839698	15.205427
21.876922	1026.767903	15.210445
21.992808	1028.144773	15.215463
22.125375	1039.788194	15.220480
21.590226	1034.229502	15.225498
21.754862	1056.156011	15.230515
21.880831	1036.084073	15.235533
22.037312	1042.027424	15.240551
21.941803	1037.201437	15.245568
21.891372	1035.461130	15.250586
21.654242	1041.213683	15.255603
21.976571	1033.033825	15.260621
22.164845	1043.611307	15.265639
21.843954	1043.876321	15.270656
22.311358	1059.702457	15.275674
22.103057	1073.021420	15.280691
22.248600	1059.352797	15.285709
21.897745	1057.956210	15.290727
22.129175	1063.913072	15.295744
22.432897	1061.085307	15.300762
22.326467	1072.542128	15.305779
22.374431	1068.192281	15.310797
22.634728	1064.320416	15.315815
22.253712	1067.214217	15.320832
22.475245	1063.881767	15.325850
22.342289	1067.869658	15.330867
22.532835	1051.233789	15.335885
22.197074	1061.991220	15.340903
22.261504	1065.768299	15.345920
22.177268	1064.487731	15.350938
22.201305	1069.069573	15.355955
22.258197	1072.525937	15.360973
22.559252	1080.807236	15.365991
22.497026	1084.477929	15.371008
22.977020	1085.605248	15.376026
22.794583	1097.023499	15.381043
22.749757	1078.726626	15.386061
23.057695	1090.992711	15.391079
23.328050	1080.693920	15.396096
22.956251	1079.265898	15.401114
22.793591	1071.446038	15.406131
22.912066	1060.375777	15.411149
22.495864	1054.940457	15.416167
22.833892	1066.264519	15.421184
22.850865	1078.131207	15.426202
23.060555	1091.643474	15.431219
23.287055	1088.430165	15.436237
22.900210	1062.347720	15.441255
22.564507	1068.709028	15.446272
22.815886	1076.045037	15.451290
22.788960	1082.468426	15.456307
23.075085	1077.412218	15.461325
23.075765	1081.660046	15.466343
23.122274	1083.215051	15.471360
22.987209	1074.737602	15.476378
22.951640	1090.320672	15.481395
23.247964	1084.969368	15.486413
23.369126	1086.490586	15.491431
23.022203	1080.432164	15.496448
23.253810	1075.132029	15.501466
23.031330	1080.238502	15.506483
23.399263	1079.016478	15.511501
23.676827	1083.385029	15.516519
23.139235	1086.767278	15.521536
23.419927	1076.539454	15.526554
23.274240	1083.959770	15.531571
23.173993	1084.972868	15.536589
22.927553	1088.385241	15.541607
22.704944	1086.050200	15.546624
23.392506	1089.704406	15.551642
23.349679	1104.619582	15.556659
23.470694	1091.036831	15.561677
23.639805	1104.227255	15.566695
23.716934	1108.699801	15.571712
24.076247	1105.686591	15.576730
23.567423	1092.379250	15.581747
23.452376	1082.358597	15.586765
23.443398	1094.374532	15.591783
23.668886	1105.804617	15.596800
23.791776	1098.523842	15.601818
23.505971	1097.899715	15.606835
23.939770	1104.383472	15.611853
23.848237	1109.781868	15.616871
23.811205	1098.991573	15.621888
23.677623	1096.102929	15.626906
23.805182	1089.960695	15.631923
23.565903	1092.523018	15.636941
23.732289	1096.836406	15.641959
23.861998	1104.573351	15.646976
24.139050	1106.972724	15.651994
23.754710	1109.879677	15.657011
23.851246	1104.193588	15.662029
23.942843	1103.040105	15.667047
23.642331	1107.022698	15.672064
24.019164	1107.250978	15.677082
24.309440	1101.594497	15.682099
24.176313	1108.700424	15.687117
24.155053	1093.741911	15.692135
23.862709	1101.491331	15.697152
24.325003	1098.032788	15.702170
24.055608	1101.158420	15.707187
24.074396	1100.413985	15.712205
24.218088	1098.362384	15.717223
23.947314	1102.535981	15.722240
24.209798	1094.936684	15.727258
24.314893	1098.865193	15.732275
23.831892	1092.720788	15.737293
24.340005	1103.055686	15.742311
24.421119	1119.447338	15.747328
24.206840	1112.853716	15.752346
24.482143	1126.235806	15.757363
24.595545	1123.816555	15.762381
24.656167	1119.815014	15.767399
24.435733	1113.768322	15.772416
24.605330	1103.535798	15.777434
24.479987	1103.198961	15.782451
24.375596	1110.789546	15.787469
24.948242	1115.673617	15.792487
24.754463	1119.402800	15.797504
24.642393	1106.636057	15.802522
24.132507	1109.991878	15.807539
24.771962	1122.401707	15.812557
25.052428	1127.599810	15.817575
24.321478	1119.061065	15.822592
24.698105	1112.646265	15.827610
24.487149	1128.490383	15.832627
24.611919	1133.274214	15.837645
24.736661	1117.156691	15.842663
24.867483	1124.379062	15.847680
24.785022	1117.408171	15.852698
24.917794	1128.215311	15.857715
24.705093	1123.811614	15.862733
25.069861	1118.231821	15.867751
24.687595	1125.755494	15.872768
24.485715	1124.089402	15.877786
25.043041	1119.407266	15.882803
25.025831	1120.940699	15.887821
24.882765	1113.278700	15.892839
24.554538	1137.403277	15.897856
24.967423	1136.316220	15.902874
25.209720	1143.003569	15.907891
25.305057	1152.547926	15.912909
25.347528	1142.931759	15.917927
25.013505	1141.008652	15.922944
25.178616	1142.100101	15.927962
25.395449	1146.036360	15.932979
25.444907	1143.832257	15.937997
25.149044	1127.607051	15.943015
25.140103	1146.177769	15.948032
25.689760	1144.860994	15.953050
25.768919	1136.078546	15.958067
25.407295	1120.706269	15.963085
25.478817	1113.083234	15.968103
25.129386	1119.304697	15.973120
24.943980	1128.530102	15.978138
25.152114	1140.026045	15.983155
25.461099	1146.570400	15.988173
25.374355	1143.459810	15.993191
25.275334	1151.857476	15.998208
25.376650	1159.709348	16.003226
25.492553	1151.861588	16.008243
25.773922	1156.324237	16.013261
25.737073	1146.452247	16.018279
25.680911	1146.975592	16.023296
25.299555	1145.618491	16.028314
25.831229	1147.334177	16.033331
25.763976	1147.370099	16.038349
26.077299	1150.802080	16.043367
25.554203	1157.899697	16.048384
25.362362	1157.538563	16.053402
25.737839	1171.820197	16.058419
25.680916	1174.934643	16.063437
25.940547	1176.680332	16.068455
25.824662	1182.877848	16.073472
25.993551	1177.697965	16.078490
26.367264	1175.834384	16.083507
26.080295	1177.318567	16.088525
26.236449	1176.865039	16.093543
26.350105	1186.343426	16.098560
26.221300	1177.745023	16.103578
26.386118	1173.436804	16.108595
26.153550	1167.915871	16.113613
26.350899	1158.856111	16.118631
25.921439	1170.297334	16.123648
26.465948	1168.590035	16.128666
26.371071	1171.691491	16.133683
26.046231	1157.386419	16.138701
26.727173	1159.545789	16.143719
26.246987	1155.673156	16.148736
26.216369	1159.641877	16.153754
26.461407	1167.051502	16.158771
26.380473	1172.634453	16.163789
26.430859	1163.657679	16.168807
26.083068	1171.513649	16.173824
26.146146	1172.438045	16.178842
26.508096	1165.230244	16.183859
26.558095	1171.995071	16.188877
26.322226	1168.371341	16.193895
26.298847	1176.040781	16.198912
26.263854	1165.448948	16.203930
26.531447	1158.757718	16.208947
26.155841	1171.774755	16.213965
26.308865	1163.252127	16.218983
26.735472	1181.779887	16.224000
26.903733	1183.846014	16.229018
26.881035	1182.880851	16.234035
26.250133	1192.583198	16.239053
26.904223	1179.800506	16.244071
26.627074	1191.369360	16.249088
26.613146	1191.472669	16.254106
26.964311	1181.240056	16.259123
26.719578	1195.129721	16.264141
26.916883	1189.364699	16.269159
27.024181	1182.689107	16.274176
26.702228	1191.478336	16.279194
26.563108	1181.054290	16.284211
26.328516	1190.060209	16.289229
26.852246	1188.422438	16.294247
26.808460	1215.519580	16.299264
26.745936	1209.520699	16.304282
27.484221	1208.849727	16.309299
27.030473	1211.120613	16.314317
27.251672	1205.045721	16.319335
27.128610	1207.630878	16.324352
26.917015	1216.620584	16.329370
27.152379	1205.740208	16.334387
27.011052	1208.284044	16.339405
27.563360	1207.023656	16.344423
27.784865	1212.742275	16.349440
27.748002	1205.675840	16.354458
27.995704	1200.489914	16.359475
27.388516	1201.680279	16.364493
27.672753	1205.116827	16.369511
27.583532	1198.617191	16.374528
27.059281	1205.023868	16.379546
27.246930	1208.734333	16.384563
27.553924	1208.146715	16.389581
27.663982	1201.297110	16.394599
27.674887	1205.199373	16.399616
27.668867	1208.091248	16.404634
28.082610	1204.018582	16.409651
27.734596	1205.685905	16.414669
27.749533	1207.510963	16.419687
27.619212	1208.146917	16.424704
27.726763	1209.518796	16.429722
27.958219	1206.670772	16.434739
27.908710	1202.654908	16.439757
27.940134	1211.499236	16.444775
28.000953	1209.242851	16.449792
27.763851	1210.005992	16.454810
27.985746	1200.402709	16.459827
27.984766	1205.831128	16.464845
27.559134	1214.743912	16.469863
27.721945	1215.308693	16.474880
27.853331	1226.753599	16.479898
28.034390	1229.316357	16.484915
27.895671	1230.922487	16.489933
28.077918	1238.809053	16.494951
28.364102	1230.868305	16.499968
27.945814	1231.508352	16.504986
28.185368	1222.514534	16.510003
27.987914	1235.942374	16.515021
28.018445	1233.097424	16.520039
28.417412	1230.990033	16.525056
27.917160	1238.797334	16.530074
28.083384	1232.749982	16.535091
27.903667	1240.857367	16.540109
28.444640	1242.808298	16.545127
28.639660	1252.311843	16.550144
28.680758	1259.128592	16.555162
28.972127	1243.174203	16.560179
28.902750	1245.103995	16.565197
28.987442	1235.736790	16.570215
29.165499	1222.706751	16.575232
28.640372	1218.238370	16.580250
28.427449	1222.396618	16.585267
28.881217	1224.036153	16.590285
28.826143	1217.035685	16.595303
28.536056	1216.835114	16.600320
28.771092	1225.647547	16.605338
29.129813	1224.692051	16.610355
28.596350	1225.990790	16.615373
28.777895	1229.080505	16.620391
29.081050	1219.707484	16.625408
29.171454	1220.731745	16.630426
29.072370	1214.707032	16.635443
28.938552	1219.982695	16.640461
28.758757	1222.684043	16.645479
28.857663	1221.245377	16.650496
28.597719	1226.629168	16.655514
28.885676	1232.681374	16.660531
28.812792	1230.291296	16.665549
28.862184	1241.051606	16.670567
29.243996	1248.663905	16.675584
29.493705	1252.727585	16.680602
29.284541	1252.785741	16.685619
29.020931	1256.304980	16.690637
28.727365	1256.003964	16.695655
29.168420	1251.633510	16.700672
29.136336	1255.539364	16.705690
29.265529	1254.051768	16.710707
29.084349	1259.095014	16.715725
29.253423	1257.613793	16.720743
29.180717	1247.381280	16.725760
29.418836	1257.515566	16.730778
29.484052	1251.386200	16.735795
29.506938	1277.305309	16.740813
29.583011	1270.419975	16.745831
29.922888	1268.233473	16.750848
29.743999	1259.068505	16.755866
29.488818	1260.484596	16.760883
29.759908	1256.860315	16.765901
29.417409	1265.883179	16.770919
30.101777	1262.285667	16.775936
29.795575	1262.873438	16.780954
29.639123	1268.717567	16.785971
29.525999	1267.463602	16.790989
29.880206	1280.243292	16.796007
30.193669	1265.443637	16.801024
29.738084	1277.791608	16.806042
30.099963	1275.014660	16.811059
30.060036	1276.002539	16.816077
30.072029	1268.530780	16.821095
30.045527	1275.601132	16.826112
30.331223	1276.556928	16.831130
30.174305	1268.575131	16.836147
29.931085	1263.604964	16.841165
29.881698	1272.818600	16.846183
29.910951	1261.623334	16.851200
29.984533	1274.689992	16.856218
30.125578	1273.879056	16.861235
29.992117	1268.601347	16.866253
29.735042	1263.538674	16.871271
30.154144	1262.229723	16.876288
30.225236	1271.935737	16.881306
30.543634	1280.201789	16.886323
30.188724	1286.029679	16.891341
30.329735	1292.130176	16.896359
30.760920	1295.101892	16.901376
30.466924	1296.726046	16.906394
30.279354	1290.166043	16.911411
30.632235	1297.047570	16.916429
30.252391	1294.999077	16.921447
30.424603	1289.383126	16.926464
30.495828	1294.333186	16.931482
30.634112	1287.924108	16.936499
30.326638	1290.411934	16.941517
30.627861	1297.740225	16.946535
30.537419	1286.194456	16.951552
31.045586	1285.550069	16.956570
30.773629	1283.730834	16.961587
30.932693	1289.654927	16.966605
30.920058	1289.950543	16.971623
30.982254	1291.143336	16.976640
31.062613	1285.740600	16.981658
31.339939	1285.687819	16.986675
31.309040	1276.742659	16.991693
31.313982	1285.726876	16.996711
31.289178	1282.985265	17.001728
31.309011	1281.650505	17.006746
31.144162	1288.673107	17.011763
31.121434	1282.421806	17.016781
30.804374	1283.550939	17.021799
31.283969	1284.233351	17.026816
31.433471	1288.751410	17.031834
31.550480	1282.547645	17.036851
31.294515	1280.605980	17.041869
31.268863	1286.618976	17.046887
31.476307	1280.902831	17.051904
31.141054	1280.775609	17.056922
31.105476	1283.328135	17.061939
31.289498	1273.342570	17.066957
31.374275	1280.060963	17.071975
31.218171	1276.437336	17.076992
31.159717	1287.530162	17.082010
31.517633	1295.894174	17.087027
31.471968	1295.522758	17.092045
31.377283	1306.577089	17.097063
31.565713	1308.520146	17.102080
31.758046	1316.345203	17.107098
31.703475	1314.324642	17.112115
31.856769	1314.894073	17.117133
31.882387	1315.890620	17.122151
32.010904	1305.490842	17.127168
31.540560	1309.922980	17.132186
31.554365	1311.019211	17.137203
32.055401	1311.168072	17.142221
31.345073	1307.741731	17.147239
31.928513	1320.163631	17.152256
32.066439	1325.807017	17.157274
32.112780	1332.619817	17.162291
32.391792	1335.186178	17.167309
32.306420	1338.308266	17.172327
32.488549	1321.843884	17.177344
32.064732	1310.211472	17.182362
31.859402	1308.157726	17.187379
31.819613	1315.283826	17.192397
31.966322	1326.243541	17.197415
32.085179	1321.263967	17.202432
32.163267	1331.095153	17.207450
32.272087	1334.641265	17.212467
32.409338	1339.281181	17.217485
32.087674	1333.146129	17.222503
32.507057	1328.078440	17.227520
32.163929	1328.299602	17.232538
32.473873	1337.438036	17.237555
32.374772	1331.659447	17.242573
32.441491	1344.982861	17.247591
32.829481	1347.522681	17.252608
32.688776	1353.307564	17.257626
32.886000	1357.767669	17.262643
32.870513	1353.288833	17.267661
33.073375	1349.466934	17.272679
32.722565	1333.398477	17.277696
32.633226	1338.036023	17.282714
32.476914	1342.955472	17.287731
32.759156	1340.345632	17.292749
32.802378	1353.183566	17.297767
32.940264	1346.503121	17.302784
33.014581	1349.549696	17.307802
32.805517	1355.604075	17.312819
32.525303	1354.679250	17.317837
32.291527	1352.415354	17.322855
32.787862	1356.838061	17.327872
32.885165	1377.857143	17.332890
33.030851	1370.762042	17.337907
33.461914	1377.625038	17.342925
33.573603	1381.423184	17.347943
33.350627	1375.948022	17.352960
33.431636	1379.725726	17.357978
32.962196	1387.474613	17.362995
33.803051	1381.248925	17.368013
33.997798	1378.690658	17.373031
33.653006	1374.320219	17.378048
33.526823	1362.180376	17.383066
33.414864	1363.936966	17.388083
33.507308	1354.896700	17.393101
33.376414	1359.878445	17.398119
33.384730	1361.900222	17.403136
33.501324	1370.002267	17.408154
33.622035	1373.720099	17.413171
34.109066	1371.734599	17.418189
33.750958	1377.742908	17.423207
33.690822	1368.672890	17.428224
33.818239	1377.798916	17.433242
33.720753	1373.493875	17.438259
33.879270	1364.904016	17.443277
33.727019	1375.386720	17.448295
33.876203	1370.279299	17.453312
34.138317	1367.723103	17.458330
33.987969	1371.189903	17.463347
33.954040	1367.663885	17.468365
33.754315	1366.158384	17.473383
33.787427	1370.344392	17.478400
33.763668	1373.854477	17.483418
34.102801	1377.446567	17.488435
34.235706	1376.879907	17.493453
33.924181	1387.460159	17.498471
33.859377	1393.501416	17.503488
33.981029	1387.423125	17.508506
34.058687	1399.400443	17.513523
34.284706	1398.670865	17.518541
34.253884	1395.346334	17.523559
34.381525	1394.401788	17.528576
34.241739	1393.426555	17.533594
34.334077	1395.504602	17.538611
34.300915	1394.080303	17.543629
34.914045	1398.468943	17.548647
34.798771	1394.236114	17.553664
34.517255	1394.842113	17.558682
34.388125	1391.801238	17.563699
35.190040	1403.156980	17.568717
34.918819	1398.569873	17.573735
34.748955	1395.298686	17.578752
34.743350	1394.365549	17.583770
34.711683	1398.293460	17.588787
35.056529	1381.693072	17.593805
34.609614	1390.154824	17.598823
34.952659	1395.977541	17.603840
35.112021	1401.740673	17.608858
35.381092	1401.313631	17.613875
35.193729	1384.064452	17.618893
34.987687	1389.632357	17.623911
35.114076	1389.480144	17.628928
35.183519	1385.593930	17.633946
35.050327	1390.462431	17.638963
35.085844	1400.533864	17.643981
35.111209	1413.156881	17.648999
35.302177	1415.377274	17.654016
35.163536	1412.751312	17.659034
34.870086	1416.265789	17.664051
35.377136	1418.304110	17.669069
35.073928	1418.449587	17.674087
35.316744	1408.296940	17.679104
35.338860	1410.736298	17.684122
35.253728	1412.091043	17.689139
35.375027	1406.934330	17.694157
35.670037	1429.484679	17.699175
35.832871	1435.149444	17.704192
35.894288	1422.506778	17.709210
35.657590	1422.013805	17.714227
35.604319	1410.547343	17.719245
35.602842	1424.455879	17.724263
35.952175	1430.324961	17.729280
35.852284	1427.834942	17.734298
36.350046	1437.975989	17.739315
36.292855	1427.718851	17.744333
35.631501	1413.999649	17.749351
35.477323	1422.986774	17.754368
35.777083	1420.210069	17.759386
35.415819	1428.033546	17.764403
35.878428	1427.850746	17.769421
36.091215	1427.924846	17.774439
36.254111	1427.050517	17.779456
36.313812	1416.983361	17.784474
36.083924	1425.540520	17.789491
36.540128	1417.424723	17.794509
36.754437	1423.226592	17.799527
36.265429	1419.408933	17.804544
36.496620	1416.683999	17.809562
36.269199	1428.219967	17.814579
36.656138	1420.260193	17.819597
36.314887	1416.283679	17.824615
36.244912	1430.739460	17.829632
36.257133	1412.761523	17.834650
35.977659	1438.150703	17.839667
36.601616	1444.207145	17.844685
36.373853	1442.311539	17.849703
36.601927	1438.548789	17.854720
36.722021	1437.087850	17.859738
36.754904	1437.240632	17.864755
36.842549	1446.142542	17.869773
36.913456	1445.957994	17.874791
36.844403	1445.309361	17.879808
36.993176	1443.809214	17.884826
37.166245	1445.473815	17.889843
37.291837	1447.133230	17.894861
37.222140	1442.211568	17.899879
36.991702	1439.035073	17.904896
37.047097	1433.730882	17.909914
37.155828	1443.876078	17.914931
36.975306	1436.465972	17.919949
37.177661	1440.941074	17.924967
37.197169	1439.827267	17.929984
37.319178	1436.463003	17.935002
36.959806	1453.113332	17.940019
37.218237	1442.961375	17.945037
37.308980	1433.047143	17.950055
37.381804	1441.007749	17.955072
37.387668	1445.579912	17.960090
37.209411	1452.462663	17.965107
37.535604	1465.691862	17.970125
37.951263	1472.159661	17.975143
37.688770	1472.778462	17.980160
37.538859	1466.597519	17.985178
37.418033	1467.478157	17.990195
37.519747	1469.841934	17.995213
37.751825	1461.922185	18.000231
37.605153	1468.083596	18.005248
37.783001	1464.682175	18.010266
38.028189	1468.399459	18.015283
37.731260	1457.902143	18.020301
37.758940	1467.820201	18.025319
37.742813	1479.376748	18.030336
38.117511	1465.962258	18.035354
37.803426	1464.966991	18.040371
37.721215	1462.190164	18.045389
38.364845	1479.598590	18.050407
38.268052	1497.429167	18.055424
38.546715	1486.380884	18.060442
37.977864	1479.056851	18.065459
37.752606	1483.696794	18.070477
38.281894	1499.235904	18.075495
38.415934	1496.406253	18.080512
38.878836	1487.737086	18.085530
38.358149	1495.083776	18.090547
38.443119	1490.728028	18.095565
38.717418	1481.779131	18.100583
38.228396	1491.667700	18.105600
38.546218	1482.718296	18.110618
38.313509	1487.716029	18.115635
38.433599	1487.763626	18.120653
38.132965	1499.004984	18.125671
38.114205	1499.572975	18.130688
38.869473	1503.731079	18.135706
38.616361	1511.465061	18.140723
38.735580	1506.409635	18.145741
38.881697	1506.374256	18.150759
38.952215	1515.525047	18.155776
39.066234	1510.391537	18.160794
38.873249	1503.308418	18.165811
38.678857	1503.105473	18.170829
38.850519	1510.154337	18.175847
39.105345	1515.769999	18.180864
39.175422	1494.791080	18.185882
38.670002	1509.242562	18.190899
38.946403	1520.257820	18.195917
39.317129	1532.116723	18.200935
39.433768	1532.865481	18.205952
39.349432	1528.346894	18.210970
39.411917	1534.529208	18.215987
39.310411	1530.559289	18.221005
39.578295	1527.812810	18.226023
39.261749	1533.660016	18.231040
39.412990	1525.301605	18.236058
39.778293	1523.625508	18.241075
39.432999	1520.454370	18.246093
39.887609	1523.027962	18.251111
39.736317	1525.166287	18.256128
39.828285	1517.937526	18.261146
40.072394	1521.036426	18.266163
40.286882	1517.932225	18.271181
40.012374	1522.898645	18.276199
39.685313	1520.901818	18.281216
39.996262	1518.218023	18.286234
40.189385	1524.266252	18.291251
40.218078	1518.685340	18.296269
40.071997	1519.169134	18.301287
40.026106	1511.974598	18.306304
40.253512	1512.977412	18.311322
39.933115	1517.969956	18.316339
39.903430	1517.930562	18.321357
40.064158	1515.409166	18.326375
40.108269	1513.212167	18.331392
40.318890	1510.143289	18.336410
40.436840	1511.264242	18.341427
40.414984	1513.745219	18.346445
40.372939	1516.611229	18.351463
39.880447	1513.542054	18.356480
40.178532	1508.783666	18.361498
40.591427	1532.123596	18.366515
40.600748	1535.559099	18.371533
40.265584	1534.794360	18.376551
40.431564	1553.637909	18.381568
40.847919	1542.896236	18.386586
40.936093	1544.754037	18.391603
40.709925	1543.508295	18.396621
40.897871	1538.524147	18.401639
40.660663	1538.611945	18.406656
41.129843	1538.999342	18.411674
40.949813	1536.588139	18.416691
40.886751	1532.937258	18.421709
41.054145	1538.045895	18.426727
40.848591	1548.183585	18.431744
40.920335	1549.109800	18.436762
41.068839	1545.586722	18.441779
41.038118	1551.468051	18.446797
41.726224	1553.948257	18.451815
41.143620	1549.943253	18.456832
41.259904	1554.826362	18.461850
41.603267	1560.036829	18.466867
41.310486	1565.615223	18.471885
41.700487	1549.626171	18.476903
41.529036	1567.269691	18.481920
41.862778	1555.578389	18.486938
41.802119	1548.831142	18.491955
41.596622	1543.242731	18.496973
41.705655	1535.891363	18.501991
41.514316	1552.032597	18.507008
41.638826	1556.718749	18.512026
41.995767	1547.179332	18.517043
41.496877	1562.245244	18.522061
41.926452	1555.225516	18.527079
41.878114	1558.913066	18.532096
41.659403	1552.802835	18.537114
41.765124	1547.370799	18.542131
41.785338	1557.037601	18.547149
42.010149	1548.904348	18.552167
41.738698	1555.451429	18.557184
41.759373	1552.005185	18.562202
41.924514	1565.685745	18.567219
42.179162	1572.734256	18.572237
42.305393	1575.476076	18.577255
42.268806	1576.621246	18.582272
42.340698	1579.175911	18.587290
42.179305	1570.500370	18.592307
42.280734	1579.428590	18.597325
42.493120	1576.255276	18.602343
42.195422	1568.352210	18.607360
42.255737	1573.102075	18.612378
42.142296	1565.836047	18.617395
42.372242	1585.931989	18.622413
42.440777	1593.063319	18.627431
42.895246	1599.780717	18.632448
42.836207	1604.552447	18.637466
43.212627	1598.620369	18.642483
43.168985	1597.835199	18.647501
43.417141	1599.478582	18.652519
43.124806	1587.904287	18.657536
43.095197	1585.144446	18.662554
43.235264	1569.626902	18.667571
42.839664	1582.571627	18.672589
42.783652	1577.439490	18.677607
42.899027	1590.556638	18.682624
42.756130	1596.859520	18.687642
43.258688	1591.456818	18.692659
42.996543	1601.631808	18.697677
43.565496	1594.975255	18.702695
43.161505	1599.677948	18.707712
43.187257	1599.765573	18.712730
43.582537	1598.037434	18.717747
43.308998	1597.846888	18.722765
43.710620	1597.550560	18.727783
43.499225	1593.487385	18.732800
43.539370	1603.286795	18.737818
43.881718	1594.709052	18.742835
43.595892	1601.555062	18.747853
43.726366	1602.869728	18.752871
43.738689	1612.064402	18.757888
43.937259	1625.190632	18.762906
44.213630	1617.459545	18.767923
43.912419	1615.509152	18.772941
44.242083	1613.904906	18.777959
43.885979	1603.678720	18.782976
43.859559	1613.576932	18.787994
44.413409	1610.394296	18.793011
44.338939	1615.228410	18.798029
44.478653	1611.965486	18.803047
44.239546	1606.218211	18.808064
44.340880	1615.124372	18.813082
44.500645	1617.958780	18.818099
44.178197	1613.991899	18.823117
44.563607	1609.977233	18.828135
44.663095	1613.379689	18.833152
44.623939	1620.944489	18.838170
44.395890	1612.115261	18.843187
44.560495	1613.825388	18.848205
44.903848	1609.870963	18.853223
44.539487	1612.090020	18.858240
44.386754	1608.121798	18.863258
44.448948	1603.766435	18.868275
44.408523	1605.956831	18.873293
44.588454	1611.663157	18.878311
44.752329	1619.536990	18.883328
44.592044	1609.923936	18.888346
44.847186	1619.415101	18.893363
44.566501	1632.660609	18.898381
44.898137	1638.450478	18.903399
44.805686	1636.470531	18.908416
44.639183	1635.871875	18.913434
45.215424	1636.678023	18.918451
44.924401	1638.513189	18.923469
45.251954	1651.830681	18.928487
45.770781	1649.619252	18.933504
45.255121	1639.175035	18.938522
45.272409	1626.463396	18.943539
45.485509	1646.893422	18.948557
45.747783	1648.752360	18.953575
45.886689	1649.033707	18.958592
45.396186	1637.039125	18.963610
45.551478	1638.555043	18.968627
45.178029	1656.381785	18.973645
45.642629	1655.898855	18.978663
45.576345	1649.919351	18.983680
45.394146	1654.189656	18.988698
45.767608	1649.693990	18.993715
45.676964	1656.073917	18.998733
45.597743	1647.309721	19.003751
45.601106	1655.603214	19.008768
45.780461	1674.438483	19.013786
46.153389	1668.017754	19.018803
45.723142	1676.458094	19.023821
45.875563	1677.084481	19.028839
46.377698	1669.762991	19.033856
46.190842	1675.432126	19.038874
46.533044	1671.433684	19.043891
46.379136	1673.231591	19.048909
46.499671	1667.052389	19.053927
46.491389	1670.616915	19.058944
46.411659	1673.135386	19.063962
46.575580	1668.088691	19.068979
46.314560	1668.517909	19.073997
46.905541	1685.196289	19.079015
46.986690	1683.785617	19.084032
47.023261	1675.069541	19.089050
46.971677	1670.488978	19.094067
46.829275	1670.877520	19.099085
46.730055	1667.033451	19.104103
46.748301	1673.150157	19.109120
46.820031	1692.289501	19.114138
47.233845	1687.512934	19.119155
47.222412	1699.090979	19.124173
47.157356	1691.081977	19.129191
47.197645	1694.607338	19.134208
47.007513	1691.856851	19.139226
47.045698	1692.103484	19.144243
47.131979	1687.914750	19.149261
47.379140	1688.778772	19.154279
47.450655	1681.824563	19.159296
47.246731	1682.487845	19.164314
47.537286	1685.538470	19.169331
47.420109	1694.936522	19.174349
47.193310	1694.082209	19.179367
47.773181	1695.342252	19.184384
47.597315	1689.723905	19.189402
48.029357	1694.052625	19.194419
47.813756	1693.471127	19.199437
47.620711	1686.492091	19.204455
47.877523	1698.854974	19.209472
47.912994	1716.721854	19.214490
48.593414	1706.175411	19.219507
48.026183	1700.899260	19.224525
47.936386	1692.752114	19.229543
48.162376	1703.661768	19.234560
48.128831	1710.058016	19.239578
48.181767	1707.537702	19.244595
48.115525	1705.537861	19.249613
48.342927	1708.491080	19.254631
48.181296	1706.484092	19.259648
48.264603	1715.730818	19.264666
48.575130	1708.357278	19.269683
48.675229	1706.476549	19.274701
48.248039	1708.150010	19.279719
48.604779	1704.168220	19.284736
48.412865	1710.753391	19.289754
48.547845	1701.778873	19.294771
48.429609	1697.678987	19.299789
48.272733	1701.348856	19.304807
48.587785	1714.226516	19.309824
48.626829	1731.578427	19.314842
48.979404	1729.298358	19.319859
48.742866	1731.235457	19.324877
49.160044	1723.589566	19.329895
49.055847	1731.407614	19.334912
49.071597	1736.101385	19.339930
48.978104	1729.356058	19.344947
49.083320	1728.364513	19.349965
49.197830	1720.548282	19.354983
49.215870	1729.003621	19.360000
49.081545	1731.202432	19.365018
49.480110	1722.069835	19.370035
49.512338	1724.394037	19.375053
49.131054	1730.926830	19.380071
49.901071	1738.825675	19.385088
49.838312	1735.632323	19.390106
49.551836	1720.875793	19.395123
49.724504	1735.555750	19.400141
49.774512	1751.299568	19.405159
50.120462	1743.879435	19.410176
49.341341	1747.438510	19.415194
49.655165	1744.596433	19.420211
49.934828	1741.418862	19.425229
49.745268	1750.992396	19.430247
50.175510	1742.675382	19.435264
50.081066	1741.039737	19.440282
49.808259	1749.206120	19.445299
50.124145	1743.311884	19.450317
49.898023	1750.934436	19.455335
50.091653	1745.722110	19.460352
50.477602	1760.756857	19.465370
50.120110	1772.960403	19.470387
50.727128	1774.699065	19.475405
50.456106	1768.814718	19.480423
50.747876	1763.883673	19.485440
50.815013	1764.192047	19.490458
51.139767	1761.524990	19.495475
50.633865	1751.426336	19.500493
50.922540	1749.478186	19.505511
50.858066	1739.020027	19.510528
50.836241	1749.779177	19.515546
51.095960	1752.913544	19.520563
51.118704	1744.048114	19.525581
50.886385	1747.594105	19.530599
51.096162	1747.731799	19.535616
50.822254	1767.509233	19.540634
50.753932	1766.459664	19.545651
51.048178	1764.062489	19.550669
51.126232	1760.503068	19.555687
51.396350	1754.177317	19.560704
51.342953	1754.075361	19.565722
51.027712	1760.269595	19.570739
51.111184	1756.781913	19.575757
51.360446	1761.795732	19.580775
51.498162	1773.233685	19.585792
51.541892	1784.635876	19.590810
51.719253	1778.170005	19.595827
52.035302	1774.308190	19.600845
51.548985	1781.715886	19.605863
52.136823	1776.050445	19.610880
51.657898	1777.870882	19.615898
51.723829	1778.024801	19.620915
52.094157	1777.468271	19.625933
51.685509	1775.623060	19.630951
51.836300	1782.514347	19.635968
51.869257	1782.951160	19.640986
51.822060	1783.924425	19.646003
51.940060	1778.114833	19.651021
51.530874	1783.335969	19.656039
52.140518	1799.080515	19.661056
51.780367	1806.970257	19.666074
51.761042	1802.034291	19.671091
52.335172	1800.688391	19.676109
52.085264	1803.476554	19.681127
52.287832	1809.267765	19.686144
52.354999	1824.273611	19.691162
52.555399	1822.850556	19.696179
52.919950	1830.427938	19.701197
52.404183	1824.865958	19.706215
52.903628	1820.602992	19.711232
52.933990	1825.376553	19.716250
52.992995	1819.064919	19.721267
52.964193	1821.745855	19.726285
52.813292	1817.521664	19.731303
52.850529	1821.378908	19.736320
53.261181	1824.022552	19.741338
53.415096	1825.737530	19.746355
53.542444	1826.257391	19.751373
53.363458	1831.575026	19.756391
53.112770	1823.942208	19.761408
53.408720	1837.608794	19.766426
53.358791	1839.125322	19.771443
53.471247	1837.561401	19.776461
53.756477	1842.938859	19.781479
53.724561	1839.443992	19.786496
53.730637	1841.456707	19.791514
53.534779	1841.159306	19.796531
54.181092	1841.544207	19.801549
53.659006	1844.763208	19.806567
53.854894	1842.526610	19.811584
53.867106	1833.123109	19.816602
53.856875	1836.735314	19.821619
54.076370	1830.493211	19.826637
53.850631	1831.352432	19.831655
53.981130	1829.422744	19.836672
53.872498	1833.485893	19.841690
54.314537	1847.792358	19.846707
54.697941	1854.031807	19.851725
54.798860	1858.431383	19.856743
54.796837	1839.852451	19.861760
54.435678	1836.702677	19.866778
54.329434	1836.631093	19.871795
54.734517	1832.237732	19.876813
54.562207	1835.963699	19.881831
54.564513	1845.942750	19.886848
54.648425	1848.637591	19.891866
54.319053	1856.775013	19.896883
54.697713	1855.604910	19.901901
54.436998	1859.253208	19.906919
