Thu Aug 25 10:04:51 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.046132	104.473814	0.000000
1.177289	103.978796	0.005005
1.197178	113.005156	0.010010
1.196387	98.028124	0.015014
0.965009	83.264404	0.020019
0.468249	87.942439	0.025024
0.654248	79.985013	0.030029
0.618502	74.485772	0.035034
0.264008	67.438777	0.040038
0.330928	56.978506	0.045043
-0.287043	48.422562	0.050048
-0.669666	39.133722	0.055053
-1.124523	30.305457	0.060058
-1.614718	26.794666	0.065062
-1.627703	25.705303	0.070067
-1.570124	33.925290	0.075072
-1.604128	19.586278	0.080077
-2.139229	18.028229	0.085082
-2.549945	15.001697	0.090086
-2.926202	3.060659	0.095091
-3.284818	3.629470	0.100096
-3.419902	6.725892	0.105101
-3.667909	8.517561	0.110106
-3.952758	1.273020	0.115110
-4.509444	-0.389212	0.120115
-4.982421	2.611454	0.125120
-4.987266	-3.183668	0.130125
-4.897440	1.614408	0.135130
-4.943910	3.421955	0.140134
-5.180222	-4.244638	0.145139
-6.128676	0.393415	0.150144
-6.420541	0.331674	0.155149
-6.312633	6.038076	0.160154
-6.534616	-7.569109	0.165158
-6.228932	-9.331656	0.170163
-6.947975	2.581863	0.175168
-7.614982	-1.714301	0.180173
-7.522965	-4.942985	0.185178
-7.961400	4.205751	0.190182
-7.450743	-2.068774	0.195187
-8.240487	2.965191	0.200192
-8.791252	4.057653	0.205197
-8.538308	5.122264	0.210202
-9.014744	6.275846	0.215206
-8.894654	1.970253	0.220211
-10.192849	6.476445	0.225216
-10.233122	5.106623	0.230221
-10.473723	5.603160	0.235226
-10.533375	5.919486	0.240230
-10.329168	-8.475809	0.245235
-10.711800	-2.062965	0.250240
-10.806494	-1.734822	0.255245
-11.356965	5.213684	0.260250
-11.700529	-1.363597	0.265254
-11.842155	1.759159	0.270259
-11.878884	1.015202	0.275264
-12.023839	0.724800	0.280269
-11.967572	-0.223552	0.285274
-13.066647	7.867602	0.290278
-13.214304	-1.802878	0.295283
-13.379924	14.595546	0.300288
-13.409919	2.527491	0.305293
-13.743248	9.347064	0.310298
-14.735669	7.076063	0.315302
-14.648403	-0.157178	0.320307
-14.941833	-7.561720	0.325312
-14.925581	-0.695685	0.330317
-15.057813	-2.000479	0.335322
-15.247478	6.134847	0.340326
-15.258986	1.451241	0.345331
-15.899984	8.837874	0.350336
-16.264169	6.449457	0.355341
-16.707072	1.431648	0.360346
-16.732277	2.498711	0.365350
-16.413285	-0.626332	0.370355
-16.483032	1.668915	0.375360
-17.363604	-0.989767	0.380365
-17.882080	-2.496633	0.385370
-17.959112	6.870723	0.390374
-17.873019	0.694356	0.395379
-17.974296	-1.017083	0.400384
-18.653038	-0.192469	0.405389
-19.015762	-7.206505	0.410394
-19.142355	-1.140662	0.415398
-19.350845	3.296032	0.420403
-19.392943	6.222860	0.425408
-19.442301	-4.399488	0.430413
-20.230630	-6.598061	0.435418
-20.770729	12.443813	0.440422
-20.661204	5.684808	0.445427
-20.575965	4.643332	0.450432
-20.913093	6.654608	0.455437
-21.599245	6.249687	0.460442
-22.179360	4.407630	0.465446
-22.230495	-0.516538	0.470451
-22.534555	8.218840	0.475456
-22.566434	0.137402	0.480461
-22.215248	3.742924	0.485466
-22.516065	3.850265	0.490470
-22.622379	-5.352129	0.495475
-23.721372	-0.946751	0.500480
-23.934579	5.006116	0.505485
-24.051331	3.395177	0.510490
-24.021812	8.582353	0.515494
-24.277353	5.139206	0.520499
-24.359955	7.866737	0.525504
-24.536957	2.478236	0.530509
-24.853149	-6.083833	0.535514
-25.663480	1.484352	0.540518
-25.359247	1.063458	0.545523
-25.832672	1.849575	0.550528
-26.501024	1.233058	0.555533
-26.339447	-7.214046	0.560538
-26.652528	-1.207568	0.565542
-26.427278	-0.511940	0.570547
-27.121595	2.596174	0.575552
-27.461599	-4.187306	0.580557
-27.766862	1.185200	0.585562
-28.359752	0.291105	0.590566
-28.343431	-1.125549	0.595571
-28.122793	-1.280246	0.600576
-28.217100	-3.207911	0.605581
-28.267033	-9.891305	0.610586
-29.306721	2.815932	0.615590
-29.201082	-6.894231	0.620595
-29.498259	2.668966	0.625600
-29.805910	-0.674266	0.630605
-29.729368	-0.828531	0.635610
-30.295568	1.686871	0.640614
-30.530778	-7.476342	0.645619
-30.714723	-3.467437	0.650624
-31.224440	-2.065032	0.655629
-31.645541	2.091764	0.660634
-32.210471	-3.061945	0.665638
-31.997573	-1.459552	0.670643
-32.123678	-1.066376	0.675648
-32.512135	-3.058683	0.680653
-32.351748	-12.992555	0.685658
-32.587758	-6.624834	0.690662
-33.010747	-12.186758	0.695667
-33.340974	-11.075066	0.700672
-33.871533	-9.969951	0.705677
-33.851959	-7.394473	0.710682
-34.025561	-1.780007	0.715686
-34.435033	-5.015536	0.720691
-34.930191	-5.501002	0.725696
-35.469160	-3.420136	0.730701
-34.881093	-2.249848	0.735706
-35.304709	-0.547722	0.740710
-35.198602	-6.486777	0.745715
-35.833589	4.651111	0.750720
-36.349265	6.215802	0.755725
-36.411153	-3.120102	0.760730
-36.738799	1.838296	0.765734
-36.554588	-2.186278	0.770739
-36.863961	0.295211	0.775744
-38.095169	8.327976	0.780749
-38.022014	-3.057047	0.785754
-38.501530	7.401587	0.790758
-38.157712	-4.095447	0.795763
-38.091034	-3.384465	0.800768
-38.670460	7.637152	0.805773
-38.611592	-2.170088	0.810778
-38.948122	5.137200	0.815782
-39.370728	3.336904	0.820787
-39.633157	4.282949	0.825792
-39.615831	2.141641	0.830797
-39.941992	9.282791	0.835802
-40.936744	2.304509	0.840806
-41.051166	-4.371946	0.845811
-41.188385	1.977136	0.850816
-41.037282	-5.259777	0.855821
-41.158010	4.959142	0.860826
-41.443315	5.168457	0.865830
-41.534377	-3.235899	0.870835
-42.026434	6.183829	0.875840
-42.178347	3.999435	0.880845
-42.507296	2.801394	0.885850
-43.009522	4.281720	0.890854
-43.682361	0.119352	0.895859
-44.119008	2.212660	0.900864
-43.989601	3.227024	0.905869
-44.105057	-0.949912	0.910874
-44.289648	2.448493	0.915878
-44.378272	3.525493	0.920883
-44.850234	6.620914	0.925888
-44.691672	0.958375	0.930893
-44.204870	3.207547	0.935898
-45.433073	7.468660	0.940902
-45.813155	6.778503	0.945907
-45.949022	4.003139	0.950912
-46.201537	6.349169	0.955917
-46.413297	-2.754444	0.960922
-47.182443	1.681512	0.965926
-47.071336	-10.842072	0.970931
-47.632000	1.701524	0.975936
-47.684878	6.705456	0.980941
-47.272531	-4.337244	0.985946
-47.434211	5.951366	0.990950
-47.426875	-9.849415	0.995955
-48.366004	-5.446938	1.000960
-48.741701	-3.325216	1.005965
-48.942611	1.869588	1.010970
-49.066051	-1.973904	1.015974
-49.963506	-2.276112	1.020979
-50.107964	0.138408	1.025984
-50.573554	0.587941	1.030989
-50.526013	-5.854463	1.035994
-50.637724	7.767231	1.040998
-50.217020	-9.933292	1.046003
-50.453137	2.692330	1.051008
-50.531544	-0.161639	1.056013
-51.302465	5.286993	1.061018
-52.116767	-3.832939	1.066022
-51.645711	-2.479804	1.071027
-51.481451	-2.195398	1.076032
-52.391137	-2.435579	1.081037
-52.646291	-2.936503	1.086042
-52.923863	-5.945926	1.091046
-53.013020	-7.437801	1.096051
-53.529635	-2.402338	1.101056
-54.081739	-0.515565	1.106061
-53.991390	2.118427	1.111066
-54.551170	5.863521	1.116070
-54.426534	6.337632	1.121075
-54.714533	10.261604	1.126080
-54.628197	2.924107	1.131085
-54.546410	7.470342	1.136090
-55.490623	8.399829	1.141094
-55.828609	-3.816111	1.146099
-56.027267	3.317714	1.151104
-56.205677	12.802195	1.156109
-56.293999	9.000655	1.161114
-57.067961	16.079095	1.166118
-57.463432	7.007427	1.171123
-57.427627	0.468784	1.176128
-57.500350	5.532772	1.181133
-57.210176	1.637127	1.186138
-58.006431	11.961895	1.191142
-57.766111	-1.489935	1.196147
-58.464057	2.248334	1.201152
-59.124594	8.296602	1.206157
-58.721725	6.091719	1.211162
-59.066456	6.092046	1.216166
-58.895629	10.583202	1.221171
-59.792056	5.962324	1.226176
-60.184318	8.263813	1.231181
-60.222878	0.063202	1.236186
-60.522776	21.804082	1.241190
-60.658482	4.374227	1.246195
-61.220111	7.357149	1.251200
-61.938575	13.379694	1.256205
-61.602449	12.469748	1.261210
-61.881744	13.788596	1.266214
-62.307922	5.952437	1.271219
-62.088553	4.187593	1.276224
-62.268067	14.390417	1.281229
-61.937753	1.538251	1.286234
-62.772049	11.505149	1.291238
-63.288485	15.376331	1.296243
-63.758950	8.714532	1.301248
-63.693001	16.009380	1.306253
-63.459494	12.100465	1.311258
-64.304444	9.967715	1.316262
-64.941936	17.309510	1.321267
-64.995793	12.069393	1.326272
-65.241418	10.753893	1.331277
-65.089967	11.568651	1.336282
-64.979875	12.196901	1.341286
-65.368334	13.985268	1.346291
-66.102852	7.586306	1.351296
-66.601787	8.822510	1.356301
-66.380817	2.346602	1.361306
-66.662377	6.494190	1.366310
-66.516077	0.257773	1.371315
-67.203864	8.161099	1.376320
-67.438831	12.529178	1.381325
-67.577505	6.615820	1.386330
-67.880595	12.696666	1.391334
-68.217435	4.017609	1.396339
-68.731472	2.905518	1.401344
-69.431510	3.837876	1.406349
-69.784037	2.330321	1.411354
-69.692338	15.531005	1.416358
-69.208474	13.674097	1.421363
-69.141882	5.966371	1.426368
-69.748205	12.271900	1.431373
-69.864880	11.205114	1.436378
-70.743898	11.070860	1.441382
-70.684452	11.229321	1.446387
-71.071972	16.089537	1.451392
-71.319567	18.729027	1.456397
-70.906084	11.099822	1.461402
-71.670899	14.355027	1.466406
-72.261291	3.165723	1.471411
-72.293001	8.903490	1.476416
-72.737768	10.871522	1.481421
-72.346605	6.960052	1.486426
-72.593576	11.570455	1.491430
-73.427874	16.060916	1.496435
-73.626841	14.636866	1.501440
-74.351341	9.046254	1.506445
-73.906768	2.845357	1.511450
-73.858350	8.349106	1.516454
-74.323926	10.813944	1.521459
-74.514310	3.149648	1.526464
-75.392106	9.396473	1.531469
-75.339576	11.602959	1.536474
-75.631240	23.133150	1.541478
-75.552354	14.183306	1.546483
-75.469341	15.831361	1.551488
-76.226082	22.467345	1.556493
-76.428320	-0.899918	1.561498
-77.001855	24.702476	1.566502
-76.732691	14.140944	1.571507
-76.968397	8.226971	1.576512
-77.757055	11.447947	1.581517
-77.970760	14.445957	1.586522
-78.227989	22.019235	1.591526
-78.034810	8.549476	1.596531
-78.046185	12.819245	1.601536
-78.689929	17.548767	1.606541
-79.170425	6.819968	1.611546
-79.613124	17.323457	1.616550
-79.707307	10.485641	1.621555
-79.724009	7.204389	1.626560
-79.864076	11.162129	1.631565
-79.864089	-1.505397	1.636570
-80.845069	13.014964	1.641574
-80.768458	7.112166	1.646579
-81.010445	9.700156	1.651584
-80.892518	10.061424	1.656589
-81.385833	7.633133	1.661594
-82.249952	13.365291	1.666598
-82.570207	11.194620	1.671603
-82.443962	2.844800	1.676608
-82.649586	4.898747	1.681613
-82.186703	11.951063	1.686618
-82.636008	11.689368	1.691622
-83.190227	11.975621	1.696627
-83.690714	12.120578	1.701632
-84.196928	14.082421	1.706637
-83.926172	8.456085	1.711642
-84.083744	9.945684	1.716646
-84.125063	-0.437475	1.721651
-84.684994	11.283438	1.726656
-85.425340	16.904454	1.731661
-85.323812	5.932598	1.736666
-85.267402	13.868015	1.741670
-85.720958	13.768337	1.746675
-85.383426	-0.318817	1.751680
-86.349058	12.266093	1.756685
-86.912483	13.850924	1.761690
-87.487705	12.042906	1.766694
-87.339061	15.224584	1.771699
-86.804167	4.181660	1.776704
-87.297874	11.133929	1.781709
-87.555105	0.958607	1.786714
-88.549072	12.829788	1.791718
-88.589887	-0.274269	1.796723
-88.602999	7.257587	1.801728
-88.826439	9.399747	1.806733
-88.703774	10.557536	1.811738
-88.867015	15.040925	1.816742
-89.306413	13.844374	1.821747
-90.212113	7.491220	1.826752
-90.440921	8.808485	1.831757
-90.098676	7.555896	1.836762
-90.148306	9.297500	1.841766
-90.782725	10.665665	1.846771
-91.452297	13.801544	1.851776
-92.016560	18.164274	1.856781
-91.596251	13.071322	1.861786
-91.699477	11.480411	1.866790
-91.924938	15.103520	1.871795
-91.715494	12.770757	1.876800
-92.673449	6.637763	1.881805
-92.577585	6.559563	1.886810
-93.087438	18.845272	1.891814
-93.306252	7.676838	1.896819
-93.553506	4.551935	1.901824
-93.738268	6.460245	1.906829
-94.114042	8.483906	1.911834
-94.315405	14.678526	1.916838
-94.665222	5.488979	1.921843
-94.655771	7.091611	1.926848
-95.049521	5.660119	1.931853
-94.925091	0.923579	1.936858
-95.642123	4.762916	1.941862
-95.849269	6.035658	1.946867
-96.194652	4.903469	1.951872
-96.356334	19.130944	1.956877
-96.159572	7.454469	1.961882
-96.855895	4.798563	1.966886
-97.240326	11.724218	1.971891
-97.582067	5.456704	1.976896
-97.865243	5.646704	1.981901
-97.669944	1.819709	1.986906
-97.790938	2.999857	1.991910
-98.142536	7.664618	1.996915
-98.902591	5.440512	2.006912
-98.272985	13.160164	2.016909
-97.658302	9.554125	2.026906
-97.360399	8.338722	2.036902
-96.873462	13.166360	2.046899
-96.602148	2.293354	2.056896
-95.738084	7.147427	2.066893
-95.163309	6.379649	2.076890
-95.058316	5.809026	2.086886
-93.983966	13.037675	2.096883
-93.889301	18.968985	2.106880
-93.703973	12.576037	2.116877
-92.724875	14.085905	2.126874
-92.599177	10.711707	2.136870
-91.434329	16.484831	2.146867
-91.079936	12.333534	2.156864
-90.726161	4.916340	2.166861
-90.657422	8.441019	2.176858
-89.987798	13.176677	2.186854
-89.586062	4.852314	2.196851
-88.639768	9.598471	2.206848
-88.598041	10.742034	2.216845
-87.792251	11.252693	2.226842
-87.279998	11.178955	2.236838
-87.041504	7.850439	2.246835
-85.996993	6.213942	2.256832
-85.742866	7.226022	2.266829
-85.556136	8.552771	2.276826
-84.552315	8.956373	2.286822
-84.235215	10.139151	2.296819
-84.224324	13.118531	2.306816
-83.176812	6.368744	2.316813
-82.814378	4.611041	2.326810
-81.923007	7.740727	2.336806
-81.448638	7.109058	2.346803
-80.961072	11.401241	2.356800
-80.852235	8.948346	2.366797
-80.705053	8.950818	2.376794
-80.010022	14.417424	2.386790
-79.503659	17.800675	2.396787
-78.817146	11.569949	2.406784
-78.465244	11.803271	2.416781
-77.693596	8.616129	2.426778
-77.552702	14.334288	2.436774
-76.677202	13.433860	2.446771
-76.085983	11.206320	2.456768
-75.664480	17.241640	2.466765
-75.326717	14.021113	2.476762
-74.703470	9.948067	2.486758
-74.303300	8.250974	2.496755
-74.142301	11.301868	2.506752
-72.804794	8.520238	2.516749
-72.489680	11.353748	2.526746
-72.629332	12.554242	2.536742
-72.198951	14.577743	2.546739
-71.319476	13.283885	2.556736
-70.463324	14.885879	2.566733
-70.059561	10.311866	2.576730
-70.123969	13.312549	2.586726
-68.797948	20.904081	2.596723
-68.201852	14.975791	2.606720
-68.305764	15.689181	2.616717
-67.848593	15.418168	2.626714
-67.684256	9.443491	2.636710
-66.916076	11.347539	2.646707
-66.292399	9.042055	2.656704
-66.034790	15.581393	2.666701
-65.045211	11.425604	2.676698
-64.487746	10.711225	2.686694
-64.379913	9.211993	2.696691
-63.835691	10.533413	2.706688
-62.804024	11.886161	2.716685
-62.564044	11.436937	2.726682
-62.523142	8.877478	2.736678
-61.663957	13.931894	2.746675
-61.197197	11.030110	2.756672
-60.867640	9.898446	2.766669
-60.193178	8.595532	2.776666
-59.531285	12.058950	2.786662
-59.585204	15.526824	2.796659
-58.935796	12.000874	2.806656
-58.083095	10.749227	2.816653
-57.784023	13.753145	2.826650
-57.063075	5.090496	2.836646
-56.838547	13.035182	2.846643
-56.142917	13.401547	2.856640
-55.345054	4.296026	2.866637
-55.347502	7.784343	2.876634
-55.012180	8.444748	2.886630
-53.876800	8.184678	2.896627
-53.518758	3.091977	2.906624
-53.379690	7.780889	2.916621
-52.533467	7.949429	2.926618
-52.289260	9.796195	2.936614
-52.005993	10.749859	2.946611
-51.023818	6.959528	2.956608
-50.656996	11.989723	2.966605
-50.569428	10.921319	2.976602
-49.598927	6.467581	2.986598
-49.021209	9.741450	2.996595
-48.939616	7.109091	3.006592
-48.089430	4.967689	3.016589
-47.729598	1.895761	3.026586
-47.292050	9.217859	3.036582
-46.626591	5.207892	3.046579
-46.285992	7.571744	3.056576
-45.543453	6.011076	3.066573
-45.151374	-0.835579	3.076570
-44.869508	9.805418	3.086566
-43.940185	3.026636	3.096563
-43.893468	4.077552	3.106560
-43.277495	3.813337	3.116557
-42.324768	2.587200	3.126554
-42.205114	5.571713	3.136550
-42.164812	12.588592	3.146547
-40.800374	4.015185	3.156544
-40.506588	5.632437	3.166541
-40.479923	11.606081	3.176538
-39.294327	10.197738	3.186534
-39.227751	8.432540	3.196531
-39.104467	10.383784	3.206528
-38.231940	9.772095	3.216525
-37.862382	13.886370	3.226522
-36.668706	7.506490	3.236518
-36.585437	7.753394	3.246515
-35.972621	11.706010	3.256512
-35.883501	2.397928	3.266509
-35.462832	5.987842	3.276506
-34.711150	6.605185	3.286502
-34.143876	2.537744	3.296499
-33.329375	5.391211	3.306496
-33.109062	-0.275455	3.316493
-33.010936	2.870821	3.326490
-32.334545	6.702602	3.336486
-31.635787	0.774071	3.346483
-30.671920	8.704284	3.356480
-30.656141	3.842606	3.366477
-30.475789	5.803915	3.376474
-29.931527	10.670094	3.386470
-29.357401	6.443189	3.396467
-28.394295	7.122440	3.406464
-27.903856	17.094037	3.416461
-27.511788	10.770065	3.426458
-27.476437	6.884168	3.436454
-26.740604	11.371874	3.446451
-26.247960	7.287615	3.456448
-24.995506	6.214089	3.466445
-25.198917	11.286115	3.476442
-24.837875	7.165456	3.486438
-24.145918	12.962001	3.496435
-23.437341	15.131984	3.506432
-22.883010	17.278619	3.516429
-22.930426	17.159528	3.526426
-22.258134	15.527505	3.536422
-21.803742	15.237923	3.546419
-20.930128	17.759016	3.556416
-20.113248	5.023388	3.566413
-19.902452	3.831139	3.576410
-20.086860	5.643694	3.586406
-19.597345	10.211175	3.596403
-18.774155	5.036089	3.606400
-17.764379	3.021738	3.616397
-17.174216	14.853046	3.626394
-17.078507	11.692620	3.636390
-17.062743	8.579566	3.646387
-16.193511	10.680029	3.656384
-15.717572	11.739720	3.666381
-15.041624	17.649649	3.676378
-14.366499	12.982433	3.686374
-14.046072	8.602043	3.696371
-13.824738	8.874832	3.706368
-12.862115	8.958615	3.716365
-12.667010	9.555461	3.726362
-12.342818	11.380193	3.736358
-11.299298	11.463972	3.746355
-11.116742	11.413387	3.756352
-10.696648	11.113341	3.766349
-9.672925	11.973164	3.776346
-9.698491	17.495664	3.786342
-9.484141	9.219665	3.796339
-8.742850	8.077344	3.806336
-8.217212	11.691996	3.816333
-6.976219	9.530545	3.826330
-7.196061	10.949510	3.836326
-7.284037	12.981373	3.846323
-6.072623	18.278383	3.856320
-5.602836	16.456344	3.866317
-5.098325	19.215836	3.876314
-4.385308	20.799083	3.886310
-4.533570	26.245777	3.896307
-3.782733	42.097210	3.906304
-3.624576	41.724164	3.916301
-2.766915	54.856736	3.926298
-2.152204	63.601959	3.936294
-1.854723	74.899458	3.946291
-1.346632	75.665847	3.956288
-0.943352	94.444985	3.966285
-0.607933	99.176019	3.976282
-0.162633	117.172484	3.986278
0.000000	130.954733	3.991283
0.493963	143.750807	3.996288
0.658738	148.878867	4.001293
0.941725	165.529848	4.006298
1.074876	160.833026	4.011302
0.883671	170.515752	4.016307
1.069645	160.036767	4.021312
1.264140	154.371712	4.026317
0.971210	157.920000	4.031322
1.210338	147.638339	4.036326
0.870382	157.591139	4.041331
0.863784	164.299467	4.046336
1.328122	166.488908	4.051341
1.347821	176.322092	4.056346
1.525742	174.876940	4.061350
1.499560	177.465943	4.066355
1.378120	161.840204	4.071360
1.244151	155.416687	4.076365
1.439315	167.487635	4.081370
1.333948	157.649088	4.086374
1.590542	163.654950	4.091379
1.550851	158.545445	4.096384
1.533310	156.710138	4.101389
1.397551	163.293169	4.106394
1.268186	158.590022	4.111398
1.111961	164.534014	4.116403
1.517834	158.500479	4.121408
1.215683	155.846055	4.126413
1.219877	165.615223	4.131418
1.712278	174.899777	4.136422
1.350772	177.158502	4.141427
1.612009	178.164877	4.146432
1.816810	176.750315	4.151437
1.416967	176.392277	4.156442
1.206610	165.447036	4.161446
1.399586	165.606723	4.166451
1.520763	179.714086	4.171456
1.801338	181.476737	4.176461
1.611762	187.900529	4.181466
1.682785	173.092518	4.186470
1.709068	181.330130	4.191475
1.439753	186.292095	4.196480
1.663865	183.115447	4.201485
1.543513	191.458298	4.206490
1.729472	178.438791	4.211494
1.341891	180.344095	4.216499
1.565283	184.178488	4.221504
1.801791	188.782789	4.226509
1.686853	183.726196	4.231514
1.733521	180.124930	4.236518
1.716048	176.869076	4.241523
1.278161	185.093995	4.246528
1.732538	182.776617	4.251533
1.667440	194.834577	4.256538
2.239250	184.598847	4.261542
1.924501	191.706646	4.266547
2.002010	191.571210	4.271552
2.190868	183.040647	4.276557
2.038363	189.256149	4.281562
2.234741	187.542347	4.286566
1.910043	176.618178	4.291571
1.576211	166.818586	4.296576
1.718896	187.199513	4.301581
1.720575	188.284522	4.306586
2.026486	187.164167	4.311590
2.031293	186.492789	4.316595
1.581366	183.222433	4.321600
1.914492	183.391799	4.326605
2.095641	192.206269	4.331610
2.138901	191.348531	4.336614
1.923490	189.866929	4.341619
1.656493	190.835845	4.346624
2.164596	183.932064	4.351629
1.433921	194.619988	4.356634
2.129191	187.765974	4.361638
1.850407	183.807573	4.366643
1.639444	193.787639	4.371648
2.008890	190.964708	4.376653
1.788238	190.749438	4.381658
2.376151	186.452759	4.386662
2.021656	195.262571	4.391667
1.995472	180.495094	4.396672
2.113902	194.096695	4.401677
1.938181	194.026246	4.406682
2.186432	189.719510	4.411686
2.288939	203.450164	4.416691
2.394418	207.163830	4.421696
2.652707	190.067525	4.426701
1.971625	184.713654	4.431706
2.151480	185.400584	4.436710
2.323659	189.227184	4.441715
1.956958	186.658800	4.446720
2.095593	185.779791	4.451725
1.929058	211.913485	4.456730
2.488013	213.673652	4.461734
2.497536	213.428645	4.466739
2.557249	213.311817	4.471744
2.054066	201.899901	4.476749
2.173972	203.333385	4.481754
2.712030	213.028424	4.486758
2.587608	209.795648	4.491763
2.400687	197.837469	4.496768
2.716824	189.125608	4.501773
2.358124	201.413073	4.506778
2.417631	189.492219	4.511782
2.098536	197.363171	4.516787
2.007551	196.048736	4.521792
2.552863	202.164400	4.526797
2.431058	207.413309	4.531802
2.644299	206.048043	4.536806
2.668021	210.622413	4.541811
2.443913	220.319813	4.546816
2.505730	199.707681	4.551821
2.711346	215.307802	4.556826
2.477903	198.671351	4.561830
2.428159	202.308096	4.566835
2.343282	211.493290	4.571840
2.342896	205.564522	4.576845
2.704586	218.897071	4.581850
2.776696	216.272585	4.586854
2.614259	212.564869	4.591859
2.655004	222.309359	4.596864
2.727496	214.850553	4.601869
2.470786	220.316757	4.606874
2.905434	219.530574	4.611878
2.704844	214.335530	4.616883
2.614105	223.885485	4.621888
2.759006	209.834667	4.626893
2.510367	221.658808	4.631898
2.224073	214.502993	4.636902
2.219191	219.066028	4.641907
2.639592	225.343641	4.646912
2.774671	211.218430	4.651917
2.607096	220.786749	4.656922
2.911165	219.495837	4.661926
2.980933	220.484757	4.666931
2.709633	216.341676	4.671936
2.589803	219.568623	4.676941
2.506394	222.388064	4.681946
2.891512	221.653933	4.686950
2.880856	219.978894	4.691955
2.854326	217.477431	4.696960
2.937683	215.075812	4.701965
2.450307	223.694484	4.706970
3.061401	237.117685	4.711974
3.117687	234.853183	4.716979
3.074544	231.076152	4.721984
3.016520	225.985319	4.726989
2.644617	225.461549	4.731994
2.753533	225.302210	4.736998
3.283221	245.097379	4.742003
3.246900	242.461404	4.747008
2.972391	222.234140	4.752013
2.806165	230.603179	4.757018
2.798975	231.854097	4.762022
3.306544	241.882962	4.767027
3.073497	241.381729	4.772032
3.383422	233.737015	4.777037
2.704313	233.005112	4.782042
3.180936	235.490033	4.787046
3.607583	243.209360	4.792051
2.918451	229.089885	4.797056
2.830922	218.932131	4.802061
3.252236	231.315705	4.807066
3.412405	236.874787	4.812070
2.980596	231.222416	4.817075
2.892829	247.257677	4.822080
3.340367	235.266504	4.827085
3.039551	243.865447	4.832090
3.215047	239.557443	4.837094
3.150302	238.694479	4.842099
2.987015	240.969611	4.847104
3.492089	240.346401	4.852109
3.248539	246.063654	4.857114
3.057817	241.920598	4.862118
3.144860	245.004403	4.867123
2.897961	244.777426	4.872128
2.893186	242.269387	4.877133
2.723670	243.074335	4.882138
3.229100	250.737028	4.887142
3.408532	268.989389	4.892147
2.890961	273.705534	4.897152
3.589550	264.940041	4.902157
3.484964	269.180185	4.907162
3.813872	263.645898	4.912166
3.680542	262.154592	4.917171
3.145132	251.329831	4.922176
3.471812	259.036354	4.927181
3.356064	275.743584	4.932186
3.661702	264.246031	4.937190
3.806663	265.931861	4.942195
3.309395	256.828551	4.947200
3.553025	262.409366	4.952205
3.241787	267.634189	4.957210
3.315152	270.217099	4.962214
3.971797	264.976315	4.967219
3.707476	263.587792	4.972224
3.645666	264.568856	4.977229
3.301682	261.351488	4.982234
3.299886	262.959072	4.987238
3.500168	267.584888	4.992243
3.554869	271.490024	4.997248
4.257582	270.339131	5.002253
3.695544	268.405625	5.007258
3.867210	269.615867	5.012262
3.749377	272.491329	5.017267
3.905076	263.633725	5.022272
3.796665	243.377248	5.027277
3.150362	241.963154	5.032282
3.520562	257.781136	5.037286
3.918065	257.997364	5.042291
3.718784	264.112653	5.047296
3.843283	262.792924	5.052301
3.513512	263.509085	5.057306
3.770450	264.759751	5.062310
3.653748	267.087700	5.067315
3.760481	268.510598	5.072320
3.676870	270.447380	5.077325
3.563575	267.032513	5.082330
3.765089	268.124182	5.087334
4.071830	270.278217	5.092339
3.924489	268.735322	5.097344
3.861619	254.691712	5.102349
3.770374	260.109857	5.107354
3.801699	264.692541	5.112358
3.650640	275.087215	5.117363
3.532579	271.989473	5.122368
3.817314	263.937401	5.127373
3.718974	272.400228	5.132378
3.834946	276.561524	5.137382
4.347473	284.393965	5.142387
4.124833	281.078487	5.147392
3.793484	263.090556	5.152397
3.943861	284.378397	5.157402
4.442422	283.069662	5.162406
4.202825	275.735660	5.167411
3.997973	275.204698	5.172416
3.900198	270.537701	5.177421
4.008206	274.981821	5.182426
4.171224	281.059333	5.187430
4.483630	281.744481	5.192435
3.412328	271.395982	5.197440
4.232580	286.972631	5.202445
3.913494	288.389481	5.207450
4.277492	285.111803	5.212454
4.315487	284.713636	5.217459
4.749287	287.132506	5.222464
4.655843	277.874163	5.227469
4.004675	275.255423	5.232474
3.530093	272.425516	5.237478
4.158778	277.246807	5.242483
3.995333	292.696009	5.247488
4.667309	298.159101	5.252493
4.316230	298.413524	5.257498
4.554154	297.620195	5.262502
4.597385	295.107791	5.267507
4.117090	286.343495	5.272512
3.946338	281.903068	5.277517
4.308427	296.801691	5.282522
4.179668	290.453240	5.287526
4.633229	301.996569	5.292531
4.395229	291.682013	5.297536
4.491491	288.974637	5.302541
4.498734	294.576680	5.307546
4.396733	292.574256	5.312550
4.135663	284.683623	5.317555
3.929540	292.479968	5.322560
4.645544	295.822745	5.327565
4.517220	288.177071	5.332570
4.382183	296.528599	5.337574
4.739763	288.300585	5.342579
4.577686	291.154508	5.347584
4.607705	298.350701	5.352589
4.174513	299.102050	5.357594
4.784462	300.468253	5.362598
4.312896	294.815763	5.367603
4.453948	297.679141	5.372608
4.838305	294.189461	5.377613
4.545020	299.936671	5.382618
4.638732	300.614956	5.387622
4.632085	295.206001	5.392627
4.715633	296.496491	5.397632
4.865008	290.215195	5.402637
4.651452	299.376303	5.407642
4.408231	297.146065	5.412646
4.742293	293.094782	5.417651
4.419072	297.422973	5.422656
4.949160	287.924559	5.427661
4.942642	293.402206	5.432666
4.604498	300.358687	5.437670
4.835108	298.335786	5.442675
4.542926	301.235407	5.447680
4.651415	292.290271	5.452685
4.624272	296.584728	5.457690
4.828938	296.945067	5.462694
4.710738	287.051512	5.467699
4.314100	292.273903	5.472704
4.400510	288.698027	5.477709
4.603763	299.170080	5.482714
4.695527	301.601414	5.487718
4.880713	306.204295	5.492723
4.767682	315.760955	5.497728
5.172154	305.687418	5.502733
5.021243	321.141009	5.507738
4.838328	312.523099	5.512742
5.147703	314.771641	5.517747
4.893951	315.387307	5.522752
4.835796	312.485819	5.527757
5.195693	307.984389	5.532762
5.113472	311.638900	5.537766
5.231964	308.190873	5.542771
4.507414	312.819233	5.547776
4.819965	311.928788	5.552781
4.878054	316.776216	5.557786
5.210301	320.856178	5.562790
5.183420	320.341623	5.567795
5.160240	321.854484	5.572800
5.464089	318.225551	5.577805
5.348141	317.756589	5.582810
4.852598	304.979811	5.587814
4.687827	300.579571	5.592819
4.809549	313.386634	5.597824
5.342295	314.002459	5.602829
5.113946	314.174377	5.607834
4.937933	315.325199	5.612838
5.284051	309.022562	5.617843
4.883933	318.630532	5.622848
5.135378	304.939439	5.627853
4.938494	305.615798	5.632858
4.931504	308.394804	5.637862
4.922874	314.024651	5.642867
5.006231	317.839884	5.647872
5.545742	315.214918	5.652877
5.381420	318.913933	5.657882
5.023627	319.093476	5.662886
5.083523	321.612065	5.667891
5.250603	330.925525	5.672896
5.229716	334.494500	5.677901
5.110745	332.143548	5.682906
5.382839	341.019775	5.687910
5.386400	332.341000	5.692915
5.345644	336.216813	5.697920
5.482557	326.786309	5.702925
5.227335	332.483272	5.707930
5.441708	340.004943	5.712934
5.766515	339.036645	5.717939
5.279008	338.689174	5.722944
5.575446	330.166996	5.727949
5.242773	333.465277	5.732954
5.535095	336.817497	5.737958
5.554092	335.628190	5.742963
5.552654	333.303116	5.747968
5.380212	339.312983	5.752973
5.835349	341.279258	5.757978
5.842075	338.699800	5.762982
5.518114	335.504592	5.767987
5.051393	336.874974	5.772992
5.384259	335.861120	5.777997
5.203928	337.075897	5.783002
5.542438	331.201558	5.788006
5.655407	338.584090	5.793011
5.185053	348.721944	5.798016
5.366667	339.467930	5.803021
5.267681	344.937935	5.808026
5.309737	354.204557	5.813030
5.777626	359.598402	5.818035
5.633734	368.941623	5.823040
5.940519	365.014823	5.828045
5.836702	367.071842	5.833050
5.824194	357.098411	5.838054
5.935301	361.133936	5.843059
5.731723	354.408037	5.848064
5.864801	352.004936	5.853069
5.777682	344.669162	5.858074
5.494198	353.528037	5.863078
5.806947	354.387144	5.868083
6.014838	367.158598	5.873088
5.987080	354.039569	5.878093
5.856247	352.266286	5.883098
5.530874	345.252584	5.888102
5.939257	349.219382	5.893107
6.039614	360.609278	5.898112
5.901154	350.946655	5.903117
6.051168	354.960264	5.908122
5.925731	353.752457	5.913126
6.065176	350.402380	5.918131
5.764996	341.862942	5.923136
6.111105	351.224294	5.928141
5.932187	347.041398	5.933146
5.476791	353.405656	5.938150
5.728750	356.049183	5.943155
6.042444	358.233777	5.948160
6.127095	357.103786	5.953165
5.810366	358.517109	5.958170
5.796507	358.316893	5.963174
5.899169	359.313322	5.968179
6.168468	360.922732	5.973184
5.965732	363.226207	5.978189
6.134657	360.921895	5.983194
6.151577	359.384893	5.988198
6.106285	355.832803	5.993203
5.929428	354.598250	5.998208
5.896054	352.281341	6.003213
6.263129	358.716056	6.008218
6.118237	361.700178	6.013222
6.280274	363.744016	6.018227
5.931559	363.121695	6.023232
6.309125	369.361777	6.028237
5.911872	362.947798	6.033242
5.444773	359.930039	6.038246
5.953380	355.253435	6.043251
5.821490	371.881026	6.048256
6.029415	377.084650	6.053261
6.289831	386.601819	6.058266
6.285991	388.867807	6.063270
6.141451	366.288285	6.068275
6.256172	371.240751	6.073280
6.192755	366.647441	6.078285
6.466712	359.584123	6.083290
5.983236	365.743974	6.088294
5.965072	361.940854	6.093299
6.388154	364.155768	6.098304
6.100453	361.945146	6.103309
5.846894	355.957916	6.108314
6.027468	369.360086	6.113318
6.170786	362.763332	6.118323
6.196949	370.387273	6.123328
6.099382	362.515280	6.128333
5.949549	362.523033	6.133338
5.495001	359.693136	6.138342
6.163143	372.620276	6.143347
6.156666	383.802295	6.148352
6.438688	390.611022	6.153357
6.390377	389.881519	6.158362
6.386916	383.886733	6.163366
6.623794	366.331697	6.168371
6.123444	365.521158	6.173376
6.235453	366.895780	6.178381
6.218756	364.658516	6.183386
6.049245	356.661755	6.188390
6.422466	357.448111	6.193395
5.902310	369.675566	6.198400
6.164862	362.063531	6.203405
6.277011	360.157262	6.208410
6.199976	364.798080	6.213414
6.337805	360.179568	6.218419
6.252757	362.202007	6.223424
6.280968	362.729203	6.228429
6.458650	357.484341	6.233434
6.422721	371.850594	6.238438
6.249640	366.277866	6.243443
6.173163	353.302514	6.248448
6.235134	344.813901	6.253453
5.884041	339.519014	6.258458
6.080858	348.935394	6.263462
5.848222	356.821343	6.268467
6.063109	355.174229	6.273472
6.487723	358.398156	6.278477
6.501445	356.184601	6.283482
5.908895	339.398636	6.288486
5.612759	346.345389	6.293491
5.850871	358.251546	6.298496
6.053496	356.482965	6.303501
6.006539	359.043611	6.308506
5.874091	363.930396	6.313510
6.207922	361.843859	6.318515
6.052754	369.309545	6.323520
6.476203	352.146077	6.328525
6.177452	361.105427	6.333530
6.303354	354.625302	6.338534
6.404207	357.523463	6.343539
6.334024	363.463531	6.348544
6.281622	354.413857	6.353549
6.222948	342.691755	6.358554
5.752022	339.826462	6.363558
5.659746	352.018502	6.368563
5.919993	358.659783	6.373568
6.382680	366.316568	6.378573
6.353159	360.151863	6.383578
6.223234	365.563446	6.388582
6.186416	365.420612	6.393587
5.924626	365.822399	6.398592
6.246140	362.225491	6.403597
6.131271	361.313426	6.408602
6.304059	360.068383	6.413606
6.019771	359.818788	6.418611
6.342385	360.451719	6.423616
6.041835	343.221360	6.428621
6.271999	345.308307	6.433626
5.781454	349.536175	6.438630
6.091959	348.883334	6.443635
6.099997	359.322733	6.448640
6.072521	353.784144	6.453645
6.385007	368.671617	6.458650
5.962863	361.464259	6.463654
6.054120	357.625014	6.468659
6.186391	362.837324	6.473664
5.994968	365.661055	6.478669
6.392192	360.872184	6.483674
6.152504	356.287512	6.488678
6.087718	345.860363	6.493683
5.635154	363.063380	6.498688
5.900894	364.932781	6.503693
6.379203	359.988834	6.508698
6.034192	377.890035	6.513702
6.407277	369.732322	6.518707
6.025406	367.916112	6.523712
6.388411	370.061343	6.528717
6.404828	362.671374	6.533722
5.725673	359.224924	6.538726
6.112317	358.237445	6.543731
5.965782	369.223096	6.548736
5.861219	362.057730	6.553741
5.850906	361.837975	6.558746
6.237518	368.845446	6.563750
6.145900	370.505077	6.568755
5.941533	368.787607	6.573760
6.141992	371.135480	6.578765
6.541173	367.361884	6.583770
6.265917	374.337015	6.588774
6.520683	369.437582	6.593779
6.145444	366.573111	6.598784
6.057114	358.658544	6.603789
6.149382	352.152052	6.608794
5.781331	357.414277	6.613798
6.330696	354.588441	6.618803
6.282876	371.519240	6.623808
6.109082	357.945354	6.628813
6.191013	351.753698	6.633818
5.970758	368.524847	6.638822
6.235599	366.619964	6.643827
6.220151	363.597880	6.648832
5.900684	341.770309	6.653837
5.951460	357.600462	6.658842
6.405665	367.862391	6.663846
6.144179	351.154259	6.668851
5.947336	353.675113	6.673856
6.118247	367.970988	6.678861
6.345663	353.910293	6.683866
6.329301	358.715612	6.688870
6.199868	343.856607	6.693875
6.021165	346.099366	6.698880
5.933821	343.284706	6.703885
5.772770	345.799950	6.708890
6.112185	369.620956	6.713894
6.485368	360.624823	6.718899
6.449992	363.171000	6.723904
6.270749	351.062815	6.728909
6.154738	344.076423	6.733914
5.755055	344.882636	6.738918
5.967023	341.998933	6.743923
5.925896	350.474980	6.748928
6.160186	351.596320	6.753933
6.231124	355.176222	6.758938
5.663291	359.678798	6.763942
6.117158	359.256599	6.768947
6.102541	365.931457	6.773952
6.141015	364.147465	6.778957
6.527679	355.620629	6.783962
6.234367	363.560381	6.788966
5.998444	343.731901	6.793971
6.011528	350.509982	6.798976
6.288032	356.354599	6.803981
6.004623	352.846145	6.808986
6.065790	363.966932	6.813990
6.176851	358.666068	6.818995
6.179928	364.670590	6.824000
5.989597	348.808704	6.829005
6.257342	358.027312	6.834010
6.143915	352.087732	6.839014
6.077411	344.881607	6.844019
6.019141	349.924447	6.849024
5.810752	357.107397	6.854029
6.424166	358.194647	6.859034
6.417893	359.967458	6.864038
6.108334	339.967018	6.869043
6.092265	340.760583	6.874048
6.217201	340.067214	6.879053
6.024275	336.253517	6.884058
5.802748	341.211201	6.889062
6.254028	348.107289	6.894067
6.211751	358.668468	6.899072
6.107762	352.496450	6.904077
5.952126	345.680784	6.909082
6.351430	356.020911	6.914086
6.299150	348.227252	6.919091
5.979034	337.982484	6.924096
5.956687	342.329985	6.929101
6.272826	345.197576	6.934106
5.575185	351.292899	6.939110
6.225320	351.586608	6.944115
6.543535	362.088143	6.949120
6.214635	347.981736	6.954125
6.074971	347.367790	6.959130
5.911793	342.992600	6.964134
6.048660	346.941827	6.969139
6.174012	365.778573	6.974144
6.097483	371.979071	6.979149
6.196029	366.632708	6.984154
6.044472	376.518145	6.989158
6.264003	361.297561	6.994163
6.420962	358.064964	6.999168
6.015922	342.366440	7.004173
5.893929	332.343738	7.009178
5.862912	354.887639	7.014182
6.257832	363.921806	7.019187
6.193137	356.313590	7.024192
6.273291	354.962837	7.029197
6.418841	340.475209	7.034202
6.025756	343.083757	7.039206
5.884438	342.780123	7.044211
5.880162	346.558472	7.049216
5.925934	348.180757	7.054221
5.822206	362.276046	7.059226
5.872168	363.875529	7.064230
6.310498	365.382524	7.069235
5.958337	367.152581	7.074240
6.096982	363.688730	7.079245
6.121848	356.759355	7.084250
6.118237	366.710194	7.089254
6.515873	363.670844	7.094259
6.541401	365.919572	7.099264
6.141377	363.976490	7.104269
6.116429	365.382062	7.109274
6.072527	367.192408	7.114278
6.180278	360.367106	7.119283
6.370390	359.407256	7.124288
6.212581	356.508720	7.129293
6.100965	339.017805	7.134298
5.723711	348.970227	7.139302
6.063583	358.161715	7.144307
6.419333	362.386704	7.149312
6.000913	362.088520	7.154317
6.407598	349.094418	7.159322
6.069782	358.176947	7.164326
5.729895	347.615727	7.169331
5.981641	351.970905	7.174336
6.379076	366.905179	7.179341
6.386609	362.712049	7.184346
5.621564	361.958802	7.189350
6.158855	364.633556	7.194355
5.921138	359.536037	7.199360
5.907096	363.559533	7.204365
6.560876	365.352316	7.209370
6.335546	367.412555	7.214374
6.321142	361.659941	7.219379
6.035940	353.807859	7.224384
5.915945	347.075194	7.229389
6.268910	350.224923	7.234394
5.927297	360.260354	7.239398
6.206038	362.915505	7.244403
6.254143	368.014451	7.249408
6.183885	360.388122	7.254413
6.377598	352.011744	7.259418
6.028159	340.407969	7.264422
5.979463	339.805080	7.269427
5.907969	337.437198	7.274432
6.066919	357.224139	7.279437
6.202753	356.810641	7.284442
6.298386	363.291050	7.289446
6.233772	349.519727	7.294451
6.287823	345.942582	7.299456
5.910813	342.977151	7.304461
6.146316	336.100204	7.309466
5.545428	350.994726	7.314470
5.823152	351.397405	7.319475
6.190529	354.010193	7.324480
5.985994	360.556615	7.329485
6.230220	359.379475	7.334490
6.262667	375.222007	7.339494
6.506678	364.186470	7.344499
6.617484	368.611192	7.349504
6.105259	350.189597	7.354509
6.219055	343.489907	7.359514
6.328163	353.881829	7.364518
6.265821	340.065863	7.369523
6.275422	353.165773	7.374528
6.012623	349.157373	7.379533
6.231464	343.671945	7.384538
6.131026	345.829674	7.389542
6.331205	337.379522	7.394547
6.256362	344.066972	7.399552
6.228141	343.660195	7.404557
6.415980	341.245352	7.409562
6.003188	341.050693	7.414566
5.954955	336.521451	7.419571
5.947487	343.685570	7.424576
5.661237	350.361852	7.429581
6.070650	341.768183	7.434586
5.838771	346.854042	7.439590
6.033581	331.140640	7.444595
6.174321	335.699871	7.449600
5.984276	340.269802	7.454605
6.230239	346.976593	7.459610
6.139061	338.755591	7.464614
6.018298	329.058569	7.469619
6.404827	325.514758	7.474624
6.355643	334.675441	7.479629
6.045774	332.654961	7.484634
6.154677	339.168084	7.489638
6.039861	339.220971	7.494643
6.117939	335.807745	7.499648
5.940039	341.375536	7.504653
6.281689	337.152208	7.509658
5.793676	344.888337	7.514662
6.374208	347.660719	7.519667
6.248568	348.145580	7.524672
5.910945	337.770675	7.529677
6.029184	334.613752	7.534682
6.144133	347.896472	7.539686
6.146239	331.839932	7.544691
5.766103	333.411886	7.549696
5.912773	342.184376	7.554701
6.503998	345.217678	7.559706
6.330253	351.689669	7.564710
6.414981	343.763813	7.569715
6.580383	342.504110	7.574720
6.089236	347.934317	7.579725
5.759417	335.666235	7.584730
5.948335	345.665991	7.589734
6.094195	345.130698	7.594739
6.082206	344.404997	7.599744
6.020341	337.565150	7.604749
6.572046	335.846282	7.609754
5.816603	341.390665	7.614758
6.049864	335.352478	7.619763
5.940488	338.669559	7.624768
5.954560	348.829591	7.629773
6.194827	342.496070	7.634778
5.984193	349.454738	7.639782
6.198401	349.592118	7.644787
6.096160	345.925563	7.649792
5.659023	345.990987	7.654797
6.367099	360.057158	7.659802
6.137729	368.053334	7.664806
6.438632	362.390524	7.669811
6.114122	346.790113	7.674816
5.978745	342.103678	7.679821
6.350349	337.549786	7.684826
6.130903	338.985830	7.689830
6.170074	335.594519	7.694835
5.993913	341.326555	7.699840
5.820467	348.057929	7.704845
6.343976	330.935753	7.709850
5.744757	345.491483	7.714854
6.490600	352.388877	7.719859
6.070491	339.397772	7.724864
5.906174	343.087299	7.729869
6.337996	347.322512	7.734874
6.128986	352.746481	7.739878
5.952306	346.873762	7.744883
6.133558	343.273524	7.749888
5.959489	342.250510	7.754893
6.582766	343.541861	7.759898
5.846348	345.324665	7.764902
5.935977	342.811312	7.769907
6.260177	366.846674	7.774912
6.005569	356.955468	7.779917
6.261419	358.889694	7.784922
6.220428	354.663039	7.789926
6.549516	353.706724	7.794931
6.101604	344.029314	7.799936
5.960590	347.832252	7.804941
6.397140	338.326320	7.809946
6.070013	342.962023	7.814950
6.211020	335.631639	7.819955
5.944190	335.183153	7.824960
6.119311	346.418954	7.829965
6.144993	343.001281	7.834970
5.879339	344.915972	7.839974
5.976100	351.927720	7.844979
6.060600	353.243376	7.849984
5.926220	358.779042	7.854989
6.602652	357.483563	7.859994
5.948757	364.378807	7.864998
5.806069	347.098400	7.870003
6.329404	357.969598	7.875008
5.964857	366.724120	7.880013
5.882610	359.931751	7.885018
6.120628	357.024981	7.890022
6.195273	365.834078	7.895027
6.099109	364.586882	7.900032
6.245046	372.897586	7.905037
6.341137	360.676652	7.910042
6.056983	354.801786	7.915046
6.433625	348.102041	7.920051
