Thu Aug 25 10:13:48 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.163501	111.304780	0.000000
1.087433	104.774124	0.005005
0.832688	102.147076	0.010010
0.612809	101.552027	0.015014
1.122033	97.460679	0.020019
0.731894	103.855748	0.025024
0.525604	83.795114	0.030029
0.512185	71.281478	0.035034
0.361968	68.672858	0.040038
-0.139089	51.635540	0.045043
-0.519499	49.287617	0.050048
-1.216336	33.097240	0.055053
-0.826887	37.630075	0.060058
-1.326491	32.045330	0.065062
-1.577829	26.896250	0.070067
-1.877888	27.079394	0.075072
-2.044262	13.732389	0.080077
-2.406431	2.757243	0.085082
-2.778930	4.305820	0.090086
-3.249838	-6.180886	0.095091
-3.445170	-2.951647	0.100096
-3.338316	-7.957523	0.105101
-3.671107	-19.418148	0.110106
-4.390601	-17.903789	0.115110
-4.444004	-24.776468	0.120115
-4.790619	-5.157493	0.125120
-5.061138	-10.920486	0.130125
-4.758995	-8.727808	0.135130
-5.816827	-7.413536	0.140134
-5.778071	-9.890402	0.145139
-6.584033	-15.569499	0.150144
-6.459001	-8.524364	0.155149
-6.514197	-11.809083	0.160154
-6.520699	-10.520332	0.165158
-6.894668	-13.729794	0.170163
-7.529385	-8.669507	0.175168
-7.753633	-15.072497	0.180173
-8.051531	-13.409060	0.185178
-8.330691	-10.448262	0.190182
-7.897446	-7.643377	0.195187
-8.254131	-10.713179	0.200192
-9.228508	-7.909204	0.205197
-8.982841	-2.233887	0.210202
-9.503998	-0.655691	0.215206
-9.318698	-5.335338	0.220211
-9.558237	-15.639991	0.225216
-10.358066	-9.990688	0.230221
-10.748638	-9.752233	0.235226
-11.077890	-7.916205	0.240230
-10.690507	-2.933806	0.245235
-10.908304	-9.809207	0.250240
-10.900725	-4.767299	0.255245
-11.111857	-11.048959	0.260250
-12.104267	-4.496288	0.265254
-12.102348	-14.051001	0.270259
-12.473640	-6.741440	0.275264
-12.597430	-12.919726	0.280269
-12.739223	-6.225088	0.285274
-13.568282	-13.415998	0.290278
-13.560942	-11.537796	0.295283
-13.707742	-3.396543	0.300288
-13.854847	-6.423253	0.305293
-13.678387	-11.639350	0.310298
-14.078705	0.179931	0.315302
-14.707341	-6.659571	0.320307
-14.763398	-13.788101	0.325312
-14.966145	-1.917521	0.330317
-15.085912	-8.213497	0.335322
-15.853575	-4.090993	0.340326
-16.271001	-9.024213	0.345331
-16.614182	2.055293	0.350336
-16.588248	-5.196818	0.355341
-16.501864	-3.761270	0.360346
-16.389503	1.409753	0.365350
-16.311648	-5.157633	0.370355
-17.341564	-8.571201	0.375360
-17.632821	-2.808593	0.380365
-17.872403	-13.647912	0.385370
-18.035738	-1.989150	0.390374
-18.289155	-6.147641	0.395379
-18.792001	-4.727337	0.400384
-19.422464	-8.953300	0.405389
-19.291908	-14.472250	0.410394
-19.581935	-3.239726	0.415398
-19.460172	-2.524727	0.420403
-19.643723	-7.190873	0.425408
-19.750369	-7.164583	0.430413
-20.233438	-15.520176	0.435418
-20.703193	2.833622	0.440422
-20.837479	-5.260251	0.445427
-20.979157	-0.068407	0.450432
-20.926471	-5.992773	0.455437
-21.530858	-6.666774	0.460442
-21.958994	-1.078871	0.465446
-21.924803	-3.640444	0.470451
-22.279445	-2.604028	0.475456
-22.707516	-5.067861	0.480461
-23.560741	-12.245492	0.485466
-23.751778	-1.287904	0.490470
-23.414317	-3.605930	0.495475
-23.677668	0.336318	0.500480
-23.845518	-3.380002	0.505485
-23.712865	-9.244130	0.510490
-23.868323	-0.905367	0.515494
-24.381146	-9.487254	0.520499
-24.963785	-0.091306	0.525504
-25.585969	0.154966	0.530509
-25.607355	4.011846	0.535514
-25.489382	-3.336944	0.540518
-25.407056	-11.357186	0.545523
-25.936017	-4.788545	0.550528
-26.587563	-2.784958	0.555533
-26.676162	-12.287524	0.560538
-26.837952	0.367575	0.565542
-27.034195	-13.382849	0.570547
-27.878419	-3.183455	0.575552
-28.443436	2.261382	0.580557
-27.450938	-12.434600	0.585562
-28.008576	-9.756033	0.590566
-28.376987	-12.858797	0.595571
-28.368743	-4.650089	0.600576
-28.566965	-12.082209	0.605581
-29.292976	-16.622227	0.610586
-29.550952	-13.775479	0.615590
-30.164207	-17.649796	0.620595
-29.717495	-5.466530	0.625600
-29.737914	-9.114200	0.630605
-29.397039	-10.141954	0.635610
-30.629352	-0.134849	0.640614
-30.817807	-13.816891	0.645619
-31.109253	-6.352162	0.650624
-32.017783	-12.287267	0.655629
-32.082548	-10.983060	0.660634
-31.941474	2.494615	0.665638
-32.641538	-9.794313	0.670643
-32.772253	-11.732099	0.675648
-32.869783	3.057949	0.680653
-32.627675	-9.910113	0.685658
-33.045978	-6.161886	0.690662
-32.634118	-7.817692	0.695667
-33.484065	-0.901364	0.700672
-33.778763	-7.483141	0.705677
-33.801058	-9.089903	0.710682
-34.411930	-7.636853	0.715686
-34.622759	-14.472213	0.720691
-35.280722	-6.212904	0.725696
-35.608394	-6.594906	0.730701
-35.469597	-10.628189	0.735706
-35.716733	-1.816320	0.740710
-35.604363	-12.748748	0.745715
-35.873535	-15.120417	0.750720
-36.441590	-3.768401	0.755725
-36.865489	-2.730624	0.760730
-37.564383	0.238996	0.765734
-37.047717	-5.659992	0.770739
-37.230089	-5.153603	0.775744
-37.486661	-0.595488	0.780749
-37.737766	-5.257376	0.785754
-38.482456	-2.353346	0.790758
-38.673303	-6.736775	0.795763
-38.941079	-14.891982	0.800768
-39.287043	-3.520982	0.805773
-38.459659	-8.494222	0.810778
-38.596211	2.106818	0.815782
-39.444840	-7.482305	0.820787
-39.891607	-5.029916	0.825792
-40.293820	-3.660179	0.830797
-40.287167	-5.549887	0.835802
-40.908316	-6.202278	0.840806
-40.991503	-8.739131	0.845811
-41.256044	-1.297599	0.850816
-41.632014	4.772513	0.855821
-41.330851	0.672658	0.860826
-41.469797	1.501272	0.865830
-42.133799	-4.456329	0.870835
-42.373992	-14.653308	0.875840
-42.793146	0.690166	0.880845
-42.705456	-13.788113	0.885850
-43.028343	-1.870236	0.890854
-43.680618	-7.712615	0.895859
-44.032293	-2.250588	0.900864
-44.191100	-5.171060	0.905869
-44.133537	-4.585207	0.910874
-44.590127	0.402880	0.915878
-44.206585	-3.988291	0.920883
-44.610800	-4.807550	0.925888
-45.664839	-3.357827	0.930893
-45.773398	-5.903359	0.935898
-45.782556	-5.082426	0.940902
-45.976049	-6.731966	0.945907
-46.037543	1.531963	0.950912
-46.128316	-0.605070	0.955917
-46.547191	-2.507197	0.960922
-47.501879	-0.358034	0.965926
-47.505437	-2.812452	0.970931
-47.634068	-8.471125	0.975936
-47.725320	-9.649468	0.980941
-47.212423	-15.560518	0.985946
-47.993796	-9.031422	0.990950
-48.539789	-1.896965	0.995955
-48.879020	-8.240809	1.000960
-49.007750	-5.132738	1.005965
-48.958296	-5.035994	1.010970
-48.925802	1.568062	1.015974
-49.441068	-5.418914	1.020979
-49.835087	-4.335198	1.025984
-50.468256	3.695604	1.030989
-50.420257	-10.001340	1.035994
-50.648651	4.195446	1.040998
-51.110027	-1.344653	1.046003
-51.754757	0.692669	1.051008
-52.302252	0.142632	1.056013
-51.912210	-4.002786	1.061018
-51.978844	3.838007	1.066022
-51.792561	-0.534912	1.071027
-51.940056	-1.223554	1.076032
-52.500509	2.300177	1.081037
-52.567582	-6.114271	1.086042
-53.235441	0.431843	1.091046
-53.369760	2.730874	1.096051
-53.574735	-0.565178	1.101056
-54.043575	0.701104	1.106061
-54.233418	-8.231942	1.111066
-55.058078	-1.158224	1.116070
-54.801506	-4.134290	1.121075
-55.124685	1.127122	1.126080
-55.242165	5.941853	1.131085
-55.047711	1.067782	1.136090
-55.789539	5.236863	1.141094
-56.481303	5.649063	1.146099
-56.557941	-6.117453	1.151104
-56.968817	6.864577	1.156109
-56.498008	0.064777	1.161114
-56.627950	2.394759	1.166118
-56.605624	1.707981	1.171123
-57.117243	0.959335	1.176128
-57.895247	-3.022045	1.181133
-57.947431	-2.450633	1.186138
-58.349593	1.677879	1.191142
-58.127698	-1.764151	1.196147
-58.918149	-2.045166	1.201152
-59.222586	0.650678	1.206157
-59.458487	-9.948770	1.211162
-59.508936	-1.281615	1.216166
-59.494368	-2.941610	1.221171
-59.733580	-11.629637	1.226176
-59.931559	4.286621	1.231181
-60.464989	-5.927688	1.236186
-60.603393	-11.081793	1.241190
-60.721117	-7.269933	1.246195
-60.920126	-6.849521	1.251200
-61.671433	-4.877757	1.256205
-61.881068	-9.542976	1.261210
-62.553429	-1.423778	1.266214
-62.495660	-6.399815	1.271219
-62.207181	0.455193	1.276224
-62.283250	3.188020	1.281229
-62.611092	-3.401217	1.286234
-63.505142	-0.306104	1.291238
-63.312598	-10.371573	1.296243
-63.689829	-7.474500	1.301248
-63.827078	-3.795620	1.306253
-63.703464	-7.696811	1.311258
-64.190414	-11.062572	1.316262
-65.106412	-0.889894	1.321267
-64.633079	-2.713522	1.326272
-65.629755	-2.490825	1.331277
-65.327838	-1.535137	1.336282
-66.055790	0.015354	1.341286
-66.577401	-2.968491	1.346291
-66.191284	-4.674049	1.351296
-66.677782	5.200380	1.356301
-66.608404	0.988147	1.361306
-66.979588	-2.841842	1.366310
-66.945129	-9.595412	1.371315
-67.724209	-7.919852	1.376320
-68.050491	-7.115667	1.381325
-67.927569	-6.426161	1.386330
-68.342433	-8.759183	1.391334
-68.273635	-5.175864	1.396339
-68.250021	-6.941679	1.401344
-68.869351	-5.053869	1.406349
-69.523308	-3.072048	1.411354
-69.796060	3.095783	1.416358
-69.805859	-3.793223	1.421363
-69.896104	-4.823028	1.426368
-69.768635	-2.950995	1.431373
-70.881117	1.102158	1.436378
-71.173993	-9.649712	1.441382
-71.211984	-11.760212	1.446387
-71.132191	-20.317887	1.451392
-71.561371	1.285033	1.456397
-71.274017	-9.124321	1.461402
-71.581060	-0.106914	1.466406
-72.366638	0.471847	1.471411
-72.500973	-5.521288	1.476416
-73.153035	-0.667087	1.481421
-72.846833	-10.876914	1.486426
-72.839639	-5.284458	1.491430
-73.493058	-12.275091	1.496435
-74.058104	-10.572956	1.501440
-74.547097	-7.658371	1.506445
-74.084976	-12.371900	1.511450
-74.278617	-8.098893	1.516454
-74.671831	-12.377843	1.521459
-74.807242	-19.854598	1.526464
-75.349241	-10.278364	1.531469
-75.581672	-12.146427	1.536474
-75.692352	-12.556100	1.541478
-76.070540	-13.262377	1.546483
-75.813493	-11.891537	1.551488
-76.409416	-9.232279	1.556493
-76.866697	-13.842873	1.561498
-76.569555	-0.804112	1.566502
-76.967000	-11.384571	1.571507
-77.555293	-8.134889	1.576512
-78.441824	-9.875149	1.581517
-78.389824	-9.959138	1.586522
-78.428497	-7.491599	1.591526
-78.391332	-4.029874	1.596531
-78.753958	-9.085569	1.601536
-78.869067	-13.050592	1.606541
-78.786677	-18.030484	1.611546
-79.781615	-6.146512	1.616550
-80.105696	-8.632963	1.621555
-79.772704	-12.918135	1.626560
-80.397405	-2.569641	1.631565
-80.157419	-18.261342	1.636570
-81.133452	-3.918942	1.641574
-81.583359	-9.979686	1.646579
-81.553512	-14.150919	1.651584
-81.872920	-5.207507	1.656589
-81.470945	-9.357958	1.661594
-81.786574	-11.826749	1.666598
-81.804563	-13.684121	1.671603
-82.348136	-4.560052	1.676608
-82.920696	-4.049469	1.681613
-83.182397	-12.664368	1.686618
-83.210890	-9.783975	1.691622
-83.418652	-9.368518	1.696627
-83.736274	-16.838869	1.701632
-84.514913	-7.557747	1.706637
-84.670456	-10.728663	1.711642
-84.703360	-16.582664	1.716646
-84.969996	-7.615885	1.721651
-84.785123	-6.018602	1.726656
-84.828068	-5.068989	1.731661
-85.354042	-8.428633	1.736666
-85.960585	-6.523844	1.741670
-86.280787	-17.818752	1.746675
-86.045369	-16.039566	1.751680
-86.507346	-13.138705	1.756685
-86.487513	-4.991929	1.761690
-87.135638	-11.556284	1.766694
-87.826555	-7.471112	1.771699
-87.529530	-11.576644	1.776704
-87.902510	-12.375485	1.781709
-87.713903	-10.544670	1.786714
-87.746302	-7.989530	1.791718
-88.371476	-1.779133	1.796723
-88.723595	-11.110688	1.801728
-88.800808	-4.783674	1.806733
-89.210751	-12.157304	1.811738
-89.610493	-9.525621	1.816742
-90.324831	-9.325015	1.821747
-90.477064	-6.260718	1.826752
-90.596914	-5.868528	1.831757
-90.350734	-16.632092	1.836762
-90.635805	-12.743391	1.841766
-90.605106	-10.486038	1.846771
-91.163428	-5.216257	1.851776
-91.870799	-4.377667	1.856781
-91.648758	-4.548412	1.861786
-91.997448	-11.517189	1.866790
-92.284509	-3.429891	1.871795
-92.271791	-14.669400	1.876800
-93.268631	-5.265501	1.881805
-93.503222	-11.119537	1.886810
-93.822051	-4.365524	1.891814
-93.500916	-5.965988	1.896819
-93.750677	-8.669726	1.901824
-93.638903	-3.273991	1.906829
-93.547522	-11.687951	1.911834
-94.456584	-11.896593	1.916838
-95.192760	-6.307880	1.921843
-95.026524	-5.995319	1.926848
-94.917238	9.085022	1.931853
-95.187395	-8.491434	1.936858
-95.820108	-7.923969	1.941862
-96.419245	-8.987928	1.946867
-96.186083	-6.148534	1.951872
-96.511563	-8.992267	1.956877
-96.730936	-12.517011	1.961882
-96.946889	-10.676588	1.966886
-97.788051	-14.549988	1.971891
-97.857742	-13.412688	1.976896
-98.084842	-7.688609	1.981901
-97.666442	-13.496269	1.986906
-98.059700	-8.812335	1.991910
-98.272670	-12.720894	1.996915
-99.278341	-9.243435	2.006912
-98.337030	-9.536474	2.016909
-98.208086	-7.263020	2.026906
-97.456073	-13.003507	2.036902
-96.921264	-4.828700	2.046899
-96.884819	-1.061392	2.056896
-96.240291	-6.091292	2.066893
-95.394478	-12.799982	2.076890
-95.533082	-4.725561	2.086886
-94.208673	-7.989829	2.096883
-94.014787	-5.894444	2.106880
-94.015084	-3.245946	2.116877
-93.154061	-9.269609	2.126874
-92.594738	-5.080555	2.136870
-91.660676	-9.674318	2.146867
-91.197563	-9.429928	2.156864
-91.177573	-15.841322	2.166861
-90.837996	-10.775205	2.176858
-90.185638	-9.128627	2.186854
-89.628953	-5.217925	2.196851
-89.193955	-14.548529	2.206848
-88.682365	-13.915761	2.216845
-88.135337	-11.691979	2.226842
-87.567933	-15.059373	2.236838
-87.412618	-14.275745	2.246835
-86.097296	-8.684612	2.256832
-85.781577	-17.629061	2.266829
-85.735224	-13.090367	2.276826
-85.363288	-13.123127	2.286822
-84.521970	-10.318236	2.296819
-84.409395	-11.948103	2.306816
-82.983796	-6.475617	2.316813
-82.798948	-5.148589	2.326810
-82.995688	-7.312863	2.336806
-82.319634	1.023549	2.346803
-81.360322	-5.946847	2.356800
-80.932818	-0.039200	2.366797
-80.002930	-4.534107	2.376794
-80.159885	-3.302407	2.386790
-79.835115	-2.456633	2.396787
-79.048229	-3.726495	2.406784
-78.739336	-3.711362	2.416781
-78.247363	-4.950852	2.426778
-77.460604	3.051435	2.436774
-77.118902	-2.729298	2.446771
-76.151161	-4.423473	2.456768
-76.033887	-1.292885	2.466765
-75.742335	6.400529	2.476762
-74.842089	-2.651357	2.486758
-74.535822	-4.232380	2.496755
-74.479468	0.675381	2.506752
-73.136747	-8.474344	2.516749
-72.950717	-4.347172	2.526746
-72.654145	-1.539283	2.536742
-71.958371	-5.984835	2.546739
-71.527743	-4.138786	2.556736
-71.351456	-3.462981	2.566733
-70.140442	-5.372670	2.576730
-70.172702	-0.976877	2.586726
-69.316131	-1.098244	2.596723
-68.757489	-2.053576	2.606720
-68.682646	-0.243644	2.616717
-68.298747	-0.550708	2.626714
-67.406722	-3.382926	2.636710
-67.108926	-4.506460	2.646707
-66.668528	-5.025115	2.656704
-66.378199	-3.220438	2.666701
-65.438899	-7.529918	2.676698
-65.225819	-5.171445	2.686694
-64.598899	-3.289629	2.696691
-63.532295	-9.611598	2.706688
-63.437809	-13.633481	2.716685
-63.350721	-5.220624	2.726682
-62.253146	-5.927782	2.736678
-62.047633	-6.010490	2.746675
-61.781676	-4.335042	2.756672
-60.563488	1.828851	2.766669
-60.345331	-7.027457	2.776666
-60.391822	-10.194123	2.786662
-59.434099	-8.193079	2.796659
-58.880597	-4.171003	2.806656
-58.647840	0.661602	2.816653
-57.914812	-9.361933	2.826650
-57.406080	-5.633782	2.836646
-57.101070	-4.645528	2.846643
-56.353608	-12.004042	2.856640
-55.779267	-8.688482	2.866637
-55.593741	-10.165055	2.876634
-54.642067	-10.814505	2.886630
-54.393720	-7.561905	2.896627
-54.360960	-9.917362	2.906624
-53.555321	-14.389629	2.916621
-53.162039	-13.674965	2.926618
-52.304669	-6.881167	2.936614
-51.615054	-4.651213	2.946611
-51.526039	-6.084154	2.956608
-51.177050	-10.050882	2.966605
-50.221537	-12.329179	2.976602
-50.272887	-7.927228	2.986598
-49.217570	-4.595163	2.996595
-48.929017	-5.619046	3.006592
-48.617833	-5.373022	3.016589
-48.009718	-11.661163	3.026586
-47.285526	-4.146414	3.036582
-47.029854	-5.447078	3.046579
-46.511891	-4.466848	3.056576
-45.586388	-10.367565	3.066573
-45.367322	-10.499914	3.076570
-45.217248	-7.957339	3.086566
-44.318300	-11.984897	3.096563
-44.138765	-9.393086	3.106560
-43.520582	-10.056805	3.116557
-42.944392	-14.648341	3.126554
-42.638702	-11.113289	3.136550
-41.908889	-13.942261	3.146547
-41.036773	-19.600193	3.156544
-41.040831	-12.646078	3.166541
-40.460255	-16.132741	3.176538
-39.644820	-14.562396	3.186534
-39.620232	-15.148944	3.196531
-39.035657	-19.333148	3.206528
-38.214496	-19.768912	3.216525
-37.805479	-13.576434	3.226522
-37.701778	-15.847972	3.236518
-36.588521	-12.886114	3.246515
-36.430000	-15.001517	3.256512
-36.288234	-18.774217	3.266509
-35.663047	-19.242629	3.276506
-34.763037	-19.297941	3.286502
-33.909111	-8.882815	3.296499
-33.606295	-10.079994	3.306496
-33.711101	-10.931369	3.316493
-32.977916	-16.361626	3.326490
-32.309910	-13.019559	3.336486
-32.182238	-13.688783	3.346483
-31.439818	-9.056412	3.356480
-30.704596	-14.683392	3.366477
-30.744401	-11.293775	3.376474
-30.011560	-12.583674	3.386470
-29.478397	-13.820112	3.396467
-29.111134	-9.005415	3.406464
-28.321257	-9.407766	3.416461
-27.864791	-7.572098	3.426458
-27.267943	-14.571226	3.436454
-26.442656	-7.072315	3.446451
-26.277333	-14.624716	3.456448
-26.259796	-14.190130	3.466445
-25.772752	-13.452143	3.476442
-25.058025	-11.501720	3.486438
-23.865077	-19.801175	3.496435
-23.485928	-15.362140	3.506432
-23.363135	-18.485638	3.516429
-23.162820	-15.380733	3.526426
-22.842556	-12.836314	3.536422
-21.989788	-2.357646	3.546419
-21.239439	-10.929877	3.556416
-20.467870	-9.609247	3.566413
-20.330505	-13.992643	3.576410
-20.113060	-19.190036	3.586406
-19.411951	-11.408742	3.596403
-19.463621	-14.102595	3.606400
-18.405050	-18.228019	3.616397
-18.015567	-15.776809	3.626394
-16.927434	-19.387346	3.636390
-16.489124	-12.927026	3.646387
-16.196357	-14.559784	3.656384
-16.460997	-13.814892	3.666381
-15.152121	-6.797227	3.676378
-14.909925	-12.372300	3.686374
-14.632817	-7.990134	3.696371
-13.594377	-16.623341	3.706368
-13.540049	-11.699423	3.716365
-13.006287	-7.180074	3.726362
-11.979804	-4.964884	3.736358
-12.113475	-3.014576	3.746355
-11.337174	-13.656274	3.756352
-10.454225	-10.461922	3.766349
-10.352389	-11.333004	3.776346
-10.268290	-11.260473	3.786342
-9.530242	-12.297764	3.796339
-8.828950	-15.312333	3.806336
-8.004879	-12.301991	3.816333
-7.600538	-15.716691	3.826330
-7.361271	-19.276587	3.836326
-6.964921	-11.425366	3.846323
-6.584089	-14.361214	3.856320
-5.952266	-19.971991	3.866317
-5.299253	-14.552668	3.876314
-5.106116	-7.993742	3.886310
-4.733333	1.102953	3.896307
-4.093292	9.524218	3.906304
-3.694278	18.065615	3.916301
-3.158856	22.537196	3.926298
-2.755835	33.792776	3.936294
-2.125217	47.347375	3.946291
-1.834038	62.447205	3.956288
-1.065035	74.203002	3.966285
-1.001620	89.272018	3.976282
-0.502821	102.229589	3.986278
0.000000	125.858266	3.991283
0.263790	121.017590	3.996288
0.316173	135.202130	4.001293
0.424301	142.433472	4.006298
0.632823	150.876629	4.011302
0.920516	154.568056	4.016307
0.490664	154.066016	4.021312
0.905790	141.092879	4.026317
0.816714	159.722553	4.031322
0.888414	145.771831	4.036326
1.002097	152.388535	4.041331
0.785212	154.374653	4.046336
0.736832	149.661976	4.051341
0.520349	157.485189	4.056346
0.566670	160.445639	4.061350
1.005492	172.699871	4.066355
1.126522	180.261403	4.071360
1.465893	189.633210	4.076365
1.073366	190.308574	4.081370
1.365149	169.540212	4.086374
0.970723	166.944531	4.091379
0.964230	174.212827	4.096384
1.418385	186.221055	4.101389
1.412611	175.984069	4.106394
1.205722	160.760855	4.111398
1.147475	158.647179	4.116403
0.659075	162.349475	4.121408
1.221670	163.761044	4.126413
1.191408	181.293187	4.131418
1.661305	179.169524	4.136422
1.738709	177.803389	4.141427
1.062950	171.496385	4.146432
1.146589	156.588325	4.151437
0.997601	162.015481	4.156442
1.072219	162.364549	4.161446
1.316118	177.170852	4.166451
1.326901	182.019320	4.171456
1.530438	186.081446	4.176461
1.125039	172.442740	4.181466
1.259240	174.870564	4.186470
1.701531	178.904771	4.191475
1.468165	181.288946	4.196480
1.125125	165.033523	4.201485
0.887410	169.905105	4.206490
1.369909	182.206284	4.211494
1.276767	190.544865	4.216499
1.255427	202.871217	4.221504
1.535331	197.293999	4.226509
1.448674	189.879114	4.231514
1.514449	181.994256	4.236518
1.355576	185.556340	4.241523
1.358477	187.530171	4.246528
1.760886	185.429737	4.251533
1.662936	187.960376	4.256538
1.362446	188.782672	4.261542
1.408959	185.576894	4.266547
1.404765	195.957996	4.271552
1.593704	187.873502	4.276557
1.587610	189.845580	4.281562
1.930182	192.601429	4.286566
1.852340	198.188293	4.291571
1.830171	195.034403	4.296576
1.443247	190.928420	4.301581
1.636412	188.746875	4.306586
1.780976	194.010987	4.311590
1.747672	191.921872	4.316595
1.710931	191.994157	4.321600
1.566697	178.058261	4.326605
1.577399	186.709602	4.331610
1.663402	186.351364	4.336614
1.384999	186.271687	4.341619
1.120899	182.434365	4.346624
1.429725	183.063115	4.351629
1.782096	198.994564	4.356634
1.679494	192.623059	4.361638
1.637912	190.595354	4.366643
1.580731	197.700758	4.371648
1.746713	202.543897	4.376653
2.108546	205.764970	4.381658
1.933052	212.363729	4.386662
2.103334	202.181401	4.391667
1.768467	205.350282	4.396672
1.920186	188.378234	4.401677
1.824031	190.747240	4.406682
1.295936	200.789648	4.411686
2.291867	209.308778	4.416691
2.353410	216.743604	4.421696
1.934484	196.738305	4.426701
1.810206	195.372131	4.431706
2.000702	197.886051	4.436710
1.611761	202.525070	4.441715
1.893947	215.306914	4.446720
2.126010	219.513276	4.451725
2.002482	212.578725	4.456730
2.010399	212.232722	4.461734
1.918658	212.414865	4.466739
2.115495	213.383868	4.471744
1.995719	213.940567	4.476749
2.100372	228.123319	4.481754
2.107188	220.124294	4.486758
2.210401	215.552364	4.491763
1.994581	228.257222	4.496768
2.509918	216.014982	4.501773
1.884935	224.041436	4.506778
2.255730	213.194928	4.511782
2.267033	224.070332	4.516787
2.068564	223.709208	4.521792
2.385983	219.793420	4.526797
2.050035	212.056913	4.531802
1.997504	211.147736	4.536806
2.279264	228.637365	4.541811
2.254096	232.554999	4.546816
2.295160	216.040029	4.551821
2.295210	219.004575	4.556826
2.205446	208.375765	4.561830
2.367153	220.698760	4.566835
2.325442	214.643576	4.571840
2.191157	219.369250	4.576845
2.250042	220.979970	4.581850
2.436718	218.280577	4.586854
2.409901	219.069486	4.591859
2.602619	227.850518	4.596864
2.662417	216.711046	4.601869
2.356840	219.565290	4.606874
2.246902	211.369425	4.611878
2.042520	209.765862	4.616883
2.391754	211.625320	4.621888
2.502601	216.847264	4.626893
2.351171	213.232730	4.631898
2.498411	221.929134	4.636902
2.581147	213.753700	4.641907
2.480565	216.193006	4.646912
2.824575	213.934038	4.651917
2.392929	221.082305	4.656922
2.252769	218.275932	4.661926
2.259545	216.142570	4.666931
2.156471	214.355453	4.671936
2.075548	212.821131	4.676941
2.148082	229.549434	4.681946
2.338195	236.255435	4.686950
2.468926	245.625160	4.691955
2.567942	242.376344	4.696960
2.458195	245.152452	4.701965
2.539061	244.573552	4.706970
2.522195	236.812351	4.711974
2.513657	238.101438	4.716979
2.492286	244.277424	4.721984
2.661434	243.646727	4.726989
2.649772	247.112991	4.731994
2.336134	239.955114	4.736998
2.438006	238.278253	4.742003
2.280205	246.551061	4.747008
2.632152	258.407671	4.752013
2.956768	261.520689	4.757018
2.672568	271.958362	4.762022
3.030074	273.126824	4.767027
2.995213	265.368430	4.772032
2.686570	252.075175	4.777037
2.938780	251.121412	4.782042
2.862779	256.666876	4.787046
2.869247	254.720221	4.792051
2.744243	263.589017	4.797056
3.238803	256.488003	4.802061
3.168061	256.227090	4.807066
2.517341	249.530152	4.812070
2.935513	245.041745	4.817075
2.811414	252.742957	4.822080
2.827105	260.197640	4.827085
2.960064	271.965183	4.832090
2.983572	270.642287	4.837094
3.262629	267.621525	4.842099
3.115355	262.120710	4.847104
2.760681	240.637295	4.852109
2.952849	261.013712	4.857114
3.065074	261.768183	4.862118
3.431371	264.849360	4.867123
2.835950	254.660422	4.872128
3.062789	263.319065	4.877133
3.506411	255.915980	4.882138
2.716674	255.201403	4.887142
2.960786	250.949077	4.892147
3.270917	268.896213	4.897152
3.397351	264.152952	4.902157
2.876888	256.565560	4.907162
2.978671	265.351366	4.912166
3.513414	264.214128	4.917171
3.179186	265.886446	4.922176
3.328740	261.174364	4.927181
3.053189	255.383598	4.932186
3.087269	261.193394	4.937190
3.633277	262.803725	4.942195
2.923524	259.779703	4.947200
3.262319	263.026542	4.952205
3.533930	271.042252	4.957210
3.193101	267.280210	4.962214
3.322146	257.101148	4.967219
3.010760	271.997697	4.972224
3.534192	270.349696	4.977229
3.573146	278.620164	4.982234
3.253648	259.614794	4.987238
3.457128	267.438694	4.992243
3.445115	260.682808	4.997248
3.169506	256.935859	5.002253
3.201061	266.510962	5.007258
3.446547	274.720594	5.012262
3.417027	276.845050	5.017267
3.233156	283.916553	5.022272
3.280890	274.626592	5.027277
3.070835	279.440085	5.032282
3.198461	278.739962	5.037286
3.230622	273.391365	5.042291
3.205212	279.077608	5.047296
3.565144	263.613633	5.052301
3.242671	274.550856	5.057306
3.242552	281.707464	5.062310
3.415343	267.579455	5.067315
3.458907	286.767453	5.072320
3.500561	298.207630	5.077325
3.849044	299.216153	5.082330
3.587803	299.937391	5.087334
3.510142	302.803393	5.092339
3.595084	301.784086	5.097344
3.904350	297.470919	5.102349
3.784208	297.255711	5.107354
3.237515	283.648550	5.112358
3.819836	285.253193	5.117363
3.607107	302.696984	5.122368
4.026319	300.416732	5.127373
3.604770	293.791440	5.132378
3.420408	296.702634	5.137382
3.617928	300.379745	5.142387
3.396588	308.270225	5.147392
3.702228	299.854179	5.152397
3.774973	305.664259	5.157402
3.774927	308.391549	5.162406
3.937679	301.703179	5.167411
3.721401	311.892948	5.172416
3.885993	305.381461	5.177421
3.680725	304.904340	5.182426
3.829723	300.018326	5.187430
4.044453	296.267309	5.192435
3.650143	304.997985	5.197440
3.522336	299.763031	5.202445
3.779938	306.664131	5.207450
3.766584	313.943051	5.212454
3.785569	310.741564	5.217459
4.099240	316.681579	5.222464
3.764546	304.075748	5.227469
3.990932	310.216101	5.232474
3.743644	298.238830	5.237478
4.083316	297.163792	5.242483
3.645901	302.990528	5.247488
3.823474	306.503084	5.252493
4.095164	318.005309	5.257498
4.001147	334.731332	5.262502
4.171220	326.684533	5.267507
3.807526	331.803691	5.272512
3.939100	334.133870	5.277517
4.084628	332.117961	5.282522
3.903994	329.928527	5.287526
4.066368	334.278714	5.292531
3.823618	332.503978	5.297536
4.060023	326.746872	5.302541
4.288241	326.012003	5.307546
4.213188	329.874199	5.312550
3.963427	328.198640	5.317555
4.088713	325.322185	5.322560
4.384106	323.263814	5.327565
4.281331	329.873369	5.332570
4.085128	337.829527	5.337574
4.103548	325.902356	5.342579
3.952518	340.337233	5.347584
3.956235	334.894997	5.352589
4.236019	334.920852	5.357594
3.914434	343.222530	5.362598
3.926350	331.451401	5.367603
3.962726	354.304281	5.372608
4.308582	349.216565	5.377613
4.445907	355.253827	5.382618
4.265956	362.622145	5.387622
4.452384	356.781109	5.392627
4.150576	356.803176	5.397632
4.325755	360.607188	5.402637
4.392783	361.144114	5.407642
4.261892	353.723436	5.412646
4.579606	360.362034	5.417651
4.090365	365.086413	5.422656
4.283496	366.404024	5.427661
4.644825	356.720031	5.432666
4.342472	363.186860	5.437670
4.847487	362.177662	5.442675
4.488523	355.906378	5.447680
4.356480	357.645104	5.452685
4.912399	356.792449	5.457690
4.432165	364.922838	5.462694
4.723731	365.592264	5.467699
4.510574	363.755940	5.472704
4.590652	347.402418	5.477709
4.645613	362.219496	5.482714
4.370394	369.257888	5.487718
4.544775	352.380212	5.492723
4.343282	357.847293	5.497728
4.677179	351.185873	5.502733
4.595427	355.593299	5.507738
4.560949	355.636755	5.512742
4.592592	359.893535	5.517747
4.541748	360.964630	5.522752
4.415155	357.156346	5.527757
4.666168	358.816071	5.532762
4.620436	369.371464	5.537766
4.874300	360.830622	5.542771
4.629584	358.916984	5.547776
4.911286	358.749547	5.552781
4.613824	358.647544	5.557786
4.604659	364.619175	5.562790
4.891476	364.504721	5.567795
4.948784	366.701006	5.572800
4.869088	359.712074	5.577805
4.690609	351.498409	5.582810
4.899608	365.209333	5.587814
4.889894	363.708134	5.592819
5.150895	364.458281	5.597824
5.060184	371.787311	5.602829
4.906116	364.019077	5.607834
4.935845	346.398429	5.612838
4.644003	359.475965	5.617843
4.501385	366.512563	5.622848
5.384656	377.169180	5.627853
5.087257	372.441675	5.632858
5.021377	368.453031	5.637862
4.964185	362.298981	5.642867
4.980777	353.814302	5.647872
5.054780	357.324113	5.652877
5.277935	357.504377	5.657882
4.852864	369.055692	5.662886
4.957482	358.462777	5.667891
4.795725	369.501429	5.672896
5.120979	379.055885	5.677901
5.201108	381.239104	5.682906
5.025154	389.609736	5.687910
5.256490	381.353994	5.692915
5.057626	391.202552	5.697920
5.169979	377.991940	5.702925
4.937430	382.590681	5.707930
4.785279	381.485129	5.712934
5.241980	376.209191	5.717939
4.803106	382.593012	5.722944
5.164290	392.265234	5.727949
5.323856	391.522136	5.732954
5.355022	383.879897	5.737958
5.129993	382.864859	5.742963
5.388036	390.816308	5.747968
5.255258	381.168590	5.752973
5.201833	394.256252	5.757978
4.918454	386.552563	5.762982
5.534664	384.225615	5.767987
5.577474	391.641301	5.772992
5.406601	388.776438	5.777997
5.553482	389.626725	5.783002
4.939513	387.815233	5.788006
4.929063	391.430034	5.793011
5.043976	390.235180	5.798016
5.421948	391.182140	5.803021
5.462971	394.459840	5.808026
5.423182	396.769420	5.813030
5.284022	381.035523	5.818035
5.429744	394.272321	5.823040
5.681710	399.383621	5.828045
5.701084	391.762210	5.833050
5.481899	395.552088	5.838054
5.594169	390.434518	5.843059
5.581717	392.053267	5.848064
5.648452	387.392094	5.853069
5.351214	393.693614	5.858074
5.433646	404.551656	5.863078
5.704235	384.843080	5.868083
5.490279	401.309541	5.873088
5.610952	401.448914	5.878093
5.428363	396.099126	5.883098
5.091878	392.209823	5.888102
5.203431	393.024517	5.893107
5.635455	409.899147	5.898112
5.741576	409.582046	5.903117
5.601503	417.523118	5.908122
5.155923	414.394401	5.913126
6.020031	421.826953	5.918131
5.844081	425.046904	5.923136
5.743075	420.832793	5.928141
5.690536	407.084835	5.933146
5.694921	417.872854	5.938150
5.807815	420.933650	5.943155
5.631947	410.280245	5.948160
5.726012	416.938087	5.953165
5.778670	413.225094	5.958170
5.795343	431.569558	5.963174
6.034775	418.478213	5.968179
5.784395	417.821492	5.973184
5.583893	410.807174	5.978189
5.632772	419.579199	5.983194
5.660311	426.475263	5.988198
5.997733	412.340327	5.993203
5.780059	421.033892	5.998208
5.806124	407.741863	6.003213
5.830372	424.003341	6.008218
5.487277	412.126427	6.013222
6.076106	414.011643	6.018227
5.817246	425.600229	6.023232
5.843454	420.163934	6.028237
5.627625	418.097064	6.033242
5.703151	415.775732	6.038246
5.786197	420.480063	6.043251
5.467464	422.858662	6.048256
5.547781	422.308318	6.053261
5.882120	427.406720	6.058266
5.585422	429.845145	6.063270
5.598777	412.410499	6.068275
6.003390	443.621554	6.073280
5.788573	440.817352	6.078285
5.981129	435.361316	6.083290
5.869608	439.539305	6.088294
5.863509	432.307853	6.093299
5.920461	433.931550	6.098304
5.957099	434.840243	6.103309
5.644318	435.810011	6.108314
5.157945	430.080695	6.113318
5.733478	440.560935	6.118323
6.116896	439.615079	6.123328
6.211119	448.313574	6.128333
6.615408	439.689013	6.133338
5.812610	434.436389	6.138342
5.692101	420.600992	6.143347
5.610351	431.000710	6.148352
5.836408	422.593912	6.153357
6.064128	430.784253	6.158362
5.771110	426.717286	6.163366
6.086151	417.714406	6.168371
5.789451	430.438407	6.173376
5.743738	428.743523	6.178381
5.970115	422.269770	6.183386
5.630858	413.426357	6.188390
5.786874	417.856657	6.193395
5.886709	433.539977	6.198400
5.984696	436.422773	6.203405
6.066766	435.153967	6.208410
5.569919	425.306998	6.213414
5.977391	431.520262	6.218419
5.934630	425.851158	6.223424
6.063418	431.826507	6.228429
6.143208	421.405127	6.233434
5.706082	417.648649	6.238438
6.040119	417.352787	6.243443
5.856379	422.870890	6.248448
5.787714	427.023177	6.253453
6.019198	419.330554	6.258458
5.582645	418.282215	6.263462
5.928731	416.810688	6.268467
5.646246	430.022853	6.273472
5.555586	428.037613	6.278477
5.998600	425.718813	6.283482
5.760734	432.381212	6.288486
5.774805	428.509743	6.293491
5.915633	432.255877	6.298496
5.931105	437.151138	6.303501
6.078175	427.769601	6.308506
5.877793	425.228901	6.313510
5.625686	406.174849	6.318515
5.514772	418.135727	6.323520
5.887873	432.039293	6.328525
6.083184	439.712686	6.333530
5.693580	439.878225	6.338534
5.982485	440.946713	6.343539
5.911927	445.456813	6.348544
5.962763	446.673337	6.353549
5.918064	434.597792	6.358554
5.729981	425.667411	6.363558
5.855314	423.129462	6.368563
6.273654	430.957735	6.373568
5.878821	430.013592	6.378573
5.901152	419.689803	6.383578
5.597176	419.117411	6.388582
5.686732	415.085419	6.393587
5.790788	427.895327	6.398592
5.855648	438.765634	6.403597
6.214226	434.375104	6.408602
5.993927	423.038940	6.413606
6.104100	411.619366	6.418611
5.736123	429.369185	6.423616
5.658534	421.164992	6.428621
5.990756	414.646183	6.433626
5.777542	425.344911	6.438630
5.606234	417.351560	6.443635
5.734219	432.859623	6.448640
5.998791	438.250540	6.453645
5.838865	427.202313	6.458650
5.698741	424.750250	6.463654
5.964341	440.723986	6.468659
6.101029	431.113115	6.473664
5.861984	428.780957	6.478669
5.519547	424.370549	6.483674
5.658630	434.817928	6.488678
6.092621	439.834280	6.493683
5.895086	448.521539	6.498688
5.787571	441.473657	6.503693
6.050968	439.148196	6.508698
5.853663	442.877708	6.513702
6.157300	435.474336	6.518707
5.724315	430.717439	6.523712
5.755046	425.875232	6.528717
5.896555	419.690029	6.533722
5.501907	431.230290	6.538726
5.901066	432.433366	6.543731
6.046751	445.100719	6.548736
5.942141	445.952448	6.553741
6.154492	436.468928	6.558746
5.922317	422.964243	6.563750
5.631945	418.963304	6.568755
5.788841	414.136134	6.573760
5.615262	413.685683	6.578765
6.076989	430.707543	6.583770
5.660297	434.493573	6.588774
6.192413	430.056872	6.593779
6.053880	421.422455	6.598784
5.558482	417.247992	6.603789
5.791595	421.719998	6.608794
5.972587	432.110188	6.613798
6.262709	416.606398	6.618803
5.939965	423.364351	6.623808
5.927476	422.486855	6.628813
5.892869	412.504192	6.633818
5.994032	429.174411	6.638822
6.164754	421.545092	6.643827
5.897008	417.917103	6.648832
5.733262	429.718583	6.653837
5.732961	426.529589	6.658842
5.891582	420.180350	6.663846
5.811772	423.486479	6.668851
6.203100	421.074537	6.673856
5.897014	421.078290	6.678861
5.798359	417.518722	6.683866
5.718722	422.406733	6.688870
6.045268	418.242694	6.693875
5.848617	418.735512	6.698880
5.930204	423.572952	6.703885
6.298139	414.606079	6.708890
5.952440	424.215065	6.713894
5.815151	422.303571	6.718899
5.678235	425.431983	6.723904
5.484318	414.458694	6.728909
5.911662	419.273598	6.733914
5.911704	426.537809	6.738918
5.913996	403.381556	6.743923
6.088951	427.987719	6.748928
6.080665	419.560692	6.753933
6.114029	426.158444	6.758938
5.778444	425.825127	6.763942
5.946691	421.859900	6.768947
5.715076	417.090438	6.773952
5.664195	424.448050	6.778957
5.674514	419.298989	6.783962
5.554902	422.307628	6.788966
5.657254	419.244923	6.793971
5.826066	422.290630	6.798976
5.806192	425.258332	6.803981
5.800458	419.868171	6.808986
5.840345	414.920126	6.813990
6.189466	418.089445	6.818995
6.205815	415.875464	6.824000
6.039797	420.438480	6.829005
6.174456	416.171626	6.834010
5.732869	425.618463	6.839014
5.855808	424.656471	6.844019
5.861262	423.023175	6.849024
5.706333	424.689561	6.854029
5.714660	422.666665	6.859034
6.023549	424.896306	6.864038
