Thu Aug 25 10:10:46 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.030673	104.845480	0.000000
0.096585	104.559938	0.005005
0.257104	100.811069	0.010010
0.131494	100.716887	0.015014
0.024508	90.584327	0.020019
-0.154935	85.465033	0.025024
-0.658519	76.900572	0.030029
-0.008631	75.647170	0.035034
-0.471635	64.548512	0.040038
-1.004874	46.953018	0.045043
-0.494493	38.482806	0.050048
-1.370837	32.232527	0.055053
-1.879754	19.344079	0.060058
-2.026702	23.581253	0.065062
-2.702892	6.742188	0.070067
-2.951218	9.134958	0.075072
-2.999127	4.039371	0.080077
-2.896262	-6.736616	0.085082
-3.392567	-10.562884	0.090086
-3.779201	-9.205136	0.095091
-3.706352	-16.939219	0.100096
-4.130659	-19.074670	0.105101
-4.236821	-21.424484	0.110106
-4.881357	-29.571341	0.115110
-5.529936	-28.343395	0.120115
-5.836467	-25.220176	0.125120
-6.251142	-14.689507	0.130125
-6.072806	-30.944255	0.135130
-6.058746	-16.652634	0.140134
-6.056975	-21.699049	0.145139
-6.671030	-24.810840	0.150144
-7.298347	-11.465922	0.155149
-7.345496	-27.505010	0.160154
-7.720207	-19.555891	0.165158
-8.048985	-24.632772	0.170163
-7.839036	-20.138318	0.175168
-8.061391	-28.968253	0.180173
-8.450306	-31.814762	0.185178
-9.205597	-30.943418	0.190182
-9.198401	-32.915523	0.195187
-9.215053	-30.252174	0.200192
-9.448958	-27.333323	0.205197
-9.887110	-19.320481	0.210202
-10.040695	-14.867142	0.215206
-10.550292	-15.423177	0.220211
-10.496068	-13.761182	0.225216
-10.200487	-12.791900	0.230221
-10.915959	-15.065228	0.235226
-11.737496	-14.933311	0.240230
-11.887808	-23.448670	0.245235
-11.512224	-24.387005	0.250240
-11.977517	-19.925957	0.255245
-12.170888	-15.804905	0.260250
-12.837067	-24.100232	0.265254
-13.210056	-26.430384	0.270259
-13.107846	-25.196687	0.275264
-13.596474	-16.258449	0.280269
-13.105173	-25.412174	0.285274
-13.759280	-16.713763	0.290278
-13.790709	-10.631252	0.295283
-14.358088	-14.073060	0.300288
-14.880033	-19.043746	0.305293
-14.794961	-23.597014	0.310298
-14.903038	-21.675473	0.315302
-14.825559	-22.181124	0.320307
-15.513532	-24.360683	0.325312
-16.188764	-20.097694	0.330317
-16.101158	-33.146005	0.335322
-16.401652	-19.997833	0.340326
-16.281294	-27.429308	0.345331
-16.850759	-20.898669	0.350336
-17.529051	-19.289581	0.355341
-17.514822	-28.257824	0.360346
-17.762431	-25.545632	0.365350
-17.894434	-25.898238	0.370355
-18.144781	-23.707635	0.375360
-18.027725	-19.609913	0.380365
-18.077785	-23.822469	0.385370
-19.227102	-26.372667	0.390374
-19.113959	-32.445763	0.395379
-19.296736	-29.145783	0.400384
-19.324955	-14.486871	0.405389
-19.681129	-24.501227	0.410394
-20.476034	-26.145177	0.415398
-20.527925	-27.551206	0.420403
-20.426173	-29.693150	0.425408
-20.724759	-20.563229	0.430413
-20.656192	-25.528360	0.435418
-21.499249	-22.118597	0.440422
-22.244932	-18.293820	0.445427
-22.144598	-21.672567	0.450432
-22.362144	-17.380049	0.455437
-22.569089	-25.933989	0.460442
-22.490870	-14.003081	0.465446
-22.149733	-26.635542	0.470451
-22.734339	-21.064308	0.475456
-23.248772	-22.590853	0.480461
-23.234177	-25.867580	0.485466
-23.329043	-26.580344	0.490470
-23.968039	-27.470441	0.495475
-24.586898	-22.786016	0.500480
-24.970635	-18.568699	0.505485
-25.152096	-32.672670	0.510490
-25.463623	-19.709431	0.515494
-25.505468	-22.781163	0.520499
-25.170175	-23.950466	0.525504
-25.518441	-17.840461	0.530509
-25.892918	-21.856655	0.535514
-26.439271	-20.151180	0.540518
-26.749173	-26.926783	0.545523
-26.589222	-24.442964	0.550528
-27.257216	-23.439764	0.555533
-27.619033	-27.277606	0.560538
-28.001626	-20.624388	0.565542
-28.016643	-18.015077	0.570547
-27.669511	-23.163061	0.575552
-27.888826	-22.818617	0.580557
-28.650205	-22.256364	0.585562
-29.120542	-19.404870	0.590566
-29.470119	-24.579730	0.595571
-29.454666	-27.002381	0.600576
-29.845410	-16.035703	0.605581
-29.321465	-23.938537	0.610586
-29.453278	-19.513921	0.615590
-30.471645	-18.209050	0.620595
-30.934178	-34.170389	0.625600
-30.996895	-26.342925	0.630605
-31.006462	-18.995182	0.635610
-31.262238	-22.621851	0.640614
-31.967878	-22.764354	0.645619
-32.077448	-26.834708	0.650624
-32.617351	-20.213788	0.655629
-32.478686	-34.073688	0.660634
-32.511047	-18.626361	0.665638
-32.668982	-15.931382	0.670643
-32.443392	-28.422350	0.675648
-33.451554	-13.435890	0.680653
-33.592421	-15.745465	0.685658
-33.986858	-18.796753	0.690662
-34.237215	-17.400246	0.695667
-34.017115	-19.342437	0.700672
-34.771555	-18.256089	0.705677
-34.979874	-17.609649	0.710682
-35.410379	-25.846986	0.715686
-35.670385	-18.643501	0.720691
-35.364874	-23.259781	0.725696
-35.837046	-12.849817	0.730701
-35.686074	-23.911739	0.735706
-36.586361	-16.009982	0.740710
-36.947623	-14.709993	0.745715
-36.806909	-23.894208	0.750720
-36.743579	-17.753782	0.755725
-36.951173	-26.478461	0.760730
-37.583922	-22.206309	0.765734
-37.950417	-22.218454	0.770739
-38.254199	-20.848378	0.775744
-38.574094	-21.737853	0.780749
-38.462063	-27.108426	0.785754
-39.221119	-20.611355	0.790758
-39.441715	-25.173675	0.795763
-39.469900	-26.858664	0.800768
-39.797937	-23.668800	0.805773
-39.540348	-26.059788	0.810778
-39.243676	-20.721550	0.815782
-40.246458	-26.278113	0.820787
-40.871085	-30.732833	0.825792
-41.105588	-23.969943	0.830797
-41.029592	-22.602425	0.835802
-41.247544	-28.380036	0.840806
-41.858815	-24.196671	0.845811
-42.340602	-24.940558	0.850816
-43.022018	-25.684803	0.855821
-42.701685	-24.197383	0.860826
-42.922019	-9.356508	0.865830
-42.872127	-21.541541	0.870835
-43.078206	-25.783433	0.875840
-43.308305	-27.610791	0.880845
-43.217621	-28.203931	0.885850
-43.487991	-28.098260	0.890854
-43.972374	-18.287496	0.895859
-44.223354	-15.191962	0.900864
-44.518983	-15.971345	0.905869
-44.844042	-25.145853	0.910874
-45.512124	-31.548955	0.915878
-45.976660	-25.009449	0.920883
-45.822128	-21.145390	0.925888
-46.122777	-22.161267	0.930893
-45.787404	-26.775898	0.935898
-46.232900	-23.615086	0.940902
-46.268910	-22.283802	0.945907
-47.070620	-26.590554	0.950912
-47.284340	-12.971923	0.955917
-47.182610	-25.807315	0.960922
-47.476259	-13.403693	0.965926
-47.948017	-22.397028	0.970931
-48.544960	-29.905933	0.975936
-49.084269	-17.096827	0.980941
-48.665765	-24.771168	0.985946
-48.772997	-18.505942	0.990950
-48.962957	-20.703420	0.995955
-48.740725	-16.233038	1.000960
-49.729028	-22.589133	1.005965
-50.056072	-22.208827	1.010970
-50.245423	-23.267452	1.015974
-50.253021	-24.996795	1.020979
-50.427537	-31.521525	1.025984
-51.067178	-23.230343	1.030989
-51.722865	-26.750056	1.035994
-51.594042	-24.593554	1.040998
-51.711415	-16.890400	1.046003
-51.426031	-20.927726	1.051008
-51.776736	-12.416057	1.056013
-52.027085	-23.196797	1.061018
-53.038530	-18.147138	1.066022
-53.498860	-25.338929	1.071027
-53.078885	-22.266269	1.076032
-53.634291	-20.932696	1.081037
-53.527850	-21.136002	1.086042
-53.725770	-19.826805	1.091046
-54.276962	-18.136390	1.096051
-54.388918	-23.405428	1.101056
-54.620018	-21.489921	1.106061
-54.641212	-27.513495	1.111066
-54.816075	-22.626556	1.116070
-55.663940	-11.227585	1.121075
-55.923598	-20.086475	1.126080
-56.459797	-22.881432	1.131085
-56.390872	-21.734269	1.136090
-56.258470	-22.030227	1.141094
-56.388416	-23.658142	1.146099
-56.478808	-28.361084	1.151104
-57.743685	-13.296436	1.156109
-57.451357	-21.172470	1.161114
-57.377644	-24.676758	1.166118
-57.770036	-16.940004	1.171123
-57.748382	-22.343871	1.176128
-58.823024	-18.704830	1.181133
-59.372228	-26.312963	1.186138
-59.406612	-22.232643	1.191142
-59.340645	-19.455689	1.196147
-59.450860	-15.350832	1.201152
-59.503744	-14.962863	1.206157
-59.453550	-22.832594	1.211162
-59.991798	-17.224330	1.216166
-60.697001	-19.315765	1.221171
-61.037110	-13.542394	1.226176
-60.856693	-2.358320	1.231181
-60.930661	-10.990047	1.236186
-61.274871	-13.720175	1.241190
-61.808207	-11.073942	1.246195
-61.931074	-21.283037	1.251200
-62.514795	-14.455934	1.256205
-62.409968	-18.936367	1.261210
-62.542369	-22.500108	1.266214
-62.633510	-24.627647	1.271219
-63.221552	-23.073826	1.276224
-63.909207	-9.263875	1.281229
-63.536519	-13.824245	1.286234
-63.660827	-21.362915	1.291238
-63.744396	-12.503963	1.296243
-64.361425	-21.291038	1.301248
-65.020413	-9.336368	1.306253
-64.825426	-10.167314	1.311258
-65.193628	-28.721883	1.316262
-65.323581	-8.478847	1.321267
-65.907365	-12.427442	1.326272
-66.336656	-4.745012	1.331277
-66.648323	-20.926147	1.336282
-66.691952	-15.914237	1.341286
-66.870369	-16.534816	1.346291
-66.567668	-13.060967	1.351296
-66.906928	-16.244284	1.356301
-67.178363	-24.436940	1.361306
-67.425067	-21.266147	1.366310
-68.089986	-23.556881	1.371315
-68.261530	-19.929631	1.376320
-68.486873	-14.930377	1.381325
-68.548095	-20.349733	1.386330
-69.263622	-15.007918	1.391334
-69.353743	-9.529980	1.396339
-69.591465	-14.250968	1.401344
-69.978727	-13.513214	1.406349
-69.887841	-19.247468	1.411354
-69.835667	-14.804225	1.416358
-70.209840	-12.616364	1.421363
-70.857188	-24.328311	1.426368
-71.179568	-10.287696	1.431373
-71.441095	-18.795117	1.436378
-71.416550	-13.063065	1.441382
-71.558582	-7.418804	1.446387
-71.257584	-8.690303	1.451392
-72.411968	-4.538891	1.456397
-72.390045	-14.337244	1.461402
-72.648985	-7.668595	1.466406
-73.229461	-4.910571	1.471411
-73.531921	-26.417723	1.476416
-73.881461	-17.156433	1.481421
-74.016903	-24.687029	1.486426
-74.238885	-17.831187	1.491430
-74.461945	-22.737967	1.496435
-74.139699	-23.898900	1.501440
-74.374714	-14.532167	1.506445
-74.250450	-13.782815	1.511450
-74.888668	-16.318178	1.516454
-75.282893	-10.412940	1.521459
-75.597626	-17.646527	1.526464
-76.345062	-12.467390	1.531469
-76.308441	-17.399043	1.536474
-76.792727	-17.895764	1.541478
-76.863175	-20.491616	1.546483
-76.574533	-25.124235	1.551488
-77.086328	-11.506356	1.556493
-77.065809	-19.355620	1.561498
-77.846345	-8.356336	1.566502
-78.418793	-9.630180	1.571507
-78.447956	-17.696285	1.576512
-78.807766	-15.504347	1.581517
-78.579813	-21.260077	1.586522
-78.537463	-8.953394	1.591526
-79.346478	-9.086023	1.596531
-79.526655	-13.015601	1.601536
-79.754201	-12.578118	1.606541
-79.955734	-16.624571	1.611546
-79.983738	-26.367637	1.616550
-80.751691	-13.956136	1.621555
-80.978353	-22.136825	1.626560
-81.274668	-15.648984	1.631565
-81.186562	-24.828116	1.636570
-81.304781	-19.681134	1.641574
-81.233094	-10.368785	1.646579
-81.586181	-17.757713	1.651584
-82.506650	-8.248772	1.656589
-82.437798	-13.827715	1.661594
-82.599863	-11.144744	1.666598
-83.257850	-10.275984	1.671603
-83.277940	-14.645096	1.676608
-84.124981	-9.782543	1.681613
-84.363817	-21.447770	1.686618
-84.245098	-20.757661	1.691622
-84.145551	-17.270963	1.696627
-84.381847	-14.313771	1.701632
-84.742644	-12.052075	1.706637
-84.377737	-18.047564	1.711642
-85.172858	-21.292328	1.716646
-85.669871	-13.637255	1.721651
-85.948555	-17.769694	1.726656
-85.887605	-17.396399	1.731661
-85.655959	-13.424201	1.736666
-86.518973	-21.780424	1.741670
-87.138526	-9.309917	1.746675
-87.214445	-23.655049	1.751680
-87.237245	-10.610499	1.756685
-87.266252	-13.848757	1.761690
-87.108007	-21.545594	1.766694
-88.201167	-20.371366	1.771699
-88.510432	-20.082429	1.776704
-88.746958	-13.227471	1.781709
-88.625701	-17.833864	1.786714
-88.809452	-25.303105	1.791718
-89.428546	-19.090553	1.796723
-89.765923	-23.818069	1.801728
-90.205808	-18.826328	1.806733
-89.997764	-20.339525	1.811738
-90.297756	-17.391334	1.816742
-90.014277	-17.306007	1.821747
-90.201453	-10.000037	1.826752
-91.119347	-15.196575	1.831757
-91.575939	-12.119442	1.836762
-91.348328	-18.077599	1.841766
-91.875090	-14.707899	1.846771
-91.679451	-22.464378	1.851776
-92.084756	-17.886178	1.856781
-92.617517	-14.075777	1.861786
-92.627183	-19.376661	1.866790
-93.234359	-16.845407	1.871795
-93.040181	-21.254418	1.876800
-93.708562	-15.157528	1.881805
-94.280301	-25.891067	1.886810
-94.588229	-21.404056	1.891814
-94.901889	-17.444490	1.896819
-94.591414	-28.107456	1.901824
-94.881593	-24.641951	1.906829
-94.759698	-20.465898	1.911834
-94.757507	-18.859028	1.916838
-95.060744	-14.543592	1.921843
-95.826452	-16.565431	1.926848
-96.061605	-21.220380	1.931853
-96.229248	-17.422899	1.936858
-96.151280	-18.542392	1.941862
-96.874639	-18.530254	1.946867
-97.196953	-21.665604	1.951872
-97.715611	-21.837400	1.956877
-97.639864	-18.302682	1.961882
-97.745558	-19.985017	1.966886
-97.807800	-14.565233	1.971891
-97.789020	-35.641816	1.976896
-98.518556	-21.977173	1.981901
-99.130255	-28.778245	1.986906
-99.299462	-22.060388	1.991910
-99.350694	-28.167837	1.996915
-99.330111	-19.682235	2.006912
-99.388245	-18.776574	2.016909
-99.113181	-22.611456	2.026906
-98.247034	-23.580238	2.036902
-97.932098	-17.959172	2.046899
-97.543460	-23.379907	2.056896
-97.072723	-25.756586	2.066893
-96.247268	-25.512063	2.076890
-95.402588	-24.903089	2.086886
-95.230710	-30.974099	2.096883
-95.223050	-25.510794	2.106880
-94.509507	-28.489386	2.116877
-93.723910	-27.624066	2.126874
-92.982152	-26.770883	2.136870
-92.699948	-24.927033	2.146867
-92.565154	-28.869813	2.156864
-91.801891	-30.706286	2.166861
-91.315457	-27.354891	2.176858
-90.884364	-24.603040	2.186854
-90.186259	-18.972322	2.196851
-90.119930	-22.350012	2.206848
-89.248721	-29.072295	2.216845
-88.343447	-25.868890	2.226842
-88.258334	-25.216925	2.236838
-88.165810	-21.803806	2.246835
-87.397184	-26.184856	2.256832
-87.050524	-27.370010	2.266829
-86.029502	-24.710595	2.276826
-85.771129	-21.713102	2.286822
-85.461043	-19.860948	2.296819
-84.606303	-20.406625	2.306816
-84.275772	-19.127877	2.316813
-83.741733	-21.105830	2.326810
-82.561204	-15.572877	2.336806
-82.980461	-23.192181	2.346803
-82.564437	-21.141217	2.356800
-81.903269	-23.056727	2.366797
-81.659120	-16.901883	2.376794
-80.645453	-19.202077	2.386790
-80.166764	-23.034018	2.396787
-79.852355	-25.519249	2.406784
-79.014570	-18.266332	2.416781
-78.503207	-16.676965	2.426778
-78.339320	-18.314985	2.436774
-77.994066	-23.304437	2.446771
-77.011236	-22.001187	2.456768
-76.791788	-24.972049	2.466765
-76.371155	-27.606971	2.476762
-75.710141	-17.380309	2.486758
-75.785977	-20.970140	2.496755
-74.528631	-20.584214	2.506752
-74.308548	-16.883805	2.516749
-73.618506	-12.804038	2.526746
-73.291412	-14.907955	2.536742
-72.948387	-13.276371	2.546739
-72.605489	-8.600516	2.556736
-71.882603	-12.727314	2.566733
-70.816496	-12.156200	2.576730
-70.315669	-15.396067	2.586726
-70.224742	-14.561279	2.596723
-70.152302	-14.708779	2.606720
-69.296879	-15.840603	2.616717
-68.549586	-26.940367	2.626714
-68.432088	-21.133142	2.636710
-67.357779	-14.623700	2.646707
-66.922548	-17.035997	2.656704
-66.973228	-13.476893	2.666701
-66.528064	-19.669924	2.676698
-65.876506	-16.623163	2.686694
-64.996661	-21.313078	2.696691
-64.382137	-16.454872	2.706688
-64.446864	-13.967450	2.716685
-63.956815	-14.918480	2.726682
-62.957764	-13.104586	2.736678
-63.075982	-17.935888	2.746675
-62.431800	-21.128524	2.756672
-61.437866	-28.364211	2.766669
-61.300295	-19.376500	2.776666
-60.909899	-16.368012	2.786662
-60.035218	-21.193333	2.796659
-59.936977	-14.819220	2.806656
-58.676530	-16.138050	2.816653
-58.530221	-16.255943	2.826650
-58.505885	-13.687441	2.836646
-57.872480	-14.597577	2.846643
-56.971007	-16.148430	2.856640
-56.910166	-14.532818	2.866637
-56.061894	-20.117439	2.876634
-55.485331	-16.054736	2.886630
-55.204840	-15.176791	2.896627
-54.969205	-21.948375	2.906624
-53.997212	-24.042465	2.916621
-53.686510	-17.099762	2.926618
-53.507041	-18.550156	2.936614
-53.017194	-20.758768	2.946611
-51.903172	-16.726425	2.956608
-51.201037	-21.230104	2.966605
-51.145438	-22.851156	2.976602
-51.314773	-22.400073	2.986598
-49.903923	-16.228462	2.996595
-49.403613	-18.327841	3.006592
-49.483313	-20.859025	3.016589
-48.715040	-22.724791	3.026586
-48.113267	-22.714478	3.036582
-47.937907	-27.303509	3.046579
-47.009108	-18.857919	3.056576
-46.560177	-23.914301	3.066573
-46.576069	-18.523329	3.076570
-45.454735	-26.681799	3.086566
-45.184183	-17.477337	3.096563
-44.789045	-22.816727	3.106560
-43.914751	-21.144841	3.116557
-43.987085	-17.395445	3.126554
-43.052597	-20.934507	3.136550
-42.486575	-18.016893	3.146547
-42.082501	-22.987052	3.156544
-42.056046	-24.651054	3.166541
-41.201480	-16.741859	3.176538
-40.824300	-12.958357	3.186534
-39.776869	-18.441135	3.196531
-39.601463	-19.032420	3.206528
-39.402958	-23.783469	3.216525
-38.111772	-22.826301	3.226522
-37.894024	-14.801486	3.236518
-37.886665	-11.517569	3.246515
-37.855679	-13.020725	3.256512
-36.782354	-21.573985	3.266509
-35.698083	-20.264449	3.276506
-35.365259	-16.325111	3.286502
-35.046545	-17.195441	3.296499
-34.810529	-17.387577	3.306496
-34.441399	-23.001658	3.316493
-33.887737	-15.903786	3.326490
-32.984298	-12.582876	3.336486
-32.591252	-17.332731	3.346483
-32.061693	-18.213923	3.356480
-31.837067	-23.716664	3.366477
-30.919651	-15.513206	3.376474
-30.396590	-16.041755	3.386470
-30.482346	-14.628087	3.396467
-29.761489	-19.742915	3.406464
-29.161215	-18.547611	3.416461
-28.563636	-19.249392	3.426458
-27.936129	-17.817602	3.436454
-28.084554	-15.899939	3.446451
-26.787084	-19.850667	3.456448
-26.351938	-17.618963	3.466445
-26.393300	-18.559587	3.476442
-25.631291	-19.508878	3.486438
-24.956081	-18.657932	3.496435
-24.572739	-18.125552	3.506432
-23.993263	-15.625025	3.516429
-23.080147	-14.190468	3.526426
-23.149009	-6.890514	3.536422
-23.059654	-16.594735	3.546419
-22.383271	-22.576905	3.556416
-21.696993	-16.171383	3.566413
-21.163687	-24.700216	3.576410
-20.557227	-20.806920	3.586406
-20.205781	-17.595924	3.596403
-19.672178	-25.636963	3.606400
-18.589428	-21.092869	3.616397
-18.708928	-15.907406	3.626394
-18.452740	-15.006645	3.636390
-17.872168	-16.377335	3.646387
-16.701161	-25.734677	3.656384
-16.470023	-25.564920	3.666381
-16.263369	-20.398884	3.676378
-15.877711	-19.958732	3.686374
-14.870759	-20.575769	3.696371
-14.676847	-18.664227	3.706368
-14.264530	-16.837591	3.716365
-13.182654	-14.773740	3.726362
-13.249575	-17.154874	3.736358
-12.974626	-14.293020	3.746355
-11.732445	-17.287913	3.756352
-11.438376	-19.411995	3.766349
-11.291388	-15.883862	3.776346
-10.602638	-22.279783	3.786342
-9.891317	-23.401695	3.796339
-10.024688	-21.160108	3.806336
-8.941340	-20.062666	3.816333
-8.597584	-30.171037	3.826330
-7.693193	-26.156529	3.836326
-7.271936	-18.369504	3.846323
-7.164523	-22.346011	3.856320
-6.764466	-16.560878	3.866317
-6.024681	-14.519454	3.876314
-5.564757	-8.122810	3.886310
-5.394273	-9.102962	3.896307
-5.086548	-0.981362	3.906304
-3.957965	1.943150	3.916301
-3.858015	13.540709	3.926298
-3.739399	13.975186	3.936294
-3.091345	27.245005	3.946291
-2.617134	41.121781	3.956288
-1.828975	54.562905	3.966285
-1.697441	65.202039	3.976282
-0.996514	87.292308	3.986278
-0.704789	99.756367	3.996275
-0.631136	122.119190	4.006272
0.000000	140.092738	4.011277
0.039904	152.403088	4.016282
0.318364	172.436815	4.021286
0.504505	178.716257	4.026291
0.811270	192.487618	4.031296
0.926181	183.332648	4.036301
0.595118	182.365816	4.041306
1.127622	190.501917	4.046310
1.312778	205.611639	4.051315
1.127125	209.481594	4.056320
1.483869	218.850648	4.061325
1.343681	209.131351	4.066330
1.161913	209.517372	4.071334
1.273330	208.205960	4.076339
1.298717	212.273806	4.081344
1.352498	218.684734	4.086349
1.345755	215.667572	4.091354
1.271729	217.169346	4.096358
1.250277	208.864641	4.101363
1.215461	221.930236	4.106368
1.408184	204.765013	4.111373
1.155114	216.422114	4.116378
1.529374	221.824203	4.121382
1.596428	214.328212	4.126387
1.521549	225.463850	4.131392
1.625918	217.253323	4.136397
1.787096	223.331047	4.141402
1.496479	214.954615	4.146406
1.337070	200.831182	4.151411
1.388799	223.127794	4.156416
1.633535	211.203138	4.161421
1.569927	210.295640	4.166426
1.398700	207.165044	4.171430
1.508103	214.168374	4.176435
1.331838	224.756743	4.181440
1.550163	209.520578	4.186445
1.544264	217.886583	4.191450
1.490298	224.260610	4.196454
1.548563	215.918101	4.201459
1.708440	223.739275	4.206464
1.839429	218.849717	4.211469
1.673832	225.241234	4.216474
1.663052	226.442032	4.221478
1.303381	218.845219	4.226483
1.390833	227.756592	4.231488
1.684699	222.338472	4.236493
1.504185	226.641064	4.241498
1.401111	225.179758	4.246502
1.458570	215.878748	4.251507
0.993247	223.766241	4.256512
1.459029	230.375214	4.261517
1.792384	236.603137	4.266522
1.562264	246.494432	4.271526
2.072335	244.013229	4.276531
1.773166	256.383105	4.281536
1.611484	249.160223	4.286541
2.125065	253.585027	4.291546
1.887596	246.892883	4.296550
2.128417	249.012889	4.301555
1.702039	249.063909	4.306560
2.030020	242.261024	4.311565
1.998795	248.359410	4.316570
1.706355	250.699012	4.321574
1.812665	246.534658	4.326579
1.746487	241.767736	4.331584
1.585125	245.687678	4.336589
1.942301	251.623969	4.341594
1.874041	255.519834	4.346598
1.822807	248.716250	4.351603
1.692718	252.865414	4.356608
2.155440	253.599715	4.361613
1.944719	255.328556	4.366618
1.937052	250.302525	4.371622
2.195670	247.465246	4.376627
2.006304	252.547525	4.381632
2.138829	252.299000	4.386637
1.908787	253.891663	4.391642
1.864227	249.380782	4.396646
2.161000	243.503450	4.401651
2.052522	255.207526	4.406656
1.927764	245.694601	4.411661
1.935489	252.947998	4.416666
2.091230	250.617225	4.421670
1.853059	248.114051	4.426675
2.107550	265.313717	4.431680
2.275958	277.926727	4.436685
2.376653	269.137777	4.441690
2.393724	272.482431	4.446694
2.326447	260.916681	4.451699
2.202091	258.525387	4.456704
2.383949	245.952491	4.461709
2.243162	257.785018	4.466714
2.207978	254.661573	4.471718
2.208287	243.752805	4.476723
2.175802	253.657431	4.481728
2.609816	259.319091	4.486733
2.321134	259.497235	4.491738
2.104401	258.680165	4.496742
2.499984	264.290900	4.501747
2.164096	274.682843	4.506752
2.343094	273.186829	4.511757
2.566126	274.461729	4.516762
2.300427	274.310400	4.521766
2.462216	273.380239	4.526771
2.306886	276.163439	4.531776
2.416599	281.262142	4.536781
2.494621	275.612064	4.541786
2.245719	280.858705	4.546790
2.650954	279.162726	4.551795
2.258810	289.800777	4.556800
2.329959	284.186576	4.561805
2.827524	279.511652	4.566810
2.405231	284.032477	4.571814
2.849610	273.250269	4.576819
2.546632	279.308986	4.581824
2.391290	278.045693	4.586829
2.596714	278.545058	4.591834
2.620710	282.394836	4.596838
2.554912	289.935018	4.601843
2.370485	293.279608	4.606848
2.608572	279.872127	4.611853
2.580640	278.740733	4.616858
2.675641	286.053236	4.621862
2.594309	284.813149	4.626867
2.693628	280.061416	4.631872
2.579930	281.635851	4.636877
2.555350	285.800130	4.641882
2.676318	278.241880	4.646886
2.626245	290.971390	4.651891
2.634920	288.397895	4.656896
2.736624	280.162447	4.661901
2.557888	284.765336	4.666906
2.615044	291.068191	4.671910
2.743812	279.266065	4.676915
2.529260	289.727592	4.681920
2.496538	292.390343	4.686925
3.039271	302.147922	4.691930
3.100707	301.818786	4.696934
2.933249	295.220059	4.701939
2.689110	292.866511	4.706944
2.586292	292.392265	4.711949
2.811986	301.199757	4.716954
2.721700	304.156271	4.721958
2.835142	302.866682	4.726963
2.912900	306.530869	4.731968
3.129372	309.787339	4.736973
3.238992	311.431193	4.741978
3.225257	309.756563	4.746982
3.125717	301.011626	4.751987
3.175246	293.217787	4.756992
2.528261	289.275855	4.761997
2.705057	297.967619	4.767002
2.808049	300.226288	4.772006
3.291499	311.356758	4.777011
2.721301	320.523082	4.782016
3.107272	309.794297	4.787021
2.996281	315.595152	4.792026
2.722866	316.732700	4.797030
3.234206	308.078710	4.802035
3.196847	312.517084	4.807040
3.162097	306.596760	4.812045
3.060146	310.814296	4.817050
2.738201	315.385846	4.822054
2.900346	308.175478	4.827059
2.897766	309.473075	4.832064
3.224925	305.388001	4.837069
3.155947	305.148901	4.842074
3.315106	321.692833	4.847078
3.365574	311.807564	4.852083
3.200614	319.493011	4.857088
3.288382	311.063576	4.862093
3.419012	309.894682	4.867098
3.354777	310.882394	4.872102
3.522714	313.083432	4.877107
2.994085	315.384117	4.882112
2.944709	305.293029	4.887117
3.057991	310.751854	4.892122
3.288475	325.835593	4.897126
3.565226	329.155390	4.902131
3.145631	335.988547	4.907136
3.683173	336.420058	4.912141
3.327853	335.539276	4.917146
3.397854	332.007025	4.922150
3.275402	334.376952	4.927155
3.590816	340.930432	4.932160
3.543529	336.514871	4.937165
3.615547	330.878372	4.942170
3.325069	333.144910	4.947174
3.526462	317.284872	4.952179
3.502988	329.731827	4.957184
3.368886	334.191691	4.962189
3.409312	336.463331	4.967194
3.740357	341.960814	4.972198
3.789505	334.072103	4.977203
3.531240	327.617307	4.982208
3.114301	330.210548	4.987213
3.441924	333.769151	4.992218
3.471298	332.220645	4.997222
3.661427	334.601709	5.002227
3.614105	344.182838	5.007232
3.782032	339.122942	5.012237
3.649119	349.559057	5.017242
3.496492	350.361301	5.022246
3.865141	332.715966	5.027251
3.590235	344.117139	5.032256
3.765243	343.532922	5.037261
3.663843	342.150439	5.042266
3.392945	346.821569	5.047270
3.722233	347.478702	5.052275
3.503356	339.378878	5.057280
3.259014	332.931390	5.062285
3.558447	335.665494	5.067290
3.533770	348.163271	5.072294
3.744433	342.043130	5.077299
3.556683	346.887896	5.082304
3.761375	346.925462	5.087309
4.161540	358.375901	5.092314
3.690027	343.064205	5.097318
3.515102	340.256874	5.102323
3.760937	348.422145	5.107328
3.632904	359.167554	5.112333
3.792502	357.266441	5.117338
3.586586	364.379347	5.122342
4.009783	356.973031	5.127347
3.814712	358.465309	5.132352
3.963517	353.297671	5.137357
3.909766	359.668549	5.142362
3.654606	357.930499	5.147366
3.654355	348.141744	5.152371
3.823491	350.089493	5.157376
4.080865	347.603577	5.162381
3.970657	352.050210	5.167386
4.071861	361.313843	5.172390
4.200912	352.805152	5.177395
4.154296	359.260335	5.182400
4.157356	353.777005	5.187405
4.171556	354.939095	5.192410
3.794950	359.775489	5.197414
3.856398	357.067164	5.202419
3.870950	364.379649	5.207424
3.996901	367.213707	5.212429
4.255254	379.907610	5.217434
4.190480	384.543290	5.222438
4.555176	372.020753	5.227443
4.054582	379.091249	5.232448
4.181292	366.694591	5.237453
4.035681	364.819151	5.242458
3.690819	379.442578	5.247462
4.041274	381.045540	5.252467
4.266834	383.696311	5.257472
4.335977	380.809603	5.262477
4.586218	377.163680	5.267482
4.185488	385.256262	5.272486
4.272500	383.695556	5.277491
4.199479	389.613874	5.282496
4.190674	394.364176	5.287501
4.030253	382.686388	5.292506
4.185922	392.501499	5.297510
4.443429	381.606133	5.302515
4.530694	385.968050	5.307520
4.364285	390.338075	5.312525
4.482047	383.625023	5.317530
4.377685	395.663910	5.322534
4.872294	386.841658	5.327539
4.652618	393.833343	5.332544
4.256911	382.666992	5.337549
4.138934	390.870302	5.342554
4.426344	395.798823	5.347558
4.589292	388.699031	5.352563
4.241662	389.360984	5.357568
4.312353	397.303777	5.362573
4.435847	394.766062	5.367578
4.294889	389.798842	5.372582
4.583324	387.323872	5.377587
4.147643	392.473257	5.382592
4.103456	389.142387	5.387597
4.580889	405.459355	5.392602
4.608989	411.814263	5.397606
4.565539	411.080770	5.402611
4.559875	411.904284	5.407616
4.624435	415.184575	5.412621
4.716677	416.875455	5.417626
4.790383	425.431570	5.422630
4.738215	412.781327	5.427635
4.756318	414.705290	5.432640
4.767730	413.301963	5.437645
4.764539	410.679689	5.442650
4.695607	415.059758	5.447654
4.550159	408.144322	5.452659
5.067863	410.980283	5.457664
4.658738	409.294826	5.462669
4.610282	412.573841	5.467674
4.885287	418.747694	5.472678
5.111236	414.624669	5.477683
4.681773	409.478014	5.482688
4.768478	404.462464	5.487693
4.803949	414.714044	5.492698
4.549111	409.331217	5.497702
5.133447	418.164834	5.502707
4.779993	423.402587	5.507712
4.673506	419.549950	5.512717
4.653165	419.091252	5.517722
4.609113	416.560803	5.522726
4.817054	416.316279	5.527731
4.512243	416.395709	5.532736
4.593458	421.286940	5.537741
4.878965	417.812657	5.542746
4.723762	419.694171	5.547750
4.682583	417.204401	5.552755
4.966208	433.991533	5.557760
4.774698	432.642144	5.562765
5.391699	433.994537	5.567770
5.357661	443.361661	5.572774
5.217749	426.014220	5.577779
5.148116	427.512160	5.582784
4.885508	425.455724	5.587789
5.106301	415.148234	5.592794
4.817073	421.552865	5.597798
5.047969	421.890052	5.602803
5.120866	430.778497	5.607808
4.786655	444.663137	5.612813
5.371642	449.627309	5.617818
5.118618	447.468126	5.622822
5.337308	450.151622	5.627827
5.674565	443.875567	5.632832
4.846118	434.760704	5.637837
5.025780	435.583657	5.642842
5.128736	450.342625	5.647846
5.338016	443.564590	5.652851
5.233750	452.196060	5.657856
5.620302	443.314779	5.662861
5.437162	442.150744	5.667866
5.118039	435.284656	5.672870
5.446636	440.330126	5.677875
4.976515	445.367861	5.682880
4.984313	446.050059	5.687885
5.337379	445.219636	5.692890
5.091829	454.468043	5.697894
5.404176	454.732356	5.702899
5.221087	443.611749	5.707904
5.190239	446.812080	5.712909
5.339562	442.539699	5.717914
5.574927	447.865540	5.722918
5.572198	438.105598	5.727923
5.155918	444.299184	5.732928
5.143786	438.777079	5.737933
5.358300	439.528130	5.742938
5.287039	438.068150	5.747942
5.515459	440.788086	5.752947
5.302939	445.677890	5.757952
5.474917	446.872214	5.762957
5.769027	449.547057	5.767962
5.290745	456.765950	5.772966
5.774155	447.850508	5.777971
5.697663	443.996330	5.782976
5.582865	449.481442	5.787981
5.747642	449.009559	5.792986
5.661481	447.782871	5.797990
5.395844	442.784549	5.802995
5.256127	443.046924	5.808000
5.338430	449.833125	5.813005
5.560808	457.353537	5.818010
5.514568	468.627211	5.823014
5.680574	478.551484	5.828019
5.791569	481.732760	5.833024
5.758832	476.283476	5.838029
5.715541	476.945205	5.843034
5.912844	482.767415	5.848038
5.914091	478.337887	5.853043
5.760783	468.930559	5.858048
5.613853	460.692854	5.863053
5.965154	471.537239	5.868058
5.609098	472.333396	5.873062
5.823850	470.679900	5.878067
5.413131	477.749008	5.883072
5.575594	470.120899	5.888077
5.883997	472.277802	5.893082
5.722039	467.956107	5.898086
5.522431	471.018365	5.903091
5.563697	476.751122	5.908096
5.535096	487.455719	5.913101
5.618496	475.337861	5.918106
5.426373	473.286195	5.923110
5.957327	484.121423	5.928115
6.029912	495.990281	5.933120
6.225581	492.011190	5.938125
5.409553	485.906326	5.943130
5.806021	498.328732	5.948134
6.017797	497.915923	5.953139
6.265345	502.230609	5.958144
5.610045	499.258066	5.963149
6.115943	497.644374	5.968154
5.750760	512.410302	5.973158
6.045418	501.347687	5.978163
6.297182	497.875512	5.983168
6.649519	502.793891	5.988173
6.530253	500.072728	5.993178
5.914670	497.150912	5.998182
5.887090	491.887481	6.003187
6.223156	501.278908	6.008192
6.256288	505.497471	6.013197
6.312221	495.823222	6.018202
6.089217	493.399896	6.023206
6.226429	481.425466	6.028211
6.031072	480.484812	6.033216
5.879252	482.454389	6.038221
6.220741	489.785305	6.043226
6.405684	499.330125	6.048230
6.250949	493.846165	6.053235
6.052227	491.279826	6.058240
6.084347	485.095859	6.063245
5.974304	481.712013	6.068250
6.009113	493.504529	6.073254
6.305054	492.518535	6.078259
6.559337	491.292288	6.083264
5.822187	486.402633	6.088269
6.245086	480.673145	6.093274
6.036907	487.593461	6.098278
6.328495	479.888168	6.103283
6.044996	479.758609	6.108288
5.914348	476.450761	6.113293
6.222303	477.788302	6.118298
5.879621	480.116822	6.123302
6.246101	482.030502	6.128307
6.304527	503.791728	6.133312
5.836420	500.084320	6.138317
6.112213	493.972905	6.143322
6.152534	504.381968	6.148326
6.498269	502.151112	6.153331
6.695501	490.546933	6.158336
5.984434	483.410034	6.163341
6.215590	479.159624	6.168346
6.346939	490.481419	6.173350
6.056609	477.447655	6.178355
6.538656	474.262115	6.183360
6.292709	480.014563	6.188365
6.356751	483.475287	6.193370
6.208380	488.402509	6.198374
6.148251	479.246338	6.203379
6.007757	470.776660	6.208384
6.233851	484.791847	6.213389
6.119808	487.480024	6.218394
5.819198	480.867288	6.223398
6.173444	483.893391	6.228403
6.233572	475.256232	6.233408
6.079836	478.273338	6.238413
6.163169	477.858507	6.243418
6.305695	483.967717	6.248422
5.888228	487.389986	6.253427
6.273432	478.850593	6.258432
5.795200	480.823855	6.263437
6.306086	474.593353	6.268442
6.042057	476.017349	6.273446
5.917293	475.938851	6.278451
6.095971	474.446035	6.283456
5.829366	488.522602	6.288461
6.057845	478.482796	6.293466
5.925935	491.839055	6.298470
6.308424	479.946422	6.303475
6.044572	481.658299	6.308480
5.996370	489.999422	6.313485
6.301165	483.304485	6.318490
5.962277	485.328684	6.323494
6.207763	470.844197	6.328499
5.973959	481.236084	6.333504
5.962044	483.636169	6.338509
6.269623	481.870049	6.343514
6.172749	486.643665	6.348518
6.120089	485.690144	6.353523
6.071522	493.904772	6.358528
5.695969	500.057194	6.363533
6.124519	503.378550	6.368538
6.052917	506.885842	6.373542
6.490341	510.031798	6.378547
6.482650	497.339724	6.383552
6.215240	494.170362	6.388557
6.028578	478.624089	6.393562
5.903551	484.427198	6.398566
6.491322	483.828925	6.403571
5.981826	474.414126	6.408576
5.732068	481.147960	6.413581
6.255453	490.411952	6.418586
6.398207	511.062124	6.423590
6.082106	489.793757	6.428595
6.225130	485.266081	6.433600
6.077472	492.407876	6.438605
6.202528	481.609134	6.443610
5.689160	483.366433	6.448614
6.522623	490.158347	6.453619
6.530826	499.455606	6.458624
6.037477	486.883926	6.463629
6.370776	473.315846	6.468634
6.014272	485.074751	6.473638
6.032243	482.123277	6.478643
6.304807	477.970786	6.483648
5.991825	477.674999	6.488653
6.266554	474.550416	6.493658
6.185244	485.475247	6.498662
6.309575	479.767228	6.503667
6.443981	485.618276	6.508672
6.055533	484.992619	6.513677
6.040197	474.095653	6.518682
5.932648	477.080211	6.523686
6.100563	484.900240	6.528691
6.339017	483.622689	6.533696
5.917671	483.663429	6.538701
6.212318	477.337089	6.543706
6.077495	479.164794	6.548710
6.221283	470.109560	6.553715
6.115367	478.396443	6.558720
6.177476	476.295452	6.563725
6.244904	474.269560	6.568730
6.131791	477.027194	6.573734
6.360418	479.547782	6.578739
6.125607	477.812859	6.583744
6.412205	467.232430	6.588749
6.551990	469.181628	6.593754
6.352859	472.787990	6.598758
6.013704	472.562745	6.603763
6.072471	475.217517	6.608768
6.115604	474.644466	6.613773
6.161512	469.167042	6.618778
6.343523	481.148462	6.623782
6.168997	479.037089	6.628787
6.191308	476.616459	6.633792
5.810578	480.482235	6.638797
5.909077	477.375772	6.643802
6.443436	482.259298	6.648806
6.350786	483.083789	6.653811
6.120183	481.503234	6.658816
5.653975	490.068042	6.663821
5.991788	481.181723	6.668826
6.008479	478.217794	6.673830
6.407791	478.955712	6.678835
6.368061	478.708864	6.683840
6.542407	485.452183	6.688845
6.410297	481.853490	6.693850
6.373232	483.561472	6.698854
5.851702	472.718507	6.703859
6.380166	475.037088	6.708864
5.933240	481.887238	6.713869
6.261822	471.110399	6.718874
5.990253	481.830914	6.723878
6.153639	469.785951	6.728883
6.073945	482.621481	6.733888
5.982528	481.193129	6.738893
6.481694	478.691457	6.743898
6.173258	482.802177	6.748902
6.174530	483.466416	6.753907
6.399442	473.063332	6.758912
5.804516	462.250856	6.763917
6.338051	475.854025	6.768922
5.973650	468.485641	6.773926
5.889296	466.644886	6.778931
5.934207	474.942938	6.783936
5.928411	476.674496	6.788941
5.994173	475.623325	6.793946
5.956835	477.233270	6.798950
5.943814	472.631969	6.803955
5.801992	464.890183	6.808960
6.113257	478.676880	6.813965
6.270966	474.988485	6.818970
6.083888	476.128335	6.823974
6.023876	475.523987	6.828979
6.253815	479.063124	6.833984
5.924424	480.519508	6.838989
6.212547	478.243896	6.843994
6.071843	486.691261	6.848998
5.951845	481.151241	6.854003
5.781079	483.304125	6.859008
5.788987	473.052103	6.864013
6.236419	474.605078	6.869018
5.918282	477.549863	6.874022
6.062389	495.494728	6.879027
6.785279	504.040917	6.884032
6.488182	484.829236	6.889037
6.276236	476.358095	6.894042
6.457603	479.129703	6.899046
6.118074	483.077612	6.904051
6.491275	492.118358	6.909056
6.136336	475.896081	6.914061
6.190443	470.300311	6.919066
6.179398	473.317206	6.924070
6.167076	466.459984	6.929075
6.230403	480.348806	6.934080
5.847855	470.923610	6.939085
6.287831	477.106438	6.944090
6.436903	484.692132	6.949094
6.471530	480.991383	6.954099
5.827150	479.317468	6.959104
5.880897	480.226591	6.964109
6.081524	478.758810	6.969114
6.170534	472.132489	6.974118
6.096345	472.030248	6.979123
6.235958	478.608159	6.984128
6.234593	487.331094	6.989133
6.623603	481.891660	6.994138
6.284109	482.128387	6.999142
6.464317	471.792421	7.004147
6.006041	458.921029	7.009152
5.836865	454.252448	7.014157
6.032531	463.776587	7.019162
6.115637	473.242434	7.024166
6.371165	477.024340	7.029171
6.671073	475.392304	7.034176
5.958329	469.252280	7.039181
6.045859	460.443152	7.044186
5.786071	457.244128	7.049190
5.947030	475.335032	7.054195
6.270371	477.824961	7.059200
6.128178	484.108498	7.064205
6.085393	483.115463	7.069210
6.375917	485.680139	7.074214
6.331593	482.194245	7.079219
6.325090	461.557628	7.084224
5.714537	461.216715	7.089229
6.117019	471.040655	7.094234
6.243107	481.743158	7.099238
6.242263	480.212029	7.104243
6.380718	461.897099	7.109248
5.685519	458.592285	7.114253
5.962311	465.265760	7.119258
6.034235	478.242049	7.124262
6.210982	476.971004	7.129267
6.431563	472.658976	7.134272
6.226659	478.813128	7.139277
6.229533	468.989014	7.144282
5.826722	464.524719	7.149286
6.130346	472.168452	7.154291
5.904802	477.395671	7.159296
5.966952	480.141664	7.164301
6.471544	477.927051	7.169306
6.241165	482.326105	7.174310
6.265220	471.704549	7.179315
6.064565	469.790265	7.184320
5.991534	477.869511	7.189325
6.419069	475.508779	7.194330
6.158301	469.769350	7.199334
5.687024	471.545364	7.204339
6.078098	472.047285	7.209344
5.379491	480.702286	7.214349
6.017875	476.571575	7.219354
6.394973	483.387532	7.224358
6.384892	475.476400	7.229363
6.126110	479.047815	7.234368
6.007909	479.983880	7.239373
6.347389	475.906329	7.244378
6.361294	481.940775	7.249382
6.085416	475.782922	7.254387
6.605163	465.115343	7.259392
5.847462	479.044215	7.264397
6.299759	473.866958	7.269402
6.173748	480.138466	7.274406
5.675766	472.120278	7.279411
6.377033	475.490651	7.284416
6.388929	482.544166	7.289421
6.310866	482.904452	7.294426
6.122224	485.243639	7.299430
5.909490	479.635890	7.304435
6.087379	478.007152	7.309440
5.872555	486.219352	7.314445
6.040159	480.950653	7.319450
6.111159	482.920121	7.324454
6.079497	475.322426	7.329459
5.997311	476.430022	7.334464
5.813275	485.412536	7.339469
6.131327	470.413630	7.344474
5.908567	474.143920	7.349478
6.085574	474.065599	7.354483
6.161080	473.879791	7.359488
5.967188	476.007823	7.364493
6.373557	470.986462	7.369498
5.981551	471.908477	7.374502
6.068779	475.488956	7.379507
6.208188	474.119354	7.384512
6.126260	474.280924	7.389517
6.183714	477.204827	7.394522
6.413740	483.784393	7.399526
6.120910	488.392555	7.404531
6.242209	473.750349	7.409536
6.053771	484.252191	7.414541
6.548882	475.936030	7.419546
6.393760	477.653018	7.424550
6.237081	488.482089	7.429555
6.331526	485.556598	7.434560
6.110647	480.595546	7.439565
6.182174	479.799742	7.444570
6.367162	483.042194	7.449574
6.079507	468.299548	7.454579
5.997397	469.255267	7.459584
5.924687	478.407001	7.464589
6.335385	477.368226	7.469594
6.093170	477.586548	7.474598
6.111308	470.442972	7.479603
6.136263	466.591877	7.484608
6.255228	477.615041	7.489613
6.361449	485.416262	7.494618
6.190035	472.155057	7.499622
6.098027	465.696309	7.504627
5.798438	467.110056	7.509632
6.151531	472.657911	7.514637
6.602713	466.069761	7.519642
6.073569	462.311812	7.524646
5.851951	465.472432	7.529651
6.182504	462.750402	7.534656
6.173626	473.429753	7.539661
6.098663	477.231801	7.544666
5.958474	479.936729	7.549670
6.043788	479.202041	7.554675
6.127910	482.567868	7.559680
5.779249	483.141398	7.564685
6.303913	478.063535	7.569690
6.248458	483.343201	7.574694
6.322444	477.412112	7.579699
6.566804	480.177014	7.584704
5.895276	467.880043	7.589709
6.233385	466.115469	7.594714
6.350426	472.630474	7.599718
6.036907	456.268845	7.604723
6.049533	461.863713	7.609728
5.949646	471.592355	7.614733
6.234943	466.612112	7.619738
6.442728	470.967822	7.624742
5.865126	466.429670	7.629747
6.148614	464.638852	7.634752
5.958518	470.100966	7.639757
5.844606	460.317302	7.644762
6.203665	476.428251	7.649766
6.223792	477.946934	7.654771
6.437863	483.013524	7.659776
6.129159	485.517060	7.664781
6.280679	481.779012	7.669786
6.034036	468.143610	7.674790
5.729637	483.890269	7.679795
6.135466	479.093623	7.684800
6.062510	481.237510	7.689805
6.156162	476.897911	7.694810
6.230104	485.409724	7.699814
6.060383	487.616231	7.704819
6.224468	477.602334	7.709824
6.029205	485.900056	7.714829
5.949237	476.572985	7.719834
6.048478	489.121049	7.724838
6.000516	478.770208	7.729843
6.336731	477.581747	7.734848
6.185340	483.835086	7.739853
6.109197	473.498154	7.744858
5.917310	474.616610	7.749862
5.748767	478.752868	7.754867
6.269445	484.002379	7.759872
6.122219	490.068402	7.764877
6.273986	477.693052	7.769882
6.287620	476.558297	7.774886
6.197975	479.299599	7.779891
6.077174	479.435621	7.784896
6.240294	477.780723	7.789901
6.184176	474.957919	7.794906
6.118811	476.917114	7.799910
6.082982	482.579693	7.804915
6.216234	471.672103	7.809920
