Thu Aug 25 10:01:53 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.781035	99.551439	0.000000
1.972713	101.862700	0.005005
1.519826	98.143578	0.010010
1.693923	86.964145	0.015014
1.500074	87.263546	0.020019
1.551410	78.776731	0.025024
0.912070	62.396992	0.030029
0.389314	56.537471	0.035034
0.603947	59.873351	0.040038
0.402146	50.571997	0.045043
0.258778	47.427650	0.050048
-0.519085	43.199473	0.055053
-0.225639	36.576160	0.060058
-0.009362	23.548854	0.065062
-1.114351	28.467720	0.070067
-1.041767	10.062415	0.075072
-1.499006	18.916731	0.080077
-2.102615	8.678611	0.085082
-2.275461	0.625590	0.090086
-2.585114	4.290378	0.095091
-2.582105	-7.415845	0.100096
-3.348272	-8.222669	0.105101
-3.737805	-1.890985	0.110106
-3.440866	-11.653262	0.115110
-4.035983	-4.359227	0.120115
-3.862972	-5.658052	0.125120
-4.474463	-11.690307	0.130125
-4.559589	2.851058	0.135130
-4.546832	-16.563572	0.140134
-4.993665	-9.001707	0.145139
-5.421928	-9.858311	0.150144
-6.234516	-11.670260	0.155149
-6.474640	2.753022	0.160154
-6.678228	-8.528525	0.165158
-6.268615	4.957728	0.170163
-6.622597	-5.363789	0.175168
-6.404807	-6.429185	0.180173
-6.945749	-8.666509	0.185178
-7.551593	-0.684259	0.190182
-7.953246	-3.313566	0.195187
-7.908023	-9.008957	0.200192
-7.948913	0.646982	0.205197
-8.290868	-12.935073	0.210202
-8.581863	-5.850039	0.215206
-9.446358	-3.904817	0.220211
-9.262409	-12.089664	0.225216
-9.690528	-12.142699	0.230221
-9.819562	-2.577355	0.235226
-9.842554	-13.289248	0.240230
-9.806688	-9.912717	0.245235
-10.124424	-3.345510	0.250240
-10.534355	-9.339744	0.255245
-11.145205	-6.754059	0.260250
-11.275048	-9.498719	0.265254
-11.257148	-8.340321	0.270259
-11.796604	-10.520930	0.275264
-12.137953	-5.585681	0.280269
-12.673865	1.866760	0.285274
-12.413268	-16.033302	0.290278
-12.814291	-2.328294	0.295283
-12.638039	4.446253	0.300288
-12.722774	1.925477	0.305293
-13.765067	-0.533851	0.310298
-13.873420	6.035354	0.315302
-13.812074	-1.475393	0.320307
-13.867369	-7.155034	0.325312
-14.413268	1.206966	0.330317
-15.424020	-3.668078	0.335322
-15.073941	-10.233807	0.340326
-15.408540	0.714665	0.345331
-15.533231	-4.612420	0.350336
-15.520931	6.458873	0.355341
-15.456956	5.477687	0.360346
-16.022159	1.450319	0.365350
-16.656671	-2.822452	0.370355
-16.942716	7.675493	0.375360
-16.824011	-5.045438	0.380365
-17.251116	-5.380205	0.385370
-17.060770	-3.226937	0.390374
-18.057919	6.082126	0.395379
-18.149682	0.047529	0.400384
-18.097794	-1.836594	0.405389
-18.566127	-3.284867	0.410394
-18.430611	-0.556697	0.415398
-18.713939	1.727737	0.420403
-19.258314	3.211516	0.425408
-20.033967	4.794807	0.430413
-20.455749	4.114358	0.435418
-19.873389	-3.930437	0.440422
-20.179105	5.630956	0.445427
-20.125465	-1.900728	0.450432
-20.494838	2.966149	0.455437
-20.835391	10.843563	0.460442
-21.074500	2.272580	0.465446
-21.437969	-2.950653	0.470451
-21.494020	-2.185627	0.475456
-22.151527	-6.720548	0.480461
-22.518437	1.157827	0.485466
-22.521919	-2.495645	0.490470
-22.703395	3.964793	0.495475
-22.701238	8.536178	0.500480
-22.494191	2.132059	0.505485
-23.830402	1.946063	0.510490
-23.993012	5.391659	0.515494
-24.205520	-6.442145	0.520499
-24.415884	-4.349479	0.525504
-24.813174	-7.919100	0.530509
-24.412423	4.568795	0.535514
-24.524555	-12.364873	0.540518
-25.380620	-5.064752	0.545523
-25.232286	2.878426	0.550528
-25.566155	-9.024946	0.555533
-25.960506	-2.825385	0.560538
-26.492143	-9.847747	0.565542
-26.896457	-1.719904	0.570547
-27.192186	-2.252425	0.575552
-27.135949	-2.125087	0.580557
-27.468617	-6.138267	0.585562
-26.963713	-7.175884	0.590566
-27.017423	-5.731019	0.595571
-27.869000	-10.384227	0.600576
-27.700091	-7.594852	0.605581
-28.255810	-2.872785	0.610586
-28.572349	-7.853434	0.615590
-29.607228	-0.968218	0.620595
-29.951099	-3.995718	0.625600
-29.846622	0.366644	0.630605
-29.816192	5.392341	0.635610
-29.539856	-7.388087	0.640614
-29.920048	-2.703014	0.645619
-30.384765	-7.255486	0.650624
-30.957220	-5.045974	0.655629
-31.294582	5.485320	0.660634
-31.165720	-12.352974	0.665638
-31.512438	-3.895636	0.670643
-31.732619	-7.008954	0.675648
-31.643507	-2.561928	0.680653
-32.029666	1.848835	0.685658
-32.478342	-4.560106	0.690662
-32.761361	-3.496926	0.695667
-33.090757	-8.247770	0.700672
-32.997955	4.032111	0.705677
-33.816527	4.992542	0.710682
-33.626582	3.842923	0.715686
-34.461807	-1.527855	0.720691
-33.935479	-0.664254	0.725696
-34.192708	4.966497	0.730701
-35.072835	5.835334	0.735706
-35.439402	3.004378	0.740710
-35.922412	11.280598	0.745715
-35.536735	6.727756	0.750720
-35.766551	10.465457	0.755725
-36.093310	13.092054	0.760730
-35.662320	1.268150	0.765734
-35.987787	6.454015	0.770739
-36.980813	7.925834	0.775744
-36.616443	-0.087970	0.780749
-37.574781	6.801075	0.785754
-37.393088	1.147575	0.790758
-37.536837	0.964563	0.795763
-38.084844	10.247547	0.800768
-38.640920	-1.184415	0.805773
-38.738173	8.284204	0.810778
-38.548751	-1.258751	0.815782
-39.077955	7.065834	0.820787
-38.879987	-0.070850	0.825792
-39.396099	-5.713088	0.830797
-40.220335	-1.512094	0.835802
-39.716438	-14.530652	0.840806
-40.219834	-2.745816	0.845811
-40.177174	-5.900318	0.850816
-40.887488	-4.545562	0.855821
-41.494186	1.930882	0.860826
-41.456493	-4.788383	0.865830
-41.713552	-2.691563	0.870835
-41.792672	-0.989617	0.875840
-41.862158	-4.411284	0.880845
-42.312949	3.739662	0.885850
-42.547786	-15.892431	0.890854
-43.444186	0.671125	0.895859
-43.270335	-3.665027	0.900864
-43.308434	-7.506062	0.905869
-43.635184	5.627329	0.910874
-43.733713	-8.062467	0.915878
-43.440551	-0.534289	0.920883
-44.029445	-9.082095	0.925888
-44.067744	-4.380989	0.930893
-44.469974	5.654268	0.935898
-45.251261	-0.791142	0.940902
-45.989920	6.294436	0.945907
-46.077872	-3.904245	0.950912
-46.304448	-4.264103	0.955917
-46.570874	-0.776931	0.960922
-45.833137	1.031141	0.965926
-46.192857	-12.022943	0.970931
-46.311828	7.889433	0.975936
-46.887463	-1.229927	0.980941
-47.529878	6.865624	0.985946
-47.444690	-0.354628	0.990950
-47.790180	3.562547	0.995955
-47.844489	-2.354529	1.000960
-47.883992	0.255531	1.005965
-49.049033	6.268969	1.010970
-49.094767	-6.084508	1.015974
-49.197280	-2.800190	1.020979
-49.372386	-1.532457	1.025984
-49.300986	1.468350	1.030989
-49.650644	5.585494	1.035994
-49.527293	-0.824491	1.040998
-49.972656	-2.206758	1.046003
-50.527244	-0.259471	1.051008
-50.482835	4.011063	1.056013
-51.802452	-0.261925	1.061018
-51.754752	3.856233	1.066022
-51.610884	7.832774	1.071027
-51.800663	-2.900443	1.076032
-51.966392	5.544359	1.081037
-52.635711	11.774354	1.086042
-52.057192	-4.637947	1.091046
-52.659833	0.863427	1.096051
-53.515945	1.652573	1.101056
-53.549982	-10.095295	1.106061
-53.905886	-6.540321	1.111066
-53.682944	-9.017555	1.116070
-53.998457	-0.109526	1.121075
-53.636105	-0.080772	1.126080
-54.270837	-5.163422	1.131085
-55.522095	12.664296	1.136090
-55.278903	0.537626	1.141094
-54.885998	-5.693130	1.146099
-55.159222	3.059578	1.151104
-55.670720	4.130084	1.156109
-56.409871	1.139211	1.161114
-56.333719	4.057015	1.166118
-56.946437	9.170830	1.171123
-56.732235	8.099667	1.176128
-56.568621	-0.426845	1.181133
-57.215607	0.804095	1.186138
-57.376445	-6.092868	1.191142
-58.007217	-0.644033	1.196147
-57.887738	0.893917	1.201152
-58.082818	-1.796229	1.206157
-58.397739	3.369000	1.211162
-59.153371	-2.634339	1.216166
-59.491837	8.273612	1.221171
-59.557388	21.204736	1.226176
-59.195023	-6.452454	1.231181
-59.788527	12.746507	1.236186
-59.949112	0.417350	1.241190
-61.129096	-2.102654	1.246195
-61.120781	-5.564984	1.251200
-60.955664	-1.677196	1.256205
-61.291670	4.959314	1.261210
-61.224803	0.519702	1.266214
-61.904096	-3.448655	1.271219
-61.091975	-4.192727	1.276224
-61.779197	-12.443548	1.281229
-62.456869	-7.651753	1.286234
-62.749568	-5.780302	1.291238
-62.869063	-5.154031	1.296243
-63.067102	-6.843969	1.301248
-62.696284	0.001326	1.306253
-63.426348	10.385345	1.311258
-63.770315	-5.825464	1.316262
-63.735388	-7.877770	1.321267
-64.514627	3.807922	1.326272
-65.082096	-3.322719	1.331277
-65.435430	4.990127	1.336282
-64.979080	-4.762328	1.341286
-65.376622	-4.446830	1.346291
-65.318498	-2.329793	1.351296
-65.604929	-3.129524	1.356301
-65.896261	0.089469	1.361306
-66.936202	-3.493349	1.366310
-66.566028	1.839778	1.371315
-66.799942	0.348450	1.376320
-67.233076	-5.699092	1.381325
-67.278849	4.530247	1.386330
-67.263391	-11.502757	1.391334
-67.414125	-4.098017	1.396339
-68.313438	-6.329804	1.401344
-68.341633	-8.331091	1.406349
-69.117478	-6.823696	1.411354
-69.214050	-1.689519	1.416358
-68.888857	-4.527623	1.421363
-68.868203	-3.100739	1.426368
-69.772053	-0.102146	1.431373
-70.370258	3.066855	1.436378
-70.532013	-14.400028	1.441382
-70.343656	-6.662446	1.446387
-70.637509	-7.385083	1.451392
-69.971574	-4.632459	1.456397
-71.126929	7.343121	1.461402
-71.313921	2.857865	1.466406
-71.415047	-1.748412	1.471411
-72.221803	-4.380678	1.476416
-71.778564	-4.228559	1.481421
-72.527728	3.076963	1.486426
-72.758904	-0.018813	1.491430
-73.430910	13.013656	1.496435
-73.373430	-0.941031	1.501440
-73.277475	1.777517	1.506445
-73.767424	5.910317	1.511450
-73.766608	-3.122194	1.516454
-73.698834	-11.310980	1.521459
-74.476511	2.472027	1.526464
-74.704336	-8.391264	1.531469
-75.012782	-3.695286	1.536474
-74.903619	-8.113050	1.541478
-75.195278	-11.066469	1.546483
-75.544414	3.241010	1.551488
-75.413516	-1.585120	1.556493
-76.236796	2.941593	1.561498
-76.529291	-0.691902	1.566502
-76.239590	-3.698451	1.571507
-76.555128	1.903470	1.576512
-77.171855	-4.115303	1.581517
-77.433988	-5.058046	1.586522
-77.534540	-2.666210	1.591526
-77.636327	-5.301370	1.596531
-78.486215	-6.455736	1.601536
-78.350898	-16.480583	1.606541
-78.772386	1.362640	1.611546
-78.295874	-10.215287	1.616550
-78.373731	-3.296529	1.621555
-79.780706	-6.211230	1.626560
-79.935589	-10.198479	1.631565
-80.343723	-4.917408	1.636570
-80.212919	-5.276315	1.641574
-80.363129	-10.254548	1.646579
-80.546093	-8.422437	1.651584
-80.511358	-9.452824	1.656589
-81.447697	-5.636059	1.661594
-81.499124	-4.229517	1.666598
-81.881652	-4.093541	1.671603
-82.107751	8.815272	1.676608
-81.958581	-0.857415	1.681613
-82.594863	-3.937169	1.686618
-82.429861	-8.211822	1.691622
-82.742040	-11.449926	1.696627
-83.565131	0.903857	1.701632
-83.718821	-9.319317	1.706637
-83.897280	0.003831	1.711642
-83.619976	2.703455	1.716646
-83.741178	1.627899	1.721651
-83.922789	2.260740	1.726656
-84.236345	-0.360220	1.731661
-85.094950	4.839579	1.736666
-84.986633	1.459654	1.741670
-85.328285	8.976571	1.746675
-86.364044	1.738974	1.751680
-86.279852	-2.877357	1.756685
-86.352801	-3.198011	1.761690
-86.570912	-9.681037	1.766694
-86.646391	4.270352	1.771699
-86.655518	-2.226439	1.776704
-86.602563	-7.565536	1.781709
-87.540692	-8.035360	1.786714
-87.769252	-9.470579	1.791718
-87.937695	-0.677345	1.796723
-88.259515	-6.894185	1.801728
-87.533012	-10.146346	1.806733
-88.447754	-3.824116	1.811738
-88.905738	-4.204660	1.816742
-89.320665	-0.080453	1.821747
-89.510727	8.466237	1.826752
-89.620095	-5.345243	1.831757
-90.125568	7.854115	1.836762
-90.340716	-9.259555	1.841766
-90.882961	3.793702	1.846771
-91.052563	1.200806	1.851776
-90.936215	-5.606710	1.856781
-91.580774	4.071048	1.861786
-91.650078	-5.247864	1.866790
-91.723679	-6.615615	1.871795
-91.616561	-5.461706	1.876800
-91.660785	-2.604136	1.881805
-92.185500	-5.963961	1.886810
-92.201559	-13.592282	1.891814
-92.240262	-8.065380	1.896819
-93.188659	-7.223806	1.901824
-93.379472	-15.375234	1.906829
-93.973126	-7.451844	1.911834
-94.130814	-2.804799	1.916838
-94.274891	-5.031536	1.921843
-94.529249	2.731126	1.926848
-94.391688	2.118060	1.931853
-94.822712	-2.240371	1.936858
-95.297427	1.738181	1.941862
-95.339589	0.688206	1.946867
-95.925337	8.237042	1.951872
-95.507644	-4.034023	1.956877
-96.530153	-2.959374	1.961882
-97.145391	-3.043195	1.966886
-97.102608	-7.539142	1.971891
-97.320127	0.243057	1.976896
-97.007762	-5.952933	1.981901
-97.528304	7.217149	1.986906
-97.188052	-4.627331	1.991910
-96.766995	-6.281398	1.996915
-98.311799	-5.081083	2.006912
-98.077522	-10.366609	2.016909
-97.293103	-11.753255	2.026906
-97.388423	-5.168099	2.036902
-96.461548	-7.692130	2.046899
-95.981423	-8.555926	2.056896
-95.306611	-6.488341	2.066893
-94.531736	-2.706819	2.076890
-94.489899	-3.397402	2.086886
-94.215761	-6.889868	2.096883
-93.473745	-0.442251	2.106880
-93.076283	8.099419	2.116877
-92.240720	2.703833	2.126874
-92.028313	-2.584604	2.136870
-91.654406	-0.336821	2.146867
-90.687800	-9.338880	2.156864
-90.337915	-7.518154	2.166861
-90.178542	-7.333836	2.176858
-89.482178	-8.218843	2.186854
-88.881852	-11.787761	2.196851
-88.497692	-10.941751	2.206848
-88.083626	-9.634760	2.216845
-87.470954	-2.064483	2.226842
-86.645207	-1.937063	2.236838
-86.130184	-4.336371	2.246835
-86.172835	-4.430841	2.256832
-85.372147	-0.719886	2.266829
-85.234902	1.900766	2.276826
-84.532953	0.821648	2.286822
-83.688958	-2.060027	2.296819
-83.298706	2.279107	2.306816
-83.064658	-0.795265	2.316813
-81.945084	-1.613538	2.326810
-81.617862	-0.983518	2.336806
-81.497712	-2.776093	2.346803
-81.703425	-3.868210	2.356800
-80.623921	-6.900827	2.366797
-79.347669	0.929772	2.376794
-79.067665	-4.169686	2.386790
-78.846671	-1.720546	2.396787
-78.878098	-4.100755	2.406784
-77.962527	-9.366322	2.416781
-77.741389	10.173051	2.426778
-77.015691	7.769241	2.436774
-76.383518	-1.712609	2.446771
-76.116962	-6.505851	2.456768
-75.542011	1.716570	2.466765
-74.712400	-1.704544	2.476762
-73.934432	-4.157724	2.486758
-73.581789	0.789185	2.496755
-73.626285	6.096096	2.506752
-73.326323	5.285872	2.516749
-72.322457	-3.402079	2.526746
-72.093076	-3.551845	2.536742
-71.121660	2.473361	2.546739
-70.798506	2.483131	2.556736
-70.666431	6.241834	2.566733
-69.606814	1.489051	2.576730
-69.471706	7.977918	2.586726
-69.126196	5.969467	2.596723
-68.165372	5.968019	2.606720
-67.646648	7.420171	2.616717
-67.725380	0.321022	2.626714
-66.890210	1.508179	2.636710
-66.186055	-3.635564	2.646707
-65.972549	5.666692	2.656704
-65.047422	5.008768	2.666701
-64.734150	1.633713	2.676698
-64.754481	-4.707979	2.686694
-63.907236	-4.907040	2.696691
-63.429382	-0.423240	2.706688
-62.504586	3.252433	2.716685
-62.046930	3.947547	2.726682
-61.958927	0.395546	2.736678
-61.842103	6.779574	2.746675
-61.068470	6.021844	2.756672
-60.335475	0.518787	2.766669
-59.463767	6.138303	2.776666
-58.969040	0.498352	2.786662
-58.696133	2.571895	2.796659
-58.874782	0.933843	2.806656
-57.621510	2.882284	2.816653
-57.765306	2.977892	2.826650
-56.679688	1.072053	2.836646
-56.159308	-0.298561	2.846643
-56.164063	1.679105	2.856640
-55.131795	2.011754	2.866637
-54.627888	1.416664	2.876634
-54.332419	2.358937	2.886630
-54.035858	3.690677	2.896627
-53.485219	8.540043	2.906624
-53.023732	2.471311	2.916621
-52.027335	-1.150164	2.926618
-51.788664	-3.959165	2.936614
-51.617662	-6.371092	2.946611
-50.668863	-9.826717	2.956608
-50.412854	-1.823583	2.966605
-49.712619	-8.661481	2.976602
-49.148184	1.871914	2.986598
-48.804186	1.244859	2.996595
-48.724587	1.641249	3.006592
-47.684063	3.778250	3.016589
-47.712423	3.190532	3.026586
-46.685653	6.672834	3.036582
-46.123392	2.264077	3.046579
-45.920483	-0.878276	3.056576
-45.091076	3.227327	3.066573
-44.497392	5.066878	3.076570
-44.526095	8.166529	3.086566
-44.144080	2.322492	3.096563
-43.289934	-3.988326	3.106560
-42.645441	-0.987821	3.116557
-41.997511	-0.351030	3.126554
-41.635540	2.576535	3.136550
-41.357115	0.315669	3.146547
-41.109357	-3.904425	3.156544
-40.407044	-2.173762	3.166541
-40.010640	-0.737289	3.176538
-38.828903	-5.445846	3.186534
-38.709065	-5.062097	3.196531
-38.217806	-1.945715	3.206528
-38.067438	2.389828	3.216525
-36.781441	1.380760	3.226522
-36.668195	-3.930155	3.236518
-36.625754	-0.223932	3.246515
-35.947497	-7.634925	3.256512
-35.498662	-13.847387	3.266509
-34.468951	-9.465894	3.276506
-34.103541	-15.104585	3.286502
-34.034215	-13.673885	3.296499
-33.589049	-14.256602	3.306496
-32.896673	-3.109696	3.316493
-32.038215	-9.148757	3.326490
-31.150548	-13.304388	3.336486
-31.293332	-5.618904	3.346483
-31.110319	-6.699071	3.356480
-30.326904	-7.680076	3.366477
-30.092549	-12.743869	3.376474
-29.282878	-12.373172	3.386470
-28.721589	-5.295349	3.396467
-28.547173	-8.274846	3.406464
-27.494889	-7.124871	3.416461
-27.001995	1.360669	3.426458
-26.784847	-7.688685	3.436454
-26.874198	-6.673445	3.446451
-26.004417	-5.906688	3.456448
-24.832104	-4.686821	3.466445
-24.441619	-9.369601	3.476442
-24.252022	-1.292702	3.486438
-23.892002	-1.475607	3.496435
-23.302442	-8.853695	3.506432
-22.848485	-2.722062	3.516429
-22.385943	1.691281	3.526426
-21.413891	-5.281073	3.536422
-21.166456	-4.084185	3.546419
-21.077505	-3.486521	3.556416
-20.171978	-4.423302	3.566413
-19.763139	-1.167294	3.576410
-19.524116	4.842796	3.586406
-18.595825	1.951085	3.596403
-18.041892	-7.312597	3.606400
-17.920240	3.847713	3.616397
-16.821362	1.832095	3.626394
-16.603266	-2.868024	3.636390
-16.433307	-2.061307	3.646387
-15.819230	-0.921866	3.656384
-15.139191	-2.523400	3.666381
-15.103696	-2.728316	3.676378
-13.885672	-2.028792	3.686374
-13.620794	-3.939077	3.696371
-13.559246	-3.460663	3.706368
-12.250918	2.476918	3.716365
-12.039106	0.698492	3.726362
-11.916188	-0.536985	3.736358
-11.163160	-10.972266	3.746355
-10.588954	-6.018887	3.756352
-10.563496	-5.458792	3.766349
-9.990022	-2.900151	3.776346
-9.502522	2.944295	3.786342
-8.106458	-7.094396	3.796339
-7.594560	-8.406658	3.806336
-8.056387	-4.070228	3.816333
-7.481725	-3.444128	3.826330
-6.940354	-4.684981	3.836326
-6.473633	-0.614413	3.846323
-5.675430	4.436920	3.856320
-4.935728	6.538698	3.866317
-5.050642	1.580309	3.876314
-4.621009	10.094775	3.886310
-4.060876	15.766288	3.896307
-3.467915	27.885471	3.906304
-3.051947	39.702943	3.916301
-2.619487	47.938218	3.926298
-1.882658	67.184626	3.936294
-1.604561	61.185789	3.946291
-1.350687	80.241786	3.956288
-0.855471	97.308615	3.966285
-0.453421	116.157700	3.976282
0.000000	134.385995	3.981286
0.313886	149.893188	3.986291
0.274430	147.675346	3.991296
0.661142	151.696131	3.996301
0.740311	157.413429	4.001306
0.870592	165.710690	4.006310
0.648027	170.934263	4.011315
1.353425	172.412065	4.016320
0.703547	175.181061	4.021325
1.022172	182.284549	4.026330
1.158373	174.885387	4.031334
1.057537	181.621159	4.036339
1.220740	174.654368	4.041344
1.014584	184.994366	4.046349
1.059362	179.552087	4.051354
1.423622	177.900579	4.056358
0.907658	182.031165	4.061363
1.086802	178.118085	4.066368
1.186964	172.926560	4.071373
1.554496	173.090548	4.076378
1.371588	170.366829	4.081382
1.251066	176.396997	4.086387
1.095476	180.550214	4.091392
1.324607	178.252320	4.096397
1.193868	178.997418	4.101402
1.607519	178.439166	4.106406
1.230596	174.107008	4.111411
1.754317	185.949339	4.116416
1.234700	182.383025	4.121421
1.204311	180.891427	4.126426
1.659190	187.464201	4.131430
1.326741	191.486941	4.136435
1.541002	186.138329	4.141440
1.201472	179.674251	4.146445
1.370937	173.687251	4.151450
1.189625	175.917756	4.156454
1.125348	178.547544	4.161459
1.131671	180.574643	4.166464
1.236577	189.470681	4.171469
1.607600	182.436523	4.176474
1.709130	181.155213	4.181478
1.474298	184.548884	4.186483
1.333681	178.686396	4.191488
1.670995	182.705437	4.196493
1.192752	182.549521	4.201498
1.766072	178.353217	4.206502
1.392313	181.407984	4.211507
1.557328	182.391483	4.216512
1.533591	182.597793	4.221517
1.641581	197.115387	4.226522
1.889552	194.643695	4.231526
1.409020	187.062746	4.236531
1.433696	187.533555	4.241536
1.817806	203.836556	4.246541
2.099987	205.386998	4.251546
1.841340	194.256318	4.256550
1.733835	189.682625	4.261555
1.630638	183.994609	4.266560
1.415187	186.132387	4.271565
1.564734	190.405477	4.276570
2.236327	194.985919	4.281574
1.504505	191.038396	4.286579
1.723643	184.293793	4.291584
1.701016	182.709229	4.296589
1.586720	179.500192	4.301594
2.023530	190.707569	4.306598
1.949860	209.980324	4.311603
1.792171	201.399651	4.316608
1.161067	198.768297	4.321613
1.912995	204.706072	4.326618
2.098116	208.344000	4.331622
2.098507	210.875074	4.336627
2.042157	213.509952	4.341632
1.785949	217.862442	4.346637
2.062284	212.244665	4.351642
2.270668	212.221615	4.356646
1.901459	200.602049	4.361651
1.773025	197.594542	4.366656
2.036950	199.866022	4.371661
1.792303	198.455450	4.376666
2.103135	202.931065	4.381670
1.771969	208.029295	4.386675
1.887611	204.240055	4.391680
1.937950	204.178492	4.396685
1.840141	209.360383	4.401690
2.117165	209.225337	4.406694
2.144079	219.149184	4.411699
2.316935	214.525230	4.416704
2.697092	216.234330	4.421709
2.024759	199.609695	4.426714
2.062105	200.885284	4.431718
1.919773	203.596908	4.436723
1.946821	206.395890	4.441728
2.204716	203.580953	4.446733
2.053749	209.846859	4.451738
2.202021	213.240623	4.456742
2.395434	215.940773	4.461747
2.366534	212.541178	4.466752
2.376691	213.972889	4.471757
2.276515	214.887208	4.476762
2.712915	213.199083	4.481766
2.238724	210.935452	4.486771
1.918175	198.229413	4.491776
1.834124	198.827990	4.496781
2.085288	207.761233	4.501786
2.372042	216.027673	4.506790
2.217961	214.802228	4.511795
2.155490	216.178879	4.516800
2.169268	219.153950	4.521805
2.556117	216.480160	4.526810
2.012696	216.366094	4.531814
2.154022	224.437023	4.536819
2.383339	206.766266	4.541824
2.632186	219.477435	4.546829
2.437372	211.845381	4.551834
2.662164	208.583209	4.556838
2.105547	212.571475	4.561843
2.073225	207.444990	4.566848
2.378447	212.424528	4.571853
2.256937	206.283789	4.576858
2.237556	205.707961	4.581862
2.496899	224.216704	4.586867
2.941010	224.254797	4.591872
2.488045	223.689956	4.596877
2.236992	214.301320	4.601882
2.303761	216.958037	4.606886
2.403807	237.288782	4.611891
2.658729	238.922593	4.616896
2.489780	235.070368	4.621901
2.723122	244.499973	4.626906
3.048968	243.382830	4.631910
2.674875	235.098641	4.636915
2.704145	220.164253	4.641920
2.575027	218.308468	4.646925
2.254565	223.430335	4.651930
2.408161	237.823756	4.656934
2.452659	236.155903	4.661939
2.734595	237.769663	4.666944
2.750206	239.652943	4.671949
2.595520	252.496965	4.676954
2.684671	235.037970	4.681958
3.061211	240.765651	4.686963
3.263890	241.866640	4.691968
2.838486	247.903472	4.696973
2.655193	245.306353	4.701978
2.992646	246.693114	4.706982
3.261987	244.350946	4.711987
2.541394	245.156828	4.716992
2.627881	231.523276	4.721997
2.778133	245.746383	4.727002
2.972370	241.441778	4.732006
2.601399	242.132769	4.737011
2.919104	242.937322	4.742016
2.740686	243.876556	4.747021
2.651674	240.679365	4.752026
3.017850	244.633786	4.757030
2.715618	247.370470	4.762035
2.933945	239.464862	4.767040
3.211601	241.281775	4.772045
2.814605	241.511766	4.777050
3.040681	239.540214	4.782054
2.812657	239.389386	4.787059
3.163726	250.407752	4.792064
3.254968	239.054543	4.797069
2.858597	244.463559	4.802074
3.082209	240.562481	4.807078
3.274674	251.374742	4.812083
3.012744	238.662653	4.817088
3.280738	250.374251	4.822093
3.017838	243.031264	4.827098
3.001929	243.011719	4.832102
2.826135	250.278123	4.837107
2.849512	247.560036	4.842112
2.800416	241.901489	4.847117
2.850239	244.801314	4.852122
3.109483	254.508443	4.857126
3.136938	260.350937	4.862131
3.294086	255.210572	4.867136
3.726992	264.159660	4.872141
3.312403	245.134409	4.877146
2.842588	240.117592	4.882150
3.093217	246.051666	4.887155
3.471769	260.830643	4.892160
3.506498	260.698759	4.897165
3.303778	253.659554	4.902170
3.153218	242.391685	4.907174
3.356186	252.560052	4.912179
3.374636	252.835683	4.917184
3.302454	256.700599	4.922189
3.375905	267.854224	4.927194
3.743481	262.579645	4.932198
3.247816	254.393590	4.937203
3.411864	244.025564	4.942208
3.183147	255.118956	4.947213
3.316131	259.511718	4.952218
3.519320	263.665689	4.957222
3.352001	273.483955	4.962227
3.368538	264.942392	4.967232
3.669814	264.743434	4.972237
3.228465	267.948013	4.977242
3.815220	262.610619	4.982246
3.033687	269.127205	4.987251
3.073708	268.912233	4.992256
3.488425	265.588655	4.997261
3.421318	271.303599	5.002266
3.443891	264.621402	5.007270
3.469956	264.240935	5.012275
3.219100	268.817228	5.017280
3.289961	267.575518	5.022285
3.094896	275.234098	5.027290
3.626061	280.342771	5.032294
3.773433	287.681944	5.037299
3.883334	282.305361	5.042304
3.621255	275.889225	5.047309
3.428414	276.311859	5.052314
3.865997	285.339320	5.057318
3.943712	296.751726	5.062323
3.963547	282.685646	5.067328
3.869554	274.446138	5.072333
3.809678	276.847458	5.077338
3.889961	271.551450	5.082342
3.467344	266.865755	5.087347
3.609536	264.847231	5.092352
4.079530	263.492364	5.097357
3.494403	269.838971	5.102362
3.979724	274.907369	5.107366
3.747141	271.226460	5.112371
3.674847	280.672333	5.117376
3.926017	271.167012	5.122381
3.640939	272.812667	5.127386
3.734041	270.599351	5.132390
4.056039	293.897826	5.137395
4.121704	289.977191	5.142400
4.024739	291.539590	5.147405
3.713903	285.333572	5.152410
3.951922	278.554338	5.157414
3.914283	288.776243	5.162419
3.947575	284.658199	5.167424
3.787330	296.402122	5.172429
3.980427	292.664004	5.177434
4.165898	282.317909	5.182438
4.107500	300.193135	5.187443
3.736199	293.395467	5.192448
4.086790	299.158870	5.197453
3.654410	309.499584	5.202458
4.299629	290.757492	5.207462
4.089465	292.603386	5.212467
4.081960	288.422129	5.217472
4.501806	287.274437	5.222477
4.340640	295.073249	5.227482
4.446172	280.857699	5.232486
4.060960	271.445760	5.237491
3.972998	259.076563	5.242496
4.353429	271.387497	5.247501
3.999590	273.815892	5.252506
4.220594	269.987983	5.257510
4.208509	276.896549	5.262515
4.143044	267.111807	5.267520
4.151821	281.376092	5.272525
4.032304	295.037221	5.277530
4.885006	287.199879	5.282534
4.169767	287.144371	5.287539
3.850373	275.121476	5.292544
4.212474	278.440619	5.297549
4.354823	298.612944	5.302554
4.421550	294.711125	5.307558
4.263508	305.477095	5.312563
4.444345	301.399206	5.317568
4.709715	290.499578	5.322573
4.220367	291.319850	5.327578
4.357264	286.818572	5.332582
4.423095	295.211414	5.337587
4.401030	292.073327	5.342592
4.161035	288.425214	5.347597
4.511125	293.691978	5.352602
4.714924	297.058075	5.357606
4.437268	302.290318	5.362611
4.542075	289.311921	5.367616
4.737349	284.437661	5.372621
4.476540	286.838825	5.377626
4.270131	275.601832	5.382630
3.926027	287.709919	5.387635
4.422176	287.625963	5.392640
4.631043	292.642767	5.397645
4.499082	289.825624	5.402650
4.569645	292.611474	5.407654
4.581276	293.024218	5.412659
4.215139	297.757788	5.417664
4.212675	300.640503	5.422669
4.420111	305.303190	5.427674
4.647187	299.620337	5.432678
4.771616	302.052894	5.437683
4.512623	300.821734	5.442688
4.668424	293.020814	5.447693
4.457192	302.789029	5.452698
4.706728	298.909187	5.457702
4.528303	290.644935	5.462707
4.630058	299.845246	5.467712
4.805142	297.628573	5.472717
4.736814	289.283795	5.477722
4.332614	290.198296	5.482726
4.602320	300.204371	5.487731
4.951156	311.194651	5.492736
5.217178	308.852996	5.497741
4.776351	297.715993	5.502746
4.854202	301.573231	5.507750
4.627788	293.696152	5.512755
4.538438	291.388032	5.517760
4.633329	306.385501	5.522765
4.878503	323.447546	5.527770
5.267010	320.039479	5.532774
4.839025	321.799279	5.537779
5.032808	314.118950	5.542784
5.120666	308.033958	5.547789
4.710671	302.533180	5.552794
5.099863	294.540664	5.557798
4.741261	293.416862	5.562803
4.820120	303.187082	5.567808
5.315416	305.030014	5.572813
4.990446	312.512808	5.577818
4.859686	302.364948	5.582822
4.807215	303.885574	5.587827
5.055913	304.254846	5.592832
5.424151	309.237194	5.597837
5.012452	317.429614	5.602842
5.186212	308.217981	5.607846
5.221985	310.711888	5.612851
4.486902	299.975334	5.617856
4.990144	308.856476	5.622861
5.089762	310.758240	5.627866
5.439087	319.274356	5.632870
4.846580	312.296201	5.637875
4.988413	315.498001	5.642880
5.353504	314.985319	5.647885
4.926464	315.283294	5.652890
5.127860	319.810887	5.657894
5.022133	322.608544	5.662899
5.109741	326.239628	5.667904
5.214986	315.387221	5.672909
5.299323	320.202078	5.677914
5.062481	314.104682	5.682918
5.208828	314.281180	5.687923
5.023076	319.381968	5.692928
5.226796	316.047147	5.697933
4.935222	319.753460	5.702938
5.113125	316.185399	5.707942
5.222818	315.940527	5.712947
5.163098	323.384929	5.717952
5.269716	313.215690	5.722957
5.375093	326.316415	5.727962
5.554519	337.064331	5.732966
5.470918	328.187245	5.737971
5.450581	333.167205	5.742976
5.565345	320.421348	5.747981
5.319671	328.344148	5.752986
4.993457	322.456907	5.757990
5.263497	333.940446	5.762995
5.433149	335.514859	5.768000
5.307869	328.121800	5.773005
5.165846	337.284395	5.778010
5.824412	332.366006	5.783014
5.565311	334.349287	5.788019
5.786222	338.000617	5.793024
5.698154	339.985576	5.798029
5.494819	344.244389	5.803034
5.891207	338.152175	5.808038
5.630924	346.785965	5.813043
5.727118	333.245728	5.818048
5.331241	335.728175	5.823053
5.497688	337.068968	5.828058
5.293309	335.487558	5.833062
5.439629	330.788636	5.838067
5.587436	341.117559	5.843072
5.376278	337.876212	5.848077
5.492215	335.431516	5.853082
5.715333	328.452114	5.858086
5.453675	336.193921	5.863091
5.834727	331.837878	5.868096
5.969031	335.524924	5.873101
5.570554	338.276701	5.878106
6.046675	328.533621	5.883110
5.612999	337.599541	5.888115
5.625756	335.544340	5.893120
5.505670	337.268555	5.898125
5.605702	340.271262	5.903130
5.693211	343.029154	5.908134
5.688920	339.492799	5.913139
5.952089	343.928461	5.918144
5.986976	336.409062	5.923149
5.941013	336.701115	5.928154
5.889347	337.680607	5.933158
5.710682	345.754270	5.938163
5.980615	337.520989	5.943168
5.612725	339.540298	5.948173
5.684256	351.962963	5.953178
5.906326	363.368614	5.958182
5.863197	359.278345	5.963187
6.042457	359.642679	5.968192
5.975910	367.667147	5.973197
6.220481	369.220333	5.978202
6.186931	372.762840	5.983206
6.284066	369.343468	5.988211
5.926116	356.197078	5.993216
5.881907	342.906627	5.998221
5.637873	355.049701	6.003226
5.936825	362.507527	6.008230
5.703605	366.739390	6.013235
6.085338	366.594265	6.018240
5.954431	367.883572	6.023245
5.740760	374.168852	6.028250
5.809785	357.741129	6.033254
6.099819	362.672468	6.038259
6.158355	371.082307	6.043264
6.435414	373.244183	6.048269
5.777706	372.996158	6.053274
5.914274	375.585015	6.058278
6.323228	375.008510	6.063283
6.102866	375.172862	6.068288
6.095314	366.584403	6.073293
6.265284	376.527053	6.078298
6.001597	351.030195	6.083302
5.736554	353.109323	6.088307
6.412048	359.562172	6.093312
6.129875	348.533159	6.098317
5.700854	343.146083	6.103322
5.800335	350.679450	6.108326
6.090825	359.843893	6.113331
5.950985	360.780253	6.118336
6.047484	355.203264	6.123341
6.266496	367.368711	6.128346
6.154893	363.055048	6.133350
5.780461	350.509205	6.138355
5.664705	344.642767	6.143360
6.058570	358.169723	6.148365
6.052905	371.098051	6.153370
6.155645	370.186703	6.158374
5.956813	374.441654	6.163379
5.879428	376.494547	6.168384
5.829215	372.639507	6.173389
5.801592	370.116058	6.178394
6.224044	373.406781	6.183398
6.241925	367.535216	6.188403
5.796955	367.680974	6.193408
6.120141	365.036121	6.198413
5.923149	374.612314	6.203418
6.142568	363.457246	6.208422
6.090614	367.587940	6.213427
5.807770	376.763127	6.218432
6.173370	367.091128	6.223437
6.077784	367.394119	6.228442
5.798715	369.662112	6.233446
5.828311	369.508884	6.238451
5.601239	373.018436	6.243456
6.261757	374.272330	6.248461
6.073829	378.152244	6.253466
6.048152	374.521154	6.258470
6.004545	372.458961	6.263475
6.084043	376.021722	6.268480
6.148470	374.578529	6.273485
5.819310	376.079237	6.278490
5.727527	372.205400	6.283494
5.930437	372.850772	6.288499
5.665957	376.375677	6.293504
5.999004	376.298293	6.298509
6.180534	377.908815	6.303514
6.137812	372.575101	6.308518
6.563733	370.217876	6.313523
6.065042	370.425836	6.318528
6.270270	364.290796	6.323533
5.976474	357.006388	6.328538
5.962082	350.953221	6.333542
6.088141	346.482100	6.338547
5.876260	347.686015	6.343552
5.749907	341.368815	6.348557
5.884051	357.806036	6.353562
6.216621	364.897921	6.358566
5.781472	357.619842	6.363571
5.839109	372.325805	6.368576
6.344064	367.501078	6.373581
6.446907	373.670326	6.378586
6.271282	363.874316	6.383590
6.505052	354.238797	6.388595
6.303831	352.982763	6.393600
6.444186	347.784890	6.398605
5.720759	354.877707	6.403610
5.835789	349.316800	6.408614
5.771398	345.742403	6.413619
5.755404	342.679288	6.418624
6.294676	342.734110	6.423629
5.576157	350.727842	6.428634
5.833247	354.677232	6.433638
6.046716	355.637330	6.438643
6.153917	355.876911	6.443648
5.866373	351.518050	6.448653
5.724367	349.714890	6.453658
5.588209	352.719804	6.458662
6.090959	343.943832	6.463667
5.891306	347.910999	6.468672
5.749567	349.860075	6.473677
6.150457	366.483305	6.478682
6.224779	370.540430	6.483686
5.879326	358.762011	6.488691
5.767390	364.759260	6.493696
6.205216	367.952659	6.498701
6.166393	366.180788	6.503706
6.058934	354.437850	6.508710
5.971046	356.277247	6.513715
5.805224	358.381960	6.518720
6.201334	349.201907	6.523725
5.785241	360.179188	6.528730
5.672925	359.222440	6.533734
5.966038	362.068346	6.538739
6.012429	370.976807	6.543744
6.382637	371.162524	6.548749
5.895772	373.225789	6.553754
5.619672	375.344618	6.558758
5.715252	374.820377	6.563763
5.813853	374.469673	6.568768
6.146052	358.940366	6.573773
5.581638	363.072257	6.578778
5.933224	365.782450	6.583782
5.863588	374.196553	6.588787
6.278081	370.474352	6.593792
6.232381	367.238713	6.598797
5.843350	369.530263	6.603802
5.991022	377.343998	6.608806
5.926107	374.816899	6.613811
5.916325	370.689765	6.618816
6.108298	367.274516	6.623821
5.763413	368.505599	6.628826
6.128575	365.066379	6.633830
6.151849	365.556396	6.638835
5.946451	370.296438	6.643840
6.341992	372.971270	6.648845
6.070643	373.732079	6.653850
6.297078	377.050351	6.658854
6.206566	362.276985	6.663859
5.812527	366.439130	6.668864
6.391657	364.579930	6.673869
6.024295	363.182244	6.678874
6.079550	357.792053	6.683878
5.897759	351.755623	6.688883
5.996142	360.200343	6.693888
6.234861	362.956693	6.698893
6.066706	364.153758	6.703898
6.178406	351.538075	6.708902
6.125250	346.712213	6.713907
5.618363	348.525508	6.718912
5.653233	345.324706	6.723917
5.812707	360.185549	6.728922
6.219277	368.449107	6.733926
6.324915	362.598596	6.738931
5.818178	357.252166	6.743936
6.393311	344.741049	6.748941
5.897853	353.272482	6.753946
5.697255	344.771229	6.758950
5.636942	352.759912	6.763955
5.690722	370.035491	6.768960
6.189228	371.678607	6.773965
6.053278	367.406723	6.778970
5.995292	367.738625	6.783974
5.920046	377.086934	6.788979
6.031954	371.127868	6.793984
6.301539	371.734319	6.798989
6.102551	373.515194	6.803994
6.000485	370.060592	6.808998
6.025708	372.223960	6.814003
6.024279	367.035640	6.819008
6.228538	365.839463	6.824013
5.947245	361.840294	6.829018
5.626586	354.699304	6.834022
5.820517	364.299665	6.839027
5.697535	375.458824	6.844032
6.132220	360.283625	6.849037
5.919173	371.751128	6.854042
6.021974	379.075176	6.859046
5.947881	371.971478	6.864051
6.006546	373.047582	6.869056
6.336287	371.009152	6.874061
6.159429	381.898341	6.879066
6.596341	376.631848	6.884070
6.602460	361.492159	6.889075
6.036512	356.901665	6.894080
6.178428	342.363985	6.899085
5.838263	354.088679	6.904090
5.765440	345.301646	6.909094
5.896526	344.493428	6.914099
5.587359	349.948925	6.919104
5.873410	347.199159	6.924109
5.643672	357.327813	6.929114
5.986139	355.126036	6.934118
6.202180	361.014947	6.939123
6.274226	361.051225	6.944128
6.119649	357.383386	6.949133
6.052905	344.368552	6.954138
5.832146	344.896803	6.959142
5.876248	343.165727	6.964147
5.853742	352.483612	6.969152
5.966970	352.456489	6.974157
5.991530	372.448032	6.979162
5.735015	365.616532	6.984166
6.482060	358.849263	6.989171
6.069326	360.106796	6.994176
6.131055	351.842854	6.999181
5.953552	366.164867	7.004186
6.070870	349.811844	7.009190
5.709630	346.245991	7.014195
5.676681	349.658683	7.019200
5.844372	368.659671	7.024205
6.246506	375.936818	7.029210
5.823634	375.826009	7.034214
6.108410	367.482819	7.039219
6.278617	383.810008	7.044224
6.207563	369.555616	7.049229
5.877955	353.949669	7.054234
5.671695	354.200398	7.059238
6.293751	362.936399	7.064243
6.245627	365.620632	7.069248
6.237522	348.708284	7.074253
5.933831	355.425283	7.079258
5.737189	344.585356	7.084262
5.824189	347.931797	7.089267
6.133203	349.411608	7.094272
6.215964	354.378585	7.099277
5.757703	346.816224	7.104282
5.679143	340.716166	7.109286
5.868178	353.677251	7.114291
5.773866	379.081722	7.119296
6.302706	374.708841	7.124301
5.891475	373.821074	7.129306
5.808195	382.303759	7.134310
6.121650	373.187266	7.139315
5.814509	383.375520	7.144320
6.382203	373.096038	7.149325
5.844502	376.309405	7.154330
5.980025	382.274215	7.159334
6.294312	375.350114	7.164339
6.308604	378.157449	7.169344
6.234875	351.036266	7.174349
5.641091	351.752679	7.179354
5.849881	353.710110	7.184358
6.313843	348.996217	7.189363
5.923181	351.977730	7.194368
6.047702	348.655313	7.199373
5.837137	350.871440	7.204378
6.052368	355.593031	7.209382
6.144230	343.002609	7.214387
5.850666	356.899866	7.219392
5.861548	340.807141	7.224397
5.711548	344.703251	7.229402
6.351098	358.957355	7.234406
6.048465	350.699881	7.239411
5.904016	351.424987	7.244416
5.841719	359.951831	7.249421
5.915439	370.355655	7.254426
6.207498	363.520464	7.259430
6.194598	368.628985	7.264435
6.013619	361.184528	7.269440
5.984823	347.717649	7.274445
6.072269	344.385222	7.279450
6.053596	333.821142	7.284454
6.113965	346.707468	7.289459
5.845063	347.287556	7.294464
5.848524	342.607850	7.299469
5.508836	350.377709	7.304474
6.125049	366.296474	7.309478
6.368205	364.037489	7.314483
5.914657	366.335983	7.319488
5.917936	364.592318	7.324493
6.094777	376.438505	7.329498
5.872923	361.581312	7.334502
6.184182	369.072014	7.339507
5.980520	369.271714	7.344512
6.264659	367.132860	7.349517
6.265826	353.322754	7.354522
5.876811	343.152058	7.359526
5.939004	347.245881	7.364531
5.554093	349.229893	7.369536
6.039334	358.537831	7.374541
6.372825	364.860766	7.379546
6.099954	359.876333	7.384550
6.069294	362.355345	7.389555
5.488711	363.246864	7.394560
5.954373	346.772824	7.399565
6.145188	360.676451	7.404570
5.897353	360.060482	7.409574
6.152171	364.266499	7.414579
5.771414	359.014227	7.419584
5.795544	367.647758	7.424589
5.890214	364.871026	7.429594
6.156409	368.401370	7.434598
6.449870	368.836398	7.439603
5.699454	365.825073	7.444608
6.067417	363.429472	7.449613
6.310090	372.851355	7.454618
6.039668	363.184096	7.459622
6.362397	347.735378	7.464627
5.623031	348.556860	7.469632
6.110364	348.967839	7.474637
6.129155	342.776596	7.479642
5.901456	356.113031	7.484646
5.599647	347.494755	7.489651
6.049399	361.553967	7.494656
6.021960	358.233211	7.499661
5.759426	352.294853	7.504666
5.745125	360.418701	7.509670
6.361666	359.395214	7.514675
5.865035	374.346212	7.519680
6.529993	367.791121	7.524685
6.261972	359.964826	7.529690
6.147215	351.886726	7.534694
6.243010	340.431496	7.539699
6.076489	348.006540	7.544704
5.878126	345.323181	7.549709
5.743242	342.993714	7.554714
5.735821	341.644040	7.559718
6.291020	344.565940	7.564723
5.995324	343.008328	7.569728
5.810282	337.902570	7.574733
5.847914	339.681169	7.579738
5.744685	343.911643	7.584742
5.801621	336.230599	7.589747
6.301779	357.713693	7.594752
6.274944	357.471229	7.599757
6.133105	343.974607	7.604762
5.823140	341.593477	7.609766
6.065371	334.753449	7.614771
5.732986	343.778191	7.619776
5.854591	335.783290	7.624781
6.011455	349.217656	7.629786
5.884497	357.827398	7.634790
6.256602	358.933487	7.639795
5.772963	356.260021	7.644800
6.180012	362.922613	7.649805
6.380366	351.106139	7.654810
6.057801	348.204954	7.659814
5.995482	351.201462	7.664819
6.114472	348.009627	7.669824
5.851069	339.094267	7.674829
5.870845	350.863805	7.679834
5.830100	346.292267	7.684838
5.864994	346.473573	7.689843
6.012242	352.993366	7.694848
5.967121	347.957433	7.699853
5.949565	344.587673	7.704858
6.042225	361.262356	7.709862
6.221230	353.992457	7.714867
5.705702	346.942115	7.719872
6.149974	344.528233	7.724877
6.097915	351.009649	7.729882
5.969784	348.891099	7.734886
5.949173	347.559309	7.739891
6.229583	347.091533	7.744896
6.135711	342.253068	7.749901
5.668040	344.936593	7.754906
5.860196	349.085984	7.759910
6.144425	348.266427	7.764915
5.624990	355.887277	7.769920
6.048146	361.841815	7.774925
6.390253	362.506507	7.779930
5.912458	361.860128	7.784934
6.420748	349.293041	7.789939
5.678313	357.540464	7.794944
6.023107	344.255503	7.799949
6.146078	341.031407	7.804954
5.701746	349.118222	7.809958
6.172354	345.472656	7.814963
5.987623	355.388610	7.819968
5.978461	348.521525	7.824973
5.813415	352.075140	7.829978
5.760602	355.993991	7.834982
6.153520	371.843342	7.839987
5.809936	377.117574	7.844992
5.855658	365.287353	7.849997
6.241844	373.595236	7.855002
6.116178	373.618197	7.860006
6.283977	365.612881	7.865011
5.863397	353.415959	7.870016
5.782687	340.684894	7.875021
6.136774	359.182097	7.880026
6.080334	367.353680	7.885030
6.156694	353.402076	7.890035
6.143056	355.486108	7.895040
6.315021	352.649810	7.900045