6.582640	341.469601	7.925056
5.967735	343.464323	7.930061
6.312100	340.240332	7.935066
5.997115	338.809120	7.940070
6.038160	339.169787	7.945075
6.119856	341.162935	7.950080
5.850071	337.196761	7.955085
6.010010	325.003813	7.960090
6.305708	340.678516	7.965094
5.978859	340.900669	7.970099
5.923071	339.694605	7.975104
6.043862	343.222400	7.980109
6.334358	346.369261	7.985114
6.058768	353.369746	7.990118
6.118783	334.438481	7.995136
5.944244	342.948535	8.000154
6.284710	355.612898	8.005171
6.316630	352.215577	8.010189
5.959309	352.423134	8.015206
6.230107	341.540854	8.020224
6.216160	342.022808	8.025242
6.178352	339.993380	8.030259
6.330990	332.219082	8.035277
6.294769	330.435554	8.040294
6.128509	336.706893	8.045312
6.436049	338.485974	8.050330
5.713414	336.342944	8.055347
5.930527	335.567426	8.060365
6.156011	343.916977	8.065382
6.446465	359.773315	8.070400
6.181675	342.720281	8.075418
6.140360	354.545078	8.080435
5.865207	342.186248	8.085453
6.523801	357.950191	8.090470
6.641807	353.816719	8.095488
6.755365	349.813329	8.100506
6.369246	347.977326	8.105523
6.134557	342.759896	8.110541
5.921037	342.017137	8.115558
6.116087	342.403230	8.120576
6.353275	330.336511	8.125594
6.231788	342.186483	8.130611
6.079877	335.580186	8.135629
5.919592	343.583090	8.140646
6.424686	346.561954	8.145664
6.629369	339.868227	8.150682
6.329674	349.231006	8.155699
5.999305	340.210130	8.160717
6.204367	341.522439	8.165734
5.886763	340.745496	8.170752
6.424563	350.564024	8.175770
6.700606	360.186889	8.180787
6.659533	356.135144	8.185805
6.350279	349.559805	8.190822
6.161720	347.418300	8.195840
6.110211	340.941434	8.200858
6.237483	343.070644	8.205875
6.358224	338.169903	8.210893
6.295539	353.829107	8.215910
6.246767	356.200491	8.220928
6.526642	356.447065	8.225946
6.432603	362.779680	8.230963
6.273114	353.157679	8.235981
6.340234	347.337551	8.240998
6.515001	345.751332	8.246016
6.425704	351.149103	8.251034
5.975158	340.935253	8.256051
6.458422	353.801299	8.261069
6.683492	361.911087	8.266086
6.372377	356.491038	8.271104
6.243887	353.276637	8.276122
6.128586	361.304057	8.281139
6.286457	362.942492	8.286157
6.499909	368.636809	8.291174
6.459596	368.838877	8.296192
6.606849	361.788074	8.301210
6.315896	365.851011	8.306227
6.696224	367.195821	8.311245
6.623100	368.892539	8.316262
6.488116	370.112965	8.321280
6.729753	357.486965	8.326298
6.405486	367.042948	8.331315
6.657694	342.679117	8.336333
6.324425	339.884958	8.341350
6.234144	350.458287	8.346368
6.414739	354.958568	8.351386
6.550567	363.918609	8.356403
6.371612	355.606132	8.361421
6.769569	362.735800	8.366438
6.462233	360.019625	8.371456
6.882761	349.369495	8.376474
6.433291	351.964603	8.381491
6.342953	343.840214	8.386509
6.608680	347.374123	8.391526
6.349743	352.388228	8.396544
6.747454	356.589410	8.401562
6.701055	360.412062	8.406579
6.154234	352.501199	8.411597
6.689040	361.253563	8.416614
6.464836	369.907108	8.421632
6.692880	360.953359	8.426650
6.759714	363.612738	8.431667
6.609386	349.990985	8.436685
6.702927	338.997626	8.441702
6.214049	338.967026	8.446720
6.264665	356.748068	8.451738
6.149595	365.595945	8.456755
6.171086	367.880585	8.461773
6.706092	359.986406	8.466790
6.503952	364.272107	8.471808
6.691268	359.392487	8.476826
6.564663	371.003445	8.481843
6.541080	363.395596	8.486861
6.635077	365.596293	8.491878
6.654341	366.991363	8.496896
6.705940	372.117761	8.501914
6.480065	367.227140	8.506931
6.729128	366.039525	8.511949
6.694646	368.900967	8.516966
6.706643	373.500251	8.521984
6.879134	360.222377	8.527002
6.475900	367.177783	8.532019
6.539555	373.416268	8.537037
6.666181	363.799925	8.542054
6.322561	365.463286	8.547072
6.622540	365.261751	8.552090
6.420909	371.308276	8.557107
6.466228	378.521604	8.562125
7.066832	385.859366	8.567143
6.993868	392.150821	8.572160
6.922953	375.319839	8.577178
6.531396	367.473004	8.582195
6.644011	374.975581	8.587213
6.605099	368.099108	8.592231
6.673889	386.940816	8.597248
6.945887	385.844278	8.602266
7.073747	386.370285	8.607283
6.605362	375.493349	8.612301
6.857478	374.614517	8.617319
6.898279	368.845842	8.622336
6.894036	364.668406	8.627354
6.699704	367.018418	8.632371
6.729122	366.272306	8.637389
6.847257	362.949836	8.642407
6.581603	376.482338	8.647424
6.678276	381.238766	8.652442
6.754105	390.277648	8.657459
6.621704	384.835900	8.662477
7.008438	397.953783	8.667495
6.932453	397.460866	8.672512
7.202326	400.400856	8.677530
6.910337	378.959254	8.682547
6.511576	372.694571	8.687565
7.051566	378.990967	8.692583
6.756252	382.155205	8.697600
6.738258	400.136384	8.702618
7.052179	394.713065	8.707635
7.025728	389.207379	8.712653
7.068514	380.964287	8.717671
6.934624	374.225767	8.722688
6.842100	361.923514	8.727706
6.788247	370.392581	8.732723
6.897662	385.579890	8.737741
7.005674	390.104175	8.742759
6.896313	391.380547	8.747776
6.876537	395.397847	8.752794
7.109243	402.345144	8.757811
6.846171	395.961364	8.762829
7.352371	383.480083	8.767847
6.493300	377.170757	8.772864
6.945770	384.077303	8.777882
6.969878	399.296923	8.782899
6.964515	393.298792	8.787917
7.462697	391.725011	8.792935
7.075401	380.696514	8.797952
6.869098	374.496348	8.802970
6.874413	369.159257	8.807987
6.957780	382.144783	8.813005
7.079445	387.152912	8.818023
6.964521	385.021955	8.823040
6.954389	394.333078	8.828058
7.059474	395.093023	8.833075
7.063557	394.997807	8.838093
7.131354	390.174774	8.843111
6.976448	390.410576	8.848128
7.161073	390.274450	8.853146
6.868850	394.738372	8.858163
7.140299	397.946353	8.863181
7.054806	399.796487	8.868199
7.108950	404.963521	8.873216
6.849374	398.001692	8.878234
7.347286	398.248817	8.883251
6.927573	397.973854	8.888269
7.356236	396.919039	8.893287
7.153493	394.928070	8.898304
7.019989	395.539208	8.903322
7.047061	395.639203	8.908339
6.775914	395.574487	8.913357
7.017309	399.036481	8.918375
7.541794	399.364648	8.923392
6.970548	392.202350	8.928410
7.135197	388.623283	8.933427
6.848213	391.161381	8.938445
7.309933	385.768554	8.943463
6.944821	397.066611	8.948480
6.977953	400.438162	8.953498
7.050650	388.592832	8.958515
6.973623	389.756843	8.963533
7.216737	387.430936	8.968551
7.017525	390.775774	8.973568
6.707078	390.004018	8.978586
6.848211	384.506790	8.983603
6.858794	410.745235	8.988621
7.358022	400.663401	8.993639
7.159540	414.305325	8.998656
7.364302	422.203731	9.003674
7.103513	407.191778	9.008691
7.283486	414.649105	9.013709
7.335929	413.384997	9.018727
7.277863	419.166052	9.023744
7.439325	420.251674	9.028762
7.525431	418.998071	9.033779
7.337392	412.179659	9.038797
7.334440	395.801904	9.043815
7.300607	395.012054	9.048832
7.243996	397.242664	9.053850
7.307057	389.706434	9.058867
7.221711	397.034914	9.063885
7.442573	402.018038	9.068903
7.352098	396.945251	9.073920
6.981252	399.190382	9.078938
7.509451	410.474713	9.083955
7.209733	415.605676	9.088973
7.521701	415.156113	9.093991
7.400238	406.222390	9.099008
7.019505	406.436771	9.104026
7.258053	407.472446	9.109043
7.369666	418.048894	9.114061
7.671708	413.725630	9.119079
7.864113	414.702263	9.124096
7.310985	400.373580	9.129114
7.129809	393.083895	9.134131
7.047503	404.378670	9.139149
7.511069	421.375566	9.144167
7.329079	413.789359	9.149184
7.608159	420.546364	9.154202
7.999151	409.973408	9.159219
7.285780	403.186817	9.164237
7.133729	404.125903	9.169255
7.233814	408.686148	9.174272
7.108316	416.800396	9.179290
7.156802	419.816101	9.184307
7.468655	417.675076	9.189325
7.422227	427.967029	9.194343
7.507418	424.482455	9.199360
7.602223	425.281880	9.204378
7.944754	411.163144	9.209395
7.686605	428.279436	9.214413
7.367730	420.635780	9.219431
7.611846	423.788090	9.224448
7.236777	422.505759	9.229466
7.651342	421.860244	9.234483
7.451089	421.727617	9.239501
7.591835	413.585925	9.244519
7.387513	423.729048	9.249536
7.827355	421.053582	9.254554
7.697527	411.319607	9.259571
7.685583	420.621561	9.264589
7.802394	418.236545	9.269607
7.370092	423.899515	9.274624
7.542764	424.156574	9.279642
7.882105	414.494252	9.284659
7.957927	419.913509	9.289677
7.487146	418.097075	9.294695
7.560308	412.591554	9.299712
7.164534	422.152459	9.304730
7.497202	410.657695	9.309747
7.695877	420.043411	9.314765
7.656542	422.564801	9.319783
7.496469	426.080235	9.324800
7.602516	425.984822	9.329818
7.828547	422.342484	9.334835
7.548677	430.313671	9.339853
7.499115	423.789133	9.344871
7.527313	415.652451	9.349888
7.259141	413.696977	9.354906
7.668816	411.288166	9.359923
7.387774	428.231323	9.364941
7.301676	426.162116	9.369959
7.564774	417.215470	9.374976
7.627584	418.518516	9.379994
7.921608	415.910078	9.385011
7.492462	423.169362	9.390029
7.589233	422.602040	9.395047
8.334191	430.245402	9.400064
8.071672	426.600715	9.405082
8.036119	419.632179	9.410099
8.176831	425.451518	9.415117
8.025925	419.182698	9.420135
8.018277	421.815886	9.425152
7.910196	426.090021	9.430170
7.993815	418.481131	9.435187
7.890874	424.016758	9.440205
7.855330	422.804305	9.445223
7.987030	422.064257	9.450240
7.430487	425.253653	9.455258
7.795139	419.692991	9.460275
7.885859	421.181009	9.465293
7.754329	419.980440	9.470311
7.793179	411.488647	9.475328
7.373518	423.079283	9.480346
7.782022	421.516395	9.485363
7.785005	420.843850	9.490381
7.645595	423.434568	9.495399
7.603347	419.168402	9.500416
7.604606	421.516177	9.505434
7.437492	418.591833	9.510451
7.812593	428.685200	9.515469
7.918903	437.470025	9.520487
7.695619	427.394085	9.525504
7.996276	447.004243	9.530522
8.060769	450.926302	9.535539
8.078194	448.945012	9.540557
8.118209	427.006373	9.545575
7.820110	425.478457	9.550592
7.721575	422.417137	9.555610
7.722046	437.028278	9.560627
8.255295	444.629079	9.565645
8.003706	444.135273	9.570663
8.289067	430.637694	9.575680
7.713704	437.263497	9.580698
7.635753	430.869635	9.585715
7.742717	433.857245	9.590733
8.007905	444.886166	9.595751
7.948950	436.627432	9.600768
7.716890	447.522828	9.605786
8.337546	441.057373	9.610803
8.092182	452.481866	9.615821
8.247943	454.281583	9.620839
8.089240	445.864907	9.625856
8.076882	446.589607	9.630874
7.784714	445.382647	9.635891
8.159987	447.438300	9.640909
7.820047	450.713681	9.645927
8.334835	443.078250	9.650944
8.199246	451.279300	9.655962
8.113876	443.690565	9.660979
7.867935	446.436831	9.665997
7.866393	446.263603	9.671015
8.381976	441.099002	9.676032
8.284425	442.054796	9.681050
8.563682	442.689625	9.686067
8.550887	447.280190	9.691085
7.995294	444.934252	9.696103
8.212883	436.584852	9.701120
7.945750	449.650590	9.706138
7.974158	441.949356	9.711155
7.932990	444.928621	9.716173
7.892667	448.996488	9.721191
8.417395	444.139717	9.726208
8.238336	446.509437	9.731226
8.322623	438.632195	9.736243
8.327939	440.988804	9.741261
8.203189	448.673767	9.746279
8.286214	448.023393	9.751296
8.092968	448.839550	9.756314
8.480367	442.675725	9.761331
8.346566	444.520809	9.766349
8.072849	445.318017	9.771367
8.240394	438.513309	9.776384
7.952819	436.671324	9.781402
8.217618	450.830813	9.786419
8.577219	451.740228	9.791437
8.116590	450.565973	9.796455
8.250124	444.877417	9.801472
8.136348	445.791573	9.806490
8.149215	431.121725	9.811507
8.308644	441.832704	9.816525
8.235932	445.908801	9.821543
8.271467	446.184192	9.826560
8.277351	444.839016	9.831578
8.143504	442.502738	9.836595
8.423352	443.664484	9.841613
7.956338	451.415698	9.846631
8.203479	443.815890	9.851648
8.252848	447.203840	9.856666
8.136922	453.915452	9.861683
8.496554	459.463820	9.866701
8.426393	463.997106	9.871719
8.724548	460.397107	9.876736
8.836226	456.308783	9.881754
8.310884	450.745548	9.886771
8.517349	442.202232	9.891789
8.245320	448.386043	9.896807
8.461358	444.849406	9.901824
8.281861	440.825641	9.906842
8.174609	447.075151	9.911859
8.300556	441.170038	9.916877
8.589139	462.271619	9.921895
8.819699	453.847597	9.926912
8.376672	450.815002	9.931930
8.052001	450.272687	9.936947
8.725543	463.942118	9.941965
8.581041	464.744327	9.946983
8.866329	465.930469	9.952000
8.287835	448.247998	9.957018
8.062568	450.258890	9.962035
8.780509	456.574769	9.967053
8.343407	459.862220	9.972071
8.529208	459.514474	9.977088
8.631839	471.809092	9.982106
8.362755	469.538179	9.987123
8.718263	473.717600	9.992141
8.930977	475.760856	9.997159
9.033002	464.046579	10.002176
8.356480	451.315066	10.007194
8.602186	450.863262	10.012211
8.455334	455.509545	10.017229
8.228921	472.854433	10.022247
8.741512	471.751752	10.027264
8.788748	475.345166	10.032282
8.634489	484.331784	10.037299
8.750870	484.733362	10.042317
8.653470	485.600774	10.047335
8.836298	477.730166	10.052352
8.918908	477.269201	10.057370
8.445967	457.752467	10.062387
8.661270	465.734446	10.067405
8.762554	477.732639	10.072423
8.820634	475.028618	10.077440
8.749167	459.728186	10.082458
8.350989	457.846724	10.087475
8.619657	456.573981	10.092493
8.558158	467.938120	10.097511
8.542503	477.392160	10.102528
8.654607	474.591314	10.107546
8.645901	482.974467	10.112563
8.817298	474.452409	10.117581
8.428797	479.938123	10.122599
8.367165	470.404867	10.127616
8.713731	473.443305	10.132634
8.567259	485.666510	10.137651
8.654606	471.884350	10.142669
8.458498	484.408818	10.147687
8.425739	484.249947	10.152704
8.866079	494.478295	10.157722
8.647640	508.271737	10.162739
8.903930	496.697368	10.167757
8.994442	506.939509	10.172775
9.162012	510.346821	10.177792
8.961727	508.137706	10.182810
9.079688	497.257188	10.187827
9.188851	483.878694	10.192845
8.650633	481.406954	10.197863
8.892070	473.031711	10.202880
9.084797	475.933309	10.207898
8.852709	478.118840	10.212915
8.821936	465.437617	10.217933
8.872032	478.488385	10.222951
8.723467	471.812086	10.227968
8.674466	478.914002	10.232986
8.836702	503.891766	10.238003
9.275930	496.678400	10.243021
9.198588	505.312155	10.248039
9.213515	496.357017	10.253056
9.147085	485.088836	10.258074
8.640597	477.941603	10.263091
9.277574	470.050334	10.268109
8.809788	469.079168	10.273127
9.007835	477.584556	10.278144
9.206812	473.971693	10.283162
8.709995	470.354239	10.288179
9.118739	478.577312	10.293197
8.955340	479.978920	10.298215
9.004117	491.821249	10.303232
9.116032	495.382443	10.308250
9.180355	494.728686	10.313267
9.233734	489.671203	10.318285
8.988574	474.391660	10.323303
9.123656	479.501854	10.328320
9.385668	474.228652	10.333338
9.036303	487.799600	10.338355
8.947311	484.462223	10.343373
8.983921	484.939415	10.348391
9.114751	489.362322	10.353408
9.205908	492.541765	10.358426
9.250058	499.102082	10.363443
9.421633	488.086938	10.368461
8.796721	476.663272	10.373479
8.924170	494.262002	10.378496
9.519126	501.152580	10.383514
9.571442	500.144103	10.388531
9.525575	472.762553	10.393549
9.144640	474.015210	10.398567
9.189010	469.019104	10.403584
9.220919	476.117809	10.408602
8.579776	472.362025	10.413619
8.979795	488.415903	10.418637
9.061359	486.626527	10.423655
9.450135	498.447147	10.428672
9.570596	497.528978	10.433690
9.336004	505.149126	10.438707
9.349852	501.129767	10.443725
9.261815	489.896526	10.448743
9.377340	488.590973	10.453760
9.176244	486.934246	10.458778
9.189126	489.977632	10.463795
9.454948	492.261874	10.468813
9.652177	493.212510	10.473831
9.286879	479.864177	10.478848
9.088460	468.578817	10.483866
8.916479	491.633426	10.488883
9.201806	493.810472	10.493901
9.266658	486.327569	10.498919
8.847650	495.109524	10.503936
9.537275	495.216162	10.508954
9.280596	494.852537	10.513971
9.377203	493.117608	10.518989
9.440372	501.612583	10.524007
9.347482	494.955954	10.529024
9.505664	494.268557	10.534042
9.298359	494.342159	10.539059
9.274898	491.833946	10.544077
9.540481	497.800999	10.549095
9.265900	500.535982	10.554112
9.423714	495.667258	10.559130
9.040317	505.049545	10.564147
9.684536	505.762892	10.569165
9.727196	507.820173	10.574183
9.481817	507.940766	10.579200
9.723208	495.387290	10.584218
9.622108	502.156556	10.589235
9.335969	495.514426	10.594253
9.564797	500.603626	10.599271
9.427218	503.377103	10.604288
9.469460	496.651965	10.609306
9.747995	507.924982	10.614323
9.646891	500.808897	10.619341
9.698890	494.662891	10.624359
9.743814	487.703810	10.629376
9.998856	492.309224	10.634394
9.248165	505.210928	10.639411
9.356429	506.456367	10.644429
9.943874	506.995575	10.649447
9.649643	506.918697	10.654464
9.634956	498.832877	10.659482
9.606521	503.706769	10.664499
9.253789	492.587581	10.669517
9.393262	496.185482	10.674535
9.474192	502.717947	10.679552
9.880925	510.477453	10.684570
9.679461	509.985258	10.689587
9.730698	501.087544	10.694605
9.788178	503.432832	10.699623
9.473436	508.250600	10.704640
9.906855	505.604530	10.709658
9.517435	513.564516	10.714675
9.839493	515.603268	10.719693
9.806460	521.976874	10.724711
9.727914	526.391570	10.729728
10.026391	516.808179	10.734746
9.692844	511.565163	10.739763
9.678318	515.556421	10.744781
9.743934	508.897043	10.749799
9.995035	519.675756	10.754816
9.940957	506.363846	10.759834
10.024151	509.437244	10.764851
9.845316	497.460841	10.769869
10.127508	490.092204	10.774887
9.654070	497.001856	10.779904
10.258221	496.408684	10.784922
9.912270	496.308351	10.789939
9.872262	493.121087	10.794957
10.021315	497.651592	10.799975
9.849067	496.656210	10.804992
9.729515	494.371333	10.810010
9.865618	501.501059	10.815027
9.772250	506.060082	10.820045
9.685313	498.184395	10.825063
9.770751	503.611638	10.830080
9.798778	505.008502	10.835098
9.812933	514.912321	10.840115
9.689702	519.343485	10.845133
9.820490	521.285975	10.850151
9.844492	531.589043	10.855168
9.922201	527.035816	10.860186
9.899362	524.565370	10.865203
9.973192	529.268614	10.870221
10.203836	520.465855	10.875239
10.065495	524.549097	10.880256
10.194360	521.786643	10.885274
10.120161	520.072161	10.890291
9.854050	530.019901	10.895309
10.159828	521.438897	10.900327
10.090974	529.127760	10.905344
10.065116	520.939540	10.910362
9.876358	525.601875	10.915379
9.792538	523.888900	10.920397
10.050438	522.993376	10.925415
10.153954	523.261273	10.930432
10.185781	528.173066	10.935450
9.990120	525.265801	10.940467
9.963979	524.910235	10.945485
10.211077	524.884240	10.950503
9.828163	524.534082	10.955520
10.185518	527.375181	10.960538
10.079025	521.203506	10.965555
10.263819	528.429755	10.970573
10.087446	527.346656	10.975591
10.436744	525.139792	10.980608
10.095060	523.773329	10.985626
10.013898	518.456054	10.990643
9.815837	528.042841	10.995661
10.018926	535.231512	11.000679
10.005738	556.639260	11.005696
10.225051	548.482041	11.010714
10.009726	545.568386	11.015731
9.990689	550.245160	11.020749
10.526240	546.626884	11.025767
10.344515	542.565576	11.030784
10.338491	546.653338	11.035802
10.436974	537.748203	11.040819
10.119887	543.834966	11.045837
10.160669	550.503126	11.050855
9.917136	548.215577	11.055872
10.284025	544.172452	11.060890
10.626530	534.178214	11.065907
9.868107	546.506809	11.070925
10.315511	540.901587	11.075943
10.032481	551.126541	11.080960
9.919076	541.036476	11.085978
10.381152	545.634713	11.090995
10.549264	566.130451	11.096013
10.600659	569.101545	11.101031
10.521338	572.500215	11.106048
10.374723	555.295919	11.111066
10.647708	559.074884	11.116083
10.033723	563.838567	11.121101
10.729679	559.627117	11.126119
10.564578	562.505899	11.131136
10.432875	554.596176	11.136154
10.641124	556.595961	11.141171
10.356485	562.128542	11.146189
10.588874	565.014474	11.151207
10.585597	562.966987	11.156224
10.779840	562.409635	11.161242
10.484739	550.817483	11.166259
10.129555	552.507919	11.171277
10.404001	562.127988	11.176295
10.645259	573.997018	11.181312
10.449876	572.882181	11.186330
11.145147	574.748857	11.191347
10.678271	561.047152	11.196365
10.760908	545.997052	11.201383
10.727217	550.695058	11.206400
10.383790	545.119069	11.211418
10.907931	545.510408	11.216435
10.512496	548.182283	11.221453
10.842039	537.817693	11.226471
10.527120	541.919138	11.231488
10.420737	548.351582	11.236506
10.738905	550.690746	11.241523
10.688571	563.451202	11.246541
10.806510	570.356586	11.251559
10.773769	570.162999	11.256576
10.872280	572.744863	11.261594
10.758287	554.210032	11.266611
10.614611	561.052262	11.271629
10.693082	570.368529	11.276647
11.084050	567.123193	11.281664
10.657087	555.040463	11.286682
11.092949	549.222454	11.291699
11.151505	557.967485	11.296717
10.796008	549.808809	11.301735
10.580225	553.153117	11.306752
10.859610	544.775051	11.311770
10.703743	543.720295	11.316787
10.652206	544.779338	11.321805
10.804542	554.289148	11.326823
10.985740	565.287122	11.331840
10.828876	568.792614	11.336858
11.009639	562.490712	11.341875
11.173517	551.483047	11.346893
11.080580	547.268972	11.351911
10.973140	543.416929	11.356928
10.668864	555.516586	11.361946
10.569265	544.319836	11.366963
10.659446	552.233097	11.371981
10.894492	556.005382	11.376999
10.994520	567.738747	11.382016
11.194322	571.456598	11.387034
11.138733	568.647298	11.392051
11.171801	567.657612	11.397069
10.784776	564.411097	11.402087
11.050913	570.343374	11.407104
10.548421	564.599799	11.412122
10.765566	562.703968	11.417139
10.952785	569.140910	11.422157
10.661142	566.021460	11.427175
10.881054	565.646277	11.432192
10.355738	566.006388	11.437210
10.518510	569.606966	11.442227
11.089519	587.420310	11.447245
11.272771	587.685182	11.452263
11.516170	598.906958	11.457280
11.320823	582.969427	11.462298
11.692372	565.125364	11.467315
11.110830	571.477631	11.472333
11.218405	568.544938	11.477351
11.435365	556.329759	11.482368
10.982687	558.054405	11.487386
11.571127	544.641797	11.492403
11.603942	558.695711	11.497421
11.082349	565.073296	11.502439
11.049609	570.433870	11.507456
11.444562	572.688424	11.512474
11.463007	553.274472	11.517491
11.143121	558.970364	11.522509
11.232594	562.528776	11.527527
11.419042	560.890216	11.532544
10.485510	565.164329	11.537562
11.038149	549.816526	11.542579
10.777954	563.319911	11.547597
11.431520	559.885111	11.552615
11.352131	573.467471	11.557632
11.292899	569.819306	11.562650
11.093143	559.067424	11.567667
11.170649	576.298523	11.572685
11.269978	578.526813	11.577703
11.458005	582.710410	11.582720
11.203997	588.970340	11.587738
11.661970	588.526300	11.592755
11.651122	590.932798	11.597773
11.472391	574.468812	11.602791
11.407617	566.728477	11.607808
10.907559	568.728788	11.612826
11.439403	580.864715	11.617843
11.559503	585.159941	11.622861
11.264164	595.629844	11.627879
11.863292	588.848976	11.632896
11.735397	585.290460	11.637914
11.344379	577.200452	11.642931
11.492037	582.387599	11.647949
11.869813	585.007759	11.652967
11.182942	569.014710	11.657984
11.127222	569.033004	11.663002
11.749442	592.165277	11.668019
11.260827	586.239641	11.673037
11.503086	591.620250	11.678055
11.529851	582.287676	11.683072
11.558897	589.557287	11.688090
11.424038	585.390797	11.693107
11.741328	593.123327	11.698125
11.472260	592.521803	11.703143
11.985998	584.652949	11.708160
11.824146	590.863727	11.713178
11.942050	584.802037	11.718195
11.814844	593.547789	11.723213
11.405450	588.007368	11.728231
11.689192	580.322873	11.733248
11.495664	583.404927	11.738266
11.615604	585.241828	11.743283
11.807510	585.729404	11.748301
11.927524	590.409649	11.753319
11.970099	589.860281	11.758336
11.488896	595.190142	11.763354
11.784314	581.040785	11.768371
11.936723	588.268976	11.773389
11.976576	586.322026	11.778407
11.950659	586.373520	11.783424
11.818928	576.592416	11.788442
11.830094	568.960100	11.793459
11.717401	576.040476	11.798477
11.715766	586.527472	11.803495
12.091262	583.234065	11.808512
11.747730	591.543499	11.813530
11.908562	587.482157	11.818547
11.987873	581.224545	11.823565
11.722930	586.479495	11.828583
11.866876	573.439464	11.833600
11.852034	582.978639	11.838618
11.664013	583.169139	11.843635
11.765603	588.360350	11.848653
11.969281	590.954141	11.853671
12.110267	584.260835	11.858688
12.189852	588.997907	11.863706
12.180596	587.579354	11.868723
12.284751	585.928439	11.873741
12.104193	582.308747	11.878759
11.816456	570.305177	11.883776
11.647119	567.119228	11.888794
11.990411	570.517954	11.893811
12.327955	574.296274	11.898829
11.981486	580.141503	11.903847
12.135506	569.611893	11.908864
12.012386	581.301336	11.913882
11.797880	582.518457	11.918899
11.908222	581.532442	11.923917
11.876463	583.008106	11.928935
12.214878	579.486982	11.933952
12.148730	580.693481	11.938970
11.947900	582.776298	11.943987
11.847802	582.195636	11.949005
12.123487	589.129961	11.954023
12.098969	572.061152	11.959040
11.741071	586.870575	11.964058
11.913697	591.286958	11.969075
12.036538	584.542847	11.974093
11.742143	587.564967	11.979111
12.572559	603.030811	11.984128
12.449170	601.361898	11.989146
12.231165	598.032090	11.994163
12.073655	591.925188	11.999181
11.884383	603.170578	12.004199
12.450019	610.788466	12.009216
12.455570	615.455094	12.014234
12.347087	612.190174	12.019251
12.580966	607.612458	12.024269
12.434699	603.602384	12.029287
12.300480	587.680518	12.034304
12.061044	584.461367	12.039322
12.474913	600.831910	12.044339
12.491464	601.880288	12.049357
12.228184	603.168168	12.054375
12.642748	592.496738	12.059392
12.747554	592.751811	12.064410
12.321497	594.241918	12.069427
12.013874	591.440545	12.074445
12.439240	598.070557	12.079463
12.525501	602.068133	12.084480
12.398318	602.002951	12.089498
12.561351	603.586951	12.094515
12.534336	602.628767	12.099533
12.157582	601.706446	12.104551
12.638801	610.997501	12.109568
12.578950	601.318729	12.114586
12.664885	616.443642	12.119603
12.574879	608.931302	12.124621
12.592948	603.951902	12.129639
12.685481	599.254323	12.134656
12.612848	595.687147	12.139674
12.436825	592.404411	12.144691
12.817121	584.215641	12.149709
12.591988	592.149921	12.154727
12.434309	584.670285	12.159744
12.588839	588.511996	12.164762
12.357183	608.423484	12.169779
12.926381	595.026477	12.174797
12.709499	607.191370	12.179815
12.305953	603.205828	12.184832
12.773767	602.110155	12.189850
12.635980	605.297087	12.194867
12.961480	607.300598	12.199885
13.026093	607.565123	12.204903
12.692409	599.380916	12.209920
12.807803	596.630028	12.214938
12.709505	601.855717	12.219955
12.519261	601.147169	12.224973
12.328649	614.216815	12.229991
12.718858	607.793719	12.235008
12.741358	607.632501	12.240026
12.798874	609.693779	12.245043
12.993520	609.190011	12.250061
13.004287	606.203052	12.255079
13.240147	610.918800	12.260096
12.936924	605.513216	12.265114
12.887167	603.438294	12.270131
12.945064	598.963891	12.275149
12.893412	612.863825	12.280167
12.996372	607.618660	12.285184
13.016354	606.937133	12.290202
12.611798	605.397479	12.295219
13.247110	604.278718	12.300237
12.539111	603.383050	12.305255
12.965424	600.854844	12.310272
12.611871	598.846455	12.315290
12.817734	602.844227	12.320307
13.023518	601.871659	12.325325
12.972779	609.668171	12.330343
12.711695	598.010698	12.335360
12.989645	611.319351	12.340378
12.646523	604.054953	12.345395
13.113780	598.089999	12.350413
12.837209	608.856769	12.355431
12.812499	603.928252	12.360448
13.484441	610.355534	12.365466
13.151588	618.249900	12.370483
13.134087	600.615079	12.375501
13.006914	613.567489	12.380519
12.762143	609.686456	12.385536
13.054279	616.854897	12.390554
13.105788	623.019634	12.395571
13.272958	626.379694	12.400589
12.883979	628.955896	12.405607
13.312107	630.066021	12.410624
13.431927	627.869853	12.415642
13.361191	634.404039	12.420659
13.321357	617.612140	12.425677
13.300629	628.449288	12.430695
13.249159	624.881946	12.435712
13.389636	623.054924	12.440730
13.087665	629.041518	12.445747
13.398351	632.457988	12.450765
13.382215	633.041277	12.455783
13.528321	628.508866	12.460800
13.929366	631.201126	12.465818
13.177086	625.660769	12.470835
13.199542	605.921086	12.475853
13.319136	614.864863	12.480871
13.454092	622.799542	12.485888
13.875064	617.488770	12.490906
13.580965	610.507020	12.495923
13.828143	603.702395	12.500941
13.379956	595.365718	12.505959
13.641638	596.533477	12.510976
13.511992	594.764560	12.515994
13.309479	606.195061	12.521011
13.048988	604.254142	12.526029
13.171955	609.445165	12.531047
13.385557	614.852362	12.536064
13.512040	615.362812	12.541082
13.515273	622.099998	12.546099
13.748276	625.474989	12.551117
13.607063	625.036466	12.556135
13.766038	627.043980	12.561152
13.556951	610.578405	12.566170
13.089308	610.156314	12.571187
13.392982	619.475191	12.576205
13.784200	620.442777	12.581223
13.762113	634.852488	12.586240
13.974919	621.760607	12.591258
13.570406	626.971166	12.596275
13.552322	617.128052	12.601293
13.518494	629.153827	12.606311
13.402974	622.005239	12.611328
13.803198	628.904287	12.616346
13.371061	629.082543	12.621363
13.776782	623.916169	12.626381
13.665264	624.798423	12.631399
13.616865	636.466726	12.636416
13.753505	622.648325	12.641434
13.792973	631.519458	12.646451
13.594580	619.959444	12.651469
13.523017	624.726519	12.656487
13.756939	628.401166	12.661504
13.521166	620.845388	12.666522
13.858838	642.971434	12.671539
13.871627	646.841678	12.676557
14.070074	638.952772	12.681575
13.351133	640.697054	12.686592
13.858152	638.367635	12.691610
14.068036	652.924052	12.696627
14.285505	646.966661	12.701645
14.182050	652.884291	12.706663
13.894302	637.260988	12.711680
14.163719	637.925768	12.716698
13.859891	635.224779	12.721715
13.837657	634.108055	12.726733
13.918914	638.709179	12.731751
14.324006	644.853238	12.736768
14.024515	640.532650	12.741786
13.793435	641.973277	12.746803
14.320840	642.266278	12.751821
14.632756	643.867980	12.756839
13.712344	632.559940	12.761856
13.948519	629.591308	12.766874
14.144335	644.493902	12.771891
14.649173	639.046908	12.776909
13.993678	627.407031	12.781927
14.168104	630.365171	12.786944
14.245903	618.367412	12.791962
14.144721	631.281049	12.796979
13.976210	620.666245	12.801997
14.171941	627.616267	12.807015
14.176418	638.705091	12.812032
14.250507	638.617840	12.817050
14.271788	650.729669	12.822067
14.208054	638.769851	12.827085
14.513179	637.705977	12.832103
14.310037	637.138303	12.837120
14.152728	634.474317	12.842138
14.184923	633.737227	12.847155
14.167959	643.030615	12.852173
14.565616	643.735263	12.857191
14.380440	644.218806	12.862208
14.760271	645.734129	12.867226
14.191162	631.477190	12.872243
14.216375	636.579396	12.877261
14.233787	633.342085	12.882279
14.064112	645.363909	12.887296
14.747951	648.955445	12.892314
14.507173	644.991728	12.897331
14.364564	650.337982	12.902349
14.462707	646.819777	12.907367
14.250945	647.458963	12.912384
14.566703	644.155970	12.917402
14.108375	650.324859	12.922419
13.787283	643.031747	12.927437
13.999930	646.290012	12.932455
13.904144	656.110150	12.937472
14.165100	662.579754	12.942490
14.778701	667.911672	12.947507
14.887928	676.427916	12.952525
15.034253	666.969269	12.957543
14.630373	665.994390	12.962560
15.025567	663.291171	12.967578
14.853289	653.368055	12.972595
14.705325	653.817366	12.977613
14.780608	634.239788	12.982631
14.443210	641.601548	12.987648
14.697887	644.597609	12.992666
14.798582	644.739718	12.997683
14.628970	643.380998	13.002701
15.128327	641.415695	13.007719
14.735218	648.612619	13.012736
14.815532	648.685338	13.017754
14.827394	636.669496	13.022771
14.636323	638.252176	13.027789
15.211814	639.430731	13.032807
14.917660	650.512703	13.037824
14.604461	635.982136	13.042842
14.995286	642.017977	13.047859
14.789563	644.899981	13.052877
14.868874	642.277816	13.057895
14.538382	651.004953	13.062912
14.839910	660.557717	13.067930
14.843224	665.634961	13.072947
15.416063	675.539697	13.077965
15.032589	654.699074	13.082983
14.685033	656.082213	13.088000
14.930219	650.912581	13.093018
15.134038	664.346497	13.098035
15.296019	662.910576	13.103053
15.282436	643.637244	13.108071
15.061234	648.834866	13.113088
15.125913	642.983466	13.118106
14.678930	639.285587	13.123123
14.816362	648.681019	13.128141
14.960510	657.687242	13.133159
15.092545	674.029426	13.138176
15.030597	667.689776	13.143194
15.322754	670.118238	13.148211
15.280397	674.404225	13.153229
15.608891	656.320664	13.158247
15.105574	659.473359	13.163264
15.137655	651.695721	13.168282
15.004800	642.448085	13.173299
15.247168	652.748568	13.178317
15.378419	656.123729	13.183335
14.807676	658.172994	13.188352
14.925223	661.805922	13.193370
15.315827	675.980594	13.198387
15.184087	674.764261	13.203405
15.218921	673.878433	13.208423
15.173415	670.994954	13.213440
15.387756	671.722014	13.218458
15.426692	678.024439	13.223475
15.192668	679.579139	13.228493
15.375197	671.036308	13.233511
15.397141	668.994325	13.238528
15.398648	666.785132	13.243546
15.624539	666.860288	13.248563
15.493582	678.399544	13.253581
15.593830	674.732682	13.258599
15.401348	674.220140	13.263616
15.548742	671.177050	13.268634
15.663998	665.497598	13.273651
15.227476	666.528605	13.278669
15.452473	663.258764	13.283687
15.350018	668.245283	13.288704
15.679685	670.260771	13.293722
15.393315	670.476149	13.298739
15.513701	663.943830	13.303757
15.571550	667.049628	13.308775
15.560291	660.017232	13.313792
15.442971	665.873922	13.318810
15.493078	662.659885	13.323827
15.562486	668.941754	13.328845
15.428568	666.094218	13.333863
15.444221	673.003045	13.338880
15.587820	680.967954	13.343898
15.819349	686.867824	13.348915
15.780424	689.635339	13.353933
15.833985	686.780517	13.358951
15.959397	694.139213	13.363968
15.595471	682.725015	13.368986
15.631902	671.377484	13.374003
15.575817	679.392614	13.379021
16.017897	678.048505	13.384039
15.998585	685.196344	13.389056
16.119801	685.982176	13.394074
15.959809	671.153022	13.399091
15.479133	667.072253	13.404109
15.878053	665.899008	13.409127
15.928413	681.632306	13.414144
16.054342	683.253685	13.419162
16.054247	679.331145	13.424179
16.034821	680.722834	13.429197
16.119467	665.079030	13.434215
15.697055	672.517239	13.439232
15.686913	674.794250	13.444250
16.057545	686.374843	13.449267
16.075092	694.410000	13.454285
16.444929	682.571569	13.459303
16.153614	684.551810	13.464320
15.677568	674.417502	13.469338
16.250376	675.836320	13.474355
15.958840	683.175132	13.479373
16.448954	674.694561	13.484391
16.085714	674.092009	13.489408
16.086487	674.631625	13.494426
16.228279	674.028840	13.499443
15.948142	671.182122	13.504461
15.989772	684.922330	13.509479
16.729989	685.434453	13.514496
16.248887	682.843282	13.519514
16.118165	663.771318	13.524531
16.026778	667.354932	13.529549
16.223364	672.812149	13.534567
16.146197	683.869612	13.539584
16.301649	681.598427	13.544602
16.290728	679.233390	13.549619
16.168979	682.402043	13.554637
16.224313	686.477068	13.559655
16.229207	684.333613	13.564672
16.086058	682.207043	13.569690
16.495533	686.860895	13.574707
15.971083	684.175530	13.579725
16.261653	685.079995	13.584743
15.930254	677.659095	13.589760
15.941264	676.751754	13.594778
16.558698	692.812778	13.599795
16.352276	705.427378	13.604813
16.667721	707.031689	13.609831
16.704086	703.299090	13.614848
16.744537	702.936244	13.619866
16.235766	684.071812	13.624883
16.425164	688.299401	13.629901
16.665262	694.592404	13.634919
16.512013	706.251935	13.639936
16.309956	705.005592	13.644954
16.711678	708.493020	13.649971
16.593576	710.780639	13.654989
16.827922	700.146849	13.660007
17.084374	701.952907	13.665024
16.958272	701.641402	13.670042
16.715272	687.582631	13.675059
16.512180	689.261873	13.680077
16.783685	684.473115	13.685095
16.733259	686.513444	13.690112
16.502856	700.274195	13.695130
16.694804	697.265145	13.700147
16.698161	709.739583	13.705165
16.945817	702.414140	13.710183
16.950674	707.185041	13.715200
16.732852	708.825567	13.720218
17.371076	704.474807	13.725235
17.031498	703.360464	13.730253
16.806833	687.689363	13.735271
16.944871	678.134179	13.740288
16.718010	685.238797	13.745306
16.997221	686.416440	13.750323
16.897513	701.725145	13.755341
16.993153	697.443619	13.760359
17.046998	702.787511	13.765376
16.952550	700.520764	13.770394
17.393077	701.647886	13.775411
17.080459	691.292303	13.780429
16.892669	686.736452	13.785447
16.855936	673.361740	13.790464
16.922594	700.535407	13.795482
17.181105	691.595655	13.800499
17.121751	693.533242	13.805517
17.253913	702.998957	13.810535
17.332148	697.186440	13.815552
17.155614	686.364571	13.820570
16.642530	684.245469	13.825587
16.661515	694.536794	13.830605
16.946930	701.905138	13.835623
16.936201	697.444619	13.840640
17.056014	698.688262	13.845658
17.144632	700.539550	13.850675
17.506147	699.577290	13.855693
17.186517	708.375337	13.860711
17.346903	700.085271	13.865728
17.414533	705.436471	13.870746
17.016464	698.171175	13.875763
17.044016	711.424461	13.880781
17.238976	710.302105	13.885799
17.708035	705.457143	13.890816
17.235549	706.364398	13.895834
17.226531	703.399458	13.900851
17.074029	714.203656	13.905869
17.119363	722.461690	13.910887
17.666652	724.477801	13.915904
17.573538	722.961923	13.920922
17.505737	723.411299	13.925939
17.278993	724.081238	13.930957
17.436222	719.111560	13.935975
17.858179	727.238004	13.940992
17.478145	732.428978	13.946010
17.539419	726.335088	13.951027
17.571287	732.452447	13.956045
17.637903	729.355732	13.961063
17.606033	729.127292	13.966080
17.418514	726.379663	13.971098
17.620214	729.308300	13.976115
17.635005	724.685985	13.981133
17.748958	729.525006	13.986151
18.168192	725.356875	13.991168
17.859791	738.631260	13.996186
17.944980	720.620470	14.001203
17.942503	731.508470	14.006221
18.004102	729.895767	14.011239
17.891667	705.670624	14.016256
17.824363	707.262320	14.021274
17.911375	706.983697	14.026291
17.599255	695.630801	14.031309
17.509867	709.536723	14.036327
17.609595	710.976017	14.041344
17.674464	721.847148	14.046362
17.587026	718.386407	14.051379
17.875441	719.329081	14.056397
17.946241	719.409603	14.061415
18.073328	718.503007	14.066432
17.982867	720.019438	14.071450
17.946819	725.367954	14.076467
17.936088	718.133480	14.081485
17.796460	729.055590	14.086503
17.885333	706.670296	14.091520
18.152099	718.633256	14.096538
17.847239	713.707577	14.101555
18.045767	718.277724	14.106573
17.998283	718.493543	14.111591
18.150855	716.213338	14.116608
18.140362	721.542069	14.121626
18.281734	718.575654	14.126643
18.430159	711.335181	14.131661
18.439437	725.007906	14.136679
18.563804	718.639046	14.141696
18.398892	714.287886	14.146714
18.521379	717.023805	14.151731
18.508258	715.637405	14.156749
18.092261	720.070307	14.161767
18.397353	713.739404	14.166784
18.364607	708.849987	14.171802
18.118199	717.207377	14.176819
18.324576	718.478484	14.181837
18.205429	721.359560	14.186855
18.385731	720.267902	14.191872
17.854063	723.245169	14.196890
17.881111	708.860048	14.201907
18.553492	715.725956	14.206925
18.308753	740.625806	14.211943
18.559188	737.793778	14.216960
18.775491	738.239666	14.221978
18.493431	730.681626	14.226995
18.520483	718.426664	14.232013
18.302325	725.009228	14.237031
18.602230	733.757556	14.242048
18.418091	737.715478	14.247066
18.005158	740.080853	14.252083
18.210412	745.309517	14.257101
18.502832	743.373470	14.262119
18.820787	741.461825	14.267136
18.196405	737.255233	14.272154
18.050931	743.195255	14.277171
18.640998	748.802284	14.282189
18.486684	760.449394	14.287207
19.105382	762.028287	14.292224
18.596430	759.331015	14.297242
19.167533	756.268861	14.302259
19.072320	742.704444	14.307277
18.400007	740.512452	14.312295
18.929030	738.236378	14.317312
18.957457	742.470265	14.322330
19.107288	740.969970	14.327347
19.085035	740.960930	14.332365
18.727785	734.995727	14.337383
18.880145	736.988510	14.342400
18.819147	737.083370	14.347418
18.642050	738.928957	14.352435
19.187337	739.399040	14.357453
18.989408	746.139388	14.362471
19.075876	742.888081	14.367488
18.878887	748.817241	14.372506
18.953414	750.636028	14.377523
19.049381	751.902346	14.382541
18.805198	762.007725	14.387559
19.027504	762.847150	14.392576
19.209428	752.313060	14.397594
18.960759	757.281488	14.402611
19.429768	747.201039	14.407629
19.304280	758.272431	14.412647
19.374810	749.699774	14.417664
19.207912	748.889731	14.422682
19.378782	762.603438	14.427699
19.429658	750.799157	14.432717
19.425566	749.739544	14.437735
19.554550	742.691454	14.442752
19.022627	732.275533	14.447770
19.301663	744.713114	14.452787
19.453515	738.103255	14.457805
19.732210	727.279464	14.462823
19.528484	733.642019	14.467840
19.319148	726.640631	14.472858
19.225132	728.851896	14.477875
19.405793	719.349971	14.482893
19.102274	734.400304	14.487911
19.572224	741.891231	14.492928
19.657689	746.630579	14.497946
19.336529	742.449060	14.502963
19.212696	733.537634	14.507981
19.187306	750.276939	14.512999
19.645261	759.953570	14.518016
19.491533	750.974236	14.523034
19.281661	752.525158	14.528051
19.455065	747.489822	14.533069
19.917743	752.425690	14.538087
19.680353	747.874439	14.543104
19.786427	750.089071	14.548122
19.577130	756.263159	14.553139
19.867511	749.432775	14.558157
19.689310	764.173164	14.563175
19.489597	755.882687	14.568192
19.903940	770.694344	14.573210
19.626346	758.263023	14.578227
20.274152	747.592827	14.583245
20.337893	750.249592	14.588263
19.936104	755.544967	14.593280
20.147684	760.308741	14.598298
19.846130	755.606594	14.603315
19.845885	743.646226	14.608333
19.680125	745.262819	14.613351
19.900596	758.324967	14.618368
20.019049	745.617008	14.623386
20.043732	756.055799	14.628403
20.161520	754.083997	14.633421
20.205648	759.836527	14.638439