6.319865	472.655669	7.814925
6.109865	478.288587	7.819930
6.330514	479.412012	7.824934
6.141846	480.090191	7.829939
6.155400	481.043578	7.834944
6.294981	488.327032	7.839949
6.105387	483.573055	7.844954
6.197022	483.694775	7.849958
6.450101	494.731739	7.854963
6.223818	463.514891	7.859968
5.778231	454.618449	7.864973
6.189499	459.296623	7.869978
6.103884	478.830904	7.874982
6.027711	483.980936	7.879987
6.399409	481.885223	7.884992
6.335531	475.728956	7.889997
6.200456	469.919212	7.895002
6.134003	460.128112	7.900006
5.944722	464.818122	7.905011
6.276519	458.109473	7.910016
6.151596	455.348074	7.915021
6.016484	457.539663	7.920026
6.217103	460.371528	7.925030
5.765859	458.075718	7.930035
6.199961	462.721841	7.935040
5.893908	469.350593	7.940045
6.247685	473.743542	7.945050
6.229888	478.479456	7.950054
6.093650	477.567505	7.955059
6.080764	475.051146	7.960064
6.128055	476.875628	7.965069
6.284467	486.064236	7.970074
6.420150	476.507218	7.975078
5.839583	458.187887	7.980083
5.883036	459.332746	7.985088
5.951814	483.101355	7.990093
6.099234	470.422963	7.995098
6.291304	474.069274	8.000102
6.283075	479.167530	8.005107
6.338805	472.255351	8.010112
6.382896	481.055235	8.015130
6.433317	468.897691	8.020147
6.484803	461.448378	8.025165
5.997234	454.399103	8.030182
6.053050	446.409484	8.035200
5.704617	446.385216	8.040218
6.155453	452.736575	8.045235
6.153796	464.167022	8.050253
5.869733	463.410000	8.055270
6.409755	470.687808	8.060288
6.292440	477.718322	8.065306
6.284835	468.350094	8.070323
6.162868	465.238725	8.075341
5.794383	454.456464	8.080358
5.948269	468.090507	8.085376
6.135362	473.864669	8.090394
6.177395	476.344856	8.095411
5.886433	478.274466	8.100429
6.093579	477.494128	8.105446
6.475927	475.076902	8.110464
6.362649	470.187476	8.115482
6.199426	471.585839	8.120499
6.201552	470.963854	8.125517
6.299374	472.778901	8.130534
6.275180	470.087706	8.135552
6.284482	483.321543	8.140570
6.380426	467.736021	8.145587
6.458201	469.895031	8.150605
6.219428	478.143763	8.155622
6.443974	469.493389	8.160640
6.168295	469.063252	8.165658
5.916600	470.033670	8.170675
6.113791	480.615630	8.175693
6.173003	481.862379	8.180710
6.001696	472.074836	8.185728
6.141726	481.365579	8.190746
6.088844	479.846510	8.195763
6.373261	466.424713	8.200781
6.201493	474.016015	8.205798
6.527657	474.763352	8.210816
6.672481	474.040115	8.215834
6.291300	470.268779	8.220851
6.359791	473.899828	8.225869
6.279826	473.334886	8.230886
6.399192	464.972389	8.235904
6.151107	473.039544	8.240922
6.282956	477.749405	8.245939
6.414303	465.298320	8.250957
5.788297	473.124891	8.255974
6.372887	474.822646	8.260992
6.549029	495.020362	8.266010
6.582868	488.031389	8.271027
6.566880	472.135201	8.276045
6.152753	468.220707	8.281062
6.165844	474.091558	8.286080
6.191069	488.604143	8.291098
6.532586	498.608086	8.296115
6.556653	487.013228	8.301133
6.759651	494.959225	8.306150
6.591797	488.522554	8.311168
6.358072	484.324174	8.316186
6.084762	478.516248	8.321203
6.447561	485.064447	8.326221
6.414874	503.420369	8.331238
6.666608	498.732518	8.336256
6.658264	506.014209	8.341274
6.305715	494.131221	8.346291
6.584262	487.321655	8.351309
6.345224	490.757898	8.356326
6.490955	489.930378	8.361344
6.482265	496.192808	8.366362
6.409466	503.948494	8.371379
6.584652	502.551477	8.376397
6.115667	508.769267	8.381414
6.811952	499.928203	8.386432
6.931556	497.501648	8.391450
6.428999	498.842728	8.396467
6.563327	493.466382	8.401485
6.468151	498.748298	8.406502
6.455493	497.560591	8.411520
6.725397	504.404215	8.416538
6.398921	507.264033	8.421555
6.766197	508.920102	8.426573
6.715472	509.070092	8.431590
6.796028	488.784871	8.436608
6.463737	486.179816	8.441626
6.369027	489.246311	8.446643
6.213737	483.539810	8.451661
6.502103	500.901854	8.456678
6.911696	496.779398	8.461696
6.913041	497.719639	8.466714
6.635244	488.702999	8.471731
6.172404	486.904183	8.476749
6.370115	493.456161	8.481766
6.927286	495.287601	8.486784
6.956496	497.769800	8.491802
6.725055	497.335886	8.496819
6.947973	476.555009	8.501837
6.690148	485.507309	8.506854
6.586602	470.344355	8.511872
6.201737	474.368324	8.516890
6.484100	490.273337	8.521907
7.070188	489.834407	8.526925
6.966427	497.112110	8.531942
6.832800	482.698619	8.536960
6.499137	470.869492	8.541978
6.326345	480.720481	8.546995
6.568254	489.487189	8.552013
6.517813	499.113893	8.557030
6.399099	495.692743	8.562048
6.676437	498.353813	8.567066
6.528068	495.047762	8.572083
6.506194	494.341175	8.577101
6.738416	510.301398	8.582119
6.735131	492.718022	8.587136
6.319261	495.923199	8.592154
6.382093	502.966522	8.597171
6.715427	498.991713	8.602189
6.706432	493.470568	8.607207
6.927942	490.677757	8.612224
6.784547	506.914577	8.617242
6.786003	509.555758	8.622259
6.823802	499.773307	8.627277
7.012716	498.916930	8.632295
6.874438	491.241721	8.637312
6.900743	496.757063	8.642330
6.542985	497.854552	8.647347
6.713225	497.588074	8.652365
6.741969	497.798196	8.657383
6.997465	499.692682	8.662400
7.109624	499.760347	8.667418
6.645945	501.773825	8.672435
6.660842	498.476906	8.677453
6.558544	500.048759	8.682471
6.257861	506.246491	8.687488
6.674832	514.935290	8.692506
6.792338	523.970812	8.697523
7.090663	523.551722	8.702541
7.124266	519.172595	8.707559
7.073283	529.455801	8.712576
7.123728	530.284209	8.717594
6.834335	514.326681	8.722611
7.083883	507.389108	8.727629
6.663278	504.248784	8.732647
6.831762	506.639736	8.737664
7.129389	515.738549	8.742682
6.745401	508.818189	8.747699
7.037069	511.028897	8.752717
6.986158	520.100271	8.757735
6.853992	519.862239	8.762752
7.104867	514.543365	8.767770
6.907087	506.198982	8.772787
6.916027	503.701404	8.777805
6.976168	512.493446	8.782823
7.171130	517.064042	8.787840
6.940295	502.810931	8.792858
6.717709	508.816548	8.797875
7.117056	522.409018	8.802893
6.914000	516.495399	8.807911
7.338953	528.244049	8.812928
6.877334	510.962838	8.817946
6.704099	506.098576	8.822963
7.276505	508.877516	8.827981
7.389901	517.585479	8.832999
7.103370	498.254000	8.838016
6.961976	490.399400	8.843034
6.704870	497.486538	8.848051
6.967084	510.949009	8.853069
7.167349	513.249776	8.858087
7.023152	528.524232	8.863104
7.060959	508.469746	8.868122
7.074508	520.049323	8.873139
7.180637	515.721949	8.878157
7.156818	518.692136	8.883175
7.206056	516.166151	8.888192
7.121603	502.136255	8.893210
6.947133	504.445243	8.898227
7.010680	504.286999	8.903245
7.436572	514.372404	8.908263
7.117980	504.453288	8.913280
7.108460	495.707032	8.918298
6.829756	502.182181	8.923315
7.378489	505.933650	8.928333
6.872394	507.508811	8.933351
7.116323	523.776477	8.938368
7.496694	533.010656	8.943386
7.165356	520.802439	8.948403
7.052628	510.538643	8.953421
7.238129	516.508725	8.958439
7.128121	523.670655	8.963456
7.378980	523.300027	8.968474
7.254062	513.909132	8.973491
7.131558	501.185375	8.978509
7.449874	505.664058	8.983527
6.929612	502.877015	8.988544
6.950956	500.576307	8.993562
6.669920	518.766031	8.998579
7.145418	521.957783	9.003597
7.357597	524.363981	9.008615
7.145400	532.671691	9.013632
7.391301	516.358894	9.018650
7.137409	526.421429	9.023667
7.103779	516.101056	9.028685
7.326976	520.834484	9.033703
7.360810	530.738332	9.038720
7.326747	521.285861	9.043738
7.544642	529.784955	9.048755
7.450985	513.648438	9.053773
7.420577	517.402287	9.058791
7.451714	523.936195	9.063808
7.391183	519.123697	9.068826
7.292892	525.504317	9.073843
7.298526	530.259212	9.078861
7.479680	519.280343	9.083879
7.300978	522.997468	9.088896
7.387003	518.701645	9.093914
7.427452	526.701527	9.098931
7.284271	516.224751	9.103949
7.323127	509.885071	9.108967
7.170198	521.683235	9.113984
7.540135	516.737021	9.119002
7.276928	527.476350	9.124019
7.206595	520.254380	9.129037
7.579326	514.209522	9.134055
7.417177	525.210723	9.139072
7.288820	521.415543	9.144090
7.401390	526.431390	9.149107
7.689654	517.928797	9.154125
7.551379	515.589981	9.159143
6.994342	522.241289	9.164160
7.256703	516.390446	9.169178
7.265711	519.314465	9.174195
7.201622	524.607296	9.179213
7.526284	522.378981	9.184231
7.326203	520.557927	9.189248
7.345197	510.775260	9.194266
7.248738	514.987576	9.199283
7.102105	521.887003	9.204301
7.255921	516.428703	9.209319
6.920809	519.248851	9.214336
7.347806	533.749014	9.219354
7.621709	543.280744	9.224371
7.555983	551.849532	9.229389
7.684038	544.489173	9.234407
7.505662	544.775927	9.239424
7.726636	539.853047	9.244442
7.412200	533.802240	9.249459
7.402475	529.527727	9.254477
7.307356	543.027275	9.259495
7.521293	535.508297	9.264512
7.864519	545.303718	9.269530
7.913273	549.089352	9.274547
7.836760	537.986742	9.279565
7.530104	525.777810	9.284583
7.386261	529.659887	9.289600
7.538751	523.649533	9.294618
7.481480	528.344857	9.299635
7.840590	519.408290	9.304653
7.503130	524.999571	9.309671
7.424630	522.357902	9.314688
7.924491	533.671946	9.319706
7.625035	526.085090	9.324723
7.673713	535.150336	9.329741
7.628114	517.141225	9.334759
7.713769	530.896459	9.339776
7.451428	514.473949	9.344794
7.763298	532.914770	9.349811
7.672325	545.173451	9.354829
8.185701	522.835396	9.359847
7.396756	532.978611	9.364864
7.625806	520.449064	9.369882
7.566040	532.911129	9.374899
7.353203	531.170966	9.379917
7.801220	543.809096	9.384935
7.735262	550.916798	9.389952
8.005967	548.040532	9.394970
8.204072	547.611899	9.399987
7.580745	541.517969	9.405005
7.512381	531.427089	9.410023
7.435775	536.964880	9.415040
7.611722	544.520666	9.420058
7.695811	558.415020	9.425075
7.863625	547.829539	9.430093
8.136564	547.326065	9.435111
7.616025	545.088164	9.440128
7.767678	541.394272	9.445146
7.911753	552.000376	9.450163
7.499447	552.989651	9.455181
7.882733	552.973812	9.460199
8.071631	553.647986	9.465216
7.650718	558.384515	9.470234
7.796360	553.675403	9.475251
7.700288	554.122830	9.480269
8.190209	553.689500	9.485287
7.904381	555.602535	9.490304
7.665189	555.068850	9.495322
7.843731	553.160067	9.500339
8.016988	549.213483	9.505357
8.158523	553.145526	9.510375
7.890609	548.507523	9.515392
7.705996	539.899131	9.520410
8.098058	544.558772	9.525427
8.180892	541.304848	9.530445
7.832915	534.375680	9.535463
7.592051	531.844654	9.540480
7.865177	544.428136	9.545498
8.171440	547.157264	9.550515
7.773939	552.085781	9.555533
7.827695	544.156401	9.560551
7.799858	538.707621	9.565568
7.860802	552.946421	9.570586
8.033157	550.161303	9.575603
8.040204	553.801995	9.580621
8.268413	547.871287	9.585639
8.042644	547.632141	9.590656
8.163860	549.247873	9.595674
8.224775	531.490300	9.600691
7.587482	535.377109	9.605709
7.846548	540.606690	9.610727
7.756518	544.997886	9.615744
7.752371	558.416920	9.620762
7.624228	551.841462	9.625779
7.469253	557.470432	9.630797
7.886552	545.422609	9.635815
7.705431	548.635196	9.640832
7.659852	550.674688	9.645850
7.645823	569.538990	9.650867
8.026879	566.932607	9.655885
7.978019	573.182423	9.660903
8.345677	586.047767	9.665920
8.137498	573.065985	9.670938
8.531480	569.614984	9.675955
8.063618	573.576240	9.680973
8.226118	571.695215	9.685991
8.037700	571.336609	9.691008
8.217252	572.965293	9.696026
8.126405	574.715238	9.701043
8.109389	577.327766	9.706061
8.729918	569.779783	9.711079
7.806625	565.667335	9.716096
8.028040	565.418084	9.721114
8.415509	568.794049	9.726131
7.973178	574.692108	9.731149
8.087698	571.322763	9.736167
7.888044	573.133936	9.741184
8.269667	577.943542	9.746202
8.090055	575.573326	9.751219
8.052906	573.360667	9.756237
8.247914	569.508500	9.761255
8.049224	578.366375	9.766272
8.192136	570.571335	9.771290
8.532822	567.712504	9.776307
7.805746	567.378335	9.781325
8.035165	571.208250	9.786343
8.079114	576.054984	9.791360
8.201580	575.171146	9.796378
8.468584	570.509286	9.801395
8.200164	579.706288	9.806413
8.297039	574.654520	9.811431
8.505509	575.934694	9.816448
8.355838	580.571926	9.821466
8.434445	568.674983	9.826483
8.250763	575.299371	9.831501
8.308475	574.630804	9.836519
8.280312	574.108235	9.841536
8.204648	576.692082	9.846554
8.715798	578.041596	9.851571
8.248060	573.633709	9.856589
8.451806	572.607749	9.861607
8.343076	574.647672	9.866624
8.241630	575.155901	9.871642
8.491704	581.702863	9.876659
8.540312	579.154878	9.881677
8.398898	579.031902	9.886695
8.782654	574.234985	9.891712
8.596546	575.879936	9.896730
8.597567	571.909841	9.901747
8.638436	575.223349	9.906765
8.968926	579.936827	9.911783
8.756978	572.140582	9.916800
8.499419	561.751127	9.921818
8.528721	555.715883	9.926835
8.264753	558.572226	9.931853
8.356290	552.656618	9.936871
8.524694	567.819014	9.941888
8.311483	573.236209	9.946906
8.552502	575.666298	9.951923
8.446950	573.915633	9.956941
8.383077	569.801072	9.961959
8.934520	570.705620	9.966976
8.877325	566.056687	9.971994
8.569984	548.590323	9.977011
8.255812	553.549965	9.982029
8.563922	553.227171	9.987047
8.560125	559.750786	9.992064
8.415530	571.759114	9.997082
8.354528	570.238153	10.002099
8.805151	584.292847	10.007117
8.823080	568.306053	10.012135
8.223947	567.674130	10.017152
8.384892	576.598732	10.022170
8.649927	564.334914	10.027187
8.473173	578.260685	10.032205
8.542659	578.407620	10.037223
8.808087	570.915274	10.042240
8.598439	578.821821	10.047258
8.357699	577.108116	10.052275
8.708663	574.850427	10.057293
8.817856	569.099304	10.062311
8.878593	567.937962	10.067328
8.738337	576.183927	10.072346
9.129952	571.698201	10.077363
8.538835	577.259814	10.082381
8.628717	571.877786	10.087399
8.817923	570.866728	10.092416
8.816740	570.664977	10.097434
8.548874	569.776025	10.102451
8.279417	578.695480	10.107469
8.503290	576.950005	10.112487
8.928595	582.658477	10.117504
8.854904	583.433755	10.122522
8.795781	575.162287	10.127539
8.652730	584.084031	10.132557
8.606010	578.786519	10.137575
8.758291	583.240743	10.142592
8.529761	584.674593	10.147610
8.706217	581.383903	10.152627
8.847619	587.506085	10.157645
8.868965	591.185570	10.162663
8.781258	582.808125	10.167680
8.464104	593.303483	10.172698
8.914124	580.783454	10.177715
8.433935	579.691085	10.182733
8.566244	578.783614	10.187751
8.945619	586.168691	10.192768
8.723331	595.633025	10.197786
8.787581	592.789100	10.202803
8.842375	604.368581	10.207821
9.260707	607.783899	10.212839
9.242616	596.091435	10.217856
8.770305	585.653564	10.222874
9.068981	584.325554	10.227891
9.227384	583.376125	10.232909
9.189523	578.739939	10.237927
9.356578	578.010059	10.242944
8.989529	573.318155	10.247962
8.927533	572.930274	10.252979
8.793764	575.040391	10.257997
8.647565	574.656235	10.263015
8.692921	570.063817	10.268032
8.678822	580.521153	10.273050
8.741037	570.207822	10.278067
8.843040	581.827228	10.283085
9.217111	590.418645	10.288103
9.163213	588.151805	10.293120
9.116522	605.235091	10.298138
9.229597	589.583662	10.303155
8.740703	591.796759	10.308173
9.052883	581.198107	10.313191
9.397344	594.941242	10.318208
9.009306	588.204521	10.323226
9.022444	577.311900	10.328243
8.904345	584.412006	10.333261
9.074887	592.735514	10.338279
9.601934	590.933069	10.343296
8.777617	583.333750	10.348314
9.114095	575.429485	10.353331
9.073065	582.473334	10.358349
9.086057	594.741007	10.363367
9.180049	600.798038	10.368384
9.145637	599.096185	10.373402
9.351129	596.075496	10.378419
9.238228	588.077534	10.383437
8.988999	595.005687	10.388455
9.231309	599.770855	10.393472
9.197054	606.087822	10.398490
9.495995	590.981623	10.403507
9.512998	586.677663	10.408525
9.055445	586.045647	10.413543
9.030932	574.587731	10.418560
8.815253	593.915995	10.423578
8.927900	587.239681	10.428595
8.657205	604.831430	10.433613
9.057977	608.104333	10.438631
9.241106	612.837752	10.443648
8.712400	610.900921	10.448666
9.009670	604.050508	10.453683
8.664576	622.127298	10.458701
9.098830	625.540125	10.463719
9.728022	620.758389	10.468736
9.597014	615.208987	10.473754
9.579452	607.801989	10.478771
9.479887	601.341955	10.483789
9.241036	601.830688	10.488807
9.448187	597.203445	10.493824
9.355129	604.441645	10.498842
9.160456	604.623658	10.503859
9.495208	605.088790	10.508877
9.029992	603.754234	10.513895
9.107991	596.064028	10.518912
9.369359	618.277698	10.523930
9.365050	626.249923	10.528947
9.427306	625.899377	10.533965
9.211430	638.995041	10.538983
9.537001	624.055055	10.544000
9.876206	624.377480	10.549018
9.577682	611.927374	10.554035
9.238635	603.589300	10.559053
9.471946	612.676150	10.564071
9.392868	608.412485	10.569088
9.369373	620.777410	10.574106
9.606834	621.563898	10.579123
9.917942	619.523885	10.584141
9.360366	610.999142	10.589159
9.369760	599.258188	10.594176
9.293100	605.543929	10.599194
9.719447	610.668427	10.604211
9.931855	627.370313	10.609229
9.369433	616.567848	10.614247
9.601879	602.380924	10.619264
9.521133	601.879216	10.624282
9.415179	605.417704	10.629299
9.558353	612.915539	10.634317
9.328086	626.370053	10.639335
9.764758	619.390495	10.644352
9.671282	624.902555	10.649370
9.734994	610.098282	10.654387
9.659376	617.078136	10.659405
9.180616	617.184740	10.664423
9.315570	615.689876	10.669440
9.445021	626.695945	10.674458
9.463790	625.484371	10.679475
9.864126	627.495031	10.684493
9.744891	629.173691	10.689511
9.677648	629.875377	10.694528
9.585185	626.948703	10.699546
9.730339	630.911753	10.704563
10.079300	627.537223	10.709581
9.521287	634.201348	10.714599
9.738581	625.529944	10.719616
9.550826	620.636367	10.724634
9.539544	641.914492	10.729651
9.896165	625.783062	10.734669
9.579988	629.619579	10.739687
9.634439	623.078601	10.744704
9.629400	628.239136	10.749722
9.541757	624.219805	10.754739
9.609425	627.791055	10.759757
9.686325	640.250716	10.764775
9.850464	628.898906	10.769792
9.633634	630.864254	10.774810
9.800213	627.025996	10.779827
9.801454	628.815167	10.784845
9.838786	628.945049	10.789863
9.715590	623.372330	10.794880
9.740221	633.302923	10.799898
10.073254	642.336294	10.804915
10.514878	635.289683	10.809933
9.484218	634.965209	10.814951
9.505163	627.691025	10.819968
9.943937	643.224531	10.824986
9.590573	645.782471	10.830003
10.054507	639.846357	10.835021
9.885737	645.493295	10.840039
9.931373	649.317308	10.845056
10.247439	641.851712	10.850074
10.095059	642.715061	10.855091
10.140869	641.489781	10.860109
10.175763	634.099800	10.865127
10.337953	618.525858	10.870144
9.712676	625.080598	10.875162
9.941708	627.768191	10.880179
10.120015	620.990059	10.885197
9.849599	616.863668	10.890215
10.414939	625.671285	10.895232
10.231214	621.692255	10.900250
10.044277	625.420160	10.905267
10.445712	621.601910	10.910285
9.903394	628.503414	10.915303
10.219427	609.774833	10.920320
10.242989	609.449285	10.925338
9.960315	609.963819	10.930355
9.901290	619.232174	10.935373
9.549935	619.908948	10.940391
9.853202	625.431428	10.945408
10.162784	628.794362	10.950426
9.842210	644.629880	10.955443
10.305060	641.717183	10.960461
9.861767	647.609105	10.965479
10.341977	643.529200	10.970496
10.288694	640.031499	10.975514
9.792845	646.745849	10.980531
10.635505	637.320052	10.985549
10.265137	649.947628	10.990567
10.498964	651.807656	10.995584
10.535393	637.288501	11.000602
10.003178	635.525785	11.005619
10.151135	622.343001	11.010637
10.054034	643.009727	11.015655
10.308443	639.608984	11.020672
10.667263	640.026165	11.025690
10.322652	634.049479	11.030707
10.280033	623.115074	11.035725
10.208528	618.664029	11.040743
9.951280	630.513322	11.045760
10.295105	638.266906	11.050778
10.140419	639.468285	11.055795
10.440800	637.512002	11.060813
10.074333	648.535824	11.065831
10.067571	646.028063	11.070848
10.641941	636.350814	11.075866
10.193300	641.823852	11.080883
10.447869	638.101193	11.085901
10.582183	648.573184	11.090919
10.296326	634.082437	11.095936
10.636201	633.921922	11.100954
10.290260	645.778811	11.105971
10.797332	641.404365	11.110989
10.543585	644.328548	11.116007
10.431446	645.917735	11.121024
10.791018	637.779452	11.126042
10.302530	637.890735	11.131059
10.603990	634.419504	11.136077
10.449173	639.300554	11.141095
10.221177	636.029042	11.146112
10.839984	636.639017	11.151130
10.101569	645.502595	11.156147
10.703592	639.074633	11.161165
10.963634	643.641376	11.166183
10.087414	634.693177	11.171200
10.227881	639.054593	11.176218
10.337090	645.241799	11.181235
10.699654	644.153082	11.186253
10.650053	643.763257	11.191271
10.692831	642.191316	11.196288
10.659249	644.598167	11.201306
10.622154	644.840696	11.206323
10.567355	643.520728	11.211341
10.478992	645.857267	11.216359
10.547885	648.686718	11.221376
10.813756	641.383621	11.226394
10.786701	645.480953	11.231411
10.953881	642.153836	11.236429
10.544629	648.346536	11.241447
10.995486	641.213269	11.246464
10.999024	634.560344	11.251482
10.653581	622.982268	11.256499
10.601636	619.799940	11.261517
10.768308	618.129695	11.266535
10.510207	619.075878	11.271552
10.718598	625.859759	11.276570
10.867531	642.357011	11.281587
10.952414	633.296097	11.286605
10.645736	631.166686	11.291623
10.589314	635.871373	11.296640
10.827641	638.989855	11.301658
10.600953	651.907343	11.306675
10.651103	642.858177	11.311693
10.758305	637.243043	11.316711
10.634789	641.071467	11.321728
10.877705	638.644507	11.326746
10.602682	645.652459	11.331763
10.995136	640.352391	11.336781
10.934418	642.747715	11.341799
10.651953	644.123748	11.346816
10.635264	639.885014	11.351834
10.695886	637.672808	11.356851
10.564716	641.423537	11.361869
10.900852	653.015773	11.366887
10.853835	648.526170	11.371904
10.942383	640.897406	11.376922
10.545944	651.383131	11.381939
10.763820	649.455552	11.386957
10.705688	653.519886	11.391975
10.804204	667.841253	11.396992
11.164208	662.259085	11.402010
10.726007	680.830203	11.407027
11.127222	669.759958	11.412045
11.178182	675.546047	11.417063
10.842149	675.920621	11.422080
10.804447	670.754212	11.427098
11.024926	676.229720	11.432115
10.758735	673.052548	11.437133
10.980643	668.618634	11.442151
11.124941	672.373546	11.447168
10.925283	667.989904	11.452186
11.116845	674.880582	11.457203
11.112511	667.089636	11.462221
11.255455	665.644010	11.467239
10.925013	671.934823	11.472256
11.063769	667.324590	11.477274
11.154167	680.359675	11.482291
10.835627	669.897661	11.487309
11.264890	669.196122	11.492327
11.346415	673.904452	11.497344
11.495087	668.484781	11.502362
11.399706	672.460282	11.507379
11.052225	673.931710	11.512397
10.939771	665.251992	11.517415
10.796930	669.689362	11.522432
11.036454	670.200975	11.527450
10.836026	673.340870	11.532467
10.916376	665.224232	11.537485
11.093444	664.773646	11.542503
11.024992	688.834727	11.547520
11.409464	694.369752	11.552538
11.302461	698.511181	11.557555
11.558369	688.694453	11.562573
11.634597	693.738132	11.567591
11.471858	678.132997	11.572608
11.170946	669.170380	11.577626
10.995010	676.112327	11.582643
11.316945	681.060701	11.587661
11.657345	688.616029	11.592679
11.295632	686.706673	11.597696
11.878854	682.840993	11.602714
11.559618	682.316689	11.607731
11.702534	668.105871	11.612749
11.650375	665.993383	11.617767
11.284707	669.215971	11.622784
11.349694	665.327351	11.627802
11.386293	661.582034	11.632819
11.240164	668.746524	11.637837
11.565356	662.907880	11.642855
11.457478	667.301902	11.647872
11.408571	659.751472	11.652890
11.426565	665.220832	11.657907
11.232512	662.874956	11.662925
11.478453	661.239624	11.667943
11.530193	685.767861	11.672960
12.076897	681.421911	11.677978
11.598315	679.451972	11.682995
11.480536	679.498861	11.688013
11.609341	667.650791	11.693031
11.590491	669.657707	11.698048
11.432008	664.986749	11.703066
11.140188	664.341386	11.708083
11.385186	685.320633	11.713101
11.863930	676.273726	11.718119
11.374479	683.861243	11.723136
11.874106	686.474890	11.728154
11.739572	692.034428	11.733171
11.838392	691.858032	11.738189
12.157773	686.957562	11.743207
11.863341	679.780107	11.748224
11.804253	667.589092	11.753242
11.764742	665.824915	11.758259
11.550682	663.103479	11.763277
11.650703	659.670117	11.768295
11.507149	664.890234	11.773312
11.877111	664.825990	11.778330
11.612270	659.376438	11.783347
11.769698	665.934791	11.788365
11.711215	671.554990	11.793383
11.379864	678.164683	11.798400
11.683104	682.677331	11.803418
11.569196	683.742936	11.808435
11.627965	692.503725	11.813453
12.052515	685.844777	11.818471
11.817397	691.899756	11.823488
12.202190	680.980399	11.828506
12.163605	684.631423	11.833523
11.900190	691.713314	11.838541
12.209547	683.352505	11.843559
11.798847	688.589239	11.848576
12.199034	679.579885	11.853594
12.057322	672.997041	11.858611
11.471362	659.891350	11.863629
12.007134	666.936377	11.868647
12.005420	672.926377	11.873664
12.296641	668.566810	11.878682
12.045705	663.941896	11.883699
11.659096	662.030132	11.888717
11.955189	667.373870	11.893735
11.921637	683.609418	11.898752
11.831758	679.574646	11.903770
11.724614	673.737465	11.908787
11.756517	680.451190	11.913805
11.801207	680.826072	11.918823
11.794633	690.979337	11.923840
11.717165	678.362006	11.928858
12.010962	679.322706	11.933875
11.918925	685.371044	11.938893
11.843338	676.474105	11.943911
11.866147	687.058264	11.948928
12.127936	699.460596	11.953946
12.309343	709.354045	11.958963
12.388194	706.160676	11.963981
12.488102	684.149133	11.968999
12.183529	688.062739	11.974016
11.806992	680.538387	11.979034
12.079130	689.982109	11.984051
12.124211	704.106751	11.989069
12.557988	695.237293	11.994087
12.444511	694.586076	11.999104
12.097324	688.199521	12.004122
12.135961	682.516221	12.009139
12.087733	687.500503	12.014157
12.253931	689.983356	12.019175
12.231978	694.991926	12.024192
12.256849	702.091768	12.029210
12.362939	703.192333	12.034227
12.458599	704.849953	12.039245
13.002187	698.405878	12.044263
12.475380	689.658525	12.049280
12.334933	687.809175	12.054298
12.229545	679.743723	12.059315
12.161778	687.688049	12.064333
12.068452	684.133497	12.069351
12.445714	706.016694	12.074368
12.261362	703.287442	12.079386
12.464767	704.874531	12.084403
12.580986	702.814552	12.089421
12.557502	696.778063	12.094439
12.233023	699.684935	12.099456
12.439666	708.687649	12.104474
12.284474	702.561341	12.109491
12.402481	709.747580	12.114509
12.430179	706.707392	12.119527
12.812578	698.013240	12.124544
13.119173	700.095401	12.129562
12.555456	684.811860	12.134579
12.338959	685.038318	12.139597
12.739661	679.916826	12.144615
12.509104	672.145544	12.149632
12.491755	673.287537	12.154650
12.780780	675.886843	12.159667
12.166351	683.598082	12.164685
12.425626	686.924729	12.169703
12.475695	696.845060	12.174720
12.860784	706.706595	12.179738
12.564652	701.217751	12.184755
12.380653	697.996139	12.189773
12.674150	701.055495	12.194791
12.732344	703.059811	12.199808
12.994556	695.170285	12.204826
13.046932	696.629559	12.209843
12.680719	700.082611	12.214861
12.835011	699.881746	12.219879
12.810662	702.413390	12.224896
12.702554	704.273349	12.229914
12.700583	700.732883	12.234931
12.715320	700.960980	12.239949
13.066684	698.346608	12.244967
12.814564	699.721047	12.249984
12.590122	710.492281	12.255002
12.692329	695.637725	12.260019
12.513760	699.506345	12.265037
12.997899	701.901515	12.270055
12.630028	698.412066	12.275072
12.532517	704.937794	12.280090
12.648673	702.789463	12.285107
12.565440	705.122050	12.290125
12.797174	703.479473	12.295143
12.789297	704.910318	12.300160
12.948207	713.210459	12.305178
13.001196	703.185675	12.310195
12.927527	698.996880	12.315213
12.950128	705.724695	12.320231
12.776473	699.339349	12.325248
12.769473	703.076947	12.330266
12.963093	712.693930	12.335283
13.125041	726.244857	12.340301
13.361443	721.464676	12.345319
13.054622	702.303413	12.350336
13.036534	703.000556	12.355354
12.882006	697.470592	12.360371
12.752525	707.668370	12.365389
13.227825	708.079927	12.370407
13.212831	721.608080	12.375424
13.400214	726.176762	12.380442
13.142066	703.915182	12.385459
12.861177	713.246749	12.390477
12.760554	709.112668	12.395495
13.293224	715.959385	12.400512
13.298096	714.544855	12.405530
13.454937	713.519925	12.410547
12.989198	725.607075	12.415565
13.016562	722.380745	12.420583
13.429833	720.119587	12.425600
13.208900	719.172781	12.430618
13.359920	722.522707	12.435635
13.257663	725.502062	12.440653
13.628833	721.959932	12.445671
13.150168	708.607021	12.450688
12.939672	716.706266	12.455706
13.332244	711.604974	12.460723
13.552558	727.889150	12.465741
13.494417	704.400182	12.470759
13.330417	707.127277	12.475776
13.451576	701.598298	12.480794
13.202150	690.102963	12.485811
12.969681	706.884095	12.490829
13.137558	709.858993	12.495847
13.299322	719.077027	12.500864
13.348403	728.407396	12.505882
13.279481	721.778415	12.510899
13.032994	728.554711	12.515917
13.275500	722.467070	12.520935
13.487665	723.847662	12.525952
13.285972	720.322705	12.530970
13.733059	718.605359	12.535987
13.315788	718.598187	12.541005
13.535626	715.960238	12.546023
13.240512	716.981653	12.551040
13.271389	716.986316	12.556058
13.595941	713.928018	12.561075
13.218858	724.802072	12.566093
13.405182	730.633242	12.571111
13.743331	737.996439	12.576128
13.964482	742.562990	12.581146
14.059119	741.137549	12.586163
13.548908	727.830591	12.591181
13.810765	725.356471	12.596199
14.040534	716.320151	12.601216
13.676474	725.295527	12.606234
13.616726	713.783082	12.611251
14.084433	725.537788	12.616269
13.590805	728.430140	12.621287
13.961846	717.882145	12.626304
13.636637	723.739811	12.631322
14.108809	720.153455	12.636339
13.627737	723.794921	12.641357
13.791337	718.442324	12.646375
13.484412	729.620969	12.651392
13.684106	717.474581	12.656410
13.588964	719.259926	12.661427
13.581161	722.682074	12.666445
13.613401	720.815131	12.671463
13.848941	719.897791	12.676480
13.463605	724.837072	12.681498
13.752617	724.899120	12.686515
14.080024	727.460862	12.691533
13.616388	727.432551	12.696551
14.420301	734.413502	12.701568
13.961651	725.052694	12.706586
14.005636	715.297557	12.711603
14.100432	718.470099	12.716621
13.904228	717.642495	12.721639
13.488286	710.704971	12.726656
13.915996	724.233192	12.731674
14.362425	727.041373	12.736691
14.009404	735.093529	12.741709
14.054705	727.408389	12.746727
13.778215	721.313703	12.751744
13.791196	726.550338	12.756762
14.556953	744.661487	12.761779
14.112320	739.536726	12.766797
13.903165	729.562467	12.771815
14.238610	723.955726	12.776832
14.146939	729.271875	12.781850
14.028452	715.985601	12.786867
14.293617	717.796545	12.791885
13.709935	730.681661	12.796903
14.518041	726.499871	12.801920
14.084542	736.505457	12.806938
14.255042	735.519411	12.811955
14.287961	735.287069	12.816973
14.066359	739.948235	12.821991
14.503889	730.421764	12.827008
14.090559	724.026625	12.832026
14.144147	726.053756	12.837043
14.317120	737.217175	12.842061
14.180758	734.676059	12.847079
14.454738	734.030406	12.852096
14.458919	733.786787	12.857114
14.217361	738.823465	12.862131
14.480206	724.543320	12.867149
14.186268	727.057246	12.872167
14.461491	727.130922	12.877184
14.226795	731.481714	12.882202
14.563224	734.805748	12.887219
14.424480	728.266599	12.892237
14.272120	724.380462	12.897255
14.032022	726.712384	12.902272
14.504825	740.886804	12.907290
14.654962	747.714573	12.912307
14.910410	744.383074	12.917325
14.228676	735.382261	12.922343
14.429699	740.242299	12.927360
14.486482	740.154540	12.932378
14.285229	734.464628	12.937395
14.642204	748.631956	12.942413
14.339712	746.239943	12.947431
14.944614	745.192146	12.952448
14.844432	746.586964	12.957466
14.557220	731.799703	12.962483
14.636146	736.366446	12.967501
14.502793	742.765259	12.972519
14.671211	736.111709	12.977536
14.824383	745.419466	12.982554
14.628793	734.600479	12.987571
14.415475	734.662337	12.992589
14.510831	742.271860	12.997607
14.540820	738.069970	13.002624
14.594907	740.595642	13.007642
14.615964	745.067312	13.012659
14.375479	739.194196	13.017677
14.247560	750.329029	13.022695
14.190319	738.289155	13.027712
14.478313	747.228650	13.032730
14.844711	761.356642	13.037747
14.961647	751.880390	13.042765
14.836943	766.413535	13.047783
14.587876	753.769388	13.052800
14.810874	762.337222	13.057818
14.559823	764.775006	13.062835
14.898381	755.295587	13.067853
14.711966	770.150830	13.072871
15.026126	765.229066	13.077888
14.933473	756.265334	13.082906
14.983382	766.933657	13.087923
15.425307	763.153214	13.092941
14.989632	762.334726	13.097959
15.386093	754.379960	13.102976
14.948972	748.117927	13.107994
14.861577	744.666575	13.113011
15.014076	738.435241	13.118029
14.979145	751.019799	13.123047
15.200712	745.566594	13.128064
15.568298	749.627364	13.133082
15.050493	740.386269	13.138099
14.812140	742.645336	13.143117
14.960663	738.169254	13.148135
15.039109	736.430770	13.153152
15.042485	732.879992	13.158170
15.050569	746.628611	13.163187
15.339580	749.903273	13.168205
15.072035	755.193337	13.173223
15.181730	752.932402	13.178240
15.437920	754.959351	13.183258
15.047507	754.657636	13.188275
15.200546	754.826195	13.193293
14.992991	759.390492	13.198311
15.315625	753.763658	13.203328
15.277854	750.654825	13.208346
15.178463	753.457011	13.213363
15.190764	752.574646	13.218381
15.084805	753.339207	13.223399
15.392703	744.271697	13.228416
15.677389	752.993963	13.233434
15.275311	755.291307	13.238451
15.448930	747.639702	13.243469
15.750988	763.292565	13.248487
15.671812	753.875441	13.253504
15.441285	744.753435	13.258522
15.141611	733.944444	13.263539
15.107705	737.853522	13.268557
15.389122	743.922262	13.273575
15.492476	746.007870	13.278592
15.706180	754.359406	13.283610
15.591413	748.163632	13.288627
15.475797	746.657524	13.293645
15.383216	746.312301	13.298663
15.633394	748.393840	13.303680
15.233085	741.595866	13.308698
14.963954	753.264066	13.313715
15.311827	750.161082	13.318733
14.966165	758.025903	13.323751
15.051799	752.167959	13.328768
15.411682	762.443729	13.333786
15.419707	774.387255	13.338803
15.708786	773.253240	13.343821
15.662908	780.802857	13.348839
15.670100	779.236479	13.353856
15.896173	773.751001	13.358874
15.759891	784.937658	13.363891
15.929524	778.422758	13.368909
15.614299	782.470597	13.373927
16.049423	780.755120	13.378944
16.010392	781.234641	13.383962
15.748261	776.336895	13.388979
15.669492	774.440003	13.393997
15.514841	783.896996	13.399015
15.716586	776.629137	13.404032
15.693943	773.827199	13.409050
15.923969	778.171462	13.414067
16.343996	770.960923	13.419085
16.159857	779.125495	13.424103
16.451824	775.851385	13.429120
16.291703	765.471791	13.434138
16.019430	747.516897	13.439155
16.012588	751.794124	13.444173
16.102843	748.876671	13.449191
16.048908	752.451220	13.454208
15.861449	747.595431	13.459226
15.789117	746.502264	13.464243
15.800160	748.135276	13.469261
15.788708	744.533170	13.474279
16.110612	744.858309	13.479296
16.120101	748.530217	13.484314
15.853638	759.560529	13.489331
16.139516	766.540608	13.494349
16.291566	776.385045	13.499367
16.172848	762.915736	13.504384
16.423426	758.215375	13.509402
15.888259	748.645636	13.514419
15.973086	745.470258	13.519437
16.137387	755.388504	13.524455
16.355703	763.922358	13.529472
16.284680	765.126416	13.534490
16.073375	763.935101	13.539507
16.307928	754.954817	13.544525
15.926579	767.937647	13.549543
16.088217	776.770722	13.554560
16.650610	773.129194	13.559578
16.237574	775.753306	13.564595
15.993049	770.691857	13.569613
16.210966	777.669964	13.574631
16.211328	767.325185	13.579648
16.216334	774.835269	13.584666
16.359452	780.742653	13.589683
16.814731	774.624814	13.594701
16.612554	769.282174	13.599719
16.524249	778.122853	13.604736
16.290900	775.284501	13.609754
16.378283	776.189185	13.614771
16.635988	774.760283	13.619789
16.633630	778.617090	13.624807
16.226600	764.527075	13.629824
16.678436	775.766748	13.634842
16.534555	765.605516	13.639859
16.722095	763.881495	13.644877
16.570503	775.982574	13.649895
15.986296	779.646522	13.654912
16.425511	769.750536	13.659930
16.468440	773.647584	13.664947
16.853868	768.531616	13.669965
16.408162	773.874846	13.674983
16.600918	770.909772	13.680000
16.757753	776.953862	13.685018
16.371459	776.102389	13.690035
16.866338	770.073021	13.695053
16.995762	770.885911	13.700071
16.709992	771.587127	13.705088
16.589331	773.972925	13.710106
16.642411	774.024602	13.715123
16.706100	766.964571	13.720141
16.827261	774.046200	13.725159
16.532593	774.164985	13.730176
17.043811	776.063616	13.735194
16.946896	776.476466	13.740211
16.877773	766.827386	13.745229
16.504162	777.154972	13.750247
16.768659	793.132483	13.755264
16.879870	786.986497	13.760282
16.728784	803.202700	13.765299
17.030184	795.811921	13.770317
17.207343	801.174334	13.775335
16.766714	799.782261	13.780352
17.216083	791.806565	13.785370
16.756364	799.102292	13.790387
17.211500	787.928851	13.795405
17.243616	783.319518	13.800423
17.140476	781.865101	13.805440
17.152395	781.531906	13.810458
17.253234	787.581617	13.815475
17.021445	781.195883	13.820493
16.948423	776.779750	13.825511
16.849830	780.336054	13.830528
17.099125	779.485983	13.835546
17.165171	787.374674	13.840563
17.625225	788.164164	13.845581
17.625852	777.503755	13.850599
17.512167	777.048229	13.855616
17.750463	767.208970	13.860634
17.409063	769.746118	13.865651
16.878439	762.198536	13.870669
17.295802	763.524890	13.875687
17.034504	762.726417	13.880704
17.088967	751.464297	13.885722
16.930920	767.498521	13.890739
17.228183	780.990419	13.895757
17.766907	774.897375	13.900775
17.502306	781.345169	13.905792
17.488133	767.373481	13.910810
17.266082	767.581874	13.915827
17.078790	762.817574	13.920845
17.237361	772.443236	13.925863
17.094073	782.466495	13.930880
17.678917	779.023420	13.935898
17.719977	794.354284	13.940915
17.768428	783.364486	13.945933
17.766211	789.717523	13.950951
17.322425	789.294781	13.955968
17.464566	787.969192	13.960986
17.718293	788.942488	13.966003
17.848782	796.603335	13.971021
17.752103	790.559347	13.976039
17.513459	791.682372	13.981056
17.863245	789.251271	13.986074
17.485818	774.721107	13.991091
17.590272	789.357223	13.996109
17.407571	786.308961	14.001127
17.218987	792.675420	14.006144
17.558219	784.634932	14.011162
17.639267	794.149676	14.016179
17.968424	785.530096	14.021197
17.849719	783.147152	14.026215
17.491944	791.932228	14.031232
17.463276	792.631033	14.036250
17.741217	793.903494	14.041267
17.529145	786.337549	14.046285
17.539249	789.633827	14.051303
17.752708	802.968458	14.056320
18.126006	803.307636	14.061338
18.330582	809.404217	14.066355
17.293973	797.599801	14.071373
18.032394	800.100312	14.076391
17.899341	815.512123	14.081408
18.188796	804.017491	14.086426
18.333269	808.286802	14.091443
18.003067	799.966184	14.096461
17.642489	800.038491	14.101479
17.759271	808.398926	14.106496
17.950332	800.703540	14.111514
18.011813	809.173626	14.116531
17.970184	812.285508	14.121549
18.131512	802.079591	14.126567
17.898916	809.058869	14.131584
18.115588	802.931068	14.136602
18.390395	806.198498	14.141619
18.098674	807.471852	14.146637
18.508851	796.034050	14.151655
18.469227	809.667116	14.156672
18.415735	794.186773	14.161690
18.756248	802.609982	14.166707
18.456510	795.553232	14.171725
18.238979	776.033914	14.176743
17.887788	778.275951	14.181760
18.122420	792.008045	14.186778
18.064528	795.586377	14.191795
18.190050	802.922955	14.196813
18.447665	798.259352	14.201831
18.252567	798.204746	14.206848
18.278168	792.520297	14.211866
18.494126	794.875448	14.216883
18.425722	795.754048	14.221901
18.481235	800.346566	14.226919
18.222828	798.465193	14.231936
18.436081	799.602622	14.236954
18.260628	796.161901	14.241971
18.307331	791.231543	14.246989
18.361587	790.642405	14.252007
18.586363	804.426546	14.257024
18.802618	794.218339	14.262042
18.277447	792.640696	14.267059
18.217298	788.550748	14.272077
18.443224	800.034116	14.277095
18.630494	817.876214	14.282112
18.815460	818.525768	14.287130
19.042429	819.803062	14.292147
18.704683	810.540030	14.297165
18.918266	799.691608	14.302183
18.782850	802.732976	14.307200
18.568553	781.875078	14.312218
18.689134	790.758775	14.317235
18.658485	802.257097	14.322253
18.999751	808.105043	14.327271
19.212142	812.893892	14.332288
18.776083	802.137786	14.337306
18.766915	797.389749	14.342323
18.572638	796.760656	14.347341
19.035888	808.904281	14.352359
18.899718	814.735514	14.357376
18.900461	812.390656	14.362394
19.226438	813.769202	14.367411
18.977804	807.726926	14.372429
18.565510	806.077947	14.377447
18.894782	809.841776	14.382464
19.131797	815.605072	14.387482
19.119314	815.348283	14.392499
18.760726	819.772157	14.397517
18.859136	814.439212	14.402535
18.939047	817.039745	14.407552
19.257548	824.393433	14.412570
19.166479	825.294521	14.417587
18.834878	816.563857	14.422605
19.013787	819.925211	14.427623
18.956437	826.053369	14.432640
19.051075	817.577816	14.437658
19.107834	818.610377	14.442675
18.871999	828.430410	14.447693
19.092996	830.112585	14.452711
19.653309	834.067439	14.457728
19.448238	830.019123	14.462746
19.387314	823.846444	14.467763
18.818898	824.976958	14.472781
19.253637	821.907690	14.477799
19.767032	835.709751	14.482816
19.812919	842.670656	14.487834
19.383762	818.535919	14.492851
19.332213	826.954295	14.497869
19.619281	818.953523	14.502887
19.574804	817.287939	14.507904
19.486649	816.421310	14.512922
19.470077	816.221968	14.517939
19.131401	821.854557	14.522957
19.579118	814.415599	14.527975
19.133629	826.367100	14.532992
19.741755	838.778382	14.538010
19.898018	826.951151	14.543027
19.790887	829.199136	14.548045
19.673866	817.247470	14.553063
19.530200	809.430955	14.558080
