Thu Aug 25 09:58:54 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.100080	113.842543	0.000000
0.951536	102.008159	0.005005
1.171350	114.840880	0.010010
1.165466	119.926105	0.015014
0.989042	111.335781	0.020019
1.122835	107.578543	0.025024
0.949687	105.084284	0.030029
0.739262	100.191405	0.035034
0.365046	101.139186	0.040038
0.433320	82.446609	0.045043
0.112244	78.716354	0.050048
-0.235828	76.464641	0.055053
-0.208063	71.483831	0.060058
-0.502060	68.043565	0.065062
-0.693348	56.605051	0.070067
-0.670760	52.545710	0.075072
-1.129014	41.519193	0.080077
-1.144304	31.976681	0.085082
-1.990281	24.098746	0.090086
-2.061201	8.139389	0.095091
-2.859697	13.551251	0.100096
-3.116718	10.548128	0.105101
-3.308356	6.243952	0.110106
-3.500224	10.545203	0.115110
-3.528612	6.408438	0.120115
-4.043160	4.454901	0.125120
-4.857276	6.613714	0.130125
-4.767035	6.144127	0.135130
-4.957916	6.974593	0.140134
-4.728476	4.828557	0.145139
-4.757597	5.586223	0.150144
-5.247169	6.846302	0.155149
-5.562012	12.748695	0.160154
-6.068096	11.024784	0.165158
-6.080805	3.180816	0.170163
-6.830561	15.532629	0.175168
-7.076566	5.510589	0.180173
-7.487944	9.650081	0.185178
-7.669622	8.156916	0.190182
-7.658221	4.820673	0.195187
-7.730346	7.780716	0.200192
-8.209075	12.661587	0.205197
-7.684756	6.119196	0.210202
-8.447376	14.847371	0.215206
-8.999711	17.117029	0.220211
-8.936692	9.144135	0.225216
-9.601660	21.270696	0.230221
-9.372762	8.836236	0.235226
-9.937278	11.041363	0.240230
-10.392446	9.749236	0.245235
-10.318806	6.681651	0.250240
-10.360420	18.495406	0.255245
-10.576781	3.422546	0.260250
-10.710830	16.418206	0.265254
-11.489604	22.326853	0.270259
-11.942760	15.947103	0.275264
-11.994188	12.237889	0.280269
-12.143590	14.574128	0.285274
-11.935030	15.803917	0.290278
-12.524937	11.147692	0.295283
-13.305967	14.079604	0.300288
-13.371823	17.152561	0.305293
-12.995114	10.873742	0.310298
-13.309559	13.004887	0.315302
-13.541640	6.229835	0.320307
-14.487901	1.626283	0.325312
-14.593998	9.305630	0.330317
-14.793452	4.581902	0.335322
-14.617774	18.414882	0.340326
-14.925905	4.065081	0.345331
-14.996777	4.952674	0.350336
-15.451538	5.014567	0.355341
-15.971013	5.906010	0.360346
-16.511340	10.780713	0.365350
-16.604439	3.398593	0.370355
-16.526427	1.655933	0.375360
-16.586323	10.384732	0.380365
-16.773163	0.369245	0.385370
-17.410542	1.741069	0.390374
-17.609677	6.457908	0.395379
-17.967813	9.823431	0.400384
-18.059232	14.729039	0.405389
-18.201704	11.571928	0.410394
-19.035443	20.092950	0.415398
-19.305650	9.210999	0.420403
-19.454289	15.175936	0.425408
-19.671603	11.245942	0.430413
-19.146414	5.687340	0.435418
-19.436455	8.112053	0.440422
-19.946658	1.197083	0.445427
-20.618147	7.367325	0.450432
-20.730527	4.901524	0.455437
-20.475725	3.646854	0.460442
-20.616625	9.139179	0.465446
-21.520331	13.798736	0.470451
-22.252429	3.384628	0.475456
-22.420590	19.036851	0.480461
-22.287032	5.430928	0.485466
-22.619605	11.054524	0.490470
-22.659891	-0.356990	0.495475
-22.460355	17.610429	0.500480
-22.594221	20.826921	0.505485
-23.101608	8.726124	0.510490
-23.863464	3.615954	0.515494
-23.729709	11.045750	0.520499
-23.710750	8.882072	0.525504
-24.334355	13.184531	0.530509
-24.747081	6.162538	0.535514
-25.139253	16.117152	0.540518
-25.383623	15.089389	0.545523
-25.483816	17.402099	0.550528
-25.266179	10.952052	0.555533
-25.613932	3.654125	0.560538
-26.454503	12.397677	0.565542
-26.566210	6.663620	0.570547
-26.684967	11.171714	0.575552
-27.031379	11.697521	0.580557
-26.373357	14.122385	0.585562
-27.089582	12.507331	0.590566
-27.581651	16.732234	0.595571
-27.634283	3.867328	0.600576
-28.134738	15.221464	0.605581
-28.812253	0.065842	0.610586
-29.409689	11.859113	0.615590
-28.974114	10.161667	0.620595
-29.172170	6.102107	0.625600
-29.576713	14.669774	0.630605
-29.688803	7.774682	0.635610
-29.795099	14.153762	0.640614
-29.548734	6.389424	0.645619
-30.062330	10.601879	0.650624
-30.937399	21.941949	0.655629
-30.879963	1.545899	0.660634
-31.071141	13.095183	0.665638
-31.109510	4.711072	0.670643
-31.621513	10.245724	0.675648
-32.307781	14.551674	0.680653
-32.419984	10.459679	0.685658
-32.907194	5.635507	0.690662
-32.699894	4.410425	0.695667
-32.701223	8.314827	0.700672
-32.725668	15.804212	0.705677
-32.766852	2.121268	0.710682
-33.489379	9.299252	0.715686
-33.424889	-2.274209	0.720691
-34.330041	2.613362	0.725696
-34.783339	2.197301	0.730701
-35.082827	14.133714	0.735706
-35.452083	10.015557	0.740710
-35.201224	4.819477	0.745715
-35.526569	9.964216	0.750720
-35.310295	14.144570	0.755725
-35.426176	4.981668	0.760730
-36.131308	6.322980	0.765734
-36.386806	16.436512	0.770739
-36.458897	7.560975	0.775744
-36.733291	3.174857	0.780749
-37.000101	9.553775	0.785754
-37.668686	4.675764	0.790758
-38.208384	6.487863	0.795763
-38.248729	9.559986	0.800768
-38.078630	9.001956	0.805773
-37.787119	2.220798	0.810778
-38.114790	9.238837	0.815782
-38.750823	14.701176	0.820787
-39.259257	15.068872	0.825792
-39.859320	15.678715	0.830797
-39.508703	10.046225	0.835802
-39.644915	6.404081	0.840806
-40.020195	2.565280	0.845811
-40.703114	7.519272	0.850816
-41.211907	18.472920	0.855821
-41.092564	3.910612	0.860826
-41.208486	12.195773	0.865830
-41.142788	15.346193	0.870835
-41.242409	2.172278	0.875840
-42.600232	7.254164	0.880845
-42.852083	-2.339845	0.885850
-43.117321	10.983246	0.890854
-42.178920	7.587177	0.895859
-42.537844	7.479032	0.900864
-42.689062	13.279856	0.905869
-42.899424	5.144157	0.910874
-44.235107	11.399489	0.915878
-44.318666	7.037252	0.920883
-44.227942	7.494567	0.925888
-44.412017	11.721830	0.930893
-44.490625	3.242786	0.935898
-44.670886	12.914258	0.940902
-45.214956	5.723022	0.945907
-45.118513	8.027068	0.950912
-45.807898	11.590026	0.955917
-45.914739	6.434174	0.960922
-45.900385	16.046680	0.965926
-46.323329	6.840142	0.970931
-46.884403	7.519806	0.975936
-46.979352	14.153370	0.980941
-47.184087	7.845434	0.985946
-47.388029	7.023309	0.990950
-47.821940	15.041922	0.995955
-48.397011	16.081283	1.000960
-48.854851	11.958024	1.005965
-48.496320	-1.604048	1.010970
-48.613079	14.577951	1.015974
-48.697116	6.675558	1.020979
-48.655125	2.160774	1.025984
-49.282014	18.549256	1.030989
-49.605427	-0.480486	1.035994
-50.217746	6.060134	1.040998
-50.026858	6.122105	1.046003
-50.071607	12.434592	1.051008
-50.892368	4.916553	1.056013
-50.912799	12.525530	1.061018
-51.326313	17.481605	1.066022
-51.853088	8.952558	1.071027
-51.595407	3.356778	1.076032
-52.216859	6.962876	1.081037
-51.793930	5.596441	1.086042
-52.635871	10.667099	1.091046
-53.143346	11.547173	1.096051
-53.260678	8.952435	1.101056
-53.653414	-0.850452	1.106061
-53.612524	6.046562	1.111066
-53.518721	9.980349	1.116070
-53.550764	9.526758	1.121075
-53.535974	7.980665	1.126080
-54.451496	2.938869	1.131085
-54.399969	3.348541	1.136090
-54.698375	6.537027	1.141094
-55.062288	4.237189	1.146099
-55.837359	-1.187279	1.151104
-56.220591	3.441346	1.156109
-55.819928	2.233423	1.161114
-56.123296	11.063644	1.166118
-56.074205	0.058907	1.171123
-56.639045	10.685975	1.176128
-57.637080	15.556467	1.181133
-57.645634	5.196672	1.186138
-57.651590	17.071274	1.191142
-57.675922	4.625879	1.196147
-57.698502	10.317962	1.201152
-57.975636	10.402645	1.206157
-58.161709	7.508631	1.211162
-58.711358	7.908097	1.216166
-58.616454	2.347313	1.221171
-58.736133	5.096508	1.226176
-59.648549	2.249866	1.231181
-60.240164	4.946457	1.236186
-60.562066	4.145979	1.241190
-60.396922	-1.324568	1.246195
-60.232077	7.302574	1.251200
-60.648560	4.950862	1.256205
-60.459686	8.161074	1.261210
-61.040560	4.382961	1.266214
-61.318203	12.136642	1.271219
-61.696734	11.670903	1.276224
-62.331945	17.145769	1.281229
-61.894649	3.286615	1.286234
-62.371780	13.169117	1.291238
-62.988093	8.494889	1.296243
-63.488791	13.660776	1.301248
-63.616095	12.380555	1.306253
-63.109154	7.508181	1.311258
-63.765078	5.349010	1.316262
-63.552668	3.265753	1.321267
-64.198776	8.906839	1.326272
-64.820868	13.016074	1.331277
-64.627115	6.889309	1.336282
-65.409234	17.781379	1.341286
-64.967217	13.751241	1.346291
-64.997178	2.496300	1.351296
-65.469909	6.164516	1.356301
-66.282323	9.727770	1.361306
-66.756596	2.345269	1.366310
-66.644491	-0.127231	1.371315
-66.595353	9.555750	1.376320
-67.079396	14.427963	1.381325
-67.052507	3.467833	1.386330
-67.290451	11.550650	1.391334
-67.899173	15.297123	1.396339
-67.983564	11.979054	1.401344
-68.475665	15.403534	1.406349
-68.410736	3.788876	1.411354
-68.523235	13.829378	1.416358
-68.712611	7.063458	1.421363
-69.060298	15.220419	1.426368
-69.581842	10.898337	1.431373
-69.469564	6.793317	1.436378
-70.168151	7.722319	1.441382
-70.775786	7.599362	1.446387
-70.609138	7.244352	1.451392
-71.144128	6.467772	1.456397
-71.521171	10.563920	1.461402
-71.350197	10.125974	1.466406
-71.160759	7.688813	1.471411
-71.381471	-1.324780	1.476416
-71.707415	11.352926	1.481421
-72.176252	5.551445	1.486426
-72.973824	4.129477	1.491430
-73.007553	8.124374	1.496435
-72.873148	9.900453	1.501440
-73.012724	19.249177	1.506445
-73.182574	6.864548	1.511450
-74.037425	14.158181	1.516454
-73.929367	-0.582686	1.521459
-74.516248	7.735137	1.526464
-74.604632	3.835566	1.531469
-74.471956	2.426025	1.536474
-74.875671	3.954228	1.541478
-75.396379	-6.720777	1.546483
-75.522088	1.464671	1.551488
-76.337957	4.095162	1.556493
-75.655439	-5.528189	1.561498
-75.928250	11.459699	1.566502
-76.671000	7.127987	1.571507
-77.137462	8.172477	1.576512
-77.511873	2.099939	1.581517
-77.274515	1.515552	1.586522
-77.581760	0.598883	1.591526
-77.248686	5.061487	1.596531
-77.318764	-0.305765	1.601536
-78.192987	3.558238	1.606541
-78.329301	-4.108167	1.611546
-78.576184	10.097892	1.616550
-79.002913	7.105547	1.621555
-79.453458	5.252717	1.626560
-79.945267	-2.345331	1.631565
-79.700285	-2.114668	1.636570
-80.185983	-0.292046	1.641574
-80.025765	4.482379	1.646579
-80.217735	3.142689	1.651584
-80.843654	9.011565	1.656589
-80.705981	4.238181	1.661594
-81.034206	6.940959	1.666598
-81.293378	4.377939	1.671603
-81.850878	11.400353	1.676608
-82.945822	16.017113	1.681613
-82.331328	6.126005	1.686618
-82.830047	12.791197	1.691622
-82.957797	5.572698	1.696627
-82.836810	10.600044	1.701632
-82.909181	11.750463	1.706637
-83.133913	13.377172	1.711642
-83.806833	9.566027	1.716646
-84.153261	11.616763	1.721651
-83.770551	6.988481	1.726656
-84.131748	10.509508	1.731661
-84.670785	4.832923	1.736666
-85.424915	7.472724	1.741670
-85.580146	2.084013	1.746675
-85.674953	0.972707	1.751680
-85.995440	7.284104	1.756685
-85.744918	1.774868	1.761690
-86.336017	3.174245	1.766694
-87.012738	3.773957	1.771699
-87.181675	-3.124874	1.776704
-87.605586	14.424528	1.781709
-87.400296	4.461499	1.786714
-87.535144	15.729871	1.791718
-87.593736	9.465477	1.796723
-87.299596	10.131362	1.801728
-88.387924	10.577270	1.806733
-88.814670	9.378771	1.811738
-88.921129	15.719910	1.816742
-88.843574	12.047436	1.821747
-89.054526	-1.017278	1.826752
-89.245318	15.657206	1.831757
-89.632114	-0.733524	1.836762
-89.986421	2.742130	1.841766
-90.483868	7.331706	1.846771
-90.389752	2.887849	1.851776
-90.830733	5.529201	1.856781
-91.227121	8.328082	1.861786
-91.490905	18.446074	1.866790
-91.435582	7.816845	1.871795
-91.516918	2.049561	1.876800
-91.748365	7.698439	1.881805
-92.591878	5.337712	1.886810
-92.915110	10.304949	1.891814
-93.189992	8.557473	1.896819
-93.142428	11.302609	1.901824
-93.667178	17.168290	1.906829
-93.283152	0.656778	1.911834
-93.711316	8.528954	1.916838
-93.622166	7.588139	1.921843
-94.361853	3.265441	1.926848
-94.779185	7.260334	1.931853
-94.920366	9.351676	1.936858
-94.833723	6.997061	1.941862
-94.954985	10.812686	1.946867
-95.676895	5.228032	1.951872
-96.150368	-2.537402	1.956877
-96.134794	1.626938	1.961882
-96.343008	12.454388	1.966886
-96.472714	8.093057	1.971891
-96.493065	11.908689	1.976896
-96.886931	12.258437	1.981901
-97.102191	2.899143	1.986906
-97.546665	5.914364	1.991910
-98.186176	5.445228	1.996915
-97.758579	4.147413	2.006912
-97.718497	4.128723	2.016909
-97.962565	0.508427	2.026906
-97.112701	7.392186	2.036902
-96.254917	13.029764	2.046899
-95.320198	12.395722	2.056896
-95.099916	9.152492	2.066893
-95.318599	4.739436	2.076890
-94.809006	8.942708	2.086886
-94.080448	8.334635	2.096883
-92.985843	9.088378	2.106880
-92.561027	11.454942	2.116877
-92.528461	6.305602	2.126874
-92.149206	11.197702	2.136870
-91.407200	13.318162	2.146867
-90.679954	8.281718	2.156864
-90.060158	9.844788	2.166861
-90.083765	11.923655	2.176858
-89.596609	9.113777	2.186854
-88.351195	11.212378	2.196851
-88.304685	15.504052	2.206848
-88.139821	3.621423	2.216845
-87.135103	3.153811	2.226842
-87.091989	7.373156	2.236838
-86.280414	6.406787	2.246835
-85.755115	4.987930	2.256832
-85.381151	3.326692	2.266829
-84.294056	5.684516	2.276826
-83.953399	7.570091	2.286822
-83.841876	8.839004	2.296819
-83.794334	5.920613	2.306816
-82.888472	12.060674	2.316813
-82.315173	5.838254	2.326810
-81.557909	10.772494	2.336806
-81.130407	5.456734	2.346803
-81.224197	6.307990	2.356800
-80.308820	10.606071	2.366797
-79.974954	9.996487	2.376794
-79.721334	12.196642	2.386790
-78.755279	10.623193	2.396787
-78.295253	7.421591	2.406784
-77.478201	7.803845	2.416781
-77.149371	1.401155	2.426778
-76.871780	10.588876	2.436774
-76.745488	10.648544	2.446771
-75.975996	9.834488	2.456768
-74.778843	9.298711	2.466765
-74.236763	11.067196	2.476762
-74.606894	16.222438	2.486758
-74.118920	13.355412	2.496755
-73.220705	14.285648	2.506752
-72.905576	6.120640	2.516749
-72.020164	7.996886	2.526746
-71.406454	5.547315	2.536742
-71.426375	7.758652	2.546739
-71.158641	5.996850	2.556736
-70.549920	10.526714	2.566733
-69.761904	4.682464	2.576730
-68.733390	4.445543	2.586726
-68.756698	10.854740	2.596723
-68.581931	10.951162	2.606720
-67.484653	17.805667	2.616717
-67.431182	7.971046	2.626714
-66.872143	13.623760	2.636710
-65.970750	14.702386	2.646707
-65.659690	14.698258	2.656704
-65.557897	10.133615	2.666701
-64.578513	11.222195	2.676698
-64.044199	7.983612	2.686694
-64.057813	3.158287	2.696691
-63.358320	11.994802	2.706688
-62.732310	14.608610	2.716685
-62.247263	7.785465	2.726682
-61.626590	9.066467	2.736678
-61.329552	10.515386	2.746675
-61.167469	14.323286	2.756672
-60.265132	12.709138	2.766669
-59.689714	14.396373	2.776666
-58.815615	11.985197	2.786662
-58.294520	12.258603	2.796659
-58.090098	11.853035	2.806656
-58.051205	12.940093	2.816653
-57.626400	-0.396102	2.826650
-57.030246	7.468252	2.836646
-55.683595	14.137965	2.846643
-55.665949	9.016303	2.856640
-55.374836	15.037282	2.866637
-54.859142	5.104895	2.876634
-54.231911	10.696240	2.886630
-53.899616	13.533467	2.896627
-53.045189	8.249014	2.906624
-52.644643	10.194899	2.916621
-52.343369	7.490174	2.926618
-51.402130	2.179450	2.936614
-51.164743	2.804586	2.946611
-51.171231	-1.470658	2.956608
-50.367906	1.276924	2.966605
-49.808837	5.896932	2.976602
-48.710249	4.980628	2.986598
-48.506609	7.445206	2.996595
-48.259303	11.413981	3.006592
-47.906969	1.443836	3.016589
-47.018410	2.404098	3.026586
-46.496035	7.261105	3.036582
-46.354995	5.759908	3.046579
-46.072551	11.981816	3.056576
-45.047381	12.892164	3.066573
-44.502825	11.806078	3.076570
-44.399544	8.362602	3.086566
-43.601164	15.048533	3.096563
-43.374702	9.216243	3.106560
-42.462574	8.142256	3.116557
-41.987332	9.658288	3.126554
-41.904971	15.011894	3.136550
-41.015629	8.451684	3.146547
-40.458070	2.627707	3.156544
-40.301885	7.108103	3.166541
-40.026925	4.927021	3.176538
-39.282940	3.920561	3.186534
-38.893985	8.076216	3.196531
-38.021200	13.629089	3.206528
-37.514780	2.164943	3.216525
-37.517182	8.171722	3.226522
-36.522423	3.042681	3.236518
-36.004423	5.549870	3.246515
-35.921118	10.950843	3.256512
-34.960915	11.861868	3.266509
-34.783022	5.552517	3.276506
-34.449600	7.920733	3.286502
-33.874670	13.098959	3.296499
-32.911960	7.727850	3.306496
-32.273343	7.643890	3.316493
-32.136083	5.782156	3.326490
-32.001003	3.987288	3.336486
-31.256656	8.112602	3.346483
-30.798647	3.805757	3.356480
-30.109478	6.922854	3.366477
-29.282684	3.464217	3.376474
-29.006147	6.101106	3.386470
-28.955261	1.667984	3.396467
-28.347692	0.828618	3.406464
-27.697270	2.057444	3.416461
-26.957887	2.622933	3.426458
-26.201619	0.971487	3.436454
-25.879223	5.033034	3.446451
-25.718827	7.767315	3.456448
-25.493791	9.550634	3.466445
-24.654638	5.877818	3.476442
-24.540360	8.144156	3.486438
-23.957516	8.068935	3.496435
-23.170365	12.273075	3.506432
-21.975056	9.640512	3.516429
-22.314064	5.784830	3.526426
-21.528286	4.594427	3.536422
-21.439700	11.249021	3.546419
-20.514232	10.096919	3.556416
-20.335555	11.044867	3.566413
-19.500044	6.545827	3.576410
-18.868136	11.167097	3.586406
-18.635849	8.552377	3.596403
-18.294538	11.936222	3.606400
-17.592577	5.867873	3.616397
-17.036610	11.302495	3.626394
-16.695233	8.550306	3.636390
-16.143636	7.922449	3.646387
-15.562273	5.709198	3.656384
-15.590620	7.807816	3.666381
-14.417947	2.682578	3.676378
-13.966511	-0.416305	3.686374
-13.742898	8.101971	3.696371
-12.738460	-0.259737	3.706368
-12.750776	7.763316	3.716365
-12.359774	4.711915	3.726362
-11.484964	0.232061	3.736358
-11.524617	2.405309	3.746355
-10.696602	7.394995	3.756352
-10.017246	8.818861	3.766349
-9.588211	4.614758	3.776346
-8.857964	9.641939	3.786342
-8.633476	1.399266	3.796339
-8.458020	4.517659	3.806336
-7.205668	4.518104	3.816333
-6.799711	-3.952570	3.826330
-6.734224	0.196747	3.836326
-6.172357	0.761542	3.846323
-5.668459	3.733440	3.856320
-5.432551	3.563692	3.866317
-4.590952	12.343106	3.876314
-4.134729	8.942531	3.886310
-3.716469	15.583488	3.896307
-3.296608	21.169320	3.906304
-3.036934	27.987184	3.916301
-2.473458	39.521826	3.926298
-1.903104	47.817901	3.936294
-1.535543	61.002001	3.946291
-1.195861	81.226185	3.956288
-0.441177	97.536475	3.966285
-0.025745	104.269776	3.976282
0.000000	118.311353	3.981286
0.496053	121.612664	3.986291
0.554179	134.363164	3.991296
1.048192	135.959527	3.996301
1.057138	137.321842	4.001306
0.940419	139.219540	4.006310
1.012785	141.280602	4.011315
0.827872	147.526515	4.016320
1.178502	147.803905	4.021325
1.211752	151.142934	4.026330
0.856376	143.991675	4.031334
0.972338	143.100436	4.036339
1.108519	161.574643	4.041344
1.562922	164.800230	4.046349
1.235475	162.880635	4.051354
0.876509	162.051153	4.056358
1.277734	158.666457	4.061363
1.361598	172.456997	4.066368
1.606686	176.537964	4.071373
1.331301	173.597802	4.076378
1.382101	180.420568	4.081382
1.596579	169.842228	4.086387
1.519241	164.359000	4.091392
1.483717	150.054952	4.096397
1.139566	157.749516	4.101402
1.055873	164.333918	4.106406
1.351266	164.907867	4.111411
1.589811	170.071868	4.116416
1.701572	166.865404	4.121421
1.664259	167.500972	4.126426
1.611671	165.247244	4.131430
1.515390	154.135470	4.136435
1.260026	152.308986	4.141440
1.574490	159.969961	4.146445
1.349628	171.518300	4.151450
1.630674	168.418190	4.156454
1.763757	166.511860	4.161459
1.560863	170.992048	4.166464
1.545672	161.895544	4.171469
1.595648	161.792932	4.176474
1.485240	162.430461	4.181478
1.678254	169.914316	4.186483
1.504909	172.744712	4.191488
1.655135	179.849294	4.196493
1.503842	176.516363	4.201498
1.575282	178.713617	4.206502
1.728440	184.457318	4.211507
1.379782	185.087885	4.216512
1.574613	175.648416	4.221517
1.830385	176.798053	4.226522
1.507422	174.697419	4.231526
2.123966	172.171170	4.236531
1.974633	171.346807	4.241536
1.791868	172.223466	4.246541
2.075583	182.436108	4.251546
2.271736	172.069448	4.256550
2.163029	160.943797	4.261555
1.593533	169.828450	4.266560
1.768224	166.159706	4.271565
1.529651	154.541875	4.276570
1.588559	157.367517	4.281574
1.585843	172.193521	4.286579
1.888760	172.725162	4.291584
2.105630	180.942443	4.296589
1.895643	179.887136	4.301594
2.028121	175.117682	4.306598
2.516224	172.250886	4.311603
1.834793	172.860825	4.316608
2.016138	160.383089	4.321613
1.473083	156.257325	4.326618
1.643845	164.731761	4.331622
1.920805	167.662446	4.336627
2.064777	183.632909	4.341632
2.321357	167.732828	4.346637
1.851753	175.108531	4.351642
2.207064	184.031792	4.356646
2.218360	181.980025	4.361651
1.843732	180.532895	4.366656
1.961696	177.781041	4.371661
1.952570	179.275905	4.376666
2.120001	176.193594	4.381670
1.960361	177.335551	4.386675
1.984881	179.701510	4.391680
2.319187	174.688460	4.396685
1.706554	180.675531	4.401690
1.859445	183.951527	4.406694
2.039584	178.817098	4.411699
2.113793	181.478994	4.416704
2.061494	173.932221	4.421709
1.816848	179.820506	4.426714
2.072363	177.626071	4.431718
2.035891	187.297257	4.436723
2.361713	200.537376	4.441728
2.378255	203.211474	4.446733
2.413538	204.629779	4.451738
2.107736	188.140746	4.456742
2.089624	192.386342	4.461747
2.175860	199.504122	4.466752
2.371553	194.129968	4.471757
2.419906	203.275340	4.476762
2.603316	208.963688	4.481766
2.442302	194.631809	4.486771
2.176223	209.945201	4.491776
2.220608	200.447033	4.496781
2.232418	208.943231	4.501786
2.189558	209.525886	4.506790
2.340381	206.221544	4.511795
2.151912	208.858161	4.516800
2.531728	203.284311	4.521805
2.561480	194.756557	4.526810
2.335415	200.350870	4.531814
2.528990	201.785502	4.536819
2.701817	200.559482	4.541824
2.692233	197.824445	4.546829
2.816605	203.265775	4.551834
2.593797	201.057695	4.556838
2.658472	197.279631	4.561843
2.235670	205.151054	4.566848
2.760035	201.785023	4.571853
2.460137	198.779094	4.576858
2.704316	196.108702	4.581862
2.617951	206.534368	4.586867
2.659313	203.082660	4.591872
2.811056	202.869190	4.596877
2.820843	201.475724	4.601882
2.465561	207.634455	4.606886
2.420000	200.545364	4.611891
2.460151	205.515832	4.616896
2.541782	196.122563	4.621901
2.799365	207.155569	4.626906
2.395182	203.726214	4.631910
2.548359	190.354357	4.636915
2.470034	197.776332	4.641920
2.623966	197.470769	4.646925
2.388977	193.258762	4.651930
1.988683	210.991328	4.656934
2.811205	212.571029	4.661939
2.987809	228.656643	4.666944
3.271842	221.303929	4.671949
3.228826	229.270883	4.676954
2.994881	224.685379	4.681958
3.025365	206.121980	4.686963
2.790252	209.446119	4.691968
2.975102	204.323599	4.696973
2.874789	206.848326	4.701978
2.795785	202.336628	4.706982
3.072886	204.131500	4.711987
2.740434	210.713766	4.716992
2.865466	218.265241	4.721997
3.280483	222.889075	4.727002
3.024777	218.740420	4.732006
2.872899	215.502487	4.737011
2.963045	217.586083	4.742016
3.108721	220.290571	4.747021
3.182070	212.240036	4.752026
3.109058	206.892160	4.757030
3.061346	206.460001	4.762035
2.993130	204.167588	4.767040
2.913900	201.823116	4.772045
2.926662	211.198697	4.777050
2.851110	217.791335	4.782054
3.198717	220.688813	4.787059
2.974200	225.327429	4.792064
3.295933	227.887274	4.797069
3.065032	227.502799	4.802074
2.913694	237.546354	4.807078
3.104284	228.018936	4.812083
3.003527	227.142667	4.817088
3.490857	228.828671	4.822093
3.267041	240.639485	4.827098
3.380321	232.038513	4.832102
3.713158	235.327454	4.837107
3.337955	236.525336	4.842112
3.094176	239.388924	4.847117
3.176486	231.852674	4.852122
3.072511	235.270167	4.857126
3.330837	224.884243	4.862131
2.922797	235.597610	4.867136
3.368192	236.053145	4.872141
3.151267	231.939540	4.877146
3.302983	231.564720	4.882150
2.907212	231.244043	4.887155
2.709472	242.348412	4.892160
3.181258	234.178491	4.897165
3.332911	241.004461	4.902170
3.649207	247.580008	4.907174
3.771109	241.885203	4.912179
3.504284	240.468634	4.917184
3.574308	237.138981	4.922189
3.085920	231.489179	4.927194
3.327536	235.447317	4.932198
3.446958	239.642902	4.937203
3.427923	242.733872	4.942208
3.675833	248.465912	4.947213
3.277870	248.025353	4.952218
3.588156	251.400089	4.957222
3.890029	245.452456	4.962227
4.004864	249.604469	4.967232
3.871457	236.217368	4.972237
3.658471	233.226290	4.977242
3.237940	234.193989	4.982246
3.446246	232.320159	4.987251
3.462013	232.899957	4.992256
3.587498	229.900140	4.997261
4.075185	237.091079	5.002266
3.590448	234.427319	5.007270
3.621272	230.186311	5.012275
3.580891	239.101993	5.017280
3.818001	237.495735	5.022285
3.963876	238.086785	5.027290
3.375724	233.471354	5.032294
3.619323	237.106474	5.037299
3.558539	245.028763	5.042304
3.601785	246.382547	5.047309
3.512234	247.317372	5.052314
3.103956	255.075809	5.057318
3.655304	246.406194	5.062323
3.718786	255.090473	5.067328
3.744288	250.562389	5.072333
3.379107	259.582755	5.077338
3.541805	255.893725	5.082342
3.903108	248.551039	5.087347
3.889458	280.314617	5.092352
4.213676	269.333042	5.097357
3.911562	260.464943	5.102362
3.975859	259.803259	5.107366
3.963813	256.847133	5.112371
3.820719	262.191181	5.117376
4.075159	251.435688	5.122381
3.860634	250.877802	5.127386
3.698227	259.480415	5.132390
4.084520	269.895338	5.137395
4.059050	276.638340	5.142400
4.104175	276.593436	5.147405
3.813582	276.623278	5.152410
4.063773	275.435752	5.157414
4.240999	271.630546	5.162419
3.956439	281.887990	5.167424
4.125193	277.878463	5.172429
4.300924	276.848138	5.177434
4.029510	269.174302	5.182438
3.994970	264.048174	5.187443
4.186365	276.489990	5.192448
4.264171	277.534638	5.197453
4.210135	277.318606	5.202458
4.254197	277.254885	5.207462
4.307840	261.889561	5.212467
3.870872	267.861792	5.217472
3.995482	273.685926	5.222477
3.973221	273.154864	5.227482
4.298182	280.621255	5.232486
4.362499	276.061773	5.237491
4.337887	284.304282	5.242496
4.318244	286.683502	5.247501
4.333691	284.688022	5.252506
4.175028	288.158386	5.257510
4.790865	271.629278	5.262515
4.511653	281.477754	5.267520
4.577154	265.759387	5.272525
4.269702	264.352346	5.277530
3.982381	273.271933	5.282534
4.142042	270.728670	5.287539
4.215034	278.614194	5.292544
4.232166	274.748648	5.297549
4.364188	277.967820	5.302554
4.209580	278.688210	5.307558
4.536988	281.690105	5.312563
4.338060	281.234180	5.317568
4.598162	287.236408	5.322573
4.283422	284.542842	5.327578
4.234879	282.772526	5.332582
4.107101	282.134608	5.337587
4.395778	285.645615	5.342592
4.304931	288.099267	5.347597
4.577002	289.667143	5.352602
4.258394	283.563610	5.357606
4.433116	281.979779	5.362611
4.455409	282.799004	5.367616
4.406553	295.588528	5.372621
4.636509	305.290801	5.377626
4.729038	316.757866	5.382630
5.019348	308.429682	5.387635
4.750559	300.862990	5.392640
4.379556	285.510394	5.397645
4.729479	282.067274	5.402650
4.369898	277.096475	5.407654
4.727268	298.630359	5.412659
4.636226	303.403108	5.417664
4.917749	310.506153	5.422669
4.874297	302.625741	5.427674
4.312367	295.506783	5.432678
4.409560	300.645513	5.437683
4.541496	320.329120	5.442688
4.628493	314.136717	5.447693
4.978233	314.705320	5.452698
4.707464	316.026051	5.457702
4.982068	312.101173	5.462707
4.928158	321.708725	5.467712
4.822865	302.037023	5.472717
4.827565	310.388848	5.477722
4.761499	309.367932	5.482726
5.061203	311.833163	5.487731
4.666660	302.403713	5.492736
4.946305	300.401638	5.497741
4.690411	312.701586	5.502746
4.849703	305.324088	5.507750
4.824406	308.934914	5.512755
4.671639	311.116693	5.517760
4.991022	316.451572	5.522765
5.090928	301.376363	5.527770
4.714099	310.107510	5.532774
4.724295	310.685019	5.537779
4.441976	316.028750	5.542784
4.980582	312.701597	5.547789
5.337385	320.795776	5.552794
5.123740	323.834994	5.557798
4.825806	314.751073	5.562803
5.165961	323.986831	5.567808
5.360497	320.289636	5.572813
5.044446	323.430321	5.577818
5.110285	319.041434	5.582822
5.150061	309.759069	5.587827
4.808170	315.064677	5.592832
5.216335	321.825177	5.597837
5.559420	326.915897	5.602842
5.090678	324.407808	5.607846
5.189855	308.861299	5.612851
4.998821	317.911358	5.617856
5.216273	313.182338	5.622861
4.679914	319.439082	5.627866
5.183937	331.689583	5.632870
5.644426	331.763100	5.637875
5.687097	343.272796	5.642880
5.223537	329.541877	5.647885
5.154171	325.901848	5.652890
5.044491	330.225100	5.657894
5.576603	331.527606	5.662899
5.742111	330.584303	5.667904
5.685498	326.303186	5.672909
5.354478	314.794649	5.677914
5.085383	307.623478	5.682918
5.387511	308.243833	5.687923
4.957658	309.412317	5.692928
5.121731	307.478970	5.697933
5.515485	333.414368	5.702938
5.124496	332.953732	5.707942
5.590632	330.520631	5.712947
5.316652	333.120044	5.717952
5.298170	338.533177	5.722957
5.234671	333.449532	5.727962
5.234776	343.061286	5.732966
5.618353	331.048464	5.737971
5.549347	333.119043	5.742976
5.357069	334.794479	5.747981
5.341110	339.451068	5.752986
5.290606	342.458400	5.757990
5.447299	333.850577	5.762995
5.373684	344.710931	5.768000
5.291272	336.937849	5.773005
5.695069	338.288934	5.778010
5.247438	339.643706	5.783014
5.827356	348.228132	5.788019
5.417226	351.535425	5.793024
5.958630	355.478256	5.798029
5.635889	349.919523	5.803034
5.632261	347.705558	5.808038
5.768342	336.161788	5.813043
5.515233	351.463777	5.818048
5.709169	355.828052	5.823053
6.007142	360.043147	5.828058
5.697523	353.533214	5.833062
5.582459	338.184766	5.838067
5.391280	350.737196	5.843072
5.892903	366.506251	5.848077
6.020050	361.256683	5.853082
5.923214	363.897949	5.858086
6.012460	359.853404	5.863091
5.626413	356.579367	5.868096
5.913693	361.172631	5.873101
5.660599	356.080719	5.878106
5.760717	364.161351	5.883110
6.313882	357.231493	5.888115
5.837984	361.529873	5.893120
5.531009	339.228967	5.898125
5.856693	350.615230	5.903130
5.778108	369.272000	5.908134
6.063216	371.350378	5.913139
5.937667	368.611337	5.918144
5.916355	370.253662	5.923149
5.811724	371.978644	5.928154
6.090673	369.657126	5.933158
5.959058	363.185740	5.938163
5.662430	364.991426	5.943168
5.947483	368.253076	5.948173
5.541856	368.342072	5.953178
5.809997	374.773348	5.958182
5.846157	362.220142	5.963187
5.822028	371.639553	5.968192
5.639329	365.948140	5.973197
6.103655	374.854416	5.978202
6.180585	390.727999	5.983206
6.653502	375.597447	5.988211
6.266428	370.729007	5.993216
6.115784	380.237849	5.998221
6.005279	372.061021	6.003226
5.944792	371.026572	6.008230
5.688976	371.164863	6.013235
6.034465	381.095853	6.018240
6.167256	377.420975	6.023245
6.570749	389.456309	6.028250
5.948516	378.176859	6.033254
5.904076	372.485929	6.038259
5.761875	383.758856	6.043264
5.761697	381.718356	6.048269
6.363061	370.993858	6.053274
6.499999	389.676994	6.058278
6.470224	387.024186	6.063283
5.951498	385.017475	6.068288
6.252375	373.137806	6.073293
6.057665	365.527842	6.078298
6.153654	365.361071	6.083302
6.299111	362.076524	6.088307
6.129703	365.384069	6.093312
6.047593	366.010844	6.098317
6.149175	363.233054	6.103322
5.835655	359.808445	6.108326
5.765840	369.285634	6.113331
5.877408	373.757732	6.118336
6.320113	385.609746	6.123341
6.320844	390.969264	6.128346
6.199802	376.855606	6.133350
6.267815	371.121746	6.138355
6.082065	375.817603	6.143360
5.996093	368.519637	6.148365
6.124768	369.860046	6.153370
5.862881	364.990976	6.158374
6.414668	380.967323	6.163379
6.262695	377.270622	6.168384
6.384160	364.950825	6.173389
6.480277	367.957336	6.178394
6.216817	357.444277	6.183398
6.130000	356.768301	6.188403
6.100827	362.556446	6.193408
6.291999	374.163119	6.198413
6.359653	368.717223	6.203418
5.799127	374.430434	6.208422
6.195944	359.517467	6.213427
6.206206	364.891302	6.218432
6.382110	355.587585	6.223437
6.281371	361.105363	6.228442
5.575797	370.103186	6.233446
5.827410	358.145824	6.238451
6.302642	362.390095	6.243456
5.791834	364.055328	6.248461
5.768092	362.841113	6.253466
6.055526	356.838757	6.258470
5.686688	356.659392	6.263475
6.246029	361.599178	6.268480
6.112429	362.313116	6.273485
6.242439	358.626022	6.278490
6.217183	366.014442	6.283494
6.372703	367.897984	6.288499
6.079476	364.615730	6.293504
5.975989	376.271736	6.298509
6.113948	367.404236	6.303514
5.995481	372.364801	6.308518
5.904744	362.378345	6.313523
5.826519	375.384502	6.318528
5.494173	372.959441	6.323533
5.925735	377.514284	6.328538
5.640165	386.142583	6.333542
6.527583	384.646397	6.338547
6.438876	393.965205	6.343552
6.237974	385.878466	6.348557
6.238740	389.453587	6.353562
6.365084	395.884941	6.358566
6.123243	383.074714	6.363571
6.198924	381.082441	6.368576
6.453549	369.959845	6.373581
6.217727	366.121258	6.378586
6.178255	370.000077	6.383590
6.174767	365.577748	6.388595
6.433104	368.467091	6.393600
6.272382	368.764492	6.398605
6.121868	366.437495	6.403610
6.309940	376.098912	6.408614
6.371657	358.947849	6.413619
6.220168	371.861078	6.418624
6.128146	367.661431	6.423629
6.042360	356.775680	6.428634
6.164543	366.599279	6.433638
6.431037	373.109908	6.438643
6.198975	370.539418	6.443648
5.940619	371.253920	6.448653
6.039901	361.715428	6.453658
5.758111	361.712253	6.458662
6.002589	361.879727	6.463667
5.742536	369.633972	6.468672
5.970317	360.110149	6.473677
6.074153	367.614387	6.478682
5.721705	361.234551	6.483686
5.900491	358.384552	6.488691
5.735892	363.007488	6.493696
5.835557	367.921219	6.498701
6.432322	378.183004	6.503706
5.947148	375.095340	6.508710
6.166687	385.485837	6.513715
6.444458	385.948657	6.518720
6.271087	375.532206	6.523725
6.418022	373.364252	6.528730
6.108074	363.440615	6.533734
6.431103	365.560508	6.538739
6.274122	369.951293	6.543744
6.070632	369.828281	6.548749
6.402362	370.194059	6.553754
6.040641	376.357021	6.558758
6.293493	365.136628	6.563763
6.143161	375.521793	6.568768
5.967727	365.374596	6.573773
6.419838	366.344784	6.578778
6.315354	366.918117	6.583782
6.199508	366.850976	6.588787
6.185380	366.774226	6.593792
6.268855	368.270415	6.598797
6.232156	361.031172	6.603802
6.249169	368.337039	6.608806
6.184650	358.647039	6.613811
5.791782	355.725253	6.618816
5.993693	357.642655	6.623821
6.182658	360.372020	6.628826
5.923207	368.208430	6.633830
6.270279	361.469052	6.638835
6.093318	364.663883	6.643840
5.928183	359.640448	6.648845
6.108806	364.478218	6.653850
6.016813	363.863164	6.658854
6.235096	354.900826	6.663859
6.211852	367.695880	6.668864
6.262667	364.204695	6.673869
6.290649	366.506859	6.678874
5.958892	359.256898	6.683878
6.049139	360.071808	6.688883
6.094886	364.785175	6.693888
6.038978	362.310475	6.698893
6.380014	368.072256	6.703898
6.093757	372.072001	6.708902
6.156877	362.618269	6.713907
6.146074	357.605456	6.718912
6.336351	356.639287	6.723917
6.204903	343.403661	6.728922
5.666681	351.239448	6.733926
6.178937	350.887232	6.738931
6.287644	356.365865	6.743936
6.187785	348.117776	6.748941
5.940010	340.962234	6.753946
5.833362	350.793202	6.758950
6.244156	351.440827	6.763955
5.709578	360.133439	6.768960
6.038413	360.929949	6.773965
6.245079	363.628067	6.778970
6.032898	370.596515	6.783974
6.040454	370.022813	6.788979
6.134571	357.950919	6.793984
6.166156	366.124549	6.798989
5.975156	369.315253	6.803994
5.995683	366.164176	6.808998
6.339281	366.373069	6.814003
6.138168	371.571213	6.819008
5.856868	382.163568	6.824013
6.110911	369.418028	6.829018
6.154191	378.637052	6.834022
6.460475	369.018665	6.839027
6.346924	362.430552	6.844032
6.379287	356.186582	6.849037
5.850422	356.237938	6.854042
5.867814	360.215416	6.859046
6.256421	355.934139	6.864051
6.288770	366.009098	6.869056
6.317237	369.484961	6.874061
5.886453	353.005865	6.879066
5.712188	358.525671	6.884070
6.109787	360.912295	6.889075
6.159619	370.532092	6.894080
5.980393	361.537118	6.899085
5.870831	375.911788	6.904090
5.619412	376.473341	6.909094
5.943682	366.462988	6.914099
6.011559	371.717065	6.919104
5.917990	370.396729	6.924109
6.046411	363.457486	6.929114
5.986323	368.269696	6.934118
6.366328	365.331221	6.939123
6.650009	369.409350	6.944128
6.265509	370.111978	6.949133
6.414120	364.163008	6.954138
6.025714	367.748479	6.959142
6.222159	361.950206	6.964147
6.197356	363.286188	6.969152
6.076359	372.663828	6.974157
6.232376	362.192613	6.979162
6.144427	369.995824	6.984166
6.136991	359.534402	6.989171
5.968053	376.265921	6.994176
6.319694	373.464769	6.999181
6.455672	366.201632	7.004186
6.302772	362.859426	7.009190
6.250313	347.912456	7.014195
5.732314	347.240761	7.019200
5.791460	351.736887	7.024205
6.228503	359.261682	7.029210
5.899367	365.849812	7.034214
6.189505	363.014005	7.039219
6.124357	364.441730	7.044224
6.053935	369.774424	7.049229
6.183419	358.563873	7.054234
6.334984	367.500165	7.059238
6.187333	370.380352	7.064243
5.958554	357.599735	7.069248
6.173444	357.996475	7.074253
6.250370	363.372521	7.079258
5.783532	348.265844	7.084262
6.382210	360.488879	7.089267
6.225711	362.414980	7.094272
5.972750	354.269972	7.099277
5.903816	350.408404	7.104282
6.013804	355.254074	7.109286
6.245932	359.115648	7.114291
6.347117	374.279887	7.119296
5.923281	365.984473	7.124301
5.616287	358.300354	7.129306
5.956517	363.527576	7.134310
6.387522	363.624695	7.139315
6.185613	365.054865	7.144320
6.260014	366.479709	7.149325
6.529975	371.629356	7.154330
6.098332	371.659152	7.159334
6.126318	356.161722	7.164339
6.063906	350.619150	7.169344
5.854808	347.349028	7.174349
5.931507	362.827147	7.179354
6.024706	368.238609	7.184358
6.276151	363.263801	7.189363
6.497070	374.109663	7.194368
6.157472	357.891527	7.199373
5.888579	346.240356	7.204378
5.736927	353.692867	7.209382
6.277744	359.239842	7.214387
6.286736	371.871658	7.219392
6.090638	358.677788	7.224397
6.179291	351.532806	7.229402
5.992774	358.835756	7.234406
6.003169	359.656849	7.239411
6.129853	367.980097	7.244416
6.364794	364.716332	7.249421
5.956037	356.273025	7.254426
6.031518	359.608639	7.259430
6.383155	349.742707	7.264435
5.738337	348.695407	7.269440
5.984134	361.445139	7.274445
6.432083	360.878367	7.279450
5.944797	363.944647	7.284454
6.241348	362.430307	7.289459
6.223558	360.886122	7.294464
5.887530	359.394964	7.299469
6.284107	357.608684	7.304474
6.325329	344.792100	7.309478
6.067198	345.914697	7.314483
6.157514	347.447779	7.319488
5.871203	348.982923	7.324493
5.936515	340.503311	7.329498
6.006745	363.344621	7.334502
6.342578	363.864784	7.339507
6.216660	367.864717	7.344512
6.152987	354.555188	7.349517
6.259112	348.049722	7.354522
5.898072	345.347582	7.359526
5.864051	341.755796	7.364531
5.919701	361.176150	7.369536
6.141919	371.781358	7.374541
6.219567	364.353352	7.379546
5.962452	378.235441	7.384550
6.355421	370.375206	7.389555
6.285341	365.805120	7.394560
5.906837	362.235666	7.399565
6.086813	349.074631	7.404570
6.306286	365.384610	7.409574
6.181246	365.698566	7.414579
6.260278	349.500270	7.419584
6.092915	330.284359	7.424589
5.887016	346.983677	7.429594
5.964762	355.865090	7.434598
6.103070	355.517679	7.439603
6.191880	369.921375	7.444608
5.740482	375.380202	7.449613
6.434849	373.284666	7.454618
5.957866	375.466630	7.459622
6.413129	370.561127	7.464627
6.107741	362.019362	7.469632
6.308339	362.275970	7.474637
6.152177	347.452817	7.479642
5.957919	338.941109	7.484646
5.877324	341.681068	7.489651
6.189824	354.569043	7.494656
6.102119	355.883241	7.499661
6.260145	348.252820	7.504666
6.071163	344.406898	7.509670
5.739002	347.613387	7.514675
5.818970	354.194364	7.519680
6.039225	361.651884	7.524685
6.360255	358.766944	7.529690
6.175706	370.707734	7.534694
6.245905	365.100086	7.539699
6.089733	374.733180	7.544704
5.964427	367.435049	7.549709
6.280089	371.213933	7.554714
6.291164	376.676232	7.559718
6.094508	353.453172	7.564723
6.100385	359.881242	7.569728
5.918783	366.784785	7.574733
6.197080	361.049619	7.579738
6.245967	372.773499	7.584742
6.075370	364.742134	7.589747
5.993747	367.181696	7.594752
6.057750	360.034245	7.599757
6.292295	366.777672	7.604762
6.083757	368.392382	7.609766
6.204330	350.994819	7.614771
6.022225	346.043651	7.619776
5.693235	349.768508	7.624781
6.258784	356.437922	7.629786
6.309401	368.990447	7.634790
6.305071	355.532411	7.639795
6.019693	350.056411	7.644800
5.765626	353.984669	7.649805
5.902134	357.449929	7.654810
6.204521	369.342900	7.659814
6.102672	370.007570	7.664819
6.169592	371.601268	7.669824
6.037173	356.878794	7.674829
6.459628	357.999163	7.679834
6.074140	366.038820	7.684838
6.137753	362.672182	7.689843
6.084173	370.545940	7.694848
5.971808	366.090049	7.699853
5.720088	370.897482	7.704858
6.021268	375.558176	7.709862
6.163650	366.417896	7.714867
6.206687	367.762231	7.719872
6.233980	362.012607	7.724877
6.263670	365.399691	7.729882
5.813346	369.567513	7.734886
6.032169	367.669875	7.739891
6.184781	362.508068	7.744896
6.259291	364.356845	7.749901
6.419130	359.317295	7.754906
6.095159	373.580021	7.759910
6.455499	361.741664	7.764915
6.288573	350.653491	7.769920
6.060839	338.141648	7.774925
6.107963	337.742084	7.779930
5.592548	340.692542	7.784934
6.448304	342.282868	7.789939
5.971138	349.976208	7.794944
6.022329	355.590405	7.799949
6.158031	361.311587	7.804954
6.228855	356.384063	7.809958
6.137853	339.212653	7.814963
6.147320	338.888593	7.819968
6.115924	342.908513	7.824973
5.961575	335.605455	7.829978
6.015696	350.150614	7.834982
6.214216	347.060240	7.839987
6.248026	343.495791	7.844992
6.099992	343.496970	7.849997
5.992893	340.299455	7.855002
5.824726	351.199938	7.860006
6.303209	349.799465	7.865011
6.149637	360.878004	7.870016
5.998237	361.395411	7.875021
6.301907	364.505445	7.880026
5.688576	359.220033	7.885030
5.838404	366.698082	7.890035
6.200131	373.304523	7.895040
6.308062	375.192358	7.900045
6.596907	370.869760	7.905050
6.341230	361.725410	7.910054
6.415059	354.003773	7.915059
6.111707	345.249722	7.920064
5.913982	349.672196	7.925069
5.945606	331.614698	7.930074
6.099737	345.065326	7.935078