19.907464	748.607646	14.643456
20.045040	752.379466	14.648474
20.010652	753.338004	14.653491
20.292538	749.390202	14.658509
20.097568	749.139980	14.663527
20.070702	748.951782	14.668544
20.057588	752.040311	14.673562
19.783198	756.286933	14.678579
20.082826	754.264549	14.683597
20.105043	754.456824	14.688615
20.029141	757.851838	14.693632
20.104177	755.659515	14.698650
19.837748	758.948681	14.703667
19.780947	743.595214	14.708685
20.134416	750.823527	14.713703
19.974678	753.862446	14.718720
20.286410	753.498120	14.723738
20.391251	780.628058	14.728755
20.849291	767.052678	14.733773
20.501724	758.176294	14.738791
20.240531	756.977082	14.743808
20.481104	740.526141	14.748826
19.977800	763.721375	14.753843
20.223607	761.385530	14.758861
20.559130	770.945650	14.763879
20.511530	779.729513	14.768896
20.545115	773.434817	14.773914
20.483083	780.084458	14.778931
20.716239	776.330479	14.783949
20.881145	777.390337	14.788967
20.547900	774.927465	14.793984
20.650163	768.091834	14.799002
20.646211	779.579699	14.804019
20.817896	771.142661	14.809037
20.683708	783.793336	14.814055
20.423665	772.384895	14.819072
20.556901	767.308509	14.824090
20.868027	767.089445	14.829107
20.771943	770.869476	14.834125
20.799914	774.093584	14.839143
20.400436	774.121556	14.844160
20.898445	769.540285	14.849178
20.833474	774.798672	14.854195
21.005325	772.231417	14.859213
20.833445	773.258835	14.864231
20.583627	776.031004	14.869248
20.948951	767.036609	14.874266
20.632103	776.459104	14.879283
20.836205	772.665496	14.884301
21.110536	775.276647	14.889319
20.600941	771.717937	14.894336
20.955357	767.222280	14.899354
20.671396	768.803747	14.904371
20.853588	771.634461	14.909389
20.749354	767.557804	14.914407
21.088750	786.903492	14.919424
21.465091	787.942847	14.924442
21.243101	786.791139	14.929459
21.005678	775.675797	14.934477
21.225284	781.918394	14.939495
21.268189	794.822197	14.944512
21.669394	782.903045	14.949530
20.968092	779.241826	14.954547
21.006933	769.061506	14.959565
21.181669	780.818020	14.964583
21.161015	790.863147	14.969600
21.415158	793.663656	14.974618
21.080088	799.980542	14.979635
21.481802	796.020268	14.984653
21.259840	799.943104	14.989671
21.270034	795.750682	14.994688
21.521519	795.102304	14.999706
21.437176	794.427648	15.004723
21.663863	795.916486	15.009741
21.747068	789.787579	15.014759
21.544821	792.545986	15.019776
21.393137	785.888993	15.024794
21.065216	793.299823	15.029811
21.552497	789.439753	15.034829
21.478937	792.850185	15.039847
21.445609	792.972269	15.044864
21.585841	799.344073	15.049882
21.897633	807.629826	15.054899
21.652858	803.732972	15.059917
22.204509	789.568550	15.064935
21.479667	796.855377	15.069952
21.725523	789.508089	15.074970
21.705856	798.435908	15.079987
21.749193	795.724682	15.085005
22.054185	789.819803	15.090023
21.560388	792.283062	15.095040
21.711306	787.330133	15.100058
21.716264	786.556279	15.105075
21.792603	788.813443	15.110093
21.959058	792.549189	15.115111
22.020224	792.233588	15.120128
22.133584	789.713364	15.125146
22.108625	798.320119	15.130163
21.873064	798.871520	15.135181
22.059501	796.418741	15.140199
21.948405	797.515532	15.145216
21.931072	787.665895	15.150234
21.960709	798.886577	15.155251
21.903831	795.443124	15.160269
21.895863	795.507585	15.165287
21.378598	807.284176	15.170304
21.904735	811.651539	15.175322
21.948504	815.772586	15.180339
22.241184	815.679489	15.185357
22.096320	816.759481	15.190375
22.107841	821.456786	15.195392
22.397918	813.316761	15.200410
22.456434	817.659561	15.205427
22.503850	823.250650	15.210445
22.478958	812.698436	15.215463
22.194985	817.934345	15.220480
22.683689	818.716254	15.225498
22.655446	822.990598	15.230515
22.530852	810.677280	15.235533
22.481748	794.678776	15.240551
22.096787	796.664234	15.245568
22.702070	797.090205	15.250586
22.523645	797.096166	15.255603
21.760123	802.217857	15.260621
22.087373	807.591527	15.265639
22.563636	807.816806	15.270656
22.770346	813.348219	15.275674
22.524154	805.443699	15.280691
22.188089	810.324848	15.285709
22.672304	805.761508	15.290727
22.536734	810.699607	15.295744
22.761539	806.334702	15.300762
23.030988	813.800269	15.305779
22.254042	815.408486	15.310797
22.606205	811.575893	15.315815
22.562357	820.337097	15.320832
22.309856	809.018969	15.325850
22.479472	829.735682	15.330867
22.883377	828.239753	15.335885
22.907064	833.616812	15.340903
23.077596	838.393349	15.345920
22.726104	836.075339	15.350938
22.620271	834.555133	15.355955
22.663497	846.389100	15.360973
22.834881	839.842416	15.365991
22.885795	840.361557	15.371008
22.781848	837.420935	15.376026
23.074111	836.027705	15.381043
22.950465	835.072025	15.386061
23.064183	825.637337	15.391079
22.928620	832.699308	15.396096
23.177342	825.181142	15.401114
23.299177	829.226845	15.406131
22.919699	833.284822	15.411149
23.212458	836.243390	15.416167
22.838731	837.138335	15.421184
22.916012	831.953933	15.426202
23.548090	848.486177	15.431219
23.320256	855.385887	15.436237
23.180002	840.187423	15.441255
23.562658	851.905096	15.446272
23.402277	849.812763	15.451290
23.529758	836.368018	15.456307
23.286756	834.481137	15.461325
23.573790	830.078074	15.466343
23.640050	825.561279	15.471360
23.501551	826.734949	15.476378
23.589163	822.053862	15.481395
23.321461	824.459610	15.486413
23.086040	824.726967	15.491431
23.309931	831.811513	15.496448
23.530296	848.086370	15.501466
23.785388	839.800335	15.506483
23.614164	857.897503	15.511501
23.899024	852.926726	15.516519
23.777056	846.905686	15.521536
23.645915	841.914883	15.526554
23.326381	840.238809	15.531571
23.454265	844.160491	15.536589
23.680755	844.765733	15.541607
23.619874	851.677154	15.546624
23.776008	850.191641	15.551642
23.926339	850.477454	15.556659
23.664427	854.984078	15.561677
23.972350	848.352881	15.566695
23.839420	849.077553	15.571712
23.843619	858.800086	15.576730
23.909836	842.609900	15.581747
23.809585	848.094745	15.586765
23.891484	846.289502	15.591783
23.611565	850.682180	15.596800
23.626046	852.879617	15.601818
24.138482	849.387980	15.606835
23.888244	855.344453	15.611853
23.813812	850.022869	15.616871
23.939631	852.944480	15.621888
24.240159	863.456881	15.626906
24.417310	852.431172	15.631923
24.299740	848.728973	15.636941
24.502526	845.437332	15.641959
24.180836	843.155678	15.646976
24.154089	839.092110	15.651994
23.900677	838.355579	15.657011
24.231129	861.918928	15.662029
24.456216	858.917282	15.667047
24.550134	863.431273	15.672064
24.392039	854.626141	15.677082
24.443828	847.624818	15.682099
24.176599	853.785926	15.687117
24.456280	854.045161	15.692135
25.053248	861.923340	15.697152
24.439130	853.823978	15.702170
24.369991	843.474339	15.707187
24.437158	844.839851	15.712205
24.407645	838.611823	15.717223
24.283837	852.302341	15.722240
24.474462	867.133352	15.727258
24.797713	862.557347	15.732275
24.492543	865.073113	15.737293
24.601340	857.999737	15.742311
24.517126	864.334147	15.747328
24.438270	862.942256	15.752346
24.956830	860.888714	15.757363
25.116930	863.445192	15.762381
24.907734	857.005467	15.767399
25.152745	864.610585	15.772416
25.132875	863.253633	15.777434
25.403294	852.538361	15.782451
24.969429	840.942513	15.787469
25.056358	833.781055	15.792487
24.750402	836.798715	15.797504
24.617193	841.073730	15.802522
24.681716	845.374571	15.807539
24.952904	864.970873	15.812557
24.891139	856.122245	15.817575
25.035717	856.371090	15.822592
24.871145	862.658129	15.827610
24.984980	850.853385	15.832627
24.771644	860.177653	15.837645
24.897361	853.896896	15.842663
25.149905	851.780893	15.847680
24.796980	871.134158	15.852698
25.195098	854.286041	15.857715
25.348659	866.926405	15.862733
25.501616	863.459530	15.867751
25.293425	859.500126	15.872768
25.278863	862.705667	15.877786
25.214180	860.333250	15.882803
24.931870	863.088432	15.887821
25.005731	866.671442	15.892839
25.445372	873.883149	15.897856
25.536125	887.719960	15.902874
25.529875	889.693430	15.907891
25.514924	886.622090	15.912909
25.608570	888.261169	15.917927
25.821336	881.900491	15.922944
25.455367	873.894786	15.927962
25.607644	874.139269	15.932979
25.470504	887.557346	15.937997
25.296917	891.349546	15.943015
26.067961	886.715999	15.948032
25.362200	885.100434	15.953050
25.779262	887.660836	15.958067
25.953677	890.019413	15.963085
25.452504	879.210421	15.968103
25.843148	881.162731	15.973120
25.443310	890.014459	15.978138
25.837441	887.128335	15.983155
25.851490	883.351858	15.988173
25.718198	891.637958	15.993191
25.716193	892.174860	15.998208
25.578655	892.493154	16.003226
26.014809	885.087609	16.008243
25.882367	877.136832	16.013261
25.874661	878.602440	16.018279
25.962662	881.056607	16.023296
25.844528	882.757269	16.028314
25.940989	876.840853	16.033331
25.948253	885.136485	16.038349
26.178598	891.932864	16.043367
26.478016	899.542096	16.048384
25.995156	894.218218	16.053402
26.386446	899.796479	16.058419
26.516217	886.692167	16.063437
26.582233	885.870872	16.068455
26.448568	875.449273	16.073472
26.078172	882.279811	16.078490
26.348615	868.525462	16.083507
26.002471	886.498585	16.088525
26.465343	895.139409	16.093543
26.612284	882.969691	16.098560
26.488492	885.722132	16.103578
26.620132	872.301955	16.108595
26.569985	877.198285	16.113613
26.386370	870.473679	16.118631
26.372363	876.203797	16.123648
26.335293	882.524515	16.128666
26.379866	891.666379	16.133683
26.732268	895.281494	16.138701
26.968461	899.362945	16.143719
26.945849	893.654528	16.148736
26.503692	889.229998	16.153754
26.695937	892.059157	16.158771
26.838140	900.696575	16.163789
26.653877	901.896356	16.168807
26.870950	894.619807	16.173824
26.739179	902.214546	16.178842
27.024829	897.811683	16.183859
26.618221	897.967005	16.188877
26.790310	898.779590	16.193895
26.885129	897.859107	16.198912
26.550005	885.452490	16.203930
26.631146	896.283308	16.208947
26.380676	899.061909	16.213965
26.548741	893.172138	16.218983
26.725501	884.002100	16.224000
26.830012	901.749995	16.229018
27.088116	907.973981	16.234035
27.113741	913.110917	16.239053
27.063807	921.002114	16.244071
27.120199	919.118808	16.249088
27.118249	921.684905	16.254106
27.047113	914.687036	16.259123
27.312740	910.994214	16.264141
27.382901	917.061456	16.269159
27.543162	916.092848	16.274176
27.578599	923.197490	16.279194
27.393879	921.673857	16.284211
27.555118	914.901514	16.289229
27.122985	917.576036	16.294247
27.413918	912.654785	16.299264
27.039942	920.230675	16.304282
27.708168	917.298446	16.309299
27.330132	917.600772	16.314317
27.151059	920.175685	16.319335
27.601526	904.461731	16.324352
27.529230	908.547336	16.329370
27.382929	916.340019	16.334387
27.523470	913.765025	16.339405
27.301630	921.493806	16.344423
27.344450	923.024086	16.349440
27.897792	928.169863	16.354458
27.798688	935.847862	16.359475
27.856561	946.180577	16.364493
27.833141	940.380754	16.369511
28.269530	936.149926	16.374528
28.013717	936.783400	16.379546
27.739575	922.341154	16.384563
28.140279	927.482444	16.389581
27.817637	926.665236	16.394599
28.205020	924.244072	16.399616
27.893498	930.901300	16.404634
28.167073	932.266037	16.409651
28.444467	914.022964	16.414669
27.947199	912.920689	16.419687
27.660731	906.669779	16.424704
28.178876	923.207321	16.429722
27.969061	942.370982	16.434739
28.309806	933.389822	16.439757
28.145440	938.190455	16.444775
28.185560	933.365300	16.449792
28.380946	932.268111	16.454810
27.925756	942.570755	16.459827
27.949074	932.440111	16.464845
28.161960	939.741022	16.469863
28.252421	937.704053	16.474880
28.122378	935.427073	16.479898
27.929263	933.163132	16.484915
28.300013	950.541155	16.489933
28.514312	963.140513	16.494951
28.251553	956.286261	16.499968
28.818300	955.579016	16.504986
28.971658	957.300265	16.510003
29.106140	947.392039	16.515021
28.825621	939.073111	16.520039
28.993648	931.125726	16.525056
28.831550	932.243140	16.530074
28.659320	934.599230	16.535091
28.890477	929.302327	16.540109
28.786889	929.485913	16.545127
28.447705	925.834199	16.550144
28.563846	933.364862	16.555162
28.484660	935.409725	16.560179
28.995218	935.699062	16.565197
28.565285	936.533388	16.570215
29.108063	940.579437	16.575232
29.264055	957.344167	16.580250
28.824180	951.123589	16.585267
29.049143	939.402362	16.590285
29.323795	946.100301	16.595303
29.092510	931.667112	16.600320
29.010401	930.364088	16.605338
28.680562	938.807238	16.610355
29.422663	943.342771	16.615373
29.312740	952.347925	16.620391
29.164372	948.451712	16.625408
29.215512	959.426126	16.630426
28.906163	955.962238	16.635443
29.375522	941.381395	16.640461
29.212836	959.922302	16.645479
29.392874	947.621122	16.650496
29.249026	944.304877	16.655514
28.676447	946.954070	16.660531
29.122363	948.257092	16.665549
29.393756	950.783522	16.670567
29.215181	946.159888	16.675584
29.212386	949.773860	16.680602
29.031852	964.675728	16.685619
29.471774	966.424664	16.690637
29.561370	966.761022	16.695655
29.809444	960.126537	16.700672
29.708744	950.684352	16.705690
29.626449	961.512414	16.710707
29.815675	954.779853	16.715725
29.883680	974.139864	16.720743
29.782394	958.174635	16.725760
29.736459	958.279760	16.730778
29.917163	958.756479	16.735795
29.927707	953.437329	16.740813
29.992795	957.681303	16.745831
29.875569	964.188180	16.750848
30.089073	956.359893	16.755866
29.952577	957.580595	16.760883
30.178460	953.215485	16.765901
30.000179	959.760329	16.770919
29.881455	950.235760	16.775936
30.444831	954.568922	16.780954
29.984414	963.344970	16.785971
30.252444	956.350751	16.790989
30.079280	964.633663	16.796007
30.019074	967.199427	16.801024
30.370511	965.916837	16.806042
30.036379	960.279299	16.811059
30.164264	960.786384	16.816077
30.297835	961.892189	16.821095
30.293980	963.780084	16.826112
30.383144	950.442244	16.831130
29.938865	966.707734	16.836147
30.393311	974.901787	16.841165
30.616466	977.060232	16.846183
30.220416	972.546405	16.851200
30.655109	986.256820	16.856218
30.320782	985.069050	16.861235
30.338336	987.108230	16.866253
30.500847	983.355809	16.871271
30.485117	985.261345	16.876288
30.732076	972.523623	16.881306
30.610735	989.609550	16.886323
30.846706	977.255404	16.891341
30.446227	980.101703	16.896359
30.647317	978.075798	16.901376
30.868544	971.265633	16.906394
30.572064	983.320175	16.911411
30.582425	974.946188	16.916429
30.709806	984.371775	16.921447
31.241240	990.382550	16.926464
31.105313	982.552194	16.931482
30.425778	982.964876	16.936499
30.892828	1003.578385	16.941517
31.068943	997.630514	16.946535
30.874062	998.465885	16.951552
31.525112	997.628664	16.956570
31.392558	994.812420	16.961587
31.367313	1001.424821	16.966605
31.547756	1004.779718	16.971623
31.102843	1005.632173	16.976640
31.599661	996.001671	16.981658
31.576862	991.950074	16.986675
31.308074	981.754713	16.991693
31.411288	977.090076	16.996711
31.353066	979.321011	17.001728
31.739226	976.152096	17.006746
31.529281	980.177232	17.011763
31.454232	982.710608	17.016781
31.518798	968.332023	17.021799
31.304788	978.347589	17.026816
31.859978	983.026028	17.031834
31.481449	988.573450	17.036851
31.877738	995.293376	17.041869
31.837235	988.167601	17.046887
31.525298	971.698870	17.051904
31.930785	979.477712	17.056922
31.928611	988.264028	17.061939
31.331148	981.657870	17.066957
31.651350	978.928484	17.071975
31.577350	986.204934	17.076992
31.614641	984.687537	17.082010
31.611547	987.402147	17.087027
31.615591	995.297543	17.092045
32.141965	985.564584	17.097063
31.765409	989.729437	17.102080
32.051063	990.249675	17.107098
31.918220	986.300528	17.112115
31.874059	988.201052	17.117133
32.235932	1007.098484	17.122151
32.011084	1015.701948	17.127168
32.129250	1013.414472	17.132186
31.825793	1024.239353	17.137203
32.162267	1016.546410	17.142221
32.454165	1005.221757	17.147239
32.056901	1015.098795	17.152256
32.516724	1017.466322	17.157274
32.700129	1011.264836	17.162291
32.682468	1015.108371	17.167309
32.551623	1012.932495	17.172327
32.588472	1016.360386	17.177344
32.301226	1010.797537	17.182362
32.562951	1011.075369	17.187379
32.737829	1016.154235	17.192397
32.796896	1022.822863	17.197415
32.559094	1018.634529	17.202432
32.941672	1010.236922	17.207450
33.106299	1011.233721	17.212467
32.795501	1010.013860	17.217485
33.179405	1005.377823	17.222503
32.763277	1007.017887	17.227520
32.698618	995.824845	17.232538
32.827612	1010.365826	17.237555
32.949651	1008.030407	17.242573
33.347137	1004.238010	17.247591
32.843072	995.540663	17.252608
32.762259	1006.393767	17.257626
32.736940	1004.816749	17.262643
32.727887	1015.175770	17.267661
32.665631	998.749946	17.272679
32.866312	1014.863936	17.277696
33.398444	998.966688	17.282714
32.763890	1001.969587	17.287731
32.899199	1013.072860	17.292749
33.229392	1000.628195	17.297767
32.744606	1006.820285	17.302784
33.115419	1016.819984	17.307802
33.015536	1028.187337	17.312819
33.371069	1034.544428	17.317837
33.262624	1030.111759	17.322855
33.409755	1029.757439	17.327872
33.509979	1024.660906	17.332890
33.357835	1027.029640	17.337907
33.081122	1031.822653	17.342925
33.737504	1024.827522	17.347943
33.449972	1028.170537	17.352960
33.403468	1026.631550	17.357978
33.120051	1035.641837	17.362995
33.512043	1054.594562	17.368013
34.001456	1048.029532	17.373031
34.041929	1059.176095	17.378048
34.135022	1056.368670	17.383066
34.048017	1051.386672	17.388083
34.018499	1042.173131	17.393101
33.901938	1022.757730	17.398119
33.946927	1028.292458	17.403136
33.891879	1039.567586	17.408154
34.105664	1043.800907	17.413171
33.862111	1045.552793	17.418189
33.998470	1040.021398	17.423207
33.907514	1047.644518	17.428224
34.117841	1031.854467	17.433242
34.138123	1038.273553	17.438259
34.010568	1039.350846	17.443277
34.316141	1032.962951	17.448295
34.130179	1043.532745	17.453312
34.352393	1037.748054	17.458330
34.334214	1046.262346	17.463347
34.000953	1044.642052	17.468365
34.842020	1039.849171	17.473383
34.412310	1042.775800	17.478400
34.247470	1042.101123	17.483418
34.634976	1039.673613	17.488435
34.384664	1043.184371	17.493453
34.513545	1033.794536	17.498471
34.481377	1034.585480	17.503488
34.690758	1040.144950	17.508506
34.353012	1030.389562	17.513523
34.820275	1041.832169	17.518541
34.846103	1040.578499	17.523559
34.702214	1045.246562	17.528576
34.870726	1043.822212	17.533594
34.933625	1035.771329	17.538611
34.867752	1046.675767	17.543629
35.159174	1046.999439	17.548647
34.768780	1036.072006	17.553664
34.995835	1032.151669	17.558682
35.219449	1035.970031	17.563699
35.044334	1029.546994	17.568717
34.972853	1027.721582	17.573735
35.015114	1037.002741	17.578752
34.811436	1038.748380	17.583770
34.869347	1047.727286	17.588787
35.166423	1061.329931	17.593805
35.306055	1057.805145	17.598823
35.076305	1060.810902	17.603840
34.905279	1056.044043	17.608858
35.146902	1062.112873	17.613875
35.107464	1060.765284	17.618893
35.204692	1058.670435	17.623911
35.133671	1062.979941	17.628928
35.172509	1072.479409	17.633946
35.263397	1079.215657	17.638963
35.212086	1093.917502	17.643981
35.416526	1080.072345	17.648999
35.274747	1091.209612	17.654016
35.584009	1086.212857	17.659034
35.550741	1078.940741	17.664051
35.927078	1080.469274	17.669069
36.019747	1080.009875	17.674087
36.104562	1076.872377	17.679104
35.956077	1075.980538	17.684122
36.038743	1077.567705	17.689139
35.828073	1080.040292	17.694157
36.269721	1065.754029	17.699175
36.208608	1077.399367	17.704192
35.912790	1071.437047	17.709210
36.010360	1061.815413	17.714227
36.207090	1070.018330	17.719245
36.255488	1056.336497	17.724263
36.373819	1063.346155	17.729280
36.343547	1066.970768	17.734298
36.348746	1063.362900	17.739315
36.511343	1069.280009	17.744333
36.452577	1064.899509	17.749351
36.639181	1057.223717	17.754368
36.474411	1076.074346	17.759386
36.574048	1061.036927	17.764403
36.295099	1067.300932	17.769421
36.544691	1057.649170	17.774439
36.337450	1056.255287	17.779456
36.039147	1065.952744	17.784474
36.478392	1054.762767	17.789491
36.739153	1066.600669	17.794509
36.804522	1061.948251	17.799527
36.214723	1070.558427	17.804544
36.023564	1060.303520	17.809562
36.375179	1053.769546	17.814579
36.539786	1067.639107	17.819597
36.772395	1073.996537	17.824615
37.157652	1083.558502	17.829632
36.950986	1083.792954	17.834650
37.269417	1086.119526	17.839667
37.145865	1089.660926	17.844685
37.278529	1071.213145	17.849703
36.942659	1065.607404	17.854720
36.977102	1072.567092	17.859738
37.423969	1074.359134	17.864755
37.245644	1069.647064	17.869773
37.135793	1063.106491	17.874791
37.030863	1059.121395	17.879808
37.247704	1066.014633	17.884826
37.264329	1070.982608	17.889843
37.178025	1080.201880	17.894861
37.373554	1079.906249	17.899879
37.533960	1078.022410	17.904896
37.434531	1077.574173	17.909914
37.475660	1083.560811	17.914931
37.424871	1082.893510	17.919949
37.191769	1076.564750	17.924967
37.589841	1079.314353	17.929984
37.142482	1085.671023	17.935002
37.186205	1079.415657	17.940019
37.383289	1077.933177	17.945037
37.339605	1083.153606	17.950055
37.836510	1091.126462	17.955072
37.676780	1105.665419	17.960090
38.117250	1099.518302	17.965107
37.892650	1110.816883	17.970125
37.861842	1108.458060	17.975143
38.193675	1110.280753	17.980160
38.104168	1095.118302	17.985178
37.942261	1098.403777	17.990195
37.872585	1099.595084	17.995213
38.056020	1099.970392	18.000231
37.974672	1107.614124	18.005248
38.052051	1103.101828	18.010266
38.218404	1096.167666	18.015283
38.240756	1096.950071	18.020301
38.095093	1097.250706	18.025319
38.351474	1095.405478	18.030336
38.438298	1113.052211	18.035354
38.348270	1094.655076	18.040371
38.240508	1097.190439	18.045389
38.102157	1101.895519	18.050407
38.221242	1102.053686	18.055424
38.034261	1111.231943	18.060442
38.568741	1119.101092	18.065459
38.813800	1124.292073	18.070477
38.702467	1129.478932	18.075495
39.106285	1128.437439	18.080512
38.643851	1123.034549	18.085530
38.970130	1124.422603	18.090547
38.988882	1125.565343	18.095565
38.834618	1110.356220	18.100583
38.884594	1103.566524	18.105600
38.430760	1107.689861	18.110618
38.907317	1117.666738	18.115635
38.815236	1115.349073	18.120653
38.951130	1120.374116	18.125671
39.097016	1112.471146	18.130688
38.945213	1117.995709	18.135706
39.048615	1122.154823	18.140723
39.411041	1117.739877	18.145741
39.101838	1124.213773	18.150759
38.903345	1119.429109	18.155776
38.784864	1122.449002	18.160794
39.303286	1132.719136	18.165811
39.623346	1142.057813	18.170829
39.354904	1138.417062	18.175847
39.678089	1137.871051	18.180864
39.331293	1145.556388	18.185882
39.733986	1141.636912	18.190899
39.782742	1142.847538	18.195917
39.731513	1135.363614	18.200935
39.584927	1125.322597	18.205952
39.719046	1128.981428	18.210970
39.979009	1125.321009	18.215987
39.972881	1123.627362	18.221005
40.126436	1112.573630	18.226023
39.803685	1109.796635	18.231040
39.811611	1109.713437	18.236058
39.644740	1109.670249	18.241075
39.762794	1119.375086	18.246093
39.725423	1127.147639	18.251111
40.146781	1134.005704	18.256128
39.606985	1133.664331	18.261146
39.844988	1127.315392	18.266163
40.150872	1139.351404	18.271181
39.790825	1132.275635	18.276199
39.849946	1124.515645	18.281216
39.912714	1131.909585	18.286234
40.311725	1133.646014	18.291251
40.639609	1149.146891	18.296269
40.407408	1144.642063	18.301287
40.472192	1133.466524	18.306304
40.048846	1134.972028	18.311322
40.526391	1140.628372	18.316339
40.672232	1146.500794	18.321357
40.466976	1157.802686	18.326375
40.558815	1152.808419	18.331392
40.373960	1162.219903	18.336410
40.797689	1150.868192	18.341427
41.069186	1145.949922	18.346445
40.817362	1150.117360	18.351463
41.051941	1146.984789	18.356480
40.954294	1145.961901	18.361498
41.052457	1146.277984	18.366515
41.011696	1149.711749	18.371533
40.991217	1164.964256	18.376551
40.980608	1143.799545	18.381568
41.042088	1150.347920	18.386586
41.075063	1147.202752	18.391603
41.207674	1145.755616	18.396621
41.006506	1152.730159	18.401639
41.249588	1153.544257	18.406656
41.128225	1154.200856	18.411674
41.318346	1155.963703	18.416691
41.491295	1144.177906	18.421709
41.347702	1156.369561	18.426727
41.409830	1148.154643	18.431744
41.501894	1143.778894	18.436762
41.230432	1137.620228	18.441779
41.431214	1138.586123	18.446797
41.350172	1144.759185	18.451815
41.375130	1141.400676	18.456832
41.437092	1159.600474	18.461850
41.772886	1168.264497	18.466867
41.506221	1169.186864	18.471885
41.563698	1179.254683	18.476903
42.039996	1170.308973	18.481920
41.644640	1181.249335	18.486938
41.648646	1168.483265	18.491955
41.620263	1171.321789	18.496973
41.482631	1172.659452	18.501991
42.058392	1178.373005	18.507008
42.324702	1180.196504	18.512026
42.564602	1177.116743	18.517043
42.173330	1174.113782	18.522061
42.147717	1179.321940	18.527079
42.287455	1157.849627	18.532096
42.336796	1162.165546	18.537114
42.394267	1169.680255	18.542131
42.656009	1163.965071	18.547149
42.266736	1162.950003	18.552167
42.385922	1170.180481	18.557184
42.481171	1180.387553	18.562202
42.187360	1184.930815	18.567219
42.585916	1185.449150	18.572237
42.400539	1192.266596	18.577255
42.723113	1188.678407	18.582272
42.565367	1186.200603	18.587290
42.275588	1185.671731	18.592307
42.574422	1184.662463	18.597325
42.711608	1189.889299	18.602343
43.119650	1188.755621	18.607360
42.881158	1188.060918	18.612378
42.733531	1188.649047	18.617395
42.887038	1188.385246	18.622413
42.406028	1202.797889	18.627431
42.864008	1203.127029	18.632448
43.174556	1211.403699	18.637466
43.401615	1213.697266	18.642483
43.669041	1206.450572	18.647501
43.625648	1199.328321	18.652519
43.386596	1180.083422	18.657536
43.359496	1186.554168	18.662554
43.300571	1185.481028	18.667571
43.263729	1180.008285	18.672589
43.000047	1185.222186	18.677607
43.533495	1194.754681	18.682624
43.292653	1205.816020	18.687642
43.475076	1195.824404	18.692659
43.228100	1204.614467	18.697677
43.293349	1204.910461	18.702695
43.246875	1204.804227	18.707712
43.617587	1209.704140	18.712730
43.673399	1220.321368	18.717747
43.975332	1208.843532	18.722765
43.922150	1223.649921	18.727783
43.978983	1216.619260	18.732800
44.182230	1221.425490	18.737818
44.204677	1213.254630	18.742835
44.399108	1212.387954	18.747853
44.022220	1216.956864	18.752871
44.185051	1209.805453	18.757888
44.225121	1209.789804	18.762906
44.171198	1216.457273	18.767923
44.388819	1218.171635	18.772941
44.104722	1218.673847	18.777959
44.323440	1214.347667	18.782976
44.304480	1214.372825	18.787994
44.459351	1209.245587	18.793011
44.818778	1214.055749	18.798029
44.398011	1216.157317	18.803047
45.113789	1217.228726	18.808064
44.780858	1216.621404	18.813082
44.727778	1222.884789	18.818099
44.971279	1208.973450	18.823117
44.734629	1213.785482	18.828135
44.861645	1214.125449	18.833152
44.713197	1211.220140	18.838170
44.522415	1217.726010	18.843187
44.764819	1211.139659	18.848205
44.742091	1203.307250	18.853223
45.001948	1212.699579	18.858240
44.940839	1210.648455	18.863258
44.934554	1205.634832	18.868275
44.889299	1203.518107	18.873293
45.086102	1213.090734	18.878311
45.055834	1220.123736	18.883328
45.125876	1235.422083	18.888346
45.153982	1239.451006	18.893363
45.145816	1231.786721	18.898381
45.441303	1235.129949	18.903399
45.374094	1236.298788	18.908416
45.487646	1235.772995	18.913434
45.131414	1230.880467	18.918451
45.617699	1231.912092	18.923469
45.582379	1237.077605	18.928487
45.674016	1230.994565	18.933504
45.761721	1235.553806	18.938522
45.533651	1242.444234	18.943539
45.495998	1232.392402	18.948557
45.941087	1236.498008	18.953575
46.206488	1236.087283	18.958592
46.260272	1223.610028	18.963610
46.198541	1226.223406	18.968627
46.354571	1216.213822	18.973645
46.028490	1219.007475	18.978663
46.373555	1222.828940	18.983680
46.155505	1222.291984	18.988698
46.013730	1231.696755	18.993715
46.106093	1227.582878	18.998733
45.907942	1225.947710	19.003751
45.993900	1231.864258	19.008768
46.316718	1245.971110	19.013786
46.199251	1261.491367	19.018803
46.343715	1251.524603	19.023821
46.545613	1263.952543	19.028839
46.225586	1264.684454	19.033856
46.587663	1247.096822	19.038874
46.290579	1260.524460	19.043891
46.559936	1254.770183	19.048909
46.243364	1261.848059	19.053927
46.437003	1266.633716	19.058944
46.968629	1275.125094	19.063962
46.948527	1284.277293	19.068979
46.782519	1279.929322	19.073997
46.429723	1279.492372	19.079015
46.912015	1281.032726	19.084032
47.045782	1270.010401	19.089050
46.825393	1275.861348	19.094067
47.281295	1278.444126	19.099085
47.353288	1291.125975	19.104103
47.210102	1293.300831	19.109120
47.464825	1284.531795	19.114138
47.437363	1297.926685	19.119155
47.707281	1295.757414	19.124173
47.737862	1273.027079	19.129191
47.390748	1273.624375	19.134208
47.416470	1269.593515	19.139226
47.895488	1296.716109	19.144243
47.961228	1279.783964	19.149261
47.739497	1276.984803	19.154279
47.218589	1269.186235	19.159296
47.808387	1279.571508	19.164314
47.532976	1299.039327	19.169331
47.472115	1283.875384	19.174349
47.625976	1286.331912	19.179367
47.444444	1294.215488	19.184384
48.077668	1283.815512	19.189402
47.845626	1296.936332	19.194419
48.516447	1301.997540	19.199437
48.087296	1301.395823	19.204455
48.268278	1294.935834	19.209472
48.695844	1294.547039	19.214490
48.318529	1295.461501	19.219507
48.339508	1294.076025	19.224525
47.953598	1293.155099	19.229543
48.109624	1297.053537	19.234560
48.450166	1302.873414	19.239578
48.731482	1309.340066	19.244595
48.556514	1312.646561	19.249613
48.840243	1310.651855	19.254631
48.686304	1306.109476	19.259648
48.708149	1293.583526	19.264666
49.013687	1306.768454	19.269683
49.368139	1298.668618	19.274701
49.005159	1299.987946	19.279719
49.002737	1300.505990	19.284736
48.884266	1300.284799	19.289754
48.983730	1304.207880	19.294771
49.000097	1300.285780	19.299789
49.039738	1297.496159	19.304807
48.854711	1306.380710	19.309824
49.207069	1298.833485	19.314842
49.008590	1300.199626	19.319859
48.919855	1295.883726	19.324877
49.381507	1300.658960	19.329895
49.276787	1303.938668	19.334912
49.156096	1296.613887	19.339930
49.170587	1304.996948	19.344947
49.422152	1316.445125	19.349965
49.754001	1326.186008	19.354983
49.777734	1323.140091	19.360000
49.792021	1326.372755	19.365018
49.476471	1329.044850	19.370035
49.488269	1328.702260	19.375053
49.428191	1317.530389	19.380071
49.320802	1334.914272	19.385088
49.784179	1321.059917	19.390106
49.701437	1326.138209	19.395123
49.792016	1333.505784	19.400141
50.145984	1340.702703	19.405159
50.070507	1340.657818	19.410176
50.242381	1347.501405	19.415194
49.887153	1351.274821	19.420211
50.092125	1347.512515	19.425229
50.356937	1347.436407	19.430247
50.230940	1345.591101	19.435264
50.168770	1340.526233	19.440282
50.172690	1333.061989	19.445299
50.085554	1339.658965	19.450317
50.355702	1344.306419	19.455335
50.927475	1361.681753	19.460352
51.437084	1358.215711	19.465370
50.608702	1356.205885	19.470387
51.001875	1351.918614	19.475405
51.017480	1352.512733	19.480423
50.881623	1341.523140	19.485440
50.978909	1343.388916	19.490458
51.125576	1364.943010	19.495475
51.413531	1354.717013	19.500493
51.264922	1332.667951	19.505511
50.890099	1335.645989	19.510528
51.079295	1331.580036	19.515546
51.421207	1352.630138	19.520563
51.538776	1357.762264	19.525581
51.585211	1345.017823	19.530599
51.323044	1331.573791	19.535616
51.459274	1335.942413	19.540634
51.405302	1345.270369	19.545651
51.460783	1352.065919	19.550669
51.500259	1353.025540	19.555687
51.681451	1347.651133	19.560704
51.612899	1351.073511	19.565722
51.633794	1353.490919	19.570739
51.910979	1349.840379	19.575757
51.767329	1347.379279	19.580775
51.847776	1342.512980	19.585792
51.858405	1343.868453	19.590810
51.570532	1358.314080	19.595827
51.339972	1360.764574	19.600845
51.940894	1357.479892	19.605863
52.032175	1374.564434	19.610880
52.000643	1374.503196	19.615898
51.874178	1369.956496	19.620915
52.130627	1381.479692	19.625933
52.398876	1368.763600	19.630951
52.142367	1366.449572	19.635968
52.179482	1375.125777	19.640986
52.198725	1380.207041	19.646003
52.121493	1381.532100	19.651021
52.531576	1375.500107	19.656039
52.151038	1387.337709	19.661056
52.526390	1386.196517	19.666074
52.694853	1396.445893	19.671091
52.546943	1382.832437	19.676109
53.093104	1389.229220	19.681127
52.891856	1397.835481	19.686144
52.972341	1393.322626	19.691162
52.896037	1388.515588	19.696179
52.704049	1392.285529	19.701197
53.051308	1380.838352	19.706215
52.916856	1397.396530	19.711232
53.248455	1403.587084	19.716250
53.181022	1415.246256	19.721267
53.562331	1416.521567	19.726285
53.801575	1408.793195	19.731303
53.733954	1410.138841	19.736320
53.234450	1396.274336	19.741338
53.647473	1395.913066	19.746355
54.072763	1408.224053	19.751373
53.697167	1380.450939	19.756391
53.594198	1380.224162	19.761408
54.072882	1393.079059	19.766426
53.823103	1396.757065	19.771443
53.849104	1392.170693	19.776461
53.967629	1397.959112	19.781479
53.730056	1402.455747	19.786496
53.883254	1406.247350	19.791514
53.975360	1404.364710	19.796531
53.871785	1413.902452	19.801549
53.877687	1405.254396	19.806567
54.001259	1406.506969	19.811584
54.093211	1398.732248	19.816602
53.799789	1399.040258	19.821619
53.953323	1424.825437	19.826637
54.552473	1424.245650	19.831655
54.327710	1424.501876	19.836672
54.429837	1427.379955	19.841690
54.688542	1422.425743	19.846707
54.512635	1425.675599	19.851725
54.646307	1420.627364	19.856743
54.761459	1420.975507	19.861760
54.664598	1416.013886	19.866778
54.896185	1420.395993	19.871795
54.896459	1413.168981	19.876813
55.167876	1401.178231	19.881831
54.937510	1413.923319	19.886848
55.271594	1421.136010	19.891866
55.564062	1424.776405	19.896883
55.199470	1421.813403	19.901901
55.495150	1407.054259	19.906919
55.403411	1410.237275	19.911936
55.234776	1410.487863	19.916954
55.084263	1411.483565	19.921971
55.019601	1419.951668	19.926989
55.442908	1435.377882	19.932007
55.455313	1441.520627	19.937024
55.610269	1439.019042	19.942042
55.781873	1435.722711	19.947059
55.676018	1433.142065	19.952077
56.063694	1442.647039	19.957095
55.818309	1435.606835	19.962112
55.422605	1433.718565	19.967130
55.746748	1432.165656	19.972147
55.591069	1436.864071	19.977165
55.922289	1436.124281	19.982183
56.073653	1451.498439	19.987200
56.063905	1466.667469	19.992218
56.548940	1465.550115	19.997235
56.412975	1466.953812	20.002253
56.463418	1460.309080	20.007271
56.720582	1463.573146	20.012288
56.077216	1453.259469	20.017306
56.781855	1447.831424	20.022323
56.611813	1455.596502	20.027341
56.669892	1454.205202	20.032359
56.373865	1445.604431	20.037376
56.492429	1451.531722	20.042394
56.626006	1457.579745	20.047411
56.516866	1458.146073	20.052429
56.774575	1456.900227	20.057447
56.763630	1449.233128	20.062464
56.369173	1460.880447	20.067482
56.904733	1466.477313	20.072499
57.058985	1474.153719	20.077517
57.488848	1476.264062	20.082535
57.554654	1480.372343	20.087552
57.470892	1472.517818	20.092570
57.340944	1478.136902	20.097587
57.622206	1474.258471	20.102605
57.683621	1467.479468	20.107623
57.775204	1471.350170	20.112640
57.772556	1475.525982	20.117658
57.881472	1464.829335	20.122675
57.838522	1476.484711	20.127693
57.971181	1472.184577	20.132711
57.717166	1468.074419	20.137728
57.737197	1471.151568	20.142746
57.908396	1461.827464	20.147763
57.554131	1472.840464	20.152781
57.751627	1472.926387	20.157799
57.833666	1471.938446	20.162816
57.707603	1473.208044	20.167834
57.879796	1466.386437	20.172851
57.576165	1480.686303	20.177869
57.790191	1482.779967	20.182887
57.892780	1490.937865	20.187904
57.678204	1501.174728	20.192922
58.047805	1498.301820	20.197939
58.006644	1520.702917	20.202957
58.244401	1512.539214	20.207975
58.456136	1509.167152	20.212992
58.377658	1520.247429	20.218010
58.830035	1527.369043	20.223027
59.043914	1531.255313	20.228045
59.564526	1531.697729	20.233063
59.188810	1522.743316	20.238080
58.998781	1513.390571	20.243098
59.414216	1517.210543	20.248115
59.128780	1516.712538	20.253133
59.190839	1508.216587	20.258151
59.448825	1513.266795	20.263168
59.394953	1522.815744	20.268186
59.455211	1511.937337	20.273203
59.416927	1513.190028	20.278221
59.247140	1515.309115	20.283239
59.456144	1525.953018	20.288256
59.408877	1536.192091	20.293274
59.422940	1532.604831	20.298291
59.579249	1536.812559	20.303309
59.824810	1535.066816	20.308327
59.785805	1530.705197	20.313344
59.519257	1533.483258	20.318362
59.947569	1535.499173	20.323379
59.679883	1530.930374	20.328397
59.670838	1535.498539	20.333415
60.106865	1547.956271	20.338432
60.049543	1554.785351	20.343450
60.295973	1547.882652	20.348467
60.465855	1554.666667	20.353485
60.314154	1559.740049	20.358503
60.473775	1557.966742	20.363520
60.241605	1550.785560	20.368538
60.574530	1538.526294	20.373555
60.588711	1556.513067	20.378573
60.599088	1553.453424	20.383591
60.513753	1556.865846	20.388608
60.666397	1546.383217	20.393626
60.832086	1547.013791	20.398643
60.548957	1541.469065	20.403661
60.520851	1559.569768	20.408679
60.768299	1563.248804	20.413696
61.258883	1572.223305	20.418714
61.404505	1571.724038	20.423731
61.078226	1578.068221	20.428749
61.013494	1575.127645	20.433767
61.198724	1560.410927	20.438784
60.919691	1568.054268	20.443802
61.382353	1567.874575	20.448819
61.604562	1567.293877	20.453837
61.374401	1572.985498	20.458855
61.983201	1568.973676	20.463872
61.569485	1579.563690	20.468890
61.496753	1576.157285	20.473907
61.459139	1584.835833	20.478925
61.399925	1591.384344	20.483943
61.591048	1586.907757	20.488960
61.642310	1590.172546	20.493978
61.915018	1588.877003	20.498995
61.797323	1600.986003	20.504013
62.080281	1614.685963	20.509031
62.384813	1613.675780	20.514048
62.071496	1616.543236	20.519066
62.535613	1622.867748	20.524083
62.856339	1615.555732	20.529101
62.682587	1614.907675	20.534119
62.749708	1608.266588	20.539136
62.374410	1611.721294	20.544154
62.579400	1615.861452	20.549171
62.842201	1609.792493	20.554189
62.593143	1611.791460	20.559207
63.028209	1606.942117	20.564224
62.657506	1610.828470	20.569242
62.885373	1606.418708	20.574259
62.906315	1610.240544	20.579277
63.026409	1611.190704	20.584295
63.088319	1602.357044	20.589312
63.065338	1622.394765	20.594330
63.419969	1623.822601	20.599347
63.425041	1633.299255	20.604365
63.244404	1642.786073	20.609383
63.478000	1632.906123	20.614400
63.474864	1641.692911	20.619418
63.240969	1633.893397	20.624435
63.468470	1626.794808	20.629453
63.268008	1627.179780	20.634471
63.693835	1624.559988	20.639488
63.474815	1629.347276	20.644506
63.718073	1643.978175	20.649523
64.115763	1637.121175	20.654541
64.247531	1653.855641	20.659559
64.399000	1640.381285	20.664576
63.998806	1654.920491	20.669594
64.491348	1647.168112	20.674611
64.269699	1641.601099	20.679629
64.523018	1649.583968	20.684647
64.569014	1638.578324	20.689664
64.700651	1644.241686	20.694682
64.623229	1636.316665	20.699699
65.256161	1639.228386	20.704717
64.713684	1630.637734	20.709735
64.851284	1620.955876	20.714752
64.306276	1622.773983	20.719770
64.217536	1625.082366	20.724787
64.630934	1638.345321	20.729805
64.479692	1637.362361	20.734823
64.733109	1638.092808	20.739840
64.507641	1639.949220	20.744858
64.841199	1653.593943	20.749875
65.305407	1649.914042	20.754893
65.052605	1664.527998	20.759911
65.502043	1663.444614	20.764928
65.576419	1657.903803	20.769946
65.536325	1658.926403	20.774963
65.463943	1656.526681	20.779981
65.205484	1656.368446	20.784999
65.621741	1651.086514	20.790016
65.803217	1662.489088	20.795034
65.844438	1671.726557	20.800051
66.133596	1669.617346	20.805069
65.842572	1679.418140	20.810087
66.300934	1678.453283	20.815104
66.285489	1672.301659	20.820122
66.158567	1681.051053	20.825139
66.099655	1672.880106	20.830157
66.229857	1686.761852	20.835175
66.473606	1683.097549	20.840192
66.489053	1684.868881	20.845210
66.045225	1678.471930	20.850227
66.208790	1669.246750	20.855245
66.234793	1673.853643	20.860263
66.423182	1681.480607	20.865280
66.435905	1693.831183	20.870298
66.617229	1696.343429	20.875315
67.059353	1694.715205	20.880333
66.609077	1699.074816	20.885351
66.973871	1691.951535	20.890368
66.914126	1690.578676	20.895386
66.770341	1688.363716	20.900403
67.393015	1702.824760	20.905421
67.423445	1719.745587	20.910439
67.663904	1708.980846	20.915456
67.690083	1693.348457	20.920474
67.120857	1695.265045	20.925491
67.766498	1697.578306	20.930509
67.319250	1713.838626	20.935527
67.920642	1715.486599	20.940544
67.937677	1714.294223	20.945562
67.954092	1714.342244	20.950579
68.153147	1703.208432	20.955597
68.132254	1709.018796	20.960615
68.103334	1710.784457	20.965632
68.084922	1705.860961	20.970650
68.202684	1714.262750	20.975667
68.228050	1699.615148	20.980685
68.204820	1713.094897	20.985703
68.252948	1710.016689	20.990720
68.489414	1705.955869	20.995738
68.415285	1705.339541	21.000755
68.709065	1704.255294	21.005773
68.527404	1702.522818	21.010791
68.123124	1709.608299	21.015808
68.406985	1710.185649	21.020826
68.391941	1708.149342	21.025843
68.558663	1709.934848	21.030861
68.790890	1726.113971	21.035879
68.810883	1721.143425	21.040896
68.968244	1727.967340	21.045914
68.818143	1724.481505	21.050931
68.907050	1730.722822	21.055949
69.403683	1729.139708	21.060967
69.253661	1720.149835	21.065984