19.444145	817.829486	14.563098
19.595977	818.282260	14.568115
19.623034	827.212186	14.573133
20.087776	834.880639	14.578151
19.701923	820.739924	14.583168
19.564608	820.736225	14.588186
19.815980	819.159988	14.593203
19.643144	836.342155	14.598221
19.998208	822.934269	14.603239
19.885002	830.494455	14.608256
20.036293	826.901548	14.613274
19.730911	822.793210	14.618291
20.018658	835.021156	14.623309
19.749060	823.033431	14.628327
19.880194	825.985703	14.633344
20.198536	828.533101	14.638362
20.099885	820.018403	14.643379
20.140285	812.734783	14.648397
20.266664	799.766689	14.653415
20.275799	808.847738	14.658432
19.983406	806.116462	14.663450
20.246102	809.035495	14.668467
19.938204	818.077858	14.673485
19.904469	809.887510	14.678503
19.991549	809.264827	14.683520
19.532005	811.495442	14.688538
19.891913	829.859616	14.693555
20.155634	838.635703	14.698573
20.394497	830.661413	14.703591
20.373163	839.343306	14.708608
20.235997	836.477250	14.713626
20.216551	833.049949	14.718643
20.232572	840.542556	14.723661
19.997757	839.345452	14.728679
20.478697	843.473691	14.733696
20.113660	844.547094	14.738714
20.494842	829.983234	14.743731
20.331249	838.722129	14.748749
20.303384	836.104038	14.753767
19.975503	838.736908	14.758784
19.813165	838.342651	14.763802
20.531867	833.067150	14.768819
20.289482	846.154497	14.773837
20.399865	845.300941	14.778855
20.545964	838.202723	14.783872
20.273717	847.324722	14.788890
20.753578	843.781318	14.793907
20.398100	841.123037	14.798925
20.284651	844.467086	14.803943
20.641940	858.454570	14.808960
20.674944	868.314555	14.813978
20.442023	869.525050	14.818995
20.533414	870.539565	14.824013
20.674580	863.473668	14.829031
20.690728	856.392648	14.834048
20.544068	866.744688	14.839066
20.896478	873.181049	14.844083
20.940989	867.506237	14.849101
20.755415	867.203983	14.854119
20.809597	868.902831	14.859136
20.710700	860.880462	14.864154
21.176250	861.170473	14.869171
21.078153	859.241886	14.874189
20.850471	852.110707	14.879207
21.280711	854.842549	14.884224
21.063141	842.663622	14.889242
20.942767	830.362176	14.894259
20.792707	831.913139	14.899277
20.546221	832.898539	14.904295
20.677661	846.993984	14.909312
20.839178	850.733612	14.914330
21.085685	846.709214	14.919347
20.897425	854.770323	14.924365
20.985366	846.870166	14.929383
20.793979	851.141617	14.934400
20.792916	860.530404	14.939418
21.098904	843.548327	14.944435
21.156755	853.937745	14.949453
21.395182	855.812853	14.954471
21.231737	850.363134	14.959488
21.060316	856.805823	14.964506
21.307235	853.453550	14.969523
21.099163	856.257000	14.974541
20.805312	851.951187	14.979559
21.213730	852.590979	14.984576
20.791500	858.410241	14.989594
21.339681	861.849447	14.994611
21.506462	873.228519	14.999629
21.597825	879.213473	15.004647
21.656509	879.601947	15.009664
21.399516	868.899796	15.014682
21.501674	853.723221	15.019699
21.621461	856.077668	15.024717
21.358970	848.891984	15.029735
21.549746	858.443219	15.034752
21.221182	858.377965	15.039770
21.012371	878.690080	15.044787
21.192427	876.982999	15.049805
21.517454	884.329379	15.054823
21.854159	869.176003	15.059840
21.557132	875.707806	15.064858
21.876375	880.517802	15.069875
21.769889	886.177148	15.074893
21.477110	879.725194	15.079911
21.978135	880.877502	15.084928
21.441113	885.884774	15.089946
22.028871	883.053455	15.094963
22.072748	877.362960	15.099981
21.778910	880.722655	15.104999
21.692632	874.604425	15.110016
21.795324	884.005372	15.115034
21.945533	880.870219	15.120051
21.789820	886.884420	15.125069
21.700238	884.809327	15.130087
22.097265	878.956202	15.135104
21.852035	880.632535	15.140122
21.713004	867.816430	15.145139
21.915923	882.790648	15.150157
21.740277	881.439102	15.155175
22.077734	869.911660	15.160192
21.736103	880.376307	15.165210
21.732616	866.828904	15.170227
21.565215	871.857156	15.175245
21.888485	887.847635	15.180263
22.169097	884.218676	15.185280
22.064269	897.246637	15.190298
22.330187	901.635800	15.195315
22.336710	895.424127	15.200333
22.114581	897.062127	15.205351
22.735191	889.652855	15.210368
22.201126	888.957074	15.215386
22.008325	871.690198	15.220403
22.450519	881.722766	15.225421
22.208214	888.447974	15.230439
22.630962	890.568764	15.235456
22.275321	876.262324	15.240474
22.355163	874.728737	15.245491
22.366719	877.687129	15.250509
22.349630	888.779436	15.255527
22.156102	886.644890	15.260544
22.033177	892.054347	15.265562
22.309486	891.260000	15.270579
22.323344	888.547000	15.275597
22.178500	896.118483	15.280615
22.580245	890.233057	15.285632
22.578968	897.059360	15.290650
22.696819	883.836919	15.295667
22.309149	880.372627	15.300685
22.444220	897.894778	15.305703
22.223291	887.515172	15.310720
22.536692	891.401427	15.315738
22.599344	895.822435	15.320755
22.751467	909.378198	15.325773
22.722006	923.842900	15.330791
23.180743	915.326033	15.335808
22.655522	901.854036	15.340826
22.684493	890.071953	15.345843
23.458612	894.952696	15.350861
22.975636	892.737265	15.355879
22.986199	886.354547	15.360896
22.899284	883.644714	15.365914
22.917820	882.903378	15.370931
22.721715	893.402037	15.375949
22.784386	890.517286	15.380967
22.648183	888.714588	15.385984
22.900831	896.561467	15.391002
23.142319	906.426677	15.396019
23.141542	910.327447	15.401037
23.369728	913.027840	15.406055
23.191107	902.023053	15.411072
22.902852	897.631144	15.416090
23.108699	901.196578	15.421107
23.580580	902.511245	15.426125
23.255344	908.179626	15.431143
23.422615	892.080779	15.436160
23.342877	890.619531	15.441178
23.020854	889.647528	15.446195
23.020910	891.241249	15.451213
22.775536	892.346399	15.456231
23.053190	902.117577	15.461248
23.373375	912.314447	15.466266
23.127046	910.200794	15.471283
23.412271	911.241746	15.476301
22.896259	918.675731	15.481319
23.172929	916.309719	15.486336
23.256151	912.932589	15.491354
23.503414	914.452865	15.496371
23.783543	912.436610	15.501389
23.387406	920.555565	15.506407
23.584320	917.624530	15.511424
23.495368	912.791132	15.516442
23.622693	909.047328	15.521459
23.904554	908.056448	15.526477
23.885900	905.607319	15.531495
23.518229	915.356535	15.536512
23.613006	914.514889	15.541530
23.637460	905.141410	15.546547
23.747858	910.675263	15.551565
23.528998	913.038596	15.556583
23.812527	921.319309	15.561600
23.945607	907.135089	15.566618
23.424766	913.752466	15.571635
23.866042	914.513346	15.576653
23.559999	914.065863	15.581671
23.563352	906.715426	15.586688
23.865092	923.028049	15.591706
23.888973	937.241404	15.596723
24.265341	930.397409	15.601741
24.135221	924.547966	15.606759
24.306184	917.095522	15.611776
24.241734	909.209747	15.616794
23.999586	910.058769	15.621811
24.008686	910.663298	15.626829
23.792802	908.140927	15.631847
23.910527	904.363913	15.636864
23.887921	907.255079	15.641882
24.087384	924.230675	15.646899
24.405660	934.617207	15.651917
24.346107	940.871983	15.656935
24.525696	920.444521	15.661952
24.237957	910.315214	15.666970
23.993034	906.241565	15.671987
24.378090	919.208567	15.677005
23.962548	920.400342	15.682023
24.131708	920.187677	15.687040
24.275741	926.842900	15.692058
24.200357	933.557751	15.697075
24.295931	925.138805	15.702093
24.123232	935.842108	15.707111
24.382688	923.238087	15.712128
24.471986	925.663593	15.717146
24.243873	936.271435	15.722163
24.142262	924.055348	15.727181
24.292522	930.438195	15.732199
24.295040	929.459523	15.737216
24.794375	948.325845	15.742234
24.625341	940.371234	15.747251
24.803544	946.011241	15.752269
24.212676	937.728243	15.757287
24.856282	948.243694	15.762304
24.944729	949.378597	15.767322
24.813391	948.957389	15.772339
24.832152	938.574914	15.777357
24.683714	933.239584	15.782375
24.390604	937.485967	15.787392
24.919482	941.079693	15.792410
24.767508	940.254616	15.797427
25.022662	947.368969	15.802445
25.148280	952.171451	15.807463
24.813060	948.948239	15.812480
25.101867	943.042620	15.817498
24.681060	947.495208	15.822515
24.934119	946.404696	15.827533
24.790532	955.304618	15.832551
25.000814	945.087793	15.837568
25.221687	943.611000	15.842586
24.842947	945.144153	15.847603
25.076671	939.764724	15.852621
25.429133	938.418794	15.857639
25.353125	941.037462	15.862656
25.321343	940.266138	15.867674
24.920847	941.496582	15.872691
25.154336	941.930253	15.877709
25.044652	942.868977	15.882727
24.937776	937.763823	15.887744
25.207464	943.809223	15.892762
25.066094	931.176477	15.897779
24.905094	935.578888	15.902797
25.069981	945.408785	15.907815
25.492000	951.992061	15.912832
25.750105	966.459080	15.917850
25.204690	956.815093	15.922867
25.446101	963.205761	15.927885
25.413450	966.950589	15.932903
25.554292	965.243333	15.937920
25.719853	964.964958	15.942938
25.607913	969.773107	15.947955
25.953834	965.054599	15.952973
25.315760	953.288622	15.957991
25.376380	952.373430	15.963008
25.510829	954.261685	15.968026
25.385509	964.670399	15.973043
25.640226	959.836792	15.978061
25.850615	957.743094	15.983079
25.749890	957.433857	15.988096
25.859701	955.381164	15.993114
26.048847	965.210427	15.998131
26.396367	961.570969	16.003149
26.378556	959.572986	16.008167
26.005935	950.144929	16.013184
25.869943	932.099068	16.018202
25.557454	943.682666	16.023219
25.884262	940.213717	16.028237
26.157232	949.531214	16.033255
26.254202	952.214301	16.038272
26.111318	959.921206	16.043290
25.719805	957.287488	16.048307
26.348270	961.335836	16.053325
26.218049	962.738533	16.058343
26.054412	963.221803	16.063360
26.484718	950.884487	16.068378
26.196165	960.116397	16.073395
26.148242	955.721534	16.078413
26.140846	957.259623	16.083431
26.129722	962.620026	16.088448
26.320442	956.906498	16.093466
26.127422	961.869361	16.098483
26.026366	953.885158	16.103501
26.220239	958.534935	16.108519
26.288752	961.282443	16.113536
26.057402	957.629539	16.118554
26.132113	965.078288	16.123571
26.278281	954.215088	16.128589
25.831179	967.864780	16.133607
26.335224	972.617444	16.138624
26.338740	982.680931	16.143642
26.597809	987.954826	16.148659
26.460619	982.349472	16.153677
27.058496	982.391532	16.158695
27.034038	981.505448	16.163712
26.862613	976.404084	16.168730
26.710664	981.082803	16.173747
26.611908	980.252541	16.178765
26.928421	980.067282	16.183783
26.738906	982.934117	16.188800
27.127317	977.233791	16.193818
26.731105	987.842754	16.198835
26.847559	978.915575	16.203853
27.054746	985.794459	16.208871
26.978114	984.742977	16.213888
27.219251	977.367878	16.218906
26.679057	967.530559	16.223923
26.999913	975.972710	16.228941
27.160262	970.516404	16.233959
27.035567	977.109607	16.238976
27.099717	980.675168	16.243994
26.980486	979.974348	16.249011
27.225348	980.535628	16.254029
27.237594	963.305965	16.259047
27.343121	974.524284	16.264064
27.075282	963.912138	16.269082
27.170625	964.509468	16.274099
26.979195	974.625584	16.279117
27.034864	979.338046	16.284135
26.720777	974.662983	16.289152
27.409205	978.051836	16.294170
27.405178	973.277700	16.299187
27.245837	984.831018	16.304205
27.393699	972.932422	16.309223
27.310260	977.587782	16.314240
27.146893	978.383439	16.319258
27.169015	974.959065	16.324275
27.073095	982.134750	16.329293
27.420844	990.222394	16.334311
27.570302	1011.466308	16.339328
27.809521	999.591251	16.344346
27.753339	1000.600492	16.349363
27.625310	1001.463197	16.354381
27.738369	1000.823814	16.359399
27.442107	1001.532994	16.364416
27.400017	1011.972877	16.369434
27.633565	1001.395764	16.374451
27.643181	1005.029835	16.379469
27.644371	1010.126387	16.384487
27.298147	1004.108801	16.389504
27.242478	997.038977	16.394522
27.247933	1013.054116	16.399539
27.893086	1016.437133	16.404557
28.061201	1017.038842	16.409575
28.027698	1010.091774	16.414592
28.161706	1013.292939	16.419610
28.233577	1016.377607	16.424627
27.728718	1015.585724	16.429645
28.141695	1009.701655	16.434663
28.150148	1010.104313	16.439680
27.916797	1010.020985	16.444698
28.243810	1013.845173	16.449715
28.017035	1011.510689	16.454733
28.243418	1011.203849	16.459751
28.016604	1023.692429	16.464768
28.173534	1010.757266	16.469786
28.475581	1010.870924	16.474803
28.086566	1008.789081	16.479821
28.400384	1008.869336	16.484839
28.073678	1007.200616	16.489856
28.219641	1001.238462	16.494874
28.537210	1010.274445	16.499891
28.406549	1008.278358	16.504909
28.594011	1001.176751	16.509927
28.504457	1020.198532	16.514944
28.573752	1020.528541	16.519962
28.590338	1007.230354	16.524979
28.445807	1009.465287	16.529997
28.582499	1004.306172	16.535015
28.473263	1009.473675	16.540032
28.295090	996.278595	16.545050
28.798916	1007.040048	16.550067
28.720953	1024.466311	16.555085
28.708595	1026.522744	16.560103
28.678466	1038.901622	16.565120
28.841370	1030.263791	16.570138
29.001709	1021.626366	16.575155
28.900433	1027.117680	16.580173
29.198575	1026.064282	16.585191
28.890332	1022.947285	16.590208
29.044823	1011.685107	16.595226
28.839437	1012.522063	16.600243
28.897658	1015.122867	16.605261
29.211834	1026.671451	16.610279
29.033002	1026.336580	16.615296
29.255500	1026.961327	16.620314
29.240873	1020.304792	16.625331
28.807308	1021.186966	16.630349
29.119384	1011.503275	16.635367
29.430427	1023.547817	16.640384
29.034274	1015.433093	16.645402
29.284291	1019.796374	16.650419
28.798501	1015.700477	16.655437
29.432390	1026.233277	16.660455
29.248167	1024.068853	16.665472
29.468339	1026.139347	16.670490
29.421157	1026.459203	16.675507
29.022455	1029.428249	16.680525
28.981143	1025.915973	16.685543
29.238595	1035.071842	16.690560
29.760257	1023.203010	16.695578
29.118285	1021.346995	16.700595
29.133304	1028.707291	16.705613
29.570258	1037.497360	16.710631
29.601592	1045.571488	16.715648
29.658353	1039.550713	16.720666
30.052157	1043.594820	16.725683
29.935953	1042.820939	16.730701
29.826082	1033.440035	16.735719
29.669818	1033.063757	16.740736
29.532895	1044.446340	16.745754
30.259966	1046.229130	16.750771
29.632094	1043.313690	16.755789
29.631080	1034.010405	16.760807
29.899936	1041.305690	16.765824
30.071655	1037.267720	16.770842
30.585566	1042.400716	16.775859
30.372764	1035.623744	16.780877
29.904105	1022.051273	16.785895
29.876240	1018.789360	16.790912
29.827360	1035.968077	16.795930
30.706586	1032.668183	16.800947
30.179989	1034.303405	16.805965
30.109642	1018.756079	16.810983
29.876032	1030.087529	16.816000
29.976996	1036.115214	16.821018
30.489474	1036.205370	16.826035
30.314556	1048.130405	16.831053
30.226019	1037.758371	16.836071
30.137499	1033.978930	16.841088
30.210795	1038.489826	16.846106
30.431783	1031.452383	16.851123
30.432827	1043.466612	16.856141
30.631944	1034.646377	16.861159
30.604126	1031.930418	16.866176
30.267536	1035.060150	16.871194
30.646517	1022.159617	16.876211
30.892974	1034.930666	16.881229
30.846405	1029.320566	16.886247
30.922397	1033.357660	16.891264
30.939501	1036.548743	16.896282
30.749650	1034.094860	16.901299
30.686961	1040.634190	16.906317
30.866837	1039.946466	16.911335
30.965205	1039.839567	16.916352
30.774569	1038.102187	16.921370
31.052087	1032.138346	16.926387
30.746045	1035.512605	16.931405
30.607680	1027.976034	16.936423
30.253875	1037.325507	16.941440
30.766625	1027.042311	16.946458
30.928728	1032.192554	16.951475
30.500152	1032.493269	16.956493
30.709930	1030.989804	16.961511
30.491908	1040.210705	16.966528
30.494185	1057.239413	16.971546
31.333443	1055.867699	16.976563
31.148672	1059.497522	16.981581
31.027153	1059.519751	16.986599
31.010346	1060.642749	16.991616
31.359563	1055.336710	16.996634
31.060347	1052.751634	17.001651
30.879251	1068.695064	17.006669
31.321679	1057.782228	17.011687
31.089532	1071.313112	17.016704
31.352081	1079.685550	17.021722
31.758501	1071.328288	17.026739
31.632794	1090.198015	17.031757
31.771369	1063.752262	17.036775
31.692100	1058.140964	17.041792
31.407882	1064.030189	17.046810
31.516741	1056.192935	17.051827
31.350512	1069.760828	17.056845
31.653550	1065.336196	17.061863
31.923268	1070.699968	17.066880
31.880530	1077.731657	17.071898
31.978186	1074.134481	17.076915
31.821037	1080.013269	17.081933
32.050427	1073.059701	17.086951
31.789492	1055.891686	17.091968
31.576046	1069.208195	17.096986
32.084941	1064.719752	17.102003
31.867806	1075.581581	17.107021
31.787754	1068.758551	17.112039
32.199292	1071.540696	17.117056
32.091590	1077.055123	17.122074
32.470416	1070.882889	17.127091
31.958834	1079.455514	17.132109
32.031436	1067.830583	17.137127
32.042404	1069.400519	17.142144
31.872839	1072.112761	17.147162
32.241585	1073.061741	17.152179
32.282762	1071.067127	17.157197
32.202875	1065.623185	17.162215
32.366988	1068.036990	17.167232
32.321608	1074.583087	17.172250
32.343010	1059.346405	17.177267
32.216046	1065.340382	17.182285
32.128314	1067.250836	17.187303
32.374047	1057.962530	17.192320
32.043447	1073.686387	17.197338
32.282186	1060.643693	17.202355
32.456511	1085.169055	17.207373
32.221236	1094.907093	17.212391
32.810728	1095.512213	17.217408
32.267256	1094.764246	17.222426
32.606141	1087.471619	17.227443
32.585826	1087.702058	17.232461
32.924209	1095.945855	17.237479
32.633979	1089.064227	17.242496
32.727681	1097.649325	17.247514
32.951088	1083.854764	17.252531
33.065318	1086.011293	17.257549
32.855400	1091.841548	17.262567
33.031864	1084.943606	17.267584
32.687271	1092.316090	17.272602
33.053523	1083.936712	17.277619
33.001561	1091.036125	17.282637
32.865467	1089.855094	17.287655
32.793122	1091.980895	17.292672
33.039115	1093.075344	17.297690
33.319607	1098.267019	17.302707
33.188054	1106.385631	17.307725
33.277101	1096.282391	17.312743
33.395594	1099.530185	17.317760
33.227632	1095.826295	17.322778
33.297467	1095.294668	17.327795
33.236415	1105.611343	17.332813
33.130749	1109.190911	17.337831
33.406643	1107.976889	17.342848
33.555529	1109.001345	17.347866
33.650188	1107.124583	17.352883
33.818243	1113.627787	17.357901
33.573257	1108.373804	17.362919
33.586745	1105.332619	17.367936
33.503749	1113.797083	17.372954
33.578312	1104.664962	17.377971
33.438977	1110.818686	17.382989
33.458744	1110.821934	17.388007
33.717776	1110.633057	17.393024
33.527307	1108.554809	17.398042
33.852239	1108.011617	17.403059
33.692149	1111.221008	17.408077
33.700728	1109.020054	17.413095
33.839542	1104.113047	17.418112
33.572634	1120.047877	17.423130
33.856236	1126.075380	17.428147
34.122289	1138.347961	17.433165
34.328254	1132.723509	17.438183
34.596507	1123.497913	17.443200
34.235073	1120.304024	17.448218
33.954017	1107.465816	17.453235
34.226782	1106.956044	17.458253
34.085931	1109.304023	17.463271
34.418703	1118.943607	17.468288
34.194766	1110.704024	17.473306
34.051487	1120.686445	17.478323
34.439537	1122.790609	17.483341
34.100948	1127.981457	17.488359
34.310819	1125.019956	17.493376
34.187197	1134.800484	17.498394
34.745656	1126.308920	17.503411
34.456758	1121.885497	17.508429
34.356941	1128.941928	17.513447
34.719108	1124.463835	17.518464
34.505299	1120.760811	17.523482
34.508237	1129.842995	17.528499
34.511599	1119.267162	17.533517
34.720216	1118.385579	17.538535
34.899263	1107.394055	17.543552
34.839540	1119.540936	17.548570
34.417234	1121.604804	17.553587
34.682979	1120.389215	17.558605
34.508799	1132.967457	17.563623
35.266149	1133.861867	17.568640
34.640458	1143.863077	17.573658
35.058719	1142.617280	17.578675
35.175924	1137.754676	17.583693
35.162316	1144.876504	17.588711
35.519204	1130.653885	17.593728
35.195095	1137.660252	17.598746
34.708217	1119.893243	17.603763
34.797709	1125.572454	17.608781
35.014038	1138.335674	17.613799
35.393316	1135.761048	17.618816
35.022284	1146.416654	17.623834
35.061551	1140.120868	17.628851
35.210967	1136.881651	17.633869
35.335638	1136.966295	17.638887
35.445459	1132.338385	17.643904
35.296071	1144.278420	17.648922
35.341894	1130.641037	17.653939
35.366666	1137.520157	17.658957
35.036275	1142.343643	17.663975
35.619944	1157.602429	17.668992
35.471655	1159.007972	17.674010
35.680312	1157.406840	17.679027
35.922245	1159.574929	17.684045
35.722718	1166.845818	17.689063
35.847276	1159.034462	17.694080
35.721835	1170.314339	17.699098
35.658093	1164.208257	17.704115
35.913837	1161.409980	17.709133
36.118750	1159.604302	17.714151
35.934076	1152.557784	17.719168
36.017606	1163.322065	17.724186
35.873885	1153.024884	17.729203
35.970452	1157.595282	17.734221
36.046849	1159.113948	17.739239
36.071746	1153.773486	17.744256
36.080304	1157.600262	17.749274
36.080316	1150.307053	17.754291
36.293939	1150.743842	17.759309
36.671956	1160.313242	17.764327
36.265908	1151.868638	17.769344
36.286634	1154.869822	17.774362
36.067871	1148.033779	17.779379
36.155296	1149.938890	17.784397
36.428729	1147.245143	17.789415
36.604913	1150.105202	17.794432
36.320269	1158.755920	17.799450
36.350899	1164.819915	17.804467
37.040643	1183.170649	17.809485
36.735422	1182.533676	17.814503
36.664089	1171.303624	17.819520
36.493202	1167.461318	17.824538
36.962374	1179.178226	17.829555
37.238228	1169.077235	17.834573
36.483418	1167.567094	17.839591
37.019926	1162.809207	17.844608
36.618661	1171.727517	17.849626
37.401081	1178.285970	17.854643
36.777323	1166.665935	17.859661
36.974309	1175.159147	17.864679
37.188120	1183.558206	17.869696
37.231441	1182.409021	17.874714
36.996224	1180.476635	17.879731
37.016921	1173.063408	17.884749
37.308176	1183.886676	17.889767
36.902303	1179.150198	17.894784
36.918918	1184.174954	17.899802
37.210953	1184.675201	17.904819
37.491566	1180.875764	17.909837
37.240210	1187.283757	17.914855
37.051080	1185.085367	17.919872
37.247228	1183.498816	17.924890
37.413309	1185.833431	17.929907
37.264936	1183.341470	17.934925
37.439814	1186.678278	17.939943
37.480129	1178.075362	17.944960
37.371317	1180.673958	17.949978
36.893249	1193.151527	17.954995
37.494898	1195.761892	17.960013
37.546521	1209.213705	17.965031
37.565400	1204.366489	17.970048
37.991211	1204.277716	17.975066
37.533787	1205.602306	17.980083
37.918622	1214.577359	17.985101
37.584625	1208.223263	17.990119
37.826696	1206.698945	17.995136
37.919973	1205.238966	18.000154
37.521950	1212.799756	18.005171
37.879050	1203.077348	18.010189
37.918632	1222.015994	18.015207
38.112343	1230.222559	18.020224
38.217968	1233.349314	18.025242
38.164025	1233.506126	18.030259
38.449287	1233.663443	18.035277
38.385293	1235.541792	18.040295
38.351439	1227.367051	18.045312
38.664116	1231.900453	18.050330
38.572660	1220.518884	18.055347
38.657127	1211.031696	18.060365
38.471480	1205.926182	18.065383
38.342406	1201.171578	18.070400
38.737387	1198.408286	18.075418
38.591074	1195.000792	18.080435
38.647051	1196.753041	18.085453
38.393429	1196.360454	18.090471
38.353025	1207.273571	18.095488
38.970977	1208.704236	18.100506
38.759330	1223.323961	18.105523
38.743397	1218.636834	18.110541
38.625270	1226.825982	18.115559
38.890660	1229.965575	18.120576
38.935245	1223.722577	18.125594
38.765563	1226.015127	18.130611
39.075068	1220.863589	18.135629
38.821837	1223.535312	18.140647
39.108951	1223.196863	18.145664
38.884821	1226.444712	18.150682
39.072108	1228.050154	18.155699
39.243118	1220.102102	18.160717
38.966818	1224.882421	18.165735
38.749462	1223.988676	18.170752
39.322879	1227.073697	18.175770
39.228263	1236.117568	18.180787
39.615798	1242.908334	18.185805
39.307205	1240.028044	18.190823
39.098716	1237.002680	18.195840
39.577747	1243.334129	18.200858
39.611524	1246.951840	18.205875
39.708765	1242.909713	18.210893
39.597388	1239.736586	18.215911
39.227372	1243.856230	18.220928
39.252662	1247.775081	18.225946
39.238874	1252.050360	18.230963
39.114072	1252.000517	18.235981
39.604589	1256.736443	18.240999
39.954628	1264.565070	18.246016
40.058726	1261.342399	18.251034
39.616841	1256.160249	18.256051
39.836403	1262.254639	18.261069
39.956887	1268.793756	18.266087
40.103732	1265.362409	18.271104
40.246858	1260.176965	18.276122
40.062845	1270.822278	18.281139
40.183295	1254.774624	18.286157
40.209163	1260.104073	18.291175
40.228629	1254.726561	18.296192
40.583425	1254.753059	18.301210
40.623474	1259.505913	18.306227
40.501508	1242.669405	18.311245
40.427441	1236.265106	18.316263
40.241100	1225.703153	18.321280
40.300533	1230.162620	18.326298
40.443844	1245.553594	18.331315
40.912386	1249.358815	18.336333
40.396985	1245.431610	18.341351
40.554281	1248.029549	18.346368
41.031138	1251.663050	18.351386
40.605160	1248.005865	18.356403
40.730590	1237.174145	18.361421
40.682124	1248.176915	18.366439
40.955835	1249.642583	18.371456
40.912692	1253.846720	18.376474
40.792919	1256.134610	18.381491
40.571051	1252.505406	18.386509
40.717651	1250.203912	18.391527
40.366121	1251.332027	18.396544
41.003411	1251.506775	18.401562
40.720093	1260.270946	18.406579
40.925180	1250.433470	18.411597
41.140113	1263.651448	18.416615
41.200871	1267.599461	18.421632
41.498045	1264.886198	18.426650
41.394357	1260.440034	18.431667
41.189331	1243.430340	18.436685
41.148326	1257.893966	18.441703
41.049876	1273.322842	18.446720
41.484828	1268.217910	18.451738
41.123834	1273.737368	18.456755
41.564251	1273.305469	18.461773
40.910053	1277.226642	18.466791
40.800279	1275.119952	18.471808
41.121282	1280.321113	18.476826
41.529625	1289.320924	18.481843
41.734860	1292.867598	18.486861
41.772120	1285.672643	18.491879
41.647167	1291.694784	18.496896
41.899468	1291.308138	18.501914
41.704659	1294.261061	18.506931
41.690682	1287.370788	18.511949
41.589577	1290.368992	18.516967
41.838016	1295.998107	18.521984
42.193868	1308.026354	18.527002
42.354086	1316.323416	18.532019
42.159358	1308.211714	18.537037
42.094349	1299.719918	18.542055
42.331071	1310.403480	18.547072
42.429534	1305.414375	18.552090
42.338427	1303.806547	18.557107
42.423018	1312.882342	18.562125
42.209295	1306.638759	18.567143
42.235415	1309.112087	18.572160
42.697297	1309.361657	18.577178
42.618782	1305.864622	18.582195
42.582613	1306.381579	18.587213
42.790552	1305.591615	18.592231
42.813100	1312.859328	18.597248
42.923508	1294.881795	18.602266
42.646278	1296.594738	18.607283
43.051882	1292.482195	18.612301
42.959063	1283.395143	18.617319
42.607620	1280.922360	18.622336
42.817247	1291.502855	18.627354
42.974363	1302.587061	18.632371
42.814316	1299.708736	18.637389
43.064438	1305.394396	18.642407
42.873331	1297.948028	18.647424
42.938471	1304.675716	18.652442
42.993110	1306.112594	18.657459
43.080808	1305.130024	18.662477
43.187727	1299.262254	18.667495
42.747089	1307.814403	18.672512
42.989920	1303.714737	18.677530
43.076870	1305.294881	18.682547
43.087190	1303.888918	18.687565
43.229850	1310.967393	18.692583
43.146237	1321.514952	18.697600
43.337439	1323.848805	18.702618
43.101046	1326.391669	18.707635
43.184787	1330.329783	18.712653
43.431759	1323.079865	18.717671
43.474217	1329.214649	18.722688
43.545090	1328.963729	18.727706
43.607263	1349.748335	18.732723
43.848100	1352.844459	18.737741
44.098802	1344.549339	18.742759
43.957794	1358.523768	18.747776
44.364870	1354.679234	18.752794
44.690779	1349.439879	18.757811
44.100179	1342.207568	18.762829
44.293532	1326.987899	18.767847
44.096822	1330.531282	18.772864
44.030652	1322.863350	18.777882
43.999201	1325.913765	18.782899
44.468744	1331.795437	18.787917
44.593013	1327.992062	18.792935
43.843204	1324.117345	18.797952
44.297553	1333.453965	18.802970
44.334101	1339.441351	18.807987
44.597126	1338.989906	18.813005
44.587499	1343.917829	18.818023
44.497867	1353.677371	18.823040
44.397156	1346.907965	18.828058
44.718184	1342.452044	18.833075
44.767048	1345.395202	18.838093
44.882333	1339.683903	18.843111
44.447800	1344.567942	18.848128
44.932218	1345.924864	18.853146
44.682405	1351.578410	18.858163
44.556468	1353.150885	18.863181
44.973163	1339.048123	18.868199
45.060513	1340.899616	18.873216
44.798855	1336.257269	18.878234
44.889182	1340.917058	18.883251
44.834905	1345.801483	18.888269
45.087533	1349.258689	18.893287
45.334767	1372.482253	18.898304
44.797923	1360.545504	18.903322
45.080838	1364.988926	18.908339
44.836914	1365.917145	18.913357
45.229031	1366.559513	18.918375
45.165639	1367.655114	18.923392
45.211310	1362.235592	18.928410
45.325668	1374.409022	18.933427
45.326643	1386.136304	18.938445
45.484674	1384.492590	18.943463
45.463817	1387.942157	18.948480
45.883981	1389.561623	18.953498
46.170779	1380.897900	18.958515
46.366137	1381.552160	18.963533
46.565216	1367.496095	18.968551
46.507841	1367.031730	18.973568
46.255462	1352.591957	18.978586
46.148349	1349.645367	18.983603
46.343742	1350.656239	18.988621
46.394583	1351.784436	18.993639
46.332653	1352.520033	18.998656
46.301938	1354.311127	19.003674
46.104353	1344.852280	19.008691
46.146207	1345.142411	19.013709
46.379759	1351.061064	19.018727
46.285278	1345.079662	19.023744
46.169725	1348.540902	19.028762
46.492926	1352.785499	19.033779
46.181070	1352.989032	19.038797
46.454419	1340.231057	19.043815
46.355153	1346.384896	19.048832
46.212565	1339.577871	19.053850
46.311788	1340.127267	19.058867
46.277425	1351.351961	19.063885
46.530167	1359.501999	19.068903
46.472012	1367.650255	19.073920
46.533209	1372.005336	19.078938
46.671163	1371.403066	19.083955
46.429834	1372.908412	19.088973
46.839389	1372.878993	19.093991
46.832316	1382.534095	19.099008
47.113633	1390.818530	19.104026
47.519664	1394.422131	19.109043
46.960825	1384.568565	19.114061
47.029457	1384.100237	19.119079
47.546217	1398.160996	19.124096
47.264721	1397.706497	19.129114
47.525074	1396.621128	19.134131
47.238422	1400.279606	19.139149
47.491008	1392.283981	19.144167
47.459177	1390.963514	19.149184
47.357846	1400.819593	19.154202
47.775378	1383.557585	19.159219
47.473296	1385.798313	19.164237
47.293669	1387.445477	19.169255
47.362600	1396.640537	19.174272
47.528612	1396.993271	19.179290
47.797337	1401.394743	19.184307
47.798124	1398.961435	19.189325
47.820899	1387.609201	19.194343
47.660178	1399.964607	19.199360
47.693095	1410.007948	19.204378
48.276359	1419.103501	19.209395
48.140832	1419.544507	19.214413
47.878709	1416.678999	19.219431
48.315578	1418.671406	19.224448
48.258523	1414.574517	19.229466
48.279914	1419.241971	19.234483
48.529055	1417.498769	19.239501
48.657818	1414.332169	19.244519
48.530115	1425.631496	19.249536
48.310422	1404.593826	19.254554
48.578028	1404.397291	19.259571
48.426648	1411.963704	19.264589
48.762080	1414.410677	19.269607
48.882072	1411.472679	19.274624
48.828523	1414.684367	19.279642
48.653988	1407.427868	19.284659
48.227589	1423.173353	19.289677
48.482941	1419.696573	19.294695
48.504139	1415.344417	19.299712
48.568101	1410.537420	19.304730
48.629816	1413.642684	19.309747
48.678589	1436.222057	19.314765
48.574305	1433.600071	19.319783
48.896592	1428.566397	19.324800
48.761649	1432.327349	19.329818
49.022243	1429.269484	19.334835
49.037129	1435.831520	19.339853
49.140689	1439.892790	19.344871
49.456526	1455.670342	19.349888
49.344008	1458.828159	19.354906
49.783181	1457.288719	19.359923
49.537628	1460.394792	19.364941
49.343994	1458.844040	19.369959
49.398608	1463.970223	19.374976
49.391437	1463.131901	19.379994
49.623822	1453.435209	19.385011
49.914859	1460.244333	19.390029
49.949479	1456.836845	19.395047
49.964800	1453.552306	19.400064
49.754836	1451.742171	19.405082
49.925469	1449.484225	19.410099
49.895296	1458.312976	19.415117
49.811473	1452.386675	19.420135
49.593917	1452.083109	19.425152
49.596699	1474.729699	19.430170
50.208304	1471.828280	19.435187
49.808994	1471.865628	19.440205
50.062580	1477.481370	19.445223
50.487868	1476.783584	19.450240
50.281657	1473.451696	19.455258
50.359238	1475.181651	19.460275
50.051418	1470.720078	19.465293
50.567966	1486.933290	19.470311
50.554684	1489.980886	19.475328
50.612630	1504.902599	19.480346
50.783805	1494.079337	19.485363
50.718901	1507.388678	19.490381
50.752150	1499.241171	19.495399
51.149437	1500.895791	19.500416
50.792720	1503.167185	19.505434
50.800277	1504.081257	19.510451
50.732417	1502.567602	19.515469
50.872910	1499.670560	19.520487
51.005443	1498.586276	19.525504
50.915626	1501.869938	19.530522
51.048390	1486.858451	19.535539
51.168412	1494.764245	19.540557
51.077154	1501.999371	19.545575
51.555778	1506.853998	19.550592
51.489700	1514.173550	19.555610
51.876415	1505.339471	19.560627
51.576605	1507.084374	19.565645
51.325776	1503.210337	19.570663
51.388236	1497.775520	19.575680
51.636093	1507.371812	19.580698
51.549206	1503.083908	19.585715
51.863414	1511.653594	19.590733
51.987888	1514.932087	19.595751
52.260064	1517.360581	19.600768
52.041449	1513.610888	19.605786
52.298343	1506.845357	19.610803
52.283108	1502.255880	19.615821
52.102077	1501.359585	19.620839
52.128210	1483.716972	19.625856
52.275483	1493.127036	19.630874
52.209024	1484.534389	19.635891
51.959275	1487.477016	19.640909
52.129667	1495.965080	19.645927
52.415558	1495.118712	19.650944
52.064389	1494.413183	19.655962
52.390779	1494.863874	19.660979
52.676474	1499.540434	19.665997
52.460752	1492.142024	19.671015
52.934014	1495.542600	19.676032
52.440195	1504.604969	19.681050
52.184800	1495.110916	19.686067
52.528480	1493.046768	19.691085
52.728402	1502.540110	19.696103
52.780299	1498.779597	19.701120
52.757825	1499.262855	19.706138
52.668377	1511.638731	19.711155
52.898483	1514.632418	19.716173
52.619048	1520.085522	19.721191
52.946297	1523.736208	19.726208
52.949993	1525.105342	19.731226
52.945644	1521.400976	19.736243
53.013568	1522.352931	19.741261
53.050525	1533.938967	19.746279
53.568667	1545.055127	19.751296
53.577032	1549.484803	19.756314
53.522633	1541.354165	19.761331
53.540823	1547.079397	19.766349
53.637398	1546.947529	19.771367
53.944627	1537.845008	19.776384
53.669713	1542.590478	19.781402
53.706879	1533.236768	19.786419
53.702991	1532.672496	19.791437
54.069878	1540.416551	19.796455
54.015814	1534.394037	19.801472
53.858788	1538.496158	19.806490
53.964690	1534.673525	19.811507
54.224247	1543.321219	19.816525
54.121537	1543.529857	19.821543
53.725759	1539.479697	19.826560
53.715714	1545.884726	19.831578
54.084043	1549.677310	19.836595
54.325861	1550.198060	19.841613
54.119612	1562.753224	19.846631
54.775797	1559.002168	19.851648
54.651620	1565.377746	19.856666
54.837991	1558.585373	19.861683
54.618667	1561.163466	19.866701
54.677746	1569.119869	19.871719
54.906196	1556.618096	19.876736
54.839553	1562.501798	19.881754
54.693389	1559.198357	19.886771
55.159755	1554.599687	19.891789
54.703281	1556.293398	19.896807
55.126615	1559.095866	19.901824
54.759768	1553.611523	19.906842
54.683037	1555.513993	19.911859
54.995804	1543.462943	19.916877
54.965455	1553.923395	19.921895
55.404991	1561.302611	19.926912
55.227300	1573.171623	19.931930
55.234771	1570.838235	19.936947
55.156564	1578.257548	19.941965
55.555636	1580.423161	19.946983
55.214464	1570.185078	19.952000
55.397316	1570.004977	19.957018
55.250997	1575.774928	19.962035
55.506064	1564.121087	19.967053
55.388013	1570.214827	19.972071
55.873630	1564.738939	19.977088
55.737064	1584.349382	19.982106
55.879261	1591.734169	19.987123
55.977153	1588.114761	19.992141
55.707449	1599.319675	19.997159
55.903154	1597.802589	20.002176
55.811113	1585.650824	20.007194
56.152886	1586.130667	20.012211
56.313885	1585.408009	20.017229
55.798481	1591.879607	20.022247
55.941299	1584.125169	20.027264
55.616864	1604.967488	20.032282
55.930097	1608.232204	20.037299
56.475095	1603.488652	20.042317
56.481970	1609.401878	20.047335
56.677290	1610.580043	20.052352
56.655776	1610.211044	20.057370
56.580171	1612.640389	20.062387
57.013185	1596.518209	20.067405
56.629474	1603.805508	20.072423
57.307749	1617.882163	20.077440
57.212072	1618.985994	20.082458
56.931593	1611.764946	20.087475
57.309004	1603.604496	20.092493
56.901073	1609.311300	20.097511
57.192968	1611.648351	20.102528
57.303157	1621.913247	20.107546
57.454599	1623.849406	20.112563
58.054089	1619.147808	20.117581
57.707595	1614.843744	20.122599
57.346978	1599.025793	20.127616
57.614642	1596.171931	20.132634
57.539041	1607.785118	20.137651
57.568318	1612.072671	20.142669
57.377112	1625.957339	20.147687
57.973818	1622.120910	20.152704
58.264762	1623.157855	20.157722
58.088144	1616.416019	20.162739
57.880996	1622.422745	20.167757
57.776835	1615.912566	20.172775
58.251489	1624.037426	20.177792
58.165201	1615.340520	20.182810
58.193147	1614.809129	20.187827
58.405414	1615.015758	20.192845
58.440943	1610.004870	20.197863
58.232984	1611.435576	20.202880
57.947368	1612.988907	20.207898
57.960158	1618.614018	20.212915
58.389580	1610.966150	20.217933
57.932736	1624.071885	20.222951
58.401273	1627.331208	20.227968
58.530350	1637.874035	20.232986
58.542254	1640.567398	20.238003
58.824837	1626.905166	20.243021
59.075993	1640.184024	20.248039
58.906132	1629.972717	20.253056
59.067953	1629.107911	20.258074
58.753635	1630.346988	20.263091
59.229684	1630.130418	20.268109
59.110606	1635.709919	20.273127
59.382277	1627.411383	20.278144
59.301258	1634.468224	20.283162
59.178323	1631.940654	20.288179
59.003273	1628.689066	20.293197
59.494072	1655.832419	20.298215
59.325509	1657.774535	20.303232
59.576680	1650.504891	20.308250
59.713815	1655.832806	20.313267
59.418886	1661.686032	20.318285
59.548925	1662.609326	20.323303
59.513218	1657.918870	20.328320
59.602984	1657.945867	20.333338
59.628654	1659.399936	20.338355
59.945262	1661.057745	20.343373
60.077998	1647.396883	20.348391
59.962080	1651.997544	20.353408
60.012049	1660.861179	20.358426
59.776490	1680.080116	20.363443
60.306429	1677.901555	20.368461
60.184925	1689.184297	20.373479
60.149521	1683.461783	20.378496
60.395106	1678.601011	20.383514
59.950815	1686.257615	20.388531
60.317617	1678.165070	20.393549
60.392857	1678.383701	20.398567
60.406859	1686.716468	20.403584
61.108511	1686.773837	20.408602
60.714999	1700.393597	20.413619
60.955089	1697.117981	20.418637
61.059948	1704.366646	20.423655
61.252961	1702.259805	20.428672
61.421067	1702.082014	20.433690
61.244574	1688.671551	20.438707
61.073602	1672.981621	20.443725
60.994800	1677.099922	20.448743
61.002420	1691.783510	20.453760
61.097520	1690.547281	20.458778
61.174776	1691.437819	20.463795
60.946086	1683.021981	20.468813
60.700224	1696.549174	20.473831
61.240946	1708.936914	20.478848
61.433265	1701.162045	20.483866
61.035397	1708.315897	20.488883
61.080103	1711.032535	20.493901
61.971438	1723.561024	20.498919
61.694963	1726.059727	20.503936
62.268842	1736.267820	20.508954
62.013764	1730.175742	20.513971
62.491017	1733.124434	20.518989
62.245508	1737.391950	20.524007
61.989935	1732.716985	20.529024
62.345830	1724.641908	20.534042
62.142183	1724.279350	20.539059
62.338841	1724.930264	20.544077
62.377205	1730.286300	20.549095
62.530279	1732.812385	20.554112
62.236721	1727.363845	20.559130
62.080273	1733.716135	20.564147
62.475008	1733.253513	20.569165
62.602299	1758.487798	20.574183
63.208978	1755.473492	20.579200
63.411166	1753.191629	20.584218
62.982761	1738.681286	20.589235
62.988333	1732.665141	20.594253
63.418211	1735.242538	20.599271
62.859540	1741.632600	20.604288
63.176769	1737.783127	20.609306
62.910442	1745.206734	20.614323
63.232501	1737.897545	20.619341
63.534258	1755.160881	20.624359
63.679113	1760.446590	20.629376
63.801196	1750.994250	20.634394
63.750169	1755.351228	20.639411
63.682928	1750.239630	20.644429
64.121432	1749.464020	20.649447
63.514376	1742.742234	20.654464
63.609723	1745.719203	20.659482
63.734233	1752.147408	20.664499
63.715083	1749.613028	20.669517
63.528668	1748.774372	20.674535
63.565802	1754.237911	20.679552
63.806237	1743.012305	20.684570
63.492284	1753.125965	20.689587
63.708142	1762.408654	20.694605
63.738198	1771.767797	20.699623
64.091114	1773.931199	20.704640
64.245659	1783.993566	20.709658
64.500636	1794.775551	20.714675
64.558437	1792.680417	20.719693
64.728209	1796.873415	20.724711
64.811287	1793.606602	20.729728
64.977754	1793.078751	20.734746
64.789885	1804.122640	20.739763
64.933686	1785.438751	20.744781
64.786568	1789.586716	20.749799
64.884240	1793.898314	20.754816
64.928999	1797.795299	20.759834
64.725438	1794.690167	20.764851
64.583365	1787.037083	20.769869
64.709397	1799.616098	20.774887
64.706283	1805.840241	20.779904
65.404307	1808.053726	20.784922
65.278791	1816.667204	20.789939
65.014869	1813.076033	20.794957
65.270782	1820.919654	20.799975
65.335624	1828.045243	20.804992
65.990263	1832.380047	20.810010
65.787860	1836.363105	20.815027
66.173774	1832.606998	20.820045
66.088496	1842.618605	20.825063
66.160747	1824.665454	20.830080
66.764720	1821.954537	20.835098
66.421048	1806.843847	20.840115
66.287730	1807.117248	20.845133
66.534628	1800.716111	20.850151
66.052956	1794.391253	20.855168
66.521982	1813.600935	20.860186
66.520704	1817.221098	20.865203
66.371637	1814.148452	20.870221
66.739227	1823.956544	20.875239
66.481435	1832.259374	20.880256
66.928626	1820.319630	20.885274
66.992662	1826.492233	20.890291
66.597591	1823.966244	20.895309
67.264215	1819.519180	20.900327
66.899845	1825.919858	20.905344
67.023869	1818.360779	20.910362
66.912423	1814.865647	20.915379
66.666223	1822.002093	20.920397
66.831580	1820.704352	20.925415
66.614166	1819.864237	20.930432
67.150020	1836.033715	20.935450
66.998470	1847.119279	20.940467
67.504304	1848.510759	20.945485
67.699359	1849.815222	20.950503
67.425549	1847.607923	20.955520
67.524682	1847.718665	20.960538
67.603541	1852.036380	20.965555
68.022424	1856.957273	20.970573
68.070103	1855.015205	20.975591
68.041632	1864.708635	20.980608
68.248773	1854.453914	20.985626