6.399904	423.723763	6.869043
6.094919	421.098210	6.874048
5.642491	420.096652	6.879053
6.259406	419.791269	6.884058
5.640952	425.231949	6.889062
5.802822	417.312948	6.894067
5.918197	420.980809	6.899072
6.080705	415.213105	6.904077
6.209485	411.564118	6.909082
5.492019	404.668767	6.914086
5.607350	410.567123	6.919091
5.891451	413.101209	6.924096
5.866010	423.561704	6.929101
6.133985	420.004803	6.934106
5.892474	423.889937	6.939110
5.904842	423.638146	6.944115
5.785502	403.395846	6.949120
5.503071	410.501825	6.954125
5.836003	417.770824	6.959130
5.539198	421.066658	6.964134
5.770655	416.639102	6.969139
6.031257	420.331665	6.974144
5.612992	416.983529	6.979149
6.050410	419.857433	6.984154
5.795119	428.594861	6.989158
5.868461	420.145552	6.994163
5.774488	420.286918	6.999168
5.601880	418.324010	7.004173
6.109751	415.890644	7.009178
5.797196	430.119942	7.014182
5.844328	420.750904	7.019187
6.260324	419.556331	7.024192
6.180762	425.365002	7.029197
6.198412	412.836768	7.034202
5.764580	415.559274	7.039206
5.746278	396.531876	7.044211
5.783483	402.303262	7.049216
6.121646	409.394264	7.054221
6.172267	405.042501	7.059226
5.859259	410.536561	7.064230
5.723258	401.123459	7.069235
5.912070	399.084942	7.074240
5.422621	404.005520	7.079245
5.747275	406.409863	7.084250
5.824026	424.773381	7.089254
5.896644	420.557377	7.094259
6.033855	425.110850	7.099264
5.815512	425.929776	7.104269
6.341215	415.897287	7.109274
5.457894	409.746107	7.114278
5.793731	414.632295	7.119283
6.065827	418.471757	7.124288
5.719554	421.303933	7.129293
6.037931	411.841779	7.134298
6.083566	408.038138	7.139302
5.687546	403.041334	7.144307
5.764652	400.988681	7.149312
5.694579	415.240088	7.154317
5.811310	419.195643	7.159322
5.505695	428.326941	7.164326
5.962271	424.803766	7.169331
5.835266	427.174472	7.174336
5.554291	427.512820	7.179341
6.006811	419.247715	7.184346
5.780584	433.694450	7.189350
6.169827	426.666818	7.194355
6.070111	415.375042	7.199360
5.904283	419.985486	7.204365
6.233691	421.237456	7.209370
5.669121	413.808771	7.214374
6.138137	421.606954	7.219379
6.311003	402.192085	7.224384
5.728499	405.140368	7.229389
5.897141	390.959126	7.234394
5.465254	389.362718	7.239398
5.627956	391.988590	7.244403
5.660149	403.072806	7.249408
6.019076	415.333396	7.254413
6.331582	413.114142	7.259418
5.734941	411.559365	7.264422
5.804615	399.949988	7.269427
6.021535	398.463898	7.274432
5.464617	394.583823	7.279437
5.740941	398.106236	7.284442
5.646979	418.148006	7.289446
6.024064	425.584100	7.294451
5.794467	423.633284	7.299456
5.960438	416.080643	7.304461
5.871335	416.980562	7.309466
6.055722	423.149682	7.314470
6.063504	409.794076	7.319475
6.111797	400.886783	7.324480
5.743282	410.072221	7.329485
5.726454	399.665992	7.334490
5.700507	399.568905	7.339494
5.747160	397.584300	7.344499
6.054509	409.748561	7.349504
6.088802	410.635474	7.354509
6.000364	399.920919	7.359514
5.970276	401.466500	7.364518
5.549514	395.185902	7.369523
5.840683	396.652674	7.374528
5.507678	391.158773	7.379533
5.885959	409.269382	7.384538
5.817953	423.457196	7.389542
5.719964	422.849365	7.394547
5.932149	429.760793	7.399552
6.003936	427.421063	7.404557
6.057450	415.355453	7.409562
5.632079	409.724155	7.414566
5.634811	417.392910	7.419571
6.075895	417.219483	7.424576
5.976641	429.210179	7.429581
6.135128	417.773539	7.434586
5.764892	407.694767	7.439590
5.716195	399.758144	7.444595
6.091210	390.983166	7.449600
5.672484	398.195919	7.454605
5.809692	394.400079	7.459610
5.889932	406.001961	7.464614
5.598565	407.417635	7.469619
5.976338	412.404821	7.474624
5.790709	418.916658	7.479629
6.259295	411.509598	7.484634
5.692309	401.414199	7.489638
5.561756	397.600200	7.494643
6.092804	417.148564	7.499648
5.937823	423.845430	7.504653
6.205050	420.070342	7.509658
5.805062	405.658638	7.514662
5.623556	393.000267	7.519667
5.693666	390.372897	7.524672
5.901982	406.950375	7.529677
6.077043	409.064939	7.534682
5.995903	407.964078	7.539686
5.658791	404.470348	7.544691
5.845136	399.654387	7.549696
5.551029	403.550921	7.554701
5.571940	415.348770	7.559706
5.650943	420.854180	7.564710
5.863782	424.101801	7.569715
6.225603	421.792560	7.574720
6.017137	431.563550	7.579725
5.775191	423.464202	7.584730
5.963792	433.631733	7.589734
5.839986	424.890602	7.594739
6.166685	413.351678	7.599744
5.977037	414.618534	7.604749
5.799458	406.531256	7.609754
5.664427	404.603591	7.614758
5.664348	417.891724	7.619763
6.206537	415.373886	7.624768
5.957229	421.784967	7.629773
5.721626	408.068855	7.634778
5.829452	414.838438	7.639782
5.849366	417.274710	7.644787
5.893728	407.662499	7.649792
5.840346	412.524247	7.654797
5.877655	410.376586	7.659802
5.778415	418.482106	7.664806
5.888863	409.726426	7.669811
5.988581	414.073794	7.674816
5.810887	410.928416	7.679821
6.018353	400.502863	7.684826
5.950657	393.505709	7.689830
5.766603	393.224582	7.694835
5.755659	398.683966	7.699840
5.514171	403.379028	7.704845
5.772655	410.020597	7.709850
5.685579	421.860681	7.714854
5.965747	415.767652	7.719859
6.278828	422.039996	7.724864
6.189264	429.859261	7.729869
5.867585	414.565229	7.734874
6.127426	414.423363	7.739878
6.080968	404.151491	7.744883
5.980507	399.918316	7.749888
6.078368	410.767616	7.754893
6.212248	399.274732	7.759898
5.657366	402.032021	7.764902
5.800011	409.640885	7.769907
5.805808	398.753375	7.774912
5.476251	400.073789	7.779917
5.809483	387.464489	7.784922
5.887096	393.394059	7.789926
5.483250	399.766070	7.794931
5.884213	402.288172	7.799936
5.480437	404.237160	7.804941
6.073139	404.157038	7.809946
5.553928	403.909441	7.814950
5.974549	415.527602	7.819955
6.091848	411.276125	7.824960
5.889797	411.431260	7.829965
6.094491	409.548445	7.834970
6.004698	402.187747	7.839974
5.693747	405.068171	7.844979
6.017086	401.534238	7.849984
5.676813	402.862659	7.854989
5.935197	402.850738	7.859994
5.780411	403.586938	7.864998
5.554167	409.927962	7.870003
6.000025	401.489899	7.875008
5.750089	404.873301	7.880013
6.015834	400.421394	7.885018
6.067793	400.248823	7.890022
5.703821	404.634040	7.895027
6.195626	399.631011	7.900032
6.016609	399.773046	7.905037
5.994608	399.283027	7.910042
5.841714	405.875153	7.915046
5.904857	404.969989	7.920051
6.209041	395.402498	7.925056
5.947430	395.358154	7.930061
6.047509	386.774955	7.935066
5.929375	395.823077	7.940070
5.788653	396.708936	7.945075
5.966564	399.335590	7.950080
5.816093	398.511353	7.955085
6.129084	397.250661	7.960090
5.992447	404.102836	7.965094
5.875336	397.183027	7.970099
6.068168	387.746884	7.975104
5.580917	392.983496	7.980109
5.617449	396.888336	7.985114
5.944605	395.144525	7.990118
5.831394	402.348820	7.995136
5.800959	386.581274	8.000154
5.556149	394.445962	8.005171
5.918742	394.313501	8.010189
6.119933	390.924357	8.015206
5.939365	389.532654	8.020224
6.094904	391.979319	8.025242
5.785351	397.067632	8.030259
6.214018	400.894745	8.035277
5.982333	394.900508	8.040294
5.915543	395.649506	8.045312
5.905960	392.877199	8.050330
5.726997	397.676812	8.055347
6.054563	394.949507	8.060365
5.792187	398.843869	8.065382
5.649876	406.834511	8.070400
5.944217	384.875000	8.075418
5.680236	400.313320	8.080435
5.866316	392.959773	8.085453
5.903689	396.914464	8.090470
6.023080	391.316493	8.095488
6.178319	395.858619	8.100506
6.002511	398.622284	8.105523
5.916205	395.025725	8.110541
6.055284	392.574101	8.115558
5.814858	400.002612	8.120576
6.012240	390.769627	8.125594
5.791222	405.964540	8.130611
5.638365	406.414605	8.135629
6.105573	398.755081	8.140646
5.804318	398.786592	8.145664
5.759048	403.502145	8.150682
5.664594	401.885514	8.155699
5.883131	407.392850	8.160717
6.247311	415.411434	8.165734
6.180777	428.253219	8.170752
6.377528	411.736855	8.175770
5.785769	396.420160	8.180787
5.763672	397.951091	8.185805
6.107035	411.706922	8.190822
5.531136	416.167953	8.195840
5.808024	415.865888	8.200858
5.970012	422.508691	8.205875
6.193242	425.254018	8.210893
6.150284	417.226304	8.215910
6.217955	438.788492	8.220928
6.390839	421.502699	8.225946
6.312301	426.302364	8.230963
6.126951	426.353584	8.235981
6.437910	419.236076	8.240998
6.009167	423.178600	8.246016
6.142689	421.157024	8.251034
5.851731	412.559110	8.256051
5.844561	422.696583	8.261069
5.982916	418.698752	8.266086
6.243061	417.484143	8.271104
5.954965	411.710175	8.276122
6.378255	426.078331	8.281139
6.178043	423.802938	8.286157
6.296190	420.480447	8.291174
6.071089	427.815052	8.296192
6.326337	416.950932	8.301210
6.182683	429.549187	8.306227
6.012148	424.116550	8.311245
6.280246	424.731029	8.316262
6.161769	426.930303	8.321280
6.221912	423.165628	8.326298
6.091080	420.803627	8.331315
6.533785	418.137172	8.336333
6.435403	417.111279	8.341350
6.036042	428.742914	8.346368
6.138863	416.757140	8.351386
6.199466	421.471888	8.356403
6.196914	429.639455	8.361421
6.233389	425.774348	8.366438
6.042112	428.493105	8.371456
6.052941	431.691428	8.376474
6.269693	429.871401	8.381491
6.362755	428.215920	8.386509
6.387380	420.701469	8.391526
5.932663	430.012836	8.396544
6.073915	427.914311	8.401562
6.317679	422.924837	8.406579
6.282547	424.243222	8.411597
6.493140	423.632813	8.416614
6.063836	434.038401	8.421632
6.274882	419.700413	8.426650
6.261268	416.231314	8.431667
6.138767	426.692967	8.436685
6.306190	420.115490	8.441702
6.207596	427.206215	8.446720
6.355102	426.488928	8.451738
6.412243	425.309282	8.456755
6.203053	427.529081	8.461773
6.116263	417.636875	8.466790
6.101217	421.732327	8.471808
6.343219	435.223195	8.476826
6.681982	444.078892	8.481843
6.249785	433.988336	8.486861
6.428410	417.613659	8.491878
5.867271	431.012616	8.496896
6.453585	441.760844	8.501914
6.493504	439.984302	8.506931
6.587389	451.425062	8.511949
6.983880	451.874260	8.516966
6.285882	445.618560	8.521984
6.288680	425.137390	8.527002
6.506108	431.793600	8.532019
6.205249	429.107950	8.537037
6.526825	436.227518	8.542054
6.670724	441.014425	8.547072
6.580377	435.244179	8.552090
6.465249	424.122511	8.557107
6.040639	431.125465	8.562125
6.428766	427.785918	8.567143
6.577652	445.677876	8.572160
6.604197	442.656908	8.577178
6.380504	434.780578	8.582195
6.404243	436.089740	8.587213
6.539541	448.679014	8.592231
6.634591	457.576058	8.597248
6.635232	449.099693	8.602266
6.532303	432.169524	8.607283
6.270219	431.418584	8.612301
6.601621	444.311639	8.617319
6.621792	448.698219	8.622336
6.587098	445.080941	8.627354
6.647290	433.098679	8.632371
6.295222	432.191427	8.637389
6.689870	439.103891	8.642407
6.461295	436.290151	8.647424
6.651098	437.301899	8.652442
6.729153	436.387213	8.657459
6.377751	435.003339	8.662477
6.590399	439.896237	8.667495
6.458354	442.523666	8.672512
6.617810	443.975663	8.677530
6.619452	442.899384	8.682547
6.676125	455.261145	8.687565
6.957704	449.214872	8.692583
6.652425	440.836935	8.697600
6.221133	434.280679	8.702618
6.420652	438.935797	8.707635
6.377620	455.201066	8.712653
6.667232	450.608337	8.717671
6.361396	459.157946	8.722688
6.586007	451.236614	8.727706
6.532297	449.967038	8.732723
6.499569	458.230863	8.737741
6.883528	442.076452	8.742759
6.572485	447.578416	8.747776
6.578941	454.608512	8.752794
6.876132	453.233464	8.757811
6.336849	456.038309	8.762829
6.429731	459.015500	8.767847
6.330214	458.766099	8.772864
6.628056	452.029323	8.777882
6.695266	459.984005	8.782899
6.549761	453.206242	8.787917
7.079990	453.909036	8.792935
6.774581	450.921143	8.797952
6.598420	453.747987	8.802970
6.715929	452.129697	8.807987
6.561100	458.658054	8.813005
6.535659	458.116184	8.818023
6.450935	468.663460	8.823040
6.921352	475.103325	8.828058
7.560438	470.269646	8.833075
6.781828	471.177512	8.838093
6.926800	452.879909	8.843111
6.730531	455.965520	8.848128
6.566536	462.880317	8.853146
6.782850	458.305382	8.858163
6.787525	461.204877	8.863181
6.992288	453.236162	8.868199
6.939959	460.531086	8.873216
6.887022	453.656770	8.878234
6.833416	448.120600	8.883251
6.784497	459.921406	8.888269
6.875535	458.039024	8.893287
6.779612	455.728352	8.898304
6.822151	455.548209	8.903322
6.933507	454.057114	8.908339
6.827160	459.987749	8.913357
7.086791	451.896830	8.918375
6.985861	455.541850	8.923392
6.762078	447.416224	8.928410
7.092374	452.268602	8.933427
6.727348	456.548283	8.938445
6.854806	455.758398	8.943463
7.050903	455.936042	8.948480
6.719390	457.291400	8.953498
7.124600	449.278657	8.958515
6.785817	457.483139	8.963533
6.709908	461.297806	8.968551
6.726043	448.113783	8.973568
6.870454	455.725013	8.978586
6.986292	452.106238	8.983603
6.998787	465.434276	8.988621
7.357574	460.524599	8.993639
7.135284	456.037320	8.998656
6.932837	453.317312	9.003674
6.879631	449.971172	9.008691
6.620545	462.669585	9.013709
7.122665	455.275962	9.018727
7.025179	458.226177	9.023744
7.078752	451.363575	9.028762
7.464669	446.894611	9.033779
7.065395	451.296419	9.038797
6.911221	454.163999	9.043815
7.022448	455.708759	9.048832
6.983454	461.117609	9.053850
7.164217	454.143561	9.058867
7.013866	457.272470	9.063885
6.759825	457.526954	9.068903
6.921614	458.372682	9.073920
6.898386	461.096671	9.078938
6.922700	462.752878	9.083955
7.265942	473.974704	9.088973
7.055970	480.107772	9.093991
7.269079	480.235415	9.099008
7.298682	474.730380	9.104026
6.821312	462.466257	9.109043
6.745177	466.732234	9.114061
7.230580	479.525447	9.119079
7.098725	475.361660	9.124096
7.093173	484.186119	9.129114
7.271064	485.733060	9.134131
7.272935	489.538702	9.139149
7.418237	487.890809	9.144167
7.430230	466.966344	9.149184
7.154211	465.450737	9.154202
7.232486	464.737985	9.159219
7.272676	460.282162	9.164237
7.048467	453.223245	9.169255
7.555025	458.963176	9.174272
6.902258	460.958995	9.179290
6.804723	462.725811	9.184307
6.736120	456.415672	9.189325
6.735179	475.890078	9.194343
7.495789	469.882351	9.199360
7.408125	484.813443	9.204378
7.308006	486.836282	9.209395
7.422599	484.852378	9.214413
7.410282	488.190035	9.219431
7.108861	487.479969	9.224448
7.099703	478.089955	9.229466
7.228316	478.407559	9.234483
7.326324	486.092344	9.239501
7.060332	478.411967	9.244519
7.478805	480.624947	9.249536
7.233773	485.296082	9.254554
7.317190	476.008327	9.259571
6.937577	477.626839	9.264589
7.108014	477.843218	9.269607
7.513860	473.046082	9.274624
7.387073	478.617014	9.279642
7.344676	473.098014	9.284659
7.181931	477.724697	9.289677
7.078560	473.856245	9.294695
7.248758	473.267943	9.299712
7.058975	478.126077	9.304730
7.508938	476.758648	9.309747
7.244050	463.451390	9.314765
7.120427	477.012200	9.319783
7.443171	483.077581	9.324800
7.279138	487.502500	9.329818
7.388183	474.606853	9.334835
7.259343	478.088995	9.339853
7.276255	474.249033	9.344871
7.495782	477.351550	9.349888
7.583720	491.286316	9.354906
7.471248	484.894679	9.359923
7.348498	478.760272	9.364941
7.181581	473.140864	9.369959
7.540632	488.857177	9.374976
7.524171	499.201274	9.379994
7.525144	502.240209	9.385011
7.597506	483.439562	9.390029
7.046227	486.085347	9.395047
7.740293	485.607465	9.400064
7.545188	499.826423	9.405082
7.375035	489.994575	9.410099
7.547208	489.516414	9.415117
7.507254	499.838946	9.420135
7.619444	497.318938	9.425152
7.455158	490.496767	9.430170
7.729081	491.432223	9.435187
7.289372	488.881926	9.440205
7.194498	498.149571	9.445223
7.797091	499.424845	9.450240
7.579559	505.931486	9.455258
7.617731	494.400752	9.460275
7.575408	504.546935	9.465293
7.646415	508.540562	9.470311
7.608420	493.790261	9.475328
7.505728	505.444890	9.480346
7.682206	502.340460	9.485363
7.616119	493.773543	9.490381
7.471236	498.359564	9.495399
7.770504	499.884333	9.500416
7.919160	498.791327	9.505434
7.718282	501.906069	9.510451
7.400403	493.728894	9.515469
7.690126	489.129827	9.520487
7.771558	490.436265	9.525504
7.621189	487.616575	9.530522
7.695357	488.280376	9.535539
7.977635	476.777677	9.540557
7.390877	476.023957	9.545575
7.653965	478.327553	9.550592
7.835789	485.257602	9.555610
7.789488	476.009106	9.560627
7.755697	470.157405	9.565645
7.342031	482.403533	9.570663
7.753709	496.069831	9.575680
7.661486	501.742650	9.580698
7.811333	498.055422	9.585715
8.098614	496.205404	9.590733
7.416011	490.988676	9.595751
7.689007	488.863190	9.600768
7.719316	494.766114	9.605786
7.960796	498.622577	9.610803
8.008617	494.503217	9.615821
7.792115	489.762562	9.620839
7.744174	477.809836	9.625856
7.516511	481.077093	9.630874
7.470875	487.591507	9.635891
7.504905	489.473409	9.640909
7.682676	508.995589	9.645927
8.016309	497.345977	9.650944
7.905502	499.588239	9.655962
7.815572	498.538927	9.660979
8.279263	494.505884	9.665997
8.045165	499.743347	9.671015
8.003003	501.447842	9.676032
8.059748	495.932236	9.681050
7.532833	492.369980	9.686067
7.860624	490.052874	9.691085
7.867933	498.155812	9.696103
8.094125	492.203409	9.701120
8.373393	505.098365	9.706138
8.055732	492.635631	9.711155
7.930660	488.152047	9.716173
7.934485	482.281825	9.721191
7.734467	468.292222	9.726208
7.644932	477.776767	9.731226
8.004218	487.683293	9.736243
7.852064	480.527870	9.741261
7.753326	495.384968	9.746279
8.099468	490.767593	9.751296
7.823134	505.478959	9.756314
8.056112	501.340053	9.761331
8.033946	502.366082	9.766349
8.061531	506.240282	9.771367
8.221173	503.261564	9.776384
8.076656	498.566432	9.781402
7.742389	489.404074	9.786419
8.084786	489.498836	9.791437
7.802497	500.951231	9.796455
8.198502	501.735018	9.801472
8.555315	498.640202	9.806490
8.040768	490.424416	9.811507
8.098268	481.263794	9.816525
7.572666	479.774668	9.821543
8.003099	492.683799	9.826560
7.953721	501.982186	9.831578
7.951579	500.354238	9.836595
8.356746	500.549617	9.841613
7.936003	506.860883	9.846631
8.028194	499.256919	9.851648
8.010173	502.462930	9.856666
8.073806	511.803575	9.861683
8.616920	498.284487	9.866701
8.299189	507.754309	9.871719
8.282570	512.645280	9.876736
8.183137	501.114012	9.881754
8.191215	503.189327	9.886771
8.134982	499.275614	9.891789
8.003623	499.674977	9.896807
7.983138	494.988814	9.901824
8.328328	500.182849	9.906842
8.174076	509.188408	9.911859
7.988630	500.668592	9.916877
8.055565	499.559988	9.921895
7.874670	501.810077	9.926912
7.948577	504.064424	9.931930
7.926521	499.100799	9.936947
8.051620	496.834385	9.941965
8.379509	504.366396	9.946983
8.209049	497.923881	9.952000
8.100127	503.662433	9.957018
7.955221	498.677032	9.962035
7.980744	504.110500	9.967053
8.448990	517.035815	9.972071
8.280227	521.303695	9.977088
8.182389	499.317129	9.982106
8.143659	520.438501	9.987123
8.333660	514.220365	9.992141
8.215377	532.056442	9.997159
8.431353	526.878791	10.002176
8.597225	530.030749	10.007194
8.405502	525.731165	10.012211
8.376827	509.433065	10.017229
8.130022	510.598432	10.022247
8.385567	516.453450	10.027264
8.447985	528.224233	10.032282
8.686435	540.065272	10.037299
8.999881	528.835364	10.042317
8.324814	517.943379	10.047335
8.058629	508.937599	10.052352
8.281251	495.809549	10.057370
8.178358	515.984773	10.062387
8.613576	514.840556	10.067405
8.171650	516.721296	10.072423
8.014509	527.658645	10.077440
8.471575	519.568318	10.082458
8.448355	523.131749	10.087475
8.933037	526.691340	10.092493
8.556673	523.301147	10.097511
8.190098	523.623756	10.102528
8.272393	526.836144	10.107546
8.476587	526.633828	10.112563
8.809245	525.483589	10.117581
8.570525	536.547333	10.122599
8.553939	525.773075	10.127616
8.696476	530.509728	10.132634
8.558300	534.498267	10.137651
8.268757	529.686996	10.142669
8.590993	537.415564	10.147687
8.559267	532.775333	10.152704
8.401096	529.319394	10.157722
8.302757	536.754101	10.162739
8.134179	527.404818	10.167757
8.293402	533.596821	10.172775
8.180008	519.647254	10.177792
8.431374	516.123994	10.182810
8.221255	526.394309	10.187827
8.523324	533.431767	10.192845
8.598308	549.344119	10.197863
8.481192	557.794779	10.202880
8.936741	543.339489	10.207898
8.726018	550.757097	10.212915
8.493966	535.021008	10.217933
8.553025	549.238052	10.222951
8.308976	548.522150	10.227968
8.834102	552.817016	10.232986
8.573746	556.297689	10.238003
8.661536	557.921869	10.243021
8.597034	548.322741	10.248039
8.703518	556.362830	10.253056
8.915352	548.146814	10.258074
8.637178	552.220407	10.263091
8.580471	552.671189	10.268109
8.778438	549.752730	10.273127
8.463234	557.587494	10.278144
8.750839	548.040494	10.283162
8.621234	556.041835	10.288179
8.995908	553.764712	10.293197
8.620742	553.747844	10.298215
8.445121	548.013013	10.303232
8.865256	551.393376	10.308250
8.469593	549.849171	10.313267
8.952640	547.917982	10.318285
8.935697	556.662212	10.323303
9.131451	546.845585	10.328320
9.075605	544.932560	10.333338
9.077340	550.934652	10.338355
8.990995	548.269021	10.343373
9.091390	554.814228	10.348391
8.706387	554.596932	10.353408
8.924184	546.421008	10.358426
9.036389	553.488222	10.363443
9.158619	549.054236	10.368461
9.358798	547.482945	10.373479
9.104572	550.666015	10.378496
9.095364	543.084231	10.383514
8.785252	545.862650	10.388531
8.788033	538.234809	10.393549
9.112152	551.173263	10.398567
8.954530	548.755482	10.403584
8.974200	534.485257	10.408602
8.523954	550.227442	10.413619
8.621972	547.422472	10.418637
9.025806	551.354494	10.423655
8.901200	559.613826	10.428672
9.245827	550.979375	10.433690
9.013570	552.748374	10.438707
9.042192	547.069902	10.443725
9.112707	549.271138	10.448743
8.828627	559.174368	10.453760
9.171942	540.129238	10.458778
8.591376	557.753752	10.463795
8.966994	546.965367	10.468813
9.187714	543.838219	10.473831
9.315018	551.265980	10.478848
9.345795	553.883693	10.483866
8.997289	555.244876	10.488883
8.689319	551.604122	10.493901
8.953107	558.707547	10.498919
8.600474	558.709239	10.503936
9.497220	547.965433	10.508954
8.957988	548.302472	10.513971
8.863377	547.853487	10.518989
9.360812	558.173903	10.524007
9.075422	550.395550	10.529024
9.030202	541.762226	10.534042
9.493281	550.068329	10.539059
9.423279	554.674189	10.544077
9.268391	549.352670	10.549095
8.768060	555.007400	10.554112
9.269096	544.022642	10.559130
8.796997	548.770396	10.564147
9.131179	547.992298	10.569165
8.965408	541.359687	10.574183
9.151846	565.772013	10.579200
9.408596	573.065894	10.584218
9.501666	580.584236	10.589235
9.252581	564.939152	10.594253
9.449838	553.399233	10.599271
9.025871	559.316551	10.604288
9.822050	558.898407	10.609306
9.383167	557.894299	10.614323
9.032072	561.013653	10.619341
8.880250	561.526675	10.624359
9.358692	568.593316	10.629376
9.347115	578.356031	10.634394
9.112496	582.069359	10.639411
9.349075	577.355521	10.644429
9.317907	577.795991	10.649447
9.419938	586.196549	10.654464
9.747681	573.512716	10.659482
9.384920	576.245740	10.664499
9.655488	581.116979	10.669517
9.690417	561.542638	10.674535
9.360633	552.808729	10.679552
9.042399	550.463450	10.684570
9.356509	568.462186	10.689587
9.360579	576.205909	10.694605
9.571717	572.158770	10.699623
9.346449	571.272669	10.704640
9.209413	575.545058	10.709658
9.645822	582.706652	10.714675
9.617556	572.215061	10.719693
9.475042	575.478460	10.724711
9.325425	585.682525	10.729728
9.459491	581.720044	10.734746
9.763717	573.764093	10.739763
9.333333	579.051268	10.744781
9.514556	575.005660	10.749799
9.745821	582.202553	10.754816
9.849498	574.063431	10.759834
9.441741	566.575640	10.764851
9.467109	573.388227	10.769869
9.962866	568.264557	10.774887
9.647073	578.343178	10.779904
9.682235	564.285094	10.784922
9.609195	550.606888	10.789939
9.464059	554.839516	10.794957
9.256502	556.566775	10.799975
9.072372	575.113793	10.804992
9.390002	571.542271	10.810010
9.490638	572.476480	10.815027
9.509063	575.440111	10.820045
9.749647	572.331936	10.825063
9.566175	570.757639	10.830080
9.760807	576.862059	10.835098
9.653367	569.163113	10.840115
9.767350	575.668329	10.845133
9.648300	574.311154	10.850151
9.564249	577.312931	10.855168
9.282692	578.748832	10.860186
9.786100	582.466445	10.865203
9.501283	580.807041	10.870221
9.805438	579.187898	10.875239
9.767416	575.602672	10.880256
9.609199	570.527819	10.885274
9.828835	583.886607	10.890291
9.702017	602.980090	10.895309
10.271873	600.299998	10.900327
9.933500	585.236926	10.905344
9.802987	574.325857	10.910362
9.864254	580.280762	10.915379
9.594526	571.733093	10.920397
9.597603	569.709848	10.925415
10.035231	576.786043	10.930432
9.683805	584.837931	10.935450
9.889038	593.885037	10.940467
9.614709	602.019526	10.945485
10.054419	604.074561	10.950503
9.959379	604.695451	10.955520
10.133984	601.922654	10.960538
10.090929	592.376946	10.965555
9.769870	584.995483	10.970573
10.099123	595.361207	10.975591
9.662730	590.228948	10.980608
9.803875	593.905495	10.985626
10.050385	603.731926	10.990643
9.852559	602.661644	10.995661
9.966663	609.138452	11.000679
10.043423	599.491917	11.005696
9.946583	610.978441	11.010714
10.187848	596.465165	11.015731
10.239037	605.908794	11.020749
10.342371	593.755565	11.025767
10.103170	597.015182	11.030784
9.696272	584.389642	11.035802
10.123233	594.850509	11.040819
10.143244	607.249677	11.045837
10.240262	591.061196	11.050855
9.803380	595.241716	11.055872
9.557039	591.629166	11.060890
9.990589	603.013648	11.065907
10.226523	602.582299	11.070925
10.218576	596.111129	11.075943
9.886044	610.392733	11.080960
9.819215	609.292458	11.085978
10.121342	608.311098	11.090995
10.189078	598.337777	11.096013
10.003668	604.056787	11.101031
10.153234	598.157380	11.106048
9.832783	609.858819	11.111066
10.139167	609.552129	11.116083
9.729545	614.340604	11.121101
10.003525	602.772853	11.126119
9.690002	613.012082	11.131136
9.810627	625.035739	11.136154
10.111345	623.881031	11.141171
9.598768	636.291083	11.146189
10.180983	624.703425	11.151207
10.099227	631.021582	11.156224
10.195521	634.657827	11.161242
10.463272	628.926084	11.166259
10.120269	637.652014	11.171277
10.031788	633.702299	11.176295
10.546075	635.966558	11.181312
10.325638	629.689615	11.186330
10.393475	628.700782	11.191347
9.906515	631.327043	11.196365
10.269034	631.570132	11.201383
10.445994	642.035483	11.206400
10.471417	652.584544	11.211418
10.941899	644.384763	11.216435
10.526969	631.792005	11.221453
10.512151	626.243391	11.226471
10.491018	628.623097	11.231488
10.275948	628.278189	11.236506
10.638863	625.381211	11.241523
10.619537	627.564975	11.246541
10.510694	630.791551	11.251559
10.827740	622.410694	11.256576
10.701820	632.440661	11.261594
10.826953	631.389202	11.266611
10.863032	632.806898	11.271629
10.782874	633.576935	11.276647
10.749494	628.185862	11.281664
10.550296	623.660209	11.286682
10.408372	601.809812	11.291699
10.533233	609.209578	11.296717
10.566356	600.513458	11.301735
10.707029	608.339932	11.306752
10.608810	606.130585	11.311770
10.627218	602.504954	11.316787
10.496477	605.296303	11.321805
10.297714	604.816298	11.326823
10.464017	616.084872	11.331840
10.719287	629.760001	11.336858
10.634304	621.805051	11.341875
10.643570	629.838314	11.346893
10.715155	628.618522	11.351911
10.803550	624.334985	11.356928
10.689359	624.583338	11.361946
10.624576	626.013681	11.366963
10.779031	620.378586	11.371981
10.634028	625.627372	11.376999
10.864687	624.849712	11.382016
10.575250	629.647762	11.387034
10.923443	623.931819	11.392051
10.604709	624.291115	11.397069
10.594452	634.403945	11.402087
10.609221	629.295660	11.407104
10.452654	629.680040	11.412122
10.698581	628.281454	11.417139
10.908396	636.927079	11.422157
10.528850	627.285752	11.427175
10.806655	629.438740	11.432192
10.549673	624.669678	11.437210
10.993704	621.292935	11.442227
10.764021	629.234250	11.447245
10.664054	622.613388	11.452263
10.786916	617.772191	11.457280
10.722312	627.391763	11.462298
10.799065	623.744363	11.467315
10.685836	626.340469	11.472333
10.726015	631.096342	11.477351
10.942084	628.301265	11.482368
11.068022	629.487132	11.487386
11.050100	625.018283	11.492403
10.702331	629.386818	11.497421
10.778809	627.140629	11.502439
10.937328	628.337170	11.507456
10.646424	636.710956	11.512474
11.066235	630.706080	11.517491
11.102320	640.445582	11.522509
10.808322	639.620738	11.527527
11.078400	652.100677	11.532544
10.832967	652.224427	11.537562
11.236065	642.681371	11.542579
10.816255	649.251316	11.547597
11.011724	645.348627	11.552615
11.427634	649.285089	11.557632
10.985773	649.527978	11.562650
11.276903	640.630469	11.567667
10.841595	639.521655	11.572685
10.601848	649.427455	11.577703
10.798574	647.926123	11.582720
11.193201	650.411103	11.587738
10.933847	643.332371	11.592755
11.185868	658.166204	11.597773
11.049313	656.773895	11.602791
11.118846	656.879854	11.607808
11.267202	662.161582	11.612826
11.045701	656.515954	11.617843
11.112763	661.138236	11.622861
11.054709	654.239397	11.627879
11.182981	647.125176	11.632896
11.036286	660.030180	11.637914
11.009419	657.210047	11.642931
11.151338	665.749559	11.647949
11.096540	654.476285	11.652967
11.204610	652.083132	11.657984
10.990555	663.808961	11.663002
10.867336	676.984853	11.668019
11.101267	677.996013	11.673037
11.140083	678.640114	11.678055
10.833486	677.801463	11.683072
10.965117	685.335899	11.688090
11.075588	678.994468	11.693107
11.194346	680.651677	11.698125
11.320241	683.847795	11.703143
11.504515	680.543297	11.708160
10.927912	679.756419	11.713178
11.506928	691.241242	11.718195
11.601562	692.643456	11.723213
11.340310	691.712493	11.728231
11.622187	685.508305	11.733248
11.469714	686.677838	11.738266
11.262469	680.297825	11.743283
11.856155	681.460900	11.748301
11.881963	677.565852	11.753319
11.700915	670.500086	11.758336
11.643339	683.157615	11.763354
11.649328	677.873968	11.768371
11.469028	675.936247	11.773389
11.064856	686.271772	11.778407
11.713443	675.923377	11.783424
11.228131	683.794316	11.788442
11.542408	679.030407	11.793459
11.851127	685.811265	11.798477
11.548298	681.494338	11.803495
11.835822	680.237553	11.808512
11.441061	684.569283	11.813530
11.480952	686.481845	11.818547
11.591957	689.544598	11.823565
11.283173	690.299966	11.828583
11.724517	686.532313	11.833600
11.849019	688.668303	11.838618
11.569150	688.857409	11.843635
11.686884	689.785790	11.848653
11.759472	691.049448	11.853671
11.692690	686.648198	11.858688
11.383984	694.298968	11.863706
11.520303	681.133812	11.868723
11.687028	688.142044	11.873741
11.417817	686.461250	11.878759
12.085913	698.209830	11.883776
11.868735	694.599002	11.888794
11.414794	688.658425	11.893811
11.719196	690.397000	11.898829
11.642675	701.842529	11.903847
12.084565	701.685020	11.908864
12.237612	701.859945	11.913882
12.002355	681.841812	11.918899
11.949132	684.299137	11.923917
11.973386	683.938821	11.928935
11.964353	677.073318	11.933952
12.125797	682.037422	11.938970
11.979055	680.075509	11.943987
11.713784	679.489158	11.949005
11.664353	687.821978	11.954023
11.848999	670.313196	11.959040
11.936058	674.257008	11.964058
11.525451	674.169954	11.969075
11.605869	687.336038	11.974093
12.006559	698.851962	11.979111
11.908031	705.592493	11.984128
12.071993	701.032011	11.989146
12.089668	705.923974	11.994163
12.363849	699.515860	11.999181
11.956651	697.310731	12.004199
11.777325	680.603736	12.009216
11.721118	688.599947	12.014234
12.057947	709.246134	12.019251
12.135192	693.931658	12.024269
11.888393	703.194811	12.029287
11.941534	698.907313	12.034304
12.239190	701.104536	12.039322
11.808516	708.458842	12.044339
12.245129	707.102956	12.049357
12.363132	718.391786	12.054375
11.946642	717.248460	12.059392
11.791114	722.603065	12.064410
12.171807	713.855588	12.069427
12.116317	706.315700	12.074445
11.703904	714.326709	12.079463
11.689877	720.870970	12.084480
12.136210	712.681253	12.089498
11.687922	717.229661	12.094515
12.517446	711.895865	12.099533
12.261580	716.855936	12.104551
12.299204	708.345250	12.109568
12.221798	707.458065	12.114586
12.007059	714.781696	12.119603
12.332660	720.064072	12.124621
12.497264	730.458828	12.129639
12.219279	718.119107	12.134656
12.421324	721.581011	12.139674
12.062139	709.888335	12.144691
12.154709	732.084447	12.149709
12.175886	734.460693	12.154727
12.594270	736.872535	12.159744
12.557291	742.309557	12.164762
12.446134	740.547189	12.169779
12.144756	734.393344	12.174797
12.605381	738.221835	12.179815
12.476834	732.135586	12.184832
12.669600	737.918462	12.189850
12.436773	733.338090	12.194867
12.317412	718.070178	12.199885
12.167386	732.932353	12.204903
12.549069	729.899873	12.209920
12.714656	728.286649	12.214938
12.441294	743.666775	12.219955
12.754331	735.188664	12.224973
12.492863	733.405666	12.229991
12.591901	732.408783	12.235008
12.726648	731.365280	12.240026
12.502041	721.456629	12.245043
12.613934	711.204927	12.250061
12.543868	717.644358	12.255079
12.486089	714.895331	12.260096
12.432292	718.072273	12.265114
12.760936	736.075213	12.270131
13.001705	728.116513	12.275149
12.635638	716.510117	12.280167
12.210938	709.776000	12.285184
12.385582	722.955750	12.290202
12.179541	738.094948	12.295219
12.525768	734.607276	12.300237
12.688410	737.601986	12.305255
12.470811	741.669287	12.310272
12.533730	741.116720	12.315290
12.071702	735.748594	12.320307
12.752831	738.529523	12.325325
12.390957	755.930619	12.330343
12.632825	762.867147	12.335360
12.991233	765.360973	12.340378
12.527047	764.733202	12.345395
12.976081	759.907133	12.350413
12.959644	767.638373	12.355431
12.974744	765.714208	12.360448
13.170134	760.265161	12.365466
12.739582	764.593051	12.370483
13.066376	754.244537	12.375501
12.732429	745.492251	12.380519
12.610911	747.357526	12.385536
12.602868	750.050777	12.390554
12.513293	756.193478	12.395571
12.623166	765.580659	12.400589
12.879681	763.950030	12.405607
12.768334	765.132058	12.410624
12.856205	759.759817	12.415642
12.942435	758.099065	12.420659
13.231522	754.146970	12.425677
13.161471	759.702788	12.430695
12.805406	760.143675	12.435712
13.036462	758.576995	12.440730
13.031767	764.192002	12.445747
13.178744	758.772631	12.450765
12.853853	759.899755	12.455783
13.027644	767.733734	12.460800
13.269603	757.395354	12.465818
12.915935	769.067387	12.470835
13.318275	759.552791	12.475853
12.804905	754.300001	12.480871
13.060749	749.311700	12.485888
13.195653	758.638152	12.490906
13.093804	763.258523	12.495923
13.037041	756.340508	12.500941
13.359484	768.370510	12.505959
12.941288	757.387638	12.510976
13.222993	759.224450	12.515994
13.273580	765.600813	12.521011
13.053001	764.944341	12.526029
13.095755	766.260015	12.531047
13.040925	783.467862	12.536064
13.452467	780.976651	12.541082
13.361733	790.076540	12.546099
13.391110	785.240478	12.551117
13.664115	779.479461	12.556135
13.358553	772.502592	12.561152
13.520472	757.714438	12.566170
13.156085	765.181457	12.571187
13.138695	760.715647	12.576205
13.224639	766.250181	12.581223
13.400429	777.779303	12.586240
13.754290	769.496752	12.591258
13.584062	780.530980	12.596275
13.489963	762.813317	12.601293
13.380382	761.744977	12.606311
12.968486	765.296771	12.611328
13.264091	777.583449	12.616346
13.166582	777.797632	12.621363
13.548172	783.929636	12.626381
13.507388	787.574767	12.631399
13.160647	793.726215	12.636416
13.603825	777.322382	12.641434
13.386729	786.366328	12.646451
13.797956	779.378135	12.651469
13.561141	782.773112	12.656487
13.198675	786.399216	12.661504
13.698700	776.389622	12.666522
13.423772	786.992133	12.671539
13.539645	781.173684	12.676557
13.541119	794.535254	12.681575
13.678905	788.268400	12.686592
13.027576	784.570942	12.691610
13.636958	793.456996	12.696627
13.455219	785.204707	12.701645
13.582190	797.148590	12.706663
13.910116	807.830227	12.711680
13.853824	801.893580	12.716698
13.728131	800.568986	12.721715
13.654229	797.585786	12.726733