69.335508	1725.969355	21.071002
69.138602	1738.475889	21.076019
69.326031	1743.537218	21.081037
69.638798	1749.386842	21.086055
69.760954	1741.304266	21.091072
70.037154	1736.041098	21.096090
69.800393	1745.716655	21.101107
69.986929	1740.379165	21.106125
69.734359	1740.617659	21.111143
70.379064	1737.764732	21.116160
70.459659	1748.656118	21.121178
70.034249	1746.460025	21.126195
70.376539	1739.453867	21.131213
70.518724	1737.074170	21.136231
70.738983	1738.702959	21.141248
70.687971	1742.315178	21.146266
70.402501	1748.694056	21.151283
70.302780	1740.882941	21.156301
70.304603	1736.757885	21.161319
70.731791	1743.848818	21.166336
70.637144	1756.468738	21.171354
70.452819	1763.267300	21.176371
71.079131	1752.943881	21.181389
70.902602	1768.312876	21.186407
70.796119	1762.693066	21.191424
71.328143	1766.674717	21.196442
71.174572	1761.144340	21.201459
71.257664	1762.766219	21.206477
70.967489	1760.163907	21.211495
71.318592	1769.961981	21.216512
71.410106	1777.405337	21.221530
71.758867	1785.685757	21.226547
71.797305	1776.543245	21.231565
71.664036	1781.301359	21.236583
71.833527	1779.264536	21.241600
71.843598	1778.316259	21.246618
71.757633	1784.689140	21.251635
71.623670	1780.998782	21.256653
71.413021	1781.426380	21.261671
71.568011	1800.694761	21.266688
71.958054	1793.554860	21.271706
72.227371	1796.719248	21.276723
72.342241	1783.752322	21.281741
72.245564	1793.159789	21.286759
72.444542	1789.029080	21.291776
72.553339	1786.285357	21.296794
72.460285	1803.414969	21.301811
72.724225	1809.849811	21.306829
72.580988	1814.013012	21.311847
72.689298	1820.582700	21.316864
72.842538	1816.623262	21.321882
72.999347	1818.142072	21.326899
73.179252	1823.078363	21.331917
72.976338	1816.586809	21.336935
73.362371	1813.837517	21.341952
73.091028	1811.841354	21.346970
72.990570	1819.188564	21.351987
73.122900	1813.427174	21.357005
73.557842	1828.116561	21.362023
73.562141	1829.091187	21.367040
73.865195	1831.499168	21.372058
73.642314	1836.713176	21.377075
73.548449	1834.294704	21.382093
73.530133	1834.095686	21.387111
73.520137	1837.786711	21.392128
73.867135	1831.852818	21.397146
73.784671	1837.208938	21.402163
74.316823	1841.165339	21.407181
74.381177	1847.764016	21.412199
74.260170	1848.736183	21.417216
74.372133	1851.849490	21.422234
74.429406	1865.979502	21.427251
74.209454	1852.932431	21.432269
74.447186	1848.278052	21.437287
74.487281	1850.364295	21.442304
75.147310	1840.417421	21.447322
74.907375	1847.019587	21.452339
74.811940	1849.663583	21.457357
74.801772	1849.848321	21.462375
74.774487	1849.625460	21.467392
75.037271	1860.087558	21.472410
75.167245	1872.299959	21.477427
75.187676	1875.437079	21.482445
75.278560	1866.822825	21.487463
74.962248	1875.639859	21.492480
75.485973	1870.154822	21.497498
75.717868	1870.336351	21.502515
75.134885	1872.561244	21.507533
75.657151	1873.416849	21.512551
75.801028	1888.615820	21.517568
76.190661	1889.369122	21.522586
75.864020	1894.037633	21.527603
76.172358	1890.375792	21.532621
76.471240	1897.288060	21.537639
76.184922	1883.320342	21.542656
76.121901	1883.361872	21.547674
76.041895	1882.519225	21.552691
76.341847	1875.529116	21.557709
76.396443	1880.475587	21.562727
76.440117	1889.728564	21.567744
76.536893	1881.735113	21.572762
76.419910	1893.901009	21.577779
76.779083	1902.975166	21.582797
77.013725	1903.866368	21.587815
76.934209	1906.533127	21.592832
77.259169	1909.190168	21.597850
77.057706	1910.051859	21.602867
77.335253	1901.045403	21.607885
77.645170	1895.514956	21.612903
77.703865	1897.822367	21.617920
77.803678	1903.856896	21.622938
77.597020	1896.075091	21.627955
77.381655	1892.236507	21.632973
77.934593	1895.911935	21.637991
77.583464	1901.862469	21.643008
77.836566	1902.829678	21.648026
78.039323	1896.498614	21.653043
78.020439	1887.598571	21.658061
77.705850	1894.244011	21.663079
77.934687	1886.646461	21.668096
77.699185	1888.867411	21.673114
77.923544	1893.219207	21.678131
78.112947	1904.188321	21.683149
77.856793	1906.014851	21.688167
78.260931	1921.390839	21.693184
78.697444	1914.357227	21.698202
78.017493	1919.115815	21.703219
78.382002	1913.245428	21.708237
78.359965	1916.853143	21.713255
78.071956	1934.275374	21.718272
78.383794	1936.666214	21.723290
78.216223	1940.520811	21.728307
78.721059	1955.723251	21.733325
79.282179	1956.086747	21.738343
79.309951	1963.145664	21.743360
79.177028	1959.076384	21.748378
79.095841	1961.446747	21.753395
78.933452	1965.414155	21.758413
79.492909	1962.902776	21.763431
79.531255	1984.954304	21.768448
79.885967	1987.991730	21.773466
79.894917	1981.160789	21.778483
80.083157	1979.490261	21.783501
80.128151	1985.893193	21.788519
80.288585	1987.016946	21.793536
80.397932	1988.312817	21.798554
80.311800	1976.409263	21.803571
80.315848	1980.022371	21.808589
80.643241	1979.109580	21.813607
80.791202	1988.715525	21.818624
80.370417	1975.725076	21.823642
80.472203	1977.817449	21.828659
80.520424	1979.261761	21.833677
80.564486	1975.552940	21.838695
80.441411	1978.302278	21.843712
80.872457	1971.948045	21.848730
80.636003	1979.916272	21.853747
80.987758	1993.362731	21.858765
81.249305	1995.196529	21.863783
80.612297	2001.084580	21.868800
80.874362	1998.032769	21.873818
81.147661	2005.659193	21.878835
81.471784	2017.276346	21.883853
81.630311	2018.154231	21.888871
81.573280	2027.596638	21.893888
81.664875	2024.195963	21.898906
81.620626	2022.186288	21.903923
81.705777	2021.623895	21.908941
82.414445	2019.871827	21.913959
81.962489	2018.109079	21.918976
82.159665	2018.245553	21.923994
82.466447	2015.363470	21.929011
82.184212	2026.144601	21.934029
82.264253	2013.776298	21.939047
82.226022	2018.121925	21.944064
82.388069	2020.299543	21.949082
82.547699	2027.312579	21.954099
82.646376	2032.630909	21.959117
82.868147	2032.974985	21.964135
82.379419	2038.249637	21.969152
82.752893	2037.774624	21.974170
82.542953	2042.961416	21.979187
83.204800	2048.466094	21.984205
82.988462	2056.825707	21.989223
83.159010	2061.249096	21.994240
83.300853	2056.148906	21.999258
83.595380	2067.089025	22.004275
83.582643	2062.360216	22.009293
83.632682	2059.316365	22.014311
83.499368	2057.945535	22.019328
83.830927	2054.270556	22.024346
83.741317	2048.464962	22.029363
83.702240	2064.125122	22.034381
84.233033	2055.883702	22.039399
84.188669	2047.047537	22.044416
84.055522	2057.745363	22.049434
84.148401	2048.786702	22.054451
84.110315	2060.539533	22.059469
84.224651	2061.484308	22.064487
84.165665	2071.842296	22.069504
84.359261	2078.714321	22.074522
84.317093	2074.466682	22.079539
84.292921	2076.140110	22.084557
84.568943	2078.116828	22.089575
84.647987	2095.759440	22.094592
84.860621	2090.644993	22.099610
85.079124	2086.410164	22.104627
84.539239	2089.846562	22.109645
85.053147	2093.995241	22.114663
85.394948	2108.121895	22.119680
85.451938	2108.283489	22.124698
85.737823	2112.991802	22.129715
85.531747	2119.424648	22.134733
85.692713	2116.928340	22.139751
85.789617	2110.399174	22.144768
85.645887	2106.334710	22.149786
86.172383	2109.051732	22.154803
85.864747	2115.664603	22.159821
85.925741	2114.020311	22.164839
85.971535	2120.962849	22.169856
86.330273	2118.539706	22.174874
86.410500	2130.823199	22.179891
86.211797	2136.838298	22.184909
86.787278	2130.975817	22.189927
86.850752	2131.429908	22.194944
86.831229	2134.282977	22.199962
86.839071	2133.518080	22.204979
86.946997	2123.335633	22.209997
86.768621	2117.992082	22.215015
86.894310	2121.254776	22.220032
86.844735	2126.473276	22.225050
87.288387	2131.718652	22.230067
86.975921	2143.284133	22.235085
87.253692	2145.405763	22.240103
87.396583	2156.821010	22.245120
87.120542	2158.407665	22.250138
87.259454	2151.262784	22.255155
87.671736	2161.083049	22.260173
87.572508	2172.798192	22.265191
87.867956	2180.840977	22.270208
87.886463	2177.136117	22.275226
88.214974	2181.282303	22.280243
88.169566	2176.028365	22.285261
88.226567	2174.460438	22.290279
88.237447	2166.549752	22.295296
88.207285	2170.578546	22.300314
88.704785	2179.123048	22.305331
88.795054	2190.357197	22.310349
89.167023	2195.055200	22.315367
89.128871	2192.612171	22.320384
88.935438	2190.004106	22.325402
89.161581	2182.261675	22.330419
89.175861	2187.224015	22.335437
89.115224	2184.200639	22.340455
89.187514	2180.282209	22.345472
89.360726	2183.237643	22.350490
89.354023	2184.188764	22.355507
89.276470	2184.201010	22.360525
89.421084	2192.387362	22.365543
89.447611	2191.461733	22.370560
89.482288	2189.846806	22.375578
89.374633	2190.185687	22.380595
89.640919	2209.083591	22.385613
89.840677	2213.051124	22.390631
90.061270	2208.926402	22.395648
89.844741	2216.582317	22.400666
90.334505	2215.372654	22.405683
89.889776	2216.868968	22.410701
90.456313	2221.432345	22.415719
90.310647	2236.629634	22.420736
90.372229	2237.661585	22.425754
91.064821	2236.476953	22.430771
90.984963	2230.404662	22.435789
90.959857	2238.437729	22.440807
90.748153	2241.788022	22.445824
90.804854	2239.109200	22.450842
90.994865	2234.774650	22.455859
91.221797	2255.610283	22.460877
91.361159	2256.339691	22.465895
91.211127	2258.884995	22.470912
90.833619	2259.376618	22.475930
91.515782	2256.170576	22.480947
91.536816	2267.087389	22.485965
91.773406	2272.671387	22.490983
92.152747	2274.401546	22.496000
91.763267	2276.807627	22.501018
92.353479	2279.369514	22.506035
92.183112	2286.226052	22.511053
92.353106	2276.377806	22.516071
92.091226	2276.999649	22.521088
92.464164	2284.478027	22.526106
92.690175	2271.875221	22.531123
92.547027	2273.693551	22.536141
92.497638	2285.382022	22.541159
93.089317	2294.208496	22.546176
92.877287	2295.854567	22.551194
92.936331	2295.763355	22.556211
92.806356	2305.665500	22.561229
92.456894	2300.317138	22.566247
93.113919	2302.060605	22.571264
93.323076	2312.900631	22.576282
93.673520	2306.562065	22.581299
93.399362	2311.421294	22.586317
93.626535	2317.666403	22.591335
93.892680	2306.919373	22.596352
93.684297	2310.679449	22.601370
94.517162	2302.706199	22.606387
94.229416	2306.510269	22.611405
93.904467	2303.881763	22.616423
94.304435	2302.004450	22.621440
93.999180	2306.609751	22.626458
94.464825	2317.302289	22.631475
94.860760	2329.694260	22.636493
94.754739	2325.049431	22.641511
94.840970	2326.399446	22.646528
94.808107	2322.784662	22.651546
95.189344	2321.803454	22.656563
94.924731	2321.040206	22.661581
95.287632	2314.387234	22.666599
94.916382	2317.532143	22.671616
95.202842	2320.690784	22.676634
95.038597	2315.726846	22.681651
95.162148	2326.056382	22.686669
95.200809	2330.162800	22.691687
95.503558	2336.244583	22.696704
95.347330	2346.895700	22.701722
95.567794	2340.261878	22.706739
96.006129	2342.279473	22.711757
95.817976	2339.579033	22.716775
95.924863	2338.969039	22.721792
95.885035	2352.278285	22.726810
96.212493	2359.413494	22.731827
96.429405	2359.884581	22.736845
96.338464	2365.709288	22.741863
96.785368	2365.563622	22.746880
96.631705	2367.235272	22.751898
96.620898	2366.555346	22.756915
96.919977	2368.648416	22.761933
96.621702	2365.059426	22.766951
96.700724	2370.778604	22.771968
96.815582	2376.255463	22.776986
97.103582	2378.905742	22.782003
97.016042	2373.652034	22.787021
97.071157	2383.771399	22.792039
97.408098	2404.880332	22.797056
97.775787	2405.984267	22.802074
97.796837	2404.251523	22.807091
97.956852	2402.392857	22.812109
97.636564	2408.395535	22.817127
98.066321	2399.993047	22.822144
98.160151	2403.257628	22.827162
98.068151	2403.713992	22.832179
98.096923	2402.791156	22.837197
98.022264	2425.025046	22.842215
98.522043	2419.010216	22.847232
98.371783	2426.062491	22.852250
98.313100	2424.042408	22.857267
99.024635	2434.857455	22.862285
98.617683	2437.108488	22.867303
99.007458	2446.225470	22.872320
98.798809	2454.997513	22.877338
99.003251	2456.887649	22.882355
99.232503	2451.290769	22.887373
99.325190	2450.427351	22.892391
99.655546	2450.284164	22.897408
99.716231	2458.247078	22.902426
99.376010	2461.551268	22.907443
99.740216	2467.061680	22.912461
99.599886	2478.417352	22.917479
100.147734	2463.529464	22.922496
99.986075	2470.280555	22.927514
100.076678	2461.609251	22.932531
100.151279	2471.040737	22.937549
100.517722	2479.994118	22.942567
100.854474	2485.452027	22.947584
100.575037	2493.364092	22.952602
100.650616	2483.303285	22.957619
100.782928	2485.529804	22.962637
101.047174	2485.441159	22.967655
101.072106	2482.148681	22.972672
101.050900	2471.897896	22.977690
100.972831	2482.344325	22.982707
101.341429	2468.169392	22.987725
101.164121	2497.233495	22.992743
101.349278	2498.561712	22.997760
101.429804	2505.341152	23.002778
101.470359	2510.794976	23.007795
101.979532	2506.754374	23.012813
101.811041	2502.785226	23.017831
101.980865	2494.574911	23.022848
101.922575	2489.843658	23.027866
102.314378	2496.201905	23.032883
102.435650	2489.498354	23.037901
102.295177	2500.708882	23.042919
102.640387	2499.310390	23.047936
102.519245	2511.423700	23.052954
102.677454	2518.531836	23.057971
103.173794	2518.350019	23.062989
102.493125	2518.384165	23.068007
103.104146	2511.900551	23.073024
102.806073	2505.322659	23.078042
102.547430	2518.903018	23.083059
102.573975	2516.235192	23.088077
102.768847	2531.713927	23.093095
103.020605	2536.718061	23.098112
103.076360	2547.487579	23.103130
103.592788	2566.586537	23.108147
103.754407	2562.171142	23.113165
103.299127	2564.603349	23.118183
103.947945	2577.274642	23.123200
104.026536	2582.795119	23.128218
103.909595	2591.423459	23.133235
104.277248	2584.068983	23.138253
104.226486	2582.884015	23.143271
104.326477	2576.827616	23.148288
104.374995	2587.743474	23.153306
104.846533	2597.822968	23.158323
105.147134	2595.184786	23.163341
104.691741	2606.820298	23.168359
104.780368	2604.884424	23.173376
105.107356	2599.732981	23.178394
104.863711	2607.693143	23.183411
105.440344	2623.806496	23.188429
105.608271	2625.598218	23.193447
105.629067	2623.092240	23.198464
105.591511	2622.870978	23.203482
105.930197	2626.832619	23.208499
106.085556	2624.034131	23.213517
106.142215	2625.726509	23.218535
106.245874	2619.180319	23.223552
106.578379	2623.957211	23.228570
106.274924	2624.282589	23.233587
106.109798	2619.990962	23.238605
106.219941	2635.123260	23.243623
106.472868	2630.955502	23.248640
106.376119	2638.334027	23.253658
106.821060	2628.047996	23.258675
106.966580	2647.280897	23.263693
107.043761	2664.390972	23.268711
107.434743	2662.574998	23.273728
107.539091	2662.565059	23.278746
107.317374	2665.374142	23.283763
107.644535	2663.946904	23.288781
107.758353	2658.042962	23.293799
107.389591	2662.794016	23.298816
107.508418	2668.472336	23.303834
107.529699	2677.615606	23.308851
108.309601	2685.008301	23.313869
108.128815	2690.004498	23.318887
108.578860	2679.354681	23.323904
108.279280	2687.964339	23.328922
108.500447	2679.310348	23.333939
108.606371	2682.137538	23.338957
108.562861	2682.059235	23.343975
108.513825	2687.473494	23.348992
108.838905	2695.344592	23.354010
108.631325	2703.668415	23.359027
108.644792	2699.781181	23.364045
108.718001	2701.739246	23.369063
108.576274	2708.818699	23.374080
109.102968	2715.329481	23.379098
109.042587	2734.023469	23.384115
109.205288	2730.232782	23.389133
109.434885	2736.588123	23.394151
109.488377	2747.610608	23.399168
109.836637	2745.056466	23.404186
109.685180	2756.836983	23.409203
110.071573	2745.174504	23.414221
110.126191	2748.170706	23.419239
110.397338	2773.447041	23.424256
110.838299	2783.755519	23.429274
110.585066	2782.431826	23.434291
110.941094	2768.410123	23.439309
110.967293	2769.428711	23.444327
110.699707	2770.291332	23.449344
111.039270	2777.863519	23.454362
111.167334	2766.143658	23.459379
111.105666	2765.594775	23.464397
111.397206	2784.091653	23.469415
111.415738	2790.180245	23.474432
111.645492	2797.081599	23.479450
111.448311	2794.224696	23.484467
111.862298	2782.134944	23.489485
112.383165	2782.779355	23.494503
112.415847	2776.607187	23.499520
112.477606	2770.241096	23.504538
112.694281	2774.430192	23.509555
112.791809	2778.442273	23.514573
112.596671	2774.919101	23.519591
112.552779	2779.240550	23.524608
113.114672	2768.844588	23.529626
112.692490	2777.754395	23.534643
112.710180	2784.670031	23.539661
113.111421	2794.012639	23.544679
112.994241	2802.678991	23.549696
113.157575	2798.272738	23.554714
112.943497	2801.831813	23.559731
113.723897	2808.912022	23.564749
113.725261	2828.590628	23.569767
114.070178	2823.540467	23.574784
114.287537	2818.238861	23.579802
114.055051	2823.322098	23.584819
113.940767	2825.126492	23.589837
114.143745	2820.568839	23.594855
114.201022	2823.166959	23.599872
114.532295	2814.609276	23.604890
114.246960	2827.433412	23.609907
114.376127	2832.545208	23.614925
114.604808	2844.594468	23.619943
114.602676	2850.945124	23.624960
115.098491	2846.957041	23.629978
114.810626	2852.219395	23.634995
114.791198	2868.994465	23.640013
114.964329	2870.233066	23.645031
115.271599	2875.036071	23.650048
115.265965	2880.263686	23.655066
115.405014	2891.493788	23.660083
115.400819	2875.663133	23.665101
115.470708	2888.756747	23.670119
115.963400	2895.295015	23.675136
116.464612	2902.548404	23.680154
116.304619	2907.437249	23.685171
116.544839	2907.320806	23.690189
116.620679	2900.813591	23.695207
116.185685	2915.870566	23.700224
116.974131	2913.730334	23.705242
116.850147	2905.417522	23.710259
117.263410	2905.917831	23.715277
117.141097	2902.604158	23.720295
116.747492	2904.177733	23.725312
117.102578	2903.396276	23.730330
117.196512	2925.080444	23.735347
117.688385	2918.937285	23.740365
117.911174	2918.823573	23.745383
117.536093	2920.772989	23.750400
117.441941	2916.959380	23.755418
117.636886	2925.908292	23.760435
117.940514	2927.094890	23.765453
118.105943	2938.611258	23.770471
118.264137	2942.140443	23.775488
118.202067	2939.609529	23.780506
118.350173	2937.648520	23.785523
118.700047	2944.089246	23.790541
118.738046	2958.084265	23.795559
118.781485	2963.979642	23.800576
119.126462	2960.753715	23.805594
119.336120	2965.303761	23.810611
119.223796	2962.114760	23.815629
119.396409	2959.477640	23.820647
119.512463	2963.445829	23.825664
119.584062	2969.488294	23.830682
119.577940	2981.893208	23.835699
119.338932	2988.243149	23.840717
119.744477	2981.305506	23.845735
119.599101	2998.447611	23.850752
120.357821	3003.173611	23.855770
120.325682	3010.933535	23.860787
120.114139	3011.758981	23.865805
120.755773	3003.408238	23.870823
120.518558	3014.511149	23.875840
121.057318	3015.348451	23.880858
121.007388	3032.169482	23.885875
121.368391	3023.850071	23.890893
121.647111	3025.027953	23.895911
121.407618	3021.006688	23.900928
121.561859	3017.046832	23.905946
121.743422	3017.905377	23.910963
121.538122	3003.460128	23.915981
121.810795	3017.803485	23.920999
121.849554	3025.789023	23.926016
121.869262	3035.942709	23.931034
122.340172	3041.376614	23.936051
122.167450	3043.051312	23.941069
122.060377	3032.349698	23.946087
121.902739	3043.212912	23.951104
122.300503	3050.779253	23.956122
122.649318	3059.139163	23.961139
123.014528	3055.458712	23.966157
123.199872	3060.520742	23.971175
123.162784	3069.622857	23.976192
123.516290	3076.517556	23.981210
123.004511	3085.552018	23.986227
123.197284	3087.519799	23.991245
123.694342	3086.220567	23.996263
123.395508	3091.794018	24.001280
124.064661	3100.507757	24.006298
123.760511	3102.809045	24.011315
123.862057	3103.929472	24.016333
124.239879	3112.458454	24.021351
124.177656	3106.594571	24.026368
124.621216	3114.977538	24.031386
124.509484	3123.217101	24.036403
124.718191	3128.610049	24.041421
125.139045	3128.935584	24.046439
125.300458	3127.963525	24.051456
125.039758	3123.355346	24.056474
125.063113	3131.564280	24.061491
125.188826	3129.054420	24.066509
125.424599	3120.101245	24.071527
125.018841	3134.396327	24.076544
125.374078	3144.895192	24.081562
125.424771	3153.396539	24.086579
125.626929	3153.068278	24.091597
126.307107	3161.136449	24.096615
126.098798	3177.297526	24.101632
126.185217	3179.584978	24.106650
126.466223	3181.340103	24.111667
126.182146	3179.847619	24.116685
126.546843	3175.494946	24.121703
126.251730	3197.145706	24.126720
126.896342	3205.124781	24.131738
126.841894	3201.033455	24.136755
126.932677	3206.571151	24.141773
127.456260	3214.913222	24.146791
127.507419	3224.623369	24.151808
127.357508	3222.377614	24.156826
127.798495	3212.606339	24.161843
127.535210	3227.706109	24.166861
128.202721	3227.112411	24.171879
128.079044	3247.473876	24.176896
128.293842	3245.186762	24.181914
128.649939	3240.500858	24.186931
128.516733	3248.478718	24.191949
128.561624	3242.705321	24.196967
128.741744	3247.316879	24.201984
128.585710	3252.179946	24.207002
129.046675	3263.419816	24.212019
128.872493	3266.505606	24.217037
129.134536	3258.924372	24.222055
128.842853	3267.930755	24.227072
129.319843	3281.986656	24.232090
129.674401	3283.165300	24.237107
129.412621	3286.264817	24.242125
129.832564	3285.867716	24.247143
129.875469	3299.038449	24.252160
130.435597	3311.096064	24.257178
130.882336	3314.220304	24.262195
130.472898	3309.969942	24.267213
130.672436	3309.118151	24.272231
130.782414	3308.567611	24.277248
130.621575	3307.851185	24.282266
130.972719	3310.943057	24.287283
131.108524	3329.966741	24.292301
131.496697	3319.963807	24.297319
131.531922	3323.256675	24.302336
131.111528	3325.086982	24.307354
131.529956	3333.073144	24.312371
131.560447	3331.288333	24.317389
131.760347	3343.617031	24.322407
131.752691	3354.598968	24.327424
132.168115	3357.901716	24.332442
132.345233	3352.053912	24.337459
131.875504	3361.003016	24.342477
132.359433	3369.752217	24.347495
132.414813	3376.371800	24.352512
132.394729	3372.638021	24.357530
133.165537	3382.592167	24.362547
132.809915	3394.761743	24.367565
133.198941	3392.898662	24.372583
133.023402	3395.697466	24.377600
133.336325	3389.250776	24.382618
133.679889	3389.758864	24.387635
133.269308	3400.403107	24.392653
133.773309	3412.008767	24.397671
133.709782	3409.815737	24.402688
133.872277	3419.312857	24.407706
134.112030	3418.678857	24.412723
133.458543	3422.521519	24.417741
134.374529	3430.893747	24.422759
134.222906	3435.055478	24.427776
134.662515	3446.254621	24.432794
135.165901	3447.974934	24.437811
135.160048	3457.062882	24.442829
135.203581	3443.954435	24.447847
135.255168	3449.176406	24.452864
135.431358	3447.756980	24.457882
135.875674	3442.489074	24.462899
135.361423	3442.497141	24.467917
135.696160	3452.753209	24.472935
136.034560	3456.538328	24.477952
136.336616	3466.060953	24.482970
136.578633	3462.614348	24.487987
136.285521	3468.253299	24.493005
136.457534	3458.719722	24.498023
136.859652	3467.049377	24.503040
137.343043	3478.825594	24.508058
137.526395	3478.702277	24.513075
136.868096	3480.595120	24.518093
137.668123	3475.356697	24.523111
137.318752	3469.231522	24.528128
137.105938	3471.064041	24.533146
137.548245	3469.179980	24.538163
137.654735	3485.026886	24.543181
137.608264	3480.160955	24.548199
138.089660	3496.359454	24.553216
138.183530	3499.157098	24.558234
138.146442	3492.638955	24.563251
138.375690	3513.024335	24.568269
138.457688	3514.324603	24.573287
138.951697	3519.417313	24.578304
138.640098	3520.312113	24.583322
138.965694	3519.983446	24.588339
138.880964	3522.758573	24.593357
139.414485	3536.745849	24.598375
139.492005	3543.794437	24.603392
139.289721	3547.664282	24.608410
139.687921	3543.306273	24.613427
139.521119	3548.511987	24.618445
139.975173	3559.510090	24.623463
140.086282	3560.344981	24.628480
139.971974	3575.857271	24.633498
140.288292	3572.269596	24.638515
140.371832	3584.607220	24.643533
140.785220	3590.305966	24.648551
141.093395	3589.531832	24.653568
140.469590	3588.083067	24.658586
141.146905	3590.858759	24.663603
140.980536	3611.880677	24.668621
141.174048	3617.112026	24.673639
141.376256	3618.642817	24.678656
141.398803	3625.475951	24.683674
141.749124	3631.323468	24.688691
141.791707	3639.583279	24.693709
142.215248	3638.888915	24.698727
141.938573	3632.386162	24.703744
142.050288	3652.332447	24.708762
142.209124	3662.960231	24.713779
142.683841	3669.435317	24.718797
142.683328	3664.205473	24.723815
143.229824	3661.676963	24.728832
142.762920	3662.570849	24.733850
143.050123	3668.664991	24.738867
142.958754	3678.511339	24.743885
143.518443	3673.127446	24.748903
143.632346	3677.790521	24.753920
143.553883	3680.861385	24.758938
143.769345	3682.200726	24.763955
143.813400	3695.005435	24.768973
144.137163	3696.646599	24.773991
144.482932	3688.076765	24.779008
144.272489	3689.858433	24.784026
144.463541	3705.578657	24.789043
145.017338	3715.838432	24.794061
145.164978	3721.481007	24.799079
145.339329	3723.757909	24.804096
145.128072	3719.678406	24.809114
145.758925	3707.172148	24.814131
145.314730	3713.759649	24.819149
145.318326	3724.699015	24.824167
146.104981	3734.508841	24.829184
145.826749	3735.815059	24.834202
145.869775	3737.844248	24.839219
146.051063	3732.664811	24.844237
146.228283	3744.820583	24.849255
146.078688	3750.683332	24.854272
146.024921	3759.551683	24.859290
146.804926	3771.758229	24.864307
146.620587	3778.655396	24.869325
146.978160	3784.776429	24.874343
147.060365	3786.098779	24.879360
147.329225	3800.869463	24.884378
147.552728	3796.614515	24.889395
147.784138	3804.144111	24.894413
147.966281	3801.751571	24.899431
148.078865	3798.789162	24.904448
148.036854	3817.301483	24.909466
148.367969	3818.373364	24.914483
148.474079	3824.723187	24.919501
148.564535	3838.423443	24.924519
148.774490	3823.833572	24.929536
148.287238	3830.099599	24.934554
148.791768	3845.218473	24.939571
148.847961	3849.152048	24.944589
148.974945	3858.036318	24.949607
149.326811	3872.585738	24.954624
149.529099	3881.032114	24.959642
149.653301	3871.950856	24.964659
149.913180	3877.736871	24.969677
150.276601	3895.705989	24.974695
150.179781	3895.269894	24.979712
150.280999	3909.053739	24.984730
150.288755	3899.050115	24.989747
150.601482	3913.375285	24.994765
150.846114	3925.056632	24.999783
150.988672	3922.263107	25.004800
150.923012	3924.965868	25.009818
151.278385	3923.950756	25.014835
151.187271	3935.204942	25.019853
151.596843	3943.236953	25.024871
151.421571	3951.458439	25.029888
151.833377	3946.893040	25.034906
151.925329	3955.037943	25.039923
152.153542	3962.552324	25.044941
152.366541	3966.483453	25.049959
152.545828	3957.832257	25.054976
152.406528	3959.994196	25.059994
153.146101	3959.632231	25.065011
153.319331	3962.455391	25.070029
153.187848	3967.807197	25.075047
153.387941	3967.602345	25.080064
153.619556	3972.808890	25.085082
153.776750	3965.562581	25.090099
153.818793	3972.127657	25.095117
153.747477	3974.802904	25.100135
154.101829	3968.781943	25.105152
153.964834	3976.599742	25.110170
154.133208	3978.653510	25.115187
154.231570	3988.097850	25.120205
154.358556	3996.985345	25.125223
154.545928	3999.550629	25.130240
154.479109	4006.921866	25.135258
154.450651	4021.000717	25.140275
154.774238	4022.604063	25.145293
154.957998	4042.874068	25.150311
155.358602	4045.112409	25.155328
155.147452	4049.782315	25.160346
155.527701	4052.083817	25.165363
155.797868	4065.121657	25.170381
155.632655	4069.260411	25.175399
156.107802	4070.877894	25.180416
155.979834	4089.520745	25.185434
156.043659	4099.371416	25.190451
156.552431	4106.049648	25.195469
156.473248	4109.909796	25.200487
156.577842	4120.369588	25.205504
157.059965	4141.413625	25.210522
156.940009	4143.815597	25.215539
157.425303	4143.973240	25.220557
157.858380	4159.359241	25.225575
157.950247	4163.400925	25.230592
158.212285	4164.250077	25.235610
158.030853	4164.026084	25.240627
158.389916	4167.211558	25.245645
158.490528	4172.375555	25.250663
158.845621	4181.363130	25.255680
159.117663	4191.941926	25.260698
158.824459	4190.210897	25.265715
159.458424	4184.404886	25.270733
158.886240	4199.607516	25.275751
159.259236	4211.082710	25.280768
159.717002	4217.317607	25.285786
159.807996	4220.112658	25.290803
160.253536	4209.513156	25.295821
159.695925	4222.519815	25.300839
160.073486	4234.281542	25.305856
160.102820	4237.600752	25.310874
160.031584	4249.738972	25.315891
160.483485	4258.935525	25.320909
160.630673	4264.436302	25.325927
161.390902	4277.807856	25.330944
161.140632	4284.330459	25.335962
161.388679	4290.064801	25.340979
161.560939	4285.644164	25.345997
161.170844	4285.575961	25.351015
161.770509	4300.465676	25.356032
161.993483	4305.219144	25.361050
161.982026	4308.399561	25.366067
162.476524	4309.426939	25.371085
162.255093	4329.293591	25.376103
162.426762	4329.692912	25.381120
162.589345	4339.278884	25.386138
162.774703	4342.677831	25.391155
163.101466	4357.424117	25.396173
163.066635	4359.645491	25.401191
163.223068	4362.919560	25.406208
163.488910	4357.032282	25.411226
163.588010	4372.499194	25.416243
164.025029	4365.694981	25.421261
164.084475	4384.738050	25.426279
164.427827	4377.651800	25.431296
163.984745	4388.986659	25.436314
164.068055	4397.953791	25.441331
164.385993	4408.749631	25.446349
164.847261	4402.014203	25.451367
164.747961	4424.494303	25.456384
165.227488	4419.965524	25.461402
165.518976	4428.896902	25.466419
165.395095	4429.724458	25.471437
165.773576	4435.391065	25.476455
165.730181	4445.539645	25.481472
165.894111	4452.436166	25.486490
165.832745	4449.964902	25.491507
166.577967	4460.229835	25.496525
166.564639	4466.724853	25.501543
166.739111	4465.375060	25.506560
166.886149	4467.978295	25.511578
166.991119	4481.765144	25.516595
167.820478	4479.299531	25.521613
167.620739	4494.491404	25.526631
167.817296	4489.195728	25.531648
168.096444	4493.719494	25.536666
167.737300	4487.131502	25.541683
167.901832	4500.959538	25.546701
168.124207	4509.276803	25.551719
168.331705	4519.326147	25.556736
168.111907	4526.926731	25.561754
168.679289	4534.757522	25.566771
169.176426	4543.378969	25.571789
169.149530	4543.206517	25.576807
169.317794	4536.520099	25.581824
169.732603	4552.982497	25.586842
169.408532	4566.527291	25.591859
169.789787	4568.585655	25.596877
169.798904	4569.127237	25.601895
169.667528	4566.969947	25.606912
170.164773	4579.016171	25.611930
170.581321	4596.497878	25.616947
170.698534	4587.726693	25.621965
170.441073	4605.610709	25.626983
170.684080	4607.330897	25.632000
171.502404	4606.429455	25.637018
171.007588	4609.736152	25.642035
171.311757	4623.918028	25.647053
171.572106	4635.669972	25.652071
171.526437	4637.312283	25.657088
172.030777	4642.239559	25.662106
171.924804	4650.889257	25.667123
172.306999	4655.785168	25.672141
172.707877	4654.125278	25.677159
172.878966	4673.031213	25.682176
172.862827	4671.667076	25.687194
173.003430	4677.522538	25.692212
173.473535	4672.622707	25.697229
173.479892	4671.409714	25.702247
173.401502	4672.814105	25.707264
173.960306	4679.434209	25.712282
173.879900	4691.286920	25.717300
174.099951	4686.726126	25.722317
174.204608	4688.736298	25.727335
174.342090	4699.980397	25.732352
174.718637	4708.908057	25.737370
174.930873	4715.055333	25.742388
174.929980	4708.660499	25.747405
174.933655	4713.666229	25.752423
175.001803	4712.961220	25.757440
175.568293	4726.893752	25.762458
175.608201	4735.814190	25.767476
175.860074	4738.000164	25.772493
176.099918	4740.497360	25.777511
175.493533	4741.419458	25.782528
175.774165	4752.410739	25.787546
175.927578	4762.601264	25.792564
176.377483	4766.880548	25.797581
176.162387	4774.688829	25.802599
176.030458	4784.968259	25.807616
176.778989	4790.406555	25.812634
176.837860	4810.608601	25.817652
177.167401	4823.700817	25.822669
177.344131	4832.189520	25.827687
177.679950	4842.569314	25.832704
178.051312	4845.620409	25.837722
178.599358	4857.734617	25.842740
178.703952	4859.236617	25.847757
178.680559	4854.193093	25.852775
178.847356	4874.207851	25.857792
179.485539	4870.367482	25.862810
179.253239	4876.846447	25.867828
179.478082	4875.548707	25.872845
180.038494	4873.210404	25.877863
179.626345	4882.943518	25.882880
179.798266	4882.869334	25.887898
180.329300	4893.502662	25.892916
180.402821	4898.529067	25.897933
180.234696	4899.890716	25.902951
180.192440	4896.845064	25.907968
180.247980	4916.438540	25.912986
180.698178	4914.802466	25.918004
180.833508	4940.200964	25.923021
181.376799	4948.790123	25.928039
180.859246	4962.220321	25.933056
181.473047	4962.869203	25.938074
181.402074	4969.973175	25.943092
181.825091	4967.290225	25.948109
181.812896	4988.419001	25.953127
181.852351	4991.187523	25.958144
182.231840	4996.614252	25.963162
182.907310	5015.359456	25.968180
182.883325	5020.701043	25.973197
183.363993	5022.109418	25.978215
183.325813	5035.300430	25.983232
183.638281	5042.123400	25.988250
183.475006	5038.702114	25.993268
183.959947	5043.550470	25.998285
184.113971	5060.878047	26.003303
183.962255	5063.862766	26.008320
184.189134	5061.927069	26.013338
184.650341	5078.944545	26.018356
184.632530	5082.634299	26.023373
184.992116	5080.166447	26.028391
184.604646	5090.157800	26.033408
185.101035	5096.721549	26.038426
185.363592	5108.375600	26.043444
185.465201	5114.568752	26.048461
185.760425	5127.859114	26.053479
185.940516	5140.766638	26.058496
186.152235	5133.211450	26.063514
186.090897	5153.135991	26.068532
186.410784	5166.097390	26.073549
186.600330	5162.450352	26.078567
186.508174	5185.599467	26.083584
187.081928	5178.656739	26.088602
187.136895	5190.412808	26.093620
187.570305	5198.422707	26.098637
187.718478	5204.564402	26.103655
187.505717	5208.104797	26.108672
188.091766	5205.033266	26.113690
187.931192	5228.082673	26.118708
188.172314	5234.686462	26.123725
188.451731	5225.251928	26.128743
188.785169	5242.999807	26.133760
188.979266	5242.451815	26.138778
189.230587	5254.334994	26.143796
189.002061	5257.735822	26.148813
189.438730	5268.437817	26.153831
189.448616	5273.003961	26.158848
189.876726	5274.935117	26.163866
189.989421	5294.052868	26.168884
190.088982	5302.635952	26.173901
190.602330	5309.758998	26.178919
190.638566	5311.050782	26.183936
190.808448	5319.139897	26.188954
190.826672	5325.646062	26.193972
191.401422	5341.556967	26.198989
191.545166	5345.436115	26.204007
191.489458	5355.808094	26.209024
191.866376	5345.875262	26.214042
191.630118	5368.371669	26.219060
192.120315	5384.573640	26.224077
192.432557	5388.454810	26.229095
192.587777	5394.844838	26.234112
192.550927	5406.656467	26.239130
192.933351	5402.833961	26.244148
193.042246	5418.855794	26.249165
193.550498	5416.929644	26.254183
193.556391	5429.697362	26.259200
194.101299	5430.846334	26.264218
194.247991	5437.821689	26.269236
194.294698	5440.639650	26.274253
194.858281	5442.316010	26.279271
194.364449	5439.685084	26.284288
194.920222	5456.126220	26.289306
195.162440	5465.476190	26.294324
195.374616	5457.242120	26.299341
195.636593	5449.969338	26.304359
195.453541	5474.098987	26.309376
195.602487	5479.776630	26.314394
196.141148	5476.529393	26.319412
196.046393	5490.960684	26.324429
196.576837	5494.091137	26.329447
196.482912	5515.848872	26.334464
196.791150	5501.860963	26.339482
196.858888	5516.112142	26.344500
196.602653	5524.201814	26.349517
197.036320	5520.185015	26.354535
197.275186	5537.102016	26.359552
197.455007	5545.865197	26.364570
197.590750	5565.541505	26.369588
197.721667	5570.906336	26.374605
197.619791	5583.315403	26.379623
198.422118	5603.512343	26.384640
198.486555	5605.109082	26.389658
198.542442	5621.237253	26.394676
198.550154	5636.359698	26.399693
199.294651	5635.280381	26.404711
199.502021	5648.648020	26.409728
199.325456	5657.656486	26.414746
200.034627	5669.891204	26.419764
200.274013	5685.987529	26.424781
200.605629	5672.330435	26.429799
200.539770	5679.891598	26.434816
200.691642	5687.642778	26.439834
200.811003	5685.951141	26.444852
200.806948	5702.353934	26.449869
201.187604	5702.742646	26.454887
201.296041	5707.066179	26.459904
201.684994	5717.608611	26.464922
201.936045	5727.711778	26.469940
201.801994	5729.576374	26.474957
201.957846	5729.154313	26.479975
202.241031	5735.761166	26.484992
202.639716	5752.520750	26.490010
202.921231	5752.839764	26.495028
202.663583	5775.721981	26.500045
203.285302	5773.942167	26.505063
203.523903	5780.063577	26.510080
203.636033	5793.480967	26.515098
204.136088	5802.869636	26.520116
204.060206	5808.434238	26.525133
204.345991	5806.208291	26.530151
204.668776	5814.933421	26.535168
204.618393	5817.432041	26.540186
205.146211	5823.508158	26.545204
204.656087	5833.307654	26.550221
205.083929	5843.973491	26.555239
205.301925	5848.728146	26.560256
205.488258	5870.376107	26.565274
205.645739	5874.404738	26.570292
206.198521	5884.056665	26.575309
206.539522	5887.384171	26.580327
206.558804	5892.634003	26.585344
206.422162	5896.247837	26.590362
206.970901	5906.714839	26.595380
206.974343	5914.328377	26.600397
207.502514	5918.216872	26.605415
207.671377	5936.076440	26.610432
207.598939	5936.248876	26.615450
208.111261	5939.738956	26.620468
208.214383	5956.412448	26.625485
208.963846	5952.538644	26.630503
209.309339	5953.097019	26.635520
209.156089	5957.613130	26.640538
209.518807	5953.679957	26.645556
209.254775	5974.975595	26.650573
209.703045	5967.275678	26.655591
209.711178	5973.212288	26.660608
209.652894	5990.652926	26.665626
209.815038	5989.642724	26.670644
209.862719	6006.571172	26.675661
210.480867	6016.260280	26.680679
210.675449	6030.192101	26.685696
211.026545	6039.452705	26.690714
211.474056	6049.326399	26.695732
211.439710	6053.129426	26.700749
211.857040	6048.044940	26.705767
211.804423	6056.289195	26.710784
211.938273	6070.786145	26.715802
212.485870	6071.584343	26.720820
212.075361	6092.022334	26.725837
212.578159	6098.108777	26.730855
213.030601	6095.774613	26.735872
212.685353	6102.098082	26.740890
213.184063	6106.733067	26.745908
212.972173	6132.228657	26.750925
213.801008	6135.059939	26.755943
213.965704	6148.213658	26.760960
214.133270	6147.281517	26.765978
214.224510	6150.705020	26.770996
214.319691	6156.946885	26.776013
214.855486	6170.664365	26.781031
214.852993	6164.471304	26.786048
214.800421	6170.698438	26.791066
215.426356	6182.820273	26.796084
215.471035	6186.923466	26.801101
215.669536	6196.024963	26.806119
215.914865	6221.890998	26.811136
216.151734	6224.660349	26.816154
216.486291	6226.574698	26.821172
216.609959	6237.689326	26.826189
216.725177	6242.378110	26.831207
216.720886	6250.264480	26.836224
217.092467	6265.870250	26.841242
217.150639	6270.593231	26.846260
217.634166	6282.506998	26.851277
217.681807	6292.885415	26.856295
217.761681	6296.575895	26.861312
217.852004	6313.823095	26.866330
218.523249	6321.799389	26.871348
218.911852	6342.314507	26.876365
219.151769	6342.204412	26.881383
219.243315	6346.306613	26.886400
219.044965	6363.968425	26.891418
219.308916	6367.150252	26.896436
219.640724	6389.552607	26.901453
219.909811	6398.513719	26.906471
220.348572	6406.886346	26.911488
220.408101	6425.161275	26.916506
220.628717	6430.701715	26.921524
220.794759	6437.964848	26.926541
221.118942	6445.664103	26.931559
221.859535	6461.126998	26.936576
221.556544	6474.066948	26.941594
222.008535	6466.899740	26.946612
222.036952	6479.348981	26.951629
222.248137	6484.496314	26.956647
222.724012	6486.915740	26.961664
222.511942	6514.249150	26.966682
222.972641	6512.996428	26.971700
222.877343	6523.779342	26.976717
223.223765	6541.791625	26.981735
223.559571	6539.305209	26.986752
223.687441	6564.710292	26.991770
224.054013	6575.379844	26.996788
224.293171	6584.077405	27.001805
224.624283	6601.470251	27.006823
224.972909	6594.963179	27.011840
224.569464	6598.865178	27.016858
224.887848	6612.396072	27.021876
225.360710	6633.482330	27.026893
225.568467	6640.997869	27.031911
226.069484	6648.792624	27.036928
226.513132	6668.604980	27.041946
226.823208	6666.870750	27.046964
226.837419	6666.644485	27.051981
226.649835	6678.168020	27.056999
227.233977	6687.281956	27.062016
227.344361	6694.162461	27.067034
227.808090	6702.922761	27.072052
227.840673	6712.820778	27.077069
227.771881	6711.676245	27.082087
228.325825	6719.345936	27.087104
228.613195	6734.996868	27.092122
229.009677	6728.453841	27.097140
228.976477	6735.306345	27.102157
228.967051	6747.900598	27.107175
229.357785	6749.430538	27.112192
229.304091	6763.458634	27.117210
229.871324	6764.462142	27.122228
229.909468	6777.361492	27.127245
229.724961	6782.510916	27.132263
230.051820	6787.883292	27.137280
230.366394	6801.133962	27.142298
230.654412	6805.865271	27.147316
231.223870	6827.893151	27.152333
230.690221	6833.226715	27.157351
231.340498	6851.128564	27.162368
231.446470	6861.914872	27.167386
231.779046	6873.622221	27.172404
232.372016	6881.592084	27.177421
232.259818	6893.637456	27.182439
232.601035	6903.045263	27.187456
232.573865	6917.527069	27.192474
233.349909	6916.966788	27.197492
233.835581	6923.602333	27.202509
233.875846	6929.695220	27.207527
234.493914	6934.564272	27.212544
234.408305	6945.219640	27.217562
234.729658	6946.211168	27.222580
235.133804	6944.910454	27.227597
235.481858	6966.123981	27.232615
235.578064	6972.476455	27.237632
235.483100	6973.593183	27.242650
235.844637	6969.552647	27.247668
236.149693	6980.030031	27.252685
236.489356	6988.494215	27.257703
236.746735	6985.180294	27.262720
236.333422	6990.791799	27.267738
236.649694	6999.812110	27.272756
237.000767	7000.224430	27.277773