67.827829	1840.179019	20.990643
67.947829	1859.266697	20.995661
68.391773	1862.166978	21.000679
68.245439	1865.169207	21.005696
68.219309	1865.264859	21.010714
67.879176	1861.240622	21.015731
67.764150	1863.833977	21.020749
68.267872	1858.339385	21.025767
68.253568	1864.069809	21.030784
68.363718	1878.702772	21.035802
68.426991	1892.601427	21.040819
68.858128	1886.057779	21.045837
68.809709	1889.899951	21.050855
68.712078	1891.266053	21.055872
68.957797	1891.290709	21.060890
68.860041	1888.629760	21.065907
69.084842	1883.674354	21.070925
69.524796	1893.490083	21.075943
69.387276	1895.749274	21.080960
69.201159	1891.309554	21.085978
69.480217	1901.402977	21.090995
69.383028	1903.807339	21.096013
69.619668	1904.461463	21.101031
69.624096	1914.840933	21.106048
69.667072	1906.698028	21.111066
69.478201	1910.331821	21.116083
69.521843	1908.125274	21.121101
70.007291	1895.150627	21.126119
69.980564	1914.182451	21.131136
69.972870	1903.273350	21.136154
70.051624	1907.802548	21.141171
70.046497	1924.252536	21.146189
70.201961	1920.942799	21.151207
69.798935	1929.823887	21.156224
70.125265	1913.781258	21.161242
70.406008	1930.767171	21.166259
70.591494	1929.624069	21.171277
70.750448	1930.451323	21.176295
70.431318	1932.511739	21.181312
70.708063	1927.993180	21.186330
70.910476	1949.646510	21.191347
70.879707	1941.915957	21.196365
71.069503	1944.979154	21.201383
71.647832	1945.276769	21.206400
71.723802	1941.266222	21.211418
71.298592	1924.176759	21.216435
70.558844	1924.766094	21.221453
70.876741	1926.234365	21.226471
70.965343	1934.583964	21.231488
71.229096	1943.439493	21.236506
71.013347	1942.678011	21.241523
70.718766	1957.847851	21.246541
71.396338	1953.765139	21.251559
71.622774	1965.851980	21.256576
71.621469	1967.389201	21.261594
72.026340	1971.065692	21.266611
71.538171	1973.218872	21.271629
72.033477	1982.650411	21.276647
71.967654	1996.073877	21.281664
72.149738	1993.186020	21.286682
72.763556	1991.988430	21.291699
72.741932	1992.048660	21.296717
72.705430	1991.723029	21.301735
72.799558	1990.733102	21.306752
72.554999	1971.911035	21.311770
72.741320	1965.254225	21.316787
72.506772	1976.220320	21.321805
73.051876	1979.268884	21.326823
72.962632	1980.103466	21.331840
72.676303	1964.866885	21.336858
72.653475	1973.322329	21.341875
72.768333	1980.683156	21.346893
73.123943	1971.506560	21.351911
72.891855	1978.833374	21.356928
73.047081	1978.783840	21.361946
72.945248	1975.082029	21.366963
73.105851	1976.890551	21.371981
73.129531	1981.261127	21.376999
73.619229	2008.973275	21.382016
73.422256	2001.224552	21.387034
73.807754	1999.829187	21.392051
73.698504	2010.532658	21.397069
73.899847	2006.540326	21.402087
73.849816	1997.998511	21.407104
73.795131	2008.384141	21.412122
74.078711	2005.171090	21.417139
74.053542	2006.336486	21.422157
74.244081	1997.444533	21.427175
74.051678	1998.083824	21.432192
73.993842	2000.021253	21.437210
74.319114	2005.777421	21.442227
74.167544	2015.821603	21.447245
74.516642	2011.550483	21.452263
74.509549	2021.458415	21.457280
74.665097	2019.483649	21.462298
75.002575	2008.312106	21.467315
74.532085	2015.922457	21.472333
75.054327	2008.910022	21.477351
75.081035	2010.859455	21.482368
74.782194	2020.642669	21.487386
74.981722	2019.427929	21.492403
75.005118	2038.048060	21.497421
75.445082	2041.031051	21.502439
75.264863	2042.526877	21.507456
75.311584	2041.863135	21.512474
75.377157	2034.278406	21.517491
75.331969	2039.565568	21.522509
75.690866	2033.232016	21.527527
75.569105	2040.734088	21.532544
75.469586	2049.075341	21.537562
75.955388	2058.937631	21.542579
75.835660	2067.506138	21.547597
76.206331	2066.700115	21.552615
76.156598	2072.313072	21.557632
75.905405	2068.672514	21.562650
76.284680	2047.881097	21.567667
76.392844	2047.255068	21.572685
76.505941	2054.505740	21.577703
76.663245	2056.292695	21.582720
76.388191	2063.389572	21.587738
76.719381	2050.262243	21.592755
76.378448	2052.083073	21.597773
76.946349	2063.860843	21.602791
76.618789	2069.933924	21.607808
76.873805	2082.382467	21.612826
77.101190	2079.973530	21.617843
76.985096	2071.224263	21.622861
77.170398	2077.302208	21.627879
76.917678	2072.011279	21.632896
77.020814	2072.676859	21.637914
77.141026	2078.099077	21.642931
77.315026	2096.518934	21.647949
77.313519	2095.039018	21.652967
77.160064	2099.869753	21.657984
77.697216	2102.815435	21.663002
77.791997	2098.173853	21.668019
77.673091	2102.528925	21.673037
77.348228	2097.646953	21.678055
77.964423	2115.887089	21.683072
77.933755	2124.842488	21.688090
78.156651	2128.847347	21.693107
78.067548	2129.609325	21.698125
78.212610	2124.669501	21.703143
78.610139	2119.967857	21.708160
78.345934	2127.381821	21.713178
78.494322	2110.659939	21.718195
78.456573	2120.948299	21.723213
78.675954	2125.572294	21.728231
79.140906	2122.422331	21.733248
78.943793	2122.424842	21.738266
78.822645	2116.084413	21.743283
79.055247	2130.824639	21.748301
79.109482	2136.298240	21.753319
79.241619	2140.320476	21.758336
79.462339	2139.702059	21.763354
79.803954	2138.231502	21.768371
79.396677	2144.885187	21.773389
79.179012	2137.676176	21.778407
79.624038	2137.180419	21.783424
79.362899	2134.611309	21.788442
79.746186	2131.461515	21.793459
79.646817	2136.719322	21.798477
79.734477	2133.492758	21.803495
79.913673	2133.616207	21.808512
79.725036	2133.554269	21.813530
79.837483	2158.359063	21.818547
79.922345	2160.087945	21.823565
79.930782	2166.727004	21.828583
80.111797	2162.355940	21.833600
80.075756	2168.803137	21.838618
80.123031	2170.238083	21.843635
80.433649	2182.662204	21.848653
80.473224	2173.415089	21.853671
80.534113	2175.630606	21.858688
80.341210	2181.534292	21.863706
80.598266	2188.415297	21.868723
80.948918	2199.873715	21.873741
80.969595	2201.060345	21.878759
80.912044	2199.642854	21.883776
80.952238	2205.835103	21.888794
81.352818	2202.313328	21.893811
81.122168	2199.048253	21.898829
81.083221	2206.174472	21.903847
82.016585	2213.508153	21.908864
81.717887	2219.134912	21.913882
82.303364	2213.109809	21.918899
82.132837	2214.449483	21.923917
82.196739	2222.610566	21.928935
82.153369	2214.638853	21.933952
82.098861	2216.114998	21.938970
82.500948	2218.561109	21.943987
82.532026	2218.187014	21.949005
82.361521	2211.999462	21.954023
82.659366	2215.557061	21.959040
82.511655	2220.863495	21.964058
83.011672	2205.323614	21.969075
82.687518	2195.158250	21.974093
82.427288	2207.438276	21.979111
82.674388	2212.644979	21.984128
82.614019	2215.580145	21.989146
82.683903	2212.848699	21.994163
82.791107	2209.445476	21.999181
82.748968	2209.486828	22.004199
82.613787	2218.808972	22.009216
82.730974	2231.998797	22.014234
82.994664	2235.454444	22.019251
82.876225	2231.174465	22.024269
83.052902	2240.188963	22.029287
83.340510	2249.684745	22.034304
83.426039	2271.246313	22.039322
83.653675	2266.426069	22.044339
83.606572	2270.836209	22.049357
83.801552	2265.481393	22.054375
83.945068	2261.718990	22.059392
83.618971	2262.275086	22.064410
83.749383	2274.244625	22.069427
83.791861	2287.200021	22.074445
83.651216	2295.904469	22.079463
84.119539	2290.096529	22.084480
84.202016	2307.075989	22.089498
84.927403	2312.428713	22.094515
84.664581	2309.364336	22.099533
84.657918	2317.555454	22.104551
84.919073	2310.905729	22.109568
85.355348	2305.705617	22.114586
85.227919	2308.499813	22.119603
85.348942	2301.834172	22.124621
85.251729	2302.774169	22.129639
84.945600	2300.376199	22.134656
85.341537	2299.528335	22.139674
85.397035	2298.632815	22.144691
85.235973	2302.416976	22.149709
85.165883	2325.006624	22.154727
85.893597	2321.865958	22.159744
85.624573	2335.905390	22.164762
85.827405	2330.669255	22.169779
85.865101	2327.535699	22.174797
85.936052	2328.016966	22.179815
86.004729	2314.659149	22.184832
86.027077	2319.986310	22.189850
86.013195	2331.924841	22.194867
86.233782	2336.293058	22.199885
86.320026	2344.027780	22.204903
86.805423	2334.231009	22.209920
86.521254	2347.985619	22.214938
87.020357	2342.419015	22.219955
86.892448	2338.260425	22.224973
86.791999	2348.022202	22.229991
87.126416	2338.097591	22.235008
87.346061	2332.164482	22.240026
86.741459	2334.926134	22.245043
87.166526	2345.950071	22.250061
87.293659	2360.419806	22.255079
87.470511	2354.982588	22.260096
87.373850	2371.491512	22.265114
87.647821	2351.618885	22.270131
87.622539	2363.054248	22.275149
87.134042	2363.004571	22.280167
87.957514	2355.433522	22.285184
87.790029	2364.363135	22.290202
88.453231	2375.671703	22.295219
88.338042	2380.064133	22.300237
88.270749	2380.595465	22.305255
88.487315	2392.153917	22.310272
88.301346	2377.119032	22.315290
88.629019	2374.700656	22.320307
88.826366	2374.884385	22.325325
88.611762	2382.909277	22.330343
88.608444	2377.355100	22.335360
88.681938	2372.110811	22.340378
88.750125	2368.499057	22.345395
88.487591	2379.384567	22.350413
88.665839	2381.420761	22.355431
88.977441	2392.759177	22.360448
89.368378	2398.934415	22.365466
89.408217	2393.013676	22.370483
89.413703	2397.216774	22.375501
89.568267	2404.931350	22.380519
89.593017	2393.483486	22.385536
89.596543	2405.027982	22.390554
89.525751	2411.060949	22.395571
89.333246	2406.956648	22.400589
89.362040	2410.297638	22.405607
89.649319	2419.187591	22.410624
90.094523	2432.496602	22.415642
89.800688	2432.646822	22.420659
89.811134	2420.730922	22.425677
90.039954	2437.715983	22.430695
90.808076	2434.613153	22.435712
90.572392	2445.882697	22.440730
90.854536	2442.597204	22.445747
91.008821	2440.609966	22.450765
90.794598	2440.173302	22.455783
90.904106	2446.282184	22.460800
90.995637	2440.028251	22.465818
90.540167	2442.750774	22.470835
91.129615	2436.961684	22.475853
91.351993	2456.785112	22.480871
91.321907	2463.717523	22.485888
91.400792	2462.871984	22.490906
91.293254	2463.718922	22.495923
91.904599	2456.686044	22.500941
91.709757	2457.464601	22.505959
91.912508	2454.971103	22.510976
92.052565	2457.710790	22.515994
91.958253	2453.483787	22.521011
92.424665	2445.552035	22.526029
92.209909	2449.171054	22.531047
92.244676	2444.201081	22.536064
92.260680	2455.377546	22.541082
92.459485	2463.770092	22.546099
92.610436	2472.728772	22.551117
92.688131	2474.477744	22.556135
92.888209	2467.496670	22.561152
92.831869	2469.424446	22.566170
92.926952	2469.750443	22.571187
93.084335	2471.193411	22.576205
93.215847	2477.125270	22.581223
92.841999	2463.688336	22.586240
93.089605	2474.538165	22.591258
93.010124	2492.600473	22.596275
93.646373	2486.015006	22.601293
93.408727	2490.085788	22.606311
93.542986	2491.595503	22.611328
93.673656	2485.957177	22.616346
93.509069	2491.004377	22.621363
93.688157	2504.411945	22.626381
93.543619	2521.742787	22.631399
94.115284	2517.329370	22.636416
94.133370	2515.148847	22.641434
93.926326	2516.595260	22.646451
94.233910	2530.642345	22.651469
93.861757	2530.486067	22.656487
94.272556	2535.013900	22.661504
94.256012	2535.600408	22.666522
94.310960	2553.553345	22.671539
94.486030	2548.059538	22.676557
94.816192	2558.643994	22.681575
94.940700	2555.070720	22.686592
94.918019	2553.177474	22.691610
94.934338	2569.069215	22.696627
95.712894	2569.082985	22.701645
95.471049	2580.262051	22.706663
95.408142	2581.638545	22.711680
95.532684	2577.784366	22.716698
95.368879	2586.394742	22.721715
95.622723	2583.492393	22.726733
95.905706	2583.249255	22.731751
95.974508	2575.846848	22.736768
95.982749	2573.686796	22.741786
96.134123	2594.206381	22.746803
96.173077	2593.692174	22.751821
96.275676	2599.941061	22.756839
96.833531	2593.232124	22.761856
96.867544	2601.745237	22.766874
96.331264	2596.725818	22.771891
96.870085	2591.736801	22.776909
96.589731	2598.900997	22.781927
96.942540	2595.200420	22.786944
97.070204	2606.697191	22.791962
97.291685	2617.854189	22.796979
97.401784	2622.788955	22.801997
97.651340	2637.021959	22.807015
97.707120	2622.952646	22.812032
97.810537	2623.078503	22.817050
97.650133	2623.602337	22.822067
97.803903	2617.524804	22.827085
97.828322	2618.499414	22.832103
97.969132	2619.954460	22.837120
98.014410	2622.188258	22.842138
97.898236	2631.318269	22.847155
98.290341	2617.234142	22.852173
97.944719	2615.741816	22.857191
98.012779	2633.345603	22.862208
98.425403	2637.661715	22.867226
98.125285	2640.946970	22.872243
98.123185	2644.286531	22.877261
98.182491	2649.036738	22.882279
98.691016	2652.911750	22.887296
98.908432	2660.228383	22.892314
98.642599	2663.786011	22.897331
99.159055	2672.539188	22.902349
99.481530	2683.547846	22.907367
99.283508	2684.472094	22.912384
99.353164	2683.489120	22.917402
99.175620	2677.665467	22.922419
99.322940	2682.780631	22.927437
99.711494	2697.613668	22.932455
99.494067	2701.640299	22.937472
100.113913	2704.383759	22.942490
100.009289	2708.799863	22.947507
100.132088	2706.726001	22.952525
100.420230	2700.879880	22.957543
100.429387	2711.640964	22.962560
100.484716	2719.857271	22.967578
100.478593	2731.457143	22.972595
100.530161	2726.456055	22.977613
100.898048	2726.609914	22.982631
100.908196	2720.207670	22.987648
100.909214	2718.809367	22.992666
100.994650	2730.098214	22.997683
101.369945	2725.273651	23.002701
101.672886	2739.864487	23.007719
101.462249	2738.218444	23.012736
101.844418	2743.593511	23.017754
101.620623	2746.453370	23.022771
101.932333	2746.928490	23.027789
101.877570	2748.262691	23.032807
101.670195	2754.418168	23.037824
102.134288	2751.599631	23.042842
101.847861	2757.852710	23.047859
102.255035	2742.939210	23.052877
102.234060	2739.555969	23.057895
102.248930	2744.663496	23.062912
102.276715	2732.066099	23.067930
102.347356	2748.359788	23.072947
102.278845	2761.793715	23.077965
102.150833	2762.738560	23.082983
102.189721	2774.331407	23.088000
102.536238	2783.448973	23.093018
102.797830	2795.644488	23.098035
102.692488	2791.659003	23.103053
103.032024	2788.014121	23.108071
103.468895	2807.147849	23.113088
103.823122	2818.811255	23.118106
103.672704	2822.442362	23.123123
103.731659	2814.214482	23.128141
103.701737	2819.319579	23.133159
103.532238	2818.778056	23.138176
103.754699	2815.590219	23.143194
103.919861	2821.589513	23.148211
104.135673	2828.919091	23.153229
104.244270	2825.749091	23.158247
103.896322	2833.804543	23.163264
103.944314	2838.095770	23.168282
104.303139	2852.324450	23.173299
104.678967	2854.569614	23.178317
104.927648	2846.839077	23.183335
104.887293	2848.647611	23.188352
105.245387	2850.229599	23.193370
105.275333	2844.215576	23.198387
105.303076	2846.455306	23.203405
105.605561	2844.438493	23.208423
105.787823	2857.934201	23.213440
105.879198	2856.711101	23.218458
106.046732	2861.176133	23.223475
106.103659	2858.288810	23.228493
106.404002	2843.025847	23.233511
106.188904	2841.951761	23.238528
106.532268	2842.851166	23.243546
106.534387	2851.438830	23.248563
106.589593	2845.578658	23.253581
106.568185	2843.489499	23.258599
106.267204	2840.348946	23.263616
106.592266	2845.994954	23.268634
106.629661	2850.739178	23.273651
106.635230	2850.716246	23.278669
106.625298	2844.490694	23.283687
106.796924	2862.583468	23.288704
106.960028	2863.725735	23.293722
107.197169	2872.235558	23.298739
107.183906	2875.024579	23.303757
107.297406	2876.376614	23.308775
107.396398	2893.489757	23.313792
107.665328	2890.809085	23.318810
107.872821	2899.604466	23.323827
108.030518	2893.172733	23.328845
108.303082	2897.125797	23.333863
108.039261	2891.501807	23.338880
107.876331	2890.002928	23.343898
107.915139	2907.318040	23.348915
108.271580	2920.985347	23.353933
108.470742	2924.634298	23.358951
108.454657	2929.860350	23.363968
108.710411	2910.984162	23.368986
109.078701	2916.992694	23.374003
108.946063	2913.279734	23.379021
109.280683	2922.484452	23.384039
109.171259	2929.647249	23.389056
109.491463	2933.043679	23.394074
109.593485	2940.463723	23.399091
109.682865	2932.540330	23.404109
109.657696	2928.564346	23.409127
109.744315	2936.214048	23.414144
109.449324	2926.643375	23.419162
109.762096	2930.151436	23.424179
109.492586	2936.329334	23.429197
110.053544	2946.369714	23.434215
109.730919	2958.069816	23.439232
110.339861	2957.671452	23.444250
110.418464	2954.411443	23.449267
110.245601	2971.920746	23.454285
110.646585	2976.478636	23.459303
110.931835	2986.925196	23.464320
111.134132	2983.882518	23.469338
111.093869	2970.964213	23.474355
110.931665	2990.245649	23.479373
111.090406	2980.234586	23.484391
111.010821	2984.381713	23.489408
111.510433	2990.754753	23.494426
111.807495	3003.664468	23.499443
111.478158	3001.841311	23.504461
111.651900	3003.736254	23.509479
111.665258	3007.379613	23.514496
112.114461	3021.348084	23.519514
112.177839	3022.026242	23.524531
112.355344	3016.825439	23.529549
112.727830	3013.812904	23.534567
112.504166	3018.310857	23.539584
112.762175	3007.551986	23.544602
112.747844	3010.338040	23.549619
112.922996	3011.768800	23.554637
113.182040	3005.781955	23.559655
112.828739	3020.876670	23.564672
112.872591	3030.458400	23.569690
113.061253	3026.893920	23.574707
113.344832	3037.908889	23.579725
113.544269	3039.310598	23.584743
113.468319	3042.384056	23.589760
113.620787	3053.261766	23.594778
113.921613	3061.004209	23.599795
113.765577	3063.241196	23.604813
114.088192	3053.706257	23.609831
114.109678	3062.903293	23.614848
114.469470	3058.986906	23.619866
114.293247	3074.442138	23.624883
114.344058	3077.375807	23.629901
114.663087	3079.718273	23.634919
114.569301	3089.170098	23.639936
114.869173	3089.842770	23.644954
115.078965	3077.806829	23.649971
114.757154	3088.929301	23.654989
115.261411	3100.357919	23.660007
115.112552	3099.999371	23.665024
115.249143	3110.560824	23.670042
115.500671	3101.652460	23.675059
115.817321	3129.926856	23.680077
115.986002	3122.922043	23.685095
115.808432	3131.446461	23.690112
115.670054	3123.808008	23.695130
115.913649	3124.994494	23.700147
115.794115	3138.256790	23.705165
116.273990	3132.598273	23.710183
116.211606	3144.888970	23.715200
116.370222	3147.537481	23.720218
116.505908	3134.465244	23.725235
116.796908	3142.196637	23.730253
116.932413	3135.045518	23.735271
116.526041	3152.133925	23.740288
116.674601	3164.631462	23.745306
117.307446	3165.438188	23.750323
117.214845	3168.883556	23.755341
117.409751	3154.763625	23.760359
117.749248	3167.284906	23.765376
117.832271	3181.493932	23.770394
118.263526	3189.904057	23.775411
117.835640	3189.500847	23.780429
118.211066	3174.430997	23.785447
118.434836	3178.492768	23.790464
118.234470	3185.988694	23.795482
118.277800	3176.731007	23.800499
118.485072	3192.621788	23.805517
118.615936	3195.183123	23.810535
119.007470	3200.714673	23.815552
119.195968	3201.338517	23.820570
119.120747	3202.309832	23.825587
118.945104	3202.482570	23.830605
119.380855	3202.976146	23.835623
119.238129	3204.030630	23.840640
119.205622	3214.299856	23.845658
119.618701	3216.302513	23.850675
119.484242	3227.764998	23.855693
119.635888	3226.396712	23.860711
119.715402	3230.089721	23.865728
119.352567	3234.505374	23.870746
120.142227	3244.371217	23.875763
119.975680	3251.154872	23.880781
120.246101	3253.227226	23.885799
120.380094	3272.412058	23.890816
120.673388	3277.491898	23.895834
121.002143	3278.794459	23.900851
121.136435	3280.705081	23.905869
121.181628	3275.846871	23.910887
120.993355	3276.472932	23.915904
121.126875	3286.555219	23.920922
121.243368	3287.925754	23.925939
121.525588	3301.043165	23.930957
121.785661	3296.870912	23.935975
121.449381	3296.709004	23.940992
121.883951	3312.191841	23.946010
122.082348	3310.772038	23.951027
122.159915	3319.644793	23.956045
122.312779	3320.122723	23.961063
122.120135	3314.304385	23.966080
122.405643	3319.565364	23.971098
122.746405	3325.300595	23.976115
122.535842	3333.508339	23.981133
122.998755	3325.453659	23.986151
123.439018	3326.991255	23.991168
123.173822	3323.649322	23.996186
123.594588	3331.249998	24.001203
123.459328	3328.058146	24.006221
123.703719	3333.445508	24.011239
123.896324	3344.039354	24.016256
124.134851	3348.111476	24.021274
124.184369	3359.838755	24.026291
124.050340	3345.416706	24.031309
124.065010	3355.631277	24.036327
124.825763	3352.570484	24.041344
124.470294	3358.913493	24.046362
124.291660	3351.161313	24.051379
124.573285	3356.710131	24.056397
124.621646	3353.003442	24.061415
125.053957	3347.784718	24.066432
124.346155	3355.274993	24.071450
124.548357	3360.788911	24.076467
124.314696	3366.008146	24.081485
124.903471	3384.225467	24.086503
125.244167	3395.020237	24.091520
125.268977	3400.350489	24.096538
125.259867	3385.422771	24.101555
125.600106	3411.885370	24.106573
125.544608	3421.946845	24.111591
125.897029	3423.406680	24.116608
125.999640	3427.099266	24.121626
126.173542	3442.600961	24.126643
126.424877	3449.076187	24.131661
126.566734	3453.185573	24.136679
126.756222	3447.780767	24.141696
126.388959	3454.182470	24.146714
126.964009	3459.234001	24.151731
127.202687	3471.566130	24.156749
127.180853	3473.103540	24.161767
127.419910	3479.331355	24.166784
127.255309	3462.322689	24.171802
127.557556	3465.343281	24.176819
127.694712	3480.352072	24.181837
127.530941	3486.702968	24.186855
127.740779	3482.727920	24.191872
127.900956	3494.889299	24.196890
127.801805	3492.177829	24.201907
128.283827	3508.587665	24.206925
128.408620	3506.623870	24.211943
128.545065	3505.093818	24.216960
128.630699	3509.385621	24.221978
129.037690	3525.314844	24.226995
129.051965	3538.032524	24.232013
129.263022	3526.276999	24.237031
129.074371	3525.075631	24.242048
129.243432	3529.310180	24.247066
129.243091	3529.344986	24.252083
129.868394	3543.822846	24.257101
129.493515	3549.193665	24.262119
130.215353	3542.745914	24.267136
129.614577	3550.200564	24.272154
130.207479	3548.649497	24.277171
130.518855	3563.144992	24.282189
130.931178	3566.066292	24.287207
130.956655	3561.299471	24.292224
130.752617	3572.905640	24.297242
130.908828	3563.282876	24.302259
130.742441	3559.249970	24.307277
131.423609	3564.010308	24.312295
131.519585	3552.537924	24.317312
131.114101	3570.570321	24.322330
131.443700	3569.792767	24.327347
131.942910	3580.925790	24.332365
132.145809	3585.492776	24.337383
132.168326	3578.731627	24.342400
132.064385	3577.898898	24.347418
132.064298	3576.144039	24.352435
132.408960	3582.453190	24.357453
132.177627	3581.713013	24.362471
132.439172	3593.445102	24.367488
132.519881	3609.513894	24.372506
132.583798	3611.265136	24.377523
132.615616	3609.855625	24.382541
132.845137	3623.193000	24.387559
132.865855	3635.000721	24.392576
133.003410	3637.030810	24.397594
133.185817	3630.831667	24.402611
133.523371	3637.675369	24.407629
132.909111	3657.962608	24.412647
133.632802	3665.796880	24.417664
133.163839	3673.489747	24.422682
133.953738	3676.790641	24.427699
133.955919	3678.198053	24.432717
133.847567	3679.341869	24.437735
134.157730	3689.216797	24.442752
134.395708	3702.325650	24.447770
134.560642	3700.709054	24.452787
134.483456	3719.283555	24.457805
134.707897	3720.974939	24.462823
134.873391	3724.654579	24.467840
134.680395	3729.993800	24.472858
135.369345	3742.956278	24.477875
135.702250	3758.676372	24.482893
135.479897	3761.782357	24.487911
135.742880	3750.545660	24.492928
136.144375	3763.812008	24.497946
136.071735	3756.614344	24.502963
136.027583	3765.361196	24.507981
136.363361	3775.339474	24.512999
137.178125	3770.423693	24.518016
136.660350	3776.495578	24.523034
136.827624	3778.757753	24.528051
136.896188	3774.640644	24.533069
136.989250	3780.550551	24.538087
137.316816	3791.344460	24.543104
137.061611	3807.327175	24.548122
137.277257	3798.386216	24.553139
137.740525	3794.825910	24.558157
137.831358	3795.569236	24.563175
137.514394	3811.678415	24.568192
137.905024	3829.362244	24.573210
137.975907	3823.814934	24.578227
138.140077	3818.814841	24.583245
138.792767	3834.819475	24.588263
139.152104	3833.188193	24.593280
138.994831	3836.148273	24.598298
138.872804	3832.771189	24.603315
139.169125	3837.415138	24.608333
138.998940	3840.320426	24.613351
139.180944	3832.587291	24.618368
139.196092	3849.976454	24.623386
139.509689	3862.625374	24.628403
139.639120	3868.510674	24.633421
139.400577	3860.786597	24.638439
140.108786	3869.696546	24.643456
140.209609	3884.894434	24.648474
140.258759	3874.057299	24.653491
140.425689	3873.803922	24.658509
140.037038	3886.575502	24.663527
140.287668	3883.591386	24.668544
140.499647	3903.803114	24.673562
140.774731	3906.016851	24.678579
141.193584	3916.881756	24.683597
141.090468	3922.727753	24.688615
141.077343	3921.385230	24.693632
141.561605	3910.928109	24.698650
141.848903	3926.141007	24.703667
141.906932	3920.428394	24.708685
141.934973	3949.885582	24.713703
142.165566	3943.779788	24.718720
141.893049	3950.962226	24.723738
142.369040	3951.490556	24.728755
142.599900	3948.061322	24.733773
142.900132	3967.776370	24.738791
143.171568	3957.832334	24.743808
143.211359	3954.805485	24.748826
143.150982	3963.495003	24.753843
143.445452	3956.883647	24.758861
143.373860	3959.773508	24.763879
143.497124	3963.242023	24.768896
143.562902	3962.562600	24.773914
143.753612	3956.886004	24.778931
143.702324	3965.788733	24.783949
143.527102	3975.339001	24.788967
144.021224	3978.749418	24.793984
144.484120	3978.531739	24.799002
144.176594	3989.002309	24.804019
144.939705	3996.997840	24.809037
144.521649	4001.835815	24.814055
144.886078	4002.018640	24.819072
145.000668	4005.299139	24.824090
144.712972	4001.985854	24.829107
145.412607	4013.539110	24.834125
145.286542	4028.068790	24.839143
145.338698	4030.895086	24.844160
144.974191	4035.778339	24.849178
145.832872	4056.447602	24.854195
146.038687	4053.287409	24.859213
145.888609	4064.086872	24.864231
146.341051	4075.375880	24.869248
146.430159	4076.798112	24.874266
146.612624	4071.791927	24.879283
146.674588	4061.634453	24.884301
146.982374	4077.803811	24.889319
147.168133	4085.457407	24.894336
147.905758	4083.283911	24.899354
147.852855	4088.143611	24.904371
147.728197	4089.375230	24.909389
147.735527	4088.613424	24.914407
148.191511	4075.717589	24.919424
148.494449	4076.566578	24.924442
148.354996	4073.810833	24.929459
148.465562	4071.457813	24.934477
148.297957	4082.020146	24.939495
148.751274	4092.854508	24.944512
149.010849	4100.016773	24.949530
149.056873	4107.625985	24.954547
149.076683	4092.595305	24.959565
149.177421	4106.262540	24.964583
148.992846	4108.418903	24.969600
148.932285	4126.239993	24.974618
149.177304	4119.958278	24.979635
149.379900	4127.946989	24.984653
149.834393	4162.312204	24.989671
149.791761	4157.748437	24.994688
149.978685	4163.078767	24.999706
150.052494	4176.283125	25.004723
150.328260	4179.298518	25.009741
150.281130	4188.222800	25.014759
150.328117	4202.460369	25.019776
150.602391	4198.623423	25.024794
150.763766	4215.273522	25.029811
151.018623	4219.901970	25.034829
151.270319	4227.431665	25.039847
151.306183	4224.777843	25.044864
151.618209	4235.691241	25.049882
151.884747	4244.976745	25.054899
152.130792	4251.835017	25.059917
152.285593	4251.908648	25.064935
152.390028	4241.289894	25.069952
152.838150	4247.990250	25.074970
152.547297	4248.828112	25.079987
152.748221	4257.173818	25.085005
152.955694	4262.901824	25.090023
153.188727	4264.134233	25.095040
153.323899	4260.906161	25.100058
153.042518	4266.111033	25.105075
153.293266	4269.338685	25.110093
153.410289	4281.665176	25.115111
154.014095	4282.836343	25.120128
154.009961	4279.551180	25.125146
153.877244	4284.275085	25.130163
154.025517	4300.188711	25.135181
154.185313	4304.604811	25.140199
154.487662	4304.724768	25.145216
155.159469	4301.857674	25.150234
154.759374	4307.516744	25.155251
154.913084	4325.175048	25.160269
155.362259	4331.278703	25.165287
155.350629	4325.021343	25.170304
155.711640	4321.600057	25.175322
155.313210	4331.412744	25.180339
155.700391	4359.703268	25.185357
156.104588	4363.588689	25.190375
155.876632	4357.747138	25.195392
156.068321	4358.051723	25.200410
156.011350	4374.250083	25.205427
156.193595	4380.395573	25.210445
156.370448	4385.989532	25.215463
156.666328	4400.765895	25.220480
156.422367	4411.321443	25.225498
156.776710	4421.884270	25.230515
157.057257	4426.051062	25.235533
157.329845	4436.939195	25.240551
157.118256	4448.622861	25.245568
157.719913	4451.334728	25.250586
157.753566	4458.238979	25.255603
157.648412	4467.074637	25.260621
158.405932	4478.019396	25.265639
158.707239	4475.958402	25.270656
158.950418	4468.676256	25.275674
158.630672	4487.501027	25.280691
159.069798	4499.177475	25.285709
159.563802	4492.424190	25.290727
159.400645	4499.630745	25.295744
159.548751	4495.355815	25.300762
159.786540	4492.010619	25.305779
160.140163	4508.943359	25.310797
160.172681	4511.703365	25.315815
160.601838	4517.658710	25.320832
160.583479	4516.089697	25.325850
160.537690	4527.245559	25.330867
160.446386	4515.221116	25.335885
160.660098	4516.188270	25.340903
160.818462	4523.265552	25.345920
161.161987	4534.092128	25.350938
161.093212	4540.318032	25.355955
161.286279	4536.591588	25.360973
161.573312	4535.713345	25.365991
161.661788	4557.021508	25.371008
162.060318	4551.520497	25.376026
162.080093	4568.859121	25.381043
161.662101	4556.383950	25.386061
161.746389	4579.652968	25.391079
161.663541	4587.288884	25.396096
162.221912	4597.466325	25.401114
162.452678	4610.526464	25.406131
162.580823	4611.743764	25.411149
163.018325	4635.882369	25.416167
163.241710	4644.458316	25.421184
163.695176	4637.528251	25.426202
163.540523	4632.426372	25.431219
163.903208	4634.244541	25.436237
164.044551	4647.350280	25.441255
164.132949	4642.510188	25.446272
164.413812	4642.431499	25.451290
164.378139	4647.897853	25.456307
164.428778	4651.845039	25.461325
164.756234	4652.046291	25.466343
165.087670	4674.661196	25.471360
165.146563	4671.296647	25.476378
165.154672	4673.040952	25.481395
165.218879	4670.385782	25.486413
165.507243	4677.123953	25.491431
165.521451	4691.051391	25.496448
166.137468	4702.741294	25.501466
165.944565	4700.558840	25.506483
165.846832	4707.591090	25.511501
166.195331	4716.614632	25.516519
166.440554	4727.292585	25.521536
166.688870	4721.947630	25.526554
166.504340	4738.522983	25.531571
166.756344	4742.912119	25.536589
167.035463	4746.113317	25.541607
167.114016	4766.741474	25.546624
167.430223	4777.686110	25.551642
167.096676	4770.828786	25.556659
167.585777	4788.466562	25.561677
167.880919	4793.205639	25.566695
168.162235	4791.589655	25.571712
168.453105	4809.151185	25.576730
168.797896	4816.404550	25.581747
168.909613	4815.408559	25.586765
168.818566	4818.689857	25.591783
168.900366	4825.981270	25.596800
169.454228	4829.177319	25.601818
169.412339	4835.525373	25.606835
169.588831	4842.079114	25.611853
169.620978	4847.080363	25.616871
169.676894	4867.854225	25.621888
170.116287	4853.596820	25.626906
170.096057	4860.257143	25.631923
170.450666	4876.328340	25.636941
171.097261	4880.365292	25.641959
171.146247	4892.968005	25.646976
171.057808	4885.257853	25.651994
171.287262	4885.777490	25.657011
171.110907	4891.771002	25.662029
171.600708	4903.322981	25.667047
171.389783	4905.306798	25.672064
171.611660	4905.366768	25.677082
171.776526	4910.580826	25.682100
171.906767	4920.238406	25.687117
171.947180	4920.257360	25.692135
172.262123	4947.221745	25.697152
172.397098	4954.040867	25.702170
172.508555	4963.622498	25.707188
172.946663	4969.485050	25.712205
173.237431	4968.015928	25.717223
173.117334	4979.556181	25.722240
173.527631	4986.717283	25.727258
173.842258	5002.125666	25.732276
173.486588	5003.772323	25.737293
174.010118	5005.202329	25.742311
174.071623	5027.206554	25.747328
174.238083	5025.172938	25.752346
174.485692	5026.608293	25.757364
174.465016	5031.595772	25.762381
174.922178	5028.875832	25.767399
174.987252	5044.171832	25.772416
175.187720	5049.415075	25.777434
175.409412	5043.865864	25.782452
175.458447	5053.807700	25.787469
175.566078	5059.706272	25.792487
176.408865	5069.236520	25.797504
176.401403	5065.976990	25.802522
176.294192	5073.771597	25.807540
176.094122	5074.781510	25.812557
176.412263	5084.883225	25.817575
176.433412	5095.842711	25.822592
176.633396	5091.575298	25.827610
176.865295	5107.110367	25.832628
177.288658	5112.325023	25.837645
177.154477	5112.885851	25.842663
177.267516	5140.055764	25.847680
177.425007	5141.420019	25.852698
177.817641	5149.060595	25.857716
178.017533	5161.450458	25.862733
178.467596	5166.957666	25.867751
178.573232	5193.320732	25.872768
178.505635	5195.894505	25.877786
178.994010	5196.648211	25.882804
179.320233	5197.869243	25.887821
179.348153	5202.558750	25.892839
179.544697	5214.160027	25.897856
179.722376	5209.804539	25.902874
179.885467	5215.375658	25.907892
180.104106	5219.151445	25.912909
180.087982	5230.432511	25.917927
180.098598	5236.576770	25.922944
180.249587	5240.255836	25.927962
180.586138	5255.904058	25.932980
180.196548	5276.808155	25.937997
180.599879	5276.113682	25.943015
180.877282	5293.911379	25.948032
181.161859	5292.443202	25.953050
181.137136	5314.505475	25.958068
181.724027	5323.157373	25.963085
181.940223	5339.525289	25.968103
181.689206	5341.455458	25.973120
182.263728	5346.614934	25.978138
182.508967	5361.368448	25.983156
182.515099	5359.795525	25.988173
183.091182	5360.554439	25.993191
182.977084	5394.095644	25.998208
183.413787	5388.698886	26.003226
183.756693	5389.510113	26.008244
183.589134	5386.016764	26.013261
183.909111	5394.183355	26.018279
183.895573	5416.120890	26.023296
184.302141	5411.748437	26.028314
184.669630	5400.828954	26.033332
184.708103	5431.899944	26.038349
185.040848	5429.508788	26.043367
185.135794	5440.469547	26.048384
185.499796	5432.890307	26.053402
185.385059	5428.990939	26.058420
185.421588	5449.190838	26.063437
185.553984	5449.208010	26.068455
186.119158	5459.397499	26.073472
185.789471	5464.004204	26.078490
185.899908	5466.228146	26.083508
186.327421	5485.429314	26.088525
186.401900	5483.848830	26.093543
186.702790	5499.395523	26.098560
186.843349	5508.972882	26.103578
186.856035	5493.222447	26.108596
187.152421	5511.361457	26.113613
187.380628	5521.689000	26.118631
187.449924	5521.062632	26.123648
187.710218	5529.248104	26.128666
188.217935	5543.345099	26.133684
187.919880	5549.067480	26.138701
188.056966	5545.911485	26.143719
188.516931	5568.883008	26.148736
188.563265	5574.393612	26.153754
188.799667	5575.606646	26.158772
188.852559	5589.607627	26.163789
189.152753	5596.928268	26.168807
189.231836	5604.539241	26.173824
190.089584	5625.125219	26.178842
190.129552	5621.337310	26.183860
189.955965	5635.449566	26.188877
190.197782	5630.540985	26.193895
190.327297	5646.168314	26.198912
190.701923	5648.805451	26.203930
190.881507	5644.938845	26.208948
190.965490	5666.495230	26.213965
191.303728	5666.827389	26.218983
191.961833	5669.805233	26.224000
191.643500	5674.359705	26.229018
192.341084	5677.100929	26.234036
192.264459	5687.239570	26.239053
192.532613	5686.992411	26.244071
192.709306	5688.268469	26.249088
192.821129	5691.151967	26.254106
192.974436	5691.285817	26.259124
192.961187	5706.013814	26.264141
193.180378	5708.931002	26.269159
193.223541	5707.952017	26.274176
193.620981	5720.377604	26.279194
193.695344	5726.092203	26.284212
193.725958	5742.511652	26.289229
194.081541	5754.798612	26.294247
194.087915	5762.796687	26.299264
194.124424	5763.788514	26.304282
194.813589	5778.466507	26.309300
194.669849	5789.136572	26.314317
195.184521	5802.838093	26.319335
195.137373	5807.713134	26.324352
195.597650	5807.634747	26.329370
195.788691	5810.597398	26.334388
195.918729	5833.100087	26.339405
195.947417	5833.262930	26.344423
196.164373	5843.437740	26.349440
196.177102	5863.111500	26.354458
196.470670	5860.391816	26.359476
196.703797	5873.736596	26.364493
197.202161	5879.208044	26.369511
197.005691	5880.460501	26.374528
197.304733	5896.743336	26.379546
197.855323	5898.093417	26.384564
197.950314	5910.260314	26.389581
198.220441	5919.988054	26.394599
198.473131	5921.804649	26.399616
198.482080	5926.364731	26.404634
198.933198	5928.361741	26.409652
199.038750	5945.719804	26.414669
198.984584	5943.023016	26.419687
199.276562	5957.182540	26.424704
199.515213	5962.909358	26.429722
199.619890	5975.387296	26.434740
199.719991	5974.554057	26.439757
199.747864	5982.552016	26.444775
200.040695	5997.576381	26.449792
200.486992	6007.724825	26.454810
200.887413	6002.238870	26.459828
200.774632	6008.314332	26.464845
200.814590	6019.309307	26.469863
201.354684	6020.493736	26.474880
201.330413	6027.530768	26.479898
201.780105	6026.832164	26.484916
201.835733	6054.407023	26.489933
202.029262	6050.695984	26.494951
202.362456	6048.535121	26.499968
202.547352	6067.651798	26.504986
203.025439	6082.047430	26.510004
202.663372	6075.841211	26.515021
202.826108	6083.230934	26.520039
203.316314	6083.229934	26.525056
203.272545	6104.232322	26.530074
203.407039	6088.740086	26.535092
203.601595	6115.709276	26.540109
203.713810	6124.451704	26.545127
204.122631	6140.900650	26.550144
204.143517	6158.382665	26.555162
204.458608	6156.281446	26.560180
204.722142	6172.153398	26.565197
204.625567	6174.049987	26.570215
205.231914	6189.716725	26.575232
205.328425	6198.638428	26.580250
205.891572	6201.233487	26.585268
206.132961	6213.052505	26.590285
206.194212	6226.604404	26.595303
206.225257	6226.763726	26.600320
206.255098	6238.742172	26.605338
207.066196	6240.685980	26.610356
206.929685	6248.432013	26.615373
207.261199	6252.430248	26.620391
207.726500	6256.909451	26.625408
207.633394	6269.835269	26.630426
208.104369	6265.105280	26.635444
208.405850	6270.771844	26.640461
208.418014	6292.005599	26.645479
208.784969	6279.251593	26.650496
208.723952	6290.893904	26.655514
209.185477	6284.318677	26.660532
209.250886	6294.691102	26.665549
209.316436	6307.349019	26.670567
209.849188	6312.354323	26.675584
209.960965	6301.016633	26.680602
209.956951	6312.463779	26.685620
210.314127	6314.352435	26.690637
210.232518	6322.680216	26.695655
210.684857	6331.918741	26.700672
210.292672	6346.340429	26.705690
210.686277	6338.055374	26.710708
211.401090	6366.594432	26.715725
211.367139	6374.804283	26.720743
211.555729	6363.874374	26.725760
211.704520	6385.263615	26.730778
212.050040	6388.650425	26.735796
212.262727	6394.990707	26.740813
212.344557	6403.330802	26.745831
212.905188	6412.284076	26.750848
212.465688	6420.349131	26.755866
213.064895	6432.803576	26.760884
213.239295	6443.840881	26.765901
213.155084	6442.607169	26.770919
213.591922	6450.127725	26.775936
213.720740	6466.968078	26.780954
213.902561	6464.875076	26.785972
214.179593	6470.678117	26.790989
214.513475	6487.508463	26.796007
214.588608	6488.705784	26.801024
214.784942	6497.807717	26.806042
215.024088	6508.146733	26.811060
215.217629	6518.770699	26.816077
215.282277	6524.464972	26.821095
216.004698	6530.763330	26.826112
215.651872	6546.672184	26.831130
215.721336	6547.655734	26.836148
216.554911	6552.648704	26.841165
216.213388	6561.995926	26.846183
216.871948	6576.859299	26.851200
217.029636	6594.156143	26.856218
217.325382	6595.915552	26.861236
217.624364	6610.885792	26.866253
217.845827	6614.023748	26.871271
217.982463	6617.585382	26.876288
218.268253	6629.634476	26.881306
218.273484	6640.562657	26.886324
218.515717	6643.021802	26.891341
218.851357	6661.487274	26.896359
219.126694	6662.994182	26.901376
219.097049	6665.369647	26.906394
219.615385	6665.888280	26.911412
219.638125	6682.019375	26.916429
219.781414	6694.314972	26.921447
220.344730	6701.364390	26.926464
220.246542	6715.030019	26.931482
220.131117	6712.677340	26.936500
220.637470	6728.394932	26.941517
220.604939	6744.244310	26.946535
220.863297	6754.469965	26.951552
221.263029	6764.995479	26.956570
221.769343	6784.005729	26.961588
221.939442	6787.827330	26.966605
221.885697	6800.750512	26.971623
222.014552	6806.829423	26.976640
222.471210	6822.248665	26.981658
222.269295	6834.554237	26.986676
223.028672	6839.521029	26.991693
223.085761	6863.763221	26.996711
223.662142	6865.882774	27.001728
223.791408	6881.198666	27.006746
223.874837	6896.193437	27.011764
224.311325	6898.259143	27.016781
224.114577	6900.654502	27.021799
224.586918	6909.321949	27.026816
224.798936	6911.467018	27.031834
225.198618	6931.737938	27.036852
225.470572	6933.182262	27.041869
225.733469	6948.035312	27.046887
225.867639	6947.127241	27.051904
226.001188	6960.299000	27.056922
225.887676	6968.663641	27.061940
226.512435	6973.531596	27.066957
226.374763	6995.553606	27.071975
226.913052	7001.776798	27.076992
226.941182	7017.399082	27.082010
226.910501	7024.841584	27.087028
227.561163	7045.733105	27.092045
227.611385	7054.615123	27.097063
228.145112	7055.847976	27.102080
227.943586	7060.087738	27.107098
228.394417	7080.985350	27.112116
228.385413	7077.807782	27.117133
228.611969	7098.383816	27.122151
229.190227	7097.639781	27.127168
229.450982	7105.447060	27.132186
229.715355	7123.134932	27.137204
229.691407	7129.733524	27.142221
229.948430	7129.601742	27.147239
229.967190	7132.730503	27.152256
230.245213	7149.863801	27.157274
230.414522	7153.998139	27.162292
230.819700	7169.719332	27.167309
231.156078	7178.193535	27.172327
231.670654	7187.365920	27.177344
231.912939	7198.958136	27.182362
231.700224	7208.023479	27.187380
232.322527	7197.088273	27.192397
232.128313	7212.584550	27.197415
232.430740	7216.862209	27.202432
232.730436	7223.394350	27.207450
232.803143	7238.444747	27.212468
232.793291	7235.251500	27.217485
233.236512	7258.126750	27.222503