13.729334	798.303101	12.731751
13.919357	812.351511	12.736768
14.223533	793.608891	12.741786
13.716286	794.909756	12.746803
13.751312	783.903194	12.751821
13.605911	778.403394	12.756839
13.862904	792.059443	12.761856
13.885723	791.790868	12.766874
13.904307	789.096137	12.771891
13.861243	786.190158	12.776909
13.979050	785.906701	12.781927
13.897250	781.413108	12.786944
13.563669	783.037057	12.791962
13.803768	792.233435	12.796979
14.018506	808.774219	12.801997
13.775925	802.974057	12.807015
13.713908	809.128236	12.812032
13.716731	811.030841	12.817050
13.969052	815.655694	12.822067
13.930269	807.179024	12.827085
13.743407	808.530678	12.832103
13.867225	813.106236	12.837120
13.676732	815.525126	12.842138
13.804485	817.998294	12.847155
13.797454	818.883114	12.852173
14.152844	802.202678	12.857191
13.969442	805.822821	12.862208
14.029068	804.377672	12.867226
14.069709	823.382037	12.872243
14.165056	832.547467	12.877261
14.494403	830.987471	12.882279
14.306456	821.047775	12.887296
14.091799	814.312267	12.892314
13.977072	811.568992	12.897331
14.405770	815.582384	12.902349
14.665750	805.746084	12.907367
14.311086	806.369789	12.912384
13.972792	809.297831	12.917402
14.198594	796.020741	12.922419
14.081696	801.678586	12.927437
14.761493	796.238837	12.932455
14.233846	814.619019	12.937472
14.389524	809.106751	12.942490
14.088070	811.006536	12.947507
14.419549	805.608736	12.952525
14.266238	801.826933	12.957543
13.969123	810.432147	12.962560
14.392105	819.681936	12.967578
14.541403	823.726484	12.972595
14.623156	836.362291	12.977613
14.515681	816.762645	12.982631
14.007242	811.256601	12.987648
14.322633	813.463683	12.992666
14.358302	821.470805	12.997683
14.604796	828.775865	13.002701
14.929756	831.931353	13.007719
14.661229	836.565234	13.012736
14.502002	825.169358	13.017754
14.303302	826.904722	13.022771
14.411391	828.323774	13.027789
14.624155	823.386383	13.032807
14.569237	832.221905	13.037824
14.625670	831.181199	13.042842
14.895527	830.438415	13.047859
14.602149	826.867901	13.052877
14.592000	826.509817	13.057895
14.560773	827.067067	13.062912
14.255179	826.988805	13.067930
14.646649	828.322430	13.072947
14.377814	831.864445	13.077965
14.795680	814.808133	13.082983
14.315216	836.472463	13.088000
14.618781	827.714924	13.093018
14.615455	821.829932	13.098035
14.425140	828.805798	13.103053
14.880994	827.655173	13.108071
14.403202	843.121063	13.113088
14.770898	831.743609	13.118106
14.705564	824.874248	13.123123
14.849523	833.826934	13.128141
14.982303	823.470909	13.133159
14.751621	821.433768	13.138176
14.352628	831.654955	13.143194
14.824416	840.944446	13.148211
15.346831	850.481631	13.153229
14.978070	845.537518	13.158247
14.975803	841.807780	13.163264
15.049461	831.530442	13.168282
15.290713	823.252886	13.173299
14.760471	836.776692	13.178317
14.502729	825.825443	13.183335
14.782474	833.510304	13.188352
14.816493	846.740581	13.193370
15.117458	851.304172	13.198387
15.108093	858.993318	13.203405
15.374658	857.143353	13.208423
15.051652	857.269791	13.213440
15.223880	854.345849	13.218458
15.202043	833.344204	13.223475
15.260172	841.092195	13.228493
14.984811	828.622597	13.233511
14.997170	833.250339	13.238528
15.071251	841.784785	13.243546
14.921977	853.645756	13.248563
14.725500	853.285307	13.253581
15.026490	859.508861	13.258599
15.295440	867.204896	13.263616
15.113095	854.818537	13.268634
15.651571	849.972119	13.273651
15.030184	854.967407	13.278669
15.239717	850.510201	13.283687
15.151318	852.802645	13.288704
15.096286	854.600709	13.293722
15.320038	853.117217	13.298739
15.376434	854.714785	13.303757
15.579322	850.728838	13.308775
15.529938	855.975333	13.313792
15.135610	854.298347	13.318810
15.484320	854.613031	13.323827
15.193515	853.588859	13.328845
15.569227	852.892605	13.333863
15.848726	858.510452	13.338880
15.405895	859.605567	13.343898
15.346502	851.962087	13.348915
15.540562	848.750701	13.353933
15.453523	854.306054	13.358951
15.414447	855.817594	13.363968
15.696710	861.460255	13.368986
15.514434	857.484161	13.374003
15.090551	857.011019	13.379021
15.468763	854.092672	13.384039
15.488944	863.588633	13.389056
15.671823	851.542687	13.394074
15.605870	854.241872	13.399091
15.559037	864.429992	13.404109
15.740539	853.854875	13.409127
15.719261	866.566807	13.414144
15.495718	865.207046	13.419162
15.652738	853.168306	13.424179
15.476142	852.148331	13.429197
15.605627	862.485550	13.434215
15.550288	850.795667	13.439232
15.396391	862.284981	13.444250
15.954009	860.181129	13.449267
15.709931	879.378487	13.454285
15.454046	866.634411	13.459303
15.706669	877.283707	13.464320
15.668162	886.416488	13.469338
15.975670	881.315913	13.474355
15.981525	887.197551	13.479373
15.892947	884.933010	13.484391
15.953972	885.179160	13.489408
15.720423	882.034765	13.494426
15.936919	876.049041	13.499443
15.944909	881.507462	13.504461
15.998193	881.849499	13.509479
15.763451	881.946329	13.514496
15.761781	877.238183	13.519514
16.184476	874.675784	13.524531
15.906839	882.356479	13.529549
16.076068	882.011315	13.534567
16.177493	878.382088	13.539584
16.105198	878.380881	13.544602
16.226109	882.789654	13.549619
15.884811	881.034928	13.554637
16.069678	871.424958	13.559655
16.304045	875.850667	13.564672
16.014300	877.404639	13.569690
16.024057	875.910493	13.574707
15.946589	876.424497	13.579725
15.991565	877.784013	13.584743
16.198763	881.633307	13.589760
16.187243	877.179171	13.594778
16.271153	877.595306	13.599795
15.980678	885.524169	13.604813
15.875669	875.306357	13.609831
15.821531	881.301536	13.614848
16.099968	870.023251	13.619866
16.537810	869.222587	13.624883
16.118721	878.386591	13.629901
15.975489	873.460783	13.634919
15.974743	874.808528	13.639936
16.281782	888.595665	13.644954
16.771895	890.734356	13.649971
16.319957	895.722041	13.654989
16.034959	886.286668	13.660007
16.529062	894.117852	13.665024
16.614417	899.125497	13.670042
16.304076	885.244372	13.675059
16.241964	896.501574	13.680077
16.548026	898.353520	13.685095
16.623567	906.534316	13.690112
16.495030	907.476048	13.695130
16.788897	905.725943	13.700147
16.134084	903.846766	13.705165
16.284694	908.900994	13.710183
16.619802	903.092337	13.715200
16.229403	908.297603	13.720218
16.415653	906.816827	13.725235
16.682308	903.934886	13.730253
16.206334	902.507375	13.735271
16.246456	901.396637	13.740288
15.996144	901.221348	13.745306
16.638743	906.728670	13.750323
16.531367	917.699485	13.755341
16.621183	928.314359	13.760359
17.157540	926.857622	13.765376
16.737064	926.828917	13.770394
17.048260	912.859855	13.775411
16.686150	908.495356	13.780429
16.986443	905.005381	13.785447
16.819730	903.661959	13.790464
16.624140	903.661135	13.795482
16.551821	903.921866	13.800499
16.965185	918.743260	13.805517
16.661661	924.133737	13.810535
17.135403	923.971236	13.815552
17.145445	917.632833	13.820570
17.202490	910.453927	13.825587
16.826350	904.447438	13.830605
16.615586	914.067974	13.835623
17.270671	899.095136	13.840640
16.918116	900.832522	13.845658
17.066947	907.310309	13.850675
17.346765	901.182109	13.855693
16.875267	901.697890	13.860711
16.865904	902.116016	13.865728
16.604657	905.221352	13.870746
17.248390	914.020033	13.875763
16.968537	913.735763	13.880781
17.369393	919.599705	13.885799
17.169061	911.132518	13.890816
17.051940	905.905961	13.895834
17.257226	898.836379	13.900851
16.862822	900.296297	13.905869
16.793527	917.159398	13.910887
17.112216	911.495324	13.915904
17.079216	925.853324	13.920922
17.492008	920.881411	13.925939
17.396289	925.844850	13.930957
17.326126	920.509945	13.935975
17.232293	922.768535	13.940992
17.198481	925.718318	13.946010
17.333339	934.072871	13.951027
17.141430	932.051734	13.956045
17.143122	928.737928	13.961063
17.204166	931.297305	13.966080
17.120831	921.748264	13.971098
16.956005	934.154529	13.976115
17.410273	923.580816	13.981133
17.403440	928.555575	13.986151
17.543438	926.204721	13.991168
17.446609	938.944321	13.996186
17.198061	927.117401	14.001203
17.416779	927.588155	14.006221
17.262500	933.214029	14.011239
17.773410	929.877244	14.016256
17.460709	942.720098	14.021274
17.630598	941.914077	14.026291
17.668905	943.577603	14.031309
17.772503	943.296370	14.036327
17.776951	935.753306	14.041344
17.476283	933.291612	14.046362
17.603439	926.067001	14.051379
17.789611	941.201725	14.056397
17.561833	938.264701	14.061415
17.857707	942.333648	14.066432
17.688634	948.059675	14.071450
17.764594	945.788281	14.076467
17.873123	947.825818	14.081485
17.694174	934.627821	14.086503
17.850732	944.455911	14.091520
17.542408	953.460586	14.096538
17.727234	951.626575	14.101555
18.018892	947.677192	14.106573
17.890539	960.639499	14.111591
17.983147	949.860501	14.116608
18.077839	950.297039	14.121626
17.980773	952.612945	14.126643
17.842812	940.560404	14.131661
17.908091	951.744031	14.136679
17.963866	947.746398	14.141696
17.838128	947.573682	14.146714
17.895207	946.311959	14.151731
18.000519	948.586689	14.156749
17.840076	958.205676	14.161767
18.239547	951.885140	14.166784
18.167050	947.371112	14.171802
17.824135	940.084445	14.176819
17.997961	942.941737	14.181837
18.054107	948.673503	14.186855
18.505283	939.375225	14.191872
17.952736	943.428778	14.196890
17.961021	947.230357	14.201907
17.964018	942.587735	14.206925
18.055987	939.281874	14.211943
18.203891	942.061175	14.216960
18.211613	942.498716	14.221978
17.795360	941.711947	14.226995
18.155466	944.887195	14.232013
18.013561	955.680405	14.237031
18.135895	943.571299	14.242048
17.939060	952.681583	14.247066
18.115105	969.477890	14.252083
18.622376	968.293954	14.257101
18.310796	969.491589	14.262119
18.558332	967.458400	14.267136
18.375831	977.816166	14.272154
18.570089	968.659113	14.277171
18.541688	966.340951	14.282189
18.452177	967.648961	14.287207
18.594320	968.699766	14.292224
18.578852	965.944071	14.297242
18.158858	967.294394	14.302259
18.480693	969.446837	14.307277
18.442481	967.947576	14.312295
18.793286	969.000402	14.317312
18.955466	969.723016	14.322330
18.541613	969.260922	14.327347
18.679503	954.245994	14.332365
18.632824	954.720462	14.337383
18.359983	967.333024	14.342400
18.531406	967.091657	14.347418
18.426971	972.390993	14.352435
18.806078	959.790359	14.357453
18.760956	974.888766	14.362471
18.837849	972.247988	14.367488
18.945017	965.468311	14.372506
18.971591	969.872951	14.377523
18.762434	962.811473	14.382541
18.756232	964.816495	14.387559
19.020381	965.456860	14.392576
18.765322	964.512288	14.397594
18.548142	964.309717	14.402611
18.869701	974.493829	14.407629
18.541042	972.027048	14.412647
18.746286	970.385498	14.417664
18.762012	960.372786	14.422682
18.790138	961.031196	14.427699
18.894126	968.945628	14.432717
18.491873	976.696382	14.437735
19.024464	967.823995	14.442752
19.158823	976.538413	14.447770
19.051804	985.937602	14.452787
19.009693	977.704373	14.457805
18.962309	987.709610	14.462823
19.119541	996.193232	14.467840
18.944620	997.587211	14.472858
19.188460	998.672578	14.477875
19.349031	990.862029	14.482893
19.239761	998.992927	14.487911
19.236019	999.283941	14.492928
19.353545	992.729852	14.497946
19.160212	995.903458	14.502963
19.472912	995.813527	14.507981
19.003691	984.071638	14.512999
19.610680	990.944736	14.518016
19.530803	991.146691	14.523034
19.062143	984.690761	14.528051
18.984986	974.752555	14.533069
19.321544	994.045257	14.538087
19.321135	989.163312	14.543104
19.308111	992.630563	14.548122
19.327867	996.140017	14.553139
19.358083	986.207073	14.558157
19.106402	990.046237	14.563175
19.327230	990.788065	14.568192
19.570441	990.781606	14.573210
19.168548	999.946134	14.578227
19.352197	995.982104	14.583245
19.203683	995.203877	14.588263
19.356717	998.834462	14.593280
19.479601	1002.293045	14.598298
19.619407	1021.910098	14.603315
19.517632	1009.709827	14.608333
19.464871	1018.289478	14.613351
19.777549	1024.656428	14.618368
20.062016	1017.571237	14.623386
19.774907	1020.677488	14.628403
19.878142	1001.252912	14.633421
19.722248	993.438296	14.638439
19.620814	986.110619	14.643456
19.435529	991.350044	14.648474
19.747771	1012.050928	14.653491
20.131568	1011.230323	14.658509
19.548336	1017.027575	14.663527
19.619741	1017.029100	14.668544
20.160409	1013.804403	14.673562
19.647371	1014.904216	14.678579
19.653633	1006.723356	14.683597
19.892929	1013.480501	14.688615
19.874671	1015.449547	14.693632
19.999640	1009.184625	14.698650
20.031686	1014.396317	14.703667
20.107169	1006.027883	14.708685
19.992514	1019.587699	14.713703
19.831332	1008.886299	14.718720
20.382548	1009.996092	14.723738
20.178211	1016.582902	14.728755
19.970707	1012.837947	14.733773
20.038207	1016.163197	14.738791
19.849915	1015.662604	14.743808
20.145191	1014.098465	14.748826
19.643447	1016.114861	14.753843
20.240628	1021.452607	14.758861
20.240695	1012.414323	14.763879
20.237422	1014.541969	14.768896
20.261996	1018.672376	14.773914
20.197871	1016.643831	14.778931
20.511080	1020.243013	14.783949
20.296529	1025.035746	14.788967
20.230507	1019.321460	14.793984
20.653408	1022.991820	14.799002
20.341748	1025.196189	14.804019
20.118004	1031.066511	14.809037
20.315085	1038.063813	14.814055
20.418464	1039.291112	14.819072
20.560434	1043.257962	14.824090
20.470993	1034.378859	14.829107
20.682445	1035.926902	14.834125
20.541749	1037.246093	14.839143
20.705648	1033.253591	14.844160
20.374539	1026.277468	14.849178
20.484911	1031.255983	14.854195
20.747696	1043.390195	14.859213
20.752412	1035.525149	14.864231
20.233286	1043.025995	14.869248
20.420767	1041.229429	14.874266
20.544364	1043.050018	14.879283
20.408353	1035.213334	14.884301
20.763717	1042.753892	14.889319
20.694566	1041.376239	14.894336
20.916291	1036.907609	14.899354
20.378457	1045.926199	14.904371
21.029399	1039.477868	14.909389
21.129840	1042.523402	14.914407
20.799713	1035.932136	14.919424
20.855751	1025.641668	14.924442
20.935494	1045.508003	14.929459
20.501064	1031.488413	14.934477
20.622213	1035.212366	14.939495
20.486484	1041.769501	14.944512
21.064517	1036.901056	14.949530
20.748078	1042.681762	14.954547
20.954914	1036.366132	14.959565
20.888206	1038.648890	14.964583
21.079089	1056.332906	14.969600
21.084539	1049.348224	14.974618
21.075948	1050.574132	14.979635
21.004539	1052.857629	14.984653
21.234510	1046.857113	14.989671
21.149459	1057.619385	14.994688
21.121465	1054.698378	14.999706
21.093535	1062.336870	15.004723
21.056416	1051.811669	15.009741
21.380449	1062.610836	15.014759
21.015456	1061.645614	15.019776
21.308097	1055.524820	15.024794
21.100813	1062.875828	15.029811
21.408520	1062.950784	15.034829
21.380264	1059.487009	15.039847
20.878526	1057.637480	15.044864
21.423024	1053.812563	15.049882
21.178612	1060.844333	15.054899
21.255963	1055.366353	15.059917
21.408514	1054.196963	15.064935
21.438961	1055.341015	15.069952
21.476297	1053.820441	15.074970
21.320743	1063.274614	15.079987
21.163749	1062.144256	15.085005
21.495478	1060.331399	15.090023
21.330470	1057.921018	15.095040
21.445518	1064.019140	15.100058
21.692026	1082.426626	15.105075
21.756101	1087.046330	15.110093
21.665230	1065.641810	15.115111
21.333237	1069.619808	15.120128
21.545844	1076.551576	15.125146
21.508853	1083.932716	15.130163
21.618002	1085.802911	15.135181
21.934546	1083.377038	15.140199
21.394398	1087.400277	15.145216
21.843727	1086.512596	15.150234
21.807371	1077.666181	15.155251
21.982280	1081.785671	15.160269
22.036059	1083.705568	15.165287
21.645515	1082.981037	15.170304
21.846401	1085.789930	15.175322
21.667625	1089.119065	15.180339
21.617848	1076.771743	15.185357
22.101648	1078.741030	15.190375
21.877172	1089.275853	15.195392
21.995830	1085.164193	15.200410
22.150312	1077.783758	15.205427
22.067560	1092.708276	15.210445
22.163360	1075.547541	15.215463
22.058597	1084.277385	15.220480
22.047288	1081.536800	15.225498
22.152990	1081.113221	15.230515
22.145860	1084.118811	15.235533
22.054660	1085.168313	15.240551
22.168692	1082.187178	15.245568
22.277712	1084.316175	15.250586
22.169146	1079.069292	15.255603
21.851141	1086.267240	15.260621
22.089750	1085.428354	15.265639
22.090700	1085.522970	15.270656
22.364313	1082.630444	15.275674
22.270579	1084.046423	15.280691
21.973552	1089.887219	15.285709
22.589674	1098.813398	15.290727
22.619473	1104.887020	15.295744
22.417006	1106.449428	15.300762
22.218162	1089.012946	15.305779
22.163504	1102.238370	15.310797
22.539718	1105.695152	15.315815
22.428613	1111.509981	15.320832
22.419757	1111.555640	15.325850
22.819723	1115.374783	15.330867
22.680636	1105.995328	15.335885
23.036540	1104.131342	15.340903
22.405063	1102.333694	15.345920
22.660291	1102.448431	15.350938
22.638555	1105.390040	15.355955
22.544784	1103.675405	15.360973
22.950191	1099.392580	15.365991
22.765859	1115.112531	15.371008
22.892920	1112.359729	15.376026
22.954608	1108.932346	15.381043
22.611154	1104.627992	15.386061
22.645760	1100.876644	15.391079
22.546020	1106.825393	15.396096
22.738485	1104.466296	15.401114
22.773715	1105.663251	15.406131
22.836211	1108.313946	15.411149
22.854028	1097.537109	15.416167
22.878325	1107.351298	15.421184
23.051107	1098.844497	15.426202
22.872764	1099.595223	15.431219
22.786349	1112.869812	15.436237
23.223284	1103.226535	15.441255
22.755454	1109.198243	15.446272
22.957294	1105.827799	15.451290
23.059713	1105.133329	15.456307
22.508369	1109.959918	15.461325
22.548280	1108.631445	15.466343
22.787553	1114.801641	15.471360
23.124248	1132.551251	15.476378
22.958905	1126.319150	15.481395
23.056116	1124.928047	15.486413
23.264789	1128.619371	15.491431
23.287469	1134.189179	15.496448
23.431510	1124.399273	15.501466
23.386550	1123.999299	15.506483
23.389297	1132.251565	15.511501
23.452164	1128.177040	15.516519
23.369660	1131.494255	15.521536
22.946759	1138.210031	15.526554
23.234259	1128.700609	15.531571
23.387466	1130.923676	15.536589
23.497979	1124.298052	15.541607
23.660347	1131.704782	15.546624
23.401538	1130.770257	15.551642
23.543295	1130.678706	15.556659
23.199560	1135.482242	15.561677
23.740872	1146.802850	15.566695
23.826432	1141.149985	15.571712
23.831428	1133.363749	15.576730
23.900861	1123.209984	15.581747
23.442583	1135.930615	15.586765
23.595280	1129.771762	15.591783
23.443354	1134.314866	15.596800
23.651970	1141.326181	15.601818
23.699883	1149.211608	15.606835
23.767332	1152.641035	15.611853
24.169061	1151.871265	15.616871
23.853020	1143.595670	15.621888
24.004924	1143.938041	15.626906
24.119141	1145.719083	15.631923
24.136573	1138.918686	15.636941
23.866630	1128.622427	15.641959
24.014305	1126.311371	15.646976
23.990939	1126.529721	15.651994
24.043004	1124.826949	15.657011
24.222274	1120.014648	15.662029
23.800098	1118.225232	15.667047
23.922803	1125.467757	15.672064
23.986419	1141.477093	15.677082
24.229873	1139.501331	15.682099
23.923811	1148.663543	15.687117
24.027433	1150.907004	15.692135
23.967978	1155.561860	15.697152
23.939396	1156.169200	15.702170
24.489816	1149.064379	15.707187
23.988575	1154.324952	15.712205
24.256823	1152.765035	15.717223
24.180499	1144.574960	15.722240
24.171769	1148.429742	15.727258
24.618628	1141.596776	15.732275
24.200468	1148.441203	15.737293
24.385171	1135.328095	15.742311
24.269416	1133.130897	15.747328
24.513191	1144.618046	15.752346
24.572575	1148.149723	15.757363
24.503782	1150.969321	15.762381
24.285676	1145.553385	15.767399
24.270339	1154.073588	15.772416
24.329608	1165.529697	15.777434
24.933765	1167.628463	15.782451
24.534662	1177.815149	15.787469
24.964917	1159.314331	15.792487
24.489165	1156.119472	15.797504
24.555506	1172.450309	15.802522
24.582228	1172.714461	15.807539
24.701120	1175.829712	15.812557
24.534394	1167.019459	15.817575
24.847525	1171.641189	15.822592
24.427879	1173.979263	15.827610
24.775894	1167.811885	15.832627
24.835385	1176.686457	15.837645
24.677981	1178.080860	15.842663
25.043519	1174.265023	15.847680
24.975670	1178.185879	15.852698
25.086757	1164.431016	15.857715
25.091950	1167.365260	15.862733
24.935790	1173.108271	15.867751
24.943211	1170.516219	15.872768
24.685474	1174.485762	15.877786
25.104657	1169.796809	15.882803
24.782451	1173.208394	15.887821
24.655001	1168.545126	15.892839
25.013260	1176.508176	15.897856
24.958912	1195.310063	15.902874
25.306587	1186.406580	15.907891
25.347553	1203.483054	15.912909
25.273629	1188.781991	15.917927
25.451365	1195.160677	15.922944
25.398274	1187.301466	15.927962
25.267305	1177.280058	15.932979
25.273318	1177.291828	15.937997
25.325208	1183.633422	15.943015
25.215324	1181.233322	15.948032
25.382769	1189.387224	15.953050
25.369487	1182.471699	15.958067
24.999604	1190.416293	15.963085
25.346049	1184.186038	15.968103
25.486575	1195.320158	15.973120
25.301532	1187.456374	15.978138
25.578473	1180.908798	15.983155
25.546136	1186.247396	15.988173
25.696627	1182.367417	15.993191
25.831097	1170.568689	15.998208
25.585841	1180.131654	16.003226
25.634140	1177.627873	16.008243
25.781841	1172.489137	16.013261
26.010186	1178.298141	16.018279
26.063198	1177.052819	16.023296
25.953438	1187.440335	16.028314
26.070114	1187.510508	16.033331
25.948240	1185.582513	16.038349
25.779828	1193.176797	16.043367
25.950478	1184.452534	16.048384
25.631318	1184.117612	16.053402
25.969378	1186.112902	16.058419
25.936784	1178.714398	16.063437
25.663198	1182.967299	16.068455
25.768608	1188.259068	16.073472
25.635627	1194.228834	16.078490
26.256356	1184.348428	16.083507
26.013864	1185.390082	16.088525
25.904549	1186.978928	16.093543
26.271681	1201.135598	16.098560
26.155180	1210.044073	16.103578
26.547139	1203.822459	16.108595
26.124527	1195.844411	16.113613
26.132251	1194.997513	16.118631
26.281426	1199.733304	16.123648
26.100036	1205.716971	16.128666
26.337795	1201.674988	16.133683
26.387660	1202.449924	16.138701
26.146885	1209.033047	16.143719
26.281384	1205.297584	16.148736
26.315753	1213.772157	16.153754
26.471264	1206.476716	16.158771
26.173704	1213.586303	16.163789
26.168829	1206.738881	16.168807
26.228027	1205.088634	16.173824
26.290020	1209.389951	16.178842
26.758773	1205.362270	16.183859
26.419778	1213.923745	16.188877
26.413424	1202.768769	16.193895
26.760785	1220.141245	16.198912
26.360907	1226.739834	16.203930
26.735960	1231.465490	16.208947
26.877262	1227.801543	16.213965
26.847498	1232.694770	16.218983
27.119522	1227.650152	16.224000
26.716654	1223.989412	16.229018
26.899083	1219.485867	16.234035
27.040262	1209.658492	16.239053
26.638506	1203.558082	16.244071
26.864786	1208.584760	16.249088
26.792703	1224.391364	16.254106
27.228415	1225.759116	16.259123
27.225827	1240.835304	16.264141
26.955243	1226.259699	16.269159
27.123091	1225.917901	16.274176
26.962319	1233.403705	16.279194
27.216094	1223.186286	16.284211
27.579498	1218.947885	16.289229
27.015510	1211.212892	16.294247
27.254177	1209.203158	16.299264
26.804969	1206.972987	16.304282
27.146130	1226.489288	16.309299
27.519541	1224.673040	16.314317
27.284394	1228.544379	16.319335
27.229803	1229.241005	16.324352
27.467037	1245.055971	16.329370
27.477966	1222.840027	16.334387
27.436324	1226.699982	16.339405
27.359840	1227.803993	16.344423
27.467259	1225.019536	16.349440
27.436739	1223.730493	16.354458
27.503893	1221.984321	16.359475
27.335081	1219.050636	16.364493
27.382253	1230.982065	16.369511
27.751436	1219.673564	16.374528
27.636704	1226.965954	16.379546
27.446431	1217.376705	16.384563
27.711136	1229.965190	16.389581
27.431393	1230.498273	16.394599
27.681727	1229.515528	16.399616
27.816012	1228.134389	16.404634
27.672261	1228.074948	16.409651
27.625225	1220.498804	16.414669
27.275957	1225.669313	16.419687
27.957755	1222.731745	16.424704
27.486177	1229.979059	16.429722
27.533022	1228.889338	16.434739
27.725904	1246.648971	16.439757
27.721695	1253.854626	16.444775
27.991242	1249.921265	16.449792
27.862853	1254.182993	16.454810
27.990360	1248.406752	16.459827
27.967481	1248.075901	16.464845
28.157102	1249.280236	16.469863
28.347832	1249.335650	16.474880
27.872636	1251.209053	16.479898
28.275385	1251.407979	16.484915
28.238065	1251.540151	16.489933
27.936451	1250.296736	16.494951
27.805012	1244.204453	16.499968
28.094112	1247.110007	16.504986
28.262863	1237.057384	16.510003
28.489521	1255.862646	16.515021
28.516669	1251.642206	16.520039
28.273629	1247.363111	16.525056
28.082967	1259.492774	16.530074
28.181242	1270.725083	16.535091
28.387255	1266.498706	16.540109
28.539669	1271.596937	16.545127
28.506706	1276.478054	16.550144
28.458618	1276.346818	16.555162
28.813240	1279.204240	16.560179
28.972728	1272.507771	16.565197
28.333234	1277.944680	16.570215
28.923479	1275.624226	16.575232
28.704793	1271.786291	16.580250
28.640449	1267.198319	16.585267
28.790410	1267.588334	16.590285
28.960501	1267.467097	16.595303
29.002724	1269.423539	16.600320
29.097294	1263.917550	16.605338
28.768693	1271.129855	16.610355
28.923324	1263.247533	16.615373
28.803200	1276.407601	16.620391
28.813229	1269.882877	16.625408
28.917284	1271.479327	16.630426
29.048482	1271.143270	16.635443
29.240323	1269.191360	16.640461
28.868245	1279.588470	16.645479
28.833996	1278.918563	16.650496
29.123053	1271.655823	16.655514
28.878970	1275.657963	16.660531
29.290368	1272.882678	16.665549
28.927810	1271.503639	16.670567
29.026685	1264.867163	16.675584
28.920326	1274.004461	16.680602
28.738997	1276.870114	16.685619
29.220457	1277.145073	16.690637
29.375124	1289.921260	16.695655
29.234085	1289.350138	16.700672
29.280483	1290.223454	16.705690
29.458510	1281.920879	16.710707
29.614220	1290.688911	16.715725
29.356863	1290.678828	16.720743
29.444890	1297.191531	16.725760
29.322243	1299.158028	16.730778
29.120221	1287.632857	16.735795
29.329011	1282.983151	16.740813
29.398658	1285.440242	16.745831
29.587553	1284.252520	16.750848
29.299596	1296.293307	16.755866
29.778476	1306.004822	16.760883
29.756258	1306.276644	16.765901
29.700129	1303.849169	16.770919
29.941106	1314.109220	16.775936
29.776628	1316.606153	16.780954
29.407195	1307.606677	16.785971
29.994379	1310.774816	16.790989
30.052316	1315.922577	16.796007
29.920643	1312.004727	16.801024
29.753536	1304.589375	16.806042
29.892770	1311.690526	16.811059
29.942710	1305.907485	16.816077
29.875162	1309.863038	16.821095
30.222600	1301.022654	16.826112
30.341834	1310.727403	16.831130
29.952082	1306.250367	16.836147
30.077908	1303.838567	16.841165
29.850918	1311.902842	16.846183
30.115929	1312.132817	16.851200
30.387477	1328.564193	16.856218
30.289634	1327.292002	16.861235
30.138354	1327.543019	16.866253
30.311666	1336.794326	16.871271
30.323457	1335.719558	16.876288
30.330249	1343.147595	16.881306
30.237435	1341.221342	16.886323
30.505077	1331.702301	16.891341
30.312205	1330.296671	16.896359
30.788070	1324.459514	16.901376
30.587045	1322.051583	16.906394
30.439968	1326.717056	16.911411
30.925437	1319.196297	16.916429
30.861804	1331.135687	16.921447
30.941593	1323.994079	16.926464
30.831915	1322.884693	16.931482
30.687673	1323.374457	16.936499
31.003252	1318.206220	16.941517
30.793332	1329.527880	16.946535
31.112536	1323.734204	16.951552
31.318413	1324.273256	16.956570
30.843808	1299.734801	16.961587
30.873811	1296.214514	16.966605
30.874310	1305.757976	16.971623
31.208324	1314.794739	16.976640
31.121485	1316.515779	16.981658
30.736281	1311.485746	16.986675
31.005108	1317.761839	16.991693
31.088049	1322.053590	16.996711
31.034114	1320.152806	17.001728
31.517506	1315.507405	17.006746
31.342476	1323.721340	17.011763
31.504576	1322.061271	17.016781
31.166386	1319.807380	17.021799
31.046213	1323.446123	17.026816
31.292403	1322.855356	17.031834
30.820094	1325.779230	17.036851
31.105079	1324.955159	17.041869
31.364984	1322.790601	17.046887
31.505432	1315.712078	17.051904
31.531236	1321.019514	17.056922
31.213445	1323.483664	17.061939
31.564319	1322.093830	17.066957
31.449560	1319.606109	17.071975
31.111124	1328.315878	17.076992
31.325014	1331.634030	17.082010
31.309052	1343.755314	17.087027
31.641334	1348.563445	17.092045
31.583250	1346.199389	17.097063
31.604700	1357.648923	17.102080
31.739900	1350.167252	17.107098
31.409090	1350.036129	17.112115
31.671802	1342.685966	17.117133
31.613148	1336.973580	17.122151
31.840339	1350.233926	17.127168
31.979471	1357.754847	17.132186
31.832882	1369.776690	17.137203
32.194484	1372.150179	17.142221
32.049431	1375.754960	17.147239
32.331925	1377.566467	17.152256
32.369656	1365.858509	17.157274
32.154664	1355.051719	17.162291
32.120881	1349.174480	17.167309
32.340943	1361.735339	17.172327
32.055521	1355.234783	17.177344
32.465707	1363.871459	17.182362
32.228372	1362.277126	17.187379
32.471538	1353.632940	17.192397
32.510068	1365.969771	17.197415
32.008862	1368.128137	17.202432
32.083963	1360.532797	17.207450
32.407981	1376.529948	17.212467
32.583142	1368.836873	17.217485
32.819702	1357.804693	17.222503
32.574383	1361.920659	17.227520
32.748396	1359.943129	17.232538
32.719322	1364.309247	17.237555
32.381618	1361.506145	17.242573
32.571266	1361.811047	17.247591
32.329792	1365.288917	17.252608
32.782384	1361.557234	17.257626
32.392882	1360.630549	17.262643
33.013429	1355.430300	17.267661
32.531313	1367.274330	17.272679
32.610047	1363.525480	17.277696
33.032935	1357.658742	17.282714
32.897862	1365.023806	17.287731
32.816939	1358.759461	17.292749
32.525666	1365.028649	17.297767
32.606998	1367.411335	17.302784
32.944681	1381.509645	17.307802
32.870409	1392.715414	17.312819
32.993020	1379.854860	17.317837
33.062452	1379.752549	17.322855
32.515173	1380.453790	17.327872
33.103574	1386.761890	17.332890
33.062625	1389.233168	17.337907
33.071095	1380.698327	17.342925
32.960830	1387.598750	17.347943
32.640000	1401.052298	17.352960
33.236711	1400.999922	17.357978
33.251457	1413.248990	17.362995
33.596816	1410.073761	17.368013
33.957199	1413.182776	17.373031
33.392250	1414.170819	17.378048
33.596138	1407.580956	17.383066
33.537109	1409.884649	17.388083
33.853851	1409.024040	17.393101
33.861859	1408.678879	17.398119
33.674905	1409.535111	17.403136
33.750655	1402.993730	17.408154
33.627841	1411.912762	17.413171
33.972500	1402.659337	17.418189
33.905313	1403.755590	17.423207
33.730783	1414.169165	17.428224
33.921039	1400.865637	17.433242
33.622843	1403.241517	17.438259
33.799115	1399.313270	17.443277
33.986227	1396.143901	17.448295
33.666041	1405.740818	17.453312
33.881535	1407.780584	17.458330
33.818763	1400.901132	17.463347
33.886413	1419.535812	17.468365
34.367175	1420.164348	17.473383
34.202698	1426.498901	17.478400
34.266625	1419.883623	17.483418
34.356963	1422.634148	17.488435
34.128079	1421.442444	17.493453
34.334571	1417.765088	17.498471
34.180420	1428.238596	17.503488
34.329831	1427.599870	17.508506
34.435285	1424.907212	17.513523
34.646388	1417.565105	17.518541
34.892987	1424.286548	17.523559
34.847038	1428.850993	17.528576
34.796879	1416.831711	17.533594
34.726320	1411.420979	17.538611
34.572693	1399.474727	17.543629
34.756612	1396.495215	17.548647
34.753063	1394.046866	17.553664
34.635493	1387.775629	17.558682
34.623822	1396.655148	17.563699
34.715094	1413.351542	17.568717
34.705443	1410.926239	17.573735
34.879414	1418.441728	17.578752
34.819336	1416.002233	17.583770
34.725913	1420.630920	17.588787
34.589007	1422.899478	17.593805
34.979712	1416.441294	17.598823
35.094758	1432.603786	17.603840
35.164992	1417.434962	17.608858
34.977890	1420.509833	17.613875
34.703711	1415.878957	17.618893
34.864584	1418.173444	17.623911
34.812485	1411.317563	17.628928
35.092696	1410.437430	17.633946
35.305190	1412.922652	17.638963
35.196931	1412.390572	17.643981
35.086059	1425.845958	17.648999
35.369285	1440.306311	17.654016
35.612003	1440.258903	17.659034
35.380212	1448.510191	17.664051
34.930704	1440.217498	17.669069
35.743581	1448.929983	17.674087
35.466354	1439.493098	17.679104
35.437925	1438.080630	17.684122
35.613137	1440.549606	17.689139
35.377692	1436.449164	17.694157
35.385014	1438.543641	17.699175
35.468510	1443.438117	17.704192
35.540787	1436.152468	17.709210
35.678109	1437.254552	17.714227
35.576284	1443.086970	17.719245
35.869160	1446.582124	17.724263
35.947771	1468.727687	17.729280
36.089605	1454.396560	17.734298
36.371146	1460.048993	17.739315
35.895237	1443.220487	17.744333
36.190686	1436.442691	17.749351
35.820835	1438.725657	17.754368
36.024594	1449.922616	17.759386
35.846133	1452.169285	17.764403
36.160917	1456.513109	17.769421
36.400626	1447.954630	17.774439
36.069005	1454.129181	17.779456
36.185165	1450.756317	17.784474
36.376146	1454.384206	17.789491
36.167064	1460.599523	17.794509
36.087167	1456.979653	17.799527
36.413042	1461.369080	17.804544
36.436250	1456.909358	17.809562
36.419412	1451.761607	17.814579
36.411169	1455.496453	17.819597
36.294598	1456.840298	17.824615
36.461472	1460.812806	17.829632
36.667981	1466.297109	17.834650
36.993970	1467.041417	17.839667
36.767446	1460.910307	17.844685
37.112248	1462.068251	17.849703
36.477577	1452.889342	17.854720
37.063692	1454.605948	17.859738
36.858896	1447.758197	17.864755
36.330082	1451.470459	17.869773
36.895857	1464.800922	17.874791
36.638386	1478.250913	17.879808
36.537929	1475.789333	17.884826
36.826232	1475.611702	17.889843
36.873763	1476.573216	17.894861
37.084916	1477.471223	17.899879
36.756623	1470.150487	17.904896
36.792762	1471.243179	17.909914
36.879631	1482.000861	17.914931
36.857679	1503.963401	17.919949
37.397936	1496.743267	17.924967
37.445681	1507.106290	17.929984
37.746560	1506.570067	17.935002
37.382681	1499.254895	17.940019
37.190046	1501.850944	17.945037
37.568536	1494.829732	17.950055
37.592163	1503.637500	17.955072
37.894360	1492.986289	17.960090
38.167565	1484.327866	17.965107
37.492232	1481.028511	17.970125
37.421166	1472.143156	17.975143
37.528011	1481.202972	17.980160
37.582037	1502.512951	17.985178
38.023215	1498.341197	17.990195
37.726266	1497.141216	17.995213
37.630694	1493.668969	18.000231
37.813891	1494.063250	18.005248
37.579477	1497.940844	18.010266
37.757197	1490.910063	18.015283
38.052151	1498.804278	18.020301
38.048897	1493.414535	18.025319
38.086913	1490.113870	18.030336
38.073788	1489.506920	18.035354
38.228189	1479.320704	18.040371
37.867440	1490.318945	18.045389
38.124230	1473.460821	18.050407
37.929938	1486.421217	18.055424
38.199741	1489.055268	18.060442
38.321366	1496.979795	18.065459
38.105802	1508.460249	18.070477
38.827575	1510.490135	18.075495
38.706026	1511.957846	18.080512
38.712068	1504.859279	18.085530
38.579750	1488.327206	18.090547
38.388448	1488.041674	18.095565
38.499256	1502.854153	18.100583
38.979902	1499.676648	18.105600
38.805340	1497.539114	18.110618
38.432451	1485.371527	18.115635
38.649470	1507.880478	18.120653
38.879156	1505.480781	18.125671
38.847383	1516.099276	18.130688
38.765099	1514.259720	18.135706
38.695161	1505.465694	18.140723
38.559875	1516.242424	18.145741
38.884239	1517.037485	18.150759
38.852613	1510.263568	18.155776
38.902960	1511.792712	18.160794
38.808842	1506.480321	18.165811
38.794517	1517.036120	18.170829
39.213760	1509.509878	18.175847
39.133081	1510.018091	18.180864
39.218275	1527.974765	18.185882
39.408209	1524.299981	18.190899
39.500522	1532.721444	18.195917
39.504537	1526.686740	18.200935
39.582785	1524.342327	18.205952
39.208157	1510.095230	18.210970
39.712570	1523.072418	18.215987
39.139587	1534.110249	18.221005
39.121955	1527.772809	18.226023
39.140524	1539.642652	18.231040
39.183742	1538.973221	18.236058
39.660851	1528.982581	18.241075
