Thu Aug 25 10:07:50 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.254795	106.175887	0.000000
2.134893	103.980114	0.005005
1.951846	86.671450	0.010010
2.133411	96.871520	0.015014
2.086997	85.036907	0.020019
2.017114	77.075256	0.025024
1.737376	67.605740	0.030029
1.339743	60.609775	0.035034
1.289918	57.096397	0.040038
0.976116	41.842559	0.045043
0.699266	43.097729	0.050048
0.046936	29.589552	0.055053
0.219741	28.597608	0.060058
0.031844	14.133987	0.065062
-0.375389	7.063618	0.070067
-0.506547	2.746747	0.075072
-1.616370	0.323277	0.080077
-1.707209	-12.643258	0.085082
-1.922111	-15.725798	0.090086
-1.815905	-11.215047	0.095091
-1.818285	-14.919342	0.100096
-2.381005	-22.522156	0.105101
-2.416657	-25.455610	0.110106
-2.727588	-28.871113	0.115110
-3.589916	-22.354659	0.120115
-3.802946	-32.391393	0.125120
-3.860579	-20.072171	0.130125
-3.584283	-25.591823	0.135130
-4.426461	-21.875273	0.140134
-5.200402	-16.653982	0.145139
-4.774135	-18.536684	0.150144
-5.732625	-15.067663	0.155149
-5.595667	-22.147355	0.160154
-5.940735	-20.906810	0.165158
-5.625295	-25.024731	0.170163
-5.717296	-30.306342	0.175168
-6.885895	-27.807308	0.180173
-7.210995	-25.579641	0.185178
-7.002642	-28.696859	0.190182
-7.155278	-25.183262	0.195187
-7.177360	-19.478664	0.200192
-7.306414	-18.781327	0.205197
-7.879278	-29.201442	0.210202
-8.232873	-15.614641	0.215206
-8.452661	-18.550883	0.220211
-8.330471	-31.446378	0.225216
-9.182083	-26.817194	0.230221
-9.583947	-19.733811	0.235226
-9.671281	-22.564255	0.240230
-9.712804	-21.893288	0.245235
-9.362558	-33.078130	0.250240
-9.930787	-21.049065	0.255245
-10.415653	-15.063148	0.260250
-10.920500	-18.818427	0.265254
-11.477890	-19.031573	0.270259
-11.322859	-18.559081	0.275264
-11.823085	-16.769044	0.280269
-11.279367	-19.638253	0.285274
-11.399251	-20.995622	0.290278
-12.398874	-20.029003	0.295283
-12.263490	-18.828936	0.300288
-13.222412	-23.202763	0.305293
-12.712188	-19.720259	0.310298
-13.363682	-21.098735	0.315302
-13.042338	-22.265810	0.320307
-13.810450	-21.132986	0.325312
-14.361970	-12.289257	0.330317
-14.843085	-16.355138	0.335322
-14.606502	-15.319623	0.340326
-14.633761	-17.039516	0.345331
-14.205478	-21.497820	0.350336
-15.267253	-11.027071	0.355341
-15.328471	-30.306737	0.360346
-15.446042	-14.861837	0.365350
-15.638672	-23.895700	0.370355
-15.693832	-30.439088	0.375360
-16.628002	-21.086157	0.380365
-16.643681	-15.116808	0.385370
-16.895547	-9.790654	0.390374
-16.960286	-12.387359	0.395379
-17.959758	-21.734563	0.400384
-18.284567	-23.907705	0.405389
-18.582852	-29.856181	0.410394
-18.554520	-18.932984	0.415398
-18.371903	-15.804107	0.420403
-18.385591	-19.171273	0.425408
-18.650856	-11.251915	0.430413
-18.655621	-20.682209	0.435418
-19.419649	-16.962084	0.440422
-20.167108	-14.668238	0.445427
-19.841907	-15.430959	0.450432
-20.562132	-12.973701	0.455437
-20.304639	-13.713158	0.460442
-20.169005	-20.520562	0.465446
-21.192027	-16.367551	0.470451
-21.676206	-20.056465	0.475456
-22.018949	-19.553435	0.480461
-21.992808	-14.745404	0.485466
-21.868227	-12.518592	0.490470
-22.166577	-6.542914	0.495475
-21.918340	-11.052103	0.500480
-22.738930	-10.505839	0.505485
-23.032321	-17.657308	0.510490
-23.361344	-16.741978	0.515494
-23.433362	-14.414759	0.520499
-23.191403	-19.011547	0.525504
-24.054824	-12.697398	0.530509
-24.474751	-12.270859	0.535514
-24.555681	-13.327448	0.540518
-25.119293	-16.655904	0.545523
-24.682092	-13.718777	0.550528
-24.863632	-15.993461	0.555533
-25.564361	-15.431176	0.560538
-26.100742	-22.658464	0.565542
-26.407219	-15.197722	0.570547
-26.476511	-16.392175	0.575552
-26.496211	-15.446218	0.580557
-26.135368	-16.821962	0.585562
-26.555991	-16.281419	0.590566
-27.367515	-14.547008	0.595571
-27.421507	-18.920256	0.600576
-27.885534	-5.471169	0.605581
-27.685066	-22.852468	0.610586
-28.270823	-18.717351	0.615590
-28.963251	-17.593221	0.620595
-29.105070	-17.257714	0.625600
-29.324999	-11.939729	0.630605
-29.093749	-15.911583	0.635610
-29.315707	-22.814815	0.640614
-29.516139	-21.571621	0.645619
-29.388022	-21.069603	0.650624
-30.346765	-17.704944	0.655629
-30.678940	-23.097620	0.660634
-30.741606	-20.189739	0.665638
-30.641341	-17.111234	0.670643
-30.889548	-18.853455	0.675648
-31.749616	-20.246705	0.680653
-31.978788	-19.998751	0.685658
-32.024715	-18.865188	0.690662
-32.329312	-15.144282	0.695667
-32.469994	-11.294035	0.700672
-33.185859	-14.677728	0.705677
-33.265374	-16.414743	0.710682
-33.403894	-6.604344	0.715686
-33.587379	-3.259915	0.720691
-33.415573	-17.308468	0.725696
-33.700118	-16.200791	0.730701
-33.880908	-14.176067	0.735706
-34.262147	-15.467174	0.740710
-35.059222	-8.505360	0.745715
-34.812336	-16.345757	0.750720
-34.992698	-11.530679	0.755725
-35.885126	-16.927321	0.760730
-36.242417	-8.057076	0.765734
-36.518080	-16.350269	0.770739
-36.564219	-10.078755	0.775744
-36.510043	-11.434922	0.780749
-36.532855	-13.044781	0.785754
-36.316834	-13.138665	0.790758
-36.924890	-5.051700	0.795763
-37.285191	-16.931971	0.800768
-37.409923	-6.845323	0.805773
-38.152845	-14.555940	0.810778
-38.416953	-12.967413	0.815782
-39.250546	-1.909154	0.820787
-39.138747	-15.052967	0.825792
-39.146969	-5.357895	0.830797
-39.399604	-8.719259	0.835802
-39.497080	-10.728706	0.840806
-39.579368	-15.910602	0.845811
-39.217645	-6.672128	0.850816
-40.440814	-11.365216	0.855821
-40.825676	-16.736983	0.860826
-40.659453	-6.781345	0.865830
-40.941582	-12.197684	0.870835
-40.561576	-16.180191	0.875840
-41.265613	-6.531117	0.880845
-41.856073	-13.898630	0.885850
-42.151873	-5.892229	0.890854
-42.417298	-3.800459	0.895859
-42.199074	-14.309729	0.900864
-43.186227	-6.261441	0.905869
-43.398666	-2.608756	0.910874
-43.664081	-10.814972	0.915878
-43.914910	-8.564139	0.920883
-43.868909	-14.781697	0.925888
-44.335070	-13.262750	0.930893
-44.061339	-11.413647	0.935898
-43.843748	-6.309747	0.940902
-44.484106	-11.540242	0.945907
-45.101908	-11.326306	0.950912
-45.231345	-16.453357	0.955917
-45.129977	-14.096359	0.960922
-45.970183	-12.673826	0.965926
-46.790981	-4.436468	0.970931
-46.818753	-7.048457	0.975936
-46.901692	-6.851889	0.980941
-46.965444	-8.616684	0.985946
-46.715458	-0.838168	0.990950
-47.305715	-3.437953	0.995955
-47.154578	-13.228033	1.000960
-47.169607	-5.126421	1.005965
-47.795740	-9.226525	1.010970
-47.946579	-5.602476	1.015974
-48.597393	-5.956004	1.020979
-49.076925	-7.231710	1.025984
-49.604506	-4.510406	1.030989
-49.865512	-5.238224	1.035994
-49.630094	-12.668703	1.040998
-50.091691	-3.971937	1.046003
-49.833265	-13.082805	1.051008
-49.955000	-4.904362	1.056013
-50.015701	-10.412344	1.061018
-50.668169	-8.946461	1.066022
-51.211979	-1.388414	1.071027
-51.245386	-10.934445	1.076032
-51.809921	-9.472849	1.081037
-51.710387	-6.454340	1.086042
-51.700968	1.159391	1.091046
-52.327486	-5.781696	1.096051
-52.447535	-12.539547	1.101056
-52.765578	-5.636971	1.106061
-52.949664	-9.834812	1.111066
-53.769160	-3.926171	1.116070
-54.310952	-2.101144	1.121075
-53.372665	-13.631235	1.126080
-54.229872	-4.265043	1.131085
-54.278722	-11.198565	1.136090
-54.019401	-19.752751	1.141094
-54.597703	-16.229403	1.146099
-55.467320	-18.016622	1.151104
-55.511145	-11.223454	1.156109
-55.824228	-11.231269	1.161114
-55.854364	-16.823131	1.166118
-55.914138	1.520200	1.171123
-55.918702	-6.166907	1.176128
-56.365006	-6.179158	1.181133
-57.318629	-13.426489	1.186138
-57.521101	-6.760321	1.191142
-57.354516	-11.266207	1.196147
-57.180997	-11.432525	1.201152
-57.369713	0.277660	1.206157
-57.669930	-17.746521	1.211162
-58.121056	-10.677563	1.216166
-58.619692	-9.036467	1.221171
-58.797790	-13.418742	1.226176
-59.199188	-9.204942	1.231181
-59.946736	-16.702860	1.236186
-59.921381	-13.334209	1.241190
-60.179132	-6.621415	1.246195
-60.004092	-7.907936	1.251200
-60.421001	-4.792687	1.256205
-60.588979	-5.424349	1.261210
-60.386496	-12.549112	1.266214
-60.884238	-7.975367	1.271219
-61.271292	-9.521826	1.276224
-61.459447	-1.709460	1.281229
-61.802218	-1.649348	1.286234
-61.661007	-6.603675	1.291238
-61.938426	-5.313616	1.296243
-62.484270	-4.762942	1.301248
-62.970534	-1.285650	1.306253
-63.035813	-4.268247	1.311258
-62.739135	-3.602816	1.316262
-63.734630	-2.004089	1.321267
-64.015544	-2.928103	1.326272
-64.420275	-5.518990	1.331277
-64.440899	-2.073531	1.336282
-64.436584	-1.817868	1.341286
-64.850991	-2.616561	1.346291
-65.496208	-6.982592	1.351296
-66.012569	-2.836197	1.356301
-66.056693	-1.010056	1.361306
-65.716657	-11.250513	1.366310
-66.012861	-1.722288	1.371315
-65.887643	-10.034003	1.376320
-65.989563	1.153219	1.381325
-66.744235	-8.105790	1.386330
-66.883604	-9.615128	1.391334
-67.414601	-1.034037	1.396339
-67.423772	-0.792080	1.401344
-67.717868	-10.249806	1.406349
-68.837447	-4.373239	1.411354
-68.786510	-5.482127	1.416358
-69.044090	-5.726428	1.421363
-68.860360	-16.698525	1.426368
-68.864844	-10.623363	1.431373
-68.956832	-8.160138	1.436378
-69.018450	-12.035482	1.441382
-70.280200	3.417867	1.446387
-70.597815	-13.391876	1.451392
-70.543190	-9.670309	1.456397
-70.504792	-3.690449	1.461402
-70.459532	-8.436752	1.466406
-70.534680	-3.242691	1.471411
-71.244732	-13.255332	1.476416
-71.960686	-7.388226	1.481421
-71.961258	-8.707342	1.486426
-72.102868	-6.799487	1.491430
-72.014444	-8.781114	1.496435
-72.542970	-1.045130	1.501440
-73.002195	-7.047484	1.506445
-73.464783	-1.182111	1.511450
-72.989664	-6.413384	1.516454
-73.761356	-0.423648	1.521459
-73.223987	-4.652277	1.526464
-74.226970	-4.460242	1.531469
-74.505115	-3.394694	1.536474
-74.509372	-10.623103	1.541478
-75.115059	-3.605854	1.546483
-75.138112	-8.578733	1.551488
-75.112254	-2.793060	1.556493
-75.741970	-3.611799	1.561498
-75.870682	-8.647216	1.566502
-76.005721	-3.383660	1.571507
-76.075304	-4.603377	1.576512
-76.484472	-1.479849	1.581517
-77.576694	-8.667497	1.586522
-77.697696	-12.628448	1.591526
-77.762117	-6.610333	1.596531
-77.568310	-10.127069	1.601536
-77.946633	-9.365363	1.606541
-78.117870	-12.226952	1.611546
-77.889171	-15.284085	1.616550
-78.134000	-4.169387	1.621555
-78.826566	-12.261211	1.626560
-79.212885	-8.138358	1.631565
-79.317369	-4.657613	1.636570
-79.136425	-9.007562	1.641574
-80.041705	-8.631519	1.646579
-80.742298	-12.862320	1.651584
-80.935967	-10.474911	1.656589
-81.066777	-8.736427	1.661594
-81.080685	-10.154692	1.666598
-81.090351	-8.919243	1.671603
-81.030872	-8.058458	1.676608
-81.040055	-4.576827	1.681613
-81.889493	-0.650323	1.686618
-82.299451	-10.058256	1.691622
-82.733729	-7.443320	1.696627
-82.586269	-2.439164	1.701632
-82.524973	-10.993961	1.706637
-82.946119	-6.160136	1.711642
-83.691711	-10.744552	1.716646
-84.288183	-7.322757	1.721651
-84.137884	-10.997191	1.726656
-84.361439	-5.153456	1.731661
-84.407154	-0.565117	1.736666
-84.312454	-9.754734	1.741670
-84.520128	-6.118615	1.746675
-84.971832	-12.330952	1.751680
-85.326779	-7.751109	1.756685
-85.432907	-9.113795	1.761690
-85.255253	-9.037153	1.766694
-86.172759	-4.495710	1.771699
-86.604733	-9.682923	1.776704
-86.992500	-3.275620	1.781709
-87.657557	-0.361931	1.786714
-86.863321	-4.868091	1.791718
-86.846794	-6.335418	1.796723
-87.172776	-12.352320	1.801728
-87.774354	-15.187605	1.806733
-88.450487	0.461880	1.811738
-88.398807	-13.491918	1.816742
-88.977587	-10.518983	1.821747
-88.559709	-11.201316	1.826752
-89.200746	-14.558763	1.831757
-89.970162	-5.709363	1.836762
-89.813815	-4.142423	1.841766
-89.893276	0.697975	1.846771
-90.158384	-4.562842	1.851776
-90.233449	-7.442665	1.856781
-90.256338	7.389461	1.861786
-90.772691	-3.124931	1.866790
-91.104607	-5.825303	1.871795
-91.306231	-7.850066	1.876800
-91.469191	-4.328521	1.881805
-92.350809	-6.189787	1.886810
-91.985167	-9.701811	1.891814
-92.964122	-8.757404	1.896819
-92.930844	-12.676091	1.901824
-92.947462	-9.101548	1.906829
-93.030740	-1.976331	1.911834
-93.126039	-11.927110	1.916838
-93.105884	-7.159271	1.921843
-93.955396	-6.617959	1.926848
-94.311975	-6.451279	1.931853
-94.552991	-1.851321	1.936858
-94.332200	-7.976047	1.941862
-95.028400	-2.684671	1.946867
-95.029646	-8.439247	1.951872
-95.437555	-12.677943	1.956877
-95.857092	-1.583325	1.961882
-95.831412	-3.371624	1.966886
-95.698382	-3.791025	1.971891
-96.578020	-8.072863	1.976896
-96.941498	-13.368883	1.981901
-97.037581	-9.968549	1.986906
-97.354503	-17.154289	1.991910
-97.190548	-5.331694	1.996915
-97.396104	-11.215749	2.006912
-97.240898	-3.874801	2.016909
-97.298606	-3.390439	2.026906
-96.782928	-5.568171	2.036902
-96.111541	-8.685794	2.046899
-95.240330	-6.630044	2.056896
-94.697750	-5.992656	2.066893
-94.605337	-7.714426	2.076890
-94.435199	-13.294075	2.086886
-93.674963	-11.838656	2.096883
-92.371286	-8.441004	2.106880
-92.059744	-6.927948	2.116877
-92.141342	-5.625720	2.126874
-91.954772	-11.901690	2.136870
-90.788427	-12.778045	2.146867
-90.741076	-10.998679	2.156864
-89.702540	-5.614456	2.166861
-89.211297	-11.627723	2.176858
-89.134872	-12.244596	2.186854
-88.078389	-11.646551	2.196851
-87.631574	-10.278236	2.206848
-87.510748	-13.496488	2.216845
-87.310370	-18.646886	2.226842
-86.978965	-10.956582	2.236838
-85.815488	-12.684623	2.246835
-85.261603	-12.302429	2.256832
-84.892776	-16.408508	2.266829
-84.721300	-14.353988	2.276826
-84.184305	-20.713375	2.286822
-83.181215	-12.127297	2.296819
-82.726315	-9.965132	2.306816
-82.351563	-17.119556	2.316813
-82.157875	-10.380184	2.326810
-81.150599	-11.215774	2.336806
-80.888950	-8.947300	2.346803
-80.751030	-6.247627	2.356800
-79.794704	-12.599863	2.366797
-79.524207	-8.726706	2.376794
-78.646821	-3.858921	2.386790
-78.034125	-11.696862	2.396787
-77.937607	-8.962191	2.406784
-77.728506	-10.309439	2.416781
-76.769417	-9.290654	2.426778
-76.471380	-8.380530	2.436774
-75.797937	-9.680160	2.446771
-75.266412	-9.981873	2.456768
-74.913972	-11.509970	2.466765
-74.717197	-11.787741	2.476762
-73.915940	-8.586958	2.486758
-73.667525	-12.427083	2.496755
-73.011297	-11.012385	2.506752
-72.130139	-13.846096	2.516749
-71.654834	-12.555103	2.526746
-71.301393	-16.715792	2.536742
-70.585456	-19.118136	2.546739
-70.733912	-11.713768	2.556736
-70.004170	-10.842778	2.566733
-69.371604	-20.194866	2.576730
-68.952549	-15.112716	2.586726
-68.053999	-15.592314	2.596723
-67.804811	-7.239726	2.606720
-67.646214	-13.707716	2.616717
-66.756660	-7.549379	2.626714
-66.552505	-14.205072	2.636710
-65.648213	-17.783670	2.646707
-65.077051	-16.884664	2.656704
-65.043723	-6.990383	2.666701
-64.784896	-9.758259	2.676698
-64.218368	-3.660177	2.686694
-63.240707	-12.201533	2.696691
-62.715776	-11.041859	2.706688
-62.552794	-11.688134	2.716685
-61.849603	-8.693729	2.726682
-61.222329	-11.696733	2.736678
-61.207047	-8.170055	2.746675
-59.774046	-11.422852	2.756672
-59.613174	-14.492157	2.766669
-59.795919	-14.228955	2.776666
-59.051602	-12.400407	2.786662
-58.117802	-12.087243	2.796659
-58.010201	-11.125105	2.806656
-57.360431	-7.624986	2.816653
-56.987325	-9.245019	2.826650
-55.804839	-11.739473	2.836646
-55.566176	-9.967908	2.846643
-55.098040	-10.342050	2.856640
-55.041230	-13.737172	2.866637
-54.684478	-8.160584	2.876634
-53.864741	-16.873596	2.886630
-53.619593	-13.699716	2.896627
-52.636717	-9.187413	2.906624
-52.315740	-11.831978	2.916621
-51.918149	-10.072645	2.926618
-51.109642	-5.311272	2.936614
-50.824556	-9.515105	2.946611
-50.468969	-6.311011	2.956608
-49.498377	-9.367808	2.966605
-49.218764	2.309370	2.976602
-49.194354	-1.695230	2.986598
-48.200962	-5.085051	2.996595
-47.704566	-8.754958	3.006592
-47.336311	-7.713284	3.016589
-46.491122	-8.289056	3.026586
-46.333453	-5.788879	3.036582
-46.096021	-15.259620	3.046579
-45.551030	-11.445310	3.056576
-44.553752	-4.340837	3.066573
-44.516149	-4.489129	3.076570
-43.632114	-9.382356	3.086566
-43.411207	-9.603718	3.096563
-42.880480	-9.202054	3.106560
-42.113118	-7.864955	3.116557
-41.819769	-13.128124	3.126554
-41.202688	-9.340948	3.136550
-40.450070	-16.678124	3.146547
-40.388669	-5.654169	3.156544
-40.266950	-16.392904	3.166541
-39.203228	-18.580477	3.176538
-38.954309	-11.757890	3.186534
-38.038179	-13.016349	3.196531
-37.541276	-14.643107	3.206528
-37.528401	-12.519385	3.216525
-37.096605	-11.975507	3.226522
-36.067109	-15.383653	3.236518
-36.046758	-11.911622	3.246515
-35.176897	-15.617871	3.256512
-34.627466	-7.752647	3.266509
-34.548633	-8.639160	3.276506
-33.561962	-6.373413	3.286502
-32.975892	-10.649748	3.296499
-33.164367	-15.276722	3.306496
-32.247003	-12.296866	3.316493
-31.956733	-14.803572	3.326490
-31.234847	-11.438295	3.336486
-30.387968	-13.322628	3.346483
-30.300322	-15.531492	3.356480
-29.993563	-19.051307	3.366477
-28.990107	-11.269895	3.376474
-29.064697	-10.310886	3.386470
-28.417510	-10.459658	3.396467
-27.531637	-9.014415	3.406464
-27.334691	-10.822255	3.416461
-26.610310	-14.344151	3.426458
-26.024434	-12.611150	3.436454
-25.650175	-12.555600	3.446451
-25.530884	-18.418719	3.456448
-24.847564	-18.953287	3.466445
-24.146173	-12.724281	3.476442
-23.896646	-9.652454	3.486438
-22.942275	-9.171448	3.496435
-22.760434	-14.866973	3.506432
-22.485822	-15.413529	3.516429
-21.564571	-10.669820	3.526426
-21.384570	-15.899390	3.536422
-20.685065	-9.948852	3.546419
-19.911185	-24.901564	3.556416
-19.938848	-12.697909	3.566413
-19.592136	-8.146110	3.576410
-18.346381	-13.165702	3.586406
-18.085377	-14.799847	3.596403
-17.950459	-12.654065	3.606400
-17.170920	-11.017931	3.616397
-16.923147	-9.567739	3.626394
-16.451577	-12.546344	3.636390
-15.613333	-10.973260	3.646387
-15.274547	-7.712679	3.656384
-14.261656	-20.365012	3.666381
-13.943008	-15.650428	3.676378
-14.053175	-18.626580	3.686374
-13.827202	-20.331263	3.696371
-12.776143	-15.563543	3.706368
-11.872234	-18.942506	3.716365
-11.528417	-15.220216	3.726362
-11.219186	-10.969821	3.736358
-11.116981	-7.957273	3.746355
-9.986880	-11.514228	3.756352
-9.548076	-10.920762	3.766349
-9.601543	-12.752723	3.776346
-8.540014	-8.499823	3.786342
-7.867718	-8.101331	3.796339
-7.905313	-9.501791	3.806336
-7.514878	-14.482400	3.816333
-6.842588	-16.640317	3.826330
-6.126073	-15.000643	3.836326
-5.273890	-7.965296	3.846323
-5.216940	-12.041517	3.856320
-5.089329	-11.139533	3.866317
-4.734928	0.399220	3.876314
-4.009247	3.887454	3.886310
-3.441542	6.272704	3.896307
-2.566892	16.450163	3.906304
-2.509726	32.324711	3.916301
-2.275949	35.202611	3.926298
-1.988854	53.081215	3.936294
-1.296428	69.683059	3.946291
-0.804358	89.065971	3.956288
-0.313440	100.887510	3.966285
0.000000	116.355543	3.971290
0.402892	116.251363	3.976294
0.820154	130.685607	3.981299
0.217685	141.293287	3.986304
0.671753	129.892758	3.991309
0.769390	159.686589	3.996314
0.891709	143.756887	4.001318
1.032055	157.978276	4.006323
1.352699	165.113043	4.011328
1.320584	162.175840	4.016333
1.238598	153.567478	4.021338
1.443002	149.153702	4.026342
1.522516	152.418987	4.031347
0.765161	146.061485	4.036352
1.224930	141.474821	4.041357
1.268247	156.072082	4.046362
1.117506	133.927229	4.051366
1.142386	138.906344	4.056371
1.138664	151.812026	4.061376
1.788241	154.117955	4.066381
1.442996	149.470758	4.071386
1.188928	137.086513	4.076390
1.303073	134.290914	4.081395
1.186960	132.875994	4.086400
1.121678	132.854661	4.091405
0.810637	132.647206	4.096410
0.970091	146.574525	4.101414
1.481021	154.717191	4.106419
1.406263	162.932645	4.111424
1.551707	151.317866	4.116429
1.492279	162.084082	4.121434
1.451782	161.767798	4.126438
1.084387	163.071965	4.131443
1.336719	165.427482	4.136448
1.613561	159.901360	4.141453
1.389010	163.682527	4.146458
1.287070	157.060977	4.151462
1.723374	163.196852	4.156467
1.490866	159.968342	4.161472
1.441731	157.002169	4.166477
1.403491	166.528033	4.171482
1.289740	164.672976	4.176486
1.545097	160.336635	4.181491
1.694237	155.684742	4.186496
1.858765	156.465801	4.191501
1.470595	148.541334	4.196506
1.343657	144.995727	4.201510
1.569724	163.458963	4.206515
1.486203	157.919701	4.211520
1.360798	160.305928	4.216525
1.288080	162.085947	4.221530
1.504025	161.587113	4.226534
1.345565	173.305330	4.231539
1.329396	158.400230	4.236544
1.637907	153.808789	4.241549
1.322184	167.250589	4.246554
1.620738	174.645087	4.251558
1.430922	185.444402	4.256563
1.680841	188.129333	4.261568
1.747551	180.149398	4.266573
1.629792	189.311244	4.271578
1.733473	188.377579	4.276582
1.729186	186.344016	4.281587
1.859199	193.594086	4.286592
2.064774	184.054795	4.291597
1.549144	191.089647	4.296602
1.797115	185.457308	4.301606
2.291133	190.362931	4.306611
2.037776	188.336755	4.311616
2.271555	184.522650	4.316621
1.890771	171.465367	4.321626
1.784134	159.668614	4.326630
1.601450	167.344156	4.331635
1.582045	173.051560	4.336640
2.048387	175.889242	4.341645
1.832675	186.202230	4.346650
1.861719	178.354749	4.351654
2.203343	179.740817	4.356659
2.155249	189.692183	4.361664
2.060062	190.773366	4.366669
1.799606	193.734420	4.371674
1.976650	187.907547	4.376678
2.148956	191.344964	4.381683
1.867735	185.270353	4.386688
2.251108	185.646962	4.391693
2.142530	200.869176	4.396698
2.235512	194.767568	4.401702
1.984340	181.515962	4.406707
2.152965	189.313641	4.411712
2.491601	184.894644	4.416717
1.926745	182.183278	4.421722
1.784817	179.263278	4.426726
2.547003	186.888861	4.431731
2.063556	184.617161	4.436736
2.340603	178.467736	4.441741
1.859375	180.330746	4.446746
2.105617	188.011859	4.451750
2.407084	191.726433	4.456755
2.297783	194.897923	4.461760
2.307321	190.710823	4.466765
2.258793	198.314738	4.471770
2.243781	183.665702	4.476774
2.010319	180.415192	4.481779
1.856964	188.994152	4.486784
2.089034	185.170823	4.491789
2.154015	194.360987	4.496794
2.228424	196.266655	4.501798
2.175090	185.416995	4.506803
1.902488	193.815324	4.511808
2.324122	181.730140	4.516813
2.047922	199.465346	4.521818
2.122770	198.137562	4.526822
2.279351	195.101184	4.531827
2.586086	208.205039	4.536832
2.382589	208.442645	4.541837
2.692037	204.980514	4.546842
2.507718	200.713053	4.551846
2.374676	193.090280	4.556851
2.070689	194.840099	4.561856
2.575540	210.219310	4.566861
2.232436	211.785432	4.571866
2.380128	213.031044	4.576870
2.659316	222.311048	4.581875
2.160647	219.845573	4.586880
2.754795	217.104468	4.591885
2.622721	219.330395	4.596890
2.586366	216.514071	4.601894
2.879412	218.217803	4.606899
2.570707	217.405698	4.611904
2.665283	217.327679	4.616909
2.512700	209.793383	4.621914
2.666560	217.770560	4.626918
2.802991	218.612972	4.631923
2.945313	218.169965	4.636928
2.890470	216.979559	4.641933
2.513202	203.744529	4.646938
2.497246	207.910642	4.651942
2.699036	213.441031	4.656947
2.803176	213.089429	4.661952
2.855215	220.313761	4.666957
2.924065	223.052378	4.671962
2.797499	213.618896	4.676966
2.745869	191.217996	4.681971
2.458466	201.792164	4.686976
3.026161	207.610073	4.691981
3.013447	221.358780	4.696986
2.941184	199.945039	4.701990
2.866993	195.457843	4.706995
2.337463	205.006920	4.712000
2.764739	211.634612	4.717005
2.574936	221.763226	4.722010
2.662520	218.959120	4.727014
2.790004	219.698529	4.732019
2.813354	221.523614	4.737024
2.934387	218.666810	4.742029
2.848268	226.251317	4.747034
2.552193	208.963408	4.752038
2.449027	223.001538	4.757043
2.754163	216.809734	4.762048
2.785216	218.013510	4.767053
2.947724	233.547621	4.772058
3.304594	237.013077	4.777062
3.084557	216.552623	4.782067
2.771418	223.533614	4.787072
3.036530	222.830920	4.792077
3.048158	238.246306	4.797082
3.489070	233.460091	4.802086
3.058760	223.678721	4.807091
2.781640	221.399998	4.812096
3.018019	238.953690	4.817101
3.120239	243.300614	4.822106
3.250015	245.241905	4.827110
3.716952	241.755091	4.832115
2.947783	235.013426	4.837120
3.158233	221.512290	4.842125
2.770271	239.733287	4.847130
2.839619	231.408063	4.852134
2.872670	241.685270	4.857139
3.004901	245.356769	4.862144
3.460642	242.406389	4.867149
3.019854	248.227297	4.872154
3.164858	253.133838	4.877158
3.167706	249.900074	4.882163
3.037017	251.926469	4.887168
3.120841	250.856705	4.892173
3.539700	252.040849	4.897178
3.424898	247.999769	4.902182
3.529092	236.400889	4.907187
2.907770	249.988710	4.912192
3.082828	248.135850	4.917197
3.081484	248.572739	4.922202
3.205000	246.107853	4.927206
3.979678	258.755608	4.932211
3.632343	253.567703	4.937216
3.497284	248.049143	4.942221
3.287244	253.441588	4.947226
3.372759	250.277130	4.952230
3.502821	242.432776	4.957235
3.218093	249.368196	4.962240
3.518247	248.213916	4.967245
3.397744	251.934507	4.972250
3.365454	249.345333	4.977254
3.737966	261.163914	4.982259
3.744737	256.727293	4.987264
3.626942	251.816638	4.992269
3.161704	252.544513	4.997274
3.476703	258.765867	5.002278
3.660533	269.794595	5.007283
3.620866	280.029433	5.012288
3.927124	269.025303	5.017293
3.848635	257.492998	5.022298
3.435236	250.955014	5.027302
3.379042	253.108944	5.032307
3.460852	267.852127	5.037312
3.874332	275.079962	5.042317
3.895689	273.393552	5.047322
3.335310	267.720161	5.052326
3.499385	269.194167	5.057331
3.331774	278.430309	5.062336
3.646042	272.401572	5.067341
3.919340	276.968475	5.072346
3.777934	275.573326	5.077350
3.846999	273.597864	5.082355
3.706416	278.697857	5.087360
3.986640	271.342497	5.092365
3.951168	271.259544	5.097370
3.979876	280.581988	5.102374
3.955655	272.565639	5.107379
3.690694	281.317156	5.112384
4.155742	272.825508	5.117389
3.755738	272.277645	5.122394
3.849353	278.837418	5.127398
3.955377	278.362131	5.132403
3.766527	280.369168	5.137408
4.021997	273.884565	5.142413
3.879126	280.345349	5.147418
3.845792	274.488135	5.152422
4.215047	270.969164	5.157427
3.787211	284.520368	5.162432
4.182150	275.698014	5.167437
3.940883	276.482547	5.172442
3.775492	268.852155	5.177446
4.001700	270.113943	5.182451
3.720403	271.686205	5.187456
4.136526	267.631537	5.192461
3.930254	274.700209	5.197466
3.925417	274.194835	5.202470
4.153789	271.343352	5.207475
3.942557	275.907077	5.212480
3.941605	283.057479	5.217485
3.730010	282.562354	5.222490
3.418028	277.587204	5.227494
4.190718	279.858042	5.232499
4.025117	297.927198	5.237504
4.266502	293.045677	5.242509
4.163936	303.742807	5.247514
4.225299	301.531264	5.252518
4.590377	303.584392	5.257523
4.245772	301.290922	5.262528
4.258754	290.857921	5.267533
4.361518	290.690032	5.272538
4.418017	289.422064	5.277542
4.177572	279.993735	5.282547
4.242441	281.268147	5.287552
4.470069	276.692511	5.292557
4.410254	278.587580	5.297562
3.895556	274.963496	5.302566
4.104469	280.176411	5.307571
3.826440	297.709518	5.312576
4.404103	304.595261	5.317581
4.111901	306.979167	5.322586
4.388468	308.223576	5.327590
4.269884	298.678066	5.332595
4.199287	299.641506	5.337600
4.072026	299.522313	5.342605
4.512489	308.065238	5.347610
4.655471	305.448595	5.352614
4.951462	298.271090	5.357619
4.528578	303.842435	5.362624
4.404748	308.857552	5.367629
4.374426	311.330143	5.372634
4.426127	304.662318	5.377638
4.238194	296.905730	5.382643
4.299676	294.887160	5.387648
4.680548	302.202374	5.392653
4.570165	306.677539	5.397658
4.518277	303.860471	5.402662
4.438032	305.480329	5.407667
4.336175	311.545550	5.412672
4.748983	306.624512	5.417677
4.646644	299.939695	5.422682
4.641780	306.344063	5.427686
4.753644	300.403978	5.432691
4.742129	309.397377	5.437696
4.810916	303.479860	5.442701
4.826096	305.578320	5.447706
4.192952	309.164106	5.452710
4.656159	303.928283	5.457715
4.652140	310.357830	5.462720
5.109878	321.634742	5.467725
4.863926	312.289518	5.472730
4.891714	313.167940	5.477734
4.830249	296.295610	5.482739
4.839302	306.791753	5.487744
4.483825	296.030496	5.492749
4.484473	307.053146	5.497754
4.408495	308.280025	5.502758
5.020805	324.506216	5.507763
4.525648	326.573906	5.512768
4.958743	319.431860	5.517773
4.705909	327.922068	5.522778
4.920018	327.246344	5.527782
5.032871	323.612510	5.532787
4.519537	331.396878	5.537792
4.557048	328.682860	5.542797
5.095822	327.222264	5.547802
5.222671	330.518131	5.552806
5.247665	340.840950	5.557811
5.061478	331.948267	5.562816
4.877224	327.332747	5.567821
5.008319	337.778148	5.572826
4.866448	333.668523	5.577830
5.158290	332.860394	5.582835
5.179580	336.236078	5.587840
5.089762	340.075267	5.592845
4.903735	333.004910	5.597850
4.758288	333.477035	5.602854
5.272635	329.663232	5.607859
4.844333	341.784513	5.612864
4.796339	334.822244	5.617869
4.715606	329.276164	5.622874
4.736192	330.203173	5.627878
5.284661	328.421514	5.632883
5.172434	347.083480	5.637888
5.067343	342.686510	5.642893
5.052888	341.492932	5.647898
4.967682	351.962740	5.652902
5.300206	348.421035	5.657907
5.163378	356.722235	5.662912
5.158169	358.675197	5.667917
5.280446	357.191270	5.672922
5.367062	357.611216	5.677926
5.481173	350.389420	5.682931
5.305883	352.698066	5.687936
5.442966	356.954132	5.692941
4.914750	351.218726	5.697946
4.994222	351.785326	5.702950
5.234579	353.677665	5.707955
5.202847	356.612399	5.712960
5.156113	345.843867	5.717965
5.306708	363.354174	5.722970
5.206683	346.899133	5.727974
4.988778	357.092338	5.732979
4.982585	355.872154	5.737984
5.357480	355.003555	5.742989
5.595929	370.997295	5.747994
5.118074	372.951546	5.752998
5.587488	381.875956	5.758003
5.416468	379.928607	5.763008
5.891101	378.414781	5.768013
5.333315	373.971673	5.773018
5.589620	372.248442	5.778022
5.625720	366.358172	5.783027
5.370904	368.312278	5.788032
5.512575	378.177068	5.793037
5.492343	376.538295	5.798042
5.646201	386.451801	5.803046
5.710045	382.708573	5.808051
5.676524	382.150742	5.813056
5.764971	377.837337	5.818061
5.354874	373.472330	5.823066
5.290431	381.195878	5.828070
5.929900	374.818755	5.833075
5.590929	377.751011	5.838080
5.945332	383.589741	5.843085
5.846636	380.757848	5.848090
5.793827	384.281195	5.853094
5.548774	374.638398	5.858099
5.423964	374.113853	5.863104
5.713602	381.142833	5.868109
5.427873	385.360747	5.873114
5.627995	381.808142	5.878118
5.886996	377.692645	5.883123
5.650501	389.284023	5.888128
5.602535	389.335907	5.893133
5.896889	389.505002	5.898138
5.529534	396.282579	5.903142
5.618801	392.472089	5.908147
5.286165	384.447064	5.913152
5.688969	385.611587	5.918157
5.945912	384.758304	5.923162
5.717416	389.992328	5.928166
5.749232	394.597097	5.933171
5.997864	411.864296	5.938176
6.221802	404.387984	5.943181
5.904128	401.789718	5.948186
5.691997	396.577423	5.953190
6.189469	404.023110	5.958195
5.868035	413.871893	5.963200
6.223210	407.241904	5.968205
6.015886	397.340078	5.973210
5.763172	398.303583	5.978214
5.852763	404.130028	5.983219
6.005646	413.423593	5.988224
6.307458	411.104758	5.993229
6.256502	405.351505	5.998234
6.040079	400.579652	6.003238
5.868278	389.267530	6.008243
5.824383	396.817018	6.013248
5.927138	400.739945	6.018253
6.396415	400.941745	6.023258
5.910981	403.482493	6.028262
5.902677	392.128933	6.033267
6.000989	394.439009	6.038272
5.837841	391.101511	6.043277
6.167879	405.391455	6.048282
5.937349	402.051857	6.053286
6.006493	398.206553	6.058291
5.845195	407.666404	6.063296
6.001937	408.385418	6.068301
6.246756	410.783275	6.073306
6.078685	404.222615	6.078310
5.998870	395.553683	6.083315
5.776405	393.652359	6.088320
5.955450	402.900691	6.093325
6.407231	405.743856	6.098330
6.322556	395.009713	6.103334
6.146096	391.943225	6.108339
5.457799	389.058176	6.113344
5.722945	390.006982	6.118349
6.051758	392.818790	6.123354
5.838979	398.328770	6.128358
6.046285	411.903943	6.133363
6.408879	415.931697	6.138368
6.376130	397.118515	6.143373
6.526287	393.010578	6.148378
5.948929	392.781569	6.153382
6.145212	379.124343	6.158387
5.779354	386.550264	6.163392
5.749116	396.353412	6.168397
5.833654	385.289037	6.173402
5.939807	392.270838	6.178406
6.153038	387.994828	6.183411
5.649303	394.145191	6.188416
5.617821	391.223669	6.193421
5.939713	396.950437	6.198426
6.011540	412.378688	6.203430
6.194736	405.184011	6.208435
5.838987	400.747206	6.213440
5.762134	406.080864	6.218445
6.296481	417.763458	6.223450
6.483235	409.024279	6.228454
6.038032	382.309244	6.233459
5.995327	385.979707	6.238464
5.955881	393.629740	6.243469
6.033228	386.448492	6.248474
6.140157	386.735539	6.253478
6.249613	387.541057	6.258483
6.008221	394.998100	6.263488
6.251533	393.982434	6.268493
5.961265	397.849879	6.273498
6.110815	390.669972	6.278502
6.388801	388.652271	6.283507
6.152358	391.568464	6.288512
6.102935	389.390087	6.293517
6.263790	390.026197	6.298522
5.863412	387.431400	6.303526
6.150807	391.448784	6.308531
6.226301	391.187089	6.313536
6.193047	392.239598	6.318541
6.257024	395.728829	6.323546
5.605483	389.819741	6.328550
5.778047	387.818558	6.333555
5.735957	383.617355	6.338560
5.930654	384.485448	6.343565
6.085634	379.943315	6.348570
5.942299	384.331911	6.353574
6.062582	386.192446	6.358579
6.396085	390.980904	6.363584
5.869074	388.833063	6.368589
6.004546	388.596773	6.373594
5.947184	395.869956	6.378598
5.953508	388.041761	6.383603
5.948450	388.406468	6.388608
5.443972	384.473870	6.393613
5.712013	389.702862	6.398618
5.335284	387.164473	6.403622
6.270533	388.283537	6.408627
5.711281	387.412602	6.413632
5.673251	377.661435	6.418637
6.034945	394.414184	6.423642
5.984667	403.802852	6.428646
6.054078	386.998518	6.433651
5.877967	390.519038	6.438656
5.965853	390.540145	6.443661
6.059755	411.526924	6.448666
6.081710	406.287440	6.453670
6.023140	399.693806	6.458675
5.988776	394.823825	6.463680
5.834850	395.110615	6.468685
6.107941	405.024433	6.473690
6.213127	406.014121	6.478694
6.138583	396.657815	6.483699
5.913081	384.977615	6.488704
5.939847	395.398267	6.493709
5.624007	383.349401	6.498714
6.094041	400.676814	6.503718
6.041771	394.980719	6.508723
6.153303	388.847664	6.513728
6.165872	391.025639	6.518733
5.918319	388.093679	6.523738
5.665709	386.279339	6.528742
6.172540	397.716290	6.533747
6.066554	393.183405	6.538752
5.984862	395.553322	6.543757
5.849857	397.634195	6.548762
6.280216	412.253281	6.553766
6.293107	391.291050	6.558771
6.089616	395.363201	6.563776
6.167343	390.421874	6.568781
6.033887	393.049843	6.573786
5.701272	396.123477	6.578790
5.999727	384.661746	6.583795
6.117097	382.922317	6.588800
6.252366	383.309330	6.593805
6.145742	380.263540	6.598810
5.940893	389.625799	6.603814
5.983895	384.072970	6.608819
5.728814	386.128362	6.613824
6.022163	390.021424	6.618829
6.068887	377.238698	6.623834
5.931543	388.283019	6.628838
6.009849	387.539985	6.633843
5.998097	391.224582	6.638848
5.994122	388.352536	6.643853
6.238238	386.798896	6.648858
5.994595	390.187625	6.653862
5.910808	385.606970	6.658867
5.860784	389.987275	6.663872
5.914622	390.187727	6.668877
6.142157	393.727262	6.673882
5.848318	389.954652	6.678886
6.086165	384.225759	6.683891
6.088252	391.084657	6.688896
6.268499	392.571959	6.693901
6.230645	393.182254	6.698906
5.980062	398.239403	6.703910
6.036605	393.671560	6.708915
5.914628	390.694614	6.713920
5.787079	394.577693	6.718925
5.676641	381.806934	6.723930
5.821873	392.905061	6.728934
6.108899	383.947699	6.733939
6.054107	385.225049	6.738944
6.041655	391.165555	6.743949
6.257908	389.201820	6.748954
6.017825	392.542536	6.753958
6.351736	389.873818	6.758963
5.878583	391.634341	6.763968
5.935861	387.525138	6.768973
6.147241	381.167630	6.773978
5.794382	382.950435	6.778982
5.919762	391.542768	6.783987
6.135862	390.743341	6.788992
5.923469	391.624597	6.793997
5.758289	387.853976	6.799002
5.709366	383.176108	6.804006
5.830500	385.906558	6.809011
6.069829	381.284768	6.814016
5.739558	391.884748	6.819021
6.358785	389.357992	6.824026
6.354485	389.491621	6.829030
6.363193	382.466665	6.834035
6.349366	388.799699	6.839040
6.156745	390.630165	6.844045
6.033176	386.125347	6.849050
6.184815	391.265008	6.854054
5.797276	379.705115	6.859059
5.812515	380.613981	6.864064
6.026680	390.109908	6.869069
6.337488	391.652685	6.874074
6.187413	386.810327	6.879078
5.884546	387.807001	6.884083
5.650148	397.347903	6.889088
5.847003	390.258663	6.894093
6.286779	396.969889	6.899098
6.161774	389.978536	6.904102
6.098363	392.851799	6.909107
5.887510	383.368157	6.914112
6.359078	388.201422	6.919117
6.145925	376.462345	6.924122
6.128121	389.677295	6.929126
5.856168	390.982343	6.934131
5.816688	391.630859	6.939136
5.645146	382.372017	6.944141
6.180392	382.829241	6.949146
5.974866	386.901709	6.954150
6.067887	380.081846	6.959155
6.139751	395.222169	6.964160
5.954954	393.403531	6.969165
6.002775	384.641838	6.974170
6.034486	385.171630	6.979174
6.099857	388.230362	6.984179
6.175329	386.728456	6.989184
6.140538	393.852566	6.994189
6.250326	386.922504	6.999194
6.042631	394.048395	7.004198
5.976576	380.998594	7.009203
6.046549	378.494621	7.014208
6.052679	385.194693	7.019213
6.038235	363.838136	7.024218
5.790701	369.011860	7.029222
5.733381	384.985515	7.034227
6.218140	384.004786	7.039232
6.087431	382.209312	7.044237
6.195109	376.712792	7.049242
5.924404	368.450276	7.054246
6.252445	373.236421	7.059251
6.107375	368.023119	7.064256
5.796229	368.654086	7.069261
6.194634	354.193240	7.074266
5.901313	364.809561	7.079270
5.862157	358.168607	7.084275
5.591130	368.547316	7.089280
5.683194	379.068460	7.094285
6.213815	376.992195	7.099290
6.039290	385.482816	7.104294
6.002596	389.772445	7.109299
6.023745	389.357911	7.114304
5.906409	390.812743	7.119309
6.139825	378.734770	7.124314
5.868753	387.917575	7.129318
5.694184	389.855947	7.134323
5.678056	381.078965	7.139328
5.723863	379.771536	7.144333
5.914130	380.931394	7.149338
5.977762	391.966375	7.154342
5.862096	385.796151	7.159347
5.957298	386.183115	7.164352
5.963650	384.511701	7.169357
6.276718	386.247115	7.174362
6.072610	378.271559	7.179366
5.718652	372.825224	7.184371
5.978424	386.452270	7.189376
5.869435	379.996259	7.194381
6.050297	371.897111	7.199386
5.877257	375.489915	7.204390
5.983133	381.740915	7.209395
5.898870	376.824972	7.214400
5.932917	389.395872	7.219405
6.048343	386.615852	7.224410
5.731853	391.721292	7.229414
6.017641	385.241390	7.234419
6.303685	382.105602	7.239424
6.118491	389.006498	7.244429
5.863018	390.131790	7.249434
5.806477	389.764230	7.254438
6.112725	383.287451	7.259443
6.094215	382.917097	7.264448
6.026722	378.957162	7.269453
5.976967	379.800279	7.274458
5.993638	387.916089	7.279462
5.852601	374.637591	7.284467
6.118467	387.646740	7.289472
6.091498	387.483359	7.294477
6.224686	381.318439	7.299482
5.978175	384.445021	7.304486
6.181730	386.238723	7.309491
6.044375	394.521041	7.314496
5.853399	389.634470	7.319501
5.967095	392.027558	7.324506
6.160665	387.653387	7.329510
5.924739	381.394438	7.334515
6.048809	388.107670	7.339520
6.009528	400.784981	7.344525
6.263865	381.360512	7.349530
6.070966	397.244687	7.354534
5.980143	390.880740	7.359539
6.340430	387.736482	7.364544
6.135147	393.681892	7.369549
5.979953	384.721049	7.374554
5.971429	390.518568	7.379558
5.986791	387.323948	7.384563
5.920969	398.233680	7.389568
5.985463	397.904105	7.394573
6.353119	390.307203	7.399578
6.048708	389.893057	7.404582
5.929524	391.401963	7.409587
6.008236	391.560552	7.414592
6.187913	388.403462	7.419597
6.410528	387.856120	7.424602
6.223428	385.072880	7.429606
6.230343	374.134570	7.434611
5.907729	370.705000	7.439616
5.520832	365.789021	7.444621
6.152884	363.320371	7.449626
5.787757	392.639759	7.454630
6.045901	390.239182	7.459635
6.179971	387.665052	7.464640
6.175478	385.830820	7.469645
6.092102	375.071175	7.474650
5.829831	368.151958	7.479654
5.769479	368.335499	7.484659
5.872234	379.756655	7.489664
5.892840	398.641475	7.494669
5.939436	389.114329	7.499674
5.798127	392.449059	7.504678
6.151419	390.868821	7.509683
6.098294	385.811953	7.514688
6.083920	393.882009	7.519693
6.151469	384.228193	7.524698
6.141461	389.136913	7.529702
6.241078	386.052480	7.534707
6.157149	368.471743	7.539712
6.019854	376.418679	7.544717
5.813818	368.443429	7.549722
5.662625	375.263061	7.554726
5.944607	381.321950	7.559731
6.028211	391.192681	7.564736
6.256682	387.505917	7.569741
6.298472	377.305638	7.574746
6.027781	373.086470	7.579750
6.117222	368.285685	7.584755
6.274694	368.400295	7.589760
6.185232	365.313853	7.594765
6.170037	365.170774	7.599770
5.814382	371.259962	7.604774
5.832814	370.067556	7.609779
5.774828	368.732097	7.614784
5.893207	359.617670	7.619789
6.254155	364.578994	7.624794
5.747715	366.069479	7.629798
5.993222	362.804001	7.634803
6.026859	360.767640	7.639808
5.837090	358.180979	7.644813
6.483041	350.629076	7.649818
5.934857	359.757207	7.654822
5.873210	359.317681	7.659827
5.751055	366.553547	7.664832
5.465988	370.948527	7.669837
5.745759	386.141690	7.674842
5.934360	385.704083	7.679846
6.234009	390.709820	7.684851
6.117751	391.936689	7.689856
6.417317	395.180196	7.694861
5.989341	385.218034	7.699866
5.409513	377.079880	7.704870
5.960717	386.114865	7.709875
6.179898	388.580012	7.714880
5.839855	400.083215	7.719885
6.264938	392.470986	7.724890
5.984584	396.007841	7.729894
5.789480	391.235814	7.734899
6.157414	393.794715	7.739904
5.821807	397.710394	7.744909
6.557842	387.391841	7.749914
6.232528	388.717904	7.754918
5.975700	373.913608	7.759923
5.941898	362.991176	7.764928
5.719699	368.059689	7.769933
6.186358	373.709982	7.774938
6.290637	363.658110	7.779942
5.907537	372.358578	7.784947
5.790480	363.398099	7.789952
5.801419	369.265329	7.794957
5.906744	377.474813	7.799962
6.248594	384.207706	7.804966
6.355501	380.255247	7.809971
6.051062	373.684327	7.814976
5.903396	366.807266	7.819981
5.848802	367.046854	7.824986
6.057317	368.346223	7.829990