233.766409	7265.980329	27.227520
234.053747	7271.343197	27.232538
233.843718	7294.503929	27.237556
233.859188	7292.443208	27.242573
234.251403	7318.271956	27.247591
234.821220	7318.397398	27.252608
235.213721	7330.821700	27.257626
235.408795	7345.268978	27.262644
235.916985	7347.980152	27.267661
236.080741	7356.809803	27.272679
236.418030	7356.848551	27.277696
236.343405	7360.601272	27.282714
236.570319	7387.112661	27.287732
237.009335	7379.902866	27.292749
236.952961	7394.866276	27.297767
237.342505	7406.151427	27.302784
237.561172	7412.573207	27.307802
237.668455	7432.079144	27.312820
238.069595	7433.654807	27.317837
237.753871	7448.027492	27.322855
238.044713	7452.171271	27.327872
238.518694	7456.557862	27.332890
238.585491	7476.373259	27.337908
239.199217	7486.701502	27.342925
239.553976	7498.456236	27.347943
239.855332	7506.610908	27.352960
240.461830	7502.519187	27.357978
240.260211	7517.189750	27.362996
240.671801	7530.400444	27.368013
240.753929	7533.033169	27.373031
241.126695	7535.310980	27.378048
241.571977	7539.983059	27.383066
241.653448	7552.276287	27.388084
241.753417	7546.830631	27.393101
242.012964	7563.935641	27.398119
242.242258	7570.510504	27.403136
242.706857	7560.944669	27.408154
242.655095	7584.440870	27.413172
243.175046	7586.563037	27.418189
243.301614	7585.049982	27.423207
243.375691	7590.736795	27.428224
243.543084	7604.503545	27.433242
243.647514	7618.381192	27.438260
244.057346	7622.070703	27.443277
244.324719	7637.438202	27.448295
244.248494	7648.234519	27.453312
244.550370	7657.077405	27.458330
244.586669	7676.269549	27.463348
244.991136	7678.280380	27.468365
245.043389	7700.870156	27.473383
245.381057	7704.889848	27.478400
245.997136	7713.980300	27.483418
245.798564	7721.689317	27.488436
246.259731	7736.979186	27.493453
246.507120	7746.316832	27.498471
246.550368	7752.040095	27.503488
247.050603	7767.939489	27.508506
246.780399	7783.893291	27.513524
247.415309	7797.271244	27.518541
247.419477	7802.624957	27.523559
247.639882	7823.139625	27.528576
248.130950	7835.551985	27.533594
248.042179	7854.107241	27.538612
248.285472	7866.078566	27.543629
248.967618	7879.783826	27.548647
249.151989	7885.282972	27.553664
249.252783	7916.496786	27.558682
249.353315	7925.125091	27.563700
249.788923	7939.554098	27.568717
250.410780	7952.523791	27.573735
250.472480	7963.282901	27.578752
250.795476	7969.704318	27.583770
250.827331	7993.506803	27.588788
251.237939	8000.811114	27.593805
251.678312	8007.858199	27.598823
251.760993	8022.235218	27.603840
252.050869	8029.637380	27.608858
252.109975	8042.161747	27.613876
252.611500	8048.021678	27.618893
252.622898	8063.524344	27.623911
253.005056	8075.309883	27.628928
253.269692	8088.474543	27.633946
253.779109	8095.034127	27.638964
253.999031	8101.550664	27.643981
254.069307	8111.424532	27.648999
254.063363	8135.504631	27.654016
254.786164	8131.280901	27.659034
254.977302	8144.011964	27.664052
255.658450	8156.981985	27.669069
255.209520	8166.593094	27.674087
255.576220	8185.554054	27.679104
256.138922	8184.414624	27.684122
256.117715	8208.636122	27.689140
256.792658	8209.414414	27.694157
256.738139	8231.570098	27.699175
256.818420	8246.686431	27.704192
257.349418	8245.624578	27.709210
257.321360	8260.435868	27.714228
257.789124	8257.666449	27.719245
258.057342	8278.445645	27.724263
257.917971	8296.763017	27.729280
258.635065	8306.336765	27.734298
258.949548	8319.541139	27.739316
258.785627	8334.957839	27.744333
259.193833	8339.825360	27.749351
259.461606	8356.576218	27.754368
259.940681	8365.862099	27.759386
260.027944	8382.423416	27.764404
260.516299	8382.779475	27.769421
260.781265	8392.310438	27.774439
261.021996	8409.011909	27.779456
261.118541	8415.569985	27.784474
261.452990	8426.084580	27.789492
261.669513	8441.984801	27.794509
262.054086	8442.344491	27.799527
261.894505	8452.286120	27.804544
262.289399	8464.745543	27.809562
262.595913	8473.783838	27.814580
262.787880	8486.372936	27.819597
263.093433	8505.681620	27.824615
263.118040	8505.466269	27.829632
263.765374	8514.220722	27.834650
264.016846	8527.422487	27.839668
264.298478	8532.306730	27.844685
264.385415	8545.884727	27.849703
264.445049	8556.934965	27.854720
264.935705	8575.611706	27.859738
265.255370	8584.464881	27.864756
265.621387	8592.205788	27.869773
265.764431	8609.342646	27.874791
265.745605	8616.603973	27.879808
266.154886	8618.494184	27.884826
266.463941	8635.731348	27.889844
266.582238	8641.376829	27.894861
266.883340	8658.258498	27.899879
267.235028	8679.470232	27.904896
267.541703	8687.776140	27.909914
267.898930	8697.696929	27.914932
268.178914	8706.316431	27.919949
268.687837	8712.658468	27.924967
268.937541	8731.335226	27.929984
269.374437	8733.221123	27.935002
269.475577	8753.281928	27.940020
269.628580	8758.641017	27.945037
269.735419	8769.444040	27.950055
269.715562	8788.182026	27.955072
270.333300	8800.104771	27.960090
270.453043	8811.849802	27.965108
270.686327	8823.996963	27.970125
271.167110	8829.923540	27.975143
270.902227	8852.715947	27.980160
271.793087	8862.180679	27.985178
271.739123	8873.804571	27.990196
271.745510	8886.492471	27.995213
272.522574	8906.343369	28.000231
272.942852	8924.576849	28.005248
273.493692	8925.223070	28.010266
273.720818	8940.490613	28.015284
273.839950	8958.597653	28.020301
273.988838	8964.917246	28.025319
274.290464	8972.857835	28.030336
274.528780	8985.222162	28.035354
274.760958	8994.667013	28.040372
275.217843	9011.815068	28.045389
275.783348	9011.180312	28.050407
275.732071	9024.060460	28.055424
276.463689	9034.039599	28.060442
276.561014	9040.338880	28.065460
276.310994	9044.520388	28.070477
276.801991	9057.012515	28.075495
276.913684	9073.523264	28.080512
277.332054	9080.182710	28.085530
277.317315	9090.395615	28.090548
277.440656	9112.076159	28.095565
278.065734	9121.781567	28.100583
277.908186	9144.323881	28.105600
278.527122	9150.266807	28.110618
278.774827	9169.973590	28.115636
278.845306	9183.096828	28.120653
279.655129	9196.770442	28.125671
279.816742	9215.101559	28.130688
280.377634	9227.999614	28.135706
280.052176	9228.530536	28.140724
280.541394	9250.592789	28.145741
280.842827	9252.518905	28.150759
280.723401	9263.657602	28.155776
281.436132	9270.788800	28.160794
281.701934	9280.203271	28.165812
281.851608	9292.666937	28.170829
281.850567	9297.740899	28.175847
282.288827	9318.147324	28.180864
282.793566	9326.299359	28.185882
282.881447	9343.145593	28.190900
283.125976	9357.444621	28.195917
283.347201	9367.630186	28.200935
283.368745	9386.602245	28.205952
283.806104	9398.544163	28.210970
284.358097	9411.071177	28.215988
284.099392	9438.596143	28.221005
284.956382	9445.512215	28.226023
285.168834	9460.621462	28.231040
285.418837	9474.679766	28.236058
285.602948	9489.758746	28.241076
285.467427	9507.827279	28.246093
286.375697	9519.420820	28.251111
286.372835	9544.402103	28.256128
286.349716	9557.676032	28.261146
287.057915	9563.854540	28.266164
287.308516	9589.134013	28.271181
288.024954	9597.461391	28.276199
288.282207	9622.067353	28.281216
288.579000	9625.165611	28.286234
289.113355	9640.038295	28.291252
289.160392	9652.755081	28.296269
289.822295	9651.811573	28.301287
289.913994	9667.021995	28.306304
290.171535	9665.159892	28.311322
290.900612	9677.551998	28.316340
290.715402	9684.770344	28.321357
291.252323	9691.313562	28.326375
291.725938	9704.187733	28.331392
291.825513	9710.711062	28.336410
291.879319	9712.676018	28.341428
292.126012	9722.027402	28.346445
292.421173	9729.044222	28.351463
292.707487	9752.256564	28.356480
293.024111	9751.234529	28.361498
293.289699	9765.176946	28.366516
293.190030	9780.878415	28.371533
293.892491	9797.726668	28.376551
294.504895	9808.488988	28.381568
294.190402	9821.502483	28.386586
294.332699	9821.773862	28.391604
294.570785	9859.476800	28.396621
294.884255	9867.122281	28.401639
295.132813	9897.795312	28.406656
295.546990	9905.001943	28.411674
296.021535	9920.960893	28.416692
296.143297	9949.892045	28.421709
296.341288	9962.487517	28.426727
296.764257	9981.438345	28.431744
297.143472	9993.083487	28.436762
297.363784	10013.689002	28.441780
297.715433	10039.161647	28.446797
298.226182	10041.582346	28.451815
298.641345	10053.038764	28.456832
298.757758	10066.985831	28.461850
299.067120	10083.078149	28.466868
299.210334	10096.717927	28.471885
299.797070	10105.558411	28.476903
300.043502	10109.675017	28.481920
300.087994	10127.918027	28.486938
300.500616	10138.042459	28.491956
300.615166	10154.648443	28.496973
301.021688	10160.495517	28.501991
301.387259	10182.107789	28.507008
301.561377	10189.165845	28.512026
301.695468	10203.078671	28.517044
302.161586	10222.439768	28.522061
302.511488	10236.012540	28.527079
302.971885	10245.201256	28.532096
303.181869	10259.724253	28.537114
303.206630	10263.278859	28.542132
303.688940	10298.636328	28.547149
303.792674	10294.284919	28.552167
304.306029	10317.853926	28.557184
304.535366	10329.633267	28.562202
304.973774	10337.862447	28.567220
305.413791	10365.563498	28.572237
305.624876	10372.751605	28.577255
306.005290	10396.376268	28.582272
305.987988	10406.789216	28.587290
306.571913	10420.650683	28.592308
306.732715	10445.361251	28.597325
306.946733	10445.615090	28.602343
307.863916	10456.926811	28.607360
307.953750	10477.812192	28.612378
308.499873	10479.318052	28.617396
308.467635	10495.202165	28.622413
308.916502	10500.297545	28.627431
308.906455	10512.038721	28.632448
309.472439	10520.276415	28.637466
309.824855	10536.769698	28.642484
309.928647	10552.856733	28.647501
310.566205	10559.008754	28.652519
310.469828	10576.027053	28.657536
310.699534	10594.573044	28.662554
311.847819	10607.983134	28.667572
311.865183	10628.046451	28.672589
312.076264	10633.760100	28.677607
312.220728	10651.555381	28.682624
312.662975	10658.135876	28.687642
313.205251	10668.221343	28.692660
313.049957	10691.551394	28.697677
313.623097	10707.763965	28.702695
314.064045	10711.168209	28.707712
314.021602	10724.985933	28.712730
314.717610	10740.554095	28.717748
315.179068	10755.173860	28.722765
315.051840	10761.755187	28.727783
315.303444	10779.969547	28.732800
315.670016	10789.147971	28.737818
316.307148	10803.468706	28.742836
316.162688	10814.331226	28.747853
316.469826	10832.786385	28.752871
317.002910	10849.289534	28.757888
316.753874	10865.953104	28.762906
317.598752	10877.911078	28.767924
318.096485	10899.194038	28.772941
318.335186	10907.688414	28.777959
318.863854	10917.195156	28.782976
318.996701	10929.125766	28.787994
319.236417	10943.941450	28.793012
319.389583	10971.315740	28.798029
319.500189	10976.142166	28.803047
320.132120	10979.484968	28.808064
320.360012	11002.111235	28.813082
320.890767	11022.009300	28.818100
321.171076	11028.852113	28.823117
321.287610	11053.289393	28.828135
321.898287	11055.056744	28.833152
322.299175	11075.259392	28.838170
322.981313	11077.315522	28.843188
322.702070	11077.103532	28.848205
323.115967	11093.767660	28.853223
323.465689	11099.216599	28.858240
322.845394	11130.795052	28.863258
323.415581	11141.413196	28.868276
323.620811	11164.848398	28.873293
324.065263	11179.486948	28.878311
324.674479	11187.190847	28.883328
324.704148	11216.896211	28.888346
325.033164	11233.153796	28.893364
325.387678	11250.859907	28.898381
325.829178	11265.631606	28.903399
326.203555	11293.278004	28.908416
326.301004	11311.368621	28.913434
326.795354	11340.104624	28.918452
327.125192	11346.804017	28.923469
327.687385	11369.583608	28.928487
328.208110	11380.257001	28.933504
328.409361	11397.532558	28.938522
328.622338	11413.189577	28.943540
329.078359	11436.825816	28.948557
329.275916	11454.212521	28.953575
329.976485	11470.832079	28.958592
329.874358	11479.209590	28.963610
330.190367	11493.884294	28.968628
330.666912	11515.439675	28.973645
330.758887	11542.341260	28.978663
331.294413	11553.186106	28.983680
331.314735	11570.120715	28.988698
331.846566	11590.713905	28.993716
332.467644	11610.705809	28.998733
332.836373	11634.475963	29.003751
333.186332	11636.704184	29.008768
333.113917	11659.081462	29.013786
333.382109	11673.283828	29.018804
333.982088	11693.740149	29.023821
334.186871	11714.024727	29.028839
334.910990	11718.262642	29.033856
335.412888	11751.216779	29.038874
335.830796	11762.484357	29.043892
336.324950	11777.320840	29.048909
335.936613	11793.814430	29.053927
336.462593	11791.455362	29.058944
337.151604	11826.748606	29.063962
337.358754	11841.450108	29.068980
337.885944	11848.453486	29.073997
337.942306	11864.170149	29.079015
338.281694	11877.070008	29.084032
338.408199	11894.433515	29.089050
338.835415	11911.503631	29.094068
339.200896	11933.016893	29.099085
338.925943	11937.878701	29.104103
339.852955	11963.664873	29.109120
339.899133	11992.686804	29.114138
340.283869	12001.386160	29.119156
340.558572	12032.983813	29.124173
341.086574	12053.151815	29.129191
341.459637	12065.077097	29.134208
342.005568	12085.570732	29.139226
342.544724	12096.926882	29.144244
343.177026	12113.380871	29.149261
342.914272	12119.308139	29.154279
343.543913	12135.093117	29.159296
344.219133	12153.706648	29.164314
344.380777	12177.443614	29.169332
344.679821	12174.715852	29.174349
344.744285	12189.648389	29.179367
345.197190	12197.329826	29.184384
344.986549	12217.200038	29.189402
345.570179	12214.980304	29.194420
345.722776	12230.480101	29.199437
345.667407	12248.301882	29.204455
346.347777	12269.690418	29.209472
346.611136	12297.876721	29.214490
346.852956	12314.123639	29.219508
347.525534	12327.982112	29.224525
347.491211	12347.812210	29.229543
348.135918	12363.253978	29.234560
348.452183	12392.464738	29.239578
349.131384	12412.142085	29.244596
349.505890	12421.427434	29.249613
349.495408	12447.740060	29.254631
350.199948	12460.851537	29.259648
350.122259	12482.845364	29.264666
350.134057	12498.209544	29.269684
350.768346	12520.376094	29.274701
350.989120	12538.262260	29.279719
351.435092	12559.839419	29.284736
351.922313	12591.193144	29.289754
352.314205	12615.387218	29.294772
352.755051	12635.875809	29.299789
352.899706	12663.847571	29.304807
353.683654	12670.387887	29.309824
353.952538	12700.392852	29.314842
354.166997	12712.930752	29.319860
354.530892	12719.480041	29.324877
354.846544	12743.515698	29.329895
355.457806	12771.518739	29.334912
356.104163	12787.355332	29.339930
356.435027	12804.308721	29.344948
356.813111	12809.036879	29.349965
357.191812	12830.729096	29.354983
357.729233	12852.920685	29.360000
357.903621	12862.755493	29.365018
358.184313	12879.003125	29.370036
358.752714	12890.623596	29.375053
358.853048	12901.910025	29.380071
359.352484	12919.579218	29.385088
359.691469	12932.505128	29.390106
360.134210	12932.325284	29.395124
360.550462	12949.584376	29.400141
360.796081	12955.271219	29.405159
361.465228	12966.455956	29.410176
361.869294	12983.685409	29.415194
362.369394	12994.261902	29.420212
362.576789	13000.393696	29.425229
362.998397	13024.507851	29.430247
363.309047	13033.955086	29.435264
363.504893	13038.137107	29.440282
363.902623	13047.706498	29.445300
364.014161	13058.643894	29.450317
364.184095	13072.685864	29.455335
364.732319	13085.086467	29.460352
365.170053	13092.802228	29.465370
365.197803	13122.940374	29.470388
365.802101	13137.318569	29.475405
366.045401	13159.003951	29.480423
366.502384	13174.261051	29.485440
366.938204	13194.378399	29.490458
366.822537	13211.812632	29.495476
367.649218	13231.278259	29.500493
367.464485	13256.239279	29.505511
367.821124	13270.713212	29.510528
368.448549	13279.106719	29.515546
368.661223	13310.665701	29.520564
368.992469	13317.479267	29.525581
369.142438	13335.276223	29.530599
369.808004	13352.183993	29.535616
370.112909	13372.072557	29.540634
370.469852	13390.446635	29.545652
371.006740	13409.282032	29.550669
371.585419	13425.688726	29.555687
371.375600	13444.502170	29.560704
371.980153	13463.762824	29.565722
371.817506	13483.724742	29.570740
372.800479	13496.193311	29.575757
373.269426	13526.951434	29.580775
373.138519	13535.034352	29.585792
373.888695	13558.327169	29.590810
374.094993	13593.014046	29.595828
374.250248	13602.391166	29.600845
374.533168	13628.365779	29.605863
375.211718	13641.826377	29.610880
375.659067	13669.543782	29.615898
376.222333	13687.898463	29.620916
376.554108	13705.885193	29.625933
376.869801	13729.486288	29.630951
377.201422	13750.994295	29.635968
377.654150	13772.461251	29.640986
377.949074	13796.277271	29.646004
378.357528	13807.585453	29.651021
378.893924	13836.444999	29.656039
379.242148	13855.373553	29.661056
379.979228	13876.215004	29.666074
380.192798	13894.018313	29.671092
380.628292	13906.926615	29.676109
381.024469	13929.738468	29.681127
381.031918	13954.449236	29.686144
381.478876	13953.428679	29.691162
381.614522	13985.547195	29.696180
382.234970	14008.627189	29.701197
382.491032	14031.385317	29.706215
383.050562	14051.901067	29.711232
383.827375	14071.890142	29.716250
383.855504	14094.854586	29.721268
384.388663	14117.585205	29.726285
384.885256	14128.229204	29.731303
385.353585	14142.512614	29.736320
385.798777	14161.745254	29.741338
385.953997	14184.058277	29.746356
386.409586	14201.129180	29.751373
386.595867	14212.071324	29.756391
387.014221	14238.947728	29.761408
387.985536	14259.471839	29.766426
388.078618	14278.870285	29.771444
388.451103	14277.147641	29.776461
388.407796	14300.802520	29.781479
389.192002	14319.325326	29.786496
389.844403	14345.789403	29.791514
389.650080	14363.764420	29.796532
390.417012	14372.307105	29.801549
390.740905	14393.472813	29.806567
391.329583	14410.346202	29.811584
391.857406	14422.378219	29.816602
392.122332	14435.787322	29.821620
392.372215	14451.014729	29.826637
392.736160	14471.315232	29.831655
392.935700	14484.232463	29.836672
393.480875	14506.108962	29.841690
393.309955	14530.807361	29.846708
393.916503	14539.365769	29.851725
394.426606	14570.577070	29.856743
394.948193	14588.247512	29.861760
395.507943	14600.258851	29.866778
395.170943	14619.412350	29.871796
395.625489	14629.621072	29.876813
396.132689	14648.661318	29.881831
396.412778	14670.942720	29.886848
397.196038	14696.777258	29.891866
397.237693	14713.682911	29.896884
397.704778	14738.224796	29.901901
398.189475	14759.880511	29.906919
398.454375	14790.063106	29.911936
399.111071	14793.652226	29.916954
399.373561	14831.225481	29.921972
399.508196	14847.620848	29.926989
400.155072	14862.078960	29.932007
400.227174	14886.616581	29.937024
400.548026	14918.183393	29.942042
400.983807	14937.250905	29.947060
401.332078	14965.377340	29.952077
402.182202	14993.295721	29.957095
402.570600	15017.196534	29.962112
402.887473	15043.237242	29.967130
403.651308	15066.646629	29.972148
403.884559	15087.116698	29.977165
404.625095	15105.520783	29.982183
404.890570	15123.433967	29.987200
405.472026	15142.418860	29.992218
405.785424	15158.931775	29.997236
406.405252	15176.558951	30.002253
406.795865	15190.049962	30.007271
406.800429	15215.823996	30.012288
407.645585	15226.101346	30.017306
408.026019	15240.254069	30.022324
408.405735	15255.843935	30.027341
408.998663	15269.467545	30.032359
409.106341	15291.606130	30.037376
409.212617	15304.983845	30.042394
409.626236	15331.366679	30.047412
410.192848	15356.083268	30.052429
410.595635	15378.864240	30.057447
410.853216	15400.805764	30.062464
411.088682	15413.436908	30.067482
411.629665	15444.875361	30.072500
412.155957	15468.006617	30.077517
412.465137	15487.195576	30.082535
412.708267	15520.910586	30.087552
413.196682	15534.566547	30.092570
413.708623	15561.565965	30.097588
414.008183	15589.290365	30.102605
414.654219	15602.315284	30.107623
415.059531	15633.772140	30.112640
415.381370	15652.709772	30.117658
415.961103	15686.985071	30.122676
416.480379	15703.826263	30.127693
416.833004	15723.731919	30.132711
417.538997	15747.075402	30.137728
417.874117	15752.951203	30.142746
418.492622	15780.799633	30.147764
418.730268	15793.373835	30.152781
419.467694	15804.836974	30.157799
419.214433	15823.909073	30.162816
419.835018	15843.539162	30.167834
420.223669	15874.503157	30.172852
420.537315	15886.926547	30.177869
421.164967	15910.421470	30.182887
421.359178	15924.632294	30.187904
421.755740	15946.205251	30.192922
422.324769	15963.591599	30.197940
422.142635	15981.114570	30.202957
423.076593	15992.114336	30.207975
423.696899	16018.108844	30.212992
424.213135	16032.935734	30.218010
424.353858	16053.468706	30.223028
424.821818	16064.617308	30.228045
425.436767	16081.421738	30.233063
425.701085	16099.781356	30.238080
426.001330	16113.110302	30.243098
426.452891	16139.289327	30.248116
426.516466	16158.416359	30.253133
427.280476	16178.668648	30.258151
427.536365	16193.116369	30.263168
428.243982	16214.789354	30.268186
428.481890	16233.933373	30.273204
428.710400	16259.879031	30.278221
429.437559	16285.099135	30.283239
429.386688	16297.952586	30.288256
429.973473	16322.923100	30.293274
430.570564	16356.413580	30.298292
430.920586	16389.289013	30.303309
431.572339	16407.272392	30.308327
431.647520	16434.676251	30.313344
431.980537	16460.441569	30.318362
432.812452	16480.077113	30.323380
433.080021	16515.088180	30.328397
433.536343	16532.423212	30.333415
433.834393	16572.227367	30.338432
434.565420	16583.755148	30.343450
434.812145	16606.912619	30.348468
435.235437	16637.626055	30.353485
435.897641	16653.157021	30.358503
436.056929	16689.483516	30.363520
436.546536	16711.371245	30.368538
437.197456	16735.343632	30.373556
437.567950	16769.066151	30.378573
438.323155	16779.816423	30.383591
438.492049	16810.213066	30.388608
438.640974	16830.214946	30.393626
439.139684	16853.187952	30.398644
439.779028	16892.190734	30.403661
440.532633	16900.802982	30.408679
440.639939	16929.506997	30.413696
440.960518	16956.408851	30.418714
441.199930	16980.288070	30.423732
441.999031	17014.654564	30.428749
442.276989	17031.698968	30.433767
442.811919	17059.360195	30.438784
443.245620	17090.069563	30.443802
443.864812	17107.288004	30.448820
444.237160	17139.257863	30.453837
444.696517	17162.572212	30.458855
445.064345	17188.592058	30.463872
445.572759	17218.108609	30.468890
446.007794	17242.304958	30.473908
446.479953	17261.871307	30.478925
446.974299	17286.974422	30.483943
447.413604	17310.778519	30.488960
447.648780	17344.216853	30.493978
448.098975	17362.738079	30.498996
448.639146	17391.731906	30.504013
449.173072	17411.585645	30.509031
449.700725	17442.059753	30.514048
450.205354	17459.037444	30.519066
450.620694	17479.377306	30.524084
451.416154	17505.040002	30.529101
452.195826	17521.589313	30.534119
452.305363	17542.204563	30.539136
452.838275	17548.255250	30.544154
453.452601	17561.987696	30.549172
453.565455	17574.901636	30.554189
454.051348	17585.672433	30.559207
454.743521	17596.234041	30.564224
454.796737	17617.464658	30.569242
455.334815	17633.976098	30.574260
455.392183	17646.260723	30.579277
456.257830	17668.684475	30.584295
456.462557	17681.002897	30.589312
457.118304	17713.238869	30.594330
457.162324	17729.941488	30.599348
457.456528	17762.309978	30.604365
457.803815	17779.123074	30.609383
458.198676	17808.323492	30.614400
458.379024	17834.487286	30.619418
459.201873	17857.278053	30.624436
459.685995	17902.896269	30.629453
460.542073	17923.931979	30.634471
460.700654	17954.647909	30.639488
460.750834	17986.240042	30.644506
461.553127	18011.175833	30.649524
462.302680	18037.490811	30.654541
462.836219	18056.694574	30.659559
463.570635	18088.230242	30.664576
463.759449	18111.398587	30.669594
464.295997	18129.306861	30.674612
464.708272	18164.835241	30.679629
465.435174	18187.849905	30.684647
465.500219	18212.850890	30.689664
466.098397	18243.965923	30.694682
466.974131	18268.593619	30.699700
467.183253	18289.282512	30.704717
467.426174	18317.351379	30.709735
468.418675	18339.389623	30.714752
468.684962	18348.792739	30.719770
468.940731	18371.736111	30.724788
469.817024	18409.194938	30.729805
470.434347	18423.900442	30.734823
470.943745	18437.662583	30.739840
471.138077	18467.375541	30.744858
471.677081	18480.627665	30.749876
472.570475	18507.047106	30.754893
472.514033	18516.456630	30.759911
472.827475	18544.672722	30.764928
473.086399	18577.812535	30.769946
473.527394	18587.005191	30.774964
473.958485	18626.720083	30.779981
474.302965	18654.565047	30.784999
474.773537	18683.230556	30.790016
475.385234	18713.718774	30.795034
475.935508	18743.231096	30.800052
476.361670	18773.748467	30.805069
476.493879	18805.821866	30.810087
477.380984	18823.656923	30.815104
477.625703	18860.583770	30.820122
478.163410	18889.106394	30.825140
479.004888	18915.945179	30.830157
479.086787	18948.165683	30.835175
479.736129	18968.306197	30.840192
480.410343	18999.549524	30.845210
480.946251	19029.544684	30.850228
481.329235	19058.173921	30.855245
481.730313	19077.184637	30.860263
482.216706	19107.238214	30.865280
482.947881	19137.480941	30.870298
483.302551	19167.902724	30.875316
483.405953	19186.903310	30.880333
484.049817	19207.101791	30.885351
484.884863	19225.217040	30.890368
484.954440	19257.452620	30.895386
485.443493	19274.491206	30.900404
486.209880	19301.178020	30.905421
486.512551	19322.491467	30.910439
486.825796	19336.367101	30.915456
487.479167	19372.068417	30.920474
488.031532	19398.757296	30.925492
488.453968	19422.427635	30.930509
489.161117	19444.638190	30.935527
489.570397	19463.344737	30.940544
490.113671	19485.517827	30.945562
490.314443	19508.818639	30.950580
490.527653	19536.811785	30.955597
490.986941	19561.133590	30.960615
491.685379	19592.001313	30.965632
492.307872	19625.003828	30.970650
492.760289	19647.222922	30.975668
493.489460	19686.267803	30.980685
493.561154	19714.277049	30.985703
494.092702	19745.139564	30.990720
494.687404	19783.390673	30.995738
494.975636	19798.685799	31.000756
495.942598	19838.881536	31.005773
496.343528	19878.603701	31.010791
497.047289	19887.509414	31.015808
497.143410	19925.800984	31.020826
497.919882	19939.269636	31.025844
498.263319	19971.646725	31.030861
499.091371	19995.734407	31.035879
499.609046	20026.308905	31.040896
499.864344	20068.063430	31.045914
500.769383	20086.459155	31.050932
501.042181	20110.785580	31.055949
501.217963	20147.239158	31.060967
501.664301	20176.732021	31.065984
502.384825	20206.573711	31.071002
502.979059	20224.816065	31.076020
503.296835	20253.469905	31.081037
503.954602	20294.207826	31.086055
504.464420	20315.666822	31.091072
505.013902	20351.007105	31.096090
505.498354	20374.567793	31.101108
506.203165	20404.153198	31.106125
506.618801	20431.863188	31.111143
507.117152	20456.773906	31.116160
507.165126	20484.453100	31.121178
508.082617	20516.583222	31.126196
508.877128	20541.416070	31.131213
509.264714	20576.813708	31.136231
509.680799	20589.713744	31.141248
509.837940	20628.540502	31.146266
510.658610	20664.281158	31.151284
511.374151	20687.445883	31.156301
511.650193	20725.458099	31.161319
512.373456	20749.683172	31.166336
512.648451	20779.936709	31.171354
513.245611	20802.463000	31.176372
513.833108	20835.536222	31.181389
514.211440	20858.393816	31.186407
514.579275	20878.889997	31.191424
514.840009	20919.672447	31.196442
515.782273	20943.471717	31.201460
516.154017	20978.442907	31.206477
516.392741	21006.465747	31.211495
517.234724	21032.422785	31.216512
517.784889	21059.828261	31.221530
518.201559	21085.523422	31.226548
518.739326	21115.875326	31.231565
518.883879	21140.254706	31.236583
519.505023	21164.995447	31.241600
520.085243	21195.732571	31.246618
520.660180	21223.538780	31.251636
521.192447	21254.618389	31.256653
521.717767	21288.454016	31.261671
522.877358	21300.233424	31.266688
522.576275	21333.901590	31.271706
523.061013	21358.695532	31.276724
523.558472	21385.263030	31.281741
523.806218	21426.547730	31.286759
524.603698	21443.862149	31.291776
525.396661	21482.003377	31.296794
525.823588	21511.861445	31.301812
526.589785	21541.186207	31.306829
526.634124	21573.789702	31.311847
527.890521	21604.377331	31.316864
528.716711	21631.380210	31.321882
528.838919	21644.105815	31.326900
529.509479	21670.368566	31.331917
529.594159	21707.793419	31.336935
530.840683	21730.522368	31.341952
531.121765	21761.300909	31.346970
531.264812	21782.926371	31.351988
532.043865	21817.013826	31.357005
532.420154	21844.460265	31.362023
533.238776	21876.993541	31.367040
533.710143	21902.011417	31.372058
534.258468	21927.409033	31.377076
534.645227	21952.996274	31.382093
535.201315	21990.733274	31.387111
535.786953	22026.589043	31.392128
536.455079	22049.838627	31.397146
536.768038	22074.742519	31.402164
537.536404	22103.461175	31.407181
537.658768	22139.674053	31.412199
538.627771	22168.727871	31.417216
539.404606	22200.453098	31.422234
539.612647	22231.186941	31.427252
540.313395	22256.510557	31.432269
540.319510	22282.208391	31.437287
541.318315	22307.403246	31.442304
541.409895	22351.399851	31.447322
542.268694	22373.520470	31.452340
543.037828	22410.820497	31.457357
543.133427	22445.926001	31.462375
543.744098	22463.055734	31.467392
544.322338	22503.046093	31.472410
544.546305	22535.370281	31.477428
545.545591	22566.290346	31.482445
545.701299	22609.335957	31.487463
546.393851	22636.525437	31.492480
546.976868	22671.694018	31.497498
547.590161	22701.177151	31.502516
548.448101	22732.574581	31.507533
548.821754	22763.858339	31.512551
549.728804	22789.200879	31.517568
550.266015	22819.346962	31.522586
550.753427	22846.865854	31.527604
551.593762	22872.351649	31.532621
551.390097	22894.980482	31.537639
552.290182	22924.204183	31.542656
552.793614	22954.842329	31.547674
553.061989	22995.242399	31.552692
553.771960	23014.650884	31.557709
554.269024	23044.102178	31.562727
554.793528	23070.326475	31.567744
555.414187	23092.630536	31.572762
556.010434	23121.327075	31.577780
556.621676	23135.683208	31.582797
556.772238	23172.752955	31.587815
557.667734	23186.129373	31.592832
557.942401	23219.748477	31.597850
558.524569	23251.328942	31.602868
559.268129	23268.969371	31.607885
559.645144	23303.431993	31.612903
560.241867	23332.703808	31.617920
561.063793	23375.160158	31.622938
561.414360	23404.445354	31.627956
562.210727	23429.016148	31.632973
562.309490	23460.173436	31.637991
563.098568	23481.326735	31.643008
563.690152	23512.324770	31.648026
564.031390	23549.346396	31.653044
564.986946	23571.914508	31.658061
565.211866	23610.957672	31.663079
565.827959	23639.032562	31.668096
566.849237	23676.775745	31.673114
567.250365	23717.914804	31.678132
567.814115	23741.593479	31.683149
568.174068	23763.705310	31.688167
568.757759	23789.731707	31.693184
569.444870	23831.401271	31.698202
569.880886	23865.147857	31.703220
570.512976	23898.339285	31.708237
571.093148	23935.918228	31.713255
571.727068	23963.744328	31.718272
572.564700	23992.037794	31.723290
572.775728	24032.733320	31.728308
573.519880	24065.806366	31.733325
573.851438	24096.719647	31.738343
574.105536	24133.585379	31.743360
575.228583	24175.794053	31.748378
575.666854	24200.339731	31.753396
576.519429	24236.934978	31.758413
576.761920	24277.303782	31.763431
577.025179	24305.074658	31.768448
577.885155	24341.668938	31.773466
578.617520	24380.779480	31.778484
579.368967	24413.883558	31.783501
580.014958	24445.917246	31.788519
580.869797	24476.951385	31.793536
581.582200	24503.280852	31.798554
581.889911	24536.473588	31.803572
582.519231	24555.567594	31.808589
583.013433	24592.181701	31.813607
583.681706	24621.046069	31.818624
584.203902	24649.478345	31.823642
584.642017	24674.808261	31.828660
585.393228	24709.290540	31.833677
585.873980	24739.593723	31.838695
586.415287	24772.901937	31.843712
586.962350	24804.989611	31.848730
587.495663	24838.002162	31.853748
588.279169	24868.150689	31.858765
588.875082	24903.940519	31.863783
589.573825	24931.498708	31.868800
590.135116	24952.512295	31.873818
590.726084	24986.413457	31.878836
591.642075	25009.494975	31.883853
592.243480	25038.180826	31.888871
592.667028	25075.103908	31.893888
593.276833	25089.783987	31.898906
593.277771	25115.770664	31.903924
593.976125	25144.353007	31.908941
594.962597	25161.337736	31.913959
595.177839	25185.515088	31.918976
596.103862	25215.155196	31.923994
596.570829	25243.717041	31.929012
596.893315	25256.628460	31.934029
597.376507	25293.687959	31.939047
597.486149	25322.849381	31.944064
598.149505	25353.289208	31.949082
598.639537	25397.685144	31.954100
599.553606	25435.189329	31.959117
600.419129	25471.614171	31.964135
600.852778	25509.383331	31.969152
601.753298	25541.423148	31.974170
602.187611	25577.011971	31.979188
602.892834	25598.781041	31.984205
603.562417	25634.598556	31.989223
604.126111	25661.180353	31.994240
605.189784	25695.368917	31.999258
605.098414	25734.686948	32.004276
606.030418	25770.684804	32.009293
606.602730	25793.549294	32.014311
606.763684	25830.717128	32.019328
607.448845	25865.205419	32.024346
607.769187	25902.594902	32.029364
608.698822	25942.714075	32.034381
609.206986	25980.485088	32.039399
609.950009	26025.108226	32.044416
610.778582	26056.635569	32.049434
611.226094	26098.669692	32.054452
611.899928	26129.260735	32.059469
612.551212	26167.224565	32.064487
612.935183	26217.794675	32.069504
613.725108	26243.463317	32.074522
614.460271	26286.906405	32.079540
615.423200	26319.032489	32.084557
615.736819	26355.102957	32.089575
616.190740	26399.133864	32.094592
616.899287	26433.012730	32.099610
617.149373	26470.521710	32.104628
618.231626	26506.073899	32.109645
619.075594	26537.542702	32.114663
619.192782	26577.796697	32.119680
620.166016	26612.727807	32.124698
620.518666	26642.788469	32.129716
620.997140	26689.622344	32.134733
621.838834	26718.374082	32.139751
622.536274	26758.430118	32.144768
622.903732	26796.186770	32.149786
623.765868	26849.464493	32.154804
624.640588	26888.728267	32.159821
625.221605	26925.598474	32.164839
625.472181	26961.509246	32.169856
626.438303	26984.572544	32.174874
627.362227	27039.301087	32.179892
627.812526	27066.193229	32.184909
628.295012	27086.816885	32.189927
628.840885	27134.823141	32.194944
629.644155	27165.452365	32.199962
629.942800	27213.295273	32.204980
630.801667	27237.582855	32.209997
631.405077	27284.164681	32.215015
632.062735	27319.380291	32.220032
632.523734	27352.768548	32.225050
633.177205	27398.938289	32.230068
633.657183	27429.751273	32.235085
634.219413	27471.018141	32.240103
635.015517	27506.591622	32.245120
635.513631	27538.021338	32.250138
636.371037	27565.924872	32.255156
637.081425	27605.708772	32.260173
637.500631	27634.155066	32.265191
637.929404	27669.843245	32.270208
638.869175	27697.064083	32.275226
639.081962	27738.904506	32.280244
640.076858	27771.672590	32.285261
640.543598	27815.059863	32.290279
641.089248	27857.581589	32.295296
641.811161	27873.276401	32.300314
642.627785	27922.980284	32.305332
643.481504	27960.681908	32.310349
643.770967	27996.272384	32.315367
644.604667	28033.067105	32.320384
645.303635	28062.089608	32.325402
645.659071	28106.613691	32.330420
646.516699	28138.025956	32.335437
647.415494	28174.166027	32.340455
647.666562	28219.231318	32.345472
648.248030	28260.705358	32.350490
649.097866	28304.077920	32.355508
649.128702	28341.251762	32.360525
650.247598	28381.719052	32.365543
650.559184	28429.265710	32.370560
651.542601	28467.099659	32.375578
652.151806	28520.667883	32.380596
652.669346	28557.721650	32.385613
653.676161	28601.101864	32.390631
654.499788	28643.550090	32.395648
654.767179	28678.076987	32.400666
655.804973	28716.560253	32.405684
656.678584	28751.479042	32.410701
657.411676	28793.183252	32.415719
657.827311	28843.445204	32.420736
658.635205	28878.368182	32.425754
659.132454	28912.726738	32.430772
659.855333	28952.574519	32.435789
660.665369	28994.810691	32.440807
661.512354	29046.573186	32.445824
662.351227	29058.382163	32.450842
662.559768	29103.411814	32.455860
663.420408	29135.172797	32.460877
663.962140	29169.796621	32.465895
664.389149	29208.490244	32.470912
665.571493	29233.538645	32.475930
666.261431	29277.772691	32.480948
666.733081	29312.116963	32.485965
667.954854	29347.974653	32.490983
668.643811	29380.249625	32.496000
669.297041	29403.352032	32.501018
670.121419	29431.781625	32.506036
670.537462	29458.340949	32.511053
671.561955	29498.079347	32.516071
671.824194	29526.660316	32.521088
672.780087	29549.424718	32.526106
673.120573	29570.344934	32.531124
673.782315	29599.185818	32.536141
674.641561	29624.399079	32.541159
675.829549	29662.304343	32.546176
675.742439	29695.194398	32.551194
676.716578	29719.890411	32.556212
677.486655	29751.047058	32.561229
677.771366	29775.661470	32.566247
678.608655	29804.721679	32.571264
679.398943	29839.434133	32.576282
679.746502	29869.822728	32.581300
680.122349	29898.753054	32.586317
680.919211	29921.188787	32.591335
681.597650	29954.863305	32.596352
682.159511	29987.721728	32.601370
682.659367	30015.703573	32.606388
682.838863	30046.169318	32.611405
683.708338	30076.312130	32.616423
684.145451	30115.050127	32.621440
684.879723	30155.467378	32.626458
685.714093	30200.079034	32.631476
685.717145	30246.085243	32.636493
686.801952	30291.037157	32.641511
687.432717	30334.315577	32.646528
688.002635	30376.832408	32.651546
689.184599	30426.523081	32.656564
689.477849	30474.418698	32.661581
690.298524	30515.790300	32.666599
690.764949	30566.282399	32.671616
691.680391	30612.873505	32.676634
692.496915	30654.846574	32.681652
692.901892	30704.065376	32.686669
693.908257	30744.485420	32.691687
694.259912	30801.911781	32.696704
695.529961	30845.590558	32.701722
696.082974	30888.079481	32.706740
696.979542	30942.658386	32.711757
697.763943	30978.789709	32.716775
698.139794	31022.798542	32.721792
698.940251	31062.644584	32.726810
700.022651	31092.616464	32.731828
700.370460	31149.178330	32.736845
701.452173	31186.761680	32.741863
702.028573	31236.346842	32.746880
702.821350	31285.582155	32.751898
703.651630	31313.653090	32.756916
703.912070	31362.225993	32.761933
705.055791	31399.591404	32.766951
705.731223	31450.394299	32.771968
706.103130	31486.237089	32.776986
707.505535	31521.463400	32.782004
708.161310	31569.557644	32.787021
709.021390	31602.422508	32.792039
709.605392	31638.782340	32.797056
710.289617	31679.324199	32.802074
711.055186	31715.908604	32.807092
711.221037	31761.494404	32.812109
712.130116	31796.558211	32.817127
712.941876	31836.012018	32.822144
713.517416	31887.602888	32.827162
714.338812	31924.741562	32.832180
715.001456	31963.864940	32.837197
715.641402	32008.491976	32.842215
716.245758	32049.230399	32.847232
717.123408	32097.221578	32.852250
718.204159	32127.909592	32.857268
718.447082	32179.812472	32.862285
719.416113	32218.167648	32.867303
720.569697	32254.654307	32.872320
720.744226	32294.486940	32.877338
722.075065	32329.985035	32.882356
722.463721	32365.858328	32.887373
723.281856	32415.604428	32.892391
724.119038	32450.642666	32.897408
724.861998	32490.083200	32.902426
725.477730	32516.710010	32.907444
726.193703	32568.735761	32.912461
727.261925	32582.540235	32.917479
727.633377	32620.237409	32.922496
728.047391	32646.390209	32.927514
728.892959	32679.929189	32.932532
729.639956	32717.770036	32.937549
730.490037	32729.212697	32.942567
731.649386	32762.456112	32.947584
732.101974	32797.928165	32.952602
732.879289	32815.059529	32.957620
733.597927	32863.956150	32.962637
734.413826	32884.160407	32.967655
734.668493	32906.829699	32.972672
734.998743	32956.811546	32.977690
736.183508	32980.251980	32.982708
736.368640	33035.807605	32.987725
737.231329	33056.200690	32.992743
737.783309	33108.512677	32.997760
738.386442	33157.415427	33.002778
739.205050	33199.488145	33.007796
739.936004	33248.472247	33.012813
740.703939	33287.429885	33.017831
741.476692	33335.851287	33.022848
741.819344	33389.372698	33.027866
742.909947	33430.669900	33.032884
743.287818	33489.060547	33.037901
743.980624	33538.215681	33.042919
745.103789	33587.784035	33.047936
745.766146	33642.501528	33.052954
746.509366	33682.879983	33.057972
747.665527	33745.436038	33.062989
748.295278	33790.726007	33.068007
749.184012	33841.090360	33.073024
749.756837	33891.257730	33.078042
750.851007	33932.808262	33.083060
751.530425	33981.119319	33.088077
752.132257	34024.346715	33.093095
753.071794	34067.110355	33.098112
753.459267	34119.425330	33.103130
754.462003	34160.668183	33.108148
755.139757	34207.399389	33.113165
755.886994	34263.205327	33.118183
756.663983	34298.989504	33.123200
757.391471	34353.540583	33.128218
758.296863	34404.573871	33.133236
759.485647	34452.660826	33.138253
760.275673	34494.582550	33.143271
761.129171	34543.872936	33.148288
761.830840	34576.723030	33.153306
762.731564	34630.267687	33.158324
763.070904	34668.612156	33.163341
763.892035	34710.573697	33.168359
764.793875	34749.462496	33.173376
765.362413	34794.998149	33.178394
766.142274	34837.130796	33.183412
767.237588	34889.027020	33.188429
767.598426	34935.455394	33.193447
768.736284	34970.077718	33.198464
769.108231	35027.765402	33.203482
770.111595	35062.339389	33.208500
770.466373	35108.882902	33.213517
771.426923	35154.003864	33.218535
772.782565	35202.825140	33.223552
773.330660	35252.392626	33.228570
773.598521	35295.124835	33.233588
774.225895	35335.044059	33.238605
774.785652	35390.047713	33.243623
776.403578	35439.606179	33.248640
776.926940	35488.450956	33.253658