54.588782	1854.751196	19.911936
54.945669	1858.201738	19.916954
54.715583	1876.735274	19.921971
55.085348	1873.893880	19.926989
55.169671	1877.264046	19.932007
54.927653	1874.745737	19.937024
55.267543	1870.693961	19.942042
55.425145	1876.375467	19.947059
55.513529	1875.900980	19.952077
55.116988	1876.777496	19.957095
55.495775	1871.933781	19.962112
55.594598	1872.827365	19.967130
55.530397	1877.647316	19.972147
55.654684	1868.036877	19.977165
55.276945	1872.590350	19.982183
55.693755	1874.904813	19.987200
56.009447	1883.960572	19.992218
55.920625	1890.539125	19.997235
56.293697	1890.070530	20.002253
55.967425	1879.381889	20.007271
55.963279	1880.664016	20.012288
56.318451	1884.768126	20.017306
55.934909	1894.078619	20.022323
56.596390	1881.897071	20.027341
56.473990	1897.664874	20.032359
56.529453	1886.247346	20.037376
56.229147	1891.429362	20.042394
56.133259	1887.540539	20.047411
56.591685	1891.543261	20.052429
56.285112	1892.150045	20.057447
56.458129	1892.669065	20.062464
56.776763	1887.500233	20.067482
56.070323	1893.443359	20.072499
56.491817	1884.041983	20.077517
56.443871	1892.712878	20.082535
56.378272	1905.890173	20.087552
57.042135	1904.987828	20.092570
56.796269	1909.306040	20.097587
57.041058	1909.589739	20.102605
57.109375	1917.595448	20.107623
56.887219	1913.634878	20.112640
57.229264	1912.981783	20.117658
56.992903	1911.977469	20.122675
57.270016	1920.124046	20.127693
57.317972	1932.276800	20.132711
57.384317	1942.299524	20.137728
57.750149	1936.425803	20.142746
57.585048	1938.348575	20.147763
57.650213	1940.251050	20.152781
57.785050	1937.992445	20.157799
57.779959	1932.179996	20.162816
58.084371	1935.569343	20.167834
57.797374	1936.160438	20.172851
58.233853	1932.087204	20.177869
58.080601	1929.561291	20.182887
57.879819	1933.329610	20.187904
57.936244	1934.747427	20.192922
58.055026	1929.947589	20.197939
58.242409	1930.186630	20.202957
58.149781	1928.118309	20.207975
58.090642	1930.084443	20.212992
58.351329	1927.238039	20.218010
58.165492	1948.172756	20.223027
58.166908	1945.174453	20.228045
58.658155	1955.200045	20.233063
58.471098	1950.766877	20.238080
58.806068	1954.858388	20.243098
58.648559	1953.999518	20.248115
58.883494	1956.244651	20.253133
58.694971	1956.239609	20.258151
58.601112	1954.067330	20.263168
58.727807	1948.628730	20.268186
58.679101	1947.910615	20.273203
59.141444	1959.704953	20.278221
58.968196	1970.219698	20.283239
59.108268	1971.608633	20.288256
59.325675	1975.971050	20.293274
59.099897	1976.681951	20.298291
59.460219	1983.117580	20.303309
59.411261	1976.485110	20.308327
59.172007	1977.198123	20.313344
59.757034	1974.420824	20.318362
59.488877	1969.839400	20.323379
59.167484	1974.194709	20.328397
59.422496	1974.145425	20.333415
59.376377	1979.161400	20.338432
59.775454	1984.019256	20.343450
59.610841	1999.935783	20.348467
59.984617	1997.646047	20.353485
59.984939	2003.251242	20.358503
60.029638	1997.749730	20.363520
60.315947	1989.224764	20.368538
60.134623	2004.550580	20.373555
60.366041	1994.367827	20.378573
60.536639	1994.385421	20.383591
60.184487	1991.164776	20.388608
60.692248	1992.985289	20.393626
60.511409	1993.651277	20.398643
60.586362	1985.607582	20.403661
60.585849	1984.755673	20.408679
60.544807	1992.450323	20.413696
60.795671	1991.076157	20.418714
60.529050	1991.332677	20.423731
60.705814	2005.541966	20.428749
60.723570	2011.788262	20.433767
60.874781	2013.147051	20.438784
61.212199	2016.629079	20.443802
60.912164	2024.036093	20.448819
60.697540	2016.337577	20.453837
61.099588	2015.261638	20.458855
60.934873	2021.539682	20.463872
61.226046	2022.753457	20.468890
61.521743	2041.015423	20.473907
61.295536	2044.077641	20.478925
61.472214	2044.984285	20.483943
61.388828	2040.471731	20.488960
61.755154	2028.061753	20.493978
61.660850	2029.771456	20.498995
61.872143	2033.102822	20.504013
61.948904	2027.006100	20.509031
61.559356	2035.045725	20.514048
62.371176	2033.018738	20.519066
61.766601	2043.313905	20.524083
62.193202	2033.346721	20.529101
62.355020	2023.976489	20.534119
61.970695	2036.541049	20.539136
62.197938	2026.797621	20.544154
62.212489	2044.800660	20.549171
62.380759	2048.621643	20.554189
62.857755	2051.021382	20.559207
62.590419	2062.115853	20.564224
63.041020	2050.996100	20.569242
62.659123	2054.638175	20.574259
62.685404	2049.824393	20.579277
62.792769	2049.896078	20.584295
62.382413	2050.351857	20.589312
62.606563	2053.425574	20.594330
62.489128	2045.995862	20.599347
62.477649	2049.535716	20.604365
62.738582	2048.990006	20.609383
62.819379	2077.814223	20.614400
63.105718	2080.145999	20.619418
63.359374	2080.895407	20.624435
62.971132	2086.744556	20.629453
63.288633	2079.158317	20.634471
63.493586	2082.768418	20.639488
63.960265	2070.942337	20.644506
63.699865	2071.797531	20.649523
63.676348	2066.044735	20.654541
63.758884	2076.847696	20.659559
63.419238	2077.267148	20.664576
63.684201	2071.229293	20.669594
63.478902	2072.470360	20.674611
63.476662	2079.991698	20.679629
63.676965	2081.137657	20.684647
63.704341	2102.581988	20.689664
64.255638	2097.988917	20.694682
64.103660	2104.028291	20.699699
63.933789	2107.564568	20.704717
63.904219	2102.797395	20.709735
64.156228	2102.347763	20.714752
64.467928	2107.866334	20.719770
64.659223	2121.041410	20.724787
64.604998	2115.100889	20.729805
64.881735	2114.183444	20.734823
64.758346	2119.940612	20.739840
65.193596	2114.507272	20.744858
65.135146	2118.300671	20.749875
64.866262	2119.864152	20.754893
65.147011	2118.835616	20.759911
64.929750	2117.900886	20.764928
64.793197	2105.282443	20.769946
65.097278	2113.418572	20.774963
65.186035	2119.480199	20.779981
65.296725	2110.124245	20.784999
64.745746	2112.031748	20.790016
65.588033	2100.648610	20.795034
65.321801	2104.607114	20.800051
65.121157	2115.142017	20.805069
65.446094	2114.295921	20.810087
65.450907	2129.529560	20.815104
65.635369	2133.057668	20.820122
65.330391	2137.716581	20.825139
65.637755	2135.866456	20.830157
65.998275	2137.224021	20.835175
66.028404	2152.093923	20.840192
65.991394	2144.878805	20.845210
66.296535	2153.251491	20.850227
66.046304	2155.152906	20.855245
66.233973	2154.192605	20.860263
66.036648	2153.169535	20.865280
66.182576	2150.344233	20.870298
66.039813	2142.227272	20.875315
66.485707	2142.037620	20.880333
66.932399	2149.021555	20.885351
66.696223	2152.757592	20.890368
66.611265	2152.881503	20.895386
66.692493	2154.323856	20.900403
67.018163	2170.839116	20.905421
67.260875	2173.805795	20.910439
66.815684	2164.767297	20.915456
67.128805	2165.311716	20.920474
67.005967	2161.837343	20.925491
66.843973	2164.160471	20.930509
67.204242	2170.517275	20.935527
67.501329	2172.115174	20.940544
67.436287	2169.196679	20.945562
67.496115	2174.937783	20.950579
67.368920	2169.052862	20.955597
67.605149	2165.093009	20.960615
67.260170	2173.169897	20.965632
67.696739	2171.100694	20.970650
67.670829	2180.828712	20.975667
67.910816	2190.316244	20.980685
68.130255	2187.851833	20.985703
67.834032	2182.908648	20.990720
68.201913	2184.738473	20.995738
68.320958	2187.768715	21.000755
68.110128	2190.434040	21.005773
68.151961	2183.821987	21.010791
68.264330	2186.727032	21.015808
68.135428	2186.823111	21.020826
68.403549	2178.332465	21.025843
68.378142	2182.347937	21.030861
68.457302	2186.858308	21.035879
68.214210	2187.524589	21.040896
68.813121	2196.820179	21.045914
68.888747	2205.617044	21.050931
68.725795	2214.132530	21.055949
68.899859	2214.076991	21.060967
68.632415	2207.828991	21.065984
69.023183	2207.313432	21.071002
69.427567	2199.457889	21.076019
69.240082	2203.132656	21.081037
69.250246	2205.526654	21.086055
69.286437	2208.702436	21.091072
69.392644	2202.755687	21.096090
69.261152	2206.532144	21.101107
69.058978	2219.049356	21.106125
69.557885	2220.442055	21.111143
69.274566	2227.761319	21.116160
69.554970	2233.852924	21.121178
69.712615	2232.625900	21.126195
69.281666	2236.162078	21.131213
70.159695	2241.891787	21.136231
70.177243	2250.694617	21.141248
70.195251	2253.444030	21.146266
70.430794	2252.574061	21.151283
70.227414	2257.662093	21.156301
70.522970	2242.438370	21.161319
70.604038	2247.412400	21.166336
70.757324	2244.636427	21.171354
70.728936	2245.202794	21.176371
70.486491	2252.054877	21.181389
70.488235	2244.334988	21.186407
70.971051	2246.901113	21.191424
70.446546	2239.036439	21.196442
70.894280	2238.821249	21.201459
70.651783	2233.800199	21.206477
70.867740	2235.953658	21.211495
70.729444	2247.987472	21.216512
70.804350	2259.082097	21.221530
70.749774	2266.460221	21.226547
70.795974	2262.025146	21.231565
71.177218	2265.162657	21.236583
71.277953	2284.922993	21.241600
71.399978	2288.839644	21.246618
71.774255	2283.668294	21.251635
71.617877	2292.933933	21.256653
71.353977	2294.992153	21.261671
71.813153	2300.348809	21.266688
71.736491	2297.779283	21.271706
71.950590	2284.398814	21.276723
72.029888	2294.198781	21.281741
72.128154	2277.825564	21.286759
72.050480	2288.189809	21.291776
72.220807	2298.180661	21.296794
72.585286	2301.484921	21.301811
72.600149	2311.165593	21.306829
72.509348	2299.653942	21.311847
72.879523	2307.823990	21.316864
72.554583	2287.142740	21.321882
72.627951	2290.833464	21.326899
72.720910	2289.780687	21.331917
72.897409	2293.846608	21.336935
72.550676	2301.990107	21.341952
72.807027	2308.069725	21.346970
73.151934	2290.411202	21.351987
72.821035	2305.602905	21.357005
73.048987	2299.173107	21.362023
73.156525	2291.209384	21.367040
73.071541	2290.525343	21.372058
72.974480	2296.666640	21.377075
73.297026	2311.323588	21.382093
73.224058	2320.831816	21.387111
73.669794	2324.839782	21.392128
73.624088	2326.456684	21.397146
73.617232	2315.402129	21.402163
73.751296	2330.539942	21.407181
73.688247	2320.851305	21.412199
73.792054	2321.633669	21.417216
74.064968	2335.875497	21.422234
74.174888	2337.480643	21.427251
74.288044	2349.301543	21.432269
74.468590	2346.559156	21.437287
74.336642	2342.685352	21.442304
74.438499	2349.934851	21.447322
74.961700	2336.565881	21.452339
74.458316	2342.269035	21.457357
74.567845	2346.582168	21.462375
74.440577	2343.187356	21.467392
74.745954	2347.053201	21.472410
74.949221	2328.176488	21.477427
74.573409	2339.707884	21.482445
74.726469	2333.542294	21.487463
74.721392	2347.164907	21.492480
75.044510	2353.840050	21.497498
74.963422	2361.616878	21.502515
74.867262	2364.030712	21.507533
75.119596	2365.313719	21.512551
75.347329	2367.026652	21.517568
75.470974	2383.112971	21.522586
75.416215	2369.891337	21.527603
75.711764	2385.499403	21.532621
75.822846	2377.939067	21.537639
75.909906	2376.281240	21.542656
76.001640	2388.591561	21.547674
76.274845	2374.447457	21.552691
76.224576	2374.493344	21.557709
76.107987	2382.679723	21.562727
76.279909	2371.521378	21.567744
76.227974	2383.667995	21.572762
76.077886	2376.069676	21.577779
76.030925	2378.911345	21.582797
76.344618	2391.177425	21.587815
76.598800	2395.613086	21.592832
76.728638	2398.244005	21.597850
76.833003	2397.700723	21.602867
76.634725	2396.207530	21.607885
77.036280	2401.102986	21.612903
77.198400	2390.937179	21.617920
77.094938	2403.887220	21.622938
77.146987	2395.884804	21.627955
77.220891	2401.074614	21.632973
77.334599	2395.107690	21.637991
77.402001	2384.208731	21.643008
77.407697	2390.618010	21.648026
77.519763	2390.076678	21.653043
77.696495	2391.974346	21.658061
77.245677	2390.719554	21.663079
77.439383	2395.246749	21.668096
77.759395	2415.629342	21.673114
77.563504	2412.141117	21.678131
77.489735	2415.334163	21.683149
77.704174	2407.489354	21.688167
77.764056	2412.700301	21.693184
77.881747	2431.284072	21.698202
78.100099	2420.105797	21.703219
78.291646	2439.864700	21.708237
78.224066	2434.314367	21.713255
78.260857	2432.228868	21.718272
78.223430	2442.526931	21.723290
78.445988	2432.137016	21.728307
78.562237	2455.745558	21.733325
78.565642	2453.901995	21.738343
79.069280	2455.079357	21.743360
78.563874	2454.536925	21.748378
79.066542	2449.739926	21.753395
78.948566	2458.131704	21.758413
79.206084	2462.106068	21.763431
79.344624	2465.732964	21.768448
79.102357	2480.551131	21.773466
79.340686	2473.491578	21.778483
79.434988	2479.599800	21.783501
79.515709	2476.503769	21.788519
80.135896	2485.887705	21.793536
79.854260	2484.035143	21.798554
80.107015	2475.291121	21.803571
80.069419	2468.599879	21.808589
79.751778	2470.088969	21.813607
79.930794	2466.352629	21.818624
80.045239	2472.820646	21.823642
79.951989	2473.043697	21.828659
80.501122	2489.985033	21.833677
80.663699	2497.736369	21.838695
80.560999	2487.552032	21.843712
80.478204	2507.082565	21.848730
80.529578	2504.496106	21.853747
80.796481	2496.551510	21.858765
80.579008	2489.373996	21.863783
81.215064	2489.915172	21.868800
80.867277	2493.293188	21.873818
80.816674	2489.084684	21.878835
81.170190	2491.456488	21.883853
80.643049	2502.500406	21.888871
81.073087	2502.641473	21.893888
81.217786	2511.282484	21.898906
81.379123	2502.262408	21.903923
81.126849	2505.855859	21.908941
81.459218	2508.382472	21.913959
81.474562	2521.594878	21.918976
81.541357	2537.582934	21.923994
81.791211	2542.132931	21.929011
81.928950	2544.371273	21.934029
81.911173	2547.669191	21.939047
82.241172	2539.108715	21.944064
81.579190	2540.661228	21.949082
81.873283	2541.445350	21.954099
82.287076	2548.412504	21.959117
82.329889	2556.744419	21.964135
82.545411	2554.233231	21.969152
82.383954	2556.739380	21.974170
82.788413	2560.984264	21.979187
82.517464	2561.493959	21.984205
82.477712	2566.815245	21.989223
82.753377	2576.007028	21.994240
83.028767	2588.317118	21.999258
83.124315	2584.448648	22.004275
83.401443	2591.572944	22.009293
83.519631	2590.557227	22.014311
83.450308	2590.842809	22.019328
83.186541	2587.898571	22.024346
83.387114	2580.415658	22.029363
83.579456	2576.775047	22.034381
83.367821	2577.808836	22.039399
83.561283	2575.136982	22.044416
83.904243	2572.318618	22.049434
83.885742	2577.709168	22.054451
83.667219	2580.965952	22.059469
83.869411	2586.719601	22.064487
84.281913	2594.564380	22.069504
84.038093	2604.774939	22.074522
84.061475	2609.827542	22.079539
84.204770	2605.878997	22.084557
84.302244	2608.215184	22.089575
84.532819	2605.335519	22.094592
84.198911	2613.672828	22.099610
84.298861	2619.401477	22.104627
84.754939	2627.378313	22.109645
84.641995	2626.553457	22.114663
85.021836	2627.204215	22.119680
84.441717	2632.515496	22.124698
84.454439	2638.563962	22.129715
85.170526	2645.931965	22.134733
84.803488	2658.061857	22.139751
85.101961	2647.956602	22.144768
85.501106	2665.622268	22.149786
85.817569	2663.606546	22.154803
85.955563	2668.549681	22.159821
85.974128	2673.823988	22.164839
85.961382	2672.623631	22.169856
85.966276	2665.449081	22.174874
86.087305	2663.249360	22.179891
86.336269	2667.023116	22.184909
86.338356	2671.239539	22.189927
86.522716	2668.594347	22.194944
86.257947	2667.001083	22.199962
86.387231	2670.111863	22.204979
86.540358	2660.619572	22.209997
86.772537	2664.806256	22.215015
86.584028	2659.372641	22.220032
86.527227	2669.695962	22.225050
86.630325	2673.836593	22.230067
86.875541	2680.400973	22.235085
86.938798	2685.712468	22.240103
87.279089	2679.687858	22.245120
87.160500	2671.753083	22.250138
87.248376	2674.892444	22.255155
87.359199	2658.662096	22.260173
87.502041	2669.743175	22.265191
87.602306	2672.703851	22.270208
87.532306	2692.096866	22.275226
87.528497	2695.054914	22.280243
87.814613	2694.697766	22.285261
88.235593	2698.226805	22.290279
88.310460	2697.861724	22.295296
88.539196	2692.892961	22.300314
88.607239	2700.185772	22.305331
88.543759	2693.489034	22.310349
88.388694	2688.763459	22.315367
88.424532	2687.732234	22.320384
88.453773	2688.769320	22.325402
88.679427	2686.969816	22.330419
88.816188	2690.104677	22.335437
88.849874	2696.370809	22.340455
88.816002	2692.282726	22.345472
88.897918	2688.517367	22.350490
88.413058	2687.050111	22.355507
88.647802	2703.226620	22.360525
88.668136	2716.514135	22.365543
89.058092	2713.637888	22.370560
88.611565	2716.368622	22.375578
89.076543	2725.606570	22.380595
89.609186	2728.941375	22.385613
89.278637	2740.813113	22.390631
89.513681	2732.002305	22.395648
89.899977	2728.747890	22.400666
89.507490	2742.125351	22.405683
89.839740	2757.112540	22.410701
89.774315	2763.075451	22.415719
90.290061	2758.064860	22.420736
90.340061	2749.459780	22.425754
90.135343	2755.043679	22.430771
90.449557	2755.616352	22.435789
90.047124	2765.138559	22.440807
90.842195	2772.888761	22.445824
91.011111	2780.815972	22.450842
91.131761	2783.871313	22.455859
91.011299	2783.741984	22.460877
90.979417	2778.668845	22.465895
91.482951	2780.117678	22.470912
91.188723	2782.022895	22.475930
91.026182	2782.190525	22.480947
91.396274	2774.340107	22.485965
91.308825	2776.856785	22.490983
91.518446	2770.335006	22.496000
91.319365	2778.761733	22.501018
91.682472	2797.503115	22.506035
91.491551	2795.813053	22.511053
91.068018	2804.745227	22.516071
91.611591	2815.968764	22.521088
91.984464	2821.597906	22.526106
92.077348	2829.698015	22.531123
92.442013	2816.233595	22.536141
92.768107	2824.502315	22.541159
92.404716	2822.889770	22.546176
92.545247	2818.704898	22.551194
92.417655	2822.351469	22.556211
92.750080	2833.788000	22.561229
92.782012	2842.708801	22.566247
92.890655	2843.039097	22.571264
93.098079	2845.408589	22.576282
93.301357	2847.084371	22.581299
93.599961	2831.181096	22.586317
93.680938	2832.292145	22.591335
93.670633	2826.420256	22.596352
94.234426	2822.891834	22.601370
93.794583	2828.490500	22.606387
93.731059	2822.945724	22.611405
94.097846	2833.909758	22.616423
93.897870	2830.428403	22.621440
94.199231	2824.416157	22.626458
94.026291	2830.187626	22.631475
94.515815	2816.031379	22.636493
94.434224	2822.874258	22.641511
94.529892	2822.414387	22.646528
94.918753	2829.666457	22.651546
94.569655	2823.421565	22.656563
94.586251	2821.298154	22.661581
94.723569	2830.814736	22.666599
94.535803	2820.883406	22.671616
94.641081	2822.811252	22.676634
94.588171	2842.249095	22.681651
94.771842	2845.275636	22.686669
94.874295	2844.937792	22.691687
95.065280	2847.884284	22.696704
95.010784	2844.607378	22.701722
94.713622	2863.493305	22.706739
94.739152	2871.098997	22.711757
95.072927	2879.631658	22.716775
95.416068	2892.537330	22.721792
95.708300	2894.517955	22.726810
95.420745	2903.387842	22.731827
95.718059	2900.125245	22.736845
95.881215	2911.023387	22.741863
95.957865	2912.447583	22.746880
96.497050	2910.011885	22.751898
96.294998	2918.164554	22.756915
96.723830	2922.500392	22.761933
96.550702	2922.653902	22.766951
96.250151	2919.431313	22.771968
96.722633	2919.259585	22.776986
97.004058	2933.872986	22.782003
97.085052	2932.812578	22.787021
97.173980	2947.547678	22.792039
97.331279	2940.639511	22.797056
97.495038	2935.573551	22.802074
97.431424	2942.401034	22.807091
97.825883	2928.199626	22.812109
97.943137	2934.847272	22.817127
97.429023	2931.512956	22.822144
97.634378	2926.689821	22.827162
97.573162	2938.349057	22.832179
97.778479	2934.886245	22.837197
98.086660	2942.416121	22.842215
97.880689	2949.635185	22.847232
97.836640	2956.696323	22.852250
97.626975	2967.024827	22.857267
97.937629	2974.099836	22.862285
98.312845	2977.421479	22.867303
98.472993	2984.927222	22.872320
98.357144	2978.342737	22.877338
98.526116	2996.013228	22.882355
99.097416	2989.693515	22.887373
98.843709	2998.460304	22.892391
98.924437	3004.993762	22.897408
99.767028	2998.218080	22.902426
99.508613	3004.634237	22.907443
99.632695	3003.617574	22.912461
99.715563	2996.673704	22.917479
99.371007	2997.800933	22.922496
99.691954	2994.351556	22.927514
100.067752	3020.262079	22.932531
100.134220	3011.458609	22.937549
99.777940	3023.624934	22.942567
100.110920	3018.147382	22.947584
100.416872	3015.593557	22.952602
100.288181	3026.777366	22.957619
100.264905	3014.755997	22.962637
100.494996	3024.649517	22.967655
100.661555	3030.888635	22.972672
100.910015	3027.794636	22.977690
100.963695	3046.493226	22.982707
101.189436	3046.262312	22.987725
101.229567	3050.340302	22.992743
100.790820	3048.152486	22.997760
101.332083	3042.869542	23.002778
101.118325	3044.260340	23.007795
101.018836	3047.315498	23.012813
101.157022	3050.185077	23.017831
100.885464	3062.129845	23.022848
101.470864	3063.351253	23.027866
101.231881	3069.622359	23.032883
101.735822	3072.665043	23.037901
101.704549	3087.763118	23.042919
102.077045	3085.628104	23.047936
102.194385	3087.187968	23.052954
102.213615	3087.497558	23.057971
102.421320	3074.562533	23.062989
102.288064	3083.105337	23.068007
102.427322	3100.521777	23.073024
102.745193	3106.229064	23.078042
102.600971	3120.871428	23.083059
102.751753	3109.463440	23.088077
102.484539	3110.575402	23.093095
102.805605	3115.884508	23.098112
103.266329	3123.857683	23.103130
103.384352	3119.988734	23.108147
103.528899	3124.473316	23.113165
103.740883	3126.302416	23.118183
103.449517	3126.938417	23.123200
103.603630	3120.207429	23.128218
104.269864	3137.351969	23.133235
104.291884	3131.869445	23.138253
103.947332	3135.111354	23.143271
104.087569	3144.794925	23.148288
104.242322	3139.566195	23.153306
104.355974	3145.081397	23.158323
104.569802	3148.358920	23.163341
104.956655	3139.129602	23.168359
104.515291	3146.865370	23.173376
104.948958	3139.213145	23.178394
104.740328	3146.385360	23.183411
105.013154	3161.533697	23.188429
105.089065	3163.371494	23.193447
105.018745	3169.486805	23.198464
105.179408	3159.286075	23.203482
105.438082	3161.234113	23.208499
105.132118	3159.824007	23.213517
105.609168	3177.730471	23.218535
105.753178	3185.005265	23.223552
106.039100	3179.525568	23.228570
105.996917	3195.903718	23.233587
106.081812	3190.685918	23.238605
106.104836	3186.405747	23.243623
106.084057	3198.699532	23.248640
106.197520	3209.088018	23.253658
106.401182	3225.642302	23.258675
106.483657	3217.776785	23.263693
106.665489	3215.731597	23.268711
106.574093	3211.579814	23.273728
106.628217	3218.054393	23.278746
106.250825	3232.626067	23.283763
106.684850	3234.963265	23.288781
107.137419	3245.999331	23.293799
107.305514	3265.011629	23.298816
107.825496	3256.544144	23.303834
107.495412	3256.725402	23.308851
107.599640	3256.702898	23.313869
108.030857	3262.951134	23.318887
107.730901	3257.004547	23.323904
108.062651	3261.074772	23.328922
107.939003	3257.881219	23.333939
108.150084	3262.169193	23.338957
108.459501	3272.609078	23.343975
108.476176	3284.663491	23.348992
108.588418	3271.822186	23.354010
108.802873	3276.851355	23.359027
108.630833	3280.583887	23.364045
108.856056	3277.768080	23.369063
108.413761	3284.566645	23.374080
108.915007	3286.833350	23.379098
109.264259	3290.348495	23.384115
109.147868	3300.668888	23.389133
109.375630	3299.837966	23.394151
109.359339	3313.210565	23.399168
109.514290	3303.957527	23.404186
109.784161	3303.634477	23.409203
109.327988	3306.306840	23.414221
110.048568	3308.510779	23.419239
110.136456	3325.338950	23.424256
110.270651	3319.513700	23.429274
110.674677	3325.384310	23.434291
110.211952	3326.820447	23.439309
110.550825	3315.370237	23.444327
110.355777	3325.747155	23.449344
110.213749	3315.666354	23.454362
110.359684	3331.077745	23.459379
110.259788	3336.648556	23.464397
111.071925	3341.883949	23.469415
110.892939	3350.304638	23.474432
111.061580	3369.301179	23.479450
111.348760	3370.307362	23.484467
111.546518	3369.156041	23.489485
112.205476	3369.242317	23.494503
111.709633	3365.662022	23.499520
111.946253	3369.586206	23.504538
111.793672	3367.129421	23.509555
111.697377	3363.997846	23.514573
112.311453	3374.472122	23.519591
112.072871	3388.258356	23.524608
112.440746	3390.271374	23.529626
111.990609	3385.351968	23.534643
112.306478	3390.387373	23.539661
112.952072	3400.948259	23.544679
112.774054	3405.717012	23.549696
112.911341	3410.187022	23.554714
112.847276	3414.268793	23.559731
113.087060	3409.515887	23.564749
113.486960	3400.969305	23.569767
112.912578	3413.678221	23.574784
113.266246	3421.213797	23.579802
113.499111	3427.944514	23.584819
113.449602	3433.295990	23.589837
113.726197	3432.586819	23.594855
113.958789	3444.358165	23.599872
113.949987	3444.678466	23.604890
114.237713	3454.872509	23.609907
114.402489	3451.223418	23.614925
114.588624	3449.786691	23.619943
114.431783	3458.200804	23.624960
114.659864	3453.320312	23.629978
114.901545	3443.706423	23.634995
115.412129	3467.339732	23.640013
115.203906	3465.759630	23.645031
115.296372	3468.301873	23.650048
115.484508	3471.637137	23.655066
115.633692	3473.286735	23.660083
115.421030	3477.802118	23.665101
115.905364	3467.285378	23.670119
115.847437	3472.783374	23.675136
116.267627	3468.172628	23.680154
116.226454	3464.767271	23.685171
115.832946	3473.663505	23.690189
116.031346	3470.166957	23.695207
116.171879	3467.080323	23.700224
116.116702	3471.356405	23.705242
116.034533	3473.774507	23.710259
116.452800	3486.277456	23.715277
116.410733	3477.171979	23.720295
116.654039	3486.776460	23.725312
116.609355	3490.823650	23.730330
117.037323	3489.058654	23.735347
116.993766	3516.739989	23.740365
117.319956	3511.206540	23.745383
117.124256	3514.958608	23.750400
117.192957	3517.962245	23.755418
117.275855	3519.742170	23.760435
117.165321	3532.460563	23.765453
118.000545	3536.941199	23.770471
117.881704	3535.034613	23.775488
117.917636	3535.108029	23.780506
118.295672	3525.592674	23.785523
117.970695	3537.561904	23.790541
118.429303	3549.196908	23.795559
118.641543	3557.821529	23.800576
118.468749	3554.698749	23.805594
118.960898	3555.527641	23.810611
118.568771	3558.868610	23.815629
118.802587	3572.483129	23.820647
119.179961	3571.998043	23.825664
119.081807	3574.074626	23.830682
119.416774	3574.530450	23.835699
119.291937	3579.051037	23.840717
119.718256	3590.867879	23.845735
119.696613	3599.538631	23.850752
119.601246	3603.745289	23.855770
120.041494	3593.481575	23.860787
119.862247	3595.561396	23.865805
120.152992	3605.297387	23.870823
120.424272	3618.233776	23.875840
120.546792	3615.232004	23.880858
120.809841	3618.527152	23.885875
120.878886	3620.416573	23.890893
120.772831	3609.837587	23.895911
121.066696	3613.550852	23.900928
121.094991	3618.202118	23.905946
121.351914	3623.265762	23.910963
121.388401	3642.557895	23.915981
121.452344	3640.742601	23.920999
121.719056	3637.784518	23.926016
121.682762	3640.239643	23.931034
121.964230	3641.574994	23.936051
121.688594	3643.003938	23.941069
121.862948	3644.176161	23.946087
122.212805	3650.380465	23.951104
121.911234	3658.744750	23.956122
122.282718	3652.721245	23.961139
122.118694	3670.353034	23.966157
122.294026	3677.698872	23.971175
122.577643	3691.428775	23.976192
122.664736	3692.100190	23.981210
123.128332	3698.703327	23.986227
123.218216	3704.276082	23.991245
123.429465	3706.550400	23.996263
123.773797	3706.906914	24.001280
123.786849	3707.381613	24.006298
124.167861	3705.630266	24.011315
123.938231	3711.540307	24.016333
123.889876	3699.601319	24.021351
124.182309	3704.261726	24.026368
123.899145	3704.050564	24.031386
124.450120	3706.006526	24.036403
124.010130	3712.189404	24.041421
124.006094	3716.242901	24.046439
124.837009	3721.484935	24.051456
124.446190	3728.603859	24.056474
124.859590	3714.929132	24.061491
124.818002	3728.186061	24.066509
125.185826	3737.193560	24.071527
125.095039	3736.728159	24.076544
125.090398	3740.279899	24.081562
125.464981	3735.344816	24.086579
125.201349	3732.226768	24.091597
125.418961	3738.252972	24.096615
125.116363	3753.368860	24.101632
125.578086	3759.451518	24.106650
125.984722	3761.663668	24.111667
125.914809	3772.513626	24.116685
126.206103	3777.104790	24.121703
126.317794	3770.307612	24.126720
126.619179	3782.747015	24.131738
126.639635	3796.016368	24.136755
126.817378	3803.472352	24.141773
126.999688	3806.713901	24.146791
126.908810	3801.507682	24.151808
127.157885	3806.449510	24.156826
127.441007	3822.894048	24.161843
127.491360	3821.945705	24.166861
127.553390	3825.032503	24.171879
127.865793	3820.148171	24.176896
127.801927	3825.322101	24.181914
128.110395	3813.115660	24.186931
127.648085	3829.901090	24.191949
128.404755	3834.738152	24.196967
128.549087	3837.123973	24.201984
128.427274	3845.213986	24.207002
128.674086	3843.130140	24.212019
128.718495	3848.293426	24.217037
128.662835	3854.599208	24.222055
129.065509	3860.255574	24.227072
128.899381	3863.040393	24.232090
129.012286	3862.375790	24.237107
129.365157	3887.827169	24.242125
129.738117	3886.582085	24.247143
129.509961	3891.671299	24.252160
129.762991	3893.203663	24.257178
129.796247	3890.503059	24.262195
129.982570	3903.055262	24.267213
130.462313	3907.998856	24.272231
131.033801	3913.900239	24.277248
130.781371	3912.756288	24.282266
130.974164	3917.508113	24.287283
130.834894	3910.866985	24.292301
131.010561	3913.708737	24.297319
131.369705	3912.926645	24.302336
130.829970	3911.868737	24.307354
131.352203	3908.652789	24.312371
131.300472	3917.369440	24.317389
131.571962	3931.843172	24.322407
131.718469	3922.180814	24.327424
131.618091	3926.767095	24.332442
131.776389	3924.548759	24.337459
131.989554	3932.636832	24.342477
132.085553	3952.522838	24.347495
132.293178	3944.088190	24.352512
132.383709	3963.997160	24.357530
132.803576	3948.121253	24.362547
132.394407	3958.528922	24.367565
132.628526	3977.777825	24.372583
132.949812	3976.540830	24.377600
132.890207	3978.753456	24.382618
132.850649	3970.398555	24.387635
132.964554	3978.653706	24.392653
133.185606	3998.359195	24.397671
133.435441	4000.299242	24.402688
133.226519	3998.365686	24.407706
133.993120	4006.067232	24.412723
133.547703	4012.146901	24.417741
133.888087	4020.221395	24.422759
134.114934	4023.632764	24.427776
134.213466	4023.475428	24.432794
134.356727	4033.575646	24.437811
134.344113	4045.584652	24.442829
134.434239	4045.333941	24.447847
135.107463	4047.217131	24.452864
135.093711	4060.217432	24.457882
134.803000	4068.435009	24.462899
135.370802	4075.315504	24.467917
135.426998	4079.804697	24.472935
135.616391	4070.394366	24.477952
135.379294	4085.219349	24.482970
135.819550	4086.138464	24.487987
135.471389	4094.560750	24.493005
135.939797	4093.957230	24.498023
136.267585	4105.834037	24.503040
136.100365	4112.501434	24.508058
136.799082	4111.555661	24.513075
136.547989	4115.212370	24.518093
136.631008	4127.039159	24.523111
136.983760	4121.302511	24.528128
137.266736	4129.723783	24.533146
137.792011	4135.010668	24.538163
137.712965	4128.596755	24.543181
137.689915	4135.156351	24.548199
138.029896	4124.150511	24.553216
137.831123	4128.442932	24.558234