5.955040	359.392921	7.834995
6.174011	365.278176	7.840000
6.113554	363.101531	7.845005
5.892794	362.933712	7.850010
5.771985	359.763596	7.855014
6.038616	360.743805	7.860019
6.261299	371.203350	7.865024
6.139665	376.967966	7.870029
5.748006	377.076865	7.875034
5.690265	364.753450	7.880038
5.969124	370.844462	7.885043
5.861177	378.160366	7.890048
5.760755	390.565670	7.895053
6.242508	387.025887	7.900058
5.790603	396.214883	7.905062
5.959021	396.077836	7.910067
6.390782	386.465032	7.915072
6.344331	390.556870	7.920077
6.265942	376.680086	7.925082
5.921469	371.545482	7.930086
6.043553	363.376452	7.935091
5.782064	361.107917	7.940096
5.788208	366.279860	7.945101
5.954679	365.965945	7.950106
5.836703	374.485666	7.955110
5.856735	375.235591	7.960115
6.261319	378.627158	7.965120
6.203039	392.234438	7.970125
6.464516	382.177045	7.975142
5.973996	371.505521	7.980160
5.962894	366.679053	7.985178
6.165463	362.567019	7.990195
5.905945	367.745300	7.995213
6.093041	361.455074	8.000230
5.639402	379.605464	8.005248
5.946888	369.963909	8.010266
6.189766	371.999251	8.015283
6.008190	378.796842	8.020301
5.722030	359.468664	8.025318
5.863490	379.696961	8.030336
6.036358	381.986266	8.035354
6.297433	390.156680	8.040371
6.151165	395.793742	8.045389
6.160647	391.257527	8.050406
6.415589	385.193344	8.055424
6.257997	376.719697	8.060442
6.336978	368.890627	8.065459
6.277108	368.423567	8.070477
5.969005	371.397288	8.075494
6.160584	368.962672	8.080512
5.792218	370.648827	8.085530
6.390113	360.620954	8.090547
5.933681	367.259638	8.095565
5.771654	365.732477	8.100582
6.099584	374.615072	8.105600
6.108836	374.386485	8.110618
6.097595	369.408563	8.115635
5.975352	381.918216	8.120653
6.140890	383.482849	8.125670
6.510430	398.048742	8.130688
5.877667	392.120488	8.135706
6.316762	385.541466	8.140723
6.113440	400.354905	8.145741
6.438014	386.885900	8.150758
6.283966	385.000888	8.155776
6.100145	377.907254	8.160794
6.277926	366.954300	8.165811
6.067665	368.931256	8.170829
6.122478	375.458282	8.175846
5.894348	387.956128	8.180864
5.985591	389.582895	8.185882
6.359271	380.694652	8.190899
6.356621	397.218617	8.195917
6.675332	389.920011	8.200934
6.305661	383.101643	8.205952
5.823182	382.423092	8.210970
6.479260	381.903814	8.215987
6.147426	395.153202	8.221005
6.162184	401.008028	8.226022
5.986387	393.042146	8.231040
5.949538	398.677844	8.236058
6.286023	390.022638	8.241075
6.466951	397.564997	8.246093
6.254918	392.400783	8.251110
6.285735	396.697310	8.256128
6.357684	393.744958	8.261146
6.603006	388.969824	8.266163
6.362724	393.286737	8.271181
6.034118	387.900952	8.276198
6.139942	386.650551	8.281216
6.191382	392.231389	8.286234
6.365157	390.998743	8.291251
6.077870	386.745708	8.296269
6.404152	391.018030	8.301286
6.379283	389.362081	8.306304
6.278944	393.111123	8.311322
6.251375	391.086375	8.316339
6.065957	401.078189	8.321357
6.414467	400.856405	8.326374
6.330917	399.878667	8.331392
6.419430	390.937272	8.336410
6.423080	401.057250	8.341427
6.401644	391.041194	8.346445
6.272327	383.503526	8.351462
6.230755	393.668454	8.356480
6.010347	394.996918	8.361498
6.426736	392.372444	8.366515
6.185173	400.747847	8.371533
6.512167	399.109349	8.376550
6.338876	395.532715	8.381568
6.278413	397.533539	8.386586
6.531504	409.918133	8.391603
6.746215	398.833143	8.396621
6.394662	393.605584	8.401638
6.805633	400.108373	8.406656
6.600290	404.003255	8.411674
6.503325	392.241282	8.416691
6.416894	398.948235	8.421709
6.340576	393.762756	8.426726
6.487416	385.493866	8.431744
6.539919	397.711068	8.436762
6.461869	404.751218	8.441779
6.240231	401.914292	8.446797
6.341339	399.411798	8.451814
6.622703	392.008592	8.456832
6.544810	394.248827	8.461850
6.603831	386.804722	8.466867
6.479285	395.584658	8.471885
6.451334	391.543448	8.476902
6.539614	379.648319	8.481920
6.257634	402.609590	8.486938
6.865859	403.981789	8.491955
6.462444	396.263004	8.496973
6.424427	399.961258	8.501990
6.616373	408.975628	8.507008
6.660714	397.765857	8.512026
6.762233	395.509448	8.517043
6.568156	393.542345	8.522061
6.357476	388.235912	8.527078
6.622350	385.389030	8.532096
6.791991	394.990701	8.537114
6.712169	394.034470	8.542131
6.353978	392.465459	8.547149
6.049976	401.983558	8.552166
6.850154	401.132438	8.557184
6.655845	415.228123	8.562202
6.917131	412.078848	8.567219
6.802748	411.430983	8.572237
6.568526	412.603826	8.577255
6.636244	396.741977	8.582272
6.465424	409.593769	8.587290
6.288788	408.860986	8.592307
6.887943	419.610335	8.597325
6.748681	421.705558	8.602343
6.863015	421.602514	8.607360
6.475545	419.820342	8.612378
6.706625	422.160490	8.617395
7.008753	418.749199	8.622413
6.640995	409.813013	8.627431
6.818117	408.298980	8.632448
6.810621	399.252706	8.637466
6.412172	396.989427	8.642483
6.491012	406.968241	8.647501
6.631716	408.618817	8.652519
6.788938	408.865653	8.657536
6.496014	418.877477	8.662554
6.691710	421.889033	8.667571
6.725835	422.562248	8.672589
6.811229	423.492513	8.677607
7.010193	426.591918	8.682624
7.328007	426.860929	8.687642
6.596525	418.546607	8.692659
6.512389	418.099126	8.697677
6.806889	414.771080	8.702695
6.835429	412.510324	8.707712
6.749306	427.362227	8.712730
6.918238	420.216462	8.717747
6.926646	422.316949	8.722765
6.836572	426.906975	8.727783
6.889267	414.376781	8.732800
6.858190	428.128170	8.737818
6.645510	420.411047	8.742835
6.653404	421.400791	8.747853
7.050491	419.984834	8.752871
7.139101	429.870614	8.757888
6.911995	429.631723	8.762906
6.623074	416.037917	8.767923
6.994239	412.824089	8.772941
6.574763	418.421916	8.777959
7.097993	418.390503	8.782976
7.069400	419.266045	8.787994
6.987600	412.437275	8.793011
6.732173	409.002893	8.798029
6.918621	414.695126	8.803047
7.225815	410.771812	8.808064
6.969293	409.313100	8.813082
6.919291	392.314696	8.818099
7.315249	401.918779	8.823117
6.595138	398.004952	8.828135
6.658732	398.083424	8.833152
6.807714	398.353641	8.838170
7.042982	415.824938	8.843187
6.951566	414.548636	8.848205
6.660590	415.963897	8.853223
7.114143	420.651779	8.858240
7.240650	424.198030	8.863258
6.670901	409.991833	8.868275
7.155099	414.722248	8.873293
7.418181	421.658464	8.878311
7.153406	404.864109	8.883328
6.622501	405.291345	8.888346
6.931377	404.413063	8.893363
7.141186	416.810755	8.898381
6.787959	411.510871	8.903399
7.053961	413.034519	8.908416
7.244650	422.213192	8.913434
6.766041	420.628333	8.918451
7.140579	413.447201	8.923469
7.004987	417.176525	8.928487
7.096506	411.627079	8.933504
7.156414	421.214400	8.938522
7.106008	418.060312	8.943539
7.117278	414.650414	8.948557
7.043548	424.378593	8.953575
7.148946	422.913665	8.958592
6.726394	427.183407	8.963610
6.808830	421.846816	8.968627
6.937729	423.174200	8.973645
6.950430	430.152805	8.978663
7.472777	426.120039	8.983680
7.199723	429.088278	8.988698
6.802667	427.244492	8.993715
7.101710	419.532396	8.998733
6.845066	428.150012	9.003751
7.221135	422.606470	9.008768
7.320583	417.655372	9.013786
7.415986	423.573309	9.018803
7.040803	418.371534	9.023821
7.253213	425.142125	9.028839
7.463452	418.728334	9.033856
7.338052	422.803196	9.038874
7.250092	422.523568	9.043891
7.337166	417.315638	9.048909
7.186672	425.418012	9.053927
7.178106	426.845829	9.058944
7.389116	425.515829	9.063962
7.324335	420.123411	9.068979
7.436289	423.498376	9.073997
7.247466	423.202995	9.079015
7.258633	414.014936	9.084032
7.087575	420.504787	9.089050
7.290825	425.077255	9.094067
7.176963	416.120220	9.099085
7.140915	423.358921	9.104103
7.264313	425.857950	9.109120
7.259521	420.591830	9.114138
7.199215	437.023882	9.119155
7.199356	429.800420	9.124173
6.902390	435.072949	9.129191
7.369007	428.379148	9.134208
7.228946	429.505681	9.139226
7.099570	426.360810	9.144243
7.187383	421.597723	9.149261
7.191516	427.334305	9.154279
7.376185	425.471955	9.159296
7.497387	422.319381	9.164314
7.022886	426.622507	9.169331
7.213701	421.016476	9.174349
7.316485	425.421652	9.179367
7.484005	422.381739	9.184384
7.640540	427.422268	9.189402
7.552850	428.524817	9.194419
7.603889	418.238618	9.199437
7.154820	412.922192	9.204455
6.886479	424.845707	9.209472
7.564464	414.499148	9.214490
7.515678	417.934011	9.219507
7.163793	414.650439	9.224525
7.377888	422.963925	9.229543
7.338486	413.616535	9.234560
7.394590	423.119247	9.239578
7.238904	427.072625	9.244595
7.549453	425.843792	9.249613
7.331836	430.135072	9.254631
7.327885	422.546187	9.259648
7.574378	432.741741	9.264666
7.463044	437.322478	9.269683
7.896857	438.324383	9.274701
7.521537	434.463820	9.279719
7.632313	431.432796	9.284736
7.720187	426.549780	9.289754
7.572868	425.522073	9.294771
7.529724	419.170073	9.299789
7.456589	418.733491	9.304807
7.370345	424.850299	9.309824
7.388313	419.372334	9.314842
7.297408	419.639113	9.319859
7.214376	413.776194	9.324877
7.224794	437.288132	9.329895
7.274619	446.312166	9.334912
7.396974	445.128598	9.339930
7.502879	451.410965	9.344947
7.693731	441.244856	9.349965
7.652712	444.107316	9.354983
7.932785	455.531520	9.360000
7.823657	448.432467	9.365018
7.613108	450.983824	9.370035
8.058875	452.867468	9.375053
7.705625	452.310675	9.380071
7.626669	437.014561	9.385088
7.761286	435.668129	9.390106
7.685043	438.239465	9.395123
7.501742	424.335620	9.400141
7.444850	428.169379	9.405159
7.930760	443.370316	9.410176
7.933026	434.246756	9.415194
7.562650	425.415112	9.420211
7.436815	428.650614	9.425229
7.603967	427.415847	9.430247
7.788696	449.584542	9.435264
8.140465	450.971681	9.440282
7.618618	444.817751	9.445299
7.352182	427.285189	9.450317
7.416185	438.942050	9.455335
8.141991	438.528608	9.460352
7.863349	444.123312	9.465370
7.163690	439.051265	9.470387
7.596743	443.067033	9.475405
7.845593	443.848614	9.480423
7.903169	443.782865	9.485440
7.688135	442.907776	9.490458
7.889803	453.851967	9.495475
7.837820	451.499682	9.500493
8.013167	444.135156	9.505511
7.860273	452.547182	9.510528
8.086888	452.707408	9.515546
7.807002	446.471385	9.520563
7.697282	435.427738	9.525581
7.742413	441.445074	9.530599
8.053360	445.618828	9.535616
8.189900	436.152341	9.540634
7.567104	421.392723	9.545651
7.415275	428.532804	9.550669
7.714136	439.351306	9.555687
7.809460	443.076014	9.560704
8.003815	444.282693	9.565722
7.689445	458.075336	9.570739
7.465233	446.920235	9.575757
7.804393	450.871822	9.580775
7.737388	457.193907	9.585792
7.689997	444.161830	9.590810
7.418584	450.686350	9.595827
7.352386	450.264459	9.600845
8.072198	463.336500	9.605863
8.167888	462.056124	9.610880
7.932377	451.483450	9.615898
7.596921	457.869686	9.620915
8.044734	462.498518	9.625933
8.363879	468.015346	9.630951
8.283423	462.770536	9.635968
8.187040	459.459545	9.640986
7.970955	458.120724	9.646003
8.046038	452.747407	9.651021
8.138893	458.205013	9.656039
7.971516	453.911085	9.661056
7.846939	449.499999	9.666074
8.018376	451.877899	9.671091
7.766350	451.043318	9.676109
8.121675	453.654334	9.681127
7.671312	456.479948	9.686144
7.799917	453.054813	9.691162
8.100236	472.071761	9.696179
8.095787	474.881158	9.701197
8.145623	477.259179	9.706215
8.151295	473.932196	9.711232
8.101634	468.433255	9.716250
7.910777	468.785122	9.721267
7.936408	474.906508	9.726285
8.309858	478.881131	9.731303
8.176020	486.154114	9.736320
8.395661	480.385759	9.741338
7.851521	467.314734	9.746355
7.924494	473.425546	9.751373
7.787683	483.012165	9.756391
8.509544	485.363786	9.761408
8.424858	478.320851	9.766426
8.579937	483.923349	9.771443
7.955743	467.469268	9.776461
8.264719	456.350538	9.781479
7.955735	465.140472	9.786496
8.193804	465.472470	9.791514
7.714205	466.292449	9.796531
8.023849	482.044893	9.801549
8.549542	473.890169	9.806567
8.177778	483.646142	9.811584
8.242628	468.605176	9.816602
7.913828	476.849118	9.821619
8.171302	473.419567	9.826637
8.670735	470.769447	9.831655
8.585253	484.125467	9.836672
8.394540	467.518262	9.841690
8.219839	471.032823	9.846707
8.288170	466.768231	9.851725
8.242754	472.866035	9.856743
7.892344	478.809660	9.861760
8.132357	473.331601	9.866778
8.202892	475.128875	9.871795
8.008004	474.780795	9.876813
8.152396	476.538095	9.881831
7.979585	472.854074	9.886848
8.514782	476.251096	9.891866
8.548301	470.445636	9.896883
7.976638	476.300852	9.901901
8.705697	470.455839	9.906919
8.235288	477.039949	9.911936
8.083724	479.588380	9.916954
7.994025	471.457496	9.921971
8.100522	465.874129	9.926989
8.665663	471.573316	9.932007
8.434265	473.291667	9.937024
8.816098	475.674474	9.942042
8.409569	475.031355	9.947059
8.299612	476.216290	9.952077
8.535505	470.855640	9.957095
8.416573	475.885695	9.962112
8.109533	478.436396	9.967130
8.369970	478.484026	9.972147
7.892679	486.868002	9.977165
8.619300	483.974004	9.982183
8.824562	499.272610	9.987200
8.528172	493.130674	9.992218
8.621621	485.005801	9.997235
7.974429	477.148453	10.002253
8.064340	494.263911	10.007271
8.374722	504.481053	10.012288
8.385703	504.214324	10.017306
8.615417	508.220941	10.022323
8.546842	509.774930	10.027341
9.139625	500.158031	10.032359
8.911416	515.584528	10.037376
8.600435	506.355378	10.042394
9.085151	501.296556	10.047411
9.018210	488.469479	10.052429
8.686094	473.209843	10.057447
8.535316	480.810521	10.062464
8.958755	478.841328	10.067482
8.867872	473.506632	10.072499
8.239929	484.637631	10.077517
8.660548	476.553017	10.082535
8.511402	482.386215	10.087552
8.512319	481.729748	10.092570
8.935634	480.009880	10.097587
8.504327	480.623480	10.102605
8.533913	476.699467	10.107623
8.819487	482.893735	10.112640
8.205069	481.080844	10.117658
8.472152	479.805170	10.122675
8.339661	482.031881	10.127693
8.837151	491.175142	10.132711
8.714816	494.675191	10.137728
8.717437	491.254010	10.142746
8.346996	497.295453	10.147763
8.787241	499.325132	10.152781
8.791385	505.894859	10.157799
8.375795	506.704810	10.162816
8.372488	512.786563	10.167834
8.809823	508.457833	10.172851
8.754238	504.547158	10.177869
8.771414	510.054508	10.182887
8.594416	509.615263	10.187904
8.727104	506.571326	10.192922
8.976578	509.101106	10.197939
8.448231	513.377976	10.202957
8.653659	506.330599	10.207975
8.934328	506.094197	10.212992
9.016319	509.985107	10.218010
8.810444	504.681042	10.223027
8.844962	511.195519	10.228045
9.110528	512.100715	10.233063
9.082251	511.704438	10.238080
8.772253	510.765331	10.243098
9.187269	509.614797	10.248115
8.837185	509.347837	10.253133
8.982843	504.301113	10.258151
9.049365	508.355391	10.263168
8.578040	502.452297	10.268186
8.903264	500.299677	10.273203
8.693918	507.922166	10.278221
8.878360	506.732022	10.283239
8.887448	507.472278	10.288256
8.836419	495.731441	10.293274
8.893119	493.784994	10.298291
8.679255	502.108768	10.303309
8.989061	499.589340	10.308327
8.787631	514.673973	10.313344
8.788665	498.185017	10.318362
9.082533	504.674635	10.323379
8.985727	507.766749	10.328397
8.838594	505.511416	10.333415
8.710319	508.283416	10.338432
8.927021	520.575960	10.343450
9.154887	525.930384	10.348467
8.906899	539.027887	10.353485
9.564296	534.822460	10.358503
9.213620	524.838980	10.363520
8.686542	530.210707	10.368538
9.545337	528.192231	10.373555
8.896410	521.445966	10.378573
9.153163	517.110814	10.383591
9.044075	513.350530	10.388608
8.766289	526.421135	10.393626
9.310500	525.685854	10.398643
8.914418	535.562430	10.403661
9.236819	533.927795	10.408679
9.462849	537.609952	10.413696
9.163380	532.923295	10.418714
9.141593	521.682782	10.423731
9.196474	534.701270	10.428749
9.158096	529.929525	10.433767
9.209027	532.468326	10.438784
9.016569	534.950589	10.443802
9.225974	535.981349	10.448819
9.227875	533.784711	10.453837
9.274356	528.980735	10.458855
9.433723	524.727111	10.463872
9.235048	524.256549	10.468890
9.244845	515.885995	10.473907
9.277269	527.229129	10.478925
9.150894	517.437725	10.483943
9.149972	527.725747	10.488960
9.370932	530.436721	10.493978
9.118332	530.959207	10.498995
9.514530	538.382690	10.504013
9.418442	534.266918	10.509031
9.294459	525.888920	10.514048
8.717141	530.441707	10.519066
9.382393	522.492310	10.524083
9.388832	536.225282	10.529101
9.390350	523.680939	10.534119
9.689984	531.037499	10.539136
9.146527	529.841483	10.544154
9.598604	525.737654	10.549171
9.505391	537.671674	10.554189
9.432138	530.200898	10.559207
9.384711	523.224690	10.564224
9.284439	541.155777	10.569242
9.494421	528.635572	10.574259
9.344305	527.857603	10.579277
9.449582	522.148178	10.584295
9.441004	527.874161	10.589312
9.356638	524.037418	10.594330
9.639218	522.544721	10.599347
9.827845	532.433822	10.604365
9.340861	515.102985	10.609383
9.662002	506.585826	10.614400
9.328834	504.113491	10.619418
9.370896	509.430751	10.624435
9.665462	521.367117	10.629453
9.433786	521.075293	10.634471
9.841708	520.011076	10.639488
9.551817	511.766375	10.644506
9.690188	499.282657	10.649523
9.308207	500.617510	10.654541
9.198646	498.230060	10.659559
9.406279	508.573755	10.664576
9.319815	525.388679	10.669594
9.291088	531.449175	10.674611
9.652815	532.374018	10.679629
9.176986	530.346906	10.684647
9.335629	524.976253	10.689664
9.101293	527.225238	10.694682
9.117388	532.117389	10.699699
9.439517	536.797491	10.704717
9.592767	554.821412	10.709735
9.984477	550.278917	10.714752
9.748657	556.349779	10.719770
9.864562	538.362730	10.724787
9.082836	537.554336	10.729805
9.437962	548.474541	10.734823
9.609069	553.225646	10.739840
10.030554	560.083449	10.744858
9.849052	555.400393	10.749875
9.861820	560.321475	10.754893
9.660346	560.959027	10.759911
9.855388	553.742846	10.764928
9.677836	561.675954	10.769946
9.713842	561.367434	10.774963
9.814150	560.468176	10.779981
9.232382	559.811486	10.784999
9.798247	556.589217	10.790016
10.009762	563.445207	10.795034
9.629625	563.227135	10.800051
9.718271	559.366433	10.805069
9.678458	562.806228	10.810087
9.978177	557.170468	10.815104
9.623544	566.854375	10.820122
9.945176	555.645240	10.825139
10.003559	561.234510	10.830157
9.756547	567.035733	10.835175
9.963718	560.780161	10.840192
9.657423	561.194297	10.845210
9.936471	555.227264	10.850227
9.825373	559.760658	10.855245
9.968512	558.684278	10.860263
10.012947	559.684083	10.865280
10.068374	562.847027	10.870298
10.061119	565.713683	10.875315
9.962796	562.434535	10.880333
9.909427	564.778246	10.885351
9.820273	559.831413	10.890368
9.626616	562.572641	10.895386
9.621082	566.272152	10.900403
9.939497	567.696085	10.905421
10.013199	558.460284	10.910439
10.263394	558.266525	10.915456
9.726691	571.128425	10.920474
10.166030	560.017607	10.925491
9.945850	560.882150	10.930509
9.543290	560.844314	10.935527
9.974784	566.706483	10.940544
9.491819	567.836260	10.945562
9.892317	582.902378	10.950579
10.377270	577.591035	10.955597
9.786819	576.560167	10.960615
10.218865	575.334379	10.965632
10.322080	580.803023	10.970650
10.394307	572.381637	10.975667
10.296383	573.432150	10.980685
10.015203	574.694411	10.985703
10.232556	569.447089	10.990720
9.405692	570.220497	10.995738
9.983625	587.957007	11.000755
10.310294	573.089524	11.005773
9.943372	577.214886	11.010791
10.224524	582.213842	11.015808
10.090624	589.180766	11.020826
9.923338	585.770409	11.025843
10.040581	578.569564	11.030861
10.160952	577.294781	11.035879
10.072393	580.133153	11.040896
10.049699	577.760484	11.045914
9.855468	580.154669	11.050931
10.237070	576.166012	11.055949
9.717403	582.953537	11.060967
10.058709	594.589141	11.065984
10.225669	602.076971	11.071002
10.314885	609.684282	11.076019
10.596329	602.132655	11.081037
10.395663	607.778307	11.086055
10.216668	597.225093	11.091072
10.436589	600.946090	11.096090
10.375708	604.635346	11.101107
10.726485	604.596240	11.106125
10.243639	602.705916	11.111143
10.750014	606.271580	11.116160
10.300110	581.026481	11.121178
10.323447	583.402357	11.126195
10.317142	576.460710	11.131213
10.262268	583.522546	11.136231
10.402779	590.695782	11.141248
10.266791	591.152662	11.146266
10.084783	595.813939	11.151283
10.721209	600.861377	11.156301
10.301467	602.700768	11.161319
10.523574	600.340232	11.166336
10.382326	603.836954	11.171354
10.194007	610.222281	11.176371
10.561358	600.757414	11.181389
10.453504	605.426010	11.186407
10.901412	594.919739	11.191424
10.770414	601.851499	11.196442
10.826845	605.787460	11.201459
10.816114	596.798396	11.206477
10.261776	590.857787	11.211495
10.961895	592.900408	11.216512
10.863232	592.439420	11.221530
10.282482	587.604317	11.226547
10.343866	573.725132	11.231565
10.347656	590.832086	11.236583
10.721305	592.708110	11.241600
10.789879	591.804356	11.246618
10.845436	599.839811	11.251635
10.636676	591.752772	11.256653
10.402783	590.549273	11.261671
10.509016	593.615901	11.266688
11.077430	602.186378	11.271706
10.425025	595.547926	11.276723
10.677427	593.507690	11.281741
10.341797	606.641065	11.286759
10.698447	601.267768	11.291776
10.444933	593.998777	11.296794
10.946245	599.783746	11.301811
11.120002	594.748374	11.306829
11.013888	600.211953	11.311847
11.106849	601.185222	11.316864
10.639494	591.819585	11.321882
10.804360	598.581912	11.326899
10.935439	585.723738	11.331917
10.799956	592.649886	11.336935
10.794460	589.861114	11.341952
10.652986	589.321627	11.346970
10.669781	600.720905	11.351987
11.065638	601.993852	11.357005
10.958114	609.849738	11.362023
11.018854	596.406134	11.367040
10.791310	581.862163	11.372058
10.429090	593.465986	11.377075
10.583235	596.237931	11.382093
10.993419	604.116839	11.387111
10.722454	602.471027	11.392128
10.963057	612.702320	11.397146
10.892106	617.295710	11.402163
11.018623	612.065764	11.407181
10.752991	616.850602	11.412199
10.784599	603.966976	11.417216
10.660170	609.730071	11.422234
10.804635	617.328728	11.427251
10.793636	613.363707	11.432269
10.659417	612.633736	11.437287
10.373539	606.619500	11.442304
11.136633	619.063186	11.447322
10.955196	625.359079	11.452339
11.416972	623.664729	11.457357
10.903652	611.551282	11.462375
10.908068	609.455226	11.467392
11.337820	623.936132	11.472410
11.064855	614.748306	11.477427
11.085295	608.812307	11.482445
10.849087	607.536587	11.487463
10.827952	617.218761	11.492480
11.126767	622.584188	11.497498
10.957938	632.942759	11.502515
11.745487	625.759946	11.507533
11.230181	630.653334	11.512551
11.057569	619.300693	11.517568
11.291496	610.399520	11.522586
11.043338	606.307558	11.527603
11.215272	611.544541	11.532621
11.269023	616.566513	11.537639
11.112860	618.049029	11.542656
11.328223	616.140825	11.547674
11.442638	619.300849	11.552691
11.105591	606.629615	11.557709
11.252962	615.897226	11.562727
11.137830	615.675501	11.567744
11.319206	622.757140	11.572762
11.409582	630.610429	11.577779
11.163259	616.224005	11.582797
11.203773	621.219651	11.587815
11.100788	631.750941	11.592832
11.584966	627.780914	11.597850
11.122988	624.757548	11.602867
11.603084	622.539623	11.607885
11.309091	616.084846	11.612903
11.008600	624.548480	11.617920
11.263654	619.342574	11.622938
11.360914	626.251203	11.627955
11.305917	627.361265	11.632973
11.399955	637.079052	11.637991
11.002778	634.818699	11.643008
11.221936	629.170292	11.648026
10.998088	632.878776	11.653043
11.358276	624.705735	11.658061
11.106654	628.185041	11.663079
10.988435	636.272986	11.668096
11.709566	640.748589	11.673114
11.491518	660.213027	11.678131
11.690792	649.237598	11.683149
11.904525	653.799016	11.688167
11.792800	647.400876	11.693184
11.562866	637.849693	11.698202
11.514138	635.184451	11.703219
11.546248	630.272247	11.708237
11.622932	632.598746	11.713255
11.351906	634.705171	11.718272
11.564636	630.799765	11.723290
11.220642	633.517222	11.728307
11.677919	638.684258	11.733325
11.529673	641.642444	11.738343
11.654813	646.861522	11.743360
11.649465	642.920855	11.748378
11.667379	658.921135	11.753395
11.566017	660.436093	11.758413
11.715820	662.277770	11.763431
11.854948	669.653225	11.768448
11.687003	640.415967	11.773466
11.566450	648.469569	11.778483
11.708302	648.687259	11.783501
11.922341	654.987470	11.788519
11.479188	654.703531	11.793536
12.023901	652.765811	11.798554
12.095995	650.166842	11.803571
11.734097	640.604776	11.808589
11.651435	629.083401	11.813607
11.819758	631.711120	11.818624
11.905219	641.061027	11.823642
11.635531	640.491134	11.828659
11.812956	637.310779	11.833677
11.722861	642.364764	11.838695
11.813101	641.514417	11.843712
11.684119	643.131530	11.848730
11.885393	649.528412	11.853747
11.709784	659.342110	11.858765
11.684045	659.425113	11.863783
11.928772	662.905552	11.868800
12.063177	654.509098	11.873818
11.938515	660.310116	11.878835
11.903092	656.891708	11.883853
12.103987	649.087595	11.888871
11.785912	659.592641	11.893888
11.783805	650.024690	11.898906
11.654295	653.980328	11.903923
12.007773	654.742369	11.908941
11.927272	651.507750	11.913959
11.475329	654.699713	11.918976
11.996983	648.227580	11.923994
11.889661	657.815983	11.929011
12.201785	657.511536	11.934029
12.121462	657.981786	11.939047
11.792416	666.705534	11.944064
11.596270	653.904893	11.949082
11.756964	669.441001	11.954099
12.316709	667.358913	11.959117
12.318134	673.168581	11.964135
11.871903	672.200317	11.969152
12.399031	675.728030	11.974170
12.194045	660.303148	11.979187
12.360079	664.518594	11.984205
12.316001	653.407723	11.989223
12.123922	656.622086	11.994240
12.376665	663.518992	11.999258
12.412573	659.988421	12.004275
12.163915	658.604195	12.009293
12.283453	660.494795	12.014311
12.096528	663.446422	12.019328
12.219445	663.067479	12.024346
12.158248	668.669207	12.029363
12.112406	662.368036	12.034381
12.265709	655.499180	12.039399
11.896405	658.397331	12.044416
12.365414	662.543215	12.049434
12.363131	676.195610	12.054451
12.100802	677.148812	12.059469
12.216677	678.244728	12.064487
12.242804	684.230409	12.069504
12.545001	678.562665	12.074522
12.507623	678.413963	12.079539
12.371321	681.846809	12.084557
12.615098	681.246957	12.089575
12.322281	671.579376	12.094592
12.339928	684.269294	12.099610
12.753648	688.076709	12.104627
12.131967	671.271752	12.109645
12.610825	670.038623	12.114663
12.048425	669.312622	12.119680
12.693965	675.592568	12.124698
12.685594	678.765529	12.129715
12.282524	677.386560	12.134733
12.364611	673.608911	12.139751
12.376195	682.181466	12.144768
12.613522	687.427160	12.149786
12.486116	688.027864	12.154803
12.166110	687.005108	12.159821
12.643387	686.157233	12.164839
12.413813	686.568818	12.169856
12.399221	694.492231	12.174874
12.372539	691.331222	12.179891
12.220889	688.060406	12.184909
12.575881	677.461348	12.189927
12.389616	682.940666	12.194944
12.687002	683.900846	12.199962
12.756138	676.319336	12.204979
12.455366	682.349925	12.209997
12.843249	683.333794	12.215015
12.972395	690.158557	12.220032
13.028809	681.947880	12.225050
12.876541	684.187182	12.230067
12.800344	689.226379	12.235085
12.824918	683.359135	12.240103
12.765717	685.183069	12.245120
12.538913	679.626611	12.250138
12.694401	675.869019	12.255155
12.417359	682.953081	12.260173
12.694751	681.802010	12.265191
12.870512	682.377304	12.270208
12.857950	672.990859	12.275226
12.777007	675.982686	12.280243
12.563670	684.953400	12.285261
12.655708	687.346927	12.290279
12.783217	699.369548	12.295296
12.860198	697.896427	12.300314
13.306472	703.491239	12.305331
12.881218	697.322085	12.310349
12.720518	688.214462	12.315367
12.680639	687.084699	12.320384
12.687849	698.207831	12.325402
13.132967	703.335765	12.330419
13.025624	704.842197	12.335437
12.965713	707.871760	12.340455
12.785599	704.681140	12.345472
13.003793	698.183952	12.350490
13.278207	710.041552	12.355507
13.053039	714.678065	12.360525
13.167808	700.673653	12.365543
13.391719	714.375843	12.370560
12.603151	701.150438	12.375578
12.751094	700.300515	12.380595
12.823048	707.812742	12.385613
13.170708	712.735043	12.390631
12.898397	706.081177	12.395648
12.944289	704.808586	12.400666
12.986230	709.942888	12.405683
12.975516	704.551381	12.410701
12.938683	700.107550	12.415719
13.001438	705.289083	12.420736
12.766213	708.879445	12.425754
13.297537	708.294500	12.430771
12.747410	708.879386	12.435789
12.982930	721.159653	12.440807
12.978148	737.671643	12.445824
13.107218	741.870808	12.450842
13.648844	733.079154	12.455859
12.997769	745.350028	12.460877
13.315992	735.627699	12.465895
13.495440	731.825316	12.470912
13.349151	724.454264	12.475930
13.539176	735.829642	12.480947
13.426660	740.202358	12.485965
13.969520	729.586457	12.490983
13.573366	720.140168	12.496000
13.363363	716.884802	12.501018
13.387052	714.924569	12.506035
13.055730	709.602227	12.511053
13.232891	706.952075	12.516071
13.347282	718.497082	12.521088
13.288610	734.007656	12.526106
13.884374	732.349108	12.531123
13.170939	727.216019	12.536141
13.535004	732.883681	12.541159
13.769193	732.439965	12.546176
13.303899	726.207647	12.551194
13.652292	707.010044	12.556211
13.256062	713.106092	12.561229
13.441128	731.832106	12.566247
13.692548	731.335197	12.571264
13.452742	732.546805	12.576282
13.946896	730.863151	12.581299
13.548141	721.919042	12.586317
13.474942	708.139734	12.591335
13.488821	719.173472	12.596352
13.413316	727.317881	12.601370
13.664225	725.063270	12.606387
13.544780	728.761727	12.611405
13.561741	726.152452	12.616423
13.912204	728.464469	12.621440
13.749505	725.062834	12.626458
13.819778	731.022680	12.631475
13.527629	736.900457	12.636493
13.477092	735.071772	12.641511
13.857232	730.603628	12.646528
13.436643	731.985572	12.651546
13.707772	736.310800	12.656563
13.492614	728.619178	12.661581
13.470271	730.885466	12.666599
13.798155	734.113049	12.671616
13.547300	729.213595	12.676634
13.707529	732.644171	12.681651
13.112149	736.322526	12.686669
13.654981	741.574017	12.691687
13.654986	750.009563	12.696704
13.849602	758.613438	12.701722
14.300343	762.973647	12.706739
14.208832	773.635766	12.711757
13.910053	754.302826	12.716775
14.034802	747.482590	12.721792
13.691091	748.344405	12.726810
13.900286	748.734582	12.731827
13.776652	754.399769	12.736845
14.096426	754.829425	12.741863
14.175629	761.523185	12.746880
13.776434	755.807520	12.751898
14.209362	752.621826	12.756915
14.292183	758.702791	12.761933
13.856762	747.006237	12.766951
13.995341	752.062293	12.771968
13.944680	759.672649	12.776986
14.126831	753.244206	12.782003
13.864960	758.618628	12.787021
13.855011	763.666402	12.792039
14.295002	763.237776	12.797056
14.319790	763.568484	12.802074
14.265452	754.810236	12.807091
13.978569	765.329391	12.812109
13.812696	755.452527	12.817127
13.908335	759.193030	12.822144
14.206555	768.108880	12.827162
14.282213	759.024148	12.832179
14.129508	758.716790	12.837197
14.223534	761.195222	12.842215
14.058236	756.793597	12.847232
13.805627	762.239153	12.852250
14.144359	765.572339	12.857267
14.102800	761.602606	12.862285
14.137313	764.068273	12.867303
14.110811	758.196384	12.872320
13.919627	776.287118	12.877338
14.401988	783.233300	12.882355
14.490413	791.358365	12.887373
14.431578	791.806317	12.892391
14.680056	780.741048	12.897408
14.666497	787.878542	12.902426
14.272229	771.880461	12.907443
14.586333	769.546515	12.912461
14.305207	768.334625	12.917479
14.995222	767.961500	12.922496
14.417543	764.653279	12.927514
14.942979	757.473613	12.932531
14.657754	761.040261	12.937549
14.599497	757.982018	12.942567
14.396002	749.401777	12.947584
14.480871	750.108080	12.952602
14.681544	754.507468	12.957619
14.538239	753.990353	12.962637
14.519098	756.051015	12.967655
14.762908	751.541110	12.972672
14.595096	761.142202	12.977690
14.869936	751.423506	12.982707
14.689567	761.774492	12.987725
14.274328	759.292890	12.992743
14.771658	758.527077	12.997760
14.346222	754.213548	13.002778
14.575672	751.495236	13.007795
14.744954	757.553187	13.012813
14.559917	756.083245	13.017831
14.982778	755.938171	13.022848
14.472050	764.482149	13.027866
14.816508	752.732826	13.032883
14.718521	751.129325	13.037901
14.580757	754.704425	13.042919
14.752345	775.812077	13.047936
14.805955	783.469222	13.052954
14.566974	786.447960	13.057971
15.199987	788.946089	13.062989
15.190783	784.381144	13.068007
15.391663	762.082339	13.073024
14.619719	756.197859	13.078042
14.929059	752.280446	13.083059
14.796955	753.939084	13.088077
14.703112	764.989727	13.093095
14.650690	754.110475	13.098112
14.898168	769.194415	13.103130
15.114632	772.145972	13.108147
14.970872	774.248252	13.113165
14.655485	783.642104	13.118183
14.971808	773.664431	13.123200
14.670588	784.858033	13.128218
14.853184	778.609391	13.133235
15.077923	782.534799	13.138253
14.817099	774.487394	13.143271
14.930114	774.681202	13.148288
14.843542	786.150442	13.153306
14.324005	779.828774	13.158323
14.793949	781.475136	13.163341
14.581093	794.822943	13.168359
15.270937	792.442746	13.173376
15.127480	805.479884	13.178394
15.228407	804.416415	13.183411
15.333545	813.097451	13.188429
15.046241	808.639189	13.193447
15.457450	803.803240	13.198464
15.695096	801.793696	13.203482
15.889002	795.151955	13.208499
15.781533	788.573216	13.213517
15.267526	776.958383	13.218535
15.067215	774.405233	13.223552
15.035426	779.320734	13.228570
15.029767	779.634121	13.233587
14.763005	778.120178	13.238605
14.565382	786.646666	13.243623
15.004148	795.938142	13.248640
14.916272	808.092413	13.253658
15.104318	810.392019	13.258675
15.442413	804.103226	13.263693
15.165272	810.736071	13.268711
15.316094	800.500291	13.273728
15.533223	807.465949	13.278746
15.535455	797.556410	13.283763
15.552760	804.944697	13.288781
15.648866	810.105255	13.293799
15.496465	800.636511	13.298816
15.600515	811.280635	13.303834
15.418232	812.634714	13.308851
15.648632	808.874825	13.313869
15.364362	812.668553	13.318887
16.016337	808.236693	13.323904
15.619051	804.038663	13.328922
15.670511	815.779786	13.333939
16.060014	807.554732	13.338957
15.845759	803.179700	13.343975
15.789268	809.411899	13.348992
15.726756	807.812302	13.354010
15.672437	800.297421	13.359027
15.526107	802.624169	13.364045
15.467813	812.889786	13.369063
16.021382	800.526997	13.374080
16.171174	808.595119	13.379098
15.888572	806.272610	13.384115
15.824838	814.380500	13.389133
15.479798	814.046472	13.394151
15.784835	798.219666	13.399168
15.520009	802.449004	13.404186
16.028501	803.088934	13.409203
15.729042	803.918572	13.414221
15.630512	814.938423	13.419239
15.943902	803.137130	13.424256
15.824745	812.241475	13.429274
15.774901	801.974018	13.434291
16.004823	805.368442	13.439309
15.366161	808.185743	13.444327
15.836530	809.200877	13.449344
15.957532	811.586728	13.454362
15.874211	819.972246	13.459379
16.047644	823.716353	13.464397
16.055233	838.140501	13.469415
16.047867	838.021810	13.474432
16.202590	830.458383	13.479450
16.025338	826.879127	13.484467
16.016246	822.945319	13.489485
16.177924	832.674706	13.494503
16.314576	818.079790	13.499520
16.327131	805.476716	13.504538
15.944007	808.216109	13.509555
15.864970	799.272359	13.514573
16.032703	812.705716	13.519591
15.754335	824.353355	13.524608
16.187568	813.514738	13.529626
16.046380	824.364553	13.534643
16.385904	823.557190	13.539661
16.441842	822.923649	13.544679
16.044087	818.593144	13.549696
16.364200	829.039323	13.554714
16.155198	834.033097	13.559731
16.629840	820.735914	13.564749
16.349488	821.818181	13.569767
16.382331	832.968938	13.574784
16.421764	821.747047	13.579802
16.063444	829.591831	13.584819
16.084123	822.538562	13.589837
16.085704	821.623202	13.594855
15.925106	815.724967	13.599872
16.137511	821.028254	13.604890
16.219718	821.286849	13.609907
16.161353	823.359976	13.614925
16.143981	837.911112	13.619943
16.165982	846.166531	13.624960
16.642552	848.887998	13.629978
16.767265	846.419613	13.634995
16.963856	845.950227	13.640013
17.027749	840.736338	13.645031
16.910367	828.762680	13.650048
16.655592	822.503655	13.655066
16.374661	821.537885	13.660083
16.543630	814.975784	13.665101
16.317702	820.054258	13.670119
16.576280	819.354253	13.675136
16.620621	819.047578	13.680154
16.261716	832.336244	13.685171
16.828526	838.164679	13.690189
16.845959	836.107582	13.695207
16.817940	841.817776	13.700224
16.771149	838.480010	13.705242
16.459903	847.494548	13.710259
16.567764	838.761338	13.715277
16.470458	848.616519	13.720295
16.792332	848.701863	13.725312
17.025798	860.184124	13.730330
16.816020	858.181559	13.735347
16.721734	854.516714	13.740365
16.763323	855.012050	13.745383
16.780459	853.122257	13.750400
17.089299	848.286556	13.755418
16.591910	851.514077	13.760435
16.965636	850.909639	13.765453
16.804899	855.119524	13.770471
16.876806	857.386839	13.775488
16.974200	857.620965	13.780506
16.399832	854.731934	13.785523
16.972945	855.434325	13.790541
16.591102	845.992039	13.795559
16.697928	863.480743	13.800576
17.025671	868.926920	13.805594
17.126105	880.821360	13.810611
17.353832	870.440946	13.815629
17.191910	879.586739	13.820647
17.214326	866.066886	13.825664
17.413325	850.524894	13.830682
17.262754	852.568290	13.835699
17.119451	846.702049	13.840717
16.981809	846.610080	13.845735
16.873907	848.804581	13.850752
17.167739	859.665153	13.855770
17.160788	871.112506	13.860787
17.501157	873.107385	13.865805
17.534893	867.724642	13.870823
17.427935	854.565898	13.875840
17.184275	844.455017	13.880858
16.879185	851.199555	13.885875
16.804990	856.506731	13.890893
17.414460	867.636592	13.895911
17.067658	865.904806	13.900928
17.641104	869.365340	13.905946
17.541421	877.775540	13.910963
17.666705	857.066376	13.915981
17.640371	867.099797	13.920999
17.550394	862.724214	13.926016
17.694858	865.207382	13.931034
17.565589	865.252958	13.936051
17.351511	858.810818	13.941069
17.492703	853.733138	13.946087
17.568591	871.333996	13.951104
17.698858	864.594902	13.956122
17.418493	865.487824	13.961139
17.753332	865.719461	13.966157
17.583522	863.925230	13.971175
17.502579	869.691062	13.976192
17.220952	871.824422	13.981210
17.038360	869.306353	13.986227
17.181395	862.678869	13.991245
17.303394	868.416060	13.996263
17.375866	866.987814	14.001280
17.592610	870.027707	14.006298
17.350222	878.103657	14.011315
17.816156	886.715576	14.016333
17.804549	885.461450	14.021351
18.107293	886.837371	14.026368
18.221815	882.524417	14.031386
17.862267	878.071145	14.036403
17.703451	870.957618	14.041421
17.994114	867.642713	14.046439
17.818751	868.617014	14.051456
17.436390	864.908939	14.056474
17.819819	879.738140	14.061491
17.829492	877.171010	14.066509
18.039234	888.230969	14.071527
18.119839	888.063780	14.076544
18.168039	886.879178	14.081562
17.878030	883.121916	14.086579
18.153401	889.018121	14.091597
18.203425	891.667569	14.096615
17.750014	872.974116	14.101632
18.223620	881.632168	14.106650
17.998564	888.168518	14.111667
17.957322	887.196747	14.116685
18.262797	883.753286	14.121703
18.474465	891.603465	14.126720
18.049115	862.522940	14.131738
18.048008	864.205245	14.136755
18.013736	865.536138	14.141773
18.095630	873.050033	14.146791
18.027035	883.184759	14.151808
18.199811	881.406278	14.156826
18.091390	884.209940	14.161843
18.206720	890.677180	14.166861
18.409065	890.885395	14.171879
17.972435	896.546018	14.176896
17.953450	893.592053	14.181914
18.441238	888.848225	14.186931
18.161200	895.068142	14.191949
18.168548	886.038230	14.196967
18.184765	884.063370	14.201984
18.479759	884.484288	14.207002
18.370014	893.353668	14.212019
18.370453	880.831334	14.217037
18.423961	880.359119	14.222055
18.564843	887.870090	14.227072
18.737128	881.304290	14.232090
18.705862	878.547912	14.237107
18.404761	881.369140	14.242125
18.541622	878.542238	14.247143
18.279327	887.747944	14.252160
18.741513	882.702014	14.257178
18.691618	883.861785	14.262195
18.380365	886.899200	14.267213
18.316599	891.863923	14.272231
18.391470	890.769818	14.277248
18.457176	883.640042	14.282266
18.221711	897.742555	14.287283
18.646842	911.665836	14.292301
19.152995	900.544341	14.297319
19.160137	908.170950	14.302336
18.794493	888.763132	14.307354
18.624132	888.922445	14.312371
18.597703	890.596097	14.317389
19.148488	903.483507	14.322407
18.763864	902.373031	14.327424
18.816662	887.504016	14.332442
18.621222	881.399777	14.337459
18.684993	895.878286	14.342477
19.104208	901.761425	14.347495
18.713168	916.475314	14.352512
18.644371	909.915717	14.357530
18.890649	904.329248	14.362547
18.912887	899.929762	14.367565
19.109700	908.852104	14.372583
18.658328	905.524066	14.377600
19.055651	918.003181	14.382618
19.195295	917.091431	14.387635
18.711307	916.160626	14.392653
19.092939	912.361241	14.397671
18.722397	908.733357	14.402688
19.035529	914.128188	14.407706
18.780489	908.393044	14.412723
18.871370	910.755224	14.417741
19.544344	901.109769	14.422759
18.851012	913.649311	14.427776
19.043840	910.665312	14.432794
19.253611	919.531980	14.437811
19.137634	932.744788	14.442829
19.744019	917.785855	14.447847
19.611737	917.658333	14.452864
19.305533	915.295325	14.457882
19.308251	903.558422	14.462899
19.313052	912.233137	14.467917
19.444934	905.045647	14.472935
19.365614	917.608910	14.477952
19.622202	913.415702	14.482970
19.543451	911.806016	14.487987
19.500255	907.262145	14.493005
19.403048	905.374482	14.498023
19.895097	906.648161	14.503040
19.612973	902.930685	14.508058
19.526779	904.664195	14.513075
19.416315	908.560100	14.518093
19.836874	902.353027	14.523111
19.688101	903.361033	14.528128
19.527602	905.595340	14.533146
19.556893	912.735638	14.538163
19.357189	914.089299	14.543181
19.832408	900.933979	14.548199
19.611662	916.372274	14.553216
19.374808	913.162105	14.558234
19.406939	916.331918	14.563251
19.224939	911.771923	14.568269
19.273390	906.453136	14.573287