5.891449	340.605488	7.940083
6.082972	339.075968	7.945088
5.556757	351.408805	7.950093
5.965088	352.477602	7.955098
6.277555	371.433778	7.960102
6.152078	362.977722	7.965107
6.244721	360.498730	7.970112
6.135928	370.978627	7.975117
6.485492	362.255149	7.980122
5.904099	358.110347	7.985139
6.115639	357.275778	7.990157
6.257151	356.237590	7.995174
6.195789	362.618771	8.000192
6.110754	345.575467	8.005210
5.932359	347.623220	8.010227
6.286196	346.775823	8.015245
5.877461	355.799131	8.020262
5.787701	367.448534	8.025280
6.297600	359.798157	8.030298
6.343597	373.824655	8.035315
6.134460	371.288781	8.040333
6.454130	359.666732	8.045350
6.427176	368.002237	8.050368
6.201986	346.474497	8.055386
6.027249	352.538930	8.060403
6.278252	344.831295	8.065421
6.154790	345.415648	8.070438
5.767567	355.461199	8.075456
6.228378	351.482329	8.080474
6.427697	369.745045	8.085491
6.458753	366.827563	8.090509
6.455456	350.727637	8.095526
5.735057	351.484411	8.100544
6.539173	349.364128	8.105562
5.896291	353.520109	8.110579
6.607707	363.829022	8.115597
6.206564	353.604299	8.120614
6.041619	355.694127	8.125632
6.498213	352.665793	8.130650
6.029085	360.388936	8.135667
6.567744	362.355900	8.140685
6.369089	361.307894	8.145702
5.959344	352.252144	8.150720
6.463730	343.655917	8.155738
6.467684	346.407230	8.160755
6.241885	348.333026	8.165773
6.213569	351.695297	8.170790
6.267447	348.676415	8.175808
6.370614	348.426858	8.180826
6.256264	347.248882	8.185843
6.182627	347.393092	8.190861
6.619668	351.827984	8.195878
6.203725	350.678327	8.200896
6.070145	353.324961	8.205914
6.424045	365.393988	8.210931
6.584166	367.335058	8.215949
6.736476	352.826488	8.220966
6.540707	362.895694	8.225984
6.356245	347.572066	8.231002
6.106141	355.557528	8.236019
6.433274	344.189934	8.241037
6.205508	341.496042	8.246054
5.713223	342.295968	8.251072
6.333494	354.651450	8.256090
6.158183	371.486513	8.261107
6.292289	376.492727	8.266125
6.116091	370.085911	8.271142
6.274554	378.335567	8.276160
6.582697	381.856562	8.281178
6.451903	375.508900	8.286195
6.577210	380.797356	8.291213
6.843405	374.138191	8.296230
6.324444	366.923563	8.301248
6.719367	364.725382	8.306266
6.474643	369.434352	8.311283
6.519474	366.549425	8.316301
6.666790	365.235777	8.321318
6.610983	375.472406	8.326336
6.418576	355.514233	8.331354
6.368453	358.659021	8.336371
6.140405	367.862304	8.341389
6.933624	368.937335	8.346406
6.611138	363.039425	8.351424
6.630486	350.826977	8.356442
6.626903	353.686768	8.361459
6.440815	349.310647	8.366477
6.654223	351.584186	8.371494
6.197509	347.092681	8.376512
5.975941	347.824945	8.381530
6.197256	365.285810	8.386547
6.365105	369.087554	8.391565
7.155117	370.166244	8.396582
6.542175	374.730939	8.401600
6.600753	372.575990	8.406618
6.439760	374.671512	8.411635
6.482781	365.784651	8.416653
6.406979	370.470309	8.421670
6.430726	372.549508	8.426688
6.353517	372.353458	8.431706
6.363096	376.684921	8.436723
6.463680	375.826710	8.441741
6.340859	362.942266	8.446758
6.326824	375.801080	8.451776
6.268900	364.187698	8.456794
6.150636	369.558493	8.461811
6.304845	397.005198	8.466829
6.524085	388.254815	8.471846
6.716299	394.643613	8.476864
6.783154	389.404203	8.481882
6.651979	391.943170	8.486899
6.402945	394.582653	8.491917
6.894794	394.597239	8.496934
6.481482	404.220880	8.501952
6.398038	399.601451	8.506970
6.885594	391.954562	8.511987
6.654116	397.964785	8.517005
6.934460	387.383964	8.522022
6.913163	402.579185	8.527040
6.950606	395.226876	8.532058
6.932679	377.384091	8.537075
6.634182	375.250374	8.542093
6.612729	365.742467	8.547110
6.658968	368.809044	8.552128
6.334089	368.339381	8.557146
6.860376	389.492038	8.562163
6.741569	388.463077	8.567181
6.831216	382.112432	8.572199
6.354154	383.679976	8.577216
6.776950	390.092604	8.582234
7.334165	388.948257	8.587251
6.912713	381.279697	8.592269
6.927957	375.565548	8.597287
6.622652	372.079086	8.602304
6.597511	368.665490	8.607322
6.713343	366.176529	8.612339
6.393137	378.382742	8.617357
6.766607	376.115340	8.622375
6.876823	387.638751	8.627392
6.999118	392.321779	8.632410
6.813014	397.173047	8.637427
6.918662	395.594532	8.642445
7.016384	375.660305	8.647463
6.417714	375.842597	8.652480
6.590390	376.620388	8.657498
6.794453	381.760807	8.662515
6.811887	391.335887	8.667533
6.448438	385.687380	8.672551
6.854218	396.628012	8.677568
6.798000	394.431086	8.682586
7.430386	392.397665	8.687603
6.485951	403.335262	8.692621
6.999332	396.634204	8.697639
6.966433	399.757366	8.702656
7.152161	401.798566	8.707674
7.266092	399.691744	8.712691
7.082362	391.881793	8.717709
6.810359	373.962058	8.722727
6.610254	384.366465	8.727744
6.758950	389.272569	8.732762
6.815783	394.454994	8.737779
7.022744	403.208293	8.742797
7.036841	394.013531	8.747815
7.024879	399.733746	8.752832
7.050853	398.215051	8.757850
6.961897	386.230982	8.762867
6.728894	391.017014	8.767885
6.703037	390.746647	8.772903
6.492870	392.408072	8.777920
6.429209	389.489648	8.782938
6.755557	403.639498	8.787955
7.003811	402.073352	8.792973
6.941324	384.404796	8.797991
6.843440	400.328369	8.803008
6.578338	398.968886	8.808026
6.864663	400.158053	8.813043
7.004403	404.159865	8.818061
7.458327	407.118392	8.823079
7.223756	401.784197	8.828096
7.017446	407.276094	8.833114
7.077406	398.295046	8.838131
6.707116	403.762142	8.843149
7.233269	396.535229	8.848167
7.106189	401.146881	8.853184
6.883367	401.819385	8.858202
7.217996	403.471189	8.863219
6.704052	403.539223	8.868237
7.197443	398.548554	8.873255
6.896266	402.414326	8.878272
7.012599	409.187396	8.883290
7.328128	417.608117	8.888307
7.136741	414.422528	8.893325
6.849185	407.297857	8.898343
7.235993	412.993466	8.903360
7.260428	423.533124	8.908378
7.353199	410.292980	8.913395
6.950833	411.277633	8.918413
7.259163	402.667915	8.923431
6.893100	400.535314	8.928448
7.193996	417.055972	8.933466
7.499362	406.676342	8.938483
7.261669	407.584702	8.943501
7.159295	397.635029	8.948519
7.207273	400.859126	8.953536
7.046272	396.340211	8.958554
7.018708	396.275235	8.963571
7.124402	401.020825	8.968589
7.729729	405.855389	8.973607
7.254928	400.757645	8.978624
7.133292	398.331132	8.983642
7.485732	396.218498	8.988659
7.439911	397.175688	8.993677
7.328070	391.834889	8.998695
7.116140	397.876763	9.003712
7.126205	391.614321	9.008730
7.035752	387.971119	9.013747
6.709962	403.220360	9.018765
6.455492	399.839534	9.023783
7.187934	407.655296	9.028800
7.043203	417.208461	9.033818
7.386505	421.613877	9.038835
7.405941	419.272553	9.043853
7.592850	421.733286	9.048871
7.330452	422.446704	9.053888
7.276678	423.272600	9.058906
7.513918	422.784289	9.063923
6.825669	429.576134	9.068941
7.063587	424.950528	9.073959
7.578966	421.953998	9.078976
7.309677	424.047558	9.083994
7.468064	413.422715	9.089011
7.282147	427.520304	9.094029
7.202199	424.888444	9.099047
7.197961	427.347568	9.104064
7.208778	424.714110	9.109082
7.601924	426.072731	9.114099
7.301605	427.366438	9.119117
7.220410	420.389306	9.124135
7.279863	426.104652	9.129152
7.411611	426.421806	9.134170
7.346572	416.851275	9.139187
7.100036	431.169799	9.144205
7.675985	424.629338	9.149223
7.237585	431.826998	9.154240
7.174051	424.806073	9.159258
7.431112	419.738820	9.164275
7.119448	434.957473	9.169293
7.379799	430.580811	9.174311
7.699668	439.944432	9.179328
7.612835	428.846769	9.184346
7.618210	421.916032	9.189363
7.536611	426.435359	9.194381
7.484244	421.239865	9.199399
7.479455	431.001480	9.204416
7.463739	427.980866	9.209434
7.558930	424.867136	9.214451
7.586903	423.625831	9.219469
7.586553	431.780476	9.224487
7.653177	428.286221	9.229504
7.810627	427.658935	9.234522
7.988014	430.348374	9.239539
7.744504	429.206409	9.244557
7.880693	426.414453	9.249575
7.597287	427.879077	9.254592
7.810953	436.905892	9.259610
7.860709	428.876309	9.264627
7.475751	431.391930	9.269645
7.622076	436.336287	9.274663
8.080427	424.884968	9.279680
7.823221	417.566192	9.284698
7.808390	405.289635	9.289715
7.573011	406.487961	9.294733
7.304846	404.838629	9.299751
7.655072	393.685132	9.304768
7.289818	398.700166	9.309786
7.356815	398.522546	9.314803
7.606388	419.977366	9.319821
8.077040	418.559407	9.324839
7.857971	410.227975	9.329856
7.205951	405.069636	9.334874
7.627328	403.848743	9.339891
7.702595	419.202415	9.344909
7.857688	411.528714	9.349927
7.726414	413.196713	9.354944
7.334309	413.756888	9.359962
7.633607	413.590208	9.364979
7.781566	421.469151	9.369997
7.875865	426.339607	9.375015
8.024096	421.273627	9.380032
7.582574	413.548238	9.385050
7.893380	405.758625	9.390067
7.502384	411.156386	9.395085
7.472321	422.717578	9.400103
7.907290	418.900529	9.405120
7.872120	416.728704	9.410138
7.721612	429.709924	9.415155
7.779633	426.744027	9.420173
8.108542	434.708232	9.425191
7.902586	410.198372	9.430208
7.451047	403.263494	9.435226
7.513056	407.716135	9.440243
7.741769	418.936983	9.445261
7.422625	417.469203	9.450279
7.594145	415.214503	9.455296
7.480301	432.481798	9.460314
7.170125	428.475388	9.465331
7.508733	429.012592	9.470349
7.422614	421.190491	9.475367
8.319404	434.291640	9.480384
8.204790	430.219877	9.485402
7.699778	424.606161	9.490419
7.875948	424.812215	9.495437
7.755804	424.960557	9.500455
8.255917	418.715997	9.505472
8.066721	427.824863	9.510490
7.690556	413.181299	9.515507
7.919093	417.910802	9.520525
7.981385	415.382887	9.525543
7.899572	412.419967	9.530560
7.707798	415.994051	9.535578
7.601441	415.935108	9.540595
7.732660	420.944943	9.545613
8.067772	442.373765	9.550631
8.630575	436.687412	9.555648
7.907797	431.710562	9.560666
7.640507	430.020066	9.565683
7.599641	428.120527	9.570701
8.169479	439.578270	9.575719
8.129318	434.131555	9.580736
7.814409	437.450385	9.585754
8.076261	450.171355	9.590771
8.259755	450.909585	9.595789
8.173873	438.123438	9.600807
8.496476	431.117748	9.605824
8.100083	422.504831	9.610842
7.870802	419.416695	9.615859
7.832299	426.690549	9.620877
7.811331	417.709549	9.625895
8.210274	418.808489	9.630912
7.898862	427.961750	9.635930
8.117479	425.377783	9.640947
7.806086	433.852557	9.645965
7.847564	442.164752	9.650983
8.132194	441.400776	9.656000
7.988157	446.785099	9.661018
8.164591	439.193248	9.666035
8.106891	450.436901	9.671053
8.336568	440.485670	9.676071
8.296712	447.472572	9.681088
7.875806	447.260945	9.686106
8.063778	447.168510	9.691123
8.013720	438.210992	9.696141
8.264035	449.204416	9.701159
8.227810	447.215787	9.706176
8.031794	454.356544	9.711194
7.992197	450.134169	9.716211
8.448795	458.438134	9.721229
8.170852	457.314184	9.726247
8.269075	445.572144	9.731264
8.161393	450.941305	9.736282
8.076916	452.450500	9.741299
8.007755	447.917182	9.746317
7.796142	457.171584	9.751335
8.287715	446.841650	9.756352
8.185914	448.789053	9.761370
8.483304	453.507778	9.766387
8.278713	444.015901	9.771405
7.999112	452.621400	9.776423
8.566277	441.844131	9.781440
8.062658	444.775970	9.786458
8.389655	445.018353	9.791475
8.595011	446.933409	9.796493
8.077520	448.103356	9.801511
8.466288	456.938648	9.806528
8.337300	444.626302	9.811546
8.146253	448.455894	9.816563
8.408614	441.772059	9.821581
8.308583	449.800321	9.826599
8.818532	439.281322	9.831616
8.492670	445.688196	9.836634
8.225210	451.606247	9.841651
8.607468	439.251672	9.846669
8.163147	449.949996	9.851687
8.305284	457.072486	9.856704
8.450551	454.727221	9.861722
8.274960	457.793857	9.866739
8.374360	454.815160	9.871757
8.398147	449.759202	9.876775
8.346202	455.908571	9.881792
8.147477	456.492096	9.886810
8.289524	457.378829	9.891827
8.720598	454.941448	9.896845
8.664742	454.372828	9.901863
8.447755	450.427551	9.906880
8.646537	453.091552	9.911898
8.631364	451.762332	9.916915
8.581309	447.289136	9.921933
8.442493	446.720891	9.926951
8.455757	447.529973	9.931968
8.356072	447.596216	9.936986
8.489917	454.199305	9.942003
8.515034	452.898486	9.947021
8.171876	456.480517	9.952039
8.319754	449.341253	9.957056
8.181326	451.846652	9.962074
8.274230	451.810137	9.967091
8.456364	441.159466	9.972109
8.252529	457.522561	9.977127
8.361952	447.539676	9.982144
8.224128	450.761336	9.987162
8.394626	469.580927	9.992179
8.783707	463.252765	9.997197
8.571414	473.012202	10.002215
8.765137	472.110992	10.007232
8.383937	480.363200	10.012250
8.784973	472.360608	10.017267
8.966170	468.715852	10.022285
8.416095	480.314375	10.027303
8.750409	474.903648	10.032320
8.715624	480.299266	10.037338
8.544331	482.465841	10.042355
8.582720	480.064736	10.047373
8.265932	482.222550	10.052391
8.536913	470.484982	10.057408
8.808232	480.522096	10.062426
8.822159	485.351514	10.067443
9.010655	478.653992	10.072461
8.421272	476.928751	10.077479
8.886197	472.217074	10.082496
8.736082	480.777053	10.087514
8.597204	475.200627	10.092531
8.790793	472.428074	10.097549
8.736808	465.550801	10.102567
8.783642	474.269264	10.107584
8.679023	470.732404	10.112602
8.832205	479.926506	10.117619
8.857307	473.737417	10.122637
8.959429	479.001133	10.127655
9.039592	467.886747	10.132672
8.754531	475.435934	10.137690
8.465358	483.941964	10.142707
8.893480	471.586492	10.147725
8.829987	482.868943	10.152743
8.917949	482.883694	10.157760
8.813505	475.149646	10.162778
8.613153	473.000540	10.167795
8.838500	472.993766	10.172813
8.730368	482.683240	10.177831
8.928294	476.369245	10.182848
8.711337	480.060894	10.187866
8.720523	483.682398	10.192883
8.874127	473.430648	10.197901
8.806935	481.633657	10.202919
8.802730	473.123366	10.207936
8.944095	466.609956	10.212954
9.139399	482.430861	10.217971
9.415227	473.188739	10.222989
9.055584	478.095620	10.228007
9.124597	477.734650	10.233024
8.993359	480.396714	10.238042
8.881883	473.257051	10.243059
9.252333	472.119871	10.248077
9.302270	473.349236	10.253095
8.803751	458.380827	10.258112
8.968841	456.158687	10.263130
8.546914	464.616081	10.268147
8.800920	465.021376	10.273165
8.742691	483.308783	10.278183
9.206705	480.847303	10.283200
9.140969	479.724817	10.288218
9.083906	476.224685	10.293235
9.512872	478.862092	10.298253
9.084957	471.282866	10.303271
9.004603	479.724619	10.308288
8.839845	475.234674	10.313306
9.060034	482.124042	10.318323
9.143956	472.044154	10.323341
8.777178	474.329717	10.328359
8.924159	476.468515	10.333376
8.975849	469.060295	10.338394
8.694118	477.221178	10.343411
9.130101	471.595710	10.348429
9.266270	474.405221	10.353447
8.980058	483.614521	10.358464
9.221565	483.573657	10.363482
8.925902	484.746720	10.368499
8.860757	481.800112	10.373517
8.856774	484.177154	10.378535
8.745626	485.147740	10.383552
9.454867	499.184027	10.388570
9.475069	514.981904	10.393587
9.346692	490.541828	10.398605
9.159466	489.507803	10.403623
8.951052	485.094122	10.408640
8.908745	491.421871	10.413658
9.217242	491.676621	10.418675
9.260421	496.801256	10.423693
9.195517	506.629135	10.428711
9.224997	499.382171	10.433728
9.127768	504.371019	10.438746
9.476578	504.180802	10.443763
9.389825	505.964909	10.448781
9.233026	503.515489	10.453799
9.118021	507.923308	10.458816
9.318867	504.108210	10.463834
9.112368	507.195475	10.468851
9.378264	496.222383	10.473869
9.250877	504.867173	10.478887
9.395534	508.019339	10.483904
9.497368	498.892826	10.488922
9.005874	510.709406	10.493939
9.182474	506.636178	10.498957
8.867246	500.541428	10.503975
8.803629	509.292992	10.508992
9.335402	507.941189	10.514010
9.402875	520.067822	10.519027
9.091233	527.539146	10.524045
9.353208	534.671292	10.529063
9.430183	526.299734	10.534080
9.836282	529.985290	10.539098
9.619245	541.746265	10.544115
9.778817	515.496964	10.549133
9.658948	507.181502	10.554151
9.706652	510.951609	10.559168
9.771405	502.862839	10.564186
9.371233	502.231402	10.569203
9.298964	504.338284	10.574221
9.551721	499.331642	10.579239
9.378374	509.454222	10.584256
9.335486	508.391269	10.589274
9.467380	506.281619	10.594291
9.629274	513.659809	10.599309
9.270857	503.712325	10.604327
9.341026	507.453665	10.609344
9.871193	524.071042	10.614362
9.680457	521.289270	10.619379
9.379234	504.285999	10.624397
9.523609	519.550035	10.629415
9.733556	530.246880	10.634432
10.042185	522.328172	10.639450
9.575852	512.899358	10.644467
9.677193	509.248170	10.649485
9.709045	501.533780	10.654503
9.244960	506.640068	10.659520
9.555094	506.828290	10.664538
9.533598	528.196325	10.669555
9.627635	522.902124	10.674573
9.852839	531.308649	10.679591
9.728458	537.576691	10.684608
9.688661	531.400907	10.689626
9.700633	538.856245	10.694643
9.898237	533.829833	10.699661
9.618945	528.770847	10.704679
9.878880	524.589885	10.709696
10.132546	511.138267	10.714714
9.502915	511.647298	10.719731
9.072824	498.157656	10.724749
9.633142	522.249465	10.729767
9.706454	518.208197	10.734784
10.193859	524.134230	10.739802
10.292949	528.192932	10.744819
9.921068	516.303597	10.749837
9.506332	512.726956	10.754855
9.511236	521.919065	10.759872
9.803246	524.360189	10.764890
9.784547	530.084657	10.769907
10.030524	521.746581	10.774925
10.022814	532.218757	10.779943
10.015140	537.916255	10.784960
9.820609	514.499513	10.789978
9.704210	527.039964	10.794995
10.079870	521.045239	10.800013
9.751819	521.563823	10.805031
9.747496	532.104896	10.810048
9.716963	526.644021	10.815066
9.960396	532.589348	10.820083
9.814667	534.726677	10.825101
9.675464	533.861848	10.830119
9.878192	537.828576	10.835136
10.207453	531.837962	10.840154
9.970823	535.318113	10.845171
9.928196	528.173952	10.850189
9.830921	529.192859	10.855207
9.730542	538.985289	10.860224
10.096241	541.367534	10.865242
10.042362	538.766285	10.870259
9.800511	536.011454	10.875277
9.815542	531.363939	10.880295
9.607681	532.469600	10.885312
9.829203	527.287966	10.890330
10.207532	528.784614	10.895347
9.755099	536.028695	10.900365
9.566943	538.778580	10.905383
9.806207	554.128763	10.910400
10.006837	560.797166	10.915418
10.218868	562.622827	10.920435
10.072642	562.333448	10.925453
10.328583	563.574723	10.930471
10.129672	567.307744	10.935488
10.350552	555.284484	10.940506
10.469129	557.358314	10.945523
10.372592	551.128298	10.950541
10.267567	532.579488	10.955559
9.930023	532.840787	10.960576
10.418213	535.699294	10.965594
10.143380	542.461121	10.970611
10.042846	540.375261	10.975629
10.029418	542.826374	10.980647
10.083339	551.269212	10.985664
10.520720	552.261155	10.990682
10.247165	553.686375	10.995699
10.079823	554.148222	11.000717
10.579930	557.976844	11.005735
10.408669	559.862559	11.010752
10.480623	537.158265	11.015770
9.926188	530.955818	11.020787
10.314652	537.626340	11.025805
10.739820	542.306135	11.030823
10.367622	544.519973	11.035840
10.403192	526.589764	11.040858
10.192277	529.955432	11.045875
10.359251	531.024454	11.050893
10.069732	523.325694	11.055911
10.379771	534.183582	11.060928
10.391662	534.961326	11.065946
10.424804	529.155962	11.070963
10.092957	528.072011	11.075981
10.164288	538.683284	11.080999
10.469109	548.005139	11.086016
10.653857	555.648006	11.091034
10.828510	558.678717	11.096051
10.707672	548.450989	11.101069
10.180758	531.038090	11.106087
9.717177	536.844887	11.111104
10.529739	549.508044	11.116122
10.548795	550.922131	11.121139
10.546990	553.645977	11.126157
10.770122	555.507768	11.131175
10.520145	555.319850	11.136192
10.551230	547.214245	11.141210
10.733424	556.545850	11.146227
10.308703	543.001684	11.151245
10.615255	551.212438	11.156263
10.497531	552.502791	11.161280
10.520536	549.652812	11.166298
10.527510	545.937508	11.171315
10.385053	551.365796	11.176333
10.629693	541.857129	11.181351
10.362064	558.798350	11.186368
10.377216	551.127581	11.191386
10.636027	552.617711	11.196403
10.207463	557.664799	11.201421
10.239761	552.692685	11.206439
10.369478	558.144602	11.211456
10.642070	560.724471	11.216474
10.671915	560.230782	11.221491
10.519480	559.102940	11.226509
10.904354	554.567884	11.231527
10.643126	559.989537	11.236544
10.763199	549.449511	11.241562
10.463377	561.501177	11.246579
10.823164	564.376652	11.251597
10.650752	555.094265	11.256615
10.986859	560.002611	11.261632
10.596249	550.075923	11.266650
10.796203	548.261715	11.271667
10.355773	558.224199	11.276685
10.621763	551.129504	11.281703
10.860665	558.012814	11.286720
10.566851	565.746445	11.291738
11.241168	568.607353	11.296755
10.531111	571.524220	11.301773
10.993052	562.953474	11.306791
10.814295	563.152025	11.311808
10.874900	560.365580	11.316826
10.777739	561.368692	11.321843
10.788504	578.723900	11.326861
11.526623	579.492001	11.331879
10.856415	567.709333	11.336896
10.546755	556.031127	11.341914
10.919713	549.030125	11.346931
10.547273	563.702995	11.351949
10.856941	565.254585	11.356967
11.311307	575.471354	11.361984
11.151205	572.782603	11.367002
11.080345	566.939874	11.372019
10.436523	562.256726	11.377037
11.279092	567.082565	11.382055
11.016372	569.500158	11.387072
11.120723	566.246116	11.392090
10.990118	546.685140	11.397107
10.743560	557.191598	11.402125
11.135775	565.770786	11.407143
11.010176	574.686727	11.412160
10.863413	569.054703	11.417178
11.182317	571.807198	11.422195
11.111193	578.253101	11.427213
11.026818	567.580995	11.432231
11.049202	575.596446	11.437248
10.949944	582.930375	11.442266
11.160077	573.373449	11.447283
11.295779	584.817256	11.452301
11.211201	568.780361	11.457319
10.888541	564.072139	11.462336
11.274558	585.688815	11.467354
11.346120	574.458947	11.472371
11.067396	579.593017	11.477389
11.017206	579.234942	11.482407
11.372200	582.505643	11.487424
11.040513	580.241402	11.492442
11.475752	573.549366	11.497459
10.804901	572.247131	11.502477
10.769171	567.131037	11.507495
11.429353	574.529010	11.512512
11.128173	580.742718	11.517530
11.239166	571.472723	11.522547
11.153559	585.930258	11.527565
11.472009	575.264461	11.532583
11.340447	568.951564	11.537600
10.894735	574.509423	11.542618
11.377763	575.936023	11.547635
11.122386	579.062517	11.552653
11.144042	575.919258	11.557671
11.303361	576.263653	11.562688
11.039430	576.185218	11.567706
11.479871	569.564951	11.572723
11.112009	574.864463	11.577741
11.466743	572.880835	11.582759
11.165068	579.870941	11.587776
11.295573	580.753178	11.592794
11.702497	583.652828	11.597811
11.351422	581.890238	11.602829
11.597902	577.042347	11.607847
11.478005	573.911800	11.612864
11.449354	578.798406	11.617882
11.255520	574.726398	11.622899
11.409984	586.063126	11.627917
11.648480	579.007441	11.632935
11.924417	585.591472	11.637952
11.715483	579.218111	11.642970
11.666652	578.708346	11.647987
11.435141	587.984867	11.653005
11.372608	585.372345	11.658023
11.912331	580.535312	11.663040
11.658751	576.857670	11.668058
11.775381	574.703067	11.673075
11.549622	573.542532	11.678093
11.437223	577.438723	11.683111
11.522270	573.663844	11.688128
11.417264	573.251243	11.693146
11.742498	574.677320	11.698163
11.523262	573.086577	11.703181
11.446433	578.753897	11.708199
11.580824	570.796195	11.713216
11.519003	575.741647	11.718234
11.427746	570.495398	11.723251
11.248802	577.482053	11.728269
11.388958	581.086212	11.733287
11.490582	590.768127	11.738304
11.515207	596.653085	11.743322
11.580131	601.051669	11.748339
11.827481	601.732564	11.753357
12.003352	593.777821	11.758375
12.253027	600.072484	11.763392
11.893589	605.840896	11.768410
12.164341	599.916230	11.773427
12.046593	587.570467	11.778445
11.461849	576.121539	11.783463
11.395632	566.980296	11.788480
11.495950	593.814061	11.793498
11.607018	600.859426	11.798515
11.971046	610.437123	11.803533
12.024539	604.555963	11.808551
11.902578	611.754608	11.813568
11.769270	615.774003	11.818586
11.882692	603.571889	11.823603
11.861076	605.292152	11.828621
11.725582	603.849230	11.833639
12.062311	604.737026	11.838656
12.208725	602.454679	11.843674
11.729261	605.168166	11.848691
11.593083	604.451181	11.853709
11.835404	594.450547	11.858727
11.925775	592.640881	11.863744
11.621683	608.098334	11.868762
11.593432	605.556176	11.873779
11.570885	599.305083	11.878797
11.769684	607.927218	11.883815
12.475801	598.724910	11.888832
11.749951	598.583150	11.893850
12.088561	602.765286	11.898867
12.087159	605.324976	11.903885
11.892617	603.096049	11.908903
11.913349	617.192967	11.913920
11.701937	622.190271	11.918938
12.332542	621.611921	11.923955
12.466221	628.764207	11.928973
12.138957	624.706781	11.933991
12.139935	612.244570	11.939008
11.891605	621.372266	11.944026
12.111546	614.224801	11.949043
12.001764	626.357188	11.954061
12.126990	621.550374	11.959079
12.338634	626.077454	11.964096
12.571966	628.925416	11.969114
12.270516	632.680827	11.974131
12.495874	631.806210	11.979149
12.524124	613.548858	11.984167
12.431795	599.753755	11.989184
11.728727	602.584326	11.994202
12.297827	600.573421	11.999219
12.042436	610.140872	12.004237
12.087716	618.332633	12.009255
12.776645	623.198339	12.014272
12.134311	620.872313	12.019290
12.410907	614.593280	12.024307
12.473181	623.650221	12.029325
12.334788	610.685987	12.034343
12.320939	607.349471	12.039360
12.743939	618.511603	12.044378
12.230898	618.456419	12.049395
12.156033	621.264305	12.054413
12.450033	618.450750	12.059431
12.758162	626.506658	12.064448
12.151119	617.532177	12.069466
12.219068	611.604569	12.074483
12.425637	626.496038	12.079501
12.422861	635.225508	12.084519
12.559389	631.975879	12.089536
12.334259	634.046766	12.094554
12.783785	627.223085	12.099571
12.611976	632.337262	12.104589
12.020100	637.290040	12.109607
12.029026	625.394615	12.114624
11.917028	630.625652	12.119642
12.410688	634.957071	12.124659
12.275936	627.110941	12.129677
12.349510	632.811517	12.134695
12.542143	626.826500	12.139712
12.071561	632.940536	12.144730
12.500952	647.355300	12.149747
12.783747	651.770253	12.154765
13.074375	664.897120	12.159783
12.708594	636.094868	12.164800
12.622080	643.597239	12.169818
12.370689	625.279548	12.174835
12.853111	640.326622	12.179853
12.813378	645.783025	12.184871
12.278302	639.978291	12.189888
12.371810	657.983328	12.194906
12.969688	657.861382	12.199923
12.728483	664.068878	12.204941
12.972223	666.842631	12.209959
12.780414	656.793217	12.214976
12.955666	664.402905	12.219994
13.045236	660.349590	12.225011
13.500685	635.694766	12.230029
12.744732	631.818114	12.235047
12.770413	633.666669	12.240064
12.647162	639.382307	12.245082
12.503320	633.465785	12.250099
12.764912	627.047087	12.255117
12.703256	648.550945	12.260135
12.837671	648.245996	12.265152
12.844930	656.576275	12.270170
12.684358	659.530139	12.275187
13.050927	661.038109	12.280205
12.768908	655.222124	12.285223
12.693900	660.882873	12.290240
12.948851	654.275859	12.295258
12.808364	661.960262	12.300275
12.781735	663.018600	12.305293
12.849899	661.793072	12.310311
12.906215	653.901215	12.315328
12.946685	657.388466	12.320346
13.045551	659.758885	12.325363
13.371944	653.099652	12.330381
12.936501	655.642148	12.335399
13.121367	655.783728	12.340416
13.264898	650.718419	12.345434
12.957179	648.835421	12.350451
13.333274	656.735528	12.355469
13.172481	653.074890	12.360487
13.203510	649.573545	12.365504
12.751720	659.367452	12.370522
13.215419	664.823878	12.375539
13.231103	655.448853	12.380557
13.019955	664.832676	12.385575
12.955469	653.725060	12.390592
13.069834	657.383769	12.395610
13.137267	649.496483	12.400627
13.431527	649.157022	12.405645
13.014734	648.184202	12.410663
13.128818	652.833872	12.415680
13.054109	648.913595	12.420698
13.269083	651.915914	12.425715
12.974312	652.574453	12.430733
12.957896	656.297834	12.435751
13.495642	661.622737	12.440768
13.512658	675.884385	12.445786
13.206290	671.085220	12.450803
13.162172	657.512892	12.455821
13.180175	665.096725	12.460839
13.366499	667.668036	12.465856
13.378053	666.981551	12.470874
13.412871	680.703929	12.475891
13.943442	673.226905	12.480909
13.648338	661.934512	12.485927
13.508875	663.079956	12.490944
13.417007	649.433065	12.495962
13.207927	651.902224	12.500979
13.621208	647.653027	12.505997
12.991924	651.936331	12.511015
13.456364	667.245020	12.516032
13.810675	670.392768	12.521050
13.131522	667.504461	12.526067
13.779169	669.198766	12.531085
13.640288	673.670326	12.536103
13.826200	661.886002	12.541120
13.675100	663.427743	12.546138
13.572233	663.652274	12.551155
13.559923	651.252078	12.556173
13.534345	654.055402	12.561191
13.754066	655.690521	12.566208
13.338069	658.681249	12.571226
13.467980	654.984530	12.576243
13.748074	665.872437	12.581261
13.862080	663.623562	12.586279
13.700941	662.149940	12.591296
13.867140	660.713393	12.596314
13.332325	662.078570	12.601331
13.873206	658.355330	12.606349
13.799661	658.950806	12.611367
13.481694	649.552321	12.616384
13.798675	654.662504	12.621402
13.717159	672.694978	12.626419
13.995961	665.642412	12.631437
13.756418	676.223580	12.636455
13.492337	674.513622	12.641472
13.952529	667.530464	12.646490
13.760131	665.285414	12.651507
14.088548	671.258498	12.656525
13.955370	671.595075	12.661543
13.562796	669.435037	12.666560
13.647163	669.586051	12.671578
13.767575	674.622897	12.676595
13.742481	667.049902	12.681613
13.793515	664.804581	12.686631
13.625064	664.913156	12.691648
13.814436	657.969278	12.696666
13.859212	671.232499	12.701683
13.861104	666.135729	12.706701
13.831921	676.576641	12.711719
14.092157	673.941936	12.716736
14.264326	665.697408	12.721754
13.830565	664.017192	12.726771
14.196026	671.593926	12.731789
14.114871	664.957518	12.736807
14.031680	666.883094	12.741824
14.115041	660.495465	12.746842
13.781745	669.352477	12.751859
14.272865	667.438989	12.756877
13.714651	677.113881	12.761895
14.465211	670.766879	12.766912
14.132458	665.921356	12.771930
13.819247	656.632575	12.776947
14.059258	660.236885	12.781965
14.137954	666.599385	12.786983
14.171470	673.947263	12.792000
14.250218	665.666880	12.797018
14.337563	671.835524	12.802035
14.344185	676.309533	12.807053
14.180625	671.339670	12.812071
13.956433	667.894089	12.817088
14.047576	667.965146	12.822106
13.686382	674.459688	12.827123
13.991863	686.533364	12.832141
14.123441	695.753053	12.837159
14.088303	692.445103	12.842176
14.671453	696.771983	12.847194
14.505254	695.368578	12.852211
14.414019	693.284399	12.857229
14.368917	699.641062	12.862247
14.346814	698.701073	12.867264
14.756618	689.863881	12.872282
14.839151	696.036443	12.877299
14.657143	688.191379	12.882317
14.587827	688.666273	12.887335
14.161389	681.746287	12.892352
14.559290	676.615870	12.897370
14.381664	688.872538	12.902387
14.405334	694.530461	12.907405
14.493862	691.493468	12.912423
14.335276	690.259284	12.917440
14.730181	694.328481	12.922458
14.311980	695.309317	12.927475
14.432455	689.102055	12.932493
14.439225	684.512599	12.937511
14.662679	694.932873	12.942528
14.565444	700.571871	12.947546
14.178633	702.705968	12.952563
14.604936	693.370728	12.957581
14.287830	688.447009	12.962599
14.314515	696.840535	12.967616
14.299274	694.791786	12.972634
14.633498	693.215302	12.977651
14.804712	699.497047	12.982669
14.548682	700.285217	12.987687
14.802835	708.535812	12.992704
14.860401	710.332042	12.997722
14.503594	704.843338	13.002739
14.795308	708.531075	13.007757
15.082216	711.143437	13.012775
14.964029	719.127328	13.017792
14.973749	692.601444	13.022810
14.820169	695.895045	13.027827
14.971589	699.428036	13.032845
14.759966	694.150117	13.037863
14.416206	695.494830	13.042880
15.147136	702.755540	13.047898
14.742567	700.846685	13.052915
14.637620	703.305848	13.057933
14.858670	714.045246	13.062951
15.023610	722.824221	13.067968
15.337876	729.093030	13.072986
15.049310	709.638676	13.078003
14.980835	703.300068	13.083021
14.590182	703.708545	13.088039
14.747325	707.982254	13.093056
15.088720	729.483020	13.098074
14.860890	719.628563	13.103091
15.206834	725.188665	13.108109
15.102379	721.746403	13.113127
15.039487	721.131539	13.118144
15.145955	714.715025	13.123162
15.048942	709.431768	13.128179
14.972829	709.816209	13.133197
14.875257	715.272228	13.138215
15.203474	716.944002	13.143232
15.226343	716.719645	13.148250
15.011781	722.878805	13.153267
14.783075	716.486402	13.158285
15.226101	716.899958	13.163303
14.858769	721.981679	13.168320
15.111358	710.054333	13.173338
15.311691	714.974528	13.178355
15.492147	719.878903	13.183373
15.136157	720.878396	13.188391
14.778891	721.865465	13.193408
15.315167	717.524397	13.198426
15.212060	723.145387	13.203443
15.044553	713.666490	13.208461
15.078011	720.701972	13.213479
15.186885	727.006117	13.218496
15.811939	736.694463	13.223514
15.489284	744.363262	13.228531
15.840462	722.994071	13.233549
15.501119	719.777960	13.238567
15.344873	715.573798	13.243584
15.205838	713.080540	13.248602
15.391143	730.951348	13.253619
15.489626	719.979102	13.258637
15.079725	717.187457	13.263655
15.212572	736.483443	13.268672
15.711982	738.096839	13.273690
15.523939	738.044383	13.278707
15.842540	752.107361	13.283725
16.033190	742.824797	13.288743
15.354953	738.945412	13.293760
15.731655	717.417594	13.298778
15.626509	719.845232	13.303795
15.637637	712.313879	13.308813
15.876986	713.396818	13.313831
15.598417	722.911156	13.318848
15.710002	720.801508	13.323866
15.792755	716.058127	13.328883
15.943218	721.506844	13.333901
15.844895	720.124361	13.338919
15.463023	719.218649	13.343936
15.702405	717.884240	13.348954
15.686545	713.866366	13.353971
15.439547	711.128093	13.358989
15.842033	710.945243	13.364007
15.860391	721.239877	13.369024
16.049301	716.719705	13.374042
15.813427	717.391109	13.379059
15.609564	733.369452	13.384077
15.540038	709.888687	13.389095
15.380571	723.029313	13.394112
15.797257	735.499010	13.399130
15.740881	743.877170	13.404147
15.865159	739.900449	13.409165
16.127730	739.657470	13.414183
16.134907	739.814268	13.419200
16.212146	744.387683	13.424218
16.404259	742.230702	13.429235
15.932852	729.877135	13.434253
15.988584	730.423955	13.439271
16.283427	721.017781	13.444288
16.254625	722.357329	13.449306
16.040185	725.275462	13.454323
16.090830	724.238868	13.459341
15.657575	715.338093	13.464359
15.909408	727.161427	13.469376
16.340825	729.416636	13.474394
16.127461	720.560301	13.479411
15.874250	714.638797	13.484429
15.960101	722.729576	13.489447
16.009432	739.286792	13.494464
16.195477	745.414751	13.499482
16.062608	749.834894	13.504499
16.043905	742.308203	13.509517
16.506455	742.381029	13.514535
16.259654	741.599320	13.519552
16.273896	746.441383	13.524570
16.105582	751.188972	13.529587
16.064736	746.038916	13.534605
16.185231	748.134559	13.539623
16.289574	743.829601	13.544640
16.459525	750.073692	13.549658
16.274009	743.895419	13.554675
16.342018	742.767740	13.559693
16.661540	735.749792	13.564711
16.231099	744.953421	13.569728
16.397927	746.966065	13.574746
16.204777	747.930578	13.579763
16.362703	750.427455	13.584781
16.450461	740.592968	13.589799
16.779960	747.831386	13.594816
16.646679	740.029157	13.599834
16.221038	740.701892	13.604851
16.201701	737.650234	13.609869
16.478769	737.067313	13.614887
16.495662	737.677024	13.619904
16.231667	734.291314	13.624922
16.422910	747.771485	13.629939
16.397576	745.594924	13.634957
16.531094	744.308658	13.639975
16.425903	750.674753	13.644992
16.619925	756.246044	13.650010
16.844132	759.177507	13.655027
16.854719	762.136129	13.660045
16.421978	741.299994	13.665063
16.474262	749.171982	13.670080
16.604673	758.161512	13.675098
16.918141	767.740904	13.680115
16.898771	770.316056	13.685133
16.868858	759.764691	13.690151
16.777471	773.588965	13.695168
16.640083	763.524653	13.700186
16.843301	757.973435	13.705203
16.615056	778.023476	13.710221
17.193335	763.883334	13.715239
16.881078	766.147768	13.720256
16.782701	764.231958	13.725274
17.388180	763.259909	13.730291
16.895916	755.838967	13.735309
16.891361	747.599999	13.740327
17.007213	745.508614	13.745344
16.724036	734.302668	13.750362
17.013662	746.022264	13.755379
16.981276	759.660558	13.760397
16.578161	758.685588	13.765415
16.969862	768.956468	13.770432
17.195927	763.471097	13.775450
17.121681	763.968856	13.780467
16.893276	768.088392	13.785485
16.989920	763.147162	13.790503
17.216023	769.344593	13.795520
16.924531	765.142675	13.800538
16.879189	770.483230	13.805555
16.874919	762.742829	13.810573
16.587124	753.500508	13.815591
16.724246	760.188403	13.820608
16.905575	759.285966	13.825626
16.950081	763.255443	13.830643
16.867216	784.627089	13.835661
17.115437	782.082614	13.840679
17.314309	782.657502	13.845696
17.748212	786.360847	13.850714
17.712312	793.770144	13.855731
17.524307	775.675897	13.860749
17.087341	763.285352	13.865767
17.219661	772.735338	13.870784
17.321354	779.719127	13.875802
17.097213	772.745319	13.880819
17.339889	787.277814	13.885837
17.354515	778.736024	13.890855
17.472133	784.234088	13.895872
17.645584	783.052016	13.900890
17.502756	774.459159	13.905907
17.238826	783.343229	13.910925
17.295001	783.861580	13.915943
17.539248	777.505506	13.920960
17.418591	788.929650	13.925978
17.392429	780.498392	13.930995
17.202412	786.956687	13.936013
17.484042	783.879956	13.941031
17.699286	787.847935	13.946048
17.290962	783.389762	13.951066
17.666691	775.574038	13.956083
17.356767	783.647959	13.961101
17.246576	774.781744	13.966119
17.449299	786.044766	13.971136
17.353878	787.410536	13.976154
17.842508	786.860738	13.981171
17.871721	812.008144	13.986189
17.819512	801.359261	13.991207
17.835489	800.807778	13.996224
17.818072	790.494279	14.001242
17.822096	776.002287	14.006259
17.815551	775.163998	14.011277
17.688431	779.201395	14.016295
17.844359	793.608631	14.021312
17.790353	807.079935	14.026330
18.408230	800.135137	14.031347
17.555801	795.238456	14.036365
17.584651	791.604881	14.041383
17.783216	804.127735	14.046400
18.142841	801.796178	14.051418
18.022170	799.991155	14.056435
18.004499	816.271760	14.061453
18.336199	805.430181	14.066471
18.032069	789.083502	14.071488
17.899016	792.370748	14.076506
18.010494	788.553813	14.081523
17.764246	803.554247	14.086541
18.166691	811.585994	14.091559
18.261930	803.255626	14.096576
18.398425	809.274605	14.101594
18.131034	787.232235	14.106611
18.364433	786.536232	14.111629
18.480280	776.975036	14.116647
18.406366	778.731912	14.121664
18.242607	773.083552	14.126682
18.159616	781.876155	14.131699
18.088801	782.565882	14.136717
18.151774	779.539190	14.141735
18.272983	779.564512	14.146752
18.201422	782.816876	14.151770
17.823646	785.470275	14.156787
17.928841	793.147799	14.161805
18.190436	798.711672	14.166823
18.359788	803.804004	14.171840
18.050979	807.721551	14.176858
18.528948	807.113462	14.181875
18.474499	808.214037	14.186893
18.572439	807.952670	14.191911
18.398472	802.406886	14.196928
18.187275	801.401844	14.201946
18.537288	799.049702	14.206963
18.523283	813.344723	14.211981
18.181256	809.286413	14.216999
18.128629	811.661653	14.222016
18.022036	815.058367	14.227034
18.666606	803.479800	14.232051
18.292601	812.059237	14.237069
18.342241	804.051594	14.242087
18.458838	809.025960	14.247104
18.420793	820.938955	14.252122
18.581288	828.352209	14.257139
18.669623	832.545210	14.262157
18.777584	834.693320	14.267175
18.829510	826.177222	14.272192
18.718344	831.234617	14.277210
19.117266	825.362380	14.282227
18.968271	829.529449	14.287245
18.570618	807.785174	14.292263
18.597678	807.304537	14.297280
18.465466	823.877652	14.302298
18.820926	821.966469	14.307315
18.657150	829.607255	14.312333
18.698585	828.815096	14.317351
19.200329	828.130697	14.322368
19.031582	826.042868	14.327386
19.202421	823.030827	14.332403
19.092783	820.327820	14.337421
19.209715	825.702927	14.342439
19.075652	815.612818	14.347456
18.669336	813.334993	14.352474
19.058041	816.562586	14.357491
18.954566	818.854275	14.362509
18.873042	821.931481	14.367527
18.838675	824.136604	14.372544
18.928787	835.467793	14.377562
18.681457	829.965054	14.382579
18.923701	827.405730	14.387597
19.101626	833.528680	14.392615
19.313961	819.370091	14.397632
18.888560	827.036088	14.402650
19.107413	821.223624	14.407667
18.826858	825.291383	14.412685
18.803550	813.290430	14.417703
19.461673	826.142086	14.422720
19.169929	822.868005	14.427738
19.223763	821.439583	14.432755
19.290965	828.984219	14.437773
19.351147	821.703911	14.442791
19.432846	813.725956	14.447808
19.286400	823.270138	14.452826
19.092284	819.747231	14.457843
19.217251	831.931341	14.462861
19.200672	837.690289	14.467879
19.782761	834.118348	14.472896
19.515900	846.935062	14.477914
19.361947	836.213737	14.482931
19.378007	840.840945	14.487949
19.724537	843.320908	14.492967
19.531106	839.924123	14.497984
19.360647	830.994738	14.503002
19.532661	841.028680	14.508019
19.697463	846.885446	14.513037
19.595423	849.085396	14.518055
20.114952	843.197412	14.523072
19.563581	827.820403	14.528090
19.506793	818.418778	14.533107
19.621518	815.163064	14.538125
19.511056	819.668077	14.543143
20.087156	817.384652	14.548160
19.454546	821.867333	14.553178
19.844655	819.938098	14.558195
19.718340	814.880308	14.563213
19.379760	819.746111	14.568231
19.408157	833.485393	14.573248
19.188422	851.905779	14.578266
19.934978	840.352235	14.583283
19.939664	849.980051	14.588301
20.058624	836.972174	14.593319
20.219168	836.805140	14.598336
19.830434	844.260272	14.603354
20.038492	853.840447	14.608371
20.082471	843.684556	14.613389
19.931214	845.529297	14.618407
20.290376	839.641194	14.623424
20.165026	849.971041	14.628442
20.009310	841.490625	14.633459
20.079562	844.219004	14.638477
19.864184	848.579516	14.643495
20.316247	850.825194	14.648512
20.108591	845.941087	14.653530