39.805448	1532.425241	18.246093
39.392268	1535.014822	18.251111
39.523673	1532.141349	18.256128
39.592130	1542.756780	18.261146
39.728800	1543.032115	18.266163
39.972030	1555.434839	18.271181
39.950255	1557.167799	18.276199
40.188684	1564.001033	18.281216
40.039743	1555.282479	18.286234
40.249457	1551.585655	18.291251
40.208212	1557.639003	18.296269
39.991304	1533.549022	18.301287
39.987676	1545.791592	18.306304
39.956566	1555.936615	18.311322
40.445645	1549.150531	18.316339
40.469958	1555.089460	18.321357
40.328454	1546.243508	18.326375
40.159220	1550.969318	18.331392
40.427559	1552.691539	18.336410
40.283828	1551.290815	18.341427
40.337702	1547.261787	18.346445
40.692881	1537.937214	18.351463
40.801993	1543.534635	18.356480
40.765507	1546.907836	18.361498
41.174157	1542.412950	18.366515
40.839681	1552.144733	18.371533
40.782872	1545.513610	18.376551
40.932932	1542.946495	18.381568
40.947894	1547.072218	18.386586
41.196150	1543.871153	18.391603
40.634637	1540.509770	18.396621
40.679015	1540.512374	18.401639
41.048811	1545.977430	18.406656
40.958657	1548.336513	18.411674
40.985470	1544.788273	18.416691
41.291654	1537.715255	18.421709
40.768476	1544.661496	18.426727
40.815111	1537.158908	18.431744
40.932459	1539.109921	18.436762
41.012395	1546.214144	18.441779
40.884059	1548.642328	18.446797
41.070211	1559.160430	18.451815
41.279273	1566.815657	18.456832
41.391670	1577.171747	18.461850
41.620206	1572.806064	18.466867
41.199987	1573.436907	18.471885
41.362226	1583.696826	18.476903
41.626001	1560.999014	18.481920
41.461504	1568.643339	18.486938
41.388621	1563.602171	18.491955
41.190221	1571.094012	18.496973
41.242674	1573.541213	18.501991
41.637829	1584.067610	18.507008
41.627846	1598.974837	18.512026
41.799770	1589.653702	18.517043
41.758865	1593.314795	18.522061
41.892529	1585.501891	18.527079
41.939609	1593.778984	18.532096
41.621815	1591.300945	18.537114
42.221961	1590.203411	18.542131
41.994173	1591.501571	18.547149
41.948505	1583.533720	18.552167
41.781164	1581.480255	18.557184
41.983733	1607.037090	18.562202
42.184230	1608.100883	18.567219
42.325910	1607.763178	18.572237
42.397178	1611.902186	18.577255
42.717492	1606.278667	18.582272
42.579408	1616.446797	18.587290
42.544860	1614.019054	18.592307
42.458501	1613.489849	18.597325
42.496961	1611.009641	18.602343
42.698058	1604.464327	18.607360
42.421449	1608.730426	18.612378
42.766347	1605.230172	18.617395
42.838121	1606.219454	18.622413
42.492427	1604.187618	18.627431
42.639122	1594.674764	18.632448
42.449028	1606.069235	18.637466
42.354172	1605.222609	18.642483
42.715442	1601.246397	18.647501
42.850732	1605.567886	18.652519
43.168888	1617.084714	18.657536
43.027283	1636.430937	18.662554
43.007740	1622.159676	18.667571
43.122471	1629.132242	18.672589
43.445434	1619.493922	18.677607
43.705563	1606.229789	18.682624
43.738809	1616.958083	18.687642
43.500779	1608.177719	18.692659
43.093974	1598.855730	18.697677
43.010990	1586.232378	18.702695
43.612837	1599.052339	18.707712
43.530168	1618.067401	18.712730
43.609484	1614.447802	18.717747
43.583405	1615.597590	18.722765
43.789630	1618.459383	18.727783
43.764180	1617.497736	18.732800
43.569369	1618.020677	18.737818
43.829411	1613.053572	18.742835
44.196948	1612.576334	18.747853
43.964606	1614.430658	18.752871
44.041547	1609.788902	18.757888
44.064109	1616.027942	18.762906
43.858698	1621.722005	18.767923
43.947886	1613.316425	18.772941
44.059534	1619.617252	18.777959
44.040562	1610.401758	18.782976
44.107605	1614.443593	18.787994
43.924363	1611.704617	18.793011
43.896422	1616.793333	18.798029
44.208756	1616.447827	18.803047
44.009088	1597.619198	18.808064
43.998432	1614.300191	18.813082
43.961282	1617.932297	18.818099
44.125777	1620.478721	18.823117
44.070952	1638.302801	18.828135
44.103292	1646.569604	18.833152
44.235760	1643.500277	18.838170
44.400654	1644.396073	18.843187
44.393262	1642.579485	18.848205
44.974581	1665.261942	18.853223
44.880632	1656.828228	18.858240
45.172987	1665.029053	18.863258
45.040881	1656.613941	18.868275
45.162075	1633.992027	18.873293
45.157813	1641.731204	18.878311
45.032846	1635.281149	18.883328
44.884990	1641.695229	18.888346
44.673731	1633.866915	18.893363
44.814880	1647.630137	18.898381
44.943247	1649.345894	18.903399
45.343298	1656.721915	18.908416
45.550473	1654.909580	18.913434
45.238574	1661.358836	18.918451
45.544030	1650.410361	18.923469
45.047989	1666.107046	18.928487
45.323014	1663.873803	18.933504
45.440592	1653.614360	18.938522
45.351006	1660.177115	18.943539
45.730841	1647.932509	18.948557
45.314297	1651.027588	18.953575
45.413777	1652.173486	18.958592
45.237030	1661.659698	18.963610
45.146395	1654.932843	18.968627
45.750828	1663.447708	18.973645
45.746952	1677.681823	18.978663
45.664172	1682.813865	18.983680
45.799238	1680.747724	18.988698
45.690911	1677.346870	18.993715
46.100779	1676.847218	18.998733
45.838578	1680.284212	19.003751
45.803704	1676.584657	19.008768
45.743941	1677.998516	19.013786
45.492380	1681.954578	19.018803
46.125502	1681.394700	19.023821
46.323204	1706.223410	19.028839
46.672679	1697.215246	19.033856
46.484339	1704.453088	19.038874
46.637495	1692.922502	19.043891
47.197623	1690.467852	19.048909
46.521343	1677.457684	19.053927
46.447772	1665.665977	19.058944
46.547950	1671.615151	19.063962
46.426141	1678.508026	19.068979
46.895825	1682.546755	19.073997
46.899476	1691.345121	19.079015
47.013389	1687.347682	19.084032
46.715766	1681.483268	19.089050
46.573023	1685.150869	19.094067
46.812273	1685.441694	19.099085
46.715070	1689.070600	19.104103
46.739410	1681.921757	19.109120
47.130391	1686.073809	19.114138
46.721851	1695.807806	19.119155
47.400075	1690.538462	19.124173
46.791439	1695.045960	19.129191
47.051998	1690.975049	19.134208
47.208798	1693.958213	19.139226
47.364330	1716.574896	19.144243
47.773384	1715.358964	19.149261
47.494508	1712.818002	19.154279
47.776137	1697.170828	19.159296
47.623576	1690.551498	19.164314
47.396560	1692.430243	19.169331
47.702295	1691.830135	19.174349
47.572637	1700.955521	19.179367
47.690012	1707.347005	19.184384
48.020461	1709.681237	19.189402
47.733445	1711.023401	19.194419
48.094535	1716.830720	19.199437
47.805247	1717.589385	19.204455
47.948701	1713.925001	19.209472
48.225219	1711.492692	19.214490
47.923582	1713.225332	19.219507
48.003906	1718.278179	19.224525
48.217999	1711.396256	19.229543
48.241731	1721.706358	19.234560
48.192527	1711.829638	19.239578
47.817304	1713.056227	19.244595
48.244441	1709.016020	19.249613
48.258883	1715.253211	19.254631
48.411514	1702.425595	19.259648
48.534777	1709.223277	19.264666
48.346726	1709.682042	19.269683
48.278102	1705.946740	19.274701
48.260325	1711.223250	19.279719
48.448377	1716.887256	19.284736
48.739039	1718.867943	19.289754
48.400820	1733.495331	19.294771
48.383295	1733.138385	19.299789
48.486708	1743.518071	19.304807
48.809767	1728.363024	19.309824
48.733543	1730.423286	19.314842
48.674777	1731.764405	19.319859
48.383422	1737.295236	19.324877
49.157617	1748.683891	19.329895
49.118314	1752.344766	19.334912
49.112378	1758.730339	19.339930
49.064534	1757.674358	19.344947
49.279260	1747.819385	19.349965
49.170080	1750.396082	19.354983
49.745516	1759.227979	19.360000
49.793425	1753.454580	19.365018
49.523075	1749.671976	19.370035
50.043047	1739.491456	19.375053
49.471150	1750.863783	19.380071
49.255591	1749.486921	19.385088
49.393510	1741.935229	19.390106
49.440360	1755.804832	19.395123
50.055281	1748.929526	19.400141
49.846065	1744.695507	19.405159
49.615391	1744.056357	19.410176
50.088770	1740.507544	19.415194
49.696223	1745.385163	19.420211
49.789045	1743.609672	19.425229
50.026926	1760.109841	19.430247
50.119100	1763.904762	19.435264
50.412743	1764.202847	19.440282
50.310964	1770.354118	19.445299
50.279919	1762.415456	19.450317
50.437067	1769.835893	19.455335
50.299714	1779.814641	19.460352
50.653991	1774.466633	19.465370
50.331559	1779.740399	19.470387
50.757629	1766.731031	19.475405
50.512876	1770.310484	19.480423
50.542078	1764.123422	19.485440
50.532720	1767.950032	19.490458
50.127972	1771.153742	19.495475
50.816500	1764.961214	19.500493
50.838015	1769.234293	19.505511
50.428861	1766.716890	19.510528
50.689433	1781.651311	19.515546
50.889982	1795.452681	19.520563
50.900732	1796.464159	19.525581
51.011753	1790.775539	19.530599
50.828978	1792.644207	19.535616
50.869400	1789.665020	19.540634
50.670492	1798.794994	19.545651
51.095450	1783.096885	19.550669
50.811563	1798.691014	19.555687
51.056952	1817.061562	19.560704
51.423779	1806.920779	19.565722
51.423162	1810.575605	19.570739
51.309765	1812.392377	19.575757
51.578766	1820.088817	19.580775
51.519868	1816.774872	19.585792
51.698308	1810.681184	19.590810
51.966553	1816.682974	19.595827
51.913294	1814.273916	19.600845
52.179365	1812.016810	19.605863
51.966722	1804.160234	19.610880
52.188462	1804.434869	19.615898
51.752509	1805.926614	19.620915
51.832509	1809.278457	19.625933
52.079060	1810.155156	19.630951
52.006803	1804.280640	19.635968
52.348239	1803.889543	19.640986
52.121145	1806.342702	19.646003
52.418384	1799.454031	19.651021
52.448119	1799.253789	19.656039
52.289801	1798.584365	19.661056
52.567586	1797.477363	19.666074
52.424518	1806.273525	19.671091
52.194910	1799.647289	19.676109
52.369692	1806.427469	19.681127
52.530186	1817.631437	19.686144
52.805331	1823.300768	19.691162
52.425887	1826.541552	19.696179
52.807893	1825.156271	19.701197
53.029796	1833.870016	19.706215
52.955864	1833.695485	19.711232
52.697864	1824.438431	19.716250
53.031130	1822.435900	19.721267
52.981884	1822.472108	19.726285
53.340555	1820.528717	19.731303
53.037100	1828.873463	19.736320
52.966649	1822.591535	19.741338
52.874846	1826.314302	19.746355
53.010671	1837.702040	19.751373
53.092305	1840.993670	19.756391
53.408482	1849.235031	19.761408
53.340216	1842.643465	19.766426
53.652251	1845.062657	19.771443
53.530036	1845.706783	19.776461
53.626337	1847.875735	19.781479
53.348925	1853.716861	19.786496
53.537510	1844.004796	19.791514
53.625718	1852.101984	19.796531
53.669691	1868.736782	19.801549
54.333835	1866.029113	19.806567
54.289859	1873.477949	19.811584
54.421350	1855.278861	19.816602
54.261565	1850.273320	19.821619
54.052067	1846.809384	19.826637
54.294793	1835.678109	19.831655
54.190168	1841.321735	19.836672
54.481422	1835.721635	19.841690
54.587779	1835.518856	19.846707
54.596299	1837.357558	19.851725
54.565771	1837.785333	19.856743
54.304469	1832.350707	19.861760
54.563976	1846.218622	19.866778
54.426209	1851.248868	19.871795
54.625646	1859.587425	19.876813
54.512798	1859.876611	19.881831
54.470930	1871.229091	19.886848
54.768808	1855.377249	19.891866
54.510060	1862.783986	19.896883
54.652553	1861.906473	19.901901
54.449004	1854.023202	19.906919
54.288156	1874.868642	19.911936
54.978840	1874.223996	19.916954
54.993648	1882.294827	19.921971
54.774875	1880.921614	19.926989
54.938897	1871.611039	19.932007
55.105291	1888.545431	19.937024
55.276741	1894.085856	19.942042
55.699498	1902.471500	19.947059
55.639226	1901.477421	19.952077
55.529176	1896.167410	19.957095
55.622465	1896.026643	19.962112
55.651196	1908.097122	19.967130
55.884301	1899.113402	19.972147
55.532171	1898.152427	19.977165
55.836316	1893.490780	19.982183
55.839736	1900.828053	19.987200
55.924081	1893.142671	19.992218
56.105524	1890.239209	19.997235
56.198516	1898.389321	20.002253
56.302520	1890.498876	20.007271
56.122443	1899.357689	20.012288
56.467255	1893.512479	20.017306
56.747296	1891.537216	20.022323
56.214948	1893.018823	20.027341
56.389261	1889.415845	20.032359
56.496587	1897.749916	20.037376
56.401375	1897.600810	20.042394
56.369657	1892.714056	20.047411
56.304889	1889.170628	20.052429
56.347890	1881.889385	20.057447
56.261581	1884.664502	20.062464
56.532531	1881.851167	20.067482
56.606874	1893.103397	20.072499
56.527018	1903.704407	20.077517
56.862006	1904.898635	20.082535
56.671053	1921.829083	20.087552
57.010788	1918.872412	20.092570
56.769037	1913.867071	20.097587
56.436372	1910.520257	20.102605
56.721766	1913.868344	20.107623
56.947111	1942.208848	20.112640
57.149043	1937.228666	20.117658
57.366076	1947.571733	20.122675
57.517212	1940.526006	20.127693
57.506747	1926.688609	20.132711
57.355821	1941.788629	20.137728
57.423079	1932.587863	20.142746
57.452879	1943.588310	20.147763
57.582090	1940.424763	20.152781
57.898535	1938.099785	20.157799
57.597955	1959.702568	20.162816
57.987736	1965.871572	20.167834
58.083813	1956.098195	20.172851
57.782281	1963.145578	20.177869
58.198253	1955.405055	20.182887
57.928527	1968.516482	20.187904
58.145624	1955.435571	20.192922
58.373208	1961.134491	20.197939
58.353188	1958.073222	20.202957
58.446691	1947.675361	20.207975
58.326753	1965.986528	20.212992
58.452485	1955.463684	20.218010
58.375076	1962.239251	20.223027
57.963498	1962.827724	20.228045
58.484191	1970.914015	20.233063
58.746259	1985.229792	20.238080
58.831290	1982.372981	20.243098
58.706384	1978.132009	20.248115
58.528971	1981.659924	20.253133
59.133053	1983.055011	20.258151
58.948440	1982.171934	20.263168
58.961828	1982.823222	20.268186
59.063046	1982.217277	20.273203
58.944709	1980.014066	20.278221
58.859887	1986.011266	20.283239
58.794345	1986.151021	20.288256
59.294839	1996.383429	20.293274
59.458981	2003.509357	20.298291
59.430050	2005.230858	20.303309
59.435204	2004.396948	20.308327
59.479949	2006.454069	20.313344
59.514740	2004.053282	20.318362
59.678222	1996.469074	20.323379
59.644794	2002.268865	20.328397
59.902933	1996.446670	20.333415
59.592107	1997.073011	20.338432
59.581931	2003.815967	20.343450
59.942387	1993.837035	20.348467
59.806299	2004.052411	20.353485
59.831688	1998.440263	20.358503
59.730229	2016.552912	20.363520
59.792554	2016.148733	20.368538
60.091772	2025.203933	20.373555
60.169641	2025.131857	20.378573
60.319916	2019.171909	20.383591
60.422514	2026.064474	20.388608
60.273348	2016.054914	20.393626
60.182731	2024.451617	20.398643
60.362406	2036.848853	20.403661
60.769689	2045.000287	20.408679
60.581231	2050.736014	20.413696
60.401643	2041.725357	20.418714
60.581546	2046.399751	20.423731
60.871639	2047.844038	20.428749
60.689668	2040.392836	20.433767
61.053543	2052.006931	20.438784
61.134214	2055.948894	20.443802
61.270601	2067.721727	20.448819
61.463539	2070.478370	20.453837
61.759654	2060.310651	20.458855
61.414403	2061.384233	20.463872
61.653252	2055.675502	20.468890
61.763523	2048.935958	20.473907
61.541302	2042.261134	20.478925
61.661386	2046.244261	20.483943
61.735865	2053.166490	20.488960
61.645407	2056.327320	20.493978
61.986127	2052.486783	20.498995
61.899596	2062.542939	20.504013
62.103072	2058.758620	20.509031
61.868714	2060.755327	20.514048
61.922100	2055.788918	20.519066
62.003534	2043.672852	20.524083
62.005125	2055.094384	20.529101
62.338712	2057.185157	20.534119
62.258609	2052.886651	20.539136
62.172872	2059.003948	20.544154
62.433259	2057.240044	20.549171
61.954363	2062.926599	20.554189
62.191687	2067.535193	20.559207
62.891323	2064.648353	20.564224
62.515388	2077.927990	20.569242
62.721865	2080.755102	20.574259
62.452278	2087.803841	20.579277
62.570980	2074.889749	20.584295
62.600196	2078.937617	20.589312
62.781112	2081.803450	20.594330
62.964981	2075.131266	20.599347
62.670989	2075.420432	20.604365
62.822064	2090.732056	20.609383
63.046017	2094.301258	20.614400
63.356189	2099.409726	20.619418
63.529213	2095.406092	20.624435
63.393504	2104.002415	20.629453
63.341213	2094.735083	20.634471
63.148057	2106.442799	20.639488
62.868778	2100.174555	20.644506
63.158993	2098.390195	20.649523
63.322999	2114.558257	20.654541
63.643523	2117.560025	20.659559
64.217590	2118.530604	20.664576
64.143391	2116.528760	20.669594
64.464539	2118.713015	20.674611
64.205301	2112.754075	20.679629
64.485014	2108.680069	20.684647
64.212821	2108.113687	20.689664
64.162971	2112.558988	20.694682
64.383019	2115.175680	20.699699
64.359330	2115.602391	20.704717
63.934069	2112.967532	20.709735
64.363910	2109.147737	20.714752
64.537878	2116.723486	20.719770
64.421450	2115.823406	20.724787
64.422640	2122.918104	20.729805
64.767827	2112.076741	20.734823
64.756440	2108.417601	20.739840
64.485427	2112.544075	20.744858
64.678111	2114.104623	20.749875
64.730687	2131.066546	20.754893
64.962292	2121.899899	20.759911
65.350621	2132.926347	20.764928
65.154174	2133.471651	20.769946
65.022124	2132.182668	20.774963
64.973850	2138.177348	20.779981
64.993845	2135.447477	20.784999
65.219198	2137.075498	20.790016
65.225272	2155.562790	20.795034
65.562586	2163.248676	20.800051
65.404560	2161.758618	20.805069
65.593197	2170.989020	20.810087
65.656147	2158.225626	20.815104
65.718159	2157.812024	20.820122
65.985512	2147.257412	20.825139
65.663718	2151.202488	20.830157
65.727416	2156.393773	20.835175
66.126235	2162.473060	20.840192
65.941757	2181.826588	20.845210
66.343294	2188.883836	20.850227
66.212226	2190.760224	20.855245
66.265534	2186.806886	20.860263
66.054325	2175.838047	20.865280
66.118759	2192.166958	20.870298
66.772973	2185.039159	20.875315
66.617327	2176.223515	20.880333
66.592489	2177.663502	20.885351
66.892442	2176.720275	20.890368
66.946140	2179.255734	20.895386
67.034082	2181.271390	20.900403
67.076741	2186.434421	20.905421
67.133278	2191.841451	20.910439
67.149622	2176.749861	20.915456
66.988510	2178.649891	20.920474
67.059083	2180.138051	20.925491
67.268110	2190.271057	20.930509
67.399509	2188.088658	20.935527
67.588493	2189.362591	20.940544
67.525116	2192.004764	20.945562
67.483301	2187.217350	20.950579
67.301975	2194.706774	20.955597
67.129820	2186.846842	20.960615
67.420366	2185.696789	20.965632
67.774470	2204.268470	20.970650
68.158605	2198.473810	20.975667
67.615258	2197.094616	20.980685
67.824808	2209.815522	20.985703
68.269263	2215.259620	20.990720
67.969594	2221.969113	20.995738
68.012901	2214.937017	21.000755
68.279831	2223.830105	21.005773
68.258474	2217.025907	21.010791
68.285679	2214.411669	21.015808
67.856240	2209.855407	21.020826
68.134453	2216.486983	21.025843
68.242030	2232.026467	21.030861
67.919460	2239.440201	21.035879
68.891055	2237.283962	21.040896
68.702007	2239.696502	21.045914
68.466661	2233.392923	21.050931
69.180160	2234.673051	21.055949
68.869711	2239.216021	21.060967
69.390069	2243.758225	21.065984
69.122515	2251.210685	21.071002
69.138899	2253.995018	21.076019
69.205563	2253.255611	21.081037
69.450130	2251.304803	21.086055
69.898095	2242.896370	21.091072
69.726956	2248.601042	21.096090
69.701625	2256.157578	21.101107
69.936603	2248.808236	21.106125
69.794107	2250.235102	21.111143
69.908915	2245.972289	21.116160
69.626594	2246.196507	21.121178
69.600471	2242.085174	21.126195
70.148677	2252.919376	21.131213
70.021577	2250.057886	21.136231
70.284233	2239.718568	21.141248
70.131706	2246.673283	21.146266
70.329771	2243.685103	21.151283
70.203526	2239.968186	21.156301
69.761822	2247.750913	21.161319
70.118788	2250.134717	21.166336
70.483968	2264.731233	21.171354
70.307378	2271.506675	21.176371
70.565380	2271.545244	21.181389
70.816419	2268.409893	21.186407
70.792957	2262.824252	21.191424
70.669037	2271.343063	21.196442
70.843132	2270.126036	21.201459
70.717152	2280.841801	21.206477
70.992533	2289.298060	21.211495
71.182600	2283.069835	21.216512
71.401181	2282.224567	21.221530
71.408573	2280.336164	21.226547
71.492009	2287.092965	21.231565
71.224110	2287.535849	21.236583
71.816686	2288.083781	21.241600
71.556742	2292.281151	21.246618
71.307782	2292.465425	21.251635
71.501751	2291.683978	21.256653
71.601328	2290.740579	21.261671
71.719733	2303.437959	21.266688
71.971542	2312.232466	21.271706
72.106572	2316.260653	21.276723
71.868661	2316.146525	21.281741
71.858882	2319.957537	21.286759
72.047496	2307.231159	21.291776
72.375138	2313.340585	21.296794
71.973910	2310.481005	21.301811
72.404761	2324.341383	21.306829
72.350900	2331.675182	21.311847
72.392388	2332.555631	21.316864
72.769078	2331.196396	21.321882
72.843696	2342.338402	21.326899
72.845496	2337.739791	21.331917
72.625561	2340.359173	21.336935
72.900540	2328.465079	21.341952
72.705010	2330.367361	21.346970
72.908042	2326.854479	21.351987
73.055723	2322.681181	21.357005
72.797700	2333.506035	21.362023
73.216379	2347.134788	21.367040
72.783021	2348.897592	21.372058
72.995326	2352.487608	21.377075
73.360874	2353.535056	21.382093
73.380421	2361.535926	21.387111
73.654951	2369.777742	21.392128
73.922433	2377.155896	21.397146
73.786489	2375.305721	21.402163
74.185311	2374.574234	21.407181
73.723350	2372.409031	21.412199
74.036920	2370.542083	21.417216
74.150481	2374.763012	21.422234
74.375686	2374.358554	21.427251
74.218531	2360.638488	21.432269
74.367791	2374.685047	21.437287
74.239289	2368.424646	21.442304
74.658181	2372.228474	21.447322
74.348994	2374.442085	21.452339
74.436730	2372.815665	21.457357
74.848842	2381.629276	21.462375
75.031497	2389.591979	21.467392
75.221900	2395.094872	21.472410
74.945432	2383.811052	21.477427
75.131227	2373.095500	21.482445
75.059566	2384.178392	21.487463
75.036540	2383.061675	21.492480
75.370911	2386.623105	21.497498
75.536470	2384.318555	21.502515
75.563780	2383.632649	21.507533
75.242106	2390.938998	21.512551
75.640819	2378.675159	21.517568
75.180526	2385.349912	21.522586
75.560191	2386.388839	21.527603
75.703010	2385.104114	21.532621
75.535052	2389.353373	21.537639
75.825964	2395.831533	21.542656
75.779880	2399.578817	21.547674
75.654737	2403.483669	21.552691
76.067713	2407.370490	21.557709
76.041093	2404.464827	21.562727
76.005496	2414.383800	21.567744
76.464501	2407.008762	21.572762
76.075970	2428.329214	21.577779
76.314414	2428.594931	21.582797
76.067644	2434.646058	21.587815
76.502341	2433.779547	21.592832
76.691931	2427.232581	21.597850
76.556338	2425.319224	21.602867
76.778087	2436.106846	21.607885
76.811207	2442.824247	21.612903
77.184814	2453.420814	21.617920
77.503798	2449.286925	21.622938
77.087052	2462.907786	21.627955
77.139600	2453.428165	21.632973
77.265878	2455.516749	21.637991
77.151041	2450.137889	21.643008
77.412059	2449.718350	21.648026
76.974586	2459.053309	21.653043
77.474314	2454.667018	21.658061
77.489329	2468.526380	21.663079
77.564561	2468.397906	21.668096
77.733591	2473.474942	21.673114
77.417249	2481.014044	21.678131
78.088256	2480.132600	21.683149
78.134810	2476.442214	21.688167
77.771873	2472.860172	21.693184
78.195693	2484.777612	21.698202
78.350211	2496.863497	21.703219
78.284553	2492.303821	21.708237
78.772109	2494.957561	21.713255
78.643161	2500.696732	21.718272
78.688286	2497.085468	21.723290
78.723558	2489.669477	21.728307
79.057516	2482.954691	21.733325
78.944888	2493.674804	21.738343
78.846799	2487.501124	21.743360
78.950855	2493.850790	21.748378
78.378999	2495.777332	21.753395
79.057154	2496.425483	21.758413
79.110466	2512.563906	21.763431
79.267364	2511.128629	21.768448
79.275888	2512.105779	21.773466
79.396365	2511.692478	21.778483
79.477335	2502.441930	21.783501
79.410528	2515.783921	21.788519
79.123863	2524.666053	21.793536
79.835965	2533.521111	21.798554
80.162664	2541.543373	21.803571
80.152420	2537.306396	21.808589
80.085767	2537.941840	21.813607
79.974917	2541.898136	21.818624
80.254920	2534.939294	21.823642
80.134424	2537.240137	21.828659
80.213224	2538.313586	21.833677
80.080847	2544.924398	21.838695
80.314764	2544.209272	21.843712
80.405345	2553.572011	21.848730
80.200082	2562.526624	21.853747
80.681886	2556.599772	21.858765
80.621158	2566.333398	21.863783
81.082901	2578.087152	21.868800
80.953307	2571.435492	21.873818
80.893314	2576.920861	21.878835
81.036989	2573.931681	21.883853
81.232956	2581.144381	21.888871
81.180557	2576.143904	21.893888
81.711775	2572.926731	21.898906
81.603112	2571.652989	21.903923
81.585583	2561.679309	21.908941
81.814155	2580.848620	21.913959
81.805048	2585.881006	21.918976
82.328564	2591.445391	21.923994
82.507942	2583.315591	21.929011
82.436195	2579.602689	21.934029
82.471611	2560.783557	21.939047
82.152044	2560.006809	21.944064
82.280294	2560.296106	21.949082
82.390927	2565.678992	21.954099
82.649476	2555.037149	21.959117
82.415150	2569.958239	21.964135
82.148687	2583.315780	21.969152
83.094930	2578.569138	21.974170
82.817742	2592.000957	21.979187
82.979124	2581.175486	21.984205
82.904478	2587.108169	21.989223
82.529024	2582.675910	21.994240
82.857968	2584.720132	21.999258
82.870256	2579.665333	22.004275
83.127627	2578.006006	22.009293
83.298806	2585.850661	22.014311
83.367399	2599.859537	22.019328
83.477897	2598.674545	22.024346
83.611486	2607.525593	22.029363
83.406827	2604.363740	22.034381
83.668183	2602.217742	22.039399
83.195549	2608.313782	22.044416
83.563275	2595.211963	22.049434
83.462545	2601.795744	22.054451
83.498570	2614.676682	22.059469
83.916888	2625.869168	22.064487
83.973788	2631.415144	22.069504
84.018259	2621.204476	22.074522
84.032311	2646.609274	22.079539
84.337983	2648.818113	22.084557
84.411550	2645.612663	22.089575
84.198956	2656.181258	22.094592
84.549575	2651.647850	22.099610
84.573976	2655.071686	22.104627
84.980359	2664.059922	22.109645
84.952210	2673.400296	22.114663
84.957166	2683.439309	22.119680
85.248794	2668.420954	22.124698
85.189073	2674.212456	22.129715
85.099479	2674.128742	22.134733
85.256378	2667.356413	22.139751
85.189348	2679.859025	22.144768
85.063978	2676.511149	22.149786
85.782558	2685.280052	22.154803
85.851508	2694.942932	22.159821
86.112498	2693.109438	22.164839
85.906881	2695.919153	22.169856
85.997665	2693.765150	22.174874
86.090465	2687.365813	22.179891
86.033422	2691.862881	22.184909
86.499704	2684.518153	22.189927
86.293635	2689.941227	22.194944
86.412399	2681.634667	22.199962
86.313242	2698.964919	22.204979
86.995228	2707.824782	22.209997
86.833533	2705.729271	22.215015
86.779385	2718.116271	22.220032
86.707818	2708.482372	22.225050
86.816685	2705.861580	22.230067
87.017395	2703.387363	22.235085
87.116379	2704.498690	22.240103
86.928102	2713.457029	22.245120
87.413794	2701.283497	22.250138
87.361303	2711.426210	22.255155
87.775705	2724.052264	22.260173
87.515162	2735.603670	22.265191
87.222529	2732.244115	22.270208
87.426725	2727.288611	22.275226
87.749763	2730.473147	22.280243
87.623973	2728.387789	22.285261
88.142741	2721.249441	22.290279
87.859136	2725.696798	22.295296
88.199360	2733.628655	22.300314
88.258854	2746.815314	22.305331
88.322335	2752.884218	22.310349
88.535809	2752.459498	22.315367
88.258091	2754.109583	22.320384
88.507316	2753.152183	22.325402
88.339295	2749.596357	22.330419
88.239769	2747.784624	22.335437
88.765667	2759.948216	22.340455
88.651099	2764.277570	22.345472
88.886119	2767.362282	22.350490
89.053342	2775.860966	22.355507
89.169316	2777.196879	22.360525
89.191601	2780.580040	22.365543
89.053946	2776.145193	22.370560
89.395541	2785.828529	22.375578
89.378304	2786.598267	22.380595
89.179090	2805.667563	22.385613
89.639164	2803.913334	22.390631
89.757255	2803.797081	22.395648
89.819120	2802.622851	22.400666
89.945558	2795.429164	22.405683
89.780572	2804.399679	22.410701
90.165316	2810.727575	22.415719
90.274994	2819.954902	22.420736
90.209151	2814.047488	22.425754
90.358617	2806.973278	22.430771
90.638900	2818.294821	22.435789
90.822768	2811.890640	22.440807
90.769631	2816.696432	22.445824
90.988630	2815.488115	22.450842
91.276553	2807.685231	22.455859
90.944666	2805.865710	22.460877
91.032689	2794.060567	22.465895
91.399331	2820.780147	22.470912
91.675352	2815.832303	22.475930
91.661196	2811.507501	22.480947
91.236168	2820.897507	22.485965
91.440469	2826.426762	22.490983
91.309360	2830.487292	22.496000
91.394219	2820.308058	22.501018
91.655378	2823.066754	22.506035
91.558194	2831.101902	22.511053
91.741645	2842.205074	22.516071
91.902145	2845.986364	22.521088
91.759690	2842.596947	22.526106
92.125905	2837.038449	22.531123
92.203949	2846.046657	22.536141
92.658006	2851.852408	22.541159
92.583387	2863.709321	22.546176
92.623220	2866.625791	22.551194
92.892566	2872.466799	22.556211
92.645126	2874.257335	22.561229
92.995774	2859.863967	22.566247
93.137167	2863.594599	22.571264
93.039322	2859.910978	22.576282
93.300817	2859.008461	22.581299
92.843412	2865.594565	22.586317
93.045540	2875.473390	22.591335
93.114986	2886.288301	22.596352
93.738537	2877.609039	22.601370
94.052655	2883.477755	22.606387
93.656355	2884.139608	22.611405
93.788885	2874.173807	22.616423
93.870516	2888.193489	22.621440
93.864540	2891.451695	22.626458
94.054110	2893.956499	22.631475
93.882676	2898.929188	22.636493
94.351981	2904.600007	22.641511
94.083866	2898.998844	22.646528
94.591788	2890.927898	22.651546
94.663913	2907.287817	22.656563
94.535146	2911.575244	22.661581
95.061393	2918.587994	22.666599
94.906558	2929.053014	22.671616
94.838634	2929.013246	22.676634
95.185707	2932.250865	22.681651
95.041927	2923.597115	22.686669
94.843217	2919.629446	22.691687
95.111442	2928.573182	22.696704
95.138250	2926.760574	22.701722
95.359269	2933.707528	22.706739
94.942892	2948.010433	22.711757
95.664586	2951.268268	22.716775
95.759164	2950.085748	22.721792
95.609058	2948.951031	22.726810
96.149230	2948.001694	22.731827
95.648698	2954.250561	22.736845
96.043671	2957.247121	22.741863
96.142294	2963.152781	22.746880
96.192626	2965.168107	22.751898
96.414957	2971.417350	22.756915
96.463460	2964.264211	22.761933
96.515454	2975.782586	22.766951
96.850535	2984.838967	22.771968
96.851707	2993.253302	22.776986
97.033982	2994.749279	22.782003
96.786575	2997.960113	22.787021
96.772447	2990.586373	22.792039
96.988771	2992.818723	22.797056
97.414112	3004.559525	22.802074
97.278519	3014.374558	22.807091
97.490259	3031.545953	22.812109
97.696825	3028.925589	22.817127
97.769208	3020.831293	22.822144
97.672895	3020.704443	22.827162
97.748187	3014.058392	22.832179
97.865413	3017.177383	22.837197
97.845320	3033.917984	22.842215
98.460431	3042.577027	22.847232
98.394557	3049.123948	22.852250
98.596444	3040.043553	22.857267
98.299438	3046.891807	22.862285
98.693834	3035.234192	22.867303
98.564777	3037.959372	22.872320
98.600648	3047.949557	22.877338
98.748265	3047.790802	22.882355
98.547472	3058.884871	22.887373
98.799849	3056.352012	22.892391
99.011383	3062.183203	22.897408
99.224194	3082.349725	22.902426
99.710997	3087.042590	22.907443
99.414662	3092.972297	22.912461
99.864868	3075.302786	22.917479
99.565250	3081.813747	22.922496
99.538874	3091.453900	22.927514
99.838602	3082.938899	22.932531
99.687786	3088.135657	22.937549
100.289804	3088.360205	22.942567
100.117644	3100.545021	22.947584
100.235136	3105.485125	22.952602
100.444013	3098.035372	22.957619
100.324022	3096.949584	22.962637
100.510016	3092.296673	22.967655
100.740201	3100.804583	22.972672
100.953464	3120.926892	22.977690
101.340462	3124.287696	22.982707
101.320278	3133.301969	22.987725
101.385926	3122.645827	22.992743
101.463909	3127.295442	22.997760
101.320724	3128.984450	23.002778
101.426541	3121.790708	23.007795
101.613288	3126.962996	23.012813
101.771530	3122.450143	23.017831
102.050113	3120.957879	23.022848
101.876566	3122.872580	23.027866
101.527856	3113.619601	23.032883
101.288920	3121.039529	23.037901
101.617013	3119.078701	23.042919
101.463165	3136.108631	23.047936
102.236012	3143.998141	23.052954
102.363181	3142.842065	23.057971
102.596386	3143.818766	23.062989
102.638384	3149.679703	23.068007
102.669674	3131.207807	23.073024
102.544163	3148.425839	23.078042
102.821373	3145.194708	23.083059
103.164336	3168.225728	23.088077
102.954882	3154.945653	23.093095
103.033513	3156.161196	23.098112
102.972696	3160.930408	23.103130
103.086748	3160.568599	23.108147
103.316098	3182.938849	23.113165
103.159205	3182.114492	23.118183
103.405669	3184.152769	23.123200
103.354443	3194.750054	23.128218
103.785012	3197.131924	23.133235
103.797080	3207.056490	23.138253
103.975448	3201.628311	23.143271
103.882387	3209.101171	23.148288
104.101742	3226.880714	23.153306
104.462849	3226.240323	23.158323
104.651742	3221.782612	23.163341
104.563908	3222.007930	23.168359
105.040674	3225.424127	23.173376
104.723894	3228.402839	23.178394
105.012821	3222.480740	23.183411
105.035423	3239.129624	23.188429
105.496075	3244.205377	23.193447
105.591801	3245.225717	23.198464
105.497054	3253.503702	23.203482
105.706718	3249.194229	23.208499
105.720273	3252.938659	23.213517
105.918706	3244.581483	23.218535
105.956849	3246.822843	23.223552
106.102584	3251.083126	23.228570
106.437286	3248.104937	23.233587
106.538190	3250.955089	23.238605
106.408840	3236.939622	23.243623
106.437290	3233.128825	23.248640
106.075432	3237.967315	23.253658
106.410151	3250.562037	23.258675
106.531403	3252.051815	23.263693
106.619931	3261.910776	23.268711
106.873832	3262.767461	23.273728
106.425773	3262.780935	23.278746
107.038545	3272.324205	23.283763
106.728633	3283.795321	23.288781
106.704452	3290.111703	23.293799
107.249097	3282.416738	23.298816
107.445993	3310.700735	23.303834
107.695424	3305.747455	23.308851
107.784207	3315.524342	23.313869
107.709926	3311.729623	23.318887
108.183256	3300.656004	23.323904
108.018019	3310.737811	23.328922
107.831620	3304.353592	23.333939
108.300065	3327.207343	23.338957
108.260179	3332.225822	23.343975
108.597811	3334.511803	23.348992
108.352804	3340.802831	23.354010
108.665370	3332.935892	23.359027
108.748555	3332.316947	23.364045
108.854163	3339.017013	23.369063
108.831119	3329.163711	23.374080
108.836837	3343.451298	23.379098
109.353967	3349.537706	23.384115
109.350333	3354.951357	23.389133
109.059171	3356.278506	23.394151
109.319763	3352.522845	23.399168
109.373551	3363.668747	23.404186
109.576069	3367.459346	23.409203
109.820883	3374.096585	23.414221
109.711322	3379.075492	23.419239
109.844876	3379.695380	23.424256
109.751999	3384.229798	23.429274
109.583647	3393.270570	23.434291
110.109683	3408.272070	23.439309
110.144253	3411.675519	23.444327
110.749443	3425.077026	23.449344
110.587261	3426.052564	23.454362
111.086471	3426.940263	23.459379
111.360141	3428.248363	23.464397
110.844808	3428.316564	23.469415
111.066173	3422.423923	23.474432
111.456267	3432.248355	23.479450
111.524507	3440.144230	23.484467
111.876261	3439.426392	23.489485
111.505120	3445.920282	23.494503
111.746701	3443.849878	23.499520
111.972467	3450.108220	23.504538
112.006393	3456.295618	23.509555
112.105194	3447.966583	23.514573
112.479479	3454.779257	23.519591
112.647056	3438.668687	23.524608
112.561285	3442.027870	23.529626
112.511476	3430.332283	23.534643
112.623241	3446.743293	23.539661
113.038080	3457.965251	23.544679
112.881635	3461.146133	23.549696
112.800439	3461.556635	23.554714
113.082471	3460.467809	23.559731
113.169556	3467.874677	23.564749
113.176126	3471.266742	23.569767
113.355187	3477.724944	23.574784
113.554627	3491.742420	23.579802
114.018485	3485.316230	23.584819
113.819886	3486.644668	23.589837
113.794687	3495.637813	23.594855
113.765524	3480.489135	23.599872
113.688934	3487.934279	23.604890
113.978420	3495.031694	23.609907
114.289353	3503.915369	23.614925
114.085492	3508.072669	23.619943
114.639059	3511.435858	23.624960
114.813177	3526.713532	23.629978
114.800534	3530.263277	23.634995
115.303123	3533.394578	23.640013
115.059300	3534.307161	23.645031
115.103345	3521.327979	23.650048
115.304762	3525.835263	23.655066
115.631538	3524.846737	23.660083
115.507792	3531.251397	23.665101
115.194906	3544.793673	23.670119