237.321772	7019.683866	27.282791
237.477609	7024.701118	27.287808
237.476350	7034.443608	27.292826
237.787820	7051.145439	27.297844
237.983523	7056.045964	27.302861
237.595272	7077.873756	27.307879
238.503031	7086.580467	27.312896
238.624504	7099.331242	27.317914
239.036762	7113.498125	27.322932
239.114163	7123.222025	27.327949
239.418195	7138.968556	27.332967
239.599146	7155.826676	27.337984
239.949652	7166.587484	27.343002
240.249251	7183.496496	27.348020
240.496891	7191.324863	27.353037
240.545873	7217.011545	27.358055
240.856613	7221.057506	27.363072
241.417314	7227.488835	27.368090
241.614960	7237.926368	27.373108
241.769926	7237.201349	27.378125
241.900628	7261.464141	27.383143
242.132937	7272.562379	27.388160
242.178751	7291.743204	27.393178
242.471990	7291.845740	27.398196
242.899977	7294.260151	27.403213
242.917535	7319.661460	27.408231
243.271172	7325.670661	27.413248
243.416139	7344.731830	27.418266
243.634937	7353.963316	27.423284
244.005410	7367.609729	27.428301
244.211035	7374.295623	27.433319
244.659719	7391.825491	27.438336
245.001588	7404.043152	27.443354
245.363733	7412.519796	27.448372
246.135527	7417.993133	27.453389
245.712858	7429.222482	27.458407
246.204360	7429.827489	27.463424
246.327112	7422.051684	27.468442
246.476959	7434.997136	27.473460
246.661245	7444.770758	27.478477
246.772987	7448.317572	27.483495
247.136802	7463.947679	27.488512
247.740940	7472.149668	27.493530
247.994895	7465.439292	27.498548
248.017739	7462.932328	27.503565
248.384160	7479.351284	27.508583
248.675757	7480.186498	27.513600
249.278011	7478.254889	27.518618
249.314568	7473.362257	27.523636
249.564180	7483.261417	27.528653
249.527666	7510.862405	27.533671
250.029095	7502.762058	27.538688
250.064786	7499.602739	27.543706
250.036493	7515.256431	27.548724
250.328783	7520.063024	27.553741
250.605198	7535.217551	27.558759
250.755765	7544.589258	27.563776
250.968095	7556.713662	27.568794
250.884463	7574.317623	27.573812
251.523807	7587.255955	27.578829
251.520920	7603.893882	27.583847
252.155225	7602.086677	27.588864
252.086829	7630.311609	27.593882
252.315862	7627.652357	27.598900
252.851898	7642.172785	27.603917
252.627303	7657.251203	27.608935
252.994769	7685.294288	27.613952
253.536430	7690.068176	27.618970
253.867905	7700.630231	27.623988
253.918826	7709.818739	27.629005
254.268593	7737.094364	27.634023
254.302615	7735.775809	27.639040
254.884114	7752.701168	27.644058
254.789750	7760.087701	27.649076
255.352466	7771.775357	27.654093
255.692485	7792.653296	27.659111
256.160851	7801.482853	27.664128
256.289927	7808.041988	27.669146
256.738647	7817.423954	27.674164
257.091005	7826.470589	27.679181
257.106258	7838.720762	27.684199
257.517208	7832.894887	27.689216
257.356948	7845.147302	27.694234
257.902563	7858.731917	27.699252
258.176404	7860.434961	27.704269
258.266298	7874.299342	27.709287
258.327674	7890.406548	27.714304
258.489162	7887.366366	27.719322
258.649494	7910.397280	27.724340
259.298358	7930.889191	27.729357
259.353343	7941.156891	27.734375
259.686275	7949.682559	27.739392
259.901147	7968.300905	27.744410
259.917668	7986.148448	27.749428
260.571080	7993.272709	27.754445
260.695186	8007.422281	27.759463
260.879234	8014.061275	27.764480
261.525658	8037.736013	27.769498
261.195611	8050.299298	27.774516
261.602549	8065.358045	27.779533
261.610045	8074.714549	27.784551
262.488337	8085.434260	27.789568
262.579546	8094.319884	27.794586
262.703930	8102.565740	27.799604
262.960463	8113.427066	27.804621
262.942481	8120.441870	27.809639
263.331807	8135.844399	27.814656
263.803914	8141.510130	27.819674
263.788756	8164.922446	27.824692
264.319685	8164.893043	27.829709
264.625242	8190.941840	27.834727
264.952388	8187.512592	27.839744
265.423819	8209.093393	27.844762
265.419224	8227.648511	27.849780
265.544603	8219.568877	27.854797
266.332762	8241.920948	27.859815
266.335436	8240.158959	27.864832
267.174661	8255.210129	27.869850
267.234962	8265.338264	27.874868
267.561134	8267.292032	27.879885
267.596261	8262.484658	27.884903
267.400017	8270.272521	27.889920
267.988032	8286.660643	27.894938
267.884208	8308.031747	27.899956
268.314769	8316.330765	27.904973
268.508308	8321.768678	27.909991
268.773248	8348.152400	27.915008
269.436565	8354.792210	27.920026
269.301349	8370.021378	27.925044
269.678737	8382.354096	27.930061
269.896950	8403.090794	27.935079
269.972193	8419.300474	27.940096
270.687102	8424.009531	27.945114
270.582184	8442.643722	27.950132
271.326227	8446.243221	27.955149
271.494848	8465.134514	27.960167
271.916375	8477.602454	27.965184
272.037553	8492.059099	27.970202
272.053548	8504.969441	27.975220
272.557757	8513.686384	27.980237
272.902971	8530.873632	27.985255
273.143206	8530.905553	27.990272
273.502457	8549.347168	27.995290
273.685003	8562.225145	28.000308
274.040462	8572.196711	28.005325
274.303639	8582.002780	28.010343
274.204570	8594.501835	28.015360
274.528307	8599.205914	28.020378
275.145606	8619.147874	28.025396
275.319095	8627.881949	28.030413
275.518821	8640.226885	28.035431
275.685846	8661.031877	28.040448
276.207507	8665.262963	28.045466
276.507505	8676.354601	28.050484
276.854736	8679.675332	28.055501
277.180393	8689.967348	28.060519
277.122639	8698.178859	28.065536
277.549216	8713.629708	28.070554
277.818912	8724.962911	28.075572
278.289466	8735.734248	28.080589
278.598018	8734.647294	28.085607
278.376796	8750.840562	28.090624
278.970439	8771.026339	28.095642
279.121068	8789.311442	28.100660
279.302587	8796.547825	28.105677
279.611824	8804.585078	28.110695
279.725645	8823.276945	28.115712
279.947672	8826.989867	28.120730
280.301152	8852.075455	28.125748
280.836771	8860.096212	28.130765
281.096168	8866.992074	28.135783
281.242057	8880.204366	28.140800
281.705198	8889.120511	28.145818
281.813006	8904.214173	28.150836
282.211591	8908.666658	28.155853
282.626177	8929.499473	28.160871
282.450375	8937.473846	28.165888
283.153103	8943.735146	28.170906
282.948341	8962.748581	28.175924
283.419261	8963.820983	28.180941
283.507857	8981.806585	28.185959
283.854949	9001.485035	28.190976
284.327750	9013.784286	28.195994
284.484115	9036.018441	28.201012
284.815982	9039.698413	28.206029
285.319819	9062.929531	28.211047
285.446647	9072.097354	28.216064
286.080654	9080.102796	28.221082
286.199850	9083.557197	28.226100
286.448586	9111.362152	28.231117
286.961006	9126.853572	28.236135
287.228310	9130.155334	28.241152
287.436777	9143.452728	28.246170
287.651063	9157.314371	28.251188
288.002873	9170.570387	28.256205
288.068141	9170.566574	28.261223
288.359088	9192.517782	28.266240
289.114438	9199.973846	28.271258
289.163152	9218.306910	28.276276
289.623488	9223.665408	28.281293
290.005951	9238.132222	28.286311
290.364715	9241.770135	28.291328
290.602861	9247.308680	28.296346
290.492449	9259.784701	28.301364
290.776822	9277.338947	28.306381
290.942044	9290.861074	28.311399
291.074674	9304.489350	28.316416
291.418809	9320.477731	28.321434
291.635999	9334.105411	28.326452
291.936781	9357.807572	28.331469
292.528062	9377.021933	28.336487
292.658888	9394.688747	28.341504
292.982159	9398.035464	28.346522
293.073749	9419.888719	28.351540
293.159405	9439.267598	28.356557
294.036734	9450.064037	28.361575
293.970178	9459.385480	28.366592
294.327016	9486.586801	28.371610
294.563703	9502.759509	28.376628
294.962269	9522.076828	28.381645
295.567883	9527.415815	28.386663
295.914162	9547.909562	28.391680
296.128973	9556.031395	28.396698
296.458566	9564.084734	28.401716
296.662342	9583.360011	28.406733
297.151794	9585.544089	28.411751
297.687518	9610.362197	28.416768
297.887267	9612.004394	28.421786
298.076104	9626.050342	28.426804
298.369110	9634.709338	28.431821
298.704921	9646.177987	28.436839
298.632772	9661.543570	28.441856
298.986577	9669.138503	28.446874
299.382337	9673.961028	28.451892
299.720680	9694.926626	28.456909
299.978357	9708.526138	28.461927
300.085162	9723.936359	28.466944
300.261129	9747.241797	28.471962
300.949225	9748.217081	28.476980
300.873626	9764.700997	28.481997
301.423027	9772.249546	28.487015
301.318836	9795.605245	28.492032
301.639757	9801.967695	28.497050
302.259306	9824.439659	28.502068
302.477916	9835.895210	28.507085
302.992465	9845.934107	28.512103
302.894358	9869.323677	28.517120
302.949913	9878.051556	28.522138
303.479310	9890.936114	28.527156
303.647510	9912.228562	28.532173
304.187436	9916.905429	28.537191
304.724052	9936.125776	28.542208
304.836047	9948.011716	28.547226
305.285545	9962.920102	28.552244
305.628066	9988.612006	28.557261
306.262561	9990.422942	28.562279
306.315200	10013.975365	28.567296
306.567364	10023.417664	28.572314
307.194709	10032.684372	28.577332
306.914917	10041.565896	28.582349
307.776649	10052.639828	28.587367
307.933372	10067.562587	28.592384
308.509932	10077.355090	28.597402
308.707407	10102.406814	28.602420
308.699972	10105.019265	28.607437
309.103334	10116.518669	28.612455
309.852773	10127.610237	28.617472
309.930116	10149.286607	28.622490
310.044110	10153.755558	28.627508
310.337236	10167.138305	28.632525
310.789940	10181.225431	28.637543
310.880714	10196.809056	28.642560
311.560472	10202.332388	28.647578
311.533582	10207.031813	28.652596
311.794364	10234.577649	28.657613
311.961644	10250.231428	28.662631
312.185221	10272.544941	28.667648
312.699603	10280.613850	28.672666
312.957142	10306.085852	28.677684
313.312320	10324.690901	28.682701
313.636634	10336.297548	28.687719
313.645385	10356.851374	28.692736
314.206968	10366.659006	28.697754
314.363349	10377.351058	28.702772
314.611318	10403.983485	28.707789
315.035930	10426.745627	28.712807
315.435667	10444.664958	28.717824
315.975259	10460.566868	28.722842
316.145304	10474.338541	28.727860
316.279425	10508.358527	28.732877
316.733045	10514.220496	28.737895
316.661606	10535.219655	28.742912
317.478194	10556.382854	28.747930
317.836069	10567.895977	28.752948
318.161964	10591.557885	28.757965
318.589199	10607.805902	28.762983
318.664277	10617.749868	28.768000
318.843527	10630.029869	28.773018
320.032304	10636.297708	28.778036
320.027129	10655.587880	28.783053
320.350383	10655.420512	28.788071
320.681068	10667.370537	28.793088
321.031199	10682.181395	28.798106
321.358733	10691.656432	28.803124
321.496935	10705.960570	28.808141
321.863194	10712.069944	28.813159
322.482913	10724.056825	28.818176
322.113285	10734.638869	28.823194
322.771801	10725.773666	28.828212
323.000787	10753.353666	28.833229
323.328756	10753.829697	28.838247
323.692027	10777.912253	28.843264
323.800829	10787.427917	28.848282
324.370843	10797.348128	28.853300
324.490038	10803.208896	28.858317
324.615519	10818.550787	28.863335
324.940425	10832.437398	28.868352
324.713986	10863.243290	28.873370
325.795130	10875.019057	28.878388
325.662657	10890.897150	28.883405
326.238808	10904.611842	28.888423
326.444712	10936.183725	28.893440
326.845820	10945.413706	28.898458
327.324317	10961.098270	28.903476
327.661756	10973.053747	28.908493
328.223668	10994.917271	28.913511
328.900991	11001.366395	28.918528
329.146663	11016.572791	28.923546
329.550333	11029.683077	28.928564
329.510552	11037.033939	28.933581
330.217835	11052.733264	28.938599
330.659230	11063.197923	28.943616
330.639002	11071.698255	28.948634
331.412738	11079.758463	28.953652
331.439232	11090.954381	28.958669
331.443697	11106.167057	28.963687
332.145583	11117.042479	28.968704
332.147951	11128.955816	28.973722
332.276322	11145.380578	28.978740
332.579527	11169.293065	28.983757
333.203253	11190.679810	28.988775
333.395549	11194.025267	28.993792
333.838908	11217.922177	28.998810
333.902638	11229.803862	29.003828
334.283338	11256.969295	29.008845
334.646596	11271.270188	29.013863
334.900789	11282.942088	29.018880
335.246681	11308.423719	29.023898
335.789954	11314.508721	29.028916
335.589727	11337.619303	29.033933
335.996511	11350.953519	29.038951
336.633638	11380.248258	29.043968
336.791738	11405.528930	29.048986
337.671343	11422.025718	29.054004
337.635598	11453.206884	29.059021
338.064833	11471.539391	29.064039
338.739682	11478.295362	29.069056
338.879143	11498.886803	29.074074
339.169579	11502.750588	29.079092
339.506569	11523.996327	29.084109
339.992985	11539.538042	29.089127
340.535638	11561.878896	29.094144
340.592223	11579.489936	29.099162
341.064280	11583.925246	29.104180
340.943710	11609.167744	29.109197
341.257121	11621.263181	29.114215
341.564926	11642.428368	29.119232
341.979127	11662.152797	29.124250
342.686007	11675.967571	29.129268
342.766217	11701.576611	29.134285
343.274408	11716.625619	29.139303
343.872660	11723.933645	29.144320
344.183695	11748.714011	29.149338
344.423760	11749.693283	29.154356
344.554562	11762.985765	29.159373
345.002533	11777.283248	29.164391
345.080431	11784.821220	29.169408
345.703069	11797.973530	29.174426
345.961557	11815.859463	29.179444
346.207041	11830.630785	29.184461
346.730195	11844.038698	29.189479
347.251083	11856.414401	29.194496
347.514002	11871.009349	29.199514
347.810492	11872.854479	29.204532
348.128245	11886.139868	29.209549
348.362776	11903.764389	29.214567
348.851682	11917.796634	29.219584
348.879656	11939.315447	29.224602
349.082282	11954.153576	29.229620
349.614850	11972.732479	29.234637
350.083511	11998.138977	29.239655
350.194644	12008.807472	29.244672
350.374494	12037.508583	29.249690
351.229640	12054.653943	29.254708
351.356053	12070.094602	29.259725
351.483667	12089.131772	29.264743
352.276422	12103.653380	29.269760
352.520240	12123.701813	29.274778
353.050468	12133.916326	29.279796
353.196832	12154.002160	29.284813
353.770725	12176.897779	29.289831
354.083828	12191.365120	29.294848
354.115235	12212.656347	29.299866
354.950129	12228.368250	29.304884
355.178968	12250.755923	29.309901
355.289556	12270.013830	29.314919
355.638563	12276.922183	29.319936
356.022832	12301.537074	29.324954
356.562069	12314.955436	29.329972
356.899428	12344.308111	29.334989
357.481323	12365.570123	29.340007
357.863155	12367.869289	29.345024
358.129807	12384.665042	29.350042
358.452290	12399.446854	29.355060
358.926450	12417.754302	29.360077
359.005561	12445.363421	29.365095
359.713216	12444.261115	29.370112
359.719084	12467.378692	29.375130
360.140002	12487.456612	29.380148
360.739691	12508.914942	29.385165
360.940228	12526.886416	29.390183
361.054192	12542.613617	29.395200
361.471216	12561.489090	29.400218
362.092390	12578.535794	29.405236
362.741450	12587.355123	29.410253
362.467216	12611.729362	29.415271
363.070366	12618.143303	29.420288
363.252615	12648.496522	29.425306
363.987081	12656.124627	29.430324
364.278700	12684.897636	29.435341
364.403067	12699.094934	29.440359
364.769421	12712.461715	29.445376
365.023936	12735.562776	29.450394
365.352214	12758.478629	29.455412
366.083993	12774.068196	29.460429
366.148826	12795.118004	29.465447
366.670823	12806.237326	29.470464
366.777489	12832.712175	29.475482
367.255196	12865.384716	29.480500
367.700235	12881.369813	29.485517
368.175026	12896.320789	29.490535
368.681927	12907.448852	29.495552
368.947472	12926.061050	29.500570
369.206179	12935.649058	29.505588
369.537807	12938.174055	29.510605
369.774375	12957.135034	29.515623
370.260757	12961.334746	29.520640
370.917551	12978.300443	29.525658
371.047007	12990.040311	29.530676
371.327182	13007.027132	29.535693
371.629738	13034.722113	29.540711
372.350621	13045.595686	29.545728
372.435001	13065.891149	29.550746
372.659007	13076.785727	29.555764
373.268247	13094.213719	29.560781
373.667178	13119.133700	29.565799
374.203620	13126.676172	29.570816
374.764437	13133.662192	29.575834
374.633348	13161.700025	29.580852
375.216077	13179.261723	29.585869
375.380000	13200.460673	29.590887
375.811874	13208.761676	29.595904
376.257921	13227.911170	29.600922
376.625693	13251.124597	29.605940
377.156202	13267.766120	29.610957
377.290784	13293.037217	29.615975
377.771161	13296.221083	29.620992
378.101058	13320.656343	29.626010
378.332989	13341.200573	29.631028
378.857231	13354.110437	29.636045
379.083601	13371.642868	29.641063
379.576888	13384.784976	29.646080
380.244841	13406.268373	29.651098
380.348482	13432.384525	29.656116
380.842623	13449.821400	29.661133
381.177885	13476.387662	29.666151
381.289425	13494.418208	29.671168
381.768035	13524.502194	29.676186
382.191379	13541.110216	29.681204
382.435952	13562.511682	29.686221
382.768673	13591.810177	29.691239
383.341627	13603.272529	29.696256
384.198419	13633.701676	29.701274
384.448462	13652.733876	29.706292
384.900243	13667.313264	29.711309
384.999625	13692.741992	29.716327
385.630982	13707.353285	29.721344
386.018160	13725.846161	29.726362
386.337593	13746.607662	29.731380
386.793517	13762.118094	29.736397
387.153445	13783.498584	29.741415
387.806088	13795.817031	29.746432
387.978323	13817.763826	29.751450
388.089050	13829.074496	29.756468
388.873320	13850.805456	29.761485
388.754636	13864.937484	29.766503
389.589034	13883.016234	29.771520
390.161314	13903.791989	29.776538
390.720886	13918.714706	29.781556
391.276728	13924.609110	29.786573
391.416582	13951.566665	29.791591
391.913282	13956.658720	29.796608
392.103631	13965.945309	29.801626
392.481142	13997.587021	29.806644
392.918849	13989.159129	29.811661
392.987097	14019.677673	29.816679
393.124485	14034.862413	29.821696
393.594533	14056.642828	29.826714
394.048998	14076.818242	29.831732
394.354581	14091.253478	29.836749
394.636071	14107.179962	29.841767
394.931605	14124.149590	29.846784
395.701666	14141.581782	29.851802
395.969936	14164.461365	29.856820
396.860163	14174.614284	29.861837
396.864760	14193.211756	29.866855
397.558370	14204.630310	29.871872
397.337825	14226.702263	29.876890
397.676787	14251.712080	29.881908
398.014439	14259.210352	29.886925
398.187754	14283.728226	29.891943
398.856387	14303.554522	29.896960
399.448610	14328.411077	29.901978
399.675674	14354.032285	29.906996
400.155126	14374.602027	29.912013
400.271195	14390.450440	29.917031
400.708394	14409.207748	29.922048
401.009645	14438.752498	29.927066
401.231107	14460.158597	29.932084
402.006667	14491.492446	29.937101
401.969380	14529.383689	29.942119
402.720535	14549.986858	29.947136
403.159366	14566.132260	29.952154
403.403973	14604.014237	29.957172
403.942487	14635.214911	29.962189
404.277148	14665.424314	29.967207
404.902187	14687.231707	29.972224
405.210735	14706.265272	29.977242
405.386527	14740.409523	29.982260
406.092160	14765.330999	29.987277
406.669691	14785.557369	29.992295
406.857287	14814.517287	29.997312
407.731064	14832.824485	30.002330
407.581355	14856.291475	30.007348
408.296541	14876.903791	30.012365
408.709494	14912.700851	30.017383
409.461677	14926.586718	30.022400
410.143930	14946.032565	30.027418
410.457973	14958.805904	30.032436
411.164751	14975.478167	30.037453
411.446530	14997.516543	30.042471
411.944868	15006.079535	30.047488
412.369227	15013.940355	30.052506
412.577234	15039.148580	30.057524
413.115891	15051.694146	30.062541
413.487151	15065.718738	30.067559
413.554105	15090.917542	30.072576
414.389780	15106.230629	30.077594
414.261734	15122.992726	30.082612
414.800033	15140.762174	30.087629
414.916508	15165.886997	30.092647
415.441262	15179.259134	30.097664
416.018510	15210.606280	30.102682
415.958614	15234.590256	30.107700
416.414406	15258.433480	30.112717
416.780628	15283.190877	30.117735
417.493962	15307.148578	30.122752
418.297463	15339.287970	30.127770
418.297457	15361.096131	30.132788
418.635475	15376.932707	30.137805
418.998761	15397.502799	30.142823
419.644034	15423.925314	30.147840
420.467263	15438.691072	30.152858
420.667690	15460.013154	30.157876
421.138513	15478.238810	30.162893
421.675041	15496.589999	30.167911
421.711494	15523.458587	30.172928
422.353852	15542.447018	30.177946
422.595242	15567.107476	30.182964
423.223128	15573.272206	30.187981
423.284138	15594.515208	30.192999
423.493362	15603.603823	30.198016
423.967607	15634.708815	30.203034
424.340525	15649.532638	30.208052
424.581815	15667.971294	30.213069
425.244651	15697.865625	30.218087
425.609290	15714.898488	30.223104
426.410537	15740.690605	30.228122
426.386250	15768.001745	30.233140
426.845451	15785.721017	30.238157
427.077040	15818.857249	30.243175
427.388238	15847.019250	30.248192
427.984362	15874.321799	30.253210
428.560930	15903.680405	30.258228
429.280765	15925.862850	30.263245
429.727041	15943.739054	30.268263
429.867160	15973.011367	30.273280
430.670439	16004.630776	30.278298
431.167184	16021.835882	30.283316
432.053693	16029.469974	30.288333
432.434827	16042.460935	30.293351
433.134835	16056.554782	30.298368
433.515201	16071.513578	30.303386
433.857289	16086.977411	30.308404
434.443546	16103.849571	30.313421
434.762142	16123.881037	30.318439
435.002710	16130.722510	30.323456
435.583096	16155.485391	30.328474
435.878947	16174.737182	30.333492
436.259039	16191.970188	30.338509
436.737510	16202.261340	30.343527
437.060645	16231.432737	30.348544
437.436153	16250.340490	30.353562
437.698948	16274.865851	30.358580
437.809164	16299.468837	30.363597
438.425282	16328.629234	30.368615
438.484373	16350.505064	30.373632
438.909476	16374.992497	30.378650
439.614637	16417.818416	30.383668
439.929036	16437.907720	30.388685
440.613052	16467.970494	30.393703
440.915301	16489.438854	30.398720
441.688660	16510.504965	30.403738
441.976508	16542.139666	30.408756
441.911159	16566.732589	30.413773
442.817559	16582.247407	30.418791
442.987539	16625.091285	30.423808
443.244304	16643.266299	30.428826
443.944392	16676.775979	30.433844
444.457347	16703.195717	30.438861
445.108921	16742.685877	30.443879
445.360961	16761.960911	30.448896
445.957501	16796.902042	30.453914
446.396299	16818.671552	30.458932
446.784199	16836.829367	30.463949
447.520040	16872.990125	30.468967
447.157768	16898.378555	30.473984
448.038141	16925.290637	30.479002
448.755954	16962.379845	30.484020
449.027005	16977.495445	30.489037
449.758818	16999.017117	30.494055
450.208802	17030.785153	30.499072
450.290510	17049.218545	30.504090
450.690917	17080.084757	30.509108
451.375658	17099.137584	30.514125
451.801493	17125.003001	30.519143
452.258132	17153.542117	30.524160
452.542955	17161.905787	30.529178
453.071753	17187.540376	30.534196
453.681551	17210.155320	30.539213
454.227609	17229.558493	30.544231
454.497360	17255.644366	30.549248
454.797279	17270.247139	30.554266
455.219295	17297.768500	30.559284
455.653584	17317.031337	30.564301
456.141878	17343.556892	30.569319
456.556756	17371.003669	30.574336
457.310859	17397.285512	30.579354
457.656216	17422.582745	30.584372
458.276806	17442.713580	30.589389
458.647175	17455.700868	30.594407
459.320594	17486.739757	30.599424
459.528043	17503.100765	30.604442
460.174800	17526.405195	30.609460
460.328455	17548.795068	30.614477
460.840594	17580.794333	30.619495
461.439886	17606.045715	30.624512
462.037830	17626.925737	30.629530
462.443194	17654.999825	30.634548
462.631173	17681.383362	30.639565
463.342802	17707.596473	30.644583
463.640807	17739.983314	30.649600
464.571568	17753.053598	30.654618
464.814500	17787.811849	30.659636
465.224804	17803.876007	30.664653
465.558826	17830.874931	30.669671
465.787100	17857.669346	30.674688
466.456722	17877.496038	30.679706
467.300852	17895.223298	30.684724
467.475307	17919.094939	30.689741
468.369233	17942.872872	30.694759
468.613324	17970.182996	30.699776
468.912521	17998.274211	30.704794
469.334952	18010.672511	30.709812
469.673717	18037.841553	30.714829
470.430714	18059.082496	30.719847
470.622954	18091.530713	30.724864
471.614856	18118.667062	30.729882
471.968702	18152.966369	30.734900
472.449262	18178.117063	30.739917
473.159191	18189.592312	30.744935
473.443680	18221.615659	30.749952
474.010504	18239.456163	30.754970
474.661036	18253.594123	30.759988
475.081953	18281.047563	30.765005
475.523156	18298.358170	30.770023
475.952895	18317.812245	30.775040
476.476999	18340.536700	30.780058
477.022742	18348.916876	30.785076
477.226474	18380.037083	30.790093
477.872443	18395.395157	30.795111
478.405027	18428.814082	30.800128
478.903389	18444.966063	30.805146
479.342250	18464.621020	30.810164
479.389633	18497.086286	30.815181
480.046532	18502.814668	30.820199
480.616761	18535.741424	30.825216
480.916277	18555.734180	30.830234
481.559291	18567.169594	30.835252
481.705420	18605.078027	30.840269
482.438747	18633.683391	30.845287
482.738575	18655.843164	30.850304
483.393919	18682.919302	30.855322
483.829946	18698.190463	30.860340
484.013841	18726.357650	30.865357
484.850808	18747.207763	30.870375
485.413092	18766.053981	30.875392
485.351322	18789.249788	30.880410
486.316709	18806.137591	30.885428
486.496334	18831.064604	30.890445
486.838564	18848.151130	30.895463
487.385866	18873.829281	30.900480
487.824371	18898.949590	30.905498
488.524204	18929.658134	30.910516
488.804977	18952.231885	30.915533
489.444858	18986.917474	30.920551
489.493312	19003.532090	30.925568
489.659676	19032.485873	30.930586
490.730614	19062.687939	30.935604
491.001452	19101.493888	30.940621
491.517155	19126.962516	30.945639
491.987155	19157.903271	30.950656
492.400275	19193.098582	30.955674
493.290144	19221.370719	30.960692
493.602149	19251.142292	30.965709
494.254370	19285.611672	30.970727
494.798783	19309.610294	30.975744
494.811386	19332.782462	30.980762
495.757629	19363.408872	30.985780
496.470341	19402.708505	30.990797
497.312619	19416.476116	30.995815
497.599228	19451.192592	31.000832
498.011921	19473.980049	31.005850
498.449799	19498.475753	31.010868
498.699696	19523.468460	31.015885
499.202154	19561.108130	31.020903
499.769414	19581.660213	31.025920
500.264750	19613.836048	31.030938
500.800156	19648.381228	31.035956
501.572905	19674.157803	31.040973
501.913057	19699.528315	31.045991
502.553214	19737.607974	31.051008
502.962569	19754.021388	31.056026
503.346761	19779.612557	31.061044
503.891511	19823.349341	31.066061
504.831349	19853.162495	31.071079
505.147700	19875.567472	31.076096
505.531524	19904.905481	31.081114
506.205198	19935.556527	31.086132
506.531717	19963.134533	31.091149
506.963752	19985.211930	31.096167
507.893808	20004.614603	31.101184
508.359977	20039.872631	31.106202
508.910440	20061.925248	31.111220
509.311878	20086.484261	31.116237
510.055020	20111.747964	31.121255
510.531212	20140.256818	31.126272
510.599234	20165.329376	31.131290
511.357469	20189.137637	31.136308
511.628308	20215.359992	31.141325
512.408924	20243.492771	31.146343
512.964338	20271.098542	31.151360
513.072417	20299.216690	31.156378
513.811317	20322.705913	31.161396
514.040321	20352.877575	31.166413
514.588977	20373.863046	31.171431
515.225468	20408.216826	31.176448
515.493818	20427.426602	31.181466
516.344408	20464.173157	31.186484
516.731627	20502.199146	31.191501
517.179642	20523.655457	31.196519
517.924963	20550.410501	31.201536
518.228050	20573.026858	31.206554
518.795943	20593.282947	31.211572
519.146970	20631.687636	31.216589
519.640422	20651.658483	31.221607
520.365222	20668.250720	31.226624
520.886535	20707.734595	31.231642
521.140508	20717.564169	31.236660
521.616075	20749.738649	31.241677
522.322882	20775.324819	31.246695
522.682561	20800.725292	31.251712
523.145159	20830.766326	31.256730
523.598938	20861.731273	31.261748
524.131586	20890.352425	31.266765
524.817925	20924.528706	31.271783
525.662090	20951.704788	31.276800
525.903871	20982.715766	31.281818
526.310486	20998.492492	31.286836
527.168004	21034.556641	31.291853
527.740684	21058.369749	31.296871
527.441051	21092.151039	31.301888
528.522751	21128.047560	31.306906
528.965221	21149.075767	31.311924
529.894493	21184.193816	31.316941
530.410088	21219.951704	31.321959
530.844669	21246.478353	31.326976
531.306721	21272.507890	31.331994
532.000710	21299.366775	31.337012
532.619026	21325.820525	31.342029
533.292456	21369.799663	31.347047
533.824933	21393.031847	31.352064
533.807416	21410.221186	31.357082
534.647688	21443.976191	31.362100
535.245224	21480.069239	31.367117
535.452088	21510.846411	31.372135
536.207505	21543.490166	31.377152
536.391735	21578.169570	31.382170
537.189783	21605.726580	31.387188
537.712273	21651.954146	31.392205
537.789899	21679.276566	31.397223
538.953375	21709.076478	31.402240
539.300656	21750.978158	31.407258
539.931623	21769.538496	31.412276
540.557104	21814.511850	31.417293
540.826645	21843.415707	31.422311
541.719366	21879.728640	31.427328
541.914944	21911.658210	31.432346
542.928850	21935.403275	31.437364
543.151537	21967.777320	31.442381
543.693286	22012.821108	31.447399
544.217219	22036.908423	31.452416
545.085988	22066.495964	31.457434
545.735417	22097.476442	31.462452
546.326042	22128.384034	31.467469
546.587165	22156.563005	31.472487
547.296601	22174.934509	31.477504
547.745236	22219.734281	31.482522
548.213841	22250.534798	31.487540
548.517104	22276.969661	31.492557
549.234466	22318.732437	31.497575
549.778563	22348.611368	31.502592
550.018030	22384.958035	31.507610
550.749993	22404.817481	31.512628
551.637716	22447.792349	31.517645
552.043372	22477.175007	31.522663
552.523428	22505.674045	31.527680
552.921419	22545.888633	31.532698
553.658319	22565.330418	31.537716
554.521533	22590.894453	31.542733
554.877537	22607.906271	31.547751
555.758008	22645.486322	31.552768
556.243511	22660.752827	31.557786
556.924984	22686.244346	31.562804
557.491822	22699.412881	31.567821
557.657338	22734.906071	31.572839
558.529449	22748.071060	31.577856
559.025021	22782.015041	31.582874
559.381782	22803.747207	31.587892
559.570872	22823.180258	31.592909
559.815024	22861.972526	31.597927
560.823447	22894.730547	31.602944
561.181673	22929.189175	31.607962
561.708358	22960.518819	31.612980
562.062761	22998.339908	31.617997
562.751008	23033.050345	31.623015
563.366662	23062.243003	31.628032
563.712242	23100.350026	31.633050
564.408903	23133.252056	31.638068
564.805850	23174.106311	31.643085
565.574464	23210.605424	31.648103
566.222532	23240.804331	31.653120
566.910109	23279.243603	31.658138
567.219030	23319.935007	31.663156
567.939159	23355.449869	31.668173
568.356337	23395.947536	31.673191
569.511685	23425.441674	31.678208
569.559532	23455.324163	31.683226
570.455359	23490.843346	31.688244
571.486354	23521.020621	31.693261
572.252327	23557.280654	31.698279
572.858379	23586.229135	31.703296
573.403289	23606.472962	31.708314
573.903960	23632.227827	31.713332
574.585328	23668.134795	31.718349
574.765015	23692.682471	31.723367
575.850568	23712.197165	31.728384
575.969543	23743.471830	31.733402
576.673319	23772.525345	31.738420
577.477419	23803.326282	31.743437
577.638630	23832.673396	31.748455
578.321460	23854.747442	31.753472
578.214418	23893.185963	31.758490
578.958839	23923.294984	31.763508
580.037972	23962.129246	31.768525
580.946326	23994.133791	31.773543
581.726081	24022.417444	31.778560
581.972187	24054.361500	31.783578
582.675357	24077.595380	31.788596
582.980488	24093.548456	31.793613
583.725891	24139.096002	31.798631
584.530126	24168.829499	31.803648
584.936499	24191.560203	31.808666
585.573901	24223.070398	31.813684
585.910874	24242.671257	31.818701
586.177295	24277.949168	31.823719
586.985446	24308.232054	31.828736
587.672357	24337.649245	31.833754
588.158279	24366.819899	31.838772
588.721565	24403.144812	31.843789
589.304630	24442.367358	31.848807
589.589384	24468.005450	31.853824
590.371852	24507.658221	31.858842
591.117712	24543.348118	31.863860
591.728927	24570.881639	31.868877
591.784479	24608.525079	31.873895
592.434319	24639.433622	31.878912
593.277436	24670.596326	31.883930
593.364018	24707.072284	31.888948
594.069019	24732.733373	31.893965
594.387226	24773.173497	31.898983
595.254386	24798.291063	31.904000
595.662238	24834.407275	31.909018
596.245986	24874.237247	31.914036
596.655445	24907.572686	31.919053
597.440838	24950.227723	31.924071
598.250140	24989.883566	31.929088
598.586137	25017.056342	31.934106
599.236752	25061.685516	31.939124
599.935569	25095.898630	31.944141
600.229014	25139.996179	31.949159
601.358857	25174.786538	31.954176
601.825853	25218.294620	31.959194
602.344572	25255.064122	31.964212
602.957906	25293.657934	31.969229
603.610107	25337.503816	31.974247
604.299872	25370.770845	31.979264
604.740587	25416.678685	31.984282
605.418070	25458.005576	31.989300
606.405338	25498.392935	31.994317
607.106618	25534.382292	31.999335
607.621987	25576.164567	32.004352
608.118397	25597.542948	32.009370
608.780338	25639.744792	32.014388
609.241117	25671.708361	32.019405
609.960806	25712.283414	32.024423
610.676715	25749.490612	32.029440
611.534236	25777.309532	32.034458
612.175733	25828.900103	32.039476
612.574771	25851.412638	32.044493
613.357036	25892.951532	32.049511
614.025583	25931.626400	32.054528
614.816382	25963.829468	32.059546
615.335671	25998.242875	32.064564
616.186955	26024.641110	32.069581
616.513781	26060.784853	32.074599
616.987272	26093.524465	32.079616
617.831450	26117.850959	32.084634
617.986849	26159.754019	32.089652
618.700705	26203.269807	32.094669
619.482729	26242.768072	32.099687
619.884811	26279.380748	32.104704
620.717414	26310.585566	32.109722
621.305761	26363.892260	32.114740
622.119787	26392.161252	32.119757
622.327854	26422.876279	32.124775
623.043660	26461.026510	32.129792
624.100212	26504.780006	32.134810
624.496269	26534.163804	32.139828
625.281315	26568.094149	32.144845
625.855831	26598.480285	32.149863
626.692339	26649.163902	32.154880
627.282845	26680.603135	32.159898
627.590493	26703.889362	32.164916
628.141299	26734.317336	32.169933
628.779107	26774.313246	32.174951
629.382936	26812.361591	32.179968
630.408347	26845.768098	32.184986
630.760931	26891.996467	32.190004
631.710760	26916.813005	32.195021
632.463550	26961.702156	32.200039
633.027528	26988.544829	32.205056
633.430847	27015.235729	32.210074
633.587455	27051.104522	32.215092
634.669394	27087.093918	32.220109
635.396645	27115.314309	32.225127
635.603470	27151.763209	32.230144
636.820894	27179.521381	32.235162
636.991850	27215.008993	32.240180
637.543145	27240.008430	32.245197
637.914426	27262.381515	32.250215
638.447395	27306.237705	32.255232
639.290685	27334.888979	32.260250
639.923646	27364.925809	32.265268
641.108303	27400.368759	32.270285
642.102684	27425.829952	32.275303
642.663299	27460.530116	32.280320
643.082685	27473.358306	32.285338
643.583484	27513.168555	32.290356
644.181421	27548.084240	32.295373
644.809108	27581.623776	32.300391
645.175703	27613.396586	32.305408
646.099522	27649.411745	32.310426
646.831328	27689.628599	32.315444
646.988577	27726.383359	32.320461
647.545681	27762.772178	32.325479
648.268673	27803.041201	32.330496
649.069777	27844.517945	32.335514
649.565230	27893.121722	32.340532
650.288055	27931.166171	32.345549
651.046227	27973.161871	32.350567
651.622183	28013.909424	32.355584
652.382076	28048.610985	32.360602
652.343979	28099.226612	32.365620
653.632074	28146.076125	32.370637
654.344298	28179.401144	32.375655
654.727121	28231.733617	32.380672
655.552799	28270.660133	32.385690
655.780121	28324.072755	32.390708
656.302492	28354.267422	32.395725
657.552953	28405.870311	32.400743
658.115408	28450.925294	32.405760
658.989468	28492.208629	32.410778
659.505029	28534.110742	32.415796
660.072465	28581.655631	32.420813
660.933776	28624.647852	32.425831
661.489374	28663.061180	32.430848
662.389535	28709.871608	32.435866
662.720330	28753.901634	32.440884
663.616361	28802.122475	32.445901
664.747320	28840.155270	32.450919
664.504053	28885.634473	32.455936
665.814483	28921.439635	32.460954
666.407830	28969.537608	32.465972
666.832077	29003.850893	32.470989
667.935579	29044.284008	32.476007
668.338226	29088.986165	32.481024
669.149548	29122.638537	32.486042
669.788627	29172.171010	32.491060
670.513774	29201.867419	32.496077
671.403994	29239.262309	32.501095
671.655623	29282.281860	32.506112
672.526810	29321.930172	32.511130
672.925364	29369.478053	32.516148
673.853638	29409.509499	32.521165
674.770703	29450.731144	32.526183
675.302877	29485.236928	32.531200
676.182774	29499.776827	32.536218
677.137345	29537.870149	32.541236
677.907583	29579.759801	32.546253
678.806839	29606.016121	32.551271
679.180658	29648.144986	32.556288
679.738734	29666.907362	32.561306
680.637479	29698.492615	32.566324
680.811661	29727.827267	32.571341
681.729276	29751.072019	32.576359
681.959760	29783.855620	32.581376
682.401601	29825.095549	32.586394
683.220422	29855.239683	32.591412
683.501829	29896.226745	32.596429
684.182985	29933.996990	32.601447
684.866223	29980.262738	32.606464
685.635251	30017.343000	32.611482
686.263504	30057.321555	32.616500
686.763371	30098.369627	32.621517
687.805651	30140.059787	32.626535
688.207529	30179.309152	32.631552
689.145465	30219.473413	32.636570
689.764849	30279.144724	32.641588
690.181953	30314.978438	32.646605
691.195970	30357.672238	32.651623
691.316684	30407.080257	32.656640
692.204145	30461.988043	32.661658
693.094942	30495.857791	32.666676
693.955618	30547.286901	32.671693
695.217078	30585.972571	32.676711
695.657213	30633.263998	32.681728
696.367023	30666.157259	32.686746
696.981737	30710.115399	32.691764
697.526413	30748.705015	32.696781
698.600944	30789.297821	32.701799
699.466733	30832.268678	32.706816
700.121354	30873.237162	32.711834
700.950640	30913.925513	32.716852
701.562206	30953.269942	32.721869
702.537724	30987.696171	32.726887
703.125653	31037.424464	32.731904
703.696103	31061.831342	32.736922
704.213198	31097.909940	32.741940
705.102072	31145.176515	32.746957
705.891762	31183.791789	32.751975
706.641730	31226.339089	32.756992
707.436836	31266.148458	32.762010
708.442888	31298.136590	32.767028
709.091308	31339.985679	32.772045
709.624155	31367.117123	32.777063
709.752205	31400.165873	32.782080
711.038745	31449.185191	32.787098
712.205601	31483.139763	32.792116
712.507521	31517.305701	32.797133
713.895276	31541.578833	32.802151
714.526125	31580.845574	32.807168
715.193969	31606.628626	32.812186
715.547162	31637.809190	32.817204
716.293260	31663.282935	32.822221
717.500091	31699.311463	32.827239
717.599392	31734.084770	32.832256
718.189689	31767.801365	32.837274
718.994686	31802.514849	32.842292
719.191079	31843.929998	32.847309
720.144874	31888.728915	32.852327
720.990257	31925.933404	32.857344
721.493886	31963.077685	32.862362
722.348073	31993.845270	32.867380
722.804152	32045.423645	32.872397
723.618364	32083.632156	32.877415
724.393116	32132.107368	32.882432
724.782656	32169.585979	32.887450
725.970344	32213.539764	32.892468
726.381230	32269.696528	32.897485
727.127143	32299.918868	32.902503
727.681857	32342.638116	32.907520
728.372383	32378.078547	32.912538
729.137225	32413.798212	32.917556
729.582495	32456.990017	32.922573
730.634742	32488.656652	32.927591
731.197242	32530.844017	32.932608
731.849504	32578.896909	32.937626
732.628255	32611.719240	32.942644
733.250789	32652.721549	32.947661
733.701157	32697.322872	32.952679
734.470804	32748.796983	32.957696
735.183264	32799.211739	32.962714
735.888058	32846.511011	32.967732
736.515675	32900.113003	32.972749
737.738509	32936.147493	32.977767
738.292300	32983.350600	32.982784
739.282206	33028.215858	32.987802
740.443293	33067.187412	32.992820
740.768728	33111.063163	32.997837
741.847277	33154.625082	33.002855
742.566451	33195.101221	33.007872
743.264769	33236.522718	33.012890
744.099210	33276.936709	33.017908
744.462025	33333.186046	33.022925
745.608756	33371.749470	33.027943
746.302726	33418.457435	33.032960
747.325725	33464.171955	33.037978
748.020287	33501.554610	33.042996
748.597381	33546.845997	33.048013
749.470405	33583.530684	33.053031
750.057425	33629.579377	33.058048
750.737223	33674.621030	33.063066
751.726044	33720.929444	33.068084
752.334545	33769.952924	33.073101
753.489732	33810.153334	33.078119
754.373485	33855.896838	33.083136
754.725511	33885.696327	33.088154
755.797378	33932.479031	33.093172
756.466316	33976.106802	33.098189
757.146754	34016.053183	33.103207
757.965761	34056.983215	33.108224
758.890088	34098.016963	33.113242
759.811517	34132.836216	33.118260
760.316054	34184.254207	33.123277
761.126190	34218.920323	33.128295
762.409696	34259.253241	33.133312
762.506985	34302.825789	33.138330
763.498302	34331.817674	33.143348
763.933067	34385.883594	33.148365
764.766683	34421.260819	33.153383
766.029030	34455.458188	33.158400
766.251089	34504.449056	33.163418
767.461754	34526.142170	33.168436
768.194846	34573.314450	33.173453
768.878580	34609.758699	33.178471
769.997330	34630.751856	33.183488
770.621276	34679.477871	33.188506
771.386478	34718.255262	33.193524
772.236167	34753.314395	33.198541
773.058589	34791.836376	33.203559
773.512311	34831.212826	33.208576
774.156031	34871.318324	33.213594
775.165314	34919.010851	33.218612
775.962524	34953.471551	33.223629
776.404409	34992.926029	33.228647
777.608828	35030.244206	33.233664
778.027764	35076.973630	33.238682
778.814292	35107.497155	33.243700
779.190333	35144.300327	33.248717
779.996999	35165.892975	33.253735
780.779827	35213.703825	33.258752
781.023741	35260.657070	33.263770
782.131823	35293.254987	33.268788
783.051623	35337.137143	33.273805
783.931659	35388.872315	33.278823
784.637680	35420.774642	33.283840
785.142208	35459.897714	33.288858