19.376792	912.840201	14.578304
19.961306	928.587844	14.583322
19.919362	928.805932	14.588339
19.946141	925.582856	14.593357
19.808021	917.680264	14.598375
19.874321	912.570120	14.603392
19.664529	914.222010	14.608410
20.069671	914.272217	14.613427
19.837297	905.519699	14.618445
20.066608	908.863745	14.623463
19.583149	909.649633	14.628480
19.935384	923.183554	14.633498
19.845920	925.473006	14.638515
20.025839	930.143936	14.643533
20.263606	929.825888	14.648551
20.342040	943.191282	14.653568
20.066957	924.536106	14.658586
19.998944	917.263165	14.663603
19.867018	921.339162	14.668621
20.228561	924.167026	14.673639
20.042062	923.044442	14.678656
19.775760	935.128924	14.683674
19.890734	930.768550	14.688691
19.848441	936.815530	14.693709
20.134015	935.136136	14.698727
20.131394	938.563865	14.703744
20.069568	943.922778	14.708762
20.121892	942.399852	14.713779
19.904607	941.297869	14.718797
20.349107	943.847648	14.723815
20.053343	937.702304	14.728832
19.969964	935.086628	14.733850
20.409559	944.027754	14.738867
20.476873	954.841823	14.743885
20.196942	951.224980	14.748903
20.304240	957.728217	14.753920
20.735340	961.220541	14.758938
20.587174	953.960142	14.763955
20.568694	955.979698	14.768973
20.490453	946.294126	14.773991
20.681138	943.111639	14.779008
20.192972	937.706505	14.784026
20.567953	941.658902	14.789043
20.629700	956.339751	14.794061
20.855163	952.848852	14.799079
20.129299	946.448997	14.804096
20.512101	958.053091	14.809114
20.885969	946.706138	14.814131
20.746216	962.800822	14.819149
20.887195	948.107291	14.824167
20.923141	948.351046	14.829184
20.629346	941.684678	14.834202
20.783028	930.864544	14.839219
20.676664	936.817420	14.844237
20.903079	928.857707	14.849255
20.631625	932.008816	14.854272
20.784025	937.431993	14.859290
21.091733	937.652104	14.864307
20.434583	946.635680	14.869325
21.146761	947.928521	14.874343
21.112950	946.201336	14.879360
20.663696	941.620091	14.884378
20.958939	940.908025	14.889395
21.026738	950.967770	14.894413
21.171652	941.013705	14.899431
20.996080	942.401457	14.904448
20.842504	932.068126	14.909466
21.028139	922.530574	14.914483
21.019476	943.171199	14.919501
21.278892	946.365367	14.924519
20.971449	944.980861	14.929536
21.298958	955.182956	14.934554
21.151209	939.606852	14.939571
20.618542	931.942798	14.944589
21.237795	938.062854	14.949607
21.195371	944.583233	14.954624
20.856678	937.519953	14.959642
21.176646	942.285709	14.964659
21.054616	946.871408	14.969677
20.803412	942.221261	14.974695
21.431372	937.982484	14.979712
21.149371	943.846115	14.984730
21.214799	938.556217	14.989747
21.208676	945.995570	14.994765
21.705588	938.836081	14.999783
21.771691	947.797857	15.004800
21.165529	942.426988	15.009818
21.332893	939.295493	15.014835
21.101669	938.498655	15.019853
21.354738	946.907268	15.024871
21.453077	943.972781	15.029888
21.574142	949.019015	15.034906
21.812038	951.225622	15.039923
21.316468	950.792097	15.044941
21.351390	947.312118	15.049959
21.815222	958.439608	15.054976
21.733234	956.887231	15.059994
21.986520	960.587297	15.065011
21.513227	947.444856	15.070029
21.537249	947.598960	15.075047
22.054370	957.086529	15.080064
21.640803	960.846897	15.085082
21.778814	942.259523	15.090099
21.943367	952.446123	15.095117
21.722602	946.759245	15.100135
21.745376	951.331724	15.105152
21.509992	961.205445	15.110170
21.801993	959.499796	15.115187
22.041243	960.923542	15.120205
21.816149	967.314758	15.125223
21.765804	960.395641	15.130240
21.682798	964.514476	15.135258
21.837238	960.302548	15.140275
21.836010	962.013284	15.145293
21.776809	964.686168	15.150311
22.202017	962.016050	15.155328
22.057221	962.332306	15.160346
22.058099	960.688048	15.165363
22.126002	964.767460	15.170381
22.159274	964.374154	15.175399
22.414124	957.467181	15.180416
22.149495	957.010095	15.185434
22.391717	961.251545	15.190451
22.258779	961.790007	15.195469
21.857127	958.176455	15.200487
22.124676	956.007572	15.205504
21.742238	958.207231	15.210522
22.345373	954.038612	15.215539
22.251368	963.912275	15.220557
21.901378	958.706393	15.225575
22.087775	958.759316	15.230592
22.207881	966.579693	15.235610
22.582763	983.774049	15.240627
22.489773	970.243796	15.245645
22.425444	974.195603	15.250663
22.519050	962.775785	15.255680
22.584919	960.452306	15.260698
22.303770	955.418678	15.265715
22.350890	964.945178	15.270733
22.808342	974.943886	15.275751
22.946114	965.385407	15.280768
22.357953	962.691025	15.285786
22.377639	964.035562	15.290803
22.822794	977.469757	15.295821
22.523704	974.761640	15.300839
22.952134	975.054355	15.305856
22.556613	972.853659	15.310874
22.707596	975.556730	15.315891
23.061285	977.432768	15.320909
22.408003	973.325300	15.325927
22.485591	973.423674	15.330944
22.867265	978.959266	15.335962
22.485530	975.689733	15.340979
22.893612	981.625137	15.345997
22.895070	982.666414	15.351015
23.215235	980.419856	15.356032
23.090492	985.084885	15.361050
22.966313	975.371781	15.366067
23.278793	986.358899	15.371085
22.888657	983.005473	15.376103
23.189668	986.581300	15.381120
22.882548	978.986030	15.386138
23.136334	984.039882	15.391155
23.118871	985.734229	15.396173
23.115763	984.579750	15.401191
23.156993	983.446728	15.406208
22.918082	990.111520	15.411226
22.939881	977.184979	15.416243
23.174074	983.595759	15.421261
22.888153	979.983005	15.426279
23.112415	989.156710	15.431296
23.243861	980.924671	15.436314
22.990484	979.758912	15.441331
23.399419	972.878285	15.446349
23.022416	983.225494	15.451367
23.133421	972.487762	15.456384
23.046409	980.555193	15.461402
23.100946	974.607419	15.466419
23.386462	982.244093	15.471437
23.309679	986.311465	15.476455
23.564401	988.853116	15.481472
23.408796	994.756921	15.486490
23.439139	989.109582	15.491507
23.623132	999.529851	15.496525
23.569843	999.140639	15.501543
23.622566	991.690957	15.506560
23.227585	993.109934	15.511578
22.986948	996.174174	15.516595
23.489319	995.202432	15.521613
22.960882	1001.079446	15.526631
23.437551	988.889526	15.531648
23.555342	996.211654	15.536666
23.475784	992.149991	15.541683
23.795318	995.656646	15.546701
23.605541	1000.227726	15.551719
23.680878	1003.119381	15.556736
23.947587	1019.945707	15.561754
23.971308	1017.070238	15.566771
24.075565	999.311772	15.571789
23.777904	1014.686463	15.576807
23.832102	993.174069	15.581824
23.674446	1000.615096	15.586842
24.157370	1012.465475	15.591859
24.067489	1003.403400	15.596877
23.667017	1009.389757	15.601895
23.844938	1003.529940	15.606912
24.091081	1017.888454	15.611930
23.980377	1024.608912	15.616947
24.109519	1020.558726	15.621965
24.408598	1021.588088	15.626983
24.481650	1014.946267	15.632000
24.420831	1007.602732	15.637018
24.201962	1009.871444	15.642035
24.506849	992.021589	15.647053
24.153511	989.230449	15.652071
24.431020	983.175152	15.657088
24.399293	988.390505	15.662106
24.314270	986.923809	15.667123
24.515999	986.453615	15.672141
23.867301	988.767579	15.677159
24.358914	983.884270	15.682176
24.201606	985.499541	15.687194
24.149724	992.980797	15.692211
24.498702	1008.345687	15.697229
24.640711	1011.687652	15.702247
24.680590	1010.049903	15.707264
24.431163	996.067608	15.712282
24.245339	1004.059012	15.717299
24.505132	1013.132487	15.722317
24.856548	1008.233268	15.727335
24.767879	1004.226680	15.732352
24.554674	1011.625921	15.737370
24.545401	1014.679161	15.742387
24.678745	1009.063015	15.747405
24.656283	1016.908907	15.752423
25.162706	1012.543986	15.757440
24.850998	1013.905736	15.762458
24.600687	1001.261656	15.767475
24.750573	1000.392480	15.772493
25.050438	1012.890088	15.777511
24.780930	1008.290129	15.782528
24.857217	1005.864024	15.787546
24.660279	1013.001938	15.792563
24.757807	1008.060446	15.797581
24.476266	1014.488925	15.802599
24.818711	1008.082613	15.807616
24.922104	1010.007339	15.812634
24.625838	1003.994595	15.817651
24.801905	1008.896527	15.822669
24.788154	1014.923282	15.827687
24.982647	1020.589203	15.832704
25.088514	1012.222300	15.837722
24.719987	1016.508961	15.842739
25.049706	1024.015649	15.847757
25.082243	1028.084837	15.852775
25.322756	1029.555729	15.857792
25.297802	1034.691139	15.862810
25.178731	1044.679228	15.867827
25.220686	1032.693091	15.872845
25.244756	1041.727773	15.877863
25.349186	1039.653867	15.882880
25.167988	1031.126802	15.887898
25.311918	1036.185257	15.892915
25.193223	1037.087570	15.897933
25.094682	1033.372861	15.902951
25.529358	1034.223186	15.907968
25.556539	1039.173700	15.912986
25.215669	1030.037325	15.918003
25.530372	1020.555239	15.923021
25.812489	1031.790143	15.928039
25.605435	1029.664054	15.933056
25.868060	1027.732623	15.938074
25.179521	1033.420134	15.943091
25.652469	1028.255711	15.948109
25.445691	1031.775406	15.953127
25.504753	1034.518136	15.958144
25.772237	1031.632874	15.963162
25.335657	1030.322244	15.968179
25.707750	1035.367041	15.973197
25.655642	1030.691989	15.978215
25.623040	1044.068544	15.983232
25.896004	1047.749766	15.988250
25.880686	1054.770876	15.993267
25.922946	1054.357224	15.998285
26.003917	1052.823488	16.003303
26.011208	1051.175062	16.008320
26.238150	1054.355403	16.013338
25.578361	1044.429530	16.018355
25.906249	1041.067735	16.023373
25.714654	1052.903902	16.028391
25.998195	1049.751030	16.033408
26.016856	1045.453056	16.038426
26.243066	1061.853414	16.043443
26.302443	1045.159149	16.048461
25.882826	1049.245535	16.053479
25.966332	1050.122480	16.058496
26.236914	1047.880526	16.063514
26.025001	1045.853028	16.068531
25.893257	1046.350280	16.073549
26.611126	1038.010555	16.078567
26.248004	1042.384739	16.083584
26.396365	1039.436088	16.088602
26.441553	1050.692347	16.093619
26.249982	1049.444314	16.098637
26.058549	1043.430912	16.103655
25.949607	1052.398076	16.108672
26.586804	1057.502331	16.113690
26.511226	1068.133727	16.118707
26.905013	1071.900167	16.123725
26.646984	1056.947165	16.128743
26.768986	1048.584028	16.133760
26.665032	1050.566493	16.138778
26.315759	1049.895444	16.143795
26.343639	1046.823656	16.148813
26.557743	1067.344313	16.153831
26.397985	1078.130918	16.158848
26.973876	1072.054087	16.163866
26.631302	1075.939057	16.168883
27.026445	1062.247045	16.173901
26.961899	1070.904300	16.178919
27.064420	1072.863884	16.183936
27.114991	1062.454309	16.188954
26.661907	1054.178119	16.193971
26.548538	1051.264162	16.198989
27.017093	1063.441880	16.204007
26.995374	1061.466633	16.209024
27.079509	1062.794768	16.214042
27.238132	1065.613423	16.219059
26.980269	1072.129733	16.224077
27.225204	1053.645414	16.229095
27.065094	1058.723110	16.234112
27.091674	1042.220181	16.239130
27.055064	1052.927515	16.244147
27.163203	1055.832975	16.249165
27.199492	1055.606454	16.254183
27.012773	1056.835013	16.259200
27.674544	1066.230548	16.264218
27.180162	1056.338714	16.269235
27.239459	1057.329907	16.274253
27.307453	1067.430714	16.279271
26.986855	1066.474300	16.284288
27.490446	1069.068490	16.289306
27.607585	1052.478778	16.294323
27.357306	1064.769124	16.299341
27.359911	1057.317800	16.304359
27.278358	1060.663243	16.309376
27.474678	1054.986723	16.314394
27.621013	1063.787661	16.319411
27.121338	1059.353142	16.324429
27.381560	1053.896988	16.329447
27.075726	1064.021649	16.334464
27.258572	1061.354775	16.339482
27.193708	1074.922604	16.344499
27.570443	1080.951318	16.349517
27.624796	1084.777255	16.354535
27.327904	1089.627077	16.359552
27.612913	1089.740291	16.364570
27.790416	1085.363770	16.369587
28.177896	1087.430190	16.374605
27.995542	1089.759464	16.379623
27.744682	1093.806797	16.384640
27.908776	1079.059043	16.389658
27.230684	1092.265365	16.394675
27.527678	1087.216858	16.399693
28.129302	1099.357972	16.404711
28.111565	1103.094220	16.409728
28.364759	1102.294061	16.414746
27.850681	1090.966216	16.419763
28.030783	1092.506540	16.424781
28.064199	1087.767578	16.429799
28.012600	1112.634522	16.434816
28.441636	1106.823691	16.439834
28.171666	1106.985988	16.444851
28.520878	1109.500228	16.449869
28.465625	1109.616260	16.454887
28.211610	1090.051875	16.459904
28.162292	1076.801882	16.464922
28.536481	1084.077562	16.469939
28.399023	1093.860273	16.474957
28.433400	1089.335759	16.479975
28.370046	1091.763156	16.484992
28.253849	1095.145593	16.490010
28.538896	1091.339212	16.495027
28.468197	1100.546567	16.500045
28.711914	1092.410497	16.505063
28.754754	1105.156728	16.510080
28.782327	1108.683903	16.515098
28.889989	1085.187445	16.520115
28.471194	1081.421916	16.525133
28.584704	1070.169327	16.530151
28.323120	1084.336041	16.535168
28.569252	1082.482929	16.540186
28.642475	1094.523790	16.545203
28.785741	1101.343343	16.550221
28.894128	1100.335493	16.555239
28.590324	1105.539860	16.560256
28.784080	1093.239558	16.565274
28.648585	1091.402057	16.570291
28.828979	1091.932457	16.575309
28.985350	1086.221159	16.580327
28.869854	1093.545164	16.585344
28.621221	1087.152537	16.590362
28.807440	1089.925846	16.595379
28.729784	1092.955099	16.600397
28.748898	1092.882750	16.605415
28.619710	1109.635488	16.610432
29.147333	1115.684754	16.615450
29.584632	1106.817744	16.620467
29.418112	1115.304801	16.625485
29.391743	1116.429343	16.630503
29.429083	1120.513579	16.635520
29.592791	1121.289597	16.640538
29.599194	1109.447837	16.645555
29.284746	1102.169249	16.650573
29.330226	1090.185677	16.655591
29.066040	1102.074276	16.660608
29.496320	1111.092687	16.665626
29.876199	1117.679510	16.670643
29.585511	1117.381140	16.675661
29.872647	1091.234025	16.680679
29.122468	1095.993921	16.685696
29.567643	1100.014253	16.690714
29.554573	1109.805886	16.695731
29.158007	1108.173393	16.700749
29.542232	1106.923505	16.705767
29.605107	1120.850059	16.710784
29.665413	1117.687969	16.715802
29.884847	1119.222132	16.720819
29.911957	1118.545760	16.725837
29.780461	1105.930328	16.730855
29.693275	1120.754570	16.735872
29.835930	1109.560507	16.740890
29.564837	1108.116642	16.745907
29.565434	1113.872934	16.750925
30.125145	1112.390419	16.755943
29.884949	1120.538720	16.760960
30.003525	1110.910586	16.765978
30.047354	1112.917241	16.770995
30.417759	1118.577722	16.776013
30.255702	1115.358952	16.781031
30.241679	1121.287953	16.786048
30.243002	1111.271083	16.791066
29.923597	1111.125539	16.796083
30.031443	1122.955862	16.801101
29.957656	1113.758662	16.806119
29.745654	1127.289623	16.811136
30.195938	1132.637786	16.816154
30.598587	1137.930295	16.821171
30.385895	1154.121788	16.826189
30.751301	1142.637178	16.831207
30.371176	1144.666079	16.836224
30.245488	1140.526401	16.841242
30.558289	1136.788248	16.846259
30.396119	1140.635499	16.851277
30.415739	1135.703022	16.856295
30.369310	1136.764434	16.861312
30.479877	1137.384673	16.866330
30.752302	1139.377605	16.871347
30.529806	1136.064157	16.876365
30.658571	1136.621583	16.881383
30.500684	1139.171097	16.886400
30.341621	1139.795711	16.891418
30.565879	1135.102577	16.896435
30.413134	1137.414595	16.901453
30.573280	1145.313985	16.906471
30.975566	1160.525484	16.911488
31.010264	1161.773008	16.916506
30.912807	1154.817014	16.921523
31.004444	1165.510633	16.926541
31.060912	1158.483183	16.931559
31.101887	1164.703391	16.936576
31.402814	1159.067253	16.941594
31.254218	1137.476003	16.946611
31.103264	1135.988065	16.951629
30.908930	1130.211778	16.956647
31.111902	1129.832906	16.961664
31.024779	1140.254710	16.966682
31.338254	1145.643246	16.971699
31.187278	1157.880227	16.976717
31.572167	1154.026631	16.981735
31.427578	1155.412701	16.986752
31.181479	1153.349520	16.991770
31.727572	1151.326324	16.996787
31.557616	1150.867023	17.001805
31.588634	1138.955113	17.006823
31.282342	1136.945548	17.011840
31.621291	1136.270809	17.016858
31.770762	1139.021481	17.021875
31.396594	1135.971643	17.026893
31.486976	1143.405426	17.031911
31.689480	1147.810937	17.036928
31.456403	1153.474462	17.041946
31.799117	1146.768250	17.046963
31.797607	1151.821123	17.051981
31.803418	1144.798460	17.056999
31.606239	1156.035953	17.062016
31.425000	1161.685047	17.067034
31.511686	1147.870882	17.072051
31.558899	1153.796611	17.077069
31.768223	1160.378614	17.082087
31.973908	1150.515899	17.087104
31.617879	1148.378422	17.092122
31.897189	1145.368210	17.097139
32.013542	1154.079214	17.102157
31.944774	1170.109314	17.107175
32.182897	1168.254292	17.112192
32.133358	1167.413198	17.117210
32.379146	1166.046137	17.122227
32.055466	1173.588990	17.127245
32.429337	1169.333165	17.132263
32.428902	1167.960500	17.137280
32.367613	1159.629186	17.142298
32.495142	1147.058350	17.147315
32.225936	1146.321102	17.152333
32.126382	1146.336776	17.157351
32.239681	1161.158043	17.162368
32.339061	1173.251664	17.167386
32.132307	1169.869470	17.172403
32.055104	1181.608902	17.177421
32.240094	1166.327613	17.182439
32.443699	1167.037420	17.187456
32.270117	1169.769283	17.192474
32.284930	1153.075587	17.197491
32.262945	1174.927269	17.202509
32.337850	1182.751667	17.207527
33.003921	1193.629863	17.212544
32.694329	1190.734004	17.217562
32.598890	1190.427132	17.222579
32.605626	1196.302412	17.227597
32.753499	1189.639335	17.232615
33.078767	1184.485382	17.237632
33.226482	1185.620524	17.242650
33.192664	1176.205585	17.247667
33.115657	1183.706638	17.252685
32.934961	1193.609789	17.257703
33.055201	1188.563700	17.262720
33.061321	1188.616467	17.267738
33.107314	1192.282787	17.272755
33.213343	1191.934882	17.277773
33.081548	1186.751552	17.282791
33.345054	1181.796630	17.287808
33.305800	1182.828518	17.292826
33.499976	1181.239164	17.297843
33.350787	1183.698956	17.302861
33.161844	1188.295201	17.307879
33.433537	1179.577182	17.312896
33.232736	1191.004618	17.317914
33.254868	1188.315567	17.322931
33.333382	1192.128274	17.327949
33.283364	1181.557661	17.332967
33.324900	1186.654293	17.337984
33.084606	1186.442703	17.343002
33.313779	1184.964633	17.348019
33.282444	1193.026593	17.353037
33.636978	1198.168865	17.358055
33.645843	1203.204348	17.363072
33.682896	1209.573512	17.368090
33.848921	1208.714420	17.373107
34.047813	1216.074427	17.378125
34.110756	1206.145681	17.383143
33.965057	1204.404443	17.388160
33.869532	1209.610922	17.393178
34.093540	1197.517253	17.398195
34.083306	1210.186666	17.403213
34.005121	1200.592468	17.408231
34.036350	1192.748428	17.413248
33.977760	1203.594999	17.418266
34.150559	1195.813986	17.423283
33.869570	1209.021294	17.428301
34.487180	1201.413589	17.433319
34.240210	1202.582168	17.438336
34.158517	1195.727833	17.443354
34.335820	1199.884834	17.448371
34.127303	1196.818499	17.453389
34.296724	1197.076060	17.458407
34.408964	1192.428865	17.463424
34.069266	1202.290660	17.468442
34.377773	1200.954797	17.473459
34.250294	1205.733924	17.478477
34.088614	1203.253557	17.483495
34.534697	1212.960683	17.488512
34.568624	1212.545177	17.493530
34.484970	1198.498878	17.498547
34.478188	1199.774995	17.503565
34.562224	1202.163534	17.508583
34.440291	1196.278049	17.513600
34.101525	1211.971783	17.518618
34.673454	1219.421670	17.523635
34.661717	1215.645984	17.528653
34.491864	1216.471112	17.533671
34.719831	1213.775055	17.538688
34.655135	1209.262878	17.543706
34.813094	1212.353067	17.548723
34.806788	1221.228493	17.553741
34.812816	1222.319563	17.558759
34.906522	1226.956741	17.563776
35.146912	1230.406413	17.568794
35.042956	1223.192628	17.573811
34.999223	1228.905408	17.578829
35.279856	1232.664365	17.583847
35.502576	1225.074339	17.588864
35.045440	1230.634134	17.593882
34.986913	1220.408823	17.598899
35.403511	1225.396208	17.603917
35.059511	1234.453943	17.608935
35.465265	1225.863224	17.613952
35.359349	1231.333276	17.618970
35.397367	1222.948502	17.623987
35.763662	1231.932817	17.629005
35.572496	1235.626836	17.634023
36.305711	1232.577052	17.639040
36.024933	1216.500826	17.644058
35.713401	1204.222809	17.649075
35.598135	1201.460608	17.654093
35.709434	1201.048759	17.659111
35.861039	1201.245993	17.664128
35.696858	1199.488716	17.669146
36.130142	1200.818964	17.674163
35.939150	1205.232492	17.679181
35.626506	1209.927020	17.684199
35.879651	1194.496169	17.689216
35.676544	1210.743018	17.694234
35.383702	1203.192752	17.699251
36.016342	1212.558216	17.704269
36.075498	1227.943459	17.709287
36.206705	1228.541532	17.714304
36.368584	1227.001416	17.719322
36.075909	1227.451302	17.724339
36.271970	1226.158302	17.729357
36.042510	1229.706837	17.734375
36.135166	1223.405859	17.739392
35.394746	1231.468479	17.744410
35.550405	1233.817397	17.749427
35.968438	1223.968710	17.754445
36.339951	1239.406011	17.759463
36.361222	1251.262607	17.764480
36.331559	1247.432917	17.769498
36.539862	1251.578762	17.774515
36.788709	1249.447490	17.779533
36.691380	1254.625861	17.784551
36.512096	1245.028544	17.789568
36.671923	1254.644840	17.794586
36.520124	1253.557824	17.799603
36.756390	1245.596427	17.804621
36.712713	1246.281863	17.809639
36.648606	1247.428105	17.814656
36.880633	1243.456426	17.819674
36.533912	1241.065007	17.824691
36.878216	1239.319578	17.829709
36.754238	1247.995698	17.834727
37.127984	1244.434172	17.839744
36.799258	1248.373815	17.844762
36.779034	1251.312042	17.849779
37.100757	1249.630112	17.854797
36.985123	1240.975905	17.859815
36.787927	1244.970681	17.864832
37.029721	1249.038693	17.869850
37.174331	1266.433509	17.874867
37.112002	1261.245585	17.879885
36.994837	1271.044148	17.884903
37.425303	1267.113958	17.889920
37.275280	1268.030659	17.894938
37.142325	1263.879467	17.899955
37.150958	1250.998973	17.904973
37.236399	1260.838373	17.909991
37.321508	1264.716336	17.915008
37.753239	1259.968572	17.920026
37.485626	1263.084421	17.925043
37.571479	1259.918303	17.930061
37.623124	1272.158330	17.935079
37.699307	1272.301109	17.940096
37.542934	1263.047341	17.945114
37.538525	1260.005822	17.950131
37.872661	1263.851080	17.955149
37.720494	1276.107263	17.960167
38.075124	1284.493812	17.965184
38.040971	1273.396779	17.970202
37.662718	1277.637686	17.975219
38.241846	1280.756576	17.980237
38.055405	1295.729063	17.985255
38.121971	1290.738693	17.990272
38.191785	1284.169865	17.995290
38.236128	1279.807848	18.000307
38.105595	1267.605574	18.005325
38.280415	1284.645370	18.010343
38.474422	1276.990391	18.015360
38.240587	1263.848066	18.020378
37.995826	1283.244782	18.025395
38.614401	1282.068622	18.030413
38.339132	1290.235119	18.035431
38.548770	1279.961446	18.040448
38.298404	1283.207145	18.045466
38.052314	1284.315628	18.050483
38.519915	1286.915490	18.055501
38.052458	1288.522575	18.060519
37.994027	1287.080090	18.065536
38.421240	1286.669237	18.070554
38.553933	1305.457711	18.075571
38.803870	1306.494791	18.080589
38.626125	1304.928983	18.085607
38.642814	1312.273394	18.090624
38.623418	1309.281553	18.095642
38.501919	1310.430479	18.100659
38.505257	1308.138843	18.105677
38.509099	1316.596148	18.110695
38.567471	1312.604323	18.115712
38.814510	1327.133365	18.120730
38.793554	1327.048359	18.125747
39.184799	1325.475454	18.130765
39.141144	1340.435074	18.135783
39.317434	1328.888454	18.140800
39.534601	1331.770565	18.145818
39.811352	1323.001189	18.150835
39.790947	1325.447135	18.155853
39.427049	1311.444656	18.160871
39.645748	1301.431491	18.165888
39.788340	1296.362934	18.170906
39.579255	1291.428376	18.175923
39.779694	1283.097024	18.180941
39.787051	1293.286356	18.185959
39.241461	1282.294696	18.190976
39.697905	1289.046317	18.195994
39.743721	1290.929600	18.201011
39.561913	1283.380839	18.206029
39.634721	1293.481020	18.211047
39.496031	1291.606127	18.216064
39.641670	1286.215193	18.221082
39.567589	1305.171768	18.226099
39.841540	1305.848468	18.231117
40.010371	1316.915104	18.236135
40.204216	1313.435401	18.241152
40.190354	1314.337082	18.246170
39.944802	1320.349764	18.251187
39.977846	1320.205803	18.256205
40.213699	1320.771704	18.261223
40.033156	1313.042845	18.266240
39.833527	1318.906316	18.271258
39.939645	1315.181573	18.276275
40.312144	1314.769824	18.281293
40.251226	1318.086836	18.286311
40.390980	1316.556491	18.291328
40.189209	1310.885455	18.296346
39.927783	1315.089132	18.301363
40.118449	1317.325276	18.306381
40.314029	1321.062863	18.311399
40.731149	1335.290700	18.316416
40.628105	1329.023503	18.321434
40.459075	1335.888920	18.326451
40.808008	1336.225658	18.331469
40.847235	1337.822791	18.336487
40.777946	1340.995946	18.341504
40.926888	1339.473628	18.346522
40.489722	1340.763536	18.351539
40.546735	1337.567208	18.356557
40.927990	1334.821868	18.361575
40.863028	1343.233159	18.366592
40.826708	1337.965396	18.371610
40.542346	1335.882941	18.376627
40.750975	1336.396302	18.381645
40.754983	1340.031359	18.386663
40.762903	1343.539568	18.391680
40.758432	1353.872805	18.396698
41.096972	1355.120075	18.401715
41.200837	1364.451699	18.406733
41.087858	1375.704541	18.411751
40.927848	1360.253071	18.416768
41.338989	1357.585099	18.421786
41.190762	1361.742648	18.426803
41.499173	1369.599973	18.431821
41.546069	1385.356514	18.436839
41.335184	1388.504523	18.441856
41.801920	1379.812655	18.446874
41.816729	1382.366705	18.451891
41.841864	1385.215794	18.456909
41.785329	1377.628430	18.461927
42.038554	1386.633695	18.466944
41.767427	1365.130797	18.471962
41.286525	1367.749888	18.476979
42.113227	1364.369843	18.481997
41.929447	1377.432652	18.487015
42.031884	1377.224167	18.492032
42.343441	1372.593035	18.497050
42.045365	1378.269971	18.502067
42.160462	1371.978048	18.507085
42.431768	1371.326524	18.512103
42.216794	1375.598679	18.517120
42.366493	1378.122126	18.522138
42.550092	1376.329277	18.527155
42.311745	1371.560233	18.532173
42.373870	1363.698654	18.537191
41.991812	1368.905890	18.542208
42.098545	1371.221466	18.547226
42.246027	1377.964722	18.552243
42.432748	1375.057345	18.557261
42.591397	1376.140291	18.562279
42.265634	1374.348350	18.567296
42.249054	1370.854267	18.572314
42.627970	1375.999083	18.577331
42.258035	1370.212360	18.582349
42.447376	1384.936689	18.587367
42.425833	1391.580196	18.592384
42.634692	1392.491169	18.597402
42.625521	1395.979974	18.602419
42.819490	1394.182343	18.607437
43.011087	1398.624341	18.612455
42.876987	1395.259123	18.617472
42.962386	1390.013301	18.622490
42.892664	1393.836653	18.627507
42.872812	1395.174794	18.632525
43.478085	1390.068433	18.637543
42.906616	1387.851068	18.642560
43.166004	1395.646655	18.647578
43.134878	1399.227267	18.652595
43.355738	1413.116673	18.657613
43.882978	1419.371240	18.662631
43.791741	1404.022570	18.667648
43.676277	1398.653576	18.672666
43.268763	1400.689952	18.677683
43.228650	1394.457054	18.682701
43.398414	1403.235554	18.687719
43.663561	1417.897539	18.692736
43.713598	1411.555833	18.697754
43.608336	1424.044619	18.702771
43.566478	1420.232582	18.707789
43.833274	1420.484358	18.712807
43.996436	1431.138526	18.717824
44.104562	1413.142348	18.722842
43.626506	1414.116763	18.727859
43.989497	1410.717842	18.732877
44.061160	1411.142207	18.737895
43.780191	1414.875580	18.742912
43.980907	1408.349315	18.747930
43.900307	1418.325274	18.752947
44.094760	1418.124463	18.757965
43.922074	1411.988073	18.762983
44.074480	1423.849486	18.768000
44.162084	1436.210229	18.773018
44.594330	1443.073002	18.778035
44.431371	1443.133325	18.783053
44.744174	1437.725622	18.788071
44.396958	1436.511416	18.793088
44.934671	1425.031188	18.798106
44.839381	1438.092800	18.803123
44.935559	1441.644007	18.808141
44.904648	1427.693409	18.813159
44.676648	1415.048696	18.818176
44.586080	1420.377540	18.823194
45.034645	1426.240477	18.828211
44.955697	1426.710532	18.833229
45.266342	1423.057868	18.838247
44.582721	1420.908564	18.843264
44.853795	1421.582564	18.848282
44.877866	1432.545715	18.853299
44.602026	1430.720699	18.858317
44.917827	1426.802129	18.863335
44.930815	1427.226219	18.868352
44.986650	1433.655640	18.873370
44.835548	1433.941332	18.878387
45.367252	1437.900846	18.883405
45.648993	1443.748900	18.888423
45.274632	1440.389757	18.893440
45.235953	1428.296063	18.898458
45.458750	1438.956673	18.903475
45.573597	1443.644245	18.908493
45.439645	1447.887943	18.913511
45.367306	1443.263291	18.918528
45.490098	1445.314418	18.923546
45.517898	1445.827711	18.928563
45.528030	1441.489951	18.933581
45.940688	1432.815997	18.938599
45.802289	1442.532771	18.943616
46.030912	1452.659124	18.948634
46.023562	1451.865057	18.953651
45.518130	1446.875897	18.958669
45.628009	1443.759633	18.963687
45.549910	1458.989847	18.968704
46.017111	1462.640724	18.973722
46.034155	1471.840833	18.978739
45.830602	1473.996746	18.983757
46.142021	1474.569748	18.988775
46.101510	1469.132183	18.993792
46.026556	1461.613943	18.998810
46.314891	1468.382505	19.003827
46.080083	1465.717890	19.008845
46.656640	1460.562358	19.013863
46.158949	1466.595658	19.018880
46.546614	1461.523372	19.023898
46.420942	1462.032307	19.028915
46.645187	1481.983786	19.033933
46.802981	1481.791874	19.038951
47.081144	1482.616251	19.043968
47.310171	1480.607982	19.048986
47.009428	1474.289654	19.054003
46.877028	1469.229418	19.059021
47.051867	1456.748786	19.064039
46.815447	1458.158734	19.069056
46.723213	1456.986630	19.074074
47.152886	1477.985248	19.079091
46.920906	1485.049941	19.084109
47.307945	1472.898984	19.089127
47.069781	1483.568724	19.094144
46.899517	1485.621588	19.099162
47.302913	1483.292497	19.104179
47.427295	1484.516524	19.109197
47.536737	1482.059913	19.114215
47.317019	1483.839647	19.119232
47.560896	1479.490503	19.124250
47.719875	1482.274454	19.129267
47.297825	1492.843616	19.134285
47.763367	1482.293038	19.139303
47.578938	1484.887786	19.144320
47.570090	1475.973727	19.149338
47.722107	1479.642430	19.154355
47.322229	1481.778608	19.159373
47.323391	1486.190502	19.164391
47.419959	1499.436703	19.169408
47.845815	1500.285279	19.174426
48.286125	1498.518472	19.179443
48.102331	1504.329027	19.184461
48.195769	1498.400231	19.189479
47.804783	1495.577036	19.194496
48.027771	1498.593968	19.199514
48.187000	1497.669653	19.204531
47.988591	1495.305457	19.209549
48.239679	1495.988903	19.214567
48.558259	1504.049830	19.219584
48.486608	1513.011383	19.224602
48.681856	1517.856799	19.229619
48.532153	1512.344806	19.234637
48.323595	1497.573038	19.239655
48.378306	1504.542326	19.244672
48.653305	1516.614977	19.249690
48.795010	1514.831834	19.254707
48.721034	1519.889853	19.259725
49.007820	1519.078102	19.264743
49.038585	1517.081957	19.269760
49.091272	1506.725443	19.274778
49.095513	1511.177888	19.279795
48.834415	1508.501606	19.284813
49.193344	1513.460237	19.289831
48.850330	1517.717771	19.294848
48.912048	1512.384102	19.299866
49.113818	1516.158631	19.304883
48.838472	1511.837179	19.309901
49.059317	1512.089844	19.314919
48.940472	1506.850740	19.319936
48.945628	1513.534293	19.324954
48.997175	1527.901617	19.329971
49.202066	1530.350163	19.334989
49.532107	1538.150523	19.340007
49.505955	1536.911253	19.345024
49.457116	1540.005497	19.350042
49.440295	1531.648106	19.355059
49.213822	1545.008072	19.360077
49.216764	1549.921499	19.365095
49.941120	1556.997337	19.370112
50.031144	1570.080506	19.375130
49.874985	1560.378405	19.380147
50.005654	1568.696032	19.385165
50.268205	1562.706003	19.390183
50.518246	1559.504640	19.395200
50.201962	1541.505397	19.400218
50.250829	1531.521869	19.405235
49.930892	1535.794727	19.410253
49.834566	1548.787152	19.415271
50.273564	1554.784181	19.420288
50.302110	1551.668018	19.425306
50.595549	1553.373670	19.430323
50.787355	1555.275135	19.435341
50.768259	1549.114633	19.440359
50.365747	1553.943257	19.445376
50.258488	1554.600795	19.450394
50.519956	1555.478286	19.455411
50.374177	1551.732998	19.460429
50.734173	1555.419627	19.465447
50.785323	1553.694852	19.470464
50.411649	1566.468799	19.475482
50.789526	1560.899379	19.480499
50.824282	1568.663962	19.485517
51.178579	1570.495787	19.490535
51.085162	1568.263460	19.495552
50.780247	1574.765233	19.500570
50.883870	1573.051170	19.505587
50.919326	1575.352692	19.510605
50.955458	1572.670858	19.515623
51.508951	1576.052607	19.520640
51.095771	1584.897283	19.525658
51.086994	1585.460494	19.530675
51.614127	1592.826036	19.535693
51.382128	1601.629710	19.540711
51.654805	1598.475289	19.545728
51.511640	1599.548729	19.550746
51.764086	1592.181119	19.555763
51.510937	1595.616667	19.560781
51.839435	1599.885780	19.565799
51.971847	1594.458955	19.570816
51.554423	1595.973016	19.575834
51.959879	1592.965058	19.580851
52.165814	1591.619990	19.585869
51.651477	1602.913767	19.590887
52.078115	1591.100525	19.595904
51.991615	1597.265113	19.600922
51.978101	1587.849932	19.605939
51.985615	1586.185642	19.610957
52.000478	1590.983597	19.615975
52.143063	1607.110368	19.620992
52.356481	1613.887567	19.626010
52.519512	1614.344961	19.631027
52.654594	1617.902732	19.636045
52.854063	1612.178203	19.641063
52.806424	1611.800715	19.646080
52.606341	1625.386992	19.651098
52.667369	1607.969227	19.656115
52.520892	1616.945710	19.661133
52.691314	1611.386686	19.666151
52.848987	1611.658718	19.671168
52.655082	1615.025024	19.676186
52.519127	1613.648310	19.681203
52.290099	1607.315543	19.686221
52.821427	1620.405349	19.691239
53.077337	1627.062281	19.696256
52.903763	1632.732414	19.701274
53.218547	1633.652051	19.706291
53.659876	1644.407939	19.711309
53.298876	1631.395726	19.716327
53.372036	1639.305809	19.721344
53.212339	1640.520704	19.726362
53.588119	1643.002455	19.731379
53.714964	1629.689736	19.736397
53.216971	1634.366075	19.741415
53.457846	1632.188667	19.746432
53.102649	1645.622528	19.751450
53.154441	1627.224686	19.756467
53.763476	1648.432100	19.761485
53.805256	1660.105864	19.766503
54.274051	1654.193950	19.771520
53.740553	1659.336629	19.776538
54.177144	1660.546468	19.781555
54.080625	1657.033293	19.786573
53.883871	1658.828382	19.791591
54.028755	1657.104691	19.796608
53.866182	1657.871890	19.801626
53.899700	1663.197145	19.806643
54.216641	1660.875266	19.811661
54.332876	1664.720036	19.816679
54.071532	1672.994983	19.821696
54.468932	1679.055380	19.826714
54.680054	1675.250992	19.831731
54.780353	1674.203350	19.836749
54.884950	1682.515647	19.841767
55.153259	1673.570689	19.846784
54.838117	1683.627726	19.851802
55.102778	1673.215813	19.856819
55.258367	1661.628038	19.861837
54.717372	1651.190879	19.866855
54.837510	1644.879134	19.871872
54.932144	1666.063017	19.876890
54.895203	1662.887664	19.881907
54.950344	1665.580610	19.886925
54.862018	1670.265359	19.891943
55.209139	1667.651557	19.896960
54.874473	1669.515594	19.901978
55.080791	1672.970692	19.906995
55.264569	1670.202591	19.912013
55.261606	1689.063219	19.917031
55.573557	1691.166793	19.922048
55.638996	1691.648947	19.927066
55.652292	1685.047800	19.932083
55.705755	1691.739630	19.937101
55.322764	1693.630177	19.942119
55.397177	1686.211523	19.947136
55.771493	1690.773297	19.952154
55.651799	1691.499064	19.957171
55.773464	1697.952981	19.962189
55.756541	1692.148715	19.967207
55.956649	1688.573280	19.972224
56.007345	1693.744366	19.977242
55.849896	1717.394749	19.982259
56.324191	1715.243880	19.987277
56.325027	1721.590498	19.992295
56.244579	1713.937306	19.997312
56.444498	1713.947087	20.002330
56.333582	1711.436602	20.007347
56.335172	1710.076202	20.012365
56.261889	1717.378068	20.017383
56.522535	1709.655657	20.022400
56.508241	1710.137681	20.027418
56.550689	1710.001711	20.032435
56.732087	1711.355683	20.037453
56.952113	1725.447447	20.042471
57.165858	1720.680064	20.047488
57.186506	1715.406420	20.052506
56.865402	1713.010922	20.057523
57.332471	1713.774153	20.062541
57.142829	1706.466294	20.067559
57.191202	1700.894805	20.072576
57.234500	1721.291491	20.077594
57.374676	1723.216843	20.082611
57.555994	1730.504073	20.087629
57.381574	1741.277594	20.092647
57.496796	1725.990979	20.097664
57.086822	1732.461928	20.102682
57.554984	1732.963042	20.107699
57.775703	1741.396036	20.112717
57.329460	1744.943921	20.117735
57.475019	1733.326112	20.122752
57.370920	1734.923644	20.127770
57.514811	1731.558991	20.132787
57.533526	1745.754898	20.137805
57.694365	1757.018731	20.142823
57.778895	1765.495165	20.147840
58.165674	1754.546490	20.152858
57.790795	1752.601250	20.157875
57.888202	1751.140623	20.162893
57.886633	1767.428988	20.167911
58.150773	1764.907073	20.172928
58.505329	1785.059393	20.177946
58.443849	1789.276037	20.182963
58.574876	1787.699680	20.187981
58.353477	1784.477461	20.192999
58.861232	1788.740627	20.198016
58.843428	1779.995087	20.203034
58.844034	1776.968474	20.208051
59.069831	1773.325877	20.213069
58.650398	1777.971008	20.218087
58.954140	1767.432989	20.223104
59.047774	1776.725404	20.228122
59.092273	1776.336633	20.233139
59.511977	1778.852550	20.238157
59.164384	1773.207369	20.243175
59.034460	1765.741798	20.248192
59.121290	1775.603355	20.253210
59.307823	1771.821735	20.258227
59.468607	1767.381393	20.263245
59.122512	1771.778333	20.268263
59.659851	1773.313242	20.273280
59.605327	1765.539194	20.278298
59.270388	1775.416337	20.283315
59.625892	1769.733587	20.288333
59.366974	1768.868460	20.293351
59.496427	1773.004690	20.298368
59.822522	1787.237683	20.303386
59.767971	1791.487957	20.308403
60.352190	1789.263049	20.313421
60.349061	1791.996704	20.318439
60.248616	1786.495844	20.323456
60.320739	1775.965706	20.328474
59.926502	1782.159636	20.333491
60.230838	1777.917720	20.338509
59.959318	1789.214597	20.343527
60.115582	1790.607230	20.348544
60.067820	1780.212644	20.353562
60.035326	1783.531600	20.358579
60.336780	1783.771640	20.363597
59.946134	1803.731449	20.368615
60.432742	1798.138609	20.373632
60.448975	1812.170847	20.378650
60.147927	1811.763626	20.383667
60.697890	1798.318213	20.388685
60.782233	1811.017417	20.393703
60.953194	1815.295485	20.398720
60.715694	1814.556396	20.403738
60.811078	1830.611864	20.408755
60.983516	1830.868963	20.413773
60.962385	1829.417434	20.418791
61.051884	1838.432800	20.423808
60.828003	1827.343057	20.428826
60.995234	1838.012611	20.433843
61.624514	1842.083170	20.438861
61.940459	1857.595989	20.443879
61.426304	1855.861919	20.448896
61.812632	1855.021933	20.453914
61.584996	1851.655504	20.458931
62.184437	1847.641907	20.463949
61.891616	1846.381276	20.468967
62.053302	1849.332129	20.473984
62.007104	1840.938168	20.479002
61.845333	1850.990205	20.484019
62.041362	1842.331060	20.489037
61.982185	1851.985147	20.494055
62.113687	1850.317186	20.499072
62.317533	1843.127513	20.504090
61.981325	1850.827256	20.509107
62.213336	1841.603861	20.514125
62.024122	1844.975787	20.519143
62.180698	1844.679915	20.524160
62.586651	1846.064992	20.529178
62.578260	1865.949200	20.534195
62.596211	1863.718324	20.539213
62.561094	1861.167539	20.544231
62.618994	1865.614820	20.549248
63.170673	1862.858481	20.554266
62.939701	1862.954709	20.559283
63.041372	1860.451924	20.564301
62.930028	1854.728675	20.569319
62.778154	1856.314767	20.574336
63.024307	1849.806471	20.579354
63.153928	1863.445419	20.584371
63.332065	1869.410838	20.589389
63.491297	1868.079380	20.594407
63.106482	1876.578906	20.599424
63.590579	1863.838086	20.604442
63.653570	1877.986133	20.609459
63.844862	1875.598701	20.614477
63.813733	1867.849348	20.619495
63.668803	1873.502444	20.624512
63.800663	1878.389450	20.629530
64.051884	1874.146365	20.634547
64.045375	1864.827777	20.639565
63.812174	1869.377476	20.644583
63.836526	1876.578898	20.649600
64.133879	1870.709554	20.654618
63.765674	1876.984651	20.659635
64.232471	1867.636089	20.664653
64.222070	1869.095869	20.669671
64.090996	1872.048410	20.674688
64.332336	1869.823561	20.679706
64.439163	1880.313245	20.684723
64.511415	1872.304680	20.689741
64.443348	1883.064779	20.694759
64.750998	1889.953559	20.699776
64.989769	1895.862147	20.704794
64.820740	1888.999137	20.709811
64.777727	1885.777355	20.714829
64.712135	1893.084400	20.719847
64.645864	1897.257635	20.724864
64.797578	1894.718601	20.729882
64.834119	1887.586683	20.734899
65.274264	1898.200890	20.739917
65.016937	1896.915759	20.744935
64.924992	1910.324352	20.749952
65.219001	1912.856826	20.754970
65.446202	1919.461557	20.759987
65.688743	1914.623335	20.765005
65.799578	1914.748066	20.770023
65.366263	1911.641083	20.775040
65.772188	1907.537864	20.780058
65.669334	1910.485990	20.785075
65.726255	1911.976253	20.790093
65.313970	1912.132448	20.795111
65.864422	1920.608546	20.800128
65.905217	1918.225751	20.805146
65.991483	1930.931052	20.810163
66.069438	1937.385592	20.815181
66.371252	1944.407861	20.820199
66.442910	1937.589179	20.825216
66.499574	1931.258875	20.830234
66.510217	1939.156793	20.835251
66.569120	1937.752680	20.840269
66.460830	1935.109200	20.845287
66.519570	1936.384571	20.850304
66.650676	1938.080979	20.855322
66.584886	1934.878537	20.860339
66.610654	1925.778937	20.865357
66.729950	1945.750534	20.870375
66.273493	1945.528615	20.875392
67.003448	1956.072203	20.880410
66.937484	1963.480327	20.885427
67.253717	1964.967839	20.890445
67.525832	1963.410391	20.895463
66.871124	1961.209147	20.900480
67.132663	1955.149714	20.905498
67.045376	1956.675199	20.910515
66.955240	1968.388769	20.915533
67.472998	1965.517801	20.920551
67.271053	1976.384144	20.925568
67.378324	1977.651915	20.930586
67.472444	1981.064687	20.935603
67.447254	1985.805903	20.940621
67.609052	1979.348649	20.945639
67.656054	1995.121491	20.950656
68.245951	1993.346982	20.955674
67.987233	2000.179364	20.960691
68.430412	2000.248869	20.965709
68.208379	1999.983910	20.970727