138.091113	4134.266933	24.563251
138.355394	4144.774367	24.568269
138.194441	4162.870146	24.573287
138.546564	4154.974603	24.578304
138.508113	4151.249893	24.583322
138.640811	4152.952639	24.588339
138.940485	4149.383279	24.593357
138.888051	4165.921733	24.598375
139.401894	4168.189737	24.603392
139.198399	4175.288956	24.608410
139.710948	4172.655259	24.613427
139.401113	4169.462305	24.618445
139.025227	4174.262258	24.623463
139.816761	4178.364823	24.628480
139.582617	4191.339773	24.633498
139.985323	4195.692642	24.638515
140.254990	4196.076648	24.643533
140.241327	4204.190911	24.648551
140.268413	4215.117473	24.653568
140.214594	4222.442617	24.658586
140.550808	4218.125762	24.663603
140.508493	4232.399540	24.668621
140.938900	4247.476756	24.673639
141.179257	4239.933267	24.678656
141.229212	4246.636131	24.683674
141.274742	4253.200808	24.688691
141.686424	4259.723905	24.693709
141.527795	4267.390600	24.698727
141.837417	4267.042370	24.703744
142.161889	4269.952402	24.708762
141.842833	4274.064846	24.713779
142.135458	4285.031916	24.718797
142.441356	4294.702777	24.723815
142.620307	4286.932157	24.728832
142.407419	4296.333931	24.733850
142.575015	4295.865912	24.738867
143.263540	4302.939063	24.743885
143.376852	4309.824567	24.748903
143.606377	4308.756592	24.753920
143.609349	4311.846412	24.758938
143.539571	4307.649957	24.763955
143.525086	4304.353892	24.768973
143.461726	4307.005890	24.773991
143.790561	4314.034390	24.779008
143.482534	4328.182581	24.784026
143.935895	4327.966497	24.789043
144.287791	4344.081935	24.794061
144.244876	4346.503472	24.799079
144.470374	4342.150273	24.804096
144.576689	4348.907474	24.809114
144.610474	4365.268467	24.814131
145.040008	4369.913882	24.819149
145.187024	4375.301132	24.824167
145.289111	4382.169483	24.829184
145.847553	4400.127542	24.834202
145.480757	4398.919408	24.839219
146.039083	4400.634407	24.844237
146.015877	4399.801722	24.849255
146.155846	4400.026134	24.854272
146.362103	4413.187920	24.859290
146.478950	4423.065229	24.864307
146.763041	4423.292314	24.869325
146.741780	4423.706122	24.874343
146.743277	4424.182649	24.879360
146.991403	4422.085907	24.884378
146.880017	4430.698518	24.889395
147.389532	4442.947946	24.894413
147.307063	4442.086666	24.899431
147.587307	4438.027887	24.904448
147.601104	4460.127378	24.909466
147.841313	4458.246511	24.914483
147.849500	4463.532436	24.919501
148.054222	4475.062617	24.924519
148.246966	4482.728014	24.929536
148.257748	4489.244561	24.934554
148.505896	4490.316898	24.939571
148.959741	4501.353536	24.944589
148.777741	4517.445452	24.949607
149.207500	4507.747876	24.954624
148.953955	4519.700248	24.959642
149.250554	4516.961451	24.964659
149.743006	4525.473193	24.969677
149.777615	4519.429581	24.974695
149.709259	4524.367678	24.979712
150.057198	4535.578752	24.984730
150.186918	4545.394138	24.989747
150.427183	4550.255483	24.994765
150.360364	4555.755200	24.999783
150.820341	4548.331845	25.004800
150.398817	4559.833932	25.009818
150.675720	4575.734059	25.014835
151.120692	4579.490138	25.019853
150.963336	4579.028830	25.024871
151.100842	4576.482242	25.029888
151.102396	4592.466555	25.034906
151.350512	4609.876864	25.039923
151.546812	4607.655648	25.044941
151.798798	4625.886053	25.049959
152.107689	4620.828452	25.054976
152.127354	4623.915710	25.059994
151.915846	4623.475511	25.065011
152.363997	4632.221511	25.070029
152.593539	4648.047053	25.075047
152.415678	4657.351987	25.080064
152.811660	4664.720476	25.085082
152.887539	4679.714708	25.090099
153.177556	4681.806360	25.095117
153.102004	4674.384783	25.100135
153.488296	4686.584239	25.105152
153.892596	4696.583958	25.110170
153.680362	4704.009870	25.115187
154.166613	4706.755742	25.120205
154.205379	4707.381107	25.125223
154.249592	4709.523896	25.130240
154.673597	4720.562187	25.135258
154.844215	4735.257538	25.140275
154.728808	4718.517868	25.145293
154.903684	4726.195637	25.150311
155.379645	4730.909628	25.155328
155.389711	4735.219977	25.160346
155.408839	4748.584930	25.165363
155.897376	4734.998677	25.170381
155.774542	4744.882145	25.175399
155.729180	4744.699999	25.180416
156.108940	4755.423279	25.185434
156.114587	4767.502502	25.190451
156.554703	4766.657187	25.195469
156.414372	4771.300445	25.200487
156.829975	4777.109745	25.205504
157.013205	4789.483126	25.210522
156.643230	4799.727307	25.215539
157.098941	4793.159938	25.220557
157.092982	4807.693620	25.225575
157.051312	4812.113101	25.230592
157.363460	4819.175978	25.235610
157.252066	4823.511689	25.240627
157.843757	4825.975913	25.245645
158.096764	4832.123200	25.250663
158.350636	4841.890887	25.255680
158.486322	4852.838697	25.260698
158.355839	4863.679856	25.265715
158.537256	4861.063219	25.270733
158.458328	4875.583134	25.275751
158.670885	4885.802389	25.280768
158.845278	4886.535930	25.285786
159.323425	4912.578334	25.290803
159.480536	4908.712352	25.295821
159.587512	4906.246258	25.300839
159.624380	4923.295396	25.305856
160.215015	4923.392395	25.310874
160.240682	4934.808876	25.315891
160.591296	4927.440379	25.320909
160.656499	4943.891668	25.325927
160.737650	4946.423266	25.330944
161.523363	4953.784478	25.335962
161.170495	4966.178835	25.340979
161.469395	4959.089891	25.345997
161.544127	4957.124419	25.351015
161.627177	4950.722699	25.356032
161.584418	4950.896833	25.361050
161.952177	4974.731257	25.366067
162.132256	4978.863514	25.371085
162.381600	4975.655413	25.376103
162.199957	4977.098142	25.381120
162.061594	4976.084608	25.386138
162.202434	4995.778496	25.391155
162.907520	5005.611315	25.396173
162.472750	5000.108248	25.401191
162.316053	5014.148035	25.406208
163.233938	5025.336411	25.411226
163.272548	5029.273041	25.416243
163.163148	5030.256224	25.421261
163.470987	5044.245355	25.426279
163.150310	5049.819713	25.431296
163.673464	5063.128030	25.436314
163.810150	5072.724807	25.441331
164.307205	5071.678009	25.446349
164.269685	5086.412565	25.451367
164.629486	5094.070988	25.456384
165.068203	5098.844573	25.461402
165.201461	5096.254387	25.466419
165.315862	5100.772593	25.471437
165.604105	5102.170126	25.476455
165.671328	5130.205885	25.481472
165.790650	5109.688539	25.486490
165.588968	5118.672313	25.491507
166.107828	5123.247112	25.496525
166.370419	5130.794517	25.501543
166.242609	5139.915088	25.506560
166.675038	5134.800114	25.511578
166.437262	5145.131100	25.516595
166.662728	5157.801147	25.521613
166.943350	5159.891170	25.526631
167.012567	5168.747302	25.531648
167.537000	5163.681038	25.536666
167.308506	5176.419059	25.541683
167.641286	5176.922622	25.546701
168.039651	5181.516312	25.551719
168.016924	5183.142495	25.556736
168.282053	5191.825899	25.561754
168.544564	5205.102553	25.566771
168.646989	5193.770278	25.571789
168.728717	5190.231705	25.576807
168.824910	5205.488342	25.581824
169.381599	5214.678484	25.586842
169.167429	5219.952114	25.591859
169.354761	5215.585749	25.596877
169.570114	5228.371066	25.601895
169.909636	5248.144582	25.606912
170.043041	5249.118148	25.611930
170.245480	5247.069506	25.616947
170.407657	5238.654007	25.621965
170.582709	5242.155794	25.626983
170.646286	5257.370235	25.632000
170.839578	5262.917800	25.637018
170.707095	5276.029112	25.642035
170.982825	5275.929234	25.647053
171.750853	5286.642508	25.652071
171.450444	5289.748456	25.657088
171.755790	5286.064351	25.662106
171.971677	5294.149451	25.667123
171.757215	5289.729220	25.672141
172.108906	5308.285602	25.677159
172.010096	5315.687680	25.682176
172.305004	5312.762791	25.687194
172.494507	5330.170347	25.692212
172.431923	5336.389343	25.697229
172.870766	5346.724924	25.702247
172.845629	5354.027090	25.707264
173.258639	5356.961309	25.712282
173.252783	5360.371508	25.717300
173.932193	5390.391970	25.722317
174.054396	5391.944960	25.727335
174.060235	5390.372186	25.732352
174.357461	5385.814950	25.737370
174.534015	5392.312162	25.742388
174.757170	5387.794939	25.747405
174.688259	5399.387515	25.752423
174.871915	5412.228434	25.757440
175.025502	5403.236543	25.762458
175.008935	5413.302593	25.767476
175.023196	5411.580136	25.772493
175.264282	5417.858911	25.777511
175.555419	5430.190571	25.782528
175.924401	5430.874710	25.787546
175.972663	5448.686459	25.792564
176.392033	5451.111479	25.797581
176.483663	5453.458422	25.802599
176.357667	5458.298476	25.807616
176.709264	5471.495079	25.812634
176.937922	5475.023235	25.817652
176.757999	5483.912237	25.822669
177.287840	5495.265868	25.827687
177.137315	5511.492621	25.832704
177.461309	5506.915378	25.837722
177.593253	5518.097766	25.842740
177.665161	5527.787004	25.847757
177.921385	5535.042008	25.852775
178.163443	5547.302520	25.857792
178.808599	5558.328773	25.862810
178.588038	5552.820388	25.867828
178.972101	5562.946866	25.872845
179.221233	5574.117243	25.877863
179.181706	5577.879990	25.882880
179.461482	5574.850104	25.887898
179.648163	5594.063960	25.892916
179.728858	5605.014524	25.897933
180.087540	5601.056842	25.902951
179.865007	5614.043610	25.907968
180.594661	5621.956826	25.912986
180.783715	5628.294332	25.918004
180.587272	5634.474422	25.923021
180.969529	5630.456220	25.928039
181.119406	5656.718422	25.933056
181.036522	5646.813301	25.938074
181.250796	5643.591639	25.943092
181.280066	5655.086923	25.948109
182.192680	5667.365576	25.953127
181.856174	5678.637234	25.958144
182.227746	5680.372150	25.963162
182.281846	5687.794616	25.968180
182.529205	5701.878959	25.973197
182.917862	5702.620004	25.978215
182.903931	5715.975063	25.983232
182.761524	5715.956473	25.988250
183.298044	5729.181113	25.993268
183.171138	5744.179581	25.998285
183.629404	5736.692882	26.003303
183.724578	5750.580136	26.008320
184.409476	5759.425332	26.013338
184.726979	5767.854585	26.018356
184.695897	5768.850792	26.023373
184.601206	5763.935021	26.028391
184.835613	5773.535799	26.033408
185.084370	5782.903895	26.038426
185.101609	5793.634076	26.043444
185.388434	5798.567380	26.048461
185.552914	5797.556863	26.053479
185.622564	5820.327942	26.058496
186.017850	5817.027385	26.063514
186.309216	5823.371028	26.068532
186.272717	5830.921387	26.073549
186.623888	5838.584635	26.078567
186.262286	5847.593819	26.083584
186.753615	5846.128037	26.088602
186.970251	5841.832693	26.093620
186.941922	5857.229338	26.098637
187.393652	5853.629516	26.103655
187.515590	5868.358662	26.108672
187.506472	5873.584572	26.113690
188.138409	5875.578605	26.118708
188.160460	5897.233450	26.123725
188.160218	5893.268801	26.128743
187.862111	5896.428154	26.133760
188.282843	5912.448971	26.138778
188.693470	5923.212301	26.143796
188.329596	5926.912290	26.148813
188.647751	5935.335206	26.153831
188.291709	5947.127790	26.158848
188.827749	5957.278030	26.163866
189.268072	5973.718832	26.168884
189.609800	5996.428566	26.173901
189.573618	6005.481548	26.178919
190.405043	6014.338638	26.183936
190.327750	6021.709220	26.188954
190.787699	6034.437845	26.193972
190.820275	6053.022882	26.198989
191.171182	6052.241997	26.204007
190.839874	6059.292520	26.209024
191.287078	6072.256767	26.214042
191.430763	6075.602635	26.219060
191.259794	6102.515521	26.224077
191.571568	6099.950892	26.229095
192.284726	6117.829594	26.234112
192.566309	6120.427816	26.239130
192.422566	6124.566870	26.244148
192.589747	6139.570097	26.249165
192.963245	6144.985528	26.254183
193.416561	6149.586641	26.259200
193.395059	6153.251979	26.264218
193.637458	6168.937933	26.269236
193.614176	6172.953954	26.274253
193.876161	6186.711233	26.279271
194.233952	6199.143458	26.284288
194.153180	6197.416875	26.289306
194.688886	6208.908931	26.294324
194.708635	6223.610177	26.299341
195.006118	6213.894545	26.304359
195.367860	6223.352498	26.309376
195.466464	6247.514862	26.314394
196.362585	6238.762951	26.319412
195.952502	6248.591215	26.324429
196.403546	6240.840276	26.329447
196.349721	6249.861419	26.334464
196.470741	6263.653467	26.339482
196.914896	6261.765724	26.344500
196.344525	6265.315037	26.349517
196.822429	6274.909500	26.354535
196.936075	6287.398974	26.359552
197.386951	6286.624517	26.364570
197.552970	6308.885493	26.369588
198.043319	6310.292499	26.374605
198.072447	6321.649326	26.379623
198.256451	6330.200771	26.384640
198.308371	6331.505996	26.389658
198.604909	6339.743079	26.394676
198.498526	6340.217616	26.399693
198.929383	6347.167790	26.404711
199.185249	6356.696063	26.409728
199.173191	6359.239304	26.414746
199.503182	6364.147060	26.419764
199.868118	6382.860302	26.424781
200.087744	6380.534202	26.429799
199.781304	6375.064276	26.434816
200.214687	6382.961104	26.439834
200.354685	6383.419143	26.444852
200.531268	6402.752232	26.449869
201.119348	6407.354397	26.454887
200.738984	6408.882032	26.459904
200.899982	6424.066399	26.464922
201.216744	6430.393648	26.469940
201.402422	6450.157844	26.474957
201.665047	6455.808557	26.479975
202.129748	6458.229770	26.484992
202.633283	6473.960310	26.490010
202.433671	6469.951006	26.495028
202.588547	6492.030855	26.500045
202.803805	6490.955524	26.505063
203.194231	6494.875236	26.510080
203.430546	6508.197982	26.515098
203.858044	6502.837173	26.520116
203.341451	6514.165966	26.525133
204.123916	6520.240352	26.530151
204.327511	6525.155325	26.535168
204.565958	6528.439079	26.540186
205.080651	6536.421098	26.545204
204.943270	6547.510566	26.550221
204.966433	6544.040886	26.555239
205.208421	6545.594152	26.560256
204.959723	6572.538845	26.565274
205.316179	6567.346989	26.570292
205.533897	6587.687170	26.575309
205.870477	6587.786107	26.580327
206.079613	6591.898396	26.585344
206.267740	6609.345269	26.590362
206.423335	6616.935309	26.595380
206.942058	6631.852300	26.600397
207.108605	6637.660178	26.605415
207.200261	6648.761179	26.610432
206.992877	6651.297177	26.615450
207.485396	6661.255748	26.620468
207.692627	6668.326313	26.625485
207.931324	6686.099961	26.630503
208.389172	6686.845996	26.635520
208.175142	6694.535012	26.640538
208.555842	6710.010353	26.645556
209.022743	6721.980726	26.650573
208.782672	6715.177580	26.655591
209.436002	6735.534918	26.660608
209.497159	6741.918102	26.665626
209.982371	6744.670769	26.670644
210.144420	6755.413552	26.675661
210.207297	6761.569180	26.680679
210.575066	6752.394704	26.685696
210.615759	6769.738552	26.690714
211.005041	6774.053112	26.695732
211.094431	6787.121275	26.700749
211.203031	6783.603440	26.705767
211.554420	6798.417351	26.710784
211.765881	6803.242774	26.715802
211.991747	6809.657003	26.720820
211.775104	6831.340874	26.725837
212.193951	6818.916258	26.730855
212.447468	6825.686044	26.735872
212.557180	6848.202732	26.740890
212.919568	6859.431919	26.745908
213.054463	6866.476009	26.750925
213.420832	6873.171309	26.755943
213.811591	6886.530117	26.760960
214.134453	6887.979193	26.765978
213.998661	6877.895438	26.770996
214.147897	6888.583483	26.776013
214.304255	6907.932902	26.781031
214.750105	6898.026352	26.786048
214.989026	6902.313987	26.791066
215.055609	6904.270431	26.796084
215.195052	6918.063243	26.801101
215.484016	6925.660930	26.806119
215.560845	6926.820236	26.811136
215.422621	6943.219956	26.816154
216.172387	6946.931943	26.821172
215.949590	6955.225407	26.826189
216.245220	6973.040925	26.831207
216.242134	6972.195499	26.836224
216.427665	6999.991449	26.841242
216.994994	7001.667417	26.846260
216.844067	7017.996585	26.851277
217.512128	7024.360557	26.856295
218.005925	7028.822964	26.861312
217.851515	7046.551211	26.866330
218.285479	7048.443804	26.871348
218.555056	7061.856450	26.876365
219.066021	7069.021648	26.881383
219.083849	7079.010615	26.886400
218.898113	7082.323038	26.891418
219.124463	7092.494015	26.896436
219.322898	7099.840776	26.901453
219.329138	7113.310497	26.906471
219.747586	7115.843225	26.911488
219.985413	7141.598142	26.916506
220.538306	7143.693099	26.921524
220.179218	7146.691742	26.926541
220.347861	7165.458634	26.931559
221.178544	7181.631014	26.936576
221.304777	7189.099613	26.941594
221.677389	7193.830443	26.946612
221.798193	7203.380317	26.951629
222.060369	7220.686737	26.956647
222.155246	7223.004987	26.961664
222.350176	7242.721234	26.966682
222.731207	7246.030135	26.971700
222.916723	7247.753313	26.976717
223.038768	7267.667264	26.981735
223.319614	7262.837479	26.986752
223.379698	7275.872697	26.991770
223.516928	7294.104803	26.996788
224.050081	7301.875908	27.001805
224.000731	7319.057591	27.006823
224.266913	7315.729642	27.011840
224.874253	7344.896448	27.016858
224.860735	7353.997056	27.021876
225.209355	7356.629152	27.026893
225.220894	7367.635802	27.031911
225.647910	7371.471049	27.036928
225.458167	7390.704718	27.041946
226.029115	7404.035676	27.046964
226.409163	7406.328218	27.051981
226.272842	7421.048558	27.056999
226.685602	7424.712416	27.062016
226.764836	7439.910432	27.067034
226.959826	7453.521310	27.072052
227.039321	7457.493098	27.077069
227.460765	7482.755653	27.082087
227.770427	7484.532015	27.087104
227.842720	7491.349379	27.092122
228.332818	7508.399375	27.097140
228.544534	7502.904763	27.102157
228.461640	7518.238737	27.107175
228.978154	7526.347185	27.112192
228.905689	7531.097315	27.117210
229.172722	7551.127767	27.122228
229.677942	7555.496961	27.127245
229.897995	7569.511251	27.132263
230.410255	7572.862795	27.137280
230.381280	7586.543584	27.142298
230.438141	7587.402988	27.147316
230.562663	7600.873479	27.152333
230.510922	7618.339945	27.157351
230.832883	7618.864221	27.162368
231.111894	7641.276432	27.167386
231.645649	7649.385391	27.172404
231.799894	7663.356392	27.177421
231.993214	7661.479394	27.182439
232.205282	7680.978749	27.187456
232.452062	7694.853195	27.192474
232.835049	7704.782140	27.197492
233.130915	7719.823327	27.202509
233.066407	7730.065479	27.207527
233.321626	7737.555136	27.212544
233.491025	7751.195500	27.217562
233.822531	7758.329099	27.222580
234.178291	7777.544013	27.227597
233.922895	7787.197322	27.232615
234.779742	7794.835846	27.237632
234.651829	7813.495160	27.242650
234.986649	7822.355165	27.247668
235.435535	7830.022886	27.252685
235.686585	7857.629915	27.257703
235.974767	7855.292893	27.262720
236.315095	7869.200173	27.267738
236.070255	7878.286764	27.272756
236.436463	7885.392877	27.277773
236.847935	7901.738906	27.282791
237.075318	7902.609497	27.287808
237.204567	7921.193907	27.292826
237.591096	7919.135077	27.297844
237.991197	7930.182218	27.302861
238.238560	7936.482976	27.307879
238.525289	7946.692325	27.312896
239.064045	7960.685399	27.317914
238.833650	7966.783190	27.322932
239.083408	7966.368512	27.327949
239.619576	7987.039202	27.332967
240.025069	7992.661696	27.337984
240.076873	7996.148593	27.343002
240.212787	7997.554434	27.348020
240.364190	8008.659524	27.353037
240.490082	8018.120626	27.358055
241.049717	8031.472755	27.363072
241.766847	8027.221627	27.368090
242.272459	8021.879717	27.373108
242.596885	8025.219729	27.378125
242.438724	8022.580074	27.383143
242.547046	8019.437740	27.388160
242.748772	8021.537301	27.393178
242.760791	8018.097504	27.398196
243.115552	8027.355432	27.403213
243.128179	8039.186308	27.408231
243.746042	8040.150433	27.413248
243.304154	8043.162189	27.418266
243.516112	8057.771649	27.423284
244.101785	8062.740837	27.428301
243.833047	8078.284342	27.433319
244.091013	8090.370427	27.438336
244.546121	8103.192808	27.443354
244.612811	8112.237025	27.448372
244.898401	8121.960458	27.453389
244.946186	8137.340773	27.458407
245.195424	8138.839370	27.463424
245.283561	8146.311170	27.468442
245.733026	8163.788034	27.473460
246.281812	8185.593527	27.478477
246.026228	8200.086916	27.483495
246.472016	8206.508225	27.488512
246.750219	8225.659985	27.493530
246.897507	8235.585099	27.498548
247.116574	8242.834371	27.503565
247.307715	8257.548278	27.508583
247.660318	8277.562958	27.513600
247.898302	8284.020005	27.518618
247.943503	8290.437797	27.523636
248.426020	8302.201545	27.528653
248.401369	8321.359806	27.533671
249.114470	8331.429961	27.538688
249.293642	8345.034504	27.543706
249.568085	8358.011650	27.548724
250.139891	8374.696053	27.553741
250.458381	8385.011169	27.558759
250.578090	8401.283376	27.563776
251.088717	8402.873649	27.568794
251.332702	8403.760607	27.573812
251.342487	8412.712857	27.578829
251.291866	8427.714187	27.583847
252.014995	8443.014218	27.588864
252.334697	8446.415033	27.593882
252.310813	8449.907558	27.598900
252.816994	8460.183842	27.603917
252.645597	8466.013668	27.608935
253.355350	8468.251539	27.613952
253.545078	8481.523029	27.618970
253.658337	8495.283238	27.623988
253.556295	8501.146410	27.629005
254.063644	8521.724344	27.634023
254.345098	8520.265985	27.639040
254.881644	8540.053233	27.644058
254.592287	8549.484942	27.649076
255.138757	8556.490463	27.654093
255.360352	8572.405887	27.659111
255.577066	8583.096974	27.664128
255.881078	8598.832180	27.669146
255.660788	8613.156189	27.674164
255.938253	8627.815825	27.679181
256.106276	8640.181562	27.684199
256.707007	8665.215593	27.689216
256.877691	8664.336553	27.694234
257.020960	8686.812342	27.699252
257.692033	8694.499292	27.704269
257.813327	8708.469932	27.709287
258.106684	8716.402335	27.714304
258.152671	8732.604296	27.719322
258.265488	8747.469779	27.724340
258.657181	8748.226271	27.729357
258.734774	8775.514553	27.734375
258.975569	8785.797864	27.739392
259.589687	8800.992139	27.744410
259.737895	8819.804958	27.749428
260.018721	8828.396072	27.754445
259.985811	8848.654880	27.759463
260.456625	8870.823848	27.764480
261.207890	8881.096704	27.769498
261.509878	8902.613354	27.774516
261.776509	8893.778860	27.779533
262.012149	8908.170592	27.784551
261.936171	8925.275849	27.789568
262.148560	8930.714191	27.794586
262.535202	8942.016626	27.799604
262.642107	8944.516329	27.804621
263.037439	8963.707336	27.809639
263.370484	8974.503558	27.814656
263.754051	8975.046641	27.819674
263.557690	8975.112269	27.824692
264.017101	8996.124468	27.829709
264.182266	9006.081924	27.834727
264.216046	9027.429200	27.839744
264.933492	9028.927143	27.844762
265.003338	9051.800061	27.849780
265.062314	9058.086514	27.854797
265.222347	9080.238115	27.859815
265.732020	9091.950755	27.864832
266.400296	9105.078267	27.869850
266.264118	9125.454587	27.874868
266.968980	9127.510188	27.879885
266.981579	9136.190822	27.884903
266.944822	9147.010345	27.889920
267.259510	9162.845391	27.894938
267.277728	9182.556661	27.899956
268.045980	9194.667721	27.904973
267.963149	9219.907459	27.909991
268.432399	9230.256261	27.915008
268.986743	9237.652312	27.920026
268.757611	9254.428249	27.925044
269.622268	9263.676383	27.930061
270.047590	9278.591214	27.935079
270.389567	9293.389663	27.940096
270.524677	9286.596251	27.945114
270.694084	9302.214221	27.950132
271.013821	9314.600844	27.955149
270.915630	9315.955056	27.960167
271.288164	9333.454551	27.965184
271.810979	9342.898354	27.970202
271.923232	9366.188093	27.975220
272.597578	9360.797272	27.980237
272.676895	9377.155596	27.985255
272.845186	9384.088069	27.990272
273.181561	9383.334592	27.995290
273.207258	9416.997073	28.000308
273.694170	9417.956533	28.005325
273.743000	9441.114223	28.010343
274.326466	9445.758932	28.015360
274.603168	9456.861050	28.020378
274.960026	9468.039024	28.025396
275.101249	9476.863848	28.030413
275.637577	9491.208930	28.035431
275.671381	9490.670185	28.040448
276.155643	9500.154838	28.045466
276.473524	9522.910548	28.050484
276.806379	9521.286194	28.055501
277.214933	9535.079850	28.060519
277.225706	9544.414528	28.065536
277.826470	9538.681562	28.070554
277.835959	9543.091005	28.075572
277.655453	9558.741903	28.080589
278.012247	9569.417931	28.085607
278.339900	9582.270779	28.090624
278.745285	9586.990782	28.095642
278.660886	9598.869425	28.100660
278.965716	9622.252454	28.105677
279.402668	9636.221705	28.110695
279.636142	9655.846082	28.115712
280.130310	9653.890184	28.120730
279.779145	9677.009791	28.125748
279.824271	9676.955500	28.130765
280.052914	9697.894137	28.135783
280.190887	9711.727153	28.140800
280.864266	9741.304173	28.145818
281.093791	9759.836830	28.150836
281.349420	9771.561282	28.155853
281.773106	9781.235539	28.160871
281.758953	9799.736946	28.165888
282.339205	9819.209294	28.170906
282.664303	9838.901603	28.175924
283.263779	9852.697160	28.180941
283.662560	9869.144798	28.185959
283.571971	9878.410272	28.190976
284.241771	9890.758230	28.195994
284.225140	9909.717955	28.201012
284.596854	9916.489308	28.206029
285.002082	9933.327510	28.211047
285.160478	9941.013201	28.216064
285.326686	9948.280896	28.221082
285.593366	9964.683006	28.226100
285.965080	9968.461160	28.231117
286.807533	9976.873265	28.236135
286.767069	9991.245940	28.241152
287.176036	9988.409810	28.246170
287.586962	10013.993212	28.251188
287.936521	10007.052278	28.256205
288.137262	10014.642960	28.261223
288.121927	10031.010371	28.266240
289.024845	10035.008438	28.271258
289.163120	10057.246704	28.276276
289.497164	10050.289241	28.281293
289.740014	10050.974385	28.286311
290.088718	10068.238343	28.291328
290.639911	10069.642439	28.296346
290.388420	10071.121757	28.301364
290.850019	10093.028407	28.306381
290.938007	10100.197904	28.311399
291.019585	10111.195211	28.316416
290.872617	10120.138106	28.321434
291.273112	10150.108999	28.326452
291.759982	10153.171360	28.331469
292.457105	10181.172959	28.336487
292.421578	10183.742503	28.341504
292.676169	10207.854034	28.346522
292.903528	10216.185786	28.351540
293.209031	10230.987539	28.356557
294.097466	10243.655119	28.361575
294.091605	10265.060543	28.366592
294.520234	10266.190211	28.371610
294.958768	10278.135770	28.376628
295.142740	10289.082409	28.381645
295.424428	10297.768794	28.386663
295.332309	10322.076871	28.391680
295.854637	10326.200929	28.396698
296.196229	10353.857483	28.401716
296.521524	10357.355659	28.406733
296.715207	10358.092722	28.411751
296.638893	10379.057794	28.416768
297.417660	10380.012638	28.421786
297.462678	10397.959125	28.426804
297.613624	10413.498825	28.431821
298.298857	10431.057725	28.436839
298.457789	10445.191121	28.441856
298.564969	10457.245536	28.446874
299.123664	10473.034003	28.451892
299.165096	10481.448675	28.456909
299.606272	10498.196505	28.461927
299.669207	10524.643439	28.466944
300.161467	10534.957793	28.471962
300.515812	10547.402968	28.476980
300.793908	10565.003669	28.481997
300.704984	10558.715359	28.487015
300.772941	10587.324484	28.492032
301.018466	10586.970410	28.497050
301.534983	10620.738155	28.502068
302.125847	10624.463170	28.507085
302.576593	10636.650175	28.512103
302.653852	10656.508473	28.517120
303.334622	10672.963169	28.522138
303.856538	10674.744489	28.527156
303.992603	10691.142439	28.532173
303.952274	10708.452144	28.537191
303.809681	10722.333017	28.542208
304.134945	10734.486064	28.547226
304.729647	10750.897476	28.552244
305.264442	10767.403540	28.557261
305.611887	10782.745416	28.562279
305.687396	10797.113174	28.567296
306.281545	10808.213736	28.572314
306.624521	10826.928607	28.577332
306.770435	10846.337452	28.582349
307.227517	10855.726018	28.587367
307.365098	10865.028861	28.592384
307.734618	10891.270410	28.597402
308.221335	10901.576363	28.602420
308.090214	10917.994263	28.607437
308.666589	10923.107780	28.612455
308.910310	10950.799495	28.617472
309.157667	10966.933963	28.622490
309.695543	10976.234151	28.627508
309.717585	10994.519512	28.632525
310.288427	11005.784879	28.637543
310.594141	11030.502035	28.642560
310.916918	11043.154571	28.647578
311.502300	11058.544657	28.652596
311.453657	11072.988910	28.657613
312.080629	11082.303613	28.662631
311.975354	11096.712550	28.667648
312.209728	11115.264740	28.672666
312.758382	11131.724749	28.677684
313.002047	11150.114480	28.682701
313.738932	11163.431636	28.687719
313.393968	11179.169643	28.692736
314.170598	11186.462189	28.697754
314.655989	11202.237497	28.702772
314.676494	11211.176782	28.707789
315.348692	11221.302292	28.712807
315.524637	11245.345384	28.717824
315.569164	11247.792017	28.722842
315.764448	11262.071901	28.727860
316.353071	11281.718138	28.732877
316.661380	11293.125848	28.737895
316.715714	11308.943509	28.742912
316.924963	11322.068716	28.747930
317.682029	11341.960187	28.752948
317.749799	11357.892616	28.757965
318.148356	11375.364694	28.762983
318.913618	11386.584049	28.768000
318.851808	11411.081405	28.773018
319.459024	11415.621851	28.778036
319.565052	11435.359634	28.783053
319.910931	11433.966748	28.788071
319.965927	11449.961251	28.793088
320.236856	11466.531371	28.798106
320.890945	11476.931417	28.803124
320.776574	11499.242549	28.808141
321.557262	11516.471755	28.813159
321.725356	11535.025269	28.818176
322.020309	11538.465270	28.823194
322.221056	11539.261270	28.828212
322.650557	11561.904094	28.833229
322.729763	11562.681243	28.838247
323.138978	11581.774887	28.843264
323.481879	11592.350050	28.848282
323.913389	11601.556695	28.853300
324.123155	11620.732144	28.858317
324.738215	11629.322722	28.863335
324.919083	11647.820666	28.868352
324.838235	11660.056877	28.873370
325.662532	11658.642714	28.878388
325.336096	11692.544438	28.883405
325.788887	11702.249872	28.888423
326.410166	11732.899199	28.893440
326.742104	11746.561240	28.898458
327.240357	11750.600975	28.903476
327.162543	11773.045644	28.908493
327.789537	11793.772660	28.913511
328.055825	11802.938973	28.918528
328.400075	11823.685051	28.923546
328.901795	11836.647970	28.928564
329.051653	11864.482045	28.933581
329.392645	11871.827315	28.938599
329.289447	11890.632086	28.943616
329.944859	11910.871648	28.948634
330.388974	11927.670824	28.953652
330.439380	11949.852473	28.958669
330.918347	11972.134376	28.963687
330.930562	11990.374880	28.968704
331.223365	12004.782152	28.973722
331.844733	12020.937884	28.978740
332.443519	12049.061894	28.983757
332.852607	12065.882468	28.988775
333.215328	12079.691503	28.993792
333.045892	12094.736490	28.998810
333.488222	12107.194183	29.003828
333.872624	12133.122520	29.008845
334.814567	12152.679590	29.013863
334.951775	12161.698937	29.018880
334.993510	12180.449717	29.023898
335.688997	12186.766986	29.028916
335.637840	12208.371186	29.033933
336.345696	12220.799994	29.038951
336.583973	12247.029262	29.043968
336.876868	12259.557832	29.048986
337.099996	12267.246972	29.054004
337.321561	12289.844300	29.059021
337.494257	12305.862146	29.064039
338.186625	12331.717253	29.069056
338.153785	12349.030451	29.074074
338.770381	12366.851392	29.079092
339.259773	12388.459544	29.084109
339.278432	12403.667939	29.089127
340.032873	12420.204213	29.094144