20.141276	849.820917	14.658547
19.972774	831.632039	14.663565
19.752439	839.704571	14.668583
20.141040	845.071833	14.673600
19.901782	855.495271	14.678618
20.414511	846.957458	14.683635
20.152257	847.778168	14.688653
20.154944	850.927392	14.693671
20.235250	845.736233	14.698688
19.951932	849.125928	14.703706
20.113113	846.617173	14.708723
20.212170	845.405727	14.713741
20.027202	850.525184	14.718759
20.244587	841.023784	14.723776
19.860406	846.000882	14.728794
20.326102	857.118604	14.733811
20.659539	864.618386	14.738829
20.400977	876.657488	14.743847
20.556433	876.617484	14.748864
20.550079	873.257653	14.753882
20.476647	863.786027	14.758899
20.479365	865.161674	14.763917
20.293527	874.374382	14.768935
20.233139	873.026969	14.773952
20.131040	875.343697	14.778970
20.383125	876.412028	14.783987
20.722559	866.787350	14.789005
20.343433	869.778646	14.794023
19.973978	869.678872	14.799040
20.592828	871.705916	14.804058
20.291628	867.455001	14.809075
20.800044	876.953415	14.814093
20.467952	894.498349	14.819111
21.046667	889.131257	14.824128
20.644043	894.641438	14.829146
20.775611	891.487214	14.834163
21.181350	884.818620	14.839181
20.827751	890.210664	14.844199
20.995295	881.818437	14.849216
20.571947	865.698652	14.854234
21.029658	876.751365	14.859251
20.851575	877.722991	14.864269
20.765911	879.671068	14.869287
20.939571	886.631000	14.874304
21.067208	894.974088	14.879322
20.842837	895.934033	14.884339
21.148703	885.449906	14.889357
20.977284	897.683654	14.894375
21.037873	889.374453	14.899392
20.670981	885.430475	14.904410
20.827032	893.182126	14.909427
21.150083	890.023148	14.914445
20.748710	891.960730	14.919463
20.818522	889.583050	14.924480
21.047309	885.290119	14.929498
21.203771	884.094923	14.934515
21.005886	877.413608	14.939533
20.558147	892.754957	14.944551
20.796981	902.365050	14.949568
20.839896	912.939972	14.954586
21.114035	918.441956	14.959603
21.027327	918.414647	14.964621
21.323730	915.524930	14.969639
21.715837	908.110530	14.974656
21.337217	909.230344	14.979674
21.113328	911.793378	14.984691
21.506087	904.571384	14.989709
21.470391	917.986253	14.994727
21.477911	913.393465	14.999744
21.488903	907.203281	15.004762
21.620825	912.964234	15.009779
22.097818	913.470305	15.014797
21.479548	913.848175	15.019815
21.844633	909.376092	15.024832
21.971795	914.607611	15.029850
21.695632	915.443126	15.034867
21.545731	903.884829	15.039885
21.634734	917.437952	15.044903
21.575050	911.899475	15.049920
21.560802	920.053364	15.054938
21.859565	918.002729	15.059955
21.772983	905.109059	15.064973
21.548393	923.397735	15.069991
21.505551	912.829370	15.075008
21.282684	909.926337	15.080026
21.496587	918.082349	15.085043
21.795675	911.960636	15.090061
21.508748	920.214053	15.095079
21.747063	913.757874	15.100096
21.456626	925.609497	15.105114
21.745936	931.989588	15.110131
22.294900	938.660361	15.115149
21.821387	943.534716	15.120167
21.709165	940.008421	15.125184
21.837051	935.453574	15.130202
21.633355	932.910455	15.135219
22.190119	934.672676	15.140237
22.122028	939.748599	15.145255
22.001341	933.052012	15.150272
22.047776	935.733644	15.155290
22.121356	929.454750	15.160307
22.214293	929.153140	15.165325
22.320307	942.896123	15.170343
22.472264	932.322473	15.175360
22.415468	934.480630	15.180378
22.403006	934.356480	15.185395
22.667597	927.738388	15.190413
22.111095	921.753879	15.195431
21.829632	916.941277	15.200448
22.084833	940.860551	15.205466
22.176633	938.769756	15.210483
22.655220	938.016398	15.215501
22.067114	941.782071	15.220519
22.420941	942.294818	15.225536
22.379644	941.679719	15.230554
22.206539	938.251327	15.235571
22.384273	937.065418	15.240589
22.222708	944.983621	15.245607
22.362960	937.293085	15.250624
22.144853	935.986158	15.255642
22.044533	939.233588	15.260659
22.204312	944.235940	15.265677
22.391991	949.672584	15.270695
22.565073	955.439725	15.275712
22.800235	965.769960	15.280730
22.612869	968.838527	15.285747
22.839353	959.105262	15.290765
22.907437	971.304691	15.295783
22.756690	958.013932	15.300800
22.822141	965.640952	15.305818
22.764884	961.023587	15.310835
23.105168	956.334468	15.315853
22.856596	942.399476	15.320871
22.482288	943.231435	15.325888
22.592954	946.815043	15.330906
22.574550	954.512002	15.335923
22.740429	952.232872	15.340941
22.709140	964.959113	15.345959
22.890414	956.264894	15.350976
22.942776	952.652849	15.355994
22.799034	965.551345	15.361011
23.163934	958.030733	15.366029
23.129889	967.289135	15.371047
22.856006	960.354605	15.376064
22.635161	957.681625	15.381082
23.135756	959.739830	15.386099
23.293206	959.352371	15.391117
22.775892	963.725503	15.396135
22.701102	963.169300	15.401152
22.956249	958.761767	15.406170
22.896622	976.630171	15.411187
23.331900	989.368536	15.416205
22.852274	982.942766	15.421223
23.008895	980.362122	15.426240
23.599122	979.569179	15.431258
23.272440	987.140881	15.436275
23.635962	985.373587	15.441293
23.348575	983.635691	15.446311
23.211018	986.087379	15.451328
23.638490	983.006699	15.456346
23.684585	982.090725	15.461363
23.694186	970.343290	15.466381
23.589276	979.347710	15.471399
23.842699	966.416503	15.476416
23.534689	951.610336	15.481434
23.257143	952.215693	15.486451
23.260963	956.948991	15.491469
23.546392	968.741975	15.496487
23.756578	975.569985	15.501504
23.921879	967.178069	15.506522
23.623490	965.419809	15.511539
23.877383	960.955667	15.516557
23.426786	948.857465	15.521575
23.600731	951.187758	15.526592
23.952991	959.543021	15.531610
23.897238	948.708411	15.536627
24.160752	942.538611	15.541645
23.651670	948.191721	15.546663
23.416791	953.057092	15.551680
23.524493	942.256837	15.556698
23.618670	963.638828	15.561715
23.907082	969.895995	15.566733
24.037660	972.788514	15.571751
24.130113	972.600588	15.576768
23.908509	978.284407	15.581786
23.880998	974.473430	15.586803
24.274826	969.400373	15.591821
24.375720	977.990690	15.596839
23.810043	966.825703	15.601856
24.083558	969.093060	15.606874
23.975690	978.239956	15.611891
24.318761	981.238041	15.616909
23.959454	980.073155	15.621927
23.688814	978.196935	15.626944
24.337720	982.573545	15.631962
24.334402	980.841636	15.636979
24.259231	981.686689	15.641997
24.139239	978.944254	15.647015
24.101806	978.296990	15.652032
24.387311	970.697292	15.657050
23.823848	974.563254	15.662067
23.917469	970.969988	15.667085
24.030886	978.889304	15.672103
24.042759	974.358935	15.677120
24.480676	983.748530	15.682138
24.648977	997.368185	15.687155
24.518962	989.013062	15.692173
23.979820	989.993926	15.697191
24.240629	1003.346625	15.702208
24.532530	1005.620573	15.707226
24.336309	1009.504744	15.712243
24.352789	1005.595348	15.717261
24.459381	1008.775658	15.722279
24.471535	1002.828260	15.727296
24.840002	996.733518	15.732314
24.724533	1004.830720	15.737331
24.632398	1006.031888	15.742349
24.800369	997.219811	15.747367
24.749044	1003.830025	15.752384
24.801838	989.516415	15.757402
24.696759	991.802066	15.762419
24.501172	995.058120	15.767437
24.437538	994.212987	15.772455
24.442427	1006.428652	15.777472
25.124012	1010.030121	15.782490
24.835189	1014.152868	15.787507
24.955913	1011.950234	15.792525
24.868088	1012.658414	15.797543
24.806419	1011.516321	15.802560
25.194817	1012.604330	15.807578
25.071062	1019.311106	15.812595
24.987356	1013.063138	15.817613
25.092050	1010.418040	15.822631
25.194525	1019.055468	15.827648
25.294848	1014.460736	15.832666
24.941032	1017.706872	15.837683
25.083615	1013.695664	15.842701
25.320120	1014.504510	15.847719
24.780045	1012.430655	15.852736
25.399691	1010.970373	15.857754
25.184828	1013.004980	15.862771
25.388372	1012.805961	15.867789
25.212778	1003.659541	15.872807
24.997968	1010.721412	15.877824
25.369187	1008.962377	15.882842
25.233782	1004.969479	15.887859
25.379780	1003.539226	15.892877
25.432451	999.949214	15.897895
25.077054	1011.489175	15.902912
25.242681	1008.648335	15.907930
25.293064	1016.905753	15.912947
25.459704	1026.792317	15.917965
25.277985	1031.393756	15.922983
25.320530	1038.219652	15.928000
25.447367	1035.126106	15.933018
25.566373	1029.730012	15.938035
25.468634	1031.235022	15.943053
25.569701	1034.561371	15.948071
25.592710	1034.059272	15.953088
25.752123	1039.156384	15.958106
25.231637	1042.592742	15.963123
25.549362	1039.409326	15.968141
26.028928	1052.749878	15.973159
25.694344	1053.023341	15.978176
25.996354	1050.694468	15.983194
25.969001	1060.251676	15.988211
25.974342	1046.974265	15.993229
25.902516	1039.203303	15.998247
25.897101	1052.354748	16.003264
26.182611	1048.598855	16.008282
25.959607	1044.676479	16.013299
26.020215	1051.300732	16.018317
26.210101	1045.704176	16.023335
26.226373	1053.329472	16.028352
26.239433	1045.141256	16.033370
26.049511	1036.852302	16.038387
26.119603	1041.827707	16.043405
26.405568	1044.433956	16.048423
26.001900	1041.960023	16.053440
26.230074	1045.320109	16.058458
26.362556	1054.243191	16.063475
26.107079	1061.806924	16.068493
26.233695	1053.809200	16.073511
26.371231	1049.205474	16.078528
26.706272	1050.951952	16.083546
26.407761	1048.360555	16.088563
26.209054	1058.493729	16.093581
26.485700	1040.607285	16.098599
26.440848	1053.086400	16.103616
26.578317	1056.100932	16.108634
26.191588	1049.042034	16.113651
26.468008	1055.982776	16.118669
26.279123	1050.322485	16.123687
26.121530	1067.398428	16.128704
26.459960	1050.177648	16.133722
26.357992	1059.282635	16.138739
25.988139	1061.240543	16.143757
26.610904	1072.153907	16.148775
26.687145	1081.941054	16.153792
27.048625	1083.200546	16.158810
26.900033	1079.919767	16.163827
26.707273	1082.222323	16.168845
26.630397	1086.690583	16.173863
26.655414	1090.297106	16.178880
26.767967	1083.055825	16.183898
26.925840	1087.386317	16.188915
26.734689	1087.754075	16.193933
26.896559	1077.248215	16.198951
26.836201	1082.035784	16.203968
27.088718	1084.609408	16.208986
26.666396	1087.367663	16.214003
27.027255	1076.609715	16.219021
26.955318	1076.330778	16.224039
26.776808	1074.083500	16.229056
26.835095	1080.859609	16.234074
27.014532	1084.400911	16.239091
27.264027	1096.654055	16.244109
27.589024	1100.317724	16.249127
27.281421	1086.398180	16.254144
27.068110	1072.921473	16.259162
27.210069	1083.635616	16.264179
27.677807	1099.471191	16.269197
27.561439	1090.971867	16.274215
27.233893	1079.090988	16.279232
27.216475	1070.487806	16.284250
27.553017	1081.638529	16.289267
27.498799	1088.473294	16.294285
27.808719	1092.783120	16.299303
27.503369	1073.712858	16.304320
27.693829	1065.474748	16.309338
27.659779	1066.187128	16.314355
27.229780	1075.955756	16.319373
27.475093	1082.033519	16.324391
27.254687	1086.167653	16.329408
27.577349	1094.287771	16.334426
27.690409	1099.717217	16.339443
27.522684	1089.370290	16.344461
27.793193	1085.683013	16.349479
27.682300	1097.241526	16.354496
27.822632	1094.530871	16.359514
28.031887	1098.525105	16.364531
27.945846	1108.063131	16.369549
28.521180	1087.261156	16.374567
28.411360	1081.705234	16.379584
28.344092	1082.564833	16.384602
28.151797	1070.889991	16.389619
27.720793	1064.491288	16.394637
28.185439	1067.482963	16.399655
28.012828	1067.333410	16.404672
28.061387	1067.906612	16.409690
27.770431	1063.458382	16.414707
27.982118	1085.039861	16.419725
28.418465	1086.041466	16.424743
28.304480	1086.460252	16.429760
28.327608	1084.225562	16.434778
28.335692	1077.436161	16.439795
28.039239	1078.420032	16.444813
28.209170	1073.817535	16.449831
28.319776	1085.013126	16.454848
28.261755	1084.271253	16.459866
28.263415	1088.834507	16.464883
28.010694	1089.811527	16.469901
28.539568	1085.806053	16.474919
28.371116	1091.664620	16.479936
28.058385	1085.004377	16.484954
28.430173	1096.017039	16.489971
28.290875	1091.680743	16.494989
28.263174	1086.537995	16.500007
28.554552	1099.920692	16.505024
28.359969	1083.414565	16.510042
28.305201	1092.417498	16.515059
28.414325	1104.010972	16.520077
28.808739	1106.338301	16.525095
28.764027	1117.469884	16.530112
28.448052	1116.225614	16.535130
29.020152	1112.159712	16.540147
28.796983	1117.540856	16.545165
28.791984	1117.245119	16.550183
28.986676	1118.720098	16.555200
29.016530	1119.069009	16.560218
28.973576	1107.010976	16.565235
28.933371	1115.541414	16.570253
28.676125	1108.462205	16.575271
28.820686	1110.339521	16.580288
28.873919	1117.602440	16.585306
29.180580	1108.759112	16.590323
28.662067	1108.231400	16.595341
28.674190	1106.834737	16.600359
28.792425	1108.974960	16.605376
28.742350	1113.082413	16.610394
29.131652	1122.000005	16.615411
29.090683	1135.908181	16.620429
29.503252	1132.507912	16.625447
29.034747	1133.319923	16.630464
29.134135	1139.152320	16.635482
29.512063	1138.957536	16.640499
29.323341	1140.877605	16.645517
29.154721	1135.097345	16.650535
29.584852	1139.552454	16.655552
29.494873	1135.369369	16.660570
29.708289	1130.403431	16.665587
29.494322	1139.832127	16.670605
29.675523	1126.164178	16.675623
29.726227	1134.850799	16.680640
29.667603	1129.327868	16.685658
29.965141	1132.105889	16.690675
29.382733	1140.257377	16.695693
29.711398	1134.238253	16.700711
29.778010	1147.460537	16.705728
29.927154	1137.821346	16.710746
30.120703	1141.584515	16.715763
29.876525	1137.233081	16.720781
30.116684	1131.385619	16.725799
29.837422	1132.837025	16.730816
30.017957	1141.244526	16.735834
30.015443	1125.500392	16.740851
29.729982	1127.590255	16.745869
29.852916	1131.238251	16.750887
29.518347	1131.041488	16.755904
29.980412	1135.567334	16.760922
29.752776	1130.850384	16.765939
29.921232	1128.346761	16.770957
29.995061	1128.631978	16.775975
29.632682	1136.155685	16.780992
29.677974	1133.428357	16.786010
30.124540	1142.652575	16.791027
30.319688	1155.406591	16.796045
30.177316	1155.504770	16.801063
30.194555	1160.554763	16.806080
30.405004	1160.029605	16.811098
30.355823	1169.618695	16.816115
30.674207	1168.555905	16.821133
30.593354	1160.230869	16.826151
30.333138	1162.294690	16.831168
30.307451	1172.580705	16.836186
30.514293	1160.237339	16.841203
30.362443	1170.309585	16.846221
30.348920	1161.402785	16.851239
29.938340	1160.119685	16.856256
30.114634	1160.543486	16.861274
30.313908	1162.693109	16.866291
30.345895	1162.199068	16.871309
30.556121	1174.947579	16.876327
30.951360	1177.773418	16.881344
30.770834	1183.611815	16.886362
30.959464	1185.883032	16.891379
30.926685	1176.995020	16.896397
30.679894	1181.502549	16.901415
30.992179	1168.688209	16.906432
30.964784	1174.265920	16.911450
30.998696	1180.613530	16.916467
31.181438	1186.319270	16.921485
31.194866	1176.325772	16.926503
30.910773	1158.997291	16.931520
31.207647	1168.879308	16.936538
31.464582	1153.861378	16.941555
31.123459	1152.011962	16.946573
31.087229	1151.310853	16.951591
31.300796	1146.259678	16.956608
30.950827	1153.551070	16.961626
31.146361	1151.207307	16.966643
31.168519	1158.610814	16.971661
31.457264	1171.921392	16.976679
31.476469	1174.537896	16.981696
31.410301	1184.315853	16.986714
31.733618	1171.035868	16.991731
31.420045	1158.136552	16.996749
31.215471	1151.342571	17.001767
31.314667	1160.984150	17.006784
31.258868	1175.469050	17.011802
31.660578	1171.556067	17.016819
31.607998	1174.685604	17.021837
31.475814	1176.218113	17.026855
31.852977	1176.493675	17.031872
31.733209	1174.363416	17.036890
31.585092	1176.968266	17.041907
31.636056	1170.380399	17.046925
31.687491	1169.693957	17.051943
31.974823	1167.657710	17.056960
31.806487	1172.850393	17.061978
31.672309	1175.377318	17.066995
31.447687	1165.055041	17.072013
31.878529	1169.809855	17.077031
31.886100	1177.304020	17.082048
31.704344	1177.689243	17.087066
31.780556	1168.721042	17.092083
31.769598	1170.291363	17.097101
31.965640	1180.192341	17.102119
32.006024	1188.135816	17.107136
32.085657	1201.621194	17.112154
32.474908	1190.981809	17.117171
32.123865	1185.233270	17.122189
32.083431	1191.441049	17.127207
32.480362	1188.750139	17.132224
32.286752	1195.736176	17.137242
32.400999	1195.803616	17.142259
32.475807	1188.359918	17.147277
32.253145	1196.568678	17.152295
32.885528	1183.155052	17.157312
32.685141	1199.843341	17.162330
32.471990	1193.735515	17.167347
32.526223	1199.215235	17.172365
32.306743	1190.795136	17.177383
32.536590	1192.532864	17.182400
32.721800	1191.595082	17.187418
32.342153	1188.098014	17.192435
32.258484	1195.669599	17.197453
32.460431	1196.755274	17.202471
32.547574	1195.006015	17.207488
32.520787	1198.510221	17.212506
32.514731	1192.202686	17.217523
32.679064	1190.251981	17.222541
32.255197	1196.715502	17.227559
32.660402	1203.352095	17.232576
32.696449	1204.574219	17.237594
33.147233	1207.085239	17.242611
33.200346	1210.955635	17.247629
32.906915	1215.505194	17.252647
33.032564	1213.513209	17.257664
33.089706	1218.093051	17.262682
33.232665	1207.782586	17.267699
33.073440	1202.237524	17.272717
32.984497	1210.090816	17.277735
33.631905	1205.763779	17.282752
33.435918	1213.223578	17.287770
33.600688	1206.551594	17.292787
33.526391	1209.277430	17.297805
33.150731	1213.839871	17.302823
33.416489	1216.891136	17.307840
33.213573	1208.272769	17.312858
33.343329	1209.186714	17.317875
33.209845	1214.812618	17.322893
33.132276	1214.247375	17.327911
33.412401	1212.941262	17.332928
33.424505	1206.880192	17.337946
33.731833	1208.905590	17.342963
33.940683	1215.219492	17.347981
33.719467	1208.131443	17.352999
33.496520	1194.239577	17.358016
33.533891	1211.632259	17.363034
33.597683	1208.258218	17.368051
33.766132	1201.926495	17.373069
33.443543	1207.266436	17.378087
33.864164	1219.000535	17.383104
34.005788	1235.098770	17.388122
33.745309	1226.558842	17.393139
34.047836	1230.276553	17.398157
33.845080	1232.669060	17.403175
33.755832	1228.302796	17.408192
34.032877	1223.749753	17.413210
33.946034	1224.195848	17.418227
34.450767	1213.118623	17.423245
34.116058	1233.716045	17.428263
34.017718	1232.563904	17.433280
34.256263	1227.174268	17.438298
34.047655	1232.931872	17.443315
34.115917	1233.877544	17.448333
34.485172	1230.947960	17.453351
34.281624	1225.087933	17.458368
34.277507	1223.668559	17.463386
34.277476	1220.064669	17.468403
34.442043	1215.510315	17.473421
34.230115	1227.693829	17.478439
34.391600	1226.093869	17.483456
34.470859	1240.971084	17.488474
34.655521	1245.196428	17.493491
34.638117	1236.350161	17.498509
34.628283	1245.295636	17.503527
34.732025	1244.566282	17.508544
34.777157	1247.506948	17.513562
34.802830	1249.589104	17.518579
34.813856	1238.627087	17.523597
34.745236	1246.890633	17.528615
35.019229	1242.887188	17.533632
34.803045	1242.624537	17.538650
34.948197	1247.389419	17.543667
34.792741	1240.076452	17.548685
34.580112	1255.371806	17.553703
34.942698	1230.071132	17.558720
34.983861	1240.520287	17.563738
34.766070	1243.044542	17.568755
34.908195	1234.832863	17.573773
34.825888	1244.809046	17.578791
34.523426	1241.113676	17.583808
34.860587	1261.530121	17.588826
35.304168	1260.495049	17.593843
35.242538	1257.557229	17.598861
35.141563	1264.026991	17.603879
35.068056	1263.887156	17.608896
35.370662	1256.972644	17.613914
35.566755	1258.226503	17.618931
35.370367	1253.867552	17.623949
35.150292	1263.524494	17.628967
35.233676	1267.371224	17.633984
35.543448	1266.227725	17.639002
35.850053	1273.555155	17.644019
35.848964	1264.583237	17.649037
35.557050	1267.800782	17.654055
35.653270	1265.008648	17.659072
35.970287	1274.821295	17.664090
35.856272	1275.508341	17.669107
35.844724	1266.282433	17.674125
35.875828	1263.064987	17.679143
36.058434	1262.209663	17.684160
35.902569	1259.135124	17.689178
35.690672	1262.485303	17.694195
35.794869	1265.549266	17.699213
36.085733	1287.254289	17.704231
36.365130	1278.645530	17.709248
36.342591	1280.924597	17.714266
36.100158	1275.206350	17.719283
36.231078	1273.582773	17.724301
36.434924	1280.929461	17.729319
36.205976	1267.912662	17.734336
36.401025	1268.260942	17.739354
36.151038	1266.103736	17.744371
36.422433	1271.360100	17.749389
35.926082	1287.201721	17.754407
36.177150	1284.782967	17.759424
36.194690	1280.466233	17.764442
35.976989	1278.531192	17.769459
36.424328	1279.180781	17.774477
36.634702	1279.245785	17.779495
36.729776	1274.254166	17.784512
36.486366	1272.840721	17.789530
36.255777	1282.354149	17.794547
36.594636	1275.856840	17.799565
36.714162	1289.108809	17.804583
36.850596	1295.061689	17.809600
36.817531	1289.096033	17.814618
36.453115	1291.261403	17.819635
36.741595	1298.702139	17.824653
36.876067	1300.025617	17.829671
36.839453	1299.447643	17.834688
37.255436	1298.659898	17.839706
37.021624	1303.496793	17.844723
37.175456	1293.900966	17.849741
36.696296	1298.236640	17.854759
37.170226	1294.463799	17.859776
37.446595	1288.064642	17.864794
36.855853	1297.015949	17.869811
37.364522	1287.276165	17.874829
37.060539	1296.665396	17.879847
37.117296	1290.897112	17.884864
37.119173	1292.459122	17.889882
37.050020	1290.453466	17.894899
37.585659	1297.344222	17.899917
37.508126	1312.526937	17.904935
37.609371	1307.597460	17.909952
37.528212	1298.811645	17.914970
37.119050	1301.078704	17.919987
37.896178	1305.713026	17.925005
37.993623	1313.729671	17.930023
37.533878	1293.345259	17.935040
37.727507	1298.033129	17.940058
37.715652	1302.039961	17.945075
37.765946	1296.367364	17.950093
37.970840	1305.042534	17.955111
37.883494	1295.370881	17.960128
37.897537	1306.600676	17.965146
37.758853	1306.370064	17.970163
37.941204	1309.876239	17.975181
38.125860	1310.270331	17.980199
38.146916	1314.959997	17.985216
37.956649	1311.827720	17.990234
37.838238	1297.780535	17.995251
38.019249	1292.633431	18.000269
37.873565	1304.904452	18.005287
38.117922	1304.153064	18.010304
38.297004	1293.028979	18.015322
38.273321	1296.741008	18.020339
38.305747	1302.855357	18.025357
38.238106	1301.887756	18.030375
38.224107	1293.287087	18.035392
38.446868	1292.532772	18.040410
38.588732	1295.540344	18.045427
38.392955	1307.917048	18.050445
38.523205	1311.270436	18.055463
38.629756	1322.034452	18.060480
38.942477	1324.838529	18.065498
39.058861	1326.414160	18.070515
39.111109	1306.785830	18.075533
38.762378	1308.150301	18.080551
38.612498	1301.868417	18.085568
38.455375	1298.311215	18.090586
38.701351	1317.416531	18.095603
38.939563	1316.126445	18.100621
38.654929	1321.028114	18.105639
38.733737	1321.839590	18.110656
39.231838	1322.983018	18.115674
39.039013	1325.818963	18.120691
38.753356	1321.644401	18.125709
39.179827	1319.564245	18.130727
39.134389	1328.720475	18.135744
38.665975	1316.258729	18.140762
38.763635	1327.055700	18.145779
38.868943	1330.895854	18.150797
39.008109	1344.431974	18.155815
39.363557	1342.189369	18.160832
39.689612	1341.425179	18.165850
39.420869	1355.384992	18.170867
39.420025	1350.414692	18.175885
39.362063	1350.616416	18.180903
39.432169	1351.299864	18.185920
39.608237	1337.222290	18.190938
39.515950	1344.274563	18.195955
39.360062	1352.359320	18.200973
39.551586	1347.147435	18.205991
39.644936	1355.657063	18.211008
39.525364	1355.477106	18.216026
39.626160	1366.204180	18.221043
39.971321	1366.361679	18.226061
39.853760	1367.932940	18.231079
40.221533	1369.484968	18.236096
40.440425	1359.364498	18.241114
40.307388	1368.793258	18.246131
40.031754	1345.211401	18.251149
40.205829	1355.223218	18.256167
40.173588	1339.483553	18.261184
40.024038	1334.675416	18.266202
39.943518	1347.917745	18.271219
40.273385	1350.223661	18.276237
40.651584	1361.932942	18.281255
40.718864	1358.217488	18.286272
40.549426	1352.554054	18.291290
40.087559	1349.019340	18.296307
40.017903	1354.433309	18.301325
40.501738	1355.244447	18.306343
40.263330	1365.415574	18.311360
40.735947	1358.512257	18.316378
40.525001	1365.510544	18.321395
40.502402	1353.367101	18.326413
40.677640	1353.570158	18.331431
40.492071	1365.200507	18.336448
40.779614	1366.831379	18.341466
40.370206	1364.228906	18.346483
40.706997	1362.311124	18.351501
40.857849	1362.101422	18.356519
41.017213	1362.830849	18.361536
41.004683	1360.488099	18.366554
40.855108	1354.875202	18.371571
40.770746	1365.322006	18.376589
41.166384	1385.139275	18.381607
41.297659	1389.227846	18.386624
41.708076	1387.828721	18.391642
41.261974	1375.852605	18.396659
41.017597	1371.444337	18.401677
41.125437	1375.568136	18.406695
41.408198	1384.411032	18.411712
41.404100	1383.809025	18.416730
41.115123	1382.633092	18.421747
41.187755	1389.599582	18.426765
41.505342	1377.547995	18.431783
41.359784	1389.989474	18.436800
41.853896	1382.442128	18.441818
41.552208	1382.950291	18.446835
41.622669	1387.629080	18.451853
41.753638	1380.138631	18.456871
41.733688	1384.724282	18.461888
41.841512	1375.410185	18.466906
41.796781	1381.012768	18.471923
41.785708	1381.103000	18.476941
42.069481	1380.866160	18.481959
41.887677	1377.265470	18.486976
41.794035	1378.684657	18.491994
41.637683	1380.422949	18.497011
41.654144	1392.592883	18.502029
41.914578	1403.964023	18.507047
41.968860	1413.413952	18.512064
42.249753	1405.679089	18.517082
41.849546	1413.111005	18.522099
42.242296	1409.199375	18.527117
42.484858	1401.568353	18.532135
42.154420	1410.175963	18.537152
42.420260	1400.256406	18.542170
42.313215	1416.933428	18.547187
42.176677	1409.409137	18.552205
42.106130	1410.831020	18.557223
42.250121	1436.106495	18.562240
42.696123	1429.194697	18.567258
42.266509	1428.290114	18.572275
42.677153	1428.153321	18.577293
42.815859	1426.361246	18.582311
42.982226	1428.058448	18.587328
43.147529	1416.914353	18.592346
42.998333	1426.364611	18.597363
43.100817	1415.968846	18.602381
43.182807	1412.345754	18.607399
42.905620	1426.505768	18.612416
43.159720	1423.174458	18.617434
43.405287	1428.356017	18.622451
43.115903	1416.440529	18.627469
42.957530	1405.965716	18.632487
43.042701	1422.069809	18.637504
43.306106	1431.780484	18.642522
43.134705	1432.176714	18.647539
42.995885	1431.782013	18.652557
43.626844	1429.196418	18.657575
43.434591	1428.529211	18.662592
43.186147	1419.416082	18.667610
43.188147	1431.853406	18.672627
43.289886	1428.722698	18.677645
43.613923	1424.307414	18.682663
43.384376	1417.605609	18.687680
43.536456	1420.930350	18.692698
43.255426	1428.447746	18.697715
43.375475	1429.328508	18.702733
43.617512	1441.355831	18.707751
43.949435	1456.670184	18.712768
43.816800	1445.828383	18.717786
43.579094	1456.084661	18.722803
43.848731	1447.985455	18.727821
44.093317	1443.797218	18.732839
43.732475	1447.126584	18.737856
44.230081	1445.647520	18.742874
43.683062	1444.098585	18.747891
43.597344	1446.561148	18.752909
43.912418	1455.582060	18.757927
44.356717	1468.549740	18.762944
44.631075	1467.478052	18.767962
44.179786	1465.434414	18.772979
43.998275	1471.935804	18.777997
44.359573	1470.414976	18.783015
44.335968	1466.912563	18.788032
44.637138	1460.973381	18.793050
44.533798	1469.810538	18.798067
44.509553	1462.884038	18.803085
44.637780	1462.378066	18.808103
44.643390	1456.261122	18.813120
44.683570	1465.902644	18.818138
44.788700	1466.255549	18.823155
44.798485	1481.298489	18.828173
44.962527	1474.604427	18.833191
45.322897	1485.849505	18.838208
44.912838	1472.984013	18.843226
45.048667	1463.690730	18.848243
44.826921	1459.348325	18.853261
45.204747	1467.545181	18.858279
45.241718	1481.252058	18.863296
45.075844	1487.700510	18.868314
45.112478	1481.550293	18.873331
45.007339	1487.998696	18.878349
45.201518	1486.254731	18.883367
45.054817	1488.786817	18.888384
45.206607	1485.638789	18.893402
45.410844	1482.599314	18.898419
45.133391	1487.446252	18.903437
45.482274	1473.549786	18.908455
45.266951	1489.290749	18.913472
45.388890	1493.879445	18.918490
45.728015	1492.870194	18.923507
45.802843	1500.151977	18.928525
46.240502	1495.185521	18.933543
45.552225	1487.867567	18.938560
45.901534	1501.989446	18.943578
46.062281	1500.389579	18.948595
45.985892	1498.735343	18.953613
46.069558	1494.114695	18.958631
46.129657	1492.574781	18.963648
46.166354	1483.306486	18.968666
46.191636	1481.898265	18.973683
45.779421	1478.901723	18.978701
46.191525	1486.979604	18.983719
46.148042	1502.914571	18.988736
46.369229	1497.840012	18.993754
46.400492	1501.578190	18.998771
46.505963	1489.704935	19.003789
46.648812	1489.471238	19.008807
46.273231	1503.021853	19.013824
46.452155	1500.781637	19.018842
46.563651	1513.211331	19.023859
46.514265	1505.026377	19.028877
46.686392	1493.925349	19.033895
46.169816	1506.753255	19.038912
46.564291	1494.487564	19.043930
46.873829	1492.135363	19.048947
46.461084	1497.252820	19.053965
46.727298	1497.290141	19.058983
46.701883	1510.665973	19.064000
47.043710	1524.785887	19.069018
47.270249	1513.288141	19.074035
47.026632	1520.174837	19.079053
47.071625	1515.913708	19.084071
47.027244	1515.895546	19.089088
47.027165	1514.526011	19.094106
47.335688	1508.431020	19.099123
46.980029	1512.289785	19.104141
47.264680	1518.866485	19.109159
47.194978	1516.882982	19.114176
47.615270	1514.365097	19.119194
47.340062	1511.293432	19.124211
47.491269	1522.574460	19.129229
47.804448	1516.150519	19.134247
47.535706	1520.891955	19.139264
47.300971	1515.147176	19.144282
47.788541	1530.980030	19.149299
47.989439	1548.524152	19.154317
48.268208	1544.412590	19.159335
47.927994	1530.636669	19.164352
47.529751	1525.135266	19.169370
47.888821	1530.223329	19.174387
47.787927	1537.586310	19.179405
48.250748	1538.334475	19.184423
47.850628	1541.076694	19.189440
48.088817	1542.421812	19.194458
48.467807	1530.767620	19.199475
48.078365	1538.885897	19.204493
48.186297	1535.990895	19.209511
48.236866	1533.411008	19.214528
48.397684	1549.635914	19.219546
48.383062	1532.870791	19.224563
48.347580	1533.873761	19.229581
48.603624	1530.946086	19.234599
48.308059	1537.149776	19.239616
48.141030	1544.406351	19.244634
48.496108	1553.629338	19.249651
48.672508	1558.793369	19.254669
48.966163	1564.049489	19.259687
49.092293	1559.832445	19.264704
49.013405	1562.745254	19.269722
49.253385	1557.090196	19.274739
48.738396	1549.833432	19.279757
48.967849	1556.033769	19.284775
48.901677	1566.664041	19.289792
48.698066	1564.748852	19.294810
49.075221	1563.395953	19.299827
49.225574	1567.405833	19.304845
48.954793	1566.596283	19.309863
49.021844	1563.130143	19.314880
49.146124	1561.971505	19.319898
49.291096	1554.930090	19.324915
49.040049	1559.350013	19.329933
49.070578	1567.765438	19.334951
48.846993	1578.423536	19.339968
49.271385	1578.619120	19.344986
49.343203	1578.450202	19.350003
49.285574	1575.202419	19.355021
49.246715	1583.600319	19.360039
49.636357	1591.277805	19.365056
49.883777	1610.307466	19.370074
50.140152	1606.934738	19.375091
50.027279	1604.465659	19.380109
50.043492	1604.513746	19.385127
50.194692	1601.056506	19.390144
50.436994	1600.169723	19.395162
50.411308	1598.046763	19.400179
50.128791	1600.177246	19.405197
49.864419	1600.019973	19.410215
50.092371	1595.752252	19.415232
50.393498	1603.604565	19.420250
50.782661	1591.929804	19.425267
50.748581	1602.959032	19.430285
50.777028	1593.082873	19.435303
50.648696	1593.301937	19.440320
50.721574	1592.511129	19.445338
50.471398	1590.480150	19.450355
50.583148	1600.268330	19.455373
50.333402	1586.897933	19.460391
50.345317	1596.613386	19.465408
49.997299	1592.663135	19.470426
50.429010	1590.844073	19.475443
50.349574	1604.474603	19.480461
50.594873	1608.501177	19.485479
50.895804	1606.481686	19.490496
50.916072	1610.609792	19.495514
50.976252	1609.767322	19.500531
50.742219	1615.655270	19.505549
50.901459	1631.833158	19.510567
51.179345	1630.994449	19.515584
51.277490	1633.134726	19.520602
51.918851	1632.895510	19.525619
51.681371	1640.541878	19.530637
51.781086	1636.549872	19.535655
51.718073	1632.946298	19.540672
51.465448	1636.025202	19.545690
51.798216	1628.288428	19.550707
51.815919	1629.421932	19.555725
51.583060	1633.602326	19.560743
51.815405	1631.031817	19.565760
51.645685	1638.317255	19.570778
51.874957	1627.563815	19.575795
52.086009	1636.784163	19.580813
52.070993	1637.487272	19.585831
51.764173	1628.979659	19.590848
51.851206	1634.953016	19.595866
52.219411	1630.767459	19.600883
51.977972	1627.299144	19.605901
51.841996	1625.266049	19.610919
52.237016	1619.634019	19.615936
51.862039	1624.256420	19.620954
51.733261	1626.646855	19.625971
51.833854	1642.925465	19.630989
52.214244	1644.952092	19.636007
52.615575	1643.380794	19.641024
52.254498	1653.350386	19.646042
52.124840	1647.876294	19.651059
52.672262	1653.739655	19.656077
52.724823	1663.644445	19.661095
52.515999	1678.134792	19.666112
52.946706	1672.989486	19.671130
53.059714	1674.275327	19.676147
52.898921	1675.468360	19.681165
53.215230	1679.698431	19.686183
53.180821	1671.495274	19.691200
53.005038	1673.369189	19.696218
52.899924	1672.057126	19.701235
53.194461	1669.145491	19.706253
53.450614	1680.340744	19.711271
53.626625	1662.340051	19.716288
53.651106	1661.253851	19.721306
53.806148	1664.445623	19.726323
53.587892	1665.291033	19.731341
53.449201	1665.050949	19.736359
53.385128	1664.209008	19.741376
53.264469	1667.895279	19.746394
53.530614	1663.170255	19.751411
53.222442	1662.281347	19.756429
53.071586	1660.708194	19.761447
53.843504	1678.671091	19.766464
53.863330	1676.200147	19.771482
54.057032	1689.115727	19.776499
54.093276	1690.378881	19.781517
54.021699	1693.208511	19.786535
53.955315	1687.150107	19.791552
54.119118	1693.780522	19.796570
54.298491	1684.455055	19.801587
54.157476	1695.277019	19.806605
54.272410	1701.482726	19.811623
54.316842	1687.226674	19.816640
54.180178	1688.917727	19.821658
54.127257	1688.654737	19.826675
54.410195	1694.187144	19.831693
54.651152	1708.190456	19.836711
54.680088	1706.961536	19.841728
54.878020	1707.782770	19.846746
54.695621	1701.284921	19.851763
54.905348	1710.593883	19.856781
54.989335	1705.767992	19.861799
55.062845	1706.924317	19.866816
55.016257	1712.385276	19.871834
54.912434	1705.925610	19.876851
55.135943	1704.139157	19.881869
54.675052	1706.493269	19.886887
55.057544	1697.912341	19.891904
54.934585	1705.556573	19.896922
55.020982	1701.683410	19.901939
55.249460	1705.359172	19.906957
55.127665	1712.599260	19.911975
55.303359	1715.125051	19.916992
55.176994	1730.435698	19.922010
55.465114	1731.596273	19.927027
55.583491	1734.339341	19.932045
55.572819	1737.475034	19.937063
55.826943	1717.659982	19.942080
55.869342	1732.278279	19.947098
55.994274	1731.750724	19.952115
56.057225	1722.374045	19.957133
55.947325	1723.360281	19.962151
56.186762	1714.956400	19.967168
55.865525	1723.079854	19.972186
56.222899	1718.116448	19.977203
55.983137	1723.901181	19.982221
55.893204	1724.732801	19.987239
56.134104	1720.245260	19.992256
55.962133	1720.692080	19.997274
55.925951	1732.075187	20.002291
55.856002	1738.704370	20.007309
56.270351	1757.733282	20.012327
56.534006	1741.101101	20.017344
56.368490	1742.323282	20.022362
56.251164	1741.054155	20.027379
56.530031	1752.381602	20.032397
56.434322	1760.488674	20.037415
56.940395	1755.400968	20.042432
57.159903	1763.117808	20.047450
57.013374	1753.953825	20.052467
57.573354	1762.532557	20.057485
57.382006	1761.950406	20.062503
57.492539	1741.245746	20.067520
56.981643	1742.869197	20.072538
56.956710	1748.648684	20.077555
57.332597	1744.304099	20.082573
57.227782	1759.286328	20.087591
57.745889	1756.226036	20.092608
57.768786	1757.024200	20.097626
57.606414	1765.217462	20.102643
57.817775	1756.508674	20.107661
57.585473	1765.975287	20.112679
57.873477	1752.618350	20.117696
57.584211	1757.318879	20.122714
57.890387	1756.377897	20.127731
57.787634	1748.630407	20.132749
57.675556	1751.403272	20.137767
58.097465	1752.113673	20.142784
58.014842	1743.028050	20.147802
58.165255	1741.155210	20.152819
58.372946	1738.506493	20.157837
58.022957	1750.017676	20.162855
58.274406	1751.171374	20.167872
58.104627	1745.946549	20.172890
57.852852	1739.822494	20.177907
57.932139	1753.166324	20.182925
58.322594	1766.313080	20.187943
58.226205	1776.418005	20.192960
58.285186	1783.538275	20.197978
58.452817	1783.587887	20.202995
58.470130	1777.162868	20.208013
58.270207	1791.162733	20.213031
58.771636	1788.957166	20.218048
58.987455	1803.415798	20.223066
58.681674	1807.778081	20.228083
58.845469	1798.391875	20.233101
58.878182	1792.175890	20.238119
58.858578	1802.054192	20.243136
58.988956	1797.694407	20.248154
58.961366	1799.803908	20.253171
59.226665	1798.285470	20.258189
59.070087	1803.867836	20.263207
59.440872	1815.083086	20.268224
59.493591	1815.478926	20.273242
59.471611	1826.471679	20.278259
59.756078	1823.189190	20.283277
59.727084	1814.420196	20.288295
59.719156	1822.974318	20.293312
59.906549	1822.853566	20.298330
59.761211	1821.569886	20.303347
60.159254	1821.898998	20.308365
60.156513	1824.784140	20.313383
60.436354	1814.073162	20.318400
60.286312	1804.871830	20.323418
59.718267	1798.873050	20.328435
59.705956	1792.881882	20.333453
60.316217	1797.154294	20.338471
60.269545	1811.123852	20.343488
60.282753	1811.409109	20.348506
60.148448	1814.791417	20.353523
60.552116	1813.497467	20.358541
60.137809	1823.819496	20.363559
60.649737	1815.167737	20.368576
60.583120	1808.500221	20.373594
59.989898	1827.191577	20.378611
60.332415	1829.072672	20.383629
60.657869	1842.838776	20.388647
60.619887	1855.254255	20.393664
60.751166	1845.245074	20.398682
60.698837	1843.792176	20.403699
60.699353	1840.592043	20.408717
60.785993	1862.544371	20.413735
60.891678	1865.226328	20.418752
61.300532	1869.817509	20.423770
61.061199	1866.604453	20.428787
61.447172	1861.137879	20.433805
61.337762	1870.547420	20.438823
61.388230	1862.614918	20.443840
61.203691	1876.211627	20.448858
61.470823	1865.256441	20.453875
61.740814	1877.671023	20.458893
61.645382	1880.939949	20.463911
61.768352	1886.481700	20.468928
61.876555	1890.330988	20.473946
62.006879	1887.580755	20.478963
62.434787	1889.356953	20.483981
62.109722	1885.011695	20.488999
62.070873	1885.683831	20.494016
62.312285	1891.096565	20.499034
62.251678	1888.663442	20.504051
62.463607	1881.182192	20.509069
62.237154	1885.569937	20.514087
62.419200	1882.461284	20.519104
62.237728	1873.239593	20.524122
62.140370	1881.429034	20.529139
62.737568	1878.479415	20.534157
62.485206	1880.362193	20.539175
62.479709	1882.342002	20.544192
62.782781	1885.914590	20.549210
62.551452	1905.401450	20.554227
62.924546	1904.096504	20.559245
62.979749	1904.659224	20.564263
62.839571	1901.818817	20.569280
63.036494	1895.264623	20.574298
62.715991	1903.179746	20.579315
62.720984	1903.857638	20.584333
63.146657	1895.348751	20.589351
63.138217	1905.140148	20.594368
63.551994	1914.010121	20.599386
63.206773	1913.401577	20.604403
63.434839	1925.832230	20.609421
63.457890	1919.908068	20.614439
63.597316	1916.493641	20.619456
63.822885	1906.971459	20.624474
63.577400	1916.269792	20.629491
64.083016	1911.706013	20.634509
63.635245	1912.802002	20.639527
63.546949	1913.986848	20.644544
63.974329	1908.699977	20.649562
63.747833	1913.810462	20.654579
63.961824	1921.884864	20.659597
64.020899	1929.888862	20.664615
63.990919	1936.350899	20.669632
64.438764	1941.036983	20.674650
64.208187	1938.482149	20.679667
64.391002	1934.694823	20.684685
64.543407	1925.856326	20.689703
64.540984	1940.081001	20.694720
64.990051	1928.210431	20.699738
64.627077	1936.154315	20.704755
64.382576	1923.805393	20.709773
64.274107	1932.400568	20.714791
64.959442	1943.964275	20.719808
65.388616	1953.488308	20.724826
65.271214	1962.195357	20.729843
65.352111	1962.274339	20.734861
65.613991	1939.592160	20.739879
65.353499	1939.333282	20.744896
65.119082	1928.844827	20.749914
65.230863	1928.322483	20.754931
65.111679	1939.311600	20.759949
65.322708	1950.318419	20.764967
65.309628	1959.766568	20.769984
65.401690	1956.763524	20.775002
65.571996	1962.597704	20.780019
65.397358	1959.163042	20.785037
65.760448	1951.572867	20.790055
65.898472	1952.889526	20.795072
66.088755	1964.325668	20.800090
66.138291	1976.866384	20.805107
66.492673	1974.930003	20.810125
66.198210	1963.049662	20.815143
66.273238	1957.114188	20.820160
66.704641	1962.399341	20.825178
66.195915	1957.710429	20.830195
66.672256	1954.391542	20.835213
66.582655	1970.375179	20.840231
66.708428	1969.673904	20.845248
66.746587	1963.049880	20.850266
66.766308	1960.364304	20.855283
66.632263	1953.164463	20.860301
66.286267	1953.666957	20.865319
66.168690	1965.504807	20.870336
66.671117	1974.818545	20.875354
66.434261	1972.198414	20.880371
66.801077	1977.048692	20.885389
66.873117	1988.853693	20.890407
66.750670	1999.736052	20.895424
66.958414	1995.929027	20.900442
67.174330	2000.802953	20.905459
67.239116	1998.242865	20.910477
67.793061	2005.475037	20.915495
67.524940	2012.555121	20.920512
67.605251	1998.836038	20.925530
67.464493	2009.554003	20.930547
67.749947	2011.163171	20.935565
68.015007	2012.283193	20.940583
67.846885	2012.710481	20.945600
67.992249	2010.472305	20.950618
68.026799	2015.983764	20.955635
68.037933	2005.235871	20.960653
68.278837	2013.391311	20.965671
68.306202	2011.029601	20.970688
68.273236	2011.056990	20.975706
68.056894	2008.682966	20.980723
67.979312	2001.483728	20.985741
68.140346	2004.693559	20.990759
68.187027	2009.041696	20.995776
68.657127	2004.527643	21.000794
68.783742	2010.274003	21.005811
68.649219	2012.583332	21.010829
68.431028	2021.820634	21.015847
68.452680	2036.874806	21.020864
68.913308	2030.771589	21.025882
68.669601	2029.443341	21.030899
68.568283	2027.796117	21.035917
68.706490	2031.744885	21.040935