68.361474	2004.305850	20.975744
68.454828	1999.633001	20.980762
68.774499	2004.724163	20.985779
68.527394	1992.820544	20.990797
68.729592	1993.855677	20.995815
68.648555	1998.485718	21.000832
68.915016	1996.054932	21.005850
68.923449	2001.103331	21.010867
68.645427	1998.016186	21.015885
69.014605	1990.033636	21.020903
68.776417	1995.994893	21.025920
68.946276	1987.740594	21.030938
69.000444	1995.597001	21.035955
68.895093	1987.499438	21.040973
68.895910	1994.313247	21.045991
68.852473	1994.288568	21.051008
68.866213	2002.192341	21.056026
69.503521	2010.566505	21.061043
69.280803	2017.011373	21.066061
69.499019	2011.665660	21.071079
69.239000	2011.905304	21.076096
69.711948	2021.065828	21.081114
69.609054	2022.164543	21.086131
69.707673	2036.891000	21.091149
70.095257	2031.648143	21.096167
69.898707	2038.988389	21.101184
70.033565	2032.115584	21.106202
70.092815	2030.234849	21.111219
70.227917	2024.798004	21.116237
70.532024	2024.254937	21.121255
70.353380	2027.420098	21.126272
70.418089	2024.241378	21.131290
70.171291	2026.470408	21.136307
70.324859	2025.146138	21.141325
70.561993	2017.241072	21.146343
70.826883	2029.287250	21.151360
70.786522	2047.696490	21.156378
70.510539	2046.938172	21.161395
70.790768	2042.630538	21.166413
71.563476	2033.761020	21.171431
71.304199	2042.985780	21.176448
71.388518	2038.427954	21.181466
71.234327	2039.503147	21.186483
71.112108	2036.492578	21.191501
71.453486	2028.965679	21.196519
71.504860	2025.306176	21.201536
71.539770	2035.336969	21.206554
71.611789	2032.075045	21.211571
71.629206	2035.405164	21.216589
71.963713	2023.662883	21.221607
71.599996	2035.895921	21.226624
71.632745	2027.587341	21.231642
71.896152	2034.265343	21.236659
71.567085	2034.064492	21.241677
71.965199	2039.623091	21.246695
71.784883	2042.709617	21.251712
71.761936	2049.164226	21.256730
72.264002	2049.912522	21.261747
72.309310	2061.380854	21.266765
72.681468	2051.513654	21.271783
72.443290	2051.459521	21.276800
72.196461	2044.551832	21.281818
72.229174	2047.216789	21.286835
72.312129	2054.794137	21.291853
72.431557	2057.193027	21.296871
72.793225	2073.651995	21.301888
72.647744	2086.592545	21.306906
73.270218	2082.117663	21.311923
72.926991	2080.303136	21.316941
73.073990	2081.646747	21.321959
73.067224	2075.834453	21.326976
73.159869	2076.432286	21.331994
73.253181	2082.108086	21.337011
72.719186	2074.882431	21.342029
73.442863	2074.516642	21.347047
73.798726	2098.099728	21.352064
73.558633	2095.887160	21.357082
73.458913	2093.198129	21.362099
73.758235	2102.449018	21.367117
73.798442	2094.830412	21.372135
73.659487	2096.215670	21.377152
73.648341	2094.885641	21.382170
73.853072	2097.706705	21.387187
73.846748	2094.646408	21.392205
73.629743	2097.565108	21.397223
73.576024	2102.711643	21.402240
73.991905	2121.273556	21.407258
74.437798	2109.529547	21.412275
74.410558	2114.949669	21.417293
74.460964	2102.538581	21.422311
74.345396	2113.587148	21.427328
74.583356	2127.341878	21.432346
74.856731	2137.609944	21.437363
74.849308	2138.883071	21.442381
75.044410	2132.531007	21.447399
75.070729	2139.006334	21.452416
74.910625	2136.509808	21.457434
75.442002	2131.885071	21.462451
75.147861	2139.423699	21.467469
75.627336	2138.338716	21.472487
75.406303	2132.635719	21.477504
75.145337	2133.257395	21.482522
75.740908	2127.019328	21.487539
75.176093	2132.892938	21.492557
75.225561	2138.607186	21.497575
75.630643	2153.547676	21.502592
75.534837	2153.932020	21.507610
75.749886	2150.231067	21.512627
75.717331	2161.149884	21.517645
76.078743	2162.311574	21.522663
75.971786	2169.177051	21.527680
75.849371	2172.327116	21.532698
76.304930	2184.870588	21.537715
76.183117	2185.959653	21.542733
76.188723	2189.395801	21.547751
76.400368	2182.242644	21.552768
76.278597	2187.308339	21.557786
76.545536	2188.219723	21.562803
76.900587	2198.471870	21.567821
77.071725	2203.709447	21.572839
77.406900	2201.981140	21.577856
77.156091	2202.377146	21.582874
77.314240	2179.505711	21.587891
77.311300	2173.307747	21.592909
77.347846	2167.242465	21.597927
77.189743	2183.401086	21.602944
77.346257	2182.398261	21.607962
77.590279	2192.800355	21.612979
77.446740	2198.857311	21.617997
77.726542	2197.989817	21.623015
77.739811	2197.003122	21.628032
77.577521	2201.866869	21.633050
77.986161	2197.728444	21.638067
77.499054	2201.244945	21.643085
77.946503	2198.590101	21.648103
77.654655	2196.404565	21.653120
77.574338	2200.655817	21.658138
77.688193	2193.470636	21.663155
77.799372	2209.167334	21.668173
78.155035	2210.932736	21.673191
78.018724	2218.140530	21.678208
78.138243	2212.668198	21.683226
78.557423	2217.598652	21.688243
78.506836	2224.815110	21.693261
78.526929	2234.977735	21.698279
78.747109	2243.256404	21.703296
78.687512	2240.914544	21.708314
79.027611	2238.749924	21.713331
78.882165	2250.330320	21.718349
79.040948	2247.998430	21.723367
78.838601	2246.174438	21.728384
78.854892	2249.833004	21.733402
79.127627	2251.557750	21.738419
79.317161	2264.688958	21.743437
79.228806	2260.214938	21.748455
79.268945	2260.432807	21.753472
79.427353	2259.918872	21.758490
79.851293	2266.451879	21.763507
79.797896	2270.522190	21.768525
79.806535	2272.809067	21.773543
80.172145	2280.342226	21.778560
79.613905	2284.797776	21.783578
80.227028	2282.394698	21.788595
80.319042	2287.253342	21.793613
80.440642	2278.476249	21.798631
80.623085	2282.702134	21.803648
80.574271	2283.808172	21.808666
80.538354	2280.282224	21.813683
80.621311	2280.594378	21.818701
80.570951	2279.658677	21.823719
80.649113	2280.580705	21.828736
80.621902	2286.796206	21.833754
81.170562	2292.318674	21.838771
81.291982	2305.069229	21.843789
81.029286	2307.209257	21.848807
81.463351	2300.769197	21.853824
80.994365	2305.438005	21.858842
81.568385	2303.000022	21.863859
81.714343	2304.088171	21.868877
81.566668	2304.729975	21.873895
81.405600	2298.591459	21.878912
81.375825	2295.610547	21.883930
81.560695	2290.923285	21.888947
81.424796	2306.494662	21.893965
81.471808	2310.710211	21.898983
81.795685	2312.991889	21.904000
81.869696	2324.995582	21.909018
82.283580	2322.361760	21.914035
81.919886	2319.117552	21.919053
82.181352	2318.376012	21.924071
82.266134	2321.452611	21.929088
82.482172	2336.312410	21.934106
82.364283	2331.255968	21.939123
82.581320	2342.621828	21.944141
82.655652	2337.093415	21.949159
82.991258	2333.667053	21.954176
82.760629	2341.366243	21.959194
83.062678	2326.378079	21.964211
83.164867	2327.779227	21.969229
82.855240	2325.217730	21.974247
83.141329	2318.633575	21.979264
83.006854	2336.057377	21.984282
83.367366	2343.323094	21.989299
83.460091	2345.480031	21.994317
83.677413	2349.223897	21.999335
83.611742	2349.833919	22.004352
83.589980	2351.989857	22.009370
83.886705	2361.121357	22.014387
83.874958	2349.448893	22.019405
83.725405	2354.484271	22.024423
83.874761	2351.986571	22.029440
83.575951	2356.865437	22.034458
83.979303	2359.696454	22.039475
83.992457	2375.828416	22.044493
84.214122	2377.513834	22.049511
84.498910	2369.260291	22.054528
84.535855	2370.094099	22.059546
84.502528	2376.995461	22.064563
84.845913	2387.091741	22.069581
84.485910	2375.814680	22.074599
84.648899	2392.232479	22.079616
84.636453	2403.123044	22.084634
84.898113	2398.152298	22.089651
84.737847	2404.088856	22.094669
84.672716	2409.603374	22.099687
84.584673	2406.211812	22.104704
85.048079	2417.428656	22.109722
85.298523	2410.304047	22.114739
85.232944	2414.149059	22.119757
85.079827	2434.220690	22.124775
85.464828	2440.835609	22.129792
85.834382	2437.081985	22.134810
85.948951	2440.235997	22.139827
86.186620	2440.063124	22.144845
86.395488	2444.685732	22.149863
86.471791	2431.800099	22.154880
86.317935	2435.602137	22.159898
86.302202	2428.907424	22.164915
86.416244	2435.896184	22.169933
86.296603	2430.918891	22.174951
86.565487	2439.297327	22.179968
86.471025	2445.106813	22.184986
86.875572	2456.676919	22.190003
87.057724	2460.640934	22.195021
86.998253	2464.241980	22.200039
87.007648	2458.818388	22.205056
87.238065	2457.330553	22.210074
87.030048	2451.009974	22.215091
87.619415	2452.764034	22.220109
87.362721	2454.429723	22.225127
87.608960	2448.025350	22.230144
87.030000	2451.117591	22.235162
87.202048	2445.359221	22.240179
87.722155	2459.707535	22.245197
87.569683	2471.001968	22.250215
87.995257	2471.522404	22.255232
88.196491	2476.878435	22.260250
88.104230	2482.561343	22.265267
88.681691	2478.844573	22.270285
88.391309	2477.113252	22.275303
88.673938	2479.603406	22.280320
88.405208	2476.688307	22.285338
88.316213	2472.416325	22.290355
88.389472	2471.606427	22.295373
88.180263	2478.784718	22.300391
88.408033	2489.221092	22.305408
88.516896	2497.804525	22.310426
88.550717	2491.632253	22.315443
88.932849	2496.944167	22.320461
88.668134	2496.259809	22.325479
88.977679	2497.940939	22.330496
88.891010	2511.465930	22.335514
89.231586	2515.651314	22.340531
89.465586	2518.549919	22.345549
88.827730	2526.751690	22.350567
89.248473	2517.697216	22.355584
89.088006	2523.813744	22.360602
89.618057	2536.670873	22.365619
89.885305	2544.055436	22.370637
90.044912	2540.950129	22.375655
89.750021	2542.675464	22.380672
89.819911	2540.051319	22.385690
90.053669	2547.068708	22.390707
90.788682	2554.522015	22.395725
90.536377	2558.090169	22.400743
90.420104	2557.701321	22.405760
90.405578	2556.930422	22.410778
90.661299	2564.708159	22.415795
91.014943	2553.669508	22.420813
90.722600	2558.206553	22.425831
90.846424	2547.345937	22.430848
90.945771	2554.226582	22.435866
91.030117	2554.547992	22.440883
91.261852	2563.049083	22.445901
90.949344	2578.837734	22.450919
91.395084	2580.519626	22.455936
91.366993	2570.531797	22.460954
91.487204	2576.307692	22.465971
92.025942	2584.845910	22.470989
91.514580	2573.728152	22.476007
91.869154	2573.233974	22.481024
91.802271	2586.951602	22.486042
91.790944	2599.666354	22.491059
92.135273	2599.565141	22.496077
92.365832	2597.805845	22.501095
92.389939	2605.077033	22.506112
92.638637	2603.387486	22.511130
92.002865	2603.979527	22.516147
92.857961	2601.333349	22.521165
92.702173	2605.568116	22.526183
92.854345	2624.178179	22.531200
93.101607	2621.728227	22.536218
92.631427	2622.313261	22.541235
93.303594	2626.980107	22.546253
93.064970	2631.616063	22.551271
93.030897	2623.970996	22.556288
93.373592	2613.672560	22.561306
93.266837	2615.838690	22.566323
93.430242	2619.467971	22.571341
93.383918	2641.028578	22.576359
93.728538	2651.254215	22.581376
93.870244	2646.538906	22.586394
93.786163	2647.615775	22.591411
93.987793	2649.840902	22.596429
93.915667	2643.041324	22.601447
93.888262	2645.791536	22.606464
94.239028	2653.349272	22.611482
94.324734	2664.208836	22.616499
94.956424	2659.830211	22.621517
94.618753	2672.908602	22.626535
94.518971	2663.907202	22.631552
94.641485	2664.866489	22.636570
94.514373	2664.558240	22.641587
94.510381	2661.532198	22.646605
94.729829	2673.450216	22.651623
95.002536	2676.986636	22.656640
95.269098	2678.917541	22.661658
95.546328	2686.452094	22.666675
95.553946	2680.732035	22.671693
95.471301	2682.998549	22.676711
95.915672	2682.947941	22.681728
95.794485	2681.477301	22.686746
95.792721	2687.038787	22.691763
95.777804	2668.662953	22.696781
95.821852	2675.820580	22.701799
96.083138	2667.993506	22.706816
95.815852	2678.204562	22.711834
95.248801	2686.294315	22.716851
95.798776	2693.120192	22.721869
96.099727	2696.188237	22.726887
96.149909	2702.625312	22.731904
96.476539	2713.349319	22.736922
96.080069	2730.060228	22.741939
96.543622	2732.701973	22.746957
96.486374	2725.865314	22.751975
96.528795	2741.409130	22.756992
97.114292	2736.636892	22.762010
96.678182	2746.890218	22.767027
96.883202	2747.044386	22.772045
97.514693	2752.487741	22.777063
97.631692	2764.478681	22.782080
97.518379	2765.645353	22.787098
97.368132	2775.254237	22.792115
97.383612	2774.551219	22.797133
97.570318	2780.761781	22.802151
97.672930	2794.374107	22.807168
98.230179	2790.086019	22.812186
98.000502	2798.839414	22.817203
98.347631	2799.359527	22.822221
98.290254	2795.129858	22.827239
98.280257	2793.853251	22.832256
98.890701	2812.748359	22.837274
98.525491	2816.321627	22.842291
99.038430	2816.632705	22.847309
99.108842	2820.667962	22.852327
99.099174	2812.318322	22.857344
99.312623	2812.297581	22.862362
99.219316	2805.520196	22.867379
99.028680	2816.795575	22.872397
99.296438	2814.421290	22.877415
99.321579	2812.782530	22.882432
99.135603	2805.543082	22.887450
99.358495	2828.971219	22.892467
99.632076	2828.634907	22.897485
99.826460	2833.603909	22.902503
99.665901	2831.334600	22.907520
99.939667	2831.058228	22.912538
99.971869	2836.466098	22.917555
100.233831	2847.610620	22.922573
100.377416	2858.603261	22.927591
100.435385	2853.102504	22.932608
100.515197	2848.601991	22.937626
100.562922	2860.168295	22.942643
100.746709	2847.634798	22.947661
100.982977	2843.030869	22.952679
100.768963	2854.874891	22.957696
101.164322	2866.494045	22.962714
101.222762	2863.044728	22.967731
101.329859	2867.904323	22.972749
101.532616	2872.168195	22.977767
101.301309	2869.417602	22.982784
101.571704	2876.956463	22.987802
101.226402	2878.121613	22.992819
101.656155	2875.904999	22.997837
101.779470	2878.262360	23.002855
101.857807	2898.522334	23.007872
101.861784	2903.079319	23.012890
102.425954	2902.722730	23.017907
102.392442	2891.813965	23.022925
102.585292	2892.159413	23.027943
102.536766	2893.104478	23.032960
102.710173	2883.157498	23.037978
102.352089	2892.136208	23.042995
102.945898	2893.012200	23.048013
102.772148	2882.052820	23.053031
102.223813	2899.494664	23.058048
103.144840	2903.630230	23.063066
103.428102	2917.084943	23.068083
103.271325	2917.936503	23.073101
103.728145	2922.744477	23.078119
103.282127	2915.365823	23.083136
103.736874	2912.135308	23.088154
103.577546	2922.364306	23.093171
103.412085	2912.145314	23.098189
103.438027	2918.955538	23.103207
103.730458	2935.669173	23.108224
103.853117	2936.776792	23.113242
103.779242	2939.881511	23.118259
104.328339	2946.802309	23.123277
104.494899	2961.458912	23.128295
104.273266	2960.095516	23.133312
103.972809	2961.149492	23.138330
104.146890	2959.907158	23.143347
104.147355	2978.115269	23.148365
104.995890	2982.287461	23.153383
105.309297	2994.257251	23.158400
105.337759	2987.476502	23.163418
105.241140	2983.682179	23.168435
105.281248	2988.249307	23.173453
105.260991	2979.692939	23.178471
105.541085	2995.641606	23.183488
105.727883	3001.041086	23.188506
105.644877	3008.938366	23.193523
105.726284	3004.885744	23.198541
106.456678	3003.095444	23.203559
106.077890	3009.205309	23.208576
106.136641	2998.509272	23.213594
106.647084	3002.355694	23.218611
106.176276	3001.564731	23.223629
106.634528	3006.732312	23.228647
106.800073	3020.215014	23.233664
106.836859	3018.811126	23.238682
107.050149	3019.765678	23.243699
106.970148	3021.649919	23.248717
107.552532	3023.168418	23.253735
107.007440	3022.764681	23.258752
106.940660	3023.223401	23.263770
107.062449	3027.572588	23.268787
106.998237	3021.614334	23.273805
107.159753	3036.527442	23.278823
107.194347	3027.103968	23.283840
107.380684	3042.836963	23.288858
107.498466	3063.327659	23.293875
107.732028	3072.276888	23.298893
107.950241	3067.666263	23.303911
107.818878	3074.558002	23.308928
108.488413	3080.746678	23.313946
108.334972	3087.746037	23.318963
108.211975	3088.384001	23.323981
108.484088	3094.429793	23.328999
108.553457	3098.206465	23.334016
108.953093	3080.563787	23.339034
108.674741	3086.998814	23.344051
108.882552	3104.903134	23.349069
109.125149	3120.804131	23.354087
109.058856	3121.357463	23.359104
109.595410	3113.837412	23.364122
109.328177	3108.939866	23.369139
109.220100	3107.959507	23.374157
109.739465	3110.441067	23.379175
109.564406	3129.456417	23.384192
109.848882	3126.176792	23.389210
110.010700	3134.291424	23.394227
110.148228	3126.837039	23.399245
110.362834	3123.243270	23.404263
110.184212	3142.328629	23.409280
110.428013	3136.795515	23.414298
110.436803	3146.480679	23.419315
110.430697	3160.940404	23.424333
110.911459	3151.898306	23.429351
110.636197	3155.141925	23.434368
111.193549	3157.137792	23.439386
110.888413	3154.057849	23.444403
111.019418	3167.991101	23.449421
111.367111	3176.625816	23.454439
111.098896	3182.024044	23.459456
111.341227	3181.998779	23.464474
111.274427	3184.632152	23.469491
111.496819	3193.908284	23.474509
111.707503	3191.748048	23.479527
111.323942	3201.182243	23.484544
111.710203	3207.308033	23.489562
112.093473	3226.472730	23.494579
112.489304	3228.642255	23.499597
112.707036	3224.789163	23.504615
112.701339	3225.601286	23.509632
112.941048	3220.561162	23.514650
113.062052	3217.079882	23.519667
112.826072	3228.138528	23.524685
113.204035	3226.488641	23.529703
112.949269	3247.107350	23.534720
112.750839	3240.160053	23.539738
113.274718	3246.463139	23.544755
113.170745	3246.892972	23.549773
113.207879	3251.422758	23.554791
113.920296	3263.191340	23.559808
113.776323	3266.000940	23.564826
114.162037	3259.757492	23.569843
114.056900	3271.067103	23.574861
114.633250	3259.251413	23.579879
114.282527	3259.663092	23.584896
114.223105	3263.576758	23.589914
114.628669	3273.231390	23.594931
114.788863	3284.174346	23.599949
115.116539	3280.468143	23.604967
114.811890	3290.300335	23.609984
114.936253	3280.742727	23.615002
115.284789	3280.009604	23.620019
115.196715	3283.492200	23.625037
115.344763	3276.174981	23.630055
115.159633	3291.802265	23.635072
115.076716	3301.650225	23.640090
115.793274	3310.710121	23.645107
115.368773	3313.055522	23.650125
115.581954	3309.758627	23.655143
115.626363	3322.405188	23.660160
115.866841	3325.883662	23.665178
116.071964	3323.093029	23.670195
116.102077	3323.703858	23.675213
116.298972	3319.408979	23.680231
116.262255	3344.841653	23.685248
116.799812	3347.970587	23.690266
116.982454	3345.454911	23.695283
116.910826	3352.608836	23.700301
117.102173	3353.424813	23.705319
117.310374	3352.391733	23.710336
117.235210	3349.727072	23.715354
117.033787	3340.201536	23.720371
117.818844	3360.035681	23.725389
117.945660	3359.050071	23.730407
117.933534	3362.669129	23.735424
117.693378	3366.885728	23.740442
117.856066	3367.286411	23.745459
117.841689	3367.497053	23.750477
117.847821	3366.675538	23.755495
117.953785	3373.820586	23.760512
118.301778	3379.955586	23.765530
118.672201	3384.426876	23.770547
118.261200	3386.489263	23.775565
118.566375	3384.175324	23.780583
118.647737	3396.904524	23.785600
118.745630	3398.596806	23.790618
119.045997	3404.616182	23.795635
119.058360	3407.799002	23.800653
119.297264	3414.219389	23.805671
119.509514	3414.290369	23.810688
119.388821	3418.857548	23.815706
119.915483	3419.845089	23.820723
119.758450	3427.596336	23.825741
119.914510	3424.791280	23.830759
119.871506	3431.789251	23.835776
120.545894	3448.030048	23.840794
120.242661	3443.037049	23.845811
120.608260	3447.114576	23.850829
120.535182	3451.178767	23.855847
120.405979	3454.588933	23.860864
120.552401	3455.664455	23.865882
121.010724	3461.614916	23.870899
120.982344	3475.503939	23.875917
121.343535	3470.009145	23.880935
121.566308	3469.993257	23.885952
121.712791	3469.878850	23.890970
122.114410	3464.147316	23.895987
121.770890	3465.735165	23.901005
122.150395	3459.969221	23.906023
122.063646	3469.136114	23.911040
121.923278	3471.137172	23.916058
122.045527	3470.095459	23.921075
122.254507	3481.201331	23.926093
122.451071	3482.499408	23.931111
122.280089	3489.703672	23.936128
122.546328	3488.721462	23.941146
122.816612	3485.421902	23.946163
122.868070	3489.962128	23.951181
122.981636	3503.506993	23.956199
122.815574	3508.355900	23.961216
123.059604	3513.516159	23.966234
123.331038	3500.220437	23.971251
123.049044	3513.255992	23.976269
123.177434	3518.538527	23.981287
123.542517	3529.004494	23.986304
123.394187	3537.732876	23.991322
123.689312	3547.837371	23.996339
123.769176	3558.862517	24.001357
123.775310	3555.257136	24.006375
124.159814	3563.021443	24.011392
124.074092	3588.736736	24.016410
124.450923	3580.414565	24.021427
124.034598	3580.056921	24.026445
124.312846	3584.571109	24.031463
124.746283	3602.674141	24.036480
125.131157	3610.772980	24.041498
125.233151	3606.407681	24.046515
125.273772	3619.578991	24.051533
125.204108	3613.817087	24.056551
125.768022	3613.681470	24.061568
125.793152	3626.400703	24.066586
126.108419	3629.801237	24.071603
126.229404	3631.079603	24.076621
126.239919	3632.826630	24.081639
126.291998	3630.138835	24.086656
125.947885	3632.042422	24.091674
126.503958	3626.636990	24.096691
126.657236	3629.191760	24.101709
126.481026	3646.844307	24.106727
126.937055	3644.793927	24.111744
126.426967	3659.165724	24.116762
127.165893	3650.092402	24.121779
127.299544	3651.059466	24.126797
127.288412	3646.487782	24.131815
127.494621	3652.455710	24.136832
127.258268	3670.000919	24.141850
127.251096	3667.133022	24.146867
127.852513	3672.193147	24.151885
127.857484	3688.236032	24.156903
128.329982	3691.533037	24.161920
128.027851	3696.712631	24.166938
128.313571	3693.994536	24.171955
128.343113	3702.594128	24.176973
128.200740	3706.457758	24.181991
128.652405	3708.653315	24.187008
128.539265	3723.979312	24.192026
128.584650	3717.145136	24.197043
128.853893	3736.902693	24.202061
129.134180	3737.139771	24.207079
129.392013	3734.596480	24.212096
129.370540	3750.280585	24.217114
129.539295	3758.025120	24.222131
129.701837	3774.134929	24.227149
129.956686	3769.007060	24.232167
130.155205	3767.694561	24.237184
129.972868	3761.454716	24.242202
130.417659	3760.084697	24.247219
130.843090	3769.424006	24.252237
130.852784	3770.031736	24.257255
130.669348	3772.405710	24.262272
131.030985	3769.691492	24.267290
131.300297	3771.353798	24.272307
131.496684	3775.805107	24.277325
131.200008	3776.909036	24.282343
131.505010	3770.917941	24.287360
131.495194	3772.911204	24.292378
131.702257	3770.337987	24.297395
131.987071	3782.912487	24.302413
131.831673	3795.499148	24.307431
132.163987	3791.343916	24.312448
132.196714	3796.783555	24.317466
132.109088	3790.159571	24.322483
132.424168	3794.169339	24.327501
132.292309	3794.963377	24.332519
132.697918	3809.952512	24.337536
132.671090	3818.595710	24.342554
132.902265	3820.194555	24.347571
133.268904	3815.396357	24.352589
132.963864	3812.906521	24.357607
133.178942	3814.836148	24.362624
133.412263	3836.736289	24.367642
133.461090	3836.065881	24.372659
133.370593	3838.175951	24.377677
133.465574	3840.361123	24.382695
133.815650	3842.601020	24.387712
133.881934	3858.340909	24.392730
134.034551	3855.599454	24.397747
133.961873	3862.277136	24.402765
133.835021	3867.811237	24.407783
134.152000	3881.927381	24.412800
134.434250	3887.021788	24.417818
134.383065	3892.199999	24.422835
134.806956	3900.999881	24.427853
134.932437	3910.405195	24.432871
135.162398	3907.806277	24.437888
134.982067	3910.375476	24.442906
135.491059	3921.769192	24.447923
135.738279	3936.407639	24.452941
135.768540	3934.161953	24.457959
135.896998	3931.840912	24.462976
135.560365	3935.217381	24.467994
135.928505	3946.674212	24.473011
136.090928	3948.703638	24.478029
136.344039	3964.177622	24.483047
136.605901	3972.845105	24.488064
136.440792	3984.316063	24.493082
136.612920	3976.988476	24.498099
137.181516	3983.168032	24.503117
137.012689	3988.816063	24.508135
137.539640	3989.109191	24.513152
137.365224	3993.318791	24.518170
137.584045	4004.451851	24.523187
137.874643	3996.067247	24.528205
137.993762	4021.621652	24.533223
138.110653	4018.699543	24.538240
138.532081	4025.170462	24.543258
138.366806	4018.580654	24.548275
138.418689	4027.198994	24.553293
138.668962	4025.900463	24.558311
139.077944	4028.610926	24.563328
138.764156	4039.963174	24.568346
139.391459	4038.877023	24.573363
139.283446	4038.161740	24.578381
139.458956	4043.964163	24.583399
139.861209	4023.138523	24.588416
139.809977	4051.074318	24.593434
139.723266	4036.625418	24.598451
139.775755	4033.126309	24.603469
140.281270	4055.776324	24.608487
140.358721	4052.607877	24.613504
139.996247	4052.475357	24.618522
140.209472	4053.209030	24.623539
140.081267	4042.620575	24.628557
140.293728	4073.109642	24.633575
140.530830	4069.288059	24.638592
140.589181	4085.714326	24.643610
140.940169	4100.484999	24.648627
141.409327	4103.255486	24.653645
140.829784	4103.766158	24.658663
141.283142	4113.757802	24.663680
141.348507	4123.213678	24.668698
141.686838	4132.292215	24.673715
141.842424	4124.481075	24.678733
141.676289	4135.431483	24.683751
142.238742	4134.251325	24.688768
142.283118	4146.121993	24.693786
142.393648	4139.031252	24.698803
142.563054	4143.145988	24.703821
142.520294	4145.157079	24.708839
142.797122	4170.529166	24.713856
143.006975	4176.727115	24.718874
143.082542	4170.913872	24.723891
143.231187	4176.774206	24.728909
142.841864	4174.082887	24.733927
143.080769	4192.324306	24.738944
143.652760	4200.520353	24.743962
143.545058	4198.110021	24.748979
144.246712	4210.887809	24.753997
144.402684	4217.921195	24.759015
144.802274	4219.765144	24.764032
144.373394	4221.757825	24.769050
144.673865	4213.964981	24.774067
144.772997	4210.853082	24.779085
144.825820	4215.027133	24.784103
144.892204	4226.297842	24.789120
145.215542	4236.717102	24.794138
145.060480	4243.480428	24.799155
145.241175	4237.211952	24.804173
145.717854	4253.831660	24.809191
145.690358	4257.393332	24.814208
145.661353	4274.663595	24.819226
145.710890	4273.008255	24.824243
146.452212	4272.977414	24.829261
146.321376	4292.236414	24.834279
146.429701	4298.756485	24.839296
146.629029	4291.582332	24.844314
146.977727	4294.273872	24.849331
147.020915	4297.830791	24.854349
147.204562	4308.331949	24.859367
147.375601	4307.263606	24.864384
147.403460	4312.180195	24.869402
147.258300	4316.028610	24.874419
147.434664	4312.011323	24.879437
147.358476	4331.899403	24.884455
147.728654	4336.118456	24.889472
148.102403	4344.105737	24.894490
148.139702	4359.654904	24.899507
148.401194	4358.613421	24.904525
148.579385	4357.146243	24.909543
148.705181	4357.170801	24.914560
148.937207	4370.792450	24.919578
149.100833	4384.554239	24.924595
149.456769	4378.340327	24.929613
149.439561	4382.923100	24.934631
149.472180	4377.463729	24.939648
149.700751	4369.126549	24.944666
149.942105	4391.256523	24.949683
150.035896	4390.490671	24.954701
150.195107	4402.176223	24.959719
150.280810	4393.419512	24.964736
150.623568	4395.174534	24.969754
150.455799	4403.174080	24.974771
150.714151	4408.206095	24.979789
150.611394	4415.144364	24.984807
150.454486	4411.902095	24.989824
150.936945	4431.961593	24.994842
151.225194	4447.777696	24.999859
151.364058	4451.183928	25.004877
151.680237	4439.799636	25.009895
151.651902	4450.810712	25.014912
151.965349	4457.080909	25.019930
151.858231	4470.389616	25.024947
152.192671	4465.899314	25.029965
152.209338	4476.518268	25.034983
152.181790	4470.556948	25.040000
152.172564	4476.713568	25.045018
152.475809	4492.912449	25.050035
152.333307	4485.876997	25.055053
152.772309	4498.541473	25.060071
152.328990	4509.273544	25.065088
153.312890	4511.553112	25.070106
153.380733	4527.397502	25.075123
153.547637	4539.530157	25.080141
153.983637	4541.308462	25.085159
153.954233	4543.762567	25.090176
154.020136	4538.465227	25.095194
154.527460	4556.077857	25.100211
154.421081	4553.575732	25.105229
154.678702	4559.438056	25.110247
154.397482	4564.633558	25.115264
154.716341	4566.505974	25.120282
154.987934	4574.367320	25.125299
155.400618	4566.749291	25.130317
155.549928	4577.072910	25.135335
155.424403	4575.006218	25.140352
155.677546	4588.116529	25.145370
156.259690	4598.325003	25.150387
156.277494	4591.485349	25.155405
156.186549	4600.031644	25.160423
156.211147	4603.130689	25.165440
156.819020	4596.318536	25.170458
156.755690	4602.461579	25.175475
156.689157	4604.959387	25.180493
156.849332	4613.873533	25.185511
156.968682	4623.166545	25.190528
157.020703	4613.979409	25.195546
157.298917	4629.566820	25.200563
157.440250	4635.529456	25.205581
157.469698	4647.750004	25.210599
157.784296	4646.605490	25.215616
158.246361	4662.148344	25.220634
157.916923	4672.228214	25.225651
158.019935	4657.307186	25.230669
158.605538	4669.595287	25.235687
159.011174	4680.579549	25.240704
159.102681	4677.973805	25.245722
159.290920	4689.367754	25.250739
159.478172	4689.474223	25.255757
159.568288	4681.524746	25.260775
159.092709	4686.592907	25.265792
159.528108	4696.227848	25.270810
159.611089	4704.901612	25.275827
159.941476	4706.406083	25.280845
159.809135	4716.038440	25.285863
160.027653	4722.269941	25.290880
160.262803	4725.181352	25.295898
160.211853	4737.575538	25.300915
160.442060	4743.956728	25.305933
160.676166	4753.875755	25.310951
160.692363	4758.592276	25.315968
161.319520	4769.491383	25.320986
161.093375	4783.008357	25.326003
161.277632	4781.407622	25.331021
161.449569	4792.258112	25.336039
161.646166	4805.762535	25.341056
162.131001	4801.876736	25.346074
161.894024	4815.452248	25.351091
162.121033	4817.326454	25.356109
162.393081	4830.929553	25.361127
162.663547	4831.657447	25.366144
162.820193	4842.507207	25.371162
162.866574	4846.101612	25.376179
162.867819	4853.131076	25.381197
163.192332	4850.141586	25.386215
163.079740	4864.117465	25.391232
163.640102	4870.453288	25.396250
163.512335	4872.859717	25.401267
163.896263	4874.879799	25.406285
164.081451	4883.187261	25.411303
164.040879	4898.777497	25.416320
164.301480	4890.365618	25.421338
164.278573	4904.633662	25.426355
164.662673	4908.667590	25.431373
164.843705	4920.583642	25.436391
164.870702	4924.875537	25.441408
165.223480	4921.398657	25.446426
165.448305	4944.759789	25.451443
165.587097	4949.185690	25.456461
165.971262	4940.473498	25.461479
165.746927	4949.930998	25.466496
166.021988	4943.830576	25.471514
166.229591	4955.865593	25.476531
166.361073	4968.281860	25.481549
166.533937	4968.305359	25.486567
166.507026	4976.036878	25.491584
167.246486	4985.453885	25.496602
166.968509	4996.103520	25.501619
166.737279	4996.461789	25.506637
167.303073	4996.019691	25.511655
167.625952	5010.214706	25.516672
168.061016	5011.791187	25.521690
167.858427	5012.829942	25.526707
167.993792	5022.401582	25.531725
168.289684	5030.470810	25.536743
168.239470	5043.527965	25.541760
168.619084	5046.710356	25.546778
168.564995	5060.030125	25.551795
168.602810	5065.788161	25.556813
168.919014	5060.397794	25.561831
169.121565	5084.895802	25.566848
169.077984	5087.039701	25.571866
169.651243	5089.219540	25.576883
169.197523	5102.709271	25.581901
169.916251	5112.543103	25.586919
169.995705	5113.948031	25.591936
170.273591	5128.945644	25.596954
170.557456	5138.191049	25.601971
170.489228	5150.698703	25.606989
170.995690	5140.606771	25.612007
170.936656	5161.891433	25.617024
171.219486	5169.356705	25.622042
171.334610	5176.639920	25.627059
171.474491	5178.467839	25.632077
172.089710	5174.173277	25.637095
172.041886	5192.927797	25.642112
172.330789	5194.454592	25.647130
172.302107	5193.534281	25.652147
172.043802	5188.568480	25.657165
172.728036	5186.561097	25.662183
172.648891	5197.801546	25.667200
173.080226	5208.996751	25.672218
173.367909	5207.405029	25.677236
173.211505	5207.609533	25.682253
173.270713	5205.873679	25.687271
173.288975	5221.436035	25.692288
173.689229	5219.078565	25.697306
173.624059	5222.046575	25.702324
173.980858	5233.875321	25.707341
174.152722	5233.558066	25.712359
174.428459	5244.310494	25.717376
174.617934	5243.210800	25.722394
174.551143	5254.553516	25.727412
174.948776	5267.922620	25.732429
174.827498	5267.389290	25.737447
175.185799	5273.223447	25.742464
175.288774	5285.770661	25.747482
175.317838	5283.793307	25.752500
175.186606	5291.187764	25.757517
175.552472	5297.936159	25.762535
176.029635	5312.675428	25.767552
176.028479	5316.378384	25.772570
176.263463	5322.869511	25.777588
176.191193	5334.689784	25.782605
176.487409	5335.290558	25.787623
176.923947	5361.125407	25.792640
177.283874	5375.908347	25.797658
177.302350	5364.304963	25.802676
177.612523	5377.851993	25.807693
177.586795	5383.427530	25.812711
177.933860	5392.495864	25.817728
177.888675	5387.360885	25.822746
177.952124	5391.265228	25.827764
178.303211	5413.893787	25.832781
178.607709	5411.627052	25.837799
178.275667	5424.495042	25.842816
178.540104	5433.260678	25.847834
179.012079	5448.764775	25.852852
179.311520	5461.533861	25.857869
179.437502	5466.788933	25.862887
179.323383	5473.533673	25.867904
179.340269	5485.646269	25.872922
180.058006	5492.620552	25.877940
180.101227	5495.912543	25.882957
180.529972	5507.831209	25.887975
180.611411	5515.113522	25.892992
180.520109	5526.277162	25.898010
180.959943	5527.357351	25.903028
181.012296	5533.346848	25.908045
181.445814	5536.366206	25.913063
181.653010	5554.809674	25.918080
181.963326	5560.812431	25.923098
181.961750	5572.842747	25.928116
181.765541	5575.209484	25.933133
182.103580	5571.542236	25.938151
182.304394	5585.425375	25.943168
182.740671	5579.937129	25.948186
183.030547	5588.960857	25.953204
183.247872	5590.145354	25.958221
183.626181	5588.296340	25.963239
183.630814	5605.663609	25.968256
183.756437	5612.497108	25.973274
184.324961	5610.119540	25.978292
184.243273	5603.762279	25.983309
184.384608	5597.568950	25.988327
184.341454	5595.429260	25.993344
184.700825	5617.128717	25.998362
185.015908	5609.755984	26.003380
185.011395	5626.591230	26.008397
185.219444	5619.165814	26.013415
185.212852	5614.062605	26.018432
185.319012	5622.818405	26.023450
185.683417	5638.945595	26.028468
186.102226	5643.596115	26.033485
185.623098	5644.293114	26.038503
186.058253	5664.591823	26.043520
185.948170	5668.605485	26.048538
186.364554	5668.480353	26.053556
186.274689	5681.042266	26.058573
186.632931	5689.392433	26.063591
186.797352	5702.059731	26.068608
186.835555	5704.481303	26.073626
187.106333	5711.285786	26.078644
186.935656	5723.112256	26.083661
187.773428	5732.435336	26.088679
187.706017	5747.575940	26.093696
187.649081	5752.462009	26.098714
188.012142	5759.308873	26.103732
188.280496	5770.321617	26.108749
188.763565	5766.038153	26.113767
188.270477	5782.662825	26.118784
188.956688	5792.647331	26.123802
189.107365	5799.221283	26.128820
188.865970	5802.744162	26.133837
189.229486	5815.102559	26.138855
189.774061	5823.218411	26.143872
189.701812	5832.633601	26.148890
190.085433	5851.630563	26.153908
190.222495	5855.703406	26.158925
190.676940	5865.253912	26.163943
190.274920	5882.842986	26.168960
190.450758	5885.943809	26.173978
191.198931	5897.159251	26.178996
191.120356	5895.479641	26.184013
191.424308	5899.482155	26.189031
191.657784	5919.509699	26.194048
191.725266	5925.623224	26.199066
191.928277	5930.642236	26.204084
192.416170	5947.533218	26.209101
192.762908	5951.746854	26.214119
192.795908	5953.882014	26.219136
192.813146	5966.149552	26.224154
192.931489	5962.955429	26.229172
193.228740	5969.667473	26.234189
193.347824	5974.832227	26.239207
193.572875	5998.024212	26.244224
193.552212	6000.953809	26.249242
193.682016	6003.932438	26.254260
194.018323	6015.108305	26.259277
194.099705	6017.810417	26.264295
194.752228	6035.101848	26.269312
194.857661	6048.103770	26.274330
194.972441	6046.690588	26.279348
195.455730	6065.318605	26.284365
195.814882	6068.460189	26.289383
195.769269	6071.447371	26.294400
196.013576	6066.614089	26.299418
196.105020	6062.672859	26.304436
195.944830	6082.604418	26.309453
196.097613	6077.062579	26.314471
196.710219	6087.993174	26.319488
196.773877	6108.176955	26.324506
197.349602	6099.816170	26.329524
197.344636	6095.953172	26.334541
197.614845	6113.550797	26.339559
197.465109	6133.108277	26.344576
197.618437	6136.749317	26.349594
197.987649	6134.753308	26.354612
198.205370	6150.367283	26.359629
198.728902	6156.769310	26.364647
198.831714	6150.629181	26.369664
198.980263	6160.833861	26.374682
199.016234	6167.511148	26.379700
199.362256	6174.465011	26.384717
199.369234	6174.094653	26.389735
199.889621	6166.683221	26.394752
199.539593	6177.584741	26.399770
199.875673	6191.374546	26.404788
200.036310	6196.444464	26.409805
200.177511	6203.376760	26.414823
200.269788	6211.891948	26.419840
199.917223	6226.155846	26.424858
200.593035	6225.788037	26.429876
200.390210	6251.616981	26.434893
200.725994	6261.082112	26.439911
201.139949	6271.226334	26.444928
201.420648	6288.607824	26.449946
201.779315	6293.810899	26.454964
202.133544	6303.828755	26.459981
202.372547	6310.903609	26.464999
202.454032	6311.695898	26.470016
202.358437	6332.924515	26.475034
202.628760	6327.847175	26.480052
202.809885	6352.700644	26.485069
203.081327	6361.430906	26.490087
203.666102	6361.749753	26.495104
203.548681	6381.703347	26.500122
203.825845	6374.285740	26.505140
203.935731	6385.023786	26.510157
203.804465	6398.009373	26.515175
204.528965	6401.696729	26.520192
204.543608	6414.236458	26.525210
204.780815	6424.054894	26.530228
204.761006	6439.608467	26.535245
205.214600	6449.219393	26.540263
205.733768	6453.475583	26.545280
205.673595	6467.179303	26.550298
206.141595	6474.297266	26.555316
206.328642	6476.831367	26.560333
206.460644	6482.275197	26.565351
206.927606	6496.821303	26.570368
207.060486	6508.427099	26.575386
207.280302	6505.968306	26.580404
207.257028	6504.917653	26.585421
207.449892	6522.133187	26.590439
207.753568	6523.316846	26.595456
207.546042	6532.646256	26.600474
207.990821	6537.223488	26.605492
208.501939	6553.530539	26.610509
208.396529	6555.873705	26.615527
208.831189	6561.011286	26.620544
208.964580	6577.589040	26.625562
209.285171	6576.607629	26.630580
209.457262	6579.109362	26.635597
209.421503	6599.820665	26.640615
209.893284	6595.971265	26.645632
209.834185	6610.091625	26.650650
210.167928	6623.244442	26.655668
210.625613	6627.908066	26.660685
210.191907	6634.763278	26.665703
210.451179	6645.607504	26.670720
210.361116	6659.827458	26.675738
210.689561	6668.387937	26.680756
211.328252	6676.874563	26.685773
211.475740	6701.203426	26.690791
211.678736	6696.452217	26.695808
211.749911	6725.790353	26.700826
212.162250	6731.727005	26.705844
212.536811	6731.497932	26.710861
212.795911	6752.747233	26.715879
213.215848	6756.757022	26.720896
213.297773	6756.251793	26.725914
213.654389	6760.041052	26.730932
213.944634	6760.292403	26.735949
213.767670	6776.518036	26.740967
214.006483	6762.609468	26.745984
214.139275	6774.401701	26.751002
214.078305	6780.279928	26.756020
214.544921	6780.364748	26.761037
214.033551	6798.978865	26.766055
214.870265	6806.376981	26.771072
214.942683	6817.613621	26.776090
215.370965	6820.346742	26.781108
215.759660	6837.004697	26.786125
215.689487	6857.222896	26.791143
216.034058	6853.447039	26.796160
216.282031	6868.719103	26.801178
216.506049	6867.077236	26.806196
216.621990	6869.786688	26.811213
216.412992	6896.589822	26.816231
217.008735	6886.820737	26.821248
217.242999	6906.192607	26.826266
217.287273	6915.312292	26.831284
217.596556	6919.004822	26.836301
217.547915	6942.370312	26.841319
218.288592	6947.185413	26.846336
218.176782	6960.392487	26.851354
218.427319	6965.192827	26.856372
218.940123	6979.255446	26.861389
218.981784	6992.959389	26.866407
219.004743	6997.855371	26.871424
219.474125	7010.617860	26.876442
219.580405	7014.253819	26.881460
220.063355	7024.700186	26.886477
219.739663	7038.698166	26.891495
220.512095	7048.695113	26.896512
220.542951	7072.884894	26.901530
220.533829	7076.261135	26.906548
220.784753	7079.868133	26.911565
221.393189	7098.013532	26.916583
221.668378	7101.657773	26.921600
221.524833	7116.498899	26.926618
221.886833	7130.089622	26.931636
222.319670	7137.222825	26.936653
222.356527	7149.626986	26.941671
222.730287	7163.234833	26.946688
222.976105	7163.793058	26.951706
223.139230	7166.280491	26.956724
223.516512	7165.785807	26.961741
223.536285	7184.329732	26.966759
223.956360	7187.897625	26.971776
224.313196	7187.008370	26.976794
224.339794	7203.240373	26.981812
224.587226	7212.985021	26.986829
224.529449	7217.606429	26.991847
224.739887	7230.949474	26.996864
224.992752	7244.803620	27.001882
225.070521	7250.480317	27.006900
225.763110	7256.319570	27.011917
225.727147	7263.955608	27.016935
226.232245	7276.138124	27.021952
226.412727	7285.422914	27.026970
226.427739	7292.949956	27.031988
226.816596	7303.553286	27.037005
227.166615	7318.661361	27.042023
226.979132	7315.464403	27.047040
227.253441	7339.070243	27.052058
227.409455	7344.447429	27.057076
227.824346	7356.473655	27.062093
228.041274	7376.742157	27.067111
228.099061	7373.175284	27.072128
228.532747	7389.766711	27.077146
228.597686	7404.202886	27.082164
229.089954	7396.274470	27.087181
229.249420	7398.601504	27.092199
229.118627	7416.171648	27.097216
229.222456	7412.095597	27.102234
229.669374	7445.233834	27.107252
230.123610	7449.828758	27.112269
230.328273	7458.472138	27.117287
230.560685	7471.098439	27.122304
230.789016	7467.924709	27.127322
230.872791	7478.926358	27.132340
231.135483	7483.627065	27.137357
231.381356	7493.511013	27.142375
231.827917	7505.121968	27.147392
232.063531	7511.133915	27.152410
231.782531	7536.844315	27.157428
231.943003	7531.600749	27.162445
232.369646	7546.889585	27.167463
232.604950	7557.375052	27.172480
233.021284	7574.455541	27.177498
233.325865	7575.834865	27.182516
233.723868	7572.880783	27.187533
233.800898	7589.458809	27.192551
233.676845	7603.384900	27.197568
234.221397	7610.305053	27.202586