777.725351	35538.637496	33.258676
778.640742	35576.735330	33.263693
779.574212	35609.582346	33.268711
780.391643	35644.926188	33.273728
780.862888	35682.157962	33.278746
781.785868	35716.695023	33.283764
782.375871	35753.307642	33.288781
783.179895	35795.748241	33.293799
784.025055	35833.598290	33.298816
784.486578	35876.560587	33.303834
785.395132	35913.806488	33.308852
786.065058	35955.819469	33.313869
786.933587	36004.465952	33.318887
787.607626	36049.848673	33.323904
788.253262	36096.683928	33.328922
789.314465	36134.658762	33.333940
789.943717	36178.651364	33.338957
790.606822	36232.622993	33.343975
791.277181	36269.514782	33.348992
792.297212	36328.065632	33.354010
793.119654	36371.092550	33.359028
794.277796	36416.096733	33.364045
794.460149	36472.831610	33.369063
795.432050	36505.364160	33.374080
796.147979	36569.173627	33.379098
797.010493	36611.486553	33.384116
798.263624	36667.845606	33.389133
799.050717	36716.386326	33.394151
799.667951	36757.871662	33.399168
800.757403	36813.295590	33.404186
801.290114	36859.030977	33.409204
802.338108	36910.262961	33.414221
802.960479	36958.665619	33.419239
803.888664	37001.032268	33.424256
804.791004	37062.050706	33.429274
805.543604	37102.807295	33.434292
806.300611	37134.324772	33.439309
806.995116	37188.704923	33.444327
808.092460	37225.854000	33.449344
808.618500	37289.265359	33.454362
809.445383	37329.131788	33.459380
810.381806	37377.834007	33.464397
811.244023	37425.593110	33.469415
812.457786	37476.749906	33.474432
812.975245	37518.720281	33.479450
814.356343	37560.144472	33.484468
815.039176	37598.010428	33.489485
816.486392	37645.008121	33.494503
816.946483	37672.968458	33.499520
817.259804	37709.039668	33.504538
818.660252	37751.744887	33.509556
819.720031	37793.763675	33.514573
820.226715	37834.572813	33.519591
821.355086	37865.192176	33.524608
821.490079	37908.108511	33.529626
822.219335	37950.615693	33.534644
823.685464	37988.226888	33.539661
824.050312	38030.721731	33.544679
824.802267	38075.065794	33.549696
825.338106	38118.545825	33.554714
825.999127	38149.036417	33.559732
827.290932	38202.686914	33.564749
828.064419	38243.056656	33.569767
828.893648	38294.281941	33.574784
829.860230	38348.103879	33.579802
830.244719	38374.951339	33.584820
831.171667	38423.492999	33.589837
832.010222	38470.688993	33.594855
832.561350	38506.812836	33.599872
833.511412	38562.376944	33.604890
834.143049	38601.896883	33.609908
835.209840	38635.644642	33.614925
835.660914	38681.301838	33.619943
836.670794	38725.436110	33.624960
836.957913	38772.339679	33.629978
837.920566	38829.382295	33.634996
839.128456	38858.283170	33.640013
839.695563	38920.870798	33.645031
840.618349	38962.375789	33.650048
841.737549	39013.721802	33.655066
841.921231	39057.170333	33.660084
843.008751	39109.217170	33.665101
843.571366	39155.914009	33.670119
844.753736	39212.316127	33.675136
845.814564	39255.532847	33.680154
846.440649	39305.382084	33.685172
846.941698	39344.727785	33.690189
847.707627	39414.969437	33.695207
849.381167	39453.701703	33.700224
850.279419	39515.606789	33.705242
850.930635	39552.570463	33.710260
852.395246	39600.954691	33.715277
853.351241	39652.150701	33.720295
854.480803	39682.494206	33.725312
855.248081	39724.341219	33.730330
856.035635	39762.991428	33.735348
857.177062	39801.832938	33.740365
857.726023	39854.029140	33.745383
858.695838	39886.655686	33.750400
859.441161	39930.372178	33.755418
860.257918	39969.897251	33.760436
861.314373	40018.169246	33.765453
861.936877	40061.114701	33.770471
862.636449	40100.620415	33.775488
863.592620	40149.850723	33.780506
864.396063	40200.154892	33.785524
865.127610	40243.134226	33.790541
866.131425	40287.690041	33.795559
866.815416	40338.209288	33.800576
867.831490	40393.900574	33.805594
868.207124	40430.883597	33.810612
869.574219	40493.812176	33.815629
869.990125	40551.583699	33.820647
870.849488	40602.588375	33.825664
872.343308	40651.678713	33.830682
872.946954	40696.348620	33.835700
873.930998	40741.888751	33.840717
874.393526	40800.033099	33.845735
875.581911	40843.928705	33.850752
876.710525	40891.027633	33.855770
877.502129	40949.664759	33.860788
878.339810	40999.876870	33.865805
879.228472	41055.906025	33.870823
880.035324	41098.236475	33.875840
881.248729	41148.839140	33.880858
881.656471	41202.382520	33.885876
882.811991	41242.969989	33.890893
883.582712	41297.911426	33.895911
884.740260	41333.179739	33.900928
885.654090	41382.299293	33.905946
886.058431	41435.793179	33.910964
887.446122	41483.118454	33.915981
887.768007	41545.239726	33.920999
888.925245	41585.043300	33.926016
890.227757	41638.314822	33.931034
890.596321	41683.516883	33.936052
891.785634	41731.771871	33.941069
892.648502	41778.541163	33.946087
893.613140	41814.574133	33.951104
894.169750	41846.964730	33.956122
894.649261	41890.568651	33.961140
895.801813	41929.519738	33.966157
896.602730	41979.569084	33.971175
897.554613	42026.552661	33.976192
898.631762	42063.479199	33.981210
898.943543	42117.507875	33.986228
899.930280	42163.512260	33.991245
901.051788	42208.363484	33.996263
901.379987	42266.064712	34.001280
902.549222	42306.512859	34.006298
903.236903	42373.107830	34.011316
904.072818	42419.351414	34.016333
905.036849	42477.326808	34.021351
906.064291	42533.451857	34.026368
907.241506	42582.475932	34.031386
907.910618	42643.299912	34.036404
909.131703	42692.639939	34.041421
910.371017	42747.189053	34.046439
911.111664	42801.955535	34.051456
912.490983	42862.523439	34.056474
913.497015	42908.298658	34.061492
913.736377	42948.324327	34.066509
914.766506	42999.168688	34.071527
915.884972	43058.867160	34.076544
916.545272	43100.016318	34.081562
917.963917	43166.182972	34.086580
918.756271	43214.218739	34.091597
919.626479	43262.014712	34.096615
920.720158	43313.368512	34.101632
921.382924	43361.216157	34.106650
921.909233	43423.879980	34.111668
923.275145	43471.478611	34.116685
924.141128	43528.194417	34.121703
924.960321	43579.294525	34.126720
926.428841	43630.868682	34.131738
926.989546	43693.483605	34.136756
928.452625	43740.510974	34.141773
929.445938	43788.699956	34.146791
930.053548	43837.404860	34.151808
931.153705	43887.089085	34.156826
932.011470	43949.575987	34.161844
932.618412	43994.909914	34.166861
933.902851	44048.847938	34.171879
934.826774	44098.870176	34.176896
936.106415	44142.675855	34.181914
936.645927	44203.068979	34.186932
937.497945	44256.056816	34.191949
938.395894	44304.375708	34.196967
938.975346	44347.608273	34.201984
940.472335	44401.298807	34.207002
941.247897	44455.621122	34.212020
942.200799	44512.180345	34.217037
942.806443	44570.483007	34.222055
943.794552	44623.646503	34.227072
944.963440	44679.482846	34.232090
946.040013	44742.576599	34.237108
946.997182	44788.072374	34.242125
948.392422	44837.933919	34.247143
949.272995	44889.324733	34.252160
950.499729	44930.470827	34.257178
950.895152	44977.174585	34.262196
951.906840	45024.926898	34.267213
952.819945	45076.572403	34.272231
954.114669	45127.823012	34.277248
954.896624	45173.764505	34.282266
955.369253	45222.423988	34.287284
956.538192	45264.123762	34.292301
957.512906	45305.132887	34.297319
958.402533	45350.096368	34.302336
959.279960	45402.285903	34.307354
959.797476	45440.229269	34.312372
960.977597	45482.813313	34.317389
962.062849	45536.033356	34.322407
963.018793	45577.697481	34.327424
963.602924	45625.897573	34.332442
964.114399	45676.803965	34.337460
965.179883	45733.513126	34.342477
966.411895	45792.226971	34.347495
966.996783	45853.110867	34.352512
968.028894	45902.285188	34.357530
968.637213	45969.150062	34.362548
969.930914	46021.370750	34.367565
971.087934	46087.517468	34.372583
972.070624	46151.382685	34.377600
973.194153	46209.361813	34.382618
974.148406	46268.265891	34.387636
975.259438	46339.664835	34.392653
976.656810	46382.665724	34.397671
977.270997	46447.304324	34.402688
978.584325	46487.022683	34.407706
979.127546	46546.687716	34.412724
980.027607	46608.789532	34.417741
981.431011	46658.698140	34.422759
982.004959	46731.675388	34.427776
983.434973	46790.253294	34.432794
984.346528	46846.160633	34.437812
985.272373	46904.855733	34.442829
986.404540	46958.173019	34.447847
987.475839	47015.959962	34.452864
988.992398	47062.201506	34.457882
990.313020	47119.709280	34.462900
990.973584	47163.858209	34.467917
992.193545	47221.230172	34.472935
992.706992	47267.490016	34.477952
993.897188	47316.965318	34.482970
995.044254	47374.526220	34.487988
996.051462	47423.973470	34.493005
997.247839	47474.447714	34.498023
997.680868	47528.198454	34.503040
998.914235	47576.029029	34.508058
999.917129	47639.300613	34.513076
1000.496720	47686.930116	34.518093
1002.065695	47746.690769	34.523111
1002.760191	47801.248962	34.528128
1003.859742	47855.560399	34.533146
1004.748577	47910.702096	34.538164
1005.633351	47960.656826	34.543181
1006.913836	48020.045820	34.548199
1007.482237	48078.926458	34.553216
1009.326703	48127.883543	34.558234
1010.434766	48188.445079	34.563252
1011.011512	48238.391709	34.568269
1012.067249	48290.629601	34.573287
1012.619505	48334.139798	34.578304
1014.102719	48395.048051	34.583322
1014.800788	48444.697766	34.588340
1016.096030	48486.295161	34.593357
1017.280433	48539.911671	34.598375
1018.091605	48586.804541	34.603392
1019.015767	48641.461651	34.608410
1020.022291	48695.536593	34.613428
1020.906381	48754.306282	34.618445
1022.204308	48806.083548	34.623463
1022.956750	48858.762487	34.628480
1023.902900	48909.880142	34.633498
1024.968825	48956.063247	34.638516
1026.301166	49007.386381	34.643533
1027.099410	49037.244144	34.648551
1027.758114	49082.358765	34.653568
1028.709115	49124.681866	34.658586
1029.806612	49188.126422	34.663604
1030.763814	49233.966482	34.668621
1031.864126	49285.358203	34.673639
1032.486066	49342.588732	34.678656
1033.475245	49409.151034	34.683674
1034.584591	49461.414850	34.688692
1035.496381	49522.067599	34.693709
1036.865494	49582.497061	34.698727
1037.941623	49639.783760	34.703744
1038.894221	49695.343694	34.708762
1039.992063	49753.487748	34.713780
1040.912484	49823.573505	34.718797
1042.155129	49877.038514	34.723815
1043.230085	49936.300173	34.728832
1044.400140	49996.603716	34.733850
1045.171280	50061.911327	34.738868
1046.093997	50123.588943	34.743885
1047.425218	50172.289117	34.748903
1048.425982	50245.919423	34.753920
1049.560339	50302.907612	34.758938
1050.735825	50366.178709	34.763956
1051.608983	50428.187585	34.768973
1053.473156	50482.404537	34.773991
1054.199200	50540.855554	34.779008
1055.431035	50597.202816	34.784026
1056.416591	50647.185599	34.789044
1057.537988	50699.678127	34.794061
1058.492620	50752.652447	34.799079
1059.199023	50812.176536	34.804096
1060.762302	50869.674757	34.809114
1062.011722	50934.340501	34.814132
1062.880746	50982.804716	34.819149
1064.047336	51042.542080	34.824167
1064.667219	51100.232869	34.829184
1066.213651	51160.999377	34.834202
1067.512008	51217.685746	34.839220
1068.283140	51277.181915	34.844237
1069.550768	51336.904221	34.849255
1069.844196	51408.459683	34.854272
1070.974022	51458.864557	34.859290
1072.431989	51510.996188	34.864308
1073.461708	51581.563716	34.869325
1074.843102	51635.593212	34.874343
1075.721285	51696.370838	34.879360
1076.792811	51752.556189	34.884378
1077.900773	51799.491403	34.889396
1078.903643	51860.635919	34.894413
1080.349963	51911.251657	34.899431
1081.359323	51976.204671	34.904448
1082.199561	52043.304099	34.909466
1083.215757	52103.630904	34.914484
1084.606839	52156.476828	34.919501
1085.780415	52211.103363	34.924519
1087.018941	52268.225623	34.929536
1088.373890	52313.876654	34.934554
1089.336505	52364.088204	34.939572
1090.149878	52430.401990	34.944589
1091.341493	52469.219638	34.949607
1092.285334	52529.071637	34.954624
1093.490540	52586.294810	34.959642
1094.402028	52639.950940	34.964660
1095.460425	52680.049027	34.969677
1096.378016	52735.273716	34.974695
1097.446999	52771.845710	34.979712
1098.026967	52823.187558	34.984730
1099.637406	52872.963406	34.989748
1100.656963	52929.330587	34.994765
1101.480511	52971.092204	34.999783
1102.393855	53024.552764	35.004800
1103.431633	53087.061858	35.009818
1104.738278	53141.429280	35.014836
1105.127070	53205.065417	35.019853
1106.289043	53252.627900	35.024871
1107.990075	53323.816990	35.029888
1108.860133	53385.676045	35.034906
1110.082860	53442.885918	35.039924
1110.739939	53517.618192	35.044941
1112.056797	53582.179491	35.049959
1113.215546	53643.582706	35.054976
1114.090145	53709.732330	35.059994
1115.488826	53768.889811	35.065012
1116.679247	53835.768700	35.070029
1117.975307	53900.739131	35.075047
1119.509050	53961.514939	35.080064
1120.319365	54026.466842	35.085082
1122.044135	54083.099753	35.090100
1122.892684	54145.116051	35.095117
1124.592672	54200.202718	35.100135
1125.854632	54246.637799	35.105152
1126.703557	54304.496818	35.110170
1128.180717	54361.213463	35.115188
1128.964586	54418.513403	35.120205
1130.261400	54471.391977	35.125223
1131.480261	54523.706999	35.130240
1132.463115	54586.323605	35.135258
1133.950636	54638.312047	35.140276
1134.933094	54695.296795	35.145293
1135.867085	54740.455245	35.150311
1137.431457	54803.456014	35.155328
1138.218233	54855.877389	35.160346
1139.714630	54903.099753	35.165364
1140.724799	54961.042720	35.170381
1141.636553	55015.476303	35.175399
1142.697296	55071.177688	35.180416
1143.407339	55133.509374	35.185434
1144.927145	55189.885928	35.190452
1145.920529	55251.787531	35.195469
1147.012975	55312.490356	35.200487
1148.385572	55376.566880	35.205504
1149.491098	55439.514609	35.210522
1151.320657	55481.857298	35.215540
1152.363051	55539.537165	35.220557
1153.240482	55587.053984	35.225575
1154.793563	55651.419425	35.230592
1156.113891	55692.873939	35.235610
1157.392296	55747.675820	35.240628
1158.191291	55794.312998	35.245645
1159.485076	55836.012407	35.250663
1160.731698	55885.630094	35.255680
1161.732222	55942.874490	35.260698
1163.102010	55991.707347	35.265716
1163.927666	56040.967240	35.270733
1165.217644	56098.097079	35.275751
1166.318631	56144.516791	35.280768
1167.185663	56197.048810	35.285786
1168.504701	56248.560870	35.290804
1170.100721	56317.592016	35.295821
1170.806018	56355.650491	35.300839
1172.298423	56404.908017	35.305856
1173.346300	56448.406404	35.310874
1174.737667	56484.345119	35.315892
1175.758460	56531.727464	35.320909
1177.119821	56565.360977	35.325927
1177.936274	56606.914957	35.330944
1178.415506	56658.116356	35.335962
1179.530785	56696.313716	35.340980
1180.665707	56747.267093	35.345997
1181.285281	56809.781884	35.351015
1182.832200	56857.677427	35.356032
1183.808648	56912.560907	35.361050
1185.088629	56968.877967	35.366068
1186.433778	57035.064466	35.371085
1187.727962	57090.101138	35.376103
1188.578207	57141.568266	35.381120
1189.536488	57212.201809	35.386138
1191.046765	57281.477011	35.391156
1191.968187	57338.983970	35.396173
1193.239801	57400.961521	35.401191
1194.524698	57456.171373	35.406208
1195.821932	57540.050203	35.411226
1197.166176	57596.586526	35.416244
1198.373392	57667.441931	35.421261
1199.566988	57731.578123	35.426279
1201.077069	57788.500332	35.431296
1202.059320	57866.796660	35.436314
1203.404292	57918.953836	35.441332
1204.520000	57990.121988	35.446349
1205.440353	58051.187836	35.451367
1206.980437	58112.707465	35.456384
1208.060794	58171.615614	35.461402
1209.294275	58238.246970	35.466420
1210.498990	58303.933620	35.471437
1211.724482	58388.295003	35.476455
1213.448966	58438.090021	35.481472
1214.663247	58510.073418	35.486490
1216.461111	58569.712019	35.491508
1217.224723	58627.392334	35.496525
1218.515726	58693.933662	35.501543
1219.744787	58745.022116	35.506560
1220.950669	58808.937721	35.511578
1222.581138	58862.406743	35.516596
1223.922645	58921.345463	35.521613
1225.090627	58982.830621	35.526631
1226.282573	59032.533009	35.531648
1227.393057	59078.716392	35.536666
1228.530731	59138.491396	35.541684
1229.817425	59203.908147	35.546701
1230.588101	59270.792026	35.551719
1232.076361	59323.233624	35.556736
1233.503797	59388.090827	35.561754
1234.708022	59449.039809	35.566772
1236.047447	59514.892215	35.571789
1237.164796	59571.114226	35.576807
1238.429951	59621.654531	35.581824
1239.660051	59685.973754	35.586842
1240.927116	59738.748372	35.591860
1242.417788	59813.192590	35.596877
1243.385787	59872.242728	35.601895
1244.951213	59927.553568	35.606912
1246.184762	59986.347203	35.611930
1246.990496	60029.706404	35.616948
1248.517500	60090.511518	35.621965
1249.464670	60152.565902	35.626983
1251.225635	60209.214004	35.632000
1252.045906	60273.010262	35.637018
1253.259001	60331.934528	35.642036
1254.414827	60395.286128	35.647053
1255.490637	60447.471898	35.652071
1257.210166	60490.309078	35.657088
1258.227770	60541.067281	35.662106
1259.193881	60582.541374	35.667124
1260.628634	60631.873539	35.672141
1261.511209	60688.584302	35.677159
1263.008565	60735.349590	35.682176
1264.491696	60796.391209	35.687194
1265.270240	60848.681340	35.692212
1266.793930	60906.507598	35.697229
1267.698680	60955.923384	35.702247
1269.215419	61022.954802	35.707264
1270.383159	61075.146510	35.712282
1271.494888	61124.074473	35.717300
1273.029947	61187.223167	35.722317
1274.076054	61254.278250	35.727335
1275.499619	61312.007198	35.732352
1276.699988	61373.442673	35.737370
1278.079269	61436.312548	35.742388
1279.213941	61498.385300	35.747405
1280.302028	61569.315036	35.752423
1281.823483	61618.509013	35.757440
1283.131663	61689.847753	35.762458
1284.905916	61749.352252	35.767476
1286.636444	61808.996673	35.772493
1287.598429	61881.808128	35.777511
1288.816928	61935.531961	35.782528
1289.988859	62002.809935	35.787546
1291.084563	62064.219206	35.792564
1292.582447	62128.882741	35.797581
1294.011482	62190.569322	35.802599
1295.492303	62252.399878	35.807616
1296.811975	62321.162207	35.812634
1297.712480	62381.501345	35.817652
1299.464328	62444.771258	35.822669
1300.450543	62505.394808	35.827687
1301.751159	62566.298471	35.832704
1303.184718	62629.827585	35.837722
1304.524616	62687.503219	35.842740
1306.054924	62752.068353	35.847757
1307.241145	62823.245874	35.852775
1308.685992	62879.341902	35.857792
1310.240467	62952.006783	35.862810
1311.334074	63009.664745	35.867828
1312.754373	63070.164751	35.872845
1314.183426	63131.682752	35.877863
1315.726603	63189.593615	35.882880
1316.561093	63243.146170	35.887898
1318.185984	63312.376246	35.892916
1319.602544	63363.242404	35.897933
1320.674072	63433.319111	35.902951
1322.090484	63487.958594	35.907968
1323.556560	63559.480584	35.912986
1324.865493	63616.536490	35.918004
1326.574335	63672.491695	35.923021
1327.074879	63728.731129	35.928039
1328.929665	63787.620181	35.933056
1330.237808	63843.315628	35.938074
1331.123094	63899.115377	35.943092
1332.593261	63958.717105	35.948109
1333.563836	64018.682063	35.953127
1335.175867	64086.802092	35.958144
1336.757405	64147.076891	35.963162
1338.336973	64220.786129	35.968180
1339.404377	64267.903971	35.973197
1340.689328	64328.808072	35.978215
1342.134024	64390.003858	35.983232
1343.555048	64451.222492	35.988250
1344.225760	64507.209125	35.993268
1345.904886	64557.517488	35.998285
1346.746422	64615.744086	36.003303
1347.898619	64657.771997	36.008320
1349.150368	64712.028426	36.013338
1350.353321	64778.675955	36.018356
1352.114500	64829.389864	36.023373
1353.114336	64891.283276	36.028391
1354.383282	64937.465499	36.033408
1355.698295	65011.180487	36.038426
1356.771780	65082.046549	36.043444
1358.490583	65141.878078	36.048461
1359.518361	65223.273891	36.053479
1361.007758	65284.439538	36.058496
1362.232549	65357.055391	36.063514
1363.792551	65418.659820	36.068532
1365.670637	65480.708438	36.073549
1367.003254	65553.371290	36.078567
1368.281459	65625.549038	36.083584
1369.749270	65684.395496	36.088602
1371.410278	65748.992234	36.093620
1373.039568	65813.777707	36.098637
1374.155577	65872.103532	36.103655
1375.703492	65939.130657	36.108672
1376.969942	65997.053346	36.113690
1378.184475	66072.306666	36.118708
1380.092667	66138.125632	36.123725
1381.513288	66199.842425	36.128743
1382.627381	66266.400162	36.133760
1384.264596	66328.868450	36.138778
1385.743720	66393.735897	36.143796
1387.023678	66462.655109	36.148813
1388.419006	66520.387876	36.153831
1389.646041	66586.276640	36.158848
1391.216800	66650.478266	36.163866
1392.407041	66718.532148	36.168884
1394.144625	66772.419384	36.173901
1395.444285	66849.827041	36.178919
1396.779526	66919.802527	36.183936
1398.484269	66977.025700	36.188954
1399.532642	67045.210298	36.193972
1401.356834	67102.510031	36.198989
1402.495782	67172.966476	36.204007
1403.978007	67240.089632	36.209024
1405.166480	67307.100655	36.214042
1406.381276	67373.138998	36.219060
1407.967142	67441.835694	36.224077
1409.805002	67508.118768	36.229095
1411.401301	67574.515805	36.234112
1412.606838	67639.777494	36.239130
1413.648129	67704.197619	36.244148
1414.949422	67766.114177	36.249165
1416.574541	67836.091124	36.254183
1417.868113	67905.309696	36.259200
1419.465199	67971.555680	36.264218
1420.602011	68048.650546	36.269236
1422.074357	68116.860283	36.274253
1423.733399	68181.108930	36.279271
1425.173453	68250.660088	36.284288
1427.071871	68324.021103	36.289306
1427.906965	68391.533505	36.294324
1429.559387	68450.173843	36.299341
1430.705579	68513.363862	36.304359
1432.158690	68584.889428	36.309376
1434.271782	68649.270799	36.314394
1435.241562	68716.579346	36.319412
1436.826564	68776.706324	36.324429
1438.207172	68846.072107	36.329447
1439.652480	68894.564084	36.334464
1441.256774	68950.623321	36.339482
1442.207936	69000.123645	36.344500
1443.433590	69050.936150	36.349517
1444.762940	69111.819444	36.354535
1445.922063	69178.175083	36.359552
1447.387714	69242.070399	36.364570
1448.314252	69308.152506	36.369588
1449.903038	69375.992760	36.374605
1451.741986	69446.478850	36.379623
1452.815750	69513.545243	36.384640
1454.202002	69577.878069	36.389658
1455.722901	69654.556687	36.394676
1457.186291	69719.245056	36.399693
1458.515275	69796.549358	36.404711
1460.165068	69870.865528	36.409728
1461.726821	69934.829832	36.414746
1463.461700	70007.834971	36.419764
1465.660244	70072.510471	36.424781
1466.927937	70146.336332	36.429799
1468.268940	70205.763950	36.434816
1470.027651	70261.795530	36.439834
1471.476789	70344.002859	36.444852
1473.030055	70406.171272	36.449869
1474.712742	70470.497908	36.454887
1476.124621	70540.730870	36.459904
1477.634163	70596.105611	36.464922
1478.765763	70667.940553	36.469940
1480.552836	70741.078896	36.474957
1481.807202	70801.699267	36.479975
1483.081611	70884.695542	36.484992
1484.783283	70944.385018	36.490010
1486.566001	71009.115271	36.495028
1487.917469	71076.306871	36.500045
1489.366979	71156.312990	36.505063
1490.905754	71227.072534	36.510080
1492.328688	71299.116913	36.515098
1494.100680	71365.622845	36.520116
1495.668173	71438.024934	36.525133
1497.082768	71513.896095	36.530151
1498.420904	71582.484255	36.535168
1500.019311	71651.272498	36.540186
1501.389140	71723.706314	36.545204
1503.109473	71798.073931	36.550221
1504.741054	71857.877786	36.555239
1506.074270	71939.854967	36.560256
1507.984652	72014.535417	36.565274
1509.425325	72073.749037	36.570292
1510.670887	72149.762480	36.575309
1512.378972	72217.344480	36.580327
1513.817751	72282.131712	36.585344
1515.405906	72348.415598	36.590362
1516.680825	72437.293549	36.595380
1518.006531	72505.164118	36.600397
1519.994396	72567.256976	36.605415
1521.318949	72655.570602	36.610432
1523.063488	72713.750171	36.615450
1524.418359	72778.513757	36.620468
1525.715362	72849.619490	36.625485
1527.584444	72925.436248	36.630503
1528.997974	73001.311859	36.635520
1530.687837	73061.286649	36.640538
1532.193900	73136.084223	36.645556
1533.889556	73199.174254	36.650573
1535.650399	73256.415181	36.655591
1536.890057	73340.260593	36.660608
1538.650753	73381.909857	36.665626
1540.123026	73462.375394	36.670644
1541.710432	73521.961946	36.675661
1543.126036	73569.339967	36.680679
1544.093024	73626.946603	36.685696
1545.700362	73677.752689	36.690714
1547.022275	73737.659937	36.695732
1548.146117	73803.412159	36.700749
1549.680789	73860.461796	36.705767
1550.703847	73923.608156	36.710784
1552.630357	73990.159855	36.715802
1554.250873	74074.631958	36.720820
1555.605166	74147.872829	36.725837
1557.083727	74211.708567	36.730855
1558.655399	74287.525099	36.735872
1560.445186	74360.128397	36.740890
1561.982885	74439.319987	36.745908
1563.466577	74513.238271	36.750925
1565.253695	74587.818603	36.755943
1566.370990	74663.428649	36.760960
1568.605390	74741.828090	36.765978
1570.091235	74814.986865	36.770996
1571.847641	74884.759451	36.776013
1573.560004	74961.214547	36.781031
1574.927631	75043.816595	36.786048
1577.037308	75114.623843	36.791066
1578.269049	75183.807976	36.796084
1579.832771	75258.627811	36.801101
1581.828956	75339.789691	36.806119
1583.013441	75415.644680	36.811136
1584.714906	75492.546342	36.816154
1586.760478	75559.057979	36.821172
1588.252259	75641.731101	36.826189
1590.221673	75705.075556	36.831207
1591.522815	75784.282803	36.836224
1593.485957	75852.049456	36.841242
1595.075154	75924.422370	36.846260
1596.414622	75990.817574	36.851277
1598.105253	76055.574559	36.856295
1599.504165	76132.829418	36.861312
1601.249546	76211.816381	36.866330
1603.098133	76275.751125	36.871348
1604.437480	76351.546503	36.876365
1606.040757	76418.344831	36.881383
1607.527828	76499.526545	36.886400
1609.118851	76579.248123	36.891418
1611.194628	76656.955917	36.896436
1612.600094	76724.305333	36.901453
1614.322235	76787.944384	36.906471
1615.564612	76870.368936	36.911488
1617.275547	76953.024431	36.916506
1619.113522	77021.675015	36.921524
1620.479776	77099.900493	36.926541
1622.423283	77176.908409	36.931559
1623.823527	77255.293696	36.936576
1625.517676	77329.427446	36.941594
1627.448295	77404.727848	36.946612
1628.551079	77483.781078	36.951629
1630.750033	77546.979910	36.956647
1631.993741	77625.226073	36.961664
1633.986637	77701.087612	36.966682
1635.718556	77775.710721	36.971700
1636.942130	77849.894196	36.976717
1638.427339	77925.354422	36.981735
1640.241401	78009.466495	36.986752
1641.921136	78067.021730	36.991770
1643.571787	78153.034728	36.996788
1645.111854	78234.390669	37.001805
1646.770686	78290.302756	37.006823
1648.323575	78369.338771	37.011840
1650.307058	78437.197369	37.016858
1651.812556	78492.538448	37.021876
1653.339172	78557.821129	37.026893
1654.803118	78610.964625	37.031911
1656.303612	78671.209579	37.036928
1657.878575	78739.436905	37.041946
1659.309204	78794.194885	37.046964
1660.887539	78864.347627	37.051981
1662.826910	78933.607910	37.056999
1664.059964	79010.288769	37.062016
1665.572932	79081.503800	37.067034
1667.480901	79161.500022	37.072052
1668.966729	79234.886062	37.077069
1670.494365	79304.857827	37.082087
1672.366764	79387.115330	37.087104
1674.090170	79474.261272	37.092122
1675.541876	79547.450778	37.097140
1677.436920	79635.381181	37.102157
1679.153730	79717.271276	37.107175
1680.792946	79798.755676	37.112192
1682.799003	79880.309595	37.117210
1684.640412	79959.685087	37.122228
1686.014511	80044.683053	37.127245
1687.912410	80124.088181	37.132263
1689.435794	80203.716849	37.137280
1691.347477	80297.005851	37.142298
1693.011859	80368.884638	37.147316
1694.668648	80459.857577	37.152333
1696.882743	80534.324005	37.157351
1698.550414	80627.310227	37.162368
1699.991703	80704.013855	37.167386
1701.982394	80774.867070	37.172404
1703.589004	80859.425708	37.177421
1705.805579	80942.064719	37.182439
1707.564413	81024.471538	37.187456
1709.127159	81101.993447	37.192474
1710.973893	81176.379716	37.197492
1712.313737	81262.565036	37.202509
1714.286373	81340.023458	37.207527
1716.140911	81402.778237	37.212544
1717.392003	81497.517631	37.217562
1719.786885	81569.652614	37.222580
1721.494271	81660.773578	37.227597
1722.748065	81738.535647	37.232615
1724.466986	81826.475179	37.237632
1726.176665	81905.762788	37.242650
1728.139205	81989.458248	37.247668
1729.658111	82073.489457	37.252685
1731.399980	82139.798481	37.257703
1733.463004	82232.196006	37.262720
1734.696740	82326.079328	37.267738
1736.810359	82390.227506	37.272756
1738.737944	82496.609729	37.277773
1740.378447	82564.430713	37.282791
1741.748071	82657.863079	37.287808
1743.625454	82735.378261	37.292826
1745.210975	82820.528933	37.297844
1746.977460	82911.619347	37.302861
1749.031504	82989.525705	37.307879
1750.697833	83080.036818	37.312896
1752.300434	83166.934397	37.317914
1754.262993	83246.363580	37.322932
1755.845131	83334.569951	37.327949
1757.705975	83419.121822	37.332967
1759.322048	83496.870040	37.337984
1761.170697	83584.313244	37.343002
1762.979531	83671.205431	37.348020
1764.526024	83751.486728	37.353037
1766.339377	83822.502071	37.358055
1768.235141	83896.925847	37.363072
1769.902851	83968.179751	37.368090
1771.362088	84038.490790	37.373108
1773.230285	84106.469889	37.378125
1774.991009	84173.350916	37.383143
1776.253265	84249.965476	37.388160
1777.924010	84321.751972	37.393178
1779.631524	84398.956150	37.398196
1781.294800	84484.872570	37.403213
1782.995454	84573.266959	37.408231
1785.348527	84657.694785	37.413248
1786.531159	84750.060864	37.418266
1788.096519	84827.047685	37.423284
1789.760086	84929.780271	37.428301
1791.690554	85015.466393	37.433319
1793.634166	85111.566661	37.438336
1795.050329	85209.713875	37.443354
1797.107695	85303.097948	37.448372
1798.945868	85408.313882	37.453389
1800.480473	85511.638943	37.458407
1802.788157	85607.455800	37.463424
1804.544815	85707.578890	37.468442
1806.694715	85807.184605	37.473460
1808.640581	85906.835263	37.478477
1810.438179	86008.435589	37.483495
1812.358273	86097.585964	37.488512
1814.194199	86198.952866	37.493530
1816.454363	86284.869941	37.498548
1818.133022	86383.778389	37.503565
1820.121494	86473.071282	37.508583
1821.947356	86561.921027	37.513600
1823.936928	86645.638552	37.518618
1825.887837	86730.363471	37.523636
1827.572551	86828.537496	37.528653
1829.661596	86915.319580	37.533671
1831.869519	87009.433250	37.538688
1833.697796	87094.964101	37.543706
1835.724814	87173.912488	37.548724
1837.419150	87256.892282	37.553741
1838.925940	87348.278144	37.558759
1841.139206	87434.066553	37.563776
1843.095953	87516.942659	37.568794
1845.256918	87605.172877	37.573812
1846.690433	87684.025427	37.578829
1848.572681	87764.569463	37.583847
1850.714578	87850.496986	37.588864
1852.522315	87936.464380	37.593882
1854.342383	88020.668585	37.598900
1855.968724	88110.948258	37.603917
1857.784089	88194.266603	37.608935
1859.925562	88277.787609	37.613952
1861.183299	88368.404553	37.618970
1863.207833	88457.190940	37.623988
1865.292344	88546.880662	37.629005
1866.612689	88632.736262	37.634023
1868.868622	88715.784370	37.639040
1871.041175	88817.209037	37.644058
1872.520502	88895.424005	37.649076
1874.314292	88986.377171	37.654093
1876.376293	89092.407759	37.659111
1878.220637	89161.289536	37.664128
1879.983854	89264.731464	37.669146
1882.217245	89352.169836	37.674164
1883.987814	89438.388208	37.679181
1885.591333	89522.148989	37.684199
1887.571924	89614.304166	37.689216
1889.133398	89704.535480	37.694234
1891.017512	89798.113076	37.699252
1892.566518	89872.771136	37.704269
1893.915883	89944.102131	37.709287
1895.965287	90029.556190	37.714304
1897.681540	90115.037278	37.719322
1899.359190	90196.621164	37.724340
1901.227630	90285.919045	37.729357
1902.902141	90381.609753	37.734375
1904.284349	90481.478157	37.739392
1906.470498	90582.805321	37.744410
1908.013456	90677.997933	37.749428
1909.990934	90785.023648	37.754445
1911.853850	90899.811456	37.759463
1913.898902	91007.283651	37.764480
1915.766249	91116.304922	37.769498
1917.820652	91231.051354	37.774516
1920.088707	91335.029796	37.779533
1921.297248	91449.275710	37.784551
1923.780913	91558.899220	37.789568
1926.138854	91677.465492	37.794586
1928.291838	91786.038908	37.799604
1930.435546	91887.744657	37.804621
1931.812037	91999.000562	37.809639
1934.141199	92106.254767	37.814656
1936.032684	92214.427030	37.819674
1938.075160	92324.958866	37.824692
1939.942252	92437.102871	37.829709
1941.659072	92548.104737	37.834727
1943.788669	92655.011867	37.839744
1945.601389	92774.567639	37.844762
1947.771853	92887.882607	37.849780
1949.815267	92998.936406	37.854797
1951.804860	93117.096961	37.859815
1954.294971	93228.398569	37.864832
1956.447962	93334.543922	37.869850
1958.283658	93446.366995	37.874868
1960.382879	93551.355412	37.879885
1961.297814	93670.966437	37.884903
1963.857421	93786.403956	37.889920
1965.709026	93906.693218	37.894938
1967.521484	94014.225100	37.899956
1969.942038	94110.482604	37.904973
1971.467027	94234.398681	37.909991
1973.636076	94357.149745	37.915008
1975.520641	94476.460065	37.920026
1977.411270	94596.631830	37.925044
1979.532263	94706.830400	37.930061
1981.515016	94834.948907	37.935079
1983.652362	94950.089259	37.940096
1985.643984	95088.614117	37.945114
1987.669502	95191.338019	37.950132
1989.971163	95315.605891	37.955149
1991.853776	95422.726060	37.960167
1993.901914	95529.554505	37.965184
1995.889821	95639.016653	37.970202
1997.830978	95759.983590	37.975220
2000.014293	95874.638483	37.980237
2001.888127	95993.892923	37.985255
2004.250225	96102.537583	37.990272
2006.151341	96222.143554	37.995290
2007.766941	96327.749440	38.000308
2010.011909	96453.171563	38.005325
2011.584438	96570.282351	38.010343
2013.768230	96681.694994	38.015360
2015.435449	96806.384965	38.020378
2017.371688	96931.958715	38.025396
2019.456292	97047.558717	38.030413
2021.574338	97173.181038	38.035431
2023.116963	97303.216607	38.040448
2025.232712	97403.284235	38.045466
2027.058586	97517.886957	38.050484
2028.811138	97613.778075	38.055501
2030.751676	97731.444067	38.060519
2032.838892	97842.964654	38.065536
2034.906367	97949.963091	38.070554
2036.522872	98062.432801	38.075572
2038.895657	98183.341500	38.080589
2040.342590	98309.833945	38.085607
2042.785484	98433.128571	38.090624
2044.662475	98560.264632	38.095642
2046.520359	98688.507099	38.100660
2048.296986	98815.621847	38.105677
2049.891419	98953.452511	38.110695
2051.873279	99088.218631	38.115712
2053.859086	99231.110873	38.120730
2056.109491	99382.975980	38.125748
2058.045160	99525.167439	38.130765
2060.004678	99678.866976	38.135783
2062.157033	99836.505154	38.140800
2064.474637	99984.597340	38.145818
2066.596686	100137.728492	38.150836
2068.624891	100284.662950	38.155853
2070.277099	100452.397809	38.160871
2073.094708	100599.273568	38.165888
2074.867130	100756.874245	38.170906
2077.369051	100911.978082	38.175924
2079.622736	101074.664942	38.180941
2081.695552	101225.945247	38.185959
2083.895173	101369.003633	38.190976
2086.080042	101525.630660	38.195994
2087.635135	101693.082812	38.201012
2090.212599	101836.946248	38.206029
2092.337023	101990.199831	38.211047
2094.465009	102138.103256	38.216064
2097.095470	102301.421892	38.221082
2098.992315	102453.381993	38.226100
2101.229230	102599.127762	38.231117
2103.167754	102769.327373	38.236135
2105.490296	102922.326072	38.241152
2107.907973	103078.214046	38.246170
2109.198173	103223.273883	38.251188
2111.662797	103386.446319	38.256205
2113.625023	103548.328827	38.261223
2115.876952	103707.580264	38.266240
2118.086468	103853.640127	38.271258
2119.820622	104017.741406	38.276276
2122.318120	104172.024434	38.281293
2124.241447	104342.792351	38.286311
2126.638168	104495.254135	38.291328
2128.821346	104654.051698	38.296346
2130.824298	104815.616978	38.301364
2132.829294	104974.431251	38.306381
2135.083128	105138.520095	38.311399
2136.871028	105302.581198	38.316416
2139.166787	105465.435142	38.321434
2141.230849	105625.105454	38.326452
2143.668308	105788.965847	38.331469
2145.653316	105949.563004	38.336487
2147.936799	106125.076590	38.341504
2150.246110	106280.096099	38.346522
2152.090112	106450.189665	38.351540
2154.511728	106609.707216	38.356557
2156.210675	106780.053361	38.361575
2158.220998	106945.152721	38.366592
2160.900820	107108.664530	38.371610
2162.748245	107279.459097	38.376628
2164.822128	107428.193120	38.381645
2166.615704	107593.545075	38.386663
2169.089525	107730.247423	38.391680
2171.087390	107864.780310	38.396698
2173.013146	108026.030498	38.401716
2174.794240	108161.181764	38.406733
2177.139767	108319.590565	38.411751
2179.134748	108474.314086	38.416768
2181.080491	108632.913673	38.421786
2182.978778	108799.599178	38.426804
2184.944910	108963.738662	38.431821
2187.316544	109144.072621	38.436839
2189.379319	109317.265622	38.441856
2191.301256	109496.885525	38.446874
2193.508661	109687.316860	38.451892
2195.571645	109853.740675	38.456909
2197.600311	110039.573194	38.461927
2199.875758	110228.475044	38.466944
2202.425786	110429.255599	38.471962
2204.309247	110614.771462	38.476980
2206.868595	110801.780445	38.481997
2208.845229	111004.175769	38.487015
2211.095454	111193.644712	38.492032
2213.409279	111395.571009	38.497050
2214.991780	111599.286885	38.502068
2218.031202	111790.296866	38.507085
2220.246329	111987.498872	38.512103
2222.270372	112200.381659	38.517120
2224.895965	112401.465880	38.522138
2227.185395	112594.588595	38.527156
2229.689996	112803.075096	38.532173
2231.896003	112990.252259	38.537191
2234.149508	113190.118163	38.542208
2237.390155	113384.732331	38.547226
2239.150663	113575.622121	38.552244
2241.423228	113761.740194	38.557261
2243.884119	113963.772021	38.562279
2246.456430	114152.686142	38.567296
2248.950966	114335.969508	38.572314
2250.988493	114532.858037	38.577332
2253.393337	114705.427477	38.582349
2256.091812	114896.456450	38.587367
2257.771685	115090.296556	38.592384
2260.417454	115281.805052	38.597402
2262.306754	115477.948148	38.602420
2264.587879	115663.909647	38.607437
2266.827558	115857.590097	38.612455
2268.995171	116056.242084	38.617472
2271.407626	116249.910232	38.622490
2273.292414	116441.023740	38.627508
2275.293316	116643.357826	38.632525
2277.475811	116851.778179	38.637543
2279.561875	117046.008867	38.642560
2282.407006	117252.285681	38.647578
2284.778515	117457.267852	38.652596
2286.895994	117657.141155	38.657613
2289.086045	117872.757840	38.662631
2291.352842	118082.376808	38.667648
2293.643164	118278.725518	38.672666
2295.855118	118482.685413	38.677684
2297.957760	118694.312194	38.682701
2300.917306	118898.436419	38.687719
2302.715749	119112.764162	38.692736
2305.024726	119318.768243	38.697754
2306.903668	119537.791757	38.702772
2309.168970	119743.462463	38.707789
2311.451405	119963.351262	38.712807
2313.596017	120172.239709	38.717824
2315.893965	120374.179313	38.722842
2318.137098	120585.477403	38.727860
2320.268850	120783.474727	38.732877
2322.813905	120980.025721	38.737895
2324.432839	121173.221471	38.742912
2326.852252	121370.770851	38.747930
2328.839685	121586.440048	38.752948
2330.753849	121783.487025	38.757965
2333.163902	122006.830517	38.762983
2335.156320	122226.067065	38.768000
2337.442094	122446.375273	38.773018
2339.247203	122687.843527	38.778036
2341.749570	122925.715585	38.783053
2344.154025	123153.176618	38.788071
2346.131772	123401.548673	38.793088
2348.697660	123642.307466	38.798106
2351.103856	123890.678964	38.803124
2353.564559	124136.493556	38.808141
2355.684498	124387.437453	38.813159
2358.400494	124633.595729	38.818176
2360.635939	124882.875416	38.823194
2362.885199	125144.802886	38.828212
2365.135678	125405.209468	38.833229
2367.915903	125653.368361	38.838247
2370.198362	125909.193284	38.843264
2372.860913	126163.590172	38.848282
2375.327307	126428.422556	38.853300
2377.986857	126694.583932	38.858317
2380.691131	126944.043895	38.863335
2382.823076	127197.959259	38.868352
2384.795481	127452.624304	38.873370
2387.623354	127720.250339	38.878388
2390.015760	127979.864375	38.883405
2392.771117	128231.747354	38.888423
2394.843042	128507.337510	38.893440
2397.625600	128757.734953	38.898458
2399.963700	129016.323511	38.903476
2402.360170	129278.063766	38.908493
2405.386088	129537.309175	38.913511
2407.546159	129789.599083	38.918528
2409.983776	130048.406744	38.923546
2412.531702	130302.542206	38.928564
2415.304846	130564.916596	38.933581
2417.487028	130817.335985	38.938599
2419.942169	131075.956781	38.943616
2422.452689	131336.372206	38.948634
2424.844628	131594.752223	38.953652
2426.824559	131854.264060	38.958669
2429.528473	132114.019470	38.963687
2432.081456	132387.110426	38.968704
2433.993845	132653.349869	38.973722
2436.372272	132920.000197	38.978740
2438.600658	133202.942755	38.983757
2441.483008	133459.670942	38.988775
2444.038734	133732.351068	38.993792
2446.489395	134001.470972	38.998810
2448.856259	134266.456244	39.003828
2451.199781	134539.237945	39.008845
2453.824810	134806.850774	39.013863
2456.056980	135071.379676	39.018880
2458.649080	135351.753755	39.023898
2461.665082	135627.812254	39.028916
2463.844355	135896.186499	39.033933
2466.349056	136163.750036	39.038951
2468.474296	136445.523618	39.043968
2470.866066	136714.465848	39.048986
2473.208052	136994.749560	39.054004
2475.549511	137265.758651	39.059021
2477.605498	137530.875020	39.064039
2479.825726	137798.632146	39.069056
2482.320779	138047.388608	39.074074
2484.468060	138315.731175	39.079092
2486.796296	138589.656122	39.084109
2489.311284	138838.540573	39.089127