68.835509	2046.371959	21.045952
69.298620	2041.934737	21.050970
69.169796	2057.441722	21.055987
69.276546	2063.137559	21.061005
69.458365	2061.565901	21.066023
69.486414	2067.889497	21.071040
69.759023	2050.065799	21.076058
69.700914	2060.811874	21.081075
69.637318	2064.565032	21.086093
69.881047	2059.802388	21.091111
69.644500	2059.123159	21.096128
69.859083	2061.961666	21.101146
69.835005	2080.144362	21.106163
69.850690	2079.327777	21.111181
70.055182	2079.466297	21.116199
70.250715	2091.958971	21.121216
70.101278	2072.336153	21.126234
69.955348	2082.486885	21.131251
69.839995	2084.739567	21.136269
70.344634	2089.861795	21.141287
70.582483	2096.218807	21.146304
70.636310	2093.120738	21.151322
70.502161	2103.234919	21.156339
70.981154	2097.627458	21.161357
70.813247	2090.347654	21.166375
70.629313	2097.796463	21.171392
70.612632	2094.125572	21.176410
71.146711	2106.035000	21.181427
71.838982	2111.904224	21.186445
71.484698	2098.805462	21.191463
71.284285	2104.347448	21.196480
71.531239	2099.770495	21.201498
71.466795	2108.854356	21.206515
71.251213	2108.588439	21.211533
71.721782	2108.069843	21.216551
71.562875	2111.020526	21.221568
71.322675	2111.440172	21.226586
71.912673	2111.183753	21.231603
71.538475	2115.026612	21.236621
71.870624	2107.741045	21.241639
71.977677	2112.193367	21.246656
71.742026	2108.219083	21.251674
71.793679	2118.667107	21.256691
72.189232	2132.154188	21.261709
72.371399	2132.031098	21.266727
72.484388	2137.441935	21.271744
72.730861	2129.336585	21.276762
72.498734	2133.927266	21.281779
72.618301	2135.808608	21.286797
72.823690	2138.863179	21.291815
72.829269	2138.581548	21.296832
72.848910	2127.500863	21.301850
72.875843	2123.867318	21.306867
72.749026	2123.379194	21.311885
72.581030	2124.185190	21.316903
72.834004	2133.878947	21.321920
72.716489	2122.485213	21.326938
73.201532	2137.940276	21.331955
73.230155	2137.342586	21.336973
73.474488	2150.203226	21.341991
73.313007	2157.014175	21.347008
73.457082	2148.378861	21.352026
73.383010	2145.919408	21.357043
73.338067	2147.226875	21.362061
73.701053	2145.219695	21.367079
73.644722	2143.423390	21.372096
73.489636	2150.277519	21.377114
73.629390	2137.666260	21.382131
73.715431	2161.042427	21.387149
73.900426	2168.954214	21.392167
73.988377	2172.683650	21.397184
73.924892	2170.651759	21.402202
74.055986	2169.157473	21.407219
74.036489	2173.257222	21.412237
74.699277	2181.220400	21.417255
74.717529	2198.370864	21.422272
74.744941	2187.576126	21.427290
74.647917	2188.456219	21.432307
74.917062	2186.558419	21.437325
75.022890	2185.547812	21.442343
74.779280	2191.282800	21.447360
74.955119	2184.785458	21.452378
74.769029	2187.983430	21.457395
74.962989	2184.383669	21.462413
75.059794	2177.677787	21.467431
74.929595	2185.875668	21.472448
74.965350	2184.487844	21.477466
75.407312	2200.776599	21.482483
75.211602	2209.953666	21.487501
75.549950	2212.955859	21.492519
75.718927	2217.401661	21.497536
75.496834	2206.835366	21.502554
75.634393	2219.362461	21.507571
75.403087	2212.679569	21.512589
76.011110	2211.688117	21.517607
75.683149	2217.366896	21.522624
76.224996	2226.813457	21.527642
76.070043	2220.352148	21.532659
76.180932	2234.032240	21.537677
76.055774	2221.879027	21.542695
76.058558	2229.967723	21.547712
76.054121	2225.764667	21.552730
76.160072	2229.216718	21.557747
76.471310	2248.369615	21.562765
76.371932	2244.970448	21.567783
76.488373	2249.686443	21.572800
76.683936	2254.648841	21.577818
76.913249	2250.715297	21.582835
76.893504	2251.034129	21.587853
77.478528	2251.775807	21.592871
77.092478	2241.872705	21.597888
76.790378	2250.151201	21.602906
77.223714	2258.033587	21.607923
77.231049	2268.785313	21.612941
77.317955	2264.984540	21.617959
77.334895	2274.065201	21.622976
77.425768	2269.386416	21.627994
77.541911	2271.063164	21.633011
77.660508	2266.335851	21.638029
78.103609	2261.535606	21.643047
77.728063	2270.832405	21.648064
77.851476	2285.561547	21.653082
78.039365	2286.409632	21.658099
78.373310	2299.511982	21.663117
78.745336	2294.628181	21.668135
78.307049	2289.735624	21.673152
78.845924	2288.243718	21.678170
78.573785	2274.882626	21.683187
78.654780	2268.573697	21.688205
78.485762	2260.934205	21.693223
78.320417	2277.176155	21.698240
78.614277	2290.025980	21.703258
78.769281	2284.352447	21.708275
78.521402	2288.349136	21.713293
78.870035	2290.254571	21.718311
78.788434	2281.888101	21.723328
78.777423	2283.559522	21.728346
79.125683	2297.549642	21.733363
78.748971	2307.676692	21.738381
79.550628	2307.649065	21.743399
79.064356	2314.877064	21.748416
79.302424	2312.690605	21.753434
79.367552	2302.824089	21.758451
79.271477	2316.132691	21.763469
79.793418	2322.420027	21.768487
79.972004	2322.414271	21.773504
79.851213	2329.755445	21.778522
80.026352	2327.660901	21.783539
79.824931	2323.652801	21.788557
80.050232	2332.883901	21.793575
79.988626	2324.949817	21.798592
79.987395	2335.510405	21.803610
80.440174	2341.950607	21.808627
80.524168	2355.098470	21.813645
80.907402	2356.897497	21.818663
80.669712	2357.408281	21.823680
80.682854	2358.043884	21.828698
80.646929	2355.215475	21.833715
80.382124	2357.551572	21.838733
80.906390	2347.003973	21.843751
80.782440	2361.945517	21.848768
80.944080	2367.172061	21.853786
81.566490	2368.457047	21.858803
81.268315	2375.074880	21.863821
81.636539	2369.039681	21.868839
81.131205	2382.510290	21.873856
81.461164	2382.632312	21.878874
81.543055	2374.748314	21.883891
81.799934	2378.792186	21.888909
81.685257	2367.915450	21.893927
81.535877	2365.268931	21.898944
81.613541	2376.319001	21.903962
82.504374	2380.415043	21.908979
82.015836	2386.813373	21.913997
82.314988	2392.725345	21.919015
82.509719	2387.171800	21.924032
82.339987	2386.942880	21.929050
82.840479	2389.515719	21.934067
82.444013	2383.739189	21.939085
82.649112	2387.822736	21.944103
82.603481	2390.929303	21.949120
82.668866	2393.169487	21.954138
82.917529	2384.132631	21.959155
82.838632	2396.447587	21.964173
83.171099	2397.121533	21.969191
82.830386	2389.991768	21.974208
83.008588	2403.165936	21.979226
82.967486	2401.493463	21.984243
83.238426	2412.712108	21.989261
83.059626	2410.512046	21.994279
83.288482	2411.571489	21.999296
82.952138	2419.874364	22.004314
83.453679	2416.289490	22.009331
83.142218	2427.230126	22.014349
83.310272	2427.118713	22.019367
83.891537	2428.785727	22.024384
83.886834	2436.449615	22.029402
83.903656	2433.148982	22.034419
83.764051	2442.178509	22.039437
84.098550	2449.486273	22.044455
84.316037	2449.758473	22.049472
84.346384	2449.779099	22.054490
84.585213	2455.495397	22.059507
84.495158	2467.452353	22.064525
84.541479	2455.417297	22.069543
84.835148	2453.910141	22.074560
84.953248	2453.393105	22.079578
84.668949	2444.013644	22.084595
84.685320	2442.256416	22.089613
84.949236	2449.988689	22.094631
85.101405	2467.746494	22.099648
85.115403	2473.302344	22.104666
85.478447	2473.147757	22.109683
85.299974	2476.278308	22.114701
85.579534	2478.178805	22.119719
85.784949	2473.721886	22.124736
85.560076	2466.340389	22.129754
85.527795	2459.430544	22.134771
85.484897	2461.561457	22.139789
85.871780	2480.895275	22.144807
86.234548	2495.198887	22.149824
86.111547	2496.685883	22.154842
86.550802	2489.348665	22.159859
86.386507	2497.062831	22.164877
85.968701	2488.389141	22.169895
86.437678	2486.207513	22.174912
86.415211	2488.972764	22.179930
86.566995	2489.536153	22.184947
86.222215	2492.882128	22.189965
86.310846	2498.044402	22.194983
86.635562	2508.026953	22.200000
86.583681	2517.216360	22.205018
87.167409	2504.992923	22.210035
87.227296	2510.106049	22.215053
87.332225	2512.191716	22.220071
87.398195	2505.351675	22.225088
87.090780	2510.538128	22.230106
87.239140	2516.669446	22.235123
87.465525	2532.092784	22.240141
87.353251	2542.068071	22.245159
88.063130	2532.946257	22.250176
87.500963	2537.699212	22.255194
87.586437	2534.845442	22.260211
87.532169	2538.755043	22.265229
88.088250	2548.890736	22.270247
88.035262	2553.876378	22.275264
88.071315	2547.407118	22.280282
88.222145	2544.748256	22.285299
88.430810	2556.683720	22.290317
88.200981	2555.571029	22.295335
88.362869	2548.122593	22.300352
88.622202	2566.100415	22.305370
88.712352	2571.862137	22.310387
88.786829	2572.608071	22.315405
89.008394	2569.868688	22.320423
89.070508	2562.186543	22.325440
88.653599	2566.680038	22.330458
88.971487	2564.875559	22.335475
89.030257	2572.649494	22.340493
89.309904	2572.034554	22.345511
89.733018	2583.090595	22.350528
89.402312	2599.346118	22.355546
89.817538	2583.184925	22.360563
89.989136	2594.608616	22.365581
89.767142	2601.135693	22.370599
90.167012	2594.940811	22.375616
89.735780	2600.269777	22.380634
90.328980	2590.298277	22.385651
90.237754	2579.566077	22.390669
90.012565	2585.853783	22.395687
90.517100	2580.381042	22.400704
90.062580	2585.227609	22.405722
90.164714	2585.631504	22.410739
90.645741	2604.502535	22.415757
90.725772	2613.393584	22.420775
91.067105	2597.859401	22.425792
90.612364	2604.426100	22.430810
90.396854	2601.622631	22.435827
90.613519	2604.836480	22.440845
91.148119	2614.530561	22.445863
91.347760	2623.131448	22.450880
90.942756	2634.822245	22.455898
91.074642	2627.488941	22.460915
91.006932	2626.407657	22.465933
91.267499	2626.524772	22.470951
91.900677	2643.345766	22.475968
91.443480	2646.693601	22.480986
91.921829	2653.600176	22.486003
92.074823	2648.116212	22.491021
91.855137	2656.227330	22.496039
92.115140	2653.623939	22.501056
91.779645	2657.416662	22.506074
92.222210	2660.598284	22.511091
92.355216	2667.069767	22.516109
92.194352	2671.333804	22.521127
92.519224	2670.759118	22.526144
92.482294	2677.421347	22.531162
92.937407	2670.911638	22.536179
92.981014	2671.368891	22.541197
93.090882	2682.619253	22.546215
93.128016	2688.534501	22.551232
93.279819	2706.825990	22.556250
93.403371	2696.697613	22.561267
93.488162	2691.792428	22.566285
93.351438	2694.834416	22.571303
93.855473	2694.228503	22.576320
93.680370	2685.469349	22.581338
93.585042	2691.493723	22.586355
94.119262	2688.702183	22.591373
93.812055	2690.672539	22.596391
93.627636	2686.642757	22.601408
94.019685	2700.168689	22.606426
94.088244	2715.964090	22.611443
94.416067	2706.283439	22.616461
94.522659	2715.104098	22.621479
94.540380	2714.284010	22.626496
94.674732	2716.141004	22.631514
94.460205	2711.576231	22.636531
94.605194	2711.837700	22.641549
94.415806	2719.884133	22.646567
94.727973	2727.826742	22.651584
94.522650	2741.645134	22.656602
94.945795	2739.186604	22.661619
95.043320	2733.414626	22.666637
95.045853	2750.564923	22.671655
95.485478	2748.731886	22.676672
95.448523	2765.711639	22.681690
95.390029	2760.740512	22.686707
95.325369	2754.413203	22.691725
95.493538	2760.724559	22.696743
95.811663	2749.268486	22.701760
95.697110	2758.445741	22.706778
95.842913	2775.478932	22.711795
96.033993	2774.044634	22.716813
95.882848	2788.384810	22.721831
96.042778	2778.660989	22.726848
95.906007	2787.352534	22.731866
96.439968	2795.787504	22.736883
97.056961	2795.599443	22.741901
96.530043	2801.249607	22.746919
96.733863	2808.347592	22.751936
96.597860	2801.599048	22.756954
97.111826	2804.466519	22.761971
97.309468	2797.182811	22.766989
96.994726	2801.379458	22.772007
97.051887	2808.954908	22.777024
97.383422	2820.524119	22.782042
97.839293	2822.576933	22.787059
98.181117	2828.330869	22.792077
97.988101	2824.160375	22.797095
98.003524	2821.519530	22.802112
98.281296	2825.320361	22.807130
97.930497	2829.753064	22.812147
98.018288	2827.407030	22.817165
97.864925	2832.061295	22.822183
98.262075	2819.573353	22.827200
97.726740	2821.516341	22.832218
98.487718	2825.140471	22.837235
98.603465	2835.976549	22.842253
98.263656	2847.092314	22.847271
98.435575	2836.710099	22.852288
98.449297	2844.743703	22.857306
98.883705	2855.286843	22.862323
99.259504	2864.971222	22.867341
99.411557	2863.091698	22.872359
99.266164	2871.055557	22.877376
98.902751	2871.191529	22.882394
99.061407	2862.736647	22.887411
99.136534	2871.388723	22.892429
99.152733	2891.368108	22.897447
99.516842	2884.859955	22.902464
99.599214	2880.946140	22.907482
100.050789	2887.108985	22.912499
100.038477	2897.368644	22.917517
100.071433	2896.669252	22.922535
100.217028	2906.209817	22.927552
100.467403	2906.842990	22.932570
100.425892	2907.263086	22.937587
100.892157	2900.091905	22.942605
100.594689	2901.599954	22.947623
100.597911	2896.836897	22.952640
100.848919	2905.616087	22.957658
100.790919	2913.986046	22.962675
101.703580	2919.098246	22.967693
101.492800	2921.353357	22.972711
101.708781	2915.051460	22.977728
101.447823	2922.471646	22.982746
101.321844	2923.905488	22.987763
101.809699	2921.903912	22.992781
101.513394	2917.875825	22.997799
101.691041	2920.429887	23.002816
101.574684	2920.587121	23.007834
101.326031	2922.863947	23.012851
101.656402	2924.797563	23.017869
101.931188	2942.924840	23.022887
102.213848	2945.519265	23.027904
102.039923	2948.721776	23.032922
102.383854	2941.721242	23.037939
102.380843	2939.581947	23.042957
102.360205	2951.307415	23.047975
102.799874	2962.897651	23.052992
103.196114	2962.731550	23.058010
103.285311	2962.714551	23.063027
102.982987	2962.588456	23.068045
102.912991	2962.650054	23.073063
103.154803	2964.155681	23.078080
103.437862	2957.612857	23.083098
103.710562	2953.606084	23.088115
104.032319	2967.427289	23.093133
103.604441	2960.639196	23.098151
103.869727	2956.699864	23.103168
103.880093	2962.890828	23.108186
103.551966	2982.924260	23.113203
103.884422	2986.899618	23.118221
103.991913	2992.223202	23.123239
103.959779	2982.229523	23.128256
104.299336	2981.845056	23.133274
104.205853	3009.839568	23.138291
104.235992	3013.278398	23.143309
104.009519	3018.035695	23.148327
104.491357	3022.306434	23.153344
104.745545	3033.720622	23.158362
105.055362	3039.552233	23.163379
104.845522	3032.007181	23.168397
105.102735	3036.944358	23.173415
104.919215	3030.237891	23.178432
105.642858	3045.268145	23.183450
105.632117	3048.536638	23.188467
105.979172	3053.270371	23.193485
106.046107	3052.212153	23.198503
105.817076	3046.895232	23.203520
106.331963	3046.685292	23.208538
105.913017	3057.532681	23.213555
106.516473	3041.480462	23.218573
106.566901	3048.195423	23.223591
106.626566	3047.561277	23.228608
106.558460	3043.409036	23.233626
106.244139	3052.721893	23.238643
106.392617	3055.223733	23.243661
106.424736	3071.817364	23.248679
106.353837	3069.616096	23.253696
106.956547	3089.926746	23.258714
107.136496	3100.080651	23.263731
107.354383	3091.903599	23.268749
107.144461	3104.839248	23.273767
106.983619	3096.841465	23.278784
107.591944	3093.306011	23.283802
107.712300	3118.038378	23.288819
108.015655	3112.631716	23.293837
107.848354	3118.405541	23.298855
107.557575	3121.276049	23.303872
107.765969	3116.682788	23.308890
107.418018	3128.434402	23.313907
108.102253	3130.312601	23.318925
108.307962	3133.231576	23.323943
108.298501	3136.291574	23.328960
108.993905	3134.664612	23.333978
109.159629	3140.329458	23.338995
108.952772	3135.365690	23.344013
109.101670	3133.180479	23.349031
108.950825	3132.566685	23.354048
109.376828	3141.997163	23.359066
109.415673	3154.123754	23.364083
109.664921	3161.738696	23.369101
109.739071	3170.214319	23.374119
109.986081	3158.775442	23.379136
109.946845	3146.298832	23.384154
109.533567	3142.800329	23.389171
109.733460	3150.293593	23.394189
109.918989	3150.147878	23.399207
109.986933	3152.425631	23.404224
109.813178	3146.714960	23.409242
109.863127	3165.941335	23.414259
109.806751	3173.626258	23.419277
110.249538	3175.163541	23.424295
110.053553	3171.558397	23.429312
110.521486	3190.832938	23.434330
110.751614	3199.041108	23.439347
110.784088	3203.372824	23.444365
110.980646	3199.355832	23.449383
111.030839	3216.811574	23.454400
111.265024	3216.052237	23.459418
111.394943	3222.947339	23.464435
111.563376	3217.634378	23.469453
111.780084	3220.810456	23.474471
111.738801	3220.128995	23.479488
111.939645	3227.650549	23.484506
111.949767	3243.528160	23.489523
112.319258	3245.342058	23.494541
112.488465	3239.126283	23.499559
111.893643	3244.013941	23.504576
112.016246	3244.364146	23.509594
112.292850	3252.041122	23.514611
112.497357	3255.660992	23.519629
112.835596	3263.075816	23.524647
112.906771	3261.672891	23.529664
113.417875	3256.230483	23.534682
112.845229	3262.755921	23.539699
113.004216	3260.720614	23.544717
113.444531	3277.272576	23.549735
113.339684	3292.903118	23.554752
113.443647	3292.883806	23.559770
113.494357	3292.834961	23.564787
113.822590	3283.898815	23.569805
113.492911	3299.943338	23.574823
113.858583	3308.117697	23.579840
114.158469	3298.116014	23.584858
114.121134	3310.715458	23.589875
114.202063	3312.053789	23.594893
114.440195	3320.948825	23.599911
114.941425	3332.267686	23.604928
115.171902	3331.231174	23.609946
114.981279	3337.428506	23.614963
114.613534	3334.617209	23.619981
114.874092	3330.965757	23.624999
114.539326	3339.211991	23.630016
115.073241	3357.469526	23.635034
115.272754	3358.246405	23.640051
115.669801	3352.241084	23.645069
115.585302	3355.839971	23.650087
115.760546	3352.315506	23.655104
116.019913	3357.252433	23.660122
116.038672	3370.190320	23.665139
116.510880	3384.796280	23.670157
116.660466	3375.897546	23.675175
116.695100	3374.415118	23.680192
116.849731	3362.914834	23.685210
116.806164	3363.161668	23.690227
117.372484	3372.245189	23.695245
117.055599	3338.516614	23.700263
116.699815	3342.795565	23.705280
117.024563	3345.759051	23.710298
117.145187	3354.779826	23.715315
117.451059	3357.847272	23.720333
117.786909	3361.714869	23.725351
117.414429	3366.009066	23.730368
117.689841	3364.103852	23.735386
117.614318	3357.238312	23.740403
117.477430	3361.640787	23.745421
117.586106	3362.469772	23.750439
117.473734	3386.942279	23.755456
117.772724	3382.593572	23.760474
117.617784	3390.369779	23.765491
118.190839	3399.894137	23.770509
118.357709	3404.350034	23.775527
117.831063	3417.682717	23.780544
118.196849	3426.930246	23.785562
118.576256	3429.045613	23.790579
118.856785	3441.298659	23.795597
119.278585	3440.140635	23.800615
118.934291	3447.529903	23.805632
119.200341	3457.294923	23.810650
119.127820	3459.184405	23.815667
119.190106	3462.514126	23.820685
119.526342	3466.684689	23.825703
119.453109	3493.316420	23.830720
119.937230	3480.047421	23.835738
120.149709	3482.286791	23.840755
120.158379	3486.309831	23.845773
120.209400	3492.702923	23.850791
120.481833	3502.539562	23.855808
120.765592	3494.219444	23.860826
121.109877	3510.751948	23.865843
120.790384	3507.683717	23.870861
121.296082	3501.115287	23.875879
120.927704	3508.959702	23.880896
120.891257	3502.880214	23.885914
121.435290	3518.052631	23.890931
121.553162	3528.519507	23.895949
121.645080	3527.353190	23.900967
121.600646	3530.829052	23.905984
121.716587	3529.327561	23.911002
121.975229	3522.037162	23.916019
121.853498	3526.500428	23.921037
122.577837	3531.926379	23.926055
121.985278	3552.977164	23.931072
122.504670	3552.188913	23.936090
122.422257	3545.617915	23.941107
122.402935	3550.857374	23.946125
122.593478	3557.181286	23.951143
122.476395	3558.979915	23.956160
122.637902	3564.115296	23.961178
122.737047	3566.255649	23.966195
122.978266	3578.625418	23.971213
123.204488	3583.122562	23.976231
123.035049	3600.205920	23.981248
123.315067	3591.030985	23.986266
123.355555	3597.952868	23.991283
123.573738	3617.674158	23.996301
123.552053	3619.508348	24.001319
123.856119	3618.719109	24.006336
124.136821	3617.163391	24.011354
124.089110	3637.033674	24.016371
124.163852	3635.778508	24.021389
124.248645	3628.969812	24.026407
124.363148	3643.395300	24.031424
124.948411	3651.008308	24.036442
125.311130	3661.067613	24.041459
125.202180	3667.990840	24.046477
125.241900	3659.762537	24.051495
125.457666	3661.000862	24.056512
125.826909	3651.597288	24.061530
125.498435	3661.127303	24.066547
125.527072	3660.087676	24.071565
125.854657	3644.144429	24.076583
125.471050	3653.547356	24.081600
125.864751	3667.537739	24.086618
126.126221	3665.514738	24.091635
126.252788	3673.786694	24.096653
126.369758	3669.804162	24.101671
126.528094	3671.660654	24.106688
126.507566	3669.470359	24.111706
126.895906	3686.699982	24.116723
126.986561	3696.195915	24.121741
127.311380	3687.499987	24.126759
127.274229	3700.797221	24.131776
127.362931	3692.804267	24.136794
127.307021	3688.208081	24.141811
127.525379	3703.308581	24.146829
127.934088	3708.900819	24.151847
127.699396	3722.554119	24.156864
127.850270	3725.645911	24.161882
128.170201	3721.808325	24.166899
128.110472	3725.277151	24.171917
128.192417	3723.310677	24.176935
128.167103	3744.383287	24.181952
128.631673	3735.602314	24.186970
128.873204	3749.502973	24.191987
128.927950	3752.941245	24.197005
129.040809	3747.984032	24.202023
129.052663	3760.187854	24.207040
129.496684	3769.401209	24.212058
129.448229	3766.154748	24.217075
129.368359	3757.916730	24.222093
129.726101	3766.607023	24.227111
129.431524	3763.099270	24.232128
129.481714	3775.439131	24.237146
129.986792	3778.926797	24.242163
130.145341	3789.564207	24.247181
130.470945	3776.313514	24.252199
130.355677	3773.402622	24.257216
129.923478	3781.342374	24.262234
130.449107	3790.798618	24.267251
130.430746	3800.532630	24.272269
130.796026	3812.551707	24.277287
131.366337	3821.865245	24.282304
131.221037	3826.600567	24.287322
131.622325	3826.938686	24.292339
131.440941	3835.378903	24.297357
131.683066	3824.350698	24.302375
131.366750	3823.664956	24.307392
131.421831	3834.994061	24.312410
131.942649	3854.295749	24.317427
132.084265	3857.938219	24.322445
132.007624	3850.940099	24.327463
132.247718	3860.450583	24.332480
132.249269	3870.367737	24.337498
132.497413	3876.827930	24.342515
132.501752	3879.885891	24.347533
132.776150	3883.261369	24.352551
132.801750	3895.358969	24.357568
133.247852	3896.791639	24.362586
133.434817	3893.606120	24.367603
133.644419	3906.978477	24.372621
133.789625	3894.671304	24.377639
133.159847	3893.387615	24.382656
133.480055	3899.284163	24.387674
134.209452	3902.168566	24.392691
134.072673	3920.238206	24.397709
133.670812	3917.548946	24.402727
134.060238	3918.087777	24.407744
134.153149	3913.878546	24.412762
134.425414	3925.375690	24.417779
134.292375	3935.323434	24.422797
134.710946	3933.414672	24.427815
134.891355	3943.130245	24.432832
134.727497	3958.445500	24.437850
135.364065	3954.226841	24.442867
135.330326	3972.037349	24.447885
135.478954	3964.227426	24.452903
135.628705	3966.366211	24.457920
136.068494	3976.587219	24.462938
136.199004	3982.762867	24.467955
135.860591	3985.606251	24.472973
135.813385	3979.001173	24.477991
136.365417	3992.168441	24.483008
136.548230	4004.781224	24.488026
136.786407	4006.795688	24.493043
136.646457	4005.529942	24.498061
136.712121	4009.174874	24.503079
136.489866	4016.548409	24.508096
136.479764	4014.470068	24.513114
137.413963	4028.192984	24.518131
137.229242	4021.685187	24.523149
137.546098	4040.289904	24.528167
137.641107	4055.422648	24.533184
137.623447	4060.115939	24.538202
137.977991	4047.848463	24.543219
137.952197	4059.610178	24.548237
138.184642	4079.083540	24.553255
138.224235	4072.824658	24.558272
138.274386	4076.045921	24.563290
138.880157	4072.466494	24.568307
138.443962	4081.300260	24.573325
138.825905	4089.762815	24.578343
139.075841	4092.015332	24.583360
138.962963	4100.788987	24.588378
139.293520	4104.619698	24.593395
139.497376	4120.082648	24.598413
139.676044	4114.247016	24.603431
139.965665	4122.714580	24.608448
140.010090	4114.494803	24.613466
140.481297	4126.087163	24.618483
140.347877	4142.351038	24.623501
140.389774	4135.763507	24.628519
140.990645	4136.221874	24.633536
140.729306	4137.879026	24.638554
140.776548	4140.501039	24.643571
141.086598	4143.845730	24.648589
140.970610	4130.379884	24.653607
140.992199	4152.856533	24.658624
141.241953	4159.329200	24.663642
141.514333	4150.076270	24.668659
141.680733	4167.495786	24.673677
141.378198	4163.392639	24.678695
141.703763	4185.348245	24.683712
141.987596	4184.214948	24.688730
142.292987	4181.689454	24.693747
142.035466	4193.894736	24.698765
142.332684	4199.583505	24.703783
142.824319	4200.286249	24.708800
142.255455	4202.496611	24.713818
142.840956	4205.034307	24.718835
142.877157	4210.697687	24.723853
142.504313	4210.702571	24.728871
143.087557	4222.249033	24.733888
143.293003	4232.828854	24.738906
143.744739	4224.538903	24.743923
143.738766	4241.161670	24.748941
143.896396	4250.663184	24.753959
143.595680	4252.544308	24.758976
144.237290	4271.464530	24.763994
144.158950	4254.375432	24.769011
144.303267	4261.833676	24.774029
144.813093	4270.882315	24.779047
144.759467	4275.186743	24.784064
144.829334	4284.553672	24.789082
144.918741	4276.664512	24.794099
144.751517	4279.440089	24.799117
144.968760	4285.258202	24.804135
145.414809	4291.132008	24.809152
145.199733	4295.894165	24.814170
145.908786	4303.181885	24.819187
145.721071	4316.124387	24.824205
145.751504	4321.129010	24.829223
145.980827	4321.617183	24.834240
145.959157	4338.823282	24.839258
145.759349	4344.286945	24.844275
146.361965	4359.687628	24.849293
146.409883	4368.663484	24.854311
146.847060	4369.822982	24.859328
146.774908	4382.292899	24.864346
147.047612	4379.254842	24.869363
147.316954	4399.417185	24.874381
147.444871	4398.813334	24.879399
147.558026	4390.289115	24.884416
147.400964	4407.396545	24.889434
148.112384	4412.749037	24.894451
147.919456	4422.633831	24.899469
147.966285	4415.815006	24.904487
148.137289	4422.754634	24.909504
148.122915	4438.848614	24.914522
148.619375	4445.762515	24.919539
148.758618	4448.183929	24.924557
148.890010	4464.595993	24.929575
149.626031	4469.114498	24.934592
149.245202	4463.666271	24.939610
149.567244	4456.747498	24.944627
149.518474	4464.176103	24.949645
149.603701	4468.073735	24.954663
149.502156	4475.352790	24.959680
149.926898	4488.770784	24.964698
150.024305	4491.205071	24.969715
150.310403	4498.189826	24.974733
150.509874	4515.386699	24.979751
151.188145	4518.588548	24.984768
150.977852	4513.344012	24.989786
151.214505	4518.657281	24.994803
151.346388	4515.047847	24.999821
151.027172	4511.111371	25.004839
151.568138	4521.035911	25.009856
151.496304	4539.500021	25.014874
151.789930	4528.652709	25.019891
151.914792	4541.868362	25.024909
151.831627	4540.413763	25.029927
152.190444	4541.904353	25.034944
152.254212	4551.064048	25.039962
152.449257	4557.217156	25.044979
152.552069	4559.969409	25.049997
152.213342	4565.095063	25.055015
152.580920	4568.964266	25.060032
152.778346	4586.404575	25.065050
153.222112	4581.259566	25.070067
152.766431	4585.993206	25.075085
153.423039	4608.143667	25.080103
153.445105	4606.132818	25.085120
153.507109	4606.198992	25.090138
153.564501	4610.994300	25.095155
153.792581	4628.322527	25.100173
154.084887	4635.315833	25.105191
154.363635	4635.830993	25.110208
153.979684	4647.305142	25.115226
154.348662	4652.020082	25.120243
154.446159	4657.058483	25.125261
154.297133	4673.704056	25.130279
154.929727	4673.712404	25.135296
154.889234	4685.767225	25.140314
155.185342	4687.084574	25.145331
156.024681	4698.774298	25.150349
155.943159	4706.227072	25.155367
156.106562	4703.348128	25.160384
155.985167	4711.804604	25.165402
156.329718	4709.531737	25.170419
156.542581	4719.858161	25.175437
156.667751	4732.676185	25.180455
156.934466	4714.898138	25.185472
157.179884	4727.943528	25.190490
157.114233	4718.203505	25.195507
157.223778	4728.893335	25.200525
157.608754	4744.205339	25.205543
157.754324	4738.908143	25.210560
157.611373	4747.036579	25.215578
157.763274	4743.840624	25.220595
157.683551	4745.339960	25.225613
157.951772	4765.420817	25.230631
158.530577	4774.386303	25.235648
158.347050	4775.078054	25.240666
158.496327	4783.552134	25.245683
158.953718	4790.342872	25.250701
158.529953	4804.395916	25.255719
159.211058	4785.511230	25.260736
159.355839	4799.554114	25.265754
159.452166	4812.288330	25.270771
160.051832	4811.850456	25.275789
159.677269	4820.147784	25.280807
159.804319	4817.015683	25.285824
159.919914	4826.735571	25.290842
159.911223	4831.888508	25.295859
160.384176	4845.649589	25.300877
160.224269	4848.528271	25.305895
160.655632	4856.670948	25.310912
160.598013	4870.878169	25.315930
160.410027	4869.357895	25.320947
160.885146	4877.720997	25.325965
160.917957	4894.663408	25.330983
161.048280	4895.899423	25.336000
161.606377	4916.983004	25.341018
161.769686	4923.074921	25.346035
161.975658	4919.163400	25.351053
162.188150	4932.596036	25.356071
162.616676	4936.364230	25.361088
162.753815	4944.726651	25.366106
162.547357	4946.122753	25.371123
162.519559	4946.051482	25.376141
162.495131	4951.866636	25.381159
162.792530	4960.039817	25.386176
163.236212	4974.582091	25.391194
163.263685	4970.319737	25.396211
163.711377	4971.922702	25.401229
163.484724	4988.028328	25.406247
163.736302	4988.131091	25.411264
163.781921	4991.441610	25.416282
164.014634	4990.758192	25.421299
164.437295	5014.609303	25.426317
164.566718	5014.866936	25.431335
164.617509	5011.901419	25.436352
164.716693	5027.700353	25.441370
164.928202	5036.900279	25.446387
165.135023	5032.796050	25.451405
165.053898	5039.232486	25.456423
165.309712	5038.570699	25.461440
165.422986	5045.450166	25.466458
165.382520	5064.935776	25.471475
166.066292	5066.015654	25.476493
166.295473	5083.527224	25.481511
166.356862	5083.760794	25.486528
166.472470	5075.273749	25.491546
166.266874	5076.436140	25.496563
166.827941	5092.039664	25.501581
166.630147	5109.908554	25.506599
167.271444	5111.850520	25.511616
167.189388	5112.444316	25.516634
167.439053	5124.513945	25.521651
167.455037	5123.327858	25.526669
167.375655	5130.556353	25.531687
167.805077	5147.320071	25.536704
168.274508	5148.051588	25.541722
168.351457	5150.975282	25.546739
168.455781	5161.208481	25.551757
168.796586	5184.447636	25.556775
169.034827	5178.709656	25.561792
168.949023	5181.876656	25.566810
168.867259	5186.592906	25.571827
169.776849	5189.935409	25.576845
169.829213	5199.447598	25.581863
169.995805	5197.060505	25.586880
169.992822	5192.083169	25.591898
170.140643	5210.333621	25.596915
170.580385	5219.737785	25.601933
170.580604	5220.337635	25.606951
170.694726	5212.687255	25.611968
170.828837	5212.780014	25.616986
171.133738	5223.095462	25.622003
171.517625	5230.582862	25.627021
171.243158	5237.444232	25.632039
171.268302	5236.556578	25.637056
171.527147	5240.761776	25.642074
171.571946	5255.988615	25.647091
172.028612	5251.239130	25.652109
171.748251	5255.333095	25.657127
172.268470	5266.426081	25.662144
172.737659	5282.214620	25.667162
172.838011	5287.555782	25.672180
172.918247	5282.840008	25.677197
172.898831	5285.475787	25.682215
173.069462	5296.844520	25.687232
173.458398	5307.509861	25.692250
173.581688	5303.996316	25.697268
173.901379	5306.995645	25.702285
173.782548	5314.795425	25.707303
173.851760	5324.424991	25.712320
174.137896	5326.911896	25.717338
174.195938	5328.708515	25.722356
174.477354	5341.278371	25.727373
174.656988	5350.480293	25.732391
174.910760	5359.064535	25.737408
174.595468	5356.402530	25.742426
174.562105	5366.600595	25.747444
175.068235	5380.849317	25.752461
175.516877	5378.253870	25.757479
175.698159	5384.803994	25.762496
175.962112	5394.213691	25.767514
175.875105	5405.345072	25.772532
176.426071	5404.185638	25.777549
176.330444	5400.668491	25.782567
176.476156	5407.097929	25.787584
176.823543	5418.060254	25.792602
176.693998	5420.533377	25.797620
177.113897	5419.151414	25.802637
177.240534	5441.048162	25.807655
177.226113	5444.178771	25.812672
177.564507	5448.090615	25.817690
177.092073	5460.747087	25.822708
177.913129	5471.319575	25.827725
177.954979	5478.964830	25.832743
177.846585	5493.063695	25.837760
178.247538	5503.042278	25.842778
178.510146	5519.213772	25.847796
178.522342	5518.972088	25.852813
178.962529	5530.522861	25.857831
179.329710	5535.714968	25.862848
179.593516	5542.861452	25.867866
179.601205	5548.210894	25.872884
179.763148	5547.649026	25.877901
180.115485	5552.360497	25.882919
179.999044	5565.857759	25.887936
180.281909	5576.833443	25.892954
180.310407	5575.231845	25.897972
180.502196	5578.538511	25.902989
180.900109	5598.246426	25.908007
180.852599	5591.154685	25.913024
181.110604	5609.050513	25.918042
181.260563	5621.331805	25.923060
181.456607	5620.625699	25.928077
181.589502	5636.647159	25.933095
181.821826	5640.420986	25.938112
181.911165	5648.109380	25.943130
182.050060	5671.819565	25.948148
182.351875	5672.934068	25.953165
182.471625	5678.010302	25.958183
182.889172	5688.633505	25.963200
182.987018	5692.147466	25.968218
182.741988	5709.651855	25.973236
183.157331	5715.909739	25.978253
183.614644	5719.979786	25.983271
183.592162	5729.387180	25.988288
184.342090	5736.959497	25.993306
184.342172	5750.890045	25.998324
184.342283	5740.791939	26.003341
184.511824	5744.730300	26.008359
184.501296	5762.545237	26.013376
185.103155	5764.727050	26.018394
185.156839	5764.545154	26.023412
185.428530	5776.696996	26.028429
185.393092	5790.399545	26.033447
185.617115	5782.750651	26.038464
185.400827	5784.069438	26.043482
185.721983	5807.505025	26.048500
186.279352	5813.926937	26.053517
186.184040	5823.039590	26.058535
186.432097	5826.820461	26.063552
186.593367	5834.677596	26.068570
186.670451	5843.554910	26.073588
187.095897	5857.229500	26.078605
187.346775	5863.715229	26.083623
187.766456	5864.527177	26.088640
187.765189	5861.680163	26.093658
187.935287	5862.370218	26.098676
188.286889	5863.230711	26.103693
188.119110	5877.954732	26.108711
188.229071	5883.354541	26.113728
188.620735	5878.782384	26.118746
188.768885	5889.773049	26.123764
188.855303	5897.102141	26.128781
188.829216	5903.659683	26.133799
188.701456	5906.615568	26.138816
189.346364	5922.241397	26.143834
189.237744	5935.068482	26.148852
190.002086	5948.955215	26.153869
190.166875	5947.641591	26.158887
190.373449	5957.354144	26.163904
190.620685	5962.571478	26.168922
190.668588	5978.663374	26.173940
190.803936	5981.230813	26.178957
190.965040	5984.507637	26.183975
191.317160	6001.678845	26.188992
191.178082	5999.443706	26.194010
191.642456	6011.044660	26.199028
191.896815	6011.652073	26.204045
192.299736	6029.522455	26.209063
192.077399	6033.935802	26.214080
192.213511	6033.693639	26.219098
192.276604	6045.729973	26.224116
192.760541	6054.379502	26.229133
193.049966	6056.124161	26.234151
192.832535	6074.050733	26.239168
193.126234	6075.166533	26.244186
193.422826	6082.267056	26.249204
193.953348	6103.476291	26.254221
193.888993	6102.889880	26.259239
193.998527	6112.788182	26.264256
194.033922	6127.145959	26.269274
194.428734	6128.713121	26.274292
194.946061	6136.511450	26.279309
195.199329	6150.437363	26.284327
195.345137	6159.272496	26.289344
195.506626	6165.425094	26.294362
195.627739	6166.293300	26.299380
195.836541	6172.201731	26.304397
195.602947	6177.503924	26.309415
195.655947	6188.326582	26.314432
196.344078	6188.395691	26.319450
196.222579	6204.287037	26.324468
196.378559	6206.904941	26.329485
196.954751	6221.114936	26.334503
197.310867	6228.389283	26.339520
197.400924	6225.025980	26.344538
197.710621	6243.599351	26.349556
197.615872	6255.212289	26.354573
198.043187	6249.147619	26.359591
197.482971	6266.051621	26.364608
198.109644	6271.979855	26.369626
198.415846	6280.209073	26.374644
198.505367	6279.415458	26.379661
198.797655	6294.070896	26.384679
198.749166	6306.478440	26.389696
199.359410	6310.600427	26.394714
199.659373	6331.738716	26.399732
199.922084	6326.577393	26.404749
200.050681	6326.181722	26.409767
199.766992	6330.431128	26.414784
200.110692	6346.925272	26.419802
200.106307	6346.458886	26.424820
200.321736	6341.478589	26.429837
200.868518	6358.458641	26.434855
200.661209	6376.456529	26.439872
200.962630	6373.495724	26.444890
201.102658	6394.968506	26.449908
201.036789	6398.688188	26.454925
201.617952	6409.191477	26.459943
201.813789	6422.637292	26.464960
202.239199	6415.051290	26.469978
202.525854	6429.856089	26.474996
202.600372	6448.371806	26.480013
202.656718	6450.793848	26.485031
203.016780	6470.530733	26.490048
203.475565	6467.257992	26.495066
203.757844	6479.260274	26.500084
203.639791	6480.759442	26.505101
204.203064	6474.834397	26.510119
204.162277	6494.308953	26.515136
204.392099	6501.003400	26.520154
204.445301	6494.946749	26.525172
204.650456	6491.688482	26.530189
204.814341	6515.537903	26.535207
204.457240	6526.620729	26.540224
205.002632	6533.562493	26.545242
205.200388	6545.960035	26.550260
205.445111	6553.674976	26.555277
205.657760	6560.258490	26.560295
205.831677	6576.886771	26.565312
206.003025	6575.966679	26.570330
206.093627	6593.138373	26.575348
206.177199	6606.819731	26.580365
206.586287	6613.274629	26.585383
206.872996	6643.608046	26.590400
207.155056	6650.922575	26.595418
207.425190	6652.553512	26.600436
207.753926	6663.260647	26.605453
208.164090	6666.927907	26.610471
207.859871	6681.178322	26.615488
208.112852	6701.705658	26.620506
208.476743	6701.393079	26.625524
208.885627	6716.185275	26.630541
209.264807	6723.822402	26.635559
209.011323	6730.131747	26.640576
209.361080	6736.043534	26.645594
209.620849	6747.493913	26.650612
209.622652	6752.418453	26.655629
210.043924	6755.282150	26.660647
210.353337	6776.391061	26.665664
210.377264	6771.740550	26.670682
210.335111	6787.736774	26.675700
210.516292	6808.253378	26.680717
210.768960	6808.011889	26.685735
210.966249	6834.625061	26.690752
211.247443	6833.409943	26.695770
211.583891	6843.689799	26.700788
211.615185	6856.195707	26.705805
211.852411	6863.081696	26.710823
212.264590	6886.068758	26.715840
212.279673	6889.046619	26.720858
212.814783	6903.756055	26.725876
212.768725	6909.581533	26.730893
213.245398	6928.154695	26.735911
213.131973	6933.870772	26.740928
213.855523	6929.792508	26.745946
214.158578	6946.078891	26.750964
214.314652	6949.394560	26.755981
214.391459	6944.719936	26.760999
214.708297	6942.646869	26.766016
214.547309	6949.952002	26.771034
215.478034	6954.052344	26.776052
215.488184	6960.045818	26.781069
215.184421	6967.796349	26.786087
215.244075	6975.811954	26.791104
215.664505	6985.093783	26.796122
215.848503	6995.277644	26.801140
216.155223	6989.256881	26.806157
216.613549	7012.006418	26.811175
216.376936	7019.228719	26.816192
216.723527	7023.366918	26.821210
217.409377	7036.496496	26.826228
217.122520	7049.169180	26.831245
217.504832	7049.933373	26.836263
217.392200	7060.694100	26.841280
217.959892	7060.782086	26.846298
217.884756	7068.897770	26.851316
217.972297	7083.854253	26.856333
217.984174	7098.809973	26.861351
218.199730	7104.960731	26.866368
218.544099	7120.183230	26.871386
218.951400	7128.340170	26.876404
219.015938	7146.709780	26.881421
219.458074	7157.974000	26.886439
219.648830	7173.485790	26.891456
220.028020	7185.855342	26.896474
220.220779	7188.158247	26.901492
220.336774	7205.500166	26.906509
220.997753	7209.106147	26.911527
220.981184	7222.519527	26.916544
220.939230	7231.693972	26.921562
221.787528	7238.462276	26.926580
221.624520	7245.726803	26.931597
221.997644	7259.963106	26.936615
221.984068	7284.728426	26.941632
222.448620	7278.357678	26.946650
222.489889	7276.485591	26.951668
222.325891	7300.927234	26.956685
222.818365	7307.852329	26.961703
223.265158	7323.519866	26.966720
224.029391	7331.264246	26.971738
224.298091	7323.822387	26.976756
224.050702	7344.873958	26.981773
224.492325	7349.909705	26.986791
224.564410	7351.262349	26.991808
224.519072	7353.075362	26.996826
225.069486	7363.145202	27.001844
224.751093	7377.221585	27.006861
225.197601	7375.488050	27.011879
225.516379	7382.626645	27.016896
225.532298	7388.000590	27.021914
226.062259	7398.954446	27.026932
225.972895	7416.896989	27.031949
226.474801	7418.677949	27.036967
226.221478	7437.249178	27.041984
226.259729	7447.834959	27.047002
227.018959	7455.119257	27.052020
227.114069	7474.428340	27.057037
227.309375	7475.717493	27.062055
227.581492	7492.703743	27.067072
227.860887	7497.490287	27.072090
228.258273	7514.384323	27.077108
228.381461	7521.847212	27.082125
228.835788	7516.478749	27.087143
229.168466	7535.217149	27.092160
229.506928	7549.878987	27.097178
229.720967	7549.242603	27.102196
229.645075	7550.940457	27.107213
229.910632	7557.291895	27.112231
230.097277	7562.209795	27.117248
230.061668	7563.828729	27.122266
230.319140	7569.654220	27.127284
230.486570	7578.754995	27.132301
230.828130	7593.220649	27.137319
230.842379	7591.447472	27.142336
230.887549	7615.168538	27.147354
231.257282	7611.177126	27.152372
231.157849	7638.336750	27.157389
231.667998	7650.414598	27.162407
231.743915	7667.870570	27.167424
232.126884	7671.018231	27.172442
232.286779	7692.407335	27.177460
232.526079	7701.834713	27.182477
232.880810	7718.861899	27.187495
233.348976	7726.081408	27.192512
233.573392	7755.217279	27.197530
233.653880	7754.541826	27.202548
233.977671	7768.164318	27.207565
234.278306	7780.151949	27.212583
234.516204	7782.113213	27.217600
234.407335	7797.101043	27.222618
235.125912	7801.629446	27.227636
235.276572	7835.073721	27.232653
235.732264	7827.008844	27.237671
236.056122	7832.584085	27.242688
236.146190	7847.000938	27.247706
236.656630	7844.824832	27.252724
236.554040	7853.889117	27.257741
236.745788	7872.375275	27.262759