5.974485	348.185356	7.905050
5.803460	355.767436	7.910054
6.281684	343.318961	7.915059
5.695451	347.365681	7.920064
6.133494	346.908008	7.925069
5.906092	347.434136	7.930074
6.071483	358.174773	7.935078
5.979801	353.886465	7.940083
5.988440	354.922949	7.945088
5.823507	349.035741	7.950093
5.954309	353.511127	7.955098
5.904323	351.560670	7.960102
5.694453	352.602916	7.965107
5.864779	352.402328	7.970112
6.046125	359.951347	7.975117
6.489143	370.335275	7.980122
6.420860	361.872015	7.985139
6.158019	354.273262	7.990157
5.933479	347.249167	7.995174
5.960407	351.858745	8.000192
5.962139	355.768542	8.005210
5.853864	351.373893	8.010227
5.931828	338.571586	8.015245
5.696036	346.781995	8.020262
5.848514	345.713665	8.025280
6.017367	359.783999	8.030298
5.832059	370.924503	8.035315
6.109736	375.996562	8.040333
6.209762	373.156610	8.045350
6.339783	372.962781	8.050368
6.117565	360.226426	8.055386
6.134855	355.894152	8.060403
5.974938	351.526529	8.065421
6.037794	357.395930	8.070438
5.830661	359.381894	8.075456
6.094801	368.653206	8.080474
6.006388	376.483939	8.085491
6.110728	380.835247	8.090509
6.055713	379.802581	8.095526
6.108505	375.228059	8.100544
6.331048	373.416617	8.105562
5.943722	379.201928	8.110579
6.109474	373.391591	8.115597
6.148788	370.119348	8.120614
5.984321	373.998386	8.125632
6.380426	378.442832	8.130650
6.192583	381.612336	8.135667
6.083224	369.978580	8.140685
5.941275	382.907915	8.145702
6.243920	375.028052	8.150720
6.738442	374.401579	8.155738
6.095144	380.763473	8.160755
6.023366	370.928913	8.165773
6.120510	371.500769	8.170790
6.221926	375.928272	8.175808
6.649358	376.296903	8.180826
6.005837	372.844474	8.185843
5.939913	365.839699	8.190861
5.849570	377.101025	8.195878
6.043537	376.644717	8.200896
6.231097	369.546578	8.205914
6.043810	381.653056	8.210931
6.123249	367.395699	8.215949
5.805864	376.319481	8.220966
5.941880	368.412081	8.225984
6.191986	366.416443	8.231002
6.045110	379.791507	8.236019
6.499872	373.172198	8.241037
6.213660	385.379383	8.246054
6.130794	382.757430	8.251072
6.315261	363.674268	8.256090
6.474624	370.642529	8.261107
6.675185	370.680640	8.266125
6.406456	375.071465	8.271142
6.461190	376.233778	8.276160
6.594797	362.242488	8.281178
6.544412	372.901116	8.286195
6.880761	370.942458	8.291213
6.351061	370.943511	8.296230
6.509656	365.980036	8.301248
6.952491	362.480472	8.306266
6.478529	357.682380	8.311283
6.013141	348.565897	8.316301
5.786216	357.642750	8.321318
5.757072	364.728904	8.326336
6.052189	365.705234	8.331354
5.778348	373.694404	8.336371
6.081820	366.937859	8.341389
6.274884	363.799314	8.346406
6.115574	367.194714	8.351424
6.438911	368.598958	8.356442
6.057316	382.162276	8.361459
6.527595	384.913091	8.366477
6.363342	397.981628	8.371494
6.634428	384.170749	8.376512
6.801760	378.622089	8.381530
6.248112	380.343619	8.386547
6.390553	375.619353	8.391565
6.543945	374.008090	8.396582
6.166609	372.852360	8.401600
6.832717	368.326909	8.406618
6.420426	374.870353	8.411635
6.511713	368.771889	8.416653
6.557017	366.988218	8.421670
6.398467	368.436407	8.426688
6.566260	358.330793	8.431706
6.572535	379.877317	8.436723
6.364313	371.001390	8.441741
6.652349	372.458502	8.446758
6.647608	376.915261	8.451776
6.452095	370.839643	8.456794
6.755466	374.336117	8.461811
6.508889	363.282431	8.466829
6.596872	362.722811	8.471846
6.440595	373.950285	8.476864
6.514609	368.832808	8.481882
6.340609	380.018882	8.486899
6.742473	373.587738	8.491917
6.431809	372.273242	8.496934
6.564533	369.668003	8.501952
7.169419	372.574448	8.506970
6.809671	380.280441	8.511987
6.920621	370.770694	8.517005
6.669696	373.972171	8.522022
6.607314	375.061317	8.527040
6.590079	362.390672	8.532058
6.341835	375.409237	8.537075
6.507603	378.974608	8.542093
6.854954	374.252951	8.547110
6.438698	372.904507	8.552128
6.454101	373.201997	8.557146
6.283845	377.113500	8.562163
6.240025	372.077599	8.567181
6.763777	372.210237	8.572199
6.652253	370.463760	8.577216
6.837224	362.132134	8.582234
6.224924	374.267329	8.587251
6.451929	375.074454	8.592269
6.546002	371.528548	8.597287
6.403797	374.277498	8.602304
6.430090	372.250657	8.607322
6.912687	371.316790	8.612339
6.567538	372.273519	8.617357
6.388047	376.483109	8.622375
6.721055	386.762944	8.627392
6.771933	383.665608	8.632410
6.326011	383.716650	8.637427
6.465709	395.383748	8.642445
7.125640	394.447341	8.647463
6.959431	393.043939	8.652480
6.940654	382.601477	8.657498
6.617158	375.952630	8.662515
6.300582	379.407386	8.667533
6.578837	389.525391	8.672551
6.576826	396.645176	8.677568
7.035128	388.078212	8.682586
6.967275	393.696711	8.687603
6.867781	393.330563	8.692621
7.141992	385.669741	8.697639
7.059809	385.528095	8.702656
6.781086	366.508036	8.707674
6.507212	373.279095	8.712691
6.614390	370.671548	8.717709
6.818229	364.580697	8.722727
6.831466	369.211359	8.727744
6.735909	374.439724	8.732762
6.682761	381.431818	8.737779
6.387306	389.462250	8.742797
6.792916	396.278332	8.747815
6.390838	398.215952	8.752832
6.450388	393.807621	8.757850
7.319923	396.312849	8.762867
6.968852	405.475448	8.767885
7.029232	391.713355	8.772903
7.252463	405.630041	8.777920
6.926631	396.810398	8.782938
7.076940	393.454489	8.787955
6.760718	381.878382	8.792973
6.259990	379.091531	8.797991
6.211539	403.840270	8.803008
6.710170	400.126832	8.808026
6.477535	401.381509	8.813043
6.687629	406.726093	8.818061
6.701135	399.058776	8.823079
6.525657	406.357220	8.828096
6.801767	416.917382	8.833114
7.020531	424.374965	8.838131
7.063483	422.806247	8.843149
7.238467	429.746837	8.848167
6.905509	413.373435	8.853184
6.780793	404.875720	8.858202
6.909667	419.378392	8.863219
7.301159	420.226017	8.868237
7.113863	406.051447	8.873255
7.054156	408.203663	8.878272
7.051666	401.744347	8.883290
7.046065	396.377409	8.888307
6.914853	399.373945	8.893325
7.136433	400.772045	8.898343
7.164212	400.903499	8.903360
7.150130	400.097943	8.908378
6.994214	409.318327	8.913395
6.841717	400.585131	8.918413
7.160496	401.699764	8.923431
6.879199	397.019794	8.928448
6.829759	404.292177	8.933466
7.203278	401.750190	8.938483
7.136604	407.147606	8.943501
7.196045	396.329969	8.948519
7.034038	399.561699	8.953536
7.099782	394.738994	8.958554
7.357300	393.098792	8.963571
7.372716	406.839761	8.968589
7.480746	387.778017	8.973607
7.191471	398.625565	8.978624
6.815539	393.591202	8.983642
6.689665	403.870363	8.988659
6.983153	403.404773	8.993677
6.942211	397.314395	8.998695
6.851079	399.039197	9.003712
6.878531	398.754143	9.008730
7.155373	406.354094	9.013747
7.173426	418.453670	9.018765
7.642938	414.407127	9.023783
6.898220	404.476017	9.028800
7.084538	402.430411	9.033818
7.272446	408.106669	9.038835
7.122394	400.042109	9.043853
7.303773	400.818514	9.048871
6.777513	398.856154	9.053888
7.069156	413.623646	9.058906
7.515706	419.799017	9.063923
7.414264	420.976336	9.068941
7.076673	402.965834	9.073959
7.159865	409.851372	9.078976
7.296708	408.201674	9.083994
7.766134	408.816186	9.089011
6.968845	403.336607	9.094029
7.006287	408.938613	9.099047
6.741900	403.148324	9.104064
7.401526	423.775196	9.109082
7.458042	420.519182	9.114099
7.404343	427.331503	9.119117
7.533818	432.079666	9.124135
7.205358	414.834570	9.129152
7.138291	400.922028	9.134170
7.179224	416.003353	9.139187
7.290328	420.511399	9.144205
7.387135	425.820091	9.149223
7.122965	431.352597	9.154240
7.192463	425.434251	9.159258
7.889720	432.371905	9.164275
7.290658	425.933470	9.169293
6.834360	423.218544	9.174311
7.454418	419.085297	9.179328
7.600142	420.624670	9.184346
7.482349	425.215917	9.189363
6.897604	428.198312	9.194381
7.462714	424.291420	9.199399
7.563508	421.624906	9.204416
7.195687	428.587428	9.209434
7.545400	427.052696	9.214451
7.263871	438.441844	9.219469
7.365916	429.854940	9.224487
7.309879	426.376724	9.229504
7.315050	428.326277	9.234522
7.301258	428.224407	9.239539
7.286569	417.301609	9.244557
7.426648	420.937284	9.249575
7.551137	430.315714	9.254592
7.455612	424.789290	9.259610
7.723469	420.004338	9.264627
7.175582	432.003250	9.269645
7.420154	422.693442	9.274663
7.539402	426.518571	9.279680
7.271530	433.468591	9.284698
7.527102	426.956210	9.289715
7.016227	436.765546	9.294733
7.283884	429.598029	9.299751
7.093092	426.478592	9.304768
7.187771	434.119720	9.309786
7.510284	444.656849	9.314803
7.329654	450.286723	9.319821
7.502764	444.513080	9.324839
7.646040	448.170350	9.329856
7.642974	452.910883	9.334874
8.116068	442.984601	9.339891
7.545019	437.598950	9.344909
7.699123	424.516412	9.349927
7.589475	427.784124	9.354944
7.510905	434.524606	9.359962
7.508934	423.180097	9.364979
7.244465	431.448687	9.369997
7.851382	431.792353	9.375015
7.804337	429.357281	9.380032
7.573079	423.151547	9.385050
7.857753	425.565383	9.390067
7.556013	425.641170	9.395085
7.596861	428.493989	9.400103
7.618527	428.878861	9.405120
7.410043	425.225718	9.410138
7.609381	427.498292	9.415155
7.462817	431.055806	9.420173
7.915118	443.901545	9.425191
7.752930	436.804530	9.430208
7.474812	429.186048	9.435226
7.411607	433.203865	9.440243
7.682957	444.733605	9.445261
7.806132	445.408681	9.450279
7.726781	449.009315	9.455296
7.721090	459.427466	9.460314
8.130760	445.727367	9.465331
7.840005	447.347753	9.470349
7.515114	433.652304	9.475367
7.776299	440.285907	9.480384
7.948518	441.426661	9.485402
7.658588	439.260013	9.490419
7.834932	434.502019	9.495437
7.835668	424.798076	9.500455
8.070419	426.793707	9.505472
7.737828	426.145350	9.510490
7.731197	425.830923	9.515507
7.607149	426.042968	9.520525
7.740954	438.380037	9.525543
7.496638	437.768340	9.530560
7.595410	445.345716	9.535578
7.950604	453.160626	9.540595
7.728934	453.646739	9.545613
7.311890	455.368962	9.550631
7.714492	450.673342	9.555648
7.300847	452.439213	9.560666
7.792302	447.477211	9.565683
7.606892	446.846817	9.570701
7.716786	449.925503	9.575719
7.609134	452.621715	9.580736
7.613967	464.865403	9.585754
7.996355	465.966918	9.590771
7.890418	472.071083	9.595789
7.959000	478.034299	9.600807
8.079388	475.730775	9.605824
8.057910	479.884073	9.610842
7.960116	463.076154	9.615859
8.041810	456.281741	9.620877
7.923382	457.439633	9.625895
7.668517	453.983096	9.630912
7.992983	469.379799	9.635930
8.226497	469.573691	9.640947
8.290977	466.423717	9.645965
8.008937	462.371843	9.650983
8.188404	455.858753	9.656000
8.046946	460.747202	9.661018
8.015717	458.533706	9.666035
8.206774	455.348124	9.671053
8.395134	448.151999	9.676071
7.827605	453.896142	9.681088
8.006087	460.896156	9.686106
8.226519	458.393925	9.691123
8.136925	459.818695	9.696141
8.065170	460.839889	9.701159
7.975607	454.078621	9.706176
7.945961	449.769457	9.711194
7.800333	458.508580	9.716211
8.107959	461.622559	9.721229
7.976046	453.621402	9.726247
8.041617	453.633328	9.731264
7.939839	466.171426	9.736282
7.749541	457.573511	9.741299
8.246282	456.366029	9.746317
7.911997	461.884285	9.751335
7.921755	450.597880	9.756352
7.813300	470.076535	9.761370
8.134696	477.931464	9.766387
8.406160	472.132934	9.771405
8.363889	477.466588	9.776423
8.088376	474.470868	9.781440
8.524794	478.893244	9.786458
8.167373	467.617023	9.791475
7.824203	469.315050	9.796493
7.873557	468.196598	9.801511
7.907045	481.066959	9.806528
8.136950	486.553628	9.811546
8.564464	489.759279	9.816563
8.466418	488.420927	9.821581
8.792156	485.028048	9.826599
8.560675	473.921435	9.831616
8.197015	469.352180	9.836634
8.184018	455.686740	9.841651
7.940414	471.393352	9.846669
7.740448	458.400980	9.851687
7.923753	468.795835	9.856704
8.239519	488.766612	9.861722
8.379646	480.123226	9.866739
8.111316	479.650988	9.871757
8.222451	489.227198	9.876775
8.177102	481.688987	9.881792
8.218329	486.350007	9.886810
8.333621	478.420559	9.891827
8.127199	485.181092	9.896845
8.209685	481.933622	9.901863
8.577925	477.341207	9.906880
8.559714	484.365736	9.911898
8.540302	481.178412	9.916915
8.531443	474.843142	9.921933
8.106378	478.709385	9.926951
8.393173	476.881554	9.931968
8.496901	480.535560	9.936986
8.555180	479.526162	9.942003
8.764979	478.622409	9.947021
8.474612	489.085180	9.952039
8.933407	470.561673	9.957056
8.360449	471.768692	9.962074
8.433279	468.166136	9.967091
8.783888	468.051352	9.972109
7.791577	474.852965	9.977127
8.080281	472.412618	9.982144
8.446017	478.386080	9.987162
8.475181	478.097600	9.992179
8.738820	481.322614	9.997197
8.188057	484.318628	10.002215
8.404823	471.832145	10.007232
8.412170	484.179591	10.012250
8.602819	476.039525	10.017267
8.554801	479.183982	10.022285
8.000117	491.947693	10.027303
8.486666	475.635178	10.032320
8.641238	485.135154	10.037338
8.397600	471.619446	10.042355
8.875936	472.592321	10.047373
8.396791	489.481394	10.052391
8.392895	475.786111	10.057408
8.660995	477.571399	10.062426
8.620379	476.602742	10.067443
8.847504	485.299254	10.072461
8.611823	484.089763	10.077479
8.371756	481.176850	10.082496
8.376710	473.940024	10.087514
8.710322	485.371675	10.092531
8.651877	481.578248	10.097549
8.394695	484.676585	10.102567
8.919432	478.573286	10.107584
8.755365	481.003790	10.112602
8.510312	480.581553	10.117619
8.906811	479.759000	10.122637
8.780335	486.750001	10.127655
8.500397	477.209925	10.132672
8.542138	480.201466	10.137690
8.620971	485.970577	10.142707
8.828102	489.763016	10.147725
8.793997	494.154978	10.152743
8.604420	477.273064	10.157760
8.570256	490.977685	10.162778
8.373830	492.068906	10.167795
8.663854	488.059936	10.172813
8.463722	484.377070	10.177831
8.305485	501.017062	10.182848
8.543591	506.991596	10.187866
8.797540	512.922625	10.192883
9.024570	509.198072	10.197901
8.882793	511.943820	10.202919
8.586392	517.370951	10.207936
8.962964	507.017949	10.212954
9.056707	511.617100	10.217971
8.782776	507.592346	10.222989
8.943188	509.473404	10.228007
8.849816	505.840077	10.233024
8.938478	501.146296	10.238042
9.126395	503.174520	10.243059
9.392862	484.283506	10.248077
8.432449	487.141736	10.253095
8.711846	474.670684	10.258112
8.812032	484.340124	10.263130
8.726390	498.169579	10.268147
9.260834	495.955810	10.273165
9.045235	493.704927	10.278183
9.039143	480.767367	10.283200
8.741362	476.127828	10.288218
8.844764	476.799692	10.293235
8.984216	477.844598	10.298253
8.956992	494.344137	10.303271
9.174928	486.572171	10.308288
8.866926	485.058435	10.313306
8.551274	483.239790	10.318323
8.942250	488.758027	10.323341
8.825110	507.862548	10.328359
9.098672	502.360321	10.333376
9.012887	507.924861	10.338394
8.888285	502.188378	10.343411
9.325756	505.364069	10.348429
9.388010	503.246373	10.353447
9.103996	492.450933	10.358464
8.773038	490.883990	10.363482
8.870089	501.052541	10.368499
9.057919	499.833498	10.373517
9.005907	504.979340	10.378535
9.155254	500.771505	10.383552
8.815985	502.147036	10.388570
8.901999	514.933453	10.393587
9.311503	499.005369	10.398605
9.156109	497.344647	10.403623
8.942222	497.012199	10.408640
9.264767	503.216495	10.413658
9.099404	501.825575	10.418675
9.175463	495.827283	10.423693
9.330753	495.339163	10.428711
9.200854	502.548454	10.433728
9.507528	496.883254	10.438746
9.278696	505.916300	10.443763
9.111903	504.393061	10.448781
8.567685	504.560488	10.453799
8.609082	504.604603	10.458816
9.023372	488.937706	10.463834
8.996281	502.391922	10.468851
9.186497	488.918677	10.473869
9.153055	503.743490	10.478887
9.205556	500.608010	10.483904
9.241877	502.041456	10.488922
9.215622	499.713569	10.493939
9.305736	491.901668	10.498957
9.266354	501.930651	10.503975
9.203304	500.933950	10.508992
9.104159	500.081758	10.514010
9.257295	505.826611	10.519027
8.964177	508.321519	10.524045
9.662571	521.548473	10.529063
9.443706	512.787751	10.534080
9.411863	501.539389	10.539098
9.111034	505.133712	10.544115
9.462351	499.969593	10.549133
9.546085	510.048719	10.554151
9.228549	499.381602	10.559168
9.361568	499.824766	10.564186
9.292830	504.430438	10.569203
9.118630	501.901671	10.574221
9.385773	517.575637	10.579239
9.095362	518.290270	10.584256
10.090598	515.269008	10.589274
9.713800	521.576573	10.594291
9.137451	496.424015	10.599309
9.459339	508.431866	10.604327
9.267801	520.696892	10.609344
9.884459	521.452440	10.614362
9.447693	513.439062	10.619379
9.671343	500.014217	10.624397
9.689836	496.697877	10.629415
9.974391	498.284931	10.634432
9.666572	495.761322	10.639450
9.428671	503.050650	10.644467
9.755278	493.649058	10.649485
9.382873	493.095297	10.654503
9.429606	501.924222	10.659520
9.714854	491.863245	10.664538
10.155102	497.613602	10.669555
9.973360	483.015228	10.674573
9.466887	498.116120	10.679591
9.372122	496.628933	10.684608
9.442379	488.766496	10.689626
9.077969	493.816117	10.694643
9.443835	492.263070	10.699661
9.528030	493.083109	10.704679
9.648907	496.857505	10.709696
9.945228	484.106087	10.714714
9.453842	495.758522	10.719731
9.766597	497.811367	10.724749
9.402308	491.074195	10.729767
9.267876	500.723600	10.734784
9.651919	495.525954	10.739802
9.424636	500.393147	10.744819
9.398509	494.603368	10.749837
9.990733	509.380648	10.754855
9.495397	514.393984	10.759872
9.704888	506.626488	10.764890
10.035631	518.241643	10.769907
9.978630	505.999999	10.774925
9.409135	497.925374	10.779943
9.709142	510.296412	10.784960
9.782265	506.536014	10.789978
9.920602	514.728907	10.794995
9.840145	504.933501	10.800013
9.694056	498.345173	10.805031
9.530609	500.175988	10.810048
9.899445	511.712588	10.815066
9.699664	519.724932	10.820083
9.976873	524.888625	10.825101
9.816144	523.206646	10.830119
9.864563	523.533680	10.835136
10.198782	516.866934	10.840154
9.880116	510.381380	10.845171
9.771583	499.870862	10.850189
9.949192	500.710978	10.855207
9.664683	524.468091	10.860224
9.904194	513.738933	10.865242
9.888333	515.208958	10.870259
9.528206	523.877581	10.875277
10.506406	527.568151	10.880295
9.622714	524.699269	10.885312
9.974776	519.329904	10.890330
9.817385	531.924099	10.895347
9.842731	529.225209	10.900365
9.896378	531.280786	10.905383
9.827078	530.812075	10.910400
9.862961	525.637412	10.915418
9.957449	524.256269	10.920435
10.068761	527.281098	10.925453
10.054532	529.120094	10.930471
9.843825	522.428273	10.935488
9.975294	521.268551	10.940506
10.019923	527.462752	10.945523
9.853783	519.501642	10.950541
10.036306	510.084748	10.955559
10.223878	525.846927	10.960576
9.689441	519.912721	10.965594
9.857200	524.203636	10.970611
10.034367	530.844126	10.975629
9.889331	525.142394	10.980647
9.898588	523.408535	10.985664
9.862222	520.779276	10.990682
9.704121	530.732204	10.995699
9.669524	538.033873	11.000717
10.175085	547.841803	11.005735
10.141905	546.963494	11.010752
10.553748	544.535402	11.015770
10.053924	545.267068	11.020787
10.052345	541.903371	11.025805
10.053356	548.322162	11.030823
10.042247	548.626965	11.035840
10.360484	545.490867	11.040858
10.187861	547.929033	11.045875
10.082633	548.125507	11.050893
10.437481	546.163932	11.055911
9.806520	547.711399	11.060928
10.080066	556.993959	11.065946
10.251918	553.741941	11.070963
10.211486	546.202931	11.075981
10.240586	546.899062	11.080999
10.009258	548.951954	11.086016
10.207189	549.340769	11.091034
10.447361	550.761214	11.096051
9.799591	555.568074	11.101069
10.434286	554.458891	11.106087
10.240751	570.501725	11.111104
10.811208	569.172234	11.116122
10.244666	557.751997	11.121139
10.266436	556.858766	11.126157
10.446959	555.934351	11.131175
9.877607	572.796612	11.136192
10.755455	557.849125	11.141210
10.751173	570.365709	11.146227
10.616512	568.070577	11.151245
10.454751	542.370162	11.156263
10.802819	556.964833	11.161280
10.455369	540.489443	11.166298
10.405841	550.075080	11.171315
9.970034	544.844930	11.176333
10.466181	533.718948	11.181351
10.335333	547.527122	11.186368
10.305072	561.549918	11.191386
10.915434	570.413642	11.196403
10.594393	566.752859	11.201421
10.263158	554.191235	11.206439
10.376447	561.813723	11.211456
10.721409	564.448503	11.216474
11.118891	564.446294	11.221491
10.789661	554.715085	11.226509
10.818356	547.455576	11.231527
10.600535	554.561900	11.236544
10.299940	544.857768	11.241562
10.855014	547.784670	11.246579
10.517946	550.523154	11.251597
10.665141	542.282569	11.256615
10.759514	543.056834	11.261632
10.625485	549.332683	11.266650
10.326545	547.432518	11.271667
10.375024	553.196940	11.276685
10.948236	543.365368	11.281703
10.462838	544.533426	11.286720
10.661385	547.964308	11.291738
10.678864	543.682451	11.296755
10.418380	553.165444	11.301773
10.695912	563.457230	11.306791
10.428436	566.187967	11.311808
10.708966	576.681260	11.316826
10.971925	568.873802	11.321843
10.730767	575.191691	11.326861
11.049991	573.933121	11.331879
10.769531	578.685592	11.336896
11.051540	569.975752	11.341914
10.364606	560.966454	11.346931
10.938620	576.466160	11.351949
11.187918	567.761446	11.356967
10.674928	559.333960	11.361984
10.617768	552.113146	11.367002
10.828315	552.926014	11.372019
10.746524	569.099660	11.377037
11.166864	564.644226	11.382055
10.795205	571.998720	11.387072
10.740393	575.049586	11.392090
11.130128	574.079767	11.397107
11.132207	570.668155	11.402125
10.639891	553.388638	11.407143
10.625989	564.836919	11.412160
10.836332	562.206868	11.417178
10.779678	562.313682	11.422195
10.921309	569.051272	11.427213
11.001577	568.745317	11.432231
10.653148	565.559036	11.437248
10.897828	565.874255	11.442266
11.023500	570.537845	11.447283
10.651153	579.912147	11.452301
11.317615	570.002835	11.457319
11.272585	564.818747	11.462336
10.773837	570.451166	11.467354
11.129776	561.180641	11.472371
10.985838	571.879291	11.477389
10.662362	559.833994	11.482407
10.508554	565.260889	11.487424
10.402862	575.578011	11.492442
11.036404	582.336362	11.497459
11.250777	590.034542	11.502477
10.898964	596.606459	11.507495
11.194386	598.270715	11.512512
11.017452	598.639370	11.517530
11.354965	583.038069	11.522547
11.412086	601.234924	11.527565
11.253391	604.677609	11.532583
10.948428	588.312282	11.537600
11.500200	595.922887	11.542618
11.384218	587.909708	11.547635
11.117848	577.950889	11.552653
11.299949	579.427772	11.557671
11.113860	574.805421	11.562688
10.953237	579.539116	11.567706
11.588923	595.054422	11.572723
11.372209	588.827418	11.577741
11.357439	577.424856	11.582759
11.231073	563.455207	11.587776
11.031057	574.500313	11.592794
11.410482	580.471665	11.597811
11.167589	597.954980	11.602829
11.442175	603.024433	11.607847
11.529799	592.710343	11.612864
11.422367	586.409413	11.617882
11.131996	575.494999	11.622899
11.522928	591.802881	11.627917
11.454157	581.080959	11.632935
11.318465	573.364362	11.637952
11.225618	582.574954	11.642970
11.660553	575.226537	11.647987
11.202508	578.552019	11.653005
11.615277	582.826650	11.658023
11.591713	583.881325	11.663040
11.210208	568.597818	11.668058
11.662263	578.104882	11.673075
11.211536	580.261580	11.678093
11.645004	587.177511	11.683111
11.767451	586.748184	11.688128
11.593364	575.862887	11.693146
11.458588	566.315798	11.698163
11.166322	566.885557	11.703181
11.449989	584.150660	11.708199
11.745776	584.230656	11.713216
11.495321	587.548860	11.718234
11.508066	586.107937	11.723251
11.773887	595.451686	11.728269
11.442547	586.090018	11.733287
11.855106	592.068805	11.738304
11.264324	582.943446	11.743322
11.752358	575.435232	11.748339
11.524363	588.135202	11.753357
11.371375	592.135563	11.758375
11.768986	591.451686	11.763392
11.270449	600.293509	11.768410
11.932288	593.007363	11.773427
11.920848	594.826994	11.778445
11.839578	588.793361	11.783463
11.731682	591.117250	11.788480
11.294788	591.476143	11.793498
11.655570	587.913653	11.798515
12.031017	598.209052	11.803533
11.674116	602.768381	11.808551
11.728130	601.311522	11.813568
11.697798	597.731416	11.818586
11.720906	585.398271	11.823603
11.811582	596.558789	11.828621
12.051085	592.908004	11.833639
11.945900	595.581760	11.838656
11.994406	595.520621	11.843674
12.040748	583.751877	11.848691
11.483297	580.866584	11.853709
11.770767	583.683943	11.858727
12.113066	589.938823	11.863744
12.134946	595.025777	11.868762
11.831559	571.660698	11.873779
11.350409	577.154663	11.878797
11.717032	587.991077	11.883815
11.931834	588.847460	11.888832
11.590911	589.670995	11.893850
11.794778	594.224511	11.898867
11.637909	595.722947	11.903885
11.767015	592.237781	11.908903
11.823446	592.787621	11.913920
11.993192	599.309379	11.918938
12.176298	584.240350	11.923955
11.686630	596.933989	11.928973
11.949172	594.024357	11.933991
12.355006	588.656014	11.939008
11.798339	588.045914	11.944026
12.236464	601.686089	11.949043
12.196979	607.218159	11.954061
12.058441	599.205352	11.959079
12.269512	594.268306	11.964096
11.864597	596.086471	11.969114
12.149604	591.216737	11.974131
12.225590	599.690835	11.979149
12.039486	591.890610	11.984167
12.424437	593.439852	11.989184
12.063141	595.885495	11.994202
12.564960	598.224307	11.999219
12.420299	596.684969	12.004237
12.074094	596.313291	12.009255
12.260471	590.310306	12.014272
12.018657	593.021248	12.019290
12.192776	592.934116	12.024307
12.173093	600.978239	12.029325
11.952236	586.789848	12.034343
12.315637	589.749945	12.039360
12.436967	596.897821	12.044378
12.124418	592.923279	12.049395
12.118250	597.241462	12.054413
12.197948	595.083153	12.059431
12.250630	593.083710	12.064448
12.001614	599.295542	12.069466
12.185440	586.422823	12.074483
12.130693	606.230879	12.079501
12.092759	618.708589	12.084519
12.671048	612.843006	12.089536
12.704036	630.990025	12.094554
12.452617	608.655009	12.099571
12.516589	598.827456	12.104589
12.427535	602.375993	12.109607
12.635497	601.090673	12.114624
12.270728	597.013860	12.119642
12.164228	598.469691	12.124659
11.866808	609.132451	12.129677
12.300381	616.269282	12.134695
12.303171	613.573914	12.139712
12.018482	623.360536	12.144730
12.422328	615.338480	12.149747
12.413229	619.960083	12.154765
12.546763	623.224443	12.159783
12.661972	618.245606	12.164800
12.415502	624.280324	12.169818
12.209341	617.682429	12.174835
12.607397	619.317982	12.179853
12.353569	622.968079	12.184871
12.302958	616.544628	12.189888
12.451625	622.896129	12.194906
12.454063	627.957737	12.199923
12.689620	630.704343	12.204941
12.932372	638.514861	12.209959
12.684309	620.584786	12.214976
12.577648	617.016634	12.219994
12.490950	629.748144	12.225011
12.666256	633.488795	12.230029
12.956649	633.670622	12.235047
13.006054	634.805385	12.240064
12.635565	618.863705	12.245082
12.708920	615.068535	12.250099
12.825026	614.280440	12.255117
12.788823	617.309463	12.260135
12.571045	607.223094	12.265152
12.604995	624.088708	12.270170
12.916071	625.232964	12.275187
13.235177	625.713247	12.280205
13.129149	618.313872	12.285223
13.014091	612.512742	12.290240
12.633152	618.966155	12.295258
12.786115	613.517504	12.300275
12.890722	617.556406	12.305293
12.936464	619.389171	12.310311
12.779324	621.001260	12.315328
12.794966	618.897165	12.320346
12.855707	614.889377	12.325363
13.273990	610.494214	12.330381
12.938829	618.818146	12.335399
12.766904	609.380996	12.340416
12.908922	619.836057	12.345434
12.761568	624.324689	12.350451
13.019879	625.603445	12.355469
12.979554	625.117569	12.360487
12.950777	620.565232	12.365504
13.103602	625.653769	12.370522
12.824504	642.429593	12.375539
13.422137	641.278875	12.380557
13.134019	626.491924	12.385575
12.827864	618.921934	12.390592
13.073573	633.217127	12.395610
12.839034	641.900843	12.400627
13.041317	644.065687	12.405645
12.782315	637.109993	12.410663
13.167882	634.436698	12.415680
13.152795	636.708182	12.420698
13.250157	638.561263	12.425715
13.175883	637.348563	12.430733
13.009708	645.699679	12.435751
13.376088	636.720968	12.440768
13.277449	638.058807	12.445786
12.880327	642.031159	12.450803
13.236097	627.547264	12.455821
13.290222	631.641415	12.460839
13.381375	625.388252	12.465856
13.152975	632.480486	12.470874
13.348905	630.250312	12.475891
13.384362	637.260182	12.480909
13.066418	640.652086	12.485927
13.592343	634.548548	12.490944
13.506029	641.381840	12.495962
13.539880	643.052369	12.500979
13.559824	637.261636	12.505997
13.445746	643.395537	12.511015
13.341683	634.843984	12.516032
13.065852	630.118915	12.521050
13.368648	645.260391	12.526067
13.477872	638.568893	12.531085
13.217744	635.788484	12.536103
13.647006	633.379741	12.541120
13.330740	632.772998	12.546138
13.310641	636.519021	12.551155
13.381964	634.863789	12.556173
13.448516	638.690909	12.561191
13.384243	631.158755	12.566208
13.286267	630.101247	12.571226
13.247346	634.292028	12.576243
13.597161	633.855477	12.581261
13.058842	636.095333	12.586279
13.559894	639.759702	12.591296
13.627280	638.070373	12.596314
13.451455	642.203711	12.601331
13.397056	650.625679	12.606349
13.640895	640.870906	12.611367
13.813411	644.634088	12.616384
13.931834	648.194308	12.621402
13.464365	645.556836	12.626419
13.673341	634.762962	12.631437
13.506237	637.276014	12.636455
13.422845	650.237393	12.641472
13.866775	658.044801	12.646490
13.589157	661.594492	12.651507
14.045773	663.274524	12.656525
13.646638	658.013347	12.661543
13.862896	655.319240	12.666560
14.147527	645.649591	12.671578
13.634518	653.493323	12.676595
13.784677	628.214126	12.681613
13.806201	638.075854	12.686631
13.603410	637.350347	12.691648
14.110056	639.663162	12.696666
13.871158	638.034445	12.701683
14.187300	636.962545	12.706701
13.808178	632.294684	12.711719
13.729350	638.479865	12.716736
13.790407	635.765897	12.721754
13.358999	645.026412	12.726771
14.040898	649.583938	12.731789
13.966514	659.066231	12.736807
14.072408	664.594476	12.741824
14.364126	654.860596	12.746842
13.954420	652.996709	12.751859
13.945388	643.587666	12.756877
13.822273	652.616846	12.761895
13.784466	650.088778	12.766912
14.204395	659.080213	12.771930
14.077268	659.456845	12.776947
14.157611	655.155644	12.781965
14.248933	654.125280	12.786983
13.820554	643.642700	12.792000
14.591153	639.911848	12.797018
13.894589	641.800960	12.802035
13.711948	641.394186	12.807053
14.223432	657.547541	12.812071
13.940607	656.547396	12.817088
14.074682	655.311518	12.822106
14.160977	659.631008	12.827123
14.130892	661.967961	12.832141
13.796986	659.012916	12.837159
14.025750	658.245038	12.842176
14.303772	650.034399	12.847194
14.067645	660.394098	12.852211
14.035433	662.068668	12.857229
13.964155	653.152209	12.862247
13.881927	655.446838	12.867264
14.296718	643.503562	12.872282
14.019886	664.507810	12.877299
14.321585	664.100888	12.882317
14.439329	675.645378	12.887335
14.176594	668.242133	12.892352
14.517474	664.515490	12.897370
14.467121	683.445633	12.902387
14.531354	673.523324	12.907405
14.545748	660.446725	12.912423
14.237595	659.005581	12.917440
14.649883	658.054315	12.922458
14.536805	659.621635	12.927475
14.402240	657.982880	12.932493
14.316121	655.446602	12.937511
14.576266	655.626857	12.942528
14.336768	649.636929	12.947546
14.527337	655.991345	12.952563
14.752689	664.401046	12.957581
14.751401	660.027428	12.962599
14.299589	659.637581	12.967616
14.559397	658.353601	12.972634
14.654146	648.757882	12.977651
14.832990	653.978050	12.982669
14.407819	660.807636	12.987687
14.484054	658.949662	12.992704
14.504821	655.576131	12.997722
14.547604	668.886982	13.002739
15.000488	666.916345	13.007757
14.773172	665.850697	13.012775
14.128947	666.747003	13.017792
14.645252	672.406606	13.022810
14.420893	677.188183	13.027827
14.694818	683.586353	13.032845
14.698804	678.498694	13.037863
14.800878	674.137280	13.042880
15.236861	674.327854	13.047898
14.794251	682.469836	13.052915
14.983220	670.432536	13.057933
15.065911	677.043702	13.062951
14.688430	677.001969	13.067968
14.861236	668.429111	13.072986
14.967647	682.329603	13.078003
15.098855	668.442590	13.083021
14.945185	654.347760	13.088039
14.738635	658.997154	13.093056
14.833975	653.137799	13.098074
14.777241	664.091084	13.103091
14.922029	669.651106	13.108109
15.001122	678.326725	13.113127
14.677095	685.541260	13.118144
14.889050	685.255696	13.123162
14.775266	680.110750	13.128179
14.856756	674.158884	13.133197
14.961844	680.015462	13.138215
14.708453	685.776731	13.143232
15.079069	677.737763	13.148250
14.854985	685.817106	13.153267
14.766532	684.098541	13.158285
15.258278	680.300919	13.163303
14.798343	677.554965	13.168320
15.091186	678.187687	13.173338
15.108960	688.709592	13.178355
15.076660	685.855609	13.183373
15.113003	672.709290	13.188391
15.011435	691.663246	13.193408
15.392434	675.900416	13.198426
14.932841	682.303060	13.203443
15.148853	683.951364	13.208461
14.926246	682.020289	13.213479
14.831009	689.167420	13.218496
15.118429	691.025442	13.223514
15.346534	702.268636	13.228531
15.254676	698.594008	13.233549
15.569374	706.828784	13.238567
15.450661	699.996251	13.243584
15.839137	703.914957	13.248602
15.495371	703.356702	13.253619
15.288870	687.386111	13.258637
15.327447	683.880396	13.263655
15.611052	679.045571	13.268672
15.510302	673.059143	13.273690
14.960495	684.796593	13.278707
15.750264	697.251971	13.283725
15.580128	687.438958	13.288743
15.762803	683.074381	13.293760
15.446235	679.857840	13.298778
15.192342	673.153794	13.303795
15.158099	675.254716	13.308813
15.575986	689.406212	13.313831
15.576812	696.838096	13.318848
15.564350	697.708002	13.323866
15.463688	700.952265	13.328883
15.436459	707.198813	13.333901
15.678195	697.166629	13.338919
16.022742	697.440957	13.343936
15.856130	682.716972	13.348954
15.605529	681.828541	13.353971
15.513427	668.165865	13.358989
15.290255	675.487669	13.364007
15.742230	689.876821	13.369024
15.571069	696.010217	13.374042
15.970132	688.803074	13.379059
15.634478	696.821007	13.384077
15.786155	686.894457	13.389095
16.131525	705.406017	13.394112
15.596350	688.944123	13.399130
15.668196	694.155821	13.404147
15.721771	688.233570	13.409165
16.171635	687.178586	13.414183
15.852102	694.379797	13.419200
15.878670	679.190047	13.424218
15.993880	684.688437	13.429235
15.756052	687.755373	13.434253
16.115677	689.087687	13.439271
15.738316	684.741428	13.444288
15.886334	686.835885	13.449306
16.019270	684.031752	13.454323
15.751090	694.996094	13.459341
15.965026	686.902776	13.464359
16.280826	696.355513	13.469376
16.094895	679.434966	13.474394
15.875209	681.066328	13.479411
15.638571	680.257760	13.484429
16.232059	684.633488	13.489447
15.885303	702.240477	13.494464
16.019187	703.100076	13.499482
15.996493	702.201182	13.504499
16.079478	698.817895	13.509517
16.245924	700.401383	13.514535
16.066026	702.414676	13.519552
16.466841	704.747237	13.524570
16.244997	704.065738	13.529587
16.284000	705.909034	13.534605
15.977514	687.445247	13.539623
16.183854	701.812935	13.544640
16.358493	696.203073	13.549658
15.899432	698.973315	13.554675
15.702673	702.213700	13.559693
16.385836	698.701663	13.564711
16.285787	704.994333	13.569728
16.221974	697.181213	13.574746
16.172581	698.154735	13.579763
16.016456	694.739485	13.584781
16.423727	689.077397	13.589799
16.115283	704.674453	13.594816
16.244012	702.161311	13.599834
16.220002	696.623598	13.604851
16.164912	701.722642	13.609869
16.222022	698.993504	13.614887
16.099380	697.879896	13.619904
16.277754	713.021989	13.624922
16.683285	718.538018	13.629939
16.502618	723.798755	13.634957
16.422850	724.805440	13.639975
16.544745	724.843255	13.644992
16.720092	719.529920	13.650010
16.889511	713.030933	13.655027
16.839282	711.186456	13.660045
16.948536	703.797497	13.665063
16.293534	698.440698	13.670080
16.169223	693.824415	13.675098
16.512312	700.224377	13.680115
16.682995	709.153905	13.685133
16.692367	718.522120	13.690151
16.673552	720.554358	13.695168
16.586708	718.822915	13.700186
16.620772	721.137201	13.705203
16.677947	715.927589	13.710221
16.519344	726.230998	13.715239
16.868271	717.535848	13.720256
16.454291	721.217369	13.725274
16.868256	717.135281	13.730291
16.712968	716.105682	13.735309
16.855976	715.821453	13.740327
17.077266	712.691048	13.745344
17.076867	716.159446	13.750362
17.341186	720.826599	13.755379
17.091025	709.432432	13.760397
16.558042	697.132689	13.765415
16.839741	692.907228	13.770432
16.763252	709.162221	13.775450
16.910035	708.170501	13.780467
16.902352	705.255854	13.785485
17.137919	702.217888	13.790503
16.796047	709.627732	13.795520
16.747897	713.460217	13.800538
16.815943	712.376691	13.805555
16.637727	702.899451	13.810573
17.073114	712.630105	13.815591
16.858551	716.412924	13.820608
16.792106	710.228604	13.825626
16.863550	707.907473	13.830643
16.798968	709.968971	13.835661
17.066065	716.989915	13.840679
17.172619	729.325144	13.845696
17.120342	733.287667	13.850714
17.179337	730.637124	13.855731
17.089699	736.416933	13.860749
17.181516	734.398719	13.865767
17.431611	732.879571	13.870784
17.392657	731.146934	13.875802
17.696727	713.395344	13.880819
17.149276	705.443402	13.885837
17.030601	710.505075	13.890855
17.030270	701.864653	13.895872
17.045581	734.203028	13.900890
17.310693	721.036609	13.905907
17.559834	733.396837	13.910925
17.669739	726.203426	13.915943
17.973359	726.241171	13.920960
17.506821	717.875758	13.925978
17.553671	700.817733	13.930995
17.484158	712.315848	13.936013
17.429299	696.214192	13.941031
17.267155	696.069292	13.946048
17.636655	695.187844	13.951066
17.701428	708.987584	13.956083
17.477750	700.214900	13.961101
17.766644	695.925195	13.966119
17.607148	698.392882	13.971136
17.769776	712.104709	13.976154
17.665915	696.944848	13.981171
17.680540	705.428610	13.986189
17.330106	700.241841	13.991207
17.169884	701.169612	13.996224
16.833080	706.779855	14.001242
17.737857	721.413668	14.006259
17.543454	738.965263	14.011277
17.613451	727.994293	14.016295
17.795310	729.540655	14.021312
17.693715	730.800068	14.026330
17.860918	730.445776	14.031347
17.839803	723.822004	14.036365
18.305149	718.535816	14.041383
17.969773	727.058648	14.046400
17.690669	725.016500	14.051418
18.001668	721.843636	14.056435
17.985756	729.612671	14.061453
17.915497	730.415895	14.066471
17.915607	732.224263	14.071488
17.933884	730.195481	14.076506
18.161125	717.517837	14.081523
17.876534	715.545977	14.086541
17.874812	714.605927	14.091559
17.652041	721.975024	14.096576
17.623227	725.192256	14.101594
18.005474	730.674067	14.106611
17.960648	728.071348	14.111629
18.027613	725.728825	14.116647
17.951328	729.818186	14.121664
17.834577	730.818042	14.126682
18.374140	725.684325	14.131699
18.259239	729.823917	14.136717
18.117704	731.645010	14.141735
18.459841	729.480280	14.146752
18.013872	729.146320	14.151770
18.457374	726.072615	14.156787
18.230880	728.058498	14.161805
18.159860	726.321418	14.166823
18.173500	727.367117	14.171840
17.950308	733.653844	14.176858
18.040673	723.635895	14.181875
17.794134	737.919934	14.186893
18.115664	733.568302	14.191911
17.993418	727.597847	14.196928
17.775685	732.801278	14.201946
18.015740	738.964934	14.206963
18.184698	749.210722	14.211981
18.683372	743.758359	14.216999
18.295116	743.661509	14.222016
18.646798	753.834490	14.227034
18.095879	746.182874	14.232051
18.759286	744.144531	14.237069
18.677697	753.710054	14.242087
18.801990	747.457967	14.247104
18.710792	747.592285	14.252122
18.992527	749.072507	14.257139
18.565643	730.662253	14.262157
18.528929	726.802254	14.267175
18.488002	720.677048	14.272192
18.344305	725.755269	14.277210
18.539214	731.774516	14.282227
18.771924	740.441877	14.287245
19.007673	743.674464	14.292263
18.440163	733.500808	14.297280
18.557930	737.307302	14.302298
18.842200	736.925200	14.307315
18.955056	737.513541	14.312333
18.616427	730.305198	14.317351
18.579116	735.335194	14.322368
18.765088	740.415415	14.327386
18.982809	742.931303	14.332403
18.507609	742.690285	14.337421
18.500426	742.622092	14.342439
19.005656	743.944220	14.347456
18.062046	754.582079	14.352474
18.701435	750.549871	14.357491
18.366350	744.379227	14.362509
18.826016	751.950683	14.367527
19.011762	752.568630	14.372544
18.575939	748.187333	14.377562
19.097859	755.253574	14.382579
19.025604	763.896144	14.387597
19.271839	771.169688	14.392615
18.990587	756.744470	14.397632
18.932721	758.202162	14.402650
19.065202	756.953904	14.407667
19.321972	760.262096	14.412685
18.712064	759.840212	14.417703
19.144605	763.726781	14.422720
19.491874	770.328086	14.427738
19.060166	762.632539	14.432755
19.215608	768.058378	14.437773
19.284866	763.695772	14.442791
19.144303	757.586165	14.447808
19.035064	765.581278	14.452826
19.261753	773.678396	14.457843
19.014422	763.246274	14.462861
19.021760	771.551328	14.467879
19.480487	773.095340	14.472896
19.334655	768.542370	14.477914
19.418941	773.250367	14.482931
19.197808	766.651607	14.487949
19.269585	771.576159	14.492967
19.685820	774.509074	14.497984
19.518871	776.274193	14.503002
19.735577	766.924391	14.508019
19.705999	759.052231	14.513037
19.298355	762.877935	14.518055
19.341347	761.662632	14.523072
19.426750	771.618567	14.528090
19.551441	765.426372	14.533107
20.196584	759.304114	14.538125
19.400933	756.648616	14.543143
19.658702	755.607947	14.548160
19.543047	756.550828	14.553178
19.842729	758.485831	14.558195
19.442929	744.057108	14.563213
19.696479	760.004817	14.568231
19.411646	753.169889	14.573248
19.763029	767.792616	14.578266
19.978780	764.202322	14.583283
19.546785	763.705225	14.588301
19.482602	775.230947	14.593319
19.681099	763.602347	14.598336
19.644026	768.796418	14.603354
19.693981	764.985947	14.608371
19.882442	764.022408	14.613389
19.898939	772.180860	14.618407