115.800829	3551.630063	23.675136
115.789091	3546.742885	23.680154
115.830466	3551.502502	23.685171
116.095374	3542.768644	23.690189
115.707498	3553.428351	23.695207
116.003043	3559.315980	23.700224
116.024603	3566.079800	23.705242
116.451020	3564.636935	23.710259
116.342796	3575.486408	23.715277
116.475538	3595.271511	23.720295
116.687341	3592.694434	23.725312
117.127315	3603.265503	23.730330
117.182933	3588.520084	23.735347
117.236031	3590.572922	23.740365
117.312238	3592.587420	23.745383
117.778841	3586.034512	23.750400
117.237854	3591.627110	23.755418
117.544383	3599.709821	23.760435
117.547818	3611.722280	23.765453
117.655959	3623.629967	23.770471
117.856830	3607.428811	23.775488
118.172260	3622.725459	23.780506
118.494357	3632.172428	23.785523
118.388145	3625.526183	23.790541
118.542571	3638.506086	23.795559
118.760027	3628.902166	23.800576
118.889338	3643.580948	23.805594
119.125429	3632.197101	23.810611
119.478192	3637.400341	23.815629
118.920396	3646.240279	23.820647
118.967871	3634.526161	23.825664
119.368893	3647.328560	23.830682
119.320159	3647.374160	23.835699
119.591770	3656.030503	23.840717
119.313794	3658.106811	23.845735
119.687096	3663.493063	23.850752
119.865002	3677.192113	23.855770
120.043754	3690.480718	23.860787
120.147486	3687.690148	23.865805
120.069551	3691.834074	23.870823
120.176363	3685.236497	23.875840
120.142253	3696.655194	23.880858
120.133639	3702.836716	23.885875
120.670230	3699.138746	23.890893
120.725624	3719.049731	23.895911
120.817098	3725.382865	23.900928
121.019293	3727.065163	23.905946
120.798191	3729.984777	23.910963
121.476996	3735.193779	23.915981
121.573928	3748.782472	23.920999
121.520250	3756.151541	23.926016
121.882317	3750.236750	23.931034
121.713551	3747.684556	23.936051
122.273311	3746.189224	23.941069
122.322045	3747.352677	23.946087
122.531216	3749.624119	23.951104
122.784137	3759.110399	23.956122
122.380690	3767.531673	23.961139
122.775754	3768.533553	23.966157
123.041505	3768.394161	23.971175
123.136933	3763.187127	23.976192
123.206424	3772.437020	23.981210
123.286857	3767.074517	23.986227
123.216267	3755.457727	23.991245
123.379235	3763.547221	23.996263
123.403673	3759.424464	24.001280
123.108975	3769.277458	24.006298
123.390277	3786.141979	24.011315
124.069147	3778.198521	24.016333
123.902595	3795.587729	24.021351
123.857834	3782.982096	24.026368
123.976146	3795.506945	24.031386
124.145525	3813.866194	24.036403
124.481462	3807.412587	24.041421
124.186232	3813.408638	24.046439
124.480147	3813.602562	24.051456
124.649317	3818.058157	24.056474
124.689460	3830.418521	24.061491
125.288576	3832.114397	24.066509
125.052994	3834.692254	24.071527
124.977848	3837.102941	24.076544
125.191796	3838.164765	24.081562
125.301575	3843.169406	24.086579
125.620369	3850.909423	24.091597
125.574282	3849.720475	24.096615
126.012504	3837.752471	24.101632
126.032082	3845.918125	24.106650
125.993659	3869.596874	24.111667
126.292554	3869.884709	24.116685
126.359822	3864.555804	24.121703
126.393577	3866.387602	24.126720
126.589067	3867.168248	24.131738
126.295006	3881.294906	24.136755
127.168111	3888.136912	24.141773
126.982594	3894.062142	24.146791
126.959634	3898.147001	24.151808
127.111820	3895.522407	24.156826
127.130628	3913.779094	24.161843
127.308057	3915.616795	24.166861
127.211636	3918.671568	24.171879
127.716890	3923.806811	24.176896
127.693178	3937.092598	24.181914
127.929649	3939.296660	24.186931
127.855978	3935.545903	24.191949
128.105293	3939.644928	24.196967
128.549832	3953.753775	24.201984
128.658738	3962.432600	24.207002
128.399550	3964.108296	24.212019
129.021610	3949.873550	24.217037
129.178071	3964.358957	24.222055
129.267611	3977.134636	24.227072
129.578216	3980.097243	24.232090
129.458739	3984.787484	24.237107
129.856120	3977.976989	24.242125
129.719274	3982.767798	24.247143
129.817834	3980.069529	24.252160
129.828865	3967.912700	24.257178
129.592208	3984.817522	24.262195
129.853073	3988.267692	24.267213
130.039635	3993.440259	24.272231
130.492358	4005.729792	24.277248
130.476544	3997.872980	24.282266
130.743111	4010.021237	24.287283
130.450032	4025.378841	24.292301
130.664998	4028.479539	24.297319
131.050702	4036.474289	24.302336
131.410172	4033.653069	24.307354
131.530264	4051.177527	24.312371
131.609484	4049.744832	24.317389
131.623159	4045.983524	24.322407
131.801087	4047.259324	24.327424
132.059792	4050.334235	24.332442
131.699135	4048.610626	24.337459
131.995636	4046.222225	24.342477
132.340840	4067.660070	24.347495
132.484457	4070.636228	24.352512
132.776424	4067.910802	24.357530
132.258478	4070.738094	24.362547
132.548799	4071.731152	24.367565
132.779139	4078.298322	24.372583
132.654447	4095.125733	24.377600
133.190977	4091.831714	24.382618
132.897484	4093.471762	24.387635
133.108594	4090.607493	24.392653
133.151400	4110.473535	24.397671
133.375139	4115.277327	24.402688
133.751084	4112.867002	24.407706
133.460781	4123.947338	24.412723
133.866000	4136.329626	24.417741
134.456713	4140.564595	24.422759
134.011194	4140.928028	24.427776
134.348843	4141.774793	24.432794
134.346305	4151.837890	24.437811
134.614575	4153.535129	24.442829
134.839116	4160.160052	24.447847
135.217776	4152.967345	24.452864
135.199262	4171.678348	24.457882
134.965506	4171.434138	24.462899
135.584573	4177.126091	24.467917
135.322373	4193.574273	24.472935
135.585127	4186.847921	24.477952
135.712254	4191.165000	24.482970
136.014472	4197.026542	24.487987
136.282391	4199.216240	24.493005
136.113747	4200.243333	24.498023
136.170851	4213.324120	24.503040
136.731551	4207.895714	24.508058
136.482024	4205.835881	24.513075
136.673994	4212.393330	24.518093
136.992974	4236.903517	24.523111
137.138950	4234.314569	24.528128
137.115683	4228.106475	24.533146
136.865579	4237.248855	24.538163
137.018435	4239.715411	24.543181
137.320894	4247.663324	24.548199
137.289573	4261.626015	24.553216
137.849831	4272.481649	24.558234
137.763224	4284.975813	24.563251
137.945773	4275.951490	24.568269
137.994708	4284.633552	24.573287
138.513575	4298.308063	24.578304
139.104586	4292.568710	24.583322
139.171584	4293.347410	24.588339
138.892999	4289.956951	24.593357
139.005493	4283.345641	24.598375
139.196732	4289.445550	24.603392
139.242312	4288.800900	24.608410
139.232377	4306.601647	24.613427
139.743952	4308.781593	24.618445
139.825182	4305.473643	24.623463
139.661030	4316.111370	24.628480
139.955387	4306.918006	24.633498
140.056421	4311.895740	24.638515
140.387135	4325.138910	24.643533
140.718221	4335.070931	24.648551
141.067708	4327.876412	24.653568
141.057675	4327.912794	24.658586
141.006184	4329.612799	24.663603
141.250355	4321.367908	24.668621
141.323833	4323.941604	24.673639
141.294584	4329.268023	24.678656
141.491403	4332.551533	24.683674
141.682319	4348.496435	24.688691
141.653885	4347.702400	24.693709
141.921470	4348.866327	24.698727
141.891724	4358.394051	24.703744
141.494142	4347.307888	24.708762
142.024297	4364.512735	24.713779
142.107499	4372.441395	24.718797
142.257036	4386.473697	24.723815
141.759093	4390.724617	24.728832
142.080480	4395.898272	24.733850
142.384569	4406.162832	24.738867
142.668571	4416.831413	24.743885
143.185890	4424.647894	24.748903
143.109170	4439.814129	24.753920
143.102461	4423.366998	24.758938
143.208549	4443.898971	24.763955
143.451537	4448.504137	24.768973
143.822581	4449.948569	24.773991
143.586486	4456.500570	24.779008
144.124905	4469.376721	24.784026
144.422323	4479.733905	24.789043
144.565819	4478.480494	24.794061
144.685260	4478.083096	24.799079
144.507094	4491.080996	24.804096
144.766727	4490.623757	24.809114
145.154961	4498.962371	24.814131
145.221163	4501.338375	24.819149
145.156758	4502.563793	24.824167
144.881100	4504.633519	24.829184
145.591237	4523.259137	24.834202
145.601150	4524.671771	24.839219
145.708580	4524.774975	24.844237
146.196741	4535.970337	24.849255
146.164709	4557.767727	24.854272
146.358734	4543.340747	24.859290
146.529745	4557.836975	24.864307
146.212638	4558.767401	24.869325
146.251467	4560.080813	24.874343
146.702670	4570.783264	24.879360
146.614316	4580.348694	24.884378
147.187198	4585.685018	24.889395
147.074651	4591.248674	24.894413
147.764209	4599.088750	24.899431
147.687474	4618.557420	24.904448
147.739492	4619.366889	24.909466
147.980951	4620.197184	24.914483
148.028562	4615.066840	24.919501
148.362278	4624.686116	24.924519
148.336410	4631.587180	24.929536
148.491290	4636.865903	24.934554
149.166161	4643.511991	24.939571
148.907969	4638.435863	24.944589
148.849410	4639.300534	24.949607
149.386300	4662.322018	24.954624
149.244224	4661.937178	24.959642
149.426996	4658.262886	24.964659
149.439302	4670.498768	24.969677
149.879976	4675.117212	24.974695
149.702770	4691.748230	24.979712
150.054914	4688.678696	24.984730
150.055426	4688.151570	24.989747
149.928654	4704.200216	24.994765
150.517100	4715.421013	24.999783
150.691465	4721.507929	25.004800
150.833410	4711.391289	25.009818
151.054191	4727.069855	25.014835
151.156982	4737.100993	25.019853
151.535203	4734.058931	25.024871
151.763052	4742.018752	25.029888
151.395668	4739.989947	25.034906
151.450825	4738.586220	25.039923
151.629055	4749.132682	25.044941
152.239232	4760.309068	25.049959
151.945680	4761.153743	25.054976
151.994585	4760.707416	25.059994
152.580127	4766.202793	25.065011
152.336823	4771.540781	25.070029
152.685335	4777.243747	25.075047
152.809408	4789.616868	25.080064
153.090980	4783.578626	25.085082
153.314581	4790.630058	25.090099
153.412257	4801.056597	25.095117
153.482200	4794.887366	25.100135
153.308997	4806.925134	25.105152
153.670718	4804.602175	25.110170
153.889611	4821.925665	25.115187
154.101615	4831.646189	25.120205
154.236145	4825.886647	25.125223
154.606615	4831.302103	25.130240
154.476451	4829.109864	25.135258
154.951570	4845.477843	25.140275
154.631452	4847.911259	25.145293
155.521760	4845.840076	25.150311
155.092618	4855.263335	25.155328
155.061550	4856.098458	25.160346
155.281204	4877.676879	25.165363
155.348262	4882.410727	25.170381
155.540654	4887.734151	25.175399
155.588674	4910.229641	25.180416
155.762667	4904.451266	25.185434
156.173255	4912.177357	25.190451
156.197733	4934.499800	25.195469
156.613001	4932.869188	25.200487
156.434440	4945.352958	25.205504
156.506798	4954.883937	25.210522
156.876970	4958.124621	25.215539
157.007387	4962.305638	25.220557
157.201820	4967.612983	25.225575
157.082247	4983.796479	25.230592
157.564063	4977.802559	25.235610
158.119983	4993.820263	25.240627
157.875070	5006.854240	25.245645
158.242148	5006.238112	25.250663
158.621429	5003.883968	25.255680
158.454748	5003.297799	25.260698
158.535944	5012.688536	25.265715
158.780300	5033.199513	25.270733
159.043217	5023.859200	25.275751
159.218645	5032.326097	25.280768
159.407747	5043.167743	25.285786
159.707064	5041.220692	25.290803
159.614835	5049.543292	25.295821
159.770538	5047.634522	25.300839
159.814939	5052.779160	25.305856
160.269286	5055.334327	25.310874
160.866839	5061.023620	25.315891
160.739932	5065.137651	25.320909
160.709031	5061.787157	25.325927
160.644019	5072.558152	25.330944
160.630478	5071.054682	25.335962
161.264493	5085.295714	25.340979
161.064709	5089.108668	25.345997
161.089532	5083.798681	25.351015
161.629352	5102.953474	25.356032
161.997053	5115.433852	25.361050
162.089964	5111.233773	25.366067
161.687769	5114.421876	25.371085
161.967279	5124.081476	25.376103
162.236098	5133.739600	25.381120
162.242597	5145.831509	25.386138
162.801836	5132.786246	25.391155
162.686958	5156.036729	25.396173
163.103261	5165.195120	25.401191
162.888655	5165.288805	25.406208
162.943691	5166.271438	25.411226
163.279876	5171.218882	25.416243
163.354363	5190.610810	25.421261
163.545607	5194.397248	25.426279
163.466519	5193.970963	25.431296
163.813815	5209.415478	25.436314
163.671096	5216.710703	25.441331
163.967759	5229.707343	25.446349
164.274774	5235.259126	25.451367
164.771573	5235.048807	25.456384
164.665232	5246.571335	25.461402
165.175472	5261.823068	25.466419
165.418188	5255.692903	25.471437
165.436073	5262.120175	25.476455
165.774421	5265.530044	25.481472
165.434960	5279.241913	25.486490
165.535983	5278.067703	25.491507
165.526973	5294.660294	25.496525
165.692719	5306.891505	25.501543
165.968240	5314.919867	25.506560
166.416649	5329.594215	25.511578
166.641484	5330.146210	25.516595
166.823648	5344.401416	25.521613
166.947319	5344.123288	25.526631
167.282374	5351.132225	25.531648
167.540462	5369.864258	25.536666
167.740608	5364.195279	25.541683
167.758058	5362.084017	25.546701
168.022958	5372.112205	25.551719
168.219827	5382.195249	25.556736
168.271088	5382.177838	25.561754
168.480238	5378.818087	25.566771
168.825928	5389.367096	25.571789
168.825460	5397.217769	25.576807
169.121396	5405.482876	25.581824
168.929056	5408.934875	25.586842
169.196378	5411.127973	25.591859
168.964744	5427.301008	25.596877
169.565433	5424.419692	25.601895
169.784162	5423.504816	25.606912
170.000480	5445.589493	25.611930
170.354017	5444.729256	25.616947
170.218960	5458.074633	25.621965
170.600943	5453.144201	25.626983
171.007723	5470.262102	25.632000
170.729055	5481.483485	25.637018
171.260255	5483.291179	25.642035
171.002392	5476.428108	25.647053
171.210076	5482.636325	25.652071
171.838768	5490.912474	25.657088
171.672791	5502.368746	25.662106
171.939453	5491.133626	25.667123
171.668984	5510.763022	25.672141
171.781894	5518.542322	25.677159
172.305463	5517.652287	25.682176
172.029602	5535.448547	25.687194
172.668152	5535.348598	25.692212
172.816129	5551.907359	25.697229
172.766084	5553.051681	25.702247
173.082673	5567.286003	25.707264
173.079311	5564.028957	25.712282
173.488349	5577.712173	25.717300
173.534229	5598.081265	25.722317
173.599097	5600.151427	25.727335
174.271247	5595.737383	25.732352
174.612326	5620.236506	25.737370
174.862234	5623.698178	25.742388
174.632329	5621.429924	25.747405
174.799808	5627.644489	25.752423
175.054653	5619.949757	25.757440
174.774023	5619.472962	25.762458
175.020606	5618.679980	25.767476
175.202783	5635.062999	25.772493
175.133275	5638.562087	25.777511
175.407255	5648.630042	25.782528
175.542805	5668.233878	25.787546
175.653374	5670.221129	25.792564
175.763964	5687.777063	25.797581
175.990648	5699.408694	25.802599
176.517344	5710.254669	25.807616
176.627417	5712.592393	25.812634
176.939399	5711.031559	25.817652
176.953604	5728.031275	25.822669
177.650950	5737.619428	25.827687
177.867517	5729.927490	25.832704
177.591032	5744.248549	25.837722
178.152193	5754.609337	25.842740
178.366362	5763.474560	25.847757
178.641518	5760.719952	25.852775
178.480449	5759.567833	25.857792
178.831627	5755.756454	25.862810
178.959890	5778.177310	25.867828
179.220222	5783.900723	25.872845
179.017588	5788.670744	25.877863
179.257441	5781.458109	25.882880
179.439522	5797.402510	25.887898
179.706613	5804.365449	25.892916
179.895974	5805.106105	25.897933
179.740288	5821.415954	25.902951
180.077680	5829.996743	25.907968
180.199096	5839.807759	25.912986
180.663987	5849.817506	25.918004
180.562132	5861.118749	25.923021
180.664563	5868.480000	25.928039
181.437330	5873.539172	25.933056
181.114948	5890.036189	25.938074
181.272891	5886.463399	25.943092
181.440532	5892.580172	25.948109
181.819366	5907.679415	25.953127
182.304359	5908.503186	25.958144
182.033468	5915.260032	25.963162
182.496207	5922.953133	25.968180
182.779347	5936.536388	25.973197
182.716513	5937.161879	25.978215
182.820798	5945.094235	25.983232
183.158289	5956.269887	25.988250
183.179911	5950.306710	25.993268
183.695868	5954.440184	25.998285
183.241018	5981.147916	26.003303
183.842074	5978.477959	26.008320
184.112476	5989.739903	26.013338
184.391076	5994.870214	26.018356
184.864717	5999.376507	26.023373
184.748904	6004.369736	26.028391
185.033108	5995.729543	26.033408
185.311435	6012.100995	26.038426
185.185480	6020.482984	26.043444
185.354371	6007.210993	26.048461
185.524051	6032.356240	26.053479
185.953141	6036.998947	26.058496
185.875726	6048.605836	26.063514
186.192847	6047.918585	26.068532
186.036650	6057.968927	26.073549
186.276752	6069.096771	26.078567
186.683274	6072.897018	26.083584
186.576095	6070.031799	26.088602
186.791730	6074.701643	26.093620
186.946597	6075.150981	26.098637
186.957657	6088.603352	26.103655
187.457119	6102.648450	26.108672
187.618343	6113.697132	26.113690
187.664143	6114.772809	26.118708
188.138443	6119.260088	26.123725
188.228803	6136.443971	26.128743
189.007820	6127.994522	26.133760
188.857790	6129.770109	26.138778
188.987714	6131.132499	26.143796
188.911690	6146.584149	26.148813
189.352450	6155.063666	26.153831
189.455965	6158.343186	26.158848
189.919597	6171.557411	26.163866
189.578366	6182.735358	26.168884
189.865296	6185.550517	26.173901
190.064321	6189.443274	26.178919
190.343931	6200.056771	26.183936
190.400162	6206.364725	26.188954
190.532582	6218.778547	26.193972
190.868310	6220.459102	26.198989
191.133646	6229.468061	26.204007
191.483293	6228.766238	26.209024
191.472698	6257.295675	26.214042
191.833600	6256.756239	26.219060
191.654825	6266.396696	26.224077
192.147420	6277.946000	26.229095
192.422084	6273.647732	26.234112
192.803330	6281.830425	26.239130
192.321278	6289.753770	26.244148
192.727782	6305.379346	26.249165
192.901446	6311.662625	26.254183
193.575708	6323.050913	26.259200
193.756651	6328.464944	26.264218
193.908130	6339.123849	26.269236
193.860189	6342.465011	26.274253
193.933932	6343.053336	26.279271
194.354523	6349.761992	26.284288
194.365821	6360.600709	26.289306
194.569322	6374.799713	26.294324
194.864971	6379.870639	26.299341
194.769480	6391.903587	26.304359
195.325190	6397.868188	26.309376
195.797802	6401.705503	26.314394
195.656669	6408.347498	26.319412
196.343839	6403.779386	26.324429
195.920287	6417.025444	26.329447
196.105272	6426.337513	26.334464
196.473722	6428.685360	26.339482
196.606274	6442.125272	26.344500
197.053879	6450.212412	26.349517
197.193327	6460.557592	26.354535
197.491996	6457.028939	26.359552
197.861462	6463.553081	26.364570
197.799168	6479.343796	26.369588
197.861504	6470.024701	26.374605
197.729233	6480.541889	26.379623
197.804821	6492.200853	26.384640
198.160064	6489.098970	26.389658
198.297617	6512.646251	26.394676
198.589127	6526.648490	26.399693
198.352348	6529.943506	26.404711
199.121958	6542.529211	26.409728
199.109476	6554.303030	26.414746
199.342022	6564.106495	26.419764
199.657626	6573.556018	26.424781
199.560131	6577.615270	26.429799
200.101789	6585.618285	26.434816
199.999417	6598.574239	26.439834
200.348119	6605.783560	26.444852
200.318509	6609.248171	26.449869
200.728951	6624.090510	26.454887
201.091221	6633.254951	26.459904
201.410381	6642.015763	26.464922
201.426621	6654.094515	26.469940
201.813450	6660.985358	26.474957
202.035081	6666.532016	26.479975
201.535430	6684.367603	26.484992
202.055128	6680.261305	26.490010
202.059779	6699.476364	26.495028
202.783174	6706.990062	26.500045
202.870444	6711.118261	26.505063
202.763137	6723.888823	26.510080
203.243186	6741.552045	26.515098
203.037193	6750.638256	26.520116
203.569214	6759.539404	26.525133
203.656931	6775.180598	26.530151
203.977401	6793.307673	26.535168
204.664221	6802.759139	26.540186
204.292923	6805.573336	26.545204
204.764462	6806.683378	26.550221
205.044765	6813.174261	26.555239
205.534115	6818.877907	26.560256
205.363874	6834.954171	26.565274
205.568922	6836.456375	26.570292
205.983220	6833.130517	26.575309
206.116631	6848.502595	26.580327
206.371372	6859.066704	26.585344
206.791088	6858.596962	26.590362
206.571026	6867.578100	26.595380
206.961509	6872.315464	26.600397
207.174982	6883.495329	26.605415
207.221883	6887.513087	26.610432
207.791220	6893.889268	26.615450
207.498526	6900.760381	26.620468
207.977118	6905.105124	26.625485
208.148349	6930.185066	26.630503
208.158436	6929.331216	26.635520
208.483377	6930.404251	26.640538
208.820313	6963.315763	26.645556
208.924219	6961.983152	26.650573
209.093547	6968.412553	26.655591
209.312934	6979.105389	26.660608
209.652049	6981.565239	26.665626
209.466537	6993.953628	26.670644
210.022980	7009.660495	26.675661
209.716867	7018.977191	26.680679
210.382065	7036.207610	26.685696
210.759041	7036.319116	26.690714
210.661546	7039.510322	26.695732
210.970866	7051.085671	26.700749
211.371470	7062.978202	26.705767
210.848636	7071.732221	26.710784
211.587479	7081.144114	26.715802
211.452100	7102.777626	26.720820
211.967180	7111.170180	26.725837
211.746559	7117.196656	26.730855
212.181380	7137.875887	26.735872
212.693400	7136.349895	26.740890
212.629334	7159.954847	26.745908
213.271044	7162.578832	26.750925
213.393890	7182.192593	26.755943
213.589160	7197.065948	26.760960
213.599904	7191.691261	26.765978
213.811499	7194.663598	26.770996
214.162217	7201.099391	26.776013
214.085291	7211.706192	26.781031
214.532664	7216.491558	26.786048
214.909066	7223.968280	26.791066
214.739194	7236.509071	26.796084
215.368089	7238.895148	26.801101
215.488150	7263.655239	26.806119
215.745168	7268.192628	26.811136
215.865947	7269.913271	26.816154
216.123043	7289.910204	26.821172
216.187547	7286.320213	26.826189
216.714958	7296.601931	26.831207
216.347701	7308.185568	26.836224
216.822924	7307.975461	26.841242
216.857787	7329.228991	26.846260
216.957042	7338.918003	26.851277
217.117057	7359.924661	26.856295
217.385993	7369.508184	26.861312
217.740917	7374.604829	26.866330
218.048363	7393.801591	26.871348
218.541072	7395.634456	26.876365
218.686860	7413.009739	26.881383
218.775926	7418.908874	26.886400
219.672419	7430.095723	26.891418
219.801758	7435.022521	26.896436
219.693112	7433.767372	26.901453
219.966127	7437.339422	26.906471
219.936582	7454.786409	26.911488
220.346365	7461.194099	26.916506
220.239482	7473.526294	26.921524
220.361604	7487.969367	26.926541
220.888829	7489.875760	26.931559
220.701160	7510.832877	26.936576
221.293446	7517.811823	26.941594
221.332137	7533.549738	26.946612
221.629379	7543.861339	26.951629
221.827998	7557.187536	26.956647
221.928583	7575.987543	26.961664
222.820926	7573.899975	26.966682
222.416712	7597.552460	26.971700
222.833223	7599.712983	26.976717
223.347601	7613.851617	26.981735
223.353308	7626.677710	26.986752
223.808774	7616.390389	26.991770
224.165459	7639.166046	26.996788
224.137374	7649.415019	27.001805
224.573126	7647.326360	27.006823
224.608009	7648.220732	27.011840
224.906888	7657.193569	27.016858
224.667462	7671.706054	27.021876
225.208042	7688.000035	27.026893
225.462103	7689.065278	27.031911
225.425484	7685.361614	27.036928
226.222667	7696.930398	27.041946
226.295732	7704.034954	27.046964
226.580426	7698.172064	27.051981
226.873845	7709.513544	27.056999
227.399348	7724.954369	27.062016
227.651812	7728.150853	27.067034
227.889915	7733.543718	27.072052
227.738866	7730.022135	27.077069
228.091662	7737.060783	27.082087
228.104655	7741.519709	27.087104
228.631383	7744.891066	27.092122
228.340310	7746.316372	27.097140
229.105821	7753.012554	27.102157
229.289558	7762.963217	27.107175
229.009055	7781.539001	27.112192
229.135063	7771.748347	27.117210
229.298504	7779.504907	27.122228
229.498643	7792.802624	27.127245
229.890497	7795.320622	27.132263
229.977737	7805.523202	27.137280
230.503703	7814.065912	27.142298
230.441140	7828.664466	27.147316
230.628867	7836.625610	27.152333
230.702392	7847.518596	27.157351
230.583822	7859.041520	27.162368
230.733078	7875.703205	27.167386
230.981148	7892.188415	27.172404
231.166149	7906.887158	27.177421
231.631904	7926.757384	27.182439
231.769203	7953.217354	27.187456
232.461504	7955.760919	27.192474
232.885852	7978.444313	27.197492
232.765156	7994.857945	27.202509
233.104337	8002.403959	27.207527
233.618310	8013.130174	27.212544
233.761360	8025.095248	27.217562
234.349129	8037.767302	27.222580
234.374479	8031.847066	27.227597
234.516999	8052.361594	27.232615
234.775951	8073.618761	27.237632
235.010935	8072.003499	27.242650
235.417095	8080.375678	27.247668
235.834358	8080.660836	27.252685
235.728264	8086.906466	27.257703
235.692643	8109.655764	27.262720
236.205810	8110.882496	27.267738
236.704568	8122.533029	27.272756
236.898283	8139.068017	27.277773
236.560676	8141.548797	27.282791
237.345216	8160.526393	27.287808
237.281284	8167.589447	27.292826
237.424447	8176.555361	27.297844
237.589530	8197.729506	27.302861
238.179445	8207.844090	27.307879
238.218528	8225.372610	27.312896
238.707755	8229.782306	27.317914
238.852143	8243.145910	27.322932
238.858667	8251.773356	27.327949
239.182164	8263.754516	27.332967
239.588179	8269.010734	27.337984
239.814098	8282.330023	27.343002
240.356595	8304.714327	27.348020
240.286070	8301.429433	27.353037
240.949588	8313.679385	27.358055
240.954756	8324.378148	27.363072
241.225024	8327.515121	27.368090
241.404597	8339.613591	27.373108
241.485471	8352.074814	27.378125
241.957136	8360.818871	27.383143
242.192824	8380.492001	27.388160
242.342018	8375.477294	27.393178
242.750550	8387.691470	27.398196
242.719889	8400.946853	27.403213
242.875982	8399.678578	27.408231
243.025408	8419.658876	27.413248
243.464502	8415.037586	27.418266
243.548545	8421.165143	27.423284
243.616165	8454.146766	27.428301
244.152215	8459.925698	27.433319
244.065453	8476.918513	27.438336
244.473303	8489.435949	27.443354
244.508282	8496.777249	27.448372
244.946208	8502.843081	27.453389
245.244728	8506.395560	27.458407
245.117454	8522.258187	27.463424
245.942515	8537.498067	27.468442
246.041524	8551.989794	27.473460
246.115673	8564.856331	27.478477
246.492603	8570.335037	27.483495
246.725960	8581.629635	27.488512
246.977610	8586.932227	27.493530
247.274721	8594.377731	27.498548
247.470985	8609.046854	27.503565
247.490691	8619.980298	27.508583
247.573387	8639.715556	27.513600
248.036510	8655.305850	27.518618
248.348762	8672.264751	27.523636
248.350466	8689.464905	27.528653
248.728415	8687.350460	27.533671
248.843558	8713.650815	27.538688
249.094549	8717.924305	27.543706
249.374269	8732.132131	27.548724
249.505896	8750.922156	27.553741
250.202983	8773.118637	27.558759
250.423942	8786.969476	27.563776
250.671285	8794.905909	27.568794
250.955944	8804.588747	27.573812
250.716096	8830.152420	27.578829
251.030424	8829.276079	27.583847
251.587301	8848.855190	27.588864
251.888473	8862.314654	27.593882
252.422588	8878.642276	27.598900
252.383107	8898.624268	27.603917
252.870959	8904.360376	27.608935
253.129031	8911.597432	27.613952
253.313214	8934.395397	27.618970
253.701131	8933.974794	27.623988
253.409156	8953.387055	27.629005
254.105704	8960.643844	27.634023
254.441813	8980.617603	27.639040
254.756775	8981.910177	27.644058
255.246167	8996.985173	27.649076
255.238937	9010.445698	27.654093
255.892781	9006.633606	27.659111
255.957084	9010.317590	27.664128
256.071590	9024.848304	27.669146
256.599199	9024.045890	27.674164
256.571171	9044.869229	27.679181
257.006792	9051.750174	27.684199
257.288183	9047.876443	27.689216
257.084101	9070.141836	27.694234
257.445224	9071.761854	27.699252
257.600376	9089.727652	27.704269
257.789975	9101.060994	27.709287
258.069807	9109.721799	27.714304
258.390908	9122.496363	27.719322
258.680195	9142.202950	27.724340
258.848410	9162.073758	27.729357
259.352293	9156.106615	27.734375
259.518591	9183.877222	27.739392
259.710522	9186.912952	27.744410
259.995333	9199.743771	27.749428
260.104253	9215.611035	27.754445
260.789874	9227.226680	27.759463
260.620878	9240.289638	27.764480
260.641102	9249.120624	27.769498
261.300666	9270.063827	27.774516
261.366800	9292.126133	27.779533
261.892780	9293.328842	27.784551
262.046665	9298.858493	27.789568
262.477000	9317.406547	27.794586
262.435999	9324.378044	27.799604
262.753300	9337.279643	27.804621
262.848635	9347.585996	27.809639
263.327086	9356.986182	27.814656
263.477473	9378.072417	27.819674
263.949032	9373.231111	27.824692
264.104261	9397.903303	27.829709
264.503909	9401.664282	27.834727
264.807431	9407.041075	27.839744
264.660344	9432.549998	27.844762
265.029612	9424.327437	27.849780
265.053918	9454.094010	27.854797
265.693513	9457.665861	27.859815
265.884748	9479.863502	27.864832
265.823881	9480.138341	27.869850
266.656080	9496.902883	27.874868
266.883857	9511.492009	27.879885
267.082788	9523.007271	27.884903
267.500307	9525.060521	27.889920
267.668949	9548.158463	27.894938
268.427265	9543.246934	27.899956
268.320867	9553.701824	27.904973
268.450640	9573.446486	27.909991
268.974896	9577.279545	27.915008
268.875895	9580.856617	27.920026
269.127828	9606.192764	27.925044
269.366889	9618.118568	27.930061
269.865541	9630.799365	27.935079
270.001473	9639.940775	27.940096
269.887632	9661.858060	27.945114
270.511006	9671.371470	27.950132
270.544419	9686.992061	27.955149
270.864700	9702.090966	27.960167
271.188611	9713.997225	27.965184
271.262818	9735.755687	27.970202
272.396027	9745.593411	27.975220
272.396778	9769.194690	27.980237
272.851879	9767.358518	27.985255
273.052880	9777.313875	27.990272
273.376556	9784.563099	27.995290
273.377699	9792.188059	28.000308
273.898679	9809.446828	28.005325
274.039182	9820.150510	28.010343
274.414441	9824.161673	28.015360
274.165294	9847.723263	28.020378
274.515531	9847.643228	28.025396
274.850845	9877.838522	28.030413
275.335106	9886.379260	28.035431
275.821696	9889.406836	28.040448
275.819875	9904.673187	28.045466
276.043619	9915.581745	28.050484
276.545397	9935.738968	28.055501
276.540222	9940.595943	28.060519
276.841532	9953.431013	28.065536
276.855684	9982.754827	28.070554
277.470206	9986.052860	28.075572
277.730938	9996.169478	28.080589
277.960351	10010.294600	28.085607
278.170149	10032.411056	28.090624
278.072994	10050.047889	28.095642
278.813499	10049.600449	28.100660
278.939091	10072.800508	28.105677
279.293716	10076.372920	28.110695
279.844010	10101.584067	28.115712
279.910972	10115.371613	28.120730
280.355992	10124.104895	28.125748
280.970367	10139.060205	28.130765
280.770570	10133.449266	28.135783
281.239154	10150.906006	28.140800
281.129504	10161.004955	28.145818
281.534115	10161.759437	28.150836
282.092905	10169.133009	28.155853
282.529416	10179.272710	28.160871
282.736968	10190.057668	28.165888
282.421632	10204.536655	28.170906
282.727883	10211.788775	28.175924
283.023723	10223.387172	28.180941
282.946894	10239.953784	28.185959
283.372181	10256.710138	28.190976
283.845106	10277.481639	28.195994
284.292595	10293.704096	28.201012
284.669973	10307.212663	28.206029
284.423557	10328.283196	28.211047
285.396758	10332.825979	28.216064
285.479203	10353.314571	28.221082
285.674706	10362.952199	28.226100
285.977947	10386.506872	28.231117
286.400734	10387.950004	28.236135
286.798297	10411.808838	28.241152
286.566247	10426.183383	28.246170
287.188768	10438.368550	28.251188
287.275337	10451.253391	28.256205
287.447434	10470.259837	28.261223
287.800272	10487.924474	28.266240
287.966991	10515.763307	28.271258
288.611164	10527.023152	28.276276
289.104611	10540.371619	28.281293
289.292536	10555.116208	28.286311
289.681150	10583.621348	28.291328
289.692951	10590.045112	28.296346
290.196857	10607.518850	28.301364
290.557465	10613.076502	28.306381
290.881298	10622.425773	28.311399
291.406543	10633.817983	28.316416
291.304991	10655.314558	28.321434
291.795243	10660.517219	28.326452
292.177310	10683.292642	28.331469
292.345772	10684.971404	28.336487
292.799678	10698.458794	28.341504
292.600466	10724.179727	28.346522
293.258068	10732.580030	28.351540
293.729595	10739.932767	28.356557
293.547774	10757.832975	28.361575
294.090080	10764.435772	28.366592
294.202341	10787.572498	28.371610
294.532258	10798.461784	28.376628
294.959581	10823.825788	28.381645
295.191965	10829.270975	28.386663
295.406421	10845.963001	28.391680
295.670325	10863.480890	28.396698
295.850466	10876.259797	28.401716
296.377644	10891.519867	28.406733
296.785882	10907.982667	28.411751
297.031693	10922.314310	28.416768
297.376855	10938.032360	28.421786
297.780554	10947.100890	28.426804
298.274957	10950.667363	28.431821
298.253622	10972.435917	28.436839
298.824736	10988.431213	28.441856
299.246514	10994.730900	28.446874
298.952586	11003.362480	28.451892
299.664079	11022.367088	28.456909
299.348931	11031.920860	28.461927
300.101718	11037.676127	28.466944
300.099594	11052.264582	28.471962
300.207260	11068.335703	28.476980
300.619081	11077.864032	28.481997
300.936669	11090.106868	28.487015
301.319556	11115.989759	28.492032
301.345141	11124.808162	28.497050
301.721473	11146.255700	28.502068
301.750484	11157.852270	28.507085
301.865680	11180.477490	28.512103
302.918805	11190.991635	28.517120
302.791316	11212.988655	28.522138
303.546952	11229.552042	28.527156
303.770039	11235.421924	28.532173
304.208698	11263.194009	28.537191
304.611186	11265.511895	28.542208
304.619493	11287.914010	28.547226
304.792099	11298.019878	28.552244
305.016722	11314.729675	28.557261
305.076041	11336.119730	28.562279
305.676152	11342.315817	28.567296
306.139302	11374.830154	28.572314
306.360083	11394.091995	28.577332
306.790823	11404.331155	28.582349
306.983747	11428.160191	28.587367
307.196215	11443.934186	28.592384
307.511058	11453.771560	28.597402
307.837916	11473.607348	28.602420
308.137503	11488.278342	28.607437
308.468512	11505.164261	28.612455
309.120097	11512.656456	28.617472
309.468196	11523.186500	28.622490
309.658608	11550.334789	28.627508
310.244687	11566.002997	28.632525
310.852962	11582.226649	28.637543
311.012945	11582.918469	28.642560
311.075540	11596.477280	28.647578
311.389851	11613.170136	28.652596
312.170091	11615.905702	28.657613
312.147353	11634.271264	28.662631
312.638721	11644.624208	28.667648
312.568234	11661.112139	28.672666
312.849145	11674.412612	28.677684
313.173443	11680.339406	28.682701
313.194446	11696.828825	28.687719
313.873625	11715.081356	28.692736
314.046375	11731.120745	28.697754
314.255290	11753.160431	28.702772
314.639178	11764.682839	28.707789
314.805619	11787.351287	28.712807
315.141511	11798.347581	28.717824
315.875350	11814.302307	28.722842
315.877794	11829.171685	28.727860
316.368977	11843.554013	28.732877
316.240653	11866.991847	28.737895
316.890296	11871.999365	28.742912
317.574513	11901.818027	28.747930
317.710565	11912.501501	28.752948
318.153030	11915.179503	28.757965
318.055541	11928.523642	28.762983
318.540046	11952.206620	28.768000
318.400268	11972.438121	28.773018
318.746203	11989.685278	28.778036
319.556823	12008.555369	28.783053
319.362728	12027.841799	28.788071
319.767229	12044.388285	28.793088
320.535404	12070.682645	28.798106
320.590090	12087.438697	28.803124
321.250020	12102.934740	28.808141
321.217035	12116.111020	28.813159
321.587250	12123.331761	28.818176
321.922521	12138.376606	28.823194
321.891874	12152.439877	28.828212
322.372356	12167.067277	28.833229
322.792482	12187.050255	28.838247
323.097035	12204.250409	28.843264
323.166442	12220.887436	28.848282
323.674130	12250.023802	28.853300
324.056311	12260.078413	28.858317
324.473765	12274.068423	28.863335
324.485065	12287.278936	28.868352
325.238171	12310.361361	28.873370
325.228643	12330.342323	28.878388
325.734179	12344.959622	28.883405
326.133731	12356.877824	28.888423
326.276722	12370.819324	28.893440
326.889117	12386.184105	28.898458
326.947892	12406.536543	28.903476
327.303378	12418.625892	28.908493
327.538638	12442.370635	28.913511
327.864272	12467.721214	28.918528
328.366586	12475.101394	28.923546
328.357745	12499.913897	28.928564
329.048730	12514.142286	28.933581