237.169662	7871.867019	27.267776
237.003962	7882.778605	27.272794
237.462460	7892.013890	27.277812
237.868940	7904.461735	27.282829
237.972246	7914.238859	27.287847
238.309201	7915.679492	27.292864
238.220894	7931.068313	27.297882
238.744022	7943.128535	27.302900
238.940370	7948.139730	27.307917
238.979943	7959.511706	27.312935
239.508781	7969.575789	27.317952
239.183655	7975.022274	27.322970
239.697406	7987.860632	27.327988
239.960001	7999.952234	27.333005
240.492473	8010.887121	27.338023
240.713711	8028.630062	27.343040
240.612829	8032.346087	27.348058
241.060949	8042.233430	27.353076
241.480326	8060.156886	27.358093
241.674639	8073.095859	27.363111
241.796695	8081.982995	27.368128
241.927089	8094.960410	27.373146
242.013824	8099.136405	27.378164
242.204973	8122.686872	27.383181
242.709108	8136.363469	27.388199
243.108534	8135.540171	27.393216
243.074161	8142.387104	27.398234
243.864390	8157.597446	27.403252
243.715304	8166.309258	27.408269
243.516997	8169.639621	27.413287
244.031874	8174.897747	27.418304
244.388392	8189.680393	27.423322
244.722047	8203.093293	27.428340
244.914295	8214.176312	27.433357
245.175976	8226.823856	27.438375
245.438655	8233.838972	27.443392
245.417115	8242.420342	27.448410
245.914570	8252.991477	27.453428
246.092740	8254.766408	27.458445
246.353731	8259.808605	27.463463
246.355204	8270.530061	27.468480
246.570577	8280.750762	27.473498
246.796590	8293.451297	27.478516
246.915310	8306.449632	27.483533
247.010952	8318.933823	27.488551
247.323929	8337.319370	27.493568
247.494657	8359.121134	27.498586
248.135774	8364.533180	27.503604
248.500391	8384.754450	27.508621
248.446424	8391.184646	27.513639
249.076443	8394.820974	27.518656
248.997719	8413.299529	27.523674
249.403903	8422.107591	27.528692
249.810063	8446.164660	27.533709
250.009717	8437.520829	27.538727
250.518416	8460.737839	27.543744
250.743202	8470.979271	27.548762
250.630078	8467.057004	27.553780
251.055747	8486.782620	27.558797
251.391332	8497.003553	27.563815
251.541260	8510.745388	27.568832
251.719859	8523.020978	27.573850
252.214347	8535.060819	27.578868
252.558852	8546.499045	27.583885
252.418783	8557.501727	27.588903
253.010149	8556.477857	27.593920
253.104113	8567.614370	27.598938
253.464175	8576.843321	27.603956
253.812362	8592.909405	27.608973
253.662492	8608.740965	27.613991
253.995721	8606.554647	27.619008
254.000322	8626.864151	27.624026
254.672418	8641.225177	27.629044
254.619430	8640.340128	27.634061
254.795884	8666.545619	27.639079
255.286161	8671.182620	27.644096
255.606350	8693.583328	27.649114
255.754778	8699.198943	27.654132
255.916424	8705.781746	27.659149
256.165831	8723.741945	27.664167
256.692454	8737.260764	27.669184
256.730289	8754.259620	27.674202
257.135534	8767.762746	27.679220
257.378315	8774.999033	27.684237
257.572145	8802.638520	27.689255
257.888616	8806.150402	27.694272
258.176075	8825.298162	27.699290
258.391871	8839.408788	27.704308
258.809528	8855.710480	27.709325
259.000283	8861.458431	27.714343
259.243194	8870.368059	27.719360
259.226512	8889.355153	27.724378
259.932302	8883.678545	27.729396
260.181407	8909.317327	27.734413
260.197754	8916.627027	27.739431
260.391437	8928.509027	27.744448
260.592468	8939.398515	27.749466
261.144233	8949.330098	27.754484
261.629064	8960.396146	27.759501
261.633298	8976.945828	27.764519
261.917481	8987.241386	27.769536
262.096349	8986.367359	27.774554
262.426045	8998.127066	27.779572
262.720855	9008.367298	27.784589
262.624392	9009.004517	27.789607
263.037423	9015.952177	27.794624
263.590547	9042.234955	27.799642
263.376135	9036.841371	27.804660
264.002855	9051.456090	27.809677
263.771145	9055.824262	27.814695
264.423192	9065.604438	27.819712
264.407126	9091.281854	27.824730
264.935026	9096.298255	27.829748
265.253174	9110.181517	27.834765
265.508258	9119.382982	27.839783
265.653589	9128.424838	27.844800
265.759325	9143.222275	27.849818
266.336417	9153.484671	27.854836
266.571144	9157.157819	27.859853
266.566168	9179.707928	27.864871
267.034618	9191.663874	27.869888
266.805578	9207.382054	27.874906
267.427437	9221.037858	27.879924
267.384703	9234.321033	27.884941
267.497824	9252.549361	27.889959
268.304444	9264.727063	27.894976
268.364123	9278.935097	27.899994
268.652874	9292.532630	27.905012
269.050089	9313.368637	27.910029
269.240281	9321.333238	27.915047
269.870129	9343.218945	27.920064
270.194264	9344.718533	27.925082
270.404889	9368.769544	27.930100
270.871037	9370.145854	27.935117
270.787417	9384.913158	27.940135
271.414841	9399.026031	27.945152
271.806430	9398.794326	27.950170
272.030494	9418.025248	27.955188
272.471151	9430.140410	27.960205
272.426815	9438.918499	27.965223
272.741607	9442.411823	27.970240
272.781627	9445.840843	27.975258
273.057735	9462.686201	27.980276
273.887547	9476.057033	27.985293
273.441040	9480.496840	27.990311
273.980410	9502.447425	27.995328
274.253264	9513.812227	28.000346
274.431128	9524.819351	28.005364
274.802392	9534.419591	28.010381
274.691179	9553.409542	28.015399
275.268379	9562.440789	28.020416
275.566050	9581.559315	28.025434
275.809934	9590.705937	28.030452
276.125071	9604.653188	28.035469
276.241898	9623.831660	28.040487
276.453997	9632.958023	28.045504
276.535285	9651.059120	28.050522
276.466589	9657.810953	28.055540
277.014352	9674.768659	28.060557
277.279835	9697.889555	28.065575
278.166099	9713.158760	28.070592
278.231593	9726.876834	28.075610
278.218625	9748.712163	28.080628
278.461997	9759.747053	28.085645
278.988032	9781.845297	28.090663
279.392359	9791.926726	28.095680
279.391630	9809.838753	28.100698
279.578447	9819.007057	28.105716
280.037613	9837.390138	28.110733
280.478282	9859.366079	28.115751
280.558974	9861.320621	28.120768
281.054952	9876.313258	28.125786
281.290594	9882.045023	28.130804
281.889392	9880.893629	28.135821
282.016062	9893.452953	28.140839
282.110630	9912.619422	28.145856
282.346204	9917.849183	28.150874
282.684430	9931.461537	28.155892
282.814978	9933.484054	28.160909
283.134716	9961.377077	28.165927
283.470706	9964.264116	28.170944
283.538314	9984.464195	28.175962
283.798627	9993.962072	28.180980
284.283922	10011.709751	28.185997
284.549674	10020.180631	28.191015
284.695753	10037.820445	28.196032
285.266491	10053.199348	28.201050
285.486807	10064.755848	28.206068
285.773355	10079.172074	28.211085
286.096237	10096.080142	28.216103
286.119270	10102.868286	28.221120
286.689155	10113.110243	28.226138
287.188621	10140.429145	28.231156
287.674863	10137.672449	28.236173
287.900272	10153.822268	28.241191
288.217754	10159.910719	28.246208
288.669659	10172.728713	28.251226
288.841512	10183.579297	28.256244
289.394547	10189.637173	28.261261
289.012426	10194.348072	28.266279
289.282960	10199.907126	28.271296
289.933693	10222.125287	28.276314
290.277941	10230.789201	28.281332
290.722472	10238.452286	28.286349
290.648161	10253.212504	28.291367
291.025152	10254.205011	28.296384
291.043352	10269.806419	28.301402
291.713310	10283.351278	28.306420
291.928979	10290.298761	28.311437
291.863694	10310.346350	28.316455
291.947203	10322.091785	28.321472
292.368858	10333.118033	28.326490
292.488228	10349.584591	28.331508
292.893855	10360.550217	28.336525
293.581656	10378.036029	28.341543
293.486777	10396.244382	28.346560
293.644294	10414.577405	28.351578
294.061042	10440.135203	28.356596
294.311490	10446.051114	28.361613
294.483119	10474.918509	28.366631
294.623647	10490.399898	28.371648
295.079829	10501.761846	28.376666
295.073663	10530.335114	28.381684
296.050658	10541.179767	28.386701
295.938920	10562.911535	28.391719
296.498263	10585.087611	28.396736
297.070594	10602.490682	28.401754
297.069234	10617.170294	28.406772
297.503349	10615.719432	28.411789
298.094231	10639.709360	28.416807
298.264880	10652.341244	28.421824
298.992761	10653.948203	28.426842
298.860091	10667.218067	28.431860
298.810876	10681.460014	28.436877
299.565562	10693.915186	28.441895
299.524318	10706.990778	28.446912
300.079328	10711.302404	28.451930
300.107394	10735.652166	28.456948
300.472042	10743.166940	28.461965
300.491024	10753.565014	28.466983
300.757150	10757.479850	28.472000
301.576807	10778.983873	28.477018
301.860494	10789.962538	28.482036
302.263931	10794.642099	28.487053
302.013484	10806.838002	28.492071
302.232539	10830.807483	28.497088
302.620491	10840.974143	28.502106
302.909309	10856.685211	28.507124
303.270801	10870.951378	28.512141
303.809874	10883.816201	28.517159
304.176363	10896.872262	28.522176
303.893154	10913.130829	28.527194
304.152991	10932.414545	28.532212
304.292052	10943.564361	28.537229
305.139188	10958.537598	28.542247
305.042895	10978.492874	28.547264
305.636510	10996.208737	28.552282
305.744402	11019.160186	28.557300
305.872051	11037.931087	28.562317
306.340338	11062.613328	28.567335
306.915068	11082.773045	28.572352
307.634293	11100.472488	28.577370
307.666796	11117.663788	28.582388
308.057769	11137.230303	28.587405
308.423897	11142.244187	28.592423
308.518248	11156.306126	28.597440
309.060151	11170.607414	28.602458
309.334494	11191.947884	28.607476
309.707922	11200.140353	28.612493
309.554102	11218.649237	28.617511
309.710385	11240.548208	28.622528
310.540628	11260.873338	28.627546
310.345203	11282.284340	28.632564
310.436744	11291.689326	28.637581
311.171266	11317.795337	28.642599
311.775320	11346.365830	28.647616
312.435330	11365.176814	28.652634
312.503984	11375.172748	28.657652
313.144126	11386.825342	28.662669
313.404104	11401.571989	28.667687
313.800546	11419.218095	28.672704
314.030365	11418.045473	28.677722
314.357807	11437.922231	28.682740
314.575172	11449.881071	28.687757
314.802659	11468.794647	28.692775
315.176352	11473.052756	28.697792
315.799978	11483.277580	28.702810
316.106017	11502.065208	28.707828
316.469604	11497.628711	28.712845
316.570255	11514.089753	28.717863
316.942373	11525.358134	28.722880
317.628315	11530.890406	28.727898
317.931328	11541.386520	28.732916
317.941032	11541.220933	28.737933
318.053939	11552.015234	28.742951
318.031415	11565.764233	28.747968
318.614515	11578.035313	28.752986
318.729196	11595.135236	28.758004
319.238900	11602.580269	28.763021
319.322214	11622.021812	28.768039
319.861627	11644.363310	28.773056
320.043055	11644.259237	28.778074
320.550952	11667.530901	28.783092
320.723027	11677.352911	28.788109
321.199952	11695.968712	28.793127
321.116903	11708.053718	28.798144
321.657671	11713.776144	28.803162
321.787300	11736.961894	28.808180
322.153158	11751.777490	28.813197
322.415003	11758.961430	28.818215
322.367204	11788.992520	28.823232
322.632415	11789.014262	28.828250
323.456741	11806.937898	28.833268
323.635284	11832.528596	28.838285
323.898029	11843.482741	28.843303
324.184275	11869.542906	28.848320
324.916406	11880.407758	28.853338
325.087412	11902.014683	28.858356
325.027790	11917.569654	28.863373
325.629390	11927.150838	28.868391
325.817272	11946.273193	28.873408
326.403939	11956.813524	28.878426
326.659633	11979.092501	28.883444
327.019167	11998.222756	28.888461
327.383416	12009.423191	28.893479
327.575936	12038.978109	28.898496
328.083463	12039.043996	28.903514
328.604994	12062.718207	28.908532
328.583425	12083.979734	28.913549
329.007447	12090.648945	28.918567
329.054653	12107.355710	28.923584
329.737859	12126.157511	28.928602
329.903028	12144.667862	28.933620
330.469318	12159.578694	28.938637
330.789550	12174.228093	28.943655
330.912589	12196.044967	28.948672
331.217861	12212.989285	28.953690
331.226335	12235.629384	28.958708
331.589444	12250.196339	28.963725
331.887299	12279.836184	28.968743
332.392786	12304.994217	28.973760
332.828244	12311.510142	28.978778
333.441762	12340.566968	28.983796
333.286273	12354.024747	28.988813
334.039054	12370.134920	28.993831
334.421917	12393.395491	28.998848
335.074763	12414.485434	29.003866
335.232548	12427.426837	29.008884
335.433683	12439.982520	29.013901
336.018909	12444.896122	29.018919
336.005731	12473.789222	29.023936
336.577314	12484.575367	29.028954
336.937462	12499.945067	29.033972
337.300053	12517.925922	29.038989
337.797623	12527.248978	29.044007
337.900753	12554.624013	29.049024
338.616974	12552.222523	29.054042
338.550296	12579.526300	29.059060
338.914203	12582.459904	29.064077
339.172209	12605.291882	29.069095
339.444619	12623.946955	29.074112
339.814525	12640.587854	29.079130
339.950702	12660.770598	29.084148
340.315003	12672.132471	29.089165
340.564255	12691.485966	29.094183
340.786414	12721.760461	29.099200
341.570955	12745.091178	29.104218
341.889427	12751.732948	29.109236
342.376819	12778.009176	29.114253
342.869377	12785.173160	29.119271
342.839323	12803.910526	29.124288
343.450670	12824.524274	29.129306
344.245018	12834.473624	29.134324
343.865887	12842.412065	29.139341
344.569823	12862.695563	29.144359
344.649227	12869.207455	29.149376
344.712551	12879.391338	29.154394
344.531147	12889.187245	29.159412
345.420179	12922.464968	29.164429
345.800275	12926.460303	29.169447
345.592334	12951.844637	29.174464
345.961316	12971.429139	29.179482
346.841157	12991.830486	29.184500
347.308781	13019.543839	29.189517
347.612046	13024.062811	29.194535
347.513571	13056.696503	29.199552
348.106482	13061.520644	29.204570
348.693052	13086.313332	29.209588
348.736973	13105.105725	29.214605
349.121473	13123.011094	29.219623
349.461820	13146.759260	29.224640
349.970576	13168.257886	29.229658
350.096664	13189.999640	29.234676
350.265833	13211.472560	29.239693
350.751117	13218.874695	29.244711
351.081050	13250.819499	29.249728
351.773200	13274.168502	29.254746
352.111897	13291.373822	29.259764
352.436167	13317.726880	29.264781
352.705047	13318.420700	29.269799
352.981270	13345.981350	29.274816
353.707611	13360.937541	29.279834
353.838178	13384.223063	29.284852
354.262099	13410.270107	29.289869
354.583765	13424.917095	29.294887
354.702529	13457.460604	29.299904
355.400349	13473.564544	29.304922
355.640831	13489.721186	29.309940
355.669765	13515.356546	29.314957
356.209064	13536.850808	29.319975
356.639554	13546.557522	29.324992
357.262075	13563.548100	29.330010
357.451276	13585.239366	29.335028
357.711239	13612.562942	29.340045
358.573384	13627.125426	29.345063
359.049306	13642.155804	29.350080
359.280741	13652.853791	29.355098
359.500466	13664.696821	29.360116
359.932222	13679.168861	29.365133
360.451814	13694.047171	29.370151
360.807608	13724.428658	29.375168
361.216262	13732.417761	29.380186
361.639458	13746.666973	29.385204
361.820306	13768.151326	29.390221
362.122464	13785.425980	29.395239
362.322792	13793.870919	29.400256
362.557767	13809.921324	29.405274
362.840914	13827.306368	29.410292
363.261730	13846.751019	29.415309
363.698682	13863.916205	29.420327
364.325908	13894.249131	29.425344
364.618357	13906.958862	29.430362
365.429466	13923.834956	29.435380
365.683280	13930.060932	29.440397
365.945635	13947.484082	29.445415
366.059261	13962.470406	29.450432
366.186275	13983.454987	29.455450
366.697182	14000.956101	29.460468
366.728830	14027.595996	29.465485
367.211366	14036.723197	29.470503
367.626174	14063.277859	29.475520
367.705684	14074.950466	29.480538
368.032361	14085.406395	29.485556
368.374726	14122.754217	29.490573
368.512754	14133.280778	29.495591
368.957775	14168.177713	29.500608
369.459532	14185.143553	29.505626
369.915186	14205.849517	29.510644
370.019000	14228.682339	29.515661
370.727423	14247.899180	29.520679
370.537152	14277.309116	29.525696
371.378699	14291.840602	29.530714
371.833531	14310.127685	29.535732
372.357792	14323.660396	29.540749
372.949620	14354.154349	29.545767
372.899910	14374.709113	29.550784
373.274145	14389.680218	29.555802
373.872279	14410.780962	29.560820
374.263980	14442.234900	29.565837
374.625443	14456.620642	29.570855
374.939473	14486.823558	29.575872
375.192914	14504.747603	29.580890
375.612796	14516.048191	29.585908
375.831161	14543.502789	29.590925
376.437519	14561.453720	29.595943
377.062011	14582.560002	29.600960
376.939844	14608.997413	29.605978
377.745117	14630.580740	29.610996
377.728707	14650.941093	29.616013
378.461094	14677.772162	29.621031
378.744427	14695.691705	29.626048
378.806630	14718.209495	29.631066
379.503011	14736.727599	29.636084
379.908330	14765.391247	29.641101
380.517547	14772.509292	29.646119
380.752872	14806.758073	29.651136
380.856261	14820.815003	29.656154
381.583153	14851.377028	29.661172
381.515591	14869.926494	29.666189
382.523237	14891.481576	29.671207
382.639398	14908.915872	29.676224
382.701635	14936.297586	29.681242
383.104698	14951.706770	29.686260
383.878146	14980.862612	29.691277
384.654881	15001.310706	29.696295
385.184934	15020.467839	29.701312
385.473356	15032.942086	29.706330
385.996989	15033.024426	29.711348
385.671952	15071.002914	29.716365
386.704042	15087.415910	29.721383
387.015388	15106.105224	29.726400
387.214694	15127.357667	29.731418
387.542747	15136.844373	29.736436
387.780551	15164.653704	29.741453
388.444070	15174.192106	29.746471
388.710637	15193.965491	29.751488
388.845020	15204.957481	29.756506
389.567084	15224.027894	29.761524
389.376705	15247.407025	29.766541
389.712423	15267.706562	29.771559
390.350264	15293.694255	29.776576
390.716963	15317.377840	29.781594
391.066628	15343.423372	29.786612
391.176884	15359.396711	29.791629
391.901688	15390.572638	29.796647
392.525257	15415.125702	29.801664
392.762922	15435.513418	29.806682
393.261144	15447.680301	29.811700
393.948413	15475.315456	29.816717
393.984419	15496.249630	29.821735
393.975567	15511.992246	29.826752
394.566996	15535.495617	29.831770
395.072439	15541.370034	29.836788
396.054509	15556.587947	29.841805
396.378076	15564.363752	29.846823
396.859837	15569.834462	29.851840
397.431164	15588.568801	29.856858
397.954729	15592.921234	29.861876
398.133365	15599.191117	29.866893
398.011210	15615.081057	29.871911
398.634035	15637.306824	29.876928
399.153225	15644.846727	29.881946
398.971318	15657.903547	29.886964
399.300851	15678.397150	29.891981
399.822358	15697.587886	29.896999
400.186883	15726.941573	29.902016
400.336464	15741.620460	29.907034
400.952964	15763.869473	29.912052
401.479045	15783.564918	29.917069
401.608660	15822.964431	29.922087
402.323316	15827.381738	29.927104
402.405221	15868.361690	29.932122
402.793330	15880.552414	29.937140
403.084723	15901.064862	29.942157
403.405942	15936.057065	29.947175
404.183243	15958.104247	29.952192
404.043873	15989.135413	29.957210
404.917295	16005.773038	29.962228
405.289095	16046.095230	29.967245
405.842147	16063.721136	29.972263
406.298877	16081.592710	29.977280
406.627906	16118.545401	29.982298
406.887414	16139.205228	29.987316
407.419509	16152.261091	29.992333
407.671880	16179.911692	29.997351
408.341216	16195.952921	30.002368
408.635709	16229.351674	30.007386
409.283280	16240.936625	30.012404
409.827800	16275.006945	30.017421
410.081829	16302.347935	30.022439
410.776113	16316.291300	30.027456
411.116438	16336.881828	30.032474
411.769256	16349.558852	30.037492
412.042318	16384.477295	30.042509
412.632938	16406.712158	30.047527
412.649372	16415.806125	30.052544
412.799328	16434.683098	30.057562
413.858786	16453.648199	30.062580
414.173722	16473.390061	30.067597
414.573935	16490.989764	30.072615
414.677768	16505.483733	30.077632
414.940957	16529.731449	30.082650
415.709024	16544.200367	30.087668
415.841303	16574.008649	30.092685
416.357553	16590.522694	30.097703
417.078463	16599.683279	30.102720
417.056293	16628.561968	30.107738
417.878696	16645.795626	30.112756
418.176245	16675.256009	30.117773
418.406407	16695.715727	30.122791
419.042846	16722.773160	30.127808
419.054261	16746.191991	30.132826
419.543959	16765.900462	30.137844
419.868810	16790.473653	30.142861
420.260387	16819.369942	30.147879
420.571078	16844.839288	30.152896
421.100820	16875.103780	30.157914
421.420670	16891.042405	30.162932
422.095681	16916.186304	30.167949
422.158354	16926.441935	30.172967
422.499478	16958.760739	30.177984
422.892923	16977.075783	30.183002
423.515150	17000.661410	30.188020
423.501388	17023.437013	30.193037
423.915321	17051.350990	30.198055
424.864089	17071.973347	30.203072
424.955078	17105.307579	30.208090
425.623073	17134.653785	30.213108
425.905173	17166.966390	30.218125
426.229387	17187.048659	30.223143
426.827551	17208.856859	30.228160
427.355996	17234.466335	30.233178
427.800401	17262.306355	30.238196
428.161354	17277.916684	30.243213
428.452524	17311.169378	30.248231
429.389750	17330.707255	30.253248
429.520981	17357.276160	30.258266
429.955613	17390.531789	30.263284
430.452943	17410.675617	30.268301
431.076736	17434.394193	30.273319
431.476409	17448.217120	30.278336
431.879810	17477.302063	30.283354
432.286922	17502.608717	30.288372
432.446141	17517.562251	30.293389
432.964870	17559.851393	30.298407
433.527344	17584.508405	30.303424
433.901723	17611.431249	30.308442
434.389598	17633.364599	30.313460
435.048369	17665.366345	30.318477
434.848816	17692.650844	30.323495
435.486898	17709.247846	30.328512
435.837099	17749.820204	30.333530
436.399674	17765.721534	30.338548
437.092630	17796.227238	30.343565
437.564812	17831.562487	30.348583
438.239045	17840.591996	30.353600
438.470521	17873.475961	30.358618
438.921447	17899.685983	30.363636
439.664369	17923.279104	30.368653
439.789819	17944.069259	30.373671
440.200729	17964.599931	30.378688
440.574854	17984.984767	30.383706
440.990966	18013.973763	30.388724
441.512684	18039.831743	30.393741
441.549367	18069.935272	30.398759
442.404512	18098.830359	30.403776
442.263356	18129.953685	30.408794
443.383663	18155.484313	30.413812
443.713176	18182.389709	30.418829
444.064786	18205.602239	30.423847
444.727142	18232.645098	30.428864
445.053929	18263.720613	30.433882
445.843381	18277.666293	30.438900
446.390279	18308.479972	30.443917
446.897558	18328.958031	30.448935
447.192583	18343.202315	30.453952
447.658388	18368.197665	30.458970
447.909856	18389.195992	30.463988
448.661191	18395.819317	30.469005
448.868713	18435.063491	30.474023
449.222978	18438.198528	30.479040
449.539258	18483.016850	30.484058
450.018234	18502.684552	30.489076
450.619958	18522.023484	30.494093
451.103338	18551.533429	30.499111
451.561584	18572.379531	30.504128
451.869253	18593.495629	30.509146
452.006655	18617.614042	30.514164
452.617884	18637.027411	30.519181
452.740061	18660.952414	30.524199
453.481645	18675.973568	30.529216
453.774146	18703.428805	30.534234
454.404382	18732.416925	30.539252
454.920736	18756.861535	30.544269
454.918773	18785.399114	30.549287
455.507653	18801.739417	30.554304
455.684203	18838.007287	30.559322
456.216803	18864.256361	30.564340
456.672006	18889.500435	30.569357
457.043178	18929.787674	30.574375
457.805012	18946.562208	30.579392
458.511367	18976.145276	30.584410
459.198958	19010.469676	30.589428
459.271591	19034.049100	30.594445
459.791420	19066.359224	30.599463
460.196092	19078.021841	30.604480
460.699883	19118.408737	30.609498
460.958425	19145.225496	30.614516
461.469501	19181.334204	30.619533
461.869632	19209.158685	30.624551
462.868813	19229.206848	30.629568
463.213562	19266.428438	30.634586
463.117409	19285.959571	30.639604
463.887622	19323.531611	30.644621
464.426100	19345.357886	30.649639
465.186069	19373.852800	30.654656
465.664370	19394.519741	30.659674
465.617288	19432.283182	30.664692
466.546102	19459.797768	30.669709
466.916423	19489.825962	30.674727
467.507353	19511.998014	30.679744
467.903907	19539.716121	30.684762
468.602462	19569.971018	30.689780
469.132601	19592.001051	30.694797
469.290022	19624.760578	30.699815
469.669563	19639.788643	30.704832
470.274714	19674.474615	30.709850
470.570485	19701.659071	30.714868
471.412625	19730.249042	30.719885
471.962555	19757.077865	30.724903
472.406839	19784.517168	30.729920
472.618190	19808.871874	30.734938
472.950047	19831.192274	30.739956
473.736677	19861.086335	30.744973
474.063297	19894.312622	30.749991
474.604084	19901.936114	30.755008
475.222992	19946.217588	30.760026
475.559499	19974.893432	30.765044
476.360836	19993.185348	30.770061
476.729240	20023.871747	30.775079
477.350645	20057.172184	30.780096
477.661920	20077.164697	30.785114
478.075179	20102.379002	30.790132
478.431778	20118.958975	30.795149
478.892570	20145.991838	30.800167
479.601286	20172.512045	30.805184
480.300672	20194.118204	30.810202
480.556080	20217.183927	30.815220
481.051351	20233.142050	30.820237
481.902462	20266.817549	30.825255
482.091149	20296.439475	30.830272
482.520185	20305.552772	30.835290
482.681054	20332.298003	30.840308
483.922831	20363.145098	30.845325
483.751412	20366.432287	30.850343
484.403438	20387.407937	30.855360
484.779163	20413.557303	30.860378
484.998738	20430.923511	30.865396
485.816578	20447.797981	30.870413
485.981956	20473.247454	30.875431
486.163546	20493.709301	30.880448
486.898845	20522.418260	30.885466
487.453644	20553.960856	30.890484
487.933834	20576.322055	30.895501
488.336372	20607.376802	30.900519
488.558183	20630.568321	30.905536
489.223470	20656.565248	30.910554
489.466604	20696.914092	30.915572
490.177419	20719.744801	30.920589
490.447509	20756.127940	30.925607
490.989969	20777.860418	30.930624
491.576223	20805.676973	30.935642
491.907666	20842.183349	30.940660
492.855074	20861.919068	30.945677
493.102615	20895.178392	30.950695
493.583791	20920.743261	30.955712
494.337177	20962.421738	30.960730
494.459775	21001.210478	30.965748
494.963250	21016.694073	30.970765
495.590123	21057.185743	30.975783
496.196176	21085.517708	30.980800
496.882867	21114.633211	30.985818
496.918569	21148.014600	30.990836
497.614017	21173.982214	30.995853
498.510802	21206.704401	31.000871
498.351910	21241.500179	31.005888
499.476980	21266.528671	31.010906
499.720973	21312.262024	31.015924
500.353802	21334.871878	31.020941
500.879664	21367.563969	31.025959
501.474318	21384.859636	31.030976
502.076539	21423.037008	31.035994
502.709485	21446.714812	31.041012
503.487381	21466.458735	31.046029
503.773652	21493.887267	31.051047
503.863668	21525.396802	31.056064
504.542994	21545.503767	31.061082
505.022810	21577.489414	31.066100
505.638761	21597.448393	31.071117
505.924309	21634.690067	31.076135
506.633000	21659.531531	31.081152
507.125554	21678.271463	31.086170
507.531815	21725.117716	31.091188
508.274173	21730.441953	31.096205
508.929450	21764.378167	31.101223
509.016563	21789.051763	31.106240
510.001919	21812.592669	31.111258
510.113246	21846.291965	31.116276
510.975966	21866.016687	31.121293
511.499949	21901.667117	31.126311
511.338522	21933.583169	31.131328
512.139150	21949.949814	31.136346
512.348983	21988.151824	31.141364
513.282494	22009.729635	31.146381
513.444521	22045.790866	31.151399
513.986065	22073.344509	31.156416
514.634631	22098.019017	31.161434
515.423767	22144.471401	31.166452
515.842682	22164.973639	31.171469
515.994936	22196.145915	31.176487
516.618351	22227.832098	31.181504
517.262990	22253.303588	31.186522
517.233383	22282.469818	31.191540
518.079230	22295.486998	31.196557
518.538426	22326.977900	31.201575
518.976272	22358.510109	31.206592
519.582667	22385.238896	31.211610
520.080429	22420.426770	31.216628
520.889507	22441.620135	31.221645
521.148177	22464.492093	31.226663
521.764531	22500.685199	31.231680
521.959759	22528.887696	31.236698
522.264853	22567.606693	31.241716
523.290223	22601.511657	31.246733
523.655302	22625.314976	31.251751
523.927806	22658.472255	31.256768
524.599909	22688.022057	31.261786
524.908262	22717.230778	31.266804
525.515089	22752.136763	31.271821
526.031782	22790.873607	31.276839
526.564571	22815.642972	31.281856
527.441354	22854.127653	31.286874
527.617806	22898.668314	31.291892
528.190896	22929.245030	31.296909
528.892633	22963.018048	31.301927
529.118225	22995.469183	31.306944
530.381471	23030.936352	31.311962
530.495822	23061.187017	31.316980
531.244623	23090.466324	31.321997
531.606809	23127.161676	31.327015
532.458214	23156.418691	31.332032
533.209197	23180.275980	31.337050
533.062838	23223.187037	31.342068
534.244518	23251.823742	31.347085
534.853512	23277.738155	31.352103
535.005800	23310.378220	31.357120
535.727739	23338.101264	31.362138
536.491878	23370.835176	31.367156
536.868976	23395.307371	31.372173
537.361532	23429.423585	31.377191
537.564274	23463.212415	31.382208
538.320317	23489.856061	31.387226
538.692014	23535.214343	31.392244
539.333612	23554.912194	31.397261
540.309397	23584.188275	31.402279
540.578225	23621.531086	31.407296
541.640502	23652.146046	31.412314
541.634341	23683.730942	31.417332
542.491257	23704.842336	31.422349
543.275590	23733.049064	31.427367
543.289983	23772.409951	31.432384
543.884187	23794.301947	31.437402
544.320024	23831.043934	31.442420
545.101613	23855.105779	31.447437
545.287860	23896.816069	31.452455
545.994273	23922.008296	31.457472
546.464944	23951.913815	31.462490
547.104145	23988.251398	31.467508
547.755301	24022.982047	31.472525
548.352310	24047.869278	31.477543
548.982268	24087.481943	31.482560
549.481233	24110.988017	31.487578
549.937667	24139.581606	31.492596
550.605413	24168.382279	31.497613
551.251081	24200.820139	31.502631
551.587176	24230.380624	31.507648
552.140387	24254.118510	31.512666
552.625819	24284.767914	31.517684
553.459761	24318.048566	31.522701
554.023814	24343.914530	31.527719
554.272776	24368.496460	31.532736
555.317533	24393.351915	31.537754
555.376535	24422.406283	31.542772
555.908364	24442.615128	31.547789
556.419400	24465.601528	31.552807
556.691187	24494.072874	31.557824
557.189604	24521.503957	31.562842
557.782768	24559.714060	31.567860
558.270541	24590.856492	31.572877
559.017352	24624.334569	31.577895
559.592329	24660.335856	31.582912
559.990964	24685.356065	31.587930
560.536761	24717.753529	31.592948
560.950407	24747.492220	31.597965
561.511686	24790.959369	31.602983
561.844656	24838.386876	31.608000
562.805955	24866.845557	31.613018
563.263622	24902.903570	31.618036
563.990427	24933.118024	31.623053
564.763681	24976.369105	31.628071
565.031079	25009.998747	31.633088
565.546731	25039.886209	31.638106
566.423301	25082.375610	31.643124
566.558143	25114.793840	31.648141
567.386689	25148.696055	31.653159
567.646531	25185.221621	31.658176
568.099517	25223.802530	31.663194
569.257889	25264.320651	31.668212
569.759649	25299.930086	31.673229
570.434519	25332.207211	31.678247
571.040041	25372.376068	31.683264
571.716648	25403.547066	31.688282
572.158198	25440.145754	31.693300
572.676463	25471.278458	31.698317
573.680085	25510.841735	31.703335
574.049857	25542.610833	31.708352
574.833813	25569.688956	31.713370
575.222278	25606.966170	31.718388
575.537002	25627.033255	31.723405
576.813413	25656.088338	31.728423
576.984550	25692.919434	31.733440
577.817966	25718.030834	31.738458
578.427856	25757.662583	31.743476
578.723780	25794.752399	31.748493
579.476907	25825.197912	31.753511
579.776105	25854.886647	31.758528
580.855047	25885.635143	31.763546
581.168657	25919.315946	31.768564
581.825364	25946.825307	31.773581
582.427530	25976.839652	31.778599
582.637724	26011.055046	31.783616
583.691013	26050.466247	31.788634
584.385332	26076.756448	31.793652
584.924328	26116.678087	31.798669
585.238892	26136.025219	31.803687
585.878983	26175.134813	31.808704
586.620337	26204.306088	31.813722
586.977488	26237.778361	31.818740
587.677944	26267.689265	31.823757
588.410115	26301.728601	31.828775
588.609905	26334.890714	31.833792
588.780715	26368.537750	31.838810
589.381134	26407.451763	31.843828
589.599288	26446.564762	31.848845
590.591031	26484.330569	31.853863
591.391593	26525.728893	31.858880
592.152359	26558.367422	31.863898
592.704334	26585.672851	31.868916
593.082954	26619.768094	31.873933
594.143535	26643.852800	31.878951
594.447901	26673.763136	31.883968
594.898995	26696.957404	31.888986
595.769535	26731.405570	31.894004
596.027767	26770.803650	31.899021
596.645381	26799.179852	31.904039
597.075960	26827.383136	31.909056
597.545588	26856.629512	31.914074
598.241654	26895.826539	31.919092
598.599398	26932.662268	31.924109
599.805425	26959.101010	31.929127
600.066501	26998.183071	31.934144
600.732378	27036.866832	31.939162
601.388158	27074.945493	31.944180
601.819129	27111.182285	31.949197
602.586989	27147.518070	31.954215
602.886048	27188.711875	31.959232
603.960562	27226.864292	31.964250
604.504930	27252.724439	31.969268
605.154034	27298.603955	31.974285
605.671098	27327.603405	31.979303
605.987020	27371.759225	31.984320
606.673593	27411.559178	31.989338
607.264181	27452.448722	31.994356
608.122996	27492.657972	31.999373
608.667436	27528.479547	32.004391
609.385498	27563.660905	32.009408
609.642716	27600.835935	32.014426
610.481028	27642.394963	32.019444
611.103998	27683.102924	32.024461
611.997122	27717.789412	32.029479
612.717448	27760.479577	32.034496
613.154153	27796.666129	32.039514
614.015510	27830.346491	32.044532
614.588287	27865.936682	32.049549
615.161814	27900.888435	32.054567
615.518082	27937.309055	32.059584
616.508225	27977.903217	32.064602
617.101770	28009.938210	32.069620
617.578964	28049.677394	32.074637
618.595396	28078.896780	32.079655
618.810517	28109.562725	32.084672
619.829045	28144.470487	32.089690
620.382742	28179.647048	32.094708
620.323592	28212.972871	32.099725
621.095940	28251.635948	32.104743
621.793578	28294.728992	32.109760
622.599499	28334.897625	32.114778
623.674045	28358.836811	32.119796
624.040370	28405.850278	32.124813
625.279551	28432.153018	32.129831
625.900683	28469.557073	32.134848
626.123336	28494.186064	32.139866
627.158274	28520.590434	32.144884
627.353930	28561.891700	32.149901
627.812921	28582.963090	32.154919
628.496696	28612.216378	32.159936
629.298431	28645.585065	32.164954
629.984621	28676.671112	32.169972
629.889599	28716.526491	32.174989
630.565808	28741.192203	32.180007
631.175527	28782.795678	32.185024
631.795544	28829.549157	32.190042
632.193811	28856.470851	32.195060
632.620445	28911.604723	32.200077
633.438608	28938.321704	32.205095
634.349696	28975.472684	32.210112
635.276277	29024.334040	32.215130
635.956541	29054.871666	32.220148
636.176401	29085.968157	32.225165
636.905667	29109.248031	32.230183
637.571505	29138.188832	32.235200
637.937093	29178.794702	32.240218
638.773433	29208.246186	32.245236
639.346399	29246.398764	32.250253
639.981855	29281.633949	32.255271
640.910919	29325.799104	32.260288
640.983824	29352.209830	32.265306
642.100593	29394.879252	32.270324
642.562869	29422.752469	32.275341
643.161932	29463.865952	32.280359
643.662218	29505.393216	32.285376
644.152676	29545.341823	32.290394
645.326327	29575.322553	32.295412
645.558710	29620.867996	32.300429
646.245249	29661.241243	32.305447
646.644288	29707.487711	32.310464
647.652764	29745.421304	32.315482
648.377770	29785.889911	32.320500
648.360973	29834.894616	32.325517
649.326357	29876.008445	32.330535
650.241024	29917.522216	32.335552
651.204827	29966.323095	32.340570
651.986842	30003.925999	32.345588
652.288333	30046.427355	32.350605
652.828464	30080.180697	32.355623
653.703474	30117.377325	32.360640
654.106836	30160.804837	32.365658
655.412896	30205.627151	32.370676
655.452993	30246.178639	32.375693
655.880728	30283.774324	32.380711
657.236602	30327.893756	32.385728
657.567272	30371.908339	32.390746
658.626359	30416.004904	32.395764
659.089851	30447.748007	32.400781
659.670914	30489.782960	32.405799
660.940533	30535.907590	32.410816
661.171086	30578.503330	32.415834
661.908936	30606.688993	32.420852
662.419198	30651.965622	32.425869
663.219827	30687.619850	32.430887
663.563413	30734.142805	32.435904
664.468667	30775.956890	32.440922
665.368490	30806.329984	32.445940
665.553065	30852.928680	32.450957
666.497158	30891.746839	32.455975
666.837384	30927.840232	32.460992
667.537084	30979.162912	32.466010
668.344196	31007.471029	32.471028
669.214172	31058.097153	32.476045
669.728313	31095.655496	32.481063
670.653681	31135.918369	32.486080
671.573502	31174.412137	32.491098
672.341730	31201.569754	32.496116
672.708656	31242.640956	32.501133
673.497776	31288.956307	32.506151
674.176009	31318.467183	32.511168
674.607086	31353.112072	32.516186
675.732047	31392.452832	32.521204
676.265006	31437.038560	32.526221
677.131711	31468.960309	32.531239
677.913269	31497.823088	32.536256
678.197229	31531.916039	32.541274
678.736069	31564.325480	32.546292
679.454294	31598.426393	32.551309
679.998022	31633.939154	32.556327
680.596664	31645.452284	32.561344
681.385591	31689.644450	32.566362
682.339010	31717.690400	32.571380
682.623477	31749.495144	32.576397
683.210043	31787.751439	32.581415
684.194439	31816.513358	32.586432
684.571965	31856.174349	32.591450
685.194493	31882.597058	32.596468
685.565451	31928.100587	32.601485
686.201495	31968.694872	32.606503
687.288117	32010.179598	32.611520
687.917929	32060.245201	32.616538
688.571045	32087.738102	32.621556
689.282561	32127.606503	32.626573
689.949593	32172.337181	32.631591
690.995019	32210.857458	32.636608
691.319072	32243.339525	32.641626
692.116737	32290.743147	32.646644
692.841920	32339.782974	32.651661
693.130604	32377.777226	32.656679
694.114655	32412.912585	32.661696
694.969098	32463.512958	32.666714
695.561673	32497.982736	32.671732
696.094990	32553.982046	32.676749
696.504274	32604.418559	32.681767
697.383727	32628.197295	32.686784
697.991503	32689.356751	32.691802
698.957020	32730.710150	32.696820
699.961543	32778.607220	32.701837
700.206037	32820.029454	32.706855
701.325774	32865.828705	32.711872
701.660534	32915.127010	32.716890
702.472771	32960.943015	32.721908
703.483937	33003.743902	32.726925
703.989901	33049.690252	32.731943
705.241430	33084.304369	32.736960
705.459372	33128.203349	32.741978
706.212650	33177.379831	32.746996
706.716977	33222.321582	32.752013
707.884190	33260.799439	32.757031
708.546314	33300.026623	32.762048
709.278585	33344.888685	32.767066
710.005471	33394.088776	32.772084
710.716711	33426.518370	32.777101
711.100344	33478.535257	32.782119
712.255610	33522.933153	32.787136
713.281743	33566.807645	32.792154
713.870865	33616.023508	32.797172
714.139684	33648.750333	32.802189
714.795211	33696.065598	32.807207
715.556143	33736.017843	32.812224
715.896295	33776.301599	32.817242
716.791085	33817.225654	32.822260
717.547994	33868.672936	32.827277
718.100097	33922.852101	32.832295
719.345079	33966.882831	32.837312
720.085447	34005.934699	32.842330
720.602349	34053.272476	32.847348
721.497568	34098.534238	32.852365
721.809575	34138.905289	32.857383
722.946694	34167.791954	32.862400
723.081644	34226.633700	32.867418
724.316570	34256.934066	32.872436
725.177440	34309.978396	32.877453
725.504366	34354.861834	32.882471
726.583438	34394.297640	32.887488
727.365403	34437.345993	32.892506
728.258367	34472.587592	32.897524
728.614384	34500.503224	32.902541
729.415725	34536.151281	32.907559
730.268969	34563.287319	32.912576
730.884801	34606.836233	32.917594
731.588533	34634.691269	32.922612
732.297355	34660.958554	32.927629
732.939410	34700.577179	32.932647
734.024252	34736.712285	32.937664
734.227285	34780.882598	32.942682
734.609151	34814.213155	32.947700
736.026403	34865.041000	32.952717
736.404949	34910.170444	32.957735
737.327738	34939.072767	32.962752
737.900194	34993.871126	32.967770
738.419035	35033.136626	32.972788
739.178999	35085.945799	32.977805
739.834868	35136.615325	32.982823
740.479035	35172.921353	32.987840
740.933577	35229.622987	32.992858
741.977289	35278.569212	32.997876
743.112471	35325.307192	33.002893
743.606621	35383.077922	33.007911
744.646703	35422.572341	33.012928
745.076451	35478.658880	33.017946
745.800721	35527.788486	33.022964
746.586241	35568.606595	33.027981
747.300380	35626.419413	33.032999
748.480265	35662.370500	33.038016
749.079610	35711.539064	33.043034
750.028694	35756.656841	33.048052
751.152781	35806.793070	33.053069
751.572995	35849.780811	33.058087
752.353852	35898.687432	33.063104
752.787281	35945.302720	33.068122
753.432374	35994.439483	33.073140
754.531027	36040.963455	33.078157
755.491601	36077.322652	33.083175
756.788250	36128.406375	33.088192
757.431177	36174.173677	33.093210
757.912292	36212.587323	33.098228
759.235021	36257.906903	33.103245
759.227592	36292.476849	33.108263
760.563741	36332.438777	33.113280
761.283347	36369.550727	33.118298
761.528964	36405.459683	33.123316
762.656224	36455.824582	33.128333
763.252839	36499.380392	33.133351
764.015196	36541.165126	33.138368
765.033897	36583.719175	33.143386
765.358135	36624.674780	33.148404
766.770212	36671.283840	33.153421
767.374633	36709.558932	33.158439
768.123401	36752.364256	33.163456
768.840016	36794.226205	33.168474
769.556658	36834.324028	33.173492
770.447153	36873.180623	33.178509
770.980413	36923.715526	33.183527
771.609718	36962.050407	33.188544
772.255617	37019.580496	33.193562
773.572714	37056.612726	33.198580
773.988407	37091.572988	33.203597
774.481550	37146.800332	33.208615
775.369002	37195.655298	33.213632
776.513697	37242.225274	33.218650
777.144423	37291.493743	33.223668
777.829314	37316.155587	33.228685
778.384470	37364.588715	33.233703
779.270987	37399.033108	33.238720
780.273818	37443.007816	33.243738
780.426810	37478.313375	33.248756
781.043340	37516.929485	33.253773
781.799501	37557.079387	33.258791
782.275407	37605.607675	33.263808
783.218109	37659.956530	33.268826