786.060133	35502.838394	33.293876
786.578757	35555.844568	33.298893
787.244705	35592.792810	33.303911
787.872351	35645.826398	33.308928
788.800099	35703.915767	33.313946
789.787587	35747.276012	33.318964
790.729658	35796.485914	33.323981
791.242097	35847.723344	33.328999
792.138436	35896.548613	33.334016
792.676942	35956.185538	33.339034
793.312062	35992.589197	33.344052
794.056915	36049.924093	33.349069
794.950649	36103.985757	33.354087
796.310034	36160.004362	33.359104
796.485831	36218.314056	33.364122
797.434458	36265.639726	33.369140
798.608218	36326.335348	33.374157
799.615420	36374.157939	33.379175
800.800596	36421.491176	33.384192
801.168612	36470.571220	33.389210
802.387423	36516.337569	33.394228
803.332155	36568.508109	33.399245
803.964200	36613.278953	33.404263
805.212651	36653.033871	33.409280
805.507691	36699.115996	33.414298
806.401189	36744.744079	33.419316
807.003131	36798.227193	33.424333
807.664006	36844.606450	33.429351
808.873415	36887.795158	33.434368
809.670175	36952.630146	33.439386
810.573703	36993.261747	33.444404
811.061727	37038.486023	33.449421
812.002678	37083.709028	33.454439
813.037420	37117.807232	33.459456
813.676933	37177.330579	33.464474
814.645533	37218.369763	33.469492
815.222683	37260.096344	33.474509
816.137843	37320.449560	33.479527
817.479806	37363.529947	33.484544
817.764592	37410.411965	33.489562
818.981440	37464.609863	33.494580
819.796312	37506.615875	33.499597
820.426741	37544.426737	33.504615
821.421637	37587.467070	33.509632
821.974273	37631.038361	33.514650
822.742698	37688.683819	33.519668
823.753445	37732.676819	33.524685
824.416494	37786.848427	33.529703
825.244622	37832.014798	33.534720
825.968980	37876.925598	33.539738
827.094546	37925.308578	33.544756
827.613593	37980.274706	33.549773
828.067825	38022.331877	33.554791
829.425311	38063.299139	33.559808
830.019460	38109.331133	33.564826
831.183796	38165.233774	33.569844
832.091204	38211.191640	33.574861
832.682963	38259.873968	33.579879
833.585536	38298.769169	33.584896
833.834408	38345.399577	33.589914
834.853057	38378.857287	33.594932
836.018764	38435.082928	33.599949
836.988294	38476.206585	33.604967
837.741532	38514.973791	33.609984
838.221930	38557.129090	33.615002
839.118993	38598.510958	33.620020
839.708265	38641.047774	33.625037
840.203237	38690.992029	33.630055
841.082898	38737.138754	33.635072
841.986603	38785.014558	33.640090
842.507557	38852.997175	33.645108
843.477259	38902.431234	33.650125
844.335667	38951.610904	33.655143
845.691475	38991.441892	33.660160
846.686787	39054.095665	33.665178
847.444346	39098.896307	33.670196
848.109171	39156.125560	33.675213
848.616587	39209.996268	33.680231
849.817683	39260.881057	33.685248
851.094219	39314.625267	33.690266
851.792311	39369.756619	33.695284
852.873417	39418.908806	33.700301
853.509609	39470.318905	33.705319
854.677554	39505.981068	33.710336
855.770045	39559.874865	33.715354
856.888136	39597.796371	33.720372
857.570543	39647.839968	33.725389
858.386342	39687.465890	33.730407
859.856060	39734.565836	33.735424
860.573395	39777.040565	33.740442
861.261363	39814.700945	33.745460
862.109942	39859.223293	33.750477
862.284172	39899.335838	33.755495
863.707295	39946.500460	33.760512
864.427512	39992.687480	33.765530
865.196302	40040.504973	33.770548
866.433806	40087.490267	33.775565
866.977270	40142.799579	33.780583
868.108981	40177.228964	33.785600
868.828241	40224.934458	33.790618
869.877315	40276.073113	33.795636
870.529537	40330.752414	33.800653
871.219795	40368.628423	33.805671
872.361924	40412.334370	33.810688
872.728914	40466.761430	33.815706
873.799097	40518.668924	33.820724
874.636108	40574.844080	33.825741
875.537637	40632.116053	33.830759
876.460343	40676.672740	33.835776
877.063972	40725.516862	33.840794
877.958823	40787.577898	33.845812
878.955068	40830.238692	33.850829
879.640396	40898.220943	33.855847
880.419362	40945.564494	33.860864
881.322660	41008.801196	33.865882
882.706297	41066.934851	33.870900
883.514980	41114.995114	33.875917
883.978838	41175.006009	33.880935
885.436974	41213.022557	33.885952
886.005320	41261.196669	33.890970
886.676479	41317.197318	33.895988
887.684656	41369.584568	33.901005
888.563327	41427.172112	33.906023
889.596959	41480.207080	33.911040
890.613076	41532.637751	33.916058
891.369105	41591.155684	33.921076
892.320660	41626.273341	33.926093
893.126952	41683.063328	33.931111
893.949964	41721.882257	33.936128
894.986882	41764.968591	33.941146
895.367087	41807.658182	33.946164
896.706578	41846.054923	33.951181
897.669940	41902.276953	33.956199
898.552540	41937.924540	33.961216
899.342509	41988.329827	33.966234
900.498314	42029.070534	33.971252
901.363946	42062.172075	33.976269
902.086688	42109.609169	33.981287
902.824749	42165.500311	33.986304
903.944363	42215.525610	33.991322
904.264914	42268.465419	33.996340
905.595288	42309.324785	34.001357
906.285002	42361.859145	34.006375
907.587551	42414.158525	34.011392
908.530233	42472.763430	34.016410
909.299152	42521.111300	34.021428
910.256685	42565.495604	34.026445
911.163497	42623.708054	34.031463
911.879103	42675.182833	34.036480
912.958140	42736.025117	34.041498
913.350409	42785.159919	34.046516
914.493411	42838.358145	34.051533
915.241736	42897.873795	34.056551
916.410030	42958.070208	34.061568
917.300358	43010.650603	34.066586
918.202224	43070.231228	34.071604
919.003339	43129.865740	34.076621
920.074682	43187.275921	34.081639
921.329373	43246.131309	34.086656
922.080066	43303.971511	34.091674
922.978938	43357.557099	34.096692
923.977279	43415.396767	34.101709
925.084391	43459.316684	34.106727
926.488202	43511.242273	34.111744
927.539051	43564.191017	34.116762
928.235189	43622.508662	34.121780
929.436118	43668.286588	34.126797
929.933794	43721.461478	34.131815
931.306823	43767.149409	34.136832
932.288939	43814.138409	34.141850
933.268169	43862.184293	34.146868
934.019671	43927.091411	34.151885
934.902545	43966.822101	34.156903
935.818413	44015.751141	34.161920
936.807332	44060.348598	34.166938
937.421907	44125.062671	34.171956
938.852578	44165.119096	34.176973
939.519008	44214.631618	34.181991
940.458767	44273.387237	34.187008
941.657029	44318.635585	34.192026
942.302405	44372.472058	34.197044
943.467477	44410.230081	34.202061
944.353856	44467.096918	34.207079
945.157712	44515.026187	34.212096
946.292268	44568.312124	34.217114
946.776373	44626.811091	34.222132
947.808343	44668.765268	34.227149
948.614379	44724.823017	34.232167
949.736417	44778.699698	34.237184
950.738639	44838.079588	34.242202
951.300167	44883.529993	34.247220
952.612404	44935.966656	34.252237
953.213027	44991.310810	34.257255
954.118473	45046.651653	34.262272
955.173657	45102.405661	34.267290
955.829828	45163.099412	34.272308
956.739361	45202.986278	34.277325
957.992161	45255.793566	34.282343
958.671055	45310.158415	34.287360
959.761979	45352.054041	34.292378
960.333956	45407.593483	34.297396
961.375762	45463.103780	34.302413
962.423536	45513.565277	34.307431
963.004954	45571.722536	34.312448
963.748925	45630.018965	34.317466
964.595439	45703.646047	34.322484
966.295690	45746.307326	34.327501
967.354652	45807.958224	34.332519
968.214745	45865.199635	34.337536
969.457706	45921.508268	34.342554
970.087303	45984.321263	34.347572
971.291975	46035.594396	34.352589
972.705445	46086.923518	34.357607
973.237906	46148.531267	34.362624
974.579208	46200.713306	34.367642
975.595197	46258.171699	34.372660
976.465351	46318.139207	34.377677
977.819055	46376.930430	34.382695
978.909827	46424.932735	34.387712
979.904866	46468.477589	34.392730
980.630563	46529.081907	34.397748
981.944545	46573.703074	34.402765
982.654605	46623.486115	34.407783
983.344312	46680.895456	34.412800
984.758169	46739.792080	34.417818
985.625889	46796.547553	34.422836
986.715930	46851.256630	34.427853
987.691166	46906.129319	34.432871
988.179447	46956.922055	34.437888
989.455838	47011.083593	34.442906
990.405948	47066.820975	34.447924
991.567897	47125.157053	34.452941
992.586035	47179.359430	34.457959
993.461068	47246.483670	34.462976
994.569301	47300.564684	34.467994
995.457946	47358.102755	34.473012
996.616346	47409.417894	34.478029
997.890984	47466.339086	34.483047
999.013969	47529.211985	34.488064
1000.038493	47580.175216	34.493082
1000.543720	47637.963821	34.498100
1001.448673	47689.584987	34.503117
1002.971029	47741.887755	34.508135
1003.516913	47797.880020	34.513152
1005.166672	47855.401410	34.518170
1005.858514	47912.573134	34.523188
1006.629683	47963.222610	34.528205
1007.442231	48015.352452	34.533223
1008.566512	48075.746669	34.538240
1009.684477	48127.727725	34.543258
1010.711247	48190.212621	34.548276
1011.922535	48249.821838	34.553293
1012.942937	48298.421186	34.558311
1013.841931	48355.631183	34.563328
1015.066627	48412.961148	34.568346
1015.989334	48473.476555	34.573364
1016.981372	48522.548995	34.578381
1017.910281	48578.413616	34.583399
1018.997339	48630.862510	34.588416
1020.226230	48679.006141	34.593434
1020.893925	48735.589002	34.598452
1021.987140	48786.499898	34.603469
1023.246936	48842.496836	34.608487
1023.589151	48896.796487	34.613504
1024.917915	48940.376094	34.618522
1025.966530	48981.253822	34.623540
1026.881394	49029.194288	34.628557
1028.083321	49068.188090	34.633575
1028.476230	49127.276072	34.638592
1029.555996	49179.385721	34.643610
1030.564515	49235.606443	34.648628
1031.741098	49283.645658	34.653645
1032.722470	49333.151739	34.658663
1033.433097	49401.092607	34.663680
1034.630346	49452.963043	34.668698
1035.540510	49514.685286	34.673716
1036.474500	49573.892166	34.678733
1038.034816	49630.343814	34.683751
1038.944837	49693.673609	34.688768
1039.861282	49749.321600	34.693786
1041.508714	49810.827977	34.698804
1042.282853	49870.440271	34.703821
1043.206091	49919.412596	34.708839
1044.491711	49977.338019	34.713856
1045.729823	50049.057724	34.718874
1046.933621	50094.430680	34.723892
1047.456431	50149.546524	34.728909
1048.694596	50204.436612	34.733927
1049.738030	50269.689533	34.738944
1050.908672	50323.394648	34.743962
1051.717048	50385.533777	34.748980
1053.138374	50440.383098	34.753997
1054.254800	50499.829544	34.759015
1055.264271	50567.733397	34.764032
1056.408489	50615.894361	34.769050
1057.613049	50666.754039	34.774068
1058.670323	50717.320527	34.779085
1059.583349	50780.425062	34.784103
1060.332805	50831.090610	34.789120
1061.670890	50890.920961	34.794138
1062.744258	50951.469937	34.799156
1063.631533	51011.953296	34.804173
1065.405804	51071.658880	34.809191
1065.885700	51132.750489	34.814208
1067.076767	51183.632402	34.819226
1068.336795	51245.772736	34.824244
1069.244690	51300.318516	34.829261
1070.222280	51360.782320	34.834279
1070.920066	51421.587479	34.839296
1072.151967	51488.446821	34.844314
1073.529802	51550.620149	34.849332
1074.220824	51607.782222	34.854349
1076.117921	51658.472385	34.859367
1076.828788	51724.971058	34.864384
1077.932048	51789.959476	34.869402
1079.203313	51837.938581	34.874420
1080.060792	51899.700763	34.879437
1081.278646	51957.369680	34.884455
1082.571723	52012.065641	34.889472
1083.547199	52063.995659	34.894490
1084.738303	52111.582912	34.899508
1085.918545	52172.738455	34.904525
1087.218047	52224.105562	34.909543
1088.203406	52270.934394	34.914560
1089.227137	52332.602093	34.919578
1090.529335	52369.592569	34.924596
1091.142440	52429.660625	34.929613
1092.527946	52475.471735	34.934631
1093.468259	52535.488836	34.939648
1094.377584	52589.132550	34.944666
1095.773684	52627.988084	34.949684
1096.778126	52679.731437	34.954701
1097.594012	52729.821227	34.959719
1098.477347	52772.712162	34.964736
1099.505507	52814.884440	34.969754
1100.703805	52862.465775	34.974772
1101.364913	52915.161956	34.979789
1102.476167	52962.725484	34.984807
1102.971340	53026.559637	34.989824
1104.581833	53087.346483	34.994842
1106.103574	53132.612342	34.999860
1106.495263	53192.324691	35.004877
1107.973303	53242.470114	35.009895
1108.656905	53320.741257	35.014912
1109.871944	53378.382493	35.019930
1110.970196	53432.270667	35.024948
1112.162177	53498.648446	35.029965
1113.131861	53556.872742	35.034983
1114.396103	53632.257031	35.040000
1115.628341	53702.868880	35.045018
1117.178445	53764.249122	35.050036
1117.966617	53823.502334	35.055053
1119.387722	53878.904031	35.060071
1120.364006	53931.742996	35.065088
1121.237801	54014.561914	35.070106
1122.848016	54069.757267	35.075124
1123.761481	54134.750282	35.080141
1125.380359	54187.710706	35.085159
1126.383492	54251.411708	35.090176
1127.957286	54319.763390	35.095194
1129.004338	54374.345191	35.100212
1129.752876	54435.561578	35.105229
1130.982921	54484.957451	35.110247
1132.528989	54543.473650	35.115264
1133.971581	54596.108209	35.120282
1135.453296	54638.889893	35.125300
1136.415101	54692.897244	35.130317
1137.858735	54741.355265	35.135335
1138.972743	54793.718962	35.140352
1140.184390	54827.132996	35.145370
1141.323340	54879.954952	35.150388
1142.065710	54927.801706	35.155405
1143.220502	54979.064617	35.160423
1144.348302	55035.730013	35.165440
1145.215164	55087.481226	35.170458
1146.347915	55135.988728	35.175476
1147.058855	55212.762029	35.180493
1148.123738	55264.140889	35.185511
1149.240825	55327.668742	35.190528
1150.094408	55398.281663	35.195546
1151.690050	55454.286265	35.200564
1152.426396	55516.412337	35.205581
1154.026309	55580.257649	35.210599
1155.060838	55651.564453	35.215616
1156.165337	55716.266106	35.220634
1157.477508	55772.910729	35.225652
1158.665452	55842.776477	35.230669
1159.575163	55899.705911	35.235687
1160.554891	55965.845396	35.240704
1161.751524	56033.425692	35.245722
1163.465705	56097.260835	35.250740
1164.325627	56163.925922	35.255757
1165.465497	56233.686427	35.260775
1166.478614	56282.569411	35.265792
1167.954924	56352.999073	35.270810
1169.079988	56414.136303	35.275828
1170.196878	56479.591217	35.280845
1171.454752	56540.935817	35.285863
1172.565732	56595.873469	35.290880
1173.420098	56644.054231	35.295898
1174.745838	56707.774613	35.300916
1175.803395	56758.195860	35.305933
1176.964970	56816.081686	35.310951
1178.008816	56876.315124	35.315968
1179.519924	56929.798542	35.320986
1180.176655	56984.915793	35.326004
1181.633001	57039.566227	35.331021
1182.431581	57098.750040	35.336039
1183.924095	57149.490087	35.341056
1184.786936	57224.265107	35.346074
1186.016392	57276.825057	35.351092
1186.978937	57352.224098	35.356109
1188.367645	57408.480881	35.361127
1189.779459	57476.613846	35.366144
1191.036604	57541.391483	35.371162
1192.080483	57595.690038	35.376180
1193.215340	57678.816282	35.381197
1194.496028	57743.869261	35.386215
1195.332049	57805.707195	35.391232
1196.883248	57879.933451	35.396250
1198.317117	57950.969401	35.401268
1199.491493	58010.191566	35.406285
1200.630575	58069.039648	35.411303
1201.773366	58135.969739	35.416320
1202.913001	58210.084224	35.421338
1204.564530	58272.188102	35.426356
1205.730771	58352.058505	35.431373
1207.300516	58407.428500	35.436391
1208.667048	58462.729167	35.441408
1209.902175	58535.222051	35.446426
1210.900721	58594.783316	35.451444
1212.146931	58655.894631	35.456461
1213.622896	58715.666277	35.461479
1215.185386	58771.474973	35.466496
1216.826847	58836.284540	35.471514
1217.887708	58881.418323	35.476532
1219.051289	58950.853876	35.481549
1220.266703	58997.514398	35.486567
1221.528344	59042.939853	35.491584
1222.651551	59098.090182	35.496602
1223.955200	59146.863890	35.501620
1224.895613	59198.504868	35.506637
1226.038912	59266.425415	35.511655
1227.595286	59317.027117	35.516672
1228.619518	59381.757543	35.521690
1230.154954	59439.856992	35.526708
1230.995331	59495.444935	35.531725
1232.310427	59550.692846	35.536743
1233.766171	59611.628190	35.541760
1234.441502	59678.534451	35.546778
1236.036678	59735.131458	35.551796
1236.943710	59790.836234	35.556813
1238.157293	59849.987139	35.561831
1239.362906	59911.753603	35.566848
1240.699768	59985.108394	35.571866
1241.695493	60050.199525	35.576884
1243.071262	60121.928223	35.581901
1244.024012	60183.070334	35.586919
1245.841078	60243.083517	35.591936
1246.813095	60303.583605	35.596954
1247.873708	60358.145259	35.601972
1248.851066	60435.089722	35.606989
1250.227889	60501.369375	35.612007
1251.539397	60567.064424	35.617024
1252.748036	60642.739009	35.622042
1254.097660	60706.244651	35.627060
1255.203571	60767.104719	35.632077
1256.472931	60819.058442	35.637095
1257.680907	60881.061196	35.642112
1258.642752	60944.811730	35.647130
1259.913447	60996.721311	35.652148
1260.924759	61064.401664	35.657165
1262.472401	61122.262673	35.662183
1263.598866	61184.709396	35.667200
1264.607792	61251.175271	35.672218
1265.845055	61317.099175	35.677236
1266.954624	61378.954010	35.682253
1268.179360	61455.761666	35.687271
1269.417203	61519.280582	35.692288
1270.719861	61591.316212	35.697306
1271.985836	61657.989822	35.702324
1273.730898	61739.027748	35.707341
1274.850328	61814.384406	35.712359
1276.608510	61883.437692	35.717376
1277.567310	61960.782310	35.722394
1278.724849	62017.630354	35.727412
1280.332011	62091.430230	35.732429
1281.393085	62160.928923	35.737447
1283.001567	62233.855439	35.742464
1284.112661	62303.612576	35.747482
1285.460575	62378.289495	35.752500
1286.629751	62445.094330	35.757517
1288.043908	62519.438456	35.762535
1289.706044	62591.895512	35.767552
1290.949747	62663.766248	35.772570
1292.264026	62741.253900	35.777588
1293.596374	62797.253416	35.782605
1294.737200	62878.250394	35.787623
1296.569039	62935.482439	35.792640
1297.947907	63016.854089	35.797658
1299.482302	63074.683771	35.802676
1300.623404	63140.994765	35.807693
1301.843859	63203.982635	35.812711
1303.709587	63258.988100	35.817728
1304.906945	63320.004743	35.822746
1305.960304	63389.710666	35.827764
1307.616392	63442.717233	35.832781
1308.862294	63517.736410	35.837799
1310.175967	63569.992860	35.842816
1311.001296	63633.562782	35.847834
1312.403100	63695.092778	35.852852
1314.112343	63763.272673	35.857869
1315.676400	63825.733528	35.862887
1317.181985	63872.592131	35.867904
1318.359405	63940.077082	35.872922
1319.624516	63997.476259	35.877940
1320.937574	64054.982016	35.882957
1322.151654	64106.438512	35.887975
1323.621762	64173.561737	35.892992
1324.914291	64238.174285	35.898010
1325.970942	64296.777981	35.903028
1327.505191	64347.589758	35.908045
1328.781922	64413.287805	35.913063
1330.292282	64467.155037	35.918080
1331.493119	64529.288327	35.923098
1332.648490	64587.237831	35.928116
1334.174424	64651.770593	35.933133
1335.028586	64717.712850	35.938151
1336.399005	64775.204953	35.943168
1337.766694	64852.380585	35.948186
1338.858401	64911.176490	35.953204
1340.612722	64974.465115	35.958221
1341.917682	65040.698520	35.963239
1343.512344	65092.325384	35.968256
1344.583466	65159.209816	35.973274
1345.952166	65207.358558	35.978292
1347.146024	65260.827535	35.983309
1348.097790	65309.465919	35.988327
1349.327577	65355.674054	35.993344
1350.431416	65424.776283	35.998362
1351.561098	65489.556827	36.003380
1353.374475	65543.872768	36.008397
1354.499106	65606.305549	36.013415
1355.904676	65655.759928	36.018432
1357.540677	65725.241854	36.023450
1358.244060	65775.667425	36.028468
1359.777289	65846.672598	36.033485
1361.150121	65920.349534	36.038503
1362.445194	65985.535985	36.043520
1363.795187	66064.028666	36.048538
1365.074167	66130.870472	36.053556
1367.032512	66188.685306	36.058573
1367.971296	66265.634828	36.063591
1369.639306	66331.143672	36.068608
1371.442160	66405.976657	36.073626
1372.377527	66468.707109	36.078644
1373.990892	66530.780757	36.083661
1375.055265	66608.053553	36.088679
1376.747707	66669.595988	36.093696
1378.292544	66742.646905	36.098714
1379.608575	66810.491401	36.103732
1381.147932	66877.326074	36.108749
1382.368186	66953.777754	36.113767
1384.142167	67017.701573	36.118784
1385.813368	67081.837919	36.123802
1387.109693	67131.932772	36.128820
1388.241650	67189.144787	36.133837
1389.754556	67263.804081	36.138855
1391.308116	67322.197720	36.143872
1392.631092	67394.411478	36.148890
1394.135154	67462.285262	36.153908
1395.871840	67520.922952	36.158925
1397.229771	67586.584875	36.163943
1398.435274	67644.514539	36.168960
1399.930358	67702.012774	36.173978
1401.349376	67779.904766	36.178996
1402.778756	67826.326768	36.184013
1404.097170	67896.624152	36.189031
1405.477935	67964.531234	36.194048
1406.836573	68041.401398	36.199066
1408.394712	68105.545352	36.204084
1409.914463	68170.702229	36.209101
1411.143007	68233.087201	36.214119
1412.116672	68292.808531	36.219136
1413.793912	68370.750544	36.224154
1414.640742	68436.557966	36.229172
1416.267295	68497.925171	36.234189
1417.742166	68572.866507	36.239207
1419.262660	68641.418357	36.244224
1420.548917	68720.701677	36.249242
1421.772838	68795.049747	36.254260
1423.656437	68857.491999	36.259277
1425.144510	68919.059180	36.264295
1426.940374	68994.249102	36.269312
1428.250665	69061.739539	36.274330
1429.495376	69127.334477	36.279348
1431.217405	69187.485298	36.284365
1432.421700	69254.707889	36.289383
1433.836139	69321.555829	36.294400
1435.678608	69374.324034	36.299418
1436.846686	69452.450331	36.304436
1438.532666	69497.828388	36.309453
1439.937691	69556.459324	36.314471
1441.448033	69609.482625	36.319488
1442.857357	69664.294850	36.324506
1443.650789	69720.438367	36.329524
1444.571441	69771.084752	36.334541
1446.261505	69833.407689	36.339559
1447.231335	69881.767002	36.344576
1448.856761	69942.479273	36.349594
1449.945233	70014.154523	36.354612
1451.068023	70074.489856	36.359629
1452.730544	70147.646021	36.364647
1453.883447	70224.453573	36.369664
1455.905938	70305.621183	36.374682
1457.155790	70376.360318	36.379700
1458.975985	70435.776792	36.384717
1460.396500	70516.697337	36.389735
1461.627656	70593.443070	36.394752
1462.981732	70666.433673	36.399770
1464.490285	70738.893707	36.404788
1466.415897	70818.051705	36.409805
1467.941048	70888.381858	36.414823
1469.678001	70966.733953	36.419840
1471.086846	71031.953395	36.424858
1472.330049	71115.753170	36.429876
1473.710032	71181.876719	36.434893
1475.374499	71266.598915	36.439911
1476.940954	71337.164447	36.444928
1478.496398	71409.099730	36.449946
1479.953690	71479.644737	36.454964
1481.398169	71552.142385	36.459981
1483.079401	71634.051464	36.464999
1484.681136	71711.287079	36.470016
1486.293919	71775.070602	36.475034
1487.667190	71854.812139	36.480052
1489.039037	71924.928429	36.485069
1490.599469	72006.464950	36.490087
1491.884014	72084.511235	36.495104
1493.718916	72150.907991	36.500122
1495.575771	72231.588221	36.505140
1496.759558	72306.155241	36.510157
1498.280192	72389.864994	36.515175
1499.864296	72463.837845	36.520192
1501.596586	72539.586240	36.525210
1503.267355	72610.886142	36.530228
1504.252886	72673.212133	36.535245
1506.182850	72749.614143	36.540263
1507.385444	72831.500536	36.545280
1509.181622	72895.498721	36.550298
1510.458768	72981.262331	36.555316
1512.163825	73044.882496	36.560333
1513.753381	73115.499844	36.565351
1515.335302	73186.333898	36.570368
1517.174336	73256.963240	36.575386
1518.421110	73333.347206	36.580404
1519.943516	73399.631356	36.585421
1521.721432	73472.804062	36.590439
1523.104927	73540.782238	36.595456
1524.775412	73606.549748	36.600474
1526.328396	73666.927327	36.605492
1527.846794	73731.870314	36.610509
1529.426216	73804.479687	36.615527
1530.908036	73870.239379	36.620544
1532.525343	73935.636037	36.625562
1533.869826	74002.937517	36.630580
1535.508950	74063.961169	36.635597
1536.794765	74129.283521	36.640615
1537.990230	74201.244749	36.645632
1539.637037	74264.205630	36.650650
1541.141103	74340.780214	36.655668
1542.658513	74390.689762	36.660685
1544.050262	74446.331711	36.665703
1545.527216	74514.285078	36.670720
1547.106784	74562.753889	36.675738
1547.979092	74639.529541	36.680756
1549.473731	74706.644626	36.685773
1551.167051	74775.882133	36.690791
1552.731940	74843.024566	36.695808
1554.585973	74896.416410	36.700826
1555.629169	74971.050905	36.705844
1557.364205	75042.283935	36.710861
1558.823730	75115.992325	36.715879
1560.125476	75201.467882	36.720896
1562.215804	75262.043643	36.725914
1563.588030	75343.645190	36.730932
1565.131990	75418.797903	36.735949
1566.465585	75490.221622	36.740967
1568.038466	75578.252695	36.745984
1569.874729	75651.523574	36.751002
1571.341140	75726.296600	36.756020
1573.124012	75810.736082	36.761037
1575.202178	75890.303375	36.766055
1576.323531	75976.924346	36.771072
1577.864709	76042.325394	36.776090
1579.425806	76138.593922	36.781108
1581.187963	76212.029931	36.786125
1582.736734	76297.229616	36.791143
1584.417430	76384.955092	36.796160
1586.231187	76452.252600	36.801178
1587.872327	76536.399841	36.806196
1589.388502	76611.040849	36.811213
1591.382766	76689.369531	36.816231
1592.703301	76778.216732	36.821248
1594.325225	76849.180879	36.826266
1596.207745	76943.780490	36.831284
1597.627410	77018.045020	36.836301
1599.792430	77083.034248	36.841319
1601.032967	77161.735614	36.846336
1603.036017	77233.071823	36.851354
1604.665171	77308.279788	36.856372
1606.076055	77387.727891	36.861389
1608.102691	77455.957337	36.866407
1609.151008	77533.423059	36.871424
1611.094964	77598.106080	36.876442
1612.653124	77670.602518	36.881460
1614.078373	77749.454024	36.886477
1615.782510	77820.141804	36.891495
1617.412309	77900.735278	36.896512
1618.870866	77973.387458	36.901530
1620.797882	78053.605492	36.906548
1622.329259	78133.695655	36.911565
1624.163483	78204.718783	36.916583
1625.358548	78291.044200	36.921600
1627.311104	78366.432493	36.926618
1628.932120	78444.520591	36.931636
1630.636703	78520.606877	36.936653
1632.068050	78592.694874	36.941671
1633.512822	78662.956684	36.946688
1635.110932	78744.279704	36.951706
1636.913942	78820.199392	36.956724
1638.225692	78903.087934	36.961741
1640.116290	78979.349076	36.966759
1641.419486	79071.626982	36.971776
1643.067344	79141.959580	36.976794
1644.889102	79224.933965	36.981812
1646.538586	79308.885725	36.986829
1648.370681	79381.166442	36.991847
1649.968132	79452.407212	36.996864
1651.638690	79508.091911	37.001882
1652.767092	79586.665747	37.006900
1654.051894	79648.644245	37.011917
1656.054535	79706.342423	37.016935
1657.653167	79785.692056	37.021952
1659.141099	79849.767621	37.026970
1660.657613	79923.100003	37.031988
1662.090793	79997.560509	37.037005
1663.816158	80071.886803	37.042023
1665.155818	80162.693006	37.047040
1666.868893	80244.407860	37.052058
1668.722684	80320.665791	37.057076
1670.112345	80408.981784	37.062093
1671.813360	80498.947030	37.067111
1673.360961	80586.618068	37.072128
1675.214637	80680.474866	37.077146
1677.098093	80767.409758	37.082164
1678.429393	80850.972541	37.087181
1680.909854	80950.002693	37.092199
1681.974619	81039.765184	37.097216
1683.857700	81124.560074	37.102234
1685.404822	81209.927258	37.107252
1686.927509	81295.894005	37.112269
1689.118966	81397.048810	37.117287
1690.805522	81493.405103	37.122304
1692.817161	81576.534161	37.127322
1694.726060	81670.702384	37.132340
1696.599793	81755.893415	37.137357
1698.418974	81838.103119	37.142375
1700.073614	81925.140762	37.147392
1702.240971	82007.942646	37.152410
1703.865513	82087.535493	37.157428
1705.290219	82174.394498	37.162445
1707.427408	82251.664961	37.167463
1708.837687	82343.708855	37.172480
1710.335008	82423.411251	37.177498
1712.228095	82502.532452	37.182516
1714.069741	82601.338972	37.187533
1715.900420	82670.359472	37.192551
1717.757139	82759.788107	37.197568
1719.372322	82845.415675	37.202586
1721.394643	82928.889153	37.207604
1722.678026	83013.568185	37.212621
1724.534875	83086.044660	37.217639
1726.023163	83170.679423	37.222656
1728.303561	83256.115432	37.227674
1729.905887	83338.300085	37.232692
1731.925882	83417.581371	37.237709
1733.660922	83496.197912	37.242727
1735.973424	83576.257464	37.247744
1737.429768	83657.236818	37.252762
1739.274909	83730.540374	37.257780
1740.621940	83808.927070	37.262797
1742.151982	83874.994550	37.267815
1743.952951	83956.072871	37.272832
1745.961549	84047.648522	37.277850
1747.343226	84131.453866	37.282868
1749.220622	84216.347617	37.287885
1751.089737	84289.800911	37.292903
1752.669499	84367.443135	37.297920
1754.037157	84459.107736	37.302938
1756.163262	84529.391648	37.307956
1757.963654	84623.523295	37.312973
1759.259789	84697.409426	37.317991
1760.997963	84785.760567	37.323008
1762.819409	84867.205733	37.328026
1764.509616	84957.516298	37.333044
1766.128993	85041.122372	37.338061
1768.003161	85112.118724	37.343079
1769.539922	85180.266283	37.348096
1771.166330	85252.480203	37.353114
1773.212669	85323.475477	37.358132
1774.338377	85407.540017	37.363149
1776.204220	85477.220727	37.368167
1777.882957	85552.303668	37.373184
1779.550724	85624.765481	37.378202
1781.381324	85719.732315	37.383220
1782.449913	85806.822824	37.388237
1784.660405	85886.676705	37.393255
1786.662595	85978.943787	37.398272
1788.272932	86071.500579	37.403290
1790.038941	86153.008737	37.408308
1791.607471	86264.517204	37.413325
1793.271523	86369.662474	37.418343
1795.429127	86460.183373	37.423360
1796.687372	86546.486096	37.428378
1798.957097	86649.269291	37.433396
1800.373134	86754.404073	37.438413
1802.711851	86859.939749	37.443431
1804.474194	86952.488227	37.448448
1806.589482	87055.829258	37.453466
1808.345899	87154.690113	37.458484
1810.471938	87256.458800	37.463501
1812.479535	87352.239642	37.468519
1814.139143	87453.676488	37.473536
1816.030542	87550.223837	37.478554
1818.374723	87632.253933	37.483572
1819.884493	87736.604547	37.488589
1821.602163	87810.065126	37.493607
1823.920550	87910.589412	37.498624
1825.450705	88020.425112	37.503642
1827.773993	88107.351478	37.508660
1829.746804	88198.400913	37.513677
1831.762949	88283.082086	37.518695
1833.703162	88377.698244	37.523712
1835.094271	88476.227853	37.528730
1837.011017	88554.842361	37.533748
1838.837314	88653.862072	37.538765
1840.588455	88755.213040	37.543783
1842.539840	88849.233326	37.548800
1844.213316	88932.069022	37.553818
1846.326764	89020.513671	37.558836
1848.099257	89121.152854	37.563853
1850.210923	89217.126245	37.568871
1852.060224	89311.810309	37.573888
1853.336313	89408.029131	37.578906
1855.634192	89504.126391	37.583924
1857.454012	89593.569197	37.588941
1858.871334	89699.563394	37.593959
1860.893832	89785.502540	37.598976
1863.095569	89892.794104	37.603994
1864.586371	89984.406048	37.609012
1866.358522	90083.895244	37.614029
1868.246272	90178.804171	37.619047
1870.314397	90268.628376	37.624064
1871.622740	90380.421237	37.629082
1873.671348	90476.117054	37.634100
1875.684252	90577.661389	37.639117
1877.604785	90671.920385	37.644135
1879.886784	90774.006274	37.649152
1881.407034	90885.957965	37.654170
1883.130552	90978.994034	37.659188
1885.313375	91080.145933	37.664205
1887.179431	91172.615314	37.669223
1889.162674	91261.669983	37.674240
1890.513276	91354.803589	37.679258
1892.444644	91429.836609	37.684276
1894.039770	91516.975596	37.689293
1895.871870	91605.002971	37.694311
1897.905841	91689.462891	37.699328
1899.947961	91768.890073	37.704346
1901.595124	91852.219591	37.709364
1903.752479	91945.140055	37.714381
1905.239951	92037.544580	37.719399
1906.954115	92134.590790	37.724416
1909.006232	92231.330936	37.729434
1911.042040	92321.014226	37.734452
1912.541920	92418.500458	37.739469
1914.508959	92512.833970	37.744487
1916.622563	92605.902725	37.749504
1918.117554	92722.744900	37.754522
1920.090299	92831.679768	37.759540
1922.032665	92934.497854	37.764557
1924.397591	93030.177609	37.769575
1926.316414	93143.469494	37.774592
1927.948654	93245.855510	37.779610
1929.971471	93362.769636	37.784628
1932.114871	93472.985607	37.789645
1933.999191	93588.515339	37.794663
1935.972784	93691.318405	37.799680
1937.747293	93807.221045	37.804698
1939.471283	93910.646958	37.809716
1941.733069	94031.252742	37.814733
1943.610187	94151.437528	37.819751
1945.673187	94263.430778	37.824768
1947.531656	94370.905977	37.829786
1949.825504	94484.993373	37.834804
1951.983648	94607.164027	37.839821
1953.902672	94721.450376	37.844839
1956.531039	94819.490155	37.849856
1958.036139	94934.856105	37.854874
1959.876632	95038.787264	37.859892
1961.695715	95160.962452	37.864909
1963.853566	95274.478277	37.869927
1966.167326	95383.660351	37.874944
1968.095312	95491.090526	37.879962
1970.140608	95595.815429	37.884980
1972.202645	95712.440758	37.889997
1974.326581	95826.217419	37.895015
1976.254651	95933.636429	37.900032
1978.110791	96053.679746	37.905050
1979.998821	96158.342410	37.910068
1982.023165	96262.895362	37.915085
1983.733690	96373.290787	37.920103
1985.916170	96493.297400	37.925120
1987.798391	96616.203619	37.930138
1989.744945	96723.622443	37.935156
1991.918837	96841.071108	37.940173
1993.076219	96971.812047	37.945191
1995.473904	97081.810879	37.950208
1997.581329	97206.649017	37.955226
1999.576482	97331.505215	37.960244
2001.685177	97445.683097	37.965261
2003.493729	97557.727968	37.970279
2005.756548	97682.467609	37.975296
2008.077171	97805.233797	37.980314
2010.104717	97913.886318	37.985332
2011.814163	98022.170647	37.990349
2013.427928	98145.200873	37.995367
2016.203120	98265.134148	38.000384
2017.669061	98384.575497	38.005402
2019.634418	98497.296379	38.010420
2021.780677	98608.468104	38.015437
2023.550382	98733.783429	38.020455
2025.825308	98824.829845	38.025472
2027.699009	98924.496415	38.030490
2028.942370	99030.562518	38.035508
2031.217692	99127.415916	38.040525
2032.877851	99237.017836	38.045543
2034.851222	99338.330829	38.050560
2037.072810	99459.420106	38.055578
2038.701906	99566.885527	38.060596
2040.772438	99701.196592	38.065613
2042.580618	99820.310831	38.070631
2044.552619	99942.696056	38.075648
2046.190528	100077.583481	38.080666
2048.324787	100205.547841	38.085684
2050.365647	100327.695549	38.090701
2052.434566	100474.979432	38.095719
2054.266192	100618.256868	38.100736
2056.094984	100756.438852	38.105754
2058.530542	100900.193543	38.110772
2060.369839	101040.340176	38.115789
2062.185081	101199.254755	38.120807
2064.023122	101345.868727	38.125824
2066.597234	101497.401437	38.130842
2068.587346	101656.620511	38.135860
2070.547461	101814.526504	38.140877
2072.339478	101974.285247	38.145895
2075.020302	102131.648934	38.150912
2076.998305	102291.925292	38.155930
2079.079309	102449.295598	38.160948
2081.488438	102608.022643	38.165965
2083.353407	102765.948083	38.170983
2085.446262	102921.784661	38.176000
2087.572645	103089.243207	38.181018
2089.925671	103241.997666	38.186036
2092.365387	103406.784261	38.191053
2094.034342	103565.492231	38.196071
2096.355943	103716.009601	38.201088
2098.749856	103875.341004	38.206106
2101.375009	104027.663439	38.211124
2103.883390	104173.792011	38.216141
2105.975171	104325.299028	38.221159
2108.232114	104458.928367	38.226176
2110.747617	104612.589272	38.231194
2112.805714	104755.126485	38.236212
2114.826862	104885.180768	38.241229
2116.911266	105038.277094	38.246247
2119.350730	105176.141061	38.251264
2121.306228	105325.708568	38.256282
2123.406215	105465.059632	38.261300
2125.427222	105611.600380	38.266317
2127.105101	105757.777013	38.271335
2129.183812	105906.960094	38.276352
2131.571253	106056.691484	38.281370
2133.499170	106219.746031	38.286388
2135.526501	106361.191663	38.291405
2137.338096	106535.272208	38.296423
2139.329402	106675.811811	38.301440
2140.851447	106834.837101	38.306458
2143.446019	107005.779643	38.311476
2145.752603	107160.689407	38.316493
2147.698196	107326.700986	38.321511
2149.811018	107497.125368	38.326528
2151.809480	107655.154242	38.331546
2153.775391	107828.190074	38.336564
2156.226743	108002.824670	38.341581
2158.455891	108156.013774	38.346599
2160.693123	108319.017210	38.351616
2162.575404	108484.879410	38.356634
2163.955830	108653.483908	38.361652
2166.635949	108813.858833	38.366669
2168.363742	108969.399855	38.371687
2170.411578	109106.859024	38.376704
2172.694559	109259.461239	38.381722
2174.953125	109412.105984	38.386740
2177.497013	109562.119784	38.391757
2179.351245	109716.972245	38.396775
2181.458058	109875.019612	38.401792
2183.474048	110026.297354	38.406810
2185.756126	110196.568974	38.411828
2187.727943	110347.233613	38.416845
2189.876560	110524.730795	38.421863
2192.137845	110689.618378	38.426880
2194.611005	110853.573181	38.431898
2196.773880	111026.479876	38.436916
2198.733645	111188.500150	38.441933
2200.860888	111368.351033	38.446951
2203.335696	111534.413912	38.451968
2205.237746	111712.133150	38.456986
2207.125488	111888.244888	38.462004
2209.026207	112080.804175	38.467021
2211.584943	112274.187348	38.472039
2213.583557	112453.049232	38.477056
2215.926935	112654.457966	38.482074
2218.102373	112859.774913	38.487092
2220.495561	113044.678235	38.492109
2222.746421	113231.113991	38.497127
2225.113377	113428.820053	38.502144
2227.570189	113618.941583	38.507162
2229.464079	113817.776434	38.512180
2232.233121	114000.951706	38.517197
2234.189769	114212.715347	38.522215
2236.760107	114402.138326	38.527232
2238.802269	114594.726887	38.532250
2241.180055	114794.505985	38.537268
2243.750051	114979.175847	38.542285
2246.038470	115176.637305	38.547303
2248.096262	115368.859661	38.552320
2250.622674	115565.639119	38.557338
2252.861097	115766.396535	38.562356
2255.877078	115945.395393	38.567373
2257.830261	116141.646099	38.572391
2259.936988	116337.429893	38.577408
2262.946962	116524.765606	38.582426
2264.859314	116720.226675	38.587444
2267.395411	116896.768437	38.592461
2269.417338	117095.004753	38.597479
2271.739457	117277.124627	38.602496
2274.072151	117457.176241	38.607514
2276.213548	117641.482427	38.612532
2278.785100	117828.271723	38.617549
2280.642742	118015.401944	38.622567
2283.225119	118216.549940	38.627584
2285.243998	118412.992495	38.632602
2287.002840	118617.937215	38.637620
2289.161479	118797.451635	38.642637
2291.745960	118988.126049	38.647655
2293.695136	119206.515081	38.652672
2295.667230	119411.976134	38.657690
2297.842883	119628.581660	38.662708
2300.014723	119826.478970	38.667725
2302.527864	120045.938857	38.672743
2304.721929	120248.363341	38.677760
2306.839301	120457.168738	38.682778
2308.860682	120675.478685	38.687796
2311.085795	120895.533903	38.692813
2313.761201	121114.276771	38.697831
2315.588042	121327.343771	38.702848
2318.014650	121522.165410	38.707866
2320.185116	121726.719722	38.712884
2322.075327	121915.246483	38.717901
2324.106498	122131.596786	38.722919
2326.381169	122331.609214	38.727936
2328.952846	122539.783803	38.732954
2330.630912	122771.682026	38.737972
2332.759776	122981.425124	38.742989
2334.787465	123204.530675	38.748007
2336.791468	123440.009960	38.753024
2339.318988	123671.019378	38.758042
2341.726756	123911.030608	38.763060
2344.167421	124144.136859	38.768077
2346.309241	124387.528998	38.773095
2348.639660	124624.943226	38.778112
2350.822036	124876.007182	38.783130
2353.465635	125122.243118	38.788148
2356.054554	125370.620439	38.793165
2358.287886	125621.173569	38.798183
2360.490588	125868.142694	38.803200
2363.464552	126117.136720	38.808218
2365.666764	126380.779429	38.813236
2368.400449	126624.193846	38.818253
2371.001804	126872.324591	38.823271
2372.820709	127124.410727	38.828288
2375.876679	127373.742069	38.833306
2378.476819	127625.366482	38.838324
2380.660197	127872.502869	38.843341
2383.745027	128128.393554	38.848359
2385.863088	128373.881075	38.853376
2388.813850	128609.470371	38.858394
2391.164904	128854.226436	38.863412
2393.744367	129096.118839	38.868429
2396.286043	129337.498339	38.873447
2398.569532	129578.665847	38.878464
2401.462316	129808.129991	38.883482
2404.045682	130059.796950	38.888500
2406.415227	130298.227157	38.893517
2408.512430	130542.220620	38.898535
2411.163843	130768.327265	38.903552
2413.707359	131011.669918	38.908570
2415.976208	131258.723833	38.913588
2418.750046	131490.309152	38.918605
2421.183691	131712.546786	38.923623
2423.773120	131954.339564	38.928640
2426.685448	132166.658347	38.933658
2428.758272	132411.808127	38.938676
2431.100546	132651.283336	38.943693
2434.011894	132877.461805	38.948711
2435.877006	133112.332006	38.953728
2438.485855	133352.023103	38.958746
2440.443212	133589.457260	38.963764
2442.669151	133820.379254	38.968781
2445.047519	134059.843759	38.973799
2447.136855	134324.733150	38.978816
2449.765308	134570.962685	38.983834
2452.019454	134829.218169	38.988852
2454.264066	135080.624345	38.993869
2456.735215	135334.344038	38.998887
2458.991117	135598.770740	39.003904
2461.645467	135851.525645	39.008922
2463.981666	136119.089840	39.013940
2466.319420	136387.061433	39.018957
2468.587539	136628.143016	39.023975
2471.169182	136900.178275	39.028992
2473.305216	137162.272445	39.034010
2475.705771	137435.595497	39.039028
2477.732763	137690.780943	39.044045
2480.191870	137944.072807	39.049063
2482.516348	138206.955571	39.054080
2484.856605	138451.322137	39.059098
2486.943784	138705.805747	39.064116
2489.312540	138973.800118	39.069133
2491.771619	139235.233558	39.074151
2493.769096	139507.362699	39.079168
2496.055730	139775.260239	39.084186
2498.306944	140061.236479	39.089204
2500.097221	140343.555422	39.094221
2502.751292	140632.619388	39.099239