19.718449	764.682637	14.623424
19.604533	771.340422	14.628442
19.799569	765.992430	14.633459
19.792113	756.207539	14.638477
19.535282	759.217505	14.643495
19.797817	761.259314	14.648512
19.901815	757.755959	14.653530
19.638058	755.162292	14.658547
20.100838	772.333242	14.663565
19.981217	786.553254	14.668583
20.033866	783.553401	14.673600
20.289389	782.945428	14.678618
20.065606	797.891827	14.683635
20.236387	782.688862	14.688653
20.287702	779.364170	14.693671
19.940119	779.582840	14.698688
20.310392	782.939525	14.703706
20.046402	783.160877	14.708723
20.300855	778.920730	14.713741
20.545712	787.242227	14.718759
20.296838	781.177984	14.723776
20.100010	770.649582	14.728794
19.922777	778.443914	14.733811
20.363153	782.057859	14.738829
20.208144	782.817559	14.743847
20.074893	783.034206	14.748864
20.441249	783.961528	14.753882
20.658140	789.851119	14.758899
20.683046	786.966067	14.763917
20.542335	782.860417	14.768935
20.275057	777.042056	14.773952
20.328899	786.838843	14.778970
20.452441	791.496513	14.783987
20.338637	775.482917	14.789005
20.416765	787.374514	14.794023
20.586087	780.862895	14.799040
20.374687	785.793949	14.804058
20.530666	783.304928	14.809075
20.616529	786.355880	14.814093
20.405576	789.753139	14.819111
20.507292	778.843440	14.824128
20.944131	783.761291	14.829146
20.454919	786.949682	14.834163
20.763503	776.641892	14.839181
20.349359	785.764073	14.844199
20.743371	785.686670	14.849216
20.616662	777.735045	14.854234
20.552782	778.177509	14.859251
20.903318	773.546767	14.864269
20.657592	773.585376	14.869287
20.685215	779.375229	14.874304
20.518435	778.877604	14.879322
20.740395	785.959297	14.884339
21.339898	797.791304	14.889357
21.444657	790.844826	14.894375
21.143902	790.191466	14.899392
21.349290	782.743230	14.904410
20.843752	784.801242	14.909427
20.996756	778.427880	14.914445
20.469643	784.512935	14.919463
20.808743	776.882805	14.924480
20.565906	782.475193	14.929498
20.733399	793.945693	14.934515
21.327263	797.172674	14.939533
21.055485	802.917926	14.944551
21.151410	797.818984	14.949568
21.053205	797.853415	14.954586
21.211984	802.593930	14.959603
21.497717	801.002920	14.964621
21.089572	803.897744	14.969639
21.238763	803.227536	14.974656
21.335880	803.654243	14.979674
21.201622	802.248957	14.984691
21.354848	797.570228	14.989709
21.407846	803.280374	14.994727
21.281969	800.078115	14.999744
21.329171	794.292528	15.004762
21.129929	798.852451	15.009779
21.083908	802.059769	15.014797
21.238726	802.534240	15.019815
21.601223	798.785247	15.024832
21.724078	791.779129	15.029850
21.440630	799.697410	15.034867
21.494840	783.742689	15.039885
21.357975	796.318075	15.044903
21.252957	796.082172	15.049920
21.564986	790.431819	15.054938
21.409122	797.389677	15.059955
21.416628	786.756666	15.064973
21.442535	800.471048	15.069991
21.438995	796.965599	15.075008
21.839637	814.632321	15.080026
21.738362	819.738636	15.085043
21.937869	801.176517	15.090061
21.727954	798.217800	15.095079
21.806948	791.489955	15.100096
21.807904	793.317132	15.105114
21.537857	806.077494	15.110131
21.885115	805.868560	15.115149
21.971888	820.141467	15.120167
21.645341	812.918574	15.125184
22.236799	811.128183	15.130202
21.744503	811.498915	15.135219
21.783317	813.935547	15.140237
21.610265	819.349754	15.145255
21.941728	817.164595	15.150272
21.981370	817.732852	15.155290
21.788774	820.972605	15.160307
22.235365	820.075918	15.165325
21.859804	813.173130	15.170343
21.740682	806.081843	15.175360
21.830216	812.695143	15.180378
21.674624	820.176832	15.185395
21.971915	816.210833	15.190413
21.983249	811.393385	15.195431
22.004255	818.017424	15.200448
22.073399	812.818532	15.205466
21.710925	830.626925	15.210483
22.201174	838.408222	15.215501
22.459587	836.941410	15.220519
22.043491	839.272594	15.225536
22.422527	841.359276	15.230554
22.654070	840.183854	15.235571
22.756182	844.305250	15.240589
22.751913	822.161618	15.245607
22.326903	823.077233	15.250624
22.389120	810.564234	15.255642
22.344273	808.002533	15.260659
22.699126	799.233831	15.265677
22.244677	803.013227	15.270695
22.486524	798.973867	15.275712
22.335688	802.074531	15.280730
22.464118	810.430059	15.285747
22.526687	811.322928	15.290765
22.949046	816.561795	15.295783
22.979363	810.766225	15.300800
22.960650	805.536918	15.305818
22.510257	807.403255	15.310835
22.614309	799.090416	15.315853
22.660327	796.956294	15.320871
22.670677	794.960305	15.325888
23.138036	795.505729	15.330906
22.904965	799.518684	15.335923
22.540783	792.304851	15.340941
22.595621	809.303067	15.345959
22.905665	795.226990	15.350976
22.872219	805.138449	15.355994
22.629278	807.297331	15.361011
22.769326	800.755577	15.366029
22.824263	802.590076	15.371047
23.348674	817.097371	15.376064
22.936915	796.639707	15.381082
22.627894	802.681130	15.386099
22.879847	815.845708	15.391117
23.044107	819.247302	15.396135
22.914804	830.590757	15.401152
23.009068	818.767013	15.406170
22.911320	823.872776	15.411187
22.900169	824.900273	15.416205
22.795988	829.830320	15.421223
22.606583	825.189488	15.426240
22.986530	819.468524	15.431258
23.014932	824.557678	15.436275
23.254713	820.805816	15.441293
23.315990	823.428279	15.446311
22.738683	825.983536	15.451328
23.404218	833.402850	15.456346
23.118757	842.990896	15.461363
23.454583	841.493020	15.466381
23.649631	844.037722	15.471399
23.046390	840.944963	15.476416
23.550797	839.875113	15.481434
23.389659	845.404227	15.486451
23.370290	854.527707	15.491469
24.095487	848.459149	15.496487
23.564941	839.800748	15.501504
23.175601	823.464203	15.506522
23.393406	834.586018	15.511539
23.732572	842.870673	15.516557
23.607215	835.846623	15.521575
23.564789	838.277052	15.526592
23.599431	831.098547	15.531610
23.579355	841.639096	15.536627
23.754795	839.784494	15.541645
23.855085	843.275011	15.546663
23.617806	826.624302	15.551680
23.566649	830.267933	15.556698
23.662356	847.629014	15.561715
23.887830	853.249036	15.566733
23.861548	845.625631	15.571751
23.771226	853.624131	15.576768
24.029815	843.898495	15.581786
23.925743	848.610778	15.586803
23.724197	854.351354	15.591821
23.796270	851.632471	15.596839
23.733455	848.019534	15.601856
24.223927	850.874558	15.606874
24.089433	851.220789	15.611891
24.044189	855.652456	15.616909
24.167754	840.813447	15.621927
23.973411	853.315827	15.626944
23.905109	849.343985	15.631962
24.005887	849.934222	15.636979
23.855435	852.050216	15.641997
24.278185	839.408126	15.647015
24.473643	847.336601	15.652032
24.084361	843.493946	15.657050
23.921082	856.512172	15.662067
23.725484	848.861646	15.667085
24.159199	833.743673	15.672103
24.003053	851.096880	15.677120
24.060510	847.035906	15.682138
24.084010	851.239049	15.687155
24.162336	861.884114	15.692173
24.481598	860.805401	15.697191
24.522790	869.392377	15.702208
24.153016	869.721823	15.707226
24.234167	868.301717	15.712243
24.240305	872.807389	15.717261
24.415832	867.787474	15.722279
24.298478	868.702225	15.727296
24.365093	871.554234	15.732314
24.431399	872.673741	15.737331
24.342459	870.210458	15.742349
24.773442	860.132753	15.747367
23.980065	871.921110	15.752384
24.582146	871.776392	15.757402
25.230846	887.435084	15.762419
24.676596	878.499509	15.767437
24.647944	873.265428	15.772455
24.821013	871.237624	15.777472
24.566770	869.699653	15.782490
24.767792	872.912459	15.787507
25.009227	887.662965	15.792525
24.894524	885.200561	15.797543
24.803092	883.229977	15.802560
25.083697	886.348265	15.807578
24.936823	881.520872	15.812595
25.016001	888.110576	15.817613
25.329577	863.341933	15.822631
24.843413	868.536968	15.827648
24.737877	858.429714	15.832666
25.022870	872.226635	15.837683
25.035695	875.970705	15.842701
25.439991	879.716557	15.847719
25.280366	876.873025	15.852736
25.046441	861.420975	15.857754
24.948612	856.639553	15.862771
24.766705	868.212182	15.867789
25.195701	873.014522	15.872807
25.431040	882.640912	15.877824
25.407297	887.043971	15.882842
25.756806	882.132493	15.887859
25.587944	873.815042	15.892877
25.419999	861.953455	15.897895
25.242872	856.698461	15.902912
25.085721	852.112529	15.907930
25.574295	864.116596	15.912947
25.295256	879.456731	15.917965
25.821710	872.788137	15.922983
25.129069	864.827313	15.928000
25.464021	868.716572	15.933018
25.685878	863.402219	15.938035
25.842880	879.614473	15.943053
25.873656	859.216790	15.948071
25.230121	859.731140	15.953088
25.176896	868.149871	15.958106
25.874115	872.723991	15.963123
25.430141	877.988158	15.968141
25.368087	868.574681	15.973159
25.594053	879.628973	15.978176
25.312468	886.590783	15.983194
25.808319	879.766034	15.988211
25.648012	875.720238	15.993229
25.519646	875.352292	15.998247
25.459731	889.455732	16.003264
25.602874	894.258683	16.008282
25.981343	892.148202	16.013299
26.020607	895.825016	16.018317
26.313356	902.879886	16.023335
26.404452	896.112236	16.028352
26.182603	886.010567	16.033370
25.985229	880.837633	16.038387
25.726523	884.374937	16.043405
26.115896	870.504123	16.048423
26.026982	888.512713	16.053440
26.253304	890.519185	16.058458
26.362565	881.627975	16.063475
26.169677	879.244094	16.068493
26.217776	874.016922	16.073511
26.005392	880.690175	16.078528
26.449123	887.030256	16.083546
26.359196	886.965558	16.088563
26.050318	890.785282	16.093581
26.257593	895.821184	16.098599
26.637900	895.383006	16.103616
26.425750	893.036856	16.108634
26.778596	895.351712	16.113651
26.468940	890.035420	16.118669
26.557181	875.078840	16.123687
26.252960	875.356989	16.128704
26.068762	888.302777	16.133722
26.716300	884.060978	16.138739
26.708652	899.462752	16.143757
26.696492	889.678525	16.148775
26.808732	900.274118	16.153792
26.527011	904.297874	16.158810
26.782788	896.996332	16.163827
26.524569	898.059389	16.168845
26.297761	903.220109	16.173863
26.325730	902.335358	16.178880
26.189244	898.323694	16.183898
26.543627	897.564527	16.188915
26.571420	897.030101	16.193933
26.581689	896.908679	16.198951
26.521145	900.295017	16.203968
26.572585	918.960151	16.208986
27.067790	914.931563	16.214003
26.869081	920.551794	16.219021
27.199948	919.789999	16.224039
27.247191	928.035225	16.229056
27.046004	919.154766	16.234074
26.950316	917.999051	16.239091
26.968938	925.759605	16.244109
26.998354	922.406760	16.249127
27.413058	915.607335	16.254144
27.194285	931.850110	16.259162
27.483189	914.100697	16.264179
27.544859	917.436331	16.269197
27.300565	909.462045	16.274215
26.977743	899.262579	16.279232
26.853905	912.713328	16.284250
27.392753	909.700394	16.289267
27.058929	914.874729	16.294285
27.435768	913.891135	16.299303
27.212998	916.106831	16.304320
27.114385	920.587901	16.309338
27.301546	915.395735	16.314355
27.109635	914.476005	16.319373
27.382166	917.283135	16.324391
27.390941	920.791161	16.329408
27.055645	921.213036	16.334426
27.611834	926.494085	16.339443
27.724112	943.855818	16.344461
27.669625	934.914497	16.349479
27.790111	937.997920	16.354496
27.837175	942.538223	16.359514
28.084014	928.102710	16.364531
27.645680	920.578547	16.369549
27.603511	931.258312	16.374567
27.953242	936.814710	16.379584
27.888492	937.067964	16.384602
28.304312	929.110165	16.389619
27.984914	922.747651	16.394637
27.759482	906.981801	16.399655
27.925330	911.490862	16.404672
27.927696	902.158793	16.409690
28.147945	901.562655	16.414707
27.800087	909.573128	16.419725
28.049033	927.910678	16.424743
28.297472	929.304613	16.429760
28.109802	930.375552	16.434778
28.119804	930.787509	16.439795
28.091559	926.875646	16.444813
28.169696	930.205547	16.449831
28.166179	929.006987	16.454848
28.031905	932.540584	16.459866
28.176835	932.063544	16.464883
27.907052	934.229803	16.469901
28.024380	930.159429	16.474919
28.597281	922.120217	16.479936
27.923251	936.140030	16.484954
28.105543	931.068545	16.489971
28.347566	929.257151	16.494989
28.113048	945.559211	16.500007
28.337745	933.714954	16.505024
28.617413	945.130107	16.510042
29.258607	942.047483	16.515059
28.807548	935.595138	16.520077
28.503977	931.571775	16.525095
28.869132	926.809314	16.530112
28.336122	932.671277	16.535130
28.498616	915.882109	16.540147
28.356840	926.082010	16.545165
28.705272	923.976232	16.550183
28.506368	938.536994	16.555200
29.080306	945.528889	16.560218
28.771756	928.586291	16.565235
28.855515	938.845538	16.570253
28.691387	947.780305	16.575271
29.375445	943.210875	16.580288
28.606124	934.217449	16.585306
28.640529	931.362443	16.590323
28.924799	948.113403	16.595341
29.064188	948.457751	16.600359
29.142558	951.109113	16.605376
29.236249	943.428999	16.610394
28.977054	940.664174	16.615411
29.158952	940.228679	16.620429
29.038820	946.265802	16.625447
29.243654	941.866131	16.630464
29.031830	942.069844	16.635482
29.246406	938.495478	16.640499
29.067909	940.675838	16.645517
29.313502	948.618594	16.650535
29.286430	947.063957	16.655552
29.139635	951.265403	16.660570
29.170175	938.823550	16.665587
29.002533	934.261331	16.670605
29.167805	943.346460	16.675623
29.728931	931.282234	16.680640
29.234179	927.333008	16.685658
29.505358	936.272151	16.690675
29.678400	944.784856	16.695693
29.476528	942.828413	16.700711
29.779001	948.190246	16.705728
29.895184	946.840385	16.710746
29.770367	935.095071	16.715763
29.629571	934.994161	16.720781
29.193234	942.071759	16.725799
30.030274	953.961329	16.730816
29.706433	965.243830	16.735834
29.808618	957.467704	16.740851
30.064245	969.075990	16.745869
29.823258	970.089012	16.750887
30.106962	964.670264	16.755904
30.113364	954.965145	16.760922
30.255382	957.322509	16.765939
29.886368	937.722687	16.770957
29.738512	942.119958	16.775975
30.151175	949.250734	16.780992
30.006979	958.087708	16.786010
30.409634	948.030171	16.791027
30.081229	942.997670	16.796045
29.821860	943.786351	16.801063
30.005637	944.300471	16.806080
30.350497	960.675872	16.811098
30.550106	962.238409	16.816115
30.484697	949.694815	16.821133
30.408132	957.968920	16.826151
30.485353	954.580176	16.831168
30.222059	945.043552	16.836186
30.121330	951.828727	16.841203
30.427618	953.838457	16.846221
30.176246	963.433850	16.851239
30.465494	950.563286	16.856256
30.001729	964.386073	16.861274
30.212404	956.858040	16.866291
30.477814	957.668643	16.871309
30.169781	954.867286	16.876327
30.511899	952.781429	16.881344
30.667696	954.092050	16.886362
30.507116	963.625880	16.891379
30.612720	959.702505	16.896397
30.694187	969.201571	16.901415
30.761665	963.917687	16.906432
30.775267	971.028944	16.911450
31.182240	966.663869	16.916467
31.305828	958.202726	16.921485
30.911958	955.171818	16.926503
31.125523	949.562089	16.931520
30.496832	953.921089	16.936538
30.691217	949.469405	16.941555
30.882221	956.268834	16.946573
30.883534	968.926835	16.951591
31.022932	964.764632	16.956608
31.264147	957.736750	16.961626
31.162735	971.231367	16.966643
31.062858	973.317360	16.971661
30.847864	968.311266	16.976679
31.006997	957.177864	16.981696
31.265002	959.116264	16.986714
31.223393	963.970271	16.991731
31.244684	965.538655	16.996749
31.066703	974.166333	17.001767
31.176157	961.901451	17.006784
31.374348	962.454339	17.011802
31.263734	970.190979	17.016819
31.366931	965.523201	17.021837
31.184335	976.325982	17.026855
31.568635	982.886850	17.031872
31.401645	986.637025	17.036890
31.550202	988.318018	17.041907
31.811472	983.300416	17.046925
31.635115	986.970006	17.051943
31.638116	980.430724	17.056960
31.561981	984.851484	17.061978
32.009048	980.480124	17.066995
31.797647	983.467230	17.072013
31.548949	987.709896	17.077031
31.676990	981.674894	17.082048
31.815038	986.200953	17.087066
31.862630	980.708738	17.092083
32.288642	975.472820	17.097101
31.890244	983.204062	17.102119
31.928580	981.897954	17.107136
32.168598	983.892824	17.112154
32.087202	988.999228	17.117171
32.258762	991.071098	17.122189
31.897069	994.024947	17.127207
31.979704	983.443165	17.132224
32.340217	981.777307	17.137242
31.915470	997.093034	17.142259
32.184170	992.396163	17.147277
31.921932	999.771558	17.152295
32.191656	998.372390	17.157312
32.396874	1010.957448	17.162330
32.694593	1008.518773	17.167347
32.837897	998.258842	17.172365
32.732170	986.598866	17.177383
32.148755	982.499414	17.182400
32.209544	979.261565	17.187418
32.451480	980.842718	17.192435
32.791959	991.235345	17.197453
32.350038	989.796196	17.202471
32.819830	991.508911	17.207488
32.936875	982.023130	17.212506
32.607020	986.297447	17.217523
32.675057	976.475360	17.222541
32.517908	985.557378	17.227559
32.393141	993.592896	17.232576
32.822316	998.070189	17.237594
32.849319	1001.897272	17.242611
32.875317	1003.244012	17.247629
32.894031	1003.124422	17.252647
32.991288	1009.910158	17.257664
33.311279	1002.484901	17.262682
32.997509	1008.369344	17.267699
32.918718	1003.559653	17.272717
33.204750	1006.964295	17.277735
33.037211	996.415390	17.282752
33.045639	1002.328246	17.287770
32.890534	1003.046944	17.292787
33.046647	999.453323	17.297805
33.061982	1001.814763	17.302823
33.055574	995.491548	17.307840
33.506888	1004.658126	17.312858
33.469706	1004.291670	17.317875
33.528673	993.369602	17.322893
33.232369	1007.295575	17.327911
33.135738	992.412044	17.332928
33.311760	989.411762	17.337946
33.462632	998.224617	17.342963
33.473402	995.392239	17.347981
33.066405	997.223392	17.352999
33.493472	1002.499447	17.358016
33.740857	1015.207291	17.363034
33.654798	1025.789846	17.368051
33.778423	1017.685281	17.373069
33.849164	1028.969117	17.378087
33.759571	1015.189015	17.383104
33.858741	1017.934959	17.388122
33.452816	1022.754543	17.393139
33.788275	1010.050268	17.398157
33.452416	1015.638367	17.403175
33.624535	1015.100260	17.408192
34.133033	1011.886935	17.413210
33.766111	1020.588420	17.418227
34.164832	1012.428133	17.423245
33.873801	1008.538489	17.428263
34.131618	1011.073381	17.433280
34.311588	1011.938399	17.438298
34.041415	1014.868445	17.443315
34.118394	1014.316842	17.448333
33.890294	1019.266356	17.453351
34.159752	1011.561830	17.458368
33.961620	1018.794643	17.463386
33.940630	1027.738582	17.468403
34.493005	1034.273137	17.473421
34.412872	1033.642005	17.478439
34.488622	1031.702016	17.483456
34.750329	1035.867881	17.488474
34.609970	1046.645151	17.493491
34.702399	1037.431446	17.498509
34.869457	1039.106389	17.503527
34.837595	1029.596576	17.508544
34.991968	1015.588897	17.513562
34.536119	1015.054503	17.518579
34.544504	1011.004336	17.523597
34.568899	1014.276400	17.528615
34.607596	1020.159272	17.533632
34.468196	1032.227129	17.538650
34.619765	1035.371972	17.543667
34.990955	1033.316265	17.548685
34.692251	1030.229407	17.553703
34.707357	1036.043396	17.558720
35.039130	1030.074289	17.563738
34.516652	1039.642769	17.568755
34.629722	1026.777663	17.573773
34.658537	1034.038042	17.578791
34.658642	1036.925745	17.583808
35.144896	1045.708167	17.588826
35.014618	1050.863274	17.593843
35.025835	1057.612014	17.598861
35.214644	1053.202204	17.603879
35.146465	1068.004526	17.608896
35.277102	1051.437976	17.613914
35.251136	1054.083610	17.618931
35.371013	1062.885573	17.623949
35.657355	1056.910952	17.628967
35.662114	1057.118602	17.633984
35.818725	1049.753638	17.639002
35.406086	1058.370784	17.644019
35.848559	1059.144183	17.649037
35.283851	1055.455201	17.654055
35.637344	1058.006668	17.659072
35.493150	1054.857726	17.664090
35.235215	1059.392196	17.669107
35.829215	1051.958702	17.674125
35.797071	1045.579540	17.679143
35.404014	1057.153815	17.684160
35.351604	1043.412047	17.689178
35.544917	1056.292497	17.694195
35.776915	1067.494287	17.699213
35.701396	1078.589627	17.704231
36.212612	1086.844285	17.709248
36.067755	1079.674868	17.714266
36.203795	1076.037040	17.719283
36.215191	1071.522475	17.724301
36.424414	1078.457955	17.729319
36.249156	1082.913204	17.734336
35.888170	1053.863331	17.739354
36.166092	1074.137348	17.744371
36.298045	1074.183055	17.749389
36.837652	1070.772338	17.754407
36.518501	1064.744255	17.759424
36.396781	1050.214907	17.764442
36.075074	1050.795605	17.769459
36.318678	1056.747373	17.774477
36.765784	1067.072844	17.779495
36.620240	1060.850302	17.784512
36.309059	1046.792462	17.789530
35.990771	1061.488795	17.794547
36.551178	1069.290762	17.799565
36.587924	1066.460614	17.804583
36.462181	1067.461898	17.809600
36.529567	1065.573709	17.814618
36.625611	1062.387127	17.819635
36.813478	1057.939592	17.824653
36.953282	1055.541433	17.829671
36.635805	1063.054899	17.834688
36.737654	1059.804290	17.839706
36.818027	1059.097516	17.844723
36.746933	1052.361530	17.849741
36.867052	1061.535847	17.854759
36.860929	1080.942330	17.859776
36.985178	1077.366310	17.864794
36.721252	1085.540439	17.869811
36.932604	1083.086883	17.874829
37.118403	1085.983371	17.879847
36.695722	1087.523494	17.884864
37.306098	1077.067259	17.889882
37.329819	1081.686996	17.894899
37.298301	1087.953284	17.899917
37.036153	1080.382513	17.904935
37.267915	1083.293890	17.909952
37.603116	1081.382674	17.914970
37.368554	1084.922546	17.919987
37.199615	1086.359797	17.925005
37.528217	1095.722378	17.930023
37.481301	1106.485043	17.935040
37.966367	1102.262339	17.940058
37.619017	1092.757739	17.945075
37.359077	1089.538563	17.950093
37.924407	1090.920732	17.955111
38.094822	1103.419788	17.960128
37.738257	1099.944343	17.965146
37.723137	1099.498687	17.970163
38.123676	1088.788137	17.975181
37.973727	1090.519064	17.980199
37.829714	1092.135450	17.985216
38.272184	1095.278909	17.990234
38.167992	1087.172136	17.995251
38.032078	1081.784382	18.000269
38.184021	1068.152591	18.005287
38.162368	1076.282446	18.010304
38.027863	1067.009605	18.015322
38.154841	1087.698614	18.020339
38.129161	1095.971123	18.025357
38.171488	1103.791158	18.030375
38.252589	1112.747548	18.035392
38.292749	1106.511673	18.040410
38.189054	1102.756762	18.045427
38.240391	1103.247455	18.050445
38.708840	1096.982351	18.055463
38.521676	1106.858100	18.060480
38.848303	1102.855884	18.065498
38.597167	1103.832633	18.070515
38.488395	1107.665232	18.075533
38.735004	1102.908676	18.080551
38.190002	1112.603803	18.085568
39.091128	1098.176097	18.090586
38.995381	1100.974684	18.095603
38.991857	1104.490985	18.100621
38.954652	1099.466465	18.105639
38.860499	1097.152293	18.110656
38.665723	1095.096889	18.115674
38.743159	1096.631242	18.120691
38.423626	1100.553666	18.125709
38.947008	1101.595263	18.130727
38.585896	1106.354197	18.135744
38.796585	1127.254203	18.140762
39.032235	1129.448595	18.145779
38.780158	1123.968573	18.150797
38.777314	1127.623630	18.155815
39.047203	1126.126595	18.160832
39.166044	1123.321447	18.165850
39.112211	1127.817644	18.170867
39.859221	1140.459921	18.175885
39.608705	1125.013396	18.180903
39.380280	1125.895068	18.185920
39.221042	1123.108242	18.190938
39.695939	1126.189820	18.195955
39.642707	1135.258788	18.200973
39.976619	1130.586377	18.205991
39.591621	1127.737089	18.211008
39.372621	1125.164758	18.216026
39.701419	1120.243837	18.221043
39.793855	1141.168699	18.226061
40.085714	1137.430704	18.231079
40.276880	1132.591305	18.236096
39.787008	1117.759813	18.241114
39.928552	1103.545788	18.246131
39.847612	1112.650645	18.251149
39.905772	1109.971773	18.256167
39.970827	1122.796625	18.261184
39.964300	1129.541861	18.266202
40.257132	1135.189291	18.271219
40.105986	1133.108111	18.276237
40.459063	1128.596804	18.281255
40.506661	1131.006856	18.286272
40.037900	1123.130759	18.291290
40.613168	1122.185495	18.296307
40.340704	1114.284958	18.301325
40.420388	1114.742808	18.306343
40.325411	1120.918062	18.311360
40.641777	1127.394952	18.316378
40.510337	1117.118037	18.321395
40.464943	1126.119499	18.326413
40.473219	1120.361996	18.331431
40.839628	1129.172705	18.336448
40.646310	1135.316034	18.341466
40.761199	1126.089297	18.346483
40.629681	1135.214713	18.351501
40.769557	1125.406536	18.356519
40.720869	1127.951596	18.361536
40.562828	1125.120399	18.366554
40.503877	1126.382627	18.371571
40.819439	1127.838647	18.376589
40.813870	1135.233845	18.381607
40.683105	1126.815630	18.386624
40.835430	1132.519787	18.391642
40.833710	1140.555027	18.396659
40.715416	1142.902708	18.401677
40.732634	1144.064638	18.406695
41.075410	1158.234590	18.411712
41.276782	1146.456964	18.416730
41.455180	1147.697785	18.421747
40.932041	1153.637170	18.426765
41.305883	1140.740592	18.431783
41.626879	1145.443160	18.436800
41.405151	1143.404596	18.441818
41.474777	1151.365546	18.446835
41.373289	1164.787736	18.451853
41.726469	1170.337357	18.456871
41.752329	1173.460894	18.461888
41.614096	1176.127291	18.466906
42.116301	1174.211991	18.471923
41.415567	1161.793036	18.476941
41.788466	1168.958534	18.481959
41.729597	1170.482689	18.486976
41.774062	1162.696582	18.491994
41.850560	1166.534881	18.497011
42.053241	1154.065907	18.502029
41.979307	1159.205905	18.507047
42.276788	1160.052520	18.512064
41.863143	1161.673287	18.517082
41.947130	1164.645700	18.522099
42.051304	1171.291555	18.527117
42.230214	1172.794236	18.532135
42.160374	1169.747237	18.537152
41.934985	1168.400382	18.542170
41.530179	1173.298727	18.547187
42.343841	1182.872541	18.552205
42.496314	1190.852087	18.557223
42.512963	1196.574366	18.562240
42.582362	1190.662093	18.567258
42.664159	1183.050014	18.572275
42.338664	1193.963679	18.577293
42.314049	1196.899464	18.582311
42.599712	1198.076144	18.587328
42.385816	1191.062670	18.592346
42.803589	1190.164169	18.597363
42.513159	1193.384603	18.602381
42.901230	1189.240193	18.607399
42.824235	1182.113752	18.612416
42.630390	1195.294809	18.617434
42.489786	1198.640097	18.622451
42.635759	1214.273701	18.627469
43.161862	1205.405384	18.632487
43.066805	1212.593723	18.637504
43.035684	1218.064711	18.642522
43.291341	1214.038874	18.647539
43.077254	1218.951532	18.652557
43.325440	1209.770141	18.657575
43.563366	1206.567615	18.662592
43.246501	1221.175492	18.667610
43.538591	1200.733320	18.672627
43.409460	1204.225138	18.677645
43.611896	1208.927364	18.682663
43.637574	1205.571895	18.687680
43.560219	1219.905553	18.692698
43.744197	1204.646511	18.697715
43.841117	1195.867533	18.702733
43.740342	1203.372353	18.707751
43.914764	1200.810956	18.712768
43.680779	1210.877140	18.717786
43.846509	1208.380221	18.722803
43.640024	1203.006643	18.727821
43.916704	1203.550398	18.732839
43.517892	1210.350814	18.737856
43.870275	1207.881457	18.742874
43.614430	1202.013827	18.747891
43.661551	1198.109031	18.752909
43.737554	1210.209533	18.757927
44.333645	1221.095592	18.762944
44.277914	1234.731578	18.767962
44.437662	1229.660384	18.772979
44.440841	1234.526383	18.777997
44.278213	1227.605850	18.783015
44.666387	1233.740160	18.788032
44.264115	1235.911432	18.793050
44.380904	1239.355260	18.798067
44.428567	1229.662462	18.803085
44.645384	1224.206776	18.808103
44.442917	1232.175678	18.813120
44.745347	1232.967871	18.818138
44.649773	1227.075121	18.823155
44.581882	1224.617959	18.828173
44.606049	1238.825270	18.833191
44.777459	1230.530080	18.838208
44.860285	1233.048239	18.843226
44.516787	1232.707679	18.848243
44.551606	1233.308264	18.853261
44.963067	1236.702766	18.858279
44.873982	1240.712195	18.863296
45.030051	1249.628505	18.868314
45.246215	1246.334705	18.873331
45.304222	1250.381052	18.878349
45.186067	1249.023702	18.883367
45.305038	1241.260602	18.888384
45.021638	1254.361057	18.893402
45.419105	1248.542535	18.898419
45.689765	1251.722409	18.903437
45.181810	1249.507765	18.908455
45.299503	1235.748665	18.913472
45.053316	1245.627426	18.918490
45.190466	1240.850112	18.923507
45.550917	1251.542729	18.928525
45.639442	1254.637527	18.933543
45.678124	1241.099091	18.938560
45.360900	1252.566934	18.943578
45.671179	1257.763531	18.948595
45.746533	1258.976323	18.953613
45.539975	1267.640178	18.958631
46.205738	1265.352095	18.963648
45.935260	1265.009561	18.968666
45.969526	1264.578255	18.973683
46.097956	1263.128619	18.978701
45.630093	1265.830895	18.983719
46.020540	1264.857775	18.988736
45.657654	1263.945879	18.993754
45.903805	1259.268250	18.998771
45.946262	1267.258755	19.003789
46.452182	1270.335498	19.008807
46.534928	1279.001371	19.013824
46.187590	1288.047066	19.018842
46.665036	1281.572199	19.023859
46.872032	1282.934786	19.028877
46.607505	1284.585850	19.033895
46.518181	1270.041779	19.038912
46.492900	1280.722263	19.043930
46.912307	1283.629521	19.048947
46.678685	1282.059878	19.053965
46.630262	1278.084825	19.058983
47.000241	1279.563891	19.064000
47.009449	1283.277054	19.069018
46.838904	1281.280950	19.074035
46.827820	1288.159508	19.079053
47.151819	1286.019645	19.084071
47.092608	1273.897743	19.089088
46.950981	1278.215223	19.094106
46.752200	1276.027877	19.099123
46.798124	1277.298931	19.104141
46.987344	1278.503351	19.109159
47.210997	1275.845864	19.114176
47.108678	1295.201378	19.119194
47.336141	1293.477440	19.124211
47.336157	1297.826383	19.129229
47.142211	1299.867190	19.134247
47.627420	1303.745629	19.139264
47.266131	1303.909643	19.144282
47.530310	1297.607045	19.149299
47.262668	1302.919449	19.154317
47.645245	1291.608815	19.159335
47.733390	1293.539150	19.164352
47.662023	1301.667429	19.169370
47.894647	1307.371685	19.174387
47.594492	1310.783018	19.179405
47.806900	1319.924073	19.184423
48.344188	1316.084470	19.189440
47.936540	1322.577034	19.194458
48.297802	1313.270573	19.199475
48.571940	1318.056271	19.204493
48.236006	1324.171514	19.209511
48.424803	1315.961926	19.214528
48.419165	1315.155006	19.219546
48.309774	1309.308577	19.224563
48.603456	1307.937192	19.229581
48.698119	1305.173674	19.234599
48.650392	1302.798551	19.239616
48.446423	1291.311563	19.244634
48.400434	1277.764274	19.249651
48.344644	1287.881480	19.254669
48.721495	1299.571978	19.259687
48.989062	1290.557927	19.264704
48.486933	1304.472196	19.269722
48.713928	1308.605693	19.274739
48.710319	1305.235859	19.279757
48.552962	1305.301649	19.284775
48.787381	1306.347505	19.289792
48.695391	1309.533713	19.294810
48.636115	1296.685947	19.299827
48.612299	1298.021579	19.304845
48.835538	1311.377223	19.309863
49.124919	1320.960670	19.314880
49.254270	1331.146726	19.319898
49.090677	1332.349621	19.324915
49.341551	1329.779383	19.329933
49.313395	1332.526390	19.334951
49.192974	1331.847909	19.339968
48.887449	1320.335787	19.344986
49.217374	1321.104741	19.350003
49.498871	1330.632622	19.355021
49.303104	1340.588745	19.360039
49.677246	1345.084218	19.365056
49.893429	1342.405800	19.370074
49.742750	1346.005167	19.375091
50.196889	1344.892671	19.380109
49.766343	1355.478900	19.385127
49.870725	1348.674281	19.390144
49.856254	1357.835123	19.395162
50.028818	1342.322122	19.400179
50.100347	1343.702782	19.405197
49.911315	1350.877497	19.410215
50.188075	1342.941303	19.415232
50.626115	1338.107353	19.420250
49.976867	1335.129013	19.425267
50.498433	1339.008075	19.430285
50.488836	1347.401260	19.435303
50.160025	1338.837243	19.440320
50.295965	1345.680164	19.445338
50.565909	1345.603264	19.450355
50.436418	1341.678769	19.455373
50.263901	1346.187304	19.460391
50.285240	1360.707591	19.465408
50.748674	1368.379711	19.470426
50.623569	1370.864193	19.475443
50.650751	1362.578915	19.480461
50.642531	1375.917221	19.485479
50.827880	1369.260861	19.490496
50.979573	1373.895339	19.495514
50.775983	1365.709335	19.500531
50.938680	1368.006708	19.505549
50.626037	1371.580961	19.510567
50.944704	1374.557668	19.515584
51.190977	1393.811334	19.520602
50.888815	1393.742015	19.525619
51.390204	1388.159640	19.530637
51.049617	1395.872533	19.535655
51.196977	1392.065603	19.540672
51.158634	1391.664606	19.545690
51.372420	1390.573986	19.550707
51.507039	1388.728880	19.555725
51.591903	1398.082470	19.560743
51.542835	1409.508399	19.565760
51.454044	1408.859675	19.570778
51.654954	1413.208730	19.575795
51.837500	1405.318829	19.580813
51.627533	1413.948575	19.585831
51.746694	1410.729905	19.590848
52.323222	1410.971058	19.595866
52.631037	1410.853510	19.600883
52.404660	1414.237523	19.605901
52.510685	1414.413532	19.610919
52.181364	1403.653038	19.615936
52.158169	1401.393983	19.620954
52.274504	1397.200579	19.625971
52.639109	1399.400048	19.630989
52.070323	1406.549073	19.636007
52.182257	1403.460930	19.641024
52.456858	1402.840482	19.646042
51.996924	1407.614978	19.651059
52.255915	1400.580981	19.656077
52.316956	1410.963985	19.661095
52.436891	1395.935729	19.666112
52.698978	1400.672842	19.671130
52.944210	1421.372114	19.676147
52.866504	1420.365033	19.681165
53.028966	1422.280583	19.686183
53.269178	1422.871086	19.691200
53.135793	1407.058813	19.696218
52.787362	1393.460987	19.701235
53.084562	1408.159006	19.706253
53.041445	1418.586737	19.711271
53.196632	1413.670846	19.716288
53.225638	1409.222868	19.721306
53.231603	1428.189161	19.726323
53.470761	1425.327244	19.731341
53.204244	1428.802759	19.736359
53.186232	1426.867950	19.741376
53.361519	1417.890386	19.746394
53.293051	1418.933210	19.751411
53.486608	1410.836446	19.756429
53.395717	1419.946174	19.761447
53.573098	1432.867264	19.766464
53.866850	1439.496140	19.771482
53.583579	1447.395743	19.776499
53.828812	1448.209531	19.781517
54.227349	1440.926428	19.786535
53.989656	1435.933225	19.791552
54.047875	1435.712765	19.796570
53.909574	1439.995048	19.801587
53.967232	1434.908231	19.806605
53.800506	1441.940627	19.811623
53.842189	1440.791758	19.816640
54.726718	1450.720704	19.821658
54.471956	1455.273711	19.826675
54.506682	1451.572782	19.831693
54.479141	1456.509929	19.836711
54.887076	1449.035994	19.841728
54.604314	1449.929351	19.846746
54.437549	1449.128733	19.851763
54.809246	1445.917830	19.856781
54.954899	1447.028098	19.861799
54.818366	1454.617524	19.866816
54.969018	1448.509392	19.871834
54.886048	1454.818585	19.876851
54.833002	1450.036299	19.881869
55.045749	1455.522802	19.886887
54.904752	1455.788008	19.891904
55.374474	1449.194366	19.896922
54.900479	1457.701391	19.901939
54.991191	1447.020235	19.906957
55.183345	1456.701042	19.911975
55.153140	1456.273520	19.916992
55.327700	1450.461455	19.922010
55.233913	1453.815234	19.927027
55.439417	1457.109499	19.932045
55.840810	1466.789089	19.937063
55.687856	1467.229745	19.942080
55.521705	1457.286289	19.947098
55.583382	1474.741679	19.952115
55.979653	1468.790725	19.957133
55.920936	1474.278738	19.962151
55.771729	1474.283288	19.967168
56.102695	1465.297089	19.972186
55.716788	1481.093158	19.977203
56.132474	1481.217495	19.982221
56.341583	1476.876987	19.987239
56.242847	1467.033421	19.992256
56.253763	1463.481393	19.997274
55.858800	1463.817949	20.002291
56.157967	1467.962267	20.007309
56.089041	1468.209870	20.012327
56.122493	1471.976081	20.017344
56.600285	1463.575974	20.022362
56.517749	1460.035432	20.027379
56.361799	1470.745970	20.032397
56.803198	1486.377710	20.037415
56.490702	1490.280180	20.042432
56.761757	1488.852364	20.047450
56.401390	1494.409736	20.052467
56.738509	1491.507213	20.057485
56.714004	1491.653178	20.062503
56.682519	1492.074804	20.067520
57.035114	1497.782417	20.072538
56.831104	1496.410095	20.077555
56.704069	1498.257397	20.082573
56.962151	1508.877841	20.087591
56.828748	1523.460376	20.092608
57.401523	1516.695922	20.097626
56.935465	1522.575988	20.102643
57.282432	1517.301804	20.107661
57.219688	1517.371706	20.112679
57.133667	1530.422501	20.117696
57.157225	1532.593366	20.122714
57.295730	1538.167269	20.127731
57.672873	1530.492989	20.132749
57.842986	1539.568197	20.137767
57.885174	1528.001462	20.142784
57.871997	1527.303015	20.147802
57.789276	1528.193437	20.152819
58.299372	1537.521504	20.157837
58.310031	1555.013369	20.162855
58.116015	1553.109277	20.167872
58.430206	1543.251469	20.172890
58.421583	1546.702381	20.177907
58.238709	1547.106700	20.182925
58.141013	1540.740787	20.187943
57.999878	1550.470707	20.192960
58.437360	1540.587272	20.197978
58.600711	1556.559296	20.202995
58.556756	1543.428072	20.208013
58.754461	1537.950039	20.213031
58.310581	1545.013274	20.218048
58.437282	1540.196490	20.223066
58.792439	1542.283843	20.228083
58.734550	1555.737367	20.233101
59.013894	1564.681860	20.238119
58.920385	1568.972935	20.243136
59.220201	1567.553231	20.248154
59.263904	1568.780470	20.253171
59.522267	1564.946644	20.258189
59.488116	1551.024891	20.263207
59.193184	1559.778476	20.268224
59.404645	1555.443893	20.273242
59.395793	1557.641930	20.278259
59.487132	1561.323348	20.283277
59.461879	1550.562464	20.288295
59.641860	1554.018544	20.293312
59.706916	1552.742924	20.298330
59.741680	1560.728454	20.303347
59.721262	1555.265654	20.308365
59.792719	1549.100464	20.313383
59.666249	1568.419030	20.318400
59.992362	1547.980600	20.323418
60.021119	1551.943232	20.328435
59.927642	1544.835008	20.333453
59.903404	1552.144938	20.338471
59.798089	1556.523070	20.343488
60.417614	1551.862610	20.348506
60.108101	1551.071729	20.353523
60.158840	1560.039413	20.358541
60.793624	1566.135201	20.363559
60.231894	1586.708619	20.368576
60.443619	1576.289307	20.373594
60.743250	1573.105452	20.378611
60.567266	1575.335989	20.383629
61.063721	1577.745208	20.388647
60.908477	1581.263282	20.393664
61.279585	1574.123285	20.398682
60.700807	1576.401150	20.403699
60.723681	1578.442733	20.408717
61.113251	1574.796642	20.413735
61.103401	1569.366898	20.418752
61.038141	1572.328047	20.423770
60.752780	1573.054551	20.428787
61.036969	1570.819903	20.433805
61.064585	1568.937892	20.438823
61.201023	1579.934061	20.443840
61.352758	1585.783630	20.448858
61.317929	1590.324305	20.453875
61.465905	1584.017720	20.458893
61.581654	1593.625362	20.463911
61.206560	1601.031309	20.468928
61.375377	1604.151460	20.473946
61.217651	1595.525798	20.478963
60.878586	1611.065321	20.483981
61.520091	1621.045063	20.488999
61.695827	1626.152390	20.494016
61.953902	1624.609827	20.499034
62.421473	1639.461234	20.504051
62.749791	1633.653423	20.509069
62.730744	1615.184665	20.514087
62.445900	1609.311975	20.519104
62.205758	1607.058481	20.524122
62.702024	1610.067366	20.529139
62.326892	1610.063129	20.534157
62.297613	1601.363688	20.539175
62.538640	1614.675746	20.544192
62.948029	1619.724371	20.549210
62.761863	1630.124142	20.554227
62.870619	1638.962849	20.559245
63.243329	1640.817079	20.564263
62.884395	1616.966998	20.569280
62.831269	1613.409193	20.574298
63.281713	1625.309293	20.579315
63.240076	1631.703596	20.584333
63.597101	1620.021200	20.589351
63.282731	1627.436579	20.594368
63.104081	1623.873192	20.599386
63.654591	1634.088115	20.604403
63.473511	1636.881220	20.609421
63.439343	1624.275450	20.614439
63.427659	1626.792692	20.619456
63.455245	1626.040515	20.624474
63.600125	1636.407359	20.629491
63.584560	1626.585389	20.634509
63.573876	1626.031722	20.639527
63.080671	1628.438205	20.644544
63.436272	1624.734306	20.649562
63.711893	1630.233104	20.654579
63.831787	1650.797638	20.659597
64.403301	1651.516133	20.664615
63.896404	1654.357131	20.669632
64.414341	1650.602546	20.674650
64.503056	1645.848492	20.679667
64.320178	1652.451133	20.684685
64.454921	1646.739922	20.689703
64.171352	1655.419186	20.694720
64.139630	1648.399081	20.699738
64.394697	1650.956588	20.704755
64.259504	1662.266778	20.709773
64.345932	1661.019362	20.714791
64.411999	1672.266466	20.719808
64.679669	1674.635800	20.724826
64.453457	1679.159143	20.729843
64.816518	1679.361159	20.734861
64.765896	1676.352089	20.739879
64.819382	1684.533567	20.744896
65.224605	1700.278467	20.749914
65.453543	1696.928932	20.754931
65.391838	1694.915728	20.759949
65.824601	1692.364281	20.764967
65.964933	1690.874875	20.769984
65.892644	1685.009886	20.775002
65.905371	1678.692899	20.780019
65.679685	1665.908810	20.785037
65.597939	1659.710778	20.790055
65.871321	1668.839304	20.795072
65.827040	1677.099216	20.800090
66.181463	1667.635845	20.805107
65.736199	1679.572168	20.810125
66.017320	1685.625573	20.815143
65.854502	1680.759432	20.820160
65.827474	1680.388215	20.825178
66.542944	1666.503568	20.830195
66.076446	1684.338575	20.835213
66.201808	1674.295673	20.840231
66.114772	1674.830154	20.845248
66.146373	1690.213837	20.850266
66.745218	1689.959168	20.855283
66.583142	1705.420548	20.860301
66.603027	1709.378293	20.865319
66.818991	1718.509528	20.870336
66.626735	1703.230108	20.875354
66.879544	1700.258705	20.880371
66.537206	1702.865635	20.885389
67.333449	1704.934397	20.890407
67.075654	1703.116025	20.895424
66.820568	1699.302652	20.900442
67.158734	1700.117672	20.905459
67.252512	1704.915953	20.910477
67.234439	1724.485962	20.915495
67.576097	1726.016844	20.920512
67.334369	1729.273926	20.925530
67.767180	1726.848707	20.930547
67.706466	1722.209568	20.935565
67.527091	1724.579518	20.940583
67.792288	1716.294658	20.945600
67.679912	1721.099994	20.950618
67.766301	1720.789906	20.955635
67.480111	1721.014744	20.960653
67.609890	1716.468845	20.965671
67.532146	1726.857996	20.970688
67.969808	1741.035639	20.975706
68.227383	1733.667200	20.980723
67.732151	1746.946377	20.985741
68.422341	1744.714374	20.990759
68.123787	1731.600809	20.995776
68.248281	1731.423614	21.000794
68.212248	1736.232773	21.005811
68.272932	1748.197176	21.010829
68.679376	1754.243594	21.015847
68.828892	1763.899688	21.020864
68.510666	1759.550209	21.025882
69.003975	1770.004560	21.030899
68.582404	1768.757826	21.035917
68.614278	1759.859368	21.040935
68.833082	1759.250806	21.045952
68.886568	1778.768636	21.050970