784.182248	37710.514346	33.273844
784.754961	37753.494685	33.278861
785.785630	37805.395554	33.283879
786.530130	37855.596043	33.288896
787.050007	37902.505595	33.293914
787.632263	37955.185291	33.298932
788.817719	38001.099200	33.303949
789.235201	38066.041249	33.308967
790.179284	38113.833386	33.313984
790.812430	38166.511953	33.319002
791.491475	38222.288410	33.324020
792.533861	38275.731569	33.329037
793.433916	38335.615759	33.334055
794.132944	38385.792987	33.339072
795.447982	38442.703559	33.344090
796.326325	38500.523729	33.349108
797.248086	38543.653351	33.354125
797.937333	38596.248299	33.359143
798.429591	38646.932801	33.364160
799.395053	38697.574941	33.369178
800.204656	38769.679557	33.374196
801.457854	38805.649760	33.379213
801.878925	38857.888935	33.384231
802.847525	38902.719395	33.389248
803.639720	38960.718711	33.394266
804.604824	39014.707016	33.399284
805.657544	39049.343046	33.404301
806.245211	39112.788111	33.409319
807.153024	39152.993132	33.414336
808.425657	39198.706227	33.419354
808.879878	39247.798120	33.424372
810.111854	39294.548600	33.429389
811.146547	39336.960156	33.434407
811.556251	39373.329001	33.439424
812.551252	39416.126371	33.444442
812.747116	39454.634753	33.449460
814.378337	39498.654395	33.454477
814.375415	39552.125270	33.459495
815.378944	39595.503478	33.464512
816.660965	39641.443709	33.469530
816.808800	39692.709496	33.474548
818.017479	39738.060622	33.479565
818.591680	39785.572877	33.484583
819.570781	39831.042361	33.489600
820.483744	39883.833078	33.494618
820.933456	39929.980142	33.499636
821.926284	39975.504697	33.504653
822.817302	40024.112550	33.509671
823.559100	40078.290257	33.514688
824.516807	40127.520325	33.519706
824.995876	40181.537052	33.524724
826.163760	40224.410136	33.529741
826.979812	40278.266822	33.534759
827.783015	40317.459522	33.539776
828.767681	40360.911783	33.544794
829.333794	40423.377455	33.549812
830.351568	40460.753343	33.554829
831.412388	40512.542157	33.559847
832.008645	40557.681000	33.564864
833.281042	40596.895599	33.569882
833.800546	40646.100592	33.574900
834.485971	40686.849236	33.579917
834.922047	40721.255630	33.584935
835.790734	40769.982487	33.589952
836.833326	40799.019429	33.594970
837.196152	40845.940975	33.599988
838.121966	40892.097743	33.605005
838.965970	40936.964569	33.610023
839.465924	40978.919160	33.615040
840.542829	41023.117243	33.620058
840.597011	41082.211764	33.625076
841.964667	41140.177385	33.630093
842.881448	41183.831655	33.635111
843.793892	41243.038877	33.640128
844.786761	41293.872524	33.645146
845.393665	41348.725944	33.650164
846.589282	41396.511234	33.655181
847.022515	41442.240324	33.660199
847.975377	41510.846709	33.665216
848.955449	41550.380761	33.670234
850.077511	41608.310184	33.675252
850.629698	41663.109712	33.680269
851.296264	41715.930798	33.685287
852.037310	41780.858576	33.690304
853.360234	41833.532895	33.695322
854.106885	41888.555526	33.700340
855.479122	41940.988366	33.705357
856.139971	41990.673907	33.710375
857.037508	42048.468881	33.715392
858.089155	42093.988647	33.720410
858.554406	42150.042672	33.725428
859.632122	42203.572184	33.730445
860.533660	42255.548190	33.735463
861.333487	42309.077198	33.740480
861.955991	42353.026548	33.745498
863.033088	42421.148280	33.750516
864.038727	42468.118111	33.755533
864.882033	42523.203095	33.760551
865.660810	42569.474970	33.765568
866.996764	42622.908142	33.770586
867.509459	42679.904835	33.775604
868.443042	42728.429809	33.780621
869.069905	42783.037006	33.785639
870.046815	42841.567988	33.790656
871.518303	42894.607419	33.795674
871.971355	42947.205564	33.800692
873.184557	42990.222454	33.805709
874.006908	43043.914172	33.810727
874.621876	43096.145762	33.815744
875.802001	43140.913862	33.820762
876.607622	43195.013376	33.825780
877.658020	43245.393443	33.830797
878.236548	43296.644485	33.835815
878.975245	43345.005249	33.840832
880.165257	43399.266456	33.845850
880.593691	43451.743150	33.850868
881.563042	43499.309107	33.855885
882.173293	43560.593961	33.860903
883.266189	43615.389576	33.865920
884.512927	43672.666055	33.870938
885.338763	43731.944134	33.875956
885.797004	43779.818435	33.880973
887.266931	43837.079368	33.885991
887.754084	43883.842431	33.891008
889.042888	43939.095224	33.896026
889.887686	43986.264254	33.901044
890.781560	44041.825832	33.906061
891.643683	44084.431745	33.911079
892.336266	44132.763495	33.916096
893.442807	44171.985155	33.921114
894.005273	44219.799806	33.926132
895.078823	44251.132610	33.931149
895.807968	44290.375619	33.936167
896.486995	44343.080850	33.941184
897.353374	44390.544658	33.946202
898.055444	44440.134365	33.951220
898.857272	44485.255392	33.956237
900.024302	44540.617307	33.961255
900.989431	44600.261748	33.966272
901.554735	44636.861637	33.971290
902.462985	44705.453297	33.976308
903.205174	44754.752771	33.981325
904.234376	44819.891043	33.986343
904.773481	44883.992931	33.991360
906.135618	44935.441335	33.996378
906.692455	44992.873521	34.001396
907.976011	45047.706070	34.006413
909.228646	45108.116540	34.011431
909.771559	45171.934001	34.016448
911.046500	45212.244454	34.021466
911.309720	45279.945736	34.026484
912.780857	45324.008471	34.031501
913.565949	45387.257261	34.036519
914.566286	45453.958042	34.041536
915.253948	45506.285118	34.046554
916.262008	45557.986498	34.051572
917.333077	45620.735709	34.056589
918.594455	45676.243814	34.061607
919.704309	45736.640383	34.066624
920.261745	45787.799241	34.071642
921.516965	45847.496476	34.076660
922.254651	45893.920876	34.081677
923.166499	45958.954319	34.086695
924.092046	46014.642364	34.091712
925.174680	46069.818851	34.096730
926.199673	46128.578683	34.101748
926.680908	46183.084169	34.106765
927.947527	46234.677038	34.111783
928.929460	46298.378352	34.116800
929.547431	46341.956727	34.121818
930.430580	46410.747318	34.126836
931.522989	46469.649311	34.131853
932.640227	46514.997064	34.136871
933.411830	46583.906867	34.141888
934.646297	46634.582076	34.146906
935.263368	46692.028153	34.151924
936.633660	46742.207876	34.156941
937.914260	46787.884866	34.161959
938.630230	46842.633544	34.166976
939.592206	46884.482665	34.171994
940.341185	46947.994547	34.177012
941.289399	47000.195734	34.182029
942.434871	47048.057981	34.187047
943.009502	47100.627881	34.192064
944.414887	47154.212882	34.197082
944.927534	47207.007828	34.202100
945.922288	47263.289120	34.207117
946.823483	47309.893278	34.212135
947.841894	47369.587344	34.217152
948.847074	47428.252444	34.222170
950.042678	47471.767862	34.227188
951.017452	47534.113616	34.232205
951.863474	47584.111592	34.237223
952.563258	47637.820873	34.242240
953.683706	47685.587166	34.247258
954.452550	47731.396806	34.252276
955.367274	47778.524904	34.257293
956.455885	47821.241636	34.262311
957.038402	47872.306392	34.267328
957.932029	47914.383222	34.272346
959.197718	47960.514100	34.277364
960.104206	48015.994965	34.282381
960.994367	48057.724645	34.287399
962.035791	48101.195823	34.292416
962.707196	48161.458756	34.297434
963.432716	48209.756154	34.302452
964.266972	48267.494875	34.307469
965.472043	48325.359153	34.312487
966.225539	48377.891352	34.317504
967.270389	48433.047893	34.322522
968.179538	48481.563856	34.327540
969.203654	48548.984966	34.332557
970.226333	48611.984149	34.337575
971.003636	48670.662831	34.342592
971.865327	48729.467638	34.347610
973.396554	48796.095161	34.352628
974.172308	48848.441484	34.357645
974.825342	48909.000299	34.362663
976.079291	48977.544487	34.367680
977.097855	49032.086568	34.372698
978.334413	49097.192061	34.377716
979.099984	49156.620392	34.382733
980.321330	49222.949704	34.387751
981.198708	49298.171700	34.392768
982.361732	49345.789296	34.397786
983.363171	49400.265341	34.402804
983.910642	49467.434791	34.407821
985.204132	49526.642232	34.412839
986.186826	49592.851809	34.417856
987.024689	49655.180512	34.422874
988.022549	49711.277560	34.427892
989.341938	49777.194526	34.432909
990.308319	49836.099671	34.437927
991.412252	49898.855576	34.442944
992.706259	49948.105274	34.447962
993.722187	50000.789922	34.452980
994.593314	50057.692216	34.457997
995.699969	50110.324947	34.463015
996.571599	50171.396999	34.468032
997.724630	50234.886408	34.473050
999.053302	50281.511962	34.478068
999.665779	50345.560845	34.483085
1000.462411	50397.198793	34.488103
1001.649912	50467.877443	34.493120
1002.614759	50519.229912	34.498138
1003.553244	50576.464611	34.503156
1004.269450	50634.246761	34.508173
1005.543214	50690.625690	34.513191
1006.409115	50755.509194	34.518208
1007.532128	50809.950563	34.523226
1008.789897	50872.140890	34.528244
1009.687848	50930.123107	34.533261
1011.004172	50991.292216	34.538279
1011.724780	51039.039537	34.543296
1013.045896	51095.810666	34.548314
1014.205837	51146.108951	34.553332
1015.137178	51209.148543	34.558349
1015.941827	51254.769802	34.563367
1017.109170	51317.380439	34.568384
1017.791433	51382.971489	34.573402
1019.338385	51427.046865	34.578420
1020.036541	51484.511265	34.583437
1020.800110	51537.106056	34.588455
1021.966754	51595.155438	34.593472
1023.128732	51635.899947	34.598490
1023.972040	51686.805804	34.603508
1025.040300	51733.171345	34.608525
1026.138230	51778.241514	34.613543
1026.857656	51828.894993	34.618560
1027.533963	51872.506414	34.623578
1028.310496	51935.344426	34.628596
1029.612250	51994.525275	34.633613
1030.562768	52043.864865	34.638631
1031.659594	52097.225012	34.643648
1032.935862	52143.799257	34.648666
1033.866804	52197.501989	34.653684
1034.566093	52256.246307	34.658701
1035.602362	52315.982084	34.663719
1036.616333	52375.613934	34.668736
1037.446214	52432.857566	34.673754
1038.835264	52498.992861	34.678772
1039.977644	52567.527220	34.683789
1041.196159	52617.509465	34.688807
1042.074415	52679.074328	34.693824
1043.126108	52737.707735	34.698842
1044.161624	52801.190936	34.703860
1045.243961	52872.507179	34.708877
1046.452042	52926.225149	34.713895
1047.407512	52989.044312	34.718912
1048.652435	53045.205677	34.723930
1049.634569	53111.039397	34.728948
1050.565213	53168.939816	34.733965
1051.895545	53228.448378	34.738983
1053.047154	53290.288450	34.744000
1053.957268	53354.457222	34.749018
1055.050595	53412.503628	34.754036
1056.016875	53483.023590	34.759053
1057.187942	53534.806054	34.764071
1058.135062	53600.671944	34.769088
1059.395213	53665.210742	34.774106
1060.531486	53719.549270	34.779124
1061.442404	53781.751053	34.784141
1062.659441	53844.847962	34.789159
1063.624998	53906.573241	34.794176
1064.661145	53972.027562	34.799194
1066.226195	54036.551285	34.804212
1067.032207	54096.644064	34.809229
1068.183819	54153.499808	34.814247
1069.389755	54212.656980	34.819264
1070.386918	54271.435652	34.824282
1071.505885	54337.295685	34.829300
1072.528895	54384.818986	34.834317
1073.649578	54444.692524	34.839335
1074.811200	54508.698503	34.844352
1075.832921	54566.145125	34.849370
1076.989039	54627.424791	34.854388
1077.423584	54686.222969	34.859405
1079.158380	54742.988832	34.864423
1080.271695	54801.332969	34.869440
1081.271835	54862.441485	34.874458
1082.634538	54902.780564	34.879476
1083.718298	54972.976503	34.884493
1084.815274	55020.622401	34.889511
1086.076663	55077.444201	34.894528
1086.911450	55128.744904	34.899546
1088.187690	55176.533919	34.904564
1089.128355	55228.527050	34.909581
1090.111806	55280.532582	34.914599
1091.495867	55334.184205	34.919616
1092.640850	55383.089019	34.924634
1093.846700	55422.510595	34.929652
1094.554748	55489.551993	34.934669
1095.606958	55531.383667	34.939687
1096.567709	55570.799562	34.944704
1097.132966	55624.567378	34.949722
1098.626668	55671.044973	34.954740
1099.938425	55723.639266	34.959757
1100.829410	55756.845371	34.964775
1102.078107	55806.146181	34.969792
1102.734191	55856.761302	34.974810
1103.971903	55901.393490	34.979828
1104.684979	55963.613002	34.984845
1105.363802	56019.515680	34.989863
1106.425679	56067.074247	34.994880
1107.822038	56135.066597	34.999898
1109.076177	56193.354140	35.004916
1109.616274	56259.670882	35.009933
1111.104062	56326.769769	35.014951
1112.362944	56395.398275	35.019968
1113.066525	56450.867729	35.024986
1114.123332	56511.661507	35.030004
1115.554349	56586.573446	35.035021
1116.650949	56653.392738	35.040039
1117.808738	56728.594724	35.045056
1118.823408	56794.148802	35.050074
1120.303243	56858.370783	35.055092
1121.290519	56922.397906	35.060109
1122.362638	56990.937112	35.065127
1123.802895	57050.931742	35.070144
1124.981624	57120.036892	35.075162
1126.248284	57179.312203	35.080180
1127.495848	57243.679174	35.085197
1128.985345	57289.141618	35.090215
1130.452537	57349.556825	35.095232
1131.313166	57408.915258	35.100250
1132.851856	57460.566472	35.105268
1134.033187	57515.545879	35.110285
1135.408184	57566.014092	35.115303
1136.416732	57615.609403	35.120320
1137.395777	57682.500601	35.125338
1138.303271	57717.441032	35.130356
1139.303819	57778.765823	35.135373
1140.433159	57831.133823	35.140391
1141.576446	57897.772057	35.145408
1142.490478	57955.376625	35.150426
1144.006772	58011.994624	35.155444
1144.756262	58075.669637	35.160461
1145.566343	58134.309912	35.165479
1147.137333	58192.128658	35.170496
1147.794290	58257.654124	35.175514
1149.212379	58342.573829	35.180532
1150.461276	58393.816709	35.185549
1151.454330	58457.353329	35.190567
1153.272942	58517.286061	35.195584
1154.075738	58590.568363	35.200602
1155.316803	58639.471126	35.205620
1156.601518	58700.886691	35.210637
1157.522601	58765.612655	35.215655
1159.033161	58823.606941	35.220672
1160.258707	58891.564219	35.225690
1161.278675	58947.401312	35.230708
1162.541250	59005.428528	35.235725
1163.355111	59068.273245	35.240743
1164.405367	59117.339766	35.245760
1165.406828	59174.098056	35.250778
1166.829702	59232.069071	35.255796
1167.906523	59300.316620	35.260813
1169.166169	59372.029659	35.265831
1170.226484	59432.444159	35.270848
1171.092008	59496.997214	35.275866
1172.670159	59556.824588	35.280884
1173.924918	59610.841500	35.285901
1174.740065	59668.199779	35.290919
1176.286902	59707.252213	35.295936
1176.856062	59770.896613	35.300954
1178.272533	59821.192149	35.305972
1179.081608	59880.406476	35.310989
1179.945575	59937.827374	35.316007
1181.217242	59993.830019	35.321024
1182.647868	60065.784185	35.326042
1183.545196	60120.187330	35.331060
1184.692120	60181.356031	35.336077
1186.023855	60251.515910	35.341095
1187.379970	60318.969344	35.346112
1188.412870	60376.333178	35.351130
1189.506778	60438.612213	35.356148
1190.931718	60501.839702	35.361165
1192.245729	60567.521723	35.366183
1193.538652	60636.676003	35.371200
1194.652336	60705.067300	35.376218
1195.773264	60762.855023	35.381236
1197.312777	60831.515496	35.386253
1198.368421	60892.548348	35.391271
1199.980089	60960.216742	35.396288
1201.037302	61026.313664	35.401306
1202.163987	61086.430687	35.406324
1203.445861	61148.985944	35.411341
1204.555299	61213.935790	35.416359
1206.055319	61265.341640	35.421376
1206.977511	61335.207924	35.426394
1208.329572	61403.316976	35.431412
1209.481067	61465.102187	35.436429
1210.433414	61528.906388	35.441447
1212.201581	61606.920810	35.446464
1213.093038	61672.482035	35.451482
1214.404788	61729.216674	35.456500
1215.300782	61799.063054	35.461517
1217.091011	61873.061524	35.466535
1218.321094	61942.577480	35.471552
1219.270351	62009.637147	35.476570
1220.663052	62072.373639	35.481588
1222.025428	62138.976508	35.486605
1223.082521	62200.392192	35.491623
1224.557221	62258.400251	35.496640
1225.646523	62342.777623	35.501658
1226.790342	62405.490620	35.506676
1227.663939	62467.745978	35.511693
1228.928728	62529.952914	35.516711
1230.361977	62607.263285	35.521728
1232.064739	62678.315234	35.526746
1233.107824	62738.164503	35.531764
1234.420487	62805.391000	35.536781
1235.432545	62874.817097	35.541799
1237.170384	62934.760655	35.546816
1238.160546	62998.518414	35.551834
1239.558769	63067.694683	35.556852
1240.935075	63129.512166	35.561869
1241.824628	63194.843488	35.566887
1243.493259	63257.755028	35.571904
1244.021006	63320.712383	35.576922
1245.782082	63382.103087	35.581940
1246.911841	63443.048339	35.586957
1248.290208	63505.151311	35.591975
1249.917686	63563.974153	35.596992
1250.677367	63632.631550	35.602010
1251.984937	63690.916019	35.607028
1253.491938	63745.010144	35.612045
1254.339064	63815.262348	35.617063
1255.670205	63871.213850	35.622080
1256.662452	63929.700177	35.627098
1257.881268	63990.835410	35.632116
1258.861824	64035.282215	35.637133
1260.207238	64082.976647	35.642151
1261.547295	64146.138121	35.647168
1262.676683	64198.108219	35.652186
1263.923582	64255.662801	35.657204
1265.183275	64308.302789	35.662221
1266.465598	64380.261086	35.667239
1267.813937	64437.705245	35.672256
1268.587659	64503.817828	35.677274
1269.432056	64570.191749	35.682292
1270.998663	64637.478397	35.687309
1272.351351	64714.693958	35.692327
1273.541434	64775.386109	35.697344
1274.697494	64849.043217	35.702362
1276.227915	64919.058601	35.707380
1277.830984	65000.477605	35.712397
1278.711222	65065.840594	35.717415
1280.348012	65137.106138	35.722432
1281.726878	65212.888317	35.727450
1282.751250	65283.148539	35.732468
1284.043612	65342.578826	35.737485
1285.505794	65420.944335	35.742503
1286.725296	65486.666829	35.747520
1287.769160	65562.331559	35.752538
1289.421250	65641.889937	35.757556
1291.259051	65708.193654	35.762573
1292.296948	65776.901994	35.767591
1293.377511	65846.813103	35.772608
1294.991366	65922.870858	35.777626
1296.628019	65985.211783	35.782644
1298.008146	66052.677024	35.787661
1299.199130	66128.238110	35.792679
1300.999881	66191.338934	35.797696
1302.193173	66241.226582	35.802714
1303.486219	66304.711068	35.807732
1305.005569	66369.337918	35.812749
1305.774548	66439.210798	35.817767
1307.433504	66495.870257	35.822784
1308.766028	66566.566990	35.827802
1309.960582	66633.398030	35.832820
1311.117706	66700.197116	35.837837
1312.328344	66764.594715	35.842855
1313.784764	66822.622544	35.847872
1315.375828	66887.771331	35.852890
1316.528830	66952.976195	35.857908
1318.194600	67022.020162	35.862925
1319.052498	67095.407573	35.867943
1320.358720	67153.428011	35.872960
1321.853934	67221.384866	35.877978
1322.935321	67290.837616	35.882996
1324.140130	67348.956684	35.888013
1325.246749	67420.925811	35.893031
1327.371696	67493.539852	35.898048
1328.489978	67557.719642	35.903066
1329.616257	67622.278241	35.908084
1331.006407	67683.940113	35.913101
1332.244226	67757.941113	35.918119
1333.708749	67818.141710	35.923136
1335.021106	67887.338316	35.928154
1336.180980	67950.227240	35.933172
1337.606016	68020.141048	35.938189
1338.905186	68099.401450	35.943207
1340.552116	68155.268682	35.948224
1342.002747	68228.737517	35.953242
1343.267850	68286.633996	35.958260
1344.072903	68346.666797	35.963277
1345.257156	68406.975968	35.968295
1347.059574	68461.559491	35.973312
1348.099453	68510.538478	35.978330
1349.278741	68575.661048	35.983348
1350.451848	68624.739704	35.988365
1351.316736	68702.088059	35.993383
1353.161362	68756.330010	35.998400
1354.382296	68821.326376	36.003418
1355.483914	68885.986992	36.008436
1356.789488	68952.249496	36.013453
1358.254842	69028.808319	36.018471
1359.470303	69089.310496	36.023488
1360.943673	69168.394954	36.028506
1362.279975	69251.211693	36.033524
1363.975826	69321.156298	36.038541
1365.360214	69391.384134	36.043559
1366.625720	69453.943593	36.048576
1368.207905	69522.633783	36.053594
1369.403539	69596.216085	36.058612
1371.233992	69669.667567	36.063629
1372.397183	69746.161834	36.068647
1373.645751	69814.265469	36.073664
1375.025469	69882.342422	36.078682
1376.740822	69960.441590	36.083700
1378.195465	70022.979150	36.088717
1379.063368	70104.453512	36.093735
1380.488843	70176.697036	36.098752
1382.296873	70249.121507	36.103770
1383.550331	70331.258110	36.108788
1384.947862	70402.607447	36.113805
1386.548261	70476.078224	36.118823
1388.021130	70561.309391	36.123840
1389.327789	70621.097973	36.128858
1390.674609	70703.943028	36.133876
1392.132698	70768.837498	36.138893
1393.276387	70845.395039	36.143911
1395.031765	70925.593210	36.148928
1396.677832	70991.446673	36.153946
1397.944764	71062.324324	36.158964
1399.682447	71124.161645	36.163981
1401.040485	71207.969084	36.168999
1402.489289	71274.791353	36.174016
1404.337565	71343.362378	36.179034
1405.607872	71417.495400	36.184052
1406.968837	71469.260378	36.189069
1408.185768	71545.086585	36.194087
1409.266817	71601.531110	36.199104
1411.094531	71670.435507	36.204122
1412.288766	71748.634263	36.209140
1413.517194	71816.176335	36.214157
1414.556265	71900.213227	36.219175
1416.341065	71968.466523	36.224192
1418.139013	72038.453106	36.229210
1419.348013	72117.359913	36.234228
1420.714205	72183.842794	36.239245
1422.057272	72257.827476	36.244263
1423.763479	72326.182662	36.249280
1425.183619	72401.561565	36.254298
1426.277921	72468.733671	36.259316
1427.736596	72536.431535	36.264333
1429.583631	72611.832879	36.269351
1431.178086	72675.089506	36.274368
1432.329830	72744.609154	36.279386
1433.827057	72822.738338	36.284404
1435.400840	72879.159139	36.289421
1436.963679	72950.603522	36.294439
1438.142009	73018.713815	36.299456
1439.783597	73073.566509	36.304474
1440.628292	73141.273364	36.309492
1441.984325	73186.152195	36.314509
1443.160600	73251.109570	36.319527
1444.344187	73317.826544	36.324544
1445.695311	73366.974916	36.329562
1446.806295	73441.936528	36.334580
1448.372910	73509.024677	36.339597
1449.821942	73591.596828	36.344615
1451.335747	73666.128701	36.349632
1452.405036	73740.971019	36.354650
1453.952505	73817.144661	36.359668
1455.606181	73881.256208	36.364685
1456.971079	73962.031389	36.369703
1458.602257	74038.876548	36.374720
1460.248891	74117.150818	36.379738
1461.255273	74199.857469	36.384756
1462.876412	74275.311567	36.389773
1464.692627	74364.326566	36.394791
1466.283692	74443.547816	36.399808
1467.719285	74507.163005	36.404826
1469.271482	74592.217432	36.409844
1470.703226	74662.711598	36.414861
1472.255086	74750.641923	36.419879
1473.506612	74829.182788	36.424896
1475.455812	74901.889279	36.429914
1477.445345	74980.137738	36.434932
1478.759293	75051.094703	36.439949
1480.478333	75133.540688	36.444967
1481.720088	75206.738743	36.449984
1483.519685	75274.618215	36.455002
1484.852356	75353.021242	36.460020
1486.288212	75424.998810	36.465037
1487.903044	75490.209661	36.470055
1489.380075	75564.334564	36.475072
1491.048431	75629.841387	36.480090
1492.618115	75707.435651	36.485108
1494.285446	75775.476430	36.490125
1495.810486	75857.954998	36.495143
1497.153691	75913.303588	36.500160
1499.089763	75987.737825	36.505178
1500.144288	76056.863280	36.510196
1501.616841	76129.787038	36.515213
1503.257307	76199.568524	36.520231
1504.856137	76269.914076	36.525248
1506.430421	76337.666816	36.530266
1508.012959	76416.084491	36.535284
1509.122319	76479.489387	36.540301
1510.655874	76549.047825	36.545319
1511.877868	76628.105253	36.550336
1513.702497	76690.853984	36.555354
1514.998904	76774.536555	36.560372
1516.438705	76849.836236	36.565389
1517.762390	76932.438265	36.570407
1519.653801	77005.666186	36.575424
1521.766552	77071.943024	36.580442
1523.045811	77156.414859	36.585460
1524.121412	77224.589898	36.590477
1526.203837	77288.693132	36.595495
1527.149533	77375.371401	36.600512
1528.756647	77441.170888	36.605530
1530.170390	77517.933315	36.610548
1531.591243	77597.735184	36.615565
1533.300551	77670.828711	36.620583
1534.396682	77746.324008	36.625600
1536.153953	77822.666148	36.630618
1537.889154	77913.441056	36.635636
1539.111042	77986.586380	36.640653
1540.638025	78055.959669	36.645671
1542.169905	78115.134373	36.650688
1543.639609	78181.881938	36.655706
1545.526061	78252.592982	36.660724
1546.476406	78314.646179	36.665741
1548.081940	78383.919326	36.670759
1549.287319	78450.987621	36.675776
1550.781229	78523.737084	36.680794
1552.145866	78610.670400	36.685812
1553.834614	78682.135601	36.690829
1555.356173	78760.860932	36.695847
1556.598122	78845.825220	36.700864
1558.476893	78918.350798	36.705882
1559.706595	79004.140954	36.710900
1561.592087	79089.144624	36.715917
1563.114849	79172.913111	36.720935
1564.356195	79263.060316	36.725952
1566.455481	79339.973916	36.730970
1568.110833	79429.334740	36.735988
1569.703352	79508.608530	36.741005
1571.622348	79590.162543	36.746023
1572.892545	79689.960394	36.751040
1574.194886	79771.180706	36.756058
1576.160323	79864.257116	36.761076
1577.753611	79946.864016	36.766093
1579.662899	80021.262747	36.771111
1581.016957	80109.925438	36.776128
1583.001278	80186.922731	36.781146
1584.343598	80274.536235	36.786164
1585.932495	80358.297951	36.791181
1587.951818	80436.088624	36.796199
1589.604869	80521.791875	36.801216
1591.207312	80603.981203	36.806234
1593.011963	80680.551882	36.811252
1594.444894	80763.401683	36.816269
1596.199224	80836.344513	36.821287
1597.454112	80929.142935	36.826304
1599.435036	80997.743060	36.831322
1601.238287	81084.159368	36.836340
1602.605727	81162.307485	36.841357
1604.454686	81236.262795	36.846375
1605.893117	81310.003816	36.851392
1607.743421	81389.952122	36.856410
1609.098888	81463.681192	36.861428
1610.943242	81556.022008	36.866445
1612.801955	81632.181396	36.871463
1613.683141	81714.638905	36.876480
1615.949699	81791.330381	36.881498
1617.080401	81865.868553	36.886516
1618.611302	81960.084236	36.891533
1620.727281	82034.937445	36.896551
1622.143836	82119.035482	36.901568
1623.716966	82188.804646	36.906586
1625.150884	82267.971716	36.911604
1627.214775	82344.088250	36.916621
1628.925169	82422.262215	36.921639
1630.445317	82501.517807	36.926656
1632.120524	82578.975506	36.931674
1633.884561	82661.627038	36.936692
1635.294695	82742.370286	36.941709
1637.040563	82818.727928	36.946727
1638.698989	82897.519522	36.951744
1639.909283	82972.250882	36.956762
1641.625465	83059.333074	36.961780
1643.330408	83138.308115	36.966797
1645.134720	83221.677201	36.971815
1646.648793	83309.450664	36.976832
1648.429232	83381.116264	36.981850
1650.070801	83448.964549	36.986868
1651.488677	83511.006788	36.991885
1653.067034	83580.702539	36.996903
1654.613986	83639.063000	37.001920
1656.152236	83711.831686	37.006938
1658.105293	83780.404934	37.011956
1659.222169	83845.130550	37.016973
1660.417008	83914.798444	37.021991
1662.042777	83988.567813	37.027008
1663.679791	84071.788178	37.032026
1665.848704	84148.247907	37.037044
1666.952318	84238.724042	37.042061
1668.608054	84317.355262	37.047079
1670.203161	84405.575574	37.052096
1672.015107	84482.788976	37.057114
1673.753503	84566.108952	37.062132
1675.202925	84655.100433	37.067149
1677.230891	84744.584526	37.072167
1679.080485	84827.279636	37.077184
1680.459958	84905.727621	37.082202
1682.435156	85002.088657	37.087220
1684.193729	85093.542051	37.092237
1685.846427	85179.398836	37.097255
1687.334110	85277.877200	37.102272
1688.948447	85368.048870	37.107290
1691.024140	85458.541440	37.112308
1692.585006	85555.653435	37.117325
1694.591925	85637.553279	37.122343
1695.925326	85741.075354	37.127360
1697.789348	85826.318090	37.132378
1699.830807	85917.742495	37.137396
1701.742912	86003.079601	37.142413
1703.071173	86097.568728	37.147431
1704.956679	86184.405814	37.152448
1706.763368	86272.332611	37.157466
1708.602146	86366.856766	37.162484
1709.957836	86454.892712	37.167501
1712.336012	86536.990439	37.172519
1713.820021	86644.509212	37.177536
1715.347557	86732.721858	37.182554
1717.299750	86815.393922	37.187572
1719.248043	86899.004577	37.192589
1721.037635	86985.580275	37.197607
1722.509076	87090.327430	37.202624
1724.568919	87170.081692	37.207642
1726.714285	87248.365464	37.212660
1728.560714	87333.133819	37.217677
1730.297682	87414.257209	37.222695
1731.515979	87498.693479	37.227712
1733.375914	87581.990432	37.232730
1734.841495	87657.657089	37.237748
1736.382692	87755.108980	37.242765
1738.203520	87841.644304	37.247783
1740.085718	87934.899472	37.252800
1741.642438	88025.113728	37.257818
1743.735365	88109.414878	37.262836
1745.337454	88207.745832	37.267853
1747.310923	88293.320810	37.272871
1748.439796	88379.927986	37.277888
1750.422770	88466.832632	37.282906
1752.331873	88551.379254	37.287924
1754.083680	88644.657074	37.292941
1756.226521	88727.760922	37.297959
1757.725293	88816.770056	37.302976
1759.546125	88905.412230	37.307994
1761.502680	88994.464317	37.313012
1763.011549	89084.499199	37.318029
1764.656108	89167.669587	37.323047
1766.091586	89244.460266	37.328064
1767.430711	89315.499884	37.333082
1769.501238	89389.479478	37.338100
1770.822607	89464.146794	37.343117
1772.382651	89546.038787	37.348135
1774.300565	89637.113915	37.353152
1776.058142	89721.826997	37.358170
1777.881075	89799.699086	37.363188
1778.905709	89885.427149	37.368205
1780.410010	89978.823933	37.373223
1782.242116	90076.402690	37.378240
1783.714981	90175.761598	37.383258
1785.662160	90280.154103	37.388276
1787.826205	90384.094802	37.393293
1789.835987	90488.072676	37.398311
1791.661984	90576.896449	37.403328
1793.585743	90676.934213	37.408346
1795.126827	90782.862185	37.413364
1796.728701	90893.242242	37.418381
1798.486319	90991.215851	37.423399
1800.467211	91106.581622	37.428416
1802.223220	91216.469804	37.433434
1804.355290	91318.695066	37.438452
1806.263722	91428.484123	37.443469
1808.139918	91530.281199	37.448487
1810.047012	91635.483156	37.453504
1811.944211	91741.954456	37.458522
1813.919164	91834.510219	37.463540
1815.837014	91948.520242	37.468557
1817.168626	92044.751496	37.473575
1819.419534	92145.693516	37.478592
1821.527058	92258.965254	37.483610
1823.479807	92360.727792	37.488628
1825.220170	92464.767309	37.493645
1826.947500	92562.104338	37.498663
1829.053589	92663.298883	37.503680
1830.996122	92774.849255	37.508698
1832.937844	92855.258272	37.513716
1834.818104	92965.830456	37.518733
1836.820940	93060.045985	37.523751
1838.724702	93167.281738	37.528768
1840.532762	93258.777910	37.533786
1842.852388	93351.436449	37.538804
1844.153117	93454.546812	37.543821
1846.283773	93544.092105	37.548839
1848.013550	93650.710348	37.553856
1850.048190	93747.191855	37.558874
1852.038150	93833.794032	37.563892
1853.927767	93941.985344	37.568909
1855.371461	94024.782253	37.573927
1857.451691	94141.601626	37.578944
1859.102434	94229.500176	37.583962
1861.053010	94319.075907	37.588980
1862.728776	94420.444994	37.593997
1864.819843	94521.356487	37.599015
1866.550650	94628.396240	37.604032
1868.040183	94724.598518	37.609050
1870.204290	94831.926086	37.614068
1871.759965	94947.423599	37.619085
1873.316398	95044.592422	37.624103
1875.604604	95152.066462	37.629120
1877.043712	95250.826076	37.634138
1879.222076	95360.054600	37.639156
1880.846902	95476.836187	37.644173
1882.641072	95582.627082	37.649191
1884.822319	95695.278815	37.654208
1886.476711	95800.078247	37.659226
1888.360292	95896.818257	37.664244
1890.096620	96007.905535	37.669261
1891.765491	96109.737544	37.674279
1893.813206	96196.502073	37.679296
1895.302911	96294.927491	37.684314
1897.353420	96385.241431	37.689332
1898.907472	96486.712346	37.694349
1900.733617	96579.394380	37.699367
1902.152686	96684.487117	37.704384
1904.078432	96803.837885	37.709402
1906.010855	96906.417171	37.714420
1907.733066	97030.503593	37.719437
1909.873395	97146.957203	37.724455
1911.826588	97255.606420	37.729472
1913.334704	97383.974373	37.734490
1915.407405	97501.086377	37.739508
1917.588085	97625.952730	37.744525
1919.266937	97754.054608	37.749543
1921.104014	97863.243826	37.754560
1922.853148	97995.062653	37.759578
1925.002177	98122.509310	37.764596
1927.215071	98256.132831	37.769613
1928.909136	98375.563802	37.774631
1931.446335	98500.187646	37.779648
1932.628133	98638.943512	37.784666
1934.847097	98763.187157	37.789684
1937.224158	98890.842067	37.794701
1939.094137	99032.585189	37.799719
1941.052086	99150.000109	37.804736
1942.703761	99290.536154	37.809754
1945.064042	99413.505150	37.814772
1947.073319	99540.231354	37.819789
1948.598503	99677.327937	37.824807
1951.122718	99800.779861	37.829824
1952.874256	99939.984647	37.834842
1955.288436	100071.568494	37.839860
1957.270334	100200.139834	37.844877
1959.213479	100326.790730	37.849895
1961.024852	100454.438930	37.854912
1962.667489	100589.200958	37.859930
1965.293992	100723.949053	37.864948
1967.202234	100843.685288	37.869965
1969.273529	100982.007766	37.874983
1972.010976	101101.057367	37.880000
1973.503245	101226.628615	37.885018
1975.388030	101352.405169	37.890036
1977.655853	101472.746713	37.895053
1979.878352	101599.561701	37.900071
1981.858498	101715.283555	37.905088
1984.170792	101844.443604	37.910106
1986.156883	101962.181257	37.915124
1987.796140	102081.228767	37.920141
1989.876565	102205.177644	37.925159
1991.905076	102309.026965	37.930176
1993.775540	102437.878125	37.935194
1995.729744	102554.786102	37.940212
1997.871471	102677.243765	37.945229
1999.814353	102797.007073	37.950247
2001.743731	102919.194569	37.955264
2003.863068	103045.524121	37.960282
2005.700560	103166.243487	37.965300
2008.027706	103293.898107	37.970317
2010.100623	103414.277245	37.975335
2011.764660	103537.294631	37.980352
2013.338452	103661.987547	37.985370
2015.183268	103801.929506	37.990388
2017.175642	103918.519341	37.995405
2018.975873	104064.758231	38.000423
2021.006173	104196.291874	38.005440
2022.794853	104332.872161	38.010458
2024.031997	104442.405512	38.015476
2025.994732	104568.334242	38.020493
2027.805091	104693.184176	38.025511
2029.854267	104817.388592	38.030528
2031.692661	104953.202854	38.035546
2033.607354	105085.937268	38.040564
2035.048217	105231.438652	38.045581
2037.207524	105371.857813	38.050599
2039.165425	105514.629462	38.055616
2040.595617	105666.867330	38.060634
2042.523888	105831.809240	38.065652
2044.932594	105985.581853	38.070669
2047.069621	106148.742811	38.075687
2049.304266	106310.278913	38.080704
2051.100308	106463.756467	38.085722
2053.489958	106629.061173	38.090740
2055.773038	106788.930862	38.095757
2057.368084	106949.593685	38.100775
2059.416685	107114.015756	38.105792
2061.619318	107280.227809	38.110810
2063.624876	107450.022029	38.115828
2066.074576	107614.789512	38.120845
2068.344840	107784.594686	38.125863
2070.734811	107950.970874	38.130880
2072.589467	108109.036998	38.135898
2074.693375	108279.834366	38.140916
2076.749084	108447.254338	38.145933
2078.867532	108612.395423	38.150951
2081.465988	108775.610772	38.155968
2083.474660	108949.520482	38.160986
2085.461348	109122.496100	38.166004
2088.210031	109282.748313	38.171021
2089.820952	109436.826006	38.176039
2092.354769	109593.042601	38.181056
2094.967529	109763.869073	38.186074
2096.891512	109916.416179	38.191092
2099.431298	110079.456574	38.196109
2101.242975	110227.647514	38.201127
2103.630385	110380.923057	38.206144
2105.773866	110538.929614	38.211162
2107.660025	110691.701579	38.216180
2110.236561	110855.855795	38.221197
2111.919357	111013.923868	38.226215
2113.605540	111175.619110	38.231232
2115.939753	111334.449051	38.236250
2117.696685	111499.076884	38.241268
2119.872427	111670.665765	38.246285
2121.696344	111837.542069	38.251303
2124.188842	112004.593554	38.256320
2126.212385	112182.917534	38.261338
2127.970426	112365.392980	38.266356
2130.188388	112526.681390	38.271373
2131.951997	112700.254704	38.276391
2133.925391	112889.560258	38.281408
2136.372468	113072.552917	38.286426
2138.438440	113244.940117	38.291444
2140.945785	113410.816326	38.296461
2142.879868	113601.983414	38.301479
2144.702227	113783.213050	38.306496
2146.902608	113973.554097	38.311514
2149.293567	114142.444990	38.316532
2151.393844	114323.874805	38.321549
2153.758486	114509.627099	38.326567
2155.237346	114685.093467	38.331584
2157.668280	114868.478163	38.336602
2159.871160	115051.518960	38.341620
2161.877231	115226.182484	38.346637
2164.217482	115407.795720	38.351655
2166.200020	115581.196277	38.356672
2167.935544	115732.909638	38.361690
2170.083019	115892.105818	38.366708
2172.432696	116055.925890	38.371725
2174.891403	116220.934565	38.376743
2176.833058	116382.498822	38.381760
2178.896411	116552.327175	38.386778
2180.637349	116725.428409	38.391796
2182.853574	116893.966023	38.396813
2184.691431	117075.640636	38.401831
2186.843452	117263.291833	38.406848
2189.032208	117443.239049	38.411866
2190.880962	117643.445984	38.416884
2193.439413	117829.501646	38.421901
2195.138147	118032.359722	38.426919
2197.336943	118230.028901	38.431936
2199.424647	118439.791944	38.436954
2201.379335	118635.877835	38.441972
2203.700100	118848.752393	38.446989
2205.634644	119068.347931	38.452007
2207.921702	119265.285655	38.457024
2210.500223	119479.962663	38.462042
2212.405242	119699.071731	38.467060
2214.909962	119923.529999	38.472077
2216.984459	120149.274628	38.477095
2219.183709	120359.931350	38.482112
2221.401172	120583.943681	38.487130
2223.418496	120812.605987	38.492148
2226.150900	121028.256959	38.497165
2228.336589	121247.648001	38.502183
2230.995898	121471.241124	38.507200
2233.432334	121691.762478	38.512218
2235.724505	121921.935891	38.517236
2238.219089	122129.638310	38.522253
2240.412655	122356.899340	38.527271
2242.530856	122570.599819	38.532288
2245.012532	122793.911107	38.537306
2247.259682	123014.063524	38.542324
2249.417768	123228.585884	38.547341
2251.780794	123447.174894	38.552359
2254.110235	123668.979913	38.557376
2256.058076	123885.048327	38.562394
2258.606160	124115.587689	38.567412
2260.677222	124334.430195	38.572429
2263.500966	124574.748191	38.577447
2265.632423	124785.362984	38.582464
2267.543442	125004.805049	38.587482
2270.116863	125235.143859	38.592500
2272.306535	125451.449240	38.597517
2274.969556	125683.514631	38.602535
2277.389399	125905.875999	38.607552
2279.332247	126128.503499	38.612570
2281.711256	126359.538782	38.617588
2284.334981	126575.287413	38.622605
2286.277649	126788.466771	38.627623
2288.600728	127013.437412	38.632640
2291.113508	127237.998985	38.637658
2292.897112	127462.307921	38.642676
2295.432002	127681.260700	38.647693
2297.511868	127920.052653	38.652711
2299.738493	128136.607396	38.657728
2301.742295	128368.423059	38.662746
2303.801025	128601.601662	38.667764
2306.556509	128831.729035	38.672781
2308.156402	129065.540241	38.677799
2310.695257	129301.185133	38.682816
2312.899835	129524.931721	38.687834
2314.925158	129768.487919	38.692852
2317.476416	129981.233040	38.697869
2320.105051	130196.771165	38.702887
2322.455558	130403.167730	38.707904
2324.553008	130607.371769	38.712922
2326.575435	130816.295830	38.717940
2328.792837	131035.518635	38.722957
2330.885173	131265.229977	38.727975
2333.129485	131477.459553	38.732992
2335.580574	131711.887971	38.738010
2337.539594	131939.250999	38.743028
2339.765464	132173.374545	38.748045
2341.774589	132414.410499	38.753063
2344.231175	132658.397695	38.758080
2346.827643	132896.146856	38.763098
2349.329791	133151.689148	38.768116
2351.465378	133383.612717	38.773133
2353.684689	133638.960981	38.778151
2356.192041	133891.626326	38.783168
2358.737324	134132.968456	38.788186
2361.145100	134391.920649	38.793204
2363.628336	134640.216225	38.798221
2365.892393	134897.658419	38.803239
2367.963183	135162.606393	38.808256
2370.552375	135414.239672	38.813274
2372.935282	135678.215507	38.818292
2375.043516	135937.236122	38.823309
2377.460787	136208.760000	38.828327
2379.574018	136470.003559	38.833344
2382.146691	136738.105402	38.838362
2384.685270	137015.173244	38.843380
2386.941914	137287.934177	38.848397
2389.521869	137573.260097	38.853415
2392.135787	137840.067494	38.858432
2394.672162	138120.073717	38.863450
2396.617748	138412.724769	38.868468
2398.909668	138691.820879	38.873485
2401.545028	138967.070467	38.878503
2403.827699	139259.153744	38.883520
2406.635623	139529.607968	38.888538
2408.939929	139823.556859	38.893556
2411.394511	140084.069236	38.898573
2414.019117	140370.775725	38.903591
2417.168532	140644.165198	38.908608
2419.828026	140904.535761	38.913626
2422.317275	141175.632925	38.918644
2424.740253	141447.744574	38.923661
2427.247771	141723.118853	38.928679
2429.148094	141990.518021	38.933696
2431.638001	142261.405381	38.938714
2433.904404	142542.152354	38.943732
2436.328197	142825.046553	38.948749
2438.830189	143112.638709	38.953767
2440.995122	143390.436551	38.958784
2443.875496	143659.049461	38.963802
2445.976920	143953.156522	38.968820
2448.345391	144231.841016	38.973837
2450.457753	144519.756066	38.978855
2452.496373	144814.068366	38.983872
2455.475867	145092.585882	38.988890
2457.670172	145395.139733	38.993908
2459.916177	145674.003628	38.998925
2462.314108	145970.309852	39.003943
2464.791393	146278.548877	39.008960
2467.300445	146567.479590	39.013978
2469.204465	146876.776482	39.018996
2471.735353	147183.629028	39.024013
2474.227115	147483.940091	39.029031
2476.327759	147792.399323	39.034048
2479.319577	148072.111400	39.039066
2481.265540	148347.990308	39.044084
2483.862116	148632.031975	39.049101
2486.494449	148900.051012	39.054119
2488.667716	149180.442775	39.059136
2491.499527	149467.917302	39.064154
2493.056562	149763.272154	39.069172
2495.476720	150060.118345	39.074189
2497.901301	150360.303818	39.079207