234.131726	7623.079782	27.207604
234.814941	7639.815451	27.212621
235.087052	7636.603264	27.217639
235.410650	7655.586246	27.222656
235.628549	7659.593159	27.227674
235.687855	7665.831668	27.232692
236.166969	7664.563337	27.237709
236.391510	7685.029878	27.242727
236.302396	7679.143455	27.247744
236.694307	7684.319621	27.252762
236.674416	7707.735246	27.257780
237.152504	7714.728992	27.262797
237.301655	7728.498725	27.267815
237.496054	7737.358523	27.272832
237.910486	7739.651972	27.277850
237.707044	7761.931478	27.282868
238.209444	7763.099876	27.287885
238.382837	7779.953424	27.292903
238.574384	7794.092252	27.297920
239.510283	7804.468108	27.302938
239.120919	7816.014476	27.307956
239.297324	7828.343564	27.312973
239.816328	7845.525031	27.317991
239.643389	7849.801578	27.323008
239.906509	7856.668045	27.328026
239.976960	7873.143174	27.333044
240.716519	7888.070727	27.338061
240.754698	7887.995366	27.343079
241.128584	7912.978601	27.348096
241.452417	7917.818223	27.353114
241.438260	7929.552134	27.358132
241.858717	7941.208496	27.363149
242.234611	7952.123624	27.368167
242.425100	7965.606081	27.373184
243.052519	7972.671244	27.378202
242.869305	7984.441144	27.383220
243.635852	7992.276943	27.388237
243.491706	7998.446410	27.393255
243.913795	7997.003882	27.398272
244.192756	8008.575113	27.403290
244.408091	8023.294448	27.408308
244.641339	8021.445825	27.413325
244.670898	8029.198197	27.418343
244.488389	8049.182735	27.423360
245.080122	8048.250330	27.428378
244.920248	8059.770370	27.433396
245.414219	8066.278730	27.438413
245.627540	8066.842076	27.443431
246.005985	8093.425481	27.448448
245.932750	8106.270581	27.453466
246.213048	8123.518117	27.458484
246.382870	8126.130916	27.463501
246.733472	8141.002795	27.468519
246.718921	8154.378598	27.473536
247.176237	8159.743551	27.478554
247.574368	8183.981438	27.483572
247.422180	8189.539751	27.488589
247.870503	8210.966305	27.493607
248.122490	8221.291682	27.498624
248.720759	8233.416041	27.503642
248.620558	8234.284233	27.508660
249.081640	8252.453858	27.513677
249.591928	8256.307756	27.518695
249.720514	8286.406562	27.523712
250.100338	8284.358152	27.528730
250.040009	8292.999238	27.533748
250.418663	8302.278754	27.538765
250.496074	8322.601723	27.543783
250.839069	8331.305930	27.548800
251.406919	8337.948040	27.553818
251.261864	8360.904217	27.558836
251.597010	8364.337262	27.563853
252.290203	8380.074390	27.568871
251.949470	8389.100418	27.573888
252.402663	8390.967980	27.578906
252.821552	8405.810432	27.583924
253.014009	8409.812023	27.588941
253.136109	8420.148388	27.593959
253.472877	8431.470886	27.598976
253.990031	8437.881032	27.603994
253.923445	8453.468889	27.609012
254.372061	8465.354802	27.614029
254.958295	8476.338319	27.619047
255.165619	8484.208263	27.624064
255.063448	8474.885494	27.629082
255.019101	8493.500764	27.634100
255.593036	8511.324623	27.639117
256.349683	8520.873380	27.644135
256.334548	8529.210723	27.649152
256.894547	8525.056653	27.654170
256.627400	8535.615074	27.659188
256.984583	8544.209815	27.664205
257.414261	8549.263496	27.669223
257.488192	8568.207600	27.674240
257.636909	8574.318752	27.679258
257.460148	8582.570938	27.684276
257.886371	8599.887617	27.689293
258.490511	8617.877334	27.694311
258.416895	8638.322181	27.699328
258.974375	8635.150364	27.704346
258.797314	8649.350748	27.709364
259.384184	8667.860997	27.714381
259.730635	8676.318565	27.719399
259.742709	8691.439665	27.724416
260.277774	8700.151843	27.729434
260.368315	8716.479346	27.734452
260.619584	8732.339678	27.739469
260.878860	8739.889031	27.744487
261.044447	8752.283574	27.749504
261.349828	8765.420268	27.754522
261.442894	8774.558486	27.759540
261.864665	8791.380362	27.764557
262.314726	8794.422937	27.769575
262.472271	8814.557089	27.774592
262.834177	8809.019560	27.779610
262.976291	8824.707638	27.784628
263.123564	8833.502729	27.789645
263.547445	8839.690837	27.794663
263.295392	8856.851963	27.799680
263.648963	8867.559598	27.804698
264.233100	8877.015591	27.809716
264.211044	8898.980741	27.814733
264.662150	8903.797529	27.819751
264.828168	8932.454985	27.824768
264.826448	8926.800737	27.829786
265.373048	8946.068993	27.834804
265.876818	8967.326721	27.839821
265.941493	8973.760579	27.844839
265.948127	8994.414253	27.849856
266.491659	9004.631252	27.854874
267.052212	9018.043876	27.859892
267.054747	9031.701788	27.864909
267.602897	9039.963749	27.869927
267.804332	9051.080507	27.874944
267.859405	9053.392532	27.879962
268.130759	9072.760869	27.884980
268.322112	9088.419355	27.889997
268.808032	9097.028917	27.895015
268.633347	9116.302995	27.900032
269.409869	9121.728731	27.905050
269.476494	9139.888406	27.910068
269.613982	9155.208088	27.915085
270.193385	9172.671801	27.920103
270.104045	9184.323565	27.925120
270.726484	9202.389917	27.930138
271.022452	9210.628315	27.935156
271.257485	9222.396625	27.940173
271.521783	9231.059911	27.945191
271.693265	9253.724494	27.950208
272.086110	9261.246822	27.955226
272.354615	9272.842585	27.960244
272.168807	9293.169964	27.965261
273.012277	9300.195483	27.970279
273.034940	9322.605621	27.975296
273.458528	9325.144108	27.980314
273.890486	9344.759097	27.985332
274.143602	9357.604456	27.990349
274.677178	9359.958381	27.995367
274.784416	9381.641792	28.000384
274.773477	9383.512705	28.005402
275.478923	9403.163846	28.010420
275.623444	9415.770515	28.015437
275.829612	9424.285132	28.020455
276.232369	9426.766908	28.025472
276.402793	9435.078747	28.030490
276.990180	9452.238371	28.035508
277.288898	9461.846725	28.040525
277.389258	9464.116977	28.045543
277.515784	9480.186929	28.050560
277.988800	9496.246819	28.055578
278.185619	9490.722322	28.060596
278.227022	9507.111892	28.065613
279.192873	9509.123433	28.070631
278.968796	9518.873703	28.075648
279.286347	9531.699617	28.080666
279.868201	9527.412454	28.085684
279.757279	9555.255461	28.090701
280.056602	9560.879218	28.095719
280.355770	9571.308465	28.100736
280.628146	9581.820849	28.105754
280.609432	9591.106430	28.110772
280.730271	9592.659931	28.115789
281.201029	9611.325080	28.120807
281.659938	9616.879653	28.125824
281.950688	9630.025567	28.130842
282.006349	9636.950456	28.135860
282.400720	9647.667938	28.140877
282.595935	9659.272266	28.145895
282.760864	9671.092889	28.150912
282.580456	9688.521403	28.155930
283.288074	9700.676960	28.160948
283.442302	9714.854676	28.165965
283.879953	9726.768378	28.170983
283.773571	9747.879466	28.176000
284.280562	9770.713137	28.181018
284.436916	9774.648061	28.186036
284.738405	9793.292549	28.191053
285.025789	9806.972712	28.196071
285.316197	9827.876494	28.201088
285.723484	9837.389101	28.206106
286.148921	9857.261402	28.211124
286.397955	9877.233977	28.216141
286.727510	9891.330687	28.221159
287.069362	9912.510670	28.226176
287.197143	9917.735160	28.231194
287.598134	9933.857230	28.236212
287.813239	9946.996275	28.241229
288.190037	9960.997229	28.246247
288.401922	9981.648262	28.251264
288.584051	9992.683358	28.256282
289.088325	10017.124878	28.261300
289.459283	10032.964415	28.266317
289.345941	10047.872615	28.271335
290.000327	10057.176126	28.276352
290.276019	10076.709016	28.281370
290.854709	10082.668060	28.286388
290.887365	10096.227311	28.291405
291.228612	10109.428803	28.296423
291.502150	10121.501079	28.301440
291.870371	10135.118302	28.306458
292.356889	10139.014213	28.311476
292.459515	10156.888229	28.316493
292.973054	10161.752403	28.321511
293.277185	10190.977444	28.326528
293.302454	10199.618636	28.331546
293.614282	10210.882982	28.336564
293.734149	10230.020502	28.341581
294.178301	10241.819849	28.346599
294.520553	10244.677479	28.351616
294.672292	10260.213703	28.356634
295.458716	10271.091153	28.361652
295.290612	10293.851245	28.366669
295.989443	10291.998932	28.371687
296.178204	10308.833427	28.376704
296.283666	10330.458228	28.381722
296.644057	10339.208018	28.386740
296.644274	10356.005784	28.391757
297.072972	10368.334930	28.396775
297.698541	10382.032004	28.401792
297.799169	10393.421112	28.406810
298.464918	10403.600796	28.411828
298.557828	10420.365155	28.416845
298.904458	10433.746011	28.421863
299.064693	10440.430635	28.426880
299.212369	10456.823337	28.431898
299.655587	10458.316938	28.436916
299.818060	10481.931673	28.441933
300.018202	10482.860273	28.446951
300.160587	10508.337949	28.451968
300.117894	10520.418974	28.456986
300.672266	10533.337939	28.462004
300.848741	10553.991996	28.467021
301.172863	10567.449096	28.472039
301.573083	10579.820732	28.477056
301.939017	10595.699425	28.482074
302.191508	10612.224247	28.487092
302.156503	10626.050240	28.492109
303.008160	10644.151557	28.497127
303.434914	10662.325767	28.502144
303.339180	10676.890697	28.507162
303.655954	10690.923706	28.512180
303.786109	10712.829259	28.517197
304.565113	10738.194893	28.522215
305.137954	10746.093793	28.527232
304.729606	10769.444665	28.532250
305.761196	10767.388621	28.537268
305.670123	10789.540474	28.542285
306.200547	10803.511682	28.547303
306.308567	10817.463816	28.552320
306.288122	10833.848451	28.557338
307.089137	10843.678803	28.562356
307.546454	10864.102914	28.567373
307.658024	10869.885940	28.572391
308.376585	10892.451029	28.577408
308.334416	10900.269512	28.582426
308.744371	10904.117586	28.587444
308.756480	10930.522465	28.592461
309.261072	10941.166592	28.597479
309.584593	10957.137491	28.602496
309.795662	10978.187608	28.607514
309.813871	10983.189585	28.612532
310.373505	11006.404907	28.617549
310.623390	11028.380486	28.622567
311.196235	11025.392167	28.627584
311.243330	11059.098390	28.632602
311.932181	11062.126043	28.637620
311.910480	11082.732787	28.642637
312.157203	11098.621109	28.647655
312.714183	11114.100878	28.652672
312.869670	11137.155482	28.657690
313.287899	11144.810376	28.662708
313.482730	11161.527857	28.667725
314.077185	11168.207875	28.672743
314.380863	11193.487549	28.677760
314.388175	11207.654679	28.682778
314.657236	11212.052209	28.687796
315.193904	11233.923111	28.692813
315.484340	11249.299495	28.697831
315.826145	11266.183503	28.702848
315.951122	11281.124819	28.707866
316.598868	11296.827343	28.712884
316.466924	11314.019270	28.717901
316.792876	11329.004925	28.722919
317.071204	11345.700018	28.727936
317.677993	11374.184819	28.732954
318.444082	11384.396690	28.737972
318.293547	11401.307421	28.742989
318.398729	11418.594919	28.748007
319.239916	11437.447011	28.753024
318.946765	11447.613280	28.758042
319.569128	11458.447660	28.763060
320.014704	11476.727074	28.768077
320.410615	11486.453871	28.773095
320.746190	11496.550098	28.778112
320.744000	11516.879546	28.783130
321.071810	11538.654056	28.788148
321.276205	11551.458037	28.793165
321.720482	11567.420013	28.798183
322.073660	11576.136781	28.803200
322.099255	11599.120726	28.808218
322.538804	11608.060804	28.813236
322.987611	11626.955607	28.818253
323.318817	11634.883265	28.823271
323.673515	11654.266489	28.828288
323.810536	11664.823355	28.833306
324.314382	11678.752017	28.838324
325.150082	11698.571486	28.843341
324.836730	11709.091564	28.848359
325.341599	11732.325839	28.853376
325.577879	11739.807387	28.858394
325.968163	11752.677118	28.863412
326.433639	11763.937279	28.868429
326.519103	11772.506612	28.873447
326.739324	11801.406280	28.878464
327.207638	11818.984613	28.883482
327.758169	11837.390035	28.888500
327.763038	11845.956238	28.893517
327.915198	11872.053148	28.898535
328.344823	11882.456939	28.903552
328.373828	11909.113163	28.908570
329.011122	11918.404500	28.913588
329.900277	11945.668105	28.918605
329.704846	11958.377107	28.923623
330.258554	11972.156079	28.928640
330.469107	11997.710358	28.933658
330.859200	12004.987927	28.938676
331.362890	12027.401738	28.943693
331.580218	12048.613121	28.948711
332.282692	12056.438592	28.953728
332.647166	12072.574546	28.958746
332.885964	12067.547959	28.963764
333.540075	12091.188756	28.968781
333.657946	12115.440927	28.973799
334.163638	12119.308995	28.978816
334.446997	12139.907003	28.983834
334.850857	12143.642612	28.988852
334.716223	12151.419260	28.993869
334.902296	12171.783079	28.998887
335.796381	12178.324951	29.003904
335.629370	12201.829258	29.008922
335.712360	12211.071785	29.013940
336.416519	12229.046174	29.018957
336.519507	12250.528317	29.023975
336.751799	12272.223907	29.028992
336.840095	12290.124305	29.034010
337.340742	12310.306371	29.039028
337.764183	12324.987033	29.044045
338.311074	12346.668164	29.049063
338.567039	12365.549709	29.054080
338.901912	12386.964106	29.059098
339.172985	12415.237820	29.064116
339.770151	12428.858745	29.069133
339.844614	12449.594023	29.074151
340.212058	12471.593927	29.079168
340.402359	12490.147995	29.084186
340.859778	12506.250815	29.089204
341.416677	12525.060117	29.094221
341.383975	12544.972303	29.099239
342.102764	12559.632147	29.104256
342.559658	12575.507744	29.109274
342.732103	12598.094121	29.114292
343.411642	12606.059204	29.119309
343.621057	12627.496685	29.124327
344.151871	12626.560992	29.129344
344.352271	12645.906252	29.134362
345.120941	12660.163630	29.139380
344.540724	12659.496707	29.144397
344.897314	12679.888049	29.149415
345.372829	12687.221976	29.154432
345.950200	12703.220912	29.159450
346.015258	12726.073735	29.164468
346.533961	12735.882999	29.169485
346.959938	12754.097254	29.174503
347.449303	12754.080674	29.179520
347.436158	12781.120519	29.184538
347.980948	12786.078384	29.189556
348.223811	12809.140296	29.194573
348.618870	12824.757370	29.199591
349.170828	12836.153051	29.204608
349.046962	12853.629323	29.209626
349.820361	12874.738741	29.214644
349.883219	12888.077381	29.219661
350.023593	12906.952311	29.224679
350.541832	12930.558604	29.229696
350.747865	12948.930659	29.234714
351.174939	12963.683883	29.239732
351.919788	12978.109446	29.244749
352.084775	13007.066982	29.249767
352.547178	13010.045170	29.254784
352.897650	13030.927326	29.259802
353.042267	13051.598590	29.264820
353.568246	13061.454254	29.269837
353.770235	13087.491355	29.274855
353.980792	13109.668159	29.279872
354.210138	13133.446277	29.284890
354.590991	13156.089097	29.289908
355.240798	13173.930797	29.294925
355.364740	13202.557162	29.299943
356.104436	13214.046824	29.304960
356.552599	13232.892814	29.309978
356.502845	13245.371435	29.314996
357.256868	13265.470624	29.320013
357.244158	13290.998467	29.325031
357.656440	13308.602759	29.330048
358.123048	13328.462819	29.335066
358.657222	13342.511127	29.340084
359.044428	13362.528928	29.345101
359.335184	13393.460035	29.350119
359.948933	13395.454553	29.355136
359.872427	13414.117638	29.360154
360.372683	13436.918939	29.365172
361.316897	13442.787073	29.370189
361.470291	13460.905757	29.375207
361.718218	13483.509790	29.380224
362.206155	13488.994660	29.385242
362.229446	13508.036955	29.390260
362.822312	13512.633788	29.395277
363.027929	13526.297895	29.400295
363.029811	13546.193084	29.405312
363.392321	13560.167387	29.410330
363.856028	13586.928417	29.415348
364.627758	13609.355810	29.420365
364.897993	13624.822566	29.425383
365.043985	13635.698089	29.430400
365.558326	13654.764669	29.435418
365.959475	13676.043826	29.440436
366.375436	13690.398290	29.445453
366.799252	13702.531441	29.450471
367.316435	13712.925689	29.455488
367.824045	13727.910064	29.460506
367.970633	13747.448045	29.465524
368.581996	13749.130331	29.470541
368.645246	13761.698963	29.475559
369.093185	13773.130454	29.480576
369.607139	13780.575636	29.485594
369.836501	13792.584559	29.490612
370.151921	13795.848016	29.495629
370.130822	13813.103801	29.500647
370.666170	13825.513258	29.505664
371.146798	13839.450318	29.510682
371.390282	13857.479477	29.515700
371.674423	13859.285665	29.520717
371.804291	13883.790868	29.525735
372.405683	13904.584156	29.530752
372.725575	13927.818532	29.535770
373.029192	13936.711537	29.540788
373.514274	13952.887053	29.545805
373.511706	13983.612424	29.550823
373.940020	14000.485333	29.555840
374.542931	14013.544370	29.560858
374.445278	14041.088750	29.565876
375.533829	14055.192865	29.570893
375.444997	14078.156691	29.575911
375.876628	14100.609518	29.580928
376.419608	14115.774988	29.585946
376.329525	14147.019626	29.590964
376.744821	14173.454308	29.595981
377.193418	14193.886557	29.600999
376.971387	14215.162875	29.606016
378.186500	14248.754990	29.611034
378.670740	14269.639665	29.616052
379.287427	14287.080208	29.621069
379.582291	14323.778927	29.626087
379.879884	14338.105052	29.631104
380.559854	14350.826963	29.636122
380.715032	14369.691555	29.641140
380.930579	14386.661299	29.646157
381.245578	14417.141820	29.651175
381.584503	14435.958747	29.656192
382.222691	14452.600220	29.661210
382.763997	14476.931205	29.666228
383.036594	14496.507064	29.671245
383.366274	14520.757560	29.676263
383.697050	14545.175298	29.681280
384.074719	14555.891890	29.686298
384.190425	14581.972980	29.691316
384.911237	14600.193361	29.696333
385.288743	14627.086212	29.701351
385.533694	14650.355317	29.706368
386.153259	14662.512111	29.711386
386.186431	14685.356494	29.716404
386.790014	14710.211757	29.721421
387.134356	14733.418022	29.726439
387.476111	14756.447861	29.731456
387.856930	14779.079992	29.736474
388.180315	14804.162443	29.741492
389.164730	14828.193920	29.746509
388.933813	14843.016936	29.751527
389.589387	14862.839530	29.756544
389.897970	14880.272032	29.761562
390.354267	14906.995025	29.766580
390.872788	14924.906316	29.771597
391.505088	14941.823907	29.776615
391.893808	14969.656639	29.781632
392.259838	14976.275898	29.786650
392.381876	15000.411092	29.791668
392.872544	15009.799569	29.796685
393.097767	15033.997598	29.801703
393.186391	15056.224197	29.806720
393.836926	15073.518040	29.811738
394.189685	15097.263491	29.816756
394.583098	15108.012670	29.821773
394.874087	15122.959439	29.826791
395.255831	15144.416985	29.831808
396.118091	15160.354428	29.836826
395.701289	15176.463811	29.841844
396.365128	15201.430290	29.846861
397.026889	15229.059560	29.851879
397.101431	15244.975180	29.856896
397.779449	15256.156764	29.861914
398.083116	15286.018266	29.866932
398.398596	15302.960538	29.871949
398.628696	15325.556918	29.876967
398.868037	15344.876719	29.881984
399.511678	15361.009648	29.887002
400.143493	15389.446050	29.892020
400.298294	15414.239878	29.897037
401.053972	15431.593377	29.902055
401.259766	15457.623650	29.907072
402.106647	15467.967221	29.912090
402.539688	15490.509899	29.917108
402.686046	15504.781632	29.922125
403.056717	15525.072759	29.927143
403.637107	15547.595583	29.932160
403.829221	15553.020010	29.937178
404.041843	15580.818049	29.942196
404.586937	15607.123846	29.947213
405.038664	15633.207428	29.952231
405.194471	15651.927904	29.957248
406.295067	15672.278563	29.962266
406.287721	15705.925770	29.967284
406.783467	15718.077368	29.972301
407.153292	15736.865472	29.977319
407.533536	15758.159706	29.982336
408.167737	15775.241977	29.987354
408.773617	15793.074075	29.992372
408.844118	15812.155490	29.997389
409.409252	15834.172543	30.002407
409.408541	15854.335846	30.007424
410.048132	15883.779290	30.012442
410.261973	15907.654893	30.017460
410.561781	15927.929121	30.022477
410.942275	15950.448988	30.027495
411.256148	15985.856135	30.032512
411.544822	15996.919111	30.037530
412.159818	16028.451179	30.042548
412.490875	16067.829070	30.047565
413.269246	16074.159877	30.052583
413.678048	16104.325187	30.057600
413.958989	16131.503746	30.062618
414.579693	16149.494935	30.067636
414.574140	16182.125679	30.072653
415.322919	16197.330060	30.077671
415.803590	16219.761908	30.082688
416.107307	16238.447155	30.087706
416.753714	16261.371077	30.092724
416.919901	16284.837697	30.097741
417.562321	16301.821239	30.102759
417.697837	16326.237093	30.107776
418.473137	16348.818768	30.112794
418.842299	16368.763593	30.117812
419.336963	16385.716659	30.122829
419.931067	16414.109955	30.127847
419.894307	16439.547858	30.132864
420.630862	16444.760920	30.137882
421.217845	16470.053786	30.142900
421.058221	16492.137740	30.147917
421.860815	16509.206925	30.152935
422.266925	16529.588319	30.157952
422.840577	16542.145160	30.162970
423.116744	16566.905675	30.167988
423.287519	16571.572535	30.173005
423.827454	16589.030367	30.178023
424.106090	16610.998434	30.183040
424.452424	16628.218153	30.188058
425.072336	16644.434848	30.193076
425.394149	16677.075166	30.198093
426.124075	16679.096069	30.203111
426.358242	16696.412382	30.208128
426.741268	16718.218928	30.213146
427.364628	16729.267807	30.218164
427.649712	16744.561047	30.223181
428.447379	16763.185227	30.228199
428.336606	16787.150671	30.233216
428.877649	16804.349526	30.238234
428.747836	16828.911809	30.243252
429.621714	16856.402813	30.248269
430.245903	16870.310130	30.253287
430.525298	16897.205745	30.258304
430.689237	16915.341845	30.263322
431.652150	16946.407155	30.268340
431.560914	16962.138540	30.273357
432.157412	16998.027604	30.278375
432.778435	17018.284255	30.283392
433.131416	17034.881059	30.288410
433.707740	17054.797306	30.293428
433.774021	17086.410742	30.298445
434.590047	17102.638169	30.303463
434.925558	17123.122850	30.308480
435.276966	17149.726422	30.313498
436.020592	17189.534726	30.318516
436.179040	17200.457706	30.323533
436.496110	17221.204386	30.328551
436.927401	17241.194081	30.333568
437.020016	17269.190240	30.338586
437.763222	17301.500287	30.343604
438.037750	17330.870469	30.348621
438.565489	17357.168749	30.353639
438.940887	17383.143477	30.358656
439.756702	17401.980223	30.363674
440.356535	17434.679352	30.368692
440.856685	17456.623162	30.373709
441.334125	17480.509965	30.378727
441.458799	17501.583995	30.383744
442.014738	17526.336665	30.388762
442.703877	17529.305333	30.393780
442.847781	17571.040382	30.398797
443.419876	17582.126211	30.403815
443.655905	17605.829876	30.408832
444.419289	17640.032533	30.413850
444.935214	17652.940282	30.418868
445.064100	17682.731805	30.423885
445.984858	17693.939973	30.428903
446.217700	17724.239618	30.433920
446.261436	17735.193503	30.438938
446.694155	17765.651428	30.443956
447.203866	17786.501206	30.448973
448.028934	17817.106232	30.453991
448.396410	17841.825652	30.459008
448.702560	17866.889533	30.464026
448.964608	17888.049862	30.469044
449.204568	17919.542693	30.474061
450.005873	17935.570972	30.479079
450.078157	17972.542113	30.484096
450.489719	17997.779176	30.489114
451.125939	18011.540134	30.494132
451.823561	18034.666626	30.499149
452.032717	18060.087093	30.504167
452.073005	18084.794897	30.509184
452.819542	18106.707171	30.514202
453.461712	18126.791103	30.519220
453.902402	18148.624980	30.524237
454.606693	18169.785841	30.529255
454.533378	18195.282317	30.534272
455.138566	18216.509291	30.539290
455.918357	18239.629476	30.544308
455.674909	18271.647141	30.549325
456.380783	18295.012719	30.554343
456.761775	18307.942041	30.559360
457.281012	18347.497269	30.564378
457.848350	18373.108430	30.569396
458.672571	18399.930274	30.574413
458.768134	18418.842923	30.579431
459.484651	18447.722290	30.584448
459.868499	18462.236990	30.589466
460.503761	18482.903596	30.594484
460.625838	18511.983566	30.599501
461.073026	18540.993705	30.604519
461.638479	18573.826498	30.609536
462.046725	18595.893396	30.614554
462.757297	18623.832624	30.619572
463.260767	18651.254694	30.624589
463.451294	18669.400908	30.629607
463.962956	18692.222476	30.634624
464.130786	18734.341658	30.639642
464.803748	18755.684962	30.644660
465.635366	18791.767965	30.649677
465.925640	18807.510583	30.654695
466.507537	18833.833976	30.659712
466.975628	18866.695150	30.664730
467.779450	18886.836683	30.669748
468.206416	18916.905615	30.674765
468.264844	18933.834484	30.679783
468.735222	18964.913853	30.684800
468.950149	18988.256080	30.689818
469.754871	19008.972518	30.694836
469.656660	19050.401188	30.699853
470.290113	19075.181605	30.704871
471.190822	19093.526552	30.709888
471.425717	19131.137796	30.714906
472.217723	19152.456574	30.719924
472.369990	19175.802522	30.724941
473.049195	19218.354399	30.729959
473.641516	19239.085398	30.734976
474.088764	19271.678851	30.739994
474.431898	19296.555565	30.745012
475.010211	19322.817003	30.750029
475.216199	19347.127698	30.755047
476.037875	19365.908582	30.760064
476.523544	19397.725443	30.765082
476.624632	19422.318015	30.770100
477.222262	19448.734545	30.775117
478.096430	19476.952638	30.780135
478.220511	19505.477796	30.785152
478.685212	19524.396880	30.790170
479.707616	19548.162966	30.795188
480.006282	19578.872177	30.800205
480.422010	19600.408332	30.805223
481.094456	19627.400960	30.810240
481.288709	19659.769331	30.815258
481.887074	19677.890513	30.820276
482.467278	19709.200270	30.825293
482.758768	19720.419731	30.830311
483.454464	19742.063825	30.835328
483.368513	19769.459747	30.840346
483.873321	19783.602677	30.845364
484.534368	19804.494101	30.850381
485.557801	19831.836393	30.855399
485.696495	19850.857401	30.860416
485.576804	19874.815406	30.865434
486.069969	19884.834530	30.870452
486.468489	19919.388984	30.875469
486.952001	19948.717752	30.880487
487.646262	19975.404176	30.885504
487.795259	20012.815754	30.890522
488.605448	20036.255543	30.895540
488.826654	20060.798513	30.900557
489.461358	20098.203679	30.905575
490.183616	20123.761290	30.910592
489.920464	20163.183702	30.915610
490.782808	20188.814229	30.920628
491.280541	20226.361138	30.925645
491.855849	20245.453143	30.930663
492.564511	20292.008484	30.935680
492.871450	20320.354552	30.940698
493.669145	20343.114298	30.945716
494.246508	20372.466911	30.950733
494.537752	20404.998234	30.955751
495.000285	20434.975478	30.960768
495.552462	20469.285696	30.965786
496.349492	20493.612653	30.970804
496.961942	20524.154153	30.975821
497.325734	20552.794929	30.980839
497.898194	20580.404772	30.985856
498.237566	20609.466464	30.990874
498.562470	20629.539493	30.995892
499.243906	20667.393346	31.000909
499.690572	20689.917833	31.005927
500.360458	20721.739586	31.010944
500.803593	20755.403957	31.015962
501.340149	20780.707186	31.020980
502.093386	20808.251125	31.025997
502.753001	20825.277019	31.031015
502.755101	20851.396981	31.036032
503.514563	20881.928649	31.041050
503.928910	20912.546010	31.046068
504.396231	20923.138373	31.051085
504.663719	20957.146521	31.056103
505.554484	20985.421062	31.061120
505.886443	21025.693438	31.066138
506.796836	21045.365586	31.071156
507.112576	21074.798138	31.076173
507.466125	21112.179771	31.081191
508.134891	21134.512021	31.086208
508.586971	21153.965411	31.091226
509.212676	21178.218957	31.096244
509.681200	21204.430614	31.101261
509.794392	21238.280178	31.106279
510.552942	21259.979294	31.111296
510.861667	21301.525896	31.116314
511.443809	21311.784559	31.121332
512.144526	21344.809334	31.126349
512.792184	21378.107854	31.131367
512.802686	21405.851105	31.136384
513.068117	21434.356925	31.141402
513.931004	21462.112078	31.146420
514.275268	21495.376174	31.151437
515.063265	21528.071656	31.156455
515.732805	21555.124265	31.161472
516.294808	21587.690959	31.166490
516.825778	21606.898651	31.171508
517.203264	21635.014412	31.176525
517.608908	21666.171393	31.181543
518.243762	21685.685144	31.186560
518.983495	21713.801148	31.191578
519.423802	21735.853931	31.196596
519.980488	21752.075323	31.201613
520.342996	21781.874409	31.206631
520.769765	21790.508480	31.211648
521.512609	21820.563989	31.216666
521.847857	21842.317410	31.221684
522.521465	21871.353891	31.226701
522.542834	21900.081853	31.231719
523.131482	21916.254144	31.236736
523.118483	21947.717250	31.241754
523.995177	21982.238350	31.246772
524.915016	22021.548695	31.251789
525.239647	22054.905271	31.256807
525.864586	22075.659442	31.261824
526.358181	22113.526541	31.266842
526.698107	22136.871890	31.271860
527.414726	22170.350512	31.276877
528.163876	22206.490640	31.281895
528.669254	22218.019247	31.286912
528.792327	22245.847146	31.291930
528.948690	22284.241302	31.296948
529.945141	22326.813421	31.301965
530.136959	22356.659063	31.306983
530.826856	22390.464505	31.312000
531.688206	22419.099573	31.317018
532.093493	22460.248034	31.322036
532.589075	22495.461612	31.327053
533.444697	22536.640802	31.332071
533.937037	22563.558255	31.337088
534.549352	22593.117231	31.342106
535.026450	22620.308863	31.347124
535.646606	22647.478126	31.352141
535.795970	22690.025725	31.357159
536.566846	22711.497028	31.362176
537.142527	22738.692339	31.367194
537.828199	22780.783314	31.372212
538.206274	22797.520105	31.377229
538.863836	22837.549286	31.382247
539.535409	22855.990528	31.387264
540.170233	22892.857547	31.392282
540.595343	22920.329452	31.397300
541.213590	22954.140761	31.402317
541.718084	22979.293856	31.407335
542.359806	23010.953101	31.412352
543.039248	23036.824520	31.417370
543.436853	23063.384663	31.422388
544.371695	23087.882819	31.427405
544.437320	23128.618250	31.432423
545.294695	23146.038561	31.437440
545.896092	23169.432643	31.442458
546.360801	23195.957177	31.447476
546.812786	23209.997107	31.452493
547.251750	23241.081837	31.457511
547.766655	23269.020416	31.462528
548.205134	23295.934661	31.467546
548.589921	23325.220725	31.472564
549.721305	23351.242943	31.477581
550.111405	23389.198198	31.482599
550.498747	23407.166296	31.487616
550.852468	23435.800191	31.492634
551.355795	23467.197474	31.497652
552.196016	23497.771095	31.502669
552.188697	23533.520264	31.507687
553.079082	23564.503201	31.512704
553.821261	23598.075022	31.517722
553.860084	23630.910275	31.522740
554.724509	23656.178476	31.527757
555.168434	23676.305470	31.532775
555.443223	23700.149446	31.537792
555.749561	23734.623906	31.542810
556.291975	23764.814867	31.547828
557.254018	23795.047580	31.552845
557.356771	23835.266774	31.557863
558.039523	23866.630265	31.562880
558.703839	23899.936738	31.567898
558.833237	23937.447277	31.572916
559.469560	23974.019055	31.577933
559.780119	24015.924938	31.582951
560.677011	24044.898035	31.587968
561.159070	24087.162691	31.592986
561.807050	24125.729859	31.598004
563.112477	24156.825660	31.603021
563.317015	24196.454568	31.608039
563.753921	24232.160689	31.613056
564.558889	24265.407826	31.618074
565.243761	24296.013324	31.623092
565.630718	24329.604094	31.628109
566.343986	24365.583144	31.633127
566.922260	24400.205747	31.638144
567.513740	24435.211832	31.643162
567.887904	24474.037421	31.648180
568.597416	24499.754365	31.653197
569.266589	24537.996712	31.658215
569.660076	24566.904062	31.663232
570.625812	24607.463615	31.668250
570.890948	24642.085122	31.673268
571.361949	24664.509207	31.678285
571.652848	24708.694676	31.683303
572.666700	24743.066384	31.688320
573.088418	24769.113132	31.693338
573.505956	24810.163410	31.698356
574.587264	24846.180478	31.703373
574.981617	24890.527096	31.708391
575.488507	24919.214963	31.713408
576.524512	24956.477983	31.718426
577.161658	24984.880117	31.723444
577.885705	25022.109961	31.728461
578.408566	25051.452767	31.733479
578.527157	25075.670430	31.738496
579.171023	25110.581015	31.743514
579.838734	25139.819107	31.748532
580.534550	25172.869977	31.753549
581.086654	25204.831129	31.758567
581.478325	25233.562770	31.763584
582.339262	25258.770352	31.768602
582.964657	25294.423566	31.773620
583.995635	25330.676902	31.778637
584.174027	25356.623486	31.783655
584.821633	25383.450911	31.788672
585.249203	25409.421736	31.793690
585.812489	25451.202559	31.798708
586.417888	25479.926358	31.803725
586.651156	25511.451304	31.808743
587.351548	25537.114131	31.813760
588.337226	25570.126578	31.818778
588.203181	25614.317392	31.823796
588.911022	25637.956813	31.828813
589.690720	25672.442628	31.833831
590.241716	25712.247783	31.838848
590.710594	25741.157655	31.843866
591.408733	25776.288415	31.848884
592.081214	25807.005601	31.853901
592.630413	25842.273562	31.858919
593.201846	25867.805330	31.863936
594.068605	25890.693361	31.868954
594.302915	25918.009668	31.873972
595.233424	25941.387053	31.878989
596.099244	25968.958445	31.884007
596.751842	25996.601189	31.889024
597.180861	26006.007788	31.894042
597.950000	26042.600459	31.899060
597.941466	26063.849843	31.904077
598.612678	26088.576259	31.909095
598.986219	26119.770504	31.914112
599.886201	26141.433848	31.919130
600.460444	26187.113963	31.924148
600.778872	26206.991393	31.929165
601.529826	26245.040900	31.934183
601.738978	26278.959820	31.939200
602.491298	26313.640625	31.944218
603.085086	26357.548430	31.949236
603.727769	26385.559829	31.954253
604.266451	26424.780545	31.959271
604.805863	26455.898771	31.964288
605.994708	26494.581707	31.969306
606.062165	26536.638359	31.974324
606.939489	26569.170121	31.979341
607.155620	26609.939601	31.984359
608.259537	26639.282202	31.989376
608.575488	26674.645030	31.994394
608.783108	26712.502422	31.999412
610.135959	26743.512655	32.004429
610.532342	26776.233838	32.009447
611.200577	26820.939984	32.014464
611.988400	26844.719983	32.019482
612.337296	26896.314859	32.024500
613.173818	26920.681429	32.029517
614.133485	26963.104858	32.034535
614.616091	27003.270886	32.039552
615.513282	27023.374493	32.044570
615.737039	27065.635295	32.049588
616.291817	27093.958499	32.054605
617.001285	27128.274511	32.059623
617.551070	27156.301527	32.064640
618.406767	27190.386171	32.069658
618.694306	27229.868993	32.074676
619.492307	27268.943285	32.079693
620.468204	27303.198907	32.084711
620.359193	27334.160896	32.089728
621.743506	27364.800573	32.094746
621.741054	27407.546264	32.099764
622.611542	27448.107498	32.104781
623.297029	27484.766445	32.109799
623.626839	27519.692461	32.114816
624.650737	27550.395185	32.119834
624.959401	27584.736818	32.124852
625.491812	27621.186126	32.129869
626.112931	27659.460882	32.134887
626.676688	27702.048991	32.139904
627.449883	27734.630538	32.144922
628.205361	27779.495787	32.149940
628.409342	27815.029830	32.154957
629.299184	27844.388747	32.159975
629.681343	27892.346598	32.164992
630.433304	27932.042476	32.170010
631.137051	27972.118899	32.175028
631.770641	28005.430655	32.180045
632.689127	28041.213469	32.185063
633.106048	28084.198291	32.190080
633.607741	28116.949384	32.195098
634.249515	28148.490302	32.200116
634.896932	28182.685079	32.205133
635.163151	28219.189787	32.210151
635.802430	28250.156068	32.215168
637.269967	28271.094420	32.220186
638.171312	28304.118223	32.225204
638.635593	28323.165830	32.230221
639.388622	28348.577475	32.235239
639.687449	28378.200384	32.240256
640.505830	28409.928954	32.245274
640.666014	28439.169134	32.250292
641.495110	28469.417057	32.255309
642.352345	28505.147072	32.260327
642.783352	28534.155350	32.265344
643.335284	28569.187435	32.270362
643.802540	28607.399578	32.275380
644.120668	28641.318011	32.280397
644.935406	28673.508983	32.285415
644.990407	28721.216616	32.290432
645.793992	28755.135060	32.295450
646.903379	28805.724426	32.300468
647.191667	28853.446398	32.305485
648.059147	28891.040151	32.310503
648.456843	28947.885260	32.315520
649.144933	28979.742577	32.320538
649.820351	29030.944064	32.325556
650.267298	29071.852984	32.330573
651.610960	29110.681009	32.335591
651.916058	29158.034440	32.340608
652.717574	29205.588360	32.345626
653.303677	29242.455662	32.350644
653.713242	29291.670385	32.355661
654.343891	29337.879706	32.360679
655.222312	29388.607820	32.365696
656.182998	29426.421839	32.370714
657.143322	29467.756836	32.375732
658.239032	29508.735695	32.380749
658.765984	29543.210779	32.385767
659.656236	29575.467198	32.390784
660.065798	29611.420962	32.395802
660.552776	29633.860689	32.400820
661.286065	29677.267073	32.405837
661.946430	29710.627984	32.410855
662.736288	29745.555286	32.415872
663.468385	29779.353878	32.420890
663.709734	29822.793364	32.425908
664.401666	29861.661668	32.430925
665.453577	29889.531625	32.435943
666.088484	29936.095613	32.440960
666.641899	29957.362181	32.445978
667.425520	29994.724564	32.450996
668.378581	30038.691492	32.456013
668.964114	30061.356460	32.461031
669.258775	30098.764000	32.466048
670.259483	30130.447721	32.471066
670.647068	30167.727050	32.476084
671.204919	30197.090772	32.481101
671.772527	30238.040008	32.486119
672.392280	30277.211183	32.491136
673.103037	30309.800291	32.496154
673.407004	30365.924398	32.501172
674.204238	30399.707488	32.506189
675.268969	30440.863736	32.511207
675.969854	30481.211015	32.516224
676.594219	30517.834397	32.521242
677.335539	30564.604390	32.526260
677.934047	30605.770767	32.531277
678.600669	30634.884185	32.536295
679.296162	30672.956960	32.541312
679.743153	30696.978153	32.546330
680.358539	30738.072614	32.551348
680.659304	30776.605650	32.556365
681.379350	30801.191067	32.561383
682.332934	30845.109062	32.566400
682.916021	30885.835905	32.571418
683.891641	30927.734057	32.576436
684.222384	30967.659815	32.581453
685.364410	30989.239848	32.586471
685.477989	31035.850031	32.591488
686.323205	31072.212233	32.596506
686.934995	31107.245590	32.601524
687.400733	31151.069951	32.606541
688.203661	31194.601377	32.611559
688.872191	31236.914902	32.616576
689.668315	31288.918588	32.621594
690.129181	31330.063710	32.626612
690.806649	31376.390377	32.631629
691.755550	31419.475864	32.636647
692.648520	31468.695933	32.641664
693.482155	31506.837112	32.646682
693.750605	31543.341040	32.651700
694.413141	31587.388372	32.656717
695.373499	31625.611073	32.661735
696.039456	31664.758674	32.666752
696.921365	31710.617869	32.671770
697.625284	31755.139532	32.676788
698.124224	31804.251415	32.681805
699.275649	31854.601460	32.686823
699.706548	31896.100096	32.691840
700.056704	31938.654565	32.696858
700.814435	31972.307329	32.701876
701.615770	32019.140747	32.706893
702.970801	32063.839267	32.711911
703.613486	32104.540204	32.716928
704.323041	32144.276139	32.721946
704.987908	32192.958352	32.726964
705.745852	32232.016753	32.731981
706.309417	32264.745785	32.736999
706.935951	32310.747449	32.742016
707.685831	32349.219390	32.747034
708.240888	32387.608116	32.752052
709.187923	32439.749098	32.757069
710.423298	32475.053783	32.762087
710.884360	32515.265559	32.767104
711.692306	32566.979778	32.772122
712.394958	32589.907345	32.777140
712.806347	32629.305254	32.782157
713.513899	32652.952839	32.787175
714.285204	32704.609915	32.792192
714.955094	32753.400126	32.797210
716.358630	32784.291467	32.802228
716.700361	32830.888901	32.807245
717.155203	32867.056172	32.812263
717.759940	32902.668972	32.817280
718.587987	32949.848016	32.822298
719.368837	32983.315452	32.827316
719.912222	33020.664012	32.832333
720.567487	33054.555848	32.837351
721.469257	33105.112390	32.842368
721.966189	33152.792621	32.847386
723.085218	33185.208511	32.852404
723.475439	33228.378911	32.857421
724.273465	33265.074774	32.862439
724.596194	33308.091529	32.867456
725.608120	33360.180391	32.872474
726.562636	33397.534785	32.877492
726.997619	33436.570148	32.882509
727.764513	33466.917327	32.887527
728.524715	33502.930398	32.892544
729.139874	33543.941921	32.897562
729.915963	33577.796717	32.902580
730.534749	33611.777358	32.907597
731.177720	33652.955444	32.912615
732.045962	33694.085687	32.917632
732.700375	33740.275800	32.922650
733.487795	33770.803554	32.927668
733.896136	33821.540254	32.932685
735.011090	33858.598483	32.937703
735.774854	33889.262885	32.942720
736.564975	33934.148717	32.947738
737.227312	33970.102047	32.952756
737.830632	34015.327106	32.957773
738.666018	34054.440009	32.962791
739.638484	34090.136336	32.967808
740.111611	34138.328332	32.972826
741.096529	34165.651832	32.977844
741.618575	34209.979594	32.982861
742.211863	34255.775769	32.987879
743.152732	34303.641994	32.992896
744.081618	34340.085310	32.997914
744.902490	34378.676316	33.002932
745.535463	34419.351661	33.007949
746.365347	34460.312380	33.012967
747.431857	34499.364626	33.017984
747.909849	34543.017145	33.023002
749.055440	34567.236884	33.028020
749.828765	34614.719082	33.033037
750.431523	34653.211971	33.038055
751.235075	34678.440124	33.043072
751.421959	34724.421091	33.048090
752.424278	34767.049883	33.053108
753.070454	34815.266909	33.058125
753.733878	34865.036736	33.063143
754.843735	34905.012388	33.068160
755.186592	34956.584031	33.073178
756.179366	34999.031427	33.078196
757.080869	35043.383713	33.083213
757.528539	35078.000506	33.088231
758.410150	35122.242263	33.093248
758.725765	35172.528845	33.098266
759.953374	35207.915232	33.103284
760.816317	35270.635549	33.108301
761.605055	35323.434445	33.113319
761.856186	35361.952074	33.118336
762.537790	35415.330712	33.123354
763.465389	35457.757622	33.128372
764.549531	35507.652763	33.133389
765.177024	35558.991610	33.138407
766.061005	35598.137704	33.143424
766.805587	35653.897155	33.148442
767.520618	35690.237188	33.153460
768.278986	35733.886194	33.158477
769.028544	35786.578565	33.163495
769.961230	35831.338615	33.168512
770.892367	35886.930358	33.173530
771.342137	35917.842895	33.178548
771.994010	35970.247512	33.183565
772.640686	36017.600936	33.188583
773.955117	36059.329843	33.193600
774.740533	36109.013933	33.198618
775.449990	36140.682838	33.203636
776.309305	36187.200307	33.208653
776.874199	36236.362792	33.213671
777.666074	36285.597340	33.218688
778.582599	36325.428903	33.223706