329.456580	12536.445404	28.938599
329.759751	12559.857558	28.943616
330.240828	12571.835756	28.948634
330.376132	12589.814341	28.953652
330.458603	12604.299168	28.958669
330.745386	12627.957128	28.963687
330.870908	12651.801429	28.968704
331.630225	12664.010833	28.973722
332.021753	12690.718741	28.978740
332.500908	12701.415232	28.983757
332.825427	12725.803184	28.988775
333.305656	12742.704736	28.993792
333.577422	12755.094782	28.998810
334.300599	12774.111972	29.003828
334.507877	12773.144862	29.008845
334.541132	12789.964894	29.013863
334.985679	12797.117409	29.018880
335.256865	12816.666494	29.023898
335.236971	12835.332778	29.028916
335.916001	12857.682218	29.033933
336.383964	12872.375287	29.038951
336.681860	12881.530803	29.043968
336.979324	12897.971650	29.048986
337.278027	12921.568111	29.054004
337.896819	12929.988120	29.059021
338.227604	12946.142737	29.064039
338.186667	12957.025054	29.069056
338.513368	12975.141392	29.074074
338.956291	12993.267964	29.079092
339.083119	13009.801953	29.084109
339.732696	13025.373013	29.089127
339.745440	13045.117556	29.094144
340.217532	13067.411240	29.099162
340.463303	13087.719330	29.104180
340.784543	13092.579672	29.109197
341.302937	13119.666213	29.114215
341.665163	13138.449782	29.119232
341.903238	13150.608521	29.124250
342.442180	13178.345619	29.129268
342.563526	13185.514173	29.134285
343.080906	13201.582936	29.139303
343.276431	13206.589319	29.144320
343.691719	13230.562646	29.149338
343.836264	13246.345633	29.154356
344.296079	13258.753923	29.159373
344.525366	13270.086731	29.164391
344.883775	13287.955241	29.169408
345.580748	13303.598056	29.174426
345.722940	13315.314016	29.179444
345.946812	13331.059384	29.184461
345.997342	13348.865649	29.189479
346.403345	13361.026640	29.194496
347.165338	13381.064704	29.199514
347.005577	13406.761005	29.204532
347.330752	13421.540028	29.209549
348.046660	13447.279221	29.214567
348.047551	13464.616515	29.219584
348.884864	13481.728065	29.224602
349.108303	13499.201062	29.229620
348.996326	13513.451773	29.234637
349.466337	13537.385337	29.239655
350.111387	13555.660793	29.244672
350.707015	13565.970045	29.249690
350.856466	13594.428788	29.254708
351.312557	13606.825258	29.259725
351.830872	13630.704004	29.264743
351.935999	13656.624423	29.269760
352.549393	13652.391424	29.274778
353.052496	13671.166087	29.279796
353.355791	13681.135916	29.284813
353.591155	13695.319723	29.289831
353.840927	13717.721633	29.294848
354.256143	13724.762251	29.299866
354.278876	13745.080718	29.304884
354.600606	13755.429821	29.309901
355.137990	13785.498684	29.314919
355.237550	13794.515178	29.319936
355.709424	13813.471725	29.324954
355.759447	13848.354098	29.329972
355.944351	13864.567089	29.334989
356.558770	13895.985182	29.340007
357.037385	13924.370752	29.345024
357.500360	13946.148977	29.350042
357.788180	13960.324766	29.355060
358.144704	13981.585992	29.360077
358.604892	13990.962955	29.365095
359.010747	14020.383282	29.370112
359.472075	14043.112459	29.375130
359.908335	14066.101395	29.380148
360.440534	14081.953836	29.385165
360.953204	14101.760124	29.390183
361.497292	14112.677787	29.395200
361.802542	14115.124957	29.400218
361.888977	14146.117715	29.405236
362.008963	14148.540222	29.410253
362.437309	14164.462687	29.415271
363.025918	14182.678113	29.420288
363.157967	14200.579783	29.425306
363.554261	14225.381611	29.430324
364.196563	14230.839371	29.435341
364.393677	14254.974494	29.440359
364.845615	14268.679510	29.445376
365.623094	14281.016606	29.450394
365.537329	14293.773161	29.455412
366.075019	14308.307994	29.460429
366.625192	14322.285051	29.465447
366.753297	14342.515015	29.470464
366.743363	14351.533133	29.475482
367.187561	14372.594734	29.480500
367.612025	14381.105841	29.485517
368.116166	14394.246939	29.490535
368.115041	14420.112404	29.495552
368.739301	14427.433196	29.500570
369.243147	14445.665310	29.505588
369.418790	14452.598451	29.510605
369.440140	14474.190649	29.515623
369.894354	14500.922872	29.520640
370.389719	14501.442259	29.525658
370.807481	14525.726336	29.530676
370.690692	14540.799692	29.535693
371.246693	14555.777147	29.540711
371.012674	14578.170583	29.545728
372.119696	14591.267913	29.550746
371.981212	14625.536969	29.555764
372.551544	14650.182605	29.560781
373.023106	14663.426897	29.565799
373.230771	14700.948489	29.570816
373.705532	14721.070865	29.575834
373.866014	14745.490269	29.580852
374.598243	14768.976905	29.585869
375.148251	14789.327589	29.590887
375.491272	14814.969139	29.595904
375.674515	14828.337664	29.600922
376.147906	14851.855472	29.605940
376.461243	14885.059382	29.610957
376.783299	14896.760776	29.615975
377.337520	14921.115572	29.620992
377.567938	14945.682188	29.626010
377.846699	14963.049959	29.631028
378.373410	14989.124073	29.636045
378.838138	15005.790048	29.641063
379.224027	15027.278396	29.646080
380.109498	15049.184359	29.651098
380.331058	15067.281267	29.656116
380.674025	15089.196455	29.661133
381.174791	15108.730890	29.666151
381.281269	15122.136910	29.671168
381.726937	15142.681179	29.676186
382.191657	15157.240725	29.681204
382.562268	15178.039975	29.686221
383.021709	15206.370454	29.691239
382.800346	15228.045738	29.696256
383.311521	15250.534837	29.701274
383.932086	15275.621890	29.706292
384.488307	15294.948857	29.711309
384.748702	15320.382948	29.716327
385.000401	15338.159561	29.721344
385.448731	15360.892348	29.726362
386.060938	15384.082714	29.731380
386.634555	15405.242043	29.736397
387.050779	15418.116532	29.741415
387.125530	15444.028347	29.746432
387.494546	15451.980123	29.751450
388.219312	15469.944899	29.756468
388.561922	15494.103015	29.761485
388.822262	15503.385698	29.766503
388.789918	15542.879433	29.771520
389.485602	15552.646657	29.776538
389.546443	15572.338908	29.781556
389.804345	15592.281405	29.786573
390.354904	15618.257893	29.791591
390.760282	15640.637690	29.796608
391.390682	15668.585182	29.801626
391.419431	15700.435935	29.806644
391.878028	15722.362163	29.811661
392.708359	15742.906834	29.816679
392.684329	15767.697547	29.821696
393.042113	15783.790339	29.826714
393.664199	15809.967494	29.831732
394.068641	15825.241310	29.836749
394.325165	15837.676815	29.841767
394.526464	15864.213685	29.846784
395.039546	15889.593160	29.851802
395.423853	15909.816234	29.856820
395.501415	15932.039266	29.861837
396.287917	15946.065777	29.866855
396.674886	15969.320560	29.871872
397.467795	15987.458337	29.876890
397.770994	15996.263944	29.881908
397.989969	16015.290724	29.886925
398.531006	16034.665036	29.891943
398.863772	16053.711931	29.896960
399.060197	16065.601117	29.901978
399.443738	16088.013283	29.906996
399.890516	16120.342502	29.912013
400.347958	16139.268884	29.917031
400.672676	16163.070586	29.922048
401.214273	16181.127892	29.927066
401.700041	16203.574715	29.932084
402.259255	16226.013220	29.937101
402.677578	16242.040062	29.942119
403.076928	16260.685086	29.947136
403.359790	16276.139387	29.952154
403.502766	16294.300298	29.957172
403.653385	16319.228606	29.962189
404.339998	16344.035088	29.967207
404.387329	16368.919629	29.972224
404.934278	16386.998400	29.977242
405.300903	16411.791922	29.982260
406.017818	16443.668771	29.987277
406.489333	16461.029818	29.992295
406.890386	16489.134455	29.997312
407.284712	16513.348925	30.002330
408.088128	16532.186759	30.007348
408.179149	16557.911176	30.012365
409.029654	16570.797380	30.017383
409.219386	16595.877845	30.022400
409.498434	16618.976601	30.027418
409.799789	16632.365787	30.032436
410.339590	16657.707350	30.037453
411.042824	16669.021638	30.042471
411.788181	16688.809959	30.047488
412.040873	16720.734714	30.052506
412.755758	16723.320207	30.057524
412.427049	16743.137846	30.062541
413.043986	16762.185152	30.067559
413.254127	16783.071293	30.072576
413.881887	16806.172507	30.077594
414.338206	16801.502289	30.082612
414.962936	16830.241998	30.087629
415.170957	16848.093182	30.092647
414.960896	16865.507660	30.097664
415.612281	16895.329832	30.102682
416.307191	16905.985428	30.107700
416.613642	16937.898963	30.112717
416.950688	16957.656761	30.117735
417.519896	16965.982108	30.122752
417.833968	16998.074587	30.127770
418.101359	17017.319034	30.132788
418.133906	17050.365366	30.137805
418.663909	17067.300869	30.142823
419.313261	17094.148284	30.147840
419.606906	17120.204951	30.152858
419.911741	17142.299023	30.157876
420.387389	17173.305198	30.162893
420.612978	17200.358116	30.167911
421.150473	17223.306564	30.172928
421.704490	17251.331499	30.177946
422.404636	17265.909471	30.182964
422.464398	17291.851390	30.187981
422.872416	17297.315153	30.192999
423.114655	17328.547654	30.198016
423.502335	17348.778033	30.203034
424.226060	17373.598984	30.208052
424.307943	17398.128831	30.213069
424.750571	17413.612718	30.218087
425.183112	17443.488970	30.223104
425.889258	17463.221058	30.228122
426.301042	17496.928923	30.233140
426.586317	17535.464140	30.238157
426.841746	17540.756036	30.243175
427.471643	17564.385322	30.248192
427.647113	17596.614218	30.253210
428.318676	17620.647673	30.258228
428.527923	17651.708979	30.263245
429.106549	17680.242388	30.268263
429.520106	17707.418189	30.273280
430.085900	17747.059650	30.278298
430.478713	17758.337921	30.283316
430.977008	17791.432597	30.288333
431.277456	17824.905777	30.293351
431.877041	17846.657568	30.298368
432.237112	17875.459243	30.303386
433.035699	17894.532916	30.308404
433.289473	17912.358965	30.313421
433.820357	17940.893919	30.318439
434.106711	17965.733600	30.323456
434.770584	17997.911933	30.328474
435.339550	18013.894545	30.333492
435.586200	18033.768683	30.338509
435.959494	18059.908902	30.343527
436.629141	18082.907166	30.348544
436.851580	18119.728711	30.353562
437.501589	18138.750088	30.358580
438.041098	18159.696683	30.363597
438.584497	18189.569358	30.368615
438.800479	18208.684057	30.373632
439.243862	18221.868892	30.378650
439.645792	18240.221662	30.383668
440.073430	18273.764141	30.388685
440.331750	18297.938977	30.393703
440.954033	18316.326799	30.398720
441.421479	18349.711551	30.403738
441.566918	18367.289649	30.408756
442.292651	18401.082582	30.413773
442.290687	18425.424699	30.418791
442.713552	18446.680484	30.423808
442.856741	18480.754330	30.428826
443.470370	18499.548009	30.433844
444.288938	18541.931261	30.438861
444.993026	18564.210808	30.443879
445.651380	18588.658184	30.448896
445.752111	18609.351792	30.453914
446.444203	18643.213594	30.458932
446.799505	18658.908005	30.463949
447.635197	18675.209494	30.468967
448.644834	18688.653427	30.473984
448.581963	18717.231984	30.479002
448.896896	18723.936367	30.484020
449.290316	18745.430847	30.489037
449.993653	18761.753141	30.494055
450.326068	18774.191290	30.499072
450.655315	18805.172468	30.504090
451.435793	18823.782386	30.509108
451.632818	18836.936732	30.514125
451.551436	18864.197996	30.519143
452.256742	18869.748315	30.524160
452.320648	18901.346123	30.529178
452.752674	18922.101892	30.534196
453.032854	18947.139646	30.539213
453.323834	18960.430986	30.544231
453.999380	18988.673159	30.549248
454.547707	19017.352275	30.554266
454.818934	19038.240756	30.559284
455.306624	19060.763257	30.564301
455.553992	19097.033099	30.569319
456.067407	19129.792845	30.574336
456.288909	19155.042228	30.579354
456.674336	19182.060237	30.584372
457.482053	19219.916770	30.589389
457.827178	19254.295186	30.594407
458.474254	19279.541251	30.599424
458.902400	19311.297479	30.604442
459.541008	19335.710981	30.609460
459.835287	19372.624731	30.614477
460.192706	19409.623429	30.619495
460.781185	19428.712572	30.624512
461.207977	19468.328775	30.629530
461.341394	19493.491306	30.634548
461.803805	19517.130254	30.639565
462.389943	19561.687604	30.644583
463.010703	19592.049437	30.649600
463.637056	19637.573631	30.654618
463.900977	19649.757712	30.659636
464.696555	19684.540182	30.664653
465.177858	19719.675203	30.669671
465.888225	19735.763449	30.674688
466.365191	19763.943081	30.679706
467.127512	19787.724923	30.684724
467.072296	19817.049418	30.689741
467.745124	19848.471247	30.694759
468.327938	19871.870634	30.699776
468.644961	19900.163966	30.704794
469.216298	19926.389399	30.709812
469.833837	19947.388881	30.714829
469.859583	19970.288056	30.719847
470.739823	19999.226216	30.724864
471.056056	20025.251650	30.729882
471.645891	20047.696112	30.734900
471.972125	20079.425324	30.739917
472.287967	20105.596243	30.744935
473.250315	20127.773952	30.749952
473.686664	20145.548177	30.754970
473.853026	20174.882729	30.759988
474.255785	20206.720206	30.765005
474.883848	20231.123846	30.770023
475.643290	20247.880875	30.775040
475.869945	20276.580634	30.780058
476.689019	20295.318599	30.785076
476.900118	20321.291393	30.790093
477.300627	20334.294831	30.795111
478.047320	20366.287200	30.800128
478.467391	20397.578908	30.805146
478.579401	20427.023442	30.810164
479.474052	20439.216636	30.815181
479.927976	20480.561841	30.820199
480.357631	20487.552143	30.825216
481.146999	20520.757506	30.830234
481.382740	20539.012108	30.835252
482.408183	20559.329168	30.840269
482.622200	20583.122040	30.845287
482.859810	20581.789661	30.850304
483.147342	20612.565416	30.855322
483.543526	20630.390602	30.860340
484.282135	20646.898505	30.865357
484.170534	20675.026313	30.870375
484.872206	20692.367742	30.875392
485.055734	20715.236754	30.880410
485.565098	20746.407622	30.885428
486.180766	20764.830387	30.890445
486.185873	20799.454325	30.895463
486.771279	20825.065877	30.900480
487.411698	20858.472057	30.905498
487.524410	20891.025825	30.910516
488.058692	20921.428541	30.915533
488.438460	20954.111181	30.920551
489.357463	20992.238046	30.925568
489.668545	21018.777398	30.930586
490.046669	21051.542598	30.935604
490.518990	21085.493606	30.940621
491.033686	21121.668457	30.945639
492.144660	21151.399904	30.950656
492.470833	21178.398357	30.955674
492.614884	21216.400614	30.960692
493.285943	21247.262618	30.965709
493.875402	21274.024090	30.970727
494.137458	21306.517242	30.975744
494.593492	21344.571977	30.980762
495.325864	21375.355074	30.985780
496.043382	21405.647698	30.990797
496.240517	21438.385021	30.995815
497.042294	21469.827165	31.000832
497.461611	21504.640207	31.005850
498.014966	21537.871620	31.010868
498.589223	21551.581611	31.015885
498.907369	21583.946380	31.020903
499.803592	21614.179742	31.025920
500.201428	21642.267049	31.030938
501.072240	21671.708331	31.035956
501.255668	21693.738114	31.040973
501.455447	21728.055168	31.045991
502.099116	21759.560451	31.051008
502.383996	21795.273358	31.056026
502.965469	21828.210197	31.061044
503.337869	21859.625434	31.066061
503.676464	21894.597137	31.071079
504.357282	21927.227920	31.076096
505.342391	21954.339066	31.081114
505.796737	21998.183295	31.086132
506.577847	22015.342846	31.091149
506.900170	22042.595835	31.096167
507.458955	22053.882193	31.101184
508.337694	22084.675069	31.106202
508.767861	22113.048645	31.111220
509.342747	22124.067133	31.116237
509.939100	22159.207453	31.121255
510.126519	22174.987849	31.126272
510.231725	22209.086754	31.131290
510.912227	22241.541179	31.136308
511.625004	22261.510891	31.141325
512.110068	22288.511252	31.146343
512.809993	22315.768665	31.151360
513.233928	22338.418658	31.156378
513.779922	22370.824856	31.161396
514.404249	22380.256025	31.166413
514.711333	22413.160989	31.171431
515.370182	22437.322430	31.176448
515.617839	22468.037817	31.181466
515.919109	22494.365848	31.186484
516.384468	22513.022319	31.191501
516.878144	22550.245702	31.196519
517.402379	22567.490201	31.201536
517.715205	22603.276016	31.206554
518.075272	22633.278969	31.211572
518.628856	22655.890062	31.216589
519.049387	22695.444235	31.221607
519.732715	22712.455416	31.226624
520.605431	22746.194913	31.231642
520.531208	22776.657880	31.236660
521.344170	22803.936176	31.241677
521.844841	22841.980484	31.246695
522.314422	22864.434358	31.251712
523.420660	22894.150225	31.256730
523.544078	22925.264921	31.261748
524.119582	22947.133585	31.266765
524.371935	22983.049618	31.271783
524.685202	23007.265881	31.276800
525.187006	23038.991313	31.281818
525.846178	23090.433016	31.286836
526.176658	23116.864721	31.291853
526.804270	23144.873938	31.296871
527.306797	23193.806476	31.301888
528.206942	23221.393968	31.306906
528.561929	23264.169664	31.311924
529.571003	23283.670619	31.316941
529.637123	23328.046210	31.321959
530.390705	23354.178154	31.326976
531.152080	23375.657986	31.331994
531.636885	23420.631722	31.337012
531.997442	23441.352905	31.342029
532.589256	23488.932510	31.347047
532.918869	23517.551337	31.352064
534.046377	23553.489312	31.357082
534.320842	23581.421751	31.362100
534.749070	23610.366506	31.367117
535.303130	23647.765747	31.372135
535.763538	23667.422526	31.377152
536.602467	23697.535344	31.382170
536.907804	23732.724031	31.387188
537.257171	23761.062065	31.392205
538.093996	23806.752495	31.397223
538.594784	23840.368844	31.402240
539.427417	23858.457191	31.407258
539.483668	23896.440414	31.412276
540.505045	23922.733383	31.417293
540.706816	23955.941764	31.422311
541.833284	23979.482060	31.427328
542.652399	24009.851229	31.432346
542.652762	24052.260758	31.437364
543.395431	24070.110612	31.442381
543.778066	24095.574897	31.447399
544.232266	24123.404111	31.452416
545.030042	24152.759413	31.457434
545.216447	24186.924820	31.462452
545.603255	24221.406468	31.467469
546.477567	24249.195337	31.472487
546.934899	24281.915552	31.477504
547.180503	24305.252943	31.482522
547.749728	24353.539611	31.487540
548.543046	24381.771076	31.492557
549.093999	24413.680585	31.497575
549.660389	24448.791729	31.502592
550.304931	24476.098700	31.507610
550.920663	24508.743920	31.512628
551.361014	24524.233782	31.517645
552.208153	24567.851526	31.522663
552.079799	24598.129840	31.527680
552.956965	24623.700612	31.532698
553.154452	24662.718539	31.537716
554.244427	24680.748371	31.542733
554.430691	24705.359443	31.547751
554.735203	24737.971626	31.552768
555.645456	24775.393027	31.557786
556.156440	24796.212130	31.562804
556.656723	24821.292374	31.567821
557.218618	24854.723908	31.572839
557.393255	24881.808005	31.577856
557.939145	24913.826538	31.582874
558.272881	24953.575732	31.587892
559.095935	24971.066222	31.592909
559.683647	25013.095085	31.597927
560.319033	25045.283083	31.602944
560.772838	25077.411096	31.607962
561.210838	25116.720862	31.612980
561.884025	25149.174855	31.617997
562.359498	25195.835099	31.623015
562.882723	25236.781211	31.628032
563.735243	25263.955567	31.633050
564.258316	25306.071005	31.638068
564.786431	25340.248055	31.643085
565.236090	25376.832664	31.648103
565.489774	25407.204036	31.653120
566.537154	25441.135616	31.658138
567.047849	25490.021932	31.663156
567.642684	25529.213142	31.668173
568.288894	25561.450832	31.673191
569.183796	25599.274328	31.678208
569.751878	25631.979399	31.683226
569.937750	25677.763412	31.688244
570.259184	25704.231552	31.693261
571.400244	25750.586602	31.698279
571.783401	25793.338007	31.703296
572.868906	25812.380757	31.708314
573.196813	25851.627040	31.713332
573.639517	25876.445861	31.718349
574.195970	25909.292244	31.723367
574.455412	25947.247519	31.728384
575.561629	25978.687032	31.733402
576.294122	26015.860506	31.738420
576.863347	26044.609734	31.743437
577.457220	26083.859055	31.748455
577.917587	26119.021325	31.753472
578.730923	26141.760008	31.758490
579.122364	26179.119919	31.763508
580.075708	26209.035317	31.768525
580.314912	26237.760666	31.773543
580.714378	26279.651014	31.778560
581.505129	26307.721272	31.783578
581.947688	26340.371311	31.788596
582.502804	26379.797921	31.793613
583.323634	26407.092549	31.798631
583.638069	26439.889218	31.803648
584.170808	26469.213580	31.808666
584.737396	26510.572619	31.813684
585.043590	26541.639014	31.818701
585.557020	26581.300072	31.823719
586.422741	26623.427799	31.828736
587.186597	26649.613001	31.833754
587.353091	26699.042809	31.838772
588.360954	26727.591587	31.843789
589.047180	26765.241386	31.848807
589.513444	26805.384290	31.853824
590.080670	26833.496607	31.858842
590.556320	26866.230796	31.863860
591.233557	26914.373962	31.868877
591.960207	26927.564491	31.873895
592.229206	26974.532957	31.878912
592.787435	27004.580940	31.883930
593.380558	27028.928875	31.888948
593.645069	27070.304766	31.893965
594.700483	27097.696316	31.898983
594.932489	27141.713033	31.904000
595.700915	27163.113662	31.909018
596.143131	27208.734582	31.914036
596.461938	27240.975667	31.919053
597.706890	27276.623829	31.924071
598.048690	27311.964751	31.929088
598.220845	27347.951706	31.934106
599.189792	27391.221504	31.939124
599.660552	27427.781238	31.944141
600.519918	27458.528546	31.949159
600.731708	27499.483775	31.954176
601.388159	27526.900467	31.959194
602.381922	27573.940104	31.964212
602.696810	27612.325927	31.969229
603.389898	27649.432729	31.974247
604.407051	27692.366951	31.979264
605.284348	27729.735795	31.984282
605.559641	27756.441384	31.989300
605.755455	27799.137873	31.994317
606.726020	27829.817763	31.999335
607.128400	27868.139802	32.004352
607.760439	27900.269669	32.009370
608.677452	27938.403791	32.014388
609.145422	27976.519822	32.019405
610.001969	28011.705494	32.024423
610.378434	28061.573455	32.029440
611.088134	28082.017192	32.034458
611.958852	28123.603674	32.039476
612.079813	28161.047518	32.044493
613.184341	28197.376644	32.049511
613.525755	28234.191950	32.054528
614.107246	28269.288410	32.059546
615.091231	28308.582071	32.064564
615.661751	28343.124152	32.069581
616.467808	28370.885156	32.074599
616.832881	28410.768963	32.079616
617.553787	28439.074340	32.084634
618.178057	28477.166828	32.089652
618.958547	28515.355015	32.094669
619.607760	28542.799495	32.099687
620.078137	28578.514366	32.104704
620.540067	28615.905642	32.109722
620.970344	28655.729148	32.114740
621.848278	28693.478912	32.119757
622.204321	28725.078106	32.124775
622.626058	28771.483195	32.129792
623.433820	28804.042070	32.134810
624.441708	28844.287474	32.139828
624.683488	28890.057321	32.144845
625.343662	28913.410950	32.149863
625.876509	28958.408459	32.154880
626.828834	29001.551543	32.159898
627.430197	29035.786558	32.164916
627.807833	29075.884606	32.169933
628.722525	29105.993641	32.174951
628.922387	29155.866642	32.179968
629.329703	29197.275046	32.184986
629.952650	29240.666169	32.190004
630.570350	29278.691646	32.195021
631.346733	29319.195477	32.200039
632.203176	29368.511051	32.205056
632.754610	29405.314534	32.210074
633.345220	29443.945062	32.215092
633.783709	29487.555228	32.220109
634.853178	29511.724073	32.225127
635.637419	29555.627896	32.230144
635.641844	29575.140599	32.235162
636.490407	29619.034484	32.240180
637.196377	29649.278145	32.245197
637.879663	29677.945113	32.250215
638.349689	29721.316953	32.255232
638.831036	29758.125724	32.260250
639.569107	29791.284953	32.265268
640.395846	29840.701131	32.270285
641.097271	29868.916720	32.275303
641.820057	29903.722041	32.280320
642.374915	29930.734351	32.285338
643.337260	29961.292310	32.290356
643.447476	30010.410230	32.295373
644.391659	30033.998794	32.300391
644.453265	30080.861481	32.305408
645.351384	30122.194882	32.310426
646.019177	30156.611002	32.315444
646.554248	30204.139412	32.320461
647.374657	30241.837823	32.325479
648.229160	30289.822111	32.330496
648.577757	30323.978754	32.335514
649.409638	30370.481254	32.340532
649.952288	30408.659645	32.345549
651.028738	30444.990840	32.350567
651.347141	30494.096269	32.355584
652.143532	30523.056452	32.360602
653.272975	30565.340657	32.365620
653.628407	30610.502314	32.370637
654.353613	30652.142002	32.375655
654.744624	30687.898254	32.380672
655.481267	30720.395450	32.385690
656.297176	30768.671362	32.390708
656.583797	30798.173235	32.395725
657.200873	30849.198719	32.400743
657.917092	30889.974246	32.405760
658.635134	30921.747696	32.410778
659.678867	30961.220408	32.415796
660.194078	31008.026799	32.420813
660.719543	31045.475756	32.425831
661.514417	31086.555432	32.430848
662.377355	31121.871874	32.435866
663.068752	31162.588610	32.440884
663.738344	31205.325439	32.445901
665.040778	31241.388746	32.450919
665.305521	31278.651377	32.455936
666.078648	31316.308583	32.460954
666.974689	31337.990720	32.465972
667.352194	31392.449796	32.470989
667.842894	31409.631234	32.476007
668.476753	31437.031410	32.481024
668.960639	31487.573590	32.486042
669.806597	31518.322773	32.491060
670.203227	31564.990948	32.496077
671.164565	31601.278989	32.501095
671.750472	31647.841848	32.506112
672.060502	31682.676878	32.511130
673.065039	31713.850362	32.516148
673.381840	31757.661385	32.521165
674.058343	31794.582298	32.526183
674.794074	31844.491655	32.531200
675.380124	31889.936072	32.536218
676.049530	31923.912353	32.541236
676.628822	31972.588470	32.546253
677.633726	32014.654912	32.551271
678.494199	32056.763023	32.556288
678.916510	32091.347244	32.561306
679.697665	32123.352885	32.566324
680.118853	32167.262216	32.571341
680.644349	32197.259708	32.576359
681.538549	32236.271480	32.581376
682.303964	32276.833405	32.586394
683.174967	32294.923278	32.591412
683.784568	32340.706376	32.596429
684.413498	32377.642096	32.601447
685.219725	32412.514436	32.606464
685.739485	32445.218995	32.611482
686.480267	32478.255670	32.616500
686.796853	32523.402280	32.621517
687.634984	32556.885341	32.626535
688.399918	32598.244544	32.631552
688.960407	32641.930753	32.636570
689.481881	32682.164990	32.641588
690.251040	32728.600414	32.646605
691.115793	32776.633106	32.651623
691.520741	32817.050226	32.656640
692.236398	32858.354440	32.661658
693.170242	32899.675143	32.666676
693.792140	32948.593429	32.671693
694.334381	32984.203503	32.676711
695.204278	33029.062244	32.681728
695.691000	33073.431058	32.686746
696.465193	33118.640055	32.691764
697.179162	33163.144170	32.696781
697.984865	33210.750874	32.701799
699.224494	33256.449959	32.706816
699.539436	33293.992829	32.711834
700.472913	33334.189088	32.716852
701.274539	33388.049558	32.721869
701.602708	33423.377788	32.726887
702.451548	33471.389279	32.731904
702.709389	33520.207854	32.736922
703.644005	33560.303211	32.741940
704.449182	33612.020428	32.746957
705.298343	33652.552943	32.751975
705.914643	33694.949169	32.756992
706.369840	33752.026013	32.762010
707.426839	33790.155347	32.767028
708.186572	33843.795941	32.772045
708.976079	33886.146461	32.777063
709.628245	33923.530164	32.782080
710.494142	33969.453716	32.787098
711.227265	34013.501420	32.792116
711.577180	34053.841025	32.797133
712.205546	34093.593368	32.802151
713.046896	34145.527520	32.807168
713.477020	34191.665218	32.812186
714.407765	34231.888916	32.817204
714.817206	34279.079585	32.822221
715.569587	34332.684641	32.827239
716.858111	34379.693612	32.832256
717.534156	34431.142227	32.837274
718.817944	34458.912462	32.842292
719.475861	34503.523035	32.847309
720.361337	34543.836613	32.852327
721.369637	34573.142282	32.857344
721.766129	34620.740393	32.862362
722.584363	34645.428778	32.867380
722.943440	34691.079204	32.872397
723.255839	34730.572418	32.877415
724.361197	34764.396521	32.882432
725.117019	34802.834090	32.887450
725.800889	34841.908945	32.892468
726.019353	34876.466452	32.897485
726.678757	34923.088308	32.902503
727.532554	34972.563002	32.907520
727.451160	35017.669803	32.912538
728.164691	35047.414305	32.917556
729.197416	35095.729490	32.922573
730.076463	35142.772674	32.927591
730.931856	35187.157759	32.932608
731.499533	35239.674903	32.937626
732.190517	35273.577361	32.942644
733.007544	35325.221052	32.947661
733.713697	35361.397506	32.952679
734.561635	35404.639775	32.957696
735.316347	35461.250701	32.962714
735.790195	35488.466260	32.967732
736.598372	35543.899296	32.972749
737.330019	35581.880492	32.977767
738.501129	35627.001103	32.982784
738.866457	35664.717342	32.987802
740.172460	35717.625886	32.992820
740.428872	35760.190109	32.997837
740.883189	35813.409308	33.002855
742.069016	35865.388588	33.007872
742.645397	35916.869069	33.012890
743.480075	35957.111097	33.017908
744.396741	36006.698499	33.022925
744.935520	36048.239005	33.027943
746.459902	36083.175695	33.032960
747.285684	36129.875320	33.037978
747.819919	36163.791102	33.042996
748.273986	36208.538359	33.048013
749.120233	36264.302439	33.053031
750.130227	36299.535026	33.058048
750.602965	36347.921788	33.063066
751.453285	36386.979749	33.068084
751.935946	36434.619019	33.073101
752.534502	36489.859713	33.078119
753.793868	36521.683347	33.083136
754.374822	36574.170093	33.088154
755.151190	36620.663542	33.093172
756.111044	36665.718272	33.098189
756.761503	36712.636327	33.103207
757.445196	36758.088602	33.108224
758.333778	36807.777118	33.113242
759.048178	36849.101984	33.118260
759.779617	36893.250789	33.123277
760.567841	36943.107096	33.128295
761.134530	36985.125631	33.133312
762.044934	37036.897970	33.138330
762.449335	37076.577158	33.143348
763.358224	37114.229812	33.148365
764.388183	37162.455280	33.153383
765.478121	37224.810643	33.158400
766.026139	37265.801934	33.163418
766.613414	37311.517099	33.168436
767.738586	37355.130943	33.173453
768.212996	37400.478240	33.178471
769.263253	37445.488841	33.183488
769.863316	37499.328092	33.188506
770.251601	37537.164192	33.193524
771.331990	37580.285950	33.198541
772.264054	37626.377794	33.203559
773.026065	37666.122221	33.208576
773.671023	37716.009086	33.213594
774.407517	37758.957408	33.218612
775.367388	37803.957623	33.223629
775.818817	37855.190426	33.228647
776.891619	37893.596589	33.233664
777.148423	37949.855758	33.238682
778.037369	37990.421952	33.243700
779.235837	38030.674160	33.248717
779.629903	38068.143518	33.253735
780.506301	38104.437089	33.258752
781.026296	38140.419758	33.263770
781.864728	38187.653088	33.268788
782.908438	38225.741893	33.273805
783.375784	38267.917620	33.278823
784.158066	38309.259967	33.283840
784.697941	38358.709470	33.288858
785.445637	38401.866007	33.293876
786.192884	38455.798434	33.298893
787.124087	38507.836667	33.303911
788.057427	38546.170980	33.308928
788.595086	38615.092453	33.313946
789.199916	38662.957847	33.318964
790.360607	38707.030520	33.323981
791.034121	38756.137490	33.328999
791.790087	38805.547855	33.334016
792.662453	38861.175477	33.339034
793.667296	38911.034052	33.344052
794.273192	38959.804259	33.349069
795.039543	39012.501918	33.354087
795.852324	39066.748131	33.359104
796.767977	39115.653578	33.364122
797.405726	39169.396243	33.369140
798.367577	39220.324696	33.374157
798.941928	39276.860120	33.379175
800.084478	39326.008770	33.384192
801.083853	39371.006075	33.389210
801.749518	39429.450112	33.394228
802.743646	39484.959087	33.399245
803.443720	39531.673153	33.404263
804.535128	39575.878608	33.409280
805.621656	39623.417734	33.414298
806.288946	39665.343533	33.419316
807.333406	39698.767609	33.424333
807.690997	39742.576058	33.429351
809.252887	39786.537518	33.434368
809.775558	39836.638160	33.439386
811.107850	39882.362272	33.444404
811.569756	39923.972902	33.449421
812.061248	39966.926040	33.454439
812.761161	40009.739113	33.459456
813.462019	40052.811417	33.464474
814.792394	40103.709537	33.469492
815.334754	40141.930826	33.474509
815.985706	40200.720755	33.479527
816.720712	40232.600390	33.484544
817.558061	40282.962676	33.489562
818.429514	40327.779621	33.494580
819.081174	40371.872155	33.499597
819.762030	40420.235473	33.504615
820.442945	40477.497286	33.509632
821.796389	40532.996947	33.514650
822.298997	40580.806689	33.519668
823.496300	40623.732817	33.524685
824.219656	40681.545069	33.529703
824.657064	40738.314445	33.534720
825.971413	40784.081214	33.539738
826.516394	40836.008432	33.544756
827.526783	40883.290286	33.549773
827.971018	40938.009976	33.554791
828.921457	40976.453431	33.559808
830.023588	41032.980344	33.564826
830.695879	41084.818649	33.569844
831.695641	41127.220141	33.574861
832.219301	41184.483135	33.579879
833.328906	41225.672273	33.584896
833.967059	41269.844631	33.589914
834.893431	41301.974148	33.594932
835.477852	41334.302725	33.599949
836.024106	41390.607701	33.604967
836.557887	41432.804470	33.609984
837.856210	41490.187297	33.615002
838.172927	41542.898247	33.620020
838.947860	41583.084242	33.625037
839.773550	41641.939233	33.630055
840.877882	41697.196252	33.635072
841.700246	41751.131418	33.640090
842.304448	41809.180349	33.645108
843.612509	41856.607439	33.650125
844.546370	41910.765880	33.655143
845.454068	41957.168016	33.660160
846.106153	42007.038327	33.665178
846.930886	42062.719538	33.670196
848.193435	42120.969796	33.675213
848.969058	42174.021516	33.680231
849.644637	42224.571727	33.685248
850.792482	42277.046771	33.690266
851.441432	42326.785475	33.695284
852.660898	42362.665601	33.700301
853.002084	42420.573908	33.705319
854.021649	42472.108114	33.710336
855.212091	42525.291800	33.715354
855.737508	42576.600029	33.720372
856.447121	42631.244432	33.725389
857.365554	42696.640422	33.730407
858.119724	42756.186371	33.735424
859.117264	42802.032269	33.740442
859.807732	42857.217859	33.745460
860.961811	42926.967225	33.750477
861.997051	42977.715849	33.755495
862.707546	43031.070785	33.760512
863.693708	43083.838723	33.765530
864.381513	43151.682046	33.770548
865.446690	43198.397372	33.775565
866.351679	43246.984831	33.780583
867.354721	43303.805087	33.785600
868.820230	43348.332782	33.790618
869.468534	43400.774868	33.795636
870.205207	43441.754575	33.800653
871.417681	43498.725971	33.805671
871.662944	43545.507165	33.810688
872.493618	43591.248000	33.815706
873.137129	43661.029026	33.820724
874.525362	43706.942132	33.825741
875.494706	43753.117010	33.830759
876.362894	43811.009687	33.835776
877.109220	43863.216132	33.840794
878.135789	43914.309832	33.845812
878.773814	43964.193088	33.850829
880.145182	44011.292312	33.855847
880.566990	44060.893372	33.860864
881.314227	44115.175000	33.865882
881.957255	44170.959554	33.870900
882.899646	44232.048705	33.875917
884.018639	44279.523266	33.880935
884.810482	44346.797311	33.885952
886.000918	44393.938329	33.890970
886.622182	44446.058192	33.895988
887.238521	44497.729835	33.901005
888.273110	44554.788726	33.906023
889.337601	44604.859663	33.911040
890.114813	44663.230569	33.916058
890.821701	44716.286492	33.921076
891.642124	44763.378696	33.926093
892.972459	44818.026177	33.931111
893.563847	44865.546648	33.936128
894.811968	44915.064502	33.941146
895.464802	44957.768057	33.946164
896.260177	45002.188934	33.951181
897.065323	45057.558131	33.956199
898.023331	45101.732341	33.961216
898.473486	45151.394644	33.966234
899.308833	45202.622455	33.971252
900.672557	45264.445503	33.976269
901.378858	45322.190335	33.981287
902.261274	45362.600419	33.986304
903.354846	45414.344949	33.991322
903.905165	45475.802535	33.996340
905.218756	45514.734726	34.001357
906.046826	45576.712095	34.006375
906.936137	45636.864527	34.011392
908.167893	45678.068145	34.016410
908.775216	45742.332544	34.021428
909.666974	45787.739378	34.026445
910.905101	45845.433914	34.031463
911.895442	45898.505190	34.036480
912.681906	45949.293222	34.041498
913.838866	46010.492810	34.046516
915.034092	46053.568996	34.051533
915.477920	46107.808081	34.056551
916.237059	46165.616396	34.061568
917.324085	46212.151171	34.066586