2500.180073	150675.035010	39.084224
2502.991494	150972.446954	39.089242
2504.819949	151298.485896	39.094260
2507.137340	151610.626929	39.099277
2509.954078	151927.921415	39.104295
2511.977783	152264.598210	39.109312
2514.566267	152591.630223	39.114330
2517.214151	152918.591382	39.119348
2519.468794	153264.720413	39.124365
2522.073524	153607.102822	39.129383
2523.853061	153961.193435	39.134400
2526.938301	154305.840601	39.139418
2528.715238	154666.092675	39.144436
2531.082144	155032.233766	39.149453
2533.804520	155393.434194	39.154471
2536.082301	155774.243309	39.159488
2538.690899	156141.394506	39.164506
2540.868034	156524.382304	39.169524
2543.290149	156898.219396	39.174541
2545.789773	157292.079211	39.179559
2548.931828	157681.461364	39.184576
2551.191260	158072.482104	39.189594
2553.780783	158472.137192	39.194612
2556.707304	158866.638711	39.199629
2559.623195	159240.908149	39.204647
2562.294795	159624.777671	39.209664
2565.188705	160008.525923	39.214682
2567.933192	160388.859421	39.219700
2570.598825	160785.762604	39.224717
2573.391372	161166.296403	39.229735
2576.299414	161544.643441	39.234752
2578.910215	161918.024361	39.239770
2581.743786	162304.258932	39.244788
2584.218085	162696.938074	39.249805
2587.249804	163063.924473	39.254823
2590.005798	163447.003940	39.259840
2592.441794	163831.595746	39.264858
2594.979288	164206.473961	39.269876
2597.354959	164588.806944	39.274893
2599.759166	164971.315386	39.279911
2602.551994	165358.208972	39.284928
2605.124663	165736.657898	39.289946
2607.460699	166136.996807	39.294964
2609.810563	166521.871303	39.299981
2612.407469	166912.702163	39.304999
2614.669441	167316.639940	39.310016
2617.096125	167708.365240	39.315034
2619.600870	168122.541446	39.320052
2621.848220	168529.903907	39.325069
2624.909036	168944.747014	39.330087
2627.224959	169349.411582	39.335104
2629.779185	169756.758334	39.340122
2633.017587	170166.793743	39.345140
2635.286944	170572.932522	39.350157
2638.174947	170973.313674	39.355175
2640.714424	171387.921927	39.360192
2643.286414	171797.372135	39.365210
2645.672115	172213.735817	39.370228
2648.309634	172629.198919	39.375245
2650.629116	173017.794627	39.380263
2653.460067	173419.213310	39.385280
2655.947717	173799.215521	39.390298
2658.358007	174199.662733	39.395316
2660.339924	174598.858354	39.400333
2663.380222	174997.039637	39.405351
2665.158729	175414.861156	39.410368
2667.715000	175826.950527	39.415386
2670.712170	176243.150741	39.420404
2673.099783	176667.664228	39.425421
2676.220401	177095.442999	39.430439
2678.335493	177528.587591	39.435456
2680.916430	177961.915485	39.440474
2683.509162	178411.599557	39.445492
2685.792737	178847.746689	39.450509
2688.461003	179301.664884	39.455527
2690.857609	179752.859542	39.460544
2693.138982	180217.865494	39.465562
2696.171064	180699.417456	39.470580
2698.365377	181167.032454	39.475597
2701.308121	181644.514242	39.480615
2703.735332	182133.660730	39.485632
2706.178487	182629.131465	39.490650
2709.450680	183175.323075	39.495668
2712.198516	183678.853702	39.500685
2715.494808	184166.655433	39.505703
2718.258670	184658.251085	39.510720
2720.893198	185147.634245	39.515738
2723.762786	185635.154250	39.520756
2726.208100	186131.175498	39.525773
2728.863910	186629.375934	39.530791
2731.399680	187135.369763	39.535808
2734.495415	187637.392246	39.540826
2737.198717	188143.161402	39.545844
2739.267758	188666.354838	39.550861
2742.417195	189163.549892	39.555879
2745.195409	189684.478145	39.560896
2748.293507	190203.910913	39.565914
2751.464050	190722.496453	39.570932
2754.483748	191244.587728	39.575949
2757.725159	191743.049428	39.580967
2760.277680	192262.297090	39.585984
2762.798567	192773.779225	39.591002
2765.953484	193285.088073	39.596020
2768.584773	193793.585146	39.601037
2771.529995	194298.682163	39.606055
2774.118012	194814.099071	39.611072
2777.285591	195325.617117	39.616090
2780.007357	195835.606515	39.621108
2782.241499	196358.273193	39.626125
2784.966676	196878.934483	39.631143
2787.847417	197400.767205	39.636160
2790.399630	197930.146687	39.641178
2793.165935	198451.188148	39.646196
2795.607955	198989.479227	39.651213
2798.086594	199510.975693	39.656231
2800.945502	200054.336428	39.661248
2803.428670	200602.482558	39.666266
2806.341588	201149.877426	39.671284
2808.707311	201701.474823	39.676301
2811.314222	202256.490984	39.681319
2814.035013	202818.019517	39.686336
2816.909883	203368.119912	39.691354
2819.612607	203926.047472	39.696372
2822.016173	204489.053186	39.701389
2825.282135	205052.662318	39.706407
2828.192415	205619.910453	39.711424
2830.788713	206172.424712	39.716442
2833.471137	206718.449153	39.721460
2836.392830	207265.733082	39.726477
2839.545944	207778.814903	39.731495
2842.335659	208322.184491	39.736512
2844.563879	208853.043098	39.741530
2847.655848	209400.203693	39.746548
2850.485808	209947.482634	39.751565
2853.179032	210494.174397	39.756583
2855.717904	211051.205183	39.761600
2858.321068	211608.125377	39.766618
2861.554661	212157.936628	39.771636
2863.956019	212725.610716	39.776653
2866.914425	213288.067135	39.781671
2869.418427	213875.313331	39.786688
2872.440157	214452.724485	39.791706
2874.962185	215037.912008	39.796724
2877.698760	215646.997214	39.801741
2880.899902	216228.549085	39.806759
2883.314085	216834.434661	39.811776
2886.161248	217432.581299	39.816794
2888.846975	218037.841561	39.821812
2891.570120	218653.385216	39.826829
2894.226000	219285.528798	39.831847
2897.825313	219906.093618	39.836864
2900.647591	220544.055191	39.841882
2903.533520	221171.083539	39.846900
2906.436454	221807.585328	39.851917
2909.202570	222440.120413	39.856935
2911.886072	223093.042757	39.861952
2914.976761	223724.867064	39.866970
2918.034637	224367.747425	39.871988
2921.413548	225007.402156	39.877005
2924.561425	225649.277789	39.882023
2927.599338	226299.426903	39.887040
2930.335100	226939.512333	39.892058
2934.061305	227586.301798	39.897076
2936.946848	228234.264053	39.902093
2939.898162	228876.626822	39.907111
2942.266105	229529.724739	39.912128
2945.721272	230178.333499	39.917146
2948.612226	230821.923779	39.922164
2951.885889	231471.830037	39.927181
2955.075977	232124.949613	39.932199
2957.865531	232774.599960	39.937216
2960.659105	233416.297483	39.942234
2963.773739	234066.124009	39.947252
2966.637633	234733.161805	39.952269
2969.841113	235383.455183	39.957287
2972.520266	236034.744038	39.962304
2975.577780	236694.177988	39.967322
2977.979159	237362.096520	39.972340
2980.997838	238030.806316	39.977357
2984.111955	238694.520694	39.982375
2986.816762	239361.777901	39.987392
2989.419815	240054.656109	39.992410
2992.176980	240722.409973	39.997428
2995.677795	241392.738600	40.002445
2999.296297	242057.026483	40.007463
3003.206731	242722.765678	40.012480
3006.047735	243386.485545	40.017498
3009.558832	244039.378605	40.022516
3012.346259	244714.076947	40.027533
3015.601166	245366.447138	40.032551
3018.515057	246030.655428	40.037568
3020.948236	246690.846815	40.042586
3023.854059	247341.842477	40.047604
3026.894270	248015.041992	40.052621
3029.646548	248670.273718	40.057639
3032.390036	249307.570341	40.062656
3035.244667	249951.908995	40.067674
3038.273367	250588.597289	40.072692
3041.166119	251235.033281	40.077709
3043.992167	251882.975753	40.082727
3046.720607	252525.621776	40.087744
3049.239250	253191.083130	40.092762
3052.302169	253843.171334	40.097780
3055.026819	254517.967520	40.102797
3057.880496	255186.643952	40.107815
3060.824091	255861.424722	40.112832
3063.505857	256553.642727	40.117850
3067.163068	257238.719274	40.122868
3070.197270	257923.660954	40.127885
3073.237466	258618.427979	40.132903
3076.305133	259324.362966	40.137920
3078.872590	260039.820926	40.142938
3082.172154	260737.278326	40.147956
3085.192936	261457.381093	40.152973
3088.267550	262176.759643	40.157991
3091.378778	262900.318729	40.163008
3094.190994	263640.912003	40.168026
3097.466311	264370.048806	40.173044
3100.538719	265107.289165	40.178061
3103.401272	265856.951717	40.183079
3106.656156	266602.966101	40.188096
3109.639498	267358.821151	40.193114
3112.504046	268108.263092	40.198132
3115.713833	268864.883624	40.203149
3118.800882	269644.705559	40.208167
3122.136445	270405.408317	40.213184
3125.016575	271187.509800	40.218202
3128.371724	271954.444125	40.223220
3131.335763	272734.867921	40.228237
3133.930725	273520.294721	40.233255
3137.044504	274309.848932	40.238272
3140.200379	275111.757084	40.243290
3143.587779	275904.250013	40.248308
3146.706693	276709.068713	40.253325
3150.357256	277507.218654	40.258343
3154.568687	278288.105491	40.263360
3158.076571	279073.030641	40.268378
3161.373308	279851.149474	40.273396
3164.795091	280621.723864	40.278413
3168.089594	281399.344307	40.283431
3171.932744	282167.703403	40.288448
3175.058601	282944.851070	40.293466
3177.920093	283715.556202	40.298484
3181.378326	284485.981759	40.303501
3184.572803	285244.403710	40.308519
3188.058787	286013.461901	40.313536
3191.268946	286779.862823	40.318554
3194.821717	287552.041473	40.323572
3197.615847	288325.142168	40.328589
3200.741875	289084.597324	40.333607
3203.907083	289854.447675	40.338624
3206.838279	290628.336971	40.343642
3209.624203	291403.458121	40.348660
3213.190884	292174.613534	40.353677
3216.143807	292954.030675	40.358695
3219.395995	293739.941424	40.363712
3222.423648	294531.767189	40.368730
3225.352144	295317.758378	40.373748
3228.507901	296103.906525	40.378765
3231.669218	296875.571836	40.383783
3235.519994	297652.221825	40.388800
3238.620733	298441.849793	40.393818
3242.027929	299207.148623	40.398836
3245.647864	299962.604293	40.403853
3248.555555	300711.865047	40.408871
3251.472574	301452.127303	40.413888
3254.710024	302189.689104	40.418906
3257.546386	302939.335983	40.423924
3260.845658	303705.603059	40.428941
3263.588135	304459.786688	40.433959
3266.672760	305220.023356	40.438976
3269.275065	306008.703180	40.443994
3272.345798	306799.531178	40.449012
3275.187514	307597.286641	40.454029
3277.999026	308404.247841	40.459047
3281.451003	309207.542116	40.464064
3284.190881	310031.036758	40.469082
3287.245595	310860.508812	40.474100
3290.598927	311697.990825	40.479117
3293.603484	312540.182479	40.484135
3296.783344	313390.097782	40.489152
3299.648048	314248.751882	40.494170
3302.633884	315120.872543	40.499188
3305.863150	316002.734452	40.504205
3308.974985	316894.367909	40.509223
3311.980715	317773.108335	40.514240
3315.006730	318692.253490	40.519258
3318.861414	319591.583012	40.524276
3321.770972	320514.311223	40.529293
3324.705472	321445.516347	40.534311
3328.135206	322373.375599	40.539328
3331.253216	323310.854493	40.544346
3334.733196	324244.576465	40.549364
3338.904466	325172.536354	40.554381
3342.377622	326119.334481	40.559399
3346.986022	327041.347607	40.564416
3350.626035	327972.193218	40.569434
3353.913697	328906.015053	40.574452
3357.672597	329828.984114	40.579469
3360.788387	330755.431345	40.584487
3364.841855	331683.612394	40.589504
3368.126591	332608.161976	40.594522
3371.801321	333538.285014	40.599540
3375.469915	334452.125772	40.604557
3378.755184	335375.135937	40.609575
3381.836626	336293.614458	40.614592
3385.481500	337222.254724	40.619610
3388.959567	338147.143409	40.624628
3392.444120	339080.073021	40.629645
3395.587160	340013.285310	40.634663
3399.120902	340935.962637	40.639680
3402.648822	341859.986203	40.644698
3405.736117	342786.742459	40.649716
3409.207991	343731.774701	40.654733
3412.572277	344671.142542	40.659751
3415.924868	345604.450867	40.664768
3419.627144	346551.930103	40.669786
3422.903904	347477.083716	40.674804
3426.266587	348402.781382	40.679821
3429.307229	349349.726542	40.684839
3433.196268	350286.192050	40.689856
3436.372418	351235.571507	40.694874
3439.711014	352181.246677	40.699892
3443.835682	353112.421134	40.704909
3447.431492	354047.758092	40.709927
3451.910008	354968.580272	40.714944
3455.542862	355895.414365	40.719962
3459.215434	356808.221331	40.724980
3463.247374	357722.973097	40.729997
3466.667361	358635.663964	40.735015
3469.944060	359526.724602	40.740020
3473.341493	360383.328796	40.745024
3476.649272	361190.777061	40.750029
3479.996009	361942.243053	40.755034
3483.854237	362646.321877	40.760039
3487.031784	363266.130630	40.765044
3490.176629	363872.922001	40.770048
3492.509412	364390.237119	40.775053
3495.551218	364856.006054	40.780058
3497.772397	365272.934947	40.785063
3500.084012	365643.424206	40.790068
3502.425233	365954.756082	40.795072
3504.601433	366220.962173	40.800077
3506.495236	366440.309004	40.805082
3508.092113	366632.236008	40.810087
3509.774634	366764.595493	40.815092
3511.309972	366858.003914	40.820096
3512.998122	366913.710476	40.825101
3514.282899	366941.939496	40.830106
3515.234267	366944.992097	40.835111
3516.329006	366907.397475	40.840116
3517.207626	366860.487021	40.845120
3517.821292	366769.283561	40.850125
3518.730940	366672.545713	40.855130
3518.976204	366538.868421	40.860135
3520.180178	366398.028338	40.865140
3520.468756	366238.808984	40.870144
3521.085346	366067.596118	40.875149
3521.707719	365869.983143	40.880154
3521.873036	365667.562034	40.885159
3522.356822	365453.910345	40.890164
3522.500042	365226.742519	40.895168
3522.735048	364993.155732	40.900173
3522.997924	364743.098137	40.905178
3523.108000	364494.078626	40.910183
3523.781264	364226.979556	40.915188
3523.526741	363965.384389	40.920192
3523.549143	363687.507108	40.925197
3523.705305	363406.531742	40.930202
3523.467469	363134.254588	40.935207
3523.609838	362851.192487	40.940212
3523.800911	362557.117450	40.945216
3523.640287	362253.463916	40.950221
3523.962015	361961.624078	40.955226
3523.359634	361667.943794	40.960231
3523.403227	361362.521294	40.965236
3523.346468	361077.161006	40.970240
3523.519319	360774.151790	40.975245
3523.340267	360466.340844	40.980250
3523.778090	360177.057469	40.985255
3523.486209	359862.777877	40.990260
3523.048344	359564.705751	40.995264
3522.862513	359249.513760	41.000269
3522.976493	358952.543754	41.005274
3522.642002	358651.930591	41.010279
3522.686065	358344.698534	41.015284
3522.087694	358043.891912	41.020288
3522.261516	357742.427914	41.025293
3522.194101	357446.971077	41.030298
3522.014380	357147.488018	41.035303
3522.051368	356848.298565	41.040308
3522.089196	356552.664219	41.045312
3521.745194	356256.248034	41.050317
3521.500819	355963.905375	41.055322
3521.449567	355670.157316	41.060327
3521.417034	355374.751512	41.065332
3521.160477	355093.687388	41.070336
3520.536077	354810.924501	41.075341
3520.583054	354512.702307	41.080346
3520.334866	354230.612474	41.085351
3519.878229	353948.298532	41.090356
3520.258297	353677.645014	41.095360
3519.950308	353403.462009	41.100365
3519.837620	353130.491586	41.105370
3519.654745	352854.784626	41.110375
3519.875963	352582.443597	41.115380
3519.584951	352303.978175	41.120384
3519.292437	352038.118329	41.125389
3519.294750	351762.906803	41.130394
3518.901116	351503.819821	41.135399
3518.856437	351226.602933	41.140404
3518.910432	350982.413872	41.145408
3518.235566	350713.349149	41.150413
3518.228506	350449.033035	41.155418
3517.980937	350202.368654	41.160423
3518.064884	349954.125347	41.165428
3518.174283	349703.842516	41.170432
3517.931446	349458.188599	41.175437
3517.692149	349195.856051	41.180442
3517.309227	348951.135396	41.185447
3517.380219	348703.494751	41.190452
3516.952615	348459.133325	41.195456
3516.878487	348232.967715	41.200461
3517.048743	347994.483519	41.205466
3516.521804	347759.436914	41.210471
3516.622053	347517.858730	41.215476
3516.404703	347283.192538	41.220480
3516.092665	347055.530753	41.225485
3516.108204	346828.045011	41.230490
3515.737169	346602.321505	41.235495
3516.123120	346371.368061	41.240500
3515.702135	346153.047510	41.245504
3515.825811	345941.403067	41.250509
3515.347959	345708.546234	41.255514
3514.743508	345502.885762	41.260519
3514.592181	345288.890376	41.265524
3514.930481	345081.681636	41.270528
3515.033261	344879.542481	41.275533
3514.786641	344664.159718	41.280538
3514.142253	344457.227929	41.285543
3514.225072	344245.274200	41.290548
3513.720927	344048.437100	41.295552
3514.095378	343859.673833	41.300557
3513.960156	343660.590268	41.305562
3513.517859	343463.968974	41.310567
3513.552168	343267.882259	41.315572
3513.475567	343081.575245	41.320576
3513.119101	342895.666941	41.325581
3513.320212	342708.907689	41.330586
3513.142213	342532.555130	41.335591
3513.255081	342339.908828	41.340596
3512.993932	342154.464748	41.345600
3512.477493	341974.373736	41.350605
3512.651836	341793.156733	41.355610
3512.118063	341621.559111	41.360615
3512.073347	341449.146810	41.365620
3512.329559	341283.068798	41.370624
3512.222358	341118.699581	41.375629
3512.459278	340929.255359	41.380634
3511.921967	340755.136751	41.385639
3511.625325	340596.185320	41.390644
3511.544292	340437.072326	41.395648
3511.584021	340272.905042	41.400653
3511.622352	340111.534281	41.405658
3511.523473	339950.591085	41.410663
3511.183067	339790.168052	41.415668
3511.429301	339627.465755	41.420672
3511.332096	339472.775475	41.425677
3511.495509	339310.796673	41.430682
3511.123040	339156.910910	41.435687
3510.932388	338997.147467	41.440692
3510.794483	338846.198850	41.445696
3510.755988	338691.012861	41.450701
3510.593361	338530.174942	41.455706
3510.453262	338381.869331	41.460711
3510.489286	338231.221517	41.465716
3510.563584	338093.027451	41.470720
3510.188905	337951.419219	41.475725
3510.212347	337804.992873	41.480730
3510.004498	337671.774631	41.485735
3510.061070	337529.766743	41.490740
3509.837253	337390.090817	41.495744
3509.606468	337255.628571	41.500749
3510.013851	337107.435583	41.505754
3509.284923	336985.002311	41.510759
3509.064191	336851.376193	41.515764
3509.063047	336727.073593	41.520768
3509.324812	336600.491597	41.525773
3509.483200	336474.739099	41.530778
3509.024708	336348.065390	41.535783
3509.101094	336208.312575	41.540788
3509.129773	336083.697962	41.545792
3508.759420	335965.731885	41.550797
3508.960521	335840.936908	41.555802
3508.993764	335726.390997	41.560807
3508.711818	335597.398313	41.565812
3508.910243	335470.974916	41.570816
3508.398963	335350.409495	41.575821
3508.618933	335234.993638	41.580826
3508.536589	335116.903526	41.585831
3508.353178	334994.149451	41.590836
3508.417925	334882.037420	41.595840
3508.034832	334772.105889	41.600845
3508.114071	334660.677578	41.605850
3507.714280	334552.731680	41.610855
3508.018883	334446.048665	41.615860
3508.008100	334328.809546	41.620864
3507.720151	334230.153308	41.625869
3507.996569	334119.633539	41.630874
3507.636285	334021.674725	41.635879
3507.893533	333919.829715	41.640884
3507.599757	333806.651488	41.645888
3507.032972	333711.597993	41.650893
3507.597984	333606.753868	41.655898
3507.275979	333508.151919	41.660903
3507.365688	333418.539326	41.665908
3507.340732	333313.939215	41.670912
3507.083021	333218.505530	41.675917
3507.253481	333119.215188	41.680922
3506.766975	333023.282691	41.685927
3507.016286	332928.582856	41.690932
3506.967551	332834.895832	41.695936
3506.287787	332752.904669	41.700941
3506.697731	332657.161723	41.705946
3506.634114	332578.405584	41.710951
3506.534564	332485.132569	41.715956
3506.593947	332397.709551	41.720960
3506.741304	332308.848315	41.725965
3506.563833	332217.850387	41.730970
3506.526258	332131.510116	41.735975
3506.539550	332042.033382	41.740980
3506.223307	331953.727031	41.745984
3505.945395	331879.504680	41.750989
3506.026539	331791.313862	41.755994
3506.102044	331718.765433	41.760999
3505.695274	331643.113048	41.766004
3506.269212	331554.437703	41.771008
3505.973010	331490.619871	41.776013
3506.221917	331400.214616	41.781018
3506.102069	331341.430306	41.786023
3505.772726	331255.769521	41.791028
3506.123710	331169.747843	41.796032
3505.841304	331097.533968	41.801037
3506.416743	331003.236185	41.806042
3505.877480	330933.427534	41.811047
3505.708523	330848.961609	41.816052
3505.685600	330769.966478	41.821056
3505.567464	330703.398030	41.826061
3505.515357	330629.544911	41.831066
3505.591463	330568.007306	41.836071
3505.745179	330491.730909	41.841076
3505.777198	330417.152066	41.846080
3505.196655	330355.742217	41.851085
3505.429448	330277.494574	41.856090
3505.103819	330209.711420	41.861095
3505.380385	330146.005294	41.866100
3505.228658	330080.305807	41.871104
3505.162616	330006.402809	41.876109
3505.122865	329934.886436	41.881114
3505.029089	329883.293893	41.886119
3504.936754	329812.243343	41.891124
3504.838772	329749.866871	41.896128
3505.027332	329694.643608	41.901133
3505.277583	329623.361110	41.906138
3504.835627	329557.884160	41.911143
3504.803664	329503.076629	41.916148
3504.958967	329440.202231	41.921152
3504.865624	329379.019894	41.926157
3504.772342	329322.949936	41.931162
3504.389440	329259.777862	41.936167
3504.425558	329211.903111	41.941172
3504.626080	329157.185925	41.946176
3504.361196	329104.906915	41.951181
3504.241224	329048.993350	41.956186
3504.389292	328995.352427	41.961191
3504.617117	328945.361672	41.966196
3504.652001	328891.229592	41.971200
3504.212739	328833.457973	41.976205
3504.586553	328768.081088	41.981210
3504.649285	328722.821447	41.986215
3504.485530	328667.219411	41.991220
3504.393036	328614.811055	41.996224
3504.480532	328557.541700	42.001229
3504.232909	328505.640730	42.006234
3504.123444	328457.508027	42.011239
3504.283366	328408.951613	42.016244
3504.473881	328360.288613	42.021248
3504.335872	328305.546862	42.026253
3504.317572	328249.590831	42.031258
3504.551367	328205.982626	42.036263
3504.088390	328145.034209	42.041268
3504.504598	328096.081240	42.046272
3503.921133	328042.273591	42.051277
3504.062649	327995.627253	42.056282
3503.874639	327956.256238	42.061287
3504.032318	327893.862288	42.066292
3503.888746	327863.336018	42.071296
3503.829473	327816.034082	42.076301
3503.600996	327769.470758	42.081306
3503.687454	327732.600236	42.086311
3503.724846	327688.284515	42.091316
3504.015293	327641.309242	42.096320
3503.713512	327599.132227	42.101325
3503.941913	327548.859819	42.106330
3503.893622	327512.747814	42.111335
3503.766842	327463.471973	42.116340
3503.943676	327420.355104	42.121344
3503.476910	327372.226071	42.126349
3503.778149	327334.202396	42.131354
3503.540534	327292.828993	42.136359
3503.740706	327243.171090	42.141364
3503.879661	327212.116856	42.146368
3503.711500	327174.929512	42.151373
3503.889105	327111.946181	42.156378
3503.519389	327080.869622	42.161383
3503.682730	327030.708480	42.166388
3503.692870	326995.528032	42.171392
3503.582812	326958.178782	42.176397
3503.571528	326910.003420	42.181402
3503.378656	326870.759276	42.186407
3503.448466	326835.772853	42.191412
3503.466076	326795.249324	42.196416
3503.397564	326759.445042	42.201421
3503.311224	326711.306612	42.206426
3503.070764	326687.840616	42.211431
3503.493924	326650.280533	42.216436
3503.476671	326604.445937	42.221440
3503.141406	326572.524178	42.226445
3503.647806	326525.539271	42.231450
3503.421678	326504.818127	42.236455
3503.452632	326472.508353	42.241460
3503.165153	326431.396227	42.246464
3503.142817	326402.706795	42.251469
3503.503907	326359.280171	42.256474
3503.023151	326333.028012	42.261479
3503.344803	326294.313357	42.266484
3503.040071	326245.826956	42.271488
3503.034120	326225.376492	42.276493
3502.701541	326188.086753	42.281498
3502.912539	326157.783558	42.286503
3502.901741	326120.850446	42.291508
3502.898592	326107.013181	42.296512
3503.066813	326075.012313	42.301517
3502.977356	326035.725749	42.306522
3502.929800	326017.342110	42.311527
3503.166986	325974.799314	42.316532
3503.121729	325939.601165	42.321536
3502.600860	325913.304129	42.326541
3502.864887	325884.264311	42.331546
3502.761885	325852.000420	42.336551
3503.028762	325832.092166	42.341556
3502.680165	325808.515376	42.346560
3502.400225	325782.867401	42.351565
3503.028430	325751.404864	42.356570
3502.951872	325729.947688	42.361575
3502.783348	325694.361597	42.366580
3503.013551	325665.784787	42.371584
3502.700170	325634.596553	42.376589
3503.135517	325604.944687	42.381594
3502.720290	325580.258925	42.386599
3502.465744	325554.428772	42.391604
3502.625165	325526.066430	42.396608
3502.156344	325508.231735	42.401613
3502.267824	325479.775105	42.406618
3502.452361	325464.000450	42.411623
3502.232875	325438.724371	42.416628
3502.907168	325411.934908	42.421632
3502.943850	325395.216708	42.426637
3502.906732	325366.427102	42.431642
3502.646929	325338.893303	42.436647
3502.577795	325313.059447	42.441652
3502.753569	325288.637242	42.446656
3502.638442	325253.576611	42.451661
3502.938350	325225.192096	42.456666
3502.869688	325204.521982	42.461671
3502.436558	325170.274131	42.466676
3502.874203	325149.982716	42.471680
3502.464993	325115.883708	42.476685
3502.363424	325099.950138	42.481690
3502.553563	325073.846655	42.486695
3502.149025	325057.451675	42.491700
3502.494363	325044.653397	42.496704
3502.043590	325022.135081	42.501709
3502.440392	324993.658943	42.506714
3502.386989	324979.116886	42.511719
3502.292113	324962.012067	42.516724
3502.210678	324937.222855	42.521728
3502.243905	324925.668923	42.526733
3501.881638	324900.643775	42.531738
3502.288162	324894.602407	42.536743
3502.066088	324870.140398	42.541748
3502.431009	324846.095367	42.546752
3502.114872	324835.257419	42.551757
3502.346165	324801.007136	42.556762
3501.848825	324801.822725	42.561767
3502.007765	324769.186329	42.566772
3502.122417	324750.089928	42.571776
3502.221080	324745.521205	42.576781
3502.378176	324725.298879	42.581786
3502.297935	324709.463575	42.586791
3502.283904	324678.126056	42.591796
3502.261586	324665.105319	42.596800
3502.258795	324639.209789	42.601805
3502.224237	324614.896379	42.606810
3502.348980	324611.391970	42.611815
3501.994900	324586.568855	42.616820
3502.249251	324575.132884	42.621824
3501.922346	324546.566072	42.626829
3502.346245	324534.569379	42.631834
3502.286309	324522.622885	42.636839
3502.267502	324496.475386	42.641844
3502.574371	324478.595285	42.646848
3502.350161	324458.407001	42.651853
3502.405455	324440.235516	42.656858
3502.409269	324410.726564	42.661863
3502.389361	324391.142266	42.666868
3502.472451	324381.946154	42.671872
3502.351269	324361.614523	42.676877
3502.323472	324336.867439	42.681882
3502.542250	324325.029945	42.686887
3502.185075	324299.418549	42.691892
3502.334868	324278.968199	42.696896
3502.187058	324261.286280	42.701901
3502.221593	324234.901328	42.706906
3502.304314	324235.168350	42.711911
3502.442021	324200.499744	42.716916
3502.185443	324190.949676	42.721920
3502.443225	324163.054344	42.726925
3502.328956	324133.258392	42.731930
3502.113489	324120.013293	42.736935
3501.905241	324105.418819	42.741940
3502.477902	324093.424179	42.746944
3502.103630	324078.448634	42.751949
3502.335463	324058.824821	42.756954
3502.510476	324021.962515	42.761959
3502.299528	324018.001765	42.766964
3502.575361	324001.118414	42.771968
3502.377599	323981.256463	42.776973
3502.200361	323950.885135	42.781978
3502.548102	323933.278234	42.786983
3502.008555	323912.935472	42.791988
3502.583006	323896.488728	42.796993
3502.112343	323873.616749	42.801997
3502.106380	323844.465062	42.807002
3502.100262	323838.309981	42.812007
3502.172198	323822.628616	42.817012
3502.158443	323807.316783	42.822017
3501.907707	323798.299924	42.827021
3502.301098	323770.535759	42.832026
3502.566018	323764.134784	42.837031
3502.265443	323737.878222	42.842036
3502.088381	323721.116440	42.847041
3502.259800	323704.529119	42.852045
3502.145979	323694.778546	42.857050
3502.255980	323674.512189	42.862055
3502.319855	323660.994322	42.867060
3501.942585	323629.331212	42.872065
3502.224286	323616.415246	42.877069
3502.607528	323597.607026	42.882074
3502.347622	323578.136179	42.887079
3502.170442	323558.118174	42.892084
3502.301639	323531.234322	42.897089
3502.190538	323530.005317	42.902093
3502.338264	323491.874859	42.907098
3502.342456	323478.188191	42.912103
3502.103899	323457.899904	42.917108
3502.372691	323442.009546	42.922113
3501.933748	323427.247386	42.927117
3501.990199	323409.380535	42.932122
3502.176641	323395.029371	42.937127
3502.311953	323373.003620	42.942132
3502.328039	323350.360522	42.947137
3502.209109	323340.356274	42.952141
3502.416732	323315.927920	42.957146
3502.520797	323299.681675	42.962151
3502.224788	323275.637302	42.967156
3502.320280	323259.087113	42.972161
3502.212906	323256.509246	42.977165
3502.279849	323222.893886	42.982170
3501.992128	323210.194013	42.987175
3501.633900	323192.798923	42.992180
3502.186799	323181.061502	42.997185
3501.921329	323177.083756	43.002189
3502.043178	323148.827406	43.007194
3501.974811	323139.781892	43.012199
3501.851693	323131.177402	43.017204
3502.147965	323102.206895	43.022209
3501.967816	323098.597389	43.027213
3502.087541	323083.315300	43.032218
3502.212929	323066.302455	43.037223
3501.647452	323055.070552	43.042228
3502.040921	323039.364063	43.047233
3501.562227	323022.089492	43.052237
3502.076999	323009.823760	43.057242
3501.987980	323005.436823	43.062247
3501.844162	322987.626539	43.067252
3502.202009	322969.000080	43.072257
3501.859904	322964.729023	43.077261
3501.820138	322940.364564	43.082266
3502.016706	322929.318762	43.087271
3501.526776	322924.918175	43.092276
3501.961791	322914.242119	43.097281
3502.130257	322906.177100	43.102285
3501.895215	322882.351922	43.107290
3502.149415	322872.085713	43.112295
3501.844008	322855.496282	43.117300
3501.794807	322842.148463	43.122305
3501.563479	322843.176893	43.127309
3501.658593	322828.254708	43.132314
3501.924662	322802.977419	43.137319
3501.881051	322800.262357	43.142324
3501.856226	322780.042083	43.147329
3501.999660	322784.522556	43.152333
3501.927775	322765.937751	43.157338
3501.860286	322755.136700	43.162343
3501.711047	322744.679138	43.167348
3502.053800	322719.593325	43.172353
3501.614920	322716.049675	43.177357
3501.692982	322707.311887	43.182362
3501.816922	322696.684408	43.187367
3501.915677	322677.971129	43.192372
3501.923187	322668.989968	43.197377
3501.694350	322661.546683	43.202381
3502.038448	322632.899086	43.207386
3501.873961	322627.633527	43.212391
3502.331909	322617.335402	43.217396
3501.865733	322595.962944	43.222401
3501.609703	322579.213047	43.227405
3502.059121	322566.779326	43.232410
3501.970732	322556.770116	43.237415
3501.670975	322534.990017	43.242420
3501.925208	322526.402725	43.247425
3501.752490	322522.766568	43.252429
3501.602122	322497.986671	43.257434
3501.670054	322485.078337	43.262439
3501.224714	322491.838690	43.267444
3501.822544	322481.849377	43.272449
3501.592350	322477.993246	43.277453
3501.987722	322466.331132	43.282458
3501.992356	322448.268453	43.287463
3502.064760	322436.885779	43.292468
3502.035864	322418.701132	43.297473
3501.786037	322406.122286	43.302477
3501.954673	322389.865593	43.307482
3501.992089	322379.531397	43.312487
3501.570133	322355.226348	43.317492
3502.267397	322350.538339	43.322497
3501.667675	322354.575370	43.327501
3501.870000	322333.759696	43.332506
3501.988433	322325.422551	43.337511
3501.892773	322322.105045	43.342516
3502.199724	322299.695740	43.347521
3501.956054	322283.528904	43.352525
3502.213075	322272.855073	43.357530
3502.287281	322250.889163	43.362535
3501.900572	322249.448810	43.367540
3501.899291	322228.385079	43.372545
3501.851816	322219.437859	43.377549
3501.893325	322197.426153	43.382554
3501.646400	322185.152064	43.387559
3501.844972	322180.567441	43.392564
3502.204949	322162.042050	43.397569
3501.824389	322157.904120	43.402573
3501.904213	322138.659325	43.407578
3501.875747	322116.124282	43.412583
3501.527467	322098.905260	43.417588
3501.956923	322105.452592	43.422593
3501.855237	322082.776339	43.427597
3501.910694	322060.787822	43.432602
3501.774334	322061.216308	43.437607
3501.742170	322055.675591	43.442612
3502.156443	322035.004713	43.447617
3501.898290	322019.883072	43.452621
3501.858765	322012.486394	43.457626
3501.883524	321986.457704	43.462631
3501.776195	321979.427778	43.467636
3502.070255	321975.820357	43.472641
3501.986295	321963.062809	43.477645
3502.118387	321941.367526	43.482650
3501.898886	321926.595967	43.487655
3501.997517	321917.727600	43.492660
3501.995721	321899.436732	43.497665
3501.671906	321898.724291	43.502669
3502.111970	321886.673431	43.507674
3501.979147	321862.577294	43.512679
3502.073787	321871.288519	43.517684
3502.007677	321841.152680	43.522689
3501.328364	321825.511695	43.527693
3501.558050	321808.431155	43.532698
3501.872163	321810.086655	43.537703
3501.875203	321803.064884	43.542708
3501.524014	321783.810991	43.547713
3501.274602	321774.768047	43.552717
3501.721184	321762.767013	43.557722
3501.636608	321752.985974	43.562727
3501.430893	321756.885143	43.567732
3501.827244	321743.263798	43.572737
3501.285183	321736.683396	43.577741
3501.680214	321711.741449	43.582746
3501.787290	321720.883242	43.587751
3501.756062	321721.320735	43.592756
3501.917766	321701.477820	43.597761
3501.849711	321696.171627	43.602765
3501.651902	321682.515952	43.607770
3501.779917	321679.443266	43.612775
3501.578345	321668.077777	43.617780
3501.955315	321650.465347	43.622785
3501.495133	321649.392620	43.627789
3501.287659	321649.832228	43.632794
3501.649460	321646.850190	43.637799
3501.471771	321633.089593	43.642804
3501.841946	321616.851974	43.647809
3501.782656	321602.742136	43.652813
3501.966268	321604.519807	43.657818
3501.448616	321592.745792	43.662823
3501.530129	321577.977931	43.667828
3501.673445	321564.370647	43.672833
3501.767109	321575.905937	43.677837
3501.710869	321560.930645	43.682842
3501.982219	321537.305377	43.687847
3501.838921	321529.797637	43.692852
3501.965707	321512.605864	43.697857
3501.717459	321511.703521	43.702861
3501.800166	321488.438439	43.707866
3501.741321	321482.164054	43.712871
3501.696947	321472.249464	43.717876
3501.460453	321474.016499	43.722881
3501.251429	321457.487767	43.727885
3500.938975	321434.055472	43.732890
3501.132755	321431.201449	43.737895
3501.148299	321440.179531	43.742900
3501.350361	321426.868301	43.747905
3501.542218	321433.096721	43.752909
3501.508207	321427.759732	43.757914
3501.057032	321426.125907	43.762919
3501.072294	321432.178414	43.767924
3501.639521	321423.185803	43.772929
3501.011851	321417.687223	43.777933
3501.391749	321427.371551	43.782938
3501.512195	321415.879330	43.787943
3501.274322	321422.149494	43.792948
3501.446723	321421.919151	43.797953
3501.665542	321408.249133	43.802957
3501.415992	321388.139643	43.807962
3501.856474	321383.975037	43.812967
3501.692158	321385.349188	43.817972
3501.512405	321380.950826	43.822977
3501.514122	321376.574972	43.827981
3501.576882	321348.708254	43.832986
3501.639670	321345.213258	43.837991
3501.248240	321337.515314	43.842996
3501.674052	321335.642618	43.848001
3501.591084	321344.458040	43.853005
3501.736479	321324.948221	43.858010
3501.815606	321304.482024	43.863015
3501.615229	321299.450871	43.868020
3501.735031	321290.121138	43.873025
3501.710106	321291.041015	43.878029
3501.208866	321270.004088	43.883034
3501.674064	321257.414875	43.888039
3501.581998	321257.378519	43.893044
3501.703322	321252.856753	43.898049
3501.836384	321262.376186	43.903053
3501.960481	321228.750297	43.908058
3502.084530	321219.648847	43.913063
3501.838286	321210.376324	43.918068
3502.388644	321187.139726	43.923073
3501.752186	321182.634661	43.928077
3501.913321	321173.527404	43.933082
3501.597735	321144.142400	43.938087
3501.730892	321134.276298	43.943092
3501.727621	321127.662448	43.948097
3501.845992	321131.663649	43.953101
3501.835579	321117.520568	43.958106
3501.811750	321104.906002	43.963111
3501.789982	321096.895819	43.968116
3501.960914	321086.514992	43.973121
3501.792193	321063.543389	43.978125
3501.563958	321049.663303	43.983130
3501.444258	321042.075466	43.988135
3501.601032	321042.559895	43.993140
3501.671412	321037.842547	43.998145
3501.649506	321018.765790	44.003149
3501.668813	321001.895899	44.008154
3501.924591	321000.685782	44.013159
3501.771734	320999.208825	44.018164
3501.504476	320984.851450	44.023169
3501.801707	320973.153388	44.028173
3501.797584	320968.244157	44.033178
3501.778141	320975.650499	44.038183
3501.460141	320954.584767	44.043188
3501.915700	320932.482232	44.048193
3501.810055	320937.790498	44.053197
3501.489179	320925.095116	44.058202
3502.072763	320920.908093	44.063207
3501.796051	320904.516931	44.068212
3501.721725	320888.195883	44.073217
3501.694485	320887.640582	44.078221
3501.757811	320869.110124	44.083226
3501.909528	320854.407358	44.088231
3501.241726	320844.539206	44.093236
3501.999065	320842.716421	44.098241
3501.934393	320833.262785	44.103245
3501.731541	320816.605636	44.108250
3501.578381	320819.224647	44.113255
3501.160928	320817.331120	44.118260
3501.403301	320805.412624	44.123265
3501.446842	320802.022355	44.128269
3501.084214	320804.775876	44.133274
3501.264929	320804.493349	44.138279
3501.196723	320790.766244	44.143284
3501.726296	320771.577719	44.148289
3501.493181	320765.712081	44.153293
3501.883477	320761.580702	44.158298
3501.732700	320760.306936	44.163303
3501.592148	320743.818103	44.168308
3501.636761	320724.323765	44.173313
3501.358199	320722.103233	44.178317
3501.512519	320710.045832	44.183322
3501.655957	320715.391506	44.188327
3501.489412	320717.732769	44.193332
3501.640212	320704.861818	44.198337
3501.562748	320689.584251	44.203341
3501.628951	320677.515176	44.208346
3501.891459	320677.677792	44.213351
3501.705216	320682.769725	44.218356
3502.079514	320655.667947	44.223361
3501.814164	320643.599817	44.228365
3501.507183	320627.544008	44.233370
3501.981625	320627.877016	44.238375
3501.730725	320613.084467	44.243380
3501.862712	320590.727054	44.248385
3501.947039	320594.759069	44.253389
3501.713943	320587.112557	44.258394
3502.200449	320564.190892	44.263399
3501.872888	320560.502451	44.268404
3501.451766	320550.239496	44.273409
3501.507224	320528.250184	44.278413
3501.592056	320509.461801	44.283418
3501.795738	320508.615985	44.288423
3502.078023	320509.360647	44.293428
3502.130740	320488.491135	44.298433
3501.659187	320483.985655	44.303437
3502.028405	320466.170421	44.308442
3502.056556	320458.661129	44.313447
3501.674390	320442.031867	44.318452
3501.671138	320431.016653	44.323457
3501.831647	320434.502517	44.328461
3501.564389	320411.418764	44.333466
3502.155903	320404.457406	44.338471
3501.519953	320398.069559	44.343476
3501.827131	320383.927465	44.348481
3501.766814	320381.469268	44.353485
3501.441537	320354.018736	44.358490
3502.150927	320344.265891	44.363495
3501.655496	320343.020553	44.368500
3501.467852	320332.593840	44.373505
3501.889201	320325.684514	44.378509
3501.692212	320308.644638	44.383514
3501.951464	320306.594411	44.388519
3501.721532	320306.579607	44.393524
3501.986394	320278.477067	44.398529
3502.004124	320279.593824	44.403533
3501.739213	320264.905109	44.408538
3501.868491	320236.620211	44.413543
3501.847710	320228.380742	44.418548
3501.915250	320219.745850	44.423553
3501.458675	320209.717323	44.428557
3501.671251	320194.572321	44.433562
3501.577724	320180.009428	44.438567
3501.541983	320178.132518	44.443572
3501.878803	320187.594896	44.448577
3501.783745	320175.220159	44.453581
3501.554226	320149.077453	44.458586
3501.585772	320137.395259	44.463591
3501.064628	320142.208881	44.468596
3501.681956	320131.605388	44.473601
3501.405541	320139.052050	44.478605
3501.633327	320133.623088	44.483610
3501.397998	320111.246528	44.488615
3501.297900	320108.082187	44.493620
3501.839132	320105.708016	44.498625
3501.559167	320105.421184	44.503629
3501.850931	320099.422515	44.508634
3502.047527	320083.084246	44.513639
3501.486640	320075.768739	44.518644
3501.818081	320061.088485	44.523649
3501.755147	320064.736517	44.528653
3501.608243	320045.246370	44.533658
3501.325450	320028.804940	44.538663
3501.287163	320019.804938	44.543668
3501.439087	320020.391902	44.548673
3501.807979	320022.420524	44.553677
3501.394589	320019.381480	44.558682
3501.757194	320009.555571	44.563687
3501.742920	319992.665091	44.568692
3501.939449	319972.968574	44.573697
3501.847571	319971.685575	44.578701
3501.920135	319961.726912	44.583706
3501.920237	319937.023759	44.588711
3501.673844	319931.541699	44.593716
3501.792015	319928.088811	44.598721
3502.078000	319909.217835	44.603725
3501.756664	319893.952669	44.608730
3501.885446	319890.218267	44.613735
3501.694077	319890.731697	44.618740
3501.938083	319867.694927	44.623745
3501.814672	319853.569094	44.628749
3501.868366	319850.813190	44.633754
3501.789569	319839.071842	44.638759
3501.313449	319825.382759	44.643764
3501.876937	319806.417471	44.648769
3501.734369	319813.156352	44.653773
3501.688431	319812.476754	44.658778
3501.557164	319782.654941	44.663783
3501.435199	319773.489881	44.668788
3501.641968	319765.596366	44.673793
3501.575300	319766.242949	44.678797
3501.783414	319763.513780	44.683802
3502.085358	319746.751855	44.688807
3501.170922	319735.446416	44.693812
3501.696181	319724.882659	44.698817
3501.441609	319718.307879	44.703821
3501.744992	319725.714850	44.708826
3501.784502	319712.937324	44.713831
3501.475465	319701.867965	44.718836