340.218576	12443.843108	29.099162
340.562698	12452.252301	29.104180
340.943443	12468.386112	29.109197
341.398405	12489.248211	29.114215
341.686417	12496.990438	29.119232
342.341187	12520.956997	29.124250
343.058789	12516.085874	29.129268
342.931779	12534.304502	29.134285
343.184113	12545.074386	29.139303
343.514533	12557.761484	29.144320
343.413845	12564.250966	29.149338
343.751925	12582.396787	29.154356
344.206953	12600.783250	29.159373
344.379559	12614.423513	29.164391
344.766526	12617.915616	29.169408
344.933659	12647.857585	29.174426
345.618207	12655.774602	29.179444
345.973572	12683.059806	29.184461
346.163232	12694.941687	29.189479
346.438350	12715.847997	29.194496
346.386436	12727.180375	29.199514
347.028327	12742.019842	29.204532
347.363799	12775.677720	29.209549
347.523630	12787.453806	29.214567
347.755003	12808.026020	29.219584
348.140396	12832.673064	29.224602
348.856472	12853.819927	29.229620
349.031869	12874.953613	29.234637
349.279465	12906.569702	29.239655
349.842481	12920.442716	29.244672
349.993618	12950.896093	29.249690
350.822980	12958.632659	29.254708
351.002623	12987.774257	29.259725
351.622650	13000.956292	29.264743
351.550959	13020.350939	29.269760
351.762739	13045.843357	29.274778
352.529977	13061.948715	29.279796
352.696478	13082.673496	29.284813
353.280522	13106.137137	29.289831
353.996712	13121.097898	29.294848
354.145533	13138.408626	29.299866
354.534375	13151.257501	29.304884
355.107773	13169.247025	29.309901
355.620174	13173.414330	29.314919
356.178708	13195.432584	29.319936
356.178339	13202.427629	29.324954
356.789726	13205.932058	29.329972
357.108399	13221.381490	29.334989
357.310451	13230.994358	29.340007
357.432172	13241.456673	29.345024
357.860838	13261.433203	29.350042
358.571936	13277.184375	29.355060
358.510853	13294.423913	29.360077
358.804608	13308.727821	29.365095
359.584077	13317.568166	29.370112
359.880386	13343.906712	29.375130
360.204554	13345.804539	29.380148
360.208154	13365.642494	29.385165
360.613636	13382.941664	29.390183
360.878122	13392.592205	29.395200
361.217865	13420.544097	29.400218
361.473668	13427.852793	29.405236
361.528977	13449.031194	29.410253
361.939313	13469.481355	29.415271
362.364473	13493.920922	29.420288
362.810189	13521.808993	29.425306
363.145131	13536.447685	29.430324
363.569669	13559.778976	29.435341
364.000529	13591.247497	29.440359
364.564171	13609.096858	29.445376
365.002669	13630.651245	29.450394
364.938231	13648.384281	29.455412
365.399268	13671.779468	29.460429
365.713999	13691.929042	29.465447
366.162835	13712.951355	29.470464
366.432632	13726.135072	29.475482
366.822711	13753.056366	29.480500
367.368582	13766.187392	29.485517
367.746851	13789.737802	29.490535
368.322650	13798.506063	29.495552
368.321701	13818.016765	29.500570
368.912859	13829.706988	29.505588
369.204755	13852.260429	29.510605
369.689077	13867.671808	29.515623
370.082209	13878.429873	29.520640
370.197785	13897.344480	29.525658
370.556576	13902.230784	29.530676
370.880905	13920.983235	29.535693
371.110535	13947.456228	29.540711
371.885494	13961.988429	29.545728
372.115483	13991.603710	29.550746
372.682830	14004.876810	29.555764
372.851214	14021.013632	29.560781
373.357262	14041.411522	29.565799
373.847507	14046.495181	29.570816
373.663129	14074.432233	29.575834
373.987019	14088.716220	29.580852
374.384293	14111.777706	29.585869
374.610847	14133.485871	29.590887
375.345835	14158.143043	29.595904
375.818566	14183.697174	29.600922
376.082487	14201.376133	29.605940
376.417319	14228.066738	29.610957
376.651447	14249.199072	29.615975
377.156861	14272.171177	29.620992
377.514215	14293.454796	29.626010
378.158895	14309.997293	29.631028
378.361090	14327.941846	29.636045
378.647737	14348.810255	29.641063
379.120834	14370.435858	29.646080
379.151329	14394.335200	29.651098
379.917753	14426.216790	29.656116
380.698154	14445.577323	29.661133
380.867594	14469.473943	29.666151
381.459041	14481.306642	29.671168
381.573936	14509.952254	29.676186
381.868460	14525.147561	29.681204
382.298127	14544.948430	29.686221
382.498819	14578.333751	29.691239
383.375124	14600.237541	29.696256
383.273338	14628.591979	29.701274
383.829154	14638.424911	29.706292
384.040919	14662.738340	29.711309
384.223414	14674.458359	29.716327
384.895582	14703.560180	29.721344
385.436825	14723.694317	29.726362
385.793472	14749.425302	29.731380
386.558202	14771.466779	29.736397
386.633562	14796.913434	29.741415
386.813153	14810.374165	29.746432
387.421212	14838.513505	29.751450
388.096049	14850.731308	29.756468
388.556368	14864.321807	29.761485
388.740850	14885.787920	29.766503
389.574291	14904.989019	29.771520
389.664905	14918.356384	29.776538
390.377104	14941.571673	29.781556
390.702634	14948.134166	29.786573
390.963656	14964.367815	29.791591
391.461923	14970.855885	29.796608
391.597907	14989.263061	29.801626
391.707797	15006.076269	29.806644
392.341966	15008.168895	29.811661
392.545878	15047.349914	29.816679
393.462539	15062.129217	29.821696
393.155347	15083.249360	29.826714
393.700733	15093.646333	29.831732
394.338873	15105.592122	29.836749
394.771286	15126.599622	29.841767
395.231002	15130.071325	29.846784
395.361553	15152.708428	29.851802
395.690484	15166.414472	29.856820
396.598521	15168.258930	29.861837
396.619579	15184.040822	29.866855
396.989653	15200.102835	29.871872
396.940133	15213.476565	29.876890
397.507681	15239.566803	29.881908
398.259600	15257.754586	29.886925
398.538112	15278.454740	29.891943
398.844851	15293.272911	29.896960
399.209951	15306.648085	29.901978
399.108507	15327.875235	29.906996
400.023871	15344.455193	29.912013
400.221612	15368.140057	29.917031
400.808813	15389.227825	29.922048
401.302338	15414.249756	29.927066
401.535576	15422.870298	29.932084
402.322381	15451.671058	29.937101
402.469820	15463.040162	29.942119
403.248241	15482.045172	29.947136
403.321921	15495.226094	29.952154
403.299115	15525.025477	29.957172
404.243374	15539.137580	29.962189
404.345381	15561.448013	29.967207
404.803183	15583.364799	29.972224
405.504331	15611.010631	29.977242
405.839365	15628.616607	29.982260
406.390758	15648.071088	29.987277
406.452851	15664.712335	29.992295
407.075865	15684.281969	29.997312
407.410370	15704.023147	30.002330
407.678929	15726.658262	30.007348
408.249025	15737.645489	30.012365
408.483191	15766.069007	30.017383
409.266704	15791.440806	30.022400
409.579606	15804.038070	30.027418
409.682064	15823.095608	30.032436
410.432098	15838.504868	30.037453
410.829428	15874.037776	30.042471
411.308501	15876.157955	30.047488
411.567670	15899.584342	30.052506
411.401968	15917.101622	30.057524
412.323943	15937.505880	30.062541
412.563740	15968.607138	30.067559
413.171462	15992.443329	30.072576
413.076322	16017.978323	30.077594
413.563856	16050.977018	30.082612
414.376376	16063.161402	30.087629
414.568860	16086.677424	30.092647
414.721953	16108.187726	30.097664
415.465474	16131.734352	30.102682
415.491903	16162.067104	30.107700
416.615766	16178.820429	30.112717
417.124795	16211.705489	30.117735
417.571368	16229.784106	30.122752
417.909561	16250.971839	30.127770
417.984138	16274.155970	30.132788
418.758386	16285.348421	30.137805
418.844571	16310.176333	30.142823
419.070342	16328.630742	30.147840
419.492365	16354.887427	30.152858
419.672029	16383.266702	30.157876
420.689702	16405.223072	30.162893
420.941920	16429.077588	30.167911
421.361534	16456.089666	30.172928
421.699767	16464.997447	30.177946
422.185660	16490.391522	30.182964
422.717883	16503.706614	30.187981
423.222272	16527.474376	30.192999
423.342463	16548.582878	30.198016
423.495818	16559.942230	30.203034
424.126023	16579.814870	30.208052
424.549599	16604.059685	30.213069
424.758246	16635.132158	30.218087
425.453410	16648.961935	30.223104
426.041847	16672.877797	30.228122
426.400832	16695.373549	30.233140
427.255317	16704.961783	30.238157
427.715028	16733.029234	30.243175
427.795103	16746.298451	30.248192
427.907875	16765.750124	30.253210
428.660937	16783.177977	30.258228
429.071356	16799.468744	30.263245
429.502108	16829.742375	30.268263
429.786177	16858.497656	30.273280
430.357473	16873.859943	30.278298
430.367934	16898.630986	30.283316
431.128611	16923.777288	30.288333
431.413128	16951.641924	30.293351
432.088836	16972.073226	30.298368
432.435664	16988.260406	30.303386
432.558429	17011.519999	30.308404
433.437715	17040.782451	30.313421
433.781444	17063.388415	30.318439
434.314026	17085.048834	30.323456
434.632978	17111.562750	30.328474
435.034884	17139.118679	30.333492
435.392861	17156.592962	30.338509
435.843111	17186.263965	30.343527
436.029892	17217.587171	30.348544
436.478963	17237.833152	30.353562
437.105086	17270.028895	30.358580
437.747057	17297.964387	30.363597
438.601349	17319.827371	30.368615
438.464239	17341.409774	30.373632
438.960837	17353.410729	30.378650
439.680891	17389.363365	30.383668
440.335122	17409.084644	30.388685
440.656180	17429.477222	30.393703
441.089278	17451.899077	30.398720
441.443688	17470.315479	30.403738
441.854074	17498.514958	30.408756
442.347605	17510.882897	30.413773
443.006301	17537.982232	30.418791
443.288149	17560.288921	30.423808
443.888058	17579.589305	30.428826
444.222760	17603.997757	30.433844
444.751659	17611.009431	30.438861
445.072228	17638.825190	30.443879
445.158726	17666.481814	30.448896
445.650109	17686.803765	30.453914
445.869563	17717.958413	30.458932
446.855519	17737.615435	30.463949
447.492566	17755.962571	30.468967
447.840633	17777.014613	30.473984
448.838007	17791.217986	30.479002
448.606859	17818.040143	30.484020
449.179836	17835.512952	30.489037
449.653650	17859.059720	30.494055
449.954524	17876.985819	30.499072
450.350464	17889.963126	30.504090
450.720771	17914.341123	30.509108
451.514202	17930.086413	30.514125
451.605439	17953.200458	30.519143
452.215383	17972.202743	30.524160
452.893800	17974.288779	30.529178
453.114948	17999.284088	30.534196
453.944267	18000.499951	30.539213
454.165022	18017.067838	30.544231
454.385487	18031.430982	30.549248
454.981670	18050.966169	30.554266
454.981268	18076.248978	30.559284
455.589535	18098.410399	30.564301
456.180153	18119.437458	30.569319
456.495749	18149.093126	30.574336
457.197249	18164.202302	30.579354
457.199592	18195.139022	30.584372
457.752899	18215.135953	30.589389
458.002934	18241.099951	30.594407
458.458162	18261.781953	30.599424
458.962664	18294.301696	30.604442
459.333905	18323.279252	30.609460
459.954405	18341.793794	30.614477
460.400302	18366.785962	30.619495
461.008941	18399.384334	30.624512
461.513774	18412.610276	30.629530
461.758480	18455.885645	30.634548
462.045737	18478.792720	30.639565
462.687818	18500.248048	30.644583
462.968949	18525.550521	30.649600
463.781019	18565.635307	30.654618
464.239512	18588.818939	30.659636
464.868037	18608.892942	30.664653
465.488061	18644.686685	30.669671
465.946920	18667.358621	30.674688
466.715410	18687.025404	30.679706
466.866437	18717.472157	30.684724
467.425785	18733.804409	30.689741
468.229396	18759.334919	30.694759
468.260422	18784.139897	30.699776
468.664967	18789.200349	30.704794
469.241419	18816.990355	30.709812
469.960274	18840.139825	30.714829
470.633526	18866.398482	30.719847
470.521136	18889.943553	30.724864
471.257275	18903.828555	30.729882
471.762410	18927.220089	30.734900
472.337977	18948.869548	30.739917
472.625734	18975.953184	30.744935
472.845601	19001.417500	30.749952
473.557915	19017.953473	30.754970
473.938513	19045.850297	30.759988
474.394416	19069.331845	30.765005
475.192118	19090.877174	30.770023
475.492051	19125.129845	30.775040
475.894467	19145.840014	30.780058
476.050845	19172.887641	30.785076
476.885747	19190.143750	30.790093
477.520225	19219.403622	30.795111
477.448570	19251.503462	30.800128
478.017632	19262.616071	30.805146
478.366605	19297.404702	30.810164
478.759919	19315.109160	30.815181
479.141001	19346.133698	30.820199
480.131462	19379.419425	30.825216
480.420524	19396.843344	30.830234
480.841825	19445.829930	30.835252
481.352805	19464.230022	30.840269
482.039937	19488.320289	30.845287
482.162773	19518.153548	30.850304
483.017463	19534.686616	30.855322
483.311140	19563.684486	30.860340
483.283504	19593.276073	30.865357
484.117301	19615.378631	30.870375
484.732426	19638.374713	30.875392
485.041653	19659.858186	30.880410
485.488468	19698.138701	30.885428
486.088264	19713.214474	30.890445
486.470714	19733.814671	30.895463
486.884891	19763.849076	30.900480
487.533910	19785.102561	30.905498
488.043331	19816.303605	30.910516
488.353682	19841.123037	30.915533
489.086752	19858.281965	30.920551
489.605076	19893.765393	30.925568
489.793575	19907.831662	30.930586
490.627687	19948.225430	30.935604
490.628367	19967.704184	30.940621
491.413765	20001.774947	30.945639
491.743621	20039.903862	30.950656
492.501069	20059.997081	30.955674
493.041748	20087.876640	30.960692
493.366999	20112.713037	30.965709
494.125387	20147.445374	30.970727
494.343745	20180.910265	30.975744
495.262965	20199.266064	30.980762
495.500869	20229.227702	30.985780
496.098705	20249.358752	30.990797
496.941144	20273.583620	30.995815
497.277850	20301.249021	31.000832
497.958641	20320.128781	31.005850
498.273561	20345.061865	31.010868
498.305219	20376.761954	31.015885
499.134502	20405.664546	31.020903
499.771009	20431.874204	31.025920
500.596179	20452.721731	31.030938
501.152594	20486.052057	31.035956
501.348173	20491.556373	31.040973
502.293955	20523.315709	31.045991
503.029778	20542.363977	31.051008
503.648964	20565.935481	31.056026
503.674108	20586.655724	31.061044
503.928520	20603.346903	31.066061
504.756438	20628.168408	31.071079
504.846565	20659.348011	31.076096
505.149291	20671.387708	31.081114
505.746970	20696.611824	31.086132
506.266869	20728.179144	31.091149
506.712934	20747.696326	31.096167
507.211360	20782.552645	31.101184
507.321131	20808.965357	31.106202
507.906852	20844.395722	31.111220
508.497129	20876.508277	31.116237
509.111676	20912.395493	31.121255
509.708247	20944.361850	31.126272
510.032583	20972.800982	31.131290
510.898915	21009.824169	31.136308
511.330791	21029.438630	31.141325
512.025621	21065.578927	31.146343
512.583934	21094.322786	31.151360
512.977273	21117.052058	31.156378
513.358104	21139.713813	31.161396
513.878000	21170.043420	31.166413
514.500801	21187.315566	31.171431
514.963751	21222.412006	31.176448
515.621581	21240.601215	31.181466
516.126282	21267.887828	31.186484
516.368214	21297.566130	31.191501
516.979999	21311.156404	31.196519
517.601126	21338.443835	31.201536
518.024087	21367.986475	31.206554
518.654924	21384.006461	31.211572
518.773450	21408.573584	31.216589
519.491334	21431.037557	31.221607
519.854722	21462.453650	31.226624
520.513503	21485.204959	31.231642
521.151953	21513.033319	31.236660
521.701610	21532.768845	31.241677
522.354251	21563.312057	31.246695
522.613399	21586.877992	31.251712
523.017986	21604.304736	31.256730
523.343196	21633.186989	31.261748
523.960495	21673.959477	31.266765
524.613915	21692.238257	31.271783
524.725395	21725.760427	31.276800
525.449739	21766.225681	31.281818
525.998838	21789.462104	31.286836
525.993842	21822.440316	31.291853
526.812438	21860.951160	31.296871
527.628189	21901.945785	31.301888
528.556566	21922.462777	31.306906
528.737501	21948.518338	31.311924
529.021360	21983.145001	31.316941
530.293285	22006.584407	31.321959
530.530762	22044.997064	31.326976
530.853949	22068.730469	31.331994
532.024551	22101.430240	31.337012
531.973718	22125.519277	31.342029
532.640974	22154.133881	31.347047
533.275130	22186.127960	31.352064
533.521102	22215.276228	31.357082
534.929540	22248.792036	31.362100
534.664300	22277.988868	31.367117
535.557747	22302.391501	31.372135
535.823099	22333.097664	31.377152
536.782955	22359.568875	31.382170
537.147884	22386.897884	31.387188
537.658878	22431.732672	31.392205
538.205859	22451.128316	31.397223
538.859588	22481.325239	31.402240
539.547096	22512.369972	31.407258
540.340803	22533.230958	31.412276
540.409003	22557.055437	31.417293
540.895687	22577.193646	31.422311
541.337397	22604.081241	31.427328
542.131917	22630.193254	31.432346
542.656368	22666.154644	31.437364
543.252754	22701.062200	31.442381
543.665887	22712.637206	31.447399
544.223066	22754.129064	31.452416
544.671678	22788.244767	31.457434
545.287082	22805.070842	31.462452
545.805740	22836.982960	31.467469
546.548477	22867.842668	31.472487
547.334225	22890.954856	31.477504
547.490288	22925.622138	31.482522
548.415399	22943.000135	31.487540
548.431285	22977.531485	31.492557
549.123162	23008.058148	31.497575
549.891991	23022.358023	31.502592
550.305660	23058.836683	31.507610
550.891074	23082.283788	31.512628
551.294324	23116.015375	31.517645
552.015367	23137.981588	31.522663
552.616295	23166.652278	31.527680
553.005930	23187.520369	31.532698
553.803486	23219.667464	31.537716
554.117222	23244.800290	31.542733
554.628198	23267.033355	31.547751
555.481566	23288.359733	31.552768
555.644880	23316.043877	31.557786
556.146478	23334.310042	31.562804
556.638044	23359.560503	31.567821
557.317414	23380.206481	31.572839
558.085356	23412.857743	31.577856
558.545977	23438.675561	31.582874
559.061574	23466.058290	31.587892
558.967101	23496.140130	31.592909
559.785211	23517.465957	31.597927
559.925584	23550.936129	31.602944
560.534303	23588.737533	31.607962
561.108143	23620.598032	31.612980
561.970595	23665.848187	31.617997
562.476973	23694.104735	31.623015
562.941879	23729.173715	31.628032
563.786902	23766.837339	31.633050
564.484054	23797.648759	31.638068
564.638987	23837.177370	31.643085
565.495774	23866.339823	31.648103
566.347285	23907.990210	31.653120
566.921808	23933.588611	31.658138
567.570801	23965.734902	31.663156
568.248632	23997.042569	31.668173
568.577166	24017.074300	31.673191
569.332831	24048.850132	31.678208
569.904183	24078.019683	31.683226
570.726470	24108.458098	31.688244
571.052502	24135.220534	31.693261
571.733867	24163.772634	31.698279
572.495286	24197.791207	31.703296
572.703840	24225.102997	31.708314
573.726093	24251.111963	31.713332
574.021780	24281.740548	31.718349
574.609535	24307.944028	31.723367
575.305212	24332.563404	31.728384
575.740238	24360.326511	31.733402
576.441228	24391.056094	31.738420
576.903885	24430.051079	31.743437
577.254133	24445.719364	31.748455
577.644124	24478.204063	31.753472
578.112117	24520.686779	31.758490
579.018101	24546.802815	31.763508
579.369674	24587.496510	31.768525
580.102583	24615.327071	31.773543
580.770201	24645.487189	31.778560
581.096894	24695.841351	31.783578
581.926908	24724.219300	31.788596
582.303529	24747.859059	31.793613
583.040473	24780.511097	31.798631
583.869492	24813.256202	31.803648
584.148530	24850.403827	31.808666
585.245488	24871.687435	31.813684
585.321623	24904.342053	31.818701
586.030107	24936.885050	31.823719
586.796690	24964.123091	31.828736
587.236313	25002.693059	31.833754
588.011985	25033.209701	31.838772
588.092429	25064.328212	31.843789
588.828810	25095.363001	31.848807
589.419410	25133.125926	31.853824
589.945946	25170.545049	31.858842
590.502766	25204.237151	31.863860
591.231327	25242.351541	31.868877
591.704087	25275.797817	31.873895
592.439101	25298.440444	31.878912
593.016123	25340.004088	31.883930
593.786819	25362.931912	31.888948
594.125373	25390.041654	31.893965
594.278415	25423.967997	31.898983
595.049426	25447.136022	31.904000
595.489106	25478.767699	31.909018
596.286204	25507.897659	31.914036
596.881534	25539.467135	31.919053
597.862154	25573.927708	31.924071
598.305183	25603.163817	31.929088
598.983149	25640.427381	31.934106
599.261494	25666.997093	31.939124
600.100663	25705.752312	31.944141
600.629755	25725.893380	31.949159
601.641982	25753.163542	31.954176
601.775143	25790.613827	31.959194
602.430386	25824.228354	31.964212
603.222345	25850.180671	31.969229
603.667674	25890.502082	31.974247
604.229408	25921.097820	31.979264
604.549464	25955.852101	31.984282
605.597084	25989.171612	31.989300
606.191631	26028.155364	31.994317
606.884625	26066.953132	31.999335
607.608796	26083.727023	32.004352
608.153174	26125.891487	32.009370
608.876067	26158.743889	32.014388
609.677216	26175.379400	32.019405
610.270712	26219.710475	32.024423
611.145499	26240.739613	32.029440
611.583880	26271.399443	32.034458
612.353173	26291.705703	32.039476
613.007170	26318.874734	32.044493
613.964821	26344.738539	32.049511
614.481772	26359.421550	32.054528
614.557594	26389.942417	32.059546
614.994720	26420.766994	32.064564
615.793241	26448.931111	32.069581
616.314561	26476.121133	32.074599
616.821494	26509.349219	32.079616
617.350052	26553.817601	32.084634
617.836394	26586.404378	32.089652
618.468330	26622.766857	32.094669
618.867661	26666.130725	32.099687
619.803452	26704.240710	32.104704
620.262201	26746.761173	32.109722
620.917668	26783.701720	32.114740
621.519463	26811.075517	32.119757
622.252783	26845.058734	32.124775
622.872219	26880.064771	32.129792
623.441418	26931.884448	32.134810
624.410701	26968.270559	32.139828
625.230523	26995.313405	32.144845
625.299671	27035.974109	32.149863
626.368542	27069.924113	32.154880
626.928122	27095.952351	32.159898
627.262393	27138.398324	32.164916
627.844800	27174.339765	32.169933
628.342546	27209.700411	32.174951
629.051377	27247.448778	32.179968
629.335478	27280.403326	32.184986
630.302995	27312.226987	32.190004
631.088609	27359.254576	32.195021
631.895837	27392.449722	32.200039
632.292336	27424.375628	32.205056
633.032076	27459.332222	32.210074
633.686937	27488.133373	32.215092
634.555448	27524.074870	32.220109
635.204166	27550.797627	32.225127
635.595883	27570.418487	32.230144
636.455750	27607.789923	32.235162
637.277647	27633.790410	32.240180
637.993645	27651.691943	32.245197
637.983432	27685.034549	32.250215
638.869250	27708.711801	32.255232
638.962031	27745.027999	32.260250
639.855114	27776.067655	32.265268
640.633275	27812.978220	32.270285
640.801302	27848.555950	32.275303
641.510807	27882.045308	32.280320
641.946542	27917.707645	32.285338
642.441555	27960.541000	32.290356
643.691218	27990.317899	32.295373
644.332347	28036.573282	32.300391
644.550500	28064.160548	32.305408
645.184809	28111.618096	32.310426
645.896888	28150.290451	32.315444
646.542063	28185.035558	32.320461
647.015673	28234.225148	32.325479
648.132271	28268.011668	32.330496
648.557227	28314.965213	32.335514
649.162747	28346.221435	32.340532
650.135776	28386.534692	32.345549
650.993374	28422.138164	32.350567
651.385875	28459.780302	32.355584
651.933682	28509.072708	32.360602
652.802475	28540.325921	32.365620
653.522919	28582.923012	32.370637
654.087831	28625.911158	32.375655
654.823564	28651.243791	32.380672
655.515909	28698.990695	32.385690
655.902747	28738.966632	32.390708
657.115278	28779.243157	32.395725
657.489494	28817.862234	32.400743
658.214705	28853.107937	32.405760
659.039260	28896.511095	32.410778
659.787217	28929.616896	32.415796
660.281709	28964.146733	32.420813
660.761301	28998.868589	32.425831
661.547484	29030.634846	32.430848
662.029383	29085.210646	32.435866
662.643348	29133.565011	32.440884
663.592417	29171.298282	32.445901
664.117979	29202.068975	32.450919
665.042147	29239.837878	32.455936
665.724684	29275.520822	32.460954
666.360954	29310.187063	32.465972
667.159291	29341.294510	32.470989
667.509512	29384.602318	32.476007
668.393638	29418.376582	32.481024
669.348999	29460.319243	32.486042
669.850413	29487.920957	32.491060
670.133350	29528.907118	32.496077
670.789736	29572.723634	32.501095
671.552791	29608.773816	32.506112
672.333371	29650.548282	32.511130
672.984373	29687.981521	32.516148
673.843572	29728.315250	32.521165
673.845150	29767.259960	32.526183
674.955039	29804.476159	32.531200
675.717542	29844.237387	32.536218
676.039892	29877.228057	32.541236
676.954469	29916.270274	32.546253
677.575570	29964.612835	32.551271
678.273659	30001.040512	32.556288
679.016461	30039.458774	32.561306
679.759714	30078.268957	32.566324
680.587754	30109.309704	32.571341
680.802986	30139.390809	32.576359
681.639861	30170.796901	32.581376
682.260440	30199.613564	32.586394
682.613326	30232.928730	32.591412
683.656402	30267.393810	32.596429
684.125272	30305.653185	32.601447
684.547580	30335.752718	32.606464
685.390806	30377.664242	32.611482
686.469630	30411.909039	32.616500
686.950633	30449.521999	32.621517
687.773577	30490.387576	32.626535
688.254148	30523.291287	32.631552
688.964216	30554.294288	32.636570
689.701312	30596.911914	32.641588
690.524480	30633.491801	32.646605
691.213405	30678.898582	32.651623
692.122024	30711.975775	32.656640
692.894641	30752.249212	32.661658
693.658403	30794.787213	32.666676
694.509552	30814.067409	32.671693
694.885708	30855.825475	32.676711
695.760731	30885.741126	32.681728
696.275391	30912.742130	32.686746
697.186753	30960.554810	32.691764
697.645858	30992.229926	32.696781
697.968889	31029.514673	32.701799
698.546085	31072.240501	32.706816
699.737888	31118.460839	32.711834
700.496060	31158.926979	32.716852
701.538773	31192.167270	32.721869
701.902493	31232.644753	32.726887
702.758489	31272.349842	32.731904
703.545966	31310.460036	32.736922
704.146686	31345.230094	32.741940
704.626806	31373.539373	32.746957
705.572967	31427.378566	32.751975
706.277143	31456.986750	32.756992
707.000161	31496.991249	32.762010
707.592876	31543.072451	32.767028
708.628660	31582.092519	32.772045
709.319598	31623.176982	32.777063
709.978563	31652.666090	32.782080
710.811099	31699.443407	32.787098
710.882823	31730.737792	32.792116
712.316957	31760.326923	32.797133
713.146230	31810.215326	32.802151
713.547868	31831.134677	32.807168
714.491633	31867.963379	32.812186
715.276523	31904.905531	32.817204
716.124342	31944.771235	32.822221
716.380687	31984.571595	32.827239
717.157517	32011.893321	32.832256
717.638194	32052.891446	32.837274
718.453335	32093.318879	32.842292
719.499756	32125.776173	32.847309
719.494660	32178.078331	32.852327
720.298447	32209.890986	32.857344
721.065336	32247.683706	32.862362
721.571485	32291.415715	32.867380
722.607119	32332.605650	32.872397
723.304902	32384.140767	32.877415
723.971920	32427.670854	32.882432
724.669303	32467.137543	32.887450
725.152941	32504.399783	32.892468
726.074680	32551.481148	32.897485
726.589269	32606.693320	32.902503
727.363202	32638.606136	32.907520
728.215625	32680.533521	32.912538
728.645912	32720.200569	32.917556
729.615158	32754.295707	32.922573
730.306364	32786.841271	32.927591
730.931673	32814.244679	32.932608
731.958567	32852.838622	32.937626
732.424174	32896.578246	32.942644
733.221625	32929.581556	32.947661
734.008146	32965.564368	32.952679
734.868782	33000.998250	32.957696
735.883882	33046.909156	32.962714
736.220812	33093.021196	32.967732
737.068947	33116.558853	32.972749
737.699707	33161.866366	32.977767
738.368925	33199.808873	32.982784
739.947664	33239.391893	32.987802
740.449847	33276.134180	32.992820
740.963125	33306.141581	32.997837
742.033369	33340.999502	33.002855
742.748524	33369.527578	33.007872
743.185169	33405.989532	33.012890
744.059680	33442.092154	33.017908
744.835363	33491.253260	33.022925
745.390411	33524.896090	33.027943
745.915938	33565.207347	33.032960
746.772286	33615.765995	33.037978
747.583785	33658.144315	33.042996
748.409136	33694.293005	33.048013
749.431949	33745.527682	33.053031
749.978160	33777.983692	33.058048
750.933587	33816.318742	33.063066
751.422623	33854.511936	33.068084
752.195787	33890.738683	33.073101
752.837033	33942.223266	33.078119
753.752256	33990.156100	33.083136
754.494769	34032.748299	33.088154
754.985417	34076.322077	33.093172
756.027551	34117.754770	33.098189
756.768235	34165.740626	33.103207
756.984095	34207.625335	33.108224
758.225106	34251.903903	33.113242
758.918642	34291.589601	33.118260
759.594106	34335.223489	33.123277
760.717234	34381.733692	33.128295
761.631047	34427.410579	33.133312
762.067813	34456.419988	33.138330
762.954822	34508.917025	33.143348
763.971628	34551.713904	33.148365
764.646937	34599.559242	33.153383
765.007290	34637.141741	33.158400
766.044556	34672.531822	33.163418
766.503979	34731.817377	33.168436
767.421136	34773.865266	33.173453
768.370480	34804.362917	33.178471
768.604962	34852.397992	33.183488
770.090549	34897.158082	33.188506
770.802789	34953.622663	33.193524
771.438807	34985.636522	33.198541
772.258807	35030.975333	33.203559
772.873886	35076.536013	33.208576
773.887279	35113.384817	33.213594
774.643932	35158.341806	33.218612
775.408848	35197.512204	33.223629
776.214489	35243.264703	33.228647
776.928950	35280.306034	33.233664
777.686943	35322.177607	33.238682
778.225925	35362.382705	33.243700
779.102064	35390.825086	33.248717
779.395289	35426.604830	33.253735
780.477600	35465.669117	33.258752
781.419267	35492.754594	33.263770
782.261024	35528.587718	33.268788
783.026323	35560.183859	33.273805
783.703319	35593.197569	33.278823
784.657106	35633.433069	33.283840
785.371394	35664.013034	33.288858
786.052288	35711.575479	33.293876
786.981012	35745.277151	33.298893
787.651575	35780.448303	33.303911
788.606268	35821.917005	33.308928
789.439822	35855.753894	33.313946
789.905694	35897.963209	33.318964
790.870372	35941.814370	33.323981
791.715526	35988.542363	33.328999
792.361902	36033.044247	33.334016
792.956801	36069.283680	33.339034
793.886050	36115.315890	33.344052
794.729255	36144.067952	33.349069
795.735234	36190.391819	33.354087
795.925274	36232.050616	33.359104
797.091023	36269.326519	33.364122
798.044255	36316.816058	33.369140
798.395433	36368.585925	33.374157
799.929625	36416.224993	33.379175
800.323638	36455.765633	33.384192
801.510227	36502.087190	33.389210
802.046748	36549.927048	33.394228
802.957725	36595.659644	33.399245
803.665736	36631.629392	33.404263
804.443097	36685.223945	33.409280
805.091246	36724.978219	33.414298
806.054084	36771.803324	33.419316
806.826072	36812.113789	33.424333
807.692657	36857.778019	33.429351
808.167028	36914.860483	33.434368
809.047645	36959.529969	33.439386
809.725255	37003.953109	33.444404
810.690333	37066.960015	33.449421
811.437082	37105.390617	33.454439
812.214486	37180.865373	33.459456
813.406266	37215.666401	33.464474
813.938496	37263.565439	33.469492
814.604945	37306.296272	33.474509
815.823293	37356.705990	33.479527
816.795594	37410.910507	33.484544
817.505446	37453.609543	33.489562
818.351443	37496.742639	33.494580
819.432303	37546.877130	33.499597
819.794167	37592.817994	33.504615
820.297995	37641.727767	33.509632
821.289805	37700.767483	33.514650
822.315168	37754.559852	33.519668