2505.022918	140925.552212	39.104256
2507.693686	141233.311011	39.109274
2510.002108	141548.882743	39.114292
2512.061731	141859.888518	39.119309
2514.692071	142167.304195	39.124327
2517.034653	142497.852474	39.129344
2519.501675	142814.245189	39.134362
2522.241841	143143.809129	39.139380
2524.827038	143475.975905	39.144397
2527.623608	143795.064726	39.149415
2529.662613	144136.434002	39.154432
2532.510545	144466.383266	39.159450
2535.072349	144807.510323	39.164468
2537.561891	145146.011028	39.169485
2540.756645	145465.835049	39.174503
2543.521872	145807.368528	39.179520
2546.429569	146127.317740	39.184538
2549.306895	146459.598013	39.189556
2551.696559	146798.163327	39.194573
2554.327873	147122.033136	39.199591
2557.133859	147442.196769	39.204608
2560.056806	147784.886339	39.209626
2562.771002	148105.182610	39.214644
2565.537006	148431.070281	39.219661
2568.512418	148755.695982	39.224679
2570.589169	149081.352742	39.229696
2573.156765	149407.582056	39.234714
2575.837249	149731.574385	39.239732
2578.364767	150057.547349	39.244749
2580.647682	150401.585080	39.249767
2583.103389	150736.179437	39.254784
2585.335490	151060.694099	39.259802
2588.400836	151400.960005	39.264820
2590.992349	151739.601175	39.269837
2593.967707	152069.451090	39.274855
2596.538863	152410.841382	39.279872
2599.209656	152734.941800	39.284890
2601.586663	153074.081600	39.289908
2604.291239	153425.180754	39.294925
2606.875908	153759.747716	39.299943
2609.173349	154100.543636	39.304960
2611.722349	154445.072430	39.309978
2614.207381	154785.056025	39.314996
2616.570680	155137.259988	39.320013
2619.663209	155488.260296	39.325031
2621.814027	155841.910839	39.330048
2624.491089	156187.965973	39.335066
2627.890738	156527.981684	39.340084
2630.428732	156867.296263	39.345101
2633.460915	157199.070901	39.350119
2635.763920	157548.442345	39.355136
2638.159107	157884.192356	39.360154
2641.375672	158234.745159	39.365172
2643.860437	158576.032735	39.370189
2646.350481	158919.822347	39.375207
2648.882529	159261.119035	39.380224
2651.272154	159597.057056	39.385242
2653.627071	159923.620407	39.390260
2655.905559	160260.125292	39.395277
2658.245133	160584.561650	39.400295
2660.270346	160919.078385	39.405312
2662.896527	161258.784294	39.410330
2665.328177	161599.411144	39.415348
2667.196989	161954.854993	39.420365
2669.677320	162316.083355	39.425383
2671.835441	162695.265443	39.430400
2674.304405	163076.749885	39.435418
2676.810011	163465.607259	39.440436
2678.951802	163851.616398	39.445453
2680.941272	164264.136021	39.450471
2683.022772	164673.761721	39.455488
2685.659488	165104.823516	39.460506
2688.107200	165528.312403	39.465524
2690.601817	165979.386268	39.470541
2693.239911	166413.973061	39.475559
2695.733014	166871.680649	39.480576
2698.722695	167318.254621	39.485594
2701.700968	167764.338029	39.490612
2704.658806	168221.918219	39.495629
2707.267124	168676.584886	39.500647
2710.170698	169137.125115	39.505664
2713.152198	169595.319780	39.510682
2716.216325	170045.238433	39.515700
2718.892964	170515.269615	39.520717
2722.421523	170968.308270	39.525735
2726.172062	171414.382077	39.530752
2729.110228	171857.461954	39.535770
2732.345475	172275.978692	39.540788
2734.835741	172719.603416	39.545805
2738.164340	173150.985820	39.550823
2741.027290	173591.433546	39.555840
2743.148634	174031.085461	39.560858
2746.287626	174475.278916	39.565876
2748.953184	174901.581041	39.570893
2751.754857	175334.873514	39.575911
2754.661174	175773.091534	39.580928
2757.267324	176218.749248	39.585946
2759.837867	176662.002223	39.590964
2762.589401	177112.670521	39.595981
2765.083290	177547.254394	39.600999
2767.751640	177999.718187	39.606016
2770.681509	178452.016460	39.611034
2773.503112	178915.458084	39.616052
2776.099895	179382.975521	39.621069
2778.359442	179839.220784	39.626087
2781.007209	180313.287711	39.631104
2783.803980	180775.549156	39.636122
2786.362153	181244.275959	39.641140
2788.903770	181725.376648	39.646157
2791.781604	182204.369954	39.651175
2794.725015	182677.158195	39.656192
2797.351703	183165.237459	39.661210
2800.138165	183670.285937	39.666228
2802.667375	184193.054850	39.671245
2805.615861	184676.849684	39.676263
2808.677283	185160.324392	39.681280
2811.427434	185646.415397	39.686298
2813.985872	186137.923338	39.691316
2816.669750	186640.513540	39.696333
2819.294257	187130.110827	39.701351
2822.174841	187626.223423	39.706368
2824.398762	188117.564220	39.711386
2827.827543	188629.241920	39.716404
2830.590414	189131.221695	39.721421
2833.328438	189625.739937	39.726439
2835.874783	190109.952381	39.731456
2838.045122	190591.711011	39.736474
2840.958140	191066.903739	39.741492
2843.747975	191544.835482	39.746509
2846.132795	192034.948570	39.751527
2849.267281	192524.539955	39.756544
2851.673811	193017.346014	39.761562
2854.829982	193512.322836	39.766580
2857.555913	194004.854142	39.771597
2860.565202	194500.619738	39.776615
2863.520104	195014.176568	39.781632
2866.416833	195511.462180	39.786650
2869.388549	196012.395672	39.791668
2872.642215	196533.303274	39.796685
2875.089657	197046.388158	39.801703
2877.904609	197556.648597	39.806720
2880.520553	198072.047684	39.811738
2883.528598	198591.857949	39.816756
2886.008138	199138.196085	39.821773
2889.032224	199660.801644	39.826791
2892.339189	200193.779553	39.831808
2894.764880	200736.143436	39.836826
2898.427132	201264.928680	39.841844
2901.077158	201807.311729	39.846861
2904.024810	202351.402688	39.851879
2906.748097	202890.576897	39.856896
2909.727803	203441.016759	39.861914
2912.617368	203985.299479	39.866932
2915.768033	204539.322970	39.871949
2918.810319	205084.626389	39.876967
2921.643413	205631.945416	39.881984
2924.713840	206193.174991	39.887002
2927.658568	206747.338245	39.892020
2930.786487	207311.787895	39.897037
2933.836388	207861.441103	39.902055
2937.026236	208419.380560	39.907072
2940.130254	208978.147625	39.912090
2943.074453	209540.802229	39.917108
2945.490802	210104.937782	39.922125
2948.125576	210672.241185	39.927143
2950.846410	211241.056485	39.932160
2953.867619	211829.666076	39.937178
2957.019395	212388.940652	39.942196
2959.879374	212985.198711	39.947213
2962.321249	213557.745385	39.952231
2965.668759	214141.532229	39.957248
2968.670481	214737.491661	39.962266
2971.546029	215321.201705	39.967284
2974.347347	215919.810822	39.972301
2977.286640	216509.863481	39.977319
2980.492596	217104.778131	39.982336
2983.447263	217693.788263	39.987354
2987.074041	218286.555328	39.992372
2989.944474	218885.411198	39.997389
2992.636278	219483.152377	40.002407
2995.843172	220071.515641	40.007424
2998.719343	220673.928676	40.012442
3001.566415	221266.058028	40.017460
3004.566972	221877.674029	40.022477
3007.406375	222475.775170	40.027495
3010.422574	223071.054454	40.032512
3012.887087	223689.969779	40.037530
3015.917593	224293.274839	40.042548
3019.286680	224906.155185	40.047565
3022.269052	225526.945894	40.052583
3025.037488	226139.056427	40.057600
3028.204848	226759.868899	40.062618
3031.325080	227357.850332	40.067636
3034.140658	227947.140218	40.072653
3036.589072	228533.794457	40.077671
3039.656883	229122.307668	40.082688
3042.436089	229717.750169	40.087706
3045.086634	230308.411039	40.092724
3047.636904	230912.170208	40.097741
3050.512120	231525.074289	40.102759
3053.071921	232149.865347	40.107776
3055.910569	232779.642110	40.112794
3058.588247	233415.413221	40.117812
3061.306747	234059.916058	40.122829
3063.598914	234717.567624	40.127847
3066.745313	235376.431001	40.132864
3069.840442	236048.511251	40.137882
3072.593585	236732.608910	40.142900
3075.697011	237417.819040	40.147917
3078.623905	238104.528778	40.152935
3082.410684	238796.945372	40.157952
3085.203307	239495.384027	40.162970
3088.045980	240186.725602	40.167988
3091.374202	240898.744013	40.173005
3094.663500	241613.179871	40.178023
3098.399670	242297.187003	40.183040
3102.000836	242998.639817	40.188058
3105.324670	243688.677088	40.193076
3108.968017	244403.303098	40.198093
3111.992393	245104.559981	40.203111
3115.065666	245797.576324	40.208128
3118.221144	246512.144265	40.213146
3121.797754	247207.032897	40.218164
3125.093660	247910.218628	40.223181
3128.169941	248610.692494	40.228199
3131.774156	249313.290994	40.233216
3135.155864	250009.393014	40.238234
3138.255551	250717.246541	40.243252
3141.150717	251413.850452	40.248269
3144.306632	252113.687312	40.253287
3147.563121	252820.084264	40.258304
3151.239146	253498.826105	40.263322
3155.442866	254187.287209	40.268340
3158.940268	254865.694852	40.273357
3161.581567	255563.385540	40.278375
3165.161118	256240.173207	40.283392
3168.323553	256931.272552	40.288410
3171.208333	257611.387645	40.293428
3174.162870	258313.662955	40.298445
3177.088367	259007.226424	40.303463
3180.276214	259706.993383	40.308480
3182.666554	260394.663392	40.313498
3185.549437	261103.359779	40.318516
3188.986213	261819.026320	40.323533
3191.858825	262539.780234	40.328551
3195.433676	263239.312536	40.333568
3198.439370	263970.399154	40.338586
3201.450321	264685.859343	40.343604
3204.807970	265403.114503	40.348621
3207.943779	266131.473197	40.353639
3211.256502	266855.404936	40.358656
3213.974362	267575.309783	40.363674
3217.230573	268314.300801	40.368692
3220.431462	269050.221531	40.373709
3223.608117	269786.064039	40.378727
3226.829310	270515.493448	40.383744
3230.094090	271252.580181	40.388762
3232.897029	271997.555360	40.393780
3236.212149	272733.250357	40.398797
3239.249136	273484.804773	40.403815
3242.749390	274211.975510	40.408832
3245.864499	274928.305063	40.413850
3249.313357	275633.376465	40.418868
3252.655011	276339.194969	40.423885
3255.742817	277051.370460	40.428903
3258.600032	277767.689632	40.433920
3261.390853	278479.568407	40.438938
3264.260983	279206.741366	40.443956
3267.192837	279945.274537	40.448973
3270.448228	280690.428562	40.453991
3273.245020	281430.720258	40.459008
3275.925391	282189.255495	40.464026
3279.558162	282958.756234	40.469044
3282.709492	283726.470148	40.474061
3285.095374	284504.071656	40.479079
3288.437404	285301.727600	40.484096
3291.596970	286091.531008	40.489114
3294.815600	286905.006849	40.494132
3298.160214	287702.202144	40.499149
3301.186517	288527.647571	40.504167
3304.401482	289350.539188	40.509184
3308.272123	290173.114514	40.514202
3311.153698	291006.700896	40.519220
3314.877760	291830.622992	40.524237
3318.179830	292663.232559	40.529255
3322.122311	293489.637032	40.534272
3326.148736	294316.981738	40.539290
3329.604898	295138.285286	40.544308
3333.401388	295965.033367	40.549325
3336.957681	296779.366949	40.554343
3340.691143	297599.449609	40.559360
3344.802755	298422.431535	40.564378
3348.061891	299241.142626	40.569396
3351.803652	300039.862943	40.574413
3355.294556	300858.742105	40.579431
3358.432079	301649.764964	40.584448
3362.047950	302458.090395	40.589466
3365.297959	303292.201173	40.594484
3368.858733	304090.990655	40.599501
3372.166672	304914.709355	40.604519
3375.491420	305724.933301	40.609536
3378.760554	306539.544326	40.614554
3382.327499	307357.826867	40.619572
3385.275310	308182.233792	40.624589
3388.313999	309016.308696	40.629607
3391.430730	309840.508956	40.634624
3394.807071	310682.193051	40.639642
3398.304764	311523.944843	40.644660
3401.947933	312357.537138	40.649677
3405.104900	313203.499893	40.654695
3408.256377	314042.291026	40.659712
3411.796845	314897.299374	40.664730
3414.990341	315753.183373	40.669748
3418.343253	316606.082315	40.674765
3421.583236	317466.646638	40.679783
3424.690065	318330.082627	40.684800
3428.023940	319200.546158	40.689818
3431.303496	320081.481031	40.694836
3434.768150	320950.721509	40.699853
3437.981597	321826.682519	40.704871
3441.714320	322699.372334	40.709888
3445.087148	323583.036378	40.714906
3448.366877	324455.557179	40.719924
3452.064209	325336.823915	40.724941
3455.280349	326228.904663	40.729959
3458.816173	327110.716240	40.734976
3462.239578	327993.921355	40.739994
3465.389156	328888.997688	40.745012
3469.075072	329765.330169	40.750016
3472.147895	330614.495556	40.755021
3475.531043	331421.424423	40.760026
3478.552893	332174.753842	40.765031
3481.460130	332879.153401	40.770036
3484.581191	333517.127717	40.775040
3487.360717	334124.727867	40.780045
3490.297441	334675.352067	40.785050
3492.740795	335162.517785	40.790055
3495.715055	335599.850993	40.795060
3497.923432	335971.763653	40.800064
3500.126012	336315.191244	40.805069
3502.129968	336600.538348	40.810074
3504.028814	336851.009463	40.815079
3505.846983	337056.988930	40.820084
3507.548436	337222.501064	40.825088
3509.068741	337362.992395	40.830093
3509.988808	337457.320322	40.835098
3511.483815	337517.584035	40.840103
3512.948193	337555.372599	40.845108
3514.209373	337548.538378	40.850112
3515.150125	337527.386468	40.855117
3515.872129	337477.863733	40.860122
3516.655845	337404.376425	40.865127
3517.411920	337318.127506	40.870132
3518.091615	337200.560657	40.875136
3518.637640	337085.989638	40.880141
3519.353291	336931.415608	40.885146
3519.921798	336757.053772	40.890151
3519.943052	336591.016098	40.895156
3520.366834	336395.517099	40.900160
3521.186263	336197.412140	40.905165
3521.358760	335983.640172	40.910170
3521.538005	335749.394004	40.915175
3521.530258	335525.322590	40.920180
3521.668942	335287.570340	40.925184
3521.891809	335043.725292	40.930189
3522.274930	334792.580152	40.935194
3522.412474	334540.530733	40.940199
3522.416099	334284.990939	40.945204
3522.855331	334010.612386	40.950208
3522.794384	333744.626388	40.955213
3522.815187	333467.816914	40.960218
3523.028915	333187.287504	40.965223
3522.801095	332905.197335	40.970228
3522.956218	332617.119290	40.975232
3522.893784	332333.167826	40.980237
3522.869160	332053.862653	40.985242
3522.831162	331744.596692	40.990247
3522.668966	331470.853301	40.995252
3522.532099	331168.261809	41.000256
3522.343167	330877.324954	41.005261
3522.235418	330592.401171	41.010266
3522.499490	330294.063990	41.015271
3522.204050	330008.503954	41.020276
3522.004040	329715.296406	41.025280
3521.924516	329425.399826	41.030285
3521.828324	329129.577261	41.035290
3521.897409	328842.578203	41.040295
3521.535950	328568.667458	41.045300
3521.545175	328280.122080	41.050304
3521.436121	327984.725338	41.055309
3521.216985	327710.582912	41.060314
3520.953178	327414.112359	41.065319
3520.802856	327142.804151	41.070324
3520.946858	326859.518218	41.075328
3520.512441	326588.454163	41.080333
3520.697550	326295.364578	41.085338
3520.505303	326006.707086	41.090343
3520.175393	325731.652704	41.095348
3520.040528	325454.734448	41.100352
3519.714354	325182.677413	41.105357
3519.397346	324914.102142	41.110362
3519.246681	324640.869346	41.115367
3519.128146	324376.660334	41.120372
3518.877375	324114.327311	41.125376
3518.951992	323852.908418	41.130381
3518.728999	323598.708161	41.135386
3518.639033	323344.536424	41.140391
3518.522141	323091.003322	41.145396
3518.370628	322833.429236	41.150400
3518.178810	322580.566167	41.155405
3518.180308	322336.269946	41.160410
3517.918624	322081.812095	41.165415
3517.649793	321826.819585	41.170420
3517.796963	321586.922790	41.175424
3517.450469	321343.311219	41.180429
3517.621230	321098.981373	41.185434
3517.268205	320851.857232	41.190439
3517.048303	320615.039758	41.195444
3517.165751	320378.753370	41.200448
3516.896174	320136.598444	41.205453
3516.493681	319907.285243	41.210458
3516.446603	319666.797439	41.215463
3515.894514	319447.045636	41.220468
3516.314976	319222.383112	41.225472
3516.062056	319009.731377	41.230477
3515.855651	318779.949036	41.235482
3515.949411	318559.633820	41.240487
3515.539270	318334.282428	41.245492
3515.799904	318105.619299	41.250496
3515.480022	317897.781183	41.255501
3515.297139	317680.278004	41.260506
3515.175382	317472.254252	41.265511
3514.756932	317261.782528	41.270516
3514.607945	317046.280897	41.275520
3514.401994	316840.022889	41.280525
3514.397415	316643.655206	41.285530
3514.019309	316439.737570	41.290535
3513.891507	316254.277084	41.295540
3513.462649	316056.777323	41.300544
3513.615296	315864.376241	41.305549
3513.278568	315684.136519	41.310554
3513.387489	315488.458453	41.315559
3513.314357	315314.918610	41.320564
3513.333740	315125.588460	41.325568
3512.896467	314936.201694	41.330573
3512.759116	314761.117691	41.335578
3513.004218	314580.960728	41.340583
3512.598636	314406.706067	41.345588
3512.955141	314217.472104	41.350592
3513.205496	314047.744401	41.355597
3512.282826	313866.062413	41.360602
3512.328702	313697.026940	41.365607
3512.212166	313528.296131	41.370612
3512.228589	313357.101216	41.375616
3512.272680	313184.654541	41.380621
3511.913154	313008.148234	41.385626
3511.992082	312845.414846	41.390631
3511.624185	312691.758342	41.395636
3511.748328	312520.594394	41.400640
3511.559493	312359.504225	41.405645
3511.032253	312206.125488	41.410650
3511.156123	312045.977725	41.415655
3510.901379	311902.428262	41.420660
3511.479320	311736.152399	41.425664
3511.055781	311584.740187	41.430669
3510.772146	311447.504409	41.435674
3511.137029	311282.507107	41.440679
3510.895769	311129.436399	41.445684
3510.640097	310984.255745	41.450688
3510.639948	310837.482483	41.455693
3509.834085	310694.397209	41.460698
3510.397122	310550.944817	41.465703
3510.088821	310401.979112	41.470708
3510.035607	310263.635147	41.475712
3509.427296	310129.347229	41.480717
3509.264445	309998.297355	41.485722
3509.544193	309858.755070	41.490727
3509.600447	309740.495379	41.495732
3509.432776	309616.468529	41.500736
3509.343318	309480.825344	41.505741
3509.255970	309359.279073	41.510746
3509.226365	309224.312882	41.515751
3509.048748	309099.242933	41.520756
3509.117000	308971.818531	41.525760
3509.023735	308858.618605	41.530765
3508.706471	308737.183065	41.535770
3508.788160	308616.906325	41.540775
3508.681043	308498.261994	41.545780
3508.585505	308374.780544	41.550784
3508.501813	308255.521224	41.555789
3508.455269	308137.859005	41.560794
3508.438132	308026.808301	41.565799
3508.502354	307926.636251	41.570804
3508.163796	307798.941580	41.575808
3508.367168	307696.126186	41.580813
3507.866904	307589.145338	41.585818
3507.885358	307478.444107	41.590823
3507.657718	307374.041312	41.595828
3508.092399	307266.582776	41.600832
3507.789492	307156.567271	41.605837
3507.598400	307063.686102	41.610842
3507.744537	306950.597056	41.615847
3507.676947	306849.730889	41.620852
3507.588009	306748.816959	41.625856
3507.668187	306644.644444	41.630861
3507.400542	306545.234048	41.635866
3507.842846	306432.122976	41.640871
3507.580264	306325.204051	41.645876
3507.250899	306235.829413	41.650880
3507.191087	306138.599747	41.655885
3506.692570	306046.451868	41.660890
3507.017855	305942.315924	41.665895
3507.378109	305862.452429	41.670900
3507.137079	305767.388075	41.675904
3506.839851	305661.720152	41.680909
3506.936629	305581.922855	41.685914
3506.902261	305485.273280	41.690919
3506.472519	305401.257140	41.695924
3506.405283	305311.025519	41.700928
3506.780659	305220.979032	41.705933
3506.300484	305142.747293	41.710938
3506.509866	305060.183068	41.715943
3505.958619	304979.290026	41.720948
3505.632475	304894.824219	41.725952
3506.278369	304817.662947	41.730957
3505.936782	304740.528694	41.735962
3506.044732	304660.193773	41.740967
3505.901825	304593.946016	41.745972
3505.848183	304505.314161	41.750976
3505.931862	304431.650432	41.755981
3505.768618	304367.696016	41.760986
3505.890476	304281.352244	41.765991
3505.976013	304210.080165	41.770996
3505.746200	304130.967905	41.776000
3505.741492	304058.742641	41.781005
3505.668878	303995.842481	41.786010
3505.775891	303912.147182	41.791015
3505.743186	303845.321341	41.796020
3505.463730	303773.902126	41.801024
3505.302801	303707.935998	41.806029
3505.224931	303636.357829	41.811034
3505.332863	303557.802689	41.816039
3505.259161	303504.929369	41.821044
3505.263971	303435.475792	41.826048
3505.196422	303368.552986	41.831053
3504.624163	303305.272005	41.836058
3504.946884	303246.381138	41.841063
3504.921115	303190.980449	41.846068
3504.966675	303119.407724	41.851072
3504.704724	303067.937698	41.856077
3504.647789	303005.084792	41.861082
3505.035104	302936.512409	41.866087
3504.644263	302892.468372	41.871092
3504.731681	302835.751651	41.876096
3505.038250	302776.888233	41.881101
3504.584591	302721.528494	41.886106
3504.903040	302656.351404	41.891111
3504.888694	302595.552828	41.896116
3504.849593	302536.285076	41.901120
3504.541619	302464.334073	41.906125
3504.573085	302413.097489	41.911130
3504.616193	302347.301352	41.916135
3504.388941	302304.071115	41.921140
3504.654923	302255.724524	41.926144
3504.484778	302197.723955	41.931149
3504.123454	302152.224003	41.936154
3504.186074	302092.761697	41.941159
3504.195189	302056.569575	41.946164
3504.524237	302001.595727	41.951168
3504.434713	301956.816634	41.956173
3504.238217	301901.797592	41.961178
3504.310093	301849.994231	41.966183
3504.210656	301799.744647	41.971188
3503.939392	301741.606685	41.976192
3504.281431	301698.159698	41.981197
3504.043759	301653.963429	41.986202
3504.292001	301609.691157	41.991207
3504.256798	301559.202247	41.996212
3503.810160	301503.763785	42.001216
3503.971606	301457.748844	42.006221
3503.843348	301421.526867	42.011226
3503.993882	301364.187882	42.016231
3503.634598	301331.183333	42.021236
3503.195613	301286.611017	42.026240
3503.487991	301240.422714	42.031245
3503.451912	301204.771553	42.036250
3503.549069	301164.340189	42.041255
3503.247434	301126.821663	42.046260
3503.860362	301081.550250	42.051264
3503.906118	301039.243447	42.056269
3503.645568	301003.296380	42.061274
3503.657796	300962.623632	42.066279
3503.538928	300929.428542	42.071284
3503.571134	300880.201013	42.076288
3503.761491	300839.169457	42.081293
3503.425721	300805.371920	42.086298
3503.845874	300761.835610	42.091303
3503.792500	300725.881420	42.096308
3503.588724	300688.041873	42.101312
3503.426908	300649.152237	42.106317
3503.670171	300607.857721	42.111322
3503.352030	300564.971154	42.116327
3503.599969	300531.769376	42.121332
3503.536047	300495.104044	42.126336
3503.331731	300450.494349	42.131341
3503.473634	300422.628424	42.136346
3503.242893	300378.531829	42.141351
3503.350531	300347.667953	42.146356
3503.410139	300310.805024	42.151360
3503.537205	300271.615438	42.156365
3503.422096	300235.263351	42.161370
3503.251763	300193.345990	42.166375
3503.469147	300161.065017	42.171380
3502.961582	300129.788167	42.176384
3503.156052	300087.508274	42.181389
3503.208719	300069.760390	42.186394
3503.178875	300027.744584	42.191399
3502.891513	300000.938166	42.196404
3503.236207	299964.386754	42.201408
3503.001682	299933.092556	42.206413
3502.777144	299900.142421	42.211418
3502.953764	299863.031830	42.216423
3502.883137	299837.158611	42.221428
3503.014939	299811.177377	42.226432
3503.166458	299775.419591	42.231437
3502.629037	299746.285132	42.236442
3502.727140	299717.916660	42.241447
3502.626164	299696.044042	42.246452
3502.850785	299664.117968	42.251456
3502.962135	299634.551149	42.256461
3502.954031	299600.523474	42.261466
3503.104339	299573.292096	42.266471
3502.938195	299545.677497	42.271476
3502.791078	299521.877684	42.276480
3502.898563	299481.723424	42.281485
3502.959694	299456.643886	42.286490
3502.831557	299428.030663	42.291495
3502.781186	299398.285385	42.296500
3502.642039	299378.607470	42.301504
3502.857656	299356.837932	42.306509
3502.489363	299321.797416	42.311514
3502.584032	299307.275113	42.316519
3502.343799	299276.057787	42.321524
3502.437848	299254.052695	42.326528
3502.738856	299226.364902	42.331533
3502.844839	299218.000183	42.336538
3502.973760	299183.823568	42.341543
3503.009222	299159.486014	42.346548
3502.729618	299128.503828	42.351552
3502.916238	299099.306734	42.356557
3502.488658	299082.524434	42.361562
3502.569030	299044.257544	42.366567
3502.772613	299016.024932	42.371572
3503.037296	299002.544956	42.376576
3502.924372	298963.570121	42.381581
3502.653118	298948.163204	42.386586
3502.759696	298918.545843	42.391591
3502.490764	298887.154619	42.396596
3502.153081	298871.147216	42.401600
3502.339926	298844.113383	42.406605
3502.358786	298832.046213	42.411610
3502.740793	298813.330158	42.416615
3502.297886	298794.055854	42.421620
3502.654489	298765.086531	42.426624
3502.706384	298740.160824	42.431629
3502.430906	298717.500628	42.436634
3502.473936	298689.369307	42.441639
3502.352866	298672.793485	42.446644
3502.270962	298662.498235	42.451648
3502.425658	298629.106266	42.456653
3502.506802	298623.316017	42.461658
3502.230235	298597.601674	42.466663
3502.237051	298576.475327	42.471668
3502.306623	298554.575593	42.476672
3502.475503	298539.048848	42.481677
3502.075352	298518.876934	42.486682
3502.186452	298484.575412	42.491687
3502.686001	298482.868462	42.496692
3501.981124	298462.413288	42.501696
3502.288475	298449.079221	42.506701
3502.174289	298424.841098	42.511706
3502.511298	298404.528444	42.516711
3502.456652	298377.226711	42.521716
3502.197953	298363.752048	42.526720
3502.408243	298331.700185	42.531725
3502.516774	298325.218409	42.536730
3502.376973	298298.998951	42.541735
3502.025792	298275.968625	42.546740
3501.969731	298263.709425	42.551744
3502.002801	298244.156898	42.556749
3502.200872	298236.541207	42.561754
3502.279816	298209.854817	42.566759
3502.140552	298189.540187	42.571764
3501.947689	298194.431851	42.576768
3502.184156	298164.106566	42.581773
3502.223513	298151.170660	42.586778
3501.872043	298129.591109	42.591783
3502.280214	298106.518355	42.596788
3502.204452	298104.875884	42.601792
3502.462363	298085.746294	42.606797
3502.073250	298073.157335	42.611802
3502.486557	298038.070170	42.616807
3502.511903	298027.859845	42.621812
3502.245367	298008.252265	42.626816
3502.194142	297986.320289	42.631821
3502.258478	297980.125360	42.636826
3502.448191	297948.229210	42.641831
3502.261023	297933.877874	42.646836
3502.284967	297919.493529	42.651840
3502.295741	297890.450556	42.656845
3502.281484	297880.068228	42.661850
3502.441938	297849.118341	42.666855
3502.532229	297837.243410	42.671860
3502.175180	297812.864822	42.676864
3502.078043	297794.656030	42.681869
3502.211535	297771.397007	42.686874
3502.008993	297765.116515	42.691879
3502.137781	297746.032450	42.696884
3502.131264	297727.147700	42.701888
3502.012467	297720.854110	42.706893
3501.977807	297705.918914	42.711898
3502.165755	297681.913214	42.716903
3502.238382	297666.986687	42.721908
3501.934729	297652.704395	42.726912
3502.061382	297638.762069	42.731917
3501.740445	297636.368882	42.736922
3502.228808	297606.436610	42.741927
3502.060462	297598.929023	42.746932
3502.139499	297589.499259	42.751936
3502.322281	297556.636768	42.756941
3502.161083	297562.745267	42.761946
3502.117213	297532.208941	42.766951
3502.141448	297510.264982	42.771956
3501.857630	297506.033387	42.776960
3502.064169	297485.842610	42.781965
3502.276196	297471.250576	42.786970
3501.818586	297441.262488	42.791975
3502.151506	297431.742100	42.796980
3501.908064	297425.264342	42.801985
3502.341429	297414.608325	42.806989
3502.037472	297394.828211	42.811994
3502.487581	297384.704080	42.816999
3502.483206	297352.812484	42.822004
3502.094711	297346.840998	42.827009
3501.956416	297324.591489	42.832013
3501.943296	297306.700291	42.837018
3502.008112	297298.672608	42.842023
3502.093383	297275.904524	42.847028
3501.857870	297263.164105	42.852033
3502.365394	297257.714301	42.857037
3502.221766	297246.130344	42.862042
3502.072489	297220.548186	42.867047
3502.224368	297211.106971	42.872052
3502.220398	297190.618111	42.877057
3501.835484	297172.250486	42.882061
3502.203145	297149.947261	42.887066
3502.222673	297134.799819	42.892071
3501.855325	297120.552803	42.897076
3501.797562	297102.973955	42.902081
3502.340734	297093.395188	42.907085
3502.106006	297078.211122	42.912090
3502.177855	297057.863079	42.917095
3502.229246	297051.390090	42.922100
3501.806898	297036.362610	42.927105
3502.434864	297019.440119	42.932109
3502.235359	297002.723348	42.937114
3502.107490	296979.683032	42.942119
3502.067338	296964.392157	42.947124
3501.831102	296937.398098	42.952129
3502.107611	296927.301026	42.957133
3501.905890	296921.122123	42.962138
3502.079081	296909.183130	42.967143
3502.329620	296878.625878	42.972148
3502.097840	296878.484039	42.977153
3501.968913	296850.582306	42.982157
3501.975225	296847.908845	42.987162
3502.186531	296829.524255	42.992167
3501.889954	296807.197477	42.997172
3501.794943	296807.416052	43.002177
3501.961646	296786.645833	43.007181
3501.842835	296769.916378	43.012186
3501.711003	296746.952947	43.017191
3501.970007	296748.312470	43.022196
3501.977244	296739.428305	43.027201
3501.878010	296722.797588	43.032205
3501.793608	296703.542876	43.037210
3501.802762	296705.654150	43.042215
3501.789350	296691.835301	43.047220
3501.647317	296677.934746	43.052225
3502.131046	296666.863466	43.057229
3501.970371	296671.928401	43.062234
3501.637865	296637.720562	43.067239
3501.740962	296639.486260	43.072244
3502.186429	296633.409771	43.077249
3502.223135	296611.819858	43.082253
3502.002784	296598.415138	43.087258
3501.924391	296583.715562	43.092263
3502.025707	296556.770363	43.097268
3501.467876	296548.407214	43.102273
3502.191033	296532.131480	43.107277
3502.251696	296528.049581	43.112282
3502.010172	296503.779635	43.117287
3502.153250	296497.114077	43.122292
3501.779356	296478.515425	43.127297
3501.968448	296461.814102	43.132301
3502.041499	296459.995599	43.137306
3501.993118	296449.821970	43.142311
3501.824587	296427.856823	43.147316
3501.627716	296431.171165	43.152321
3501.931431	296404.168798	43.157325
3501.697011	296391.860717	43.162330
3501.640310	296376.521366	43.167335
3501.870683	296381.932442	43.172340
3501.693140	296374.502491	43.177345
3502.212255	296348.484553	43.182349
3502.098971	296344.251663	43.187354
3502.155252	296338.465067	43.192359
3502.049630	296305.825116	43.197364
3501.895210	296296.635262	43.202369
3502.132269	296289.547734	43.207373
3501.961063	296265.953933	43.212378
3502.158351	296261.647029	43.217383
3502.144223	296254.496954	43.222388
3501.956321	296229.404002	43.227393
3502.274757	296210.467946	43.232397
3501.922531	296198.254601	43.237402
3501.761149	296180.309869	43.242407
3502.184754	296167.364345	43.247412
3501.652482	296147.135879	43.252417
3502.179305	296133.614237	43.257421
3502.049453	296127.627639	43.262426
3501.659011	296112.467661	43.267431
3501.847617	296086.272195	43.272436
3501.817532	296092.716701	43.277441
3501.681303	296080.291389	43.282445
3501.690610	296072.501293	43.287450
3501.687635	296047.404803	43.292455
3501.959252	296042.729916	43.297460
3501.619039	296054.466312	43.302465
3501.930986	296032.807698	43.307469
3501.865198	296019.938652	43.312474
3502.069294	296008.121907	43.317479
3502.028323	295999.703326	43.322484
3501.832128	295976.367847	43.327489
3502.218774	295970.173217	43.332493
3501.918238	295961.871570	43.337498
3501.673395	295938.136426	43.342503
3502.161537	295924.340794	43.347508
3502.098073	295927.761575	43.352513
3502.338146	295894.583729	43.357517
3502.275784	295891.437344	43.362522
3502.270514	295870.057344	43.367527
3501.975819	295856.180456	43.372532
3501.814753	295853.304035	43.377537
3501.971363	295830.040607	43.382541
3501.910996	295812.436316	43.387546
3501.733833	295797.268364	43.392551
3501.769097	295787.285169	43.397556
3501.626354	295772.188190	43.402561
3501.742544	295766.086728	43.407565
3501.572707	295764.178908	43.412570
3501.352507	295762.686218	43.417575
3501.563034	295761.558899	43.422580
3501.584872	295743.534479	43.427585
3501.943169	295725.126556	43.432589
3501.797355	295724.894913	43.437594
3501.797623	295718.607941	43.442599
3501.861071	295701.976948	43.447604
3501.797137	295690.634753	43.452609
3501.819035	295690.809600	43.457613
3501.958720	295689.184284	43.462618
3502.179773	295667.005218	43.467623
3502.044278	295648.750830	43.472628
3501.676130	295645.703146	43.477633
3501.638807	295616.030194	43.482637
3501.769857	295604.632045	43.487642
3501.503450	295600.473947	43.492647
3502.127449	295589.736882	43.497652
3501.997141	295585.532051	43.502657
3501.902036	295565.005952	43.507661
3501.965464	295559.752686	43.512666
3501.890233	295543.092422	43.517671
3501.804251	295520.019517	43.522676
3501.988004	295525.336149	43.527681
3502.185603	295505.578784	43.532685
3501.798766	295490.188995	43.537690
3501.774369	295472.171719	43.542695
3501.756817	295471.869115	43.547700
3501.799271	295457.099451	43.552705
3501.830855	295437.902544	43.557709
3501.900145	295432.266546	43.562714
3501.864043	295428.937855	43.567719
3501.796053	295407.389313	43.572724
3501.578700	295399.329118	43.577729
3501.693779	295381.493638	43.582733
3501.768860	295386.954540	43.587738
3501.770016	295378.020208	43.592743
3502.019109	295358.203835	43.597748
3501.673385	295354.796277	43.602753
3501.841530	295358.180882	43.607757
3502.151327	295334.715130	43.612762
3501.771280	295317.084307	43.617767
3501.817055	295311.375612	43.622772
3501.935644	295298.732118	43.627777
3501.947086	295276.203868	43.632781
3501.950968	295268.796318	43.637786
3501.645067	295256.397355	43.642791
3502.022882	295232.971836	43.647796
3501.982702	295233.436381	43.652801
3502.105716	295220.664910	43.657805
3501.391249	295202.831797	43.662810
3501.584215	295192.340223	43.667815
3501.570487	295186.131742	43.672820
3501.356857	295178.478195	43.677825
3501.913205	295176.558639	43.682829
3501.715536	295163.150038	43.687834
3501.738066	295148.103419	43.692839
3501.656621	295146.487205	43.697844
3501.479262	295143.053313	43.702849
3501.761375	295129.595149	43.707853
3501.898112	295119.035991	43.712858
3501.786349	295100.421368	43.717863
3501.849102	295102.626135	43.722868
3501.651115	295112.533265	43.727873
3501.643038	295091.535224	43.732877
3501.607764	295076.955792	43.737882
3501.611433	295070.846395	43.742887
3501.879109	295062.710324	43.747892
3501.853523	295058.412722	43.752897
3501.775304	295025.920487	43.757901
3501.769132	295032.514095	43.762906
3501.666450	295026.268598	43.767911
3501.855107	295013.054103	43.772916
3501.457983	294994.687689	43.777921
3502.001856	294978.465004	43.782925
3502.132006	294979.335638	43.787930
3501.479968	294965.743489	43.792935
3501.663615	294947.718979	43.797940
3501.873514	294943.486369	43.802945
3501.662278	294938.021449	43.807949
3501.459094	294931.282576	43.812954
3501.461649	294916.060843	43.817959
3501.744557	294899.268041	43.822964
3501.847647	294895.815743	43.827969
3502.038316	294882.066372	43.832973
3501.956918	294879.482894	43.837978
3501.844586	294862.879143	43.842983
3501.771836	294847.363719	43.847988
3501.824304	294857.053558	43.852993
3501.857706	294827.241879	43.857997
3501.829552	294819.355655	43.863002
3501.695424	294812.325978	43.868007
3502.162740	294797.438817	43.873012
3501.709598	294789.924479	43.878017
3501.633440	294762.904376	43.883021
3501.261140	294763.802658	43.888026
3501.566164	294762.965994	43.893031
3501.715373	294759.735563	43.898036
3501.489029	294735.640680	43.903041
3501.648541	294723.143388	43.908045
3501.707932	294725.094156	43.913050
3501.835248	294726.397954	43.918055
3501.917446	294715.007269	43.923060
3501.556797	294700.453158	43.928065
3501.616104	294691.229636	43.933069
3501.436696	294691.894131	43.938074
3501.284227	294689.270848	43.943079
3501.478679	294691.505949	43.948084
3501.217714	294687.805106	43.953089
3501.349624	294676.432096	43.958093
3501.365919	294667.749828	43.963098
3501.300432	294656.025864	43.968103
3501.666612	294642.783532	43.973108
3501.742302	294653.131579	43.978113
3501.416404	294647.582743	43.983117
3501.389805	294656.648626	43.988122
3501.573574	294649.721954	43.993127
3501.575971	294626.965782	43.998132
3501.300949	294611.252831	44.003137
3501.180589	294608.089990	44.008141
3501.418876	294603.776555	44.013146
3501.605062	294601.609404	44.018151
3501.981156	294593.838129	44.023156
3501.293071	294586.920484	44.028161
3501.346383	294576.603358	44.033165
3501.708918	294562.801589	44.038170
3501.423110	294560.810043	44.043175
3501.656848	294557.744565	44.048180
3502.022734	294560.792853	44.053185
3501.749360	294549.635904	44.058189
3501.437101	294535.125095	44.063194
3501.145247	294519.058394	44.068199
3501.583842	294517.997212	44.073204
3501.371310	294522.103186	44.078209
3501.768557	294517.383082	44.083213
3501.899474	294507.995612	44.088218
3501.722954	294489.798183	44.093223
3501.816270	294477.107556	44.098228
3501.980350	294484.260052	44.103233
3501.493894	294467.485593	44.108237
3501.524165	294457.019323	44.113242
3501.283323	294445.348186	44.118247
3501.641626	294441.754145	44.123252
3501.692143	294431.793787	44.128257
3501.706177	294431.995322	44.133261
3501.741272	294424.964597	44.138266
3502.053336	294403.941713	44.143271
3501.898018	294391.315392	44.148276
3501.717158	294391.394672	44.153281
3501.992123	294377.402917	44.158285
3501.857947	294358.257025	44.163290
3501.952190	294359.413278	44.168295
3502.062820	294339.134579	44.173300
3501.678302	294322.598683	44.178305
3501.882994	294315.694155	44.183309
3501.935929	294310.493327	44.188314
3502.042091	294286.066280	44.193319
3501.992185	294272.838008	44.198324
3501.739378	294275.499407	44.203329
3501.933402	294260.273025	44.208333
3501.774112	294239.018323	44.213338
3501.490044	294229.186603	44.218343
3501.760424	294213.897363	44.223348
3501.452352	294210.203854	44.228353
3501.547937	294197.334632	44.233357
3501.565376	294192.470247	44.238362
3501.621548	294185.156202	44.243367
3501.944049	294188.618561	44.248372
3501.601763	294194.908451	44.253377
3501.987804	294168.986710	44.258381
3502.130623	294152.368323	44.263386
3501.962027	294142.747623	44.268391
3501.842379	294125.075730	44.273396
3501.700775	294115.552623	44.278401
3501.342130	294104.841643	44.283405
3501.928209	294111.495488	44.288410
3501.895311	294091.290051	44.293415
3501.817166	294070.862594	44.298420
3501.690872	294069.100636	44.303425
3501.499528	294058.745306	44.308429
3502.001650	294051.005165	44.313434
3501.604211	294040.249329	44.318439
3502.160489	294021.020838	44.323444
3501.950026	294022.733820	44.328449
3501.749181	294010.445441	44.333453
3501.758302	293997.793327	44.338458
3501.620947	293995.473102	44.343463
3501.763139	293979.236579	44.348468
3501.142861	293964.061064	44.353473
3501.644730	293954.208243	44.358477
3501.784952	293939.295641	44.363482
3501.439370	293952.178741	44.368487
3501.474601	293937.028010	44.373492
3501.560416	293951.549105	44.378497
3501.538650	293933.505492	44.383501
3501.841186	293916.709343	44.388506
3501.615877	293907.988373	44.393511
3501.733876	293892.162878	44.398516
3501.385417	293894.228344	44.403521
3501.176711	293879.344824	44.408525
3501.586201	293872.815497	44.413530
3501.522056	293869.745644	44.418535
3501.872069	293868.774663	44.423540
3501.561829	293865.056018	44.428545
3501.437024	293860.315662	44.433549
3501.593288	293856.931353	44.438554
3501.451492	293831.219257	44.443559
3501.735913	293817.505891	44.448564
3501.615630	293817.677518	44.453569
3501.576338	293825.090979	44.458573
3501.775961	293817.856279	44.463578
3501.415060	293810.785573	44.468583
3501.917024	293795.510928	44.473588
3501.726395	293794.191745	44.478593
3501.681939	293777.042535	44.483597
3501.633465	293775.777489	44.488602
3501.629458	293758.851040	44.493607
3501.711281	293746.467505	44.498612
3501.926733	293748.572087	44.503617
3501.687537	293741.456891	44.508621
3501.715815	293716.659971	44.513626
3501.526803	293699.024249	44.518631
3501.823842	293690.603401	44.523636
3501.462027	293692.340055	44.528641
3501.569100	293694.003403	44.533645
3501.883087	293685.707176	44.538650
3501.696857	293667.740103	44.543655
3501.486622	293652.424040	44.548660
3501.813314	293651.863972	44.553665
3501.603376	293649.911443	44.558669
3501.470412	293625.725145	44.563674
3501.417709	293615.475334	44.568679
3501.600364	293616.006872	44.573684
3501.798441	293613.608737	44.578689
3501.690293	293606.956671	44.583693
3501.638701	293602.332121	44.588698
3501.336870	293587.030361	44.593703
3501.508977	293573.767223	44.598708
3501.432349	293579.964737	44.603713
3501.093434	293578.643277	44.608717
3501.378996	293571.369657	44.613722
3501.463296	293562.752959	44.618727
3501.425455	293567.264414	44.623732
3501.341335	293573.615827	44.628737
3501.411940	293560.114010	44.633741
3501.546617	293537.973101	44.638746
3501.225416	293536.114327	44.643751
3501.560607	293517.683873	44.648756
3501.596768	293520.732855	44.653761
3501.759425	293528.114780	44.658765
3501.535369	293521.251736	44.663770
3501.209673	293517.917303	44.668775
3501.704791	293491.036397	44.673780
3501.693632	293491.903691	44.678785
3501.526583	293480.933553	44.683789
3501.483308	293477.122237	44.688794
3501.251325	293483.496776	44.693799
3501.767475	293480.845272	44.698804
3501.667952	293462.177309	44.703809
3501.247800	293449.744918	44.708813
3501.581481	293442.183760	44.713818
3501.481670	293441.537643	44.718823
3501.520086	293447.055366	44.723828
3501.592755	293446.000466	44.728833