2491.491909	139122.149142	39.094144
2493.721769	139384.380744	39.099162
2495.887632	139672.512771	39.104180
2497.947836	139967.287640	39.109197
2500.527385	140253.112202	39.114215
2502.668585	140553.500049	39.119232
2504.993812	140854.229024	39.124250
2507.556483	141161.877434	39.129268
2509.817282	141475.577930	39.134285
2512.418960	141785.419760	39.139303
2514.940394	142101.723295	39.144320
2517.366361	142429.821416	39.149338
2519.793002	142742.780690	39.154356
2522.045885	143074.336874	39.159373
2524.950116	143397.556514	39.164391
2527.399257	143740.166247	39.169408
2529.550151	144075.019515	39.174426
2532.080282	144414.207091	39.179444
2534.720259	144773.598103	39.184461
2537.370332	145098.150341	39.189479
2540.051986	145448.794781	39.194496
2542.625953	145806.223440	39.199514
2545.447915	146143.079606	39.204532
2548.003564	146496.594001	39.209549
2550.324531	146848.510188	39.214567
2552.932942	147199.673010	39.219584
2555.334030	147559.450869	39.224602
2558.756876	147919.299844	39.229620
2561.103428	148275.727553	39.234637
2563.614517	148633.058509	39.239655
2565.940168	148991.575935	39.244672
2568.204368	149350.092684	39.249690
2570.928059	149710.190068	39.254708
2573.322060	150083.732826	39.259725
2576.188762	150454.119732	39.264743
2578.679756	150826.928904	39.269760
2581.142693	151197.028584	39.274778
2584.146812	151569.940248	39.279796
2586.733175	151937.550334	39.284813
2589.299419	152315.156006	39.289831
2592.324673	152688.490761	39.294848
2594.778556	153059.734008	39.299866
2597.206855	153442.370251	39.304884
2599.478248	153810.638476	39.309901
2602.632242	154185.778226	39.314919
2605.676496	154555.314025	39.319936
2608.154894	154929.840728	39.324954
2610.470154	155307.645146	39.329972
2612.803426	155684.128962	39.334989
2615.435636	156054.373466	39.340007
2618.099774	156444.850646	39.345024
2620.352482	156825.010422	39.350042
2623.059849	157205.393490	39.355060
2625.629249	157595.867639	39.360077
2628.385485	157986.937150	39.365095
2630.733170	158370.557583	39.370112
2633.297694	158756.266609	39.375130
2635.785906	159147.410873	39.380148
2638.331620	159557.020352	39.385165
2641.351399	159929.868595	39.390183
2643.722048	160333.721452	39.395200
2646.305658	160734.458566	39.400218
2648.852108	161122.089409	39.405236
2651.221642	161502.374059	39.410253
2653.850263	161877.402466	39.415271
2656.258164	162257.317410	39.420288
2658.444719	162631.225924	39.425306
2661.057724	163022.958598	39.430324
2663.254328	163402.875180	39.435341
2665.943647	163804.122652	39.440359
2668.043206	164204.969639	39.445376
2670.166349	164614.144139	39.450394
2672.822540	165029.865283	39.455412
2675.303164	165451.101324	39.460429
2678.222527	165868.271922	39.465447
2681.456464	166288.874733	39.470464
2683.752881	166713.981714	39.475482
2686.708284	167147.710923	39.480500
2689.412271	167580.948865	39.485517
2692.090111	168016.301244	39.490535
2694.689470	168444.063028	39.495552
2697.189561	168894.532633	39.500570
2699.963546	169336.251923	39.505588
2702.353127	169797.321169	39.510605
2705.088008	170248.079832	39.515623
2707.816435	170703.159368	39.520640
2710.672392	171158.894692	39.525658
2713.077660	171633.063967	39.530676
2715.446957	172097.782059	39.535693
2718.239080	172578.296310	39.540711
2720.777156	173051.361558	39.545728
2723.091527	173543.803553	39.550746
2726.286836	174034.536286	39.555764
2728.164459	174531.382727	39.560781
2730.819931	175040.326179	39.565799
2733.516076	175546.866491	39.570816
2736.014813	176058.304246	39.575834
2739.281893	176561.942466	39.580852
2741.729246	177089.635793	39.585869
2744.128553	177604.285830	39.590887
2746.904318	178127.921482	39.595904
2749.642575	178659.921894	39.600922
2752.634408	179190.158842	39.605940
2755.420579	179717.510396	39.610957
2758.331566	180245.810643	39.615975
2761.384366	180781.812766	39.620992
2764.080005	181317.137330	39.626010
2766.951274	181852.335914	39.631028
2770.140543	182388.732326	39.636045
2773.044725	182934.573803	39.641063
2775.853167	183524.627058	39.646080
2778.620648	184059.727185	39.651098
2781.612335	184581.663867	39.656116
2784.083554	185120.854450	39.661133
2787.007787	185659.113462	39.666151
2789.827409	186192.565764	39.671168
2792.415042	186733.219723	39.676186
2795.185247	187259.039904	39.681204
2798.391691	187801.075665	39.686221
2801.154469	188337.595533	39.691239
2804.574624	188861.619995	39.696256
2806.907669	189410.759828	39.701274
2810.067605	189927.438490	39.706292
2812.994475	190467.321021	39.711309
2815.486159	191002.854412	39.716327
2818.935650	191529.426412	39.721344
2821.139643	192061.326425	39.726362
2824.483381	192593.253690	39.731380
2826.878588	193130.437141	39.736397
2829.959218	193646.001015	39.741415
2833.445490	194152.435311	39.746432
2835.889489	194664.241809	39.751450
2838.528823	195155.698686	39.756468
2841.091043	195661.851397	39.761485
2843.677719	196160.788118	39.766503
2846.170324	196658.903071	39.771520
2848.381908	197170.221761	39.776538
2851.291027	197687.859795	39.781556
2853.912848	198215.654494	39.786573
2856.569330	198748.780015	39.791591
2859.375307	199272.637668	39.796608
2861.728601	199812.190143	39.801626
2864.512707	200355.665192	39.806644
2867.392393	200902.327775	39.811661
2869.983672	201446.573213	39.816679
2873.251655	202003.415753	39.821696
2875.608209	202565.432288	39.826714
2878.540587	203122.407016	39.831732
2880.868223	203705.972965	39.836749
2884.112663	204289.473535	39.841767
2886.964126	204864.578171	39.846784
2889.284767	205467.558217	39.851802
2892.227027	206058.986073	39.856820
2894.746943	206659.067839	39.861837
2897.579492	207272.337358	39.866855
2900.774757	207868.912733	39.871872
2903.650958	208486.141529	39.876890
2906.377125	209106.011885	39.881908
2909.653390	209735.196964	39.886925
2912.086611	210348.689061	39.891943
2915.199485	210976.098947	39.896960
2917.414418	211617.749581	39.901978
2920.676474	212263.607240	39.906996
2924.298299	212902.246137	39.912013
2927.258038	213535.324784	39.917031
2930.583533	214167.432842	39.922048
2933.626136	214798.951126	39.927066
2937.155946	215428.666775	39.932084
2940.476814	216052.166705	39.937101
2943.632752	216682.044264	39.942119
2946.829790	217294.031879	39.947136
2950.279174	217914.186224	39.952154
2953.193889	218533.180074	39.957172
2956.256072	219142.777420	39.962189
2959.188088	219775.081442	39.967207
2962.182070	220392.870610	39.972224
2965.367198	221012.840485	39.977242
2968.047203	221638.402425	39.982260
2970.856113	222254.392618	39.987277
2973.571364	222893.794882	39.992295
2976.367702	223509.939961	39.997312
2979.780569	224131.349045	40.002330
2982.469405	224757.037725	40.007348
2985.605459	225393.427843	40.012365
2988.429733	226039.113784	40.017383
2991.297780	226670.236255	40.022400
2994.017559	227301.203939	40.027418
2996.994403	227946.611534	40.032436
2999.732348	228580.471959	40.037453
3002.753229	229219.571845	40.042471
3005.792720	229864.943211	40.047488
3008.770301	230517.944982	40.052506
3011.797983	231178.457939	40.057524
3014.442832	231830.596011	40.062541
3017.305877	232485.569913	40.067559
3020.236054	233144.368539	40.072576
3023.039078	233817.158325	40.077594
3026.336790	234475.338812	40.082612
3029.315635	235123.889337	40.087629
3032.081883	235768.966367	40.092647
3034.557340	236390.741794	40.097664
3037.368167	237039.696433	40.102682
3040.413627	237687.317576	40.107700
3043.567310	238312.158929	40.112717
3046.490536	238978.773014	40.117735
3049.564155	239634.616426	40.122752
3051.988137	240284.310672	40.127770
3054.759816	240947.006292	40.132788
3057.779714	241616.825119	40.137805
3060.359635	242298.625033	40.142823
3063.930682	242980.090193	40.147840
3066.925911	243667.435262	40.152858
3069.501498	244358.171600	40.157876
3072.681083	245050.284616	40.162893
3075.390929	245759.158379	40.167911
3078.354680	246467.304035	40.172928
3081.481837	247184.718873	40.177946
3084.619455	247902.154705	40.182964
3087.999542	248634.841992	40.187981
3090.320719	249357.505470	40.192999
3093.874522	250094.604755	40.198016
3097.094546	250836.071267	40.203034
3099.462009	251572.333238	40.208052
3102.856632	252322.529090	40.213069
3105.801559	253077.922659	40.218087
3108.969476	253833.734690	40.223104
3112.095392	254605.933185	40.228122
3115.000938	255373.538815	40.233140
3117.995097	256135.944407	40.238157
3121.153053	256920.799832	40.243175
3124.588390	257692.855894	40.248192
3127.999652	258472.378765	40.253210
3130.664274	259253.435861	40.258228
3134.169511	260044.973754	40.263245
3137.100690	260835.859459	40.268263
3140.545444	261618.353611	40.273280
3144.038969	262405.914629	40.278298
3146.939318	263199.734849	40.283316
3150.564358	263985.054082	40.288333
3153.849501	264792.873509	40.293351
3157.288128	265575.238193	40.298368
3160.557626	266360.747323	40.303386
3163.611273	267144.683870	40.308404
3166.892406	267935.817077	40.313421
3170.478761	268732.432812	40.318439
3173.440925	269525.964632	40.323456
3176.777523	270312.497479	40.328474
3180.069405	271096.516124	40.333492
3183.424988	271882.676667	40.338509
3186.575685	272675.693992	40.343527
3189.464342	273466.510053	40.348544
3192.722855	274256.930732	40.353562
3196.244361	275050.502720	40.358580
3199.750160	275822.635150	40.363597
3203.044955	276606.018153	40.368615
3206.418861	277389.406450	40.373632
3209.718300	278169.827286	40.378650
3212.992517	278945.215928	40.383668
3217.095715	279723.819152	40.388685
3220.670508	280485.609499	40.393703
3224.654097	281227.495099	40.398720
3228.307811	281982.908964	40.403738
3231.260155	282730.247752	40.408756
3235.438527	283455.751678	40.413773
3238.640696	284187.622073	40.418791
3241.795127	284916.902104	40.423808
3245.214951	285622.060545	40.428826
3248.162108	286324.720888	40.433844
3251.070423	287013.058704	40.438861
3254.388861	287705.844981	40.443879
3256.947141	288405.395375	40.448896
3259.856345	289100.058955	40.453914
3262.528430	289800.693572	40.458932
3265.351698	290514.474614	40.463949
3267.972463	291243.183400	40.468967
3270.440966	291978.432683	40.473984
3273.838836	292721.627188	40.479002
3276.232585	293478.806876	40.484020
3279.170621	294245.057391	40.489037
3282.019709	295024.184061	40.494055
3285.024492	295820.514843	40.499072
3288.003588	296604.880807	40.504090
3290.896298	297415.246691	40.509108
3293.832857	298219.704191	40.514125
3297.453163	299049.938073	40.519143
3300.599570	299872.084424	40.524160
3303.960518	300702.435420	40.529178
3307.373463	301552.338097	40.534196
3310.105076	302393.499605	40.539213
3313.539619	303255.201322	40.544231
3316.531404	304117.719594	40.549248
3319.901677	304988.261879	40.554266
3322.986239	305871.449779	40.559284
3326.361248	306747.545633	40.564301
3329.326117	307641.737539	40.569319
3332.892089	308541.225767	40.574336
3336.363125	309440.356948	40.579354
3339.620421	310348.109184	40.584372
3343.079734	311244.873388	40.589389
3346.345390	312162.234538	40.594407
3349.731288	313073.087018	40.599424
3353.254904	313996.386827	40.604442
3356.802477	314921.466229	40.609460
3360.442724	315845.649433	40.614477
3363.669636	316775.943606	40.619495
3367.026558	317687.164900	40.624512
3370.855468	318617.859182	40.629530
3374.098993	319547.483190	40.634548
3377.952608	320473.413808	40.639565
3381.144981	321399.529262	40.644583
3384.479863	322332.021994	40.649600
3388.473655	323247.593273	40.654618
3392.073959	324173.837440	40.659636
3395.863794	325094.195330	40.664653
3399.412828	326018.934158	40.669671
3402.451973	326941.854018	40.674688
3406.208984	327857.866234	40.679706
3409.053883	328782.549831	40.684724
3412.710965	329710.864851	40.689741
3416.187077	330634.289735	40.694759
3419.602860	331560.238862	40.699776
3422.764610	332492.598117	40.704794
3425.680911	333437.656663	40.709812
3429.213102	334375.543155	40.714829
3432.675819	335307.278260	40.719847
3436.388743	336254.474588	40.724864
3440.042162	337177.330646	40.729882
3443.260491	338123.389011	40.734900
3447.178312	339052.623842	40.739917
3450.729641	339993.102300	40.744935
3453.494329	340926.602680	40.749952
3457.418106	341859.161583	40.754970
3460.623360	342798.959703	40.759988
3464.051412	343740.371253	40.765005
3467.853338	344663.939369	40.770010
3471.202612	345545.050996	40.775015
3474.377745	346389.099819	40.780020
3477.523516	347174.253219	40.785024
3481.046703	347916.340426	40.790029
3483.937274	348603.370626	40.795034
3486.432935	349233.454273	40.800039
3489.086883	349799.085274	40.805044
3492.193497	350326.403728	40.810048
3494.557052	350783.086417	40.815053
3496.973093	351201.142224	40.820058
3499.162247	351571.516221	40.825063
3501.378112	351898.110334	40.830068
3503.233823	352182.740262	40.835072
3505.154902	352409.936948	40.840077
3507.207235	352588.358993	40.845082
3508.709986	352734.686396	40.850087
3510.155420	352845.639945	40.855092
3511.350807	352929.866893	40.860096
3512.469205	352975.317632	40.865101
3513.579739	352986.785544	40.870106
3514.357327	352983.791766	40.875111
3515.622219	352944.755156	40.880116
3516.264723	352888.328094	40.885120
3516.926081	352800.303109	40.890125
3517.745524	352700.535317	40.895130
3518.243877	352588.743663	40.900135
3519.176003	352448.542150	40.905140
3519.308242	352298.755151	40.910144
3519.707075	352129.556662	40.915149
3520.124593	351939.561675	40.920154
3520.448763	351761.806739	40.925159
3520.865252	351565.149902	40.930164
3521.268627	351351.107049	40.935168
3521.234680	351136.800691	40.940173
3521.469186	350913.325256	40.945178
3521.418614	350673.827452	40.950183
3522.119799	350418.068572	40.955188
3522.202036	350187.723090	40.960192
3522.253142	349919.326342	40.965197
3522.474607	349657.383042	40.970202
3522.174251	349407.162008	40.975207
3522.340853	349129.334981	40.980212
3522.459499	348861.935855	40.985216
3522.373363	348592.380319	40.990221
3522.765703	348322.773200	40.995226
3522.625510	348033.977282	41.000231
3522.649082	347765.694378	41.005236
3522.728510	347477.291458	41.010240
3522.432834	347190.673421	41.015245
3522.406543	346891.273961	41.020250
3521.928298	346611.289437	41.025255
3522.307452	346318.329775	41.030260
3521.861858	346043.699726	41.035264
3521.861580	345753.336815	41.040269
3522.130391	345469.971769	41.045274
3521.928553	345188.457621	41.050279
3521.769640	344892.620516	41.055284
3521.719311	344608.154073	41.060288
3521.613320	344320.744684	41.065293
3521.592299	344031.743245	41.070298
3521.480719	343750.279389	41.075303
3521.378739	343458.336453	41.080308
3520.938177	343183.250319	41.085312
3520.767425	342902.373573	41.090317
3521.162270	342629.491603	41.095322
3520.456718	342329.624290	41.100327
3520.611450	342050.240761	41.105332
3520.210607	341779.459779	41.110336
3519.895513	341509.019268	41.115341
3520.200975	341239.573016	41.120346
3519.962739	340968.938334	41.125351
3519.813129	340691.142604	41.130356
3519.965915	340420.010307	41.135360
3519.146386	340157.088562	41.140365
3519.368724	339875.948087	41.145370
3519.109691	339623.360249	41.150375
3518.996768	339355.058457	41.155380
3518.491608	339109.752551	41.160384
3518.231595	338843.427911	41.165389
3518.705547	338590.260459	41.170394
3518.322585	338351.770645	41.175399
3518.232944	338087.498953	41.180404
3517.994321	337838.582594	41.185408
3517.677824	337584.921350	41.190413
3517.713264	337344.375961	41.195418
3517.267795	337105.302812	41.200423
3517.504336	336862.917270	41.205428
3517.239326	336621.422299	41.210432
3516.821739	336371.074343	41.215437
3517.141079	336147.133651	41.220442
3516.527283	335915.886248	41.225447
3516.501555	335679.052364	41.230452
3516.203063	335450.448430	41.235456
3516.067627	335227.183591	41.240461
3516.107188	335008.925473	41.245466
3516.136374	334785.250765	41.250471
3516.336477	334563.404508	41.255476
3515.845183	334337.494190	41.260480
3515.546335	334113.968464	41.265485
3515.544317	333896.880207	41.270490
3515.218178	333692.176049	41.275495
3515.268051	333472.483126	41.280500
3515.151729	333265.073430	41.285504
3514.955012	333050.986344	41.290509
3515.114306	332839.233082	41.295514
3514.663474	332637.950704	41.300519
3514.646480	332433.369419	41.305524
3514.111459	332222.535122	41.310528
3513.980903	332027.023668	41.315533
3514.078232	331824.939152	41.320538
3513.874467	331631.929612	41.325543
3513.976476	331435.310556	41.330548
3513.732335	331246.298499	41.335552
3513.637993	331055.990389	41.340557
3513.710500	330856.448062	41.345562
3513.441036	330681.451450	41.350567
3512.979550	330493.639659	41.355572
3513.227424	330305.334539	41.360576
3512.785634	330124.359783	41.365581
3512.875836	329946.124280	41.370586
3512.641116	329768.803546	41.375591
3512.830223	329579.410395	41.380596
3513.053949	329407.128794	41.385600
3512.868442	329236.919800	41.390605
3512.481772	329054.736005	41.395610
3511.949636	328886.996046	41.400615
3512.215052	328705.471751	41.405620
3512.263133	328533.849667	41.410624
3512.264381	328371.289323	41.415629
3512.392667	328197.999910	41.420634
3511.891110	328038.009526	41.425639
3511.911725	327865.498573	41.430644
3511.719769	327703.830524	41.435648
3511.844610	327537.431995	41.440653
3511.787924	327364.269607	41.445658
3511.305333	327210.835544	41.450663
3511.528917	327040.578580	41.455668
3511.302403	326893.080887	41.460672
3510.979966	326736.821920	41.465677
3511.286864	326581.354251	41.470682
3511.001473	326433.864075	41.475687
3510.740214	326274.744794	41.480692
3510.559002	326125.609223	41.485696
3510.295337	325988.746804	41.490701
3510.580018	325839.333840	41.495706
3510.282110	325697.693548	41.500711
3510.436214	325549.520933	41.505716
3510.373920	325407.639292	41.510720
3510.181729	325267.380046	41.515725
3510.314712	325126.560722	41.520730
3510.163821	324978.713529	41.525735
3509.927575	324842.835046	41.530740
3510.006575	324709.679587	41.535744
3510.062652	324573.525566	41.540749
3509.858223	324426.346143	41.545754
3509.311419	324294.075760	41.550759
3509.613569	324162.053806	41.555764
3509.250838	324029.702919	41.560768
3509.123599	323917.411333	41.565773
3509.392309	323776.388088	41.570778
3509.064567	323655.172698	41.575783
3509.145159	323524.938624	41.580788
3509.315306	323405.730655	41.585792
3508.780981	323278.161277	41.590797
3509.036257	323154.411127	41.595802
3508.722510	323029.630244	41.600807
3508.842712	322914.371751	41.605812
3508.741975	322804.896771	41.610816
3508.270984	322690.213432	41.615821
3508.566491	322564.496409	41.620826
3508.183723	322458.269988	41.625831
3508.086941	322340.016529	41.630836
3508.011770	322233.487054	41.635840
3508.141047	322128.858766	41.640845
3507.757989	322017.110849	41.645850
3507.627566	321912.064707	41.650855
3507.759676	321807.002699	41.655860
3507.876814	321703.977971	41.660864
3507.387046	321598.071385	41.665869
3507.334895	321496.090219	41.670874
3507.351239	321402.773203	41.675879
3507.249648	321302.859956	41.680884
3507.425733	321201.427525	41.685888
3507.162630	321100.088954	41.690893
3507.425441	321002.255020	41.695898
3507.100329	320912.424767	41.700903
3507.302258	320813.378775	41.705908
3507.082097	320720.351641	41.710912
3506.916046	320631.615314	41.715917
3507.248034	320536.720613	41.720922
3507.053303	320432.952900	41.725927
3507.132456	320347.459507	41.730932
3506.867360	320253.598836	41.735936
3506.573528	320162.261103	41.740941
3506.747631	320074.386316	41.745946
3506.630711	319995.537529	41.750951
3506.709618	319906.176261	41.755956
3506.856685	319813.064305	41.760960
3506.609415	319736.754094	41.765965
3506.643241	319630.277387	41.770970
3506.694770	319545.957017	41.775975
3506.761115	319461.659608	41.780980
3506.806092	319374.744913	41.785984
3506.513716	319287.475720	41.790989
3506.495607	319196.779756	41.795994
3506.198041	319119.891165	41.800999
3506.373576	319030.894605	41.806004
3506.453216	318941.811087	41.811008
3506.108850	318875.665753	41.816013
3505.845588	318796.456035	41.821018
3506.215843	318724.448918	41.826023
3506.042193	318645.682867	41.831028
3505.886327	318565.361940	41.836032
3505.652501	318491.820601	41.841037
3505.891346	318407.901252	41.846042
3505.729434	318332.694675	41.851047
3505.765305	318261.375122	41.856052
3505.678184	318194.450720	41.861056
3505.419667	318124.067440	41.866061
3505.399723	318048.380222	41.871066
3505.233574	317984.266492	41.876071
3505.199211	317911.252723	41.881076
3504.846657	317849.279643	41.886080
3505.135159	317782.041465	41.891085
3505.304387	317712.633789	41.896090
3505.272486	317654.757410	41.901095
3505.284949	317580.539980	41.906100
3505.185496	317527.813366	41.911104
3504.844391	317461.258307	41.916109
3504.840002	317399.815342	41.921114
3504.833008	317338.347256	41.926119
3504.503883	317287.081046	41.931124
3504.805518	317231.950654	41.936128
3504.545529	317174.109304	41.941133
3504.819541	317107.940959	41.946138
3504.832355	317062.676394	41.951143
3504.828863	316995.075586	41.956148
3504.524518	316936.986434	41.961152
3504.292725	316873.339324	41.966157
3504.616364	316829.145412	41.971162
3504.508002	316774.180323	41.976167
3504.573721	316718.170233	41.981172
3504.716838	316659.120260	41.986176
3504.245259	316611.055910	41.991181
3504.440418	316546.476523	41.996186
3504.041706	316497.459266	42.001191
3504.282080	316442.744564	42.006196
3504.275275	316395.726816	42.011200
3504.220219	316352.762020	42.016205
3504.136708	316302.168683	42.021210
3504.042623	316257.021785	42.026215
3504.163497	316210.187426	42.031220
3504.114764	316160.682551	42.036224
3503.938911	316109.874444	42.041229
3504.213545	316064.262614	42.046234
3504.078642	316017.900579	42.051239
3504.077955	315970.855985	42.056244
3503.947303	315922.966585	42.061248
3503.742047	315880.381026	42.066253
3504.301819	315827.905547	42.071258
3504.087436	315783.514839	42.076263
3503.805113	315727.608810	42.081268
3503.874320	315689.916198	42.086272
3503.813582	315646.977059	42.091277
3504.157743	315596.621389	42.096282
3503.822582	315558.304909	42.101287
3503.958566	315514.393476	42.106292
3504.022229	315451.156140	42.111296
3503.761400	315409.825563	42.116301
3504.014287	315375.437094	42.121306
3503.318833	315336.438886	42.126311
3503.413164	315288.615414	42.131316
3503.748771	315260.600303	42.136320
3503.457128	315218.103956	42.141325
3503.872872	315176.336622	42.146330
3503.575927	315129.617349	42.151335
3503.479929	315096.148302	42.156340
3503.688039	315052.759466	42.161344
3503.401947	315025.324838	42.166349
3503.854160	314971.669319	42.171354
3503.444078	314939.292460	42.176359
3503.168739	314909.540683	42.181364
3503.897597	314861.643005	42.186368
3503.250432	314830.727996	42.191373
3503.314511	314787.590421	42.196378
3502.982622	314758.432598	42.201383
3503.164647	314728.838196	42.206388
3503.450132	314692.917471	42.211392
3503.106880	314657.705671	42.216397
3503.451148	314614.982121	42.221402
3503.311722	314591.620805	42.226407
3502.843272	314557.369933	42.231412
3503.288897	314517.760077	42.236416
3503.171868	314485.362523	42.241421
3503.188357	314457.167810	42.246426
3502.916277	314430.493959	42.251431
3503.252818	314392.758477	42.256436
3503.310239	314352.471285	42.261440
3503.057263	314320.730975	42.266445
3503.061334	314292.080105	42.271450
3502.998733	314260.717099	42.276455
3502.870724	314231.094512	42.281460
3502.907966	314190.174225	42.286464
3502.831823	314171.942559	42.291469
3502.929053	314136.636048	42.296474
3503.118318	314117.853980	42.301479
3502.925905	314081.854822	42.306484
3502.954480	314051.291640	42.311488
3502.783160	314032.413243	42.316493
3503.041567	313993.086647	42.321498
3503.085109	313968.347851	42.326503
3502.872780	313936.422808	42.331508
3503.401764	313902.778844	42.336512
3502.896364	313878.761933	42.341517
3503.209360	313845.380695	42.346522
3502.781649	313814.252576	42.351527
3502.961541	313783.691004	42.356532
3503.292299	313749.670805	42.361536
3503.308157	313717.506380	42.366541
3502.988941	313678.702378	42.371546
3502.748378	313649.173346	42.376551
3502.687569	313622.949444	42.381556
3503.101557	313591.664140	42.386560
3502.632678	313561.763632	42.391565
3502.612240	313536.780159	42.396570
3502.720208	313520.987588	42.401575
3502.817405	313499.700634	42.406580
3503.126041	313469.805734	42.411584
3502.583201	313445.667226	42.416589
3502.597816	313410.754747	42.421594
3502.754579	313392.435470	42.426599
3502.595925	313371.773686	42.431604
3502.655711	313345.072766	42.436608
3502.149412	313320.241469	42.441613
3502.257784	313302.769402	42.446618
3502.302704	313276.147101	42.451623
3502.533177	313253.439730	42.456628
3502.624999	313244.646927	42.461632
3502.537728	313218.147039	42.466637
3502.425048	313191.880112	42.471642
3502.776857	313177.677776	42.476647
3502.194414	313142.044200	42.481652
3502.416924	313123.052970	42.486656
3502.256344	313107.989256	42.491661
3502.087899	313089.466252	42.496666
3502.242819	313068.729865	42.501671
3502.285455	313064.117692	42.506676
3502.620242	313030.757905	42.511680
3502.594208	313008.243186	42.516685
3502.497438	312989.403597	42.521690
3502.270398	312957.251172	42.526695
3502.208991	312947.922478	42.531700
3502.331865	312929.353866	42.536704
3502.443886	312916.791977	42.541709
3502.645852	312883.071173	42.546714
3502.544981	312861.967562	42.551719
3502.522301	312844.083244	42.556724
3502.715857	312827.182917	42.561728
3502.255273	312789.418075	42.566733
3502.683462	312771.590467	42.571738
3502.741213	312742.853908	42.576743
3502.505500	312722.814566	42.581748
3502.715883	312699.295821	42.586752
3502.350576	312687.266507	42.591757
3502.669360	312658.005628	42.596762
3502.627529	312640.047891	42.601767
3502.512055	312614.137307	42.606772
3502.292010	312586.309219	42.611776
3502.228809	312580.568509	42.616781
3502.659567	312544.521620	42.621786
3502.377796	312525.023744	42.626791
3502.267092	312520.969842	42.631796
3502.377636	312482.581111	42.636800
3502.289272	312477.455010	42.641805
3502.412939	312442.473864	42.646810
3502.118511	312439.568271	42.651815
3501.901265	312412.248548	42.656820
3502.257878	312393.668626	42.661824
3501.974407	312381.931784	42.666829
3502.360385	312351.718730	42.671834
3502.128777	312344.401263	42.676839
3502.501857	312325.157160	42.681844
3502.447764	312303.816975	42.686848
3502.343704	312293.451557	42.691853
3502.614183	312267.480442	42.696858
3502.314252	312248.545088	42.701863
3502.155483	312224.625799	42.706868
3502.323084	312202.945564	42.711872
3502.435957	312185.192474	42.716877
3502.429442	312168.119625	42.721882
3502.611387	312147.404049	42.726887
3502.327198	312123.148079	42.731892
3502.487768	312094.598612	42.736896
3501.948062	312083.385218	42.741901
3502.267113	312057.075601	42.746906
3502.133454	312050.964159	42.751911
3502.075207	312030.082518	42.756916
3502.406338	312018.860191	42.761920
3502.091901	312015.855918	42.766925
3501.894373	311983.112960	42.771930
3502.042153	311973.166120	42.776935
3502.077678	311960.972171	42.781940
3502.135392	311945.390488	42.786945
3501.883878	311935.149826	42.791949
3502.053797	311915.810090	42.796954
3502.289840	311900.276849	42.801959
3501.800166	311881.447348	42.806964
3501.908773	311880.946935	42.811969
3501.865498	311864.134178	42.816973
3501.895357	311843.213234	42.821978
3501.958175	311849.692083	42.826983
3501.809053	311835.262308	42.831988
3502.033272	311801.511801	42.836993
3502.000063	311802.941982	42.841997
3502.014644	311784.669750	42.847002
3502.158927	311763.400088	42.852007
3501.627173	311758.088770	42.857012
3501.970216	311749.205520	42.862017
3502.141801	311726.532060	42.867021
3502.213552	311715.146647	42.872026
3502.180692	311704.540956	42.877031
3501.719477	311678.505787	42.882036
3502.057980	311666.493407	42.887041
3502.157628	311655.129063	42.892045
3502.122856	311637.882319	42.897050
3502.271421	311625.492491	42.902055
3501.755378	311607.074134	42.907060
3502.045216	311588.606118	42.912065
3502.024221	311590.899553	42.917069
3501.962724	311559.076527	42.922074
3502.132239	311551.009188	42.927079
3502.058385	311540.409870	42.932084
3502.382332	311503.437388	42.937089
3502.421302	311502.667954	42.942093
3502.369733	311480.639963	42.947098
3502.196585	311462.804088	42.952103
3502.247021	311452.185319	42.957108
3502.260240	311427.042782	42.962113
3502.041240	311425.906543	42.967117
3502.085140	311384.753737	42.972122
3502.466299	311378.129141	42.977127
3501.941596	311371.798842	42.982132
3502.059633	311340.227506	42.987137
3502.053535	311331.042519	42.992141
3502.177825	311320.106823	42.997146
3501.874601	311301.655075	43.002151
3501.441141	311300.348794	43.007156
3501.804204	311288.052573	43.012161
3501.813229	311285.252142	43.017165
3501.775342	311252.432828	43.022170
3502.294562	311247.898645	43.027175
3501.565064	311246.485968	43.032180
3502.235848	311217.907097	43.037185
3502.074184	311213.733818	43.042189
3502.220793	311206.128029	43.047194
3502.249731	311182.687785	43.052199
3502.257327	311172.279219	43.057204
3501.919979	311136.605798	43.062209
3501.849397	311122.952352	43.067213
3501.700564	311116.665039	43.072218
3501.746399	311113.502599	43.077223
3501.810645	311085.730962	43.082228
3502.029927	311081.040086	43.087233
3502.114812	311079.143841	43.092237
3502.225298	311054.825619	43.097242
3501.956394	311041.864753	43.102247
3501.991413	311028.067541	43.107252
3502.060721	310996.274580	43.112257
3501.940753	310997.667457	43.117261
3502.042939	310979.483002	43.122266
3502.001653	310959.565188	43.127271
3501.803822	310956.211817	43.132276
3501.959876	310949.775032	43.137281
3501.961303	310923.794349	43.142285
3502.099178	310910.108252	43.147290
3501.986955	310910.838322	43.152295
3502.125635	310896.414158	43.157300
3501.866006	310871.008628	43.162305
3501.911871	310868.660444	43.167309
3501.812902	310842.008366	43.172314
3501.965932	310826.793106	43.177319
3502.089173	310819.699833	43.182324
3502.260495	310808.018727	43.187329
3501.940140	310794.175220	43.192333
3502.222206	310779.041557	43.197338
3502.065523	310763.162202	43.202343
3501.876302	310751.308433	43.207348
3502.288639	310737.274024	43.212353
3501.462560	310717.097108	43.217357
3501.655932	310699.687124	43.222362
3501.769366	310693.893123	43.227367
3501.626158	310695.544106	43.232372
3501.936510	310684.884530	43.237377
3501.801249	310672.386149	43.242381
3501.888244	310662.779338	43.247386
3501.536606	310648.711664	43.252391
3501.785135	310650.937561	43.257396
3501.952315	310630.096398	43.262401
3501.580854	310624.276412	43.267405
3502.096566	310611.930706	43.272410
3501.788432	310606.787867	43.277415
3501.373660	310592.526476	43.282420
3501.772511	310577.552614	43.287425
3501.804934	310578.539985	43.292429
3501.850068	310573.291020	43.297434
3501.624983	310560.781207	43.302439
3501.410913	310544.554503	43.307444
3501.816569	310528.180014	43.312449
3501.412718	310527.836043	43.317453
3501.559372	310515.777027	43.322458
3501.772539	310518.084798	43.327463
3501.664619	310497.999084	43.332468
3501.911089	310482.540089	43.337473
3501.774630	310488.134210	43.342477
3501.667213	310478.379631	43.347482
3501.728442	310462.746019	43.352487
3501.812221	310450.849495	43.357492
3501.715888	310447.709237	43.362497
3501.467721	310446.475749	43.367501
3501.728927	310443.406825	43.372506
3501.853738	310421.834251	43.377511
3501.681317	310412.140715	43.382516
3501.994409	310406.468144	43.387521
3501.441648	310401.312635	43.392525
3501.373736	310384.935794	43.397530
3501.811406	310371.686156	43.402535
3501.545273	310368.012618	43.407540
3501.541919	310348.979244	43.412545
3501.618469	310354.158382	43.417549
3501.878465	310350.020892	43.422554
3501.514213	310331.527415	43.427559
3501.727799	310313.808773	43.432564
3501.724570	310306.735196	43.437569
3501.671992	310317.252836	43.442573
3501.488100	310313.057506	43.447578
3501.738884	310292.457591	43.452583
3501.707409	310281.698688	43.457588
3501.832967	310273.459880	43.462593
3501.894611	310271.821701	43.467597
3502.022117	310247.474961	43.472602
3502.080670	310236.320275	43.477607
3501.723358	310227.495342	43.482612
3502.316564	310211.040531	43.487617
3501.820817	310196.511769	43.492621
3501.645358	310193.765562	43.497626
3501.684255	310194.013979	43.502631
3502.076538	310166.012397	43.507636
3502.009836	310150.704042	43.512641
3502.124741	310156.793281	43.517645
3501.742049	310129.828911	43.522650
3501.713138	310115.685178	43.527655
3501.655429	310110.299562	43.532660
3501.949134	310103.281319	43.537665
3501.892903	310092.322671	43.542669
3501.669776	310072.407469	43.547674
3501.789084	310060.098149	43.552679
3501.778131	310068.471821	43.557684
3501.919843	310048.855824	43.562689
3501.564305	310034.737685	43.567693
3501.351004	310030.928628	43.572698
3501.741358	310024.226069	43.577703
3501.722708	310013.108848	43.582708
3502.078798	310005.164759	43.587713
3501.751380	309988.879248	43.592717
3501.531817	309984.511340	43.597722
3501.771248	309976.152892	43.602727
3501.471490	309970.830549	43.607732
3501.742304	309952.034068	43.612737
3501.489108	309940.800819	43.617741
3501.497889	309941.104839	43.622746
3501.773247	309929.788954	43.627751
3501.410779	309939.998871	43.632756
3501.505943	309933.240662	43.637761
3501.312047	309919.402578	43.642765
3501.509553	309896.342496	43.647770
3501.694992	309906.135954	43.652775
3501.297122	309903.424502	43.657780
3501.948102	309894.390979	43.662785
3501.696583	309892.012900	43.667789
3501.626179	309868.409415	43.672794
3501.830854	309854.559894	43.677799
3501.835765	309859.114118	43.682804
3501.601664	309843.704603	43.687809
3501.670555	309848.503293	43.692813
3501.600250	309823.831010	43.697818
3501.990574	309812.827931	43.702823
3501.585380	309813.425693	43.707828
3501.973118	309806.723513	43.712833
3501.660215	309798.909426	43.717837
3501.761713	309778.612544	43.722842
3502.031149	309761.699263	43.727847
3502.068059	309768.538701	43.732852
3501.905881	309738.358793	43.737857
3502.000111	309735.214143	43.742861
3501.819037	309723.638760	43.747866
3501.580192	309705.507138	43.752871
3501.795815	309687.202671	43.757876
3501.778300	309690.386290	43.762881
3501.497718	309685.086364	43.767885
3501.631516	309675.192124	43.772890
3501.290725	309662.980080	43.777895
3501.663590	309658.112374	43.782900
3501.825000	309640.961471	43.787905
3501.395812	309642.453624	43.792909
3501.729752	309641.307237	43.797914
3501.768527	309630.460865	43.802919
3501.548173	309620.698322	43.807924
3501.729726	309601.635745	43.812929
3501.694409	309598.562232	43.817933
3501.852628	309598.257614	43.822938
3502.189997	309578.916200	43.827943
3501.733638	309566.722198	43.832948
3502.097278	309557.631748	43.837953
3501.735761	309549.367177	43.842957
3501.283270	309525.950494	43.847962
3501.561903	309522.039042	43.852967
3501.399220	309512.929080	43.857972
3501.631043	309517.167945	43.862977
3501.578292	309526.286206	43.867981
3501.644300	309515.919042	43.872986
3501.906065	309489.057135	43.877991
3501.521771	309494.079391	43.882996
3501.787153	309483.528369	43.888001
3502.014015	309481.991568	43.893005
3501.411885	309460.455871	43.898010
3501.808950	309448.179310	43.903015
3501.313424	309449.783628	43.908020
3501.403494	309429.666515	43.913025
3501.459406	309441.236155	43.918029
3501.466443	309445.026678	43.923034
3501.730028	309437.198747	43.928039
3501.452737	309430.549591	43.933044
3501.522261	309404.430205	43.938049
3501.499221	309402.092722	43.943053
3501.421602	309399.025810	43.948058
3501.680052	309390.129902	43.953063
3501.720634	309394.856722	43.958068
3501.461042	309368.508854	43.963073
3501.447793	309364.032294	43.968077
3501.609292	309356.296650	43.973082
3501.691438	309352.899394	43.978087
3501.336303	309358.909537	43.983092
3501.844320	309341.017273	43.988097
3501.692235	309345.596090	43.993101
3501.499053	309343.412438	43.998106
3501.669561	309317.658923	44.003111
3501.578403	309322.482687	44.008116
3501.538568	309318.850029	44.013121
3501.864724	309314.956577	44.018125
3501.751939	309300.240438	44.023130
3501.685913	309287.069250	44.028135
3501.521951	309282.259987	44.033140
3501.676104	309275.263441	44.038145
3501.624808	309266.644959	44.043149
3501.542917	309253.807053	44.048154
3501.862460	309248.311468	44.053159
3501.376776	309238.081389	44.058164
3501.774120	309234.838424	44.063169
3501.384337	309233.398020	44.068173
3501.239333	309222.071348	44.073178
3501.626196	309202.289446	44.078183
3501.301214	309204.681414	44.083188
3501.552531	309198.712996	44.088193
3501.669872	309198.185743	44.093197
3501.397036	309195.709173	44.098202
3501.724667	309188.863623	44.103207
3501.704624	309178.789757	44.108212
3501.470006	309168.774882	44.113217
3501.706444	309159.424326	44.118221
3501.860020	309152.707771	44.123226
3501.667266	309145.307395	44.128231
3501.445918	309130.557282	44.133236
3501.527291	309119.984054	44.138241
3501.829088	309115.967159	44.143245
3501.681172	309117.440801	44.148250
3501.879371	309110.437346	44.153255
3501.899911	309103.792476	44.158260
3501.618344	309083.020802	44.163265
3501.692224	309071.736216	44.168269
3501.650051	309083.244935	44.173274
3501.844510	309068.022643	44.178279
3501.776409	309055.513342	44.183284
3501.413802	309031.115377	44.188289
3501.706260	309036.184561	44.193293
3501.495756	309029.397672	44.198298
3501.708356	309024.987561	44.203303
3501.182017	309015.832570	44.208308
3501.842347	308997.687343	44.213313
3501.821727	308994.000763	44.218317
3501.738215	308989.636942	44.223322
3501.803122	308979.727884	44.228327
3501.688566	308971.170133	44.233332
3501.524047	308955.265960	44.238337
3501.550058	308943.785251	44.243341
3501.466571	308948.964113	44.248346
3501.778881	308950.085890	44.253351
3501.892873	308930.092066	44.258356
3501.719629	308922.917630	44.263361
3501.772620	308909.804074	44.268365
3501.761477	308908.966092	44.273370
3501.981945	308893.179841	44.278375
3501.554370	308880.981167	44.283380
3501.711175	308866.935270	44.288385
3501.776406	308873.821301	44.293389
3501.842192	308865.642492	44.298394
3501.993817	308839.280943	44.303399
3501.540003	308837.697854	44.308404
3501.741221	308825.528098	44.313409
3501.780216	308824.707723	44.318413
3501.817867	308811.749223	44.323418
3502.069650	308797.001382	44.328423
3501.732435	308781.124151	44.333428
3501.753499	308780.408367	44.338433
3501.901556	308762.928428	44.343437
3501.472809	308759.178400	44.348442
3501.729600	308739.645671	44.353447
3501.595526	308744.832463	44.358452
3501.541651	308723.058042	44.363457
3501.636387	308711.922796	44.368461
3501.580137	308708.852499	44.373466
3501.848339	308697.893709	44.378471
3501.435231	308701.241029	44.383476
3501.478128	308688.256229	44.388481
3501.902313	308674.066686	44.393485
3501.722586	308672.008137	44.398490
3501.909033	308657.982994	44.403495
3501.661067	308661.584419	44.408500
3501.933114	308649.912492	44.413505
3502.171502	308627.939652	44.418509
3501.847115	308628.270320	44.423514
3502.011462	308617.454985	44.428519
3501.877374	308599.993651	44.433524
3501.896076	308585.689343	44.438529
3501.926518	308575.811039	44.443533
3501.321865	308554.962413	44.448538
3501.975863	308544.248643	44.453543
3501.716892	308538.461711	44.458548
3501.884930	308533.345995	44.463553
3501.679437	308525.260436	44.468557
3501.498079	308509.893146	44.473562
3501.551541	308495.837852	44.478567
3501.768009	308502.878422	44.483572
3501.477641	308500.582690	44.488577
3501.887599	308495.658175	44.493581
3501.449799	308479.491202	44.498586
3501.835804	308463.169985	44.503591
3501.696992	308463.878800	44.508596
3501.831369	308454.569513	44.513601
3501.819765	308434.595122	44.518605
3501.244682	308427.865147	44.523610
3501.622852	308408.898602	44.528615
3501.519391	308422.630986	44.533620
3501.479321	308411.618537	44.538625
3501.571922	308411.731330	44.543629
3501.318961	308404.391149	44.548634
3501.186536	308388.838038	44.553639
3501.691192	308383.771470	44.558644
3501.433555	308377.933416	44.563649
3501.414623	308379.590495	44.568653
3501.477126	308377.977565	44.573658
3501.498793	308370.823471	44.578663
3501.884670	308373.944111	44.583668
3501.285156	308364.622305	44.588673
3501.760194	308355.997717	44.593677
3501.503856	308351.050119	44.598682
3501.721294	308343.941756	44.603687
3501.636317	308335.531955	44.608692
3501.623696	308334.159796	44.613697
3501.680786	308316.337655	44.618701
3501.652199	308309.394988	44.623706
3501.702995	308298.928153	44.628711
3501.608323	308303.803461	44.633716
3501.643664	308293.720754	44.638721
3501.837308	308280.126985	44.643725
3501.763461	308267.771066	44.648730
3502.075542	308259.757232	44.653735
3501.346246	308262.314245	44.658740
3501.574109	308238.714234	44.663745
3501.680012	308216.583789	44.668749
3501.083623	308221.944705	44.673754
3501.749703	308211.483449	44.678759
3501.443145	308211.913122	44.683764
3501.830051	308205.999728	44.688769
3501.721336	308204.947960	44.693773
3501.451808	308182.774404	44.698778
3501.701913	308172.250935	44.703783
3501.570976	308179.015046	44.708788
3501.827106	308173.885521	44.713793
3501.740873	308172.346733	44.718797
3501.441712	308145.775362	44.723802
3501.407702	308129.621489	44.728807
3501.539998	308132.323732	44.733812
3501.772910	308130.022516	44.738817