823.358562	37800.217379	33.524685
824.472258	37830.263640	33.529703
825.318952	37878.076867	33.534720
826.545393	37922.314793	33.539738
827.515989	37965.865654	33.544756
828.020165	37999.517223	33.549773
828.587842	38041.461884	33.554791
829.352226	38092.867677	33.559808
830.146050	38126.202171	33.564826
831.060124	38174.169923	33.569844
831.815111	38222.915217	33.574861
832.920605	38260.014322	33.579879
833.522878	38300.657704	33.584896
834.369061	38340.124693	33.589914
834.877233	38376.558682	33.594932
835.602957	38412.130251	33.599949
836.591540	38437.409853	33.604967
836.877724	38485.735896	33.609984
837.943805	38525.693668	33.615002
838.544477	38571.289359	33.620020
838.814915	38621.047355	33.625037
839.882986	38669.074307	33.630055
840.554658	38720.869225	33.635072
841.277359	38767.255678	33.640090
842.585831	38822.024533	33.645108
843.736665	38874.231729	33.650125
844.707175	38916.412239	33.655143
845.399295	38972.447916	33.660160
846.221781	39025.478415	33.665178
847.278797	39072.932517	33.670196
848.013412	39125.180199	33.675213
848.862297	39166.241923	33.680231
849.745136	39229.179509	33.685248
850.473016	39265.707076	33.690266
851.500591	39324.410471	33.695284
852.645084	39367.500578	33.700301
853.477310	39417.008010	33.705319
854.238772	39459.424685	33.710336
855.172937	39505.672101	33.715354
856.161138	39557.261357	33.720372
856.718824	39604.750546	33.725389
858.204849	39654.718994	33.730407
858.656966	39705.450248	33.735424
859.502451	39749.112841	33.740442
860.539302	39798.380407	33.745460
861.459984	39839.438491	33.750477
862.435110	39880.298402	33.755495
862.950636	39935.681208	33.760512
864.233425	39976.385612	33.765530
864.994984	40029.864484	33.770548
865.590505	40078.202558	33.775565
867.060431	40115.399575	33.780583
868.038603	40160.964801	33.785600
868.644321	40209.548219	33.790618
869.616944	40244.318902	33.795636
870.607920	40288.788285	33.800653
872.043719	40319.995535	33.805671
872.643091	40366.689321	33.810688
873.632465	40400.648115	33.815706
874.708730	40436.111206	33.820724
874.999971	40469.287688	33.825741
876.203240	40515.823990	33.830759
876.386788	40557.751459	33.835776
877.794200	40606.722508	33.840794
878.508664	40644.519383	33.845812
879.122571	40677.221921	33.850829
879.609118	40734.805879	33.855847
880.546205	40784.907158	33.860864
881.205741	40828.613687	33.865882
882.172614	40874.580621	33.870900
883.072139	40930.234702	33.875917
884.146595	40971.568099	33.880935
884.617861	41029.237445	33.885952
885.579976	41083.465418	33.890970
886.622333	41141.766637	33.895988
887.435369	41184.412611	33.901005
888.502359	41244.164902	33.906023
889.169551	41307.414226	33.911040
889.921067	41352.391298	33.916058
891.218474	41397.301960	33.921076
891.901278	41451.258348	33.926093
893.059369	41484.819260	33.931111
893.736480	41532.129508	33.936128
894.588195	41573.094142	33.941146
895.640160	41620.870836	33.946164
896.593386	41674.513469	33.951181
897.553637	41702.514635	33.956199
898.079031	41755.971468	33.961216
898.650049	41798.099956	33.966234
899.789030	41843.751040	33.971252
900.339022	41882.398030	33.976269
901.526844	41938.660987	33.981287
902.351251	41986.619581	33.986304
903.237969	42034.562198	33.991322
904.041707	42095.085385	33.996340
904.643189	42154.090816	34.001357
905.686519	42202.489967	34.006375
906.946409	42262.063031	34.011392
907.435858	42307.114720	34.016410
908.436204	42375.343260	34.021428
909.282216	42423.546096	34.026445
910.618328	42481.539234	34.031463
911.530104	42540.889263	34.036480
912.448581	42584.697897	34.041498
913.749933	42636.631222	34.046516
914.714570	42695.992367	34.051533
915.403974	42747.661247	34.056551
916.381873	42808.873855	34.061568
917.065758	42857.843058	34.066586
918.144698	42909.925705	34.071604
919.119016	42964.150089	34.076621
920.419449	43008.557569	34.081639
920.936192	43065.263716	34.086656
921.862643	43112.120861	34.091674
922.854325	43165.172869	34.096692
923.696347	43225.351606	34.101709
925.152619	43274.839637	34.106727
926.223359	43335.678633	34.111744
926.985792	43375.016050	34.116762
928.451354	43416.716607	34.121780
929.476066	43461.788045	34.126797
930.336551	43511.743084	34.131815
931.069363	43555.778801	34.136832
932.034749	43596.628199	34.141850
933.143917	43638.271123	34.146868
933.722785	43697.568856	34.151885
934.509180	43740.609802	34.156903
935.620638	43787.154771	34.161920
936.320070	43840.405966	34.166938
937.406476	43881.641764	34.171956
938.217024	43934.420361	34.176973
939.591847	43985.870954	34.181991
940.644937	44034.898810	34.187008
941.345891	44082.565018	34.192026
942.361221	44114.735407	34.197044
943.093256	44177.179477	34.202061
944.371231	44220.410052	34.207079
945.093359	44270.021587	34.212096
945.942052	44321.352924	34.217114
946.780658	44364.930897	34.222132
947.447208	44410.110948	34.227149
948.427691	44454.881381	34.232167
949.634332	44514.500482	34.237184
950.809268	44573.511129	34.242202
951.928738	44607.228340	34.247220
952.301975	44663.176666	34.252237
953.499177	44709.488749	34.257255
954.327723	44751.765983	34.262272
955.265101	44789.984187	34.267290
956.280595	44837.444621	34.272308
957.378778	44876.409522	34.277325
957.935361	44918.109742	34.282343
958.845529	44965.226377	34.287360
959.803185	45008.059518	34.292378
960.592579	45046.174818	34.297396
961.421116	45090.249191	34.302413
962.492008	45138.296208	34.307431
963.565872	45189.005996	34.312448
964.435825	45240.102068	34.317466
965.792387	45293.633392	34.322484
966.747124	45333.779167	34.327501
967.301533	45385.468993	34.332519
968.463505	45432.370067	34.337536
969.146799	45482.464813	34.342554
970.666998	45518.682616	34.347572
971.416918	45573.511502	34.352589
972.471912	45623.377568	34.357607
973.232168	45669.582935	34.362624
974.057403	45721.231131	34.367642
975.077633	45775.322341	34.372660
975.907620	45823.927274	34.377677
976.913886	45887.054339	34.382695
977.986919	45939.157661	34.387712
978.959327	46002.967229	34.392730
980.304015	46054.661379	34.397748
981.069216	46112.101816	34.402765
982.064499	46168.449931	34.407783
983.040493	46225.130161	34.412800
984.015976	46281.551246	34.417818
985.336826	46338.006963	34.422836
985.911239	46400.519873	34.427853
987.161130	46459.650281	34.432871
988.138175	46513.851248	34.437888
988.948655	46571.064352	34.442906
990.021153	46626.092018	34.447924
991.016989	46687.445318	34.452941
992.140769	46749.544220	34.457959
993.093085	46804.249524	34.462976
994.126028	46857.189981	34.467994
995.374168	46910.039932	34.473012
995.772126	46968.735705	34.478029
997.254622	47029.621513	34.483047
998.546154	47079.985180	34.488064
999.404424	47142.727730	34.493082
1000.638431	47195.542605	34.498100
1001.336654	47248.251703	34.503117
1002.140161	47318.664474	34.508135
1003.676267	47365.713448	34.513152
1004.541518	47417.979251	34.518170
1005.464177	47462.910251	34.523188
1006.296485	47530.352105	34.528205
1007.668382	47577.876406	34.533223
1008.700216	47631.040273	34.538240
1009.581030	47685.328708	34.543258
1010.644531	47730.636754	34.548276
1011.872429	47781.195414	34.553293
1013.113722	47845.822164	34.558311
1014.228881	47892.748349	34.563328
1014.750343	47948.706933	34.568346
1015.990220	47989.116474	34.573364
1017.028779	48041.388212	34.578381
1018.259479	48084.703237	34.583399
1019.411488	48125.917598	34.588416
1020.524316	48180.588445	34.593434
1021.109581	48204.847918	34.598452
1022.101027	48263.694529	34.603469
1023.031599	48310.163331	34.608487
1024.321125	48345.966296	34.613504
1025.193703	48394.943364	34.618522
1026.506736	48419.013201	34.623540
1027.206409	48461.273294	34.628557
1027.963415	48497.216813	34.633575
1029.061690	48528.210119	34.638592
1029.764691	48573.721805	34.643610
1030.777027	48620.545388	34.648628
1031.916162	48662.718069	34.653645
1032.784683	48711.709108	34.658663
1033.962589	48760.202614	34.663680
1034.585898	48800.893611	34.668698
1035.896358	48852.593198	34.673716
1036.726331	48909.923034	34.678733
1037.476490	48968.663729	34.683751
1038.862339	49019.681252	34.688768
1040.096701	49075.296894	34.693786
1041.475443	49121.646570	34.698804
1042.196539	49178.355116	34.703821
1043.179874	49231.713797	34.708839
1044.453760	49277.131178	34.713856
1045.101720	49340.393560	34.718874
1046.063699	49393.496560	34.723892
1047.004193	49451.310274	34.728909
1047.993203	49513.577027	34.733927
1049.321093	49566.718044	34.738944
1050.149660	49630.414817	34.743962
1051.488987	49686.509016	34.748980
1052.306395	49753.624449	34.753997
1053.066678	49815.459634	34.759015
1054.688078	49876.331323	34.764032
1055.681786	49934.011382	34.769050
1056.980392	49991.643849	34.774068
1058.131965	50055.259594	34.779085
1059.075662	50118.395566	34.784103
1060.163728	50160.699223	34.789120
1061.655416	50226.976525	34.794138
1062.641029	50286.297463	34.799156
1063.892605	50339.610398	34.804173
1064.594416	50398.507848	34.809191
1065.786272	50451.741812	34.814208
1066.934073	50503.654084	34.819226
1067.786332	50563.983660	34.824244
1068.888029	50613.094109	34.829261
1069.537658	50678.346663	34.834279
1071.116238	50725.364295	34.839296
1072.210214	50793.825132	34.844314
1073.221546	50852.991647	34.849332
1074.238169	50914.916196	34.854349
1075.532759	50963.199949	34.859367
1076.722691	51020.845682	34.864384
1077.726470	51077.963894	34.869402
1078.938885	51143.135976	34.874420
1080.041298	51184.059899	34.879437
1081.414884	51246.878560	34.884455
1083.179814	51292.096500	34.889472
1083.475376	51351.256132	34.894490
1084.435324	51404.933561	34.899508
1085.626242	51443.085317	34.904525
1086.751926	51500.761287	34.909543
1087.971450	51538.497436	34.914560
1088.820770	51593.280950	34.919578
1089.980926	51645.269785	34.924596
1091.036925	51696.142416	34.929613
1091.912041	51761.293116	34.934631
1093.360973	51797.449850	34.939648
1094.273705	51863.942719	34.944666
1095.074578	51909.015405	34.949684
1096.125951	51949.410828	34.954701
1097.000384	51997.047503	34.959719
1098.048157	52047.675415	34.964736
1099.085213	52090.503135	34.969754
1099.890951	52148.249789	34.974772
1100.748286	52188.827871	34.979789
1101.807767	52248.338433	34.984807
1103.254314	52314.786983	34.989824
1104.162580	52364.070642	34.994842
1105.605526	52417.972198	34.999860
1106.559154	52467.305924	35.004877
1107.898242	52530.677649	35.009895
1108.922830	52575.317953	35.014912
1110.560946	52632.505203	35.019930
1111.533835	52683.797986	35.024948
1112.587925	52737.862407	35.029965
1113.528079	52796.576763	35.034983
1114.815476	52844.713696	35.040000
1115.658222	52905.569731	35.045018
1117.189658	52954.712782	35.050036
1118.230101	53014.196640	35.055053
1119.223465	53072.359159	35.060071
1120.168871	53129.238436	35.065088
1121.413098	53190.247506	35.070106
1122.733881	53243.980261	35.075124
1123.885096	53302.643861	35.080141
1124.962180	53363.761814	35.085159
1126.304728	53427.350584	35.090176
1127.061070	53487.335738	35.095194
1127.940032	53536.088577	35.100212
1129.376924	53608.041379	35.105229
1130.186334	53668.164233	35.110247
1131.334501	53733.872526	35.115264
1132.729871	53795.574584	35.120282
1134.173892	53860.654730	35.125300
1135.047555	53917.059884	35.130317
1135.961541	53990.475256	35.135335
1137.030648	54052.627741	35.140352
1138.513523	54117.924002	35.145370
1139.902956	54164.933916	35.150388
1141.411853	54228.992414	35.155405
1142.343172	54288.452289	35.160423
1143.700413	54347.845633	35.165440
1145.063109	54399.789909	35.170458
1146.090785	54457.146798	35.175476
1147.727073	54505.276822	35.180493
1148.313727	54570.543784	35.185511
1149.584823	54615.174697	35.190528
1150.488270	54666.356120	35.195546
1151.629631	54731.289879	35.200564
1152.998865	54779.304063	35.205581
1154.041023	54844.778919	35.210599
1155.225124	54902.574374	35.215616
1156.300874	54953.375054	35.220634
1157.761675	55006.324182	35.225652
1158.956407	55056.669796	35.230669
1159.953163	55120.513458	35.235687
1161.167695	55163.553166	35.240704
1162.402002	55223.847619	35.245722
1163.580656	55272.848244	35.250740
1164.835734	55320.457392	35.255757
1165.959669	55374.808056	35.260775
1167.044805	55418.570951	35.265792
1168.242517	55473.397589	35.270810
1169.363477	55538.469656	35.275828
1170.526746	55584.334367	35.280845
1171.268754	55644.510776	35.285863
1172.672192	55692.369575	35.290880
1173.475158	55738.639064	35.295898
1174.625472	55788.518542	35.300916
1175.730069	55843.366941	35.305933
1176.849973	55886.112673	35.310951
1177.882365	55947.712638	35.315968
1179.392080	55993.941596	35.320986
1180.316088	56046.445478	35.326004
1181.824184	56088.637164	35.331021
1182.872663	56138.767483	35.336039
1184.304546	56188.850543	35.341056
1185.219241	56234.641508	35.346074
1186.152246	56293.732756	35.351092
1187.349124	56344.004823	35.356109
1188.662164	56401.207827	35.361127
1189.907092	56455.668598	35.366144
1191.062482	56516.674858	35.371162
1192.038443	56577.260015	35.376180
1193.698583	56639.124237	35.381197
1194.361418	56705.068651	35.386215
1195.662351	56759.901082	35.391232
1197.174170	56813.384213	35.396250
1198.237055	56873.165400	35.401268
1199.845732	56936.506759	35.406285
1200.811077	56992.594758	35.411303
1201.968642	57049.380628	35.416320
1203.470554	57115.030260	35.421338
1204.310778	57174.821742	35.426356
1205.850552	57212.548519	35.431373
1206.886775	57291.752330	35.436391
1208.353210	57355.705667	35.441408
1209.691414	57412.350196	35.446426
1210.579990	57465.862736	35.451444
1211.951350	57525.078274	35.456461
1213.026141	57589.612532	35.461479
1214.756289	57644.791190	35.466496
1215.909668	57698.927353	35.471514
1217.286679	57762.838812	35.476532
1218.759584	57816.159391	35.481549
1219.814785	57877.343030	35.486567
1220.858770	57923.958769	35.491584
1222.233073	57973.130522	35.496602
1223.376441	58035.756480	35.501620
1224.847145	58083.242451	35.506637
1225.729820	58149.985545	35.511655
1226.411509	58207.279041	35.516672
1228.135372	58267.947593	35.521690
1229.166537	58322.218217	35.526708
1231.213864	58384.152920	35.531725
1232.057585	58440.636768	35.536743
1233.305518	58494.804224	35.541760
1234.328159	58547.241179	35.546778
1235.305528	58617.065796	35.551796
1236.709102	58662.987407	35.556813
1237.851797	58740.900777	35.561831
1239.433842	58797.042018	35.566848
1240.458856	58852.973107	35.571866
1241.776523	58922.295942	35.576884
1243.287118	58972.910504	35.581901
1244.672315	59031.595905	35.586919
1245.731694	59073.945385	35.591936
1246.877905	59128.579580	35.596954
1248.494556	59175.911938	35.601972
1249.790332	59237.472782	35.606989
1251.170099	59291.184646	35.612007
1252.255663	59347.518819	35.617024
1253.023764	59394.446428	35.622042
1254.400284	59452.545557	35.627060
1255.885680	59490.480644	35.632077
1256.992692	59539.267019	35.637095
1257.966546	59581.054779	35.642112
1259.512452	59625.430497	35.647130
1260.143173	59675.139877	35.652148
1261.641370	59712.953046	35.657165
1262.774398	59772.616507	35.662183
1263.450592	59823.084961	35.667200
1265.207452	59875.656712	35.672218
1265.922035	59940.620755	35.677236
1267.426601	59987.738046	35.682253
1268.770279	60051.027800	35.687271
1269.748462	60105.367678	35.692288
1270.983023	60177.289650	35.697306
1272.112227	60238.252455	35.702324
1273.652537	60297.916743	35.707341
1275.079786	60368.922941	35.712359
1276.131940	60426.480170	35.717376
1277.352537	60492.404562	35.722394
1278.695349	60562.297824	35.727412
1280.071447	60615.145994	35.732429
1281.460796	60689.292354	35.737447
1282.788790	60750.997568	35.742464
1284.481260	60815.601968	35.747482
1285.436964	60887.075943	35.752500
1287.021196	60943.481332	35.757517
1288.560524	61003.622246	35.762535
1289.682643	61069.057207	35.767552
1290.927386	61129.478755	35.772570
1292.358751	61190.782764	35.777588
1293.883618	61255.389241	35.782605
1294.912942	61311.021453	35.787623
1296.438846	61384.357280	35.792640
1297.841560	61423.397101	35.797658
1299.422240	61497.439992	35.802676
1300.697277	61541.741329	35.807693
1302.150931	61604.245608	35.812711
1303.378615	61665.361131	35.817728
1304.877339	61717.844325	35.822746
1305.923824	61777.159070	35.827764
1307.319392	61840.097163	35.832781
1308.405936	61897.677780	35.837799
1309.199336	61963.337493	35.842816
1310.890939	62024.102755	35.847834
1312.738981	62073.835338	35.852852
1313.811038	62135.906939	35.857869
1315.309518	62188.175945	35.862887
1316.215249	62259.148972	35.867904
1318.050395	62319.702584	35.872922
1319.076412	62385.649853	35.877940
1320.204430	62434.900823	35.882957
1321.759797	62508.260704	35.887975
1323.071716	62560.464747	35.892992
1324.438993	62610.906711	35.898010
1325.878351	62670.921752	35.903028
1327.063547	62723.013035	35.908045
1328.641042	62785.380643	35.913063
1329.615277	62848.216337	35.918080
1331.351411	62903.804804	35.923098
1332.519030	62969.585860	35.928116
1334.122911	63018.883782	35.933133
1335.563311	63074.373323	35.938151
1336.406202	63136.869469	35.943168
1337.519750	63189.852894	35.948186
1338.682243	63242.278011	35.953204
1340.409779	63300.147717	35.958221
1341.303032	63364.877577	35.963239
1342.873967	63420.784271	35.968256
1344.112113	63480.864421	35.973274
1345.112796	63543.064668	35.978292
1346.534414	63590.201855	35.983309
1347.660077	63641.031923	35.988327
1348.833178	63698.198011	35.993344
1350.157528	63753.460338	35.998362
1351.440440	63813.243071	36.003380
1352.777679	63880.228140	36.008397
1353.847679	63933.935338	36.013415
1355.204803	64008.552515	36.018432
1356.664383	64067.763757	36.023450
1358.246514	64140.712767	36.028468
1359.833070	64202.253177	36.033485
1360.971999	64253.835783	36.038503
1362.026728	64323.531540	36.043520
1363.574879	64390.022810	36.048538
1364.620633	64466.070217	36.053556
1365.874586	64531.848210	36.058573
1367.907710	64599.612603	36.063591
1369.400093	64670.494337	36.068608
1370.929966	64730.158302	36.073626
1372.111128	64800.766242	36.078644
1374.077269	64864.806572	36.083661
1375.218670	64927.545360	36.088679
1376.718529	65001.244149	36.093696
1378.085494	65063.821349	36.098714
1379.743298	65127.467443	36.103732
1380.761896	65185.211912	36.108749
1382.381661	65257.360567	36.113767
1383.981140	65323.162520	36.118784
1385.552148	65386.493640	36.123802
1386.234221	65445.443643	36.128820
1387.903276	65509.981631	36.133837
1389.589816	65572.313807	36.138855
1390.653006	65641.334458	36.143872
1392.333900	65702.515567	36.148890
1393.675944	65769.922786	36.153908
1395.104965	65839.133631	36.158925
1396.619330	65903.076380	36.163943
1397.779999	65969.752775	36.168960
1399.265481	66031.199525	36.173978
1400.592276	66094.311066	36.178996
1402.372547	66166.677787	36.184013
1404.106630	66230.226088	36.189031
1405.246525	66291.588276	36.194048
1406.610101	66358.322571	36.199066
1408.116032	66418.633750	36.204084
1409.098338	66482.490300	36.209101
1410.511336	66547.355931	36.214119
1412.166764	66620.174025	36.219136
1413.485123	66679.223575	36.224154
1414.838212	66754.552304	36.229172
1416.278857	66828.822860	36.234189
1418.098431	66892.650687	36.239207
1418.998050	66960.440567	36.244224
1420.746426	67015.510724	36.249242
1422.082088	67087.025263	36.254260
1423.483663	67154.673774	36.259277
1425.180384	67212.329383	36.264295
1426.208465	67289.489736	36.269312
1428.149693	67345.410511	36.274330
1429.170194	67414.069098	36.279348
1430.520891	67479.750972	36.284365
1432.038774	67538.492694	36.289383
1433.336750	67611.432890	36.294400
1434.797296	67671.158967	36.299418
1436.566679	67740.068447	36.304436
1437.651054	67811.174798	36.309453
1439.379342	67861.944369	36.314471
1440.409415	67913.728767	36.319488
1441.711593	67967.173919	36.324506
1443.136101	68021.549798	36.329524
1444.743626	68075.688198	36.334541
1446.107988	68128.471781	36.339559
1447.194259	68189.859595	36.344576
1448.554012	68241.985625	36.349594
1450.246759	68305.001041	36.354612
1451.573774	68370.942183	36.359629
1453.498164	68417.085243	36.364647
1454.492717	68485.769758	36.369664
1456.070323	68546.935888	36.374682
1457.432704	68602.975349	36.379700
1458.234914	68674.210571	36.384717
1460.542870	68731.064759	36.389735
1461.717918	68814.981869	36.394752
1463.576409	68869.456249	36.399770
1465.146328	68943.123833	36.404788
1466.151499	69005.773691	36.409805
1467.591512	69066.114103	36.414823
1469.322639	69159.120386	36.419840
1471.442206	69223.305995	36.424858
1472.816572	69291.781239	36.429876
1473.978393	69348.436265	36.434893
1475.685404	69416.967420	36.439911
1477.014688	69478.282276	36.444928
1478.382501	69544.859581	36.449946
1479.773448	69618.189841	36.454964
1480.922096	69690.500761	36.459981
1482.674974	69761.355888	36.464999
1484.547129	69837.587578	36.470016
1486.363364	69908.053257	36.475034
1487.659106	69973.249855	36.480052
1488.873229	70042.258744	36.485069
1490.677406	70110.200291	36.490087
1492.168257	70186.005102	36.495104
1493.919235	70260.426970	36.500122
1495.378875	70315.530407	36.505140
1496.752579	70388.681905	36.510157
1498.374782	70457.425389	36.515175
1499.520561	70520.177212	36.520192
1500.985955	70595.315969	36.525210
1502.819358	70662.342522	36.530228
1504.205241	70727.615556	36.535245
1505.796423	70797.757926	36.540263
1507.396354	70872.838431	36.545280
1509.028856	70945.723018	36.550298
1510.775034	71009.357246	36.555316
1511.919399	71081.115440	36.560333
1513.823168	71140.786504	36.565351
1515.176316	71214.361482	36.570368
1516.520104	71272.195402	36.575386
1517.795333	71349.937110	36.580404
1519.560865	71419.407939	36.585421
1521.214680	71485.210862	36.590439
1522.745238	71563.951789	36.595456
1524.403225	71618.444334	36.600474
1526.003661	71681.609064	36.605492
1527.531698	71753.397705	36.610509
1528.934122	71810.501712	36.615527
1530.505543	71888.236653	36.620544
1532.052377	71943.621184	36.625562
1533.827802	72009.507714	36.630580
1534.969933	72076.519434	36.635597
1536.464923	72136.092097	36.640615
1538.298829	72204.059772	36.645632
1539.504429	72270.910067	36.650650
1541.269172	72330.276297	36.655668
1542.481460	72386.803367	36.660685
1543.964688	72429.064612	36.665703
1545.270398	72497.926319	36.670720
1546.933014	72549.570292	36.675738
1548.412263	72595.974118	36.680756
1549.536399	72653.452821	36.685773
1551.312982	72710.436893	36.690791
1552.340737	72774.061189	36.695808
1554.153285	72844.516362	36.700826
1555.588053	72908.001282	36.705844
1557.200684	72974.865648	36.710861
1558.867456	73039.517835	36.715879
1560.344443	73114.332671	36.720896
1561.922383	73184.268165	36.725914
1563.790136	73252.258577	36.730932
1565.261249	73335.447219	36.735949
1566.860831	73385.456102	36.740967
1568.035759	73466.145620	36.745984
1569.684483	73544.658641	36.751002
1571.637733	73616.398464	36.756020
1572.968694	73698.926203	36.761037
1574.371851	73763.393421	36.766055
1576.084123	73848.559865	36.771072
1577.344493	73930.060728	36.776090
1579.317349	74005.421117	36.781108
1581.033262	74074.767373	36.786125
1582.537941	74156.180024	36.791143
1584.413856	74233.240872	36.796160
1585.903365	74320.900993	36.801178
1587.534151	74386.436083	36.806196
1588.806795	74471.128657	36.811213
1590.763644	74556.309747	36.816231
1592.525826	74629.462871	36.821248
1594.105349	74706.660140	36.826266
1595.849896	74782.805794	36.831284
1597.468306	74853.423343	36.836301
1599.259885	74932.576763	36.841319
1600.738923	75012.514012	36.846336
1602.574075	75088.659022	36.851354
1604.724541	75148.629868	36.856372
1606.112343	75218.815794	36.861389
1607.712049	75283.027911	36.866407
1609.309698	75354.397382	36.871424
1611.071194	75417.609136	36.876442
1612.569645	75490.375205	36.881460
1614.320501	75562.417942	36.886477
1615.769218	75633.368113	36.891495
1617.529298	75705.131110	36.896512
1618.926908	75780.890540	36.901530
1620.701481	75842.695183	36.906548
1622.197877	75910.661813	36.911565
1623.845786	75980.923023	36.916583
1625.599171	76046.379643	36.921600
1627.252097	76123.050128	36.926618
1629.112182	76192.936664	36.931636
1630.634058	76258.797387	36.936653
1631.990820	76323.290688	36.941671
1633.986358	76388.431554	36.946688
1635.427321	76457.497642	36.951706
1637.318721	76523.123831	36.956724
1638.161750	76590.105011	36.961741
1639.946308	76668.504572	36.966759
1641.890714	76730.842046	36.971776
1643.268434	76818.692471	36.976794
1644.830313	76886.271271	36.981812
1646.469945	76954.053423	36.986829
1648.009618	77033.315769	36.991847
1649.481386	77102.213995	36.996864
1650.961494	77174.290731	37.001882
1652.862027	77229.276171	37.006900
1654.020175	77294.955644	37.011917
1655.730462	77357.432541	37.016935
1657.663830	77427.488142	37.021952
1659.089577	77491.099327	37.026970
1660.263225	77546.984588	37.031988
1661.994308	77631.374622	37.037005
1663.780478	77706.977273	37.042023
1665.085795	77775.181165	37.047040
1666.722279	77848.730055	37.052058
1668.363684	77930.145349	37.057076
1669.936192	78007.910536	37.062093
1671.637146	78083.717589	37.067111
1673.759070	78167.744071	37.072128
1675.181669	78256.858934	37.077146
1676.814961	78339.974281	37.082164
1678.362015	78425.649738	37.087181
1680.386536	78513.543738	37.092199
1682.326029	78593.824859	37.097216
1683.507149	78681.623356	37.102234
1685.723994	78765.421446	37.107252
1687.063563	78848.229575	37.112269
1688.653773	78936.610963	37.117287
1691.089788	79020.008136	37.122304
1692.550765	79110.690680	37.127322
1694.690748	79193.551943	37.132340
1696.530831	79271.481528	37.137357
1697.901375	79355.464535	37.142375
1699.637275	79440.366126	37.147392
1701.348437	79519.127397	37.152410
1703.126843	79604.922338	37.157428
1705.029052	79693.776749	37.162445
1706.800874	79780.295399	37.167463
1708.711228	79854.655615	37.172480
1710.138690	79937.567272	37.177498
1711.969026	80011.978441	37.182516
1713.505580	80100.219911	37.187533
1715.609027	80188.005533	37.192551
1717.438487	80270.741248	37.197568
1718.718177	80355.957754	37.202586
1720.908823	80423.041430	37.207604
1722.231929	80515.954615	37.212621
1723.780619	80590.005987	37.217639
1726.049206	80682.949136	37.222656
1727.764752	80766.768389	37.227674
1729.582787	80842.374641	37.232692
1731.227787	80929.284128	37.237709
1732.899833	81017.786029	37.242727
1734.940246	81089.671280	37.247744
1736.492603	81176.431328	37.252762
1738.569630	81260.157481	37.257780
1740.724220	81335.927784	37.262797
1741.830457	81411.963715	37.267815
1743.685544	81495.699965	37.272832
1745.517475	81572.712371	37.277850
1747.366791	81643.894099	37.282868
1749.138374	81719.129891	37.287885
1750.873408	81810.969309	37.292903
1752.672040	81884.807611	37.297920
1754.081553	81970.591534	37.302938
1756.093732	82029.902231	37.307956
1758.198101	82111.992204	37.312973
1759.551653	82194.998136	37.317991
1761.080481	82254.980449	37.323008
1763.202121	82347.508657	37.328026
1765.054927	82413.763062	37.333044
1766.322255	82498.430515	37.338061
1767.928976	82547.720187	37.343079
1769.853803	82610.264045	37.348096
1771.350970	82684.531731	37.353114
1772.562850	82748.125074	37.358132
1774.658822	82814.557763	37.363149
1775.780069	82887.275662	37.368167
1777.622533	82970.992931	37.373184
1779.262941	83048.026669	37.378202
1780.694397	83125.688834	37.383220
1782.739101	83214.988248	37.388237
1784.125263	83298.271065	37.393255
1785.922344	83386.596115	37.398272
1787.473112	83485.527393	37.403290
1789.370284	83573.545933	37.408308
1791.017468	83668.724874	37.413325
1792.957997	83776.263019	37.418343
1794.716288	83858.602276	37.423360
1796.529374	83965.603557	37.428378
1798.386540	84073.814757	37.433396
1800.823359	84167.756742	37.438413
1802.366793	84269.074039	37.443431
1804.058482	84354.440868	37.448448
1805.996342	84459.802565	37.453466
1808.265412	84557.522751	37.458484
1810.289591	84657.359682	37.463501
1812.154978	84751.975885	37.468519
1813.935857	84842.132636	37.473536
1816.051357	84928.638631	37.478554
1817.641283	85027.417049	37.483572
1820.105943	85109.738063	37.488589
1821.703310	85209.238214	37.493607
1823.887484	85291.502268	37.498624
1826.249029	85379.922536	37.503642
1827.477957	85460.157043	37.508660
1829.462082	85548.117351	37.513677
1831.038643	85646.646547	37.518695
1833.265546	85727.828065	37.523712
1834.764446	85821.592764	37.528730
1836.710284	85909.002604	37.533748
1838.721652	86003.524037	37.538765
1840.555808	86079.547196	37.543783
1842.432380	86179.551884	37.548800
1844.293776	86265.049877	37.553818
1846.070570	86354.882517	37.558836
1848.155134	86445.224843	37.563853
1850.108123	86525.501057	37.568871
1851.830564	86615.355680	37.573888
1853.558865	86702.586524	37.578906
1855.668311	86792.964053	37.583924
1857.512049	86876.033543	37.588941
1859.259998	86969.395476	37.593959
1861.295229	87045.567108	37.598976
1862.932131	87140.480314	37.603994
1864.451424	87228.011555	37.609012
1866.534428	87309.334064	37.614029
1868.402648	87412.284291	37.619047
1870.354763	87498.151878	37.624064
1872.543136	87591.636965	37.629082
1873.666084	87676.735076	37.634100
1875.898254	87763.434025	37.639117
1877.075645	87855.392695	37.644135
1879.497827	87948.563534	37.649152
1881.261314	88048.795078	37.654170
1883.102323	88148.583957	37.659188
1885.292161	88229.917647	37.664205
1886.987448	88323.304802	37.669223
1889.127832	88415.114527	37.674240
1891.176605	88500.209544	37.679258
1892.488262	88581.592913	37.684276
1894.369977	88645.081733	37.689293
1896.146245	88727.786832	37.694311
1897.718024	88795.912115	37.699328
1899.554983	88875.604615	37.704346
1901.332980	88965.305658	37.709364
1903.007691	89045.708354	37.714381
1904.699708	89137.729890	37.719399
1906.998723	89230.467816	37.724416
1908.164939	89325.715178	37.729434
1910.032668	89418.331079	37.734452
1912.115883	89520.900165	37.739469
1913.663331	89621.094798	37.744487
1915.788098	89727.865669	37.749504
1917.773073	89826.661816	37.754522
1919.465516	89950.901856	37.759540
1921.531009	90038.584075	37.764557
1923.628748	90153.801311	37.769575
1925.326304	90268.777442	37.774592
1927.432105	90379.178283	37.779610
1929.046787	90491.975682	37.784628
1931.775248	90595.714870	37.789645
1933.303681	90714.812821	37.794663
1935.661501	90827.064283	37.799680
1937.901914	90934.493079	37.804698
1939.880873	91043.167202	37.809716
1942.254998	91143.693835	37.814733
1943.888104	91256.592610	37.819751
1945.970874	91359.890487	37.824768
1948.009557	91468.480753	37.829786
1949.692918	91577.279099	37.834804
1952.147354	91679.379231	37.839821
1953.650978	91787.940299	37.844839
1955.635818	91888.188118	37.849856