3501.432982	293438.796453	44.733837
3501.828848	293415.901938	44.738842
3501.354941	293412.412488	44.743847
3501.397878	293406.271325	44.748852
3501.224133	293401.716766	44.753857
3501.307934	293396.714668	44.758861
3501.952159	293398.726775	44.763866
3501.823531	293387.674249	44.768871
3501.738554	293378.294899	44.773876
3501.204216	293372.676711	44.778881
3501.536457	293374.101229	44.783885
3501.408015	293364.423217	44.788890
3501.501850	293366.394099	44.793895
3501.419269	293362.690739	44.798900
3501.651107	293352.956399	44.803905
3501.239112	293336.424523	44.808909
3501.217717	293328.104317	44.813914
3501.512976	293330.221892	44.818919
3501.509472	293323.629799	44.823924
3501.461128	293329.084733	44.828929
3501.505902	293323.630549	44.833933
3501.708308	293329.148100	44.838938
3501.407577	293309.900636	44.843943
3501.593901	293290.882476	44.848948
3501.651470	293289.499024	44.853953
3501.859609	293294.888408	44.858957
3501.836686	293282.648427	44.863962
3501.784143	293267.714885	44.868967
3501.956245	293246.611656	44.873972
3501.788802	293249.514301	44.878977
3501.073940	293237.713397	44.883981
3501.689304	293231.151814	44.888986
3501.444911	293213.499153	44.893991
3501.106761	293214.137572	44.898996
3501.091089	293209.201919	44.904001
3501.339806	293208.450401	44.909005
3501.628953	293202.728909	44.914010
3501.203604	293205.926424	44.919015
3501.536924	293204.321677	44.924020
3501.308838	293200.284690	44.929025
3501.203966	293204.526651	44.934029
3501.567638	293196.298953	44.939034
3501.512029	293194.475008	44.944039
3501.582007	293164.784049	44.949044
3501.889878	293160.866906	44.954049
3501.327788	293157.543955	44.959053
3501.745040	293154.678806	44.964058
3501.504669	293151.661923	44.969063
3501.663200	293128.040763	44.974068
3501.787224	293117.610510	44.979073
3501.760693	293127.414801	44.984077
3501.742415	293105.883103	44.989082
3501.696848	293112.763085	44.994087
3501.474485	293092.917842	44.999092
3501.886837	293086.769802	45.004097
3501.830889	293073.414935	45.009101
3501.708388	293064.066856	45.014106
3501.678277	293047.882472	45.019111
3501.692024	293033.829423	45.024116
3501.665999	293032.153577	45.029121
3501.355148	293035.765930	45.034125
3501.686797	293027.034121	45.039130
3501.417132	293012.821738	45.044135
3501.438626	293014.676668	45.049140
3501.540553	292999.591636	45.054145
3501.632258	292988.377317	45.059149
3501.572535	292993.910425	45.064154
3501.386285	292993.430545	45.069159
3501.691686	292981.368264	45.074164
3501.660127	292961.976788	45.079169
3501.485989	292955.589514	45.084173
3502.096264	292953.101455	45.089178
3501.486086	292948.258726	45.094183
3501.669802	292941.433683	45.099188
3501.771203	292923.039598	45.104193
3501.740786	292913.575280	45.109197
3501.768715	292907.792780	45.114202
3501.695834	292904.749699	45.119207
3501.563542	292878.348430	45.124212
3501.204020	292878.990193	45.129217
3501.126463	292873.962369	45.134221
3501.504517	292876.219745	45.139226
3501.432397	292870.783794	45.144231
3501.255531	292875.087943	45.149236
3501.137254	292872.993784	45.154241
3500.912357	292870.432654	45.159245
3501.453105	292876.151898	45.164250
3501.454848	292873.020785	45.169255
3501.317591	292875.740545	45.174260
3501.382096	292860.483146	45.179265
3501.510103	292842.084876	45.184269
3501.425210	292837.770930	45.189274
3501.384220	292840.730190	45.194279
3501.194034	292837.654535	45.199284
3501.327353	292835.673769	45.204289
3501.110511	292836.191407	45.209293
3501.176409	292829.486591	45.214298
3501.357717	292830.094711	45.219303
3501.314914	292825.341453	45.224308
3501.317193	292837.712221	45.229313
3501.393257	292832.482193	45.234317
3501.480460	292821.548549	45.239322
3501.143817	292810.452074	45.244327
3501.398333	292799.848637	45.249332
3501.260137	292795.721205	45.254337
3501.053026	292788.117238	45.259341
3501.349516	292790.387368	45.264346
3501.396500	292795.343807	45.269351
3501.464045	292793.195139	45.274356
3501.347612	292793.518896	45.279361
3501.568868	292797.098983	45.284365
3501.994161	292790.363430	45.289370
3501.499985	292767.225995	45.294375
3501.651775	292761.449571	45.299380
3501.568232	292754.437197	45.304385
3501.749175	292747.052560	45.309389
3501.478921	292742.742131	45.314394
3501.572705	292744.814861	45.319399
3501.645947	292723.421447	45.324404
3501.642640	292727.774837	45.329409
3501.654030	292734.136861	45.334413
3501.946346	292718.589262	45.339418
3501.534059	292696.533555	45.344423
3501.771506	292684.303655	45.349428
3501.969595	292678.392711	45.354433
3501.433777	292674.861986	45.359437
3501.765371	292661.879172	45.364442
3501.748697	292659.820031	45.369447
3501.640622	292639.065851	45.374452
3501.397905	292636.380222	45.379457
3501.343109	292639.036191	45.384461
3501.596722	292633.727479	45.389466
3501.444989	292615.678332	45.394471
3501.551745	292598.785149	45.399476
3501.255503	292594.987871	45.404481
3501.479946	292590.447362	45.409485
3501.790334	292593.708068	45.414490
3501.714837	292603.749194	45.419495
3502.036786	292588.247838	45.424500
3501.570388	292562.764131	45.429505
3501.422630	292563.805524	45.434509
3501.298137	292556.697709	45.439514
3501.157292	292560.487151	45.444519
3501.549605	292554.291281	45.449524
3501.571053	292564.088162	45.454529
3501.381475	292549.328596	45.459533
3501.857287	292526.166696	45.464538
3501.985828	292525.892146	45.469543
3501.721755	292517.940682	45.474548
3501.683199	292513.415829	45.479553
3501.431002	292494.796890	45.484557
3501.532259	292475.817227	45.489562
3501.598245	292475.043359	45.494567
3501.239465	292475.074091	45.499572
3501.469610	292468.725381	45.504577
3501.353279	292468.845484	45.509581
3501.477808	292469.615214	45.514586
3501.485094	292463.250435	45.519591
3501.391459	292438.039313	45.524596
3501.465389	292437.951486	45.529601
3501.382758	292428.240706	45.534605
3501.810002	292431.559517	45.539610
3501.484262	292430.057786	45.544615
3501.437461	292429.810649	45.549620
3501.701034	292419.409369	45.554625
3501.448049	292402.368732	45.559629
3501.344246	292391.388508	45.564634
3501.535058	292404.391719	45.569639
3501.300399	292402.163009	45.574644
3501.745955	292390.664164	45.579649
3501.313832	292383.858973	45.584653
3501.944462	292380.782245	45.589658
3501.574257	292362.665359	45.594663
3501.642907	292347.839917	45.599668
3501.848813	292349.844222	45.604673
3501.593332	292347.389670	45.609677
3501.826738	292328.414756	45.614682
3501.690586	292321.945112	45.619687
3501.492468	292301.586719	45.624692
3501.670727	292293.464251	45.629697
3501.738865	292304.959361	45.634701
3501.723854	292282.128653	45.639706
3501.364010	292279.054039	45.644711
3501.553844	292268.715171	45.649716
3501.677336	292269.815982	45.654721
3501.323965	292272.111366	45.659725
3501.633723	292265.291997	45.664730
3501.137906	292245.438317	45.669735
3501.411839	292233.508083	45.674740
3501.696031	292227.227263	45.679745
3501.491501	292230.161210	45.684749
3501.449518	292222.022255	45.689754
3501.398054	292226.739581	45.694759
3501.485351	292223.467783	45.699764
3501.603138	292202.830873	45.704769
3501.792026	292190.022999	45.709773
3501.700704	292181.993573	45.714778
3501.808353	292183.376867	45.719783
3501.960730	292179.916707	45.724788
3501.836799	292155.982958	45.729793
3501.842084	292156.236778	45.734797
3501.798464	292146.138028	45.739802
3501.576690	292135.583482	45.744807
3501.638366	292112.027979	45.749812
3501.837000	292111.131548	45.754817
3501.585634	292091.723247	45.759821
3501.683335	292032.754025	45.764826
3501.380935	291927.875276	45.769831
3501.806249	291779.786886	45.774836
3501.499326	291588.004041	45.779841
3500.927964	291349.398548	45.784845
3501.046016	291059.569669	45.789850
3500.742440	290725.894344	45.794855
3500.224299	290333.753317	45.799860
3499.607867	289914.896413	45.804865
3499.155840	289444.615010	45.809869
3498.999319	288921.512847	45.814874
3498.618829	288355.267020	45.819879
3497.917960	287737.210720	45.824884
3498.020917	287082.441037	45.829889
3497.240581	286366.017899	45.834893
3496.518551	285608.005584	45.839898
3495.559542	284812.827728	45.844903
3495.064276	283950.205531	45.849908
3494.546959	283058.425966	45.854913
3493.697275	282128.371386	45.859917
3493.285919	281131.100077	45.864922
3492.034578	280101.638173	45.869927
3491.209037	279005.593887	45.874932
3490.360280	277881.861950	45.879937
3489.194647	276716.814967	45.884941
3488.152742	275486.627333	45.889946
3486.814492	274224.665908	45.894951
3486.000090	272920.667636	45.899956
3484.915723	271558.306543	45.904961
3483.199655	270172.928428	45.909965
3482.217195	268736.768298	45.914970
3480.899585	267269.725847	45.919975
3479.589465	265735.409831	45.924980
3478.084652	264182.359145	45.929985
3476.705343	262577.190511	45.934989
3475.219159	260939.878080	45.939994
3473.830762	259257.911453	45.944999
3472.267659	257533.828118	45.950004
3470.893126	255775.388868	45.955009
3468.577744	253984.476468	45.960013
3467.317827	252134.700949	45.965018
3466.022997	250275.434542	45.970023
3463.987305	248361.380516	45.975028
3462.016385	246419.892366	45.980033
3459.868657	244438.809658	45.985037
3458.151931	242424.226856	45.990042
3456.093723	240372.394642	45.995047
3453.991713	238289.660273	46.000052
3452.376570	236179.380595	46.005057
3449.940742	234034.605082	46.010061
3447.951304	231840.340061	46.015066
3445.436376	229640.342369	46.020071
3442.995964	227400.417699	46.025076
3440.806279	225141.323780	46.030081
3438.062710	222845.284453	46.035085
3435.734291	220532.551910	46.040090
3433.289576	218188.338517	46.045095
3430.704728	215818.483817	46.050100
3428.504885	213432.893027	46.055105
3425.686128	211010.613376	46.060109
3423.019597	208556.902409	46.065114
3420.389089	206093.175837	46.070119
3417.643066	203604.308099	46.075124
3414.548241	201091.359061	46.080129
3411.343929	198575.255431	46.085133
3408.443829	196014.044301	46.090138
3405.422742	193448.263987	46.095143
3402.545489	190866.952819	46.100148
3399.182332	188263.007887	46.105153
3395.507924	185661.133498	46.110157
3392.241892	183034.179013	46.115162
3389.159292	180413.607144	46.120167
3385.792692	177768.507494	46.125172
3382.385646	175107.747426	46.130177
3378.750673	172462.895091	46.135181
3374.969410	169779.648227	46.140186
3371.139941	167105.022302	46.145191
3367.484410	164431.361771	46.150196
3364.029332	161750.062746	46.155201
3359.776950	159085.329589	46.160205
3355.508723	156388.946671	46.165210
3351.080311	153723.025885	46.170215
3345.936243	151063.958766	46.175220
3341.359425	148419.247241	46.180225
3336.388920	145785.837361	46.185229
3331.188367	143177.206580	46.190234
3325.585387	140579.170360	46.195239
3319.887285	138035.882001	46.200244
3314.644153	135429.075963	46.205249
3308.536949	132924.210129	46.210253
3302.612282	130473.799844	46.215258
3296.460118	128065.031190	46.220263
3289.688579	125700.289435	46.225268
3283.086303	123396.553287	46.230273
3275.545728	121138.943530	46.235277
3268.033837	118948.325099	46.240282
3260.164134	116845.121136	46.245287
3252.211952	114804.811642	46.250292
3244.005366	112842.914729	46.255297
3235.209759	110979.026476	46.260301
3227.175805	109194.194966	46.265306
3217.942181	107494.754987	46.270311
3209.413162	105900.444955	46.275316
3200.938930	104387.162272	46.280321
3191.946576	102964.418310	46.285325
3183.717302	101636.692200	46.290330
3175.838068	100414.943105	46.295335
3167.286955	99273.467606	46.300340
3159.621642	98203.282675	46.305345
3152.192829	97214.370646	46.310349
3145.052115	96300.971825	46.315354
3138.358360	95464.770651	46.320359
3131.862444	94694.693265	46.325364
3126.068639	93972.712746	46.330369
3120.196434	93313.866414	46.335373
3114.534436	92691.038860	46.340378
3108.948274	92111.822307	46.345383
3102.888389	91593.479756	46.350388
3098.557780	91093.020540	46.355393
3093.762815	90632.006379	46.360397
3088.955573	90201.864393	46.365402
3084.857836	89792.366457	46.370407
3080.252508	89413.091658	46.375412
3076.823728	89046.228990	46.380417
3072.643501	88700.388898	46.385421
3069.515141	88361.236531	46.390426
3065.931543	88037.227624	46.395431
3062.171623	87710.086273	46.400436
3058.653017	87397.318222	46.405441
3055.315568	87083.470666	46.410445
3052.401041	86776.624128	46.415450
3049.034733	86477.194682	46.420455
3045.424643	86168.608426	46.425460
3042.536445	85862.466105	46.430465
3038.795677	85564.883183	46.435469
3035.570285	85262.496819	46.440474
3032.216211	84960.908671	46.445479
3028.633343	84661.989125	46.450484
3025.402144	84359.359039	46.455489
3022.018819	84061.799209	46.460493
3018.668925	83766.218959	46.465498
3015.411990	83474.489002	46.470503
3011.918194	83159.831857	46.475508
3008.468528	82863.171373	46.480513
3004.845903	82561.955305	46.485517
3001.829158	82268.752000	46.490522
2997.928802	81979.538787	46.495527
2994.208212	81688.471267	46.500532
2991.095100	81395.203165	46.505537
2987.033262	81109.250508	46.510541
2983.625793	80819.502131	46.515546
2979.980455	80522.845998	46.520551
2976.266528	80242.589031	46.525556
2972.912015	79957.756879	46.530561
2969.119315	79689.177910	46.535565
2965.278606	79409.774741	46.540570
2961.697510	79134.017153	46.545575
2957.917379	78873.763445	46.550580
2954.350973	78601.933517	46.555585
2950.962866	78346.741981	46.560589
2947.008076	78082.230137	46.565594
2943.359806	77831.008613	46.570599
2939.837311	77572.746305	46.575604
2936.614390	77312.915526	46.580609
2932.791173	77061.487105	46.585613
2929.170387	76815.807937	46.590618
2925.643184	76562.229586	46.595623
2921.754996	76324.623127	46.600628
2918.450126	76084.908240	46.605633
2914.850012	75848.822977	46.610637
2911.304421	75605.555943	46.615642
2908.061133	75355.182878	46.620647
2904.203595	75123.893828	46.625652
2900.595586	74884.097298	46.630657
2896.655334	74655.047592	46.635661
2893.472328	74411.518739	46.640666
2889.762371	74184.710167	46.645671
2886.292968	73965.561411	46.650676
2883.280782	73725.885232	46.655681
2879.404008	73498.346646	46.660685
2876.044287	73264.494152	46.665690
2872.165061	73047.347214	46.670695
2868.481557	72822.298473	46.675700
2865.160062	72584.509502	46.680705
2861.706442	72369.396756	46.685709
2858.196201	72132.022310	46.690714
2854.871102	71912.207622	46.695719
2851.358673	71685.529163	46.700724
2848.190268	71451.586571	46.705729
2844.503320	71227.326516	46.710733
2840.984774	70998.458258	46.715738
2837.616920	70777.783613	46.720743
2834.005492	70541.074218	46.725748
2831.004342	70313.895939	46.730753
2827.190457	70093.792015	46.735757
2823.622405	69859.354784	46.740762
2820.019100	69629.489675	46.745767
2816.377107	69405.854025	46.750772
2813.052289	69181.612048	46.755777
2809.639043	68947.469904	46.760781
2806.454350	68723.927324	46.765786
2802.912935	68483.867532	46.770791
2799.002264	68258.480959	46.775796
2795.958487	68025.463783	46.780801
2792.341246	67799.235491	46.785805
2788.764432	67564.414173	46.790810
2785.305345	67332.382335	46.795815
2781.730771	67102.884381	46.800820
2778.315257	66872.582841	46.805825
2775.020758	66643.686328	46.810829
2771.259338	66400.671656	46.815834
2767.751018	66160.812532	46.820839
2764.362202	65934.933184	46.825844
2760.900814	65701.374113	46.830849
2757.360214	65478.639156	46.835853
2754.181794	65246.785548	46.840858
2750.481010	65003.171791	46.845863
2746.980623	64763.800704	46.850868
2743.552300	64530.736017	46.855873
2740.084585	64299.241032	46.860877
2736.862167	64062.086357	46.865882
2733.547774	63826.528702	46.870887
2729.728261	63587.409149	46.875892
2725.996736	63337.526585	46.880897
2722.734203	63105.464716	46.885901
2719.309078	62858.998013	46.890906
2715.435580	62631.948471	46.895911
2712.160695	62395.389030	46.900916
2708.641567	62155.722166	46.905921
2705.086266	61914.679746	46.910925
2701.445533	61676.965863	46.915930
2697.902666	61446.924389	46.920935
2694.361208	61198.550412	46.925940
2691.252143	60959.383140	46.930945
2687.666698	60728.853680	46.935949
2684.300012	60484.825734	46.940954
2680.597257	60238.999736	46.945959
2677.323902	60015.269201	46.950964
2673.705976	59761.597446	46.955969
2670.237314	59525.686057	46.960973
2666.751008	59281.752283	46.965978
2663.074952	59035.280613	46.970983
2659.645487	58800.372746	46.975988
2656.445003	58562.721764	46.980993
2652.937371	58324.569091	46.985997
2649.451562	58079.365522	46.991002
2646.116427	57831.691543	46.996007
2642.180120	57587.997491	47.001012
2638.968109	57341.819477	47.006017
2635.157719	57096.676670	47.011021
2631.679550	56852.436173	47.016026
2628.285981	56611.928534	47.021031
2624.543915	56367.740599	47.026036
2621.086689	56122.793622	47.031041
2617.649186	55884.539941	47.036045
2613.906927	55637.656574	47.041050
2610.573284	55389.036835	47.046055
2606.933741	55155.796345	47.051060
2603.737772	54909.044469	47.056065
2600.278906	54676.770190	47.061069
2596.678431	54428.278388	47.066074
2593.529077	54185.866401	47.071079
2589.532882	53939.827146	47.076084
2586.607251	53686.041549	47.081089
2582.667248	53448.569805	47.086093
2579.089790	53201.552854	47.091098
2576.061208	52952.555757	47.096103
2571.881509	52706.976827	47.101108
2568.675994	52459.592313	47.106113
2565.189970	52222.061988	47.111117
2561.651550	51976.587088	47.116122
2558.318984	51733.613743	47.121127
2554.709331	51482.401383	47.126132
2551.072837	51233.784146	47.131137
2547.671360	50978.808262	47.136141
2544.161446	50742.038993	47.141146
2540.910630	50491.523429	47.146151
2537.456290	50255.816145	47.151156
2534.071793	49992.513280	47.156161
2530.278079	49752.677645	47.161165
2526.458203	49497.605957	47.166170
2523.293655	49258.266979	47.171175
2519.667195	49015.881977	47.176180
2516.221127	48765.225460	47.181185
2512.754120	48527.489115	47.186189
2509.294552	48272.825052	47.191194
2506.279365	48015.633326	47.196199
2502.354889	47771.925423	47.201204
2498.991272	47507.969199	47.206209
2495.444513	47257.192795	47.211213
2491.765079	47000.262342	47.216218
2488.715278	46748.177049	47.221223
2485.237288	46503.848460	47.226228
2481.842844	46246.146284	47.231233
2478.204036	45990.901655	47.236237
2474.547676	45729.238095	47.241242
2470.846871	45475.030100	47.246247
2467.069729	45224.382093	47.251252
2463.981635	44968.504839	47.256257
2460.377098	44713.909902	47.261261
2456.844675	44453.180442	47.266266
2453.575807	44198.215445	47.271271
2449.954383	43950.874066	47.276276
2446.839639	43695.465825	47.281281
2443.195616	43431.094031	47.286285
2439.705729	43171.793417	47.291290
2436.055611	42906.858101	47.296295
2432.433378	42653.088533	47.301300
2429.174942	42395.409535	47.306305
2426.022190	42135.985892	47.311309
2422.302877	41870.699708	47.316314
2419.151740	41605.226386	47.321319
2415.400586	41348.790766	47.326324
2412.124246	41078.029751	47.331329
2408.648895	40816.332399	47.336333
2405.032457	40545.459974	47.341338
2401.626512	40277.918479	47.346343
2398.132634	40015.472753	47.351348
2394.716065	39744.693135	47.356353
2390.763137	39477.665507	47.361357
2386.994190	39210.606043	47.366362
2384.147663	38936.393334	47.371367
2380.544684	38676.789553	47.376372
2377.400394	38409.356948	47.381377
2373.450247	38137.450924	47.386381
2370.132091	37868.010767	47.391386
2366.692458	37591.416353	47.396391
2363.102754	37330.609473	47.401396
2359.812168	37054.943267	47.406401
2356.208255	36770.333815	47.411405
2352.123610	36518.495946	47.416410
2349.230128	36239.468920	47.421415
2345.176687	35974.941146	47.426420
2341.915918	35702.672907	47.431425
2338.709925	35435.863921	47.436429
2335.404602	35165.333778	47.441434
2332.110133	34886.647120	47.446439
2328.086420	34614.518531	47.451444
2324.753254	34331.959485	47.456449
2321.115079	34058.617738	47.461453
2317.296689	33780.357245	47.466458
2314.307939	33504.734251	47.471463
2310.518690	33239.552814	47.476468
2307.516784	32950.127597	47.481473
2304.038182	32682.115713	47.486477
2300.072009	32407.021334	47.491482
2297.024692	32119.871107	47.496487
2293.082819	31832.871115	47.501492
2290.293995	31543.508086	47.506497
2286.585226	31273.471445	47.511501
2283.278269	30982.378306	47.516506
2280.015426	30701.999423	47.521511
2276.483523	30411.082587	47.526516
2272.999584	30124.059924	47.531521
2269.178097	29827.841382	47.536525
2265.511403	29554.632847	47.541530
2262.636102	29254.801636	47.546535
2258.823691	28962.504219	47.551540
2255.607775	28665.364824	47.556545
2252.184830	28368.914835	47.561549
2248.296536	28080.995378	47.566554
2245.656942	27785.698666	47.571559
2241.625642	27489.343937	47.576564
2238.389520	27181.178026	47.581569
2234.981036	26884.576244	47.586573
2231.463285	26588.211326	47.591578
2228.193385	26283.365604	47.596583
2224.167282	25983.832173	47.601588
2221.246576	25668.999484	47.606593
2218.138225	25359.472662	47.611597
2214.325865	25055.363939	47.616602
2211.113581	24737.695870	47.621607
2207.791478	24429.179845	47.626612
2204.071524	24110.086882	47.631617
2200.794078	23795.256963	47.636621
2197.057712	23482.822581	47.641626
2193.421078	23158.682393	47.646631
2189.815561	22843.500673	47.651636
2186.597265	22518.304480	47.656641
2182.968390	22210.231837	47.661645
2179.802995	21886.475773	47.666650
2176.454029	21553.903921	47.671655
2173.099102	21242.034235	47.676660
2169.980247	20916.069604	47.681665
2166.365787	20581.952991	47.686669
2162.502249	20260.917299	47.691674
2159.299736	19923.694217	47.696679
2155.625066	19596.894594	47.701684
2152.082497	19259.888156	47.706689
2148.649503	18924.789588	47.711693
2144.980836	18604.580318	47.716698
2141.395359	18271.043311	47.721703
2138.016404	17953.864973	47.726708
2134.510986	17623.335058	47.731713
2131.085478	17279.086292	47.736717
2127.318890	16938.811031	47.741722
2123.890569	16604.774590	47.746727
2119.914860	16282.808725	47.751732
2116.764640	15968.454900	47.756737
2112.921095	15627.160376	47.761741
2109.551057	15309.169126	47.766746
2105.719790	14993.411608	47.771751
2101.861516	14681.580252	47.776756
2097.975335	14374.178451	47.781761
2094.031487	14066.632317	47.786765
2089.617528	13764.911284	47.791770
2085.818477	13479.043360	47.796775
2081.786052	13205.801365	47.801780
2077.891041	12920.751552	47.806785
2074.216820	12659.352962	47.811789
2070.298940	12396.523954	47.816794
2066.825722	12131.780151	47.821799
2062.869805	11881.665809	47.826804
2059.161805	11626.032828	47.831809
2055.321096	11391.748652	47.836813
2051.406376	11153.657953	47.841818
2047.779252	10910.327226	47.846823
2043.305966	10695.553201	47.851828
2039.292810	10482.055032	47.856833
2035.352755	10265.822307	47.861837
2032.251239	10081.065621	47.866842
2028.586437	9876.991169	47.871847
2024.896395	9675.474274	47.876852
2021.461421	9465.714834	47.881857
2017.310869	9272.900176	47.886861
2014.030313	9085.307202	47.891866
2010.819104	8891.596165	47.896871
2007.079008	8706.430776	47.901876
2004.137017	8519.942716	47.906881
2000.395568	8321.284657	47.911885
1996.953409	8143.190587	47.916890
1994.047025	7943.791867	47.921895
1990.475064	7749.357942	47.926900
1986.664004	7565.772339	47.931905
1983.378845	7372.813599	47.936909
1979.836405	7184.211099	47.941914
1976.466631	6992.769816	47.946919
1973.026625	6794.315258	47.951924
1969.649185	6611.943653	47.956929
1966.532919	6411.989858	47.961933
1962.717905	6227.272555	47.966938
1959.126714	6034.768209	47.971943
1955.496201	5853.522970	47.976948
1952.225526	5648.636075	47.981953
1949.081889	5469.783825	47.986957
1945.503473	5268.667933	47.991962
1941.941128	5070.589842	47.996967
1938.229147	4871.584760	48.001972
1934.852687	4682.808026	48.006977
1931.582150	4490.877410	48.011981
1927.715214	4295.368105	48.016986
1924.388518	4115.168579	48.021991
1920.649949	3914.175012	48.026996
1917.321675	3730.875198	48.032001
1913.843192	3532.671023	48.037005
1910.395081	3347.833786	48.042010
1907.169326	3153.249088	48.047015
1903.591240	2961.632791	48.052020
1899.855487	2767.473807	48.057025
1896.427227	2581.492682	48.062029
1893.168375	2393.851069	48.067034
1889.568497	2198.734021	48.072039
1885.908086	2020.980766	48.077044
1882.382394	1829.172157	48.082049
1878.529289	1630.408389	48.087053
1874.874740	1455.611913	48.092058
1871.500745	1255.407299	48.097063
1867.666291	1083.354177	48.102068
1863.982318	901.186147	48.107073
1860.352150	723.149968	48.112077
1856.493943	556.205893	48.117082
1853.123070	374.604879	48.122087
1849.051774	227.945954	48.127092
1844.075724	81.176722	48.132097
1836.306197	43.999881	48.137101
1826.917061	66.783836	48.142106
1821.605954	57.497223	48.147111
1817.527570	68.560290	48.152116
1814.990034	61.810452	48.157121
1813.080421	68.614172	48.162125
1810.227303	70.370574	48.167130
1807.809917	60.061637	48.172135
1804.542539	67.498624	48.177140
1800.492815	65.585610	48.182145
1797.334701	59.704863	48.187149
1794.162178	58.091181	48.192154
1790.866427	56.971356	48.197159
1787.220553	59.557353	48.202164
1783.872601	63.602700	48.207169
1780.835634	61.977300	48.212173
1777.064599	60.549038	48.217178
1773.524912	67.443343	48.222183
1770.157000	64.284671	48.227188
1767.059040	60.950875	48.232193
1763.727263	54.480378	48.237197
1760.280302	61.863218	48.242202
1756.787206	52.244676	48.247207
1753.031573	63.684363	48.252212
1749.195336	63.528672	48.257217
1746.167616	61.281730	48.262221
1742.449103	69.336673	48.267226
1739.030172	55.951093	48.272231
1735.753907	56.944820	48.277236
1732.771777	61.613147	48.282241
1729.469891	57.846199	48.287245
1725.989775	63.937080	48.292250
1722.429638	54.677060	48.297255
1718.426282	54.000199	48.302260
1714.990125	58.999017	48.307265
1711.741086	57.739028	48.312269
1708.025190	62.221636	48.317274
1704.673234	56.504139	48.322279
1701.608185	58.024814	48.327284
1697.767932	57.423675	48.332289
1694.600629	60.074013	48.337293
1690.542076	67.562082	48.342298
1687.167288	59.231699	48.347303
1683.819547	60.021490	48.352308
1680.396857	65.594025	48.357313
1677.086385	65.969854	48.362317
1673.483175	65.442359	48.367322
1670.357688	56.943252	48.372327
1666.669421	64.262643	48.377332
1662.986581	65.614257	48.382337
1659.573318	67.281192	48.387341
1655.712040	68.799943	48.392346
1652.431890	60.745832	48.397351
1649.167357	63.477840	48.402356
1645.601043	57.540810	48.407361
1642.602640	53.697921	48.412365
1638.861395	65.980122	48.417370
1635.183097	58.801430	48.422375
1631.430657	59.603955	48.427380
1628.231018	57.656044	48.432385
1624.793400	54.736129	48.437389
1621.294187	61.912046	48.442394
1618.034945	56.341426	48.447399
1614.136629	66.512653	48.452404
1610.404629	71.700178	48.457409
1607.534309	61.142651	48.462413
1603.713598	58.643374	48.467418
1600.474262	53.129758	48.472423
1596.668157	60.562525	48.477428
1592.814827	59.330713	48.482433
1589.775200	59.110515	48.487437
1586.311175	58.441043	48.492442
1582.801116	59.234125	48.497447
1579.188170	58.562653	48.502452
1575.773893	58.110028	48.507457
1572.564267	51.506589	48.512461
1569.034156	52.698288	48.517466
1565.291540	53.100661	48.522471
1561.628736	64.639767	48.527476
1558.247535	57.791099	48.532481
1555.262222	51.468938	48.537485
1551.268984	56.453755	48.542490
1547.621561	58.891376	48.547495
1544.084994	58.729989	48.552500
1540.358381	56.968993	48.557505
1537.795238	53.798341	48.562509
1534.334841	54.096442	48.567514
1530.470102	47.345618	48.572519
1527.003979	55.452864	48.577524
1523.490972	60.273939	48.582529
1519.879225	61.440467	48.587533
1516.147198	62.746047	48.592538
1512.791545	58.984428	48.597543
1509.310481	53.951611	48.602548
1505.716419	54.362392	48.607553
1502.661197	61.123995	48.612557
1498.965229	54.846646	48.617562
1495.295906	55.003452	48.622567
1491.932762	55.675491	48.627572
1488.296826	56.238367	48.632577
1484.695108	54.125646	48.637581
1481.275506	52.772205	48.642586
1477.714548	56.607368	48.647591
1474.243407	49.756995	48.652596
1470.990485	51.307142	48.657601
1467.701044	55.621835	48.662605
1463.915434	51.570026	48.667610
1460.584601	56.862484	48.672615
1456.814439	57.582425	48.677620
1453.546055	57.796713	48.682625
1450.266824	43.111234	48.687629
1446.390184	55.984154	48.692634
1443.107452	55.438217	48.697639
1439.464476	51.519117	48.702644
1435.506452	56.615523	48.707649
1432.325516	48.811734	48.712653
1428.958813	55.641091	48.717658
1425.571915	49.875388	48.722663
1422.328617	50.554001	48.727668
1418.186020	58.979140	48.732673
1414.917418	47.047675	48.737677
1411.049680	56.831352	48.742682
1407.872349	51.640300	48.747687
1404.573479	49.211282	48.752692
1401.022225	51.836381	48.757697
1397.605031	43.275478	48.762701
1393.690399	52.114197	48.767706
1390.090846	49.855639	48.772711
1386.840358	59.995127	48.777716
1383.519939	60.771246	48.782721
1379.982616	46.622913	48.787725
1376.147176	56.135786	48.792730
1372.889864	53.178247	48.797735
1370.008351	56.970364	48.802740
1366.079702	55.193605	48.807745
1362.751968	65.231297	48.812749
1358.844136	57.054093	48.817754
1355.542601	48.588996	48.822759
1351.901821	57.201363	48.827764
1348.101266	62.292135	48.832769
1344.844720	52.222283	48.837773
1341.257804	60.066913	48.842778
1338.046457	52.157187	48.847783
1334.403224	51.196313	48.852788
1330.741525	50.190875	48.857793
1327.887842	40.931180	48.862797
1323.666849	46.875554	48.867802
1320.273942	44.534054	48.872807
1317.024899	50.117473	48.877812
1312.922593	47.798439	48.882817
1309.918880	53.058715	48.887821
1306.233533	51.478015	48.892826
1303.115956	54.718637	48.897831
1300.071734	61.475404	48.902836
1295.672168	61.183443	48.907841
1292.465709	49.678904	48.912845
1288.882146	55.675371	48.917850
1285.521354	58.419392	48.922855
1281.940447	52.446831	48.927860
1278.444193	48.112518	48.932865
1274.742212	48.154294	48.937869
1271.366074	55.744482	48.942874
1267.928728	47.401923	48.947879
1264.660579	48.435657	48.952884
1260.689411	47.763433	48.957889
1257.266259	48.486073	48.962893
1253.740071	51.819151	48.967898
1250.522581	47.308331	48.972903
1247.028903	47.959757	48.977908
1243.213298	52.553039	48.982913
1240.313469	52.216150	48.987917
1236.194730	56.524693	48.992922
1233.094222	48.471106	48.997927
1229.524715	53.459306	49.002932
1226.032913	53.667515	49.007937
1222.424772	52.508200	49.012941
1218.641271	58.501187	49.017946
1215.213819	51.128383	49.022951
1212.018536	45.683949	49.027956
1208.378749	49.670745	49.032961
1205.014176	53.146218	49.037965
1201.197631	48.260959	49.042970
1197.921739	51.833284	49.047975
1194.321279	48.385360	49.052980
1190.776045	54.046822	49.057985
1187.424365	51.724226	49.062989
1183.450339	55.475454	49.067994
1180.299169	46.449046	49.072999
1176.809196	42.107465	49.078004
1173.716010	49.681854	49.083009
1169.949971	44.121144	49.088013
1166.354159	50.907348	49.093018
1162.692661	50.373347	49.098023
1159.496402	44.656999	49.103028
1155.274980	51.974588	49.108033
1152.609880	44.238851	49.113037
1149.047894	50.377516	49.118042
1144.926060	52.076455	49.123047
1141.745281	57.345515	49.128052
1137.961935	47.067160	49.133057
1134.695022	36.881969	49.138061
1131.563363	53.286183	49.143066
1128.175486	55.487160	49.148071
1124.659543	43.673643	49.153076
1120.812216	48.638932	49.158081
1117.255545	51.730052	49.163085
1113.885070	59.259287	49.168090
1110.500951	49.794809	49.173095
1106.980614	50.403001	49.178100
1103.002844	58.761315	49.183105
1099.655416	50.841352	49.188109
1096.042127	58.013134	49.193114
1092.924472	54.929426	49.198119
1089.387430	56.805753	49.203124
1085.757875	58.522558	49.208129
1082.471578	50.007731	49.213133
1077.988447	44.420126	49.218138
1075.289248	48.316653	49.223143
1072.021646	45.844894	49.228148
1068.303043	46.158273	49.233153
1064.801244	50.803727	49.238157
1061.006756	41.995152	49.243162
1057.575085	57.019490	49.248167
1054.204021	48.758394	49.253172
1050.775092	54.651631	49.258177
1047.493867	44.889496	49.263181
1043.636517	52.156452	49.268186
1040.025958	42.085215	49.273191
1036.925704	51.603307	49.278196
1033.513617	51.112564	49.283201
1029.951305	50.895282	49.288205
1026.199920	47.667210	49.293210
1022.577681	52.964293	49.298215
1018.837768	50.762657	49.303220
1015.352184	58.730725	49.308225
1012.390113	52.411447	49.313229
1008.827555	59.464581	49.318234
1005.244320	44.241607	49.323239
1001.862498	42.018714	49.328244
998.101713	50.453819	49.333249
994.880355	46.304372	49.338253
990.848950	56.079003	49.343258
987.683153	53.034508	49.348263
984.226098	55.417209	49.353268
980.677052	59.703092	49.358273
977.298796	39.544182	49.363277
973.694673	49.995402	49.368282
970.359428	51.296005	49.373287
966.727052	53.035441	49.378292
963.248935	48.733216	49.383297
960.066177	47.747845	49.388301
956.404127	45.037331	49.393306
952.515358	52.739511	49.398311
948.652943	44.488958	49.403316
945.059933	55.273810	49.408321
942.009775	53.650745	49.413325
938.722424	54.095966	49.418330
935.317011	51.342112	49.423335
931.777123	51.096045	49.428340
927.876297	52.861711	49.433345
925.205879	42.836310	49.438349
921.189180	50.966659	49.443354
917.437064	59.723142	49.448359
913.828901	53.274110	49.453364
910.577214	47.471623	49.458369
907.115228	53.759224	49.463373
903.370816	50.647172	49.468378
900.229832	43.792801	49.473383
896.629128	49.741455	49.478388
893.028248	47.128956	49.483393
889.907956	50.018946	49.488397
886.032233	50.996081	49.493402
882.798985	52.271251	49.498407
879.323296	46.886669	49.503412
875.556845	57.898019	49.508417
871.759221	57.780918	49.513421
868.493609	53.214499	49.518426
865.071141	53.380345	49.523431
861.610236	55.206866	49.528436
858.064901	54.256158	49.533441
854.602997	56.598534	49.538445
850.983821	50.768192	49.543450
847.915378	52.855968	49.548455
844.205649	43.287572	49.553460
840.285644	53.680728	49.558465
836.860222	46.086305	49.563469
833.555163	50.106238	49.568474
829.959955	57.790969	49.573479
826.644721	56.566957	49.578484
822.651227	49.785998	49.583489
819.421613	47.994922	49.588493
816.102273	57.484103	49.593498
812.891006	48.907020	49.598503
809.466654	56.900363	49.603508
805.084192	51.958362	49.608513
802.257332	50.835056	49.613517
798.616211	55.935854	49.618522
794.991051	53.779616	49.623527
791.627153	51.639416	49.628532
788.002119	50.343709	49.633537
784.615719	46.542891	49.638541
780.913543	50.903440	49.643546
777.543376	46.286993	49.648551
774.035753	49.060502	49.653556
769.777419	53.005107	49.658561
766.674891	51.754137	49.663565
763.572546	41.628755	49.668570
760.131139	55.306918	49.673575
756.762079	52.623371	49.678580
753.080676	49.172484	49.683585
749.721445	37.824993	49.688589
745.614810	46.162477	49.693594
742.024386	46.158516	49.698599
739.323169	48.932305	49.703604
735.385079	44.550345	49.708609
732.077612	49.007288	49.713613
728.580949	50.390201	49.718618
724.758801	44.696106	49.723623
721.572910	40.797475	49.728628
718.104645	42.966887	49.733633
714.529445	45.124572	49.738637
710.490491	46.446881	49.743642
707.318467	51.619781	49.748647
704.283631	43.394770	49.753652
700.429938	47.744274	49.758657
697.433459	47.103148	49.763661
693.406494	51.808823	49.768666
689.488755	53.491811	49.773671
686.532050	45.029943	49.778676
682.639082	53.568111	49.783681
679.275943	38.446885	49.788685
675.752779	53.191406	49.793690
672.362594	50.678880	49.798695
669.016832	45.878320	49.803700
665.191807	50.169564	49.808705
661.824979	49.684526	49.813709
658.560772	48.553827	49.818714
654.999834	53.790814	49.823719
651.746825	44.033925	49.828724
648.172872	44.799380	49.833729
644.353939	42.654571	49.838733
640.573261	35.957437	49.843738
637.169659	42.780145	49.848743
633.719223	45.997166	49.853748
630.306334	57.225303	49.858753
626.999159	46.973867	49.863757
623.249907	54.404375	49.868762
619.884956	42.134017	49.873767
616.886586	41.692531	49.878772
612.961107	51.134324	49.883777
609.133376	49.244008	49.888781
605.769389	42.835970	49.893786
602.156097	44.408038	49.898791
599.023430	37.100069	49.903796
595.042142	46.019094	49.908801
591.760589	54.486847	49.913805
588.359882	49.460805	49.918810
584.837007	47.082991	49.923815
581.385297	40.274250	49.928820
577.822827	51.997227	49.933825
574.293628	46.741378	49.938829
571.112707	51.716395	49.943834
567.411840	42.083471	49.948839
563.937770	36.116639	49.953844
560.092699	48.671657	49.958849
556.830068	46.031632	49.963853
552.903087	57.852838	49.968858
549.482003	57.528199	49.973863
546.321790	45.526365	49.978868
542.866814	55.410189	49.983873
539.368337	46.261272	49.988877
535.725111	40.080499	49.993882
532.424698	47.412265	49.998887
529.300095	43.599021	50.003892
525.166031	58.341189	50.008897
521.507152	42.092600	50.013901
518.115678	37.141075	50.018906
514.627157	42.050389	50.023911
511.305805	40.400347	50.028916
507.752282	36.973832	50.033921
504.385874	42.952359	50.038925
500.731550	41.572772	50.043930
496.829571	46.872719	50.048935
493.688989	47.146412	50.053940
489.992405	56.780192	50.058945
486.755554	41.639279	50.063949
483.534149	39.321857	50.068954
479.868894	46.400734	50.073959
476.301416	45.384042	50.078964
472.637083	47.021102	50.083969
468.727934	42.859363	50.088973
465.248454	50.984828	50.093978
462.067353	48.243483	50.098983
458.786686	44.758432	50.103988
454.957790	44.317371	50.108993
451.757634	49.089792	50.113997
448.129567	52.138548	50.119002
444.495498	46.491056	50.124007
441.667710	45.927997	50.129012
437.415774	52.459704	50.134017
434.212837	45.754429	50.139021
431.049720	41.124677	50.144026
427.429638	53.669810	50.149031
423.851036	54.901154	50.154036
419.803108	50.413159	50.159041
416.632408	45.094899	50.164045
413.012060	47.319880	50.169050
409.318531	45.291573	50.174055
406.121514	48.279154	50.179060
402.708228	50.354647	50.184065
399.231437	36.975617	50.189069
395.499081	42.258524	50.194074
392.077716	45.186338	50.199079
388.612629	45.495079	50.204084
384.925593	47.075618	50.209089
381.649121	47.016295	50.214093
378.088506	47.014136	50.219098
374.426183	45.724440	50.224103
371.435231	51.242403	50.229108
367.451745	47.573246	50.234113
364.311108	44.585155	50.239117
360.751344	42.652975	50.244122
356.827551	45.624701	50.249127
354.014843	41.050823	50.254132
349.833838	52.070323	50.259137
346.351858	46.873617	50.264141
342.953359	48.510216	50.269146
339.322625	52.552853	50.274151
336.150924	51.847546	50.279156
332.748105	48.524047	50.284161
329.274852	37.001626	50.289165
325.621191	47.052675	50.294170
321.985397	57.781140	50.299175
318.917000	41.209213	50.304180
314.931661	47.680225	50.309185
311.475044	51.385549	50.314189
307.787691	40.627503	50.319194
304.072410	50.235795	50.324199
301.136391	42.691498	50.329204
297.651645	49.489062	50.334209
294.192326	41.827425	50.339213
290.435421	44.633830	50.344218
286.800172	43.779693	50.349223
283.163715	44.833493	50.354228
279.568816	50.034802	50.359233
276.625879	48.268623	50.364237
272.979562	45.815362	50.369242
269.889555	51.263450	50.374247
266.613329	55.434079	50.379252
262.290884	45.579136	50.384257
258.710020	52.878991	50.389261
255.667965	51.068234	50.394266
251.851026	43.038694	50.399271
248.315954	43.677993	50.404276
244.805432	54.136919	50.409281
241.016834	40.917544	50.414285
238.297128	45.927980	50.419290
235.045332	46.070489	50.424295
231.027479	43.548900	50.429300
226.980088	48.349713	50.434305
223.822321	42.317660	50.439309
220.088143	47.439568	50.444314
216.541201	47.659959	50.449319
213.519978	39.401382	50.454324
209.795029	45.768368	50.459329
206.499655	45.854440	50.464333
203.364354	49.613869	50.469338
199.650341	47.585698	50.474343
196.180090	40.824326	50.479348
192.749922	42.611475	50.484353
188.759663	51.003709	50.489357
185.575313	40.179581	50.494362
181.929015	43.468576	50.499367
178.396688	36.229720	50.504372
174.841747	47.110075	50.509377
171.160071	42.412968	50.514381
167.716691	36.979343	50.519386
164.158015	42.636925	50.524391
160.921360	43.080811	50.529396
157.473744	42.621276	50.534401
153.553501	44.757300	50.539405
150.435603	39.443533	50.544410
146.330268	54.551484	50.549415
143.411291	51.579369	50.554420
139.854816	49.653094	50.559425
136.483536	49.529621	50.564429
133.024495	53.921925	50.569434
129.559890	52.838638	50.574439
125.847519	42.207991	50.579444
122.648394	53.143353	50.584449
118.722688	55.821251	50.589453
115.083966	54.622880	50.594458
111.815178	59.434639	50.599463
108.575215	45.945880	50.604468
104.739329	52.447347	50.609473
101.621982	42.460645	50.614477
97.951970	46.598111	50.619482
93.896268	51.495195	50.624487
90.444622	46.050241	50.629492
87.082495	46.067723	50.634497
83.617437	39.606146	50.639501
80.304936	43.725571	50.644506
77.077596	46.781289	50.649511
73.763222	44.367859	50.654516
69.676500	45.008237	50.659521
66.238758	45.850658	50.664525
62.870722	35.805178	50.669530
59.093131	47.359530	50.674535
55.840289	36.751839	50.679540
52.575645	50.500568	50.684545
48.687871	45.541579	50.689549
45.366324	48.805057	50.694554
41.930127	44.635861	50.699559
38.558611	38.330492	50.704564
34.793681	43.090293	50.709569
31.052056	47.893902	50.714573
27.920152	51.618056	50.719578
24.492662	51.234515	50.724583
21.069294	36.942476	50.729588
17.174459	49.091016	50.734593
13.538590	46.661543	50.739597
10.069695	45.806769	50.744602
6.363743	51.803861	50.749607
2.767410	45.071823	50.754612