69.170250	1790.616074	21.055987
69.464127	1800.678786	21.061005
69.217617	1792.322574	21.066023
69.614718	1791.610333	21.071040
69.408534	1791.352394	21.076058
69.392876	1792.191294	21.081075
69.820166	1791.408047	21.086093
69.723427	1780.336315	21.091111
69.932365	1791.548486	21.096128
69.968627	1790.129029	21.101146
70.047376	1776.656498	21.106163
69.950832	1783.797959	21.111181
70.123277	1786.308467	21.116199
69.989693	1774.504008	21.121216
69.570268	1780.509403	21.126234
70.593714	1796.103876	21.131251
70.393307	1801.181817	21.136269
70.293102	1803.457318	21.141287
70.536961	1803.425532	21.146304
70.309363	1810.492857	21.151322
70.615393	1796.037904	21.156339
70.674360	1802.457533	21.161357
70.502533	1806.618916	21.166375
69.883477	1802.146134	21.171392
70.489478	1808.773567	21.176410
70.935122	1814.911700	21.181427
70.816309	1826.386694	21.186445
71.000834	1817.783047	21.191463
71.517025	1821.192815	21.196480
71.060581	1829.375352	21.201498
71.325966	1817.088610	21.206515
71.065361	1829.860845	21.211533
71.390041	1830.075189	21.216551
71.722999	1833.624127	21.221568
71.797236	1842.436783	21.226586
71.753455	1845.631313	21.231603
71.635239	1843.507017	21.236621
71.926190	1845.528723	21.241639
71.823137	1838.314578	21.246656
71.786155	1837.320029	21.251674
72.074874	1846.799715	21.256691
72.040413	1835.203763	21.261709
71.867113	1838.033551	21.266727
72.390430	1848.581083	21.271744
72.279076	1849.412887	21.276762
72.548108	1840.742336	21.281779
72.353525	1841.012787	21.286797
72.625371	1842.324229	21.291815
72.556202	1838.339678	21.296832
72.189159	1849.490638	21.301850
72.715389	1855.070170	21.306867
72.798200	1868.549225	21.311885
72.616792	1882.461032	21.316903
72.913837	1875.291492	21.321920
72.972086	1873.309970	21.326938
73.037691	1865.169928	21.331955
73.075599	1869.225877	21.336973
72.725109	1873.787676	21.341991
73.142497	1865.876559	21.347008
73.011784	1884.681702	21.352026
73.191825	1883.552156	21.357043
73.392618	1889.037510	21.362061
73.380244	1890.365081	21.367079
73.813294	1892.408714	21.372096
73.595120	1888.318099	21.377114
73.985223	1891.141682	21.382131
73.960065	1879.544244	21.387149
74.142797	1885.010334	21.392167
74.257974	1872.680811	21.397184
74.074856	1882.736245	21.402202
74.334847	1881.887683	21.407219
74.350169	1884.280801	21.412237
74.120075	1888.634380	21.417255
74.620350	1888.391997	21.422272
74.265812	1902.753849	21.427290
74.510095	1903.596212	21.432307
74.636143	1905.451244	21.437325
74.622245	1915.388660	21.442343
74.702152	1896.395990	21.447360
74.937222	1901.336299	21.452378
74.813799	1899.143381	21.457395
74.902960	1897.144390	21.462413
74.725155	1900.208438	21.467431
74.999270	1899.556491	21.472448
74.917428	1915.355798	21.477466
75.330771	1919.608575	21.482483
75.278612	1916.246232	21.487501
75.241579	1915.352679	21.492519
75.790041	1920.540559	21.497536
74.997673	1930.536828	21.502554
75.438356	1937.423757	21.507571
75.942451	1936.606379	21.512589
75.762868	1948.999906	21.517607
76.315876	1939.751450	21.522624
75.994405	1943.791132	21.527642
76.129681	1942.589695	21.532659
75.876894	1946.344044	21.537677
76.002409	1945.204101	21.542695
76.080750	1934.906471	21.547712
76.197386	1939.120526	21.552730
76.740939	1936.166654	21.557747
76.881261	1938.562288	21.562765
76.680519	1939.594306	21.567783
76.556879	1937.404572	21.572800
76.214327	1943.401133	21.577818
76.791445	1949.663891	21.582835
76.785649	1956.014822	21.587853
76.652442	1960.129161	21.592871
76.925781	1958.252796	21.597888
76.961286	1960.273508	21.602906
77.094271	1961.518346	21.607923
77.546601	1965.862863	21.612941
77.138409	1957.711798	21.617959
77.503261	1958.655203	21.622976
77.135025	1965.971856	21.627994
77.497891	1970.459788	21.633011
77.803470	1980.025272	21.638029
77.410536	1988.406229	21.643047
77.953694	1972.989266	21.648064
77.863332	1980.590616	21.653082
77.793289	1987.118893	21.658099
78.112812	1977.995366	21.663117
78.002971	1974.938716	21.668135
78.287546	1971.981229	21.673152
78.000512	1978.142684	21.678170
77.800605	1975.147484	21.683187
78.352897	1985.949353	21.688205
78.103575	1990.252316	21.693223
78.267670	2000.922496	21.698240
78.337055	2001.479819	21.703258
78.405456	2001.866871	21.708275
78.680991	2005.869841	21.713293
78.462965	2005.108789	21.718311
79.053001	2015.062102	21.723328
78.965198	2026.955274	21.728346
78.823411	2030.903704	21.733363
79.201291	2022.907184	21.738381
78.729788	2027.595285	21.743399
79.096354	2017.845785	21.748416
79.277812	2030.574152	21.753434
79.581552	2038.050661	21.758451
79.787913	2043.105969	21.763469
79.840926	2046.894484	21.768487
79.909788	2037.807043	21.773504
79.947936	2045.022186	21.778522
80.108241	2041.459262	21.783539
80.238150	2039.236105	21.788557
79.900384	2042.703963	21.793575
79.920568	2039.011503	21.798592
80.234313	2037.172985	21.803610
80.469283	2053.232069	21.808627
80.792984	2036.189360	21.813645
80.420043	2028.951145	21.818663
80.378901	2030.712455	21.823680
80.383813	2041.738982	21.828698
80.292012	2041.308472	21.833715
80.684233	2054.038551	21.838733
80.735898	2065.442805	21.843751
81.126332	2057.794623	21.848768
81.018364	2061.254887	21.853786
80.862065	2055.516555	21.858803
81.087032	2061.642007	21.863821
80.825964	2065.265123	21.868839
81.148818	2064.031135	21.873856
81.355177	2072.302457	21.878874
81.398610	2083.061023	21.883891
81.665953	2081.428600	21.888909
81.300239	2100.154013	21.893927
81.679926	2093.044029	21.898944
81.962253	2092.239297	21.903962
81.655030	2085.514667	21.908979
81.714454	2089.529423	21.913997
81.943151	2105.949327	21.919015
82.178592	2113.158836	21.924032
82.177467	2112.092376	21.929050
82.560594	2112.218666	21.934067
82.563131	2102.759701	21.939085
82.453989	2107.924423	21.944103
82.543374	2102.488438	21.949120
82.663878	2110.953124	21.954138
82.743092	2108.750524	21.959155
83.068290	2098.985370	21.964173
82.294136	2096.020153	21.969191
82.649049	2102.747001	21.974208
82.940726	2117.250796	21.979226
83.002275	2126.639981	21.984243
83.246949	2127.147753	21.989261
83.324240	2126.226809	21.994279
83.010331	2124.956869	21.999296
83.292989	2125.846884	22.004314
83.105813	2121.760828	22.009331
83.626656	2120.852450	22.014349
83.220092	2129.519651	22.019367
83.808079	2139.325021	22.024384
83.915364	2146.851291	22.029402
83.947440	2145.681790	22.034419
84.024740	2140.250842	22.039437
83.986887	2144.201949	22.044455
84.173239	2143.516403	22.049472
84.246276	2137.417041	22.054490
84.138414	2141.303370	22.059507
84.435312	2141.518916	22.064525
84.169171	2149.504511	22.069543
84.224251	2150.660575	22.074560
84.473184	2165.751820	22.079578
84.069819	2160.961108	22.084595
84.670040	2164.480865	22.089613
84.817577	2167.856933	22.094631
84.809338	2182.085851	22.099648
85.063381	2179.473969	22.104666
84.704796	2176.014406	22.109683
85.182540	2178.972640	22.114701
85.101141	2183.612287	22.119719
85.444086	2199.742956	22.124736
85.671547	2200.035659	22.129754
85.918015	2203.380455	22.134771
86.195473	2196.501058	22.139789
86.224879	2208.369675	22.144807
85.866364	2194.501396	22.149824
86.113832	2194.775184	22.154842
85.799954	2201.133440	22.159859
86.272894	2190.821182	22.164877
86.188401	2186.248770	22.169895
86.582690	2188.450001	22.174912
86.083306	2185.558495	22.179930
86.840135	2191.547011	22.184947
86.728539	2184.933716	22.189965
86.525526	2191.129421	22.194983
86.617225	2192.617449	22.200000
86.424480	2198.808392	22.205018
86.838302	2209.423791	22.210035
87.094360	2209.844568	22.215053
86.940827	2212.677630	22.220071
86.870143	2212.568882	22.225088
87.357348	2209.232443	22.230106
86.976122	2207.417576	22.235123
87.359956	2209.787720	22.240141
87.404160	2227.776801	22.245159
87.335272	2240.970608	22.250176
87.679863	2231.145534	22.255194
87.861094	2231.085689	22.260211
87.996302	2233.460071	22.265229
87.891068	2236.364472	22.270247
87.629115	2234.893863	22.275264
87.993906	2247.120250	22.280282
88.147659	2255.819657	22.285299
88.276027	2254.764462	22.290317
88.157968	2258.081165	22.295335
88.455962	2249.702551	22.300352
89.126156	2250.181533	22.305370
88.616274	2256.725165	22.310387
88.573842	2256.359505	22.315405
88.983562	2252.517602	22.320423
89.165759	2244.539018	22.325440
89.203268	2247.474709	22.330458
89.151278	2251.680540	22.335475
88.722783	2238.315538	22.340493
89.090471	2248.389032	22.345511
89.082130	2259.613446	22.350528
89.317631	2263.512284	22.355546
89.458607	2267.826755	22.360563
89.768655	2267.639420	22.365581
89.785514	2271.881811	22.370599
89.404652	2276.599960	22.375616
89.689332	2266.408680	22.380634
89.534393	2274.402157	22.385651
90.081484	2284.551714	22.390669
90.283536	2288.408457	22.395687
90.137831	2294.828769	22.400704
90.159181	2285.811768	22.405722
90.015319	2291.969835	22.410739
90.285122	2289.718417	22.415757
90.289953	2298.766253	22.420775
90.474916	2307.501824	22.425792
90.896669	2303.983102	22.430810
90.588980	2317.410056	22.435827
90.792315	2304.586700	22.440845
90.960227	2307.858608	22.445863
90.849989	2317.558854	22.450880
91.422116	2324.482149	22.455898
91.244093	2330.733952	22.460915
91.526604	2330.232167	22.465933
91.602411	2336.134908	22.470951
91.530627	2328.811515	22.475968
91.954720	2324.254069	22.480986
91.508456	2331.655684	22.486003
91.666660	2325.684939	22.491021
91.672047	2329.345265	22.496039
91.821296	2336.151764	22.501056
92.195776	2341.635295	22.506074
92.291910	2353.509334	22.511091
92.444211	2349.079679	22.516109
92.645475	2348.316042	22.521127
92.398365	2355.856894	22.526144
92.907603	2346.981195	22.531162
92.688347	2352.927012	22.536179
92.698671	2340.938673	22.541197
92.784508	2348.168560	22.546215
93.117552	2355.255568	22.551232
93.317085	2352.178787	22.556250
93.258027	2367.738216	22.561267
92.979520	2371.130575	22.566285
93.422475	2377.405037	22.571303
93.338381	2373.526855	22.576320
93.498479	2370.614054	22.581338
93.564266	2368.113698	22.586355
93.555381	2365.028539	22.591373
93.634303	2373.256845	22.596391
93.717969	2387.825009	22.601408
94.327607	2389.894688	22.606426
94.299426	2404.227902	22.611443
93.871178	2398.046027	22.616461
94.279536	2395.880196	22.621479
93.854002	2397.316720	22.626496
94.440821	2392.626456	22.631514
94.612134	2403.431457	22.636531
94.588895	2417.075877	22.641549
94.704987	2409.782983	22.646567
94.711333	2415.589324	22.651584
94.861667	2412.958940	22.656602
95.149121	2418.408787	22.661619
95.100932	2413.726477	22.666637
95.196891	2415.472657	22.671655
94.980576	2414.247371	22.676672
95.457309	2401.311679	22.681690
95.429134	2412.422520	22.686707
95.292858	2425.857416	22.691725
95.490355	2423.222798	22.696743
95.533701	2432.454033	22.701760
95.555600	2434.530584	22.706778
95.426602	2431.697784	22.711795
95.500845	2443.297575	22.716813
96.062307	2451.046335	22.721831
96.095193	2452.537287	22.726848
96.188246	2457.957637	22.731866
96.157895	2455.456550	22.736883
96.207168	2453.047140	22.741901
96.716952	2466.627025	22.746919
96.501969	2465.085915	22.751936
96.752738	2472.473066	22.756954
97.067646	2475.636761	22.761971
96.949080	2471.401006	22.766989
96.982151	2460.545223	22.772007
97.299991	2477.734218	22.777024
97.355865	2458.059842	22.782042
97.081810	2469.859400	22.787059
97.121215	2487.186709	22.792077
97.842329	2492.186747	22.797095
97.365448	2492.782328	22.802112
97.769985	2492.712746	22.807130
97.820339	2490.921760	22.812147
98.190867	2487.010202	22.817165
98.030830	2488.288361	22.822183
97.675845	2506.883115	22.827200
97.979364	2523.844000	22.832218
98.199458	2513.877316	22.837235
97.971585	2519.291154	22.842253
98.038335	2517.005242	22.847271
98.180524	2542.004811	22.852288
98.295540	2529.810576	22.857306
98.749009	2541.388891	22.862323
98.687734	2556.459631	22.867341
99.202355	2550.754897	22.872359
99.209012	2558.505410	22.877376
99.321319	2549.376186	22.882394
99.655616	2552.268586	22.887411
99.349480	2551.868487	22.892429
100.167410	2541.416765	22.897447
99.663342	2550.389806	22.902464
99.698414	2539.811402	22.907482
99.898008	2542.188363	22.912499
100.487123	2539.785892	22.917517
100.491894	2537.834768	22.922535
100.552765	2542.389096	22.927552
100.709593	2539.827111	22.932570
100.951373	2545.312558	22.937587
100.917127	2539.905278	22.942605
101.264254	2538.957819	22.947623
100.803362	2541.993736	22.952640
100.499834	2531.667221	22.957658
100.687311	2532.827816	22.962675
100.441314	2531.708168	22.967693
100.893121	2546.408152	22.972711
101.153835	2551.884322	22.977728
101.085099	2561.556105	22.982746
101.186043	2567.028906	22.987763
100.756757	2565.243623	22.992781
101.369830	2569.256962	22.997799
101.352442	2579.113233	23.002816
101.618772	2575.924953	23.007834
101.486391	2581.989793	23.012851
101.732800	2583.567236	23.017869
101.892988	2584.981444	23.022887
102.069795	2603.205773	23.027904
102.006735	2608.798966	23.032922
102.440447	2613.067656	23.037939
102.393043	2610.020051	23.042957
102.619987	2600.907559	23.047975
102.422885	2599.309982	23.052992
102.832021	2602.471561	23.058010
102.896982	2605.690219	23.063027
102.826036	2600.960928	23.068045
102.936141	2617.415661	23.073063
103.132090	2625.591031	23.078080
102.959095	2627.540331	23.083098
103.194608	2625.887599	23.088115
103.019435	2625.561664	23.093133
103.860860	2637.025606	23.098151
103.976928	2659.949535	23.103168
103.641062	2652.689477	23.108186
103.777209	2655.133204	23.113203
103.847848	2654.910784	23.118221
104.517297	2649.074453	23.123239
104.318683	2656.058664	23.128256
104.470477	2655.015556	23.133274
104.448363	2646.516479	23.138291
103.766084	2649.347231	23.143309
104.436302	2650.956123	23.148327
104.690138	2668.701341	23.153344
104.746338	2675.756103	23.158362
105.043258	2663.372315	23.163379
105.082864	2680.087487	23.168397
104.839191	2660.832245	23.173415
105.241477	2675.776805	23.178432
105.066089	2689.139122	23.183450
105.529678	2691.847169	23.188467
105.123954	2690.616820	23.193485
105.588892	2694.047415	23.198503
105.707681	2699.340716	23.203520
105.615351	2699.090173	23.208538
105.934055	2716.077267	23.213555
105.352603	2722.793242	23.218573
106.079232	2716.824842	23.223591
106.132301	2729.927309	23.228608
106.210609	2736.615673	23.233626
106.697005	2744.407883	23.238643
106.508942	2745.258057	23.243661
106.957579	2729.751106	23.248679
106.639675	2741.096911	23.253696
106.668880	2731.346227	23.258714
107.156714	2730.916418	23.263731
107.199994	2746.914628	23.268749
107.253260	2751.924687	23.273767
107.567195	2752.576280	23.278784
107.646043	2756.259901	23.283802
107.672795	2750.558947	23.288819
107.674363	2761.002550	23.293837
107.919869	2751.568301	23.298855
108.022490	2750.056311	23.303872
107.854705	2756.975764	23.308890
108.516986	2746.895488	23.313907
108.201596	2757.060505	23.318925
108.231708	2754.477312	23.323943
108.456293	2769.989495	23.328960
108.687965	2772.396179	23.333978
108.889949	2768.728741	23.338995
108.493274	2769.491665	23.344013
108.508069	2774.870717	23.349031
108.864827	2771.586176	23.354048
108.824700	2771.734599	23.359066
109.152265	2775.076266	23.364083
109.141655	2798.111746	23.369101
109.304702	2794.248409	23.374119
109.002385	2792.380087	23.379136
109.324694	2785.487128	23.384154
109.339373	2790.670520	23.389171
109.144750	2805.490930	23.394189
109.752652	2805.569389	23.399207
109.793006	2810.310056	23.404224
109.818546	2817.729481	23.409242
110.144480	2823.694192	23.414259
110.090982	2836.680874	23.419277
110.553707	2836.220278	23.424295
110.438741	2841.452402	23.429312
110.664858	2829.947542	23.434330
111.201733	2829.421675	23.439347
110.979820	2830.371841	23.444365
110.937817	2829.138153	23.449383
110.999818	2849.833067	23.454400
111.036909	2852.759455	23.459418
111.428034	2850.908733	23.464435
111.517181	2854.745414	23.469453
111.348806	2851.076016	23.474471
111.657039	2856.513273	23.479488
111.706498	2864.433958	23.484506
112.377469	2874.002644	23.489523
112.071898	2879.277266	23.494541
112.014637	2874.119674	23.499559
112.226561	2870.258131	23.504576
112.352151	2883.560813	23.509594
112.428547	2873.969936	23.514611
112.524636	2877.613007	23.519629
112.557841	2889.809722	23.524647
112.933469	2884.950424	23.529664
113.009248	2894.776491	23.534682
113.199439	2901.655696	23.539699
113.373860	2892.803780	23.544717
113.290207	2885.671391	23.549735
113.476979	2889.764216	23.554752
113.523561	2889.965335	23.559770
113.881627	2883.656944	23.564787
113.519377	2896.616292	23.569805
113.900782	2909.724262	23.574823
114.045214	2910.800097	23.579840
113.837573	2911.006326	23.584858
114.219597	2910.043914	23.589875
114.199981	2911.091794	23.594893
114.089888	2916.840792	23.599911
114.631333	2927.726993	23.604928
114.266439	2942.978185	23.609946
114.689805	2936.552234	23.614963
114.782280	2942.076976	23.619981
114.958860	2929.765514	23.624999
115.063056	2938.375175	23.630016
115.132794	2951.086980	23.635034
115.382468	2953.654991	23.640051
115.416341	2956.600837	23.645069
115.508300	2951.823838	23.650087
115.721414	2953.289752	23.655104
115.354877	2954.066898	23.660122
115.799093	2957.283013	23.665139
115.861232	2972.786103	23.670157
115.815936	2978.992086	23.675175
116.195033	2972.768743	23.680192
116.432281	2976.020443	23.685210
116.509078	2972.050645	23.690227
116.612639	2962.464933	23.695245
116.256039	2979.943132	23.700263
116.540085	2992.059588	23.705280
116.781622	2997.216967	23.710298
117.042933	2985.927428	23.715315
117.170038	2988.505178	23.720333
117.025267	2992.804623	23.725351
117.642438	3004.341810	23.730368
117.327039	3013.639017	23.735386
117.647521	3010.855641	23.740403
117.420587	3021.619253	23.745421
117.726632	3015.836584	23.750439
118.004754	3004.298215	23.755456
117.773488	3014.525947	23.760474
118.378299	3016.350275	23.765491
118.701173	3029.748405	23.770509
118.456019	3032.242453	23.775527
118.775816	3034.253466	23.780544
118.424043	3036.937810	23.785562
118.765821	3034.987490	23.790579
118.638272	3041.417847	23.795597
118.512757	3047.630109	23.800615
119.313797	3055.079633	23.805632
119.148479	3062.822588	23.810650
119.360611	3056.205597	23.815667
119.418136	3059.122505	23.820685
119.251456	3055.257114	23.825703
119.607669	3069.789445	23.830720
119.576175	3080.901219	23.835738
119.696475	3068.216578	23.840755
119.797263	3086.854147	23.845773
120.158872	3088.243152	23.850791
120.609156	3090.252665	23.855808
120.747019	3098.913940	23.860826
120.768344	3100.646630	23.865843
120.682707	3101.540741	23.870861
120.913841	3097.780296	23.875879
120.849235	3093.832625	23.880896
121.019005	3101.141196	23.885914
121.145002	3103.375108	23.890931
121.095673	3121.493361	23.895949
121.137922	3128.651485	23.900967
121.473784	3114.585331	23.905984
121.298047	3119.845993	23.911002
121.637971	3139.582393	23.916019
121.703369	3144.937847	23.921037
121.990607	3141.916630	23.926055
122.248571	3145.676425	23.931072
122.265934	3143.997855	23.936090
122.648649	3153.450884	23.941107
122.862416	3157.050326	23.946125
122.890108	3173.644729	23.951143
123.129696	3160.897148	23.956160
122.766370	3164.637502	23.961178
123.057865	3160.804463	23.966195
123.212146	3160.805651	23.971213
123.145813	3165.872437	23.976231
123.208957	3158.836878	23.981248
123.353598	3174.907964	23.986266
123.745390	3178.833017	23.991283
123.626178	3177.996462	23.996301
123.422601	3188.450359	24.001319
123.675470	3181.441880	24.006336
123.990907	3202.886553	24.011354
124.093536	3208.435036	24.016371
124.049852	3201.359384	24.021389
124.398546	3208.485312	24.026407
124.410741	3209.654475	24.031424
124.419740	3220.210805	24.036442
124.535529	3233.237531	24.041459
125.031272	3223.498708	24.046477
124.771783	3235.608951	24.051495
124.973615	3236.129782	24.056512
125.150881	3250.699763	24.061530
125.180270	3250.638455	24.066547
125.631865	3258.821406	24.071565
125.338246	3266.672923	24.076583
125.762941	3258.065682	24.081600
126.055446	3278.320975	24.086618
126.000184	3284.986281	24.091635
126.166431	3277.745148	24.096653
125.934610	3277.298669	24.101671
126.086983	3283.473788	24.106688
125.882412	3290.134081	24.111706
126.070849	3305.895421	24.116723
126.598569	3300.876467	24.121741
126.531895	3329.511142	24.126759
126.932692	3325.279037	24.131776
127.062912	3325.277682	24.136794
127.003739	3324.150807	24.141811
127.655313	3336.254102	24.146829
127.648083	3345.257010	24.151847
128.115152	3348.387554	24.156864
128.045997	3349.894566	24.161882
127.964038	3345.353024	24.166899
128.426281	3341.663635	24.171917
128.072501	3341.693919	24.176935
128.489740	3331.538086	24.181952
128.685299	3340.121000	24.186970
128.667590	3362.593342	24.191987
128.732717	3362.718967	24.197005
128.716982	3370.119835	24.202023
128.874457	3362.031006	24.207040
128.621464	3370.766271	24.212058
129.093874	3382.042318	24.217075
129.385638	3394.378774	24.222093
129.085660	3394.615256	24.227111
129.405696	3389.767690	24.232128
129.748441	3409.453444	24.237146
130.019901	3418.116036	24.242163
130.408674	3398.372699	24.247181
130.386710	3406.039685	24.252199
130.731373	3403.280868	24.257216
130.848132	3396.836509	24.262234
130.928311	3400.229677	24.267251
130.947832	3404.288853	24.272269
130.820554	3394.331918	24.277287
130.971619	3400.564096	24.282304
131.115086	3410.439808	24.287322
131.666389	3423.313222	24.292339
131.349972	3417.274442	24.297357
131.539686	3426.641070	24.302375
131.591834	3418.713906	24.307392
131.476645	3422.440688	24.312410
131.432700	3421.658612	24.317427
131.523003	3436.037209	24.322445
131.232824	3444.478488	24.327463
131.734605	3452.432725	24.332480
131.749233	3461.785770	24.337498
132.335419	3465.652026	24.342515
132.859402	3482.686592	24.347533
132.419455	3501.011611	24.352551
132.976701	3490.669627	24.357568
133.141367	3484.463922	24.362586
133.025775	3486.855670	24.367603
133.427998	3489.425110	24.372621
133.318093	3505.258615	24.377639
133.606093	3500.747450	24.382656
133.824109	3514.055055	24.387674
134.113837	3504.806020	24.392691
133.892033	3505.058663	24.397709
133.819501	3508.182240	24.402727
133.730553	3494.722071	24.407744
134.305411	3517.190147	24.412762
134.557938	3523.516942	24.417779
134.641220	3521.348253	24.422797
134.939912	3526.903992	24.427815
134.968168	3521.625503	24.432832
134.987160	3520.110771	24.437850
135.084485	3537.136480	24.442867
135.472123	3542.144876	24.447885
135.347446	3550.724404	24.452903
135.570478	3549.512270	24.457920
135.669661	3545.920752	24.462938
135.217644	3555.858274	24.467955
135.613257	3562.670830	24.472973
135.929119	3566.620490	24.477991
136.234391	3569.075723	24.483008
136.301477	3575.769313	24.488026
136.264873	3591.963854	24.493043
136.509618	3594.605325	24.498061
136.623626	3587.678414	24.503079
136.548741	3592.939195	24.508096
136.804632	3614.791382	24.513114
136.728332	3625.235060	24.518131
137.130095	3615.905290	24.523149
137.230506	3636.172143	24.528167
137.665787	3649.871913	24.533184
137.572729	3654.895679	24.538202
137.403742	3645.557465	24.543219
138.166143	3660.702090	24.548237
138.467941	3667.545166	24.553255
138.224664	3675.007057	24.558272
138.579444	3665.305864	24.563290
138.112288	3674.059045	24.568307
139.135221	3680.505080	24.573325
138.633847	3686.239869	24.578343
138.858702	3687.593534	24.583360
139.417205	3691.031760	24.588378
139.232240	3685.622498	24.593395
139.761633	3687.597593	24.598413
139.733700	3705.488980	24.603431
139.673037	3715.033862	24.608448
139.898565	3705.416023	24.613466
139.683093	3711.816204	24.618483
140.068303	3701.374800	24.623501
139.826274	3715.108136	24.628519
140.402825	3726.955162	24.633536
140.433879	3730.627532	24.638554
140.478909	3741.645659	24.643571
140.646297	3742.844201	24.648589
140.833414	3762.557878	24.653607
140.858993	3761.136784	24.658624
141.413077	3763.799257	24.663642
141.411185	3766.189011	24.668659
141.445785	3763.197803	24.673677
141.421643	3774.362509	24.678695
141.539627	3778.314809	24.683712
141.750273	3770.441569	24.688730
141.929989	3794.262838	24.693747
142.495493	3787.782757	24.698765
142.456179	3781.583657	24.703783
143.024464	3787.302404	24.708800
142.937421	3782.430132	24.713818
142.861647	3797.381082	24.718835
142.944695	3784.777528	24.723853
143.100839	3791.138455	24.728871
143.015303	3786.676271	24.733888
143.212879	3796.603689	24.738906
143.432094	3813.739973	24.743923
143.816884	3808.860057	24.748941
143.826771	3808.230504	24.753959
143.543131	3806.980948	24.758976
143.483258	3819.435912	24.763994
143.570353	3837.675545	24.769011
143.714854	3830.314501	24.774029
144.072504	3842.277962	24.779047
144.453464	3850.409123	24.784064
144.407840	3859.610839	24.789082
144.642282	3883.521499	24.794099
144.785300	3883.833776	24.799117
145.014024	3890.940893	24.804135
145.294610	3893.163311	24.809152
145.809413	3904.884405	24.814170
145.558819	3912.628456	24.819187
145.815672	3909.261517	24.824205
146.216078	3911.241064	24.829223
146.257679	3917.140213	24.834240
146.463407	3915.261618	24.839258
145.970975	3919.760941	24.844275
146.435011	3924.340835	24.849293
146.670332	3932.378063	24.854311
146.528481	3935.499948	24.859328
146.964830	3940.472417	24.864346
147.024516	3950.850788	24.869363
147.123471	3954.572538	24.874381
147.473370	3956.380089	24.879399
147.449499	3962.936566	24.884416
147.833905	3965.044881	24.889434
148.117142	3985.933696	24.894451
148.025191	3970.977520	24.899469
148.384741	3982.795584	24.904487
148.203961	3986.112959	24.909504
148.519617	3972.544858	24.914522
148.702698	3991.789118	24.919539
148.888221	3998.663162	24.924557
148.832474	3996.661391	24.929575
149.072517	4006.812687	24.934592
149.148140	4001.577139	24.939610
148.781252	4005.498135	24.944627
149.476984	4007.522961	24.949645
149.489924	4026.888604	24.954663
149.379025	4027.149129	24.959680
149.674470	4041.170961	24.964698
149.940464	4044.992815	24.969715
150.291535	4048.315258	24.974733
150.656601	4050.821161	24.979751
150.334636	4057.740012	24.984768
150.893713	4062.664881	24.989786
150.342999	4068.391737	24.994803
150.718875	4070.671845	24.999821
151.128258	4081.459496	25.004839
151.070893	4097.667211	25.009856
151.709697	4098.678293	25.014874
151.491965	4092.241901	25.019891
151.499882	4098.976519	25.024909
151.853751	4120.242660	25.029927
151.717126	4120.393586	25.034944
152.422504	4120.049613	25.039962
152.265229	4122.776240	25.044979
152.336572	4125.675374	25.049997
152.772208	4128.463777	25.055015
152.976618	4140.574544	25.060032
153.020580	4130.416773	25.065050
152.971615	4139.448709	25.070067
153.435642	4134.666767	25.075085
153.766669	4131.878415	25.080103
153.221776	4134.719428	25.085120
153.925929	4139.403798	25.090138
153.640127	4145.871964	25.095155
154.055706	4150.699395	25.100173
154.135530	4150.971075	25.105191
153.920409	4150.004304	25.110208
154.219575	4154.458579	25.115226
154.750900	4167.414568	25.120243
154.154650	4165.563740	25.125261
154.539433	4177.857753	25.130279
154.676319	4194.941012	25.135296
155.044927	4205.997108	25.140314
155.320643	4204.723020	25.145331
155.447024	4208.159604	25.150349
155.554701	4220.547561	25.155367
155.518058	4226.544292	25.160384
155.960370	4219.420512	25.165402
156.089023	4238.424204	25.170419
156.218959	4244.805179	25.175437
156.685381	4250.439028	25.180455
156.481271	4250.764661	25.185472
156.648153	4249.150945	25.190490
156.655960	4270.869188	25.195507
157.285056	4271.007472	25.200525
156.939642	4263.186412	25.205543
156.941406	4277.304940	25.210560
157.578158	4286.096952	25.215578
157.610295	4295.526595	25.220595
157.349088	4294.939496	25.225613
157.519479	4311.982895	25.230631
157.921569	4310.430175	25.235648
157.769815	4324.354996	25.240666
157.988027	4341.605569	25.245683
158.262984	4354.696548	25.250701
158.899612	4358.611914	25.255719
159.006062	4378.165296	25.260736
159.093828	4374.326043	25.265754
159.061856	4380.820812	25.270771
159.412616	4376.028145	25.275789
159.695266	4381.438310	25.280807
159.259830	4385.913035	25.285824
160.084461	4396.588474	25.290842
160.176184	4412.435373	25.295859
160.190064	4416.656639	25.300877
160.357628	4409.193897	25.305895
160.601160	4428.015655	25.310912
160.868253	4427.743499	25.315930
160.990249	4434.823362	25.320947
161.118653	4433.578650	25.325965
161.300937	4435.614523	25.330983
161.805336	4452.826680	25.336000
161.902054	4458.256528	25.341018
161.948931	4452.327776	25.346035
161.742194	4455.541983	25.351053
162.098757	4448.781915	25.356071
161.970778	4458.369298	25.361088
162.449069	4465.538551	25.366106
162.670211	4473.303630	25.371123
162.719766	4481.060873	25.376141
162.696456	4476.222620	25.381159
162.509731	4487.122841	25.386176
163.025024	4491.110905	25.391194
163.242294	4496.566068	25.396211
163.292534	4502.097904	25.401229
163.882412	4502.409629	25.406247
163.566457	4519.516790	25.411264
163.981477	4517.801047	25.416282
164.158255	4519.515833	25.421299
164.263356	4529.792727	25.426317
164.425636	4514.932002	25.431335
164.509376	4537.336248	25.436352
164.498835	4537.552648	25.441370
164.496335	4544.797255	25.446387
164.354007	4550.772773	25.451405
165.073785	4559.592946	25.456423
164.994560	4570.088128	25.461440
165.538249	4573.996007	25.466458
165.926747	4584.253786	25.471475
165.814176	4592.118544	25.476493
166.161299	4594.838819	25.481511
166.438524	4588.012217	25.486528
166.515453	4595.796785	25.491546
166.846868	4599.551692	25.496563
166.701372	4609.719536	25.501581
167.290917	4600.877510	25.506599
167.041546	4603.337709	25.511616
167.293861	4619.374271	25.516634
167.561400	4615.876113	25.521651
167.635479	4620.589877	25.526669
167.926216	4619.051420	25.531687
167.756064	4621.186719	25.536704
168.232919	4640.672885	25.541722
168.577975	4648.604860	25.546739
168.521644	4654.604817	25.551757
168.764417	4652.499389	25.556775
168.958078	4646.774846	25.561792
168.864195	4647.001148	25.566810
169.329925	4665.419033	25.571827
169.450910	4670.037080	25.576845
169.698230	4671.036930	25.581863
169.481371	4669.874700	25.586880
169.692353	4678.720981	25.591898
169.788121	4690.337783	25.596915
169.873165	4691.524039	25.601933
170.344393	4699.594095	25.606951
170.462042	4722.012195	25.611968
170.475732	4715.488821	25.616986
170.766296	4715.803251	25.622003
170.871891	4739.650002	25.627021
171.056603	4745.407053	25.632039
171.233972	4747.879330	25.637056
171.440794	4750.713148	25.642074
171.714288	4759.707501	25.647091
171.660271	4769.636990	25.652109
172.045944	4773.159321	25.657127
171.728235	4781.122585	25.662144
172.512546	4791.024917	25.667162
172.454614	4794.446296	25.672180
172.678990	4792.343735	25.677197
172.827909	4804.646717	25.682215
172.721144	4816.724616	25.687232
172.819851	4810.058472	25.692250
173.375122	4825.507990	25.697268
173.284229	4843.287257	25.702285
173.492910	4832.778167	25.707303
173.499686	4855.917707	25.712320
174.122241	4860.905453	25.717338
174.446925	4863.386232	25.722356
174.181819	4870.552161	25.727373
174.401890	4876.209019	25.732391
174.604141	4877.279072	25.737408
174.617184	4877.185598	25.742426
175.077540	4879.635656	25.747444
175.101886	4895.237853	25.752461
175.111997	4905.930721	25.757479
175.115161	4914.257280	25.762496
175.296840	4918.600732	25.767514
175.655409	4929.703036	25.772532
175.732680	4936.382907	25.777549
176.118930	4946.044657	25.782567
176.216982	4952.029996	25.787584
176.498565	4962.835039	25.792602
176.766160	4977.010317	25.797620
176.968620	4976.811411	25.802637
177.276386	4980.614295	25.807655
177.435486	4984.970771	25.812672
177.781359	5002.643891	25.817690
177.687477	5007.137857	25.822708
177.893164	5006.692234	25.827725
178.294167	5000.764644	25.832743
178.196228	5009.520594	25.837760
178.231716	5027.447540	25.842778
178.986185	5026.903317	25.847796
178.553869	5032.539322	25.852813
178.645172	5040.687989	25.857831
178.775161	5056.624152	25.862848
178.574253	5062.479595	25.867866
179.234669	5064.958312	25.872884
179.428186	5079.227346	25.877901
179.662439	5093.976121	25.882919
179.793538	5102.771992	25.887936
180.025613	5106.687771	25.892954
180.307874	5117.003531	25.897972
180.624190	5131.319656	25.902989
180.747887	5134.378048	25.908007
180.976766	5133.988764	25.913024
181.244095	5148.281011	25.918042
181.466857	5163.549322	25.923060
181.586082	5164.427222	25.928077
182.060109	5156.685734	25.933095
182.145498	5176.022313	25.938112
182.053931	5169.464761	25.943130
182.807756	5166.600548	25.948148
182.651999	5169.235551	25.953165
183.157543	5166.081950	25.958183
183.053042	5162.282123	25.963200
183.112645	5180.552665	25.968218
183.370981	5189.941023	25.973236
183.374705	5190.085751	25.978253
183.554491	5184.536826	25.983271
183.927292	5194.166094	25.988288
184.150508	5210.671756	25.993306
184.311354	5207.913060	25.998324
184.008503	5218.431022	26.003341
184.284982	5217.854354	26.008359
184.763856	5219.477688	26.013376
184.666289	5234.543714	26.018394
184.644189	5236.908417	26.023412
184.668814	5252.810753	26.028429
184.836422	5258.782139	26.033447
185.130053	5273.976309	26.038464
185.583656	5276.929379	26.043482
185.696257	5286.138595	26.048500
185.986334	5309.512110	26.053517
186.140277	5309.649089	26.058535
186.569852	5315.727815	26.063552
186.409267	5324.803078	26.068570
186.892194	5339.086952	26.073588
186.514685	5338.211844	26.078605
186.755143	5337.359877	26.083623
187.519594	5346.233415	26.088640
187.617963	5362.083257	26.093658
187.863653	5348.203121	26.098676
187.715404	5354.643851	26.103693
187.730336	5370.033279	26.108711
187.927458	5382.247029	26.113728
188.137323	5387.375333	26.118746
188.257788	5401.403535	26.123764
188.658838	5409.118735	26.128781
188.677211	5422.121260	26.133799
189.348444	5426.145081	26.138816
189.460536	5435.307103	26.143834
189.758304	5431.971357	26.148852
189.716446	5443.250345	26.153869
190.070449	5449.842859	26.158887
190.116404	5455.186258	26.163904
190.189349	5460.901071	26.168922
190.528574	5472.016207	26.173940
190.592662	5475.330212	26.178957
190.575321	5484.866079	26.183975
190.641747	5489.281387	26.188992
191.278360	5503.285627	26.194010
191.427212	5501.841929	26.199028
191.548243	5524.800273	26.204045
192.024040	5524.268131	26.209063
192.331236	5532.468426	26.214080
192.410639	5546.026519	26.219098
192.846922	5533.581068	26.224116
192.910514	5533.823746	26.229133
193.229211	5531.864158	26.234151
193.245442	5538.023496	26.239168
193.155916	5552.835993	26.244186
193.278114	5555.487484	26.249204
193.883425	5564.919535	26.254221
193.813747	5584.116693	26.259239
194.701937	5581.600698	26.264256
194.775216	5580.231966	26.269274
194.847721	5577.843756	26.274292
194.866505	5571.622317	26.279309
194.749237	5583.711838	26.284327
195.547462	5588.871137	26.289344
195.136601	5603.737172	26.294362
195.889321	5596.766258	26.299380
195.505885	5610.706259	26.304397
195.752499	5627.094993	26.309415
196.195045	5624.822423	26.314432
195.849050	5629.147698	26.319450
196.194865	5641.653994	26.324468
196.315748	5646.509056	26.329485
196.294908	5647.636202	26.334503
196.537265	5667.617925	26.339520
197.087479	5676.417862	26.344538
197.329040	5702.915116	26.349556
197.305998	5697.530391	26.354573
197.987596	5712.771476	26.359591
198.197624	5723.802836	26.364608
198.180931	5742.313174	26.369626
198.141350	5728.490067	26.374644
198.523162	5740.700378	26.379661
198.652396	5751.539227	26.384679
199.165812	5755.411073	26.389696
199.002348	5768.726433	26.394714
199.322995	5763.742410	26.399732
199.498880	5770.946932	26.404749
199.884068	5773.626702	26.409767
199.647382	5774.172116	26.414784
199.952921	5802.190485	26.419802
199.818815	5803.224901	26.424820
200.529385	5806.333519	26.429837
200.741155	5820.306702	26.434855
200.719775	5823.580496	26.439872
200.946218	5828.965178	26.444890
201.305716	5837.021680	26.449908
200.925968	5846.134691	26.454925
201.500390	5855.546479	26.459943
201.690014	5853.038872	26.464960
201.907248	5870.852943	26.469978
202.406556	5877.277642	26.474996
202.408542	5889.244511	26.480013
202.644051	5898.115954	26.485031
202.696680	5898.249870	26.490048
202.956701	5913.737100	26.495066
203.070617	5919.909674	26.500084
203.156987	5920.827482	26.505101
203.622323	5941.917304	26.510119
203.779920	5948.682821	26.515136
204.074943	5966.074425	26.520154
204.244644	5971.316516	26.525172
204.471799	5960.519780	26.530189
204.250194	5989.956311	26.535207
204.506793	5983.830058	26.540224
205.111689	6005.078022	26.545242
205.065161	6011.566181	26.550260
205.451803	6025.057558	26.555277
205.427811	6035.481795	26.560295
205.900653	6039.429506	26.565312
206.294194	6059.028105	26.570330
206.682463	6058.784298	26.575348
206.803280	6064.854825	26.580365
207.091172	6065.914691	26.585383
207.044281	6064.782563	26.590400
207.342695	6085.889231	26.595418
207.244011	6077.488930	26.600436
207.862428	6090.331638	26.605453
208.079805	6099.954168	26.610471
208.502767	6104.806223	26.615488
208.390577	6108.649882	26.620506
208.774013	6117.438280	26.625524
209.209048	6128.320993	26.630541
209.174195	6134.355951	26.635559
209.378988	6127.634827	26.640576
209.726091	6125.629690	26.645594
209.854700	6138.378700	26.650612
210.304341	6146.162364	26.655629
210.071099	6155.202068	26.660647
210.350338	6148.538723	26.665664
210.221618	6158.262854	26.670682
210.646512	6163.966945	26.675700
210.915463	6169.749133	26.680717
210.738453	6176.750246	26.685735
211.260683	6189.810125	26.690752
211.633998	6203.657279	26.695770
211.649146	6204.924032	26.700788
211.187052	6223.744547	26.705805
211.714585	6227.055535	26.710823
211.924677	6241.629090	26.715840
212.492898	6250.669557	26.720858
212.503504	6265.943616	26.725876
213.167075	6273.902169	26.730893
213.337693	6288.242030	26.735911
213.422686	6282.720251	26.740928
213.736453	6298.821272	26.745946
213.971694	6301.193150	26.750964
213.795455	6305.151057	26.755981
213.888201	6310.661000	26.760999
213.816864	6318.396925	26.766016
214.466297	6326.177779	26.771034
214.444388	6332.431749	26.776052
214.710906	6344.161755	26.781069
214.608562	6366.187017	26.786087
214.952462	6369.750932	26.791104
215.239207	6373.342742	26.796122
215.140659	6390.130323	26.801140
215.694031	6389.724906	26.806157
216.235602	6413.565525	26.811175
216.392989	6413.282121	26.816192
216.656034	6422.547262	26.821210
216.867750	6438.377125	26.826228
216.996324	6440.718379	26.831245
217.293762	6449.896070	26.836263
217.352948	6463.890492	26.841280
217.523265	6475.629339	26.846298
218.036023	6490.120952	26.851316
218.616601	6484.328910	26.856333
218.544754	6494.151640	26.861351
218.937979	6499.668234	26.866368
218.970544	6515.112686	26.871386
219.163441	6518.719227	26.876404
219.489437	6529.859180	26.881421
219.620197	6543.454162	26.886439
219.882037	6546.576385	26.891456
220.218519	6540.383768	26.896474
220.381837	6561.632108	26.901492
221.007070	6573.770119	26.906509
220.817774	6571.296520	26.911527
220.859665	6572.584364	26.916544
221.067568	6578.499362	26.921562
221.118913	6589.985433	26.926580
221.558341	6604.551761	26.931597
221.682421	6607.540891	26.936615
222.019334	6615.260339	26.941632
222.014513	6624.577016	26.946650
222.177637	6648.142603	26.951668
222.770305	6644.735187	26.956685
222.562538	6664.005619	26.961703
222.854381	6668.767877	26.966720
222.838569	6677.167662	26.971738
223.040931	6692.030059	26.976756
224.029340	6707.435423	26.981773
224.099858	6727.663047	26.986791
224.377293	6731.281642	26.991808
224.619303	6745.184501	26.996826
224.783381	6748.012703	27.001844
224.779172	6744.976577	27.006861
225.528192	6763.402718	27.011879
225.584902	6762.876218	27.016896
225.716649	6761.665553	27.021914
225.645574	6786.205592	27.026932
226.057439	6790.428198	27.031949
225.723572	6794.575059	27.036967
226.274055	6813.919432	27.041984
226.587887	6817.734382	27.047002
226.836803	6836.450451	27.052020
227.174119	6838.673821	27.057037
227.461649	6856.784056	27.062055
227.572728	6869.302713	27.067072
227.517898	6871.410733	27.072090
227.451029	6894.172936	27.077108
228.105518	6897.284219	27.082125
228.653129	6908.048743	27.087143
229.206313	6911.734667	27.092160
229.281609	6909.140650	27.097178
229.106147	6915.368364	27.102196
229.625233	6919.406889	27.107213
229.791381	6937.151079	27.112231
230.237293	6935.152475	27.117248
230.363501	6937.320536	27.122266
230.277766	6947.729708	27.127284
230.661763	6954.201266	27.132301
230.411050	6957.681661	27.137319
231.054779	6966.281319	27.142336
231.200363	6978.497897	27.147354
231.070302	6993.444183	27.152372
231.567856	7003.957739	27.157389
231.339222	7015.289052	27.162407
231.633364	7029.606985	27.167424
232.219726	7035.443902	27.172442
232.160854	7058.261880	27.177460
232.548419	7073.228162	27.182477
232.490538	7080.150974	27.187495
232.546130	7094.708370	27.192512
233.390084	7109.107552	27.197530
233.790752	7121.416855	27.202548
234.564973	7133.816022	27.207565
234.396797	7145.153728	27.212583
234.825313	7141.367853	27.217600
235.223350	7133.902626	27.222618
235.269267	7145.980239	27.227636
235.619242	7157.801871	27.232653
235.588921	7155.407467	27.237671
235.394222	7163.283035	27.242688
236.149441	7172.174705	27.247706
236.343755	7182.401234	27.252724
236.710085	7188.057998	27.257741
236.394371	7207.443773	27.262759
236.358727	7209.274173	27.267776