1957.757428	91999.568349	37.854874
1959.526012	92115.174126	37.859892
1961.875048	92217.964313	37.864909
1963.544700	92331.089515	37.869927
1965.601990	92446.448584	37.874944
1967.485553	92555.979587	37.879962
1969.337514	92669.571830	37.884980
1971.710069	92779.546786	37.889997
1973.332396	92906.281522	37.895015
1975.403909	93017.584593	37.900032
1977.676127	93126.651236	37.905050
1979.373804	93248.787293	37.910068
1981.420657	93346.900822	37.915085
1983.393254	93469.590465	37.920103
1985.635307	93587.764136	37.925120
1987.689872	93702.545317	37.930138
1989.387195	93819.081297	37.935156
1991.693208	93932.150869	37.940173
1993.350588	94041.811302	37.945191
1995.346755	94151.292362	37.950208
1997.784232	94259.044288	37.955226
1999.722403	94377.902308	37.960244
2001.658820	94487.343208	37.965261
2003.594806	94608.053069	37.970279
2005.566348	94714.282377	37.975296
2007.559484	94823.157865	37.980314
2009.440413	94943.066409	37.985332
2011.163204	95067.791564	37.990349
2013.126294	95196.256986	37.995367
2015.141942	95306.055973	38.000384
2017.496062	95429.352838	38.005402
2019.557205	95539.842701	38.010420
2021.316110	95659.481553	38.015437
2022.949562	95779.901050	38.020455
2025.001832	95875.410503	38.025472
2026.803367	95985.498904	38.030490
2028.626958	96092.985642	38.035508
2030.469314	96187.603540	38.040525
2032.379563	96305.471875	38.045543
2034.474294	96415.629996	38.050560
2036.342108	96534.621339	38.055578
2038.098506	96650.930509	38.060596
2040.078546	96764.175466	38.065613
2042.201313	96896.197613	38.070631
2044.255695	97029.359219	38.075648
2046.331438	97148.789376	38.080666
2047.869091	97287.078171	38.085684
2049.992045	97406.362472	38.090701
2051.822535	97547.141907	38.095719
2053.921626	97693.926740	38.100736
2056.055729	97824.746699	38.105754
2058.052024	97982.324216	38.110772
2060.150545	98114.824279	38.115789
2062.158380	98259.775175	38.120807
2064.826014	98410.112641	38.125824
2066.970534	98544.965219	38.130842
2069.054026	98686.103092	38.135860
2071.155595	98826.566869	38.140877
2073.177043	98974.764234	38.145895
2074.959932	99117.827274	38.150912
2077.625794	99256.062177	38.155930
2079.185416	99403.192817	38.160948
2081.483502	99560.109688	38.165965
2083.998272	99705.520256	38.170983
2086.280088	99852.299075	38.176000
2088.705295	99983.766895	38.181018
2090.881476	100124.959967	38.186036
2093.247429	100263.106660	38.191053
2095.532876	100399.377547	38.196071
2097.489671	100526.103296	38.201088
2099.864114	100676.383123	38.206106
2101.653833	100817.069168	38.211124
2103.623699	100957.106413	38.216141
2106.079411	101090.222087	38.221159
2108.384217	101224.376165	38.226176
2110.537592	101351.961840	38.231194
2112.045481	101502.368377	38.236212
2114.648291	101627.209702	38.241229
2116.368029	101772.398919	38.246247
2118.216862	101911.432243	38.251264
2120.620793	102049.048068	38.256282
2122.727152	102204.359488	38.261300
2125.058233	102339.946691	38.266317
2127.343171	102487.472236	38.271335
2129.612766	102633.745654	38.276352
2131.432157	102771.823636	38.281370
2133.209732	102915.753647	38.286388
2135.319979	103060.963511	38.291405
2137.175774	103217.117659	38.296423
2139.545233	103367.068245	38.301440
2141.328247	103515.830683	38.306458
2143.171126	103675.450369	38.311476
2145.277839	103828.804093	38.316493
2148.085149	103979.982204	38.321511
2149.948685	104131.701715	38.326528
2152.197229	104292.059669	38.331546
2154.263058	104441.770965	38.336564
2156.456010	104581.547749	38.341581
2158.061051	104745.444667	38.346599
2160.592778	104897.342045	38.351616
2162.808974	105058.647002	38.356634
2164.694408	105216.137192	38.361652
2166.887580	105354.839382	38.366669
2168.821117	105494.457665	38.371687
2170.726233	105627.398720	38.376704
2173.294857	105768.947539	38.381722
2174.905135	105917.024876	38.386740
2176.616237	106066.697437	38.391757
2178.470740	106222.320506	38.396775
2180.280213	106369.886807	38.401792
2182.802203	106527.549769	38.406810
2184.817723	106701.548698	38.411828
2186.989004	106863.718829	38.416845
2188.862911	107033.912167	38.421863
2191.438233	107206.202996	38.426880
2193.610908	107372.648601	38.431898
2195.714891	107560.637251	38.436916
2197.894626	107739.434339	38.441933
2200.009198	107923.200677	38.446951
2202.010879	108109.661282	38.451968
2204.669534	108284.708856	38.456986
2206.088061	108481.229782	38.462004
2208.113310	108667.816507	38.467021
2210.592805	108862.740654	38.472039
2213.119469	109056.365044	38.477056
2215.698404	109251.466022	38.482074
2217.468736	109459.832312	38.487092
2219.648941	109650.711651	38.492109
2221.992022	109842.403513	38.497127
2224.295958	110047.570199	38.502144
2226.755534	110246.842203	38.507162
2229.004988	110439.122627	38.512180
2231.755902	110637.970813	38.517197
2234.026160	110834.168750	38.522215
2236.344037	111035.952979	38.527232
2239.009459	111214.387459	38.532250
2241.020266	111428.371146	38.537268
2243.569932	111609.641099	38.542285
2246.141584	111791.986505	38.547303
2248.422855	111987.681792	38.552320
2251.002084	112163.217618	38.557338
2253.148675	112361.941689	38.562356
2255.619866	112539.132263	38.567373
2257.758973	112716.160063	38.572391
2260.134924	112905.301437	38.577408
2262.652903	113091.606069	38.582426
2264.386067	113272.213150	38.587444
2266.646304	113448.540728	38.592461
2269.216711	113648.245543	38.597479
2271.476965	113840.656664	38.602496
2273.816467	114023.861364	38.607514
2275.882936	114202.074597	38.612532
2277.781386	114401.875981	38.617549
2279.856497	114600.090806	38.622567
2282.495652	114792.853517	38.627584
2284.722428	114976.385010	38.632602
2286.290459	115190.447495	38.637620
2289.075697	115386.259797	38.642637
2291.614564	115570.024452	38.647655
2293.711991	115780.139109	38.652672
2296.281287	115968.492377	38.657690
2298.434707	116164.496422	38.662708
2300.608660	116361.880801	38.667725
2302.949087	116565.987899	38.672743
2305.313429	116762.558222	38.677760
2307.648003	116945.600606	38.682778
2309.760596	117148.224464	38.687796
2311.742562	117346.062635	38.692813
2314.477390	117545.623247	38.697831
2316.117470	117747.170004	38.702848
2318.463014	117919.345152	38.707866
2320.564192	118115.608556	38.712884
2322.726953	118292.164677	38.717901
2325.236262	118478.789494	38.722919
2326.687449	118672.341540	38.727936
2329.128601	118874.225598	38.732954
2331.384842	119066.512099	38.737972
2333.168933	119255.955975	38.742989
2335.363892	119468.346465	38.748007
2338.170356	119696.206624	38.753024
2340.253107	119892.532779	38.758042
2342.370542	120106.511832	38.763060
2344.642416	120322.357965	38.768077
2347.265716	120548.552029	38.773095
2349.296055	120771.567422	38.778112
2351.734788	120995.725295	38.783130
2354.018751	121222.230065	38.788148
2356.053357	121459.354698	38.793165
2358.835631	121690.744181	38.798183
2361.395490	121914.368269	38.803200
2363.849024	122147.740060	38.808218
2366.024658	122387.347279	38.813236
2368.030354	122622.821632	38.818253
2370.729298	122862.375234	38.823271
2372.696942	123117.787801	38.828288
2375.322076	123346.687083	38.833306
2378.317946	123596.778704	38.838324
2380.511198	123839.994741	38.843341
2383.148954	124076.317574	38.848359
2385.153388	124325.921848	38.853376
2387.647068	124582.174870	38.858394
2389.867721	124823.603796	38.863412
2392.305667	125081.505243	38.868429
2394.878369	125340.909631	38.873447
2397.413501	125581.164765	38.878464
2399.878131	125829.602569	38.883482
2402.239261	126084.261900	38.888500
2404.745373	126342.490510	38.893517
2407.262711	126587.854446	38.898535
2409.664141	126856.455183	38.903552
2412.109642	127106.235828	38.908570
2414.563540	127353.999408	38.913588
2416.859145	127611.063594	38.918605
2419.360827	127870.736090	38.923623
2421.629502	128125.498568	38.928640
2424.608201	128374.975040	38.933658
2426.747805	128625.662697	38.938676
2429.027768	128897.848089	38.943693
2431.815756	129151.469787	38.948711
2434.294412	129419.478580	38.953728
2436.901653	129671.951703	38.958746
2439.451929	129927.594530	38.963764
2441.693036	130191.204568	38.968781
2443.920049	130446.685372	38.973799
2446.299582	130710.632216	38.978816
2448.811697	130970.106368	38.983834
2451.168188	131231.763437	38.988852
2453.239975	131506.967073	38.993869
2456.391008	131766.028842	38.998887
2458.752897	132023.134679	39.003904
2460.873863	132283.274231	39.008922
2463.496889	132541.255847	39.013940
2465.561111	132809.337831	39.018957
2468.206638	133073.536549	39.023975
2470.530786	133353.584833	39.028992
2473.174233	133618.611914	39.034010
2475.484652	133895.062088	39.039028
2477.805277	134148.557696	39.044045
2480.093769	134395.359859	39.049063
2482.760798	134650.720199	39.054080
2484.917984	134894.373324	39.059098
2487.393317	135145.261735	39.064116
2489.823519	135385.144111	39.069133
2492.659420	135641.663772	39.074151
2494.393208	135904.346793	39.079168
2496.890854	136168.878748	39.084186
2499.173538	136429.473955	39.089204
2501.547705	136698.571232	39.094221
2504.003028	136969.979650	39.099239
2506.515222	137249.832319	39.104256
2508.486450	137522.931342	39.109274
2511.074483	137802.800869	39.114292
2513.362652	138099.533561	39.119309
2515.644019	138389.137237	39.124327
2517.944704	138694.729594	39.129344
2520.363570	138992.691154	39.134362
2522.820722	139304.227518	39.139380
2525.214765	139618.174335	39.144397
2527.688489	139927.009084	39.149415
2529.972326	140250.127327	39.154432
2532.828941	140579.858955	39.159450
2535.270946	140891.687246	39.164468
2537.681662	141221.112280	39.169485
2540.340747	141538.977124	39.174503
2543.109120	141877.437537	39.179520
2545.815421	142213.638255	39.184538
2548.214714	142542.782103	39.189556
2550.579144	142884.536271	39.194573
2553.095354	143212.143312	39.199591
2555.656549	143552.944824	39.204608
2557.995522	143892.082728	39.209626
2561.330502	144218.921032	39.214644
2564.030304	144567.767096	39.219661
2566.840830	144891.912267	39.224679
2569.602014	145239.446083	39.229696
2573.101733	145573.374953	39.234714
2575.613777	145889.107474	39.239732
2577.822239	146215.957148	39.244749
2580.485806	146554.554359	39.249767
2583.262565	146891.257586	39.254784
2585.555320	147234.258073	39.259802
2588.112909	147557.139572	39.264820
2590.516352	147889.439807	39.269837
2593.307937	148219.307866	39.274855
2595.759983	148563.713707	39.279872
2598.573799	148897.796559	39.284890
2601.153053	149235.751500	39.289908
2603.756490	149582.602691	39.294925
2606.847682	149912.434353	39.299943
2609.127163	150255.684890	39.304960
2611.777752	150592.507463	39.309978
2614.515307	150937.455027	39.314996
2616.854470	151285.450060	39.320013
2619.481852	151613.435127	39.325031
2621.816194	151968.594424	39.330048
2624.344670	152315.131927	39.335066
2627.115582	152653.522278	39.340084
2628.982888	153012.150518	39.345101
2631.356895	153358.413963	39.350119
2633.953719	153730.578725	39.355136
2636.441324	154095.044933	39.360154
2639.195040	154459.509918	39.365172
2641.573474	154828.377375	39.370189
2644.604422	155191.496100	39.375207
2647.510303	155567.356551	39.380224
2649.188607	155928.228695	39.385242
2652.325337	156267.243231	39.390260
2654.781872	156612.853112	39.395277
2657.096883	156959.870874	39.400295
2659.315767	157308.505242	39.405312
2661.672427	157664.216565	39.410330
2663.913516	158014.489197	39.415348
2666.453726	158392.417788	39.420365
2668.843928	158762.704290	39.425383
2670.949890	159148.487620	39.430400
2673.368236	159535.417864	39.435418
2675.965365	159932.390026	39.440436
2678.575911	160342.477072	39.445453
2680.830956	160751.060839	39.450471
2683.755661	161157.993632	39.455488
2686.009404	161588.381464	39.460506
2688.340308	162018.810899	39.465524
2690.710795	162451.623847	39.470541
2693.716873	162883.375370	39.475559
2696.027473	163330.334177	39.480576
2698.725416	163779.457263	39.485594
2701.511899	164223.237107	39.490612
2703.688371	164682.020823	39.495629
2706.365859	165146.264947	39.500647
2709.022455	165610.756747	39.505664
2712.037775	166086.165467	39.510682
2714.962449	166559.153874	39.515700
2717.564958	167046.225838	39.520717
2720.692337	167514.554683	39.525735
2723.698824	167990.663382	39.530752
2726.327592	168471.417970	39.535770
2728.954905	168937.815548	39.540788
2732.247705	169423.386406	39.545805
2735.299737	169892.885280	39.550823
2737.799972	170370.028384	39.555840
2740.985517	170856.234925	39.560858
2743.835165	171323.222291	39.565876
2746.365770	171806.629662	39.570893
2749.023205	172287.925134	39.575911
2751.802234	172773.255183	39.580928
2754.852605	173267.523204	39.585946
2757.772757	173730.946028	39.590964
2760.166898	174221.424395	39.595981
2763.178185	174709.142646	39.600999
2765.822790	175204.438503	39.606016
2768.732425	175697.041982	39.611034
2771.494259	176186.128693	39.616052
2774.006623	176683.358865	39.621069
2776.813627	177174.196664	39.626087
2779.558820	177675.993103	39.631104
2782.170245	178172.200610	39.636122
2785.028073	178663.115163	39.641140
2788.165320	179157.315837	39.646157
2790.913781	179656.380228	39.651175
2793.852096	180166.999097	39.656192
2796.595013	180666.044549	39.661210
2799.407367	181159.875255	39.666228
2802.507582	181670.502580	39.671245
2805.157950	182167.538734	39.676263
2808.446391	182655.816823	39.681280
2810.508193	183234.581291	39.686298
2813.395762	183738.014325	39.691316
2816.187900	184238.086809	39.696333
2818.784346	184749.672759	39.701351
2821.782975	185260.258634	39.706368
2824.208065	185765.983904	39.711386
2827.161003	186271.832286	39.716404
2829.776962	186792.416725	39.721421
2832.385149	187285.243135	39.726439
2835.776407	187773.580578	39.731456
2838.088834	188251.674993	39.736474
2841.389456	188721.946141	39.741492
2844.306674	189199.137246	39.746509
2846.941219	189687.372842	39.751527
2849.614118	190170.118053	39.756544
2852.114264	190660.944203	39.761562
2854.957036	191138.129545	39.766580
2857.068066	191647.283567	39.771597
2859.605766	192149.972014	39.776615
2862.639566	192667.012576	39.781632
2864.746886	193200.253536	39.786650
2867.486893	193721.967320	39.791668
2870.045335	194259.815905	39.796685
2872.616021	194812.295869	39.801703
2875.483148	195351.599259	39.806720
2878.256006	195921.604439	39.811738
2881.127373	196463.883476	39.816756
2883.733752	197042.479543	39.821773
2886.425143	197617.736997	39.826791
2889.456240	198180.979300	39.831808
2892.055728	198775.332346	39.836826
2894.971064	199362.881345	39.841844
2897.721568	199959.095023	39.846861
2900.713893	200558.600768	39.851879
2903.532820	201161.336489	39.856896
2905.921271	201772.016407	39.861914
2909.187034	202386.422439	39.866932
2911.439759	203004.875598	39.871949
2914.661460	203626.888084	39.876967
2917.443997	204257.709831	39.881984
2920.457254	204888.903981	39.887002
2923.251495	205519.931140	39.892020
2926.144813	206169.006230	39.897037
2929.059517	206822.271440	39.902055
2931.563413	207466.610111	39.907072
2934.932149	208119.020563	39.912090
2938.166094	208772.927262	39.917108
2941.667631	209418.639368	39.922125
2944.684869	210064.378016	39.927143
2948.064194	210706.505101	39.932160
2951.113116	211350.717599	39.937178
2954.021904	212007.070911	39.942196
2957.064401	212646.104851	39.947213
2960.475674	213282.084744	39.952231
2963.708922	213933.945563	39.957248
2966.719297	214575.909544	39.962266
2969.820392	215211.026793	39.967284
2972.889160	215846.658159	39.972301
2975.760907	216491.847705	39.977319
2978.999792	217136.447242	39.982336
2981.857656	217782.682227	39.987354
2984.585602	218426.651930	39.992372
2987.468752	219079.794287	39.997389
2990.144341	219723.595666	40.002407
2992.804009	220372.404680	40.007424
2995.558453	221036.645023	40.012442
2998.904308	221693.756407	40.017460
3001.840034	222358.553516	40.022477
3004.368732	223017.851090	40.027495
3007.568394	223680.270288	40.032512
3010.848032	224349.561649	40.037530
3013.663216	225017.045831	40.042548
3016.837769	225675.302958	40.047565
3019.875115	226351.923238	40.052583
3022.719949	227012.492712	40.057600
3025.603487	227678.238368	40.062618
3029.106886	228329.635145	40.067636
3032.574645	228972.552219	40.072653
3035.249911	229597.505170	40.077671
3037.994294	230220.643206	40.082688
3040.911687	230851.298694	40.087706
3044.005834	231497.625641	40.092724
3046.964041	232137.164945	40.097741
3049.269947	232785.646117	40.102759
3052.533434	233425.339447	40.107776
3054.836977	234083.904696	40.112794
3057.830448	234754.885188	40.117812
3060.602358	235413.984907	40.122829
3063.346343	236093.410881	40.127847
3066.681638	236768.043477	40.132864
3069.931067	237452.976677	40.137882
3073.144724	238128.794182	40.142900
3076.416691	238819.258947	40.147917
3079.598257	239508.237454	40.152935
3082.803031	240176.100451	40.157952
3085.344780	240888.038645	40.162970
3088.451308	241589.293418	40.167988
3091.944026	242291.374939	40.173005
3094.225305	243004.186118	40.178023
3097.518186	243706.574075	40.183040
3100.589579	244439.427149	40.188058
3103.886242	245167.492133	40.193076
3106.846449	245894.464012	40.198093
3109.488696	246632.837920	40.203111
3112.844143	247355.728893	40.208128
3115.653849	248107.737377	40.213146
3119.298977	248851.813532	40.218164
3122.225639	249604.686390	40.223181
3125.348307	250367.025602	40.228199
3128.353251	251112.969949	40.233216
3131.352333	251872.476283	40.238234
3134.359919	252637.667509	40.243252
3137.397017	253400.411630	40.248269
3140.485958	254170.789471	40.253287
3143.884565	254940.581250	40.258304
3147.229842	255725.058939	40.263322
3149.888292	256499.148795	40.268340
3153.184868	257278.722470	40.273357
3156.175490	258082.927114	40.278375
3159.883264	258869.310221	40.283392
3162.924249	259646.876950	40.288410
3166.395540	260436.385600	40.293428
3170.217299	261218.544254	40.298445
3173.120856	262002.796873	40.303463
3176.235361	262796.281852	40.308480
3179.286402	263585.580036	40.313498
3182.731772	264367.597299	40.318516
3185.933645	265156.148942	40.323533
3189.272212	265944.317540	40.328551
3192.496153	266732.421664	40.333568
3195.517344	267520.271788	40.338586
3199.133282	268317.242065	40.343604
3202.395696	269106.108123	40.348621
3205.260768	269896.248714	40.353639
3208.824009	270679.060368	40.358656
3212.086311	271470.242606	40.363674
3215.107291	272273.087398	40.368692
3218.113579	273065.438109	40.373709
3220.913197	273860.962967	40.378727
3224.999789	274644.241114	40.383744
3228.105475	275433.709508	40.388762
3231.594049	276232.887817	40.393780
3235.122453	277016.865262	40.398797
3238.360029	277808.905349	40.403815
3241.982635	278563.825511	40.408832
3245.652357	279316.800834	40.413850
3248.949464	280039.708749	40.418868
3252.535531	280765.535613	40.423885
3255.602819	281496.261322	40.428903
3258.376032	282222.327759	40.433920
3261.440298	282954.080301	40.438938
3264.587696	283694.420644	40.443956
3267.716947	284424.217798	40.448973
3270.791091	285186.087074	40.453991
3273.635353	285927.898201	40.459008
3276.752339	286678.190321	40.464026
3279.846225	287449.578355	40.469044
3282.940127	288223.648832	40.474061
3286.121008	288998.635936	40.479079
3289.100793	289772.477098	40.484096
3292.299019	290565.165386	40.489114
3295.410064	291357.552551	40.494132
3298.582555	292164.544649	40.499149
3301.395530	292971.556879	40.504167
3304.821205	293778.487882	40.509184
3307.978262	294619.293616	40.514202
3310.714471	295448.829744	40.519220
3314.267106	296289.168760	40.524237
3317.232078	297128.368726	40.529255
3320.413800	297969.858045	40.534272
3323.547553	298843.914043	40.539290
3326.966316	299712.478906	40.544308
3330.116087	300579.955041	40.549325
3333.192107	301454.156089	40.554343
3336.688690	302342.264549	40.559360
3339.645666	303239.961887	40.564378
3342.931201	304149.472475	40.569396
3345.983946	305055.018117	40.574413
3349.282188	305963.707678	40.579431
3352.629490	306884.861814	40.584448
3355.706214	307807.158103	40.589466
3359.168348	308730.265283	40.594484
3362.573173	309673.314136	40.599501
3365.577013	310607.777581	40.604519
3369.214756	311552.352125	40.609536
3372.415695	312509.513970	40.614554
3375.597109	313471.049960	40.619572
3379.034592	314419.886992	40.624589
3382.328113	315382.761298	40.629607
3386.120278	316342.796279	40.634624
3389.588028	317304.587051	40.639642
3393.278674	318285.278792	40.644660
3397.064065	319238.450923	40.649677
3400.367600	320198.503571	40.654695
3403.761523	321171.918833	40.659712
3407.387188	322128.299765	40.664730
3411.349206	323089.884201	40.669748
3415.063997	324035.372772	40.674765
3418.545236	324993.943321	40.679783
3422.019589	325954.243141	40.684800
3425.938622	326886.719129	40.689818
3430.237708	327826.700015	40.694836
3434.108459	328755.156549	40.699853
3437.616629	329690.193340	40.704871
3441.618097	330607.270437	40.709888
3445.645720	331513.108608	40.714906
3449.216223	332405.729185	40.719924
3452.667906	333305.526426	40.724941
3456.402694	334205.765252	40.729959
3459.919571	335100.765578	40.734976
3463.949899	335982.854227	40.739994
3467.054509	336870.697519	40.745012
3470.593215	337723.884905	40.750016
3474.140217	338568.116157	40.755021
3477.138548	339347.596364	40.760026
3479.897400	340085.217265	40.765031
3482.710164	340776.180577	40.770036
3485.695695	341414.011933	40.775040
3488.534690	341992.483734	40.780045
3490.930219	342529.519865	40.785050
3493.226578	343003.176804	40.790055
3495.577618	343442.570643	40.795060
3497.895233	343822.342142	40.800064
3499.584134	344170.706285	40.805069
3501.792907	344459.339336	40.810074
3503.211039	344712.270448	40.815079
3504.819155	344929.957290	40.820084
3506.473342	345095.668482	40.825088
3507.596164	345246.385447	40.830093
3509.127464	345351.605187	40.835098
3510.650826	345431.706977	40.840103
3511.794113	345476.960963	40.845108
3513.003769	345483.738141	40.850112
3514.006634	345486.962875	40.855117
3514.269154	345445.404686	40.860122
3515.189588	345387.472239	40.865127
3515.860900	345319.002239	40.870132
3517.306315	345220.842844	40.875136
3518.023455	345106.983173	40.880141
3518.334077	344975.338819	40.885146
3518.611410	344820.384978	40.890151
3519.296307	344665.417564	40.895156
3519.543966	344478.177635	40.900160
3519.574000	344302.920362	40.905165
3520.186965	344098.078122	40.910170
3520.436942	343885.257073	40.915175
3520.695337	343682.654345	40.920180
3520.941204	343450.126659	40.925184
3521.264952	343225.034930	40.930189
3521.501094	342984.903374	40.935194
3521.102182	342742.453966	40.940199
3521.215198	342480.649815	40.945204
3521.717556	342237.827145	40.950208
3521.563606	341979.340951	40.955213
3521.634207	341707.239876	40.960218
3521.856989	341450.191045	40.965223
3521.704047	341187.071141	40.970228
3521.914484	340908.458095	40.975232
3521.961448	340636.504975	40.980237
3521.805372	340363.945811	40.985242
3521.704626	340085.451200	40.990247
3521.751855	339792.894964	40.995252
3521.871126	339513.344345	41.000256
3522.149362	339242.259797	41.005261
3521.611880	338954.924647	41.010266
3521.760207	338668.751419	41.015271
3521.760240	338374.588928	41.020276
3521.692327	338091.521833	41.025280
3521.587204	337805.203358	41.030285
3521.349149	337518.572814	41.035290
3520.921295	337224.060977	41.040295
3520.899447	336931.771990	41.045300
3520.809874	336648.391858	41.050304
3520.447001	336368.790541	41.055309
3520.304958	336089.991779	41.060314
3520.255773	335813.109133	41.065319
3520.160061	335549.862735	41.070324
3519.860627	335270.802637	41.075328
3519.682270	335000.927691	41.080333
3519.589209	334727.146407	41.085338
3519.726023	334462.253739	41.090343
3519.454410	334180.790514	41.095348
3519.432084	333909.535371	41.100352
3519.267198	333651.118468	41.105357
3519.008549	333385.618766	41.110362
3518.750947	333126.754970	41.115367
3518.603854	332871.152965	41.120372
3518.356395	332604.221776	41.125376
3518.207568	332350.345979	41.130381
3518.136431	332093.811265	41.135386
3518.308759	331838.177806	41.140391
3517.897801	331590.187650	41.145396
3518.067572	331322.215774	41.150400
3517.697857	331085.991816	41.155405
3517.458602	330842.802464	41.160410
3517.693461	330592.136046	41.165415
3516.989198	330348.685633	41.170420
3517.080712	330098.470816	41.175424
3516.876305	329851.912407	41.180429
3517.188340	329617.938352	41.185434
3516.780373	329381.430198	41.190439
3516.532654	329146.447118	41.195444
3516.180808	328902.423867	41.200448
3516.206691	328683.114380	41.205453
3515.940693	328452.403196	41.210458
3515.859172	328228.860196	41.215463
3515.263099	328000.309158	41.220468
3515.474627	327779.719266	41.225472
3515.446635	327554.714231	41.230477
3515.295853	327343.157602	41.235482
3515.412258	327114.719017	41.240487
3514.677707	326908.313243	41.245492
3514.507928	326684.139449	41.250496
3514.945044	326485.357461	41.255501
3514.148352	326287.174377	41.260506
3514.457417	326070.477145	41.265511
3514.172464	325882.921180	41.270516
3514.245277	325671.854984	41.275520
3513.979887	325473.101534	41.280525
3513.634674	325269.933410	41.285530
3513.968811	325068.540473	41.290535
3513.784652	324875.749325	41.295540
3513.524357	324676.406118	41.300544
3513.232897	324484.418486	41.305549
3512.988866	324290.947112	41.310554
3513.222541	324104.599253	41.315559
3513.328305	323925.367934	41.320564
3513.369617	323731.925642	41.325568
3512.659362	323538.040289	41.330573
3512.505353	323370.472750	41.335578
3512.555342	323179.748498	41.340583
3512.301387	323001.765061	41.345588
3512.664128	322819.079933	41.350592
3512.191560	322647.234601	41.355597
3512.133289	322472.321926	41.360602
3511.933450	322303.917763	41.365607
3511.752148	322130.727355	41.370612
3511.960609	321959.027129	41.375616
3511.879102	321793.935045	41.380621
3511.372643	321624.431303	41.385626
3511.205206	321448.819121	41.390631
3510.638623	321305.323334	41.395636
3511.262785	321135.589995	41.400640
3511.183837	320985.453281	41.405645
3510.663551	320822.664770	41.410650
3510.833155	320665.848092	41.415655
3510.760084	320515.301754	41.420660
3511.003112	320361.728893	41.425664
3510.778520	320215.784535	41.430669
3510.481493	320061.124748	41.435674
3510.580966	319908.437702	41.440679
3509.904693	319754.828306	41.445684
3510.173441	319601.299590	41.450688
3509.718939	319468.389123	41.455693
3509.542537	319327.293516	41.460698
3509.816814	319181.903701	41.465703
3509.508567	319057.542894	41.470708
3509.586482	318913.938350	41.475712
3509.159185	318791.198217	41.480717
3509.075016	318657.616767	41.485722
3509.312515	318524.696993	41.490727
3509.166947	318402.217023	41.495732
3509.068675	318260.189832	41.500736
3508.771942	318144.220493	41.505741
3508.779418	318013.217844	41.510746
3508.790176	317886.997436	41.515751
3508.737638	317775.670322	41.520756
3508.468906	317632.497405	41.525760
3508.406866	317522.723125	41.530765
3508.473026	317399.138675	41.535770
3508.416554	317271.247808	41.540775
3508.325726	317157.966043	41.545780
3508.420586	317038.065288	41.550784
3507.701475	316924.779381	41.555789
3507.603074	316810.938172	41.560794
3507.542089	316695.564246	41.565799
3507.644447	316599.933699	41.570804
3508.147041	316490.933656	41.575808
3507.968401	316376.137046	41.580813
3507.792808	316274.442905	41.585818
3507.634347	316148.956419	41.590823
3507.553144	316049.587791	41.595828
3507.730750	315957.913264	41.600832
3507.508387	315837.193806	41.605837
3507.370161	315725.340649	41.610842
3507.371749	315626.187134	41.615847
3507.309657	315524.371777	41.620852
3507.401482	315426.246903	41.625856
3507.075704	315328.237990	41.630861
3507.315750	315228.613779	41.635866
3507.131936	315121.549684	41.640871
3507.025883	315023.887419	41.645876
3506.979533	314923.747547	41.650880
3506.584608	314831.396926	41.655885
3506.474250	314737.983866	41.660890
3507.045560	314633.777521	41.665895
3506.808829	314540.053040	41.670900
3506.704679	314449.055613	41.675904
3506.332426	314361.102342	41.680909
3506.141638	314275.843073	41.685914
3506.290946	314184.042164	41.690919
3505.994820	314104.396803	41.695924
3506.352229	314025.717797	41.700928
3506.358967	313938.951242	41.705933
3506.375104	313841.241901	41.710938
3506.386596	313752.820357	41.715943
3506.178108	313669.801854	41.720948
3506.182265	313579.472776	41.725952
3506.037588	313497.105548	41.730957
3505.889490	313418.962542	41.735962
3505.851421	313333.677651	41.740967
3505.992144	313256.430674	41.745972
3506.062495	313168.965716	41.750976
3506.097713	313091.556845	41.755981
3505.534458	313005.157543	41.760986
3505.728897	312926.934710	41.765991
3505.572877	312859.402583	41.770996
3505.615087	312778.480676	41.776000
3505.769275	312704.843886	41.781005
3505.503287	312628.626367	41.786010
3505.573598	312552.585155	41.791015
3505.246287	312481.211581	41.796020
3505.522796	312409.005582	41.801024
3505.267020	312328.943733	41.806029
3505.206269	312262.846235	41.811034
3505.343227	312190.509044	41.816039
3505.578434	312123.245480	41.821044
3505.347693	312045.469326	41.826048
3505.263554	311972.046762	41.831053
3505.479686	311909.773205	41.836058
3505.595467	311830.924697	41.841063
3505.179963	311767.528311	41.846068
3505.199407	311689.381661	41.851072
3505.140503	311616.972426	41.856077
3504.961957	311548.245981	41.861082
3505.091610	311466.086740	41.866087
3504.638562	311421.932811	41.871092
3504.666128	311358.084918	41.876096
3505.055607	311288.556805	41.881101
3504.830516	311223.043352	41.886106
3504.933778	311166.613589	41.891111
3504.829603	311107.086328	41.896116
3504.668292	311029.195861	41.901120
3504.685243	310976.977970	41.906125
3504.282242	310901.669689	41.911130
3504.500897	310841.328240	41.916135
3504.575592	310781.823500	41.921140
3504.517736	310723.026457	41.926144
3504.476072	310675.474060	41.931149
3504.390331	310620.091049	41.936154
3504.685965	310542.789952	41.941159
3504.330202	310488.186947	41.946164
3504.322085	310419.788473	41.951168
3504.508771	310385.864805	41.956173
3504.176337	310324.743682	41.961178
3503.969136	310261.847094	41.966183
3504.029751	310216.542989	41.971188
3504.163311	310153.618432	41.976192
3504.225005	310108.772094	41.981197
3504.040701	310058.544048	41.986202
3504.186627	310003.174999	41.991207
3504.029183	309955.945349	41.996212
3504.058401	309900.136387	42.001216
3503.805653	309851.547413	42.006221
3503.330759	309802.229719	42.011226
3503.689167	309747.717792	42.016231
3503.508357	309700.975033	42.021236
3503.704731	309645.928495	42.026240
3503.606900	309605.127224	42.031245
3503.645651	309566.900144	42.036250