779.351156	36359.516976	33.228724
779.925637	36392.528938	33.233741
780.660564	36428.228476	33.238759
781.611165	36472.462246	33.243776
782.256727	36512.241743	33.248794
782.940982	36542.871863	33.253812
783.780657	36577.240017	33.258829
784.468770	36615.185627	33.263847
785.576541	36643.814658	33.268864
786.263480	36699.143247	33.273882
786.783331	36732.448838	33.278900
787.641495	36785.234170	33.283917
788.263419	36831.986244	33.288935
788.996529	36874.819516	33.293952
789.527985	36925.272461	33.298970
790.464757	36972.361262	33.303988
791.504847	37026.124115	33.309005
791.978919	37073.336182	33.314023
793.092901	37117.096746	33.319040
793.354973	37160.858011	33.324058
794.474637	37208.721768	33.329076
795.625415	37263.036992	33.334093
796.264859	37310.856031	33.339111
797.180536	37357.715017	33.344128
797.633575	37411.400034	33.349146
798.545278	37464.931155	33.354164
799.562837	37514.487313	33.359181
800.286580	37555.110184	33.364199
801.283575	37603.752857	33.369216
801.657123	37653.346948	33.374234
802.391927	37704.054444	33.379252
803.505651	37757.466131	33.384269
804.309920	37813.898504	33.389287
804.941075	37862.902586	33.394304
805.750995	37920.061568	33.399322
806.683821	37960.184516	33.404340
807.757752	38015.544437	33.409357
808.420319	38069.135051	33.414375
809.668911	38106.546558	33.419392
810.199805	38160.815682	33.424410
811.072823	38211.148604	33.429428
811.850406	38256.633637	33.434445
812.737224	38310.714606	33.439463
813.879112	38366.722461	33.444480
815.018944	38397.669647	33.449498
815.699108	38446.591500	33.454516
816.485916	38486.972278	33.459533
816.899188	38536.587478	33.464551
817.845969	38569.082859	33.469568
819.053378	38622.450408	33.474586
819.559873	38669.344712	33.479604
820.282269	38715.389532	33.484621
821.116826	38760.322854	33.489639
822.407014	38803.559683	33.494656
822.692334	38853.277858	33.499674
823.572233	38889.964300	33.504692
824.541797	38937.482306	33.509709
825.133992	38986.849186	33.514727
826.110037	39024.855155	33.519744
826.912785	39075.080944	33.524762
827.876957	39123.972508	33.529780
829.056229	39160.770631	33.534797
829.194577	39215.135496	33.539815
830.056037	39247.120366	33.544832
831.361758	39298.045769	33.549850
832.501567	39335.685144	33.554868
833.062111	39381.440525	33.559885
833.765310	39427.350739	33.564903
834.564090	39459.390008	33.569920
835.069079	39492.638962	33.574938
835.401313	39535.711059	33.579956
836.659577	39566.578143	33.584973
837.005009	39627.476047	33.589991
838.063664	39656.211661	33.595008
838.735862	39710.070453	33.600026
839.436197	39752.307468	33.605044
840.703044	39791.388628	33.610061
841.144538	39839.617401	33.615079
842.419586	39892.370374	33.620096
843.001912	39934.974056	33.625114
843.729427	39982.551233	33.630132
844.798405	40041.370160	33.635149
845.632751	40092.092976	33.640167
846.442754	40137.418785	33.645184
847.437405	40191.234602	33.650202
848.507727	40231.093596	33.655220
849.327941	40270.188639	33.660237
849.948971	40328.155135	33.665255
850.920646	40370.433081	33.670272
851.414889	40427.407798	33.675290
852.405929	40488.067881	33.680308
853.502622	40530.193749	33.685325
854.111394	40585.228329	33.690343
855.511833	40628.217539	33.695360
856.450393	40675.820106	33.700378
857.352077	40726.344123	33.705396
858.391785	40765.721909	33.710413
858.825674	40806.061083	33.715431
859.768958	40856.699053	33.720448
860.718817	40902.352402	33.725466
861.337505	40956.064544	33.730484
862.706201	40998.673662	33.735501
863.237678	41052.083469	33.740519
864.222066	41091.824682	33.745536
865.114060	41142.483996	33.750554
865.944934	41193.032831	33.755572
867.140956	41233.721475	33.760589
867.882336	41279.515776	33.765607
868.415642	41318.562756	33.770624
869.184116	41379.304440	33.775642
870.397303	41426.492487	33.780660
871.681983	41477.116387	33.785677
872.139386	41532.746275	33.790695
873.332698	41571.633438	33.795712
874.246605	41617.622796	33.800730
874.879533	41670.423703	33.805748
875.585523	41707.199059	33.810765
876.585996	41748.817395	33.815783
877.515477	41797.182797	33.820800
878.241215	41846.864138	33.825818
879.061161	41903.924521	33.830836
880.289844	41946.437243	33.835853
880.567579	42005.069119	33.840871
881.377299	42050.829032	33.845888
882.211580	42109.304467	33.850906
883.259035	42154.926173	33.855924
884.237372	42203.114049	33.860941
884.956035	42259.267781	33.865959
885.835227	42310.823611	33.870976
886.814289	42352.003701	33.875994
887.722434	42418.235395	33.881012
888.929925	42461.593651	33.886029
889.541931	42522.413596	33.891047
890.540749	42568.777474	33.896064
891.681875	42621.235440	33.901082
892.400216	42669.072897	33.906100
893.748020	42697.659726	33.911117
894.381476	42731.930798	33.916135
895.165804	42770.624803	33.921152
895.473467	42809.810966	33.926170
896.483646	42850.689840	33.931188
897.438788	42901.602654	33.936205
898.135847	42956.407979	33.941223
899.227622	42993.435010	33.946240
900.124814	43034.888527	33.951258
900.452615	43085.773495	33.956276
901.689366	43140.766752	33.961293
902.711047	43196.926026	33.966311
903.584254	43239.572813	33.971328
904.730591	43293.359849	33.976346
905.470256	43343.308042	33.981364
906.403414	43390.183620	33.986381
906.389104	43439.952804	33.991399
907.683749	43499.473081	33.996416
908.703218	43558.404078	34.001434
909.905050	43622.790698	34.006452
911.091937	43667.267804	34.011469
911.614990	43726.207399	34.016487
912.624565	43779.631187	34.021504
913.918935	43824.325815	34.026522
914.549171	43885.355388	34.031540
915.383359	43940.445294	34.036557
916.345343	43996.331301	34.041575
917.416411	44047.064140	34.046592
918.371787	44102.015288	34.051610
919.211815	44156.193954	34.056628
920.005279	44207.312199	34.061645
920.817261	44274.652485	34.066663
922.300750	44322.582448	34.071680
923.213311	44377.319589	34.076698
923.978599	44444.882768	34.081716
925.160436	44495.339940	34.086733
926.422499	44549.845665	34.091751
926.549970	44602.511324	34.096768
927.919477	44647.436217	34.101786
928.869435	44710.321988	34.106804
929.896271	44755.604384	34.111821
930.953961	44807.049520	34.116839
931.805662	44863.334510	34.121856
933.022966	44909.523589	34.126874
933.606705	44964.035330	34.131892
934.734876	45010.706675	34.136909
935.630684	45058.698616	34.141927
936.633453	45115.681717	34.146944
937.519722	45163.011177	34.151962
938.510850	45219.243604	34.156980
939.239886	45268.811915	34.161997
940.443344	45318.736203	34.167015
941.210156	45374.801720	34.172032
942.351298	45422.680120	34.177050
943.250888	45476.922252	34.182068
943.786275	45526.837745	34.187085
944.813594	45574.753270	34.192103
945.381560	45642.844381	34.197120
946.606484	45687.711774	34.202138
947.583208	45741.493333	34.207156
948.523365	45799.696223	34.212173
949.708833	45862.953217	34.217191
950.539658	45914.341534	34.222208
951.981107	45975.509163	34.227226
952.622884	46026.598388	34.232244
953.522696	46068.038169	34.237261
954.729827	46115.952001	34.242279
955.233276	46164.950319	34.247296
956.232977	46198.638002	34.252314
956.925869	46258.778602	34.257332
958.175016	46304.744167	34.262349
958.927913	46342.823027	34.267367
959.617326	46400.060891	34.272384
960.685964	46439.817494	34.277402
961.327559	46496.487417	34.282420
962.104683	46543.267531	34.287437
963.045658	46599.119051	34.292455
963.963796	46656.410319	34.297472
965.255372	46715.117256	34.302490
966.129476	46784.467075	34.307508
967.546680	46837.227034	34.312525
968.148836	46892.063204	34.317543
969.159478	46953.832350	34.322560
969.794004	47005.797949	34.327578
970.993903	47054.632218	34.332596
972.034231	47113.335247	34.337613
972.942566	47169.699391	34.342631
973.800685	47240.160210	34.347648
975.273721	47294.348568	34.352666
976.141011	47356.799198	34.357684
977.045087	47415.707809	34.362701
978.323259	47474.766770	34.367719
979.391775	47530.012270	34.372736
980.657359	47566.165618	34.377754
981.536851	47636.909013	34.382772
982.672882	47685.609138	34.387789
983.449156	47738.560126	34.392807
984.645692	47790.426877	34.397824
985.927579	47839.148781	34.402842
986.607035	47895.449344	34.407860
987.367979	47951.598105	34.412877
988.609624	47991.912394	34.417895
989.521127	48053.269859	34.422912
990.858008	48108.493730	34.427930
991.851014	48158.520534	34.432948
992.884288	48209.648292	34.437965
993.887138	48265.355052	34.442983
994.513673	48327.453800	34.448000
995.545074	48375.051979	34.453018
996.746101	48430.974853	34.458036
997.806129	48486.217684	34.463053
999.163803	48539.497067	34.468071
999.818545	48584.744200	34.473088
1001.125212	48629.648935	34.478106
1002.170815	48691.448973	34.483124
1002.898835	48723.348216	34.488141
1003.904191	48780.163019	34.493159
1004.608314	48847.837539	34.498176
1006.085067	48890.337301	34.503194
1006.913689	48952.209979	34.508212
1007.996757	49017.339245	34.513229
1008.960477	49049.208367	34.518247
1009.542222	49116.346084	34.523264
1010.452890	49166.255129	34.528282
1011.601212	49225.946348	34.533300
1012.222553	49280.076665	34.538317
1013.573720	49331.967008	34.543335
1014.764426	49388.564497	34.548352
1015.727490	49445.014287	34.553370
1016.478739	49504.888615	34.558388
1017.587371	49571.420035	34.563405
1019.051577	49624.172789	34.568423
1019.764967	49681.592317	34.573440
1020.425186	49728.485870	34.578458
1021.994497	49788.062025	34.583476
1022.756804	49833.604810	34.588493
1023.622907	49888.982627	34.593511
1024.451287	49938.172301	34.598528
1025.611961	49979.344284	34.603546
1026.578065	50041.426151	34.608564
1027.545106	50088.753258	34.613581
1028.321033	50137.179667	34.618599
1029.384194	50198.538126	34.623616
1029.984918	50247.612256	34.628634
1031.131073	50304.997219	34.633652
1031.890412	50359.987949	34.638669
1033.041756	50425.066233	34.643687
1034.283460	50493.351100	34.648704
1035.670582	50544.972817	34.653722
1036.762220	50604.461372	34.658740
1037.750852	50664.573623	34.663757
1039.099606	50713.481009	34.668775
1039.935892	50780.083876	34.673792
1041.019952	50843.174455	34.678810
1042.592237	50895.419681	34.683828
1043.589586	50948.900286	34.688845
1044.791941	50995.464773	34.693863
1045.834110	51049.571329	34.698880
1047.139890	51093.437023	34.703898
1048.308498	51149.523464	34.708916
1049.026501	51195.360610	34.713933
1050.224769	51241.571900	34.718951
1051.380366	51293.636498	34.723968
1052.313893	51336.472620	34.728986
1053.533476	51391.665828	34.734004
1054.200416	51454.146346	34.739021
1055.411788	51502.577045	34.744039
1056.411660	51562.746820	34.749056
1057.688226	51611.034663	34.754074
1058.531484	51668.154064	34.759092
1059.537212	51723.951023	34.764109
1060.587485	51771.034431	34.769127
1061.701881	51838.583899	34.774144
1062.411616	51892.459731	34.779162
1063.745613	51957.475767	34.784180
1064.678935	52009.007290	34.789197
1065.704269	52072.933004	34.794215
1066.801469	52137.113404	34.799232
1067.964441	52192.678057	34.804250
1069.124458	52255.456862	34.809268
1069.826214	52307.727674	34.814285
1071.165892	52375.237101	34.819303
1072.405054	52430.619547	34.824320
1073.393059	52500.519328	34.829338
1074.490741	52544.913917	34.834356
1075.430363	52608.019255	34.839373
1076.500926	52669.712149	34.844391
1077.836764	52734.249155	34.849408
1079.366536	52790.023574	34.854426
1080.311271	52842.093019	34.859444
1081.443098	52897.790788	34.864461
1082.707578	52949.089035	34.869479
1083.678071	53003.831496	34.874496
1084.454161	53057.117465	34.879514
1085.805059	53107.978563	34.884532
1086.580473	53151.456591	34.889549
1087.983332	53208.890816	34.894567
1088.858568	53268.084694	34.899584
1089.890870	53315.756212	34.904602
1090.967645	53370.343676	34.909620
1092.016349	53429.074172	34.914637
1093.304302	53483.856646	34.919655
1094.420523	53546.848277	34.924672
1095.219778	53592.145863	34.929690
1096.767367	53639.212138	34.934708
1097.764829	53688.731334	34.939725
1098.273791	53721.886764	34.944743
1099.363826	53772.828117	34.949760
1100.003770	53817.841005	34.954778
1101.208420	53853.210117	34.959796
1102.210570	53915.322004	34.964813
1103.356955	53974.399276	34.969831
1104.327809	54044.534165	34.974848
1105.629278	54099.961435	34.979866
1106.812526	54157.141270	34.984884
1107.732464	54219.526287	34.989901
1108.917135	54281.192902	34.994919
1109.895277	54347.555929	34.999936
1111.147046	54408.744083	35.004954
1112.020574	54454.803752	35.009972
1113.069398	54514.384930	35.014989
1114.413157	54584.222568	35.020007
1115.747036	54642.886137	35.025024
1116.469161	54700.759659	35.030042
1117.727345	54763.820919	35.035060
1118.861532	54844.469330	35.040077
1119.943663	54903.717201	35.045095
1121.361734	54972.050851	35.050112
1122.580341	55036.517613	35.055130
1123.733391	55100.564481	35.060148
1124.706083	55168.949442	35.065165
1126.225340	55215.972682	35.070183
1127.048081	55289.798645	35.075200
1128.401871	55356.966370	35.080218
1129.406519	55421.246179	35.085236
1130.438214	55474.003972	35.090253
1132.035016	55532.407086	35.095271
1132.901470	55604.841230	35.100288
1133.942954	55660.844468	35.105306
1135.554265	55729.409522	35.110324
1136.599541	55793.766251	35.115341
1137.935248	55852.090785	35.120359
1138.989576	55908.257141	35.125376
1140.340668	55965.079651	35.130394
1141.200652	56028.174973	35.135412
1142.533725	56087.101723	35.140429
1143.778501	56137.764473	35.145447
1145.069648	56206.197494	35.150464
1145.927915	56271.477144	35.155482
1147.796964	56332.972341	35.160500
1148.778581	56378.164442	35.165517
1149.966140	56430.691107	35.170535
1150.784402	56488.743799	35.175552
1152.020745	56545.199602	35.180570
1152.996336	56601.196382	35.185588
1154.354783	56662.854645	35.190605
1155.193479	56715.765655	35.195623
1156.154770	56769.436042	35.200640
1157.322603	56836.567440	35.205658
1158.633187	56900.278045	35.210676
1159.813883	56956.332152	35.215693
1161.303799	57016.148010	35.220711
1162.504941	57072.192859	35.225728
1163.903837	57142.953415	35.230746
1165.119025	57190.287657	35.235764
1166.035470	57249.041999	35.240781
1167.108313	57302.885990	35.245799
1168.090751	57361.250534	35.250816
1169.322856	57417.803996	35.255834
1170.629008	57466.459975	35.260852
1171.699041	57532.425097	35.265869
1172.859287	57584.819334	35.270887
1173.612455	57636.941972	35.275904
1174.794146	57680.871034	35.280922
1176.059322	57728.128892	35.285940
1176.748796	57770.919982	35.290957
1178.285475	57825.622916	35.295975
1179.344620	57881.198211	35.300992
1180.369139	57934.222061	35.306010
1181.847538	57995.883963	35.311028
1182.733350	58048.119639	35.316045
1183.920334	58094.042334	35.321063
1184.977541	58151.833791	35.326080
1185.655008	58217.843260	35.331098
1187.295453	58272.005637	35.336116
1188.107691	58342.424847	35.341133
1189.767834	58400.236435	35.346151
1190.952729	58463.325274	35.351168
1192.056938	58531.262533	35.356186
1193.155886	58595.112035	35.361204
1194.691500	58655.215973	35.366221
1195.967892	58719.006376	35.371239
1197.078976	58779.272024	35.376256
1197.853136	58848.521398	35.381274
1199.501092	58910.659120	35.386292
1200.424082	58983.316141	35.391309
1201.796385	59051.472398	35.396327
1203.508869	59107.195085	35.401344
1204.704820	59172.853821	35.406362
1205.928944	59234.653638	35.411380
1207.179025	59294.012672	35.416397
1208.464247	59357.942626	35.421415
1209.570751	59423.210950	35.426432
1210.804955	59488.136648	35.431450
1212.637324	59550.259802	35.436468
1213.369007	59611.688267	35.441485
1214.801848	59671.639917	35.446503
1216.259384	59723.080784	35.451520
1217.056451	59781.511842	35.456538
1218.425433	59841.062479	35.461556
1219.582931	59896.930831	35.466573
1220.701540	59960.483351	35.471591
1222.142558	60015.801214	35.476608
1222.888282	60087.501845	35.481626
1224.543000	60137.399908	35.486644
1225.657930	60210.948363	35.491661
1227.173007	60276.079055	35.496679
1228.530951	60329.461056	35.501696
1229.793868	60391.827422	35.506714
1231.413384	60442.136732	35.511732
1232.381684	60504.916640	35.516749
1233.630390	60557.904800	35.521767
1234.934432	60602.180815	35.526784
1235.728419	60665.203639	35.531802
1237.177528	60722.629697	35.536820
1238.386751	60781.948115	35.541837
1239.825696	60842.534683	35.546855
1241.273594	60891.257648	35.551872
1242.021273	60957.048335	35.556890
1243.095065	61006.823901	35.561908
1244.237501	61071.603599	35.566925
1245.769434	61133.853784	35.571943
1247.306330	61191.362149	35.576960
1248.364567	61258.541947	35.581978
1249.703518	61317.081744	35.586996
1250.897173	61365.104833	35.592013
1252.426739	61424.020172	35.597031
1253.557192	61468.135026	35.602048
1254.396714	61541.768569	35.607066
1255.569641	61586.136521	35.612084
1256.779253	61635.873110	35.617101
1257.762255	61694.456868	35.622119
1259.281506	61733.668756	35.627136
1260.432243	61788.061222	35.632154
1261.271261	61844.692857	35.637172
1262.313452	61892.924265	35.642189
1263.318782	61958.962156	35.647207
1265.091873	62004.249749	35.652224
1266.112943	62083.148575	35.657242
1267.114629	62137.584135	35.662260
1268.473671	62193.628742	35.667277
1270.051273	62263.439343	35.672295
1271.106747	62325.210062	35.677312
1272.432504	62388.939014	35.682330
1273.890048	62447.678166	35.687348
1275.833315	62516.349748	35.692365
1276.790355	62576.712169	35.697383
1277.936580	62638.184596	35.702400
1279.316740	62700.329562	35.707418
1280.704071	62767.943063	35.712436
1282.146286	62818.310321	35.717453
1283.545866	62883.839501	35.722471
1284.596888	62946.916545	35.727488
1285.870787	63012.573358	35.732506
1287.079014	63073.201530	35.737524
1288.473068	63134.794655	35.742541
1289.752321	63197.969550	35.747559
1291.089931	63255.456952	35.752576
1292.059990	63331.240434	35.757594
1293.459167	63392.124369	35.762612
1295.027819	63464.320061	35.767629
1296.471809	63533.724673	35.772647
1297.596715	63592.885787	35.777664
1299.226170	63665.743593	35.782682
1300.199199	63730.075643	35.787700
1301.667919	63797.856464	35.792717
1303.010635	63868.100853	35.797735
1304.602804	63926.119719	35.802752
1305.564299	63995.499855	35.807770
1306.904975	64055.679194	35.812788
1308.445320	64111.984637	35.817805
1309.446146	64188.373659	35.822823
1310.660193	64240.666096	35.827840
1312.515096	64323.277973	35.832858
1313.693141	64383.065723	35.837876
1315.180305	64443.856151	35.842893
1316.136595	64507.831962	35.847911
1317.658869	64572.453721	35.852928
1319.063562	64640.746991	35.857946
1320.497380	64711.055457	35.862964
1322.154068	64768.990210	35.867981
1323.214354	64835.907130	35.872999
1324.375697	64896.952251	35.878016
1325.776289	64952.888942	35.883034
1327.219614	65012.889908	35.888052
1328.840933	65077.984954	35.893069
1329.523009	65144.411099	35.898087
1330.602346	65199.987111	35.903104
1332.313785	65270.380305	35.908122
1333.490408	65329.809661	35.913140
1335.183190	65404.428987	35.918157
1336.518706	65467.157627	35.923175
1337.615282	65518.458135	35.928192
1338.856422	65587.494997	35.933210
1340.500959	65651.536921	35.938228
1341.908623	65715.938977	35.943245
1343.337808	65782.939952	35.948263
1344.547123	65840.814251	35.953280
1345.645678	65885.233163	35.958298
1346.827546	65942.510524	35.963316
1348.441106	65982.132215	35.968333
1349.214321	66042.879986	35.973351
1350.398182	66098.796167	35.978368
1351.929110	66151.809061	35.983386
1353.260974	66208.297458	35.988404
1354.719183	66264.329343	35.993421
1355.607086	66338.931802	35.998439
1357.118663	66381.229248	36.003456
1358.215899	66449.088031	36.008474
1359.654719	66521.160880	36.013492
1361.611190	66575.887170	36.018509
1362.592938	66642.346315	36.023527
1364.109228	66706.746551	36.028544
1365.261700	66772.248590	36.033562
1366.672636	66842.515922	36.038580
1368.608847	66912.935489	36.043597
1369.498219	66983.436808	36.048615
1370.857425	67046.602526	36.053632
1372.286465	67115.607806	36.058650
1373.577510	67179.974853	36.063668
1375.001743	67246.151036	36.068685
1376.716991	67324.337174	36.073703
1378.073546	67392.474459	36.078720
1379.920202	67449.385232	36.083738
1381.427767	67524.615970	36.088756
1382.908497	67582.945621	36.093773
1384.026966	67649.525285	36.098791
1385.448181	67718.014223	36.103808
1387.021227	67776.874392	36.108826
1387.993318	67843.103902	36.113844
1389.538654	67909.642752	36.118861
1390.711607	67984.420681	36.123879
1392.426041	68041.695386	36.128896
1393.738936	68111.702961	36.133914
1395.027801	68179.852939	36.138932
1396.797190	68237.499389	36.143949
1397.870487	68317.093399	36.148967
1399.427347	68381.833432	36.153984
1400.677808	68449.806515	36.159002
1402.125669	68516.906739	36.164020
1404.147234	68591.243340	36.169037
1405.401004	68670.309974	36.174055
1406.926429	68718.396509	36.179072
1408.221237	68779.569364	36.184090
1409.255752	68847.735598	36.189108
1410.812486	68925.824796	36.194125
1411.757538	68992.555394	36.199143
1413.394146	69062.913802	36.204160
1415.110805	69126.896184	36.209178
1416.072172	69199.785827	36.214196
1417.924441	69263.835970	36.219213
1419.530461	69346.819743	36.224231
1420.499823	69404.195115	36.229248
1422.382555	69459.926936	36.234266
1423.182094	69541.384890	36.239284
1425.712418	69598.813970	36.244301
1427.058387	69667.275551	36.249319
1428.169274	69731.442901	36.254336
1430.133936	69794.824555	36.259354
1431.205022	69858.973122	36.264372
1432.630650	69923.199329	36.269389
1434.115736	69997.269352	36.274407
1435.286869	70036.611989	36.279424
1436.942080	70103.740871	36.284442
1438.444651	70176.491558	36.289460
1439.414844	70224.211883	36.294477
1440.749973	70277.941525	36.299495
1441.762739	70329.670064	36.304512
1443.147616	70377.807019	36.309530
1444.225089	70444.824579	36.314548
1445.763914	70504.601862	36.319565
1446.717690	70576.185759	36.324583
1448.706285	70633.841247	36.329600
1450.285473	70695.208414	36.334618
1451.312677	70771.986596	36.339636
1452.915476	70834.832183	36.344653
1454.286909	70900.107807	36.349671
1455.817117	70965.219427	36.354688
1457.325671	71042.657628	36.359706
1458.655613	71109.156107	36.364724
1459.985774	71180.404116	36.369741
1461.442307	71259.459563	36.374759
1463.021521	71330.884305	36.379776
1465.266580	71406.916462	36.384794
1466.357089	71486.435171	36.389812
1467.920565	71548.934006	36.394829
1469.198695	71622.306454	36.399847
1470.713431	71706.103614	36.404864
1472.531352	71771.400182	36.409882
1474.117102	71849.309967	36.414900
1475.810779	71909.066226	36.419917
1477.331222	71983.275668	36.424935
1478.649252	72052.767449	36.429952
1480.314079	72124.649574	36.434970
1481.819976	72195.720847	36.439988
1482.923231	72258.116087	36.445005
1484.696033	72333.338259	36.450023
1486.057311	72405.154672	36.455040
1487.618929	72480.296327	36.460058
1488.689603	72555.806351	36.465076
1490.461645	72627.913717	36.470093
1492.002540	72704.515815	36.475111
1493.076051	72779.570066	36.480128
1495.273954	72853.688587	36.485146
1496.318920	72932.889475	36.490164
1497.938580	73009.695449	36.495181
1499.686913	73090.623277	36.500199
1501.166054	73167.692356	36.505216
1502.985724	73242.542467	36.510234
1504.467323	73323.360763	36.515252
1506.029782	73389.359961	36.520269
1507.486267	73463.596238	36.525287
1509.147775	73531.404211	36.530304
1510.534111	73598.242130	36.535322
1512.167671	73674.617203	36.540340
1513.982708	73733.522626	36.545357
1515.095103	73815.476839	36.550375
1516.666008	73888.442428	36.555392
1518.490342	73949.943476	36.560410
1519.985639	74024.276574	36.565428
1522.125269	74089.756517	36.570445
1523.294862	74138.820705	36.575463
1524.931866	74211.966833	36.580480
1526.620984	74280.849048	36.585498
1527.913613	74337.190269	36.590516
1529.382245	74406.411316	36.595533
1531.155421	74469.656896	36.600551
1532.264965	74532.955830	36.605568
1533.800322	74593.287596	36.610586
1535.147734	74666.809629	36.615604
1536.547429	74730.126948	36.620621
1538.055627	74796.594129	36.625639
1539.016682	74872.621885	36.630656
1540.846656	74934.453660	36.635674
1542.242965	75006.778289	36.640692
1543.718696	75066.753115	36.645709
1545.397302	75125.530964	36.650727
1546.666675	75191.149818	36.655744
1548.088525	75246.940717	36.660762
1549.207282	75315.699528	36.665780
1550.710735	75383.232934	36.670797
1552.380874	75454.755888	36.675815
1553.655742	75529.292337	36.680832
1555.591369	75592.920491	36.685850
1556.988956	75675.393108	36.690868
1558.493856	75744.459925	36.695885
1560.133797	75811.884375	36.700903
1561.926647	75897.082601	36.705920
1563.542778	75965.220529	36.710938
1565.047858	76050.400943	36.715956
1566.510613	76131.065986	36.720973
1568.347913	76201.158676	36.725991
1570.010223	76281.311571	36.731008
1571.400755	76352.247294	36.736026
1572.922566	76434.677449	36.741044
1574.334628	76516.022953	36.746061
1575.939894	76599.200602	36.751079
1577.688737	76683.508791	36.756096
1579.658775	76763.234919	36.761114
1581.144241	76834.461069	36.766132
1582.942989	76912.554972	36.771149
1584.227054	76994.948032	36.776167
1585.636411	77088.330088	36.781184
1587.678892	77161.648785	36.786202
1589.383319	77246.662406	36.791220
1591.189448	77324.363631	36.796237
1592.957789	77393.216067	36.801255
1594.481788	77480.652906	36.806272
1596.320433	77542.109255	36.811290
1597.710829	77625.754385	36.816308
1599.343060	77705.802175	36.821325
1601.513828	77772.337657	36.826343
1602.795515	77848.526266	36.831360
1604.925190	77921.478653	36.836378
1606.259619	77981.000657	36.841396
1607.473444	78050.334253	36.846413
1609.776045	78130.481060	36.851431
1611.002689	78207.832102	36.856448
1612.579306	78270.901979	36.861466
1614.191315	78356.731625	36.866484
1615.603553	78426.681209	36.871501
1617.653755	78495.517646	36.876519
1618.684883	78577.422981	36.881536
1620.839751	78652.045618	36.886554
1622.340159	78723.743090	36.891572
1623.660704	78806.959352	36.896589
1625.371153	78882.703667	36.901607
1626.817763	78955.613687	36.906624
1628.779953	79039.515689	36.911642
1630.376360	79104.231318	36.916660
1631.961750	79185.405605	36.921677
1633.393430	79261.549317	36.926695
1634.772136	79341.084121	36.931712
1636.559406	79418.540853	36.936730
1638.745398	79506.729350	36.941748
1640.204077	79571.644996	36.946765
1642.136062	79642.517171	36.951783
1643.570420	79716.469976	36.956800
1645.223062	79789.210590	36.961818
1647.104359	79867.591376	36.966836
1648.487718	79947.925349	36.971853
1650.398037	80011.428411	36.976871
1651.599529	80082.264007	36.981888
1653.271449	80129.512037	36.986906
1654.429706	80184.695483	36.991924
1655.744364	80243.477978	36.996941
1657.525238	80310.828111	37.001959
1658.769763	80386.206035	37.006976
1660.352331	80454.512415	37.011994
1661.659865	80534.517876	37.017012
1663.145244	80620.513727	37.022029
1664.857410	80704.282526	37.027047
1666.709451	80786.369976	37.032064
1668.661169	80862.259316	37.037082
1670.273766	80949.984673	37.042100
1671.725597	81042.854006	37.047117
1673.509544	81115.552198	37.052135
1675.144392	81211.877613	37.057152
1676.782005	81292.783814	37.062170
1678.680873	81379.300096	37.067188
1680.231120	81471.179870	37.072205
1682.199457	81567.124897	37.077223
1683.860590	81654.566125	37.082240
1685.567252	81737.629361	37.087258
1687.744743	81822.342278	37.092276
1689.322319	81912.736828	37.097293
1691.420585	81990.430775	37.102311
1692.455944	82082.760559	37.107328
1694.356942	82175.233916	37.112346
1696.286510	82254.576774	37.117364
1697.724633	82347.655284	37.122381
1699.612918	82429.868572	37.127399
1701.457258	82521.541032	37.132416
1703.093081	82610.775702	37.137434
1705.045736	82698.871415	37.142452
1707.060920	82785.690574	37.147469
1709.008141	82873.090806	37.152487
1710.465520	82955.867208	37.157504
1712.126008	83043.781649	37.162522
1714.056655	83123.468882	37.167540
1715.590356	83204.156087	37.172557
1717.273569	83292.409848	37.177575
1719.151935	83370.686844	37.182592
1721.076332	83461.285475	37.187610
1723.177793	83530.240348	37.192628
1724.709601	83617.872604	37.197645
1726.321012	83698.967188	37.202663
1727.925104	83779.201528	37.207680
1729.916386	83863.835661	37.212698
1731.725459	83937.778937	37.217716
1733.309588	84037.327658	37.222733
1734.885258	84110.699701	37.227751
1736.716255	84197.805416	37.232768
1738.634098	84288.052910	37.237786
1740.294290	84356.331244	37.242804
1741.875392	84440.511761	37.247821
1743.801227	84521.774883	37.252839
1745.684026	84609.367921	37.257856
1747.149664	84680.046997	37.262874
1749.276217	84764.916053	37.267892
1751.048160	84845.329855	37.272909
1752.720478	84922.338200	37.277927
1754.317658	84998.712268	37.282944
1756.164181	85086.173051	37.287962
1757.869992	85163.126114	37.292980
1759.629695	85244.024463	37.297997
1761.221767	85321.667339	37.303015
1763.211856	85404.177386	37.308032
1764.748393	85481.677325	37.313050
1766.570183	85550.224656	37.318068
1768.262212	85628.613015	37.323085
1769.934872	85685.817502	37.328103
1771.833083	85751.704964	37.333120
1772.892760	85823.426100	37.338138
1774.502281	85879.753829	37.343156
1775.999564	85968.222324	37.348173
1777.717040	86049.788474	37.353191
1779.756477	86129.251620	37.358208
1780.847372	86209.357629	37.363226
1783.004919	86294.200992	37.368244
1784.624763	86382.233394	37.373261
1786.379119	86465.670400	37.378279
1788.186614	86552.850269	37.383296
1789.676520	86653.259118	37.388314
1791.760323	86739.559945	37.393332
1793.392954	86844.002210	37.398349
1795.095939	86939.322483	37.403367
1797.253611	87031.555906	37.408384
1798.973275	87125.074708	37.413402
1800.719791	87224.013387	37.418420
1802.206827	87322.156626	37.423437
1804.344177	87419.387389	37.428455
1806.645134	87520.736781	37.433472
1808.156079	87613.858942	37.438490
1809.913985	87720.806568	37.443508
1811.766422	87824.216796	37.448525
1813.917292	87933.004596	37.453543
1815.776231	88025.211859	37.458560
1817.636731	88120.802796	37.463578
1819.708643	88219.820637	37.468596
1821.231574	88320.660901	37.473613
1823.289495	88417.970762	37.478631
1825.196912	88521.678983	37.483648
1827.267037	88620.546374	37.488666
1829.110906	88716.826185	37.493684
1831.031896	88814.640356	37.498701
1832.808529	88897.916044	37.503719
1834.647876	88997.302385	37.508736
1836.343923	89094.265560	37.513754
1838.507221	89194.260873	37.518772
1840.351048	89291.264931	37.523789
1841.965062	89379.383261	37.528807
1843.927408	89479.296920	37.533824
1845.879130	89575.904823	37.538842
1848.294111	89670.640919	37.543860
1849.864386	89769.565012	37.548877
1851.288190	89870.223278	37.553895
1853.677247	89960.845462	37.558912
1854.784398	90060.603404	37.563930
1856.918347	90166.195630	37.568948
1858.719156	90266.732866	37.573965
1860.664337	90359.884415	37.578983
1862.956973	90452.424238	37.584000
1864.886149	90549.190903	37.589018
1866.310238	90641.727813	37.594036
1868.146062	90753.959159	37.599053
1870.308562	90838.979579	37.604071
1872.404095	90950.968238	37.609088
1874.048881	91031.570959	37.614106
1876.437846	91131.981035	37.619124
1877.789426	91221.692089	37.624141
1879.459350	91312.088693	37.629159
1881.544434	91410.215211	37.634176
1883.333043	91517.906769	37.639194
1885.526299	91606.473322	37.644212
1887.245462	91698.637773	37.649229
1889.017262	91793.874128	37.654247
1890.935182	91882.585970	37.659264
1892.508682	91966.675117	37.664282
1894.573771	92032.132215	37.669300
1896.249596	92113.163896	37.674317
1898.143421	92200.574972	37.679335
1899.760782	92289.411085	37.684352
1901.154990	92374.023723	37.689370
1903.031462	92459.980686	37.694388
1904.536015	92555.704861	37.699405
1906.374389	92648.005637	37.704423
1908.336109	92759.071323	37.709440
1909.959129	92869.556675	37.714458
1912.332431	92964.601177	37.719476
1914.015497	93074.608906	37.724493
1915.591868	93180.945332	37.729511
1917.998328	93287.063510	37.734528
1919.634893	93402.555268	37.739546
1921.919842	93515.702521	37.744564
1923.459805	93627.648558	37.749581
1925.283079	93744.024990	37.754599
1927.539821	93851.993769	37.759616
1929.195896	93976.534705	37.764634
1931.237894	94088.492587	37.769652
1933.176885	94201.481018	37.774669
1935.329048	94317.212411	37.779687
1937.410485	94435.021397	37.784704
1939.872052	94545.837875	37.789722
1942.147684	94659.954125	37.794740
1944.190916	94768.415839	37.799757
1946.221616	94874.357452	37.804775
1948.232757	94981.037674	37.809792
1950.025460	95090.376308	37.814810
1951.883275	95195.572854	37.819828
1954.023760	95311.753440	37.824845
1955.895913	95422.449793	37.829863
1958.062283	95534.000488	37.834880
1959.893973	95651.016562	37.839898
1962.213093	95749.411890	37.844916
1964.109785	95875.076305	37.849933
1965.712005	95984.042248	37.854951
1968.053957	96095.618179	37.859968
1969.662759	96217.386753	37.864986
1971.640884	96323.227432	37.870004
1973.663050	96439.887070	37.875021
1975.514593	96559.362619	37.880039
1977.464386	96679.672562	37.885056
1979.408349	96805.206542	37.890074
1981.280344	96921.878789	37.895092
1983.099320	97048.345996	37.900109
1984.934472	97173.581556	37.905127
1987.040195	97290.484800	37.910144
1989.132991	97426.811074	37.915162
1991.250600	97550.254555	37.920180
1992.977046	97675.445726	37.925197
1994.865923	97810.854806	37.930215
1997.082260	97928.237489	37.935232
1999.033708	98066.819750	37.940250
2000.742571	98188.453491	37.945268
2002.728467	98320.819775	37.950285
2004.654924	98444.296637	37.955303
2006.546039	98587.974090	37.960320
2008.226823	98717.968439	37.965338
2010.332348	98866.418225	37.970356
2012.675135	98995.511454	37.975373
2014.509652	99131.200860	37.980391
2016.427245	99270.909238	37.985408
2018.595414	99401.768220	37.990426
2020.519819	99545.203879	37.995444
2022.748179	99666.318233	38.000461
2024.568984	99789.461833	38.005479
2026.094887	99907.378163	38.010496
2027.994244	100034.985601	38.015514
2029.792106	100151.427694	38.020532
2031.689145	100283.308857	38.025549
2033.524957	100420.220545	38.030567
2035.291248	100545.923790	38.035584
2037.272897	100687.479234	38.040602
2039.174917	100819.475896	38.045620
2041.502505	100964.097193	38.050637
2043.402934	101111.017308	38.055655
2045.455709	101262.503728	38.060672
2047.303931	101413.287521	38.065690
2049.346992	101567.008233	38.070708
2051.467758	101717.814175	38.075725
2053.565042	101878.488251	38.080743
2055.630600	102023.624330	38.085760
2057.986725	102184.551006	38.090778
2060.189031	102331.835068	38.095796
2062.065908	102486.486258	38.100813
2064.160801	102646.986957	38.105831
2066.307846	102792.633497	38.110848
2068.711021	102959.921307	38.115866
2070.845310	103120.380101	38.120884
2072.835380	103282.092089	38.125901
2075.031599	103442.314528	38.130919
2077.128223	103578.032100	38.135936
2079.469626	103743.862757	38.140954
2081.452350	103900.139572	38.145972
2083.707670	104063.297308	38.150989
2085.292739	104213.260170	38.156007
2087.879599	104380.374223	38.161024
2089.881980	104537.246864	38.166042
2092.256063	104706.272380	38.171060
2094.676196	104856.259611	38.176077
2096.468382	105019.824127	38.181095
2098.850535	105187.988589	38.186112
2100.993943	105339.504783	38.191130
2102.997047	105497.789227	38.196148
2104.886963	105663.902876	38.201165
2106.983964	105820.234126	38.206183
2109.352969	105981.684264	38.211200
2111.648638	106144.275161	38.216218
2113.641138	106310.160359	38.221236
2115.444962	106472.398655	38.226253
2117.751576	106639.161953	38.231271
2120.130624	106785.968747	38.236288
2121.884761	106953.948560	38.241306
2123.880320	107120.838954	38.246324
2126.273794	107291.649547	38.251341
2128.480096	107449.315274	38.256359
2130.798231	107606.735977	38.261376
2132.867794	107776.154075	38.266394
2134.704704	107941.272625	38.271412
2136.787018	108099.962495	38.276429
2139.083811	108282.979277	38.281447
2141.503035	108434.630868	38.286464
2143.672773	108596.200559	38.291482
2146.012106	108755.220960	38.296500
2148.232915	108910.671911	38.301517
2150.195957	109070.538847	38.306535
2152.511663	109223.820568	38.311552
2154.567300	109394.757789	38.316570
2156.633410	109546.951353	38.321588
2158.778928	109708.466577	38.326605
2160.667330	109873.066292	38.331623
2162.695682	110041.271762	38.336640
2164.978586	110194.334592	38.341658
2167.144286	110348.938205	38.346676
2169.326090	110486.508635	38.351693
2171.084677	110632.211321	38.356711
2172.833204	110775.164260	38.361728
2174.548487	110940.988116	38.366746
2176.393301	111090.217395	38.371764
2178.837294	111249.854112	38.376781
2180.427348	111419.047794	38.381799
2182.558775	111591.543660	38.386816
2184.810568	111759.747689	38.391834
2186.687327	111943.813052	38.396852
2188.865297	112123.621763	38.401869
2190.832921	112311.441394	38.406887
2193.125434	112495.203577	38.411904
2195.536522	112677.844783	38.416922
2197.273123	112871.448578	38.421940
2199.940773	113055.383208	38.426957
2201.704367	113257.317229	38.431975
2203.974529	113452.755720	38.436992
2206.483017	113652.647643	38.442010
2208.533890	113857.583898	38.447028
2210.432559	114055.772491	38.452045
2213.124837	114260.395051	38.457063
2215.344923	114461.160915	38.462080
2217.487475	114657.982903	38.467098
2219.415658	114879.875922	38.472116
2222.135325	115075.354228	38.477133
2224.121945	115281.614862	38.482151
2226.788381	115486.425859	38.487168
2229.166735	115690.839143	38.492186
2231.695992	115902.573664	38.497204
2234.122224	116085.267566	38.502221
2236.525547	116299.573438	38.507239
2238.878117	116505.212860	38.512256
2241.240914	116696.506522	38.517274
2242.946801	116900.917502	38.522292
2245.473487	117103.019560	38.527309
2247.721699	117316.137871	38.532327
2249.947273	117530.922536	38.537344
2252.663923	117728.089524	38.542362
2254.525540	117926.888037	38.547380
2257.071002	118125.022503	38.552397
2259.213075	118338.416872	38.557415
2261.580160	118538.052778	38.562432
2263.790137	118745.439114	38.567450
2265.578311	118959.907085	38.572468
2268.562832	119151.382278	38.577485
2270.542489	119368.625867	38.582503
2272.736361	119574.700018	38.587520
2275.022049	119783.970152	38.592538
2277.269250	119994.173437	38.597556
2279.422316	120210.671614	38.602573
2281.540142	120420.301266	38.607591
2284.206353	120641.820929	38.612608
2286.492729	120848.686560	38.617626
2288.679386	121047.932422	38.622644
2291.161152	121263.218008	38.627661
2293.387034	121488.325183	38.632679
2295.342511	121709.467375	38.637696
2297.567697	121916.170635	38.642714
2299.819870	122140.731964	38.647732
2302.076514	122355.969966	38.652749
2304.522691	122574.021077	38.657767
2306.224775	122800.131062	38.662784
2308.915314	123024.260944	38.667802
2311.195257	123260.140014	38.672820
2313.191108	123469.652784	38.677837
2315.265292	123681.247590	38.682855
2317.587769	123894.047907	38.687872
2319.931956	124088.565228	38.692890
2321.682513	124302.332525	38.697908
2324.169317	124510.543366	38.702925
2326.866336	124719.610439	38.707943
2328.337129	124937.306884	38.712960
2330.685839	125152.012700	38.717978
2332.514037	125379.792096	38.722996
2334.944232	125600.729312	38.728013
2336.975261	125835.089246	38.733031
2339.049188	126073.655815	38.738048
2341.806817	126311.989945	38.743066
2343.607127	126565.915185	38.748084
2345.448466	126812.210692	38.753101
2347.954509	127063.427756	38.758119
2350.300060	127326.013755	38.763136
2352.470817	127579.684268	38.768154
2354.935516	127847.596239	38.773172
2357.271510	128113.893391	38.778189
2359.711341	128373.705389	38.783207
2362.479904	128653.907195	38.788224
2364.754812	128912.796758	38.793242
2367.129912	129174.222462	38.798260
2369.482223	129446.247641	38.803277
2372.098928	129717.268924	38.808295
2374.530392	129977.751856	38.813312
2377.415395	130254.329963	38.818330
2379.869266	130519.012423	38.823348
2382.336147	130798.400079	38.828365
2384.898323	131062.891309	38.833383
2387.621223	131322.664332	38.838400
2390.231983	131575.782353	38.843418
2392.261927	131843.330697	38.848436
2395.004015	132116.847103	38.853453
2397.317742	132378.466841	38.858471
2399.863974	132636.740015	38.863488
2402.412447	132909.631846	38.868506
2404.938159	133180.524087	38.873524
2407.444640	133439.759852	38.878541
2409.963198	133704.756061	38.883559
2412.242319	133965.857686	38.888576
2414.954015	134218.949751	38.893594
2417.462474	134470.158967	38.898612
2419.792648	134738.794530	38.903629
2422.253755	134998.731673	38.908647
2424.582828	135271.849943	38.913664
2427.405025	135532.304697	38.918682
2429.669360	135793.964902	38.923700
2431.911168	136050.541572	38.928717
2434.409667	136320.378394	38.933735
2436.870740	136585.514735	38.938752
2439.402451	136846.606168	38.943770
2442.254054	137123.968351	38.948788
2444.543226	137376.547682	38.953805
2447.249347	137647.311558	38.958823
2449.470344	137911.731663	38.963840
2451.868372	138157.508958	38.968858
2454.219722	138425.299880	38.973876
2456.883424	138696.787142	38.978893
2459.053367	138962.705946	38.983911
2461.133848	139222.815281	38.988928
2463.502160	139494.124909	38.993946
2465.903694	139754.009269	38.998964
2467.861202	140021.325146	39.003981
2470.709426	140302.818446	39.008999
2473.314692	140584.732132	39.014016
2475.907590	140851.204482	39.019034
2477.933152	141119.810310	39.024052
2480.129426	141370.331463	39.029069
2482.590233	141623.744192	39.034087
2484.341230	141897.156463	39.039104
2487.017776	142153.304891	39.044122
2489.095449	142420.932511	39.049140