236.971822	7228.454486	27.272794
237.221055	7241.213779	27.277812
237.682829	7249.905215	27.282829
237.492383	7260.400420	27.287847
237.970164	7275.390619	27.292864
238.078397	7286.978707	27.297882
238.033476	7301.368910	27.302900
238.394567	7306.594029	27.307917
239.279503	7338.823752	27.312935
239.423454	7335.271834	27.317952
239.598926	7340.166148	27.322970
239.354500	7364.440517	27.327988
239.769182	7368.009326	27.333005
239.993582	7382.710982	27.338023
240.191258	7391.143945	27.343040
240.641492	7406.662623	27.348058
240.722890	7422.693697	27.353076
241.085820	7432.600353	27.358093
241.502783	7447.240325	27.363111
241.439459	7459.906669	27.368128
241.871096	7471.314775	27.373146
241.628726	7479.699905	27.378164
242.140680	7485.655962	27.383181
242.463668	7496.253974	27.388199
242.417833	7525.741194	27.393216
243.189215	7518.630892	27.398234
243.206350	7543.969468	27.403252
243.929494	7533.169881	27.408269
243.934500	7541.667823	27.413287
244.369145	7557.346920	27.418304
244.623910	7559.917953	27.423322
245.007722	7573.451957	27.428340
245.192305	7572.548662	27.433357
245.298117	7593.696709	27.438375
245.453554	7582.806079	27.443392
245.503267	7586.867770	27.448410
245.373059	7599.093237	27.453428
245.690146	7607.378157	27.458445
246.006417	7619.221151	27.463463
246.416285	7633.518270	27.468480
246.692030	7636.944733	27.473498
246.627699	7655.903286	27.478516
246.809142	7663.852738	27.483533
247.426522	7678.811927	27.488551
247.516125	7689.143538	27.493568
248.304370	7698.222870	27.498586
248.116814	7714.476280	27.503604
248.261696	7721.276015	27.508621
248.643851	7739.208133	27.513639
248.774011	7751.692830	27.518656
249.578134	7750.645119	27.523674
249.413414	7776.662850	27.528692
249.467995	7780.622796	27.533709
250.026833	7793.030897	27.538727
250.193679	7795.931440	27.543744
250.197348	7804.322373	27.548762
250.415559	7820.297634	27.553780
250.167911	7836.860484	27.558797
250.365474	7853.460945	27.563815
250.867732	7874.575623	27.568832
251.153203	7886.174207	27.573850
251.329949	7906.096036	27.578868
251.768647	7926.545121	27.583885
252.276425	7945.401720	27.588903
252.247932	7962.463895	27.593920
252.805778	7965.098004	27.598938
253.249232	7986.742938	27.603956
253.409303	8004.271271	27.608973
253.741534	8014.404045	27.613991
253.674656	8015.548019	27.619008
254.247252	8023.581577	27.624026
254.520144	8044.082023	27.629044
254.924262	8058.784479	27.634061
255.144572	8066.933227	27.639079
255.049184	8082.926270	27.644096
255.592949	8085.483676	27.649114
255.701161	8103.771614	27.654132
256.264795	8114.329128	27.659149
256.588757	8110.183743	27.664167
256.599780	8123.561869	27.669184
256.852241	8142.547065	27.674202
257.256354	8156.627653	27.679220
257.360885	8168.365258	27.684237
257.825071	8171.260323	27.689255
257.849352	8182.738999	27.694272
258.706247	8192.458186	27.699290
258.348791	8195.718750	27.704308
258.260780	8214.937311	27.709325
258.562463	8216.613940	27.714343
258.863565	8241.927931	27.719360
259.244200	8248.387847	27.724378
259.478096	8267.477107	27.729396
259.789556	8275.289643	27.734413
260.235427	8291.065478	27.739431
260.349994	8304.354900	27.744448
260.982715	8320.616100	27.749466
261.084012	8330.264299	27.754484
261.208355	8339.201697	27.759501
261.452566	8343.659299	27.764519
261.842798	8354.269372	27.769536
262.091731	8365.125743	27.774554
262.246730	8379.753823	27.779572
262.348318	8386.251187	27.784589
262.841934	8390.249832	27.789607
262.960957	8405.120353	27.794624
263.434103	8405.961913	27.799642
263.746627	8412.729328	27.804660
263.999406	8427.673629	27.809677
264.255248	8416.154294	27.814695
264.408848	8435.726721	27.819712
264.751065	8444.121739	27.824730
264.750656	8458.527969	27.829748
264.895479	8463.329513	27.834765
265.050531	8468.653543	27.839783
265.317742	8490.913907	27.844800
265.910752	8494.366603	27.849818
266.243090	8513.106038	27.854836
266.386331	8522.570966	27.859853
267.057222	8531.678569	27.864871
266.693172	8551.736326	27.869888
267.179866	8556.541168	27.874906
267.125095	8567.928280	27.879924
267.591246	8582.567765	27.884941
268.213647	8600.251556	27.889959
267.968558	8614.007973	27.894976
268.319604	8624.880072	27.899994
268.563308	8644.072372	27.905012
268.505480	8663.498200	27.910029
269.079500	8681.189647	27.915047
268.826922	8699.859882	27.920064
269.449955	8711.365064	27.925082
270.263891	8731.967793	27.930100
269.999920	8747.091174	27.935117
270.609835	8756.795680	27.940135
270.981557	8773.208668	27.945152
271.572758	8779.244293	27.950170
271.692634	8796.486054	27.955188
271.584713	8812.270157	27.960205
272.474925	8821.630853	27.965223
272.324923	8840.869245	27.970240
272.880707	8837.896598	27.975258
272.993392	8851.969697	27.980276
273.115457	8866.975873	27.985293
274.024583	8871.919844	27.990311
274.140978	8889.705279	27.995328
274.430510	8883.405579	28.000346
274.341786	8905.535924	28.005364
274.525147	8916.980663	28.010381
274.894305	8920.768444	28.015399
275.318244	8934.881250	28.020416
275.541318	8937.763694	28.025434
275.647166	8947.957702	28.030452
275.763099	8964.527748	28.035469
276.686807	8978.439166	28.040487
276.915869	8989.043280	28.045504
276.683542	8995.451090	28.050522
276.755154	9021.240954	28.055540
277.248642	9027.067803	28.060557
277.848121	9044.417786	28.065575
277.681678	9055.854262	28.070592
278.029007	9070.556949	28.075610
278.428938	9088.812791	28.080628
278.199490	9099.305673	28.085645
279.071756	9126.851986	28.090663
279.170881	9130.158006	28.095680
279.575381	9140.349539	28.100698
279.874493	9149.802999	28.105716
280.080638	9160.650754	28.110733
280.242903	9176.620164	28.115751
280.687395	9195.036466	28.120768
280.909354	9207.653001	28.125786
281.162007	9210.691875	28.130804
281.336799	9222.804330	28.135821
282.093497	9232.530296	28.140839
282.497186	9233.010219	28.145856
282.347170	9244.769438	28.150874
282.620587	9253.169287	28.155892
282.993392	9264.038355	28.160909
283.373647	9268.998979	28.165927
283.678754	9286.385831	28.170944
284.019116	9295.561378	28.175962
284.110322	9309.575043	28.180980
283.907605	9314.762765	28.185997
284.241401	9323.156346	28.191015
284.439709	9346.262058	28.196032
284.989345	9355.013347	28.201050
285.310164	9369.025818	28.206068
285.564935	9384.753591	28.211085
285.840433	9402.489336	28.216103
285.747353	9412.553739	28.221120
286.290279	9438.159844	28.226138
286.844699	9451.696918	28.231156
287.128828	9472.512919	28.236173
287.260026	9481.263512	28.241191
288.017706	9489.928600	28.246208
288.134108	9509.217513	28.251226
288.568422	9524.904651	28.256244
288.770086	9536.811032	28.261261
288.961439	9544.718697	28.266279
289.179308	9558.898991	28.271296
289.490042	9580.036149	28.276314
289.845147	9580.728920	28.281332
290.162541	9608.460748	28.286349
290.863573	9607.552234	28.291367
290.880909	9622.654360	28.296384
291.317731	9633.551505	28.301402
291.318257	9643.522436	28.306420
291.592565	9661.084959	28.311437
291.840869	9668.140742	28.316455
292.118149	9682.116068	28.321472
292.221200	9685.292120	28.326490
292.686401	9704.952840	28.331508
292.911598	9722.257897	28.336525
292.954590	9740.642914	28.341543
293.498866	9750.528725	28.346560
293.848498	9762.610986	28.351578
294.221702	9780.862225	28.356596
294.359822	9802.326626	28.361613
294.945039	9803.134914	28.366631
295.486191	9826.130683	28.371648
295.781605	9835.108309	28.376666
296.155139	9842.002460	28.381684
296.117979	9853.693865	28.386701
296.193380	9859.504380	28.391719
296.923456	9873.775177	28.396736
296.756506	9890.690313	28.401754
297.073355	9904.975346	28.406772
297.238780	9929.214123	28.411789
297.584094	9931.105096	28.416807
297.827995	9941.416949	28.421824
297.873001	9954.705821	28.426842
298.675329	9974.361377	28.431860
299.137043	9995.462728	28.436877
299.395388	9996.372747	28.441895
299.805336	10006.674414	28.446912
300.061603	10029.298283	28.451930
300.931721	10032.651033	28.456948
300.496725	10045.026889	28.461965
300.905075	10041.186761	28.466983
301.007309	10042.793767	28.472000
301.130943	10056.414552	28.477018
301.660607	10067.095334	28.482036
301.883026	10085.907253	28.487053
302.190282	10090.705877	28.492071
302.313685	10113.783229	28.497088
302.690858	10117.705773	28.502106
302.867265	10128.770299	28.507124
302.900447	10145.155441	28.512141
303.166346	10168.008462	28.517159
303.486747	10182.706778	28.522176
303.512492	10203.260957	28.527194
304.164768	10223.739116	28.532212
304.516659	10251.254949	28.537229
304.562343	10259.552001	28.542247
305.031590	10290.238535	28.547264
305.026498	10312.730029	28.552282
306.138879	10330.275572	28.557300
306.213565	10352.940908	28.562317
306.374195	10369.656761	28.567335
307.110124	10390.074638	28.572352
307.562956	10396.220881	28.577370
307.735701	10398.344171	28.582388
307.967034	10411.976763	28.587405
308.302922	10432.116343	28.592423
308.686810	10452.823088	28.597440
308.866989	10461.493847	28.602458
309.392650	10480.009221	28.607476
309.339437	10477.766375	28.612493
309.799074	10496.863614	28.617511
310.007760	10510.616652	28.622528
310.367615	10523.083021	28.627546
310.568318	10545.308903	28.632564
310.858144	10563.798153	28.637581
311.124291	10587.677839	28.642599
311.432428	10593.954169	28.647616
311.912879	10620.253712	28.652634
312.251089	10632.979304	28.657652
312.765601	10647.903338	28.662669
313.205687	10665.008260	28.667687
313.508747	10681.446322	28.672704
313.509618	10691.370396	28.677722
314.073963	10710.271472	28.682740
314.188786	10728.039963	28.687757
314.486354	10743.904270	28.692775
315.007071	10749.642148	28.697792
315.148846	10771.751228	28.702810
316.216758	10801.268104	28.707828
316.078872	10798.350139	28.712845
316.050381	10806.829560	28.717863
316.872652	10824.439961	28.722880
316.818851	10837.928076	28.727898
317.343126	10848.982743	28.732916
317.474712	10861.923997	28.737933
317.907111	10872.582588	28.742951
318.296506	10888.097932	28.747968
318.478997	10901.583812	28.752986
318.991435	10909.126004	28.758004
319.354581	10933.461414	28.763021
319.289309	10944.194846	28.768039
320.028527	10951.711004	28.773056
319.865362	10960.587342	28.778074
319.887396	10974.865699	28.783092
320.796458	10992.588968	28.788109
320.783450	11003.288986	28.793127
321.215304	11015.911759	28.798144
321.134658	11032.981758	28.803162
321.735433	11035.170691	28.808180
321.967798	11063.903169	28.813197
322.344216	11074.340141	28.818215
322.905376	11083.175699	28.823232
323.039974	11111.942510	28.828250
323.591234	11115.528553	28.833268
323.473268	11132.503445	28.838285
323.387544	11159.085048	28.843303
324.146611	11168.476960	28.848320
324.129178	11193.595416	28.853338
324.577672	11204.857937	28.858356
325.123190	11228.287347	28.863373
325.376830	11249.170101	28.868391
326.147676	11258.146565	28.873408
326.209458	11275.159740	28.878426
326.439649	11288.123734	28.883444
326.763080	11312.257454	28.888461
327.190249	11334.919286	28.893479
327.574244	11349.709603	28.898496
327.598136	11371.623137	28.903514
328.010495	11387.075303	28.908532
328.416957	11397.406705	28.913549
328.703241	11423.892518	28.918567
329.178617	11437.730769	28.923584
329.392104	11450.918527	28.928602
329.887675	11465.915652	28.933620
330.149939	11477.700105	28.938637
330.644384	11505.659629	28.943655
331.117524	11520.341387	28.948672
331.214517	11534.175827	28.953690
331.964557	11551.832966	28.958708
332.119759	11566.602456	28.963725
332.445632	11581.162078	28.968743
332.766768	11589.991268	28.973760
332.962237	11612.456062	28.978778
333.148974	11624.331379	28.983796
334.001814	11643.911320	28.988813
334.135994	11661.753448	28.993831
334.586992	11660.132486	28.998848
334.863134	11687.861232	29.003866
335.072799	11689.647330	29.008884
335.738165	11707.933630	29.013901
335.817088	11721.508950	29.018919
336.061040	11732.674365	29.023936
336.216475	11757.475987	29.028954
336.619716	11767.861780	29.033972
336.987365	11790.754526	29.038989
337.277353	11792.938553	29.044007
337.872373	11814.021078	29.049024
337.951047	11833.877214	29.054042
338.317230	11835.509342	29.059060
338.942704	11864.645652	29.064077
339.025632	11884.134878	29.069095
339.732816	11903.403188	29.074112
339.662904	11925.117335	29.079130
340.188114	11931.859036	29.084148
340.786069	11940.663977	29.089165
340.703257	11953.270112	29.094183
341.059583	11976.767987	29.099200
341.537842	11993.255543	29.104218
341.614565	12008.880791	29.109236
341.642561	12021.734865	29.114253
342.280941	12053.992462	29.119271
342.843984	12058.322074	29.124288
342.979139	12089.433348	29.129306
343.638074	12096.008905	29.134324
344.091552	12112.386768	29.139341
343.963373	12124.494882	29.144359
344.303198	12138.604348	29.149376
344.822337	12162.436937	29.154394
345.611368	12181.459037	29.159412
345.868862	12175.415880	29.164429
345.677932	12194.165196	29.169447
346.029943	12207.893872	29.174464
346.552323	12231.678674	29.179482
346.549581	12242.191480	29.184500
347.472127	12251.618332	29.189517
347.460284	12270.267042	29.194535
347.650479	12286.822084	29.199552
348.038539	12304.915571	29.204570
348.189476	12321.173644	29.209588
348.942489	12341.158361	29.214605
349.223992	12361.633789	29.219623
349.573372	12368.216880	29.224640
349.759232	12395.158727	29.229658
350.246770	12407.909503	29.234676
350.799123	12425.099499	29.239693
350.853134	12454.032561	29.244711
351.335379	12473.090381	29.249728
351.761217	12489.318169	29.254746
351.932673	12506.735269	29.259764
352.662569	12514.086158	29.264781
352.453257	12539.817506	29.269799
353.016589	12560.548998	29.274816
353.559970	12574.067968	29.279834
354.024364	12596.289709	29.284852
354.287132	12611.204220	29.289869
354.415691	12634.321757	29.294887
354.768185	12640.263412	29.299904
355.384543	12667.182424	29.304922
355.351261	12691.228529	29.309940
356.030265	12706.797908	29.314957
356.108133	12728.069834	29.319975
356.826678	12738.665721	29.324992
357.160170	12759.705011	29.330010
357.153857	12776.502841	29.335028
357.665992	12788.501607	29.340045
358.175247	12821.254426	29.345063
358.707671	12840.225812	29.350080
358.866212	12855.216841	29.355098
359.096469	12879.051377	29.360116
359.785908	12890.697172	29.365133
360.027984	12917.027800	29.370151
360.031625	12935.763162	29.375168
360.701835	12947.323583	29.380186
361.023859	12965.396470	29.385204
361.433574	12980.285096	29.390221
361.419789	13016.739149	29.395239
362.201845	13036.571635	29.400256
362.910960	13055.149241	29.405274
362.928529	13077.728912	29.410292
363.456924	13085.509489	29.415309
363.659479	13109.718134	29.420327
363.987120	13110.355349	29.425344
364.477116	13125.973630	29.430362
364.627029	13137.239873	29.435380
365.242252	13153.643834	29.440397
365.495745	13179.856196	29.445415
365.834971	13199.739272	29.450432
366.107730	13213.124247	29.455450
366.052295	13235.210269	29.460468
366.911115	13256.834154	29.465485
367.101689	13281.237529	29.470503
367.777375	13298.386898	29.475520
368.131628	13311.784442	29.480538
368.531194	13325.370691	29.485556
368.934682	13323.832827	29.490573
369.489025	13354.501567	29.495591
369.354550	13360.320777	29.500608
369.529153	13370.834852	29.505626
370.214602	13397.605134	29.510644
370.347648	13412.414277	29.515661
370.819668	13426.320838	29.520679
371.131580	13445.589486	29.525696
371.875792	13458.297612	29.530714
371.896242	13479.828857	29.535732
372.409653	13481.643342	29.540749
372.556057	13522.646049	29.545767
372.607050	13539.208203	29.550784
373.426393	13556.739529	29.555802
373.399496	13576.794038	29.560820
374.061900	13590.351940	29.565837
374.175213	13609.932926	29.570855
374.662282	13642.169571	29.575872
375.439678	13662.647683	29.580890
375.474354	13683.359003	29.585908
375.928485	13689.373496	29.590925
376.265832	13732.544735	29.595943
376.474875	13749.587601	29.600960
377.065393	13772.852071	29.605978
377.350592	13796.518096	29.610996
377.971180	13817.696761	29.616013
377.949591	13845.339514	29.621031
378.448906	13853.102859	29.626048
379.029768	13881.128165	29.631066
379.128574	13910.451191	29.636084
379.965072	13926.931697	29.641101
380.122377	13954.496059	29.646119
380.255957	13977.462860	29.651136
380.692391	13989.335293	29.656154
381.284323	14018.366494	29.661172
381.978616	14042.101385	29.666189
382.318451	14060.611502	29.671207
382.815898	14080.271759	29.676224
383.494708	14091.499937	29.681242
383.618899	14113.328301	29.686260
384.562773	14131.011193	29.691277
384.509758	14139.467527	29.696295
385.069107	14152.934601	29.701312
385.605128	14155.010892	29.706330
386.088740	14183.295051	29.711348
386.481804	14183.830474	29.716365
386.896259	14198.561413	29.721383
387.245861	14222.189458	29.726400
387.384153	14233.170784	29.731418
387.606491	14249.782512	29.736436
388.040697	14249.866198	29.741453
388.030463	14276.219286	29.746471
388.696140	14298.540983	29.751488
389.006877	14305.655056	29.756506
388.940747	14333.270755	29.761524
389.404185	14352.867143	29.766541
389.598228	14383.445552	29.771559
389.920159	14407.160273	29.776576
390.570043	14421.879773	29.781594
390.850633	14458.018879	29.786612
391.265721	14472.576232	29.791629
391.485043	14489.873963	29.796647
391.886959	14514.495313	29.801664
392.597127	14542.330800	29.806682
392.871155	14572.748550	29.811700
393.564914	14584.568417	29.816717
393.726493	14610.895055	29.821735
393.954170	14626.483026	29.826752
394.690638	14650.145750	29.831770
394.757210	14669.409855	29.836788
395.001033	14690.411645	29.841805
395.340275	14716.795872	29.846823
395.718508	14736.532329	29.851840
396.161959	14761.861247	29.856858
396.252846	14791.193185	29.861876
397.018243	14808.427777	29.866893
397.086596	14842.769092	29.871911
397.395031	14859.225746	29.876928
398.335236	14887.382585	29.881946
398.533435	14918.024363	29.886964
398.967739	14933.384409	29.891981
399.749608	14951.115552	29.896999
400.103638	14977.289379	29.902016
400.663427	14992.538228	29.907034
401.041254	15023.177305	29.912052
401.615725	15033.705465	29.917069
401.937194	15050.671880	29.922087
402.480581	15078.815360	29.927104
402.559447	15089.778064	29.932122
403.062326	15126.104694	29.937140
403.622174	15134.825515	29.942157
403.890598	15148.635742	29.947175
404.211602	15172.541057	29.952192
404.654533	15182.240328	29.957210
405.122297	15216.399737	29.962228
405.381662	15229.052353	29.967245
406.039357	15251.606974	29.972263
406.276486	15268.030935	29.977280
407.011730	15292.095753	29.982298
407.305777	15313.797820	29.987316
408.146565	15321.088229	29.992333
408.020999	15352.308853	29.997351
408.471513	15364.855819	30.002368
409.129446	15387.600062	30.007386
409.167357	15409.140226	30.012404
409.457475	15419.855264	30.017421
409.472890	15451.252940	30.022439
410.227315	15472.756743	30.027456
410.967039	15495.605162	30.032474
410.764785	15520.382453	30.037492
411.690453	15538.754870	30.042509
412.146747	15572.322946	30.047527
412.243174	15598.089489	30.052544
412.652412	15615.443767	30.057562
413.182839	15646.644235	30.062580
413.586771	15678.041436	30.067597
414.130305	15687.317779	30.072615
413.909850	15709.713605	30.077632
414.800438	15728.435961	30.082650
414.895762	15766.053090	30.087668
415.578743	15785.663939	30.092685
416.158740	15812.220421	30.097703
416.416395	15834.108806	30.102720
417.144456	15850.765891	30.107738
417.442901	15879.770097	30.112756
417.695654	15900.967639	30.117773
418.573136	15924.515108	30.122791
418.490572	15953.057968	30.127808
419.146472	15975.440014	30.132826
419.389475	16009.500233	30.137844
419.924372	16018.730715	30.142861
420.658692	16039.180238	30.147879
420.538375	16066.743755	30.152896
421.042982	16090.713052	30.157914
421.818762	16106.235328	30.162932
422.291003	16140.310408	30.167949
422.442288	16144.857072	30.172967
422.747600	16173.427942	30.177984
423.730640	16173.371985	30.183002
423.743678	16200.744251	30.188020
424.256533	16212.520825	30.193037
424.322154	16233.280595	30.198055
424.389805	16262.409967	30.203072
424.963261	16275.964772	30.208090
425.764069	16311.735317	30.213108
425.941930	16326.767112	30.218125
426.287421	16351.693404	30.223143
426.528118	16381.386484	30.228160
427.147293	16395.215317	30.233178
427.608016	16426.431131	30.238196
427.962602	16464.239586	30.243213
428.853491	16485.063031	30.248231
428.521490	16511.125315	30.253248
428.989504	16536.762268	30.258266
429.743291	16561.413261	30.263284
430.287602	16584.227261	30.268301
430.791900	16615.294424	30.273319
430.839953	16644.414808	30.278336
431.871425	16666.489313	30.283354
432.061899	16695.085262	30.288372
432.185423	16727.958911	30.293389
433.346374	16741.984244	30.298407
433.412542	16768.300362	30.303424
434.213109	16789.627859	30.308442
434.834938	16802.913302	30.313460
435.030552	16835.807430	30.318477
435.793492	16846.269171	30.323495
436.079894	16871.353844	30.328512
436.697077	16881.301480	30.333530
436.976643	16902.704391	30.338548
437.238814	16921.403165	30.343565
438.237368	16938.034623	30.348583
438.195892	16953.808781	30.353600
438.576800	16980.154854	30.358618
439.025268	17007.437953	30.363636
439.155534	17031.763964	30.368653
439.888413	17052.672789	30.373671
439.962313	17083.672303	30.378688
440.441280	17102.030912	30.383706
440.816293	17125.819649	30.388724
441.386111	17157.891334	30.393741
441.985819	17180.754220	30.398759
442.586391	17207.249396	30.403776
443.102349	17232.633395	30.408794
443.170263	17247.537834	30.413812
443.680296	17269.776832	30.418829
443.969408	17291.178679	30.423847
444.384766	17316.572229	30.428864
444.679408	17352.629303	30.433882
445.522402	17372.977945	30.438900
445.690462	17408.934923	30.443917
446.263296	17429.862909	30.448935
446.479963	17459.886754	30.453952
446.897380	17485.027511	30.458970
447.957492	17508.494625	30.463988
448.258852	17541.626083	30.469005
448.966873	17565.609579	30.474023
449.255378	17588.243731	30.479040
449.506320	17612.077770	30.484058
449.998525	17638.293596	30.489076
450.261290	17661.841564	30.494093
450.949922	17679.833063	30.499111
451.132979	17704.448568	30.504128
451.269100	17720.726194	30.509146
451.620102	17749.724984	30.514164
452.216951	17763.371938	30.519181
452.845075	17788.397961	30.524199
453.408582	17820.522274	30.529216
453.813344	17834.363618	30.534234
454.334620	17863.102163	30.539252
454.637691	17889.834397	30.544269
455.253480	17919.189966	30.549287
455.793733	17933.768253	30.554304
456.383022	17957.417056	30.559322
456.856950	17970.508521	30.564340
456.991142	18003.723811	30.569357
457.501436	18026.159482	30.574375
458.096377	18048.158648	30.579392
458.191122	18062.983702	30.584410
458.919082	18086.806786	30.589428
459.350372	18111.257577	30.594445
460.288802	18129.867392	30.599463
460.569840	18159.541094	30.604480
461.401172	18166.069663	30.609498
462.113759	18183.590385	30.614516
462.358454	18209.454066	30.619533
463.102233	18222.029620	30.624551
463.391828	18233.096934	30.629568
464.042831	18251.012733	30.634586
464.365788	18269.504287	30.639604
464.220339	18288.353516	30.644621
464.838497	18305.105759	30.649639
465.300521	18328.547518	30.654656
465.717696	18346.329455	30.659674
466.202728	18356.974538	30.664692
466.650049	18402.757695	30.669709
466.687862	18427.523219	30.674727
467.008805	18447.480945	30.679744
467.644164	18480.207908	30.684762
468.108398	18509.316452	30.689780
468.625238	18542.933919	30.694797
468.992205	18568.785245	30.699815
469.451076	18612.267459	30.704832
469.682824	18635.543490	30.709850
470.584953	18664.924836	30.714868
470.907842	18691.718247	30.719885
471.710570	18716.541228	30.724903
471.868002	18749.160288	30.729920
472.430318	18778.854057	30.734938
472.835607	18805.009263	30.739956
473.171337	18837.417330	30.744973
473.728314	18861.723027	30.749991
474.343675	18900.632594	30.755008
474.776336	18926.057133	30.760026
475.132066	18957.261890	30.765044
475.614921	18985.167852	30.770061
476.319421	19018.756748	30.775079
476.916128	19049.987089	30.780096
477.681090	19070.242341	30.785114
478.399814	19091.471485	30.790132
478.390399	19121.975558	30.795149
478.959181	19141.775139	30.800167
479.549230	19157.193141	30.805184
479.909092	19166.221952	30.810202
480.994713	19193.256708	30.815220
481.327685	19222.424786	30.820237
481.854537	19230.947315	30.825255
482.251877	19255.897660	30.830272
482.680386	19273.375412	30.835290
482.792663	19298.168287	30.840308
483.407915	19328.353718	30.845325
483.680325	19340.207775	30.850343
484.317964	19354.771880	30.855360
484.425589	19380.083656	30.860378
484.769753	19395.881527	30.865396
485.377080	19432.285199	30.870413
485.909305	19444.016493	30.875431
486.332218	19472.488521	30.880448
486.705457	19503.223882	30.885466
487.154607	19527.016590	30.890484
487.405180	19554.909206	30.895501
487.954697	19576.215925	30.900519
488.075847	19609.202231	30.905536
488.505680	19643.346983	30.910554
489.120227	19678.410566	30.915572
489.954705	19709.541543	30.920589
489.992763	19742.616904	30.925607
490.693311	19788.502651	30.930624
490.997390	19819.982236	30.935642
491.915538	19843.676601	30.940660
492.248995	19883.914852	30.945677
492.628061	19912.451251	30.950695
493.499364	19938.977256	30.955712
494.147030	19970.630721	30.960730
495.085176	19995.724760	30.965748
495.181164	20029.322253	30.970765
495.610134	20062.652834	30.975783
496.309022	20093.255982	30.980800
496.807499	20113.389789	30.985818
497.483682	20136.256820	30.990836
497.694318	20172.035322	30.995853
497.971299	20204.366405	31.000871
498.763535	20216.967260	31.005888
499.113227	20256.053822	31.010906
499.930742	20271.904628	31.015924
500.185052	20318.076328	31.020941
500.720928	20338.021280	31.025959
501.721476	20370.833223	31.030976
502.117853	20397.579557	31.035994
502.764418	20417.564118	31.041012
503.241127	20453.832194	31.046029
503.723597	20461.433431	31.051047
504.354242	20485.192561	31.056064
504.550349	20511.464955	31.061082
505.437111	20535.474673	31.066100
505.595724	20555.504209	31.071117
505.935835	20578.841403	31.076135
506.450072	20611.445594	31.081152
506.777474	20634.696389	31.086170
507.683119	20675.832306	31.091188
507.632861	20705.075254	31.096205
508.348710	20730.994849	31.101223
509.025051	20761.773169	31.106240
509.562555	20797.160424	31.111258
510.014680	20825.187558	31.116276
510.620436	20844.749297	31.121293
510.877332	20875.492396	31.126311
511.365619	20900.007261	31.131328
511.719450	20934.722187	31.136346
512.392443	20957.432718	31.141364
512.782940	20995.768787	31.146381
513.246298	21018.922922	31.151399
513.863390	21056.345355	31.156416
514.441836	21087.897734	31.161434
515.424489	21121.705739	31.166452
515.449221	21149.294796	31.171469
515.784839	21175.438812	31.176487
516.478190	21207.832703	31.181504
516.967597	21238.925383	31.186522
517.641717	21259.418287	31.191540
518.065420	21293.528962	31.196557
518.706481	21310.267569	31.201575
519.192816	21331.011109	31.206592
519.935605	21366.373555	31.211610
520.371971	21376.452926	31.216628
520.583784	21404.145728	31.221645
520.989876	21418.400120	31.226663
522.337162	21452.037850	31.231680
522.305301	21481.563404	31.236698
522.860578	21496.912879	31.241716
523.418163	21520.084439	31.246733
523.451068	21552.980411	31.251751
523.704465	21581.538919	31.256768
523.989209	21618.357336	31.261786
524.846913	21653.721256	31.266804
525.324162	21697.169528	31.271821
525.874707	21725.858627	31.276839
526.953436	21765.705983	31.281856
526.701033	21800.302548	31.286874
527.407384	21830.572346	31.291892
528.204477	21863.500795	31.296909
528.922826	21911.587629	31.301927
529.720388	21934.159723	31.306944
529.885773	21972.198055	31.311962
530.367316	21995.723296	31.316980
530.995042	22040.930647	31.321997
531.096167	22070.512076	31.327015
532.316559	22091.406837	31.332032
532.303250	22130.345452	31.337050
533.186155	22164.259335	31.342068
533.556754	22208.824909	31.347085
534.199937	22250.580238	31.352103
535.276839	22282.170201	31.357120
535.545164	22314.348130	31.362138
536.156450	22333.733557	31.367156
536.729492	22370.015348	31.372173
537.294572	22396.712699	31.377191
538.067902	22419.371290	31.382208
538.080094	22453.611608	31.387226
538.578612	22481.387392	31.392244
539.811961	22515.480792	31.397261
539.928847	22543.992561	31.402279
540.579479	22568.964314	31.407296
540.897313	22611.043074	31.412314
541.669490	22643.111029	31.417332
541.991412	22668.014329	31.422349
542.822237	22708.635416	31.427367
543.417639	22728.535556	31.432384
543.862665	22774.784236	31.437402
544.332480	22795.039020	31.442420
545.148280	22828.857130	31.447437
545.303505	22858.090033	31.452455
546.087656	22881.252982	31.457472
546.095088	22922.230951	31.462490
547.017262	22954.054751	31.467508
547.271296	22980.763690	31.472525
548.037404	23012.157053	31.477543
548.949069	23045.082165	31.482560
548.885040	23075.265995	31.487578
549.649591	23109.787712	31.492596
550.284640	23146.269743	31.497613
550.460384	23180.138144	31.502631
551.425857	23212.878172	31.507648
551.844589	23251.296338	31.512666
552.761933	23273.326713	31.517684
552.844989	23307.342550	31.522701
553.487163	23340.101826	31.527719
554.188644	23364.447338	31.532736
554.447295	23389.443601	31.537754
555.234936	23407.203702	31.542772
555.926984	23439.279175	31.547789
556.118306	23461.511937	31.552807
557.016199	23485.182275	31.557824
557.608765	23515.775794	31.562842
558.098443	23545.039475	31.567860
558.773754	23561.300686	31.572877
559.673766	23595.978972	31.577895
559.859034	23619.394562	31.582912
560.617859	23650.233979	31.587930
561.126412	23673.283036	31.592948
561.680959	23695.250635	31.597965
561.687917	23728.817799	31.602983
562.789010	23749.644535	31.608000
562.670572	23788.299531	31.613018
563.621384	23809.750203	31.618036
564.320920	23838.703397	31.623053
564.502992	23873.880090	31.628071
565.076033	23899.832532	31.633088
565.382090	23939.179660	31.638106
566.030696	23967.306860	31.643124
566.788949	24010.918407	31.648141
567.255820	24047.896066	31.653159
567.875799	24082.473711	31.658176
568.264750	24120.923496	31.663194
569.078715	24165.266028	31.668212
569.636280	24196.681283	31.673229
570.140863	24230.291423	31.678247
571.039712	24265.261752	31.683264
571.462021	24307.334052	31.688282
571.519741	24333.936521	31.693300
572.433006	24369.675755	31.698317
573.119218	24406.044649	31.703335
573.616747	24436.844052	31.708352
574.092070	24479.249665	31.713370
575.027928	24513.570040	31.718388
575.687533	24545.279521	31.723405
576.244031	24591.306409	31.728423
576.764368	24605.665275	31.733440
577.391722	24653.431734	31.738458
578.109636	24682.825647	31.743476
578.828519	24717.148756	31.748493
579.152823	24756.715820	31.753511
580.016503	24787.060280	31.758528
580.380190	24817.122873	31.763546
581.224128	24845.366070	31.768564
582.012789	24873.099750	31.773581
582.214082	24900.318772	31.778599
582.757532	24936.243331	31.783616
583.552819	24963.173499	31.788634
584.218414	24989.612118	31.793652
584.787685	25024.723870	31.798669
585.291103	25055.384269	31.803687
585.734745	25081.446988	31.808704
586.488215	25117.629689	31.813722
587.046437	25149.122174	31.818740
587.544343	25185.458778	31.823757
588.251191	25208.756620	31.828775
588.493603	25234.591943	31.833792
589.050052	25272.859710	31.838810
589.759009	25311.893641	31.843828
590.482026	25336.750093	31.848845
591.013033	25372.519387	31.853863
591.401509	25404.297970	31.858880
591.809263	25439.979250	31.863898
592.792459	25471.146570	31.868916
593.372848	25496.512187	31.873933
593.578414	25535.796027	31.878951
593.996981	25555.865725	31.883968
594.482815	25597.083915	31.888986
595.164905	25631.136275	31.894004
595.841366	25658.010147	31.899021
596.375405	25704.257981	31.904039
596.850583	25732.705541	31.909056
597.643718	25765.988665	31.914074
598.453113	25787.558413	31.919092
599.207112	25824.070941	31.924109
599.667449	25854.979466	31.929127
600.370715	25882.531999	31.934144
600.751296	25908.479267	31.939162
601.380677	25954.068103	31.944180
602.140405	25978.932241	31.949197
602.614470	26014.781115	31.954215
603.317706	26041.771387	31.959232
603.719405	26077.176663	31.964250
604.026100	26116.022351	31.969268
605.201799	26154.750977	31.974285
605.611870	26198.940057	31.979303
606.250592	26225.024267	31.984320
606.924453	26263.610493	31.989338
607.629219	26299.151977	31.994356
608.358927	26330.493052	31.999373
608.787990	26371.026501	32.004391
609.320699	26408.642849	32.009408
610.021025	26439.571565	32.014426
610.332322	26475.882840	32.019444
610.912717	26513.137984	32.024461
611.290817	26553.313209	32.029479
612.231382	26601.104760	32.034496
612.818325	26640.931441	32.039514
613.253690	26684.965936	32.044532
614.027280	26718.658189	32.049549
614.590939	26775.041516	32.054567
615.324651	26803.576501	32.059584
615.949504	26842.449599	32.064602
616.380846	26888.324369	32.069620
617.203854	26921.004293	32.074637
617.919573	26973.749141	32.079655
618.494348	27002.132328	32.084672
619.271754	27045.823303	32.089690
619.487203	27088.565842	32.094708
620.602244	27125.485567	32.099725
620.912104	27174.142012	32.104743
621.540739	27206.776994	32.109760
622.790471	27251.645880	32.114778
623.034248	27281.705643	32.119796
624.059471	27303.350662	32.124813
624.447751	27349.599803	32.129831
624.840902	27382.246665	32.134848
626.001042	27412.889962	32.139866
626.310764	27451.118329	32.144884
627.151615	27482.083515	32.149901
627.440309	27524.840782	32.154919
628.418291	27566.162882	32.159936
629.129279	27603.576552	32.164954
629.545258	27629.621611	32.169972
630.017048	27656.220491	32.174989
630.771270	27702.191905	32.180007
631.444456	27733.512402	32.185024
632.332406	27763.408787	32.190042
632.473704	27800.058761	32.195060
633.170690	27830.762584	32.200077
633.636137	27874.997206	32.205095
633.992668	27908.857883	32.210112
634.765153	27943.216010	32.215130
635.353018	27985.415420	32.220148
636.083151	28007.328629	32.225165
636.525578	28042.067287	32.230183
637.158108	28076.238975	32.235200
638.116555	28115.978765	32.240218
638.778123	28159.860935	32.245236
639.296004	28189.126948	32.250253
640.023514	28217.816590	32.255271
640.353345	28258.129158	32.260288
641.211355	28289.649112	32.265306
641.961863	28316.970014	32.270324
642.968860	28351.032953	32.275341
643.115383	28395.053177	32.280359
643.875247	28424.268989	32.285376
644.788955	28457.676713	32.290394
644.815639	28503.934536	32.295412
645.730504	28538.467314	32.300429
645.929937	28580.703504	32.305447
647.022123	28622.673551	32.310464
647.546226	28656.913759	32.315482
648.158802	28701.253547	32.320500
648.908851	28732.980720	32.325517
649.503366	28785.136117	32.330535
650.039540	28819.058662	32.335552
650.935834	28857.109308	32.340570
651.640736	28906.864745	32.345588
652.062765	28946.007499	32.350605
652.683000	28985.997899	32.355623
653.178835	29029.402217	32.360640
654.241905	29066.409459	32.365658
654.542221	29122.688817	32.370676
655.403363	29151.504228	32.375693
656.158508	29199.482627	32.380711
656.855811	29242.596682	32.385728
657.782370	29275.953165	32.390746
658.491497	29322.459935	32.395764
659.125286	29353.188588	32.400781
659.577339	29390.450133	32.405799
660.286577	29442.538667	32.410816
661.050646	29464.770504	32.415834
661.847789	29518.893501	32.420852
662.632661	29554.232172	32.425869
663.245924	29590.002331	32.430887
663.762755	29631.154309	32.435904
664.494678	29659.358557	32.440922
665.023365	29710.698544	32.445940
665.781571	29741.047987	32.450957
666.348024	29781.648873	32.455975
666.928173	29820.174338	32.460992
667.871062	29858.510323	32.466010
668.380032	29906.187580	32.471028
669.218258	29938.914209	32.476045
670.047662	29973.633467	32.481063
670.802368	30015.741399	32.486080
671.157017	30049.005387	32.491098
671.645345	30086.711323	32.496116
672.357218	30133.194212	32.501133
673.461976	30168.989549	32.506151
673.770414	30213.810082	32.511168
674.680937	30239.502876	32.516186
675.656016	30282.183688	32.521204
676.155287	30308.541501	32.526221
676.612815	30346.948085	32.531239
677.548176	30379.198744	32.536256
678.459553	30408.368374	32.541274
678.906640	30439.993920	32.546292
679.839667	30469.425744	32.551309
680.097760	30502.541229	32.556327
680.404572	30526.179644	32.561344
681.552384	30561.987888	32.566362
681.603650	30602.437179	32.571380
682.306113	30628.984831	32.576397
683.042000	30667.209347	32.581415
683.179916	30698.049273	32.586432
684.332981	30734.539713	32.591450
684.923927	30778.830475	32.596468
685.420016	30822.112102	32.601485
686.579660	30866.712248	32.606503
686.968948	30907.349417	32.611520
687.646143	30935.557663	32.616538
688.212222	30993.342965	32.621556
688.800091	31029.865545	32.626573
689.755887	31073.714185	32.631591
690.135959	31117.349643	32.636608
690.585184	31170.286104	32.641626
691.358745	31209.605684	32.646644
692.037522	31253.131432	32.651661
693.194642	31311.014709	32.656679
693.397570	31361.385704	32.661696
694.119052	31402.762031	32.666714
694.959414	31455.258664	32.671732
696.073156	31501.669053	32.676749
696.423085	31548.116979	32.681767
696.970090	31603.770222	32.686784
697.748329	31656.100082	32.691802
698.753949	31714.532917	32.696820
699.409396	31754.997306	32.701837
700.376223	31797.916448	32.706855
701.344746	31842.605523	32.711872
701.900867	31886.063301	32.716890
702.673917	31923.064201	32.721908
703.716602	31964.062608	32.726925
704.336628	31995.587584	32.731943
704.787841	32047.621941	32.736960
705.457591	32090.417519	32.741978
706.042791	32139.681097	32.746996
706.933704	32165.423613	32.752013
707.471931	32210.800413	32.757031
708.423254	32261.638004	32.762048
709.178637	32298.838319	32.767066
709.575722	32339.856385	32.772084
710.230060	32386.903352	32.777101
711.521287	32421.402670	32.782119
712.208049	32476.568531	32.787136
712.837012	32510.874574	32.792154
713.537268	32557.086549	32.797172
714.045144	32599.263674	32.802189
714.792505	32643.110338	32.807207
715.720622	32688.079405	32.812224
716.605268	32720.866388	32.817242
717.129337	32767.150673	32.822260
717.996562	32811.617453	32.827277
719.017630	32847.525362	32.832295
719.455595	32893.083722	32.837312
720.479057	32916.922414	32.842330
720.925047	32959.312266	32.847348
721.570254	32998.952471	32.852365
722.395456	33039.101951	32.857383
723.103788	33077.815704	32.862400
723.711644	33110.204090	32.867418
724.576473	33149.222223	32.872436
724.938497	33185.752343	32.877453
725.930104	33222.291412	32.882471
726.354698	33271.020130	32.887488
727.318604	33302.031705	32.892506
727.793314	33343.665488	32.897524
728.051342	33371.038596	32.902541
728.963740	33411.952777	32.907559
730.013270	33458.864403	32.912576
730.749211	33490.057369	32.917594
731.455211	33528.348725	32.922612
731.739952	33564.537557	32.927629
732.863055	33594.803889	32.932647
733.220111	33639.156327	32.937664
733.904552	33681.099343	32.942682
734.665656	33729.808041	32.947700
735.234837	33779.963126	32.952717
736.286281	33813.244140	32.957735
737.004146	33862.181201	32.962752
737.463322	33894.587760	32.967770
738.250627	33942.426674	32.972788
739.364323	33997.162980	32.977805
740.262080	34038.282996	32.982823
740.535510	34089.395570	32.987840
741.280965	34133.403715	32.992858
742.283127	34177.757426	32.997876
742.888851	34223.545303	33.002893
743.624110	34264.786047	33.007911
744.316245	34322.320557	33.012928
745.365665	34369.619913	33.017946
745.841226	34410.073350	33.022964
746.424700	34460.038139	33.027981
747.644938	34511.243727	33.032999
748.124760	34554.775895	33.038016
749.006730	34602.658388	33.043034
749.810559	34649.307661	33.048052
750.232933	34695.719606	33.053069
751.530297	34742.949359	33.058087
752.459219	34788.384362	33.063104
753.206205	34834.575065	33.068122
754.165092	34875.465848	33.073140
754.564439	34925.030625	33.078157
755.462080	34959.229048	33.083175
756.126805	35014.582063	33.088192
756.985037	35044.771833	33.093210
758.030223	35093.812243	33.098228
758.091066	35142.633864	33.103245
759.167673	35182.071528	33.108263
759.962857	35230.215625	33.113280
760.312883	35276.286094	33.118298
761.576515	35312.564901	33.123316
761.927209	35364.174287	33.128333
763.071582	35414.496099	33.133351
763.957763	35457.530210	33.138368
764.303896	35494.661173	33.143386
765.251954	35548.738245	33.148404
765.616422	35601.572701	33.153421
766.751784	35635.621179	33.158439
767.523259	35695.189317	33.163456
767.823064	35743.861086	33.168474
769.374322	35785.350073	33.173492
770.200905	35839.035913	33.178509
770.967985	35874.369114	33.183527
771.155333	35927.320637	33.188544
772.117948	35963.084948	33.193562
772.930476	36005.840845	33.198580
773.520073	36057.895058	33.203597
774.994657	36099.573714	33.208615
775.741074	36146.652602	33.213632
776.234378	36191.267271	33.218650
776.998025	36231.369241	33.223668
777.748195	36267.951402	33.228685
778.511262	36310.513317	33.233703
779.433740	36354.504684	33.238720
780.243116	36394.182470	33.243738
781.106048	36421.199229	33.248756
781.233909	36462.216886	33.253773
782.214206	36492.339020	33.258791
782.508094	36542.588022	33.263808
783.241784	36585.559773	33.268826
784.306987	36628.340587	33.273844
784.452082	36678.252782	33.278861