3503.722689	309514.925736	42.041255
3503.812066	309485.393509	42.046260
3504.069803	309435.019366	42.051264
3503.783066	309381.982022	42.056269
3503.688697	309328.151136	42.061274
3503.912436	309280.326845	42.066279
3503.502560	309244.078174	42.071284
3503.640207	309197.412377	42.076288
3503.449173	309148.431343	42.081293
3503.219731	309102.967963	42.086298
3503.241622	309053.088343	42.091303
3503.274353	309008.576325	42.096308
3503.326037	308978.515294	42.101312
3502.971436	308936.430351	42.106317
3503.156972	308889.095144	42.111322
3503.383298	308857.912505	42.116327
3503.164329	308818.554556	42.121332
3503.589035	308779.783020	42.126336
3503.424827	308740.849050	42.131341
3503.060062	308701.641037	42.136346
3502.926419	308655.678764	42.141351
3503.102559	308616.666039	42.146356
3502.873210	308580.617676	42.151360
3502.656821	308556.171268	42.156365
3502.750517	308528.469998	42.161370
3503.352826	308493.996526	42.166375
3503.105364	308456.653086	42.171380
3502.774551	308413.240706	42.176384
3502.829374	308382.135471	42.181389
3503.109761	308350.155185	42.186394
3502.971561	308315.924596	42.191399
3502.859953	308273.012220	42.196404
3503.042221	308235.703218	42.201408
3502.978655	308200.544769	42.206413
3502.963800	308158.711412	42.211418
3502.966746	308129.268220	42.216423
3502.613257	308100.669612	42.221428
3503.162436	308057.272026	42.226432
3503.029579	308042.024348	42.231437
3502.746167	307994.558011	42.236442
3502.647526	307964.977917	42.241447
3502.642088	307937.469946	42.246452
3502.794491	307899.681852	42.251456
3502.289263	307870.903251	42.256461
3502.172879	307839.290037	42.261466
3502.209959	307824.473783	42.266471
3502.378474	307803.325929	42.271476
3502.242617	307776.627138	42.276480
3502.507945	307743.350976	42.281485
3502.364596	307726.399837	42.286490
3502.034742	307696.779387	42.291495
3502.152222	307672.992882	42.296500
3502.725805	307640.991745	42.301504
3502.944549	307607.519192	42.306509
3502.651553	307590.565954	42.311514
3502.528912	307545.288016	42.316519
3502.728692	307521.819395	42.321524
3502.671162	307493.784914	42.326528
3502.686676	307459.275220	42.331533
3502.836605	307422.072451	42.336538
3502.682477	307396.139751	42.341543
3502.261917	307369.052635	42.346548
3502.380377	307361.628886	42.351552
3502.148063	307321.915553	42.356557
3502.112510	307307.517668	42.361562
3502.131675	307274.432364	42.366567
3501.934430	307257.947555	42.371572
3502.260885	307231.557915	42.376576
3502.215798	307214.413102	42.381581
3502.377065	307193.800531	42.386586
3502.308809	307166.276504	42.391591
3502.191616	307140.643274	42.396596
3502.306844	307121.361172	42.401600
3502.156270	307095.300518	42.406605
3501.988798	307075.986252	42.411610
3502.171745	307050.407844	42.416615
3501.974363	307028.960590	42.421620
3502.128927	307010.410292	42.426624
3501.948995	306988.095055	42.431629
3502.105709	306959.136092	42.436634
3502.330799	306942.636048	42.441639
3502.410984	306918.396945	42.446644
3502.592867	306887.092768	42.451648
3502.459308	306869.758082	42.456653
3502.290598	306845.939580	42.461658
3502.311021	306812.955566	42.466663
3502.165057	306793.383345	42.471668
3502.502889	306768.671268	42.476672
3502.018478	306748.872010	42.481677
3502.227104	306723.416662	42.486682
3502.140892	306701.264782	42.491687
3502.366362	306686.622323	42.496692
3502.145986	306659.681662	42.501696
3501.840847	306629.496848	42.506701
3502.291501	306621.715673	42.511706
3502.140392	306587.129631	42.516711
3501.896761	306577.904642	42.521716
3501.884618	306548.971840	42.526720
3502.180792	306529.915706	42.531725
3502.007187	306510.653076	42.536730
3502.100256	306483.332488	42.541735
3501.871609	306466.826879	42.546740
3502.041491	306447.306937	42.551744
3502.007571	306424.408754	42.556749
3501.781924	306419.354473	42.561754
3502.150676	306393.008675	42.566759
3502.006486	306374.250364	42.571764
3501.973660	306355.271048	42.576768
3502.174116	306333.939438	42.581773
3502.098258	306317.257201	42.586778
3502.006239	306281.414733	42.591783
3502.322929	306273.679897	42.596788
3502.342986	306244.920026	42.601792
3502.038258	306214.785795	42.606797
3502.081016	306198.212218	42.611802
3502.189895	306176.793064	42.616807
3501.702711	306162.541802	42.621812
3501.944379	306142.552445	42.626816
3501.886448	306119.683325	42.631821
3501.905161	306104.080524	42.636826
3502.060021	306079.702098	42.641831
3501.640684	306071.115253	42.646836
3501.914236	306052.800486	42.651840
3501.923843	306029.233653	42.656845
3502.330382	306013.697435	42.661850
3502.077432	305997.806240	42.666855
3502.011871	305982.343820	42.671860
3501.759869	305956.705611	42.676864
3501.975246	305943.922269	42.681869
3502.048741	305915.611933	42.686874
3502.036912	305900.013844	42.691879
3501.716976	305884.591163	42.696884
3502.024975	305854.971694	42.701888
3502.286460	305841.595797	42.706893
3502.049870	305825.269360	42.711898
3502.263773	305806.709342	42.716903
3501.784812	305773.395539	42.721908
3502.085971	305755.712569	42.726912
3502.093456	305731.153425	42.731917
3502.115112	305722.752064	42.736922
3502.178648	305694.290468	42.741927
3502.236832	305687.003139	42.746932
3502.081965	305659.059196	42.751936
3502.097757	305635.338520	42.756941
3501.919785	305615.210969	42.761946
3501.937524	305587.596286	42.766951
3501.955317	305579.068260	42.771956
3502.176191	305557.911273	42.776960
3501.706630	305538.083768	42.781965
3501.808647	305520.788134	42.786970
3501.997785	305496.785803	42.791975
3501.788017	305489.642133	42.796980
3501.927322	305471.068205	42.801985
3501.774536	305443.327410	42.806989
3501.705461	305437.510532	42.811994
3502.016562	305413.031012	42.816999
3501.660827	305404.637701	42.822004
3501.863160	305387.402686	42.827009
3501.644551	305362.166139	42.832013
3501.639865	305351.478423	42.837018
3501.923277	305340.491174	42.842023
3501.617197	305327.025731	42.847028
3501.676417	305309.813064	42.852033
3501.777128	305302.111847	42.857037
3501.739790	305284.303490	42.862042
3501.553062	305272.091826	42.867047
3501.431955	305255.161823	42.872052
3501.459314	305232.737052	42.877057
3501.607107	305221.618286	42.882061
3501.222994	305227.226374	42.887066
3501.783233	305221.031145	42.892071
3501.615281	305200.062043	42.897076
3501.337904	305182.418423	42.902081
3501.675600	305180.660676	42.907085
3501.477362	305162.673838	42.912090
3501.767470	305135.678006	42.917095
3501.714588	305132.378024	42.922100
3501.701874	305116.805282	42.927105
3501.525334	305098.178801	42.932109
3501.884381	305095.603340	42.937114
3501.856116	305065.756042	42.942119
3501.828552	305052.832315	42.947124
3502.002376	305042.880101	42.952129
3501.719044	305022.310702	42.957133
3501.582557	305009.963875	42.962138
3502.052287	304985.841088	42.967143
3501.844701	304978.697005	42.972148
3501.937225	304962.064345	42.977153
3501.839148	304934.849154	42.982157
3501.444908	304931.042644	42.987162
3501.829501	304906.169653	42.992167
3501.760565	304884.370566	42.997172
3501.552568	304883.283455	43.002177
3501.917592	304849.557156	43.007181
3501.698523	304846.181341	43.012186
3502.089210	304823.954081	43.017191
3501.795337	304807.890767	43.022196
3502.045085	304796.170634	43.027201
3502.054143	304776.318903	43.032205
3501.537575	304762.377233	43.037210
3501.573169	304747.916596	43.042215
3501.907688	304726.334308	43.047220
3501.884189	304709.643358	43.052225
3501.778571	304695.764668	43.057229
3501.499215	304674.227433	43.062234
3502.076826	304661.208994	43.067239
3501.486416	304652.725000	43.072244
3501.514906	304636.763930	43.077249
3501.736081	304632.453994	43.082253
3501.467494	304626.897259	43.087258
3501.608693	304594.936344	43.092263
3501.593488	304585.217190	43.097268
3501.621213	304561.188756	43.102273
3501.721903	304557.890177	43.107277
3501.816604	304549.120911	43.112282
3501.708601	304529.541880	43.117287
3501.506249	304518.910343	43.122292
3501.580906	304501.364148	43.127297
3501.563454	304500.501733	43.132301
3501.710141	304476.760054	43.137306
3501.545199	304454.135962	43.142311
3501.512047	304455.006564	43.147316
3501.604407	304429.975435	43.152321
3501.525057	304422.022292	43.157325
3501.473285	304419.994565	43.162330
3501.461542	304403.352576	43.167335
3501.461230	304389.151946	43.172340
3501.210694	304370.180476	43.177345
3501.435588	304371.519727	43.182349
3501.353970	304367.231658	43.187354
3501.562689	304345.948823	43.192359
3501.331467	304338.961043	43.197364
3501.427812	304333.881663	43.202369
3501.214104	304329.385196	43.207373
3501.189295	304327.531396	43.212378
3501.494584	304294.603009	43.217383
3501.226412	304296.070246	43.222388
3501.395121	304293.728099	43.227393
3501.514996	304284.344063	43.232397
3501.369050	304271.718591	43.237402
3501.455197	304246.026656	43.242407
3501.414294	304256.289361	43.247412
3501.453378	304241.828036	43.252417
3501.240787	304228.118642	43.257421
3501.087091	304212.669465	43.262426
3501.512709	304193.872166	43.267431
3501.339797	304204.639062	43.272436
3501.010579	304199.931596	43.277441
3501.263481	304196.736446	43.282445
3501.049382	304175.570543	43.287450
3501.512760	304151.931902	43.292455
3501.243521	304159.023673	43.297460
3501.542466	304155.363229	43.302465
3502.002038	304154.171735	43.307469
3501.378695	304123.424388	43.312474
3501.569032	304110.110062	43.317479
3501.550253	304111.029322	43.322484
3501.412926	304094.254170	43.327489
3501.799353	304075.310257	43.332493
3501.525760	304081.511982	43.337498
3501.446429	304047.345637	43.342503
3501.297380	304044.416915	43.347508
3501.514365	304032.778081	43.352513
3501.849002	304024.047563	43.357517
3501.548594	304007.094281	43.362522
3501.740840	303989.962173	43.367527
3501.510803	303990.201871	43.372532
3501.225441	303968.461682	43.377537
3501.372261	303973.248859	43.382541
3501.383566	303962.863750	43.387546
3501.560454	303949.398788	43.392551
3501.251905	303937.383999	43.397556
3501.267576	303921.755558	43.402561
3501.644827	303915.054337	43.407565
3501.394297	303906.542533	43.412570
3501.196346	303892.347216	43.417575
3501.202837	303878.501678	43.422580
3501.375247	303865.266441	43.427585
3501.617074	303871.133114	43.432589
3501.503717	303869.242242	43.437594
3501.761209	303837.669873	43.442599
3501.353876	303841.729305	43.447604
3501.245363	303831.897348	43.452609
3501.661613	303822.237845	43.457613
3501.173447	303814.323073	43.462618
3501.338483	303793.148639	43.467623
3501.123701	303798.654059	43.472628
3501.601513	303789.773869	43.477633
3501.507017	303780.703205	43.482637
3501.646712	303754.366409	43.487642
3502.067057	303747.862028	43.492647
3501.291151	303743.020757	43.497652
3501.272535	303727.906614	43.502657
3501.193150	303711.300427	43.507661
3501.532255	303709.338812	43.512666
3501.342272	303694.913146	43.517671
3501.249084	303685.842260	43.522676
3501.294315	303671.303466	43.527681
3501.599776	303670.314203	43.532685
3501.380817	303671.086618	43.537690
3501.529965	303652.892243	43.542695
3501.424692	303644.434036	43.547700
3501.219472	303629.069089	43.552705
3501.428031	303630.792661	43.557709
3501.385033	303621.688468	43.562714
3501.658923	303589.604387	43.567719
3501.096319	303589.208934	43.572724
3501.103074	303592.287451	43.577729
3501.291409	303582.103638	43.582733
3501.524384	303573.388939	43.587738
3501.652075	303551.863948	43.592743
3501.471827	303548.507427	43.597748
3501.515964	303548.373414	43.602753
3501.597556	303523.063582	43.607757
3501.489737	303507.479772	43.612762
3501.448199	303494.583289	43.617767
3501.397507	303493.013455	43.622772
3501.283430	303478.601312	43.627777
3501.665698	303468.845258	43.632781
3501.571773	303461.250545	43.637786
3501.250409	303462.649771	43.642791
3501.542910	303440.462718	43.647796
3501.690188	303426.009701	43.652801
3501.940065	303411.413390	43.657805
3501.559512	303396.813835	43.662810
3501.555430	303377.065421	43.667815
3501.429113	303372.300708	43.672820
3501.683206	303368.469072	43.677825
3501.738806	303341.916165	43.682829
3501.773389	303337.329894	43.687834
3501.401612	303319.140494	43.692839
3501.639728	303318.467154	43.697844
3501.782163	303305.847262	43.702849
3502.093526	303286.074947	43.707853
3501.628739	303277.647436	43.712858
3501.887784	303255.185586	43.717863
3502.139724	303246.060666	43.722868
3501.929152	303221.330815	43.727873
3501.852063	303210.603075	43.732877
3501.730638	303200.416716	43.737882
3501.574728	303177.179853	43.742887
3501.585111	303158.167147	43.747892
3501.676612	303145.326129	43.752897
3501.854174	303136.620020	43.757901
3501.521032	303117.075654	43.762906
3501.713029	303098.696236	43.767911
3501.491873	303096.007785	43.772916
3501.554532	303085.003670	43.777921
3501.596749	303061.659430	43.782925
3501.440464	303059.240787	43.787930
3501.709655	303047.898973	43.792935
3501.719846	303031.889370	43.797940
3501.604826	303034.198003	43.802945
3501.647851	303010.980865	43.807949
3501.633850	302988.383437	43.812954
3501.853312	302973.537257	43.817959
3501.485746	302973.976612	43.822964
3501.592784	302954.490618	43.827969
3501.315260	302944.125012	43.832973
3501.183643	302936.001661	43.837978
3501.524125	302926.048437	43.842983
3501.541139	302912.099197	43.847988
3501.519242	302900.930111	43.852993
3501.333748	302888.870391	43.857997
3501.616777	302884.754243	43.863002
3501.610317	302861.035771	43.868007
3501.345377	302858.659555	43.873012
3501.669985	302845.552968	43.878017
3501.512885	302822.952390	43.883021
3501.215281	302819.588719	43.888026
3501.483217	302815.118621	43.893031
3501.506828	302804.553207	43.898036
3501.450357	302774.403596	43.903041
3501.479722	302774.144639	43.908045
3501.174057	302764.216051	43.913050
3501.601219	302758.906647	43.918055
3501.485866	302736.579458	43.923060
3501.398256	302717.225609	43.928065
3501.912418	302725.518514	43.933069
3501.241073	302716.614199	43.938074
3501.738964	302694.623774	43.943079
3501.507946	302687.228534	43.948084
3501.436378	302686.399999	43.953089
3501.507657	302665.137966	43.958093
3501.420292	302652.273890	43.963098
3501.608224	302637.661598	43.968103
3501.621464	302641.731721	43.973108
3501.553577	302616.088515	43.978113
3501.534279	302603.213785	43.983117
3501.341609	302602.887739	43.988122
3501.589509	302585.262914	43.993127
3501.479124	302569.577425	43.998132
3501.403654	302562.590505	44.003137
3501.538801	302559.311864	44.008141
3501.273883	302543.803230	44.013146
3501.486359	302521.984606	44.018151
3501.464822	302523.184279	44.023156
3501.522906	302513.478731	44.028161
3501.536927	302495.915890	44.033165
3501.162082	302489.103017	44.038170
3501.199486	302484.109024	44.043175
3501.120084	302478.878787	44.048180
3501.317156	302471.289337	44.053185
3501.321110	302464.264537	44.058189
3501.058788	302449.671684	44.063194
3500.929074	302433.378366	44.068199
3500.753365	302441.015657	44.073204
3501.245140	302435.619767	44.078209
3501.416426	302435.974882	44.083213
3501.181701	302435.120950	44.088218
3501.378591	302420.914405	44.093223
3501.114270	302406.830862	44.098228
3501.180288	302385.620440	44.103233
3500.912403	302384.771691	44.108237
3501.019696	302383.100774	44.113242
3501.099257	302378.431036	44.118247
3500.839474	302387.557606	44.123252
3500.796603	302390.414898	44.128257
3501.075833	302377.315288	44.133261
3501.235927	302377.366748	44.138266
3501.319797	302371.932821	44.143271
3501.223785	302356.295923	44.148276
3500.869947	302349.352495	44.153281
3501.396397	302350.517401	44.158285
3501.188566	302345.612636	44.163290
3501.379432	302345.201176	44.168295
3501.115094	302330.277749	44.173300
3501.287351	302311.239430	44.178305
3501.518663	302297.994589	44.183309
3501.246413	302305.876047	44.188314
3501.411898	302290.783609	44.193319
3501.043881	302290.383172	44.198324
3500.987943	302274.001920	44.203329
3501.570193	302260.422248	44.208333
3501.296073	302253.720850	44.213338
3501.372709	302246.175647	44.218343
3501.290122	302252.551330	44.223348
3501.319815	302232.440899	44.228353
3501.617949	302216.436932	44.233357
3501.474149	302207.373703	44.238362
3501.547377	302204.028368	44.243367
3500.939718	302194.274139	44.248372
3501.113488	302174.828326	44.253377
3501.216943	302172.979848	44.258381
3501.229544	302168.727769	44.263386
3501.413128	302167.172170	44.268391
3501.160250	302170.342263	44.273396
3501.336291	302148.096522	44.278401
3501.785351	302140.874839	44.283405
3501.371080	302133.508170	44.288410
3501.545497	302115.385665	44.293415
3501.529843	302111.799715	44.298420
3501.233922	302096.346697	44.303425
3501.100841	302097.258411	44.308429
3501.003894	302091.343712	44.313434
3501.329167	302077.778720	44.318439
3501.171149	302071.848116	44.323444
3501.225293	302056.060400	44.328449
3501.306687	302053.833608	44.333453
3501.227249	302046.058271	44.338458
3501.505542	302035.707392	44.343463
3501.044235	302039.520893	44.348468
3500.857980	302026.366718	44.353473
3501.043233	302012.747247	44.358477
3500.932023	302008.310907	44.363482
3501.321237	302002.981909	44.368487
3501.054133	302001.445865	44.373492
3501.265470	301995.864718	44.378497
3501.729481	302004.114677	44.383501
3501.528483	302003.866281	44.388506
3501.192381	301991.117283	44.393511
3501.259535	301980.723051	44.398516
3501.437932	301969.471553	44.403521
3501.292020	301964.633423	44.408525
3500.876689	301955.027237	44.413530
3501.428478	301939.543445	44.418535
3501.166182	301937.115873	44.423540
3501.315218	301928.744884	44.428545
3501.506641	301923.726759	44.433549
3501.426291	301918.649319	44.438554
3501.421820	301897.933285	44.443559
3501.479331	301895.481164	44.448564
3501.560405	301890.403935	44.453569
3501.491710	301876.849582	44.458573
3500.849938	301856.793084	44.463578
3501.563280	301850.649875	44.468583
3501.381128	301858.084651	44.473588
3501.483642	301839.795138	44.478593
3501.340666	301828.212093	44.483597
3501.261912	301812.088772	44.488602
3501.547914	301813.367634	44.493607
3501.312462	301816.585925	44.498612
3501.243128	301797.330685	44.503617
3501.544752	301781.326042	44.508621
3501.430423	301783.125606	44.513626
3501.329848	301768.761786	44.518631
3501.328660	301772.019807	44.523636
3500.963322	301746.193626	44.528641
3501.436371	301731.129297	44.533645
3501.290940	301734.053560	44.538650
3500.974856	301730.132792	44.543655
3501.280965	301733.953591	44.548660
3501.564887	301728.920986	44.553665
3501.653586	301699.867902	44.558669
3501.463615	301700.254050	44.563674
3501.467318	301682.387144	44.568679
3501.333526	301669.886399	44.573684
3500.960816	301651.823823	44.578689
3501.321788	301647.135476	44.583693
3501.270394	301649.586927	44.588698
3500.886767	301638.525029	44.593703
3501.190786	301655.249730	44.598708
3501.512793	301646.469892	44.603713
3501.446597	301616.575651	44.608717
3501.466875	301616.165404	44.613722
3501.567069	301601.642897	44.618727
3501.244433	301595.992485	44.623732
3501.624759	301579.644616	44.628737
3501.581411	301557.280222	44.633741
3501.379488	301559.755211	44.638746
3501.360491	301557.620445	44.643751
3501.193460	301532.195823	44.648756
3501.322867	301522.071728	44.653761
3501.474971	301529.377940	44.658765
3501.212626	301530.538930	44.663770
3501.363103	301507.940606	44.668775
3501.135881	301502.555227	44.673780
3500.877551	301487.834231	44.678785
3501.493879	301485.498333	44.683789
3501.224732	301486.304075	44.688794
3501.233146	301484.317726	44.693799
3501.032353	301477.553864	44.698804
3501.591943	301458.683744	44.703809
3501.367998	301442.379403	44.708813
3501.522431	301438.919521	44.713818
3501.085291	301437.155534	44.718823
3501.417097	301420.993359	44.723828
3501.075851	301411.553648	44.728833
3501.233055	301395.571468	44.733837
3500.930044	301403.025202	44.738842
3501.079573	301402.391139	44.743847
3501.210839	301398.145898	44.748852
3500.969678	301401.441459	44.753857
3500.810844	301399.761215	44.758861
3500.631740	301399.356687	44.763866
3501.385514	301398.729960	44.768871
3501.455559	301367.719889	44.773876
3501.623938	301363.417941	44.778881
3501.352629	301353.712776	44.783885
3500.920661	301364.291694	44.788890
3501.329078	301351.095283	44.793895
3501.318564	301333.739502	44.798900
3501.457065	301325.497321	44.803905
3501.425620	301332.552295	44.808909
3500.888968	301329.124097	44.813914
3501.592899	301319.113752	44.818919
3501.511333	301302.507148	44.823924
3501.550492	301290.513746	44.828929
3501.413735	301277.835216	44.833933
3501.171763	301271.408628	44.838938
3501.381481	301243.761632	44.843943
3501.344172	301247.712510	44.848948
3501.219139	301249.106549	44.853953
3501.163854	301238.400452	44.858957
3501.196046	301229.869464	44.863962
3501.294628	301222.931510	44.868967
3501.073945	301213.192953	44.873972
3501.008634	301201.597630	44.878977
3501.484265	301187.474433	44.883981
3501.643054	301194.499684	44.888986
3501.570825	301176.669931	44.893991
3501.413781	301170.535466	44.898996
3501.406909	301155.495105	44.904001
3501.604026	301149.559779	44.909005
3501.493127	301136.648113	44.914010
3501.548598	301125.186596	44.919015
3501.346843	301118.600996	44.924020
3501.415382	301114.161931	44.929025
3501.844361	301089.509255	44.934029
3501.427421	301084.866124	44.939034
3501.371312	301082.788044	44.944039
3501.265094	301069.239353	44.949044
3501.309618	301042.152553	44.954049
3501.862741	301026.617388	44.959053
3501.415897	301036.409711	44.964058
3501.057035	301030.790354	44.969063
3501.442596	301002.224953	44.974068
3501.783251	300993.671154	44.979073
3501.502761	300985.748937	44.984077
3501.350568	300979.511888	44.989082
3501.564447	300955.758118	44.994087
3501.393962	300957.311978	44.999092
3501.184292	300942.125103	45.004097
3501.382032	300947.159106	45.009101
3501.349648	300929.043080	45.014106
3501.577348	300908.188561	45.019111
3501.194224	300910.081080	45.024116
3501.201348	300912.421611	45.029121
3501.185512	300908.326585	45.034125
3501.217915	300888.902406	45.039130
3501.263928	300877.162352	45.044135
3501.279190	300877.185555	45.049140
3501.255176	300871.997403	45.054145
3501.348130	300875.444370	45.059149
3501.391866	300859.530673	45.064154
3501.479249	300840.963222	45.069159
3501.800469	300831.139875	45.074164
3501.658074	300823.628715	45.079169
3501.263467	300807.478118	45.084173
3501.085219	300800.125267	45.089178
3501.409229	300791.701295	45.094183
3501.445102	300788.896188	45.099188
3501.250662	300772.917897	45.104193
3501.189067	300759.998433	45.109197
3500.819030	300761.023569	45.114202
3501.265929	300750.264314	45.119207
3501.336675	300745.773971	45.124212
3501.066277	300754.317099	45.129217
3501.435201	300745.937000	45.134221
3501.286449	300733.692888	45.139226
3501.316423	300710.400434	45.144231
3501.683856	300704.133017	45.149236
3501.383572	300707.005191	45.154241
3501.758944	300687.476418	45.159245
3501.500246	300683.088477	45.164250
3501.176821	300669.420935	45.169255
3501.499239	300676.395221	45.174260
3501.135775	300650.313706	45.179265
3501.176233	300645.319064	45.184269
3501.474533	300632.470560	45.189274
3501.395521	300628.207230	45.194279
3501.186740	300626.076647	45.199284
3501.237727	300613.114095	45.204289
3501.276736	300590.074689	45.209293
3501.041380	300597.467054	45.214298
3501.177346	300578.586502	45.219303
3500.993953	300586.759736	45.224308
3501.235844	300587.256534	45.229313
3501.414647	300583.920044	45.234317
3501.591512	300571.370476	45.239322
3501.599967	300554.469603	45.244327
3501.263326	300550.653766	45.249332
3501.096760	300556.584655	45.254337
3501.395613	300528.668844	45.259341
3501.151342	300521.606242	45.264346
3501.266744	300510.695155	45.269351
3501.024389	300513.761894	45.274356
3501.322600	300501.091533	45.279361
3501.212900	300504.977428	45.284365
3501.059866	300490.825078	45.289370
3501.070254	300472.676760	45.294375
3500.684258	300471.591931	45.299380
3500.966126	300475.900187	45.304385
3500.943507	300467.046780	45.309389
3501.124015	300472.516195	45.314394
3501.057929	300465.960208	45.319399
3501.152866	300468.057967	45.324404
3501.021262	300472.125449	45.329409
3501.129289	300462.004498	45.334413
3500.889824	300474.996827	45.339418
3501.256676	300449.819093	45.344423
3501.452428	300433.525185	45.349428
3501.275695	300423.143330	45.354433
3501.461320	300421.867327	45.359437
3501.393926	300424.906718	45.364442
3501.334275	300407.227453	45.369447
3501.427705	300395.759847	45.374452
3501.424441	300381.354991	45.379457
3501.531174	300374.695620	45.384461
3501.138314	300380.356490	45.389466
3501.182650	300354.516494	45.394471
3500.937907	300344.908799	45.399476
3500.910842	300346.694769	45.404481
3501.274741	300339.638868	45.409485
3501.061724	300343.362767	45.414490
3501.368159	300333.439836	45.419495
3501.208811	300334.533846	45.424500
3501.295925	300313.013889	45.429505
3501.445080	300296.549064	45.434509
3501.039712	300300.175781	45.439514
3501.008641	300295.141386	45.444519
3501.382002	300295.337667	45.449524
3501.244652	300284.720565	45.454529
3501.062311	300268.103946	45.459533
3500.732673	300263.370741	45.464538
3501.002272	300252.079174	45.469543
3501.183772	300255.563240	45.474548
3500.833454	300252.054939	45.479553
3500.901987	300249.371955	45.484557
3500.882284	300262.609943	45.489562
3501.081007	300254.332732	45.494567
3501.067817	300253.673193	45.499572
3501.222464	300252.402030	45.504577
3500.992631	300248.747634	45.509581
3500.729815	300241.255219	45.514586
3500.842904	300220.138388	45.519591
3501.089107	300214.627961	45.524596
3500.971098	300210.701565	45.529601
3501.276520	300213.275458	45.534605
3500.918869	300214.833148	45.539610
3501.087464	300203.990038	45.544615
3501.356284	300215.197713	45.549620
3501.293488	300222.130475	45.554625
3501.508154	300205.528124	45.559629
3501.173883	300188.248043	45.564634
3500.992605	300177.357820	45.569639
3501.183590	300174.961108	45.574644
3501.014241	300175.114978	45.579649
3501.023237	300164.984003	45.584653
3501.130020	300170.439524	45.589658
3501.112961	300159.192754	45.594663
3501.536095	300139.249092	45.599668
3501.203951	300143.017081	45.604673
3501.310864	300133.379822	45.609677
3501.012094	300135.844565	45.614682
3501.049488	300131.741158	45.619687
3501.060061	300127.183816	45.624692
3501.299672	300122.641570	45.629697
3501.140687	300109.049985	45.634701
3501.061006	300104.379493	45.639706
3501.104766	300091.036174	45.644711
3501.505472	300090.642795	45.649716
3501.346542	300087.409979	45.654721
3501.469447	300075.454118	45.659725
3501.431293	300058.407668	45.664730
3501.514939	300051.675512	45.669735
3501.404827	300052.023734	45.674740
3501.254258	300044.284680	45.679745
3501.349952	300030.907775	45.684749
3501.115667	300027.432220	45.689754
3501.506783	300020.041153	45.694759
3501.467690	300024.068753	45.699764
3501.482768	299998.284066	45.704769
3501.385337	299977.632730	45.709773
3501.097359	299982.946373	45.714778
3501.201620	299977.738082	45.719783
3501.391716	299974.501596	45.724788
3500.893326	299947.779096	45.729793
3501.284198	299943.493154	45.734797
3501.248663	299948.258301	45.739802
3501.463407	299928.881626	45.744807
3501.036692	299930.704638	45.749812
3501.064882	299925.813654	45.754817
3501.254871	299893.994986	45.759821
3501.030154	299852.187725	45.764826
3501.172652	299746.948277	45.769831
3501.100883	299611.276351	45.774836
3500.792500	299415.701953	45.779841
3500.871972	299176.492443	45.784845
3500.494952	298892.201231	45.789850
3500.328878	298552.491467	45.794855
3499.838909	298156.427664	45.799860
3499.416899	297734.388742	45.804865
3498.958344	297246.709473	45.809869
3498.438838	296724.750224	45.814874
3498.451020	296151.567316	45.819879
3498.004271	295532.964840	45.824884
3497.274715	294877.059109	45.829889
3496.636888	294163.350643	45.834893
3496.084511	293413.118413	45.839898
3495.617777	292604.164457	45.844903
3494.765673	291759.749902	45.849908
3494.097865	290855.626990	45.854913
3493.211359	289909.904587	45.859917
3492.121577	288917.920085	45.864922
3491.508018	287887.889696	45.869927
3490.588766	286806.161767	45.874932
3489.599929	285678.654227	45.879937
3488.675605	284499.794286	45.884941
3487.525198	283282.787176	45.889946
3486.578493	282021.352151	45.894951
3485.241654	280719.220880	45.899956
3484.075747	279372.765072	45.904961
3483.131625	277970.135902	45.909965
3481.724282	276532.545082	45.914970
3480.633777	275048.462797	45.919975
3479.730348	273531.376848	45.924980
3478.377524	271957.807770	45.929985
3476.854810	270341.943361	45.934989
3475.168184	268691.904155	45.939994
3473.475828	267001.909911	45.944999
3472.020291	265273.653332	45.950004
3470.592887	263510.985990	45.955009
3469.430155	261702.309438	45.960013
3467.432516	259851.054310	45.965018
3465.562101	257963.512492	45.970023
3463.728042	256045.198816	45.975028
3461.909647	254089.521054	45.980033
3460.086786	252089.632012	45.985037
3458.663635	250062.378815	45.990042
3456.364003	247995.584801	45.995047
3454.374467	245902.715875	46.000052
3452.229116	243770.908517	46.005057
3450.319491	241608.227041	46.010061
3448.004878	239413.015914	46.015066
3445.717154	237187.679848	46.020071
3443.426602	234937.573977	46.025076
3440.899382	232656.777479	46.030081
3439.051716	230338.349345	46.035085
3436.510129	228000.156995	46.040090
3434.255712	225631.098330	46.045095
3431.806742	223236.982362	46.050100
3429.495576	220815.060797	46.055105
3426.677646	218354.129839	46.060109
3423.934702	215879.418549	46.065114
3421.211371	213380.446412	46.070119
3418.350245	210861.571955	46.075124
3415.492592	208323.694330	46.080129
3412.583949	205762.369717	46.085133
3409.752125	203182.727486	46.090138
3406.932840	200586.005027	46.095143
3403.761286	197960.626101	46.100148
3400.229190	195315.332800	46.105153
3397.657388	192660.110555	46.110157
3394.061820	189996.522544	46.115162
3390.945731	187311.504757	46.120167
3387.930954	184614.111368	46.125172
3383.712948	181917.818462	46.130177
3380.795006	179201.512893	46.135181
3377.239347	176488.776298	46.140186
3373.465590	173748.638159	46.145191
3370.136656	171014.431535	46.150196
3366.294424	168265.230554	46.155201
3362.626421	165506.929861	46.160205
3358.314488	162763.962259	46.165210
3354.386486	160001.359335	46.170215
3350.291841	157249.760538	46.175220
3346.281557	154516.244531	46.180225
3342.623259	151761.524504	46.185229
3337.755386	149026.549023	46.190234
3333.267819	146288.739471	46.195239
3328.132791	143569.269641	46.200244
3322.991664	140877.189463	46.205249