3501.430068	308121.042249	44.743821
3501.628122	308132.640873	44.748826
3501.404523	308103.207534	44.753831
3501.517621	308106.803447	44.758836
3501.398143	308092.393361	44.763841
3501.414949	308075.773468	44.768845
3501.318967	308086.756433	44.773850
3501.340328	308086.320517	44.778855
3501.160641	308078.078164	44.783860
3501.459244	308083.935363	44.788865
3501.838247	308080.746085	44.793869
3501.489492	308059.170155	44.798874
3501.915326	308046.914195	44.803879
3502.046572	308049.972874	44.808884
3501.835971	308044.254664	44.813889
3501.682952	308023.666024	44.818893
3501.283294	308019.300646	44.823898
3501.581981	308007.548059	44.828903
3501.556396	308006.814110	44.833908
3501.603994	308001.869854	44.838913
3501.816300	307994.558663	44.843917
3501.530518	307990.938910	44.848922
3501.517160	307971.855273	44.853927
3501.232304	307975.106248	44.858932
3501.440358	307972.808911	44.863937
3501.461729	307974.968656	44.868941
3501.352994	307972.211891	44.873946
3501.498823	307968.779136	44.878951
3501.427446	307974.159789	44.883956
3501.285145	307942.601487	44.888961
3501.559505	307938.512443	44.893965
3501.562760	307939.402636	44.898970
3501.560899	307927.849704	44.903975
3501.426283	307928.888690	44.908980
3501.493363	307936.436204	44.913985
3501.513897	307921.953283	44.918989
3500.921907	307933.344648	44.923994
3501.094968	307930.391139	44.928999
3501.441920	307934.612144	44.934004
3501.529324	307918.082952	44.939009
3501.578613	307896.673750	44.944013
3501.435460	307899.088249	44.949018
3501.549265	307889.934758	44.954023
3501.672433	307887.345315	44.959028
3501.644558	307885.084858	44.964033
3501.525329	307875.407946	44.969037
3501.253934	307854.354235	44.974042
3501.309282	307846.991216	44.979047
3501.411871	307846.313569	44.984052
3501.811060	307848.974103	44.989057
3501.603760	307854.096094	44.994061
3501.182702	307851.540837	44.999066
3501.397928	307846.239538	45.004071
3501.171032	307852.178921	45.009076
3501.182153	307844.313862	45.014081
3501.455723	307838.316352	45.019085
3501.487627	307818.538491	45.024090
3501.400660	307809.747194	45.029095
3501.387442	307813.057503	45.034100
3501.279311	307813.456157	45.039105
3501.486559	307798.816771	45.044109
3501.409138	307816.286076	45.049114
3501.947556	307796.021854	45.054119
3501.752072	307782.743262	45.059124
3501.581836	307773.914081	45.064129
3501.625813	307764.873274	45.069133
3501.524905	307759.545047	45.074138
3501.644222	307769.018452	45.079143
3501.554882	307753.636539	45.084148
3501.656556	307735.603635	45.089153
3501.505866	307729.545201	45.094157
3501.052223	307718.902628	45.099162
3501.471742	307712.296985	45.104167
3501.472743	307723.799273	45.109172
3501.120996	307716.932493	45.114177
3501.569560	307715.030156	45.119181
3501.062273	307722.718393	45.124186
3501.415910	307717.929846	45.129191
3501.106768	307716.553132	45.134196
3501.334441	307716.008615	45.139201
3501.226260	307710.401594	45.144205
3501.573831	307699.430174	45.149210
3501.612387	307688.150792	45.154215
3501.784471	307684.535778	45.159220
3501.334470	307677.073605	45.164225
3501.534462	307666.481519	45.169229
3501.817541	307680.713532	45.174234
3501.833819	307653.812655	45.179239
3501.523330	307642.918654	45.184244
3501.406848	307639.959499	45.189249
3501.948275	307634.607180	45.194253
3501.818979	307628.494494	45.199258
3502.097228	307608.779827	45.204263
3501.810066	307600.070686	45.209268
3501.755993	307596.134753	45.214273
3501.842070	307571.793153	45.219277
3501.628988	307571.037615	45.224282
3501.495743	307558.868939	45.229287
3501.314720	307562.892592	45.234292
3501.329311	307556.808297	45.239297
3502.083648	307546.002281	45.244301
3501.624067	307542.002500	45.249306
3501.420936	307524.831504	45.254311
3501.593787	307520.554713	45.259316
3501.528222	307523.033444	45.264321
3501.620212	307514.773971	45.269325
3501.393704	307518.193989	45.274330
3501.269680	307502.410253	45.279335
3501.348359	307488.503417	45.284340
3501.465114	307479.552972	45.289345
3501.637430	307476.345074	45.294349
3501.491498	307486.063585	45.299354
3501.410081	307473.148795	45.304359
3501.802932	307475.403173	45.309364
3501.522411	307469.110525	45.314369
3501.442146	307442.555449	45.319373
3501.228265	307440.782115	45.324378
3501.468838	307436.240249	45.329383
3501.596759	307435.482293	45.334388
3501.162288	307433.590757	45.339393
3501.989589	307427.735660	45.344397
3501.332661	307430.332297	45.349402
3501.393121	307431.060868	45.354407
3501.418574	307408.484576	45.359412
3501.351677	307395.313017	45.364417
3501.463206	307391.580208	45.369421
3501.131055	307396.976245	45.374426
3501.453399	307383.260317	45.379431
3501.034306	307390.731234	45.384436
3501.250020	307392.300765	45.389441
3501.310279	307390.815394	45.394445
3501.055889	307391.567742	45.399450
3501.339578	307385.390460	45.404455
3501.349787	307383.709330	45.409460
3501.471392	307391.222954	45.414465
3501.434734	307376.876055	45.419469
3500.948530	307392.984330	45.424474
3501.088026	307387.389447	45.429479
3501.257715	307391.180148	45.434484
3500.993241	307381.576743	45.439489
3501.390299	307384.135843	45.444493
3501.468500	307388.627943	45.449498
3501.244172	307359.779579	45.454503
3501.372800	307349.758439	45.459508
3501.712357	307361.793186	45.464513
3501.868898	307349.146538	45.469517
3501.409175	307348.047835	45.474522
3501.435191	307344.404736	45.479527
3501.354943	307341.363555	45.484532
3501.614730	307346.361678	45.489537
3501.398170	307319.420676	45.494541
3501.467030	307319.918904	45.499546
3501.620912	307316.077677	45.504551
3501.571937	307316.772463	45.509556
3501.321034	307310.551509	45.514561
3501.496399	307306.477890	45.519565
3501.222540	307304.306759	45.524570
3501.454508	307287.322139	45.529575
3501.576450	307282.824254	45.534580
3501.323199	307283.042016	45.539585
3501.644601	307261.615446	45.544589
3501.384549	307273.693061	45.549594
3501.138355	307274.622264	45.554599
3501.335306	307270.112651	45.559604
3501.281883	307268.365121	45.564609
3501.632472	307258.334710	45.569613
3501.340356	307274.361784	45.574618
3501.475540	307239.018789	45.579623
3501.498287	307232.322426	45.584628
3501.320194	307240.951746	45.589633
3501.550218	307225.239812	45.594637
3501.237744	307237.503767	45.599642
3501.300076	307228.383649	45.604647
3501.423750	307227.397320	45.609652
3501.547151	307225.214975	45.614657
3501.635767	307216.726948	45.619661
3501.295225	307202.274818	45.624666
3501.551471	307184.701062	45.629671
3501.149768	307191.405846	45.634676
3501.418600	307194.010451	45.639681
3501.625591	307188.608578	45.644685
3501.437645	307193.396786	45.649690
3501.819141	307188.705625	45.654695
3501.691851	307174.220148	45.659700
3501.244029	307156.298389	45.664705
3501.404498	307157.596636	45.669709
3501.306415	307156.212357	45.674714
3501.467763	307155.754548	45.679719
3501.640914	307152.622842	45.684724
3501.352937	307151.649973	45.689729
3501.318945	307139.821951	45.694733
3501.394515	307140.853542	45.699738
3501.803207	307130.610436	45.704743
3501.671343	307113.937119	45.709748
3501.722424	307101.154207	45.714753
3501.905777	307099.420550	45.719757
3501.604309	307095.777735	45.724762
3501.442112	307079.592663	45.729767
3501.637159	307064.064283	45.734772
3501.567748	307067.256186	45.739777
3501.507694	307062.201426	45.744781
3501.261549	307065.649993	45.749786
3501.610184	307076.970842	45.754791
3501.333481	307072.637053	45.759796
3501.115749	307050.658477	45.764801
3501.608568	307027.398189	45.769805
3501.703915	307034.228872	45.774810
3501.498578	307017.108942	45.779815
3501.586566	306954.060057	45.784820
3501.424022	306863.566157	45.789825
3501.538720	306714.828461	45.794829
3501.427906	306524.364736	45.799834
3501.129629	306287.587819	45.804839
3500.687337	305991.740475	45.809844
3500.339057	305658.746826	45.814849
3500.482543	305278.008059	45.819853
3499.887364	304857.986491	45.824858
3499.712214	304374.093956	45.829863
3499.408183	303849.701028	45.834868
3498.695115	303275.637397	45.839873
3498.492533	302659.112856	45.844877
3497.948968	301991.987623	45.849882
3497.254741	301265.144093	45.854887
3496.828258	300516.487947	45.859892
3495.763528	299715.261630	45.864897
3495.188407	298849.654993	45.869901
3494.735538	297960.192148	45.874906
3493.584158	297015.744213	45.879911
3493.098299	296029.203884	45.884916
3492.176635	294991.628924	45.889921
3491.504717	293910.673261	45.894925
3490.455189	292780.909208	45.899930
3489.355359	291600.908598	45.904935
3488.568265	290371.884948	45.909940
3487.564703	289102.293668	45.914945
3486.590843	287791.636108	45.919949
3485.302332	286431.868716	45.924954
3483.820911	285026.305018	45.929959
3482.818808	283575.143238	45.934964
3481.451136	282101.731911	45.939969
3480.318718	280559.843917	45.944973
3478.772994	278987.436267	45.949978
3477.525242	277369.349594	45.954983
3476.138269	275712.346682	45.959988
3474.437179	274021.800495	45.964993
3473.048396	272274.339818	45.969997
3471.682941	270502.065118	45.975002
3470.250680	268680.342029	45.980007
3468.377816	266827.841460	45.985012
3466.640969	264928.328777	45.990017
3464.662175	263003.583382	45.995021
3462.882173	261040.549556	46.000026
3460.943600	259039.868696	46.005031
3459.024142	257000.163362	46.010036
3457.265680	254936.716769	46.015041
3455.533392	252837.556238	46.020045
3453.157850	250691.938162	46.025050
3451.537228	248516.936744	46.030055
3449.281618	246319.952543	46.035060
3446.802997	244073.035555	46.040065
3444.679020	241810.886144	46.045069
3442.231759	239520.649259	46.050074
3439.841430	237186.400716	46.055079
3437.639624	234838.735514	46.060084
3434.880166	232455.793572	46.065089
3433.025126	230037.221739	46.070093
3430.241380	227616.801478	46.075098
3427.349104	225152.078432	46.080103
3425.135026	222679.583112	46.085108
3422.368244	220159.398023	46.090113
3419.769081	217636.214557	46.095117
3416.903142	215079.287406	46.100122
3414.126834	212506.240672	46.105127
3411.373056	209904.839084	46.110132
3408.298202	207295.541346	46.115137
3405.648362	204646.935527	46.120141
3402.481074	201992.741009	46.125146
3399.437827	199303.295136	46.130151
3396.313414	196608.152157	46.135156
3392.898686	193895.100710	46.140161
3389.652843	191174.770451	46.145165
3386.346708	188449.723635	46.150170
3382.889598	185693.929819	46.155175
3379.124656	182939.657840	46.160180
3375.346062	180187.656042	46.165185
3372.231208	177410.248094	46.170189
3368.423976	174649.740909	46.175194
3364.614290	171867.368727	46.180199
3360.831318	169074.502153	46.185204
3356.955900	166277.696386	46.190209
3353.371609	163493.966364	46.195213
3348.924765	160706.987836	46.200218
3344.748679	157922.444007	46.205223
3340.476526	155137.775460	46.210228
3335.841153	152361.097759	46.215233
3331.212384	149598.541855	46.220237
3325.990448	146864.023935	46.225242
3321.015306	144137.194434	46.230247
3316.052001	141437.573718	46.235252
3310.842868	138656.803325	46.240257
3305.497492	135997.345599	46.245261
3299.697989	133372.041367	46.250266
3293.657839	130789.505825	46.255271
3287.908971	128238.039225	46.260276
3281.258826	125739.003940	46.265281
3274.823024	123283.863985	46.270285
3267.508938	120881.535602	46.275290
3260.159803	118538.633424	46.280295
3252.845312	116266.418100	46.285300
3245.208557	114061.184600	46.290305
3237.151463	111935.424688	46.295309
3228.974692	109892.169271	46.300314
3220.104678	107937.140621	46.305319
3211.769565	106065.875147	46.310324
3202.786613	104298.363443	46.315329
3194.154213	102610.626605	46.320333
3185.098329	101038.567649	46.325338
3176.254818	99541.412437	46.330343
3167.716659	98158.574220	46.335348
3158.643025	96870.001400	46.340353
3149.976654	95679.881958	46.345357
3141.606705	94589.594972	46.350362
3133.891413	93575.336582	46.355367
3126.814678	92640.431383	46.360372
3119.494523	91784.743423	46.365377
3112.290383	90995.173150	46.370381
3105.904303	90291.198694	46.375386
3100.228048	89624.612113	46.380391
3094.914839	89017.979622	46.385396
3089.511005	88463.237105	46.390401
3084.146802	87937.415758	46.395405
3078.971958	87475.149861	46.400410
3074.365901	87033.600026	46.405415
3070.043297	86610.878856	46.410420
3065.529937	86224.464806	46.415425
3061.367326	85852.750698	46.420429
3057.467605	85516.559100	46.425434
3053.710047	85184.147659	46.430439
3050.364768	84849.414274	46.435444
3046.776321	84547.892182	46.440449
3043.295889	84240.118893	46.445453
3039.815399	83939.539057	46.450458
3036.529460	83650.123569	46.455463
3033.540785	83355.189442	46.460468
3029.995641	83059.862663	46.465473
3026.683611	82769.888530	46.470477
3023.340748	82495.584731	46.475482
3020.230566	82194.419133	46.480487
3017.004065	81905.926656	46.485492
3013.891510	81627.098544	46.490497
3010.381192	81334.997982	46.495501
3007.018475	81049.622213	46.500506
3003.747214	80764.095315	46.505511
3000.537420	80468.806651	46.510516
2996.787854	80193.839429	46.515521
2993.755019	79905.781746	46.520525
2990.271365	79610.621185	46.525530
2986.671583	79321.718290	46.530535
2983.348187	79035.886983	46.535540
2979.776354	78740.901868	46.540545
2976.579723	78450.484377	46.545549
2972.507060	78169.503961	46.550554
2969.150337	77889.049484	46.555559
2965.921544	77604.158054	46.560564
2961.808020	77329.669914	46.565569
2958.096865	77047.996714	46.570573
2954.745836	76782.716861	46.575578
2950.728908	76509.390274	46.580583
2947.391048	76238.881221	46.585588
2943.554770	75977.558587	46.590593
2939.577538	75719.181448	46.595597
2936.445269	75458.680795	46.600602
2932.578646	75203.682073	46.605607
2929.114907	74949.905389	46.610612
2925.185872	74707.849062	46.615617
2921.666547	74458.555836	46.620621
2918.153769	74214.546687	46.625626
2914.977221	73960.670935	46.630631
2911.542505	73722.470151	46.635636
2907.364306	73480.400387	46.640641
2903.762391	73236.071246	46.645645
2900.207621	73001.895716	46.650650
2896.455866	72768.883206	46.655655
2893.308407	72537.479795	46.660660
2889.367819	72313.808607	46.665665
2885.933539	72078.200203	46.670669
2882.194802	71851.834780	46.675674
2878.253043	71636.143787	46.680679
2874.804494	71412.060452	46.685684
2871.166828	71196.909595	46.690689
2867.912445	70978.475403	46.695693
2864.480234	70761.175513	46.700698
2860.986367	70550.832465	46.705703
2857.517481	70328.018604	46.710708
2854.123930	70117.180867	46.715713
2850.457662	69899.124840	46.720717
2846.965759	69677.507303	46.725722
2843.354365	69475.107792	46.730727
2839.959532	69251.656726	46.735732
2836.168138	69042.756332	46.740737
2833.282497	68831.855941	46.745741
2829.983452	68616.171935	46.750746
2826.249879	68395.409380	46.755751
2822.796411	68180.299107	46.760756
2819.322931	67967.961487	46.765761
2815.744606	67749.052855	46.770765
2812.191919	67538.952950	46.775770
2808.546172	67317.843130	46.780775
2805.291344	67097.937289	46.785780
2801.735410	66887.741674	46.790785
2798.384048	66675.173502	46.795789
2794.845184	66459.748260	46.800794
2791.191925	66239.505886	46.805799
2787.633425	66018.419076	46.810804
2784.133760	65816.195988	46.815809
2780.442713	65597.190158	46.820813
2777.383926	65390.966118	46.825818
2774.119936	65168.653706	46.830823
2770.666394	64954.573539	46.835828
2766.915290	64733.667720	46.840833
2763.392264	64522.401205	46.845837
2760.054892	64303.084714	46.850842
2756.643042	64087.755026	46.855847
2753.369337	63855.129124	46.860852
2749.970858	63644.555033	46.865857
2746.118548	63422.673776	46.870861
2742.642518	63200.653130	46.875866
2739.132852	62986.084457	46.880871
2735.830798	62750.782252	46.885876
2732.205786	62535.213691	46.890881
2728.929775	62313.195064	46.895885
2725.215773	62081.282893	46.900890
2721.675494	61859.049460	46.905895
2717.960004	61633.849927	46.910900
2714.484235	61419.213354	46.915905
2710.806807	61200.662796	46.920909
2707.703393	60978.946472	46.925914
2704.259951	60754.721474	46.930919
2700.580783	60534.806332	46.935924
2696.910769	60314.955191	46.940929
2693.605745	60083.486512	46.945933
2690.187730	59871.411873	46.950938
2686.207796	59648.226464	46.955943
2683.216424	59419.418368	46.960948
2679.748659	59203.848070	46.965953
2676.665105	58978.098164	46.970957
2672.822525	58750.800168	46.975962
2669.345142	58520.953360	46.980967
2666.133685	58292.551994	46.985972
2662.371989	58082.761310	46.990977
2659.098077	57847.501758	46.995981
2655.658581	57625.709876	47.000986
2652.008098	57387.512355	47.005991
2648.614869	57161.123518	47.010996
2645.034555	56927.843483	47.016001
2641.699865	56702.693466	47.021005
2638.155903	56463.809517	47.026010
2634.688828	56237.973930	47.031015
2631.533778	55997.701355	47.036020
2627.720692	55772.152713	47.041025
2624.094907	55531.577771	47.046029
2620.525014	55308.704715	47.051034
2616.945063	55080.029931	47.056039
2613.486177	54838.541298	47.061044
2610.057678	54614.529647	47.066049
2606.364800	54379.420519	47.071053
2602.917272	54149.433385	47.076058
2599.612115	53916.951913	47.081063
2596.286352	53679.781163	47.086068
2592.469773	53451.254318	47.091073
2589.076092	53219.079077	47.096077
2585.697118	52981.911003	47.101082
2581.858073	52746.631695	47.106087
2578.251693	52504.473183	47.111092
2575.037056	52293.131848	47.116097
2571.640643	52055.722134	47.121101
2567.914737	51821.233781	47.126106
2564.567932	51591.604897	47.131111
2561.112430	51350.348275	47.136116
2557.403101	51121.281898	47.141121
2553.797864	50882.483170	47.146125
2550.744068	50652.259517	47.151130
2547.062891	50421.076939	47.156135
2543.830521	50179.366260	47.161140
2539.997189	49959.414495	47.166145
2536.505136	49703.147149	47.171149
2533.228010	49474.486219	47.176154
2529.503534	49233.344534	47.181159
2526.211263	49006.130525	47.186164
2522.771467	48758.637978	47.191169
2519.231641	48528.226178	47.196173
2515.733369	48289.456676	47.201178
2512.158483	48059.124869	47.206183
2508.224101	47814.694688	47.211188
2504.968641	47584.837816	47.216193
2501.486510	47345.517539	47.221197
2498.015782	47112.578573	47.226202
2494.184182	46877.878170	47.231207
2491.454600	46631.813509	47.236212
2487.743523	46388.841549	47.241217
2484.438206	46156.114887	47.246221
2480.974338	45909.177232	47.251226
2477.203685	45664.281700	47.256231
2473.612197	45423.407034	47.261236
2470.128291	45189.589428	47.266241
2466.453883	44949.107006	47.271245
2463.050609	44708.692567	47.276250
2459.489297	44472.598816	47.281255
2456.281695	44221.473125	47.286260
2452.745565	43989.039716	47.291265
2449.071586	43750.504344	47.296269
2445.551190	43512.879707	47.301274
2441.968066	43281.995689	47.306279
2438.986209	43027.531598	47.311284
2435.127655	42787.830594	47.316289
2431.852627	42553.507044	47.321293
2428.474681	42313.051157	47.326298
2424.454509	42070.859441	47.331303
2421.159806	41821.156935	47.336308
2417.301716	41585.115023	47.341313
2413.742611	41350.132192	47.346317
2410.557457	41108.917428	47.351322
2406.791280	40864.213694	47.356327
2403.764053	40619.587320	47.361332
2400.496917	40383.079139	47.366337
2396.859291	40131.851702	47.371341
2393.531648	39889.968887	47.376346
2389.848522	39642.406321	47.381351
2386.278425	39391.791883	47.386356
2383.191991	39153.468150	47.391361
2379.686239	38904.478721	47.396365
2375.948233	38645.783762	47.401370
2372.558871	38391.025231	47.406375
2368.970563	38148.403791	47.411380
2365.413463	37899.421303	47.416385
2362.231731	37650.306896	47.421389
2358.879251	37394.654127	47.426394
2354.825444	37141.447110	47.431399
2351.722992	36885.412615	47.436404
2347.848435	36631.651061	47.441409
2344.318048	36387.221033	47.446413
2341.299847	36134.681712	47.451418
2337.413226	35888.544449	47.456423
2333.969822	35634.378650	47.461428
2330.562326	35389.142110	47.466433
2327.103662	35134.521920	47.471437
2323.920157	34875.874521	47.476442
2320.271171	34619.382262	47.481447
2316.980381	34355.331906	47.486452
2313.095731	34104.898308	47.491457
2309.623244	33849.059702	47.496461
2306.553926	33580.186026	47.501466
2302.652856	33333.960316	47.506471
2299.585263	33063.153396	47.511476
2296.027777	32810.053586	47.516481
2292.235044	32533.928634	47.521485
2288.855970	32283.120756	47.526490
2285.429589	32022.163279	47.531495
2282.208193	31769.999555	47.536500
2278.724366	31501.084327	47.541505
2275.265200	31236.275665	47.546509
2271.496898	30974.053864	47.551514
2267.937809	30703.500232	47.556519
2264.867003	30429.369027	47.561524
2261.415429	30171.094215	47.566529
2257.651453	29888.180700	47.571533
2254.150665	29628.488108	47.576538
2250.935113	29360.458625	47.581543
2247.620385	29084.197080	47.586548
2243.933260	28815.361269	47.591553
2240.130905	28539.246719	47.596557
2237.084191	28256.363851	47.601562
2233.831239	27997.400883	47.606567
2230.307965	27713.769947	47.611572
2226.585348	27444.209969	47.616577
2223.175373	27162.565044	47.621581
2219.796922	26878.213382	47.626586
2216.182691	26612.367024	47.631591
2212.586103	26330.427001	47.636596
2209.129784	26051.846197	47.641601
2205.793353	25765.818114	47.646605
2202.751089	25476.839785	47.651610
2199.165291	25201.972238	47.656615
2195.435835	24907.413508	47.661620
2191.985443	24634.477658	47.666625
2188.445183	24346.898649	47.671629
2185.200240	24057.934401	47.676634
2181.250629	23765.416279	47.681639
2177.964715	23479.799298	47.686644
2174.362902	23188.052493	47.691649
2170.986301	22897.788857	47.696653
2167.607044	22617.716870	47.701658
2163.798303	22330.899446	47.706663
2160.670196	22035.174002	47.711668
2156.952735	21744.942533	47.716673
2153.376055	21464.341245	47.721677
2149.941796	21166.250443	47.726682
2146.215657	20885.554071	47.731687
2142.776162	20599.920237	47.736692
2138.828363	20323.675412	47.741697
2134.485770	20052.018990	47.746701
2130.911028	19777.452772	47.751706
2126.588515	19540.037189	47.756711
2121.861037	19305.544550	47.761716
2116.787330	19082.573563	47.766721
2112.539278	18878.712298	47.771725
2108.820850	18674.934987	47.776730
2104.918499	18480.613388	47.781735
2100.894200	18289.156694	47.786740
2097.412110	18106.313292	47.791745
2093.600194	17928.571173	47.796749
2090.402231	17735.831589	47.801754
2086.648453	17573.702370	47.806759
2083.545325	17399.337681	47.811764
2080.007059	17219.044862	47.816769
2076.532874	17047.958802	47.821773
2073.533591	16860.174923	47.826778
2069.997504	16687.999743	47.831783
2066.379123	16506.066809	47.836788
2062.946913	16341.981839	47.841793
2059.410494	16152.661282	47.846797
2056.397601	15983.953923	47.851802
2053.320496	15804.802315	47.856807
2049.644624	15622.006470	47.861812
2046.401438	15427.618837	47.866817
2042.567650	15253.134624	47.871821
2039.966045	15070.096802	47.876826
2035.812958	14877.370664	47.881831
2032.561530	14691.262306	47.886836
2029.278605	14509.818297	47.891841
2025.604430	14328.839349	47.896845
2022.292349	14138.414447	47.901850
2018.771309	13953.967090	47.906855
2015.363879	13754.936244	47.911860
2011.916410	13572.912687	47.916865
2008.161970	13388.203402	47.921869
2004.669413	13190.569052	47.926874
2001.003652	13013.574747	47.931879
1997.647740	12828.966865	47.936884
1994.582235	12652.233447	47.941889
1990.709373	12451.418043	47.946893
1987.485673	12253.735593	47.951898
1983.762387	12066.058411	47.956903
1980.322006	11877.873454	47.961908
1977.090845	11695.017366	47.966913
1973.612464	11501.710336	47.971917
1970.347267	11308.387766	47.976922
1966.648452	11118.709134	47.981927
1963.176094	10930.165126	47.986932
1959.733819	10727.008820	47.991937
1955.965608	10536.754968	47.996941
1952.540023	10343.306013	48.001946
1948.997010	10152.049007	48.006951
1945.779351	9957.052052	48.011956
1942.362442	9763.044294	48.016961
1938.921825	9562.052940	48.021965
1935.539198	9371.969057	48.026970
1931.471029	9171.659395	48.031975
1928.350537	8985.371736	48.036980
1924.746913	8782.518275	48.041985
1921.378624	8595.823829	48.046989
1918.488119	8389.846554	48.051994
1914.653209	8198.285006	48.056999
1911.175238	7990.340382	48.062004
1907.351751	7790.488488	48.067009
1903.905844	7596.970053	48.072013
1900.089072	7397.811362	48.077018
1896.754199	7192.705083	48.082023
1893.364566	7009.853402	48.087028
1890.298207	6804.744245	48.092033
1886.447718	6608.229487	48.097037
1882.952959	6401.979692	48.102042
1879.128752	6202.926905	48.107047
1875.631888	6002.875605	48.112052
1872.334776	5805.684708	48.117057
1868.655314	5607.764576	48.122061
1865.537474	5409.939094	48.127066
1861.696076	5218.260921	48.132071
1858.209794	5011.503311	48.137076
1855.172111	4815.874346	48.142081
1851.556393	4622.575315	48.147085
1848.042826	4410.202137	48.152090
1843.855563	4213.382963	48.157095
1840.713341	4007.158882	48.162100
1837.295151	3823.232860	48.167105
1833.586526	3625.266092	48.172109
1830.648857	3417.178180	48.177114
1827.001075	3221.446705	48.182119
1823.503969	3021.133975	48.187124
1820.317242	2821.550150	48.192129
1816.486393	2623.069239	48.197133
1813.056239	2408.130810	48.202138
1808.732967	2210.247282	48.207143
1805.348565	2006.115362	48.212148
1802.010278	1806.288071	48.217153
1798.489040	1621.400788	48.222157
1795.008804	1421.650623	48.227162
1791.109229	1230.602901	48.232167
1788.081939	1027.935470	48.237172
1784.455621	842.297507	48.242177
1780.514851	648.889495	48.247181
1776.535688	461.092817	48.252186
1772.982697	289.174048	48.257191
1769.307151	96.632223	48.262196
1765.027912	-58.154535	48.267201
1752.284320	24.323570	48.272205
1744.327728	34.525515	48.277210
1739.123355	45.343970	48.282215
1736.251570	44.572206	48.287220
1734.454521	40.389349	48.292225
1732.283266	39.935068	48.297229
1729.873948	35.465213	48.302234
1726.659412	34.108005	48.307239
1723.325353	41.099794	48.312244
1720.485001	41.863888	48.317249
1717.052529	40.591410	48.322253
1714.031480	36.432435	48.327258
1710.378208	40.047787	48.332263
1706.851342	37.312591	48.337268
1703.609503	30.771030	48.342273
1699.645552	45.049561	48.347277
1696.360001	35.407988	48.352282
1693.322672	38.484017	48.357287
1689.860292	38.295086	48.362292
1686.330181	40.154244	48.367297
1682.555749	44.649123	48.372301
1679.377647	34.544645	48.377306
1676.616234	39.377699	48.382311
1672.507913	42.257512	48.387316
1669.313267	37.034208	48.392321
1665.235474	37.046006	48.397325
1661.591284	39.770925	48.402330
1658.660377	43.165671	48.407335
1655.287682	41.042288	48.412340
1651.997018	32.667055	48.417345
1648.490707	47.408660	48.422349
1645.520290	32.987906	48.427354
1641.754852	35.668531	48.432359
1637.832604	35.437694	48.437364
1634.336997	36.595433	48.442369
1631.188172	38.110193	48.447373
1627.650827	39.160569	48.452378
1623.882365	44.220853	48.457383
1620.738265	37.467867	48.462388
1617.396519	38.187073	48.467393
1613.677672	38.993775	48.472397
1610.340710	32.100136	48.477402
1606.864095	36.807857	48.482407
1603.053463	32.370695	48.487412
1599.858548	34.152109	48.492417
1596.087414	40.820028	48.497421
1593.148932	34.873279	48.502426
1589.578365	39.314132	48.507431
1585.648218	42.609023	48.512436
1582.233816	32.993993	48.517441
1578.643662	50.640448	48.522445
1575.334434	36.057611	48.527450
1571.684000	34.575686	48.532455
1568.595041	34.011971	48.537460
1565.411697	40.062711	48.542465
1561.519314	43.462433	48.547469
1558.364852	39.903364	48.552474
1554.468526	38.067620	48.557479
1551.023780	47.854596	48.562484
1547.944930	40.648491	48.567489
1544.319974	37.112448	48.572493
1540.876326	31.225802	48.577498
1537.185804	36.435266	48.582503
1533.341524	31.057425	48.587508
1529.900847	35.139440	48.592513
1526.293801	33.986104	48.597517
1523.262876	32.274353	48.602522
1519.643399	40.671301	48.607527
1516.145572	40.775883	48.612532
1512.521033	34.936543	48.617537
1509.062117	41.223422	48.622541
1505.997244	37.973056	48.627546
1502.466871	47.941128	48.632551
1498.922534	35.445266	48.637556
1495.305688	31.664362	48.642561
1491.562377	34.433325	48.647565
1487.906498	33.860293	48.652570
1484.328953	31.300794	48.657575
1481.384025	39.282118	48.662580
1478.155073	28.302985	48.667585
1474.163794	35.087656	48.672589
1470.775389	32.005005	48.677594
1467.106674	41.010796	48.682599
1463.682182	47.747889	48.687604
1460.340612	32.493117	48.692609
1456.620336	45.284554	48.697613
1453.660560	33.687483	48.702618
1449.657258	35.687226	48.707623
1446.114371	33.340617	48.712628
1442.815669	26.583428	48.717633
1439.260700	33.964213	48.722637
1435.668581	20.384362	48.727642
1432.383318	32.402179	48.732647
1428.886492	36.932781	48.737652
1425.419669	31.207999	48.742657
1421.775158	35.720591	48.747661
1418.369293	18.368828	48.752666
1414.637815	30.488132	48.757671
1411.402614	34.544348	48.762676
1407.866970	29.823776	48.767681
1404.150368	38.033476	48.772685
1400.767467	31.871619	48.777690
1397.305525	28.556894	48.782695
1393.304230	32.631791	48.787700
1390.400001	28.710906	48.792705
1386.816000	32.113038	48.797709
1383.664915	32.350053	48.802714
1379.898976	30.949557	48.807719
1376.398184	42.184872	48.812724
1372.708178	34.587278	48.817729
1368.898881	29.700747	48.822733
1365.750890	34.227385	48.827738
1362.372070	38.432648	48.832743
1358.774559	32.301237	48.837748
1355.711886	33.467231	48.842753
1351.562385	46.961808	48.847757
1348.510079	38.394356	48.852762
1345.122207	31.075350	48.857767
1341.573908	41.451233	48.862772
1338.170248	27.114250	48.867777
1334.034540	41.774107	48.872781
1330.697842	27.923361	48.877786
1327.284918	35.066806	48.882791
1323.752307	31.510067	48.887796
1320.411060	27.094462	48.892801
1316.613536	36.417855	48.897805
1313.471794	34.802612	48.902810
1309.739576	35.839310	48.907815
1306.526397	36.266406	48.912820
1303.203164	28.737981	48.917825
1299.226124	31.983367	48.922829
1295.967540	26.080506	48.927834
1292.181640	39.806081	48.932839
1288.623955	40.173216	48.937844
1285.510924	33.323744	48.942849
1281.430293	42.606046	48.947853
1278.358020	31.225977	48.952858
1274.905150	31.174907	48.957863
1271.245212	30.083730	48.962868
1267.880566	29.775241	48.967873
1263.984123	39.231196	48.972877
1260.876244	34.045079	48.977882
1257.583852	39.635240	48.982887
1253.942903	32.669104	48.987892
1250.613036	31.934392	48.992897
1246.857184	39.856054	48.997901
1243.194326	33.541929	49.002906
1239.370307	23.279322	49.007911
1236.139684	34.516668	49.012916
1232.949849	31.975664	49.017921
1229.203056	31.486564	49.022925
1225.925380	34.109960	49.027930
1222.471077	33.964220	49.032935
1218.973345	35.862759	49.037940
1215.210497	31.785279	49.042945
1211.422201	36.061020	49.047949
1208.158668	37.271158	49.052954
1205.056506	32.707434	49.057959
1201.570713	32.449570	49.062964
1197.666320	32.760283	49.067969
1194.002365	33.004882	49.072973
1191.251112	27.130206	49.077978
1187.846498	33.541555	49.082983
1183.859030	31.552551	49.087988
1180.595957	31.437000	49.092993
1176.875066	35.392149	49.097997
1173.433355	32.425521	49.103002
1169.441173	37.846848	49.108007
1166.199437	33.020248	49.113012
1163.149704	24.452472	49.118017
1159.174273	32.120629	49.123021
1155.881468	35.372846	49.128026
1151.886269	32.866205	49.133031
1148.222207	33.259536	49.138036
1145.215059	23.242414	49.143041
1141.460265	35.106016	49.148045
1138.333598	27.727220	49.153050
1135.304615	32.371333	49.158055
1131.006796	37.758266	49.163060
1127.733074	31.772415	49.168065
1124.330132	39.559769	49.173069
1120.607084	34.384592	49.178074
1117.093990	32.172651	49.183079
1113.343778	40.656626	49.188084
1110.659354	35.179639	49.193089
1106.787723	38.111200	49.198093
1103.315083	43.805557	49.203098
1100.233239	33.278117	49.208103
1096.430743	31.911931	49.213108
1092.713531	25.574746	49.218113
1088.728736	38.800000	49.223117
1085.597290	30.551931	49.228122
1082.377606	39.031948	49.233127
1078.524237	34.528932	49.238132
1075.772164	27.841330	49.243137
1072.026793	36.795961	49.248141
1068.211922	25.054517	49.253146
1064.615785	34.802041	49.258151
1061.050267	35.135683	49.263156
1057.680581	43.708797	49.268161
1053.959238	44.911569	49.273165
1050.451321	39.838781	49.278170
1047.297247	38.836168	49.283175
1044.146420	40.487463	49.288180
1040.445009	31.616799	49.293185
1036.166686	46.852739	49.298189
1032.933282	34.384346	49.303194
1029.291672	41.146065	49.308199
1026.160112	47.467258	49.313204
1022.911131	41.926829	49.318209
1019.274557	42.853747	49.323213
1016.108918	40.979752	49.328218
1012.465945	39.015978	49.333223
1008.683216	41.914675	49.338228
1005.193061	38.645645	49.343233
1001.385230	39.052050	49.348237
997.955322	40.003567	49.353242
994.920808	34.948431	49.358247
991.178744	40.295861	49.363252
987.941784	30.362238	49.368257
983.932391	28.886122	49.373261
980.587792	32.500846	49.378266
977.173165	31.592838	49.383271
973.425233	37.279717	49.388276
970.098188	27.236821	49.393281
966.404176	37.303422	49.398285
963.063200	35.978923	49.403290
960.052624	31.897661	49.408295
956.313319	42.499711	49.413300
952.869281	36.654490	49.418305
949.030552	31.092538	49.423309
945.390517	30.855756	49.428314
941.991223	26.313342	49.433319
938.400553	40.403918	49.438324
934.851210	28.798134	49.443329
931.353497	40.203927	49.448333
928.372273	35.200583	49.453338
925.265551	33.741342	49.458343
921.060472	37.402233	49.463348
917.588665	34.067091	49.468353
913.647568	40.015193	49.473357
910.423290	36.929198	49.478362
907.212102	34.888366	49.483367
903.552083	33.094986	49.488372
900.732954	24.991081	49.493377
896.690339	32.328162	49.498381
892.961730	32.940507	49.503386
889.719496	28.987293	49.508391
885.888853	25.603948	49.513396
882.540090	25.755019	49.518401
879.059793	32.561128	49.523405
875.441430	21.225615	49.528410
871.936366	26.165811	49.533415
868.450909	27.306406	49.538420
865.171245	27.136614	49.543425
861.521901	30.925645	49.548429
857.974298	33.208608	49.553434
854.702070	20.230690	49.558439
850.942493	29.263542	49.563444
847.434137	21.422609	49.568449
843.869964	34.968050	49.573453
840.699530	35.322167	49.578458
837.004808	19.740187	49.583463
833.312561	32.910213	49.588468
830.551791	28.840501	49.593473
826.559855	31.895412	49.598477
822.758626	33.208858	49.603482
819.331525	32.521163	49.608487
815.897429	37.766644	49.613492
812.481212	22.862405	49.618497
808.869155	27.578929	49.623501
805.309196	37.947293	49.628506
802.249790	33.025841	49.633511
798.374550	40.020373	49.638516
795.041892	32.844812	49.643521
791.568085	33.594467	49.648525
788.354425	24.407100	49.653530
784.774983	23.278199	49.658535
781.392118	27.920877	49.663540
777.764989	29.925255	49.668545
773.663979	35.357443	49.673549
770.077260	35.115544	49.678554
767.051237	30.112948	49.683559
763.133779	40.755609	49.688564
759.768379	27.978982	49.693569
756.538870	34.530720	49.698573
753.085173	38.130965	49.703578
749.797436	34.248205	49.708583
745.837384	41.939414	49.713588
743.019729	36.217656	49.718593
738.849021	43.767849	49.723597
734.959330	29.880593	49.728602
732.126660	32.994447	49.733607
728.032259	23.005389	49.738612
725.183323	27.453740	49.743617
721.278937	29.729349	49.748621
717.511444	21.786685	49.753626
714.082817	38.961929	49.758631
710.769404	31.391082	49.763636
707.906598	24.512142	49.768641
704.088945	26.875416	49.773645
700.500056	26.393437	49.778650
697.043304	33.110495	49.783655
693.317445	31.188305	49.788660
689.971699	25.122162	49.793665
686.497953	27.279724	49.798669
682.879026	21.509468	49.803674
679.420423	25.445864	49.808679
675.955850	27.042006	49.813684
672.344535	24.921554	49.818689
668.978520	38.176581	49.823693
665.520492	25.325921	49.828698
661.705370	33.506991	49.833703
657.972058	31.699880	49.838708
655.289710	25.279919	49.843713
651.548338	29.947147	49.848717
647.598008	39.959077	49.853722
644.428174	34.634196	49.858727
641.063721	32.386508	49.863732
637.319233	21.469499	49.868737
633.603053	25.224786	49.873741
630.437669	29.074149	49.878746
627.013711	23.156324	49.883751
623.280418	38.743633	49.888756
620.113919	32.042000	49.893761
616.205943	40.057295	49.898765
612.688680	29.538144	49.903770
609.472640	30.060834	49.908775
605.410666	39.818178	49.913780
602.507297	28.791598	49.918785
598.573998	29.910682	49.923789
595.227881	30.592955	49.928794
591.591281	24.619861	49.933799
588.163729	29.389825	49.938804
585.015998	27.538490	49.943809
581.130107	30.377574	49.948813
577.651802	29.147494	49.953818
574.037198	28.394345	49.958823
570.815362	25.225839	49.963828
567.435167	26.679091	49.968833
563.542409	19.448986	49.973837
560.029883	26.908814	49.978842
556.906714	25.822439	49.983847
553.330410	27.005852	49.988852
550.018784	32.216420	49.993857
546.259809	38.484149	49.998861
542.781501	35.055263	50.003866
539.496376	27.578137	50.008871
535.809743	35.650542	50.013876
532.053403	29.886053	50.018881
528.584039	25.399076	50.023885
525.232493	33.517078	50.028890
522.017556	23.520101	50.033895
518.278339	30.866751	50.038900
514.975714	22.693187	50.043905
511.122975	22.999257	50.048909
507.079036	33.174590	50.053914
503.891114	23.657446	50.058919
500.430535	32.023487	50.063924
497.226637	28.469383	50.068929
493.931020	31.045207	50.073933
490.422495	37.283221	50.078938
486.817147	33.466130	50.083943
483.052391	44.047004	50.088948
479.557148	21.960902	50.093953
476.143744	30.259449	50.098957
472.850260	18.753028	50.103962
469.329597	21.886129	50.108967
465.378280	28.718687	50.113972
462.135222	24.958760	50.118977
458.206882	29.721784	50.123981
455.280561	28.367329	50.128986
451.941880	25.068474	50.133991
447.810527	29.553251	50.138996
445.146865	24.566787	50.144001
441.293321	34.380127	50.149005
437.558693	30.254276	50.154010
434.039011	20.668906	50.159015
430.520413	30.945477	50.164020
427.311251	24.747319	50.169025
423.646473	27.244948	50.174029
419.827767	30.706327	50.179034
416.849541	24.383415	50.184039
413.085680	40.798151	50.189044
409.752703	26.887150	50.194049
405.953569	35.328398	50.199053
402.353272	26.454859	50.204058
399.170416	27.823478	50.209063
395.397440	30.730372	50.214068
392.163641	25.586457	50.219073
388.599899	29.548915	50.224077
385.317979	36.507608	50.229082
381.695702	29.637019	50.234087
377.889896	37.914808	50.239092
374.621190	25.888853	50.244097
371.229768	33.158931	50.249101
367.859048	33.487636	50.254106
364.306739	29.209874	50.259111
360.480544	32.153593	50.264116
356.814761	38.308716	50.269121
353.308429	37.560843	50.274125
349.951928	34.967174	50.279130
346.264379	26.243371	50.284135
343.062054	25.884481	50.289140
340.077923	33.286924	50.294145
336.504161	36.871320	50.299149
332.487049	37.943535	50.304154
328.953003	34.697476	50.309159
324.901580	39.679153	50.314164
321.773185	38.517749	50.319169
318.235170	36.515675	50.324173
315.233133	35.426229	50.329178
311.792572	41.970034	50.334183
308.019822	38.793013	50.339188
304.705053	27.897442	50.344193
301.113087	37.859682	50.349197
297.604743	36.061777	50.354202
294.327437	37.926120	50.359207
290.530702	38.122272	50.364212
286.841911	32.420083	50.369217
282.984970	33.384971	50.374221
279.519909	37.502855	50.379226
276.715569	35.265646	50.384231
272.887920	38.336179	50.389236
269.659988	32.606097	50.394241
265.748615	32.845527	50.399245
262.257525	37.290199	50.404250
259.059673	33.754223	50.409255
254.871604	33.910452	50.414260
252.104773	30.734067	50.419265
248.916503	37.757226	50.424269
244.943394	37.243871	50.429274
241.608032	28.075804	50.434279
237.985047	43.418154	50.439284
234.956464	28.614831	50.444289
231.157826	28.504421	50.449293
226.926373	27.189986	50.454298
224.132463	33.069367	50.459303
220.447883	34.124340	50.464308
217.040216	35.499767	50.469313
213.194756	34.292548	50.474317
209.774963	38.729233	50.479322
206.397101	35.990271	50.484327
202.573466	34.447442	50.489332
199.127754	34.693047	50.494337
195.885229	30.797099	50.499341
192.556157	30.040504	50.504346
189.392035	21.820077	50.509351
185.286409	34.017340	50.514356
182.128034	25.906745	50.519361
178.469633	27.451180	50.524365
174.437115	30.063466	50.529370
171.360091	22.999991	50.534375
167.306928	36.748775	50.539380
164.509797	27.417331	50.544385
161.202072	35.006560	50.549389
157.490364	29.244748	50.554394
153.970374	33.637037	50.559399
150.612681	36.890260	50.564404
146.956381	24.706837	50.569409
143.295391	23.970625	50.574413
139.686288	36.017352	50.579418
136.492914	28.861386	50.584423
132.575215	29.978227	50.589428
129.102934	34.404180	50.594433
125.823068	25.860226	50.599437
122.364405	28.161166	50.604442
119.201427	26.170024	50.609447
114.890261	32.046694	50.614452
111.770291	34.104752	50.619457
108.248435	32.748806	50.624461
104.597403	21.067620	50.629466
101.497064	27.710049	50.634471
97.800211	28.188028	50.639476
94.579198	19.609561	50.644481
91.212475	26.056445	50.649485
87.140039	26.197803	50.654490
83.908409	26.564936	50.659495
80.296715	40.652712	50.664500
76.800201	34.556665	50.669505
73.298169	30.837466	50.674509
69.682852	30.707897	50.679514
66.034009	13.755580	50.684519
62.507848	28.253894	50.689524
59.434863	16.472679	50.694529
55.711421	19.669341	50.699533
52.438028	27.041251	50.704538
48.988846	25.227855	50.709543
45.312980	23.250660	50.714548
41.564188	23.477373	50.719553
38.104223	24.762985	50.724557
34.686208	25.200467	50.729562
31.285861	14.634818	50.734567
27.711336	30.067700	50.739572
24.347702	24.317857	50.744577
20.735702	23.893560	50.749581
16.961070	18.910470	50.754586
13.627140	17.550430	50.759591
9.835007	16.781039	50.764596
6.652306	21.727974	50.769601
3.398118	23.209148	50.774605