785.404781	36721.531969	33.283879
786.049421	36779.921580	33.288896
787.034116	36827.483170	33.293914
787.876494	36872.057247	33.298932
788.479832	36940.944169	33.303949
789.422081	36986.274294	33.308967
790.323409	37035.322745	33.313984
790.983540	37091.099226	33.319002
791.814566	37144.243847	33.324020
792.883316	37193.765994	33.329037
793.547152	37249.017462	33.334055
794.464289	37296.970083	33.339072
795.348079	37357.100710	33.344090
796.681674	37392.158012	33.349108
797.032335	37436.671150	33.354125
797.968246	37486.606833	33.359143
798.784278	37543.612134	33.364160
799.534494	37582.422423	33.369178
800.152548	37633.116458	33.374196
800.951385	37679.880663	33.379213
801.939495	37730.213448	33.384231
802.671552	37788.623738	33.389248
803.742809	37837.976246	33.394266
804.785847	37874.654419	33.399284
805.283483	37935.662884	33.404301
806.086758	37970.589176	33.409319
807.386784	38022.271330	33.414336
808.003262	38070.158936	33.419354
808.763125	38119.801153	33.424372
809.567141	38163.150805	33.429389
810.587686	38205.378959	33.434407
810.891804	38264.458306	33.439424
811.841622	38312.907657	33.444442
812.939049	38352.101306	33.449460
813.775512	38410.022653	33.454477
814.782886	38454.593158	33.459495
815.654672	38496.845178	33.464512
816.381153	38544.615433	33.469530
816.880774	38584.111802	33.474548
817.501296	38630.412739	33.479565
818.446936	38676.549035	33.484583
819.057621	38732.660037	33.489600
819.983175	38787.640495	33.494618
820.847265	38833.309281	33.499636
822.010076	38885.679008	33.504653
822.605428	38931.687308	33.509671
823.694394	38983.202456	33.514688
824.567232	39032.019619	33.519706
825.345164	39062.404724	33.524724
826.288024	39107.309204	33.529741
827.130996	39162.638719	33.534759
827.587400	39208.757902	33.539776
828.496642	39255.653695	33.544794
829.466892	39290.467446	33.549812
830.273846	39337.132794	33.554829
831.279757	39380.080160	33.559847
832.082891	39428.390561	33.564864
832.840157	39482.134322	33.569882
833.568658	39515.689852	33.574900
834.375476	39561.805510	33.579917
834.906678	39597.921708	33.584935
836.185094	39634.388949	33.589952
837.096287	39663.723199	33.594970
837.855824	39700.082076	33.599988
838.218914	39734.922052	33.605005
839.145493	39788.039264	33.610023
839.793153	39833.459465	33.615040
840.828340	39869.914596	33.620058
841.565214	39909.546988	33.625076
842.165790	39955.537673	33.630093
843.050823	40002.464171	33.635111
844.148885	40054.486386	33.640128
845.253360	40098.418977	33.645146
845.867783	40143.364386	33.650164
846.288195	40189.415399	33.655181
847.256883	40236.980707	33.660199
848.484482	40289.786390	33.665216
848.669642	40339.985371	33.670234
849.822861	40395.130315	33.675252
850.725406	40462.931780	33.680269
851.489606	40510.257758	33.685287
852.305974	40567.055954	33.690304
852.627855	40616.519505	33.695322
854.274820	40666.800236	33.700340
854.573575	40729.454118	33.705357
855.539390	40785.426276	33.710375
856.762581	40837.278983	33.715392
857.604767	40888.438858	33.720410
858.475840	40944.533776	33.725428
859.486699	41004.079119	33.730445
859.929374	41064.934231	33.735463
861.314286	41116.787578	33.740480
862.043373	41170.862475	33.745498
863.160856	41212.606973	33.750516
863.953126	41271.750876	33.755533
864.742434	41320.504041	33.760551
865.411267	41384.309852	33.765568
866.218412	41441.636712	33.770586
867.474489	41485.832972	33.775604
868.081184	41542.084665	33.780621
869.263040	41599.030704	33.785639
870.444020	41645.718332	33.790656
871.098559	41696.922130	33.795674
872.110075	41739.398922	33.800692
872.733463	41800.088634	33.805709
873.740293	41843.793366	33.810727
874.571717	41905.462759	33.815744
875.361660	41962.913846	33.820762
876.161007	42007.574816	33.825780
876.861111	42055.306312	33.830797
877.973468	42117.356074	33.835815
879.120765	42165.371978	33.840832
879.845591	42227.678803	33.845850
881.005976	42270.158612	33.850868
881.571025	42318.734064	33.855885
882.528729	42370.157607	33.860903
883.510983	42419.736867	33.865920
884.214255	42488.676345	33.870938
885.178856	42531.914688	33.875956
885.734997	42582.010108	33.880973
886.740666	42635.476056	33.885991
887.367468	42684.282994	33.891008
888.258070	42739.392741	33.896026
889.575070	42796.902628	33.901044
890.145385	42848.742148	33.906061
891.603273	42899.405500	33.911079
892.406833	42941.360572	33.916096
893.193877	42994.880599	33.921114
893.992543	43030.315423	33.926132
894.899506	43075.961078	33.931149
895.597126	43118.919795	33.936167
896.795214	43160.067141	33.941184
897.513505	43207.659131	33.946202
898.521177	43242.637784	33.951220
898.976211	43284.546878	33.956237
899.888360	43338.769221	33.961255
900.787961	43385.017561	33.966272
901.922596	43441.880887	33.971290
902.796735	43483.231365	33.976308
903.601683	43542.265528	33.981325
904.330470	43591.684702	33.986343
905.531245	43647.753866	33.991360
906.097447	43700.614398	33.996378
907.241122	43746.762024	34.001396
907.894513	43794.934718	34.006413
908.509661	43859.458207	34.011431
909.980950	43915.814611	34.016448
910.569270	43970.000649	34.021466
911.641421	44028.228895	34.026484
912.522483	44082.027796	34.031501
913.070902	44139.136510	34.036519
914.165411	44196.495112	34.041536
915.208368	44259.023513	34.046554
916.060040	44311.062766	34.051572
917.162139	44376.472982	34.056589
918.192236	44435.113710	34.061607
919.266171	44498.023789	34.066624
920.074883	44553.966865	34.071642
921.135873	44605.411057	34.076660
922.337309	44666.815142	34.081677
923.041934	44715.728226	34.086695
924.525671	44770.180845	34.091712
925.153270	44822.800381	34.096730
926.109487	44870.333378	34.101748
926.955910	44930.819629	34.106765
927.802403	44987.308208	34.111783
928.686606	45041.849040	34.116800
929.660450	45097.122401	34.121818
930.748499	45158.570896	34.126836
931.756474	45208.329488	34.131853
932.542686	45256.965302	34.136871
933.522084	45299.453963	34.141888
934.278898	45362.220033	34.146906
935.356587	45429.832204	34.151924
936.730973	45484.063308	34.156941
937.435663	45538.538572	34.161959
938.081976	45580.883820	34.166976
939.083470	45660.008993	34.171994
940.107215	45700.656973	34.177012
940.804966	45757.436472	34.182029
941.500826	45808.978562	34.187047
942.883447	45867.023825	34.192064
943.860678	45921.254914	34.197082
944.736933	45985.395733	34.202100
945.803916	46037.158580	34.207117
946.497334	46088.467633	34.212135
947.878060	46146.077423	34.217152
948.617920	46197.322519	34.222170
949.606052	46253.014012	34.227188
950.437277	46308.445538	34.232205
951.394550	46367.007842	34.237223
952.825262	46411.939394	34.242240
953.242572	46471.984578	34.247258
954.589426	46521.383045	34.252276
955.421923	46567.439728	34.257293
956.125728	46626.402983	34.262311
957.436455	46661.301598	34.267328
958.351717	46711.147628	34.272346
958.960244	46753.153062	34.277364
959.822536	46789.071015	34.282381
960.489074	46857.719763	34.287399
961.697004	46892.881556	34.292416
962.352199	46944.268131	34.297434
962.946975	46995.752851	34.302452
964.144870	47051.445105	34.307469
964.772725	47115.849453	34.312487
965.986813	47170.546241	34.317504
967.134195	47237.494999	34.322522
968.055544	47297.172446	34.327540
968.988952	47352.938487	34.332557
969.916586	47418.112854	34.337575
971.153171	47470.421811	34.342592
971.989177	47528.942853	34.347610
972.627760	47592.998926	34.352628
973.878268	47651.442731	34.357645
974.661523	47724.390448	34.362663
975.899837	47778.028397	34.367680
976.760291	47846.567534	34.372698
977.303287	47913.182718	34.377716
978.691785	47981.475097	34.382733
980.025249	48044.689769	34.387751
981.183782	48097.670353	34.392768
982.158021	48170.311230	34.397786
983.233075	48229.555837	34.402804
984.205717	48283.065759	34.407821
985.312188	48341.812265	34.412839
986.163932	48399.921857	34.417856
987.615612	48460.588527	34.422874
988.235254	48531.691762	34.427892
989.301953	48588.806527	34.432909
990.017421	48646.615424	34.437927
991.412092	48698.877154	34.442944
992.609659	48758.160895	34.447962
993.377401	48813.728697	34.452980
994.909804	48871.638019	34.457997
995.640474	48930.027315	34.463015
997.023208	48977.881794	34.468032
998.246474	49036.548537	34.473050
998.769581	49083.759634	34.478068
999.621544	49129.090887	34.483085
1001.214028	49190.281561	34.488103
1002.323969	49234.547683	34.493120
1002.572944	49282.940946	34.498138
1003.389016	49333.042356	34.503156
1005.019444	49393.190025	34.508173
1005.509134	49456.129474	34.513191
1006.820517	49501.130129	34.518208
1007.850614	49554.722614	34.523226
1009.004288	49613.458676	34.528244
1010.078683	49665.298243	34.533261
1011.004431	49726.480858	34.538279
1012.192529	49767.123062	34.543296
1013.202977	49821.820147	34.548314
1013.789136	49883.125946	34.553332
1014.983570	49923.166366	34.558349
1015.897462	49980.169337	34.563367
1017.137524	50029.984439	34.568384
1017.854550	50086.176995	34.573402
1018.800905	50147.053803	34.578420
1020.076403	50183.197142	34.583437
1021.152301	50247.198512	34.588455
1022.317359	50294.931651	34.593472
1023.072187	50351.207515	34.598490
1023.762147	50390.226809	34.603508
1024.478015	50439.757896	34.608525
1025.298978	50494.448285	34.613543
1026.416536	50542.239992	34.618560
1027.417545	50590.176591	34.623578
1028.346892	50640.889514	34.628596
1029.604348	50703.788095	34.633613
1030.445214	50764.278106	34.638631
1031.367488	50806.817662	34.643648
1032.418741	50866.933329	34.648666
1033.016046	50923.260561	34.653684
1034.531264	50986.511849	34.658701
1035.292974	51042.016385	34.663719
1036.260899	51108.498390	34.668736
1037.546259	51166.414222	34.673754
1038.430589	51231.606227	34.678772
1040.026831	51291.511124	34.683789
1040.910244	51354.261233	34.688807
1042.280119	51413.436268	34.693824
1043.099438	51474.146642	34.698842
1043.768018	51540.594496	34.703860
1045.223996	51596.111884	34.708877
1046.256959	51663.300306	34.713895
1047.012662	51723.603676	34.718912
1048.403798	51787.629559	34.723930
1049.160611	51859.917502	34.728948
1050.247208	51920.903577	34.733965
1051.593781	51986.835264	34.738983
1052.700673	52053.684204	34.744000
1053.713800	52103.020445	34.749018
1054.856932	52176.944697	34.754036
1056.040977	52238.270696	34.759053
1056.969971	52297.706843	34.764071
1058.122555	52351.476474	34.769088
1059.120984	52416.938687	34.774106
1059.872953	52486.103435	34.779124
1061.698374	52543.273738	34.784141
1062.467268	52610.423977	34.789159
1063.461344	52667.870283	34.794176
1064.924709	52731.697623	34.799194
1065.842849	52803.039372	34.804212
1067.197258	52858.676924	34.809229
1068.008962	52920.645175	34.814247
1069.225585	52977.595467	34.819264
1069.950383	53026.377656	34.824282
1070.811550	53095.204387	34.829300
1072.262612	53157.092149	34.834317
1073.209653	53219.286791	34.839335
1074.719901	53280.210093	34.844352
1075.854407	53330.365218	34.849370
1076.579626	53389.532303	34.854388
1077.677270	53451.520471	34.859405
1078.954016	53512.601168	34.864423
1079.893553	53570.950482	34.869440
1080.764230	53633.316379	34.874458
1081.813641	53697.230148	34.879476
1083.161649	53751.276152	34.884493
1084.190752	53816.705839	34.889511
1085.424553	53880.781083	34.894528
1086.965954	53938.923176	34.899546
1087.231873	53990.209217	34.904564
1088.473248	54058.523620	34.909581
1089.478045	54111.567383	34.914599
1090.641293	54175.357051	34.919616
1091.841694	54234.508821	34.924634
1092.794563	54302.008462	34.929652
1093.937283	54356.157608	34.934669
1095.149863	54411.200884	34.939687
1095.949156	54459.961731	34.944704
1096.859516	54510.186110	34.949722
1097.911139	54565.982699	34.954740
1099.358352	54611.465613	34.959757
1100.494248	54668.160528	34.964775
1101.229764	54716.811653	34.969792
1102.562206	54772.590080	34.974810
1103.703554	54831.315937	34.979828
1104.676094	54887.113010	34.984845
1105.782065	54940.509845	34.989863
1106.853847	54987.045821	34.994880
1108.083264	55038.676909	34.999898
1109.076745	55114.988019	35.004916
1110.415971	55157.305684	35.009933
1111.556665	55220.443548	35.014951
1112.540469	55269.702443	35.019968
1114.210098	55328.543011	35.024986
1114.830605	55392.307024	35.030004
1115.950621	55440.519728	35.035021
1117.278982	55497.781383	35.040039
1117.813604	55554.445986	35.045056
1119.533114	55613.811054	35.050074
1120.794804	55678.893057	35.055092
1121.585668	55746.017150	35.060109
1122.873003	55799.830532	35.065127
1123.861416	55863.639469	35.070144
1125.108571	55904.093274	35.075162
1126.259072	55976.174012	35.080180
1127.789524	56035.791239	35.085197
1128.789949	56094.978969	35.090215
1129.542128	56150.946416	35.095232
1130.935720	56211.250026	35.100250
1131.753622	56279.858644	35.105268
1133.139153	56339.113265	35.110285
1134.322050	56394.235413	35.115303
1135.243036	56459.695659	35.120320
1136.588442	56525.709863	35.125338
1137.748881	56589.664691	35.130356
1138.995891	56646.068467	35.135373
1139.953514	56717.004472	35.140391
1141.015154	56773.880592	35.145408
1142.323955	56825.876542	35.150426
1143.717044	56905.004151	35.155444
1144.862981	56957.620803	35.160461
1146.134967	57008.895087	35.165479
1147.155704	57071.518679	35.170496
1148.756499	57133.140249	35.175514
1149.877473	57188.001778	35.180532
1151.092891	57246.671370	35.185549
1152.503912	57295.652386	35.190567
1153.039883	57363.580410	35.195584
1154.561179	57406.234331	35.200602
1155.542751	57466.846118	35.205620
1156.785499	57516.948860	35.210637
1157.981645	57576.400755	35.215655
1159.236406	57645.520841	35.220672
1160.060937	57683.910917	35.225690
1161.401295	57745.309012	35.230708
1162.298267	57801.422207	35.235725
1163.611490	57854.755152	35.240743
1164.288335	57914.991720	35.245760
1165.671445	57976.111556	35.250778
1166.742849	58034.387892	35.255796
1167.859131	58097.980231	35.260813
1169.206177	58159.447957	35.265831
1170.040970	58214.818668	35.270848
1171.335632	58273.547984	35.275866
1172.323440	58336.053440	35.280884
1173.588591	58377.268132	35.285901
1174.939389	58429.159714	35.290919
1175.704367	58478.820252	35.295936
1177.437693	58531.791450	35.300954
1177.938269	58589.785060	35.305972
1179.256956	58648.315317	35.310989
1180.476603	58706.639692	35.316007
1181.502915	58761.057581	35.321024
1182.537482	58808.872710	35.326042
1183.394892	58867.735218	35.331060
1184.546864	58938.862547	35.336077
1185.553731	59001.670553	35.341095
1186.808698	59084.073967	35.346112
1188.427853	59138.450530	35.351130
1189.518474	59202.853641	35.356148
1190.711923	59272.836141	35.361165
1192.240384	59336.158335	35.366183
1192.969401	59389.908936	35.371200
1194.260839	59458.401840	35.376218
1195.497367	59531.764675	35.381236
1196.532713	59602.690669	35.386253
1198.324216	59669.169016	35.391271
1199.074984	59741.842641	35.396288
1200.626463	59804.004123	35.401306
1201.866389	59874.525431	35.406324
1203.101413	59929.052518	35.411341
1204.573313	59994.695628	35.416359
1205.635012	60070.233233	35.421376
1206.751653	60134.419524	35.426394
1208.334437	60194.323705	35.431412
1209.524886	60267.525064	35.436429
1211.045047	60319.349870	35.441447
1212.007444	60391.352987	35.446464
1213.489389	60446.076779	35.451482
1214.515166	60512.670972	35.456500
1215.917916	60580.833111	35.461517
1217.049499	60637.194651	35.466535
1218.273444	60710.632629	35.471552
1219.490275	60766.905163	35.476570
1220.556511	60834.392747	35.481588
1221.996004	60890.681348	35.486605
1223.671724	60947.819295	35.491623
1224.391528	61016.792188	35.496640
1225.789440	61075.410832	35.501658
1226.925645	61133.830044	35.506676
1228.432799	61191.716571	35.511693
1229.813820	61254.914908	35.516711
1230.633398	61314.137392	35.521728
1231.891920	61377.969239	35.526746
1233.210080	61441.298167	35.531764
1234.357580	61503.463912	35.536781
1235.755830	61566.710994	35.541799
1236.912121	61632.407904	35.546816
1238.016250	61689.276240	35.551834
1239.599261	61758.698457	35.556852
1240.540754	61817.719492	35.561869
1241.762132	61884.970447	35.566887
1242.453669	61946.930159	35.571904
1244.119917	62010.883396	35.576922
1245.644246	62079.005340	35.581940
1246.756530	62143.330503	35.586957
1247.950143	62205.085660	35.591975
1248.993001	62275.321874	35.596992
1250.521115	62339.823004	35.602010
1251.663959	62406.340692	35.607028
1253.272480	62465.847579	35.612045
1254.638386	62526.924541	35.617063
1255.604756	62574.206964	35.622080
1256.958607	62626.721039	35.627098
1258.319905	62674.258350	35.632116
1259.299415	62724.558613	35.637133
1260.353050	62766.478528	35.642151
1261.346431	62839.408195	35.647168
1262.279210	62891.539284	35.652186
1263.757638	62942.869721	35.657204
1265.078861	63005.239947	35.662221
1266.060185	63068.334573	35.667239
1267.181965	63125.089499	35.672256
1268.305826	63194.910483	35.677274
1269.709697	63263.757235	35.682292
1270.756134	63331.375023	35.687309
1272.472250	63400.223919	35.692327
1273.970234	63472.418067	35.697344
1275.427377	63531.204196	35.702362
1276.431909	63593.175997	35.707380
1277.431730	63668.886242	35.712397
1279.194059	63729.347007	35.717415
1280.073515	63799.207943	35.722432
1281.592632	63866.696213	35.727450
1282.833856	63932.645482	35.732468
1283.883182	64006.677686	35.737485
1285.736053	64074.253547	35.742503
1287.209628	64153.721218	35.747520
1288.390529	64211.697536	35.752538
1289.812367	64274.599639	35.757556
1290.912361	64341.198846	35.762573
1292.398016	64404.762355	35.767591
1294.006307	64480.892607	35.772608
1295.197978	64542.375311	35.777626
1296.303090	64602.675175	35.782644
1297.478458	64676.563010	35.787661
1298.864947	64739.706058	35.792679
1300.514880	64810.563450	35.797696
1301.535946	64872.440865	35.802714
1302.872067	64943.835242	35.807732
1303.996031	65018.599475	35.812749
1305.440409	65085.286028	35.817767
1306.303559	65152.272667	35.822784
1308.130964	65218.260179	35.827802
1309.805687	65281.017591	35.832820
1310.655957	65351.849741	35.837837
1312.056288	65419.778639	35.842855
1313.363972	65499.979290	35.847872
1314.647028	65554.555563	35.852890
1316.323090	65639.713261	35.857908
1317.695109	65702.791349	35.862925
1319.207727	65765.784274	35.867943
1320.885515	65839.818465	35.872960
1322.077977	65892.301355	35.877978
1323.278192	65948.664192	35.882996
1324.632753	66020.495586	35.888013
1326.224468	66073.486169	35.893031
1327.272153	66144.384604	35.898048
1328.685170	66199.663695	35.903066
1330.288873	66257.154345	35.908084
1330.639096	66318.766768	35.913101
1332.024710	66378.102594	35.918119
1333.688998	66456.540992	35.923136
1335.050764	66523.579838	35.928154
1336.391934	66579.307870	35.933172
1337.763256	66652.670631	35.938189
1339.083022	66712.498734	35.943207
1340.657770	66780.283685	35.948224
1341.601612	66844.197746	35.953242
1342.888698	66902.277596	35.958260
1344.169128	66971.964253	35.963277
1345.981472	67014.101739	35.968295
1346.733011	67081.661790	35.973312
1347.870128	67132.781969	35.978330
1348.851170	67184.794105	35.983348
1350.564853	67243.947637	35.988365
1351.481820	67296.267613	35.993383
1352.615659	67367.345919	35.998400
1353.890552	67419.819064	36.003418
1355.138874	67481.534314	36.008436
1356.346964	67561.301189	36.013453
1358.053299	67638.723586	36.018471
1359.445121	67714.017350	36.023488
1360.771576	67786.592605	36.028506
1362.351958	67863.262930	36.033524
1363.787043	67936.049547	36.038541
1365.050286	68007.229677	36.043559
1366.362313	68079.459774	36.048576
1367.770654	68155.417085	36.053594
1369.507297	68220.217242	36.058612
1370.259510	68307.712953	36.063629
1372.043475	68377.375275	36.068647
1373.734900	68440.543119	36.073664
1374.977101	68517.337985	36.078682
1376.809807	68583.903282	36.083700
1377.899134	68659.044548	36.088717
1379.103115	68726.645753	36.093735
1380.823281	68800.916192	36.098752
1382.183450	68876.541249	36.103770
1383.783961	68944.302574	36.108788
1385.188279	69016.071284	36.113805
1387.025538	69081.041491	36.118823
1387.923620	69157.695837	36.123840
1389.642900	69220.975215	36.128858
1390.966217	69286.887546	36.133876
1392.544621	69360.681555	36.138893
1394.151596	69431.184941	36.143911
1395.069410	69497.724840	36.148928
1396.314713	69568.589154	36.153946
1398.120480	69628.708921	36.158964
1399.458258	69715.338886	36.163981
1400.763010	69773.295824	36.168999
1402.227091	69846.792504	36.174016
1403.364734	69919.897234	36.179034
1405.185169	69988.279091	36.184052
1406.284140	70062.105817	36.189069
1407.780332	70135.199355	36.194087
1409.043911	70203.263677	36.199104
1410.676591	70282.921850	36.204122
1412.485818	70344.999422	36.209140
1413.688274	70415.644791	36.214157
1415.063861	70478.981040	36.219175
1416.573661	70553.416084	36.224192
1417.687960	70619.111222	36.229210
1419.202347	70693.457294	36.234228
1420.316111	70768.866809	36.239245
1421.784311	70840.877533	36.244263
1423.050844	70920.873594	36.249280
1424.568909	71003.452178	36.254298
1426.681223	71072.918382	36.259316
1427.595246	71142.610330	36.264333
1429.106066	71214.767393	36.269351
1430.537801	71284.036726	36.274368
1431.930824	71361.835939	36.279386
1433.564374	71416.015184	36.284404
1434.859322	71488.434764	36.289421
1436.508596	71566.346457	36.294439
1437.869601	71632.892092	36.299456
1439.393294	71690.230088	36.304474
1440.601410	71743.425382	36.309492
1442.108643	71811.329101	36.314509
1443.253447	71864.116594	36.319527
1444.970310	71915.535445	36.324544
1445.946639	71982.686790	36.329562
1447.089203	72030.953407	36.334580
1448.875172	72110.491829	36.339597
1449.983776	72180.194070	36.344615
1451.230552	72247.949702	36.349632
1452.528682	72323.284164	36.354650
1454.204302	72381.106512	36.359668
1455.577087	72463.965742	36.364685
1457.077472	72539.332492	36.369703
1458.265902	72618.763325	36.374720
1459.660440	72704.697680	36.379738
1461.421009	72776.680616	36.384756
1463.168384	72847.943859	36.389773
1464.388934	72925.673362	36.394791
1466.112128	73002.273146	36.399808
1467.261054	73084.143417	36.404826
1468.758647	73171.304420	36.409844
1470.399649	73247.373139	36.414861
1472.079554	73329.237052	36.419879
1473.844598	73400.245695	36.424896
1475.031046	73482.985284	36.429914
1476.589379	73559.929137	36.434932
1477.863065	73651.749923	36.439949
1479.744287	73735.204855	36.444967
1481.166776	73807.332170	36.449984
1482.607050	73892.591896	36.455002
1484.526713	73972.064321	36.460020
1485.888455	74045.126434	36.465037
1487.367831	74126.783526	36.470055
1489.223568	74196.336124	36.475072
1490.348735	74278.606446	36.480090
1491.814229	74352.337154	36.485108
1493.245417	74428.353422	36.490125
1495.085305	74503.431939	36.495143
1497.280134	74579.987780	36.500160
1498.594237	74657.163026	36.505178
1499.994937	74728.764239	36.510196
1501.789992	74800.569922	36.515213
1502.928720	74872.237855	36.520231
1504.845153	74934.866797	36.525248
1506.384317	75010.551148	36.530266
1507.803320	75071.079563	36.535284
1509.300524	75142.400771	36.540301
1510.858166	75201.451083	36.545319
1512.337266	75278.868299	36.550336
1513.617509	75355.024824	36.555354
1515.418270	75429.884055	36.560372
1516.815305	75501.728577	36.565389
1518.065342	75575.015019	36.570407
1519.953112	75638.384785	36.575424
1521.182192	75709.673460	36.580442
1523.005069	75785.252249	36.585460
1524.584322	75852.572317	36.590477
1525.847983	75924.134827	36.595495
1527.500127	75994.382655	36.600512
1528.664125	76069.672678	36.605530
1530.803164	76137.032515	36.610548
1531.740576	76211.775697	36.615565
1533.427475	76285.869746	36.620583
1534.911468	76355.992822	36.625600
1536.360397	76439.384485	36.630618
1537.391631	76506.234583	36.635636
1539.145082	76586.082783	36.640653
1540.860758	76653.598843	36.645671
1542.226082	76712.517886	36.650688
1543.481127	76782.145856	36.655706
1545.118831	76841.491253	36.660724
1546.800756	76904.212150	36.665741
1547.657135	76975.258462	36.670759
1549.305813	77035.565318	36.675776
1550.691489	77113.369773	36.680794
1552.222950	77180.181239	36.685812
1553.688370	77262.736766	36.690829
1555.075072	77341.567814	36.695847
1556.816882	77417.429871	36.700864
1558.214133	77494.600202	36.705882
1559.979856	77579.579953	36.710900
1561.720207	77661.460253	36.715917
1563.095053	77752.911785	36.720935
1565.266897	77828.238956	36.725952
1566.365595	77904.418380	36.730970
1567.927859	77983.135123	36.735988
1569.866408	78058.816150	36.741005
1571.390060	78141.111850	36.746023
1573.114440	78217.206884	36.751040
1574.340545	78303.730202	36.756058
1576.668208	78377.995691	36.761076
1578.296003	78456.412163	36.766093
1579.665326	78539.315960	36.771111
1581.539676	78608.712302	36.776128
1582.693822	78696.590985	36.781146
1584.533961	78779.295131	36.786164
1586.141794	78855.954927	36.791181
1587.662959	78941.749963	36.796199
1589.651538	79013.017084	36.801216
1591.021411	79088.941978	36.806234
1592.881448	79163.903550	36.811252
1594.691187	79244.232115	36.816269
1595.703404	79335.504955	36.821287
1597.917375	79413.072275	36.826304
1599.554870	79487.524792	36.831322
1601.207006	79564.192290	36.836340
1602.963280	79626.160313	36.841357
1604.095489	79699.970349	36.846375
1606.085306	79781.589873	36.851392
1607.429933	79857.368799	36.856410
1609.096919	79935.935369	36.861428
1610.777810	80016.032957	36.866445
1612.367693	80099.274319	36.871463
1614.336424	80168.482442	36.876480
1615.871795	80248.286744	36.881498
1617.304315	80329.044902	36.886516
1619.084219	80402.235992	36.891533
1620.632571	80474.690681	36.896551
1622.601793	80538.768544	36.901568
1624.010270	80625.029855	36.906586
1625.380974	80696.752756	36.911604
1627.176121	80764.608555	36.916621
1628.758821	80841.353791	36.921639
1630.070163	80924.083750	36.926656
1631.687914	81005.359668	36.931674
1633.540411	81086.244333	36.936692
1635.031101	81167.755994	36.941709
1636.453694	81244.502055	36.946727
1638.407951	81328.044809	36.951744
1639.879365	81414.552098	36.956762
1641.523247	81488.996298	36.961780
1643.527813	81573.342780	36.966797
1644.871684	81648.556540	36.971815
1646.422683	81720.000446	36.976832
1647.889499	81799.009025	36.981850
1649.347109	81885.241184	36.986868
1651.239528	81949.562363	36.991885
1652.610484	82024.608178	36.996903
1654.389086	82085.944669	37.001920
1655.792394	82166.180549	37.006938
1657.174412	82232.102673	37.011956
1658.794284	82300.090982	37.016973
1660.367342	82377.652821	37.021991
1661.933308	82439.238755	37.027008
1663.934053	82528.618801	37.032026
1664.788504	82612.312151	37.037044
1666.373923	82699.312356	37.042061
1668.124363	82788.326943	37.047079
1670.110334	82875.036933	37.052096
1671.687343	82964.712740	37.057114
1673.089913	83050.120812	37.062132
1674.736572	83135.085482	37.067149
1676.241395	83239.838790	37.072167
1678.605692	83326.871072	37.077184
1680.356614	83431.523218	37.082202
1681.746489	83524.334404	37.087220
1683.639495	83606.639081	37.092237
1685.334999	83713.974475	37.097255
1687.776000	83800.476698	37.102272
1689.156976	83890.490202	37.107290
1691.174298	83988.235058	37.112308
1692.919926	84054.966136	37.117325
1694.406706	84155.113385	37.122343
1696.330702	84250.288851	37.127360
1697.955842	84337.275173	37.132378
1699.472188	84418.906213	37.137396
1701.410235	84521.011503	37.142413
1703.020709	84610.674574	37.147431
1705.068549	84689.929712	37.152448
1706.821289	84781.066262	37.157466
1708.571992	84868.110570	37.162484
1710.546526	84950.469712	37.167501
1712.036863	85037.732680	37.172519
1714.092525	85125.249570	37.177536
1715.766488	85212.788447	37.182554
1717.726389	85296.088560	37.187572
1719.377544	85379.703335	37.192589
1720.544402	85461.037222	37.197607
1722.399428	85554.909953	37.202624
1724.535299	85635.775893	37.207642
1725.810212	85727.078913	37.212660
1728.114425	85809.933802	37.217677
1730.124242	85900.615489	37.222695
1731.969927	85978.410537	37.227712
1733.276396	86069.240838	37.232730
1734.926216	86145.001469	37.237748
1736.838692	86228.197643	37.242765
1738.208950	86317.041912	37.247783
1740.313173	86407.621707	37.252800
1741.545347	86491.862830	37.257818
1743.281675	86582.386694	37.262836
1744.846716	86667.830772	37.267853
1746.640729	86756.496017	37.272871
1748.802233	86844.850578	37.277888
1750.321427	86938.818356	37.282906
1752.200772	87019.550887	37.287924
1754.179939	87109.037272	37.292941
1755.727781	87191.520250	37.297959
1757.381943	87282.261901	37.302976
1759.312771	87362.835256	37.307994
1760.806873	87462.283137	37.313012
1762.621030	87545.029573	37.318029
1764.516469	87630.475451	37.323047
1766.412959	87713.855780	37.328064
1768.186279	87796.406555	37.333082
1769.472916	87866.120284	37.338100
1771.249161	87926.912023	37.343117
1772.704227	88003.658406	37.348135
1774.667860	88074.571975	37.353152
1776.215905	88159.554174	37.358170
1777.470255	88243.898246	37.363188
1779.206238	88310.285794	37.368205
1780.677478	88416.495107	37.373223
1782.302291	88518.891561	37.378240
1784.069045	88592.422466	37.383258
1785.630162	88700.595718	37.388276
1787.747305	88790.496515	37.393293
1789.591526	88897.739070	37.398311
1791.153241	88990.997055	37.403328
1793.226932	89093.705445	37.408346
1795.108890	89208.851286	37.413364
1796.925649	89303.413703	37.418381
1798.783246	89405.650058	37.423399
1800.392117	89503.984274	37.428416
1802.367563	89602.299469	37.433434
1804.309425	89718.198310	37.438452
1806.265462	89802.766518	37.443469
1808.634150	89910.843144	37.448487
1810.832037	89999.835147	37.453504
1812.867373	90095.950071	37.458522
1814.265054	90203.495334	37.463540
1816.230784	90289.153337	37.468557
1818.137802	90382.234903	37.473575
1819.436019	90488.985636	37.478592
1821.933379	90586.005715	37.483610
1823.563516	90672.819953	37.488628
1825.446913	90767.972251	37.493645
1827.443964	90878.379155	37.498663
1829.452691	90974.969999	37.503680
1831.312446	91056.236234	37.508698
1832.845433	91154.524375	37.513716
1835.100063	91240.608826	37.518733
1836.638996	91332.673640	37.523751
1838.821352	91431.330008	37.528768
1840.563061	91530.917501	37.533786
1842.305412	91637.019787	37.538804
1844.149572	91721.661608	37.543821
1845.895558	91826.597955	37.548839
1847.620670	91922.817962	37.553856
1849.733447	92017.583425	37.558874
1851.487357	92119.287570	37.563892
1853.397393	92211.753266	37.568909
1854.966564	92316.566883	37.573927
1856.764089	92417.023094	37.578944
1858.778107	92518.294960	37.583962
1860.420569	92616.456639	37.588980
1862.532249	92719.729163	37.593997
1864.197889	92822.526821	37.599015
1865.942903	92930.192198	37.604032
1868.033527	93032.962086	37.609050
1869.940670	93136.711647	37.614068
1871.921207	93238.738960	37.619085
1873.523060	93345.819806	37.624103
1875.428629	93449.798823	37.629120
1877.510488	93542.241665	37.634138
1879.231665	93650.331580	37.639156
1880.660471	93754.411583	37.644173
1882.413106	93860.938275	37.649191
1884.736790	93970.177200	37.654208
1886.693814	94075.062897	37.659226
1888.671144	94183.837092	37.664244
1890.454131	94273.400904	37.669261
1892.001898	94370.670389	37.674279
1893.718121	94463.452072	37.679296
1895.767659	94544.507781	37.684314
1897.559335	94647.900243	37.689332
1899.776222	94723.289639	37.694349
1900.809169	94816.420135	37.699367
1901.975907	94914.815701	37.704384
1903.928643	95021.277054	37.709402
1905.710331	95142.634128	37.714420
1907.646884	95238.793418	37.719437
1909.738858	95358.733803	37.724455
1911.780250	95481.014918	37.729472
1913.309018	95599.345796	37.734490
1915.468336	95719.416465	37.739508
1917.089348	95838.532398	37.744525
1919.131378	95950.623766	37.749543
1921.251461	96078.916021	37.754560
1923.276843	96201.937675	37.759578
1925.259844	96328.591829	37.764596
1927.092285	96448.133338	37.769613
1929.131416	96571.407813	37.774631
1930.890658	96691.481428	37.779648
1933.291567	96817.514401	37.784666
1935.454391	96947.413415	37.789684
1937.464216	97074.636814	37.794701
1939.638033	97177.027109	37.799719
1941.175417	97310.080522	37.804736
1943.154518	97422.009510	37.809754
1945.273692	97563.859262	37.814772
1947.335666	97680.251060	37.819789
1949.724639	97803.348836	37.824807
1951.331967	97926.645457	37.829824
1953.189047	98041.435331	37.834842
1955.365337	98168.155352	37.839860
1957.116430	98293.332435	37.844877
1959.313343	98417.324673	37.849895
1961.047370	98551.227223	37.854912
1963.023692	98667.813514	37.859930
1965.329558	98799.447163	37.864948
1967.275558	98930.123486	37.869965
1969.183529	99049.662977	37.874983
1971.333536	99180.929586	37.880000
1973.338578	99297.716513	37.885018
1975.341249	99418.421554	37.890036
1977.086788	99555.926881	37.895053
1979.001042	99679.068129	37.900071
1981.057367	99803.569470	37.905088
1983.031983	99930.011074	37.910106
1985.097867	100063.551058	37.915124
1987.201662	100191.710312	37.920141
1989.005961	100328.512457	37.925159
1990.759077	100460.607042	37.930176
1993.147031	100587.214737	37.935194
1995.283370	100717.399435	37.940212
1997.294445	100835.129140	37.945229
1999.289291	100972.398622	37.950247
2001.419390	101105.691963	37.955264
2003.176228	101223.653023	37.960282
2005.262081	101351.363245	37.965300
2007.041482	101486.031541	37.970317
2008.985662	101609.936120	37.975335
2010.840368	101734.438370	37.980352
2013.055844	101877.344334	37.985370
2015.385912	102005.361210	37.990388
2017.501208	102132.321842	37.995405
2019.458270	102249.240988	38.000423
2021.399209	102391.101791	38.005440
2023.265474	102499.630149	38.010458
2025.253861	102616.647127	38.015476
2027.110180	102736.499853	38.020493
2028.886143	102843.014879	38.025511
2030.525235	102952.024024	38.030528
2032.334197	103068.195839	38.035546
2034.232721	103192.760134	38.040564
2035.859854	103325.773482	38.045581
2037.783685	103462.861604	38.050599
2039.477914	103596.524842	38.055616
2041.387107	103725.374973	38.060634
2043.421288	103875.583045	38.065652
2045.458318	104020.567523	38.070669
2047.346950	104167.325584	38.075687
2048.983206	104330.264519	38.080704
2050.900586	104490.446875	38.085722
2053.077515	104637.466190	38.090740
2055.103177	104803.224717	38.095757
2057.765736	104973.613876	38.100775
2059.298363	105125.376844	38.105792
2061.592124	105294.253057	38.110810
2063.716620	105457.805756	38.115828
2065.345538	105638.288218	38.120845
2067.678284	105804.079686	38.125863
2069.753939	105982.490665	38.130880
2071.851643	106146.228392	38.135898
2073.845628	106317.832080	38.140916
2076.359798	106493.856678	38.145933
2078.462441	106660.385725	38.150951
2080.779802	106842.136307	38.155968
2082.982310	107007.358033	38.160986
2085.161945	107177.757720	38.166004
2087.340753	107342.946729	38.171021
2089.610708	107513.422712	38.176039
2091.713396	107686.626665	38.181056
2094.138158	107845.312524	38.186074
2096.067412	108018.494556	38.191092
2098.181195	108192.548914	38.196109
2100.740855	108357.290086	38.201127
2102.112679	108535.761043	38.206144
2104.879190	108696.996909	38.211162
2106.642080	108864.756400	38.216180
2109.022096	109035.945470	38.221197
2111.497937	109200.932011	38.226215
2113.504687	109373.740913	38.231232
2115.401815	109534.634792	38.236250
2117.900232	109692.226968	38.241268
2119.953676	109873.337263	38.246285
2122.119469	110037.666099	38.251303
2124.174668	110208.442505	38.256320
2126.205834	110366.389801	38.261338
2128.398375	110533.975915	38.266356
2130.312350	110718.511034	38.271373
2132.756503	110869.611283	38.276391
2134.716505	111040.837781	38.281408
2136.870016	111214.495100	38.286426
2139.308509	111387.018037	38.291444
2140.886140	111551.623466	38.296461
2143.209293	111725.421599	38.301479
2145.128654	111899.473984	38.306496
2146.971314	112077.851138	38.311514
2149.624314	112246.920492	38.316532
2151.670739	112420.689201	38.321549
2153.825583	112599.400569	38.326567
2155.909753	112776.437126	38.331584
2158.177486	112955.094548	38.336602
2160.533057	113118.925958	38.341620
2162.726528	113292.764638	38.346637
2164.886928	113451.960912	38.351655
2166.514375	113606.827701	38.356672
2168.846152	113738.477054	38.361690
2170.858731	113902.961755	38.366708
2172.623045	114057.390516	38.371725
2174.881293	114216.498730	38.376743
2176.610432	114389.476763	38.381760
2178.630527	114542.979752	38.386778
2180.527063	114713.662870	38.391796
2183.043355	114889.018667	38.396813
2185.354769	115053.132021	38.401831
2187.203927	115229.646518	38.406848
2188.930905	115404.570198	38.411866
2191.277572	115593.425532	38.416884
2193.183992	115777.873464	38.421901
2195.315128	115951.734507	38.426919
2197.681577	116148.301122	38.431936
2200.087094	116349.796585	38.436954
2202.294845	116538.323316	38.441972
2204.308836	116733.958835	38.446989
2206.416307	116935.935337	38.452007
2208.486134	117134.557590	38.457024
2210.569421	117334.840382	38.462042
2212.751125	117546.296137	38.467060
2214.916536	117761.421325	38.472077
2217.911817	117957.264839	38.477095
2219.877253	118180.287867	38.482112
2222.115326	118368.286282	38.487130
2224.517010	118579.776815	38.492148
2226.467428	118783.677732	38.497165
2228.925135	118997.381591	38.502183
2231.138904	119221.652997	38.507200
2233.269231	119425.630666	38.512218
2235.804011	119641.457079	38.517236
2237.845796	119857.006657	38.522253
2240.354879	120064.239184	38.527271
2242.333974	120291.103191	38.532288
2244.666952	120499.963904	38.537306
2247.285613	120717.838177	38.542324
2249.040197	120944.132243	38.547341
2251.671464	121152.911743	38.552359
2253.860096	121376.514577	38.557376
2256.411645	121590.040491	38.562394
2258.609690	121812.654886	38.567412
2260.575255	122025.437607	38.572429
2263.270199	122247.291709	38.577447
2265.639489	122464.897579	38.582464
2267.488528	122695.068760	38.587482
2269.787051	122917.648298	38.592500
2272.001252	123139.392324	38.597517
2274.429300	123362.956272	38.602535
2276.917013	123580.131092	38.607552
2279.255004	123806.604016	38.612570
2281.488439	124024.265040	38.617588
2283.814032	124257.910108	38.622605
2286.153086	124476.368972	38.627623
2288.225998	124693.437101	38.632640
2290.564218	124920.157296	38.637658
2293.222902	125130.577263	38.642676
2295.794990	125357.250629	38.647693
2297.950852	125578.611253	38.652711
2300.415171	125798.618097	38.657728
2302.583892	126012.531987	38.662746
2304.798230	126221.771115	38.667764
2307.061699	126459.536395	38.672781
2308.943312	126660.824393	38.677799
2311.416681	126891.124783	38.682816
2313.119515	127118.705094	38.687834
2315.508480	127338.833458	38.692852
2317.327332	127555.931125	38.697869
2319.764748	127765.777531	38.702887
2321.587513	127964.315234	38.707904
2324.295066	128181.226378	38.712922
2326.410966	128386.241550	38.717940
2328.348996	128598.796564	38.722957
2330.566757	128831.621728	38.727975
2332.577905	129056.360393	38.732992
2334.576697	129289.844034	38.738010
2336.833242	129520.954082	38.743028
2339.104696	129769.889517	38.748045
2341.009515	130009.317050	38.753063
2343.550233	130258.885677	38.758080
2345.861367	130517.741298	38.763098
2348.301642	130770.170748	38.768116
2350.541467	131031.146852	38.773133
2353.238512	131283.285374	38.778151
2355.776141	131538.051425	38.783168
2357.522489	131806.164147	38.788186
2360.373167	132065.782070	38.793204
2362.513755	132325.182718	38.798221
2365.111749	132594.892706	38.803239
2367.456713	132857.132177	38.808256
2369.736110	133120.753862	38.813274
2372.621546	133399.483656	38.818292
2374.558930	133662.717961	38.823309
2376.774098	133936.404244	38.828327
2379.258386	134208.032531	38.833344
2381.240886	134496.706486	38.838362
2384.538279	134773.172500	38.843380
2386.607084	135048.588847	38.848397
2388.948804	135329.090731	38.853415
2391.834868	135607.999143	38.858432
2394.066179	135890.475965	38.863450
2396.651021	136163.102775	38.868468
2399.052199	136454.325108	38.873485
2401.376516	136724.927584	38.878503
2403.990353	137013.759883	38.883520
2406.496582	137297.166804	38.888538
2409.263999	137580.623432	38.893556
2411.393401	137871.706876	38.898573
2413.887597	138149.943290	38.903591
2416.091633	138426.894266	38.908608
2418.710145	138707.639925	38.913626
2421.239319	138997.043455	38.918644
2423.672521	139284.991668	38.923661
2426.138901	139571.134371	38.928679
2428.825126	139850.467564	38.933696
2430.949976	140152.822472	38.938714
2433.374653	140436.426042	38.943732
2436.067043	140728.301978	38.948749
2438.328831	141011.883659	38.953767
2440.827119	141276.571043	38.958784
2443.365594	141577.816831	38.963802
2445.644540	141861.451560	38.968820
2447.562181	142141.413208	38.973837
2450.147406	142434.179168	38.978855
2453.158852	142719.531840	38.983872
2454.956119	143012.703711	38.988890
2457.929166	143302.279347	38.993908
2460.035698	143598.629971	38.998925
2462.597661	143889.770949	39.003943
2464.946045	144184.767273	39.008960
2467.669806	144485.773345	39.013978
2469.827496	144772.667429	39.018996
2472.256606	145070.892766	39.024013
2474.641682	145362.006455	39.029031
2477.218792	145650.946785	39.034048
2479.212041	145932.720097	39.039066
2481.496494	146200.995522	39.044084
2484.171538	146486.472918	39.049101
2486.153375	146766.970643	39.054119
2488.561561	147034.723339	39.059136
2490.447990	147339.875310	39.064154
2492.950309	147632.481192	39.069172
2494.841809	147944.033002	39.074189
2497.312759	148236.279059	39.079207
2499.902655	148547.014382	39.084224