2490.830131	142689.008676	39.054157
2493.438496	142963.536533	39.059175
2495.397973	143257.344424	39.064192
2497.554554	143537.010076	39.069210
2500.052768	143846.335241	39.074228
2502.276261	144139.878581	39.079245
2504.728194	144442.335694	39.084263
2507.153481	144763.519461	39.089280
2509.283939	145077.948440	39.094298
2511.665900	145396.731502	39.099316
2513.828057	145725.780870	39.104333
2516.615794	146065.967185	39.109351
2519.024810	146395.756463	39.114368
2521.736972	146734.004380	39.119386
2524.240481	147074.064098	39.124404
2526.193232	147417.893051	39.129421
2529.455759	147758.638134	39.134439
2531.568838	148118.718667	39.139456
2534.551646	148460.629011	39.144474
2536.827161	148820.638136	39.149492
2539.799310	149167.581111	39.154509
2542.474670	149517.682577	39.159527
2545.073744	149880.161452	39.164544
2547.543392	150233.143021	39.169562
2550.370042	150583.075402	39.174580
2553.219618	150933.996530	39.179597
2556.430062	151273.312330	39.184615
2559.085790	151620.713973	39.189632
2561.942353	151953.590172	39.194650
2564.824636	152296.593978	39.199668
2567.627375	152639.434619	39.204685
2569.949843	152975.611998	39.209703
2572.442641	153321.907252	39.214720
2575.122853	153664.951009	39.219738
2577.636406	154018.368647	39.224756
2580.050957	154366.345427	39.229773
2582.421379	154709.977064	39.234791
2584.902337	155059.496348	39.239808
2587.574479	155419.029159	39.244826
2589.976504	155774.125258	39.249844
2592.114754	156131.130875	39.254861
2594.816118	156493.915525	39.259879
2597.638416	156867.804110	39.264896
2600.315951	157232.501212	39.269914
2602.599468	157596.284653	39.274932
2604.663124	157977.179478	39.279949
2607.377067	158350.675298	39.284967
2610.020199	158733.350400	39.289984
2612.552997	159109.837169	39.295002
2614.901317	159495.026004	39.300020
2617.202044	159881.913164	39.305037
2619.666942	160270.529022	39.310055
2622.251988	160673.576052	39.315072
2624.667353	161060.046282	39.320090
2627.416528	161458.070545	39.325108
2629.877400	161863.670995	39.330125
2632.932173	162253.552470	39.335143
2635.208771	162664.887228	39.340160
2637.570303	163061.471190	39.345178
2640.357939	163466.979754	39.350196
2643.024433	163872.293921	39.355213
2645.376554	164274.904640	39.360231
2647.875274	164682.382947	39.365248
2650.407385	165061.266145	39.370266
2652.968492	165456.728548	39.375284
2655.327240	165845.470320	39.380301
2658.029532	166223.800100	39.385319
2660.520549	166621.032307	39.390336
2663.131452	167021.142896	39.395354
2665.990026	167419.820377	39.400372
2668.346195	167824.444673	39.405389
2670.850378	168227.676845	39.410407
2673.065683	168642.967903	39.415424
2675.876668	169059.145863	39.420442
2678.545006	169485.176166	39.425460
2681.394226	169903.028996	39.430477
2683.987295	170331.590045	39.435495
2686.098468	170764.838108	39.440512
2688.541326	171201.084200	39.445530
2691.246164	171644.592948	39.450548
2693.856802	172099.813558	39.455565
2696.376163	172553.095692	39.460583
2698.699186	173021.318417	39.465600
2701.443179	173480.399113	39.470618
2704.808524	173940.350344	39.475636
2707.103851	174420.851939	39.480653
2710.211483	174881.686965	39.485671
2712.645413	175352.026638	39.490688
2715.306774	175831.196825	39.495706
2718.176082	176302.718268	39.500724
2720.778020	176779.566730	39.505741
2723.718345	177253.952256	39.510759
2726.502861	177750.587248	39.515776
2729.230152	178233.494156	39.520794
2732.185066	178724.901665	39.525812
2734.614465	179212.686080	39.530829
2737.437384	179696.982946	39.535847
2740.378130	180199.652001	39.540864
2742.862304	180707.246258	39.545882
2745.941847	181202.914704	39.550900
2748.288912	181711.856635	39.555917
2751.462312	182201.140757	39.560935
2754.426464	182731.986642	39.565952
2757.057999	183283.282578	39.570970
2760.179265	183786.120394	39.575988
2762.296935	184291.352843	39.581005
2765.440304	184787.436178	39.586023
2768.207828	185305.449393	39.591040
2770.803339	185810.436910	39.596058
2773.656887	186324.733508	39.601076
2776.725920	186825.105390	39.606093
2779.824662	187341.578347	39.611111
2782.415910	187853.688195	39.616128
2785.066213	188367.391398	39.621146
2787.763207	188875.349283	39.626164
2790.363769	189407.200645	39.631181
2793.265777	189912.743512	39.636199
2796.469324	190434.294438	39.641216
2798.919971	190951.520357	39.646234
2801.858517	191472.685501	39.651252
2804.116429	191994.924565	39.656269
2807.201845	192516.426809	39.661287
2809.916001	193038.395709	39.666304
2812.663054	193558.812152	39.671322
2815.968055	194084.477660	39.676340
2818.542401	194612.342444	39.681357
2821.301471	195129.791302	39.686375
2824.251491	195660.802005	39.691392
2827.304833	196182.958878	39.696410
2830.199222	196696.226599	39.701428
2832.993195	197217.056157	39.706445
2835.895178	197702.308242	39.711463
2839.422596	198163.764202	39.716480
2842.511833	198651.911291	39.721498
2845.610328	199108.636237	39.726516
2847.898721	199595.285818	39.731533
2850.500540	200064.766831	39.736551
2853.086271	200545.682708	39.741568
2855.596448	201027.754901	39.746586
2858.370772	201523.606035	39.751604
2860.659590	202028.806409	39.756621
2863.191248	202518.423927	39.761639
2865.852425	203045.669118	39.766656
2868.095672	203568.484912	39.771674
2870.764359	204097.332268	39.776692
2872.880608	204647.910631	39.781709
2875.542738	205191.749602	39.786727
2878.162207	205756.808127	39.791744
2881.208660	206312.732532	39.796762
2884.319119	206880.384564	39.801780
2886.729192	207461.179371	39.806797
2889.595094	208028.948738	39.811815
2892.507598	208612.894033	39.816832
2895.022632	209215.574294	39.821850
2897.787282	209810.900774	39.826868
2900.808926	210408.423898	39.831885
2903.741089	211005.454240	39.836903
2906.658992	211617.222091	39.841920
2909.793257	212236.146560	39.846938
2912.773651	212847.170380	39.851956
2915.413485	213462.795845	39.856973
2918.472674	214067.357013	39.861991
2921.764482	214696.041761	39.867008
2924.346530	215332.078603	39.872026
2927.342177	215959.922516	39.877044
2930.233131	216590.781350	39.882061
2933.412387	217219.436605	39.887079
2936.257598	217851.752230	39.892096
2939.268803	218491.384357	39.897114
2942.748274	219122.890866	39.902132
2945.333204	219759.847297	39.907149
2948.133871	220400.073052	39.912167
2951.727083	221041.293125	39.917184
2954.469060	221680.233353	39.922202
2957.815692	222313.363459	39.927220
2960.848446	222962.674521	39.932237
2963.730908	223602.914657	39.937255
2966.465044	224243.152744	39.942272
2969.046278	224893.398646	39.947290
2972.237277	225545.048063	39.952308
2975.072808	226197.083287	39.957325
2977.986067	226855.152424	39.962343
2981.370396	227504.865990	39.967360
2984.006768	228168.490691	39.972378
2987.228782	228817.644796	39.977396
2990.586089	229474.017521	39.982413
2993.330604	230129.901331	39.987431
2996.803102	230784.349773	39.992448
2999.796630	231439.660053	39.997466
3002.473256	232094.485752	40.002484
3005.511851	232763.124658	40.007501
3008.324780	233424.100651	40.012519
3011.497693	234084.663816	40.017536
3013.711929	234749.872422	40.022554
3016.877699	235414.499330	40.027572
3019.655611	236093.792926	40.032589
3022.784015	236755.247910	40.037607
3025.963372	237429.471711	40.042624
3028.829701	238104.937070	40.047642
3031.753563	238734.868888	40.052660
3034.497061	239381.035006	40.057677
3037.471460	240024.648629	40.062695
3040.938854	240666.684858	40.067712
3043.650558	241314.223195	40.072730
3046.307476	241952.496270	40.077748
3049.764246	242607.434078	40.082765
3052.551432	243269.206578	40.087783
3055.486148	243932.884698	40.092800
3057.998366	244605.695708	40.097818
3061.022500	245267.806132	40.102836
3063.773138	245945.732277	40.107853
3066.401880	246634.014033	40.112871
3069.989573	247317.824911	40.117888
3072.400785	248026.381416	40.122906
3075.552259	248717.317127	40.127924
3079.143317	249421.669952	40.132941
3081.688138	250134.134313	40.137959
3085.230465	250837.218650	40.142976
3088.006142	251567.396615	40.147994
3091.186049	252271.471075	40.153012
3094.986252	252990.533855	40.158029
3098.111765	253711.603735	40.163047
3101.349771	254437.021441	40.168064
3104.417990	255164.367026	40.173082
3107.425370	255889.330533	40.178100
3110.652452	256619.564549	40.183117
3113.845345	257345.354655	40.188135
3116.978324	258079.938635	40.193152
3119.940175	258807.813877	40.198170
3123.651564	259547.658154	40.203188
3126.794841	260279.356977	40.208205
3129.465015	261018.643609	40.213223
3132.937732	261751.653170	40.218240
3136.073590	262505.462203	40.223258
3139.054493	263259.264875	40.228276
3142.175853	263990.180820	40.233293
3145.503900	264742.928108	40.238311
3148.672934	265497.701297	40.243328
3151.865359	266246.623469	40.248346
3154.961877	267003.352388	40.253364
3157.796605	267766.135812	40.258381
3160.911184	268528.640828	40.263399
3163.894808	269297.814438	40.268416
3166.702834	270076.076140	40.273434
3169.684043	270857.224831	40.278452
3172.969289	271641.011279	40.283469
3175.858293	272431.328972	40.288487
3179.247683	273218.996108	40.293504
3182.206212	274020.742285	40.298522
3185.343675	274811.303761	40.303540
3188.770892	275602.726598	40.308557
3192.382703	276397.744456	40.313575
3196.067869	277179.105431	40.318592
3198.930121	277991.544333	40.323610
3202.336837	278774.101042	40.328628
3205.829600	279567.124352	40.333645
3208.790786	280358.368596	40.338663
3212.363072	281149.838953	40.343680
3215.162411	281939.212296	40.348698
3218.423015	282733.126525	40.353716
3221.351942	283521.547944	40.358733
3224.383243	284333.814101	40.363751
3228.016919	285126.500142	40.368768
3230.999831	285932.381302	40.373786
3233.939293	286734.907806	40.378804
3237.676577	287531.028025	40.383821
3240.664648	288327.788934	40.388839
3244.183604	289096.856574	40.393856
3247.178194	289865.159033	40.398874
3250.242820	290637.732228	40.403892
3253.347861	291394.750569	40.408909
3256.579809	292163.089165	40.413927
3259.692913	292930.268722	40.418944
3262.863128	293709.337253	40.423962
3266.339472	294479.334573	40.428980
3269.530263	295258.328728	40.433997
3272.603751	296052.183065	40.439015
3275.806563	296830.824134	40.444032
3279.097767	297624.851119	40.449050
3282.197349	298419.861593	40.454068
3285.889818	299214.615698	40.459085
3289.114602	300018.443737	40.464103
3292.868024	300808.900228	40.469120
3296.193690	301615.455927	40.474138
3299.527797	302418.291827	40.479156
3303.177951	303223.630008	40.484173
3306.057561	304042.225563	40.489191
3308.876156	304848.227063	40.494208
3311.939130	305687.938322	40.499226
3314.848696	306504.281423	40.504244
3318.718083	307329.852918	40.509261
3321.672653	308187.662808	40.514279
3325.177506	309025.472014	40.519296
3328.456112	309872.591899	40.524314
3331.417171	310722.969961	40.529332
3334.585212	311578.478193	40.534349
3337.849222	312438.625911	40.539367
3341.146035	313310.655864	40.544384
3344.234353	314186.001309	40.549402
3347.911439	315068.826287	40.554420
3351.424761	315948.106698	40.559437
3354.880525	316831.363236	40.564455
3358.268560	317711.110732	40.569472
3361.871523	318602.784981	40.574490
3364.941290	319486.403911	40.579508
3368.377276	320372.358231	40.584525
3372.006412	321269.479942	40.589543
3375.641315	322151.737488	40.594560
3379.194386	323043.910663	40.599578
3382.524897	323930.948643	40.604596
3386.392550	324822.882100	40.609613
3389.489219	325725.725395	40.614631
3392.550628	326611.377181	40.619648
3396.211867	327503.537632	40.624666
3399.863147	328410.547030	40.629684
3403.610152	329293.215793	40.634701
3406.591402	330200.542333	40.639719
3410.243091	331097.595151	40.644736
3413.574033	331993.637076	40.649754
3416.661868	332909.026377	40.654772
3419.958665	333796.203038	40.659789
3423.052499	334712.866652	40.664807
3426.446685	335624.666506	40.669824
3430.291966	336550.197496	40.674842
3433.050471	337462.989607	40.679860
3436.503827	338395.992226	40.684877
3439.447127	339327.300297	40.689895
3442.991673	340254.736344	40.694912
3446.026393	341204.343649	40.699930
3449.349120	342146.880444	40.704948
3452.473490	343080.064569	40.709965
3456.040114	344029.105872	40.714983
3459.335641	344985.542856	40.720000
3462.943124	345940.129031	40.725018
3466.501548	346874.792967	40.730023
3469.911546	347783.318880	40.735028
3472.886233	348650.374662	40.740032
3476.158704	349460.062430	40.745037
3479.675670	350210.843981	40.750042
3482.593402	350927.003949	40.755047
3485.317691	351577.495063	40.760052
3488.085512	352186.355748	40.765056
3490.929492	352735.434538	40.770061
3493.774012	353216.358377	40.775066
3496.081277	353649.345138	40.780071
3498.018361	354031.650998	40.785076
3499.993400	354378.210010	40.790080
3502.124743	354686.081913	40.795085
3504.227423	354930.083541	40.800090
3506.013726	355153.570891	40.805095
3507.683354	355310.382727	40.810100
3508.884504	355458.650951	40.815104
3510.352525	355551.190235	40.820109
3511.929614	355606.172778	40.825114
3512.791319	355648.330338	40.830119
3514.068198	355646.072096	40.835124
3514.765062	355625.401699	40.840128
3515.841420	355575.850196	40.845133
3516.721185	355505.157759	40.850138
3517.317106	355415.981164	40.855143
3518.252253	355306.062464	40.860148
3518.537453	355182.367667	40.865152
3519.228891	355036.496554	40.870157
3519.751647	354869.479113	40.875162
3519.961707	354701.543834	40.880167
3520.612589	354510.307712	40.885172
3520.623836	354316.933728	40.890176
3521.301792	354112.550345	40.895181
3521.733555	353885.023474	40.900186
3521.922621	353660.506766	40.905191
3521.957698	353415.983345	40.910196
3522.115208	353169.964657	40.915200
3522.124942	352918.553101	40.920205
3522.478785	352654.961201	40.925210
3522.563025	352401.957988	40.930215
3522.749967	352136.329001	40.935220
3522.715006	351853.930543	40.940224
3522.773532	351579.954174	40.945229
3522.919095	351295.895766	40.950234
3522.744892	351016.333293	40.955239
3522.768592	350734.373415	40.960244
3522.999235	350457.233975	40.965248
3522.819385	350168.030849	40.970253
3522.877062	349866.967458	40.975258
3522.977021	349579.037235	40.980263
3522.791164	349282.658542	40.985268
3522.407975	348991.900698	40.990272
3522.459775	348692.123918	40.995277
3522.381939	348386.441419	41.000282
3522.045222	348101.312075	41.005287
3522.550256	347806.617060	41.010292
3522.165345	347510.584063	41.015296
3521.860623	347224.272758	41.020301
3522.060785	346919.118012	41.025306
3521.759615	346634.428158	41.030311
3521.773260	346331.585295	41.035316
3521.527356	346048.890275	41.040320
3521.174763	345756.268890	41.045325
3521.665491	345470.987764	41.050330
3521.330324	345187.129985	41.055335
3521.133372	344891.146227	41.060340
3520.877390	344605.059286	41.065344
3520.906520	344311.374208	41.070349
3520.731597	344028.905513	41.075354
3520.310386	343745.303435	41.080359
3520.401742	343466.729393	41.085364
3520.194875	343191.454201	41.090368
3520.052499	342904.953939	41.095373
3520.046600	342619.396158	41.100378
3519.384716	342357.457861	41.105383
3519.688406	342076.398512	41.110388
3519.315029	341826.234408	41.115392
3519.343761	341543.815291	41.120397
3519.372076	341277.057013	41.125402
3519.132210	341015.449505	41.130407
3519.114743	340748.668946	41.135412
3518.912533	340478.914793	41.140416
3518.696004	340216.865441	41.145421
3518.532384	339955.416150	41.150426
3518.343489	339693.053470	41.155431
3518.268098	339435.705925	41.160436
3517.688607	339199.159582	41.165440
3517.185103	338945.842283	41.170445
3517.412673	338694.900928	41.175450
3517.094089	338449.434163	41.180455
3517.224378	338200.284596	41.185460
3516.843173	337970.158174	41.190464
3516.752915	337728.592359	41.195469
3516.387820	337482.821135	41.200474
3516.202531	337261.229395	41.205479
3516.289709	337038.118765	41.210484
3516.156030	336804.894648	41.215488
3516.251273	336577.863690	41.220493
3516.133753	336348.957298	41.225498
3516.023890	336128.287818	41.230503
3516.029378	335895.849936	41.235508
3515.698132	335681.824404	41.240512
3515.318966	335457.225770	41.245517
3515.173396	335246.042401	41.250522
3515.156417	335026.267333	41.255527
3514.944914	334815.244406	41.260532
3514.888612	334599.974351	41.265536
3514.658899	334386.993600	41.270541
3514.621955	334188.833790	41.275546
3514.116129	333983.803259	41.280551
3514.350606	333774.866457	41.285556
3513.957654	333575.233122	41.290560
3514.024856	333375.501354	41.295565
3514.300929	333182.806160	41.300570
3513.780191	332984.054380	41.305575
3513.846609	332780.657261	41.310580
3513.568335	332596.769250	41.315584
3513.367206	332397.277730	41.320589
3513.463262	332203.512071	41.325594
3513.251006	332026.274514	41.330599
3513.360619	331828.944147	41.335604
3513.191671	331642.719980	41.340608
3512.946695	331456.786566	41.345613
3512.957764	331268.141654	41.350618
3512.687150	331089.001334	41.355623
3512.599105	330907.567993	41.360628
3512.588140	330734.209862	41.365632
3512.250288	330558.714697	41.370637
3512.672826	330387.957856	41.375642
3512.057146	330211.639778	41.380647
3512.087185	330036.517121	41.385652
3511.988602	329858.717685	41.390656
3511.994086	329700.435250	41.395661
3512.087406	329519.119669	41.400666
3511.820364	329366.855739	41.405671
3511.517429	329199.157590	41.410676
3511.396525	329029.369995	41.415680
3511.388067	328871.060949	41.420685
3511.425733	328699.873621	41.425690
3511.118804	328545.399838	41.430695
3510.905902	328375.572933	41.435700
3510.723696	328229.828348	41.440704
3510.638740	328081.473547	41.445709
3510.644395	327926.338010	41.450714
3510.189943	327787.807354	41.455719
3510.352104	327628.423771	41.460724
3510.313800	327485.324769	41.465728
3509.870458	327343.763894	41.470733
3510.022866	327207.374755	41.475738
3509.749763	327072.476129	41.480743
3510.147384	326921.014593	41.485748
3509.943860	326780.406265	41.490752
3509.970479	326649.631004	41.495757
3509.887892	326511.368464	41.500762
3509.849545	326378.821886	41.505767
3509.708794	326242.627924	41.510772
3509.452440	326109.122491	41.515776
3509.392165	325962.867269	41.520781
3509.574763	325830.640473	41.525786
3509.008222	325707.840509	41.530791
3509.147076	325575.009217	41.535796
3508.828068	325449.066379	41.540800
3508.606138	325328.704287	41.545805
3508.712353	325203.584533	41.550810
3508.624326	325073.585240	41.555815
3508.568789	324964.083497	41.560820
3508.412231	324841.191383	41.565824
3508.448353	324721.066974	41.570829
3508.819955	324598.956459	41.575834
3508.381978	324494.651775	41.580839
3508.247581	324373.662667	41.585844
3508.346258	324264.491083	41.590848
3508.109755	324152.344427	41.595853
3508.225365	324031.111719	41.600858
3507.990817	323920.286933	41.605863
3508.255797	323803.838111	41.610868
3508.039353	323696.927460	41.615872
3507.259425	323597.965235	41.620877
3507.647025	323485.719199	41.625882
3507.539664	323381.309133	41.630887
3507.617286	323270.637316	41.635892
3507.615491	323171.399787	41.640896
3507.323644	323066.152842	41.645901
3507.166122	322960.019696	41.650906
3506.957766	322875.314124	41.655911
3507.220430	322769.598149	41.660916
3506.854979	322666.778443	41.665920
3506.987377	322578.253960	41.670925
3506.723465	322480.811091	41.675930
3506.709681	322391.596761	41.680935
3507.110903	322303.563902	41.685940
3506.828119	322205.487353	41.690944
3506.540518	322117.917951	41.695949
3506.779722	322027.722024	41.700954
3506.694518	321929.588503	41.705959
3506.540463	321839.199257	41.710964
3506.567379	321755.802958	41.715968
3506.594970	321671.058068	41.720973
3506.690267	321584.343536	41.725978
3506.437005	321505.722402	41.730983
3506.208899	321415.165744	41.735988
3506.294275	321317.767340	41.740992
3506.346052	321237.851447	41.745997
3506.216564	321150.662365	41.751002
3506.102247	321068.889536	41.756007
3506.346052	320993.039064	41.761012
3506.051055	320902.822497	41.766016
3505.667263	320823.609934	41.771021
3505.886099	320746.236494	41.776026
3505.832637	320670.966176	41.781031
3505.825682	320591.643388	41.786036
3505.916305	320500.322614	41.791040
3505.823639	320445.893981	41.796045
3505.908389	320361.086664	41.801050
3505.594290	320285.525685	41.806055
3505.510096	320204.560598	41.811060
3505.547916	320139.476877	41.816064
3505.318810	320066.624405	41.821069
3505.703648	319996.525222	41.826074
3505.374701	319931.473084	41.831079
3505.332935	319855.487155	41.836084
3505.222360	319778.443322	41.841088
3505.228222	319717.968809	41.846093
3505.261631	319634.669116	41.851098
3505.225989	319584.809900	41.856103
3505.047120	319510.040538	41.861108
3505.050850	319445.978751	41.866112
3504.808049	319383.074833	41.871117
3505.203136	319313.405443	41.876122
3504.952887	319261.035263	41.881127
3504.799442	319189.492437	41.886132
3504.918981	319120.578178	41.891136
3505.224109	319062.498350	41.896141
3505.256386	318993.673857	41.901146
3504.940376	318935.894500	41.906151
3505.066643	318868.352639	41.911156
3504.645076	318809.750041	41.916160
3504.627793	318751.084160	41.921165
3504.641335	318686.587209	41.926170
3504.838762	318633.713774	41.931175
3504.708223	318570.434943	41.936180
3504.906063	318508.885615	41.941184
3504.510998	318446.996381	41.946189
3504.698348	318376.772806	41.951194
3504.548986	318327.591419	41.956199
3504.685584	318270.783544	41.961204
3504.825466	318210.896591	41.966208
3504.600399	318158.750128	41.971213
3504.573229	318084.972286	41.976218
3504.219222	318041.267191	41.981223
3504.229262	317982.901314	41.986228
3504.210393	317928.279889	41.991232
3503.914034	317885.278009	41.996237
3504.252400	317831.363881	42.001242
3503.860069	317778.836040	42.006247
3503.867783	317728.611733	42.011252
3504.179090	317682.588782	42.016256
3503.906771	317636.860567	42.021261
3504.112584	317592.507771	42.026266
3503.797712	317545.539434	42.031271
3503.860813	317501.412399	42.036276
3504.159673	317454.119032	42.041280
3503.937886	317406.754357	42.046285
3504.175445	317352.982618	42.051290
3504.097896	317308.444856	42.056295
3503.660317	317253.964384	42.061300
3503.662755	317209.057819	42.066304
3503.249598	317172.892136	42.071309
3503.613483	317123.756378	42.076314
3503.639004	317092.865013	42.081319
3503.740295	317034.280075	42.086324
3503.662269	316998.545267	42.091328
3503.420965	316949.224061	42.096333
3503.847164	316915.878308	42.101338
3503.784134	316877.189691	42.106343
3503.861818	316826.571779	42.111348
3503.635384	316787.628758	42.116352
3503.736832	316739.195120	42.121357
3503.689597	316682.871917	42.126362
3503.552514	316646.637200	42.131367
3503.663655	316603.239608	42.136372
3503.579690	316561.068298	42.141376
3503.330097	316526.581199	42.146381
3503.753884	316480.615748	42.151386
3503.397089	316438.130773	42.156391
3503.231368	316399.864886	42.161396
3503.277339	316354.238246	42.166400
3503.103768	316328.186230	42.171405
3503.457475	316287.192952	42.176410
3503.007355	316251.693820	42.181415
3503.298819	316218.317725	42.186420
3503.131223	316169.849203	42.191424
3503.010020	316148.953874	42.196429
3503.243665	316116.960679	42.201434
3502.976909	316081.916169	42.206439
3503.013848	316051.734710	42.211444
3503.246758	316018.596611	42.216448
3503.023243	315990.389524	42.221453
3502.854440	315953.930215	42.226458
3502.855782	315926.044141	42.231463
3502.784753	315888.526314	42.236468
3503.015738	315848.773105	42.241472
3502.925288	315820.443335	42.246477
3502.851316	315790.558919	42.251482
3502.806738	315769.040791	42.256487
3502.881801	315723.663397	42.261492
3503.006224	315691.203549	42.266496
3502.852256	315666.064050	42.271501
3502.611180	315631.116947	42.276506
3502.443394	315614.426838	42.281511
3502.927522	315575.982321	42.286516
3502.806983	315545.036393	42.291520
3502.649012	315528.777259	42.296525
3502.970967	315492.851499	42.301530
3502.664253	315469.694930	42.306535
3502.740535	315440.193890	42.311540
3502.955262	315408.533917	42.316544
3502.583588	315380.985704	42.321549
3502.949202	315344.086139	42.326554
3502.624615	315316.555968	42.331559
3502.691690	315290.643835	42.336564
3502.602874	315263.407540	42.341568
3502.860921	315235.811675	42.346573
3502.900689	315206.952286	42.351578
3502.496639	315182.233273	42.356583
3502.678545	315157.778852	42.361588
3502.697866	315128.820834	42.366592
3502.675137	315111.573541	42.371597
3502.770241	315076.700670	42.376602
3502.589186	315049.046121	42.381607
3502.904248	315018.184394	42.386612
3503.086005	314985.307973	42.391616
3502.473743	314965.353961	42.396621
3502.681900	314926.773932	42.401626
3502.671520	314902.273103	42.406631
3502.421678	314884.857679	42.411636
3502.823946	314853.142555	42.416640
3502.606205	314828.216114	42.421645
3502.761234	314792.977441	42.426650
3502.448740	314777.022079	42.431655
3502.794222	314748.114603	42.436660
3502.575890	314726.114263	42.441664
3502.451459	314702.954249	42.446669
3502.766156	314667.588741	42.451674
3502.387413	314648.946618	42.456679
3502.457157	314626.417754	42.461684
3502.652649	314593.106354	42.466688
3502.245656	314576.020710	42.471693
3502.757318	314540.064538	42.476698
3502.120753	314517.264382	42.481703
3502.325834	314501.406115	42.486708
3502.960070	314481.078904	42.491712
3502.615405	314449.225833	42.496717
3502.710580	314425.547905	42.501722
3502.771880	314398.974617	42.506727
3502.781962	314375.411744	42.511732
3502.629764	314337.141996	42.516736
3502.527709	314315.454055	42.521741
3502.536449	314296.318656	42.526746
3502.362442	314272.886287	42.531751
3502.229746	314245.325467	42.536756
3502.906549	314211.378766	42.541760
3502.366050	314199.657165	42.546765
3502.535635	314170.191603	42.551770
3502.265844	314151.684910	42.556775
3502.096601	314132.679046	42.561780
3502.447479	314106.060316	42.566784
3502.201619	314092.893181	42.571789
3502.188498	314075.618550	42.576794
3502.553607	314053.679338	42.581799
3502.561847	314025.078574	42.586804
3502.382294	314000.527378	42.591808
3502.396354	313974.241118	42.596813
3502.401276	313949.661054	42.601818
3502.495936	313928.756399	42.606823
3502.331719	313909.291655	42.611828
3502.179979	313876.212132	42.616832
3501.905445	313864.576086	42.621837
3501.905290	313850.149131	42.626842
3502.124945	313828.690554	42.631847
3502.470293	313817.491920	42.636852
3502.303513	313789.198263	42.641856
3502.161685	313780.772910	42.646861
3502.199159	313755.627872	42.651866
3502.249955	313729.132173	42.656871
3502.115034	313719.102719	42.661876
3502.466713	313690.880613	42.666880
3502.397530	313677.583959	42.671885
3502.382359	313645.220813	42.676890
3502.289217	313629.256202	42.681895
3502.279082	313614.728954	42.686900
3502.368831	313594.053918	42.691904
3502.238341	313576.034108	42.696909
3502.225941	313546.851046	42.701914
3502.073441	313531.862580	42.706919
3502.041558	313515.481237	42.711924
3502.102507	313493.970982	42.716928
3501.830068	313483.377747	42.721933
3502.130150	313465.901253	42.726938
3502.133249	313434.502003	42.731943
3502.150658	313424.194222	42.736948
3502.400993	313402.425313	42.741952
3502.315235	313391.751982	42.746957
3502.061766	313365.023749	42.751962
3501.954618	313358.755707	42.756967
3501.808219	313333.308402	42.761972
3502.366956	313310.473441	42.766976
3502.210047	313296.452493	42.771981
3502.137811	313267.456723	42.776986
3502.337415	313264.295874	42.781991
3502.129150	313241.351788	42.786996
3502.145251	313221.451445	42.792001
3502.322379	313198.701535	42.797005
3502.184488	313177.171330	42.802010
3502.279156	313161.482534	42.807015
3502.249792	313146.169353	42.812020
3502.223104	313129.863396	42.817025
3502.221177	313102.408673	42.822029
3502.169254	313091.221083	42.827034
3502.322828	313064.123701	42.832039
3502.183042	313049.870995	42.837044
3502.534589	313017.551857	42.842049
3502.111696	313013.953967	42.847053
3502.117774	312989.678551	42.852058
3502.231212	312978.312412	42.857063
3502.010142	312947.838455	42.862068
3501.891571	312930.401766	42.867073
3501.696464	312925.623229	42.872077
3501.794359	312889.526900	42.877082
3501.934400	312878.156577	42.882087
3501.631639	312876.753616	42.887092
3502.047362	312858.241011	42.892097
3501.785886	312843.167579	42.897101
3501.683908	312830.919058	42.902106
3501.693912	312816.235741	42.907111
3501.627248	312797.900309	42.912116
3501.666766	312773.899448	42.917121
3501.333097	312776.750654	42.922125
3501.408055	312762.108056	42.927130
3501.019990	312771.710728	42.932135
3501.434552	312758.134621	42.937140
3501.828465	312738.760243	42.942145
3501.423941	312735.057678	42.947149
3501.461354	312732.710950	42.952154
3501.608040	312734.214802	42.957159
3501.588533	312717.500455	42.962164
3501.449644	312699.710624	42.967169
3501.020268	312694.256224	42.972173
3501.393563	312692.569447	42.977178
3502.058426	312688.597910	42.982183
3501.698717	312687.712750	42.987188
3501.568668	312670.557655	42.992193
3501.620116	312653.221507	42.997197
3501.706328	312649.213208	43.002202
3501.773438	312641.543784	43.007207
3501.273778	312609.204768	43.012212
3501.432173	312597.755172	43.017217
3501.238449	312605.037425	43.022221
3501.392511	312606.616464	43.027226
3501.572949	312599.921679	43.032231
3501.578340	312592.719911	43.037236
3501.833243	312565.301053	43.042241
3501.664975	312561.790546	43.047245
3501.751090	312556.230092	43.052250
3502.030496	312548.705580	43.057255
3501.594602	312524.015559	43.062260
3501.919677	312521.089496	43.067265
3501.678377	312505.783793	43.072269
3501.659746	312480.341492	43.077274
3501.916012	312469.385469	43.082279
3501.562178	312484.657151	43.087284
3502.009630	312452.398964	43.092289
3501.829345	312443.266911	43.097293
3501.549645	312444.582981	43.102298
3501.479598	312426.909509	43.107303
3501.460200	312402.128863	43.112308
3501.531172	312378.886243	43.117313
3501.630273	312393.578235	43.122317
3501.839076	312391.204695	43.127322
3501.621804	312360.984213	43.132327
3501.712926	312353.260098	43.137332
3502.210433	312341.248515	43.142337
3501.889923	312334.352112	43.147341
3501.698381	312313.720483	43.152346
3501.750417	312308.292555	43.157351
3501.538476	312292.702293	43.162356
3501.638796	312272.686597	43.167361
3501.689434	312257.844079	43.172365
3501.463623	312256.912532	43.177370
3501.362280	312255.605289	43.182375
3501.395201	312252.648549	43.187380
3501.703584	312220.310162	43.192385
3501.680110	312224.614186	43.197389
3501.531704	312200.566075	43.202394
3501.811377	312202.100044	43.207399
3501.800308	312197.292660	43.212404
3501.651888	312179.376893	43.217409
3501.742074	312171.780121	43.222413
3501.668998	312166.269955	43.227418
3502.335621	312143.951913	43.232423
3501.992442	312132.682401	43.237428
3501.767937	312109.078714	43.242433
3501.350120	312097.948090	43.247437
3501.449026	312092.970828	43.252442
3501.412952	312080.610025	43.257447
3501.336667	312084.133508	43.262452
3501.830583	312066.219058	43.267457
3501.500156	312061.716043	43.272461
3501.557573	312045.523786	43.277466
3501.507599	312043.521477	43.282471
3501.544198	312046.289393	43.287476
3501.746801	312020.557799	43.292481
3501.878517	312024.964807	43.297485
3501.893164	312016.692790	43.302490
3501.569437	312000.534659	43.307495
3501.563248	311981.604204	43.312500
3501.891670	311965.878462	43.317505
3501.713481	311967.382239	43.322509
3501.583817	311946.842557	43.327514
3501.801142	311920.447021	43.332519
3501.501350	311923.572883	43.337524
3501.519635	311904.536788	43.342529
3501.409050	311917.353291	43.347533
3501.530222	311893.135649	43.352538
3501.693255	311880.260199	43.357543
3501.508311	311879.576710	43.362548
3501.908058	311865.977217	43.367553
3501.398511	311859.517427	43.372557
3501.607439	311843.810326	43.377562
3501.787060	311837.878930	43.382567
3501.727071	311827.124875	43.387572
3501.843810	311813.518720	43.392577
3501.350822	311807.081779	43.397581
3501.607570	311801.265549	43.402586
3501.825563	311790.976940	43.407591
3501.668991	311780.645105	43.412596
3501.700758	311765.169240	43.417601
3501.425773	311749.206968	43.422605
3501.402129	311752.976702	43.427610
3501.685024	311745.451516	43.432615
3501.156012	311730.826683	43.437620
3501.360906	311713.593427	43.442625
3501.374535	311716.950205	43.447629
3501.708918	311716.338198	43.452634
3501.786131	311704.163150	43.457639
3501.600653	311698.441491	43.462644
3501.615730	311672.739025	43.467649
3501.526901	311669.953957	43.472653
3501.285626	311670.297101	43.477658
3501.392596	311667.506868	43.482663
3501.537221	311657.433265	43.487668
3501.513902	311633.517982	43.492673
3501.327971	311633.063657	43.497677
3501.227201	311636.718229	43.502682
3501.024566	311622.576697	43.507687
3501.429525	311622.971485	43.512692
3501.543110	311622.648453	43.517697
3501.609111	311619.813731	43.522701
3501.506550	311602.628501	43.527706
3501.336728	311585.657348	43.532711
3501.526805	311571.021826	43.537716
3501.557575	311572.365718	43.542721
3501.247870	311572.643224	43.547725
3501.212089	311559.696985	43.552730
3501.566166	311547.605842	43.557735
3501.531354	311539.697715	43.562740
3501.636238	311534.973918	43.567745
3501.209790	311542.852527	43.572749
3501.504874	311530.134456	43.577754
3501.463532	311524.822820	43.582759
3501.535291	311502.622922	43.587764
3501.380517	311499.161116	43.592769
3501.623663	311495.255412	43.597773
3501.663547	311488.836903	43.602778
3501.382361	311496.616471	43.607783
3501.565273	311473.635807	43.612788
3501.627734	311461.310328	43.617793
3501.759688	311454.775636	43.622797
3501.821485	311446.394364	43.627802
3501.608553	311426.681741	43.632807
3501.152511	311417.872505	43.637812
3501.397011	311409.513555	43.642817
3501.488508	311408.888624	43.647821
3501.878116	311397.249914	43.652826
3501.881613	311381.625668	43.657831
3501.560814	311372.693496	43.662836
3501.720196	311370.607536	43.667841
3501.381200	311365.800443	43.672845
3501.452997	311333.931017	43.677850
3501.595966	311329.786502	43.682855
3501.239892	311342.565204	43.687860
3501.363269	311333.996163	43.692865
3501.617454	311328.943653	43.697869
3501.265866	311324.901902	43.702874
3501.484937	311295.884815	43.707879
3501.586844	311297.115809	43.712884
3501.546696	311285.925948	43.717889
3501.665304	311293.872059	43.722893
3501.243889	311274.242858	43.727898
3501.744245	311260.016759	43.732903
3501.707197	311247.859457	43.737908
3501.797104	311244.308488	43.742913
3501.861372	311244.069502	43.747917
3501.632977	311219.524476	43.752922
3501.390457	311216.254489	43.757927
3501.435229	311203.550020	43.762932
3501.499206	311195.168362	43.767937
3501.769141	311196.118630	43.772941
3501.602772	311170.495150	43.777946
3501.494629	311155.753447	43.782951
3501.325769	311151.683114	43.787956
3501.696528	311154.195272	43.792961
3501.835723	311146.259875	43.797965
3501.670878	311126.310595	43.802970
3501.926068	311119.247670	43.807975
3501.592423	311115.075865	43.812980
3501.543636	311092.385700	43.817985
3501.737894	311080.726561	43.822989
3501.474932	311072.116089	43.827994
3501.839920	311068.725669	43.832999
3501.699426	311056.762613	43.838004
3501.827274	311040.126418	43.843009
3501.747150	311036.500231	43.848013
3501.650128	311028.296391	43.853018
3501.755847	310998.355339	43.858023
3501.884043	310994.976487	43.863028
3502.044559	310994.111746	43.868033
3501.351837	310965.898605	43.873037
3501.626700	310957.865628	43.878042
3501.818324	310951.474215	43.883047
3501.580286	310949.704830	43.888052
3501.646442	310924.757356	43.893057
3501.723084	310920.699514	43.898061
3501.494733	310919.615659	43.903066
3501.519317	310907.168728	43.908071
3501.427336	310895.859647	43.913076
3501.846290	310874.368559	43.918081
3501.448803	310872.293300	43.923085
3501.539657	310871.210432	43.928090
3501.405323	310860.009749	43.933095
3501.293026	310855.319839	43.938100
3501.495207	310833.048345	43.943105
3501.404640	310831.993840	43.948109
3501.374743	310830.828065	43.953114
3501.489811	310829.283379	43.958119
3501.681507	310827.981175	43.963124
3501.770540	310811.350968	43.968129
3501.710040	310794.642348	43.973133
3501.615475	310781.526964	43.978138
3501.532292	310785.764115	43.983143
3501.435083	310769.213902	43.988148
3501.330237	310751.367120	43.993153
3501.421926	310738.146267	43.998157
3501.441567	310737.328992	44.003162
3501.747019	310735.271060	44.008167
3501.843729	310732.940408	44.013172
3501.810648	310711.977950	44.018177
3501.641324	310700.986270	44.023181
3501.688243	310702.302216	44.028186
3501.843869	310691.157946	44.033191
3501.362203	310683.014182	44.038196
3501.693511	310667.618360	44.043201
3501.530132	310670.901101	44.048205
3501.556293	310655.298519	44.053210
3501.526454	310636.574794	44.058215
3501.183438	310630.216031	44.063220
3501.384147	310624.841006	44.068225
3501.149144	310624.852375	44.073229
3501.651336	310620.906101	44.078234
3501.677940	310616.627038	44.083239
3501.270929	310603.076973	44.088244
3501.479934	310581.109651	44.093249
3501.646695	310579.964017	44.098253
3501.223561	310585.577542	44.103258
3501.662676	310579.579974	44.108263
3501.341269	310569.248198	44.113268
3501.706626	310555.526475	44.118273
3501.678390	310543.189492	44.123277
3501.493747	310537.543900	44.128282
3502.107809	310532.256919	44.133287
3501.678555	310518.710307	44.138292
3501.787258	310503.730930	44.143297
3501.479202	310502.455956	44.148301
3501.382647	310488.959107	44.153306
3501.686647	310476.722843	44.158311
3501.593917	310460.807983	44.163316
3501.620584	310462.508797	44.168321
3501.220844	310451.858439	44.173325
3501.208069	310456.568093	44.178330
3501.278870	310435.411148	44.183335
3501.641279	310422.351454	44.188340
3502.141006	310401.534579	44.193345
3501.763084	310403.934809	44.198349
3501.350848	310405.195314	44.203354
3501.611530	310382.787233	44.208359
3501.169414	310379.268482	44.213364
3501.842721	310374.099454	44.218369
3501.493888	310381.991565	44.223373
3501.180284	310363.032185	44.228378
3501.661999	310345.093549	44.233383
3501.722927	310343.684544	44.238388
3501.675825	310335.065638	44.243393
3501.514176	310340.994561	44.248397
3501.924242	310319.835418	44.253402
3501.711962	310296.203469	44.258407
3501.453555	310303.776098	44.263412
3501.776378	310293.139972	44.268417
3501.671352	310278.270279	44.273421
3501.555336	310260.959436	44.278426
3501.892252	310243.068846	44.283431
3501.452063	310243.544884	44.288436
3501.610303	310225.427756	44.293441
3501.600106	310230.213369	44.298445
3501.009574	310213.918215	44.303450
3501.592324	310211.944142	44.308455
3501.278501	310202.145477	44.313460
3501.275869	310203.138378	44.318465
3501.614063	310190.540445	44.323469
3501.174757	310174.425207	44.328474
3501.231172	310167.215093	44.333479
3501.474324	310174.632989	44.338484
3501.233019	310167.189508	44.343489
3501.654599	310173.587094	44.348493
3501.678266	310172.565607	44.353498
3501.611105	310148.249288	44.358503
3501.525795	310140.170698	44.363508
3501.377821	310137.063981	44.368513
3501.794823	310124.708175	44.373517
3501.707655	310120.345069	44.378522
3501.476721	310095.647182	44.383527
3501.469854	310092.900100	44.388532
3501.490044	310084.881346	44.393537
3501.353215	310084.775580	44.398541
3501.150204	310075.748410	44.403546
3501.617370	310050.279748	44.408551
3501.926874	310047.966688	44.413556
3501.888309	310037.972277	44.418561
3501.708643	310035.455780	44.423565
3501.623387	310018.547187	44.428570
3501.714756	310008.583349	44.433575
3501.453988	310009.540271	44.438580
3501.692528	310008.739654	44.443585
3501.616801	309994.577798	44.448589
3501.584485	309985.167671	44.453594
3501.959209	309969.281352	44.458599
3501.826194	309960.675810	44.463604
3501.608873	309936.662773	44.468609
3501.677864	309927.847516	44.473613
3502.015091	309926.777003	44.478618
3501.850840	309901.279745	44.483623
3501.684480	309900.058941	44.488628
3501.497126	309886.754245	44.493633
3501.754184	309878.571191	44.498637
3501.326995	309858.280695	44.503642
3502.081522	309840.680921	44.508647
3501.736302	309841.345689	44.513652
3501.884904	309834.655493	44.518657
3502.051156	309815.340963	44.523661
3501.648167	309816.421910	44.528666
3501.451568	309791.082330	44.533671
3501.593938	309778.540351	44.538676
3501.841297	309763.589960	44.543681
3501.834583	309770.130900	44.548685
3501.481898	309757.818992	44.553690
3501.950049	309738.228211	44.558695
3501.897914	309737.931076	44.563700
3501.763893	309718.256304	44.568705
3501.894391	309706.784926	44.573709
3501.778305	309691.356951	44.578714
3501.718165	309680.907797	44.583719
3501.650051	309665.472313	44.588724
3501.647209	309655.548578	44.593729
3501.608843	309650.388949	44.598733
3501.309557	309638.552152	44.603738
3501.462866	309628.553105	44.608743
3501.287497	309616.569695	44.613748
3501.469369	309606.133582	44.618753
3501.409551	309599.399598	44.623757
3501.479204	309598.854400	44.628762
3501.629743	309589.161140	44.633767
3501.090279	309586.726317	44.638772
3501.595185	309575.603524	44.643777
3501.673378	309561.468370	44.648781
3501.746419	309555.018970	44.653786
3501.728029	309554.385749	44.658791
3501.672535	309551.213642	44.663796
3501.765387	309530.434555	44.668801
3501.863374	309520.316901	44.673805
3501.475151	309515.415529	44.678810
3501.317810	309495.286267	44.683815
3501.212125	309498.305599	44.688820
3501.334380	309478.896025	44.693825
3501.300355	309468.544529	44.698829