918.059243	46278.434062	34.071604
918.645036	46326.995976	34.076621
920.071397	46398.649346	34.081639
921.341751	46459.010011	34.086656
922.008297	46501.524577	34.091674
922.750547	46562.676732	34.096692
923.900043	46607.583062	34.101709
924.994070	46665.966510	34.106727
925.280058	46728.487415	34.111744
926.695614	46780.627510	34.116762
927.507239	46842.193415	34.121780
929.060942	46896.754057	34.126797
929.765949	46944.849474	34.131815
930.688614	47008.081218	34.136832
931.754039	47050.319271	34.141850
932.773786	47115.218895	34.146868
933.225728	47164.910666	34.151885
934.253882	47213.012993	34.156903
935.388139	47270.499700	34.161920
936.293780	47322.746196	34.166938
937.151201	47387.703650	34.171956
938.144908	47443.333880	34.176973
939.328313	47484.162474	34.181991
940.058197	47546.135327	34.187008
941.124183	47594.656411	34.192026
941.675874	47652.304894	34.197044
942.743610	47702.926305	34.202061
943.747782	47756.151622	34.207079
944.657832	47827.574048	34.212096
945.332290	47871.608302	34.217114
946.076586	47928.423867	34.222132
947.536240	47988.442654	34.227149
948.839142	48036.895956	34.232167
949.550866	48095.323975	34.237184
950.350527	48145.798552	34.242202
951.561128	48200.238920	34.247220
952.312186	48259.040794	34.252237
953.441099	48308.964380	34.257255
953.892865	48366.839098	34.262272
955.061412	48408.373938	34.267290
956.153923	48464.997135	34.272308
956.749904	48517.902225	34.277325
958.066448	48558.522109	34.282343
958.513301	48606.490650	34.287360
959.680700	48652.954599	34.292378
960.444638	48709.680465	34.297396
961.034372	48763.941019	34.302413
962.183523	48810.857345	34.307431
962.765988	48869.358200	34.312448
963.728298	48919.764738	34.317466
964.656443	48989.119120	34.322484
965.677597	49049.842045	34.327501
966.816745	49103.504910	34.332519
968.011479	49171.419877	34.337536
968.911601	49228.574913	34.342554
969.662282	49286.980903	34.347572
970.499483	49345.866990	34.352589
971.700225	49407.397895	34.357607
972.531470	49479.932386	34.362624
973.535841	49541.665224	34.367642
974.845515	49606.134285	34.372660
975.698781	49676.748884	34.377677
976.906283	49736.419483	34.382695
977.929515	49796.985889	34.387712
979.078321	49857.678315	34.392730
980.084046	49923.214510	34.397748
980.633783	49984.146590	34.402765
981.586010	50033.424615	34.407783
982.765199	50096.105941	34.412800
984.021594	50165.032859	34.417818
985.120768	50227.992812	34.422836
985.896222	50288.953629	34.427853
987.379663	50343.242494	34.432871
988.171411	50406.428230	34.437888
989.304354	50459.025947	34.442906
990.163732	50514.108917	34.447924
991.113312	50574.359888	34.452941
992.308293	50633.496964	34.457959
993.154809	50698.009970	34.462976
994.392472	50759.007224	34.467994
995.391093	50814.429765	34.473012
996.407924	50872.532362	34.478029
997.713108	50924.819446	34.483047
998.475069	50985.379268	34.488064
999.388998	51039.265412	34.493082
1000.589083	51096.460379	34.498100
1001.305649	51151.181260	34.503117
1002.348091	51213.539031	34.508135
1003.426946	51273.961408	34.513152
1004.248621	51329.836825	34.518170
1005.472202	51383.485466	34.523188
1006.395326	51448.260650	34.528205
1007.575073	51489.084317	34.533223
1008.368681	51562.466476	34.538240
1009.322742	51622.099382	34.543258
1010.381915	51678.577532	34.548276
1011.622087	51745.948812	34.553293
1012.504543	51802.334709	34.558311
1013.391967	51857.384848	34.563328
1014.261886	51915.664927	34.568346
1015.657734	51967.725035	34.573364
1016.646467	52030.688206	34.578381
1017.857231	52081.777786	34.583399
1018.608569	52150.859304	34.588416
1019.418163	52204.821441	34.593434
1020.802109	52254.555476	34.598452
1021.637127	52310.102124	34.603469
1022.578314	52368.979638	34.608487
1023.792045	52418.506549	34.613504
1024.578225	52466.069304	34.618522
1025.615516	52513.206847	34.623540
1026.405262	52558.807632	34.628557
1027.515969	52609.072444	34.633575
1028.770216	52654.961373	34.638592
1029.360910	52712.888515	34.643610
1030.385499	52767.438417	34.648628
1031.299442	52830.624278	34.653645
1032.211143	52874.675250	34.658663
1033.183200	52943.237312	34.663680
1034.562215	53004.749879	34.668698
1035.606073	53057.335799	34.673716
1036.163128	53116.420882	34.678733
1037.443647	53183.777347	34.683751
1038.114295	53244.686396	34.688768
1039.307367	53309.519408	34.693786
1040.804802	53364.572517	34.698804
1041.755866	53438.688953	34.703821
1043.129707	53495.634808	34.708839
1044.120675	53551.837087	34.713856
1045.167160	53609.587507	34.718874
1046.594055	53674.764604	34.723892
1047.395707	53732.389129	34.728909
1048.301741	53790.073390	34.733927
1049.396900	53855.790191	34.738944
1050.274754	53914.428385	34.743962
1051.440886	53975.287066	34.748980
1052.467702	54042.805953	34.753997
1053.970072	54095.929920	34.759015
1054.672041	54168.220845	34.764032
1055.637034	54217.195659	34.769050
1057.274034	54283.411016	34.774068
1058.040869	54350.604453	34.779085
1059.298587	54410.146302	34.784103
1060.270852	54463.531285	34.789120
1061.378655	54532.456430	34.794138
1062.653775	54585.167772	34.799156
1063.861476	54655.855890	34.804173
1064.720133	54705.753318	34.809191
1065.567886	54772.308780	34.814208
1066.187482	54824.661319	34.819226
1067.593768	54884.959495	34.824244
1068.852069	54953.773709	34.829261
1069.291796	55016.957419	34.834279
1070.662762	55090.361480	34.839296
1071.883122	55146.145613	34.844314
1073.105430	55214.808009	34.849332
1074.380223	55275.203709	34.854349
1075.061016	55330.699372	34.859367
1076.192388	55410.242613	34.864384
1077.491937	55473.166352	34.869402
1078.636251	55520.837428	34.874420
1079.866873	55593.157523	34.879437
1081.215168	55648.024150	34.884455
1082.079833	55707.118186	34.889472
1083.266608	55774.351173	34.894490
1084.493492	55819.826549	34.899508
1085.213132	55876.772991	34.904525
1086.128649	55937.770890	34.909543
1087.242651	55999.756788	34.914560
1088.487523	56057.868182	34.919578
1089.776355	56117.896764	34.924596
1090.881940	56184.295573	34.929613
1092.155663	56234.175534	34.934631
1093.193773	56288.573248	34.939648
1094.026613	56345.243608	34.944666
1095.354317	56393.786410	34.949684
1095.758894	56446.600214	34.954701
1097.046823	56486.181525	34.959719
1097.988529	56534.025589	34.964736
1098.865996	56603.340893	34.969754
1100.134509	56649.134109	34.974772
1101.120669	56703.939620	34.979789
1102.471463	56752.814969	34.984807
1103.663042	56804.246902	34.989824
1104.241669	56860.135527	34.994842
1105.371243	56915.684869	34.999860
1106.239241	56979.078874	35.004877
1107.210494	57042.703709	35.009895
1108.434745	57096.757673	35.014912
1109.548229	57170.784398	35.019930
1110.923009	57236.276913	35.024948
1111.861629	57300.742972	35.029965
1112.940914	57364.123902	35.034983
1114.031687	57426.889282	35.040000
1115.266872	57487.100589	35.045018
1116.609844	57541.504056	35.050036
1117.487784	57616.923457	35.055053
1118.685297	57680.312029	35.060071
1120.293005	57749.016318	35.065088
1121.451255	57826.493766	35.070106
1122.977842	57871.799548	35.075124
1124.172935	57943.106989	35.080141
1125.377259	58002.843401	35.085159
1126.534735	58051.840276	35.090176
1127.240063	58113.661447	35.095194
1128.658391	58165.383592	35.100212
1129.721178	58234.440408	35.105229
1130.896267	58297.694872	35.110247
1132.261070	58344.330707	35.115264
1133.032518	58408.496780	35.120282
1134.440244	58463.455505	35.125300
1135.435940	58526.194331	35.130317
1136.700633	58580.106055	35.135335
1137.860791	58644.078982	35.140352
1138.807054	58706.420935	35.145370
1140.305186	58756.036825	35.150388
1141.419314	58817.112220	35.155405
1142.168869	58877.422018	35.160423
1143.312440	58939.815965	35.165440
1144.494895	59013.869199	35.170458
1145.420119	59068.917499	35.175476
1146.307148	59141.042572	35.180493
1147.686351	59208.533550	35.185511
1149.403168	59275.737668	35.190528
1150.073030	59333.858397	35.195546
1151.622706	59400.500379	35.200564
1152.638678	59459.409055	35.205581
1153.921471	59516.896249	35.210599
1155.399695	59573.890922	35.215616
1156.317945	59636.973887	35.220634
1157.618300	59698.940143	35.225652
1158.611511	59759.581105	35.230669
1159.950402	59821.889774	35.235687
1161.250169	59864.443418	35.240704
1161.848015	59938.565674	35.245722
1163.409074	59995.098956	35.250740
1164.536456	60063.467256	35.255757
1165.550416	60119.656056	35.260775
1167.248283	60170.047451	35.265792
1168.047421	60227.270234	35.270810
1168.739687	60276.401407	35.275828
1170.265744	60345.866437	35.280845
1171.321641	60412.829028	35.285863
1172.837026	60459.825151	35.290880
1173.428653	60516.796255	35.295898
1174.830450	60556.252492	35.300916
1175.801837	60610.847630	35.305933
1176.808316	60661.050775	35.310951
1178.046886	60706.698132	35.315968
1178.968161	60765.669098	35.320986
1179.900490	60820.599974	35.326004
1180.985642	60884.191747	35.331021
1182.164548	60948.180455	35.336039
1183.368890	61001.727198	35.341056
1184.414301	61074.757368	35.346074
1185.615923	61125.601895	35.351092
1186.785468	61205.360820	35.356109
1188.067891	61275.651556	35.361127
1189.750639	61334.314777	35.366144
1190.490019	61404.178159	35.371162
1191.847243	61471.109126	35.376180
1193.000196	61540.699256	35.381197
1194.196853	61608.890109	35.386215
1195.554909	61666.041409	35.391232
1196.589394	61740.847710	35.396250
1198.040713	61808.872646	35.401268
1199.488979	61882.595438	35.406285
1200.572302	61945.335662	35.411303
1201.446502	62013.964260	35.416320
1202.735800	62075.001384	35.421338
1204.029259	62147.514801	35.426356
1205.250672	62220.944943	35.431373
1206.901485	62284.432788	35.436391
1208.175087	62341.244377	35.441408
1209.183558	62415.322474	35.446426
1210.436533	62476.005444	35.451444
1211.541978	62547.948085	35.456461
1212.773847	62622.491929	35.461479
1214.131347	62689.616069	35.466496
1215.284434	62755.765853	35.471514
1216.371275	62822.831439	35.476532
1217.919508	62888.261350	35.481549
1218.948579	62961.666824	35.486567
1220.646083	63025.326514	35.491584
1221.519072	63092.261712	35.496602
1223.017544	63166.126070	35.501620
1224.198548	63229.873472	35.506637
1225.269484	63297.886082	35.511655
1227.030609	63359.992012	35.516672
1227.942899	63424.073185	35.521690
1229.234443	63492.583563	35.526708
1230.119738	63559.068615	35.531725
1231.690859	63626.680958	35.536743
1232.941871	63684.271498	35.541760
1233.943346	63762.710205	35.546778
1235.373303	63821.982337	35.551796
1236.707973	63886.486040	35.556813
1238.044717	63958.042028	35.561831
1239.005702	64010.854702	35.566848
1240.500303	64081.981165	35.571866
1241.583592	64145.682898	35.576884
1242.646553	64212.205182	35.581901
1244.251990	64276.762468	35.586919
1245.869000	64334.974611	35.591936
1247.029663	64401.836632	35.596954
1248.241398	64462.049756	35.601972
1249.176683	64514.323061	35.606989
1250.238000	64587.228126	35.612007
1251.923397	64647.259920	35.617024
1252.680991	64703.119409	35.622042
1254.071676	64773.251155	35.627060
1255.127224	64835.813083	35.632077
1256.266029	64888.865671	35.637095
1257.700397	64940.504610	35.642112
1258.834179	64999.762586	35.647130
1259.717080	65041.200185	35.652148
1261.011302	65109.511977	35.657165
1261.663396	65170.409525	35.662183
1263.584142	65234.381779	35.667200
1264.537614	65302.044688	35.672218
1265.636086	65367.912373	35.677236
1266.853199	65422.764522	35.682253
1267.651674	65499.353763	35.687271
1269.475551	65570.926727	35.692288
1270.930660	65640.208762	35.697306
1272.099362	65710.650110	35.702324
1273.605011	65776.967948	35.707341
1275.078588	65848.090040	35.712359
1276.698708	65908.768188	35.717376
1277.850165	65983.226994	35.722394
1279.109472	66040.308810	35.727412
1280.220742	66099.243668	35.732429
1281.725607	66170.697328	35.737447
1283.112647	66238.212564	35.742464
1284.478880	66304.775207	35.747482
1285.455386	66373.469383	35.752500
1287.328016	66435.628789	35.757517
1288.409087	66493.967813	35.762535
1289.865608	66556.407921	35.767552
1291.250607	66620.809452	35.772570
1292.099114	66692.614255	35.777588
1294.071821	66753.929360	35.782605
1295.084869	66824.062601	35.787623
1296.456493	66892.487390	35.792640
1297.590090	66954.719437	35.797658
1299.002483	67020.371327	35.802676
1300.313121	67080.467577	35.807693
1301.565367	67158.415381	35.812711
1303.089040	67211.083353	35.817728
1304.454002	67283.480119	35.822746
1305.639495	67347.851405	35.827764
1306.803979	67409.079336	35.832781
1308.369832	67482.876162	35.837799
1309.485081	67547.955426	35.842816
1310.938769	67618.528405	35.847834
1312.043425	67682.450978	35.852852
1313.669858	67750.046721	35.857869
1314.850685	67817.839032	35.862887
1316.059736	67879.105434	35.867904
1317.551559	67950.091251	35.872922
1318.322239	68010.844070	35.877940
1319.607363	68089.960941	35.882957
1320.989160	68166.783478	35.887975
1322.526117	68237.503422	35.892992
1324.105469	68302.195363	35.898010
1325.308548	68378.964197	35.903028
1327.327954	68438.769068	35.908045
1328.157700	68504.959205	35.913063
1329.399351	68573.478487	35.918080
1330.745832	68636.308156	35.923098
1332.271851	68707.113421	35.928116
1333.276852	68763.620611	35.933133
1334.876506	68840.379399	35.938151
1336.207403	68902.180049	35.943168
1337.278905	68969.017386	35.948186
1338.695890	69042.411426	35.953204
1340.118829	69096.175487	35.958221
1341.326028	69173.940171	35.963239
1342.868475	69236.151748	35.968256
1344.310439	69309.156382	35.973274
1345.084233	69362.604695	35.978292
1346.480688	69397.567255	35.983309
1347.447403	69467.107090	35.988327
1349.155254	69514.033073	35.993344
1350.326334	69579.374687	35.998362
1351.180816	69646.209753	36.003380
1352.640458	69705.497305	36.008397
1353.958525	69772.545078	36.013415
1355.344955	69836.720170	36.018432
1356.518994	69906.975930	36.023450
1358.073327	69976.209853	36.028468
1359.249333	70044.717983	36.033485
1360.607566	70119.314736	36.038503
1361.905869	70200.607976	36.043520
1363.520044	70268.161587	36.048538
1364.795607	70347.635144	36.053556
1366.646851	70411.909871	36.058573
1368.115601	70485.489866	36.063591
1369.357589	70551.266089	36.068608
1370.638851	70621.570320	36.073626
1371.887278	70690.423426	36.078644
1373.356285	70777.340250	36.083661
1375.012883	70855.349911	36.088679
1376.213716	70917.017411	36.093696
1377.831126	70994.261062	36.098714
1379.375149	71071.972368	36.103732
1381.057454	71142.139234	36.108749
1382.187682	71210.378962	36.113767
1383.181540	71279.362124	36.118784
1384.909051	71359.033981	36.123802
1386.167165	71428.064825	36.128820
1387.930477	71493.863139	36.133837
1389.101153	71573.394836	36.138855
1390.412593	71639.986167	36.143872
1391.879337	71715.786360	36.148890
1393.701176	71789.023452	36.153908
1395.065106	71857.874215	36.158925
1396.492644	71929.514255	36.163943
1397.958153	72009.596396	36.168960
1399.471580	72067.899328	36.173978
1400.624101	72140.406247	36.178996
1402.125880	72205.690002	36.184013
1403.567200	72280.001268	36.189031
1404.943369	72358.945888	36.194048
1406.446858	72423.887944	36.199066
1407.594570	72500.500274	36.204084
1409.398590	72561.887236	36.209101
1410.758563	72637.149504	36.214119
1412.329557	72703.626903	36.219136
1414.330232	72756.193491	36.224154
1415.087103	72840.606788	36.229172
1416.468239	72894.283893	36.234189
1417.983362	72968.851529	36.239207
1419.377109	73031.355073	36.244224
1421.007438	73089.502641	36.249242
1422.175905	73168.254202	36.254260
1423.380844	73227.456606	36.259277
1424.962087	73297.746368	36.264295
1426.201103	73368.469867	36.269312
1427.549652	73432.374702	36.274330
1429.128925	73516.142108	36.279348
1430.615827	73578.467700	36.284365
1432.254445	73652.511281	36.289383
1433.225442	73719.085144	36.294400
1434.952723	73787.618068	36.299418
1435.859638	73862.270748	36.304436
1437.648989	73939.306118	36.309453
1439.008337	74000.284698	36.314471
1440.074785	74064.159208	36.319488
1441.517658	74120.425747	36.324506
1442.907341	74187.517902	36.329524
1444.364703	74239.817818	36.334541
1445.652931	74316.983384	36.339559
1446.597319	74373.619814	36.344576
1448.226282	74440.117821	36.349594
1449.629524	74512.047310	36.354612
1451.379666	74588.533361	36.359629
1452.561290	74664.158615	36.364647
1454.137370	74741.799686	36.369664
1455.668050	74809.086666	36.374682
1456.856006	74887.599583	36.379700
1458.532919	74949.214630	36.384717
1459.598122	75035.169961	36.389735
1461.186796	75111.847449	36.394752
1462.328952	75188.595046	36.399770
1463.820465	75271.913015	36.404788
1466.090234	75354.400073	36.409805
1467.651249	75434.401572	36.414823
1468.711151	75520.295946	36.419840
1470.477195	75578.237692	36.424858
1471.875325	75655.541910	36.429876
1473.804082	75736.031434	36.434893
1475.497551	75816.925376	36.439911
1476.690921	75890.018789	36.444928
1478.518609	75958.731562	36.449946
1480.054867	76032.037703	36.454964
1481.242401	76108.248787	36.459981
1482.866106	76187.989361	36.464999
1484.254490	76264.296121	36.470016
1485.754390	76336.342032	36.475034
1487.132793	76422.746789	36.480052
1488.722064	76496.957954	36.485069
1490.484706	76565.505106	36.490087
1491.789410	76656.406472	36.495104
1493.326728	76729.524320	36.500122
1495.107195	76805.999253	36.505140
1496.559487	76872.226896	36.510157
1498.052754	76957.728636	36.515175
1499.814687	77036.474650	36.520192
1501.196528	77097.254042	36.525210
1502.830880	77181.442282	36.530228
1504.146061	77248.971758	36.535245
1505.916516	77341.791376	36.540263
1506.937819	77406.681634	36.545280
1508.824075	77486.726963	36.550298
1510.387076	77559.564326	36.555316
1511.564449	77637.947523	36.560333
1513.327890	77715.213097	36.565351
1514.758964	77798.738311	36.570368
1516.346423	77874.435691	36.575386
1517.794544	77949.749705	36.580404
1519.584271	78026.670002	36.585421
1521.089177	78106.903518	36.590439
1522.373777	78185.448856	36.595456
1523.595214	78246.483941	36.600474
1525.465673	78326.572206	36.605492
1527.019810	78411.802930	36.610509
1528.379201	78485.992144	36.615527
1529.763959	78569.767656	36.620544
1531.217557	78642.080274	36.625562
1532.875664	78722.329614	36.630580
1534.631991	78801.715018	36.635597
1536.056271	78869.421443	36.640615
1537.772641	78944.784880	36.645632
1538.981459	79022.204285	36.650650
1540.532086	79100.457222	36.655668
1542.075268	79166.055419	36.660685
1543.720455	79231.840508	36.665703
1544.521143	79293.830587	36.670720
1546.057274	79355.502994	36.675738
1547.568786	79423.361820	36.680756
1549.177782	79515.099189	36.685773
1550.624237	79572.263300	36.690791
1552.104679	79655.811759	36.695808
1553.811894	79726.073149	36.700826
1555.563465	79801.990854	36.705844
1556.952632	79876.901283	36.710861
1558.768680	79955.735884	36.715879
1559.932697	80026.526473	36.720896
1561.667368	80106.197735	36.725914
1563.246492	80200.615252	36.730932
1564.804119	80274.727562	36.735949
1566.792251	80353.739068	36.740967
1567.893136	80435.005449	36.745984
1569.245884	80510.125993	36.751002
1571.201393	80587.268196	36.756020
1572.650392	80673.269835	36.761037
1574.412102	80754.231007	36.766055
1576.163159	80846.622018	36.771072
1578.130496	80923.940676	36.776090
1579.524289	81000.690493	36.781108
1580.490292	81077.000689	36.786125
1582.674229	81152.030878	36.791143
1584.177563	81246.286417	36.796160
1585.962414	81328.563282	36.801178
1587.717918	81407.956266	36.806196
1588.952496	81490.053663	36.811213
1590.644505	81573.701453	36.816231
1592.115513	81659.918065	36.821248
1594.007675	81750.896282	36.826266
1595.499524	81829.090065	36.831284
1597.012618	81916.086414	36.836301
1599.163557	81998.447317	36.841319
1600.866591	82088.227228	36.846336
1602.147483	82154.557696	36.851354
1603.675710	82245.429759	36.856372
1605.206983	82324.632361	36.861389
1607.130928	82410.463625	36.866407
1608.792188	82511.109833	36.871424
1610.730343	82587.550718	36.876442
1612.198459	82667.359672	36.881460
1613.595153	82744.392539	36.886477
1615.520833	82826.487025	36.891495
1616.938811	82893.748056	36.896512
1618.480973	82975.941010	36.901530
1620.067103	83061.142911	36.906548
1621.834031	83146.734902	36.911565
1623.293763	83237.012677	36.916583
1625.007466	83316.645645	36.921600
1626.537763	83394.254887	36.926618
1628.312341	83475.437268	36.931636
1629.729900	83565.266539	36.936653
1631.327268	83650.151677	36.941671
1633.015867	83736.606645	36.946688
1634.488009	83826.364841	36.951706
1636.463230	83900.281955	36.956724
1638.168422	83988.547031	36.961741
1639.642735	84063.696020	36.966759
1641.024261	84146.462346	36.971776
1643.048053	84233.689976	36.976794
1644.312539	84324.762014	36.981812
1646.309726	84408.383075	36.986829
1647.905547	84491.458980	36.991847
1649.429385	84572.861119	36.996864
1651.115777	84636.891109	37.001882
1652.704464	84699.403308	37.006900
1653.940911	84773.843783	37.011917
1655.575957	84843.242232	37.016935
1656.855402	84916.193799	37.021952
1658.545396	84989.524797	37.026970
1660.205155	85058.704485	37.031988
1661.886440	85158.127764	37.037005
1663.292097	85230.439473	37.042023
1664.936198	85315.499630	37.047040
1666.964924	85402.831413	37.052058
1668.548339	85477.434821	37.057076
1669.962928	85564.305656	37.062093
1671.655740	85642.997986	37.067111
1673.377544	85734.421075	37.072128
1675.410371	85832.689219	37.077146
1676.779956	85919.580835	37.082164
1678.556304	86015.798892	37.087181
1680.028897	86101.027590	37.092199
1682.136599	86189.768642	37.097216
1683.566881	86285.104029	37.102234
1685.398288	86375.206772	37.107252
1686.851934	86465.673044	37.112269
1688.972578	86555.401607	37.117287
1690.792387	86665.351554	37.122304
1692.502761	86748.504724	37.127322
1694.279817	86835.829523	37.132340
1695.830912	86926.370680	37.137357
1697.555270	87012.246946	37.142375
1699.303959	87106.394682	37.147392
1701.163459	87204.833983	37.152410
1703.249188	87291.414857	37.157428
1704.991142	87382.751264	37.162445
1706.722292	87464.255804	37.167463
1708.146114	87562.092848	37.172480
1710.109529	87659.364215	37.177498
1712.224349	87736.234673	37.182516
1713.509297	87840.734818	37.187533
1715.297393	87917.568175	37.192551
1717.328862	88000.877415	37.197568
1718.947328	88099.306749	37.202586
1720.637508	88184.963690	37.207604
1721.834362	88276.502237	37.212621
1723.871396	88364.335835	37.217639
1726.139968	88456.911143	37.222656
1727.469516	88550.862972	37.227674
1729.304668	88642.049302	37.232692
1731.046871	88739.384202	37.237709
1732.723965	88824.690202	37.242727
1734.603442	88910.104181	37.247744
1736.505275	89009.049815	37.252762
1738.140939	89097.544043	37.257780
1740.042529	89186.693945	37.262797
1741.485863	89270.567719	37.267815
1743.422016	89369.128985	37.272832
1744.863017	89457.287224	37.277850
1746.662888	89548.215722	37.282868
1748.290732	89630.528159	37.287885
1750.167617	89715.818128	37.292903
1752.026587	89804.634371	37.297920
1753.434210	89907.500399	37.302938
1755.332956	89988.402690	37.307956
1757.309068	90103.904679	37.312973
1758.907842	90191.495432	37.317991
1760.771361	90269.653818	37.323008
1762.253317	90361.965284	37.328026
1764.107700	90451.988172	37.333044
1765.818996	90541.032493	37.338061
1767.590568	90613.477616	37.343079
1769.137044	90694.576357	37.348096
1770.639865	90771.157572	37.353114
1772.146953	90849.145120	37.358132
1773.725701	90931.747647	37.363149
1775.440461	91023.517757	37.368167
1777.567495	91102.790411	37.373184
1779.195454	91192.711539	37.378202
1780.807013	91281.824360	37.383220
1782.400169	91378.012492	37.388237
1784.194294	91464.296298	37.393255
1786.132772	91567.667948	37.398272
1787.485250	91660.130400	37.403290
1789.266729	91762.310555	37.408308
1791.273787	91875.254295	37.413325
1793.261284	91971.724811	37.418343
1795.081042	92070.769444	37.423360
1796.537427	92168.160212	37.428378
1798.266736	92273.062589	37.433396
1800.370753	92385.055138	37.438413
1802.036798	92488.028950	37.443431
1804.287504	92594.828080	37.448448
1806.054128	92702.007532	37.453466
1808.156842	92793.912415	37.458484
1809.877664	92915.992594	37.463501
1811.641072	93026.253658	37.468519
1813.511194	93128.424530	37.473536
1815.251533	93228.385269	37.478554
1817.240256	93334.961814	37.483572
1818.968864	93441.630134	37.488589
1820.808456	93551.082641	37.493607
1823.141758	93656.161425	37.498624
1824.940153	93762.249560	37.503642
1827.061014	93857.944663	37.508660
1828.799309	93972.585990	37.513677
1830.747903	94066.090536	37.518695
1832.703331	94163.650389	37.523712
1834.596046	94269.345253	37.528730
1836.639314	94368.159541	37.533748
1838.315827	94474.966348	37.538765
1840.227850	94568.465465	37.543783
1842.152572	94670.683618	37.548800
1843.892294	94776.695694	37.553818
1845.618533	94873.900713	37.558836
1847.881429	94980.604828	37.563853
1849.259165	95070.855381	37.568871
1851.163408	95168.477116	37.573888
1852.902249	95281.589448	37.578906
1854.908881	95370.791778	37.583924
1856.612202	95490.729999	37.588941
1858.291904	95588.045940	37.593959
1860.321010	95697.121459	37.598976
1862.033423	95801.556813	37.603994
1864.204271	95901.610938	37.609012
1865.950988	96008.259914	37.614029
1867.716326	96118.683813	37.619047
1869.800001	96228.830116	37.624064
1871.244636	96336.161285	37.629082
1873.379746	96436.704409	37.634100
1875.183737	96551.066083	37.639117
1876.987152	96658.849263	37.644135
1878.778355	96768.219265	37.649152
1880.251072	96890.708846	37.654170
1882.471867	96993.522094	37.659188
1884.257733	97102.450416	37.664205
1886.074105	97212.096903	37.669223
1888.170948	97320.888581	37.674240
1890.088162	97425.246576	37.679258
1891.523848	97516.255694	37.684276
1893.364971	97612.779372	37.689293
1895.270711	97707.391723	37.694311
1897.036493	97807.096963	37.699328
1898.650956	97918.209964	37.704346
1900.582745	98009.586556	37.709364
1902.311284	98109.653524	37.714381
1903.846833	98212.983622	37.719399
1905.687517	98320.969461	37.724416
1907.320804	98452.833581	37.729434
1909.362407	98571.145953	37.734452
1911.126262	98680.133840	37.739469
1913.453270	98802.509792	37.744487
1915.101346	98926.070013	37.749504
1917.279806	99046.150212	37.754522
1919.278132	99175.272610	37.759540
1921.197009	99302.366905	37.764557
1922.677266	99419.477158	37.769575
1924.773892	99532.066961	37.774592
1926.722457	99672.824361	37.779610
1928.335891	99802.884251	37.784628
1930.143957	99935.132790	37.789645
1932.919629	100070.374519	37.794663
1935.109808	100198.051098	37.799680
1937.167891	100323.251333	37.804698
1938.898117	100443.026543	37.809716
1940.765619	100562.768038	37.814733
1942.746830	100698.111349	37.819751
1945.017760	100824.193020	37.824768
1946.651901	100972.700782	37.829786
1948.971874	101090.991518	37.834804
1951.187886	101219.149834	37.839821
1953.186275	101352.718243	37.844839
1954.919729	101468.908805	37.849856
1956.674556	101610.579713	37.854874
1958.809327	101742.987332	37.859892
1960.503876	101875.362942	37.864909
1962.485445	102015.136399	37.869927
1964.591676	102150.364733	37.874944
1966.554030	102288.506838	37.879962
1968.618955	102420.104011	37.884980
1971.070933	102555.470087	37.889997
1972.766148	102680.254339	37.895015
1974.919955	102827.598812	37.900032
1977.023828	102944.066270	37.905050
1978.582943	103088.626878	37.910068
1980.309293	103215.589033	37.915085
1982.556008	103367.219503	37.920103
1984.558197	103491.236076	37.925120
1986.328124	103634.751756	37.930138
1988.627698	103767.572788	37.935156
1990.980169	103915.956046	37.940173
1992.559436	104057.563469	37.945191
1994.711306	104188.494732	37.950208
1996.400794	104325.572235	37.955226
1998.593172	104461.050090	37.960244
2000.643005	104601.051980	37.965261
2002.137274	104741.420332	37.970279
2004.639863	104879.146315	37.975296
2006.593021	105021.371315	37.980314
2008.444851	105159.060793	37.985332
2010.779474	105300.441147	37.990349
2012.288251	105440.011318	37.995367
2014.183278	105584.238498	38.000384
2016.167464	105732.383085	38.005402
2018.206279	105865.861843	38.010420
2020.519205	106008.985693	38.015437
2021.861715	106156.560497	38.020455
2023.655531	106280.607280	38.025472
2026.099235	106414.887083	38.030490
2027.706198	106543.985369	38.035508
2029.549349	106667.911720	38.040525
2031.535055	106818.508067	38.045543
2033.540972	106941.674490	38.050560
2034.980803	107085.205753	38.055578
2036.745065	107231.032721	38.060596
2038.648930	107375.760629	38.065613
2040.712069	107535.325747	38.070631
2042.788458	107686.139959	38.075648
2044.718859	107850.457146	38.080666
2047.041372	108003.960566	38.085684
2049.228624	108158.157908	38.090701
2051.605691	108326.592105	38.095719
2053.704381	108483.556481	38.100736
2055.456012	108644.621072	38.105754
2057.424642	108809.165079	38.110772
2059.438581	108965.181137	38.115789
2061.584315	109140.072059	38.120807
2063.412406	109307.709225	38.125824
2065.294829	109474.248110	38.130842
2067.699972	109652.562970	38.135860
2069.910161	109820.079396	38.140877
2071.621560	110006.189474	38.145895
2073.887965	110180.559449	38.150912
2076.166076	110340.205229	38.155930
2078.475337	110523.979871	38.160948
2080.788819	110695.047814	38.165965
2082.479724	110877.424609	38.170983
2085.061738	111047.501112	38.176000
2087.061045	111222.552101	38.181018
2088.731749	111400.090285	38.186036
2091.276207	111583.681431	38.191053
2093.229971	111761.836588	38.196071
2095.400917	111941.036628	38.201088
2097.667701	112115.631637	38.206106
2099.701362	112306.459136	38.211124
2101.967555	112476.718683	38.216141
2103.681009	112653.241807	38.221159
2106.316926	112839.171302	38.226176
2108.293327	113017.709616	38.231194
2110.260035	113195.806439	38.236212
2112.276085	113382.381061	38.241229
2114.462146	113565.898891	38.246247
2116.829682	113757.138387	38.251264
2118.971539	113939.751864	38.256282
2120.927384	114121.647073	38.261300
2123.251176	114301.177331	38.266317
2125.250558	114485.071433	38.271335
2127.352203	114670.535836	38.276352
2129.415516	114862.729210	38.281370
2131.155629	115051.219942	38.286388
2133.624351	115243.098208	38.291405
2135.928502	115438.453076	38.296423
2137.919809	115621.047738	38.301440
2140.357495	115806.477962	38.306458
2142.063407	115993.583673	38.311476
2144.608232	116182.144514	38.316493
2146.931950	116366.707518	38.321511
2148.696763	116542.404214	38.326528
2150.799071	116736.554488	38.331546
2152.819254	116926.507599	38.336564
2155.248182	117110.816825	38.341581
2156.891666	117304.661312	38.346599
2159.342694	117498.012615	38.351616
2161.724930	117684.272608	38.356634
2163.130288	117876.191261	38.361652
2165.685273	118047.141664	38.366669
2167.873280	118221.486206	38.371687
2169.852599	118384.207343	38.376704
2171.808048	118557.980970	38.381722
2173.799189	118742.074908	38.386740
2175.783679	118915.312876	38.391757
2177.725079	119095.268482	38.396775
2179.803992	119283.258127	38.401792
2181.801570	119469.764632	38.406810
2183.711925	119667.422859	38.411828
2185.987860	119860.762822	38.416845
2188.119808	120059.961307	38.421863
2190.420070	120253.147214	38.426880
2192.507971	120456.705555	38.431898
2194.325498	120655.283994	38.436916
2196.729861	120879.814143	38.441933
2199.109962	121084.218015	38.446951
2201.382420	121285.734880	38.451968
2203.652239	121504.251503	38.456986
2205.402662	121720.567239	38.462004
2207.815834	121931.211568	38.467021
2209.766196	122154.386606	38.472039
2211.862484	122373.569489	38.477056
2214.314817	122597.239350	38.482074
2216.451944	122828.190654	38.487092
2218.619551	123057.007319	38.492109
2221.094478	123284.495947	38.497127
2223.305181	123514.526343	38.502144
2225.538532	123740.368134	38.507162
2228.135223	123984.257411	38.512180
2230.353625	124201.211183	38.517197
2232.827390	124441.265873	38.522215
2234.863870	124664.733274	38.527232
2237.159477	124873.952626	38.532250
2239.520128	125122.135653	38.537268
2241.843039	125360.278370	38.542285
2244.217470	125589.229321	38.547303
2246.396681	125821.396453	38.552320
2248.900533	126045.775202	38.557338
2251.187690	126280.871377	38.562356
2253.451562	126509.857462	38.567373
2255.447676	126744.468971	38.572391
2257.346714	126977.460374	38.577408
2259.991883	127215.157456	38.582426
2262.260251	127445.733912	38.587444
2264.673763	127685.208071	38.592461
2266.998697	127934.606260	38.597479
2268.672706	128168.311967	38.602496
2271.154247	128407.627376	38.607514
2273.607491	128654.751411	38.612532
2275.811967	128891.524663	38.617549
2278.005510	129144.160555	38.622567
2280.233625	129388.659694	38.627584
2282.421324	129630.172238	38.632602
2284.517150	129885.581091	38.637620
2287.195138	130121.500480	38.642637
2288.927866	130373.441799	38.647655
2291.417284	130623.464504	38.652672
2293.737280	130864.798379	38.657690
2295.843643	131127.483318	38.662708
2298.442289	131380.157864	38.667725
2300.722143	131628.442809	38.672743
2302.934902	131882.995097	38.677760
2305.338010	132132.189895	38.682778
2307.532701	132388.828885	38.687796
2309.931344	132633.230932	38.692813
2312.169238	132884.422607	38.697831
2314.286661	133135.774139	38.702848
2316.757145	133359.460774	38.707866
2319.159823	133586.077614	38.712884
2321.437818	133816.953260	38.717901
2323.468863	134043.224521	38.722919
2325.464446	134271.710395	38.727936
2328.134841	134497.135275	38.732954
2330.684396	134722.592883	38.737972
2333.040201	134955.086466	38.742989
2335.201547	135191.697669	38.748007
2337.515461	135439.326112	38.753024
2339.415190	135666.945800	38.758042
2341.514671	135918.023897	38.763060
2343.571269	136168.856292	38.768077
2346.116700	136418.966412	38.773095
2348.060244	136684.970921	38.778112
2350.734154	136932.094316	38.783130
2352.650272	137212.826476	38.788148
2354.971491	137478.268880	38.793165
2357.506785	137751.115738	38.798183
2360.057152	138021.563388	38.803200
2362.472768	138288.683450	38.808218
2364.639781	138570.412466	38.813236
2367.240392	138849.549943	38.818253
2370.248810	139121.049040	38.823271
2372.502228	139393.200814	38.828288
2374.823502	139663.769893	38.833306
2376.979909	139940.610142	38.838324
2379.394868	140214.226159	38.843341
2381.948652	140499.611849	38.848359
2384.064686	140781.666540	38.853376
2386.919748	141048.543021	38.858394
2388.899441	141340.838583	38.863412
2391.030154	141616.182252	38.868429
2393.567234	141919.714628	38.873447
2395.731334	142211.872349	38.878464
2398.173960	142500.701166	38.883482
2400.539496	142791.079407	38.888500
2402.533231	143091.480387	38.893517
2405.328165	143382.696030	38.898535
2407.655809	143696.691939	38.903552
2410.519947	143988.941020	38.908570
2412.553943	144300.740212	38.913588
2414.762076	144603.464742	38.918605
2417.437510	144906.054526	38.923623
2419.533116	145218.509730	38.928640
2422.265009	145523.823164	38.933658
2424.319867	145838.712746	38.938676
2426.845760	146162.478665	38.943693
2429.244341	146464.917914	38.948711
2431.664108	146792.105948	38.953728
2434.070529	147103.648209	38.958746
2436.492492	147424.836301	38.963764
2438.989235	147739.300222	38.968781
2441.714942	148051.483586	38.973799
2443.828795	148382.067616	38.978816
2446.479001	148694.393515	38.983834
2448.888715	149015.301267	38.988852
2451.034790	149338.283080	38.993869
2453.666998	149652.622905	38.998887
2456.410456	149976.885968	39.003904
2459.300951	150296.190274	39.008922
2461.604898	150610.447386	39.013940
2463.960160	150926.843476	39.018957
2466.514985	151231.443269	39.023975
2469.084316	151556.428408	39.028992