2502.143224	148865.447341	39.089242
2504.653025	149187.559153	39.094260
2506.725577	149507.875407	39.099277
2509.116728	149836.191227	39.104295
2511.972731	150152.809277	39.109312
2514.233672	150495.734052	39.114330
2517.132557	150832.392180	39.119348
2519.253645	151171.090766	39.124365
2521.568168	151508.352189	39.129383
2524.426671	151864.507630	39.134400
2526.749525	152212.079304	39.139418
2529.106476	152550.406693	39.144436
2531.967842	152914.920938	39.149453
2534.843951	153258.693239	39.154471
2537.305512	153615.785087	39.159488
2539.545758	153972.989959	39.164506
2541.962735	154331.895834	39.169524
2544.469919	154700.996068	39.174541
2546.515821	155068.558625	39.179559
2549.516807	155437.586311	39.184576
2551.973615	155820.157682	39.189594
2554.779260	156198.056131	39.194612
2557.661256	156563.656566	39.199629
2559.917355	156939.881144	39.204647
2563.114873	157310.387785	39.209664
2565.267850	157689.426077	39.214682
2568.253301	158063.258519	39.219700
2570.892451	158440.257737	39.224717
2573.390132	158816.138843	39.229735
2576.212774	159190.993886	39.234752
2578.675536	159580.545234	39.239770
2581.111407	159954.640200	39.244788
2583.683916	160337.069675	39.249805
2586.322391	160722.779315	39.254823
2588.994440	161095.993531	39.259840
2591.162865	161492.382251	39.264858
2594.321211	161872.101335	39.269876
2596.842211	162266.941585	39.274893
2599.382470	162654.519139	39.279911
2602.103742	163028.422445	39.284928
2604.710775	163430.746952	39.289946
2607.090975	163814.623741	39.294964
2609.701295	164200.980614	39.299981
2612.671740	164598.418078	39.304999
2615.274326	165000.397263	39.310016
2617.063478	165393.478865	39.315034
2619.860727	165781.428002	39.320052
2622.499430	166187.623795	39.325069
2625.030506	166596.860627	39.330087
2627.529446	167003.717899	39.335104
2629.899329	167401.011595	39.340122
2632.088252	167807.617285	39.345140
2635.068021	168225.236870	39.350157
2637.723641	168647.417055	39.355175
2640.021677	169069.947676	39.360192
2642.610453	169479.509510	39.365210
2645.043872	169896.563943	39.370228
2647.380312	170315.261165	39.375245
2649.510911	170735.808675	39.380263
2652.263115	171127.285621	39.385280
2655.020038	171538.000675	39.390298
2657.491128	171933.766750	39.395316
2660.505627	172346.858424	39.400333
2662.963920	172756.229976	39.405351
2665.157762	173171.981266	39.410368
2667.634522	173586.141366	39.415386
2669.986395	174006.608665	39.420404
2672.835392	174436.498562	39.425421
2674.967052	174880.648649	39.430439
2677.407522	175315.648275	39.435456
2679.967576	175775.024841	39.440474
2682.329498	176215.577954	39.445492
2685.305495	176677.865873	39.450509
2687.203954	177140.604235	39.455527
2690.153661	177607.091841	39.460544
2692.824349	178089.981417	39.465562
2695.629094	178554.465052	39.470580
2698.267954	179038.761723	39.475597
2700.773647	179517.291223	39.480615
2703.712491	180007.667079	39.485632
2706.542080	180513.809373	39.490650
2709.065283	180998.287087	39.495668
2712.086688	181509.306686	39.500685
2714.736328	181991.585567	39.505703
2717.594079	182485.085861	39.510720
2720.421204	182988.778312	39.515738
2723.622549	183515.654657	39.520756
2725.952047	184054.252062	39.525773
2728.647163	184560.411534	39.530791
2731.730764	185049.977996	39.535808
2734.290027	185560.125981	39.540826
2737.434988	186078.007884	39.545844
2740.565522	186565.897861	39.550861
2743.280903	187072.701503	39.555879
2745.870172	187582.981627	39.560896
2748.830607	188085.357559	39.565914
2751.937299	188584.029924	39.570932
2754.771561	189085.769734	39.575949
2757.344181	189595.858541	39.580967
2760.872939	190085.657672	39.585984
2763.901709	190585.367008	39.591002
2766.365491	191098.349673	39.596020
2769.439994	191600.418372	39.601037
2771.904216	192105.734279	39.606055
2774.244984	192610.030132	39.611072
2776.971837	193114.826453	39.616090
2779.316849	193623.774055	39.621108
2782.428103	194133.416657	39.626125
2784.954039	194661.340030	39.631143
2787.727253	195172.588971	39.636160
2790.231150	195702.247155	39.641178
2792.618328	196224.330579	39.646196
2795.808934	196750.024314	39.651213
2798.256497	197277.233278	39.656231
2801.151545	197806.253888	39.661248
2803.537274	198354.940856	39.666266
2806.097719	198895.956496	39.671284
2808.892474	199433.279484	39.676301
2811.588609	199988.401197	39.681319
2814.478775	200524.137993	39.686336
2817.229268	201080.855249	39.691354
2819.491381	201638.692214	39.696372
2822.753193	202185.959624	39.701389
2825.532961	202739.019680	39.706407
2828.386136	203288.462769	39.711424
2831.407423	203833.105486	39.716442
2834.006218	204369.331314	39.721460
2836.783809	204887.189821	39.726477
2839.275142	205430.319484	39.731495
2842.006200	205955.529414	39.736512
2844.903851	206490.266119	39.741530
2847.366049	207031.168972	39.746548
2849.917467	207565.454362	39.751565
2852.720829	208121.599125	39.756583
2855.155524	208668.276623	39.761600
2858.073362	209239.393953	39.766618
2860.514136	209802.686725	39.771636
2863.389964	210372.111084	39.776653
2865.976957	210964.089257	39.781671
2868.526215	211541.391325	39.786688
2871.169320	212134.074387	39.791706
2873.420848	212737.006657	39.796724
2876.949226	213337.784269	39.801741
2879.443402	213955.287878	39.806759
2882.503238	214569.401588	39.811776
2885.214916	215203.207849	39.816794
2887.822279	215817.546680	39.821812
2891.040368	216438.192638	39.826829
2893.778314	217080.457005	39.831847
2896.613653	217723.240444	39.836864
2900.016218	218357.882881	39.841882
2902.772628	219001.670858	39.846900
2906.096056	219634.294649	39.851917
2908.907401	220286.407736	39.856935
2912.043203	220934.405948	39.861952
2914.733816	221576.529674	39.866970
2917.557790	222228.819939	39.871988
2921.231559	222871.120837	39.877005
2924.494315	223519.024338	39.882023
2927.638267	224165.142901	39.887040
2930.805530	224801.197906	39.892058
2933.811450	225454.578366	39.897076
2937.405752	226077.686732	39.902093
2940.448149	226722.551007	39.907111
2943.678615	227355.877670	39.912128
2947.014398	227988.704975	39.917146
2949.734298	228617.563672	39.922164
2953.007663	229240.924426	39.927181
2955.855001	229890.212713	39.932199
2958.484719	230520.913415	39.937216
2960.937302	231150.980797	39.942234
2963.650108	231798.789674	39.947252
2966.969694	232443.911783	39.952269
2969.764942	233097.142782	39.957287
2972.808032	233739.105692	39.962304
2976.197791	234383.960372	39.967322
2978.439882	235044.032633	39.972340
2981.591787	235682.190556	39.977357
2984.400710	236346.719307	39.982375
2987.320959	237004.827722	39.987392
2990.430621	237673.092112	39.992410
2992.924280	238330.400922	39.997428
2996.096356	238999.033828	40.002445
2998.899866	239667.900683	40.007463
3002.024891	240328.408772	40.012480
3004.893548	241007.804594	40.017498
3008.005583	241670.191202	40.022516
3010.879533	242339.192696	40.027533
3014.086333	243015.405549	40.032551
3017.450433	243687.933773	40.037568
3020.178218	244364.801748	40.042586
3023.028138	245031.030076	40.047604
3026.213192	245701.674732	40.052621
3029.419506	246355.090777	40.057639
3032.397521	247001.579997	40.062656
3035.797516	247640.329436	40.067674
3038.284940	248280.997507	40.072692
3041.327562	248916.648386	40.077709
3044.310508	249560.612784	40.082727
3046.918803	250203.769622	40.087744
3049.680521	250851.878737	40.092762
3052.557714	251523.540153	40.097780
3055.159436	252174.005812	40.102797
3058.102777	252856.827844	40.107815
3060.646890	253537.575413	40.112832
3063.525677	254220.299551	40.117850
3066.060939	254922.379116	40.122868
3068.910747	255618.081007	40.127885
3072.479964	256335.714931	40.132903
3075.018681	257041.567631	40.137920
3078.009846	257764.872244	40.142938
3080.595011	258503.044747	40.147956
3083.958746	259240.430649	40.152973
3086.742489	259973.305252	40.157991
3089.599821	260727.576116	40.163008
3092.469386	261472.238919	40.168026
3095.835050	262231.398722	40.173044
3098.746144	262993.088146	40.178061
3102.291979	263762.140389	40.183079
3105.546747	264541.087481	40.188096
3108.883268	265315.596502	40.193114
3112.062712	266088.219275	40.198132
3115.223794	266847.301437	40.203149
3118.466900	267633.541286	40.208167
3121.472324	268414.046466	40.213184
3125.000059	269189.790281	40.218202
3127.575378	269995.087255	40.223220
3131.175089	270766.107917	40.228237
3134.424851	271564.809046	40.233255
3137.442257	272350.561307	40.238272
3140.832095	273137.772019	40.243290
3143.930266	273933.351181	40.248308
3147.289746	274727.662897	40.253325
3150.626563	275522.249860	40.258343
3153.492351	276305.118964	40.263360
3156.817891	277102.511044	40.268378
3159.666060	277916.476728	40.273396
3163.124618	278707.838280	40.278413
3166.396414	279520.984271	40.283431
3169.722100	280331.598966	40.288448
3173.299523	281127.157356	40.293466
3176.486137	281925.104436	40.298484
3179.585354	282722.446882	40.303501
3182.564296	283532.800653	40.308519
3185.607686	284335.136099	40.313536
3189.536642	285137.298356	40.318554
3192.698285	285940.586844	40.323572
3196.131866	286737.119637	40.328589
3200.014633	287523.491997	40.333607
3203.186608	288310.829369	40.338624
3206.815069	289090.798447	40.343642
3210.302681	289876.264495	40.348660
3213.608148	290653.344900	40.353677
3217.321262	291421.719123	40.358695
3220.259953	292193.911811	40.363712
3223.913358	292955.090726	40.368730
3227.189009	293733.203093	40.373748
3230.240057	294495.675298	40.378765
3233.716065	295259.188291	40.383783
3236.701894	296026.296916	40.388800
3239.928491	296783.913285	40.393818
3243.378349	297538.387358	40.398836
3246.270509	298266.307066	40.403853
3249.420778	298996.131736	40.408871
3252.175507	299715.752338	40.413888
3255.369372	300447.251853	40.418906
3258.273222	301185.209534	40.423924
3261.190802	301919.270897	40.428941
3264.334061	302671.462807	40.433959
3266.958704	303428.319754	40.438976
3270.054563	304182.502798	40.443994
3273.145009	304961.526914	40.449012
3276.030441	305724.731648	40.454029
3279.105504	306502.566916	40.459047
3281.985168	307301.844037	40.464064
3285.473152	308085.123598	40.469082
3288.500096	308891.712972	40.474100
3291.355275	309699.407269	40.479117
3295.068257	310512.080981	40.484135
3297.851377	311346.739314	40.489152
3300.920973	312173.647825	40.494170
3303.909899	313015.071787	40.499188
3307.020247	313871.105568	40.504205
3310.247801	314731.064233	40.509223
3312.708388	315593.968985	40.514240
3316.108212	316468.688881	40.519258
3319.270906	317350.889758	40.524276
3322.493624	318252.274170	40.529293
3326.038570	319144.936218	40.534311
3329.238846	320055.803082	40.539328
3332.471409	320954.389186	40.544346
3336.043554	321873.050997	40.549364
3339.343527	322780.545198	40.554381
3342.876305	323706.912218	40.559399
3346.021338	324628.878780	40.564416
3349.648800	325546.156700	40.569434
3353.066644	326488.006946	40.574452
3356.465486	327424.510075	40.579469
3359.885101	328351.778277	40.584487
3363.031703	329290.357216	40.589504
3366.576291	330239.278398	40.594522
3370.378620	331179.028534	40.599540
3373.698306	332121.444106	40.604557
3376.901634	333074.052448	40.609575
3380.436044	334022.145721	40.614592
3383.837930	334956.233320	40.619610
3387.862941	335909.731775	40.624628
3391.050189	336855.879085	40.629645
3395.066903	337802.810655	40.634663
3398.099043	338751.520012	40.639680
3401.385305	339683.551566	40.644698
3405.052153	340646.974222	40.649716
3408.302203	341585.581013	40.654733
3412.109767	342542.741336	40.659751
3415.563247	343488.822678	40.664768
3419.340909	344430.414704	40.669786
3422.932254	345375.078337	40.674804
3426.901565	346313.849437	40.679821
3430.363490	347238.397213	40.684839
3433.554671	348186.061939	40.689856
3437.172737	349116.136926	40.694874
3440.478995	350052.268940	40.699892
3443.906655	350991.068047	40.704909
3447.416978	351918.671160	40.709927
3450.784376	352865.158078	40.714944
3454.336311	353801.168097	40.719962
3457.735014	354739.253219	40.724980
3461.384471	355664.088523	40.729997
3465.414262	356583.665444	40.735015
3468.603811	357493.584846	40.740020
3472.299678	358363.643312	40.745024
3475.824085	359186.816743	40.750029
3478.708693	359968.035789	40.755034
3482.083453	360686.822923	40.760039
3484.888976	361362.940194	40.765044
3487.704550	361964.079106	40.770048
3490.920374	362520.345089	40.775053
3493.137996	363030.688762	40.780058
3495.647485	363475.599655	40.785063
3497.744080	363872.138736	40.790068
3500.224860	364228.009234	40.795072
3501.851460	364530.727390	40.800077
3503.812260	364797.640766	40.805082
3505.649973	365016.727596	40.810087
3507.250128	365197.052068	40.815092
3509.154478	365332.661012	40.820096
3510.189661	365438.017619	40.825101
3511.842641	365512.762716	40.830106
3512.924970	365543.921203	40.835111
3513.900696	365552.712244	40.840116
3515.390015	365529.028303	40.845120
3516.394285	365478.132364	40.850125
3516.955374	365407.894133	40.855130
3518.023871	365301.853047	40.860135
3518.930136	365200.054649	40.865140
3519.682658	365050.614508	40.870144
3520.201555	364887.642163	40.875149
3520.583737	364715.390837	40.880154
3521.402502	364516.365924	40.885159
3522.142441	364320.553471	40.890164
3522.176571	364089.633385	40.895168
3522.273155	363855.093627	40.900173
3522.783914	363621.147886	40.905178
3523.316769	363370.934761	40.910183
3523.386240	363126.051763	40.915188
3523.729205	362849.869769	40.920192
3524.013701	362575.447639	40.925197
3524.155687	362303.332182	40.930202
3524.013570	362009.557953	40.935207
3524.160183	361717.717733	40.940212
3524.143743	361421.275316	40.945216
3524.374089	361123.393748	40.950221
3524.295486	360810.793335	40.955226
3524.500053	360499.898820	40.960231
3524.094595	360199.667933	40.965236
3524.099818	359891.314104	40.970240
3524.282196	359579.422477	40.975245
3524.355785	359268.713644	40.980250
3524.295230	358957.539749	40.985255
3524.289852	358631.995417	40.990260
3524.270174	358318.470561	40.995264
3524.363289	357992.268666	41.000269
3524.262994	357669.829440	41.005274
3524.111012	357337.330737	41.010279
3524.138168	357018.270308	41.015284
3523.880758	356688.957951	41.020288
3523.759883	356365.796681	41.025293
3523.346264	356052.234091	41.030298
3523.392325	355718.924569	41.035303
3523.142697	355409.828488	41.040308
3523.367221	355096.537764	41.045312
3522.929987	354777.857364	41.050317
3522.651128	354467.892393	41.055322
3522.468650	354151.021247	41.060327
3522.311179	353853.943184	41.065332
3522.345476	353526.712416	41.070336
3522.072174	353217.852691	41.075341
3521.902072	352916.370518	41.080346
3521.750132	352612.594998	41.085351
3521.515740	352310.557947	41.090356
3521.416347	352008.141078	41.095360
3521.377310	351711.532904	41.100365
3521.170019	351421.608171	41.105370
3520.963855	351119.835128	41.110375
3520.926079	350831.174991	41.115380
3520.506290	350533.471629	41.120384
3520.383417	350245.734708	41.125389
3520.210862	349961.383938	41.130394
3520.331190	349675.866390	41.135399
3520.102095	349399.018675	41.140404
3519.775252	349102.152032	41.145408
3519.549028	348834.399880	41.150413
3519.370058	348556.774590	41.155418
3519.335459	348272.235086	41.160423
3519.019688	348002.964879	41.165428
3518.830847	347737.231752	41.170432
3518.834205	347462.288958	41.175437
3518.467294	347199.324994	41.180442
3518.374191	346940.180421	41.185447
3518.109117	346682.077646	41.190452
3518.215618	346416.364097	41.195456
3518.244840	346152.516438	41.200461
3517.685464	345900.173933	41.205466
3518.033736	345650.001207	41.210471
3517.579016	345393.392779	41.215476
3517.464490	345147.432801	41.220480
3517.456703	344890.420181	41.225485
3516.923788	344644.496547	41.230490
3517.003882	344399.314320	41.235495
3516.938573	344170.094483	41.240500
3516.402797	343920.301498	41.245504
3516.188031	343684.618381	41.250509
3516.257769	343452.296178	41.255514
3516.398589	343218.283205	41.260519
3516.139871	342981.508847	41.265524
3515.663170	342751.428545	41.270528
3515.566052	342529.118616	41.275533
3515.436503	342300.125223	41.280538
3515.738969	342082.224990	41.285543
3514.931562	341875.760891	41.290548
3514.874048	341653.642592	41.295552
3515.291162	341434.169361	41.300557
3514.919143	341224.200714	41.305562
3514.713993	341003.321873	41.310567
3514.409592	340796.849057	41.315572
3514.256778	340585.596386	41.320576
3514.217525	340379.308521	41.325581
3514.153802	340187.059433	41.330586
3514.355131	339971.628423	41.335591
3514.005849	339773.776729	41.340596
3513.945631	339570.157386	41.345600
3513.807657	339370.236153	41.350605
3513.581377	339182.024730	41.355610
3513.664506	338978.761029	41.360615
3513.494390	338789.903046	41.365620
3513.368108	338592.772808	41.370624
3513.080490	338392.004922	41.375629
3512.840723	338205.468802	41.380634
3512.863340	338013.296239	41.385639
3512.496348	337837.789017	41.390644
3512.231559	337653.313744	41.395648
3512.359145	337478.922653	41.400653
3512.246209	337311.815835	41.405658
3512.250415	337133.780477	41.410663
3512.127640	336958.434261	41.415668
3511.982500	336771.977691	41.420672
3511.832111	336602.127007	41.425677
3511.499448	336437.364693	41.430682
3511.820562	336268.532258	41.435687
3511.318336	336107.863862	41.440692
3511.133544	335937.023678	41.445696
3511.520968	335778.656116	41.450701
3511.290414	335620.816814	41.455706
3511.412661	335453.613886	41.460711
3511.391397	335291.620613	41.465716
3510.866204	335135.885233	41.470720
3510.960693	334973.592727	41.475725
3510.550382	334826.281334	41.480730
3510.841622	334662.227361	41.485735
3510.490506	334523.908329	41.490740
3510.359018	334369.481502	41.495744
3510.166234	334214.631276	41.500749
3510.174793	334072.388677	41.505754
3510.095559	333924.258997	41.510759
3510.108489	333783.744008	41.515764
3510.046602	333643.672539	41.520768
3510.041533	333500.768662	41.525773
3509.520703	333365.981565	41.530778
3509.711900	333222.282970	41.535783
3509.664490	333085.538839	41.540788
3509.354796	332946.393666	41.545792
3509.531428	332810.885158	41.550797
3509.099156	332685.695435	41.555802
3509.497354	332545.904027	41.560807
3509.348276	332413.573293	41.565812
3509.310629	332281.733343	41.570816
3509.127398	332147.041725	41.575821
3508.987769	332021.117360	41.580826
3509.086902	331888.796865	41.585831
3508.877376	331767.435196	41.590836
3508.714922	331641.792919	41.595840
3508.880164	331521.211191	41.600845
3508.490910	331402.470711	41.605850
3508.657070	331274.817447	41.610855
3508.518547	331163.260272	41.615860
3508.153317	331039.224633	41.620864
3508.165984	330921.920444	41.625869
3507.963086	330809.990796	41.630874
3507.990299	330691.513657	41.635879
3507.661929	330586.241339	41.640884
3508.166995	330471.758326	41.645888
3507.988405	330369.666749	41.650893
3508.021834	330249.228823	41.655898
3508.105904	330136.565628	41.660903
3507.795659	330029.940925	41.665908
3507.791750	329923.980214	41.670912
3507.454656	329818.707177	41.675917
3507.192993	329723.977580	41.680922
3507.122470	329613.397272	41.685927
3507.289947	329510.155627	41.690932
3507.069102	329415.800427	41.695936
3506.885888	329309.001282	41.700941
3507.098940	329220.173530	41.705946
3506.957939	329118.810421	41.710951
3507.118766	329032.355898	41.715956
3506.865547	328937.317851	41.720960
3506.802751	328844.437260	41.725965
3506.826553	328745.870770	41.730970
3506.915703	328650.091741	41.735975
3506.691898	328550.317124	41.740980
3506.448210	328471.987739	41.745984
3506.563526	328379.714102	41.750989
3506.172355	328291.868972	41.755994
3506.165603	328201.191028	41.760999
3506.209343	328119.458461	41.766004
3505.703464	328031.579815	41.771008
3506.064755	327949.008733	41.776013
3506.152418	327864.928651	41.781018
3506.146554	327777.708920	41.786023
3505.913382	327706.269595	41.791028
3506.140598	327617.029042	41.796032
3505.740509	327537.425008	41.801037
3505.690319	327465.575098	41.806042
3505.917552	327377.173408	41.811047
3505.602119	327305.364677	41.816052
3505.505431	327234.030350	41.821056
3505.625188	327156.430084	41.826061
3505.603924	327088.670271	41.831066
3505.581637	327007.250983	41.836071
3505.613685	326939.304526	41.841076
3505.376661	326858.122001	41.846080
3505.606287	326785.871009	41.851085
3505.634292	326714.668884	41.856090
3505.505676	326647.866275	41.861095
3505.688566	326571.374232	41.866100
3505.661184	326492.294900	41.871104
3505.297092	326427.945260	41.876109
3505.076916	326349.709776	41.881114
3504.998242	326289.461546	41.886119
3504.982520	326212.363943	41.891124
3505.188145	326153.215738	41.896128
3505.330699	326080.620972	41.901133
3505.053083	326017.808833	41.906138
3505.038680	325945.925171	41.911143
3504.743971	325879.783191	41.916148
3504.607399	325821.044124	41.921152
3505.042428	325753.261603	41.926157
3504.917807	325704.644629	41.931162
3505.184318	325634.522564	41.936167
3504.708711	325568.993422	41.941172
3504.586522	325516.382134	41.946176
3504.781868	325450.747906	41.951181
3504.490751	325387.021143	41.956186
3504.687646	325329.628307	41.961191
3504.830796	325275.906839	41.966196
3504.820246	325216.384060	41.971200
3504.663283	325136.482891	41.976205
3504.465748	325097.593869	41.981210
3504.623685	325033.491093	41.986215
3504.563976	324970.210822	41.991220
3504.567822	324916.790477	41.996224
3504.426229	324862.858601	42.001229
3504.032781	324809.245847	42.006234
3504.504625	324739.369961	42.011239
3504.071902	324700.619082	42.016244
3503.991353	324633.653013	42.021248
3504.338309	324583.231178	42.026253
3504.061607	324543.896118	42.031258
3504.122975	324490.593416	42.036263
3503.804711	324435.798257	42.041268
3503.968166	324389.449568	42.046272
3503.973661	324343.201838	42.051277
3503.729358	324292.286999	42.056282
3503.870957	324241.667905	42.061287
3503.828568	324198.709059	42.066292
3503.693077	324149.150710	42.071296
3504.353253	324109.159994	42.076301
3503.992559	324054.599907	42.081306
3504.133303	324002.199952	42.086311
3504.332689	323951.164449	42.091316
3503.785386	323899.914917	42.096320
3504.259132	323851.532897	42.101325
3503.767994	323801.368325	42.106330
3503.700970	323749.229480	42.111335
3504.231051	323717.297372	42.116340
3503.933792	323668.476023	42.121344
3504.006068	323621.275807	42.126349
3503.566186	323573.290685	42.131354
3503.667681	323526.976154	42.136359
3503.497361	323481.645306	42.141364
3503.468768	323439.014220	42.146368
3503.845736	323394.869664	42.151373
3503.522412	323350.198568	42.156378
3503.739510	323300.380567	42.161383
3503.583066	323259.575456	42.166388
3503.608690	323218.436572	42.171392
3503.679673	323172.075538	42.176397
3503.485199	323125.323487	42.181402
3503.435713	323090.454248	42.186407
3503.305892	323052.239567	42.191412
3503.271443	323008.235239	42.196416
3503.260772	322976.870448	42.201421
3503.200683	322946.632688	42.206426
3503.247197	322902.971740	42.211431
3503.298070	322864.550563	42.216436
3503.159355	322834.528528	42.221440
3503.346396	322788.988420	42.226445
3503.080967	322750.667467	42.231450
3503.207584	322716.050217	42.236455
3502.886677	322690.101425	42.241460
3503.172993	322648.412435	42.246464
3503.223266	322616.427300	42.251469
3502.768872	322585.258784	42.256474
3502.937627	322550.990962	42.261479
3503.213400	322519.046817	42.266484
3503.090966	322480.016393	42.271488
3503.143372	322436.786510	42.276493
3502.777937	322406.545216	42.281498
3502.962689	322371.689637	42.286503
3502.918406	322349.971241	42.291508
3502.903184	322316.367981	42.296512
3502.918511	322282.734478	42.301517
3502.542463	322245.804097	42.306522
3502.743238	322225.141231	42.311527
3502.727926	322200.441784	42.316532
3502.461358	322171.380531	42.321536
3502.704216	322141.578181	42.326541
3502.775006	322121.775097	42.331546
3502.720935	322085.608311	42.336551
3502.976822	322069.007116	42.341556
3502.740652	322022.769147	42.346560
3502.862155	321998.378910	42.351565
3502.821226	321977.804589	42.356570
3502.516640	321936.665190	42.361575
3502.512616	321911.200613	42.366580
3502.675121	321879.833368	42.371584
3502.612618	321849.188155	42.376589
3502.655890	321832.950826	42.381594
3502.810582	321798.888110	42.386599
3502.742622	321773.051845	42.391604
3502.444463	321743.486436	42.396608
3502.696013	321712.003386	42.401613
3502.591241	321695.229468	42.406618
3502.633740	321660.471860	42.411623
3502.552521	321621.892117	42.416628
3502.481068	321616.128503	42.421632
3502.724512	321582.535098	42.426637
3502.455757	321557.849458	42.431642
3502.390000	321537.202483	42.436647
3502.552190	321516.061940	42.441652
3502.230328	321491.155602	42.446656
3502.497095	321465.877382	42.451661
3502.300456	321454.867206	42.456666
3502.635797	321425.049892	42.461671
3502.627881	321398.644328	42.466676
3502.504247	321366.380150	42.471680
3502.309602	321341.784558	42.476685
3502.351272	321326.132410	42.481690
3502.662419	321291.485141	42.486695
3502.699797	321271.330718	42.491700
3502.618206	321247.455164	42.496704
3502.822473	321221.550563	42.501709
3502.440513	321193.829572	42.506714
3502.832397	321169.574669	42.511719
3502.677909	321141.436476	42.516724
3502.458407	321109.848540	42.521728
3502.620636	321079.905407	42.526733
3502.408994	321064.877894	42.531738
3502.133656	321021.952205	42.536743
3502.418946	321007.610195	42.541748
3502.255388	320991.506641	42.546752
3502.742526	320958.205370	42.551757
3502.637458	320935.045643	42.556762
3502.626077	320911.209805	42.561767
3502.793845	320883.275466	42.566772
3502.847087	320858.437315	42.571776
3502.462105	320835.016010	42.576781
3502.275072	320802.176183	42.581786
3502.542381	320786.285036	42.586791
3502.271351	320763.532771	42.591796
3502.394720	320740.642512	42.596800
3502.382088	320706.223470	42.601805
3502.210732	320690.884240	42.606810
3502.030627	320654.659614	42.611815
3501.913175	320660.631193	42.616820
3502.039341	320634.763886	42.621824
3502.382730	320623.745389	42.626829
3502.250728	320596.875354	42.631834
3502.907688	320574.639365	42.636839
3502.528751	320557.449929	42.641844
3502.428085	320531.592582	42.646848
3502.290526	320498.388617	42.651853
3502.524595	320474.819450	42.656858
3502.970451	320449.054696	42.661863
3502.695461	320418.517993	42.666868
3502.536815	320398.699094	42.671872
3502.747279	320363.888727	42.676877
3502.369940	320345.248829	42.681882
3502.818949	320321.900384	42.686887
3502.278903	320284.943052	42.691892
3502.207547	320278.110725	42.696896
3502.205441	320247.938292	42.701901
3502.113838	320231.874084	42.706906
3502.272127	320204.576805	42.711911
3502.205156	320181.995856	42.716916
3501.941733	320167.586704	42.721920
3502.149265	320140.383450	42.726925
3501.861094	320141.446248	42.731930
3502.058683	320120.172275	42.736935
3502.127818	320106.296253	42.741940
3501.622521	320096.682351	42.746944
3502.221409	320065.830689	42.751949
3502.240051	320050.868581	42.756954
3502.412258	320028.886183	42.761959
3502.337003	320013.277275	42.766964
3501.687717	319990.660058	42.771968
3502.191280	319967.252009	42.776973
3501.822344	319969.319638	42.781978
3501.539891	319930.159240	42.786983
3502.142205	319920.372136	42.791988
3501.989734	319913.501551	42.796993
3501.852351	319891.287631	42.801997
3501.728469	319878.713766	42.807002
3501.810857	319870.610725	42.812007
3502.073093	319850.903860	42.817012
3501.994105	319838.399288	42.822017
3502.011265	319815.932198	42.827021
3501.887226	319787.966443	42.832026
3501.881084	319771.100026	42.837031
3502.236073	319760.435671	42.842036
3501.829912	319743.606340	42.847041
3502.156348	319722.871733	42.852045
3501.925668	319708.406425	42.857050
3502.223149	319685.386620	42.862055
3502.209893	319679.257468	42.867060
3502.043528	319657.429577	42.872065
3502.219356	319642.162899	42.877069
3502.249859	319616.564348	42.882074
3502.271738	319599.489953	42.887079
3502.196365	319583.244876	42.892084
3501.909333	319571.561431	42.897089
3502.004670	319540.177528	42.902093
3502.197567	319531.777292	42.907098
3502.176085	319507.204456	42.912103
3501.886981	319490.941876	42.917108
3501.991205	319470.572625	42.922113
3502.379924	319459.623068	42.927117
3501.987956	319449.304387	42.932122
3501.961330	319436.766071	42.937127
3502.009560	319407.119448	42.942132
3502.058424	319402.379821	42.947137
3502.251544	319374.338773	42.952141
3501.822638	319355.019589	42.957146
3501.862721	319337.306210	42.962151
3501.963150	319323.654017	42.967156
3502.177871	319309.118942	42.972161
3502.380980	319291.634471	42.977165
3502.003889	319279.481639	42.982170
3502.061952	319259.831867	42.987175
3501.963121	319233.795363	42.992180
3501.772339	319232.883963	42.997185
3502.310169	319211.607233	43.002189
3502.194395	319202.008557	43.007194
3502.020086	319176.874271	43.012199
3501.983864	319155.610936	43.017204
3502.247914	319146.232723	43.022209
3502.208412	319120.186876	43.027213
3501.982692	319107.145318	43.032218
3502.111627	319083.591829	43.037223
3501.956077	319064.560520	43.042228
3501.977417	319044.204027	43.047233
3502.292092	319027.795996	43.052237
3501.706866	319013.156911	43.057242
3501.631219	319001.821888	43.062247
3501.676357	318987.084244	43.067252
3501.451918	318979.334304	43.072257
3501.893888	318957.843462	43.077261
3501.545902	318952.911412	43.082266
3501.889771	318937.440124	43.087271
3502.013764	318919.408156	43.092276
3501.926119	318913.748476	43.097281
3502.078676	318896.169983	43.102285
3502.101349	318881.868323	43.107290
3501.842190	318871.147115	43.112295
3502.049249	318850.125455	43.117300
3501.712498	318832.318132	43.122305
3501.948273	318817.550627	43.127309
3501.587947	318795.421883	43.132314
3501.631563	318790.708452	43.137319
3501.975930	318783.836337	43.142324
3501.938936	318771.095915	43.147329
3502.007278	318757.931954	43.152333
3501.454634	318759.265108	43.157338
3501.458604	318745.729580	43.162343
3501.420444	318721.362440	43.167348
3501.974281	318708.198888	43.172353
3501.871322	318694.781829	43.177357
3501.800543	318681.563269	43.182362
3502.033485	318670.714194	43.187367
3502.180824	318666.188068	43.192372
3501.743052	318643.664285	43.197377
3502.225885	318621.581728	43.202381
3502.390499	318612.168063	43.207386
3502.011000	318589.126305	43.212391
3502.245739	318578.175159	43.217396
3501.749895	318558.382690	43.222401
3502.059077	318541.619149	43.227405
3502.242374	318535.840736	43.232410
3502.043356	318505.163594	43.237415
3501.813752	318492.911158	43.242420
3501.719647	318476.617712	43.247425
3501.671922	318453.931084	43.252429
3501.813903	318456.631282	43.257434
3501.841395	318437.927270	43.262439
3501.848665	318403.834028	43.267444
3501.960796	318405.165029	43.272449
3502.235838	318386.015222	43.277453
3502.158459	318374.654865	43.282458
3502.308967	318348.960481	43.287463
3502.398203	318328.033315	43.292468
3501.969604	318320.315176	43.297473
3502.113060	318286.912928	43.302477
3502.029280	318284.865330	43.307482
3501.888248	318261.226393	43.312487
3502.103111	318241.170017	43.317492
3501.827325	318236.659113	43.322497
3502.071279	318211.636974	43.327501
3502.007236	318195.415050	43.332506
3501.792914	318183.134696	43.337511
3501.994857	318160.129021	43.342516
3501.609001	318153.294643	43.347521
3501.504575	318141.938454	43.352525
3501.549540	318134.527877	43.357530
3502.086340	318116.176619	43.362535
3502.015876	318107.562861	43.367540
3501.874853	318103.972234	43.372545
3501.674774	318071.056046	43.377549
3501.887706	318064.458788	43.382554
3501.686357	318064.617586	43.387559
3502.161784	318039.024876	43.392564
3502.073052	318018.964978	43.397569
3502.117115	317995.907573	43.402573
3501.814687	317987.101076	43.407578
3501.986308	317981.120878	43.412583
3502.105914	317948.307272	43.417588
3501.865427	317947.352731	43.422593
3502.119623	317928.892924	43.427597
3501.893336	317915.240484	43.432602
3501.672737	317902.426745	43.437607
3501.942978	317888.518576	43.442612
3501.704402	317872.400145	43.447617
3501.868553	317856.931130	43.452621
3501.882174	317852.883787	43.457626
3501.501566	317825.084093	43.462631
3501.709184	317809.048536	43.467636
3501.726217	317807.773866	43.472641
3501.742550	317801.792478	43.477645
3501.882469	317781.569513	43.482650
3501.756887	317773.269615	43.487655
3502.058689	317759.051163	43.492660
3501.893730	317744.880235	43.497665
3502.086970	317727.065932	43.502669
3501.943735	317725.282026	43.507674
3501.969818	317685.842391	43.512679
3502.029180	317681.915093	43.517684
3501.946308	317664.093046	43.522689
3502.058430	317639.269289	43.527693
3502.126295	317637.528704	43.532698
3501.885067	317616.245786	43.537703
3501.969488	317594.479424	43.542708
3501.976651	317589.389927	43.547713
3501.895585	317561.848546	43.552717
3501.545830	317556.967500	43.557722
3501.909948	317539.380830	43.562727
3501.905079	317519.969098	43.567732
3501.664843	317511.534420	43.572737
3502.189229	317500.563166	43.577741
3501.641627	317480.472991	43.582746
3501.902728	317465.650188	43.587751
3501.944598	317460.936887	43.592756
3501.925252	317443.435572	43.597761
3501.958266	317425.900622	43.602765
3501.587834	317422.244034	43.607770
3501.864575	317401.439769	43.612775
3501.841437	317391.520903	43.617780
3501.646995	317380.483901	43.622785
3501.889707	317371.032319	43.627789
3501.948784	317354.587296	43.632794
3501.750325	317346.349596	43.637799
3502.078739	317329.506260	43.642804
3501.672632	317312.574210	43.647809
3501.876323	317299.159669	43.652813
3501.535147	317290.206435	43.657818
3501.616309	317265.361866	43.662823
3501.801946	317248.795247	43.667828
3501.772845	317251.674922	43.672833
3501.766119	317242.084210	43.677837
3501.473668	317216.814614	43.682842
3501.623031	317217.834520	43.687847
3501.673521	317200.245863	43.692852
3501.793502	317198.090030	43.697857
3501.731365	317168.459148	43.702861
3501.738431	317161.817613	43.707866
3501.772139	317165.577967	43.712871
3501.556961	317141.924579	43.717876
3501.415984	317139.987640	43.722881
3501.610644	317127.185083	43.727885
3501.863096	317124.423355	43.732890
3501.727444	317107.474387	43.737895
3501.730509	317098.365525	43.742900
3501.546875	317088.395355	43.747905
3501.902891	317069.563073	43.752909
3501.926930	317059.509543	43.757914
3501.925439	317043.811713	43.762919
3502.117691	317041.059391	43.767924
3501.490030	317015.333231	43.772929
3501.834382	316996.273757	43.777933
3501.796163	316991.216728	43.782938
3501.693140	316974.440708	43.787943
3502.084627	316948.351635	43.792948
3501.896331	316949.449779	43.797953
3502.146987	316928.471271	43.802957
3501.873233	316906.811454	43.807962
3501.679365	316898.114982	43.812967
3501.616439	316878.788374	43.817972
3501.575019	316860.069024	43.822977
3501.680642	316863.945375	43.827981
3501.424330	316861.492155	43.832986
3501.859748	316850.483764	43.837991
3502.078063	316836.608826	43.842996
3501.380142	316825.777613	43.848001
3501.909328	316809.564206	43.853005
3501.519229	316797.260061	43.858010
3501.618174	316787.449188	43.863015
3501.768160	316775.009714	43.868020
3502.059065	316772.114738	43.873025
3501.978260	316748.414690	43.878029
3501.742488	316733.669322	43.883034
3501.921480	316735.625995	43.888039
3502.086744	316722.293616	43.893044
3501.582129	316706.089138	43.898049
3501.825002	316695.441569	43.903053
3501.578689	316672.988616	43.908058
3501.698357	316657.500695	43.913063
3501.804723	316652.039379	43.918068
3501.559747	316639.127313	43.923073
3501.385388	316622.820287	43.928077
3501.507297	316624.658674	43.933082
3501.662259	316611.862175	43.938087
3501.724577	316609.002925	43.943092
3501.589887	316597.981830	43.948097
3501.392711	316571.475707	43.953101
3501.559991	316568.065742	43.958106
3501.571313	316569.488889	43.963111
3501.435823	316563.556513	43.968116
3501.328029	316550.215887	43.973121
3501.570793	316538.041716	43.978125
3501.774986	316531.471041	43.983130
3501.878644	316516.596206	43.988135
3501.593354	316500.560908	43.993140
3501.650929	316495.845050	43.998145
3501.566755	316482.373494	44.003149
3501.525639	316483.982944	44.008154
3501.225264	316474.565191	44.013159
3501.552003	316465.431040	44.018164
3501.358106	316443.707627	44.023169
3501.392684	316437.875862	44.028173
3501.576324	316431.410157	44.033178
3501.420584	316433.699049	44.038183
3501.853248	316423.835923	44.043188
3501.587947	316410.570765	44.048193
3501.346556	316389.618044	44.053197
3501.427917	316396.653176	44.058202
3501.400024	316391.009273	44.063207
3501.180793	316394.656578	44.068212
3501.823309	316387.330391	44.073217
3502.161770	316361.732685	44.078221
3501.733857	316357.881449	44.083226
3501.546795	316338.192367	44.088231
3501.793577	316320.598118	44.093236
3501.554918	316305.522299	44.098241
3501.558767	316302.697614	44.103245
3501.690793	316300.005549	44.108250
3501.277745	316285.618510	44.113255
3501.751371	316271.474492	44.118260
3501.859260	316268.201005	44.123265
3502.060193	316261.172823	44.128269
3501.693786	316244.234159	44.133274
3501.436299	316231.044056	44.138279
3501.858806	316216.195603	44.143284
3501.550298	316213.445189	44.148289
3501.748587	316182.042797	44.153293
3501.642518	316191.422598	44.158298
3501.721351	316179.960926	44.163303
3501.833651	316160.886488	44.168308
3501.658320	316142.162329	44.173313
3501.886012	316140.065937	44.178317
3501.417317	316137.518664	44.183322
3501.591968	316120.240932	44.188327
3502.107775	316098.508171	44.193332
3501.890964	316098.185969	44.198337
3501.664597	316080.334835	44.203341
3501.308540	316065.379062	44.208346
3501.207832	316056.184438	44.213351
3501.661621	316047.691866	44.218356
3501.490436	316047.718737	44.223361
3501.741385	316044.473754	44.228365
3501.550457	316036.005644	44.233370
3501.623929	316022.178541	44.238375
3501.703823	316019.062073	44.243380
3501.682498	316015.986872	44.248385
3501.481447	315989.379237	44.253389
3501.431381	315980.100350	44.258394
3501.306489	315973.911806	44.263399
3501.711855	315959.320382	44.268404
3501.256104	315968.398691	44.273409
3501.572424	315946.951477	44.278413
3501.562904	315935.096462	44.283418
3501.216685	315934.489169	44.288423
3501.661488	315922.156028	44.293428
3501.531758	315916.044562	44.298433
3501.379514	315910.470927	44.303437
3501.342910	315898.696466	44.308442
3501.317053	315888.981238	44.313447
3501.894485	315882.708324	44.318452
3501.293510	315886.491681	44.323457
3501.772049	315878.224199	44.328461
3501.314044	315857.788518	44.333466
3501.143812	315846.314813	44.338471
3501.810467	315828.222191	44.343476
3501.568164	315834.392048	44.348481
3501.272348	315841.155470	44.353485
3501.443369	315830.264495	44.358490
3501.347488	315812.291080	44.363495
3501.722890	315796.559333	44.368500
3501.413310	315795.081233	44.373505
3501.584077	315796.912016	44.378509
3501.519832	315793.309198	44.383514
3501.213099	315773.053377	44.388519
3501.569225	315759.232891	44.393524
3501.155401	315761.231400	44.398529
3501.352762	315741.278407	44.403533
3500.918594	315747.325611	44.408538
3501.335956	315754.104766	44.413543
3501.369220	315743.922281	44.418548
3501.304604	315749.784492	44.423553
3501.661917	315740.569085	44.428557
3501.534098	315734.126530	44.433562
3501.349321	315717.719028	44.438567
3501.285331	315713.607293	44.443572
3501.271316	315715.975838	44.448577
3501.173509	315715.813133	44.453581
3501.195016	315710.822952	44.458586
3501.349553	315712.834381	44.463591
3501.820025	315696.273543	44.468596
3501.557981	315685.221247	44.473601
3501.558323	315675.450990	44.478605
3501.421525	315669.518700	44.483610
3501.692270	315659.833383	44.488615
3501.744797	315641.658593	44.493620
3501.834860	315637.395549	44.498625
3501.548090	315626.067224	44.503629
3501.876094	315618.764640	44.508634
3501.741335	315603.519681	44.513639
3501.702378	315575.512507	44.518644
3501.488096	315581.474469	44.523649
3501.495264	315574.629134	44.528653
3501.464994	315552.803378	44.533658
3501.408797	315553.168482	44.538663
3501.583875	315536.780986	44.543668
3501.648972	315538.831849	44.548673
3501.523685	315527.325591	44.553677
3501.414475	315515.944036	44.558682
3501.353527	315509.236558	44.563687
3501.443403	315500.113800	44.568692
3501.435436	315503.473711	44.573697
3501.406932	315486.838145	44.578701
3501.290291	315492.937516	44.583706
3501.430708	315481.313376	44.588711
3501.677784	315454.406373	44.593716
3501.357908	315454.329272	44.598721
3501.400653	315459.207877	44.603725
3501.576482	315453.532007	44.608730
3501.595030	315446.608543	44.613735
3501.364793	315429.521064	44.618740
3501.430852	315416.560019	44.623745
3501.669700	315413.087891	44.628749
3501.703741	315407.459625	44.633754
3501.114116	315400.758453	44.638759
3501.657111	315379.606300	44.643764
3501.591696	315384.450936	44.648769
3501.244580	315369.060991	44.653773
3501.564334	315373.896298	44.658778
3501.485389	315362.179205	44.663783
3501.480986	315361.900120	44.668788
3501.054886	315336.981124	44.673793
3501.328939	315330.272134	44.678797
3501.425957	315332.165353	44.683802
3501.420933	315330.512405	44.688807
3501.760801	315319.544023	44.693812
3501.573946	315321.252629	44.698817
3501.676605	315304.011284	44.703821
3501.784262	315294.224167	44.708826
3501.511393	315281.265183	44.713831
3501.550007	315283.065760	44.718836