3318.067200	138190.543096	46.210253
3312.436586	135473.309980	46.215258
3306.860890	132847.988927	46.220263
3301.190212	130266.648051	46.225268
3294.844685	127719.567531	46.230273
3289.000999	125209.779218	46.235277
3282.084567	122762.466828	46.240282
3275.398879	120348.308618	46.245287
3268.263489	117995.906378	46.250292
3261.005147	115704.437980	46.255297
3254.046483	113473.778344	46.260301
3245.909768	111325.929932	46.265306
3237.677259	109252.816103	46.270311
3229.397652	107262.465619	46.275316
3220.850229	105356.413532	46.280321
3212.342172	103538.806987	46.285325
3203.671386	101828.820027	46.290330
3194.284175	100199.845143	46.295335
3185.258448	98676.232355	46.300340
3176.543331	97255.116089	46.305345
3168.139560	95921.868497	46.310349
3159.473494	94698.553628	46.315354
3151.309533	93548.988214	46.320359
3143.252215	92494.205709	46.325364
3135.717000	91522.619419	46.330369
3128.787475	90621.921534	46.335373
3121.442936	89793.370948	46.340378
3114.938344	89034.618357	46.345383
3108.492840	88343.557226	46.350388
3102.964807	87708.931737	46.355393
3097.566806	87112.286984	46.360397
3091.935737	86572.035639	46.365402
3087.395523	86066.789389	46.370407
3082.344887	85596.288682	46.375412
3077.687672	85167.047415	46.380417
3072.942554	84755.395617	46.385421
3069.306822	84365.782152	46.390426
3065.121060	84008.310832	46.395431
3061.066966	83661.862561	46.400436
3057.530888	83325.792186	46.405441
3053.942631	82987.142503	46.410445
3050.319266	82682.279302	46.415450
3046.770057	82383.289149	46.420455
3043.336109	82073.232839	46.425460
3039.627700	81776.077757	46.430465
3036.532732	81484.571333	46.435469
3033.165769	81208.861219	46.440474
3030.124784	80912.284082	46.445479
3027.169120	80619.215176	46.450484
3023.705045	80323.078785	46.455489
3021.028995	80035.776992	46.460493
3017.301482	79732.384579	46.465498
3014.138640	79447.641774	46.470503
3011.014554	79152.493457	46.475508
3007.470642	78863.421585	46.480513
3004.404617	78566.352551	46.485517
3000.425832	78264.882532	46.490522
2997.059743	77970.343511	46.495527
2993.672778	77674.159826	46.500532
2989.893365	77387.680376	46.505537
2986.510794	77092.518322	46.510541
2982.923256	76805.405343	46.515546
2979.536495	76514.504760	46.520551
2976.128907	76229.693815	46.525556
2972.703848	75937.306795	46.530561
2969.105991	75645.216642	46.535565
2965.570714	75364.689137	46.540570
2961.872343	75081.599369	46.545575
2958.208990	74806.037771	46.550580
2954.845368	74529.708267	46.555585
2951.273224	74250.328351	46.560589
2947.247268	73978.273385	46.565594
2943.399576	73707.399689	46.570599
2940.019569	73435.617488	46.575604
2936.512725	73172.302400	46.580609
2932.627080	72902.052348	46.585613
2928.811315	72647.032025	46.590618
2925.445485	72393.480264	46.595623
2921.749819	72136.871499	46.600628
2917.987450	71890.281599	46.605633
2914.217404	71639.174796	46.610637
2910.463675	71395.584849	46.615642
2907.381641	71160.424860	46.620647
2904.004970	70914.469449	46.625652
2900.587636	70676.890233	46.630657
2896.678859	70436.863290	46.635661
2893.195119	70207.094808	46.640666
2889.809032	69957.823228	46.645671
2886.134045	69717.664763	46.650676
2882.427042	69492.095723	46.655681
2879.165924	69255.888968	46.660685
2875.300603	69031.510435	46.665690
2871.689858	68796.441752	46.670695
2868.035851	68568.015782	46.675700
2864.450200	68356.060783	46.680705
2860.731813	68126.207780	46.685709
2856.937222	67912.365657	46.690714
2853.362666	67698.605166	46.695719
2849.953030	67472.524828	46.700724
2846.169450	67260.533650	46.705729
2842.819765	67042.611031	46.710733
2839.330244	66836.652192	46.715738
2835.835630	66626.214362	46.720743
2832.601116	66406.965192	46.725748
2829.222157	66205.424795	46.730753
2825.772265	65983.267695	46.735757
2822.177973	65777.016445	46.740762
2818.764523	65559.592557	46.745767
2815.647896	65335.503834	46.750772
2811.735740	65128.044467	46.755777
2808.281931	64903.003097	46.760781
2805.083819	64690.929114	46.765786
2801.795793	64477.081090	46.770791
2798.397629	64263.664670	46.775796
2794.558483	64046.453702	46.780801
2791.148438	63812.700793	46.785805
2787.501016	63602.635752	46.790810
2783.693963	63387.710369	46.795815
2780.424152	63171.147844	46.800820
2777.202882	62956.705767	46.805825
2773.541988	62732.350958	46.810829
2769.995547	62534.782097	46.815834
2766.190998	62313.753788	46.820839
2762.826952	62092.379305	46.825844
2759.301121	61880.900861	46.830849
2755.921641	61661.937954	46.835853
2752.591302	61464.750003	46.840858
2749.110839	61243.718648	46.845863
2745.659121	61019.200690	46.850868
2742.142124	60801.072912	46.855873
2738.615405	60584.255895	46.860877
2734.881677	60375.704038	46.865882
2731.389021	60164.013045	46.870887
2728.121189	59922.557861	46.875892
2724.533678	59717.434606	46.880897
2721.190630	59501.486885	46.885901
2717.516689	59276.537379	46.890906
2714.160842	59069.035404	46.895911
2710.669533	58847.532423	46.900916
2706.950893	58627.196541	46.905921
2703.625192	58416.230720	46.910925
2700.181991	58203.146677	46.915930
2697.032071	57969.300721	46.920935
2693.444150	57755.653134	46.925940
2689.807089	57533.531404	46.930945
2686.488827	57302.161202	46.935949
2682.781325	57086.488732	46.940954
2679.446692	56861.153298	46.945959
2675.915540	56634.499212	46.950964
2672.025999	56424.451208	46.955969
2668.835863	56197.189560	46.960973
2665.375673	55972.332626	46.965978
2661.839486	55744.069815	46.970983
2658.404988	55524.536431	46.975988
2654.588540	55302.755326	46.980993
2651.304465	55077.130620	46.985997
2647.840662	54858.356649	46.991002
2644.367379	54643.887801	46.996007
2640.994321	54414.127629	47.001012
2637.265035	54199.360253	47.006017
2634.236407	53966.371989	47.011021
2630.407417	53748.858156	47.016026
2627.103256	53517.275118	47.021031
2623.414530	53287.911544	47.026036
2619.545617	53067.257193	47.031041
2616.520007	52833.106015	47.036045
2612.999654	52618.295030	47.041050
2609.387549	52389.936964	47.046055
2605.790967	52168.880540	47.051060
2602.319204	51944.114568	47.056065
2598.916944	51716.821411	47.061069
2595.414989	51485.796928	47.066074
2591.601095	51257.779682	47.071079
2588.366678	51036.480718	47.076084
2584.779214	50817.034312	47.081089
2581.499919	50588.438893	47.086093
2578.017062	50364.108633	47.091098
2574.149883	50134.753301	47.096103
2570.758284	49892.290404	47.101108
2567.217594	49681.518757	47.106113
2563.985030	49446.869566	47.111117
2560.464239	49230.402785	47.116122
2556.760340	49001.661189	47.121127
2553.374482	48770.874091	47.126132
2549.982919	48555.084867	47.131137
2546.457782	48320.004582	47.136141
2542.614944	48092.657533	47.141146
2539.029054	47868.196559	47.146151
2535.481679	47640.636555	47.151156
2531.924340	47416.632246	47.156161
2528.841950	47184.913097	47.161165
2525.643860	46971.100192	47.166170
2522.111064	46751.316369	47.171175
2518.700916	46511.226317	47.176180
2514.597433	46289.633554	47.181185
2511.268031	46054.127551	47.186189
2507.558485	45828.050840	47.191194
2503.928645	45592.019535	47.196199
2500.719815	45367.480023	47.201204
2497.312555	45150.114851	47.206209
2494.148021	44908.379947	47.211213
2490.604605	44689.226766	47.216218
2487.224205	44458.413086	47.221223
2483.670311	44219.657411	47.226228
2479.898575	43996.570506	47.231233
2476.556634	43754.298765	47.236237
2473.215073	43520.926731	47.241242
2469.451211	43297.236833	47.246247
2465.852792	43056.147950	47.251252
2462.347156	42834.464253	47.256257
2458.820314	42610.179845	47.261261
2455.305465	42365.502618	47.266266
2451.906414	42147.131925	47.271271
2448.659899	41904.142625	47.276276
2444.892157	41675.669600	47.281281
2441.313189	41445.153012	47.286285
2437.993111	41207.300040	47.291290
2434.576111	40965.958365	47.296295
2430.867701	40742.146256	47.301300
2427.104853	40507.584892	47.306305
2423.864233	40276.602864	47.311309
2420.140604	40052.812888	47.316314
2416.524351	39822.243168	47.321319
2413.188444	39594.301334	47.326324
2409.537670	39361.434010	47.331329
2406.104257	39130.018798	47.336333
2402.801505	38904.228370	47.341338
2399.351752	38674.050583	47.346343
2396.184114	38440.737176	47.351348
2392.726110	38202.558242	47.356353
2389.120358	37965.419436	47.361357
2385.930366	37726.810761	47.366362
2382.292745	37495.952205	47.371367
2378.882007	37245.711915	47.376372
2375.022225	37006.531340	47.381377
2371.700506	36766.337351	47.386381
2368.456705	36533.525694	47.391386
2364.618231	36298.977518	47.396391
2361.356260	36052.848523	47.401396
2357.438105	35817.436945	47.406401
2354.137994	35571.477962	47.411405
2350.392259	35340.247579	47.416410
2346.976327	35101.912759	47.421415
2343.367997	34863.325465	47.426420
2340.011195	34628.416109	47.431425
2336.672752	34399.407949	47.436429
2333.191465	34156.060973	47.441434
2329.800511	33918.667383	47.446439
2326.303592	33683.403808	47.451444
2322.432784	33434.459380	47.456449
2318.869992	33194.584443	47.461453
2315.155622	32961.784269	47.466458
2311.691993	32727.236105	47.471463
2308.453578	32477.785773	47.476468
2305.181649	32257.740179	47.481473
2301.856109	32005.818202	47.486477
2297.855467	31771.605632	47.491482
2294.618995	31526.089624	47.496487
2291.055396	31281.445280	47.501492
2287.369848	31049.701356	47.506497
2283.736102	30815.955525	47.511501
2280.146969	30567.261100	47.516506
2276.662097	30345.190316	47.521511
2273.353195	30104.734534	47.526516
2269.642127	29872.215604	47.531521
2265.958220	29634.073779	47.536525
2262.613295	29400.115006	47.541530
2259.398058	29166.601225	47.546535
2255.611022	28928.718183	47.551540
2251.891239	28696.074502	47.556545
2248.797278	28458.804575	47.561549
2245.217409	28217.982343	47.566554
2241.521093	27993.416266	47.571559
2238.403857	27745.360208	47.576564
2234.410734	27519.439015	47.581569
2231.129107	27290.861675	47.586573
2227.072556	27060.735282	47.591578
2223.296444	26821.297286	47.596583
2219.906859	26603.092123	47.601588
2216.314968	26374.776408	47.606593
2212.738573	26158.943385	47.611597
2208.872333	25947.720115	47.616602
2205.099928	25732.327839	47.621607
2201.405651	25527.697042	47.626612
2196.782994	25338.280719	47.631617
2192.993472	25139.802078	47.636621
2188.454818	24977.798232	47.641626
2184.726095	24803.225284	47.646631
2180.875624	24642.580072	47.651636
2177.188660	24488.347732	47.656641
2174.032493	24321.894255	47.661645
2170.301413	24162.963876	47.666650
2166.667644	23998.501197	47.671655
2163.602108	23830.960574	47.676660
2159.988110	23675.297596	47.681665
2156.545516	23520.603689	47.686669
2152.734119	23368.243110	47.691674
2149.402094	23204.126244	47.696679
2146.362938	23051.514226	47.701684
2142.653369	22885.241697	47.706689
2139.489703	22733.994682	47.711693
2136.000582	22576.420210	47.716698
2132.475786	22412.321050	47.721703
2129.231943	22239.759971	47.726708
2125.315848	22088.971371	47.731713
2122.198624	21922.937335	47.736717
2119.001007	21767.870358	47.741722
2115.635430	21598.311346	47.746727
2112.416824	21428.673783	47.751732
2108.613411	21266.762574	47.756737
2105.096698	21093.082286	47.761741
2101.553864	20918.476425	47.766746
2098.254211	20753.684371	47.771751
2094.752881	20585.555276	47.776756
2091.808794	20425.530935	47.781761
2087.851032	20252.079126	47.786765
2084.433526	20076.948057	47.791770
2080.924746	19907.736432	47.796775
2077.881936	19731.998738	47.801780
2074.385381	19556.758012	47.806785
2070.684252	19388.366426	47.811789
2067.058606	19218.152930	47.816794
2063.671835	19045.496607	47.821799
2060.114891	18868.510653	47.826804
2056.566994	18703.876074	47.831809
2053.047280	18518.083311	47.836813
2049.469707	18350.245096	47.841818
2045.898562	18183.104044	47.846823
2042.579846	17998.918916	47.851828
2039.273005	17825.310879	47.856833
2036.167418	17645.592657	47.861837
2032.386136	17468.698918	47.866842
2028.705681	17291.246345	47.871847
2025.523850	17112.330364	47.876852
2021.636705	16934.058407	47.881857
2018.382284	16754.172270	47.886861
2015.084397	16588.135927	47.891866
2011.605250	16404.507272	47.896871
2008.167578	16223.359636	47.901876
2004.457068	16031.987330	47.906881
2000.996364	15859.475537	47.911885
1997.622076	15685.726350	47.916890
1994.112820	15501.867228	47.921895
1990.897566	15314.686629	47.926900
1987.238147	15135.648477	47.931905
1983.789784	14941.646450	47.936909
1979.990287	14750.760006	47.941914
1976.212023	14576.001241	47.946919
1973.368271	14397.595964	47.951924
1969.554187	14209.433883	47.956929
1965.564911	14031.065645	47.961933
1962.210131	13850.231502	47.966938
1958.846341	13668.048548	47.971943
1955.599913	13481.574729	47.976948
1952.001402	13306.258118	47.981953
1948.658183	13124.403279	47.986957
1945.109479	12936.734701	47.991962
1941.475089	12749.568957	47.996967
1937.983922	12568.293502	48.001972
1934.195479	12389.067174	48.006977
1931.479873	12201.446504	48.011981
1927.834386	12017.924210	48.016986
1924.270317	11824.931451	48.021991
1921.072345	11632.706495	48.026996
1917.106872	11445.450399	48.032001
1913.499718	11260.666363	48.037005
1910.205372	11072.384578	48.042010
1906.599361	10885.131649	48.047015
1903.520599	10697.434040	48.052020
1899.558518	10503.222421	48.057025
1896.112783	10310.020982	48.062029
1892.631743	10126.956819	48.067034
1889.080844	9941.341316	48.072039
1885.435141	9755.900773	48.077044
1882.056345	9572.126491	48.082049
1878.636311	9374.002125	48.087053
1875.621561	9189.842284	48.092058
1872.121946	9000.068830	48.097063
1868.849165	8801.617322	48.102068
1864.641647	8611.955454	48.107073
1861.335762	8422.838134	48.112077
1857.868546	8233.678358	48.117082
1854.410550	8036.583936	48.122087
1850.858783	7844.548390	48.127092
1847.233683	7666.031922	48.132097
1844.069224	7465.510976	48.137101
1840.416226	7268.613532	48.142106
1836.885355	7072.496670	48.147111
1833.412837	6877.053243	48.152116
1829.819855	6686.856099	48.157121
1826.377161	6490.855084	48.162125
1822.594701	6297.403271	48.167130
1819.504241	6108.019663	48.172135
1816.083790	5917.645262	48.177140
1812.093377	5723.868103	48.182145
1808.760054	5532.971378	48.187149
1805.206124	5333.914525	48.192154
1801.566286	5141.114066	48.197159
1798.423243	4948.972106	48.202164
1794.858463	4759.872922	48.207169
1791.524755	4559.081177	48.212173
1787.630124	4373.278182	48.217178
1784.240671	4171.319066	48.222183
1780.800391	3980.290816	48.227188
1776.776785	3792.460205	48.232193
1773.476975	3594.123131	48.237197
1770.031156	3407.193400	48.242202
1766.407150	3206.509540	48.247207
1763.163924	3005.211398	48.252212
1759.449219	2823.550926	48.257217
1756.092546	2627.065498	48.262221
1752.135334	2438.494993	48.267226
1748.516601	2256.898000	48.272231
1745.441181	2050.132371	48.277236
1741.782975	1874.636423	48.282241
1738.086391	1686.941128	48.287245
1734.659163	1499.091739	48.292250
1731.060203	1318.804744	48.297255
1727.654173	1129.453005	48.302260
1723.958226	954.418110	48.307265
1720.235630	766.220823	48.312269
1716.649279	585.888630	48.317274
1712.927451	415.457057	48.322279
1708.900587	254.616990	48.327284
1704.670152	101.542595	48.332289
1698.164047	19.552219	48.337293
1687.718506	53.625570	48.342298
1680.777781	60.248622	48.347303
1676.999411	59.561918	48.352308
1674.206011	70.477760	48.357313
1671.853685	57.931401	48.362317
1669.711568	58.649614	48.367322
1666.360496	57.171528	48.372327
1663.381144	58.539639	48.377332
1660.114777	66.400502	48.382337
1657.087896	62.710803	48.387341
1654.315490	69.349063	48.392346
1650.378144	68.978320	48.397351
1647.265985	58.028386	48.402356
1643.301656	64.340658	48.407361
1640.465424	60.238306	48.412365
1636.575999	52.732023	48.417370
1633.269112	60.346128	48.422375
1630.271099	57.623208	48.427380
1626.689825	61.376128	48.432385
1623.114778	60.148251	48.437389
1619.472965	66.796037	48.442394
1615.559222	63.760855	48.447399
1612.473586	62.184295	48.452404
1609.038302	70.198163	48.457409
1606.074988	67.928569	48.462413
1602.729178	64.032536	48.467418
1599.222971	59.060606	48.472423
1595.266752	50.985820	48.477428
1591.720225	66.834853	48.482433
1588.232596	58.357691	48.487437
1584.879566	60.401251	48.492442
1581.404976	65.399845	48.497447
1578.483750	57.963514	48.502452
1574.871721	61.056866	48.507457
1571.136135	62.919857	48.512461
1568.116769	63.218565	48.517466
1564.492724	54.408420	48.522471
1560.882440	57.526814	48.527476
1556.850387	54.377296	48.532481
1553.542208	61.064631	48.537485
1550.330474	59.466698	48.542490
1546.766585	61.888128	48.547495
1543.533878	54.487907	48.552500
1539.911085	62.183121	48.557505
1536.538067	59.104468	48.562509
1532.987879	53.607931	48.567514
1529.288395	59.521276	48.572519
1526.068959	60.689718	48.577524
1522.659614	55.977909	48.582529
1519.348186	52.975046	48.587533
1515.680352	59.582641	48.592538
1512.003154	62.581809	48.597543
1508.659865	51.500431	48.602548
1504.976609	59.091220	48.607553
1501.563766	61.640884	48.612557
1498.278587	53.470601	48.617562
1494.599373	62.851471	48.622567
1491.388170	53.815385	48.627572
1487.562672	64.443546	48.632577
1484.201321	57.019190	48.637581
1480.749960	56.088384	48.642586
1476.891451	60.998404	48.647591
1473.911175	50.657497	48.652596
1470.322965	68.075997	48.657601
1466.672650	55.637965	48.662605
1463.213776	51.747028	48.667610
1459.930299	60.398403	48.672615
1456.332110	57.231637	48.677620
1452.868598	70.305713	48.682625
1449.253396	54.337722	48.687629
1445.861215	51.091258	48.692634
1442.104980	66.527052	48.697639
1438.739082	53.702825	48.702644
1435.319361	61.404247	48.707649
1431.785805	58.948719	48.712653
1428.115040	61.143305	48.717658
1424.619677	65.458654	48.722663
1421.484610	64.377117	48.727668
1418.050413	71.378452	48.732673
1414.532232	63.377548	48.737677
1410.971947	59.825210	48.742682
1407.293724	65.586569	48.747687
1404.298226	55.757441	48.752692
1400.381102	59.866730	48.757697
1396.891072	58.344049	48.762701
1393.232019	64.263765	48.767706
1389.143351	63.897829	48.772711
1386.215799	58.588628	48.777716
1383.010577	59.109475	48.782721
1379.967696	53.229864	48.787725
1375.871725	57.205804	48.792730
1372.151205	63.771071	48.797735
1368.850821	49.996975	48.802740
1365.046369	62.365126	48.807745
1361.334828	63.452461	48.812749
1358.604041	58.666133	48.817754
1354.757269	61.517890	48.822759
1351.595566	57.567821	48.827764
1348.252825	64.421977	48.832769
1344.567584	65.315374	48.837773
1341.201348	56.370055	48.842778
1337.813828	68.951365	48.847783
1334.184467	65.071343	48.852788
1330.149843	65.149394	48.857793
1326.782540	61.402362	48.862797
1323.564837	69.752410	48.867802
1319.735644	58.180854	48.872807
1316.296408	54.922820	48.877812
1312.680593	65.714363	48.882817
1309.552611	61.221184	48.887821
1305.919007	61.220650	48.892826
1302.333681	63.617042	48.897831
1299.080236	56.182197	48.902836
1295.740779	59.476586	48.907841
1291.925445	59.207109	48.912845
1288.562518	59.186355	48.917850
1284.840573	64.002296	48.922855
1281.807835	57.583286	48.927860
1278.097261	60.616233	48.932865
1274.154188	55.855192	48.937869
1270.792694	52.259136	48.942874
1266.919316	64.157209	48.947879
1263.965158	56.874844	48.952884
1260.070090	60.635878	48.957889
1256.793505	63.721117	48.962893
1254.040460	62.234978	48.967898
1250.504568	67.249598	48.972903
1246.818794	55.902403	48.977908
1242.925940	62.792086	48.982913
1239.062366	53.981617	48.987917
1235.891504	58.122837	48.992922
1232.161027	60.352149	48.997927
1228.650453	49.569168	49.002932
1225.176656	55.516882	49.007937
1222.170474	56.860844	49.012941
1218.806790	48.573250	49.017946
1214.769749	57.608416	49.022951
1211.660032	50.214384	49.027956
1207.630849	59.346400	49.032961
1204.401120	51.930029	49.037965
1200.921493	54.835097	49.042970
1197.679411	65.005008	49.047975
1194.086756	56.531801	49.052980
1190.388691	61.027656	49.057985
1186.545067	51.834435	49.062989
1183.742919	53.839336	49.067994
1179.909019	66.424125	49.072999
1176.833431	52.219448	49.078004
1172.714801	52.718845	49.083009
1169.335569	55.598715	49.088013
1166.291269	59.786581	49.093018
1162.059006	60.702409	49.098023
1158.907962	56.931076	49.103028
1155.363088	65.958817	49.108033
1151.460503	59.147683	49.113037
1148.532308	45.122432	49.118042
1144.896800	58.115931	49.123047
1141.784100	58.394578	49.128052
1137.619551	59.872462	49.133057
1134.301181	55.602145	49.138061
1131.115697	59.479927	49.143066
1127.197871	55.623006	49.148071
1123.922536	66.089210	49.153076
1120.362786	63.403780	49.158081
1116.673417	59.226355	49.163085
1113.642400	53.946103	49.168090
1110.134481	54.024042	49.173095
1106.383184	52.491753	49.178100
1102.881072	55.432013	49.183105
1099.602318	56.707954	49.188109
1096.158665	52.469922	49.193114
1092.221593	51.814620	49.198119
1089.063754	56.042429	49.203124
1085.205894	55.020383	49.208129
1081.741009	58.818535	49.213133
1078.543760	49.508349	49.218138
1074.714737	63.202891	49.223143
1071.742645	60.738689	49.228148
1067.778861	60.571637	49.233153
1063.966155	61.004199	49.238157
1060.759669	53.059057	49.243162
1057.004296	58.057480	49.248167
1053.985483	54.727395	49.253172
1050.542600	59.986946	49.258177
1047.039356	68.846848	49.263181
1043.342944	65.910760	49.268186
1039.666295	67.976690	49.273191
1036.413056	60.348926	49.278196
1032.699065	58.912066	49.283201
1029.008769	47.714387	49.288205
1025.749827	48.822733	49.293210
1022.025351	53.231030	49.298215
1018.999270	50.398810	49.303220
1015.720112	51.320498	49.308225
1012.020262	49.511271	49.313229
1008.557990	59.639770	49.318234
1004.819690	61.304073	49.323239
1001.247088	49.730471	49.328244
997.887465	49.272699	49.333249
994.292874	56.932022	49.338253
990.896735	49.589249	49.343258
987.017186	55.189274	49.348263
983.949041	57.821179	49.353268
980.409766	52.721797	49.358273
976.727720	54.516510	49.363277
973.528418	50.917318	49.368282
969.839905	54.263298	49.373287
965.967337	51.880014	49.378292
962.420841	50.654242	49.383297
958.954120	50.270201	49.388301
955.825390	48.264004	49.393306
951.956908	59.357800	49.398311
949.104910	47.788453	49.403316
945.177663	56.907760	49.408321
941.688562	48.029311	49.413325
938.293124	53.553552	49.418330
935.164464	58.080561	49.423335
931.811110	60.643244	49.428340
927.586791	58.495388	49.433345
923.957627	61.129734	49.438349
920.956692	53.165118	49.443354
917.347295	62.165065	49.448359
913.872632	52.082128	49.453364
910.269365	50.798825	49.458369
906.473694	59.296426	49.463373
903.506190	47.444624	49.468378
899.551031	54.730160	49.473383
896.360575	53.122794	49.478388
892.913308	55.731832	49.483393
888.955023	53.320874	49.488397
886.051543	46.587544	49.493402
881.895010	55.065726	49.498407
878.903814	45.675903	49.503412
874.926028	53.534471	49.508417
871.477352	49.794030	49.513421
868.465281	54.043372	49.518426
864.861639	62.030023	49.523431
861.315551	52.360095	49.528436
857.785849	56.978399	49.533441
854.291040	59.971385	49.538445
850.438621	53.177849	49.543450
847.025740	56.626248	49.548455
843.758078	55.660581	49.553460
840.282164	54.939499	49.558465
836.579834	61.960842	49.563469
832.895804	53.616004	49.568474
829.418728	59.039168	49.573479
826.390856	48.794560	49.578484
822.695818	57.244792	49.583489
819.155166	59.722945	49.588493
815.481634	52.119960	49.593498
811.983954	61.039169	49.598503
808.362312	56.256480	49.603508
804.825067	62.328158	49.608513
801.761655	63.640081	49.613517
798.662241	56.118043	49.618522
794.580170	54.463672	49.623527
791.549947	48.256428	49.628532
787.622171	60.289712	49.633537
783.933225	54.543130	49.638541
780.766941	50.888219	49.643546
776.902419	59.943978	49.648551
773.360826	57.315956	49.653556
770.270882	58.423235	49.658561
766.408214	49.109815	49.663565
763.359589	51.292636	49.668570
759.341288	62.992091	49.673575
756.118292	56.906796	49.678580
752.797044	51.169087	49.683585
749.178529	51.748537	49.688589
745.512909	56.290086	49.693594
742.097037	57.679369	49.698599
738.790753	40.559223	49.703604
735.006239	53.462268	49.708609
731.407296	49.109497	49.713613
728.330925	54.492088	49.718618
724.296049	53.845930	49.723623
721.577393	46.732539	49.728628
717.634061	49.166220	49.733633
713.755680	44.920494	49.738637
710.899559	48.392479	49.743642
706.674273	51.908038	49.748647
703.589985	47.212088	49.753652
700.040953	50.020629	49.758657
696.537482	45.304907	49.763661
693.387297	44.067796	49.768666
689.473667	51.891072	49.773671
686.380370	51.119621	49.778676
682.685968	48.417492	49.783681
678.976873	45.553149	49.788685
675.561871	41.032392	49.793690
671.759027	52.555758	49.798695
668.029521	44.888844	49.803700
664.919970	47.176151	49.808705
661.216471	47.120371	49.813709
658.194179	45.024843	49.818714
654.659592	47.448321	49.823719
650.757830	44.028866	49.828724
647.381579	49.439461	49.833729
644.013364	58.464994	49.838733
640.661554	42.965550	49.843738
636.740441	49.119545	49.848743
633.607413	41.488948	49.853748
630.178946	43.522490	49.858753
626.593794	52.803464	49.863757
623.336940	39.380415	49.868762
619.532059	41.491894	49.873767
616.088529	47.257886	49.878772
612.247677	51.915512	49.883777
608.779758	39.620190	49.888781
605.551775	44.090083	49.893786
602.105072	61.632141	49.898791
598.755251	48.305915	49.903796
594.746423	52.429867	49.908801
591.057415	42.352182	49.913805
587.581157	42.532926	49.918810
584.329908	42.621484	49.923815
581.212586	45.014438	49.928820
577.318566	53.726867	49.933825
573.778178	54.509286	49.938829
570.969692	42.199288	49.943834
566.542300	51.264176	49.948839
563.390531	40.985304	49.953844
559.855690	40.846202	49.958849
556.368022	45.809202	49.963853
553.230584	49.543591	49.968858
549.560539	49.954018	49.973863
546.004431	37.596611	49.978868
542.532185	51.757442	49.983873
538.912565	53.820956	49.988877
535.310683	46.336597	49.993882
531.717512	51.442681	49.998887
528.650943	49.854009	50.003892
525.246184	48.517624	50.008897
521.839122	41.800031	50.013901
518.010419	42.795307	50.018906
513.934234	46.271777	50.023911
510.622742	43.750196	50.028916
507.176809	51.446501	50.033921
503.411114	52.511009	50.038925
499.908629	43.751920	50.043930
496.467322	46.439257	50.048935
493.917200	50.869454	50.053940
490.038555	51.825108	50.058945
486.221059	51.198794	50.063949
482.822797	54.879146	50.068954
479.054127	50.144941	50.073959
475.778683	45.248065	50.078964
471.876499	46.935080	50.083969
468.780684	49.615770	50.088973
465.748987	54.162533	50.093978
462.106068	49.127064	50.098983
458.745109	48.008473	50.103988
455.141218	48.547782	50.108993
451.102167	52.334840	50.113997
447.944708	40.585758	50.119002
443.897877	50.989473	50.124007
440.730867	48.258626	50.129012
437.464403	43.009181	50.134017
433.465715	49.725898	50.139021
430.570509	46.851241	50.144026
426.728195	52.834785	50.149031
423.174369	47.440529	50.154036
419.821472	52.151512	50.159041
416.170150	53.166504	50.164045
412.842479	39.887526	50.169050
409.129817	41.177885	50.174055
405.919817	43.275364	50.179060
402.243611	48.388172	50.184065
398.497308	50.341868	50.189069
395.281632	43.515257	50.194074
391.439874	50.409891	50.199079
388.472088	38.634291	50.204084
385.282414	50.586886	50.209089
381.461451	53.656439	50.214093
377.746326	48.815817	50.219098
374.195731	55.702817	50.224103
371.037706	40.903988	50.229108
367.174969	54.192723	50.234113
363.331816	51.877865	50.239117
360.048385	47.270189	50.244122
356.598317	44.884271	50.249127
353.321686	43.439298	50.254132
349.957309	49.227782	50.259137
346.188183	51.577381	50.264141
342.890889	46.497319	50.269146
339.145084	58.954663	50.274151
335.709848	51.045657	50.279156
332.049592	48.363641	50.284161
328.669859	49.089351	50.289165
325.282874	56.491743	50.294170
321.541280	54.543810	50.299175
318.351715	53.850843	50.304180
314.729465	46.448872	50.309185
310.850803	51.938279	50.314189
307.914189	43.603168	50.319194
304.346358	50.992764	50.324199
300.736735	37.963655	50.329204
297.150220	43.046631	50.334209
293.340534	54.052335	50.339213
289.959802	40.294509	50.344218
286.359678	50.235998	50.349223
282.929157	46.132288	50.354228
279.712870	41.751411	50.359233
276.174059	48.158867	50.364237
272.925525	42.160034	50.369242
269.108228	48.079607	50.374247
265.872336	40.215340	50.379252
262.081565	47.453212	50.384257
258.411925	44.617675	50.389261
255.123144	46.078976	50.394266
251.864785	49.699527	50.399271
248.362777	35.454523	50.404276
244.707594	38.134326	50.409281
240.969765	45.480970	50.414285
237.512686	40.929023	50.419290
234.158359	42.191792	50.424295
230.625538	47.070229	50.429300
227.373306	43.976327	50.434305
223.456126	47.342590	50.439309
220.037465	47.485980	50.444314
216.377038	47.338215	50.449319
213.109888	34.426347	50.454324
209.712837	45.149131	50.459329
205.709263	43.251784	50.464333
202.706363	31.817130	50.469338
198.751713	36.438956	50.474343
195.541326	36.340920	50.479348
192.426950	39.812382	50.484353
188.662260	38.298400	50.489357
184.756687	35.885837	50.494362
181.127197	45.354231	50.499367
178.122678	39.206480	50.504372
174.497949	45.836239	50.509377
170.803940	45.263482	50.514381
167.316437	37.327948	50.519386
163.589767	43.132121	50.524391
160.384515	38.433188	50.529396
157.452311	46.200980	50.534401
153.660844	42.742333	50.539405
150.525974	38.984669	50.544410
146.758170	45.320477	50.549415
143.078726	39.626491	50.554420
139.544756	41.958316	50.559425
136.129515	37.997809	50.564429
132.903427	36.190663	50.569434
128.995491	45.038309	50.574439
125.101811	43.547727	50.579444
121.329349	43.885791	50.584449
118.035964	48.679301	50.589453
115.047220	41.462916	50.594458
111.540809	44.821818	50.599463
107.951026	35.738074	50.604468
104.412819	39.456300	50.609473
101.062988	44.470630	50.614477
97.488818	30.287636	50.619482
94.116244	41.563438	50.624487
90.578543	36.840690	50.629492
87.062207	46.136363	50.634497
83.806526	48.317042	50.639501
80.140843	40.868207	50.644506
76.584235	42.301933	50.649511
73.107358	39.882368	50.654516
69.447456	39.076522	50.659521
65.467676	46.847116	50.664525
62.360041	41.440066	50.669530
58.799006	50.451689	50.674535
55.275193	41.974564	50.679540
52.097578	46.053931	50.684545
48.171784	43.483248	50.689549
44.638444	42.012177	50.694554
41.219588	45.844607	50.699559
38.124928	41.210654	50.704564
34.547694	42.989313	50.709569
31.112817	44.916512	50.714573
27.714855	42.386526	50.719578
23.763523	46.216969	50.724583
20.259992	35.547368	50.729588
16.787302	43.074014	50.734593
13.226497	46.229505	50.739597
10.024373	42.181876	50.744602
6.017931	57.701548	50.749607
2.610961	50.705758	50.754612