3501.118822	309470.634185	44.703834
3501.589844	309469.720873	44.708839
3501.223279	309472.959120	44.713844
3501.402989	309470.335515	44.718849
3501.748353	309464.327020	44.723853
3501.481645	309451.874358	44.728858
3501.539262	309444.002327	44.733863
3501.111880	309432.821679	44.738868
3501.154046	309441.899714	44.743873
3501.534870	309431.254331	44.748877
3500.965151	309423.047777	44.753882
3501.177566	309407.339331	44.758887
3501.530664	309404.179676	44.763892
3501.363643	309394.688706	44.768897
3501.625725	309392.154007	44.773901
3501.316276	309391.922545	44.778906
3501.483127	309394.084972	44.783911
3501.504060	309392.427723	44.788916
3501.150481	309371.438446	44.793921
3501.275068	309373.531141	44.798925
3501.018128	309365.962746	44.803930
3501.390193	309358.881291	44.808935
3501.726553	309356.055060	44.813940
3501.490288	309361.206913	44.818945
3501.952347	309354.671221	44.823949
3501.425991	309332.996424	44.828954
3501.326982	309318.303623	44.833959
3501.136278	309320.420165	44.838964
3501.172068	309319.574895	44.843969
3501.632586	309316.118523	44.848973
3501.264462	309320.731161	44.853978
3501.235858	309289.944847	44.858983
3501.068394	309288.317048	44.863988
3501.177902	309282.192722	44.868993
3501.602120	309271.973119	44.873997
3501.069676	309270.326040	44.879002
3501.605202	309269.478981	44.884007
3501.283970	309273.626246	44.889012
3501.458059	309273.522763	44.894017
3501.290867	309266.118450	44.899021
3501.096989	309247.547065	44.904026
3501.436925	309241.055897	44.909031
3500.897245	309235.567447	44.914036
3500.592668	309228.210053	44.919041
3501.118357	309227.848025	44.924045
3501.458647	309232.858859	44.929050
3501.388108	309226.635439	44.934055
3501.253555	309221.109097	44.939060
3501.362679	309227.962811	44.944065
3501.672229	309224.682718	44.949069
3501.378031	309224.474317	44.954074
3501.341837	309201.017879	44.959079
3501.115011	309196.014900	44.964084
3501.313017	309191.683467	44.969089
3501.643563	309184.786608	44.974093
3501.617074	309189.015035	44.979098
3501.411749	309188.105670	44.984103
3501.137817	309181.379655	44.989108
3501.179232	309172.772149	44.994113
3501.496297	309150.100210	44.999117
3501.469510	309147.076271	45.004122
3501.730085	309139.706850	45.009127
3501.293296	309146.467794	45.014132
3501.672947	309140.784710	45.019137
3501.795856	309111.348737	45.024141
3501.576590	309117.388606	45.029146
3501.648758	309107.453032	45.034151
3501.795445	309106.335949	45.039156
3501.775648	309084.098351	45.044161
3501.490125	309065.668460	45.049165
3501.468297	309064.933982	45.054170
3501.176617	309052.714145	45.059175
3501.393205	309063.546280	45.064180
3501.188997	309040.345056	45.069185
3502.037919	309027.565184	45.074189
3501.299957	309023.558196	45.079194
3501.303459	309015.770898	45.084199
3501.222618	309015.325563	45.089204
3501.440178	309018.981461	45.094209
3501.593859	309009.109464	45.099213
3501.470460	308996.099890	45.104218
3501.719838	308982.344959	45.109223
3501.444750	308984.907310	45.114228
3501.707581	308973.898567	45.119233
3501.570598	308957.532080	45.124237
3501.267568	308952.311965	45.129242
3501.371974	308946.799127	45.134247
3501.121853	308941.290820	45.139252
3501.336160	308946.219591	45.144257
3501.177216	308938.890280	45.149261
3501.395269	308940.688462	45.154266
3501.466800	308922.431720	45.159271
3501.273212	308921.596856	45.164276
3501.598730	308902.078933	45.169281
3501.925729	308890.067698	45.174285
3501.407864	308900.251277	45.179290
3501.960540	308886.906951	45.184295
3501.611529	308872.482125	45.189300
3501.923609	308866.758679	45.194305
3501.779636	308850.418696	45.199309
3501.326751	308841.404913	45.204314
3501.647746	308823.083685	45.209319
3501.725287	308822.460904	45.214324
3501.541491	308822.973212	45.219329
3501.603386	308803.929067	45.224333
3501.721848	308794.724162	45.229338
3501.761173	308779.831439	45.234343
3501.767432	308790.950991	45.239348
3501.525546	308775.949548	45.244353
3501.610508	308761.355052	45.249357
3501.437914	308743.823486	45.254362
3501.347424	308739.129960	45.259367
3501.379802	308741.618808	45.264372
3501.674424	308742.030873	45.269377
3501.683124	308722.104358	45.274381
3501.567089	308712.681626	45.279386
3501.516103	308701.365621	45.284391
3501.200715	308700.804268	45.289396
3501.467690	308699.821054	45.294401
3501.695490	308682.125079	45.299405
3501.577183	308675.501900	45.304410
3501.628241	308659.818440	45.309415
3501.288705	308660.456886	45.314420
3501.351964	308655.255816	45.319425
3501.332889	308640.295840	45.324429
3500.969098	308634.499901	45.329434
3501.624425	308633.888576	45.334439
3501.226892	308629.293937	45.339444
3501.207564	308621.815513	45.344449
3501.781871	308619.282856	45.349453
3501.642530	308616.352823	45.354458
3501.498204	308601.590548	45.359463
3501.432827	308580.683109	45.364468
3501.495558	308574.795034	45.369473
3501.432285	308573.227264	45.374477
3501.299928	308578.133927	45.379482
3501.485749	308577.239741	45.384487
3501.503555	308560.034605	45.389492
3501.316398	308544.591929	45.394497
3501.674699	308540.617089	45.399501
3501.550667	308535.852446	45.404506
3501.526835	308537.383091	45.409511
3501.581150	308515.184541	45.414516
3501.550950	308502.414739	45.419521
3501.625266	308490.799174	45.424525
3501.290989	308500.979581	45.429530
3501.565102	308495.312923	45.434535
3501.387156	308483.253294	45.439540
3501.023810	308463.486629	45.444545
3501.348345	308448.549216	45.449549
3501.186646	308464.173850	45.454554
3501.380667	308441.648057	45.459559
3501.458198	308441.915933	45.464564
3501.432465	308452.480719	45.469569
3501.669714	308446.412660	45.474573
3501.352440	308433.051534	45.479578
3501.865386	308418.059208	45.484583
3501.405565	308419.428992	45.489588
3501.380419	308413.122029	45.494593
3501.529788	308409.256186	45.499597
3501.317551	308392.519562	45.504602
3501.398249	308379.477915	45.509607
3501.263239	308381.840266	45.514612
3501.303389	308377.507993	45.519617
3501.406351	308367.033057	45.524621
3500.957959	308368.222923	45.529626
3501.527293	308360.805113	45.534631
3501.260334	308365.427472	45.539636
3500.829588	308353.127411	45.544641
3501.391437	308350.214976	45.549645
3501.140756	308342.340072	45.554650
3501.611357	308326.565466	45.559655
3501.562021	308326.776835	45.564660
3501.351838	308323.374357	45.569665
3501.246239	308315.756689	45.574669
3501.029560	308327.089333	45.579674
3501.350240	308319.863076	45.584679
3501.188968	308307.597217	45.589684
3501.038461	308292.988501	45.594689
3500.975228	308288.723278	45.599693
3501.062182	308287.590068	45.604698
3501.452071	308289.335962	45.609703
3501.422063	308289.264386	45.614708
3501.452020	308286.129732	45.619713
3501.641514	308292.716538	45.624717
3501.367226	308296.296701	45.629722
3501.370021	308275.098551	45.634727
3501.382945	308262.423734	45.639732
3501.093705	308254.045893	45.644737
3501.634234	308253.656092	45.649741
3501.146795	308250.958591	45.654746
3501.310220	308252.994368	45.659751
3501.469704	308254.190991	45.664756
3501.276141	308253.305216	45.669761
3501.470259	308235.817927	45.674765
3501.208093	308229.980604	45.679770
3501.302677	308209.226132	45.684775
3501.239064	308209.210705	45.689780
3501.346884	308210.822567	45.694785
3501.576370	308201.091242	45.699789
3501.287397	308211.366417	45.704794
3501.239365	308210.712365	45.709799
3501.505957	308207.006312	45.714804
3501.421282	308190.682285	45.719809
3501.490908	308177.107916	45.724813
3501.492024	308172.349119	45.729818
3501.619221	308163.117282	45.734823
3501.391795	308133.150198	45.739828
3501.028825	308085.594530	45.744833
3501.311820	307991.521285	45.749837
3500.777094	307854.899849	45.754842
3500.940658	307660.427732	45.759847
3500.815527	307418.895811	45.764852
3500.654616	307139.908699	45.769857
3500.363813	306803.249099	45.774861
3499.936522	306426.476338	45.779866
3499.691369	305985.439796	45.784871
3499.441116	305509.255227	45.789876
3498.966131	304986.300271	45.794881
3498.882592	304420.014668	45.799885
3498.269833	303801.964390	45.804890
3497.815833	303128.909716	45.809895
3497.228306	302413.314113	45.814900
3496.760758	301647.017489	45.819905
3496.063661	300845.343133	45.824909
3495.119595	299983.833316	45.829914
3494.320184	299079.833309	45.834919
3493.689735	298147.514418	45.839924
3492.629766	297155.941900	45.844929
3492.132035	296105.594149	45.849933
3491.226224	295026.375467	45.854938
3490.115825	293886.307548	45.859943
3489.633135	292708.242826	45.864948
3488.344696	291483.036009	45.869953
3487.326514	290200.461409	45.874957
3486.305540	288878.149066	45.879962
3485.264651	287508.488115	45.884967
3483.984139	286110.578191	45.889972
3482.888097	284669.026144	45.894977
3481.452265	283174.594056	45.899981
3479.958342	281640.295821	45.904986
3478.568052	280056.608016	45.909991
3477.108879	278444.178161	45.914996
3476.019597	276789.595413	45.920001
3474.952954	275074.071136	45.925005
3473.229373	273333.992028	45.930010
3471.759414	271546.248438	45.935015
3470.085796	269723.794517	45.940020
3468.680683	267860.520994	45.945025
3467.168962	265943.702804	45.950029
3465.375604	264006.902453	45.955034
3463.591128	262025.374289	45.960039
3461.939732	260011.423531	45.965044
3459.830060	257961.119334	45.970049
3457.957101	255858.589769	45.975053
3455.743538	253736.369155	45.980058
3453.880085	251573.137018	45.985063
3451.568931	249392.575967	45.990068
3449.264230	247167.824970	45.995073
3447.683064	244914.537533	46.000077
3445.596417	242627.864939	46.005082
3443.232079	240318.673902	46.010087
3440.973690	237962.457024	46.015092
3438.449237	235594.497770	46.020097
3436.518373	233179.721469	46.025101
3433.733613	230747.671887	46.030106
3431.251811	228278.203738	46.035111
3428.996035	225803.117821	46.040116
3425.827420	223289.282363	46.045121
3423.517502	220749.260691	46.050125
3420.770251	218189.703229	46.055130
3418.179892	215609.375283	46.060135
3415.412833	213002.552159	46.065140
3412.359697	210360.520182	46.070145
3409.543732	207713.229880	46.075149
3406.415630	205047.146560	46.080154
3403.494706	202352.109241	46.085159
3400.219330	199653.220382	46.090164
3396.882600	196925.583760	46.095169
3393.692662	194182.568499	46.100173
3390.315248	191439.079230	46.105178
3387.071834	188686.616417	46.110183
3383.378790	185906.382558	46.115188
3379.861958	183134.725579	46.120193
3376.924899	180333.952833	46.125197
3372.959322	177551.326623	46.130202
3369.622818	174738.571603	46.135207
3365.762548	171927.052585	46.140212
3361.723320	169112.965738	46.145217
3358.158133	166290.333857	46.150221
3354.119002	163473.071319	46.155226
3349.968265	160642.301499	46.160231
3345.522882	157839.144661	46.165236
3340.977565	155029.680337	46.170241
3336.563233	152226.019616	46.175245
3331.635602	149455.246098	46.180250
3326.331628	146673.513904	46.185255
3321.174927	143919.951635	46.190260
3316.687193	141183.396086	46.195265
3311.251726	138418.401845	46.200269
3305.746198	135759.975738	46.205274
3299.181268	133129.449937	46.210279
3293.149320	130538.799579	46.215284
3286.555203	127976.427251	46.220289
3280.161909	125482.392230	46.225293
3272.865724	123039.803356	46.230298
3265.556671	120653.208542	46.235303
3258.436431	118338.109352	46.240308
3250.309610	116089.685521	46.245313
3242.601033	113928.545519	46.250317
3233.882722	111851.072766	46.255322
3225.074861	109851.682468	46.260327
3216.392392	107961.947440	46.265332
3207.634323	106153.724914	46.270337
3198.322929	104440.514655	46.275341
3189.138137	102833.688189	46.280346
3180.209861	101333.643098	46.285351
3171.317302	99920.559753	46.290356
3162.902915	98622.573672	46.295361
3154.329268	97424.507563	46.300365
3145.324672	96303.174394	46.305370
3137.661339	95284.264914	46.310375
3130.430322	94335.137948	46.315380
3123.441430	93474.052354	46.320385
3116.408411	92667.778302	46.325389
3109.982062	91934.812708	46.330394
3104.067877	91266.524689	46.335399
3098.274340	90648.791006	46.340404
3092.473623	90097.091938	46.345409
3087.427373	89567.304304	46.350413
3082.671532	89095.596358	46.355418
3077.624918	88641.856076	46.360423
3073.154185	88231.179875	46.365428
3068.766180	87845.779660	46.370433
3064.902609	87477.466897	46.375437
3060.895490	87121.479464	46.380442
3056.992358	86784.740385	46.385447
3053.456933	86460.906311	46.390452
3050.106892	86143.119540	46.395457
3046.635891	85843.789052	46.400461
3043.196797	85542.525623	46.405466
3040.057635	85250.454237	46.410471
3037.180046	84946.835164	46.415476
3033.738901	84670.874570	46.420481
3030.414131	84360.611297	46.425485
3027.023937	84066.482337	46.430490
3023.945559	83781.212690	46.435495
3020.744236	83484.455966	46.440500
3017.266343	83199.915155	46.445505
3014.423003	82904.124723	46.450509
3010.480757	82607.391361	46.455514
3007.364569	82324.314370	46.460519
3003.875611	82023.222704	46.465524
3000.279943	81733.888002	46.470529
2997.299630	81430.728811	46.475533
2993.794354	81148.702513	46.480538
2990.327094	80848.166184	46.485543
2986.980408	80561.421215	46.490548
2983.324581	80269.507085	46.495553
2979.490176	79971.362008	46.500557
2975.928950	79693.144211	46.505562
2972.369533	79404.475650	46.510567
2969.079840	79126.081345	46.515572
2965.469318	78846.812824	46.520577
2962.364877	78566.845625	46.525581
2958.597834	78289.550467	46.530586
2954.228326	78004.287331	46.535591
2950.784656	77724.877063	46.540596
2946.896736	77466.291755	46.545601
2943.333919	77203.695521	46.550605
2939.903717	76945.538864	46.555610
2936.097738	76686.948111	46.560615
2932.870569	76424.662479	46.565620
2928.880940	76167.591283	46.570625
2925.483345	75915.128857	46.575629
2922.095008	75665.131072	46.580634
2917.960371	75420.281340	46.585639
2914.368238	75171.247062	46.590644
2910.696917	74939.003293	46.595649
2906.850398	74694.762757	46.600653
2903.357324	74466.203367	46.605658
2899.811785	74233.158681	46.610663
2896.166198	74002.125395	46.615668
2892.633507	73776.663916	46.620673
2889.445914	73542.654950	46.625677
2885.702832	73313.128617	46.630682
2882.137781	73091.030420	46.635687
2878.556834	72868.682596	46.640692
2875.125339	72637.881623	46.645697
2871.691378	72415.603497	46.650701
2867.942811	72188.132153	46.655706
2864.777678	71971.682207	46.660711
2861.257641	71740.242621	46.665716
2857.280009	71528.875534	46.670721
2854.415288	71308.168411	46.675725
2850.720847	71091.275185	46.680730
2847.449558	70861.696358	46.685735
2843.782059	70639.837972	46.690740
2840.440552	70429.243676	46.695745
2837.274049	70199.870118	46.700749
2833.301938	69974.040058	46.705754
2830.101055	69750.205364	46.710759
2826.940348	69522.595377	46.715764
2822.838667	69301.679671	46.720769
2819.228402	69075.724647	46.725773
2815.749603	68855.483468	46.730778
2812.578710	68628.701844	46.735783
2809.244807	68404.785307	46.740788
2805.265935	68182.260243	46.745793
2802.446447	67955.093136	46.750797
2798.629407	67731.537330	46.755802
2794.929666	67514.211441	46.760807
2791.808910	67278.165974	46.765812
2787.906248	67062.030964	46.770817
2784.458275	66829.855822	46.775821
2780.846272	66615.678661	46.780826
2777.467428	66394.052831	46.785831
2774.184546	66174.362620	46.790836
2770.454466	65944.746952	46.795841
2766.992114	65724.542818	46.800845
2763.714767	65501.068151	46.805850
2760.120109	65273.779566	46.810855
2756.719568	65044.977405	46.815860
2753.405025	64821.514564	46.820865
2749.554834	64598.321552	46.825869
2746.088338	64374.949914	46.830874
2742.506112	64147.739362	46.835879
2739.609683	63915.491998	46.840884
2735.667978	63700.375607	46.845889
2732.485705	63469.306842	46.850893
2728.704881	63244.541014	46.855898
2725.131002	63008.193752	46.860903
2722.065058	62773.241720	46.865908
2718.082507	62560.578682	46.870913
2714.685300	62327.377228	46.875917
2711.792986	62098.116343	46.880922
2708.243118	61861.243130	46.885927
2704.704446	61628.159235	46.890932
2700.743759	61401.972211	46.895937
2697.274173	61164.725034	46.900941
2693.924236	60939.290785	46.905946
2690.598899	60711.665327	46.910951
2687.416741	60468.750859	46.915956
2683.674805	60239.957447	46.920961
2679.764233	60002.067030	46.925965
2676.448117	59772.094498	46.930970
2672.699509	59538.809436	46.935975
2669.662868	59307.623583	46.940980
2665.878440	59079.361706	46.945985
2662.770396	58837.486224	46.950989
2659.110609	58612.889729	46.955994
2655.761463	58377.579841	46.960999
2652.035993	58141.328514	46.966004
2648.582137	57903.805997	46.971009
2645.458269	57657.642569	46.976013
2641.989986	57424.016743	46.981018
2638.179085	57175.928856	46.986023
2634.892633	56944.423940	46.991028
2631.536522	56701.269822	46.996033
2627.785783	56462.615091	47.001037
2624.298375	56225.304758	47.006042
2620.601339	55985.428151	47.011047
2617.265115	55745.516553	47.016052
2613.278478	55509.509643	47.021057
2609.842557	55273.031904	47.026061
2606.978042	55038.922529	47.031066
2603.049796	54795.921742	47.036071
2599.823382	54558.333425	47.041076
2596.494879	54318.422346	47.046081
2593.122960	54082.986967	47.051085
2589.516493	53830.644850	47.056090
2586.030196	53588.957730	47.061095
2582.169428	53348.092975	47.066100
2578.899327	53112.613307	47.071105
2575.449974	52858.163478	47.076109
2571.547566	52621.125503	47.081114
2568.453938	52380.233169	47.086119
2564.967925	52133.498528	47.091124
2561.375624	51898.963277	47.096129
2557.689751	51648.173266	47.101133
2554.442670	51406.502994	47.106138
2550.573051	51168.053684	47.111143
2547.280656	50918.738815	47.116148
2543.784641	50683.192155	47.121153
2540.067055	50440.057745	47.126157
2536.717210	50188.393634	47.131162
2533.095585	49951.028172	47.136167
2529.740020	49703.226979	47.141172
2526.061349	49468.691812	47.146177
2522.407935	49212.848619	47.151181
2519.332772	48982.530978	47.156186
2515.927128	48741.630193	47.161191
2512.294816	48497.316865	47.166196
2508.675409	48254.221956	47.171201
2505.451135	48012.342725	47.176205
2501.577282	47763.844417	47.181210
2498.284865	47519.215671	47.186215
2495.004752	47266.139348	47.191220
2491.437021	47031.808496	47.196225
2487.815425	46774.319627	47.201229
2484.276757	46528.535036	47.206234
2480.088250	46288.087157	47.211239
2476.946937	46038.237426	47.216244
2473.586535	45806.759879	47.221249
2470.357996	45561.958403	47.226253
2466.951212	45323.694380	47.231258
2463.432836	45072.328866	47.236263
2460.087455	44812.561503	47.241268
2456.387659	44577.274859	47.246273
2453.107626	44311.097883	47.251277
2449.580375	44066.258026	47.256282
2446.131366	43822.068146	47.261287
2442.624627	43570.711382	47.266292
2438.856958	43318.713406	47.271297
2435.564668	43061.145960	47.276301
2432.133828	42817.097465	47.281306
2428.235953	42552.243064	47.286311
2425.116417	42303.408308	47.291316
2421.420669	42055.674731	47.296321
2418.279776	41799.461646	47.301325
2414.424010	41557.611461	47.306330
2411.057969	41289.201538	47.311335
2407.642493	41027.840904	47.316340
2404.211476	40779.034088	47.321345
2400.893912	40518.089052	47.326349
2397.327647	40274.197774	47.331354
2393.659924	40016.103369	47.336359
2390.412992	39754.737944	47.341364
2386.664984	39500.935650	47.346369
2383.429754	39235.472438	47.351373
2379.758736	38975.374706	47.356378
2376.493783	38719.286927	47.361383
2373.135225	38451.937897	47.366388
2369.638919	38195.721335	47.371393
2366.235309	37916.821897	47.376397
2362.703062	37659.026030	47.381402
2358.825998	37404.247852	47.386407
2355.820195	37126.519997	47.391412
2352.139130	36864.122677	47.396417
2348.354545	36594.739633	47.401421
2345.030015	36333.554604	47.406426
2341.634154	36064.713335	47.411431
2338.009613	35811.607228	47.416436
2334.527009	35544.827333	47.421441
2331.169072	35278.525732	47.426445
2327.506676	35009.612716	47.431450
2323.812077	34741.088486	47.436455
2320.560372	34472.916740	47.441460
2316.780303	34204.374664	47.446465
2313.627134	33939.617214	47.451469
2310.232328	33668.010814	47.456474
2306.940805	33398.870128	47.461479
2303.185322	33127.618707	47.466484
2299.992099	32853.253088	47.471489
2296.408799	32574.230062	47.476493
2292.928042	32303.485085	47.481498
2289.315106	32033.715015	47.486503
2286.023944	31747.216374	47.491508
2282.359734	31474.932680	47.496513
2278.855816	31192.068584	47.501517
2275.589532	30910.768282	47.506522
2272.233062	30640.938124	47.511527
2268.744067	30356.321209	47.516532
2264.736156	30093.457406	47.521537
2261.610993	29796.889391	47.526541
2258.093996	29521.420619	47.531546
2254.924660	29228.479985	47.536551
2251.630758	28943.414775	47.541556
2247.808139	28668.575590	47.546561
2244.412746	28378.312346	47.551565
2240.995280	28092.448152	47.556570
2237.551104	27802.061304	47.561575
2234.109395	27515.961834	47.566580
2230.526340	27218.913422	47.571585
2227.266054	26928.529259	47.576589
2223.870448	26641.135882	47.581594
2220.124241	26341.927063	47.586599
2217.052843	26044.106112	47.591604
2213.496295	25759.221575	47.596609
2210.023606	25457.511931	47.601613
2206.597820	25155.698086	47.606618
2202.901489	24866.134052	47.611623
2199.769666	24548.481567	47.616628
2196.215404	24252.289568	47.621633
2192.841662	23941.742528	47.626637
2189.165118	23640.415182	47.631642
2185.886755	23332.986084	47.636647
2182.262421	23024.532511	47.641652
2178.537901	22731.189914	47.646657
2175.086920	22412.867409	47.651661
2172.308172	22105.100356	47.656666
2168.238975	21798.065778	47.661671
2164.867004	21484.516021	47.666676
2161.462066	21174.213444	47.671681
2157.641059	20863.708455	47.676685
2154.629808	20554.120530	47.681690
2150.592163	20233.657137	47.686695
2147.489680	19926.152064	47.691700
2143.891540	19613.947012	47.696705
2140.068538	19312.018086	47.701709
2136.845178	18993.252804	47.706714
2133.419059	18677.792759	47.711719
2129.930827	18365.856479	47.716724
2125.875307	18069.607612	47.721729
2122.371059	17754.896796	47.726733
2118.786453	17441.236022	47.731738
2114.690228	17152.379768	47.736743
2111.114324	16856.239076	47.741748
2107.410546	16571.326445	47.746753
2103.683162	16274.442560	47.751757
2099.974927	15988.332783	47.756762
2096.017061	15702.386649	47.761767
2093.049848	15414.456405	47.766772
2089.317866	15134.246306	47.771777
2085.732377	14862.534846	47.776781
2081.716465	14581.120237	47.781786
2077.921128	14312.884862	47.786791
2074.126433	14030.956156	47.791796
2070.712889	13776.546075	47.796801
2066.866536	13512.059707	47.801805
2062.990706	13269.446559	47.806810
2058.755588	13018.702197	47.811815
2055.322511	12768.826619	47.816820
2051.109261	12533.547992	47.821825
2047.346540	12315.541533	47.826829
2043.818896	12076.419214	47.831834
2039.671253	11860.618381	47.836839
2036.185248	11646.707791	47.841844
2032.747100	11439.357955	47.846849
2029.017865	11219.567128	47.851853
2025.515645	11016.385436	47.856858
2021.949050	10806.166083	47.861863
2018.214437	10597.105510	47.866868
2014.450816	10407.678512	47.871873
2011.058574	10201.025304	47.876877
2007.825220	9996.552728	47.881882
2004.455272	9799.637645	47.886887
2000.871584	9594.933068	47.891892
1997.581666	9408.708855	47.896897
1993.785809	9208.799369	47.901901
1989.940582	9006.073093	47.906906
1986.617717	8811.671238	47.911911
1983.395755	8610.310977	47.916916
1979.648329	8430.055625	47.921921
1976.141398	8231.975804	47.926925
1973.004601	8036.315371	47.931930
1969.242546	7851.522732	47.936935
1966.156775	7657.447241	47.941940
1962.418518	7462.963147	47.946945
1958.654340	7268.102190	47.951949
1955.458722	7072.945439	47.956954
1951.445198	6885.945177	47.961959
1948.429276	6708.057740	47.966964
1945.134977	6518.486333	47.971969
1941.763413	6328.663126	47.976973
1938.232545	6124.416024	47.981978
1934.686943	5937.216135	47.986983
1931.543559	5731.814583	47.991988
1927.868329	5549.721617	47.996993
1924.178846	5343.922508	48.001997
1920.771820	5150.892220	48.007002
1916.760215	4969.671014	48.012007
1913.541405	4759.089505	48.017012
1910.052210	4576.758797	48.022017
1906.452038	4378.146605	48.027021
1903.211035	4188.929671	48.032026
1899.383806	4001.727298	48.037031
1896.247511	3811.820712	48.042036
1892.770046	3622.643530	48.047041
1889.315464	3422.424156	48.052045
1885.852252	3235.261355	48.057050
1882.116736	3048.263351	48.062055
1878.624674	2846.818971	48.067060
1875.077394	2670.294575	48.072065
1871.539304	2477.246840	48.077069
1868.282410	2281.597336	48.082074
1864.121050	2110.496716	48.087079
1860.537131	1905.701081	48.092084
1857.351259	1717.577244	48.097089
1853.322935	1530.830694	48.102093
1849.832146	1341.695393	48.107098
1846.409803	1160.233575	48.112103
1842.665374	977.409708	48.117108
1839.457682	810.149394	48.122113
1835.647940	631.509365	48.127117
1831.779551	460.903897	48.132122
1827.383811	308.638003	48.137127
1823.460483	158.289533	48.142132
1818.771345	39.706512	48.147137
1809.814234	42.155535	48.152141
1802.170728	47.382460	48.157146
1796.738295	57.898107	48.162151
1793.033723	57.914772	48.167156
1790.830659	51.179021	48.172161
1787.808472	63.630223	48.177165
1785.426261	59.491517	48.182170
1782.102025	70.506170	48.187175
1779.795542	59.869810	48.192180
1776.162020	58.457977	48.197185
1772.636173	60.139316	48.202189
1769.926052	63.714669	48.207194
1766.194574	58.841147	48.212199
1763.132189	51.679892	48.217204
1759.836378	57.564732	48.222209
1756.133055	57.695112	48.227213
1752.500367	58.035905	48.232218
1748.612208	58.087646	48.237223
1745.477396	64.893273	48.242228
1741.982150	63.035862	48.247233
1738.382317	71.641707	48.252237
1735.842119	67.353728	48.257242
1732.099787	65.962104	48.262247
1728.321082	62.247612	48.267252
1724.977345	69.139728	48.272257
1721.310483	67.173139	48.277261
1718.269462	54.911664	48.282266
1714.662090	68.612419	48.287271
1711.313501	62.742508	48.292276
1708.193072	71.728921	48.297281
1704.247893	68.201846	48.302285
1700.748361	68.958423	48.307290
1697.091951	63.367651	48.312295
1693.556706	65.784489	48.317300
1690.555664	67.722248	48.322305
1687.068977	70.042902	48.327309
1683.880125	63.632302	48.332314
1680.059258	55.688097	48.337319
1676.494850	64.728181	48.342324
1673.294733	71.233996	48.347329
1669.534241	68.668301	48.352333
1666.058833	65.127832	48.357338
1662.375384	69.039045	48.362343
1659.477096	54.322291	48.367348
1656.172505	59.025272	48.372353
1652.346160	60.035497	48.377357
1648.694602	58.547439	48.382362
1645.027740	73.538863	48.387367
1641.808084	59.179298	48.392372
1638.619691	61.023004	48.397377
1634.953161	58.860241	48.402381
1631.372907	55.782292	48.407386
1627.609740	58.364539	48.412391
1624.225835	48.184770	48.417396
1620.953203	61.804676	48.422401
1617.207566	53.896182	48.427405
1613.992464	52.032938	48.432410
1610.594158	60.303548	48.437415
1607.522515	51.207551	48.442420
1603.611014	56.733210	48.447425
1599.642915	57.680218	48.452429
1596.473926	54.414526	48.457434
1592.820963	68.941868	48.462439
1589.164215	63.094925	48.467444
1586.567413	54.740876	48.472449
1582.602074	62.486465	48.477453
1578.947118	60.328239	48.482458
1575.736760	54.057091	48.487463
1571.955870	57.401443	48.492468
1568.683383	59.429177	48.497473
1564.941764	54.886361	48.502477
1561.820889	57.083359	48.507482
1558.132594	58.856634	48.512487
1554.624286	54.043183	48.517492
1551.032916	51.802249	48.522497
1547.257422	63.400116	48.527501
1543.851948	57.975779	48.532506
1540.731817	54.572743	48.537511
1537.355769	53.557303	48.542516
1533.804978	51.079066	48.547521
1530.344760	60.159828	48.552525
1527.073112	55.787079	48.557530
1523.054686	59.731783	48.562535
1519.498311	62.006450	48.567540
1516.229688	51.928905	48.572545
1512.444436	58.842723	48.577549
1509.381243	56.069873	48.582554
1505.413871	60.490654	48.587559
1501.976390	56.137543	48.592564
1498.823930	51.746150	48.597569
1494.984735	64.436022	48.602573
1491.655623	59.553416	48.607578
1488.175757	54.086961	48.612583
1484.802158	52.058741	48.617588
1481.336682	52.151992	48.622593
1477.628879	56.111367	48.627597
1474.072268	57.841913	48.632602
1470.739854	55.060595	48.637607
1467.709063	52.184610	48.642612
1463.738232	56.068101	48.647617
1460.091159	61.792867	48.652621
1456.409228	53.624533	48.657626
1453.356968	56.557478	48.662631
1449.732181	55.201347	48.667636
1446.170969	59.330780	48.672641
1442.588580	58.028127	48.677645
1439.525682	53.730305	48.682650
1435.526079	59.709579	48.687655
1431.954542	57.791455	48.692660
1428.596346	60.471735	48.697665
1425.049797	62.336766	48.702669
1421.764810	58.652687	48.707674
1418.232606	54.937703	48.712679
1415.116018	51.290544	48.717684
1411.264684	51.684666	48.722689
1407.716585	59.409293	48.727693
1404.501252	48.162341	48.732698
1401.035023	50.318531	48.737703
1397.412991	47.462351	48.742708
1393.847929	52.047988	48.747713
1390.143431	48.249254	48.752717
1386.787126	50.245871	48.757722
1383.030242	47.053297	48.762727
1379.263522	52.885402	48.767732
1376.224649	45.151127	48.772737
1372.810011	52.089232	48.777741
1369.358118	43.907079	48.782746
1365.849404	51.543290	48.787751
1362.282493	46.691634	48.792756
1358.975029	48.993830	48.797761
1355.225880	54.222072	48.802765
1351.932005	51.146859	48.807770
1348.185625	50.233749	48.812775
1344.806350	48.209632	48.817780
1341.143211	47.596710	48.822785
1337.461962	55.294742	48.827789
1334.058628	45.665475	48.832794
1330.352324	44.629038	48.837799
1327.326014	48.168567	48.842804
1324.337375	49.357831	48.847809
1320.354771	53.452027	48.852813
1316.649843	50.162760	48.857818
1313.192552	46.483549	48.862823
1309.629562	49.436373	48.867828
1306.387618	44.904032	48.872833
1302.684840	49.036687	48.877837
1299.530099	43.709242	48.882842
1295.613344	58.973976	48.887847
1292.267485	52.676691	48.892852
1288.860829	41.282571	48.897857
1285.582540	52.742558	48.902861
1281.709996	45.243230	48.907866
1277.998940	50.873663	48.912871
1274.450354	51.695013	48.917876
1271.451720	43.375505	48.922881
1267.804060	54.548468	48.927885
1264.270280	48.970320	48.932890
1260.454586	45.878753	48.937895
1257.380321	52.105538	48.942900
1253.370862	43.532987	48.947905
1249.930990	51.152128	48.952909
1246.770537	42.930730	48.957914
1243.259739	42.569246	48.962919
1239.731571	51.629080	48.967924
1237.006489	48.711641	48.972929
1232.831491	48.213693	48.977933
1229.385934	48.496905	48.982938
1225.655036	50.017536	48.987943
1221.944644	43.862772	48.992948
1218.275677	46.829053	48.997953
1215.008879	46.635027	49.002957
1211.792188	44.196359	49.007962
1208.347044	40.056540	49.012967
1204.696790	42.731991	49.017972
1201.390626	41.522229	49.022977
1197.707241	49.062446	49.027981
1194.427523	46.918392	49.032986
1190.849764	49.949499	49.037991
1187.240374	43.516344	49.042996
1183.610055	46.739181	49.048001
1179.701160	42.988353	49.053005
1176.833108	42.700276	49.058010
1172.880228	50.456701	49.063015
1169.540203	48.179727	49.068020
1166.100926	46.674438	49.073025
1162.609242	57.860978	49.078029
1159.053719	52.023682	49.083034
1155.639481	43.465561	49.088039
1152.091125	49.833035	49.093044
1148.877206	50.747569	49.098049
1145.161235	53.825640	49.103053
1141.658123	47.647950	49.108058
1138.074300	48.724804	49.113063
1134.833097	49.922027	49.118068
1131.182274	47.336218	49.123073
1127.442775	54.163902	49.128077
1124.309427	40.379538	49.133082
1120.904310	45.781787	49.138087
1116.891176	46.090623	49.143092
1113.292590	49.995058	49.148097
1110.060565	51.298421	49.153101
1106.636094	45.905708	49.158106
1103.041231	44.453276	49.163111
1099.388718	40.364948	49.168116
1096.301588	39.722050	49.173121
1092.647230	45.169657	49.178125
1089.325915	38.716754	49.183130
1085.888934	48.708326	49.188135
1082.231585	44.143030	49.193140
1078.695027	32.076480	49.198145
1074.949400	42.764950	49.203149
1071.444101	49.432595	49.208154
1068.102918	49.813419	49.213159
1064.287040	49.319429	49.218164
1061.082836	47.818504	49.223169
1057.338070	50.546771	49.228173
1054.226520	40.150602	49.233178
1050.504142	37.990486	49.238183
1046.860889	41.841823	49.243188
1043.707550	37.381133	49.248193
1039.961591	54.340287	49.253197
1036.714887	39.539154	49.258202
1032.928338	44.899910	49.263207
1029.881271	49.730432	49.268212
1026.330345	40.244635	49.273217
1022.375865	47.615379	49.278221
1018.647651	43.662324	49.283226
1015.750669	49.390011	49.288231
1011.981027	54.026788	49.293236
1008.761657	46.191198	49.298241
1005.243757	56.246086	49.303245
1001.778974	42.450393	49.308250
997.995693	46.896318	49.313255
994.541468	46.257146	49.318260
991.225052	39.278327	49.323265
987.449334	44.067923	49.328269
983.815448	43.529652	49.333274
980.346778	40.833126	49.338279
976.832333	42.819836	49.343284
973.742441	45.432941	49.348289
970.113055	43.710717	49.353293
966.790972	44.999753	49.358298
962.551624	57.356952	49.363303
959.413616	51.147481	49.368308
956.174070	47.032515	49.373313
952.593069	50.791881	49.378317
949.218489	44.416976	49.383322
945.753950	49.293906	49.388327
941.683940	46.346700	49.393332
938.420518	44.488091	49.398337
934.586850	48.337646	49.403341
931.398723	44.654405	49.408346
928.365039	50.770518	49.413351
924.707138	37.979550	49.418356
921.183549	41.264860	49.423361
917.452080	48.875972	49.428365
913.692928	50.002508	49.433370
910.118452	47.398506	49.438375
906.691190	42.784602	49.443380
903.280333	45.511262	49.448385
899.902869	50.444175	49.453389
896.897040	50.446678	49.458394
893.360762	40.487245	49.463399
889.730094	45.105465	49.468404
886.097519	36.451938	49.473409
882.291893	45.621758	49.478413
878.555897	48.244314	49.483418
875.033863	46.600231	49.488423
871.547144	42.024126	49.493428
868.781758	40.590597	49.498433
864.905282	44.927775	49.503437
861.411852	36.913701	49.508442
858.198744	37.755436	49.513447
854.441754	43.244505	49.518452
850.893957	41.905025	49.523457
847.247359	48.942882	49.528461
843.785906	39.993655	49.533466
840.324143	45.123286	49.538471
836.638345	36.705908	49.543476
833.677333	39.776603	49.548481
829.889804	44.011280	49.553485
826.069865	39.626580	49.558490
822.552088	39.070191	49.563495
819.170873	47.781265	49.568500
816.022274	40.152976	49.573505
812.608052	45.395394	49.578509
809.143290	47.279471	49.583514
805.660272	44.923784	49.588519
802.115914	55.653593	49.593524
798.261663	55.134084	49.598529
795.107127	46.706294	49.603533
791.436281	47.920291	49.608538
787.930893	44.460792	49.613543
784.119923	50.423416	49.618548
780.469986	43.781651	49.623553
776.869011	47.759343	49.628557
773.870622	42.613257	49.633562
770.701199	39.354258	49.638567
766.818777	45.850098	49.643572
763.544312	49.646949	49.648577
759.767099	44.951864	49.653581
756.186131	51.172711	49.658586
752.818878	45.397857	49.663591
749.016288	49.710855	49.668596
745.735406	41.549648	49.673601
742.357758	47.672219	49.678605
738.409062	44.165104	49.683610
735.496386	49.186636	49.688615
731.792937	48.349307	49.693620
728.920769	49.748303	49.698625
724.739875	46.470547	49.703629
720.952316	52.116314	49.708634
717.708397	42.351624	49.713639
714.602669	43.375910	49.718644
711.018667	47.189615	49.723649
707.373225	52.525227	49.728653
703.602943	52.233055	49.733658
700.081018	50.978167	49.738663
696.466515	50.095286	49.743668
693.359533	49.563199	49.748673
689.688443	46.427085	49.753677
685.942431	44.495449	49.758682
682.605092	46.207754	49.763687
679.116915	47.000879	49.768692
676.159943	46.900889	49.773697
672.474235	51.926442	49.778701
668.868062	37.327316	49.783706
665.172440	31.926633	49.788711
661.604084	42.783621	49.793716
658.416500	41.818078	49.798721
654.981591	45.054792	49.803725
651.265581	42.257926	49.808730
648.090062	32.972945	49.813735
643.790371	48.443357	49.818740
640.822687	35.142640	49.823745
637.347371	44.789160	49.828749
634.013623	35.155639	49.833754
629.968615	40.098270	49.838759
626.034242	46.175189	49.843764
622.985160	34.361545	49.848769
619.615167	39.245920	49.853773
616.505850	33.547790	49.858778
612.837692	39.870922	49.863783
609.576505	43.694216	49.868788
605.538637	42.662542	49.873793
602.137878	42.192315	49.878797
598.513678	44.300756	49.883802
595.147105	33.292991	49.888807
591.360508	34.885863	49.893812
588.326818	40.211125	49.898817
584.689660	38.442819	49.903821
581.336347	48.449902	49.908826
577.890385	39.944461	49.913831
573.815827	42.038024	49.918836
570.412490	31.703585	49.923841
566.698323	46.455891	49.928845
563.705721	34.392981	49.933850
560.233559	31.206787	49.938855
556.761450	39.856239	49.943860
553.128192	30.595535	49.948865
549.850295	41.669656	49.953869
546.440057	31.570428	49.958874
542.682051	29.416106	49.963879
538.475679	38.145764	49.968884
535.558894	40.947028	49.973889
532.239603	46.668218	49.978893
528.771783	37.198112	49.983898
524.816607	35.429020	49.988903
521.026108	40.872836	49.993908
517.918228	36.705783	49.998913
514.630187	42.817553	50.003917
511.291032	42.786967	50.008922
507.895292	44.343966	50.013927
503.741288	49.920656	50.018932
500.585437	32.697928	50.023937
497.377897	37.762542	50.028941
494.027235	37.923592	50.033946
490.521346	34.635140	50.038951
486.482577	38.358801	50.043956
482.972127	35.656364	50.048961
479.267596	41.953603	50.053965
475.487569	38.948541	50.058970
472.682040	43.605347	50.063975
468.550256	38.877347	50.068980
465.635798	45.114118	50.073985
462.092919	41.657463	50.078989
458.630134	45.003017	50.083994
454.876720	36.596412	50.088999
451.213082	40.979505	50.094004
448.365990	43.776207	50.099009
444.579442	44.268141	50.104013
441.271858	46.184679	50.109018
437.478770	37.056631	50.114023
433.997068	44.749005	50.119028
430.501822	46.802511	50.124033
426.726005	48.210263	50.129037
423.185647	43.911668	50.134042
420.192705	41.637562	50.139047
416.832426	46.064901	50.144052
413.136465	43.518099	50.149057
409.336936	43.426785	50.154061
405.840454	46.901023	50.159066
402.438022	50.037827	50.164071
398.751402	47.385164	50.169076
395.621793	36.672568	50.174081
391.939080	40.204455	50.179085
388.555227	43.591454	50.184090
385.165141	41.958538	50.189095
381.485331	36.644092	50.194100
378.058575	38.402149	50.199105
374.736162	40.026804	50.204109
370.892589	39.148300	50.209114
367.457556	36.152523	50.214119
363.624300	42.830636	50.219124
360.420816	34.825156	50.224129
357.194369	40.655243	50.229133
353.191797	37.371884	50.234138
349.631429	32.405741	50.239143
345.955578	39.400889	50.244148
343.056885	26.988013	50.249153
339.729955	34.548602	50.254157
336.256243	41.762028	50.259162
332.708864	40.837144	50.264167
328.523881	37.905074	50.269172
325.415238	29.796170	50.274177
321.863435	38.973872	50.279181
318.000120	36.959531	50.284186
314.918746	39.027340	50.289191
311.254737	39.098337	50.294196
308.100133	30.762521	50.299201
304.653038	41.872704	50.304205
300.978522	38.025451	50.309210
297.148264	32.737777	50.314215
293.555304	35.784241	50.319220
290.310574	32.976984	50.324225
286.693722	43.079216	50.329229
283.429764	39.904813	50.334234
280.094722	36.760529	50.339239
276.088349	37.385047	50.344244
273.017047	29.216532	50.349249
269.298114	35.804002	50.354253
265.729093	38.343690	50.359258
262.865752	36.786494	50.364263
259.237721	41.948693	50.369268
255.809543	39.268264	50.374273
251.908919	39.414317	50.379277
248.030049	37.611253	50.384282
244.773478	22.252079	50.389287
240.948585	31.191010	50.394292
237.638112	33.993925	50.399297
234.315755	39.013335	50.404301
230.421260	48.358651	50.409306
227.354481	37.740692	50.414311
223.165812	39.855448	50.419316
220.457512	33.616926	50.424321
216.871465	42.404558	50.429325
212.981983	35.345006	50.434330
209.798665	37.232668	50.439335
206.052696	41.976764	50.444340
202.774809	34.846715	50.449345
199.481658	35.191854	50.454349
195.849110	36.532965	50.459354
192.441281	31.210802	50.464359
188.431575	38.691743	50.469364
185.194625	31.773588	50.474369
181.754361	32.511941	50.479373
178.153475	35.955160	50.484378
174.772846	37.541551	50.489383
170.598454	42.969713	50.494388
167.770231	34.671409	50.499393
164.506189	36.957711	50.504397
161.166961	37.272119	50.509402
157.578817	41.944053	50.514407
153.796812	47.449954	50.519412
150.459851	33.523941	50.524417
146.768530	32.039554	50.529421
143.256264	45.004466	50.534426
139.547623	36.413833	50.539431
135.866614	40.878861	50.544436
132.456606	35.813328	50.549441
129.255609	23.397289	50.554445
125.691727	34.753608	50.559450
122.189843	35.865469	50.564455
118.379430	41.265103	50.569460
115.330977	39.784415	50.574465
111.782547	34.468495	50.579469
108.301565	39.297664	50.584474
105.059291	28.568054	50.589479
101.113302	33.134719	50.594484
97.596039	34.173070	50.599489
94.123044	34.900766	50.604493
90.570031	39.532419	50.609498
87.537979	37.853019	50.614503
83.692338	32.770339	50.619508
80.109763	28.968896	50.624513
76.320513	31.426101	50.629517
72.939485	32.019174	50.634522
69.607438	40.001431	50.639527
66.205869	38.620378	50.644532
62.458320	32.804168	50.649537
58.826346	43.079686	50.654541
55.466804	43.321387	50.659546
52.141599	41.437993	50.664551
48.764463	42.811913	50.669556
45.139493	41.525982	50.674561
41.757324	40.569006	50.679565
38.158005	45.888142	50.684570
34.554922	30.798495	50.689575
31.124079	40.779916	50.694580
27.621573	37.788525	50.699585
24.292693	42.505308	50.704589
20.539294	42.093724	50.709594
17.083579	39.968201	50.714599
13.375538	46.826147	50.719604
10.074108	32.274542	50.724609
6.621028	37.896641	50.729613
2.970101	39.338787	50.734618