3501.553968	315264.313206	44.723841
3501.536427	315251.924946	44.728845
3501.440430	315249.014030	44.733850
3501.519200	315241.165143	44.738855
3501.329262	315242.060034	44.743860
3501.426763	315224.666803	44.748865
3501.430427	315208.255099	44.753869
3501.459895	315204.790245	44.758874
3501.213078	315205.159709	44.763879
3501.309912	315196.951778	44.768884
3501.187665	315206.410644	44.773889
3501.651416	315199.799197	44.778893
3501.385875	315180.910635	44.783898
3501.428903	315167.775012	44.788903
3501.465875	315160.645073	44.793908
3501.390388	315165.567639	44.798913
3501.330473	315166.391316	44.803917
3501.324432	315158.046798	44.808922
3501.167970	315159.165451	44.813927
3501.355411	315141.605464	44.818932
3501.349533	315123.337822	44.823937
3501.775171	315117.928181	44.828941
3501.647011	315115.658380	44.833946
3501.523429	315112.955318	44.838951
3501.342097	315107.106248	44.843956
3501.067501	315094.987128	44.848961
3501.085037	315082.237124	44.853965
3501.269153	315070.453384	44.858970
3501.445144	315063.581578	44.863975
3501.711342	315062.115213	44.868980
3501.495913	315066.881560	44.873985
3501.503372	315068.178139	44.878989
3501.402107	315051.375681	44.883994
3501.089475	315043.791503	44.888999
3501.340113	315028.078995	44.894004
3501.149867	315028.719499	44.899009
3501.366436	315027.057340	44.904013
3501.286733	315021.217815	44.909018
3501.182802	315014.109881	44.914023
3501.186163	315014.007688	44.919028
3501.217077	315027.717221	44.924033
3501.235499	315000.107823	44.929037
3501.666001	314985.842927	44.934042
3501.597037	314989.059749	44.939047
3501.831657	314980.957457	44.944052
3501.576446	314986.773233	44.949057
3501.576774	314967.435914	44.954061
3501.461274	314958.167047	44.959066
3501.468220	314953.509830	44.964071
3501.579968	314937.284682	44.969076
3501.338496	314942.665768	44.974081
3501.554434	314928.307179	44.979085
3501.350295	314911.368089	44.984090
3501.140964	314917.024037	44.989095
3501.768366	314898.046643	44.994100
3501.265875	314903.773869	44.999105
3501.405123	314897.976429	45.004109
3501.789957	314894.786766	45.009114
3501.406640	314871.540126	45.014119
3501.819245	314854.682701	45.019124
3501.436177	314857.108988	45.024129
3501.451737	314853.544506	45.029133
3501.645816	314827.943060	45.034138
3501.558816	314822.740749	45.039143
3501.590361	314812.507436	45.044148
3501.350303	314818.549860	45.049153
3501.645976	314808.733244	45.054157
3501.510778	314798.729548	45.059162
3501.362972	314793.002416	45.064167
3501.184484	314779.723205	45.069172
3501.344691	314781.733788	45.074177
3500.928894	314778.084074	45.079181
3501.564497	314774.982418	45.084186
3501.208682	314774.376609	45.089191
3501.200553	314772.825902	45.094196
3501.124889	314763.270883	45.099201
3501.453644	314751.846109	45.104205
3501.207451	314738.755579	45.109210
3501.516048	314730.132796	45.114215
3501.540264	314728.449811	45.119220
3501.298809	314728.564000	45.124225
3501.479768	314725.711527	45.129229
3501.405394	314720.558119	45.134234
3501.343145	314697.261195	45.139239
3501.643910	314690.344382	45.144244
3501.264467	314694.245867	45.149249
3501.323156	314689.046208	45.154253
3501.677286	314682.706265	45.159258
3501.144418	314677.649976	45.164263
3501.091586	314663.435099	45.169268
3501.189411	314655.863018	45.174273
3501.050580	314663.594391	45.179277
3501.340977	314656.475641	45.184282
3501.244816	314651.274743	45.189287
3501.637012	314650.806430	45.194292
3501.434676	314653.815131	45.199297
3501.292239	314652.183641	45.204301
3501.855727	314644.131651	45.209306
3501.212680	314625.632650	45.214311
3501.557795	314608.531245	45.219316
3501.466026	314610.250456	45.224321
3501.263116	314610.918390	45.229325
3501.626598	314601.574567	45.234330
3501.154056	314592.768551	45.239335
3501.699644	314569.045759	45.244340
3501.605358	314579.289153	45.249345
3501.519663	314561.008319	45.254349
3501.553616	314577.363704	45.259354
3501.446593	314552.012730	45.264359
3501.621952	314532.444309	45.269364
3501.593195	314528.530511	45.274369
3501.408459	314521.638687	45.279373
3501.672897	314522.818773	45.284378
3500.963548	314514.787645	45.289383
3501.665143	314494.857051	45.294388
3501.487533	314498.141782	45.299393
3501.407238	314485.635903	45.304397
3501.510183	314490.505202	45.309402
3501.126680	314486.824970	45.314407
3501.228049	314492.228843	45.319412
3501.044233	314478.263384	45.324417
3501.122236	314464.969425	45.329421
3501.057439	314458.109729	45.334426
3501.007314	314455.929472	45.339431
3501.156619	314446.593657	45.344436
3501.199540	314447.630268	45.349441
3501.262828	314449.808684	45.354445
3501.363655	314436.231263	45.359450
3501.216019	314443.251612	45.364455
3501.064930	314434.497086	45.369460
3501.084767	314444.188339	45.374465
3501.108530	314435.559143	45.379469
3501.412680	314440.193437	45.384474
3500.989096	314446.010160	45.389479
3501.221080	314433.582667	45.394484
3501.167770	314436.898858	45.399489
3501.023115	314432.723285	45.404493
3501.230350	314429.663132	45.409498
3500.754760	314421.722663	45.414503
3501.100643	314407.445372	45.419508
3500.696146	314423.945691	45.424513
3500.695896	314419.722097	45.429517
3500.977278	314428.889023	45.434522
3500.871260	314432.060790	45.439527
3501.577924	314424.673371	45.444532
3501.270404	314430.421063	45.449537
3501.352024	314410.765468	45.454541
3501.204564	314401.730482	45.459546
3501.103118	314396.632158	45.464551
3501.334519	314388.861040	45.469556
3501.340903	314387.944157	45.474561
3501.330990	314389.090806	45.479565
3501.301716	314396.677875	45.484570
3501.103339	314389.152057	45.489575
3501.146375	314389.959653	45.494580
3501.355142	314388.196914	45.499585
3501.803138	314387.796209	45.504589
3501.860149	314365.014799	45.509594
3501.407359	314357.706860	45.514599
3501.704304	314345.345520	45.519604
3501.763573	314340.730950	45.524609
3501.673599	314317.921607	45.529613
3501.662339	314325.251429	45.534618
3501.557099	314318.143592	45.539623
3501.733461	314286.972314	45.544628
3501.512289	314280.544147	45.549633
3501.410861	314273.664705	45.554637
3501.623920	314276.404933	45.559642
3501.326313	314271.922482	45.564647
3501.349720	314251.792478	45.569652
3501.547023	314236.317035	45.574657
3501.140053	314232.462341	45.579661
3501.173877	314227.266518	45.584666
3501.405374	314227.154101	45.589671
3501.240232	314229.928015	45.594676
3501.536002	314231.255877	45.599681
3501.364525	314222.275500	45.604685
3501.866982	314202.808466	45.609690
3501.532500	314195.303894	45.614695
3501.821183	314186.378790	45.619700
3501.577467	314185.780892	45.624705
3501.575114	314160.464226	45.629709
3501.319767	314149.105175	45.634714
3501.252244	314152.932496	45.639719
3501.465788	314145.978348	45.644724
3501.082489	314147.997598	45.649729
3501.313671	314149.386449	45.654733
3501.330011	314145.134791	45.659738
3501.318767	314134.984349	45.664743
3501.419665	314104.689854	45.669748
3501.174671	314108.392258	45.674753
3501.192263	314099.891185	45.679757
3501.566504	314101.308561	45.684762
3501.054541	314105.917812	45.689767
3501.909324	314093.672748	45.694772
3501.676624	314091.979017	45.699777
3501.186192	314072.718043	45.704781
3501.538319	314063.401331	45.709786
3501.296148	314064.075410	45.714791
3501.465600	314061.555473	45.719796
3501.112072	314061.610851	45.724801
3501.403943	314048.054336	45.729805
3501.556071	314035.690109	45.734810
3501.239832	314033.576880	45.739815
3501.217071	314024.649547	45.744820
3501.263771	314005.915238	45.749825
3501.467243	313944.078908	45.754829
3501.326297	313854.841690	45.759834
3501.394303	313703.639458	45.764839
3501.510932	313511.895693	45.769844
3501.004947	313269.002543	45.774849
3500.697573	312982.209874	45.779853
3500.755432	312632.330587	45.784858
3500.355420	312255.140998	45.789863
3499.956482	311814.741239	45.794868
3499.679097	311333.630357	45.799873
3499.279763	310805.916242	45.804877
3498.947184	310227.572774	45.809882
3498.315973	309601.810696	45.814887
3497.853587	308926.290337	45.819892
3497.560038	308204.470565	45.824897
3496.579890	307441.750890	45.829901
3496.052298	306621.868056	45.834906
3494.922666	305761.220602	45.839911
3494.796029	304863.500298	45.844916
3493.873495	303907.965133	45.849921
3493.055255	302898.263447	45.854925
3492.276281	301844.939122	45.859930
3491.339177	300759.830080	45.864935
3490.685008	299620.926320	45.869940
3489.521608	298436.264351	45.874945
3488.574392	297193.485387	45.879949
3487.570144	295904.286451	45.884954
3486.324489	294578.035388	45.889959
3485.542445	293205.609080	45.894964
3484.412734	291788.837304	45.899969
3483.199808	290319.581351	45.904973
3481.866089	288798.862401	45.909978
3480.430136	287254.117411	45.914983
3479.511386	285644.083709	45.919988
3477.768545	284010.158779	45.924993
3476.528712	282328.865088	45.929997
3475.148624	280605.392879	45.935002
3473.691020	278840.748996	45.940007
3472.221940	277028.454540	45.945012
3470.485890	275182.347573	45.950017
3468.451547	273304.036293	45.955021
3467.052584	271374.353757	45.960026
3465.185040	269423.364406	45.965031
3463.735677	267425.390158	45.970036
3461.738616	265395.171878	45.975041
3459.814057	263329.047632	45.980045
3458.340108	261209.489337	45.985050
3455.977829	259077.934186	45.990055
3454.009725	256892.444738	45.995060
3451.801395	254687.779590	46.000065
3449.793620	252453.608404	46.005069
3448.073202	250167.176838	46.010074
3445.970259	247860.144431	46.015079
3443.760405	245517.622555	46.020084
3441.380348	243144.996694	46.025089
3438.921072	240738.205421	46.030093
3436.726343	238304.710600	46.035098
3433.978899	235854.499232	46.040103
3431.980850	233364.449009	46.045108
3429.250250	230849.413899	46.050113
3426.378497	228316.003358	46.055117
3423.936923	225741.999270	46.060122
3421.348399	223155.104341	46.065127
3418.818774	220546.452893	46.070132
3415.846787	217912.409314	46.075137
3412.854096	215246.698059	46.080141
3410.133681	212564.941652	46.085146
3407.068189	209869.915859	46.090151
3404.298937	207151.007255	46.095156
3401.216334	204402.484744	46.100161
3397.631697	201640.835967	46.105165
3394.720688	198867.691002	46.110170
3391.551949	196080.145288	46.115175
3388.228308	193283.536703	46.120180
3385.080023	190474.636364	46.125185
3381.256291	187652.615902	46.130189
3377.974420	184812.300534	46.135194
3374.300701	181979.230206	46.140199
3370.708753	179124.053962	46.145204
3367.348291	176261.982213	46.150209
3363.296939	173391.701611	46.155213
3359.675869	170525.722505	46.160218
3355.718698	167657.588912	46.165223
3351.776819	164765.231006	46.170228
3347.774783	161898.449947	46.175233
3343.351151	159035.005717	46.180237
3339.087233	156174.010939	46.185242
3333.823107	153346.870500	46.190247
3329.165467	150514.939868	46.195252
3324.222530	147693.622289	46.200257
3319.074997	144891.485324	46.205261
3313.491280	142112.537321	46.210266
3308.002785	139289.086241	46.215271
3302.137980	136587.868586	46.220276
3295.904938	133923.097862	46.225281
3289.579471	131303.417529	46.230285
3283.184274	128723.528905	46.235290
3275.735508	126192.740778	46.240295
3268.950671	123734.677804	46.245300
3261.980978	121325.464791	46.250305
3253.841330	119007.661499	46.255309
3245.767542	116740.954440	46.260314
3237.361165	114586.230544	46.265319
3228.903053	112505.297336	46.270324
3220.396146	110510.565626	46.275329
3210.884938	108615.407044	46.280333
3201.985493	106809.180973	46.285338
3192.853182	105123.838114	46.290343
3183.735854	103530.455224	46.295348
3175.042888	102042.671341	46.300353
3166.252523	100652.966605	46.305357
3157.566282	99367.512877	46.310362
3148.778511	98186.648223	46.315367
3140.745365	97077.425794	46.320372
3132.942183	96066.087423	46.325377
3125.422581	95122.814887	46.330381
3119.135033	94266.541106	46.335386
3111.884417	93486.203675	46.340391
3105.430015	92757.340033	46.345396
3099.692228	92101.471913	46.350401
3094.554468	91493.148702	46.355405
3088.845858	90924.037378	46.360410
3083.663607	90406.124074	46.365415
3078.852800	89925.402951	46.370420
3074.039888	89481.320786	46.375425
3069.508551	89068.723934	46.380429
3065.555476	88660.743398	46.385434
3061.677494	88295.929431	46.390439
3058.007115	87931.163721	46.395444
3054.572388	87582.551869	46.400449
3050.658591	87239.316992	46.405453
3047.249495	86916.271261	46.410458
3043.378242	86599.615549	46.415463
3040.479726	86292.021890	46.420468
3037.358992	85980.820075	46.425473
3033.688967	85675.398967	46.430477
3030.632186	85360.928797	46.435482
3027.268756	85073.391524	46.440487
3023.903509	84758.277416	46.445492
3020.516044	84452.037383	46.450497
3016.952284	84154.822279	46.455501
3014.161365	83852.052330	46.460506
3010.644032	83559.650718	46.465511
3007.168241	83263.460059	46.470516
3004.076514	82959.654117	46.475521
3000.629904	82656.656380	46.480525
2997.410214	82352.330704	46.485530
2993.887920	82067.820873	46.490535
2990.430730	81757.619306	46.495540
2987.223069	81456.527802	46.500545
2983.499725	81149.943892	46.505549
2979.952341	80855.199534	46.510554
2976.345412	80565.713483	46.515559
2972.823688	80253.823822	46.520564
2969.363615	79971.853113	46.525569
2965.713477	79683.043446	46.530573
2962.312656	79381.102638	46.535578
2958.654427	79093.938834	46.540583
2954.679059	78807.958002	46.545588
2951.191763	78534.947734	46.550593
2946.909015	78251.687944	46.555597
2943.561929	77972.501389	46.560602
2939.959890	77707.569541	46.565607
2936.409505	77440.346081	46.570612
2932.905732	77161.776495	46.575617
2929.287215	76911.041253	46.580621
2925.712500	76638.927126	46.585626
2922.357210	76389.019126	46.590631
2918.419746	76118.211536	46.595636
2914.663413	75866.199382	46.600641
2911.008189	75607.773132	46.605645
2907.815907	75359.309584	46.610650
2903.719996	75109.414914	46.615655
2900.399234	74871.173591	46.620660
2896.585254	74625.544385	46.625665
2892.910960	74385.902244	46.630669
2889.789730	74148.067895	46.635674
2886.257182	73911.252398	46.640679
2882.784935	73671.343773	46.645684
2879.160013	73435.181880	46.650689
2875.115202	73192.040072	46.655693
2871.588416	72959.854381	46.660698
2868.442700	72741.210998	46.665703
2864.963416	72503.802865	46.670708
2861.963908	72268.556686	46.675713
2858.244860	72036.193287	46.680717
2854.867196	71794.115479	46.685722
2851.060587	71565.858624	46.690727
2847.617990	71334.778737	46.695732
2844.160769	71097.417900	46.700737
2840.591155	70872.837674	46.705741
2837.625585	70633.893146	46.710746
2833.663266	70403.867740	46.715751
2830.226093	70168.607221	46.720756
2826.861286	69933.032778	46.725761
2822.794886	69709.041786	46.730765
2819.865671	69470.051443	46.735770
2816.248967	69244.007092	46.740775
2813.023657	69010.660145	46.745780
2809.517673	68769.423960	46.750785
2806.055672	68545.513550	46.755789
2802.470117	68305.462200	46.760794
2798.943830	68069.555421	46.765799
2795.574065	67830.147642	46.770804
2792.179982	67589.946061	46.775809
2788.284226	67363.257227	46.780813
2784.777686	67123.109349	46.785818
2781.598747	66882.315802	46.790823
2778.021791	66648.518427	46.795828
2774.547410	66420.883378	46.800833
2770.910062	66186.445886	46.805837
2767.935003	65938.958087	46.810842
2764.025556	65710.153341	46.815847
2760.790512	65471.851068	46.820852
2757.405269	65236.849743	46.825857
2753.812536	64992.869955	46.830861
2750.279899	64748.743488	46.835866
2746.752961	64508.115765	46.840871
2743.504826	64271.343840	46.845876
2740.000641	64020.200132	46.850881
2736.016319	63786.670653	46.855885
2732.601944	63538.634078	46.860890
2728.956315	63316.169421	46.865895
2725.614771	63069.547801	46.870900
2722.136316	62830.984965	46.875905
2718.317392	62594.908435	46.880909
2715.342254	62352.596756	46.885914
2711.466441	62116.736760	46.890919
2708.371389	61879.005269	46.895924
2704.943203	61636.060651	46.900929
2701.208235	61393.439298	46.905933
2697.890557	61139.960047	46.910938
2694.527688	60907.471052	46.915943
2691.064901	60659.483537	46.920948
2687.435941	60420.796153	46.925953
2683.787993	60176.777054	46.930957
2680.539417	59922.049395	46.935962
2677.115808	59689.130889	46.940967
2673.306034	59441.647849	46.945972
2669.983822	59194.674872	46.950977
2666.516070	58947.898500	46.955981
2662.963500	58703.231962	46.960986
2659.327687	58461.880615	46.965991
2656.056310	58213.583437	46.970996
2652.682297	57965.679243	46.976001
2649.026337	57737.194165	46.981005
2645.569225	57477.670535	46.986010
2642.198463	57231.429506	46.991015
2638.352807	56979.719581	46.996020
2635.154334	56740.886852	47.001025
2631.153740	56489.269760	47.006029
2627.783128	56249.288675	47.011034
2624.165208	55995.116995	47.016039
2620.386515	55756.930510	47.021044
2617.357071	55511.478615	47.026049
2613.774486	55275.588468	47.031053
2610.586817	55015.922495	47.036058
2607.149240	54772.483539	47.041063
2603.548774	54531.902228	47.046068
2600.084967	54285.585614	47.051073
2596.455854	54027.871144	47.056077
2593.384462	53785.412866	47.061082
2589.652436	53534.920712	47.066087
2586.302685	53274.569632	47.071092
2582.462579	53017.349667	47.076097
2578.775759	52777.567425	47.081101
2575.545234	52510.950918	47.086106
2572.003538	52267.693721	47.091111
2568.350205	52030.775014	47.096116
2565.292651	51777.125730	47.101121
2561.761398	51520.286283	47.106125
2557.895921	51270.460951	47.111130
2554.560571	51016.222710	47.116135
2551.045568	50756.775610	47.121140
2547.921407	50511.853879	47.126145
2543.968598	50265.332619	47.131149
2541.027845	50014.082151	47.136154
2537.438163	49761.229594	47.141159
2533.893349	49489.083199	47.146164
2530.265263	49237.771112	47.151169
2526.567807	48984.702924	47.156173
2523.339671	48720.197528	47.161178
2519.527259	48469.874146	47.166183
2515.739946	48212.026995	47.171188
2512.362100	47953.909399	47.176193
2508.686722	47702.475712	47.181197
2505.788368	47444.713844	47.186202
2502.119779	47200.775267	47.191207
2498.364891	46946.432138	47.196212
2495.116880	46682.226260	47.201217
2491.643055	46431.460120	47.206221
2488.293410	46171.994796	47.211226
2484.472525	45909.130660	47.216231
2481.080762	45658.201732	47.221236
2477.624872	45401.558778	47.226241
2473.991743	45144.565966	47.231245
2470.719963	44893.544373	47.236250
2467.165062	44641.758130	47.241255
2463.691782	44376.117924	47.246260
2460.413335	44114.033445	47.251265
2456.842108	43851.877357	47.256269
2453.368202	43594.788694	47.261274
2449.777707	43339.312949	47.266279
2446.048144	43067.945050	47.271284
2442.898176	42815.000056	47.276289
2439.166024	42545.160883	47.281293
2435.953519	42291.261458	47.286298
2432.400409	42034.089172	47.291303
2428.859636	41767.552300	47.296308
2425.497226	41498.410000	47.301313
2421.961634	41237.807506	47.306317
2418.522641	40971.099517	47.311322
2414.925956	40707.995597	47.316327
2411.407371	40445.852740	47.321332
2408.237260	40183.538047	47.326337
2404.354190	39917.089929	47.331341
2401.089977	39648.443255	47.336346
2397.225981	39385.764854	47.341351
2394.063652	39118.313456	47.346356
2390.745237	38845.633787	47.351361
2387.110421	38585.623799	47.356365
2383.764260	38310.114868	47.361370
2380.058885	38047.047506	47.366375
2376.675117	37778.030654	47.371380
2373.040464	37498.690907	47.376385
2369.253384	37239.830440	47.381389
2365.956799	36962.917254	47.386394
2362.096905	36703.802051	47.391399
2358.825196	36439.824370	47.396404
2355.957924	36164.166624	47.401409
2352.018563	35899.146313	47.406413
2348.745496	35623.907696	47.411418
2345.255690	35354.677999	47.416423
2341.569269	35074.211660	47.421428
2338.266898	34805.891443	47.426433
2334.557528	34537.327692	47.431437
2331.238884	34264.059888	47.436442
2327.967921	33985.298835	47.441447
2324.628158	33712.865506	47.446452
2321.166951	33428.043824	47.451457
2317.722157	33152.141649	47.456461
2314.462036	32870.788557	47.461466
2310.715173	32593.552882	47.466471
2307.271768	32300.928604	47.471476
2303.949465	32011.616989	47.476481
2300.115330	31739.369050	47.481485
2296.507977	31449.418986	47.486490
2293.106144	31166.057537	47.491495
2289.475160	30889.808761	47.496500
2286.243122	30606.548803	47.501505
2282.462976	30326.281092	47.506509
2279.150609	30034.840666	47.511514
2275.445667	29749.226492	47.516519
2271.924151	29454.962459	47.521524
2269.190532	29173.329913	47.526529
2265.308394	28890.062141	47.531533
2261.587119	28596.019097	47.536538
2258.459971	28308.490457	47.541543
2255.066122	28016.977316	47.546548
2251.916152	27725.455525	47.551553
2248.153256	27434.540728	47.556557
2244.606979	27129.661964	47.561562
2241.474586	26837.129936	47.566567
2238.238959	26528.821538	47.571572
2234.670077	26231.373420	47.576577
2231.034804	25930.746590	47.581581
2227.661406	25621.383726	47.586586
2224.060163	25328.801106	47.591591
2220.312631	25028.591776	47.596596
2217.152835	24706.702343	47.601601
2213.496483	24407.280007	47.606605
2210.034088	24105.772702	47.611610
2206.817594	23801.842950	47.616615
2203.012777	23490.324925	47.621620
2199.919196	23180.005572	47.626625
2196.047369	22877.111054	47.631629
2192.918674	22563.575800	47.636634
2189.198414	22256.378103	47.641639
2185.848013	21941.899075	47.646644
2182.365621	21627.635735	47.651649
2179.008324	21314.618437	47.656653
2175.176883	21001.103826	47.661658
2171.626477	20687.632580	47.666663
2168.195795	20381.375241	47.671668
2164.922720	20064.177532	47.676673
2160.606465	19760.741535	47.681677
2157.202163	19445.436645	47.686682
2153.430362	19152.566325	47.691687
2150.157143	18850.450767	47.696692
2146.200546	18559.632468	47.701697
2142.410758	18262.433278	47.706701
2138.564710	17961.801898	47.711706
2135.006260	17677.445550	47.716711
2131.576925	17386.676318	47.721716
2128.041193	17090.494026	47.726721
2124.178594	16820.495550	47.731725
2120.655455	16524.950124	47.736730
2117.190141	16241.233650	47.741735
2113.334653	15962.202363	47.746740
2109.942749	15693.054839	47.751745
2105.993043	15409.562588	47.756749
2102.344103	15136.714030	47.761754
2099.246986	14863.092758	47.766759
2095.696100	14594.055207	47.771764
2092.555591	14317.776174	47.776769
2088.811511	14056.400771	47.781773
2085.308295	13778.587370	47.786778
2081.613472	13515.552621	47.791783
2077.953469	13234.985512	47.796788
2074.491870	12967.435544	47.801793
2070.791703	12697.738987	47.806797
2067.134696	12436.267799	47.811802
2063.642290	12175.281020	47.816807
2060.106965	11920.579287	47.821812
2056.223095	11660.275064	47.826817
2052.054854	11415.455222	47.831821
2048.206553	11168.768218	47.836826
2044.451462	10936.293306	47.841831
2040.248275	10717.259932	47.846836
2036.510436	10484.354237	47.851841
2032.746998	10270.746459	47.856845
2029.663013	10040.608831	47.861850
2026.032002	9825.222227	47.866855
2022.146140	9616.129782	47.871860
2018.368702	9405.952807	47.876865
2014.711067	9201.795870	47.881869
2011.323875	8994.164444	47.886874
2007.702632	8791.079386	47.891879
2004.159479	8594.726404	47.896884
2000.946884	8388.926131	47.901889
1997.192558	8189.606662	47.906893
1993.863574	7990.400038	47.911898
1990.172455	7793.936279	47.916903
1986.603369	7591.198073	47.921908
1983.238678	7403.157264	47.926913
1979.559692	7206.194624	47.931917
1976.416433	7010.992307	47.936922
1972.826403	6815.573957	47.941927
1968.965745	6620.475386	47.946932
1965.596705	6421.383793	47.951937
1961.763825	6238.099593	47.956941
1958.955800	6036.085495	47.961946
1955.565054	5850.447806	47.966951
1951.995189	5658.731988	47.971956
1948.489819	5463.235704	47.976961
1945.098350	5277.236844	47.981965
1941.397920	5075.664161	47.986970
1938.035505	4889.357740	47.991975
1934.296733	4701.979184	47.996980
1931.321865	4506.824718	48.001985
1927.588133	4313.079069	48.006989
1924.231188	4115.868341	48.011994
1920.496592	3928.443321	48.016999
1916.851444	3733.629901	48.022004
1913.386678	3543.843932	48.027009
1909.944348	3353.879238	48.032013
1906.227038	3165.737939	48.037018
1902.595356	2970.474972	48.042023
1899.047208	2788.715722	48.047028
1895.800218	2604.484195	48.052033
1892.245033	2412.376400	48.057037
1888.922500	2219.794428	48.062042
1885.019277	2039.085544	48.067047
1881.117805	1862.814311	48.072052
1877.714292	1673.345391	48.077057
1873.820379	1490.030209	48.082061
1870.477065	1317.559303	48.087066
1866.934959	1150.816369	48.092071
1862.744911	977.009992	48.097076
1859.609262	799.272058	48.102081
1855.459653	644.392453	48.107085
1852.084224	490.911711	48.112090
1848.432299	344.167121	48.117095
1844.036351	201.820840	48.122100
1839.795522	77.323788	48.127105
1832.119379	32.339882	48.132109
1823.722536	55.987318	48.137114
1818.139463	55.342503	48.142119
1814.149594	59.317465	48.147124
1811.968831	49.847883	48.152129
1809.006308	49.482687	48.157133
1806.394470	54.551814	48.162138
1804.116004	61.593610	48.167143
1800.739314	62.416382	48.172148
1797.176456	60.281655	48.177153
1793.444502	58.692256	48.182157
1790.170380	51.931156	48.187162
1787.138591	43.676786	48.192167
1783.788325	61.393312	48.197172
1780.612377	51.465701	48.202177
1776.448425	57.783824	48.207181
1773.198514	58.488686	48.212186
1770.004233	60.466185	48.217191
1766.331339	60.212171	48.222196
1763.457647	60.772736	48.227201
1759.922454	66.416657	48.232205
1756.331994	60.344161	48.237210
1753.004197	59.621686	48.242215
1749.160996	68.072652	48.247220
1746.080921	52.080852	48.252225
1742.243123	55.601762	48.257229
1738.776129	51.819532	48.262234
1735.608500	52.998754	48.267239
1731.897693	52.393176	48.272244
1729.309674	54.123943	48.277249
1725.387935	60.989483	48.282253
1721.726436	59.404904	48.287258
1718.531294	51.713967	48.292263
1714.970926	61.243826	48.297268
1711.710412	56.106819	48.302273
1708.107249	59.812488	48.307277
1704.601363	62.756275	48.312282
1701.146107	60.095371	48.317287
1697.172002	58.632492	48.322292
1693.912085	55.020352	48.327297
1690.375398	60.392438	48.332301
1687.126470	63.545957	48.337306
1683.691110	60.578219	48.342311
1680.297418	60.837369	48.347316
1676.791777	55.583713	48.352321
1673.500520	56.510215	48.357325
1669.749183	57.489741	48.362330
1666.305848	55.918495	48.367335
1662.352213	61.526690	48.372340
1659.159610	56.201901	48.377345
1655.698956	52.020070	48.382349
1652.340573	58.208996	48.387354
1649.098338	53.920215	48.392359
1645.165726	55.738053	48.397364
1642.209431	50.256064	48.402369
1638.224843	51.702383	48.407373
1634.981824	55.041655	48.412378
1631.539220	51.002543	48.417383
1628.148881	59.224473	48.422388
1624.902926	53.626469	48.427393
1621.185153	59.672333	48.432397
1617.468355	50.936766	48.437402
1614.452609	51.503786	48.442407
1610.294361	63.433659	48.447412
1606.348530	50.383716	48.452417
1603.135407	56.284160	48.457421
1599.700859	51.019408	48.462426
1596.598589	59.234226	48.467431
1593.019445	54.757746	48.472436
1589.961878	42.033871	48.477441
1585.865144	58.509991	48.482445
1582.172995	62.232791	48.487450
1579.201359	49.485974	48.492455
1575.585941	55.515830	48.497460
1572.126549	52.466473	48.502465
1568.624846	54.666155	48.507469
1565.581388	53.326592	48.512474
1562.126310	47.599990	48.517479
1557.818610	50.365595	48.522484
1554.345524	51.108619	48.527489
1550.985870	55.782312	48.532493
1547.619766	64.392783	48.537498
1544.406289	53.819395	48.542503
1541.308923	53.453236	48.547508
1537.224126	53.162533	48.552513
1533.429995	49.210117	48.557517
1529.861223	54.685349	48.562522
1526.514095	48.492605	48.567527
1522.865877	54.587723	48.572532
1519.871824	55.559505	48.577537
1516.189503	41.984308	48.582541
1512.761741	51.521934	48.587546
1509.374174	45.999925	48.592551
1505.582508	58.008492	48.597556
1502.562190	50.685749	48.602561
1498.726098	55.921254	48.607565
1495.345224	53.884706	48.612570
1491.362582	49.759330	48.617575
1488.026196	56.587108	48.622580
1484.457221	54.108600	48.627585
1480.977828	56.981872	48.632589
1477.810588	49.289824	48.637594
1474.524487	51.848100	48.642599
1470.587273	54.831001	48.647604
1467.478708	51.445192	48.652609
1464.155078	51.237860	48.657613
1460.331257	49.770538	48.662618
1456.560827	49.174394	48.667623
1452.999685	55.869681	48.672628
1449.762364	48.448045	48.677633
1446.093121	58.722689	48.682637
1442.304107	57.825735	48.687642
1439.570487	60.525338	48.692647
1435.553560	60.211398	48.697652
1432.384019	50.320889	48.702657
1428.653854	51.385774	48.707661
1425.410543	50.666003	48.712666
1422.030815	50.907235	48.717671
1417.750748	44.844749	48.722676
1414.867772	45.156924	48.727681
1411.172997	49.465491	48.732685
1407.426577	55.319750	48.737690
1404.436923	56.898326	48.742695
1400.947376	60.772972	48.747700
1397.403671	56.968074	48.752705
1394.081143	58.981578	48.757709
1390.345759	57.633318	48.762714
1386.943317	57.409875	48.767719
1383.088534	58.155757	48.772724
1379.478659	52.213008	48.777729
1376.180332	55.178195	48.782733
1372.777059	51.044437	48.787738
1369.328559	65.834088	48.792743
1365.552143	66.744883	48.797748
1362.134102	58.405591	48.802753
1358.635707	52.502348	48.807757
1355.217311	56.758182	48.812762
1352.003569	53.600849	48.817767
1348.326981	57.460498	48.822772
1344.709397	47.447170	48.827777
1340.729438	52.866602	48.832781
1337.014670	61.427301	48.837786
1334.063718	48.500175	48.842791
1330.951315	52.616365	48.847796
1327.542689	49.907169	48.852801
1323.990711	50.086811	48.857805
1320.304539	61.177236	48.862810
1316.496260	53.408425	48.867815
1313.093048	60.632696	48.872820
1309.653693	55.688351	48.877825
1306.297946	54.935601	48.882829
1303.005380	49.601281	48.887834
1299.704945	48.463384	48.892839
1295.491014	55.463389	48.897844
1292.467667	50.469748	48.902849
1288.830337	47.846990	48.907853
1285.042539	46.022918	48.912858
1281.591452	44.348619	48.917863
1277.781238	49.228966	48.922868
1274.466527	54.164627	48.927873
1271.437874	48.327092	48.932877
1267.637913	49.906005	48.937882
1264.421277	39.333236	48.942887
1260.795773	46.411980	48.947892
1257.261315	53.992173	48.952897
1253.827310	49.290626	48.957901
1250.177158	52.124264	48.962906
1246.540555	37.479012	48.967911
1242.940425	55.263216	48.972916
1239.595352	50.886278	48.977921
1236.481899	47.906279	48.982925
1232.683749	51.478109	48.987930
1229.528052	47.368925	48.992935
1225.461643	52.485553	48.997940
1222.129624	54.921381	49.002945
1218.733632	57.322932	49.007949
1215.190341	49.095065	49.012954
1212.037845	47.320262	49.017959
1207.972613	50.782051	49.022964
1204.477168	55.049993	49.027969
1201.086038	53.059449	49.032973
1197.677680	51.141207	49.037978
1194.437620	56.859315	49.042983
1190.761411	50.547377	49.047988
1187.332156	50.666726	49.052993
1183.449822	52.824884	49.057997
1179.940336	59.284375	49.063002
1176.740328	50.572505	49.068007
1173.270429	52.254807	49.073012
1169.625980	53.470885	49.078017
1166.066423	54.483847	49.083021
1162.055716	52.055635	49.088026
1159.072375	55.525239	49.093031
1155.415066	62.707078	49.098036
1152.183798	59.951197	49.103041
1148.838108	49.019021	49.108045
1144.771847	52.756245	49.113050
1142.008070	50.876316	49.118055
1138.098513	52.307919	49.123060
1135.003622	53.684747	49.128065
1131.410327	53.551385	49.133069
1127.366272	51.080953	49.138074
1124.368649	52.667185	49.143079
1120.357553	53.529391	49.148084
1116.746375	49.162524	49.153089
1113.798199	45.707435	49.158093
1110.215278	51.871554	49.163098
1107.034721	47.845401	49.168103
1102.951337	37.936754	49.173108
1099.044018	55.797558	49.178113
1096.111289	48.255607	49.183117
1092.435446	57.711964	49.188122
1089.290039	43.853596	49.193127
1085.449366	56.091416	49.198132
1082.118962	40.933228	49.203137
1078.682088	50.054775	49.208141
1075.107597	52.240709	49.213146
1071.454283	47.136968	49.218151
1068.000908	51.698926	49.223156
1064.428875	46.329361	49.228161
1060.963603	43.898057	49.233165
1057.699077	44.741478	49.238170
1054.126132	51.040096	49.243175
1050.714377	44.487497	49.248180
1047.403383	48.536782	49.253185
1043.642416	43.861202	49.258189
1039.916858	52.100972	49.263194
1036.414333	51.333331	49.268199
1032.291760	53.722153	49.273204
1029.383112	54.680708	49.278209
1026.181662	46.298162	49.283213
1022.609170	48.929894	49.288218
1019.397263	47.888966	49.293223
1015.657085	54.381461	49.298228
1011.879080	44.035898	49.303233
1008.572168	44.642361	49.308237
1005.136762	47.730366	49.313242
1001.739523	50.423252	49.318247
998.259844	53.543503	49.323252
994.224314	42.371394	49.328257
991.123344	52.130078	49.333261
987.362287	50.596171	49.338266
984.221363	36.224622	49.343271
980.343435	39.951402	49.348276
976.782399	41.543636	49.353281
973.461890	38.191186	49.358285
970.135227	42.948471	49.363290
966.727072	44.535754	49.368295
962.611237	47.499356	49.373300
959.392899	39.268183	49.378305
955.942286	41.713173	49.383309
952.223104	38.290277	49.388314
949.559454	37.400812	49.393319
945.262881	43.344527	49.398324
941.623432	38.482286	49.403329
938.339173	39.161156	49.408333
934.918329	42.655032	49.413338
932.004766	42.478589	49.418343
927.946255	39.880796	49.423348
924.237423	37.465536	49.428353
921.015285	38.928794	49.433357
917.369896	45.102754	49.438362
913.991254	35.099676	49.443367
910.545943	56.061455	49.448372
907.302976	40.196793	49.453377
903.908319	41.032168	49.458381
899.988456	40.874097	49.463386
896.354788	35.134604	49.468391
892.650293	41.577257	49.473396
889.328363	36.532441	49.478401
885.937365	37.547584	49.483405
881.902583	42.747974	49.488410
878.709803	38.951613	49.493415
875.156344	44.494256	49.498420
871.966591	41.317525	49.503425
868.485952	38.366679	49.508429
864.740340	40.247285	49.513434
861.260614	43.471993	49.518439
858.061409	44.143900	49.523444
854.349908	39.321452	49.528449
851.571575	40.085647	49.533453
847.490553	47.457315	49.538458
843.916335	36.219381	49.543463
840.020010	38.686748	49.548468
836.824558	41.572719	49.553473
833.523237	43.652687	49.558477
829.535467	37.433992	49.563482
826.334837	35.084728	49.568487
822.954579	35.266139	49.573492
819.359547	37.695826	49.578497
815.543572	34.939883	49.583501
811.920591	30.264947	49.588506
808.554848	34.183672	49.593511
805.431151	44.774865	49.598516
801.988468	43.118413	49.603521
798.850608	36.187673	49.608525
794.809844	46.536496	49.613530
791.372306	33.663659	49.618535
787.543008	40.549836	49.623540
784.214531	48.221302	49.628545
780.974193	46.267414	49.633549
777.261761	47.896084	49.638554
774.054921	39.849850	49.643559
770.783809	43.832864	49.648564
766.852219	36.203851	49.653569
763.432195	38.754850	49.658573
759.441352	39.765896	49.663578
756.053825	42.982529	49.668583
752.895998	35.267155	49.673588
749.192813	35.369448	49.678593
745.761179	47.979911	49.683597
742.143163	42.798020	49.688602
739.009429	38.967155	49.693607
735.501960	47.419643	49.698612
731.499063	47.413853	49.703617
728.085314	42.073429	49.708621
724.540619	44.049176	49.713626
721.219450	32.325584	49.718631
717.666379	45.277774	49.723636
714.209365	32.297294	49.728641
711.052848	43.080311	49.733645
707.318705	36.106945	49.738650
704.031250	39.263631	49.743655
700.444977	41.802722	49.748660
696.295308	44.031410	49.753665
693.097242	38.470563	49.758669
690.062300	34.320524	49.763674
686.654149	32.541651	49.768679
682.704236	41.661394	49.773684
679.186467	42.373760	49.778689
675.738151	37.858190	49.783693
672.072838	45.949435	49.788698
668.574271	41.324677	49.793703
664.984177	43.538512	49.798708
661.670410	40.295858	49.803713
657.956313	37.666398	49.808717
654.853019	38.190476	49.813722
651.381074	33.397042	49.818727
647.744094	41.199117	49.823732
644.380255	38.907116	49.828737
640.351002	37.446995	49.833741
636.909418	42.965869	49.838746
634.020612	33.585397	49.843751
630.292256	39.225114	49.848756
626.847169	38.122768	49.853761
623.518538	34.278178	49.858765
619.780367	32.854738	49.863770
616.143046	24.224260	49.868775
612.388814	30.478641	49.873780
608.859710	37.226116	49.878785
605.612446	35.498007	49.883789
602.174588	38.210044	49.888794
598.698093	34.477208	49.893799
595.477151	39.341439	49.898804
591.966962	30.358863	49.903809
588.596401	40.612281	49.908813
584.741720	39.438058	49.913818
580.811427	33.153537	49.918823
577.140017	35.886342	49.923828
573.882746	33.935185	49.928833
570.350323	35.368062	49.933837
567.099427	35.507160	49.938842
563.858839	33.192724	49.943847
559.936816	36.993011	49.948852
556.396472	32.627948	49.953857
553.064498	33.545381	49.958861
549.444082	30.315999	49.963866
546.061468	35.607365	49.968871
542.353689	41.449536	49.973876
539.130785	43.049085	49.978881
535.646170	35.856383	49.983885
531.874668	42.312819	49.988890
528.295507	27.624147	49.993895
525.294578	24.544525	49.998900
521.443810	42.947106	50.003905
518.389977	27.913568	50.008909
514.754493	36.110921	50.013914
511.048644	25.086763	50.018919
507.557782	31.597325	50.023924
503.894219	25.875347	50.028929
500.648499	27.737910	50.033933
496.944457	34.044584	50.038938
493.551547	43.036024	50.043943
490.023978	48.381753	50.048948
486.291715	36.975758	50.053953
483.029656	31.921731	50.058957
479.494681	36.771909	50.063962
475.960293	29.833806	50.068967
472.706822	36.519172	50.073972
468.957107	40.482333	50.078977
465.991354	28.801271	50.083981
461.465134	32.205848	50.088986
458.514845	24.837745	50.093991
454.747241	31.394835	50.098996
451.386070	25.192082	50.104001
448.331626	27.736550	50.109005
444.652465	38.664769	50.114010
441.154996	27.234682	50.119015
437.455469	31.693031	50.124020
434.231132	38.949651	50.129025
430.756188	31.600459	50.134029
426.837269	39.861221	50.139034
423.121290	34.805551	50.144039
419.923533	36.410692	50.149044
416.692692	43.934094	50.154049
413.178322	32.728128	50.159053
409.191012	36.298255	50.164058
406.275851	37.776879	50.169063
402.289375	41.891047	50.174068
398.600524	36.340754	50.179073
395.453238	39.165539	50.184077
391.849349	47.987579	50.189082
388.180465	40.260655	50.194087
384.804716	41.017326	50.199092
381.286597	41.030669	50.204097
378.171221	37.067352	50.209101
373.804398	44.601027	50.214106
370.846777	42.941531	50.219111
367.494240	41.030684	50.224116
363.945717	35.053465	50.229121
361.129880	32.473256	50.234125
356.907380	38.329681	50.239130
353.681502	30.704229	50.244135
349.967369	33.323590	50.249140
346.198006	31.250254	50.254145
343.423876	32.289189	50.259149
339.106772	30.817350	50.264154
335.587266	30.954315	50.269159
332.343588	27.862167	50.274164
328.688189	36.834661	50.279169
325.650119	31.710810	50.284173
321.748029	33.701563	50.289178
318.040065	35.715692	50.294183
314.671165	30.561412	50.299188
311.491684	35.219920	50.304193
308.216626	29.788351	50.309197
304.275702	39.954025	50.314202
300.886050	29.987756	50.319207
297.310371	39.963340	50.324212
293.634069	35.600705	50.329217
290.147818	31.610099	50.334221
286.406934	31.123700	50.339226
283.147048	28.385288	50.344231
280.115442	31.714009	50.349236
276.936398	29.326768	50.354241
273.358611	25.723833	50.359245
269.517584	33.874372	50.364250
265.675644	29.623121	50.369255
262.059180	34.897429	50.374260
258.615818	27.593991	50.379265
255.314030	37.058445	50.384269
251.381388	35.586533	50.389274
248.199808	30.197292	50.394279
244.861760	32.276889	50.399284
241.148626	32.747945	50.404289
237.760596	29.463312	50.409293
234.250833	35.660552	50.414298
230.870353	29.745656	50.419303
227.249781	31.012139	50.424308
223.627074	30.890069	50.429313
220.362303	27.152700	50.434317
216.519468	33.715336	50.439322
213.190733	34.562783	50.444327
210.019598	37.211031	50.449332
206.250991	40.541338	50.454337
202.466545	34.506240	50.459341
199.199937	40.946976	50.464346
195.997516	38.186939	50.469351
192.417475	34.562245	50.474356
188.793600	32.928095	50.479361
185.514992	33.581039	50.484365
181.654722	37.561631	50.489370
178.113848	33.143031	50.494375
174.374326	37.459051	50.499380
171.075739	38.659295	50.504385
168.058239	40.005331	50.509389
164.286271	38.818336	50.514394
160.747692	35.804092	50.519399
157.098260	44.212563	50.524404
153.355501	31.577687	50.529409
150.200130	37.469500	50.534413
146.477685	40.020643	50.539418
143.261522	36.677485	50.544423
140.003572	33.584484	50.549428
136.170457	29.034519	50.554433
132.639047	26.221647	50.559437
128.838893	40.965430	50.564442
125.743245	29.646553	50.569447
122.393594	46.062992	50.574452
118.665396	38.244253	50.579457
115.169282	29.167949	50.584461
111.624594	46.817175	50.589466
107.871816	36.468123	50.594471
105.024018	51.831510	50.599476
101.096436	43.759276	50.604481
97.514745	45.870771	50.609485
94.173941	44.711169	50.614490
90.760343	47.096888	50.619495
87.172927	43.030468	50.624500
83.710489	37.425868	50.629505
79.955510	33.420507	50.634509
76.372268	47.779151	50.639514
73.152654	32.230794	50.644519
69.814125	38.511996	50.649524
66.066588	47.391451	50.654529
62.696349	29.867205	50.659533
58.842075	43.262242	50.664538
55.596320	38.563340	50.669543
52.149243	43.029742	50.674548
48.505600	44.812442	50.679553
45.252839	41.395962	50.684557
41.684453	47.479072	50.689562
37.936964	38.704777	50.694567
34.705159	45.608350	50.699572
31.246300	46.305411	50.704577
27.666188	40.349112	50.709581
24.151374	47.752611	50.714586
20.187824	41.821591	50.719591
16.784984	36.669591	50.724596
13.495870	43.803612	50.729601
10.214809	45.662396	50.734605
6.463699	48.784400	50.739610
3.235531	35.967736	50.744615