3501.625169	319693.805270	44.723841
3501.518593	319685.273815	44.728845
3501.383225	319686.338199	44.733850
3501.572337	319675.369042	44.738855
3501.426427	319666.105938	44.743860
3501.776511	319648.166152	44.748865
3501.483301	319656.048023	44.753869
3501.268360	319656.590582	44.758874
3501.147885	319650.554534	44.763879
3501.385428	319655.275039	44.768884
3501.548702	319651.484342	44.773889
3501.540293	319643.802534	44.778893
3501.290419	319622.598290	44.783898
3501.268701	319617.106506	44.788903
3501.468202	319608.043801	44.793908
3501.741602	319610.850610	44.798913
3501.665631	319614.398953	44.803917
3501.264377	319610.645627	44.808922
3501.566274	319609.682674	44.813927
3501.294847	319589.702964	44.818932
3501.483841	319578.097769	44.823937
3501.266400	319579.276751	44.828941
3501.650028	319567.539359	44.833946
3501.433015	319560.882359	44.838951
3501.641645	319573.697722	44.843956
3501.730627	319556.205779	44.848961
3501.618737	319535.615953	44.853965
3501.752547	319531.422790	44.858970
3501.664425	319523.499010	44.863975
3501.420709	319519.644723	44.868980
3501.729526	319519.672898	44.873985
3501.605627	319493.436957	44.878989
3501.185681	319490.424341	44.883994
3501.616480	319482.063248	44.888999
3501.828927	319484.625181	44.894004
3501.771309	319474.152490	44.899009
3501.488823	319454.479742	44.904013
3501.246614	319451.973604	44.909018
3501.579217	319448.054651	44.914023
3501.307391	319439.345453	44.919028
3501.636267	319434.155013	44.924033
3501.554610	319431.623774	44.929037
3501.899607	319421.240774	44.934042
3501.499084	319399.449380	44.939047
3501.642388	319391.972781	44.944052
3501.681952	319394.790720	44.949057
3501.803388	319392.660231	44.954061
3501.683688	319378.966167	44.959066
3501.757499	319357.787513	44.964071
3501.444617	319368.369300	44.969076
3501.807126	319354.370867	44.974081
3501.980362	319345.490304	44.979085
3501.605506	319324.712516	44.984090
3501.651455	319317.378332	44.989095
3501.483700	319318.651319	44.994100
3501.758843	319311.866456	44.999105
3501.419769	319295.433544	45.004109
3501.338122	319277.179480	45.009114
3501.419514	319273.121695	45.014119
3501.052201	319272.161592	45.019124
3501.444857	319262.432581	45.024129
3501.313844	319276.598646	45.029133
3501.600263	319275.180160	45.034138
3501.784986	319272.988888	45.039143
3501.526239	319250.335686	45.044148
3501.522657	319231.255270	45.049153
3501.532478	319234.230519	45.054157
3501.534096	319233.543477	45.059162
3501.487668	319232.100702	45.064167
3501.424814	319230.355197	45.069172
3501.760275	319219.846433	45.074177
3502.022373	319202.505373	45.079181
3501.402111	319194.410311	45.084186
3501.584863	319187.436340	45.089191
3501.277006	319196.694425	45.094196
3501.745498	319189.726666	45.099201
3501.356302	319167.093814	45.104205
3501.555053	319150.805739	45.109210
3501.892871	319145.181361	45.114215
3501.758751	319149.858260	45.119220
3501.894679	319137.065491	45.124225
3501.759393	319127.495312	45.129229
3501.779461	319114.339027	45.134234
3502.197474	319104.504250	45.139239
3501.561685	319093.434935	45.144244
3501.757960	319074.246880	45.149249
3501.167048	319075.509706	45.154253
3501.293238	319069.104273	45.159258
3501.449617	319070.377476	45.164263
3501.324130	319074.366111	45.169268
3501.638358	319070.551764	45.174273
3501.494165	319045.641687	45.179277
3501.396721	319036.294545	45.184282
3501.478264	319028.445916	45.189287
3501.562478	319036.192569	45.194292
3501.805913	319020.406291	45.199297
3501.421179	319023.748537	45.204301
3501.557283	319007.114020	45.209306
3501.938478	318990.644713	45.214311
3501.818212	318988.551991	45.219316
3501.665039	318985.090567	45.224321
3501.530402	318968.116737	45.229325
3501.402059	318958.621761	45.234330
3501.572563	318953.456024	45.239335
3501.298390	318953.804318	45.244340
3501.447694	318942.179716	45.249345
3501.202398	318961.553846	45.254349
3501.655587	318959.015288	45.259354
3501.512881	318948.581213	45.264359
3501.540631	318937.509888	45.269364
3501.448310	318919.664408	45.274369
3501.325968	318918.233491	45.279373
3501.380072	318915.528347	45.284378
3501.463631	318908.010123	45.289383
3501.194427	318906.271423	45.294388
3501.741983	318909.569693	45.299393
3501.679122	318903.473650	45.304397
3501.476271	318880.709749	45.309402
3501.931394	318862.091734	45.314407
3501.419086	318859.704113	45.319412
3501.762614	318854.002481	45.324417
3501.693611	318842.742724	45.329421
3501.611872	318836.013580	45.334426
3501.754250	318825.153281	45.339431
3501.726657	318820.069382	45.344436
3501.774358	318814.464877	45.349441
3501.808656	318798.151497	45.354445
3501.646313	318786.855435	45.359450
3501.719935	318778.270188	45.364455
3501.423654	318787.933618	45.369460
3501.292149	318774.292091	45.374465
3501.746807	318752.239466	45.379469
3501.708011	318744.256948	45.384474
3501.658492	318734.164439	45.389479
3501.606606	318737.530995	45.394484
3501.713958	318727.795586	45.399489
3501.816233	318707.273651	45.404493
3501.156028	318702.288640	45.409498
3501.523649	318695.514664	45.414503
3501.478403	318700.432135	45.419508
3501.597082	318704.687933	45.424513
3501.272205	318700.871702	45.429517
3500.911772	318691.387510	45.434522
3501.514108	318692.438354	45.439527
3501.357623	318682.515206	45.444532
3501.372356	318658.216105	45.449537
3501.348953	318657.838268	45.454541
3501.337205	318661.198555	45.459546
3501.469205	318657.132801	45.464551
3501.671457	318652.165600	45.469556
3501.819361	318652.066282	45.474561
3501.864804	318640.508721	45.479565
3501.600979	318618.415703	45.484570
3501.683474	318611.279221	45.489575
3501.467970	318612.076299	45.494580
3501.631697	318615.231064	45.499585
3501.860680	318596.063127	45.504589
3500.984155	318576.126666	45.509594
3501.360423	318572.124483	45.514599
3501.488611	318576.556900	45.519604
3501.573981	318572.396660	45.524609
3501.695714	318567.925433	45.529613
3501.728139	318566.699285	45.534618
3501.883942	318532.481172	45.539623
3501.855930	318531.722425	45.544628
3501.501701	318523.789181	45.549633
3501.836892	318519.055601	45.554637
3501.665716	318503.613816	45.559642
3501.649422	318494.253872	45.564647
3501.817508	318496.542939	45.569652
3501.666203	318494.582256	45.574657
3501.789810	318466.297089	45.579661
3501.644575	318455.685199	45.584666
3501.643738	318451.182238	45.589671
3501.658875	318460.975147	45.594676
3501.356375	318442.068328	45.599681
3501.757236	318424.654381	45.604685
3501.755957	318415.800911	45.609690
3501.752257	318404.810694	45.614695
3501.623865	318398.902920	45.619700
3501.552440	318394.232895	45.624705
3501.415030	318380.185096	45.629709
3501.730488	318373.037597	45.634714
3502.039825	318359.810418	45.639719
3501.458147	318368.780741	45.644724
3501.555083	318351.083534	45.649729
3501.690454	318342.895620	45.654733
3501.758081	318336.702772	45.659738
3501.994993	318326.107432	45.664743
3501.690728	318320.328911	45.669748
3501.853154	318295.548563	45.674753
3501.700665	318295.954164	45.679757
3501.604515	318300.599776	45.684762
3501.776104	318279.303543	45.689767
3501.826858	318270.212932	45.694772
3501.666812	318264.793487	45.699777
3501.542675	318248.631881	45.704781
3501.528603	318248.786865	45.709786
3501.429484	318243.663196	45.714791
3501.148870	318220.249615	45.719796
3501.638074	318205.009787	45.724801
3501.606905	318215.802232	45.729805
3501.460283	318201.857585	45.734810
3501.968664	318208.469504	45.739815
3501.424092	318207.791510	45.744820
3501.879077	318163.273176	45.749825
3501.667292	318113.007348	45.754829
3501.823384	318009.280819	45.759834
3501.615711	317859.178778	45.764839
3501.404830	317670.124446	45.769844
3500.999311	317411.412674	45.774849
3500.778894	317120.154685	45.779853
3500.291085	316788.711388	45.784858
3500.398209	316403.385900	45.789863
3500.117651	315979.392932	45.794868
3499.799561	315489.121216	45.799873
3498.932849	314963.613793	45.804877
3498.507315	314391.595589	45.809882
3498.142614	313769.460347	45.814887
3497.398498	313109.590275	45.819892
3497.364963	312393.111092	45.824897
3496.439074	311628.286299	45.829901
3495.630893	310813.021818	45.834906
3495.268517	309962.913579	45.839911
3494.572043	309064.722075	45.844916
3493.749720	308101.540477	45.849921
3492.861229	307116.286849	45.854925
3491.874010	306069.392547	45.859930
3491.387406	304978.345696	45.864935
3490.348901	303843.868222	45.869940
3488.995110	302657.751059	45.874945
3488.035905	301434.514405	45.879949
3487.238974	300162.433865	45.884954
3486.420579	298837.335617	45.889959
3485.401032	297474.872490	45.894964
3483.925234	296059.199339	45.899969
3482.508724	294601.762973	45.904973
3481.070756	293114.002790	45.909978
3480.301601	291568.419491	45.914983
3478.744360	289995.631778	45.919988
3477.741879	288354.087064	45.924993
3475.964106	286690.321313	45.929997
3474.443109	284985.868367	45.935002
3472.935593	283232.694032	45.940007
3471.384858	281444.756435	45.945012
3469.821186	279612.960480	45.950017
3468.367485	277745.330692	45.955021
3466.593020	275839.769194	45.960026
3464.773442	273900.636710	45.965031
3463.002003	271921.119654	45.970036
3461.662791	269907.599169	45.975041
3459.116123	267858.039610	45.980045
3457.281509	265767.837198	45.985050
3455.707660	263638.513611	45.990055
3453.527081	261492.027884	45.995060
3451.279121	259285.897165	46.000065
3449.317405	257069.061769	46.005069
3447.210743	254814.265845	46.010074
3445.410515	252524.062767	46.015079
3442.975869	250201.529592	46.020084
3440.672594	247848.356400	46.025089
3438.004973	245471.346112	46.030093
3435.354587	243064.354590	46.035098
3433.294659	240630.350811	46.040103
3430.558840	238181.683974	46.045108
3428.122140	235690.418486	46.050113
3425.523313	233179.067391	46.055117
3422.831893	230644.618008	46.060122
3420.590334	228079.985228	46.065127
3417.494153	225500.760202	46.070132
3414.908863	222888.752437	46.075137
3411.916374	220262.906002	46.080141
3409.287033	217611.975074	46.085146
3406.256184	214931.499687	46.090151
3402.742209	212241.770788	46.095156
3400.314874	209540.408577	46.100161
3397.031650	206816.770664	46.105165
3393.759513	204061.558830	46.110170
3390.363956	201301.413799	46.115175
3387.035598	198540.462233	46.120180
3384.156456	195737.394064	46.125185
3380.676191	192945.859569	46.130189
3376.896682	190144.527200	46.135194
3373.677233	187326.953438	46.140199
3369.860099	184508.044138	46.145204
3366.173444	181675.112237	46.150209
3362.460287	178842.244312	46.155213
3358.731995	175983.218755	46.160218
3355.034714	173139.983104	46.165223
3350.862484	170291.565261	46.170228
3346.973801	167455.954026	46.175233
3342.831667	164600.180675	46.180237
3338.323493	161762.074012	46.185242
3334.477213	158927.858006	46.190247
3329.634404	156113.807722	46.195252
3324.609157	153306.792070	46.200257
3319.713642	150507.352051	46.205261
3314.574746	147734.027250	46.210266
3309.201083	144978.342995	46.215271
3303.730577	142251.184394	46.220276
3298.109597	139491.654601	46.225281
3291.990524	136837.360254	46.230285
3285.796453	134228.124807	46.235290
3279.343791	131659.979241	46.240295
3272.657031	129136.262174	46.245300
3265.783809	126679.361246	46.250305
3259.204155	124276.232990	46.255309
3251.669366	121934.443021	46.260314
3244.072592	119657.188734	46.265319
3235.691914	117452.764067	46.270324
3227.676516	115337.370016	46.275329
3219.060020	113326.555604	46.280333
3210.385771	111388.523814	46.285338
3201.633160	109543.597190	46.290343
3191.973516	107802.253534	46.295348
3183.321813	106163.950447	46.300353
3174.565084	104618.068656	46.305357
3165.901180	103169.484838	46.310362
3157.230997	101818.711090	46.315367
3148.809878	100575.737338	46.320372
3140.353897	99421.505942	46.325377
3132.602560	98353.617203	46.330381
3124.997324	97362.415015	46.335386
3118.088231	96440.359164	46.340391
3111.333544	95606.082752	46.345396
3104.776359	94844.741888	46.350401
3098.620576	94127.160530	46.355405
3092.789584	93482.879963	46.360410
3087.211584	92876.123233	46.365415
3082.034094	92326.040017	46.370420
3076.914927	91800.583381	46.375425
3071.917170	91322.410820	46.380429
3067.574833	90877.510372	46.385434
3063.528228	90457.550710	46.390439
3059.170527	90055.052881	46.395444
3055.062973	89656.371222	46.400449
3051.247813	89301.433177	46.405453
3047.258398	88956.602155	46.410458
3044.031546	88612.405500	46.415463
3040.551224	88285.290313	46.420468
3037.401576	87953.121181	46.425473
3034.073240	87636.420359	46.430477
3030.758886	87318.844112	46.435482
3027.600063	87002.720724	46.440487
3023.963811	86690.423272	46.445492
3021.097805	86374.514958	46.450497
3017.848509	86060.385088	46.455501
3014.396680	85755.500847	46.460506
3011.099642	85431.780821	46.465511
3007.686709	85129.387072	46.470516
3004.176054	84813.723558	46.475521
3000.735336	84496.655152	46.480525
2997.430618	84195.702474	46.485530
2994.239408	83888.840808	46.490535
2990.504081	83585.344962	46.495540
2987.236744	83277.828469	46.500545
2984.098523	82965.366325	46.505549
2980.419196	82661.604774	46.510554
2977.465384	82353.769753	46.515559
2973.253402	82042.857560	46.520564
2969.811235	81743.654386	46.525569
2965.947465	81442.170383	46.530573
2962.505350	81139.632893	46.535578
2958.956884	80837.648774	46.540583
2955.048391	80549.467688	46.545588
2951.608216	80263.426441	46.550593
2948.081315	79972.625858	46.555597
2944.189309	79691.030509	46.560602
2940.598393	79403.256143	46.565607
2936.783411	79125.337885	46.570612
2933.612762	78849.722164	46.575617
2929.478736	78580.407148	46.580621
2926.145488	78303.171170	46.585626
2922.419628	78041.507029	46.590631
2919.112041	77775.804657	46.595636
2915.401611	77510.498069	46.600641
2911.795010	77235.970014	46.605645
2908.254417	76985.234728	46.610650
2904.541831	76714.195668	46.615655
2901.038200	76473.276537	46.620660
2897.313716	76217.598650	46.625665
2893.917494	75959.522366	46.630669
2890.294992	75724.508482	46.635674
2886.713167	75463.926004	46.640679
2883.278131	75212.517492	46.645684
2879.449371	74967.763861	46.650689
2875.923970	74725.149280	46.655693
2872.393658	74483.782171	46.660698
2868.848787	74242.089334	46.665703
2864.905496	74003.457928	46.670708
2861.401828	73767.439339	46.675713
2858.336099	73530.401943	46.680717
2854.870598	73298.267326	46.685722
2851.358130	73057.583325	46.690727
2847.773353	72828.607977	46.695732
2844.900603	72579.891793	46.700737
2840.955614	72341.224759	46.705741
2837.256113	72109.048254	46.710746
2834.094978	71866.186860	46.715751
2830.524230	71634.095979	46.720756
2826.966372	71391.999378	46.725761
2823.876940	71153.844165	46.730765
2820.197662	70908.787086	46.735770
2816.861247	70666.662539	46.740775
2813.092003	70439.222386	46.745780
2809.354117	70194.409713	46.750785
2806.242888	69953.437383	46.755789
2802.762497	69720.676388	46.760794
2799.550609	69474.334427	46.765799
2795.773476	69229.403653	46.770804
2792.207758	68985.978403	46.775809
2788.706681	68748.125383	46.780813
2785.340971	68511.726146	46.785818
2781.760715	68271.661707	46.790823
2778.348691	68044.675481	46.795828
2774.778559	67789.823095	46.800833
2771.546221	67546.149813	46.805837
2767.740331	67318.044557	46.810842
2764.509938	67066.358223	46.815847
2760.819088	66823.975950	46.820852
2757.621608	66576.212180	46.825857
2754.165141	66335.492711	46.830861
2750.780914	66089.464036	46.835866
2747.244258	65840.757565	46.840871
2743.323336	65600.282740	46.845876
2739.768377	65359.759308	46.850881
2736.455333	65112.624542	46.855885
2732.913266	64875.232916	46.860890
2729.297878	64628.188267	46.865895
2726.012077	64390.342215	46.870900
2722.717453	64136.359277	46.875905
2719.207443	63893.551534	46.880909
2715.539460	63649.647448	46.885914
2712.025443	63402.065874	46.890919
2708.424118	63156.309243	46.895924
2704.836802	62905.253328	46.900929
2701.783303	62663.230255	46.905933
2698.467383	62411.787802	46.910938
2695.242047	62165.220559	46.915943
2691.460968	61919.866017	46.920948
2688.071697	61667.763509	46.925953
2684.471382	61398.244144	46.930957
2680.760137	61162.183593	46.935962
2677.326434	60902.867440	46.940967
2673.941837	60657.526901	46.945972
2670.364909	60401.678050	46.950977
2667.268572	60145.598047	46.955981
2663.081992	59897.420619	46.960986
2659.895876	59643.035250	46.965991
2656.252529	59392.823450	46.970996
2652.782490	59142.726717	46.976001
2649.078265	58892.910322	46.981005
2645.923495	58641.424147	46.986010
2642.455280	58383.688465	46.991015
2638.678541	58129.874533	46.996020
2635.179513	57884.503663	47.001025
2631.683264	57638.906420	47.006029
2628.341997	57385.730187	47.011034
2624.900196	57129.621809	47.016039
2621.399326	56878.855336	47.021044
2617.951668	56628.616149	47.026049
2614.331530	56363.019857	47.031053
2610.628074	56120.884173	47.036058
2607.238925	55856.475611	47.041063
2603.793605	55603.778621	47.046068
2600.115105	55357.275203	47.051073
2596.623706	55101.450099	47.056077
2592.756031	54858.394894	47.061082
2589.589056	54601.813832	47.066087
2586.229392	54362.510022	47.071092
2582.814440	54097.554073	47.076097
2579.245136	53847.039616	47.081101
2575.456536	53591.512071	47.086106
2572.354352	53329.199470	47.091111
2569.150580	53086.071360	47.096116
2565.552562	52826.607982	47.101121
2562.092403	52556.385503	47.106125
2558.382878	52312.665723	47.111130
2554.811776	52050.980014	47.116135
2551.488324	51795.107489	47.121140
2548.097597	51536.710805	47.126145
2544.543770	51276.439407	47.131149
2540.892526	51012.303889	47.136154
2537.466541	50757.061475	47.141159
2534.086427	50508.297707	47.146164
2530.663010	50242.942762	47.151169
2527.017221	49984.895082	47.156173
2523.557674	49726.059972	47.161178
2520.343560	49466.104700	47.166183
2516.363777	49206.234081	47.171188
2512.687784	48939.665058	47.176193
2509.429663	48669.107489	47.181197
2505.688794	48420.562290	47.186202
2502.072683	48157.881198	47.191207
2498.582956	47900.371717	47.196212
2495.019652	47652.117916	47.201217
2491.715362	47378.126135	47.206221
2488.164777	47129.850683	47.211226
2484.957078	46872.086753	47.216231
2481.597590	46608.140320	47.221236
2477.827700	46348.364636	47.226241
2474.539410	46081.996799	47.231245
2470.902436	45829.182753	47.236250
2467.329970	45558.140664	47.241255
2464.064940	45300.276826	47.246260
2460.344316	45038.092265	47.251265
2457.409888	44775.794129	47.256269
2453.533648	44513.963485	47.261274
2450.042834	44248.162787	47.266279
2446.527995	43984.106623	47.271284
2443.083776	43718.216175	47.276289
2439.479115	43449.208631	47.281293
2435.940661	43184.157367	47.286298
2432.701239	42922.093649	47.291303
2429.364649	42651.417788	47.296308
2425.749306	42388.214365	47.301313
2422.491136	42115.820683	47.306317
2418.369082	41852.373186	47.311322
2415.349069	41574.628826	47.316327
2411.712643	41302.038070	47.321332
2408.466148	41034.950573	47.326337
2404.708264	40767.356645	47.331341
2401.403742	40504.628082	47.336346
2397.647827	40219.914507	47.341351
2394.395994	39953.551200	47.346356
2391.161913	39683.891369	47.351361
2387.674714	39410.438587	47.356365
2383.975747	39139.875484	47.361370
2380.316963	38852.850432	47.366375
2377.038636	38587.123028	47.371380
2373.565768	38312.394832	47.376385
2370.204468	38021.986758	47.381389
2366.198928	37758.412096	47.386394
2362.904358	37484.864786	47.391399
2359.372845	37206.476480	47.396404
2356.136350	36931.075957	47.401409
2352.610460	36656.427933	47.406413
2349.035562	36371.495878	47.411418
2345.340097	36092.761003	47.416423
2341.899544	35816.963006	47.421428
2338.398880	35539.206501	47.426433
2335.013697	35261.327795	47.431437
2331.692971	34994.295030	47.436442
2328.750024	34706.440192	47.441447
2324.858196	34423.523538	47.446452
2321.211475	34127.989898	47.451457
2317.974172	33851.551802	47.456461
2314.294532	33569.640269	47.461466
2311.125454	33277.961074	47.466471
2307.358284	32987.076720	47.471476
2303.928233	32707.204039	47.476481
2300.413237	32414.792333	47.481485
2296.824338	32124.189975	47.486490
2293.736840	31837.278029	47.491495
2290.162859	31556.105953	47.496500
2286.635854	31260.454585	47.501505
2283.627661	30964.833998	47.506509
2279.749567	30668.358694	47.511514
2276.172257	30368.335875	47.516519
2272.818050	30077.028289	47.521524
2269.159576	29783.079002	47.526529
2265.981428	29481.080041	47.531533
2262.336280	29183.708716	47.536538
2258.937899	28891.049621	47.541543
2255.436299	28591.224607	47.546548
2252.058363	28290.427748	47.551553
2248.707259	27978.997824	47.556557
2245.015490	27684.475458	47.561562
2241.410885	27376.585954	47.566567
2238.114759	27072.169654	47.571572
2234.824280	26773.041671	47.576577
2231.565540	26469.496649	47.581581
2227.957303	26159.395736	47.586586
2224.662070	25846.278918	47.591591
2220.879800	25535.581176	47.596596
2217.608508	25216.432055	47.601601
2214.166705	24898.176351	47.606605
2210.414391	24583.883463	47.611610
2207.138325	24259.029032	47.616615
2203.960155	23948.261297	47.621620
2200.292141	23636.516991	47.626625
2196.926107	23303.417951	47.631629
2192.696889	22996.231581	47.636634
2189.780145	22679.227745	47.641639
2186.319514	22364.075215	47.646644
2182.915392	22037.433462	47.651649
2179.915688	21710.271367	47.656653
2175.749671	21399.184852	47.661658
2171.987462	21058.488657	47.666663
2168.983090	20743.170191	47.671668
2165.583002	20420.767034	47.676673
2162.102993	20092.370330	47.681677
2158.688242	19757.938670	47.686682
2155.058776	19421.494036	47.691687
2151.415156	19102.229060	47.696692
2147.935342	18774.380152	47.701697
2144.322384	18443.884697	47.706701
2140.818982	18119.274433	47.711706
2137.793782	17793.290037	47.716711
2133.963679	17463.776264	47.721716
2130.489683	17137.049755	47.726721
2127.005051	16799.661945	47.731725
2123.392119	16482.455556	47.736730
2119.574174	16153.019225	47.741735
2115.826155	15825.540822	47.746740
2112.063090	15506.638761	47.751745
2108.636150	15186.653997	47.756749
2104.663018	14878.798476	47.761754
2100.778887	14574.606888	47.766759
2097.166264	14267.284244	47.771764
2092.522074	13994.721811	47.776769
2088.381017	13726.222726	47.781773
2083.114392	13483.536389	47.786778
2078.470150	13245.080637	47.791783
2074.659650	13014.247890	47.796788
2070.049473	12792.509187	47.801793
2066.448473	12579.137956	47.806797
2062.462284	12385.711438	47.811802
2058.891546	12172.289418	47.816807
2055.084997	11985.838693	47.821812
2051.420867	11784.931344	47.826817
2048.376100	11606.966742	47.831821
2044.832165	11413.629813	47.836826
2042.036661	11218.465107	47.841831
2038.470032	11030.900477	47.846836
2034.852115	10839.075260	47.851841
2031.410149	10648.835790	47.856845
2028.032248	10473.916102	47.861850
2024.822844	10276.923441	47.866855
2021.188351	10091.031291	47.871860
2017.963493	9899.185879	47.876865
2014.801708	9703.837885	47.881869
2011.173552	9515.592204	47.886874
2007.824428	9325.801196	47.891879
2004.438252	9123.198131	47.896884
2001.226154	8929.755873	47.901889
1997.947838	8730.736049	47.906893
1994.098278	8539.534195	47.911898
1990.961842	8334.077243	47.916903
1987.403327	8147.255752	47.921908
1983.712811	7945.320911	47.926913
1980.166071	7748.195795	47.931917
1976.851772	7555.600506	47.936922
1973.494344	7349.802940	47.941927
1969.986861	7160.242507	47.946932
1966.305110	6954.408325	47.951937
1963.447185	6748.207001	47.956941
1959.786634	6550.428889	47.961946
1956.048672	6351.772521	47.966951
1952.904539	6154.256522	47.971956
1949.003092	5945.195566	47.976961
1946.038079	5742.870746	47.981965
1942.484850	5544.915806	47.986970
1938.834292	5344.804073	47.991975
1935.252613	5136.484028	47.996980
1931.341431	4930.271790	48.001985
1928.198008	4727.356381	48.006989
1924.422436	4536.289115	48.011994
1920.922848	4330.933836	48.016999
1917.843191	4135.850496	48.022004
1914.118328	3935.506408	48.027009
1910.613435	3736.364253	48.032013
1907.232207	3534.100643	48.037018
1903.888795	3326.428612	48.042023
1900.158175	3125.138757	48.047028
1896.572881	2928.040106	48.052033
1893.404574	2724.932682	48.057037
1889.557234	2525.965047	48.062042
1885.775751	2324.815497	48.067047
1882.240365	2122.753213	48.072052
1878.710706	1915.851179	48.077057
1875.024033	1721.509097	48.082061
1871.269157	1541.256730	48.087066
1867.587911	1349.749674	48.092071
1864.179629	1163.254863	48.097076
1860.296835	976.181311	48.102081
1857.097911	806.480293	48.107085
1852.852415	632.065917	48.112090
1849.479500	452.783542	48.117095
1846.054646	279.285116	48.122100
1841.945277	126.409688	48.127105
1835.882799	14.426384	48.132109
1825.034996	61.281046	48.137114
1817.837256	64.372284	48.142119
1813.444403	63.028697	48.147124
1810.720064	69.456907	48.152129
1808.262413	70.740163	48.157133
1805.964993	73.444205	48.162138
1803.127435	79.845845	48.167143
1800.174182	65.539484	48.172148
1796.912292	76.873465	48.177153
1794.007476	77.030784	48.182157
1790.617595	63.827323	48.187162
1786.858660	63.504529	48.192167
1783.495701	65.460986	48.197172
1780.145850	71.151848	48.202177
1776.703840	62.749720	48.207181
1773.186182	67.792954	48.212186
1770.134147	67.660101	48.217191
1766.725260	76.378478	48.222196
1763.401842	83.368701	48.227201
1760.150350	71.592614	48.232205
1756.191387	75.860181	48.237210
1752.855760	77.761750	48.242215
1749.412769	76.547952	48.247220
1745.389415	71.194972	48.252225
1742.628256	64.818711	48.257229
1739.143095	72.609380	48.262234
1736.048591	68.468314	48.267239
1732.231507	69.227171	48.272244
1728.517793	74.396016	48.277249
1725.341721	71.991993	48.282253
1721.759899	72.622284	48.287258
1718.243261	75.748110	48.292263
1715.105025	69.756740	48.297268
1711.504501	73.553768	48.302273
1707.833755	76.105756	48.307277
1704.386067	75.398918	48.312282
1701.279321	59.591670	48.317287
1698.022248	71.728521	48.322292
1694.120118	67.584149	48.327297
1690.534200	57.594205	48.332301
1686.887914	72.057255	48.337306
1683.962054	64.624767	48.342311
1680.052108	61.076421	48.347316
1676.789579	69.227739	48.352321
1673.463878	61.601565	48.357325
1669.782944	68.147879	48.362330
1666.469014	68.761573	48.367335
1663.151245	63.756955	48.372340
1659.488064	74.498862	48.377345
1655.742600	67.093415	48.382349
1652.171826	73.957858	48.387354
1648.760892	63.396368	48.392359
1645.608071	63.174921	48.397364
1641.835150	82.226338	48.402369
1638.810746	69.149241	48.407373
1635.095752	70.271812	48.412378
1631.721307	66.386569	48.417383
1628.219680	63.710824	48.422388
1624.451205	64.129913	48.427393
1621.365307	62.613495	48.432397
1617.706969	66.438582	48.437402
1614.002992	67.891635	48.442407
1610.551551	60.949565	48.447412
1606.840599	67.532233	48.452417
1603.426959	64.308043	48.457421
1599.823461	69.279341	48.462426
1596.585928	75.329168	48.467431
1592.997718	66.813952	48.472436
1589.770820	64.338834	48.477441
1586.241843	61.176996	48.482445
1582.730400	75.350044	48.487450
1578.762042	67.568222	48.492455
1575.631839	69.608538	48.497460
1572.488474	75.165899	48.502465
1569.249474	63.400598	48.507469
1565.497610	76.380562	48.512474
1561.661235	68.847013	48.517479
1558.230373	68.289455	48.522484
1554.406129	64.414530	48.527489
1551.194621	56.988836	48.532493
1547.634761	62.905621	48.537498
1544.321338	66.841265	48.542503
1540.713009	58.474759	48.547508
1537.027429	65.202175	48.552513
1534.001321	59.031971	48.557517
1530.188170	72.746044	48.562522
1526.459288	65.799973	48.567527
1523.350377	64.853509	48.572532
1519.846323	66.379708	48.577537
1516.403593	62.438757	48.582541
1512.243532	66.978332	48.587546
1509.263254	64.901245	48.592551
1506.069127	63.857391	48.597556
1502.126170	62.646005	48.602561
1499.009445	63.374421	48.607565
1495.136685	69.318053	48.612570
1491.880245	73.700381	48.617575
1488.484888	65.351180	48.622580
1484.990288	69.884683	48.627585
1481.393734	60.776030	48.632589
1477.814760	64.572921	48.637594
1474.200126	58.187968	48.642599
1470.742918	58.384384	48.647604
1467.128065	57.871476	48.652609
1463.973521	49.358048	48.657613
1460.582789	61.180502	48.662618
1456.777496	63.617590	48.667623
1453.374022	56.250456	48.672628
1449.577273	60.866064	48.677633
1446.264422	59.034046	48.682637
1442.678758	70.953462	48.687642
1439.258660	64.917727	48.692647
1436.103449	65.503487	48.697652
1432.006424	62.927339	48.702657
1428.826557	59.508432	48.707661
1425.599844	68.707749	48.712666
1421.905947	61.639189	48.717671
1418.155100	58.939256	48.722676
1414.280106	66.348101	48.727681
1411.367153	63.276566	48.732685
1407.866685	54.102288	48.737690
1404.459133	65.579373	48.742695
1400.937744	59.198838	48.747700
1397.110908	67.210763	48.752705
1393.897951	56.798733	48.757709
1390.452218	55.310242	48.762714
1386.909673	65.387919	48.767719
1383.505938	59.134509	48.772724
1379.853310	63.420694	48.777729
1376.344249	61.287214	48.782733
1372.894948	54.572701	48.787738
1369.309484	60.449255	48.792743
1366.011993	55.954110	48.797748
1362.099599	56.392660	48.802753
1358.681200	60.006264	48.807757
1355.427596	60.446098	48.812762
1351.754935	57.892143	48.817767
1348.467428	57.733002	48.822772
1344.558392	57.304155	48.827777
1341.611649	62.077811	48.832781
1338.245074	65.873138	48.837786
1334.571825	70.722559	48.842791
1330.916058	59.294689	48.847796
1327.081610	66.156207	48.852801
1323.322777	63.909984	48.857805
1319.982024	64.132515	48.862810
1316.750820	59.842149	48.867815
1313.382343	58.765540	48.872820
1309.697253	70.064631	48.877825
1306.468476	55.203658	48.882829
1302.820189	60.460472	48.887834
1299.801653	56.836020	48.892839
1296.108085	61.416546	48.897844
1292.276661	69.574758	48.902849
1288.659392	60.333389	48.907853
1284.959765	61.469499	48.912858
1281.731755	65.705065	48.917863
1278.150112	55.480515	48.922868
1274.549710	57.015552	48.927873
1271.004976	53.043208	48.932877
1267.998022	62.575158	48.937882
1264.517044	59.883661	48.942887
1261.034660	65.731458	48.947892
1257.369637	63.372499	48.952897
1253.836668	55.880184	48.957901
1249.876272	58.689644	48.962906
1246.599111	57.510177	48.967911
1243.161430	55.662971	48.972916
1239.511922	58.290887	48.977921
1236.513871	59.140012	48.982925
1232.969107	62.589938	48.987930
1229.542437	67.650731	48.992935
1226.226918	61.453176	48.997940
1222.477985	60.806322	49.002945
1218.796043	58.304493	49.007949
1215.453763	50.339414	49.012954
1211.423238	57.307594	49.017959
1208.170021	56.491391	49.022964
1204.728988	52.294029	49.027969
1201.298360	56.301906	49.032973
1197.883075	62.085432	49.037978
1194.087077	62.164138	49.042983
1191.032252	61.456089	49.047988
1186.788208	70.773603	49.052993
1183.684016	65.083987	49.057997
1180.287582	64.375637	49.063002
1176.844375	68.059623	49.068007
1173.514469	60.443800	49.073012
1169.378290	60.888987	49.078017
1166.306557	58.946552	49.083021
1162.338299	64.500282	49.088026
1158.825993	60.380533	49.093031
1156.007115	64.881118	49.098036
1152.239400	67.736382	49.103041
1149.231782	60.971792	49.108045
1145.265287	64.959177	49.113050
1141.623097	71.123100	49.118055
1138.492067	58.404603	49.123060
1134.828441	66.292982	49.128065
1131.077994	59.973729	49.133069
1127.588503	57.872082	49.138074
1124.095000	57.874983	49.143079
1120.468244	57.642480	49.148084
1116.638638	45.488956	49.153089
1113.837816	52.555715	49.158093
1110.275011	56.704538	49.163098
1106.983297	64.129734	49.168103
1103.227215	60.196871	49.173108
1099.590864	70.849307	49.178113
1096.594710	58.669702	49.183117
1092.513635	59.808655	49.188122
1089.036873	71.508631	49.193127
1085.545783	51.205988	49.198132
1081.865540	63.637015	49.203137
1078.751751	53.203267	49.208141
1075.653977	56.953425	49.213146
1071.898218	54.833376	49.218151
1068.520736	60.481307	49.223156
1064.693431	53.022502	49.228161
1060.976440	53.936784	49.233165
1057.377908	60.286886	49.238170
1053.910268	50.639385	49.243175
1050.823415	48.825908	49.248180
1047.183080	60.276250	49.253185
1043.757751	56.427671	49.258189
1040.045526	55.477747	49.263194
1036.697659	59.412607	49.268199
1032.965188	53.533516	49.273204
1029.280811	52.443193	49.278209
1026.402305	56.130561	49.283213
1022.581634	49.496486	49.288218
1019.175555	59.692101	49.293223
1015.796986	52.039673	49.298228
1012.265153	60.176375	49.303233
1008.433791	50.902221	49.308237
1004.989427	53.260816	49.313242
1001.282000	43.280724	49.318247
998.083756	44.825659	49.323252
994.922199	47.206418	49.328257
991.437894	49.773753	49.333261
987.680974	53.971993	49.338266
984.064865	54.142840	49.343271
980.590746	57.822236	49.348276
977.005075	53.378689	49.353281
973.468129	55.435413	49.358285
970.237235	46.051443	49.363290
966.619950	62.987359	49.368295
963.127425	53.248880	49.373300
959.379357	67.936848	49.378305
956.247737	59.043538	49.383309
952.780343	64.879592	49.388314
949.094875	68.041595	49.393319
945.573458	61.129739	49.398324
941.913005	55.445057	49.403329
938.760603	52.911048	49.408333
935.066249	56.697711	49.413338
931.479247	55.677602	49.418343
928.224065	47.550309	49.423348
924.571657	56.990409	49.428353
920.872468	49.865956	49.433357
917.573890	53.935506	49.438362
913.929248	55.120092	49.443367
910.899694	52.389687	49.448372
907.027580	65.606951	49.453377
903.539606	50.562126	49.458381
900.209171	56.038224	49.463386
896.495261	52.554433	49.468391
893.092484	47.920932	49.473396
889.269707	56.163337	49.478401
885.818490	52.195489	49.483405
882.466502	52.277560	49.488410
878.869400	67.739183	49.493415
875.801431	45.152597	49.498420
872.102058	67.755064	49.503425
868.717968	56.715152	49.508429
864.807482	58.311547	49.513434
861.422754	60.850681	49.518439
857.950800	59.274743	49.523444
854.307250	62.164458	49.528449
850.704713	59.799043	49.533453
847.344343	53.276469	49.538458
843.991329	52.824036	49.543463
840.562366	50.251111	49.548468
836.897803	61.790729	49.553473
833.690896	50.163102	49.558477
829.896981	52.025997	49.563482
826.369926	54.552628	49.568487
823.204216	54.716283	49.573492
819.384991	62.825281	49.578497
815.706579	52.040293	49.583501
812.301496	55.626677	49.588506
808.729553	51.696747	49.593511
805.572217	43.851580	49.598516
801.901263	53.095303	49.603521
798.551120	44.549498	49.608525
795.188713	52.897015	49.613530
791.388563	56.206747	49.618535
787.998042	50.005299	49.623540
784.255047	49.462095	49.628545
780.747816	49.676082	49.633549
777.649472	52.126104	49.638554
774.109307	51.298041	49.643559
770.356371	49.639587	49.648564
766.743297	47.275858	49.653569
763.237812	53.219174	49.658573
759.948681	54.775257	49.663578
756.452337	58.597416	49.668583
752.814380	51.419157	49.673588
749.340605	53.386975	49.678593
746.250120	49.270944	49.683597
742.579627	53.319696	49.688602
738.670398	51.312405	49.693607
735.442574	47.246360	49.698612
731.289724	59.014334	49.703617
728.017925	49.766586	49.708621
724.836965	51.710703	49.713626
720.930965	50.395782	49.718631
718.162085	46.330639	49.723636
714.910127	52.904988	49.728641
711.156780	51.287752	49.733645
707.312615	52.899135	49.738650
703.566199	53.625173	49.743655
700.549195	57.558948	49.748660
696.626273	54.474972	49.753665
693.410401	48.088025	49.758669
689.822273	58.853245	49.763674
686.152592	65.078569	49.768679
682.955624	50.905778	49.773684
679.222038	45.387694	49.778689
676.138959	52.514578	49.783693
672.402580	57.139989	49.788698
668.865143	56.321030	49.793703
665.840908	49.100484	49.798708
661.499977	51.735650	49.803713
658.409017	46.139081	49.808717
654.691727	37.771065	49.813722
650.960427	49.605920	49.818727
647.694741	39.167678	49.823732
644.189406	51.584083	49.828737
640.792619	44.440877	49.833741
637.638185	52.895074	49.838746
633.680658	48.611151	49.843751
630.151622	48.284440	49.848756
626.612575	52.622698	49.853761
623.106414	52.169021	49.858765
619.643299	54.764806	49.863770
616.220438	53.522962	49.868775
613.055989	43.011929	49.873780
608.881137	50.787546	49.878785
605.744725	44.638128	49.883789
602.080319	53.956820	49.888794
599.255429	53.428092	49.893799
595.927368	48.403358	49.898804
591.580861	53.212939	49.903809
588.083058	44.807413	49.908813
584.988210	49.924006	49.913818
581.399865	50.637992	49.918823
577.575273	48.443510	49.923828
573.613336	52.800562	49.928833
570.390821	51.441936	49.933837
567.381544	52.356302	49.938842
563.936983	55.262415	49.943847
560.246082	55.062323	49.948852
556.411412	60.516262	49.953857
552.885907	54.377182	49.958861
549.576411	59.353399	49.963866
545.749395	57.007448	49.968871
543.252822	47.562435	49.973876
539.413950	43.810470	49.978881
535.930374	52.648441	49.983885
532.040845	57.215633	49.988890
528.057544	59.918235	49.993895
524.882255	51.563462	49.998900
521.849431	48.087057	50.003905
518.277217	61.599151	50.008909
514.880675	55.715136	50.013914
511.189422	54.828582	50.018919
507.984952	51.224040	50.023924
504.183867	48.700041	50.028929
500.652872	45.311161	50.033933
496.920510	52.179119	50.038938
493.314202	57.853578	50.043943
489.965467	50.259981	50.048948
486.342898	56.047721	50.053953
482.886936	41.611877	50.058957
480.078677	51.843717	50.063962
476.280259	52.584320	50.068967
472.915133	39.463037	50.073972
469.004566	53.787439	50.078977
465.280373	51.960097	50.083981
461.938964	49.794390	50.088986
458.651144	49.274940	50.093991
455.242975	44.212192	50.098996
451.561794	55.710231	50.104001
448.170283	49.803313	50.109005
444.736564	51.948466	50.114010
440.975172	52.828818	50.119015
437.822664	53.066468	50.124020
434.203785	57.689383	50.129025
430.351356	51.364283	50.134029
427.064596	62.885976	50.139034
423.491283	52.170143	50.144039
420.283368	55.093025	50.149044
416.366282	59.626614	50.154049
413.248605	48.557845	50.159053
409.441249	46.344920	50.164058
406.114435	57.053474	50.169063
402.259213	47.966858	50.174068
398.458209	53.235247	50.179073
395.600032	50.588911	50.184077
392.183046	51.390026	50.189082
388.450219	55.356924	50.194087
385.421133	51.408582	50.199092
381.879717	51.438250	50.204097
378.340616	56.415685	50.209101
374.636794	51.864353	50.214106
370.534470	60.612638	50.219111
367.585695	52.504025	50.224116
364.087240	55.947000	50.229121
360.577682	56.594948	50.234125
357.315765	58.773334	50.239130
353.340493	57.649759	50.244135
350.055910	48.499095	50.249140
346.565839	51.475689	50.254145
343.001633	38.584973	50.259149
339.434970	43.620520	50.264154
335.606608	41.414083	50.269159
332.414963	45.375321	50.274164
328.731376	56.196731	50.279169
325.475602	56.384158	50.284173
322.291183	50.947892	50.289178
318.637598	56.465303	50.294183
315.295234	51.974436	50.299188
311.318317	53.059446	50.304193
307.646765	59.712304	50.309197
304.445876	51.301523	50.314202
300.527052	47.628631	50.319207
297.638344	54.165187	50.324212
294.079099	49.240067	50.329217
290.421284	39.157643	50.334221
287.062746	38.573406	50.339226
283.251324	46.611759	50.344231
279.951653	31.787711	50.349236
276.412592	48.531196	50.354241
273.112186	51.291445	50.359245
269.339194	49.338954	50.364250
265.775715	44.256324	50.369255
262.600471	37.657550	50.374260
258.917790	40.284697	50.379265
255.759262	42.329862	50.384269
251.768611	43.692296	50.389274
247.694212	50.677199	50.394279
244.896717	53.406131	50.399284
241.033671	48.734271	50.404289
237.903650	46.279274	50.409293
234.543190	45.341017	50.414298
230.830886	50.763253	50.419303
227.764897	40.531199	50.424308
224.149001	45.881385	50.429313
220.357107	42.644229	50.434317
216.746270	48.667507	50.439322
213.041756	46.913123	50.444327
209.929032	47.457834	50.449332
206.321458	49.272806	50.454337
202.668849	51.173928	50.459341
199.449778	49.751626	50.464346
195.712872	58.727470	50.469351
192.650959	44.242697	50.474356
188.685721	44.351493	50.479361
185.477595	42.313713	50.484365
181.757192	52.074749	50.489370
178.064731	58.012755	50.494375
174.702895	47.950454	50.499380
171.195973	47.996950	50.504385
167.412997	53.446101	50.509389
164.681107	43.332575	50.514394
160.578651	48.081967	50.519399
157.333047	35.910229	50.524404
153.511007	46.664795	50.529409
149.941465	42.725284	50.534413
146.703557	47.263308	50.539418
143.306936	54.018684	50.544423
140.126243	42.801726	50.549428
136.632821	42.194386	50.554433
132.751278	45.792375	50.559437
129.646970	43.662421	50.564442
126.117898	49.100282	50.569447
122.638603	41.549454	50.574452
118.765470	48.404799	50.579457
115.271439	50.856916	50.584461
111.577565	55.931462	50.589466
108.269815	53.241765	50.594471
104.869237	41.806173	50.599476
100.989969	41.699061	50.604481
97.642542	56.748440	50.609485
94.033849	47.607542	50.614490
90.611202	54.863723	50.619495
87.526421	40.762237	50.624500
83.751999	49.952801	50.629505
80.151310	42.905065	50.634509
76.695940	46.195862	50.639514
72.711073	53.214266	50.644519
70.018455	52.358102	50.649524
66.180265	55.756338	50.654529
62.802189	43.039083	50.659533
58.872148	42.177479	50.664538
55.717969	45.250252	50.669543
51.964502	33.281522	50.674548
48.951007	50.221134	50.679553
45.235206	53.657151	50.684557
41.893270	39.070795	50.689562
38.182962	51.089218	50.694567
34.730393	38.272920	50.699572
30.942450	49.768834	50.704577
27.597075	45.129867	50.709581
24.318017	44.096681	50.714586
20.640058	54.256084	50.719591
17.086698	45.796254	50.724596
13.466022	48.844056	50.729601
10.139247	46.622453	50.734605
6.865639	48.359869	50.739610
3.089846	52.510819	50.744615