2471.699381	151857.518801	39.034010
2474.286348	152179.826474	39.039028
2476.647525	152488.601635	39.044045
2478.873215	152771.554941	39.049063
2480.933510	153063.827513	39.054080
2483.573290	153362.979965	39.059098
2485.516417	153652.113095	39.064116
2487.517926	153960.406723	39.069133
2490.131433	154264.252165	39.074151
2492.400617	154569.155925	39.079168
2494.544868	154886.825970	39.084186
2496.936893	155206.680522	39.089204
2499.027225	155537.513984	39.094221
2501.578525	155857.461442	39.099239
2503.745745	156207.734735	39.104256
2506.126205	156542.298779	39.109274
2508.402087	156893.917470	39.114292
2510.227036	157242.041514	39.119309
2512.831626	157603.730765	39.124327
2514.817932	157974.176900	39.129344
2517.426351	158344.781887	39.134362
2519.915450	158718.645061	39.139380
2522.432426	159093.953414	39.144397
2525.092049	159477.062058	39.149415
2527.237365	159870.397148	39.154432
2529.897732	160260.378717	39.159450
2532.820659	160645.167242	39.164468
2534.933192	161038.019651	39.169485
2537.463191	161435.735129	39.174503
2539.847923	161842.692955	39.179520
2542.603275	162250.407919	39.184538
2545.520768	162655.116538	39.189556
2547.760713	163057.496016	39.194573
2550.423609	163460.751316	39.199591
2553.065799	163889.912557	39.204608
2555.938730	164285.369953	39.209626
2558.895180	164705.219007	39.214644
2560.652775	165121.957131	39.219661
2563.907220	165526.071887	39.224679
2566.420857	165943.445873	39.229696
2568.907692	166358.211073	39.234714
2571.572379	166771.478116	39.239732
2574.432753	167188.284803	39.244749
2576.953911	167599.560393	39.249767
2579.475053	168024.792333	39.254784
2582.074505	168442.409037	39.259802
2584.926694	168863.785072	39.264820
2587.363270	169289.507521	39.269837
2590.512630	169689.091595	39.274855
2593.160745	170104.945333	39.279872
2595.385376	170531.317604	39.284890
2598.054059	170961.597163	39.289908
2600.424257	171383.596286	39.294925
2602.901086	171813.225044	39.299943
2605.506300	172243.356742	39.304960
2608.321692	172661.966503	39.309978
2610.798324	173095.665730	39.314996
2613.028746	173529.939182	39.320013
2615.955222	173950.049510	39.325031
2618.388484	174390.149709	39.330048
2620.585298	174827.736989	39.335066
2623.313047	175275.719575	39.340084
2625.777723	175722.475943	39.345101
2628.521853	176158.638733	39.350119
2630.904188	176614.314304	39.355136
2633.210415	177060.302646	39.360154
2635.904471	177510.220005	39.365172
2638.734714	177976.271017	39.370189
2641.317238	178414.680253	39.375207
2643.861675	178872.171106	39.380224
2646.331215	179314.081961	39.385242
2648.885366	179748.819638	39.390260
2651.428842	180178.989492	39.395277
2654.083075	180603.404139	39.400295
2656.395922	181044.535254	39.405312
2658.827427	181483.160899	39.410330
2661.344375	181932.010742	39.415348
2664.320900	182375.685766	39.420365
2667.723381	182867.604195	39.425383
2670.359268	183293.659390	39.430400
2672.857182	183727.179859	39.435418
2675.395259	184174.004957	39.440436
2677.839078	184624.021676	39.445453
2680.617343	185062.761708	39.450471
2683.490052	185519.750879	39.455488
2685.610752	185979.450432	39.460506
2688.095430	186447.654691	39.465524
2690.683369	186919.934206	39.470541
2692.846336	187393.171271	39.475559
2695.372561	187877.250089	39.480576
2697.889036	188362.704169	39.485594
2700.775831	188857.043250	39.490612
2702.771281	189366.636975	39.495629
2705.466328	189865.125271	39.500647
2708.349102	190385.075025	39.505664
2710.461705	190901.413682	39.510682
2713.316074	191421.143839	39.515700
2716.418832	191948.482978	39.520717
2718.817483	192472.607012	39.525735
2721.725166	193003.816678	39.530752
2724.385168	193530.495136	39.535770
2726.952978	194071.795783	39.540788
2729.627102	194607.646186	39.545805
2732.740278	195151.964903	39.550823
2735.369571	195702.254604	39.555840
2737.946924	196242.114610	39.560858
2741.194681	196783.599139	39.565876
2743.619894	197335.857661	39.570893
2746.881272	197891.899359	39.575911
2749.369915	198442.246959	39.580928
2751.858980	199003.087486	39.585946
2754.651005	199552.604142	39.590964
2757.440529	200120.209405	39.595981
2760.173149	200676.038919	39.600999
2762.815625	201251.901404	39.606016
2765.305069	201829.694949	39.611034
2768.173191	202392.977175	39.616052
2771.094802	202975.914383	39.621069
2773.681790	203541.733601	39.626087
2776.671758	204113.816766	39.631104
2779.541010	204696.869102	39.636122
2782.506854	205270.585192	39.641140
2785.422569	205857.977504	39.646157
2788.200195	206432.996389	39.651175
2791.272115	207012.416304	39.656192
2793.507399	207590.495183	39.661210
2796.275899	208169.279610	39.666228
2798.905140	208757.943676	39.671245
2801.993058	209336.071241	39.676263
2805.143043	209929.737257	39.681280
2807.487768	210510.346160	39.686298
2810.715655	211095.771830	39.691316
2813.454222	211680.335284	39.696333
2816.988876	212245.417849	39.701351
2821.512515	212796.298561	39.706368
2824.540275	213349.852897	39.711386
2827.444263	213897.025752	39.716404
2830.803797	214439.199869	39.721421
2833.392328	214969.835017	39.726439
2835.898863	215478.128356	39.731456
2838.434902	215993.378346	39.736474
2841.310891	216494.679862	39.741492
2843.638478	217010.801932	39.746509
2845.902174	217529.043053	39.751527
2848.705881	218053.754441	39.756544
2851.545543	218573.405302	39.761562
2854.212355	219100.679424	39.766580
2856.485219	219641.606709	39.771597
2858.958709	220181.944129	39.776615
2861.740101	220723.072089	39.781632
2864.547385	221289.676575	39.786650
2867.225500	221838.950603	39.791668
2869.517019	222397.532421	39.796685
2872.668472	222975.845953	39.801703
2875.281505	223547.994470	39.806720
2878.001951	224132.599728	39.811738
2880.798884	224716.075337	39.816756
2883.060529	225319.145041	39.821773
2885.535588	225924.721769	39.826791
2888.327258	226533.703875	39.831808
2891.168822	227158.326971	39.836826
2893.725470	227774.407864	39.841844
2896.088532	228420.419370	39.846861
2899.097713	229058.708291	39.851879
2902.092381	229717.449339	39.856896
2904.784060	230373.417450	39.861914
2907.793371	231028.217569	39.866932
2910.330135	231706.233984	39.871949
2913.177667	232374.268134	39.876967
2916.164411	233044.997948	39.881984
2919.065883	233725.038050	39.887002
2922.480357	234413.964514	39.892020
2924.886353	235093.724433	39.897037
2928.210948	235781.341758	39.902055
2931.287834	236463.992070	39.907072
2933.761992	237156.871413	39.912090
2937.264175	237844.431655	39.917108
2940.465138	238539.480780	39.922125
2943.679907	239220.046188	39.927143
2946.714551	239907.903554	39.932160
2949.774219	240614.350560	39.937178
2953.104772	241287.500425	39.942196
2956.035164	241976.842128	39.947213
2958.719869	242679.633161	39.952231
2962.012947	243373.410470	39.957248
2965.056138	244066.488030	39.962266
2967.974821	244753.613163	39.967284
2971.122325	245440.420824	39.972301
2974.340702	246120.940592	39.977319
2977.699624	246816.347361	39.982336
2980.466700	247516.441987	39.987354
2983.879499	248189.353951	39.992372
2986.861569	248873.533163	39.997389
2989.544001	249565.326390	40.002407
2992.801561	250251.438356	40.007424
2995.390015	250950.886529	40.012442
2998.507948	251627.514104	40.017460
3002.014789	252325.618633	40.022477
3004.853233	253017.372422	40.027495
3007.950429	253693.282716	40.032512
3010.643694	254384.011232	40.037530
3014.074375	255069.159741	40.042548
3016.616645	255767.880976	40.047565
3019.788238	256457.685982	40.052583
3022.776859	257145.585490	40.057600
3025.099102	257842.018565	40.062618
3027.979564	258522.510475	40.067636
3030.851917	259207.165558	40.072653
3033.763068	259865.521306	40.077671
3037.005090	260534.845329	40.082688
3039.798111	261209.214102	40.087706
3042.174534	261883.669414	40.092724
3045.401171	262564.972621	40.097741
3047.940746	263250.036564	40.102759
3050.956430	263944.648068	40.107776
3053.862804	264647.933236	40.112794
3056.433596	265348.929389	40.117812
3059.449600	266059.680470	40.122829
3061.987690	266782.845010	40.127847
3065.082691	267509.396740	40.132864
3067.810680	268253.957015	40.137882
3070.877830	268985.200587	40.142900
3073.975203	269721.208513	40.147917
3076.634173	270471.273235	40.152935
3080.214332	271217.632023	40.157952
3083.257473	271986.037166	40.162970
3086.105239	272753.780377	40.167988
3089.305901	273522.477416	40.173005
3092.198628	274300.332996	40.178023
3095.473889	275076.318344	40.183040
3098.255410	275866.696954	40.188058
3101.195510	276656.890642	40.193076
3103.951142	277449.746453	40.198093
3107.232499	278272.148380	40.203111
3110.747591	279066.519600	40.208128
3113.390026	279882.909273	40.213146
3116.586592	280695.521168	40.218164
3119.979958	281516.651172	40.223181
3123.019927	282337.065319	40.228199
3126.320742	283153.391668	40.233216
3129.359138	283979.779968	40.238234
3132.554336	284806.997282	40.243252
3135.786464	285642.095973	40.248269
3138.927286	286482.784950	40.253287
3142.110870	287312.741164	40.258304
3145.356158	288158.343976	40.263322
3148.754017	288991.571662	40.268340
3151.877935	289834.403781	40.273357
3154.761561	290671.625476	40.278375
3157.967014	291512.264095	40.283392
3160.992666	292366.985449	40.288410
3164.074379	293215.643263	40.293428
3167.691311	294069.130921	40.298445
3170.826469	294926.642300	40.303463
3174.053241	295773.869792	40.308480
3177.434565	296648.226113	40.313498
3180.692180	297495.677280	40.318516
3184.290803	298330.876418	40.323533
3187.024616	299199.556901	40.328551
3190.508670	300047.010064	40.333568
3193.698735	300902.365768	40.338586
3196.830801	301747.892631	40.343604
3200.598728	302598.662991	40.348621
3203.626875	303462.913216	40.353639
3206.713514	304306.705335	40.358656
3209.590280	305170.773071	40.363674
3213.190779	306025.980986	40.368692
3216.409302	306889.534489	40.373709
3219.672955	307746.339530	40.378727
3222.640694	308611.323755	40.383744
3225.312370	309466.516131	40.388762
3228.794371	310326.541485	40.393780
3232.134840	311177.867807	40.398797
3235.267642	312048.500613	40.403815
3238.605629	312906.775809	40.408832
3242.873668	313728.672879	40.413850
3246.228832	314545.926709	40.418868
3249.204188	315357.489674	40.423885
3252.417881	316156.438516	40.428903
3255.600152	316958.398002	40.433920
3258.835939	317778.555654	40.438938
3261.972715	318597.013254	40.443956
3264.798082	319415.402691	40.448973
3267.781688	320242.379750	40.453991
3271.119676	321081.897085	40.459008
3274.212297	321915.244701	40.464026
3277.405792	322757.238147	40.469044
3280.572389	323599.269575	40.474061
3283.421038	324456.862157	40.479079
3286.766829	325310.045700	40.484096
3289.673186	326174.088705	40.489114
3292.510780	327048.881625	40.494132
3295.538991	327926.644797	40.499149
3298.596779	328825.314756	40.504167
3302.107181	329718.337351	40.509184
3305.438472	330626.436993	40.514202
3308.242368	331542.208432	40.519220
3311.821350	332444.467689	40.524237
3314.760125	333384.451290	40.529255
3318.000383	334301.280255	40.534272
3321.111860	335233.301340	40.539290
3324.534244	336172.023015	40.544308
3327.953963	337115.337550	40.549325
3331.055060	338066.743351	40.554343
3334.157702	339022.993672	40.559360
3337.743970	339983.885721	40.564378
3340.773357	340956.505522	40.569396
3344.669023	341917.778467	40.574413
3348.201542	342884.027092	40.579431
3351.519116	343854.365339	40.584448
3354.996234	344831.726519	40.589466
3358.181327	345809.105280	40.594484
3362.050744	346787.134842	40.599501
3364.911158	347767.347523	40.604519
3368.302113	348745.445149	40.609536
3372.090921	349725.175723	40.614554
3375.711590	350717.935721	40.619572
3379.359364	351688.805654	40.624589
3382.665370	352680.869923	40.629607
3385.666422	353668.286123	40.634624
3389.638180	354654.987377	40.639642
3392.819317	355645.913487	40.644660
3396.028934	356634.775624	40.649677
3399.592712	357640.585672	40.654695
3402.705837	358643.568825	40.659712
3406.208538	359636.166828	40.664730
3409.239619	360651.314141	40.669748
3412.671531	361648.368685	40.674765
3416.209401	362661.467565	40.679783
3419.392951	363676.386586	40.684800
3422.734052	364699.812002	40.689818
3426.301662	365712.978310	40.694836
3429.698671	366730.950731	40.699853
3433.363734	367751.252535	40.704871
3436.841618	368781.683055	40.709888
3440.447369	369799.158500	40.714906
3443.762934	370827.512509	40.719924
3447.606746	371852.705562	40.724941
3451.047205	372874.199300	40.729959
3454.589188	373893.688410	40.734976
3457.744441	374929.236554	40.739994
3461.515006	375956.288958	40.745012
3465.516920	376960.908014	40.750016
3468.621942	377944.317373	40.755021
3471.845467	378863.497773	40.760026
3475.393431	379752.198239	40.765031
3478.388931	380588.745576	40.770036
3481.661726	381365.270066	40.775040
3484.441084	382089.261198	40.780045
3487.217493	382734.645601	40.785050
3490.216384	383347.656314	40.790055
3492.151915	383902.826877	40.795060
3494.803771	384392.011895	40.800064
3496.867053	384850.507461	40.805069
3499.126028	385248.208075	40.810074
3501.064840	385594.667237	40.815079
3503.054477	385912.780211	40.820084
3505.394572	386171.933855	40.825088
3506.976224	386386.825265	40.830093
3508.367552	386558.509209	40.835098
3510.193764	386683.791533	40.840103
3511.377631	386791.605465	40.845108
3512.849522	386843.216794	40.850112
3513.805977	386883.433464	40.855117
3514.734959	386869.579082	40.860122
3515.888650	386844.163637	40.865127
3516.695673	386793.389428	40.870132
3517.701226	386721.486967	40.875136
3518.505441	386623.136386	40.880141
3519.006912	386483.958311	40.885146
3519.786013	386348.620430	40.890151
3520.285842	386201.393052	40.895156
3521.028540	386016.755235	40.900160
3521.488052	385832.414227	40.905165
3521.618513	385623.216979	40.910170
3522.167811	385411.946796	40.915175
3522.363516	385195.246074	40.920180
3522.757800	384939.006547	40.925184
3523.010344	384699.340663	40.930189
3523.226340	384451.655027	40.935194
3523.387375	384183.054083	40.940199
3523.489645	383923.828574	40.945204
3523.914321	383634.715958	40.950208
3523.818993	383356.370989	40.955213
3524.137998	383072.753017	40.960218
3524.054394	382776.194383	40.965223
3523.714528	382487.137604	40.970228
3524.012902	382184.596151	40.975232
3524.161762	381895.862630	40.980237
3524.071052	381585.604923	40.985242
3524.230896	381264.436117	40.990247
3523.946156	380961.946181	40.995252
3524.055068	380641.463279	41.000256
3524.046493	380344.001739	41.005261
3524.164182	380026.023926	41.010266
3523.867613	379708.818072	41.015271
3523.747787	379391.377599	41.020276
3523.649780	379073.041061	41.025280
3523.562393	378766.609499	41.030285
3523.536389	378452.546064	41.035290
3523.509662	378134.695006	41.040295
3523.178660	377816.582959	41.045300
3522.952793	377500.152251	41.050304
3522.794782	377190.183409	41.055309
3522.513872	376867.836319	41.060314
3522.712484	376569.436485	41.065319
3522.664683	376257.103042	41.070324
3522.533919	375937.997636	41.075328
3522.276813	375633.461516	41.080333
3522.191748	375322.392991	41.085338
3521.825006	375017.333698	41.090343
3521.842833	374715.919150	41.095348
3521.798538	374412.275809	41.100352
3521.581264	374108.325928	41.105357
3521.199463	373822.051482	41.110362
3521.320585	373515.527488	41.115367
3520.693857	373223.696982	41.120372
3520.749926	372912.959911	41.125376
3520.629215	372632.195041	41.130381
3520.032136	372347.361342	41.135386
3520.426009	372059.651795	41.140391
3520.065192	371775.029281	41.145396
3520.148306	371484.339503	41.150400
3520.327499	371203.843490	41.155405
3519.796354	370917.105001	41.160410
3519.682566	370632.965639	41.165415
3519.618236	370355.445923	41.170420
3519.446759	370072.427633	41.175424
3519.373574	369801.280112	41.180429
3519.164496	369524.562327	41.185434
3518.759793	369256.205021	41.190439
3518.539807	368985.606089	41.195444
3518.401463	368713.950207	41.200448
3518.164954	368455.466875	41.205453
3518.086935	368200.970442	41.210458
3518.294402	367928.465416	41.215463
3518.187275	367672.876376	41.220468
3517.898691	367413.883610	41.225472
3517.609918	367155.269621	41.230477
3517.591099	366902.734038	41.235482
3517.419990	366656.495480	41.240487
3517.394945	366410.308199	41.245492
3517.292060	366149.725173	41.250496
3516.945646	365906.099127	41.255501
3516.834790	365657.098624	41.260506
3517.042546	365412.797414	41.265511
3516.918346	365173.043248	41.270516
3516.810813	364928.736441	41.275520
3516.261677	364693.719854	41.280525
3516.203017	364459.818895	41.285530
3516.254858	364216.853268	41.290535
3516.153679	363993.855587	41.295540
3516.245081	363751.134001	41.300544
3515.845121	363527.391799	41.305549
3515.494772	363289.029640	41.310554
3515.476948	363058.058628	41.315559
3515.379419	362848.696734	41.320564
3514.856452	362618.919297	41.325568
3514.992429	362404.791467	41.330573
3514.533910	362191.771452	41.335578
3514.852232	361971.411823	41.340583
3514.423484	361768.624631	41.345588
3514.607651	361540.100480	41.350592
3514.386030	361333.847455	41.355597
3514.153461	361131.177727	41.360602
3514.619220	360919.452572	41.365607
3514.047665	360722.321977	41.370612
3513.968176	360503.919602	41.375616
3513.512597	360299.856053	41.380621
3513.301720	360096.540645	41.385626
3513.646531	359905.182496	41.390631
3513.343595	359715.042558	41.395636
3513.039033	359516.820416	41.400640
3513.188408	359329.097792	41.405645
3512.864384	359143.633542	41.410650
3512.735468	358957.807285	41.415655
3512.286580	358777.874998	41.420660
3512.699421	358583.016239	41.425664
3512.319027	358394.303301	41.430669
3512.155863	358229.876301	41.435674
3511.878341	358041.246755	41.440679
3512.040349	357874.479749	41.445684
3512.267289	357699.950327	41.450688
3512.089920	357528.177053	41.455693
3511.566507	357351.653563	41.460698
3511.758739	357171.535361	41.465703
3511.423100	357004.078995	41.470708
3511.418991	356845.109329	41.475712
3511.371195	356674.963019	41.480717
3511.139235	356512.952036	41.485722
3511.057752	356336.048668	41.490727
3510.909875	356180.300409	41.495732
3511.018215	356023.189698	41.500736
3510.985085	355881.273539	41.505741
3510.714608	355718.679873	41.510746
3511.040842	355547.020203	41.515751
3510.316081	355399.059290	41.520756
3510.537084	355243.375759	41.525760
3510.687336	355095.759524	41.530765
3510.424889	354935.422589	41.535770
3510.158886	354788.302064	41.540775
3509.891264	354651.398651	41.545780
3510.243434	354493.276299	41.550784
3510.082350	354348.246915	41.555789
3509.947086	354200.416941	41.560794
3509.705764	354061.498898	41.565799
3509.936539	353927.259485	41.570804
3509.934571	353774.475709	41.575808
3509.525927	353629.202134	41.580813
3509.461244	353499.811028	41.585818
3509.148607	353349.158022	41.590823
3508.966827	353235.060257	41.595828
3509.462186	353101.030162	41.600832
3509.396729	352970.569465	41.605837
3508.957221	352832.083711	41.610842
3508.866620	352703.074689	41.615847
3508.646135	352575.686815	41.620852
3508.963770	352443.893150	41.625856
3508.720944	352325.429682	41.630861
3508.493314	352197.507627	41.635866
3508.799732	352069.832014	41.640871
3508.366450	351951.168169	41.645876
3508.322625	351827.155837	41.650880
3508.109987	351704.135347	41.655885
3508.305832	351593.531368	41.660890
3508.411243	351461.461819	41.665895
3507.486607	351357.463293	41.670900
3508.096872	351250.885874	41.675904
3507.955364	351129.504337	41.680909
3507.947911	351029.555597	41.685914
3508.221631	350903.609015	41.690919
3507.506185	350786.764379	41.695924
3507.383198	350676.308786	41.700928
3507.433307	350572.867105	41.705933
3507.267690	350471.797470	41.710938
3507.600013	350365.565636	41.715943
3507.339628	350270.890660	41.720948
3507.140316	350166.571550	41.725952
3506.982846	350054.441492	41.730957
3506.848685	349951.509632	41.735962
3507.098184	349849.585132	41.740967
3507.101749	349772.077180	41.745972
3507.518906	349657.517223	41.750976
3507.337393	349555.099932	41.755981
3506.842293	349449.324945	41.760986
3506.976239	349343.908850	41.765991
3506.869594	349267.052457	41.770996
3506.836771	349166.390179	41.776000
3506.722426	349063.071111	41.781005
3506.912656	348972.414741	41.786010
3506.718525	348867.328042	41.791015
3506.531602	348781.839802	41.796020
3506.538021	348685.542402	41.801024
3506.703404	348591.380702	41.806029
3506.498615	348503.250690	41.811034
3506.588677	348401.880479	41.816039
3506.508741	348323.060235	41.821044
3506.167813	348228.137737	41.826048
3506.464387	348141.072360	41.831053
3506.418833	348044.069403	41.836058
3506.208626	347957.184460	41.841063
3506.260387	347872.241260	41.846068
3506.583792	347793.432965	41.851072
3506.317782	347698.675193	41.856077
3506.050985	347614.213314	41.861082
3506.191842	347522.009928	41.866087
3506.053418	347439.815552	41.871092
3506.007156	347350.335725	41.876096
3505.985630	347274.173223	41.881101
3505.950769	347195.902554	41.886106
3506.036584	347099.537292	41.891111
3505.479957	347028.745811	41.896116
3505.908421	346947.376815	41.901120
3505.803322	346856.964219	41.906125
3505.553731	346790.420700	41.911130
3505.481143	346702.138131	41.916135
3505.612702	346630.272142	41.921140
3505.638380	346554.761622	41.926144
3505.527425	346479.551949	41.931149
3505.268976	346405.432942	41.936154
3505.504392	346329.050158	41.941159
3505.116366	346261.179797	41.946164
3505.479688	346188.869857	41.951168
3505.320967	346115.878673	41.956173
3505.127141	346037.223376	41.961178
3505.252107	345959.357033	41.966183
3504.986583	345900.263348	41.971188
3504.934882	345830.381920	41.976192
3504.878302	345765.026532	41.981197
3504.985856	345694.077551	41.986202
3504.686849	345621.717400	41.991207
3504.547528	345567.484777	41.996212
3504.544555	345497.823858	42.001216
3504.825121	345439.279590	42.006221
3504.606094	345377.889565	42.011226
3504.599310	345308.000035	42.016231
3504.517064	345256.478365	42.021236
3504.564628	345199.114194	42.026240
3504.562842	345134.054112	42.031245
3504.169744	345084.182503	42.036250
3504.241643	345019.136104	42.041255
3503.968858	344964.974231	42.046260
3504.223392	344910.526437	42.051264
3504.425936	344857.154509	42.056269
3504.399744	344806.894614	42.061274
3504.729456	344739.010686	42.066279
3504.275998	344677.300102	42.071284
3504.017421	344616.525074	42.076288
3504.224150	344566.991148	42.081293
3504.154453	344516.534230	42.086298
3504.183604	344451.518856	42.091303
3504.301399	344401.947746	42.096308
3504.012953	344341.609117	42.101312
3504.243207	344286.884452	42.106317
3503.704974	344242.983709	42.111322
3504.203838	344190.861081	42.116327
3504.156765	344143.120538	42.121332
3504.168712	344091.582382	42.126336
3504.182751	344022.780235	42.131341
3503.700423	343977.827986	42.136346
3503.844670	343926.802824	42.141351
3503.925802	343884.279446	42.146356
3504.004964	343825.636771	42.151360
3503.826441	343789.637287	42.156365
3503.517226	343728.105841	42.161370
3503.761180	343682.607430	42.166375
3503.894044	343638.651846	42.171380
3504.037027	343585.795753	42.176384
3503.716094	343539.851535	42.181389
3503.454167	343495.372704	42.186394
3503.907372	343443.866292	42.191399
3504.027031	343401.031188	42.196404
3503.724305	343353.558346	42.201408
3503.659627	343300.912260	42.206413
3503.515782	343258.347005	42.211418
3503.687690	343206.070596	42.216423
3503.207919	343173.448321	42.221428
3503.761704	343122.230813	42.226432
3503.790046	343079.765546	42.231437
3503.526695	343038.134029	42.236442
3503.719560	342985.803159	42.241447
3503.472368	342946.737010	42.246452
3503.537503	342897.833035	42.251456
3503.450420	342856.860240	42.256461
3503.197099	342815.226886	42.261466
3503.193522	342765.087596	42.266471
3503.387068	342730.579821	42.271476
3503.510803	342690.056963	42.276480
3503.187308	342641.391367	42.281485
3503.017156	342606.965754	42.286490
3503.167272	342554.666343	42.291495
3503.355017	342530.889091	42.296500
3503.303510	342480.680605	42.301504
3503.488220	342446.402765	42.306509
3503.058270	342420.535354	42.311514
3502.863837	342379.731335	42.316519
3502.798213	342342.059987	42.321524
3503.203038	342299.229790	42.326528
3503.094086	342269.726976	42.331533
3503.212158	342233.552370	42.336538
3503.191236	342199.789535	42.341543
3502.999667	342162.849621	42.346548
3503.058198	342122.793970	42.351552
3503.320732	342073.273167	42.356557
3503.227166	342042.648990	42.361562
3503.250926	342002.369799	42.366567
3503.020285	341972.936611	42.371572
3503.433381	341932.749031	42.376576
3503.110531	341884.539952	42.381581
3502.900462	341854.950888	42.386586
3503.351893	341800.009722	42.391591
3503.256908	341773.097823	42.396596
3503.040615	341734.152612	42.401600
3503.216674	341704.096227	42.406605
3503.078675	341666.410037	42.411610
3503.140846	341619.945698	42.416615
3502.913827	341594.605337	42.421620
3502.851045	341549.508061	42.426624
3502.972407	341520.705984	42.431629
3502.606279	341491.903817	42.436634
3502.982605	341452.001129	42.441639
3502.846436	341421.993315	42.446644
3502.857096	341383.495344	42.451648
3503.338219	341352.017908	42.456653
3502.962435	341312.003802	42.461658
3502.837860	341278.866530	42.466663
3502.881722	341245.474051	42.471668
3502.387131	341218.954750	42.476672
3502.647965	341179.807195	42.481677
3502.497443	341158.446613	42.486682
3502.528107	341121.801408	42.491687
3502.673423	341086.079045	42.496692
3502.168413	341067.316546	42.501696
3502.523991	341046.232755	42.506701
3502.317852	341017.506894	42.511706
3502.385468	340987.187149	42.516711
3502.191771	340967.587681	42.521716
3502.568704	340946.525919	42.526720
3502.444097	340917.812657	42.531725
3502.428251	340886.107373	42.536730
3502.204925	340860.359066	42.541735
3502.512195	340834.731207	42.546740
3502.474429	340808.496160	42.551744
3502.386476	340782.345222	42.556749
3502.278264	340772.292980	42.561754
3502.457584	340731.352324	42.566759
3502.454557	340707.145965	42.571764
3502.009226	340682.398479	42.576768
3502.438760	340656.420819	42.581773
3502.428808	340640.835413	42.586778
3502.416391	340601.399377	42.591783
3502.309293	340590.863786	42.596788
3502.049521	340556.907862	42.601792
3502.265523	340534.167367	42.606797
3502.078528	340515.990545	42.611802
3502.532522	340487.313613	42.616807
3502.390371	340458.806141	42.621812
3502.013331	340438.751918	42.626816
3502.168706	340424.767938	42.631821
3501.840309	340400.739375	42.636826
3501.849454	340379.226221	42.641831
3502.101353	340364.921995	42.646836
3501.832264	340329.543359	42.651840
3502.169718	340314.183201	42.656845
3501.864694	340291.371440	42.661850
3502.008295	340271.286581	42.666855
3501.906708	340265.428739	42.671860
3502.114870	340250.521039	42.676864
3502.359138	340233.166620	42.681869
3501.957751	340218.201635	42.686874
3502.052643	340183.910199	42.691879
3502.102214	340156.542190	42.696884
3502.051990	340149.989747	42.701888
3501.965029	340121.854792	42.706893
3501.275730	340105.409099	42.711898
3501.529396	340087.570010	42.716903
3501.811901	340086.178254	42.721908
3501.545422	340063.894307	42.726912
3501.832306	340045.897436	42.731917
3501.879917	340039.889091	42.736922
3501.624994	340011.932876	42.741927
3501.740236	340003.218589	42.746932
3501.499510	339980.879707	42.751936
3501.644899	339965.066294	42.756941
3501.501474	339953.061369	42.761946
3501.920566	339935.755757	42.766951
3501.383179	339935.534724	42.771956
3501.704679	339914.582727	42.776960
3501.814766	339903.097568	42.781965
3502.050290	339886.659756	42.786970
3501.893825	339866.723292	42.791975
3502.017187	339858.338265	42.796980
3501.880906	339843.382531	42.801985
3501.873390	339815.946900	42.806989
3501.785007	339802.865339	42.811994
3501.624873	339779.801744	42.816999
3502.027465	339775.441541	42.822004
3501.694036	339756.244669	42.827009
3502.030422	339728.195786	42.832013
3501.758951	339720.253876	42.837018
3501.984795	339692.654526	42.842023
3501.831895	339687.389458	42.847028
3501.635200	339671.171688	42.852033
3502.122968	339652.558365	42.857037
3501.620960	339639.134558	42.862042
3501.488643	339615.379946	42.867047
3501.887452	339605.502387	42.872052
3501.465834	339597.863634	42.877057
3501.741379	339582.487411	42.882061
3501.843554	339568.511412	42.887066
3501.956285	339551.736647	42.892071
3501.902611	339545.108347	42.897076
3501.915825	339521.559774	42.902081
3501.896955	339502.008447	42.907085
3501.487205	339486.332468	42.912090
3501.476164	339471.178999	42.917095
3501.770152	339467.751158	42.922100
3501.532753	339446.606552	42.927105
3501.846958	339426.291117	42.932109
3501.586977	339420.661325	42.937114
3501.748723	339408.761076	42.942119
3501.790174	339395.887923	42.947124
3501.713743	339382.448342	42.952129
3501.859070	339364.142689	42.957133
3501.316749	339352.861063	42.962138
3501.422561	339331.611874	42.967143
3501.571275	339328.333874	42.972148
3501.643846	339319.498949	42.977153
3501.815738	339296.027134	42.982157
3501.726579	339293.218603	42.987162
3501.469076	339285.248983	42.992167
3501.465043	339259.566943	42.997172
3501.443308	339244.872763	43.002177
3501.435561	339237.957512	43.007181
3501.209523	339236.823228	43.012186
3501.892989	339228.833629	43.017191
3501.533875	339210.428761	43.022196
3501.599376	339200.908343	43.027201
3502.055698	339185.885115	43.032205
3501.725768	339165.797378	43.037210
3501.745845	339148.579195	43.042215
3501.776310	339142.853094	43.047220
3501.759732	339119.588628	43.052225
3501.861333	339103.273107	43.057229
3501.672305	339089.164447	43.062234
3501.802951	339074.929518	43.067239
3502.161944	339069.686044	43.072244
3501.626106	339041.950985	43.077249
3501.840188	339023.049550	43.082253
3501.637699	339019.292426	43.087258
3501.897810	338999.900638	43.092263
3501.866434	338986.174149	43.097268
3501.681908	338975.268753	43.102273
3501.604435	338949.089398	43.107277
3501.717652	338940.934600	43.112282
3502.050962	338916.420152	43.117287
3501.776861	338911.123060	43.122292
3501.455551	338899.959310	43.127297
3501.684350	338885.632674	43.132301
3501.588438	338869.297068	43.137306
3501.752577	338856.099395	43.142311
3501.668536	338847.415982	43.147316
3501.477364	338827.128360	43.152321
3501.652811	338821.837259	43.157325
3501.467339	338814.568280	43.162330
3501.909733	338796.877043	43.167335
3501.737802	338779.968418	43.172340
3501.604665	338768.317489	43.177345
3501.796857	338759.184007	43.182349
3501.550025	338748.186567	43.187354
3501.819150	338719.486260	43.192359
3501.892504	338710.829064	43.197364
3501.574900	338687.891098	43.202369
3501.812917	338681.293321	43.207373
3501.965024	338673.844392	43.212378
3501.920338	338651.855462	43.217383
3501.716015	338642.173648	43.222388
3501.256827	338624.216415	43.227393
3501.459345	338600.535925	43.232397
3501.430414	338591.513258	43.237402
3501.614850	338583.067526	43.242407
3501.146096	338592.091893	43.247412
3501.041297	338584.810255	43.252417
3501.289622	338562.826319	43.257421
3501.371315	338554.930652	43.262426
3501.470582	338556.364674	43.267431
3501.551940	338542.162668	43.272436
3501.350056	338547.661552	43.277441
3501.568787	338527.309677	43.282445
3501.480385	338512.523903	43.287450
3501.686587	338501.531848	43.292455
3501.944649	338503.678488	43.297460
3501.489456	338481.219622	43.302465
3501.742055	338471.618901	43.307469
3501.634623	338463.498491	43.312474
3501.627310	338444.377074	43.317479
3501.598258	338431.234877	43.322484
3501.381301	338424.148744	43.327489
3501.826770	338417.747348	43.332493
3501.530139	338389.491234	43.337498
3501.671673	338371.795966	43.342503
3501.229334	338370.720899	43.347508
3501.339697	338370.017148	43.352513
3501.535389	338342.548618	43.357517
3501.370626	338340.082410	43.362522
3501.806600	338323.892264	43.367527
3501.584684	338326.724253	43.372532
3501.616913	338307.876301	43.377537
3501.666660	338291.492231	43.382541
3501.729547	338285.455774	43.387546
3501.563847	338262.188637	43.392551
3501.456712	338245.625639	43.397556
3501.302819	338247.582407	43.402561
3501.714980	338229.310747	43.407565
3501.769230	338222.233032	43.412570
3501.573984	338205.734649	43.417575
3501.595196	338198.458661	43.422580
3501.749204	338191.568778	43.427585
3501.912489	338159.146472	43.432589
3501.441374	338158.940493	43.437594
3501.583189	338144.169435	43.442599
3501.432513	338130.969855	43.447604
3501.641381	338116.391737	43.452609
3501.681314	338114.402098	43.457613
3501.478585	338096.302789	43.462618
3501.881666	338083.982933	43.467623
3501.892717	338082.201241	43.472628
3501.638713	338064.618519	43.477633
3501.696850	338042.791148	43.482637
3501.701100	338037.170686	43.487642
3501.561907	338021.934923	43.492647
3501.880289	338003.728669	43.497652
3501.290070	337993.191553	43.502657
3501.965853	337988.356126	43.507661
3501.704159	337966.095551	43.512666
3501.638544	337956.315578	43.517671
3501.846218	337941.508711	43.522676
3501.713083	337933.341341	43.527681
3501.775262	337914.768226	43.532685
3501.537370	337906.820663	43.537690
3501.487612	337886.256107	43.542695
3501.624204	337861.873415	43.547700
3501.542700	337873.405795	43.552705
3501.924963	337854.757178	43.557709
3501.621832	337829.909191	43.562714
3501.653022	337822.733285	43.567719
3501.676739	337801.724893	43.572724
3501.546195	337787.504860	43.577729
3501.853513	337770.495406	43.582733
3501.527221	337772.784306	43.587738
3501.653303	337752.853352	43.592743
3501.750439	337748.082929	43.597748
3501.645793	337740.495941	43.602753
3501.724310	337712.790955	43.607757
3501.746035	337708.846063	43.612762
3501.675250	337686.733477	43.617767
3501.549603	337681.031549	43.622772
3501.559282	337667.170991	43.627777
3501.610409	337658.491588	43.632781
3501.570230	337655.395546	43.637786
3501.712121	337640.471692	43.642791
3501.772846	337617.829912	43.647796
3501.649528	337610.957845	43.652801
3501.735872	337592.889380	43.657805
3501.577225	337572.087373	43.662810
3501.850432	337570.976703	43.667815
3501.742664	337550.446455	43.672820
3501.714451	337544.347828	43.677825
3501.938292	337525.113497	43.682829
3501.831899	337514.042864	43.687834
3501.719038	337493.233654	43.692839
3501.699908	337484.666913	43.697844
3501.926680	337476.138015	43.702849
3501.822167	337457.819594	43.707853
3501.834128	337449.858298	43.712858
3501.433979	337426.322119	43.717863
3501.752029	337417.499210	43.722868
3501.608439	337414.546463	43.727873
3501.354115	337388.012176	43.732877
3501.409731	337376.458436	43.737882
3501.658922	337364.950719	43.742887
3501.709706	337356.957904	43.747892
3501.592516	337355.272516	43.752897
3501.600470	337328.290303	43.757901
3501.595010	337328.138667	43.762906
3501.844716	337311.239724	43.767911
3501.508142	337290.490802	43.772916
3501.073807	337280.386844	43.777921
3501.205636	337263.786037	43.782925
3501.199901	337277.264862	43.787930
3501.533558	337271.236765	43.792935
3501.597742	337247.780456	43.797940
3501.482661	337244.492649	43.802945
3501.444823	337234.097821	43.807949
3501.291544	337235.698527	43.812954
3501.430341	337219.986658	43.817959
3501.452745	337200.732788	43.822964
3501.442438	337191.961159	43.827969
3501.552145	337184.721992	43.832973
3501.363574	337178.419504	43.837978
3501.240980	337160.510639	43.842983
3501.505510	337154.951069	43.847988
3501.211795	337145.282828	43.852993
3501.456460	337134.106335	43.857997
3501.539322	337138.696296	43.863002
3501.495250	337118.969606	43.868007
3501.749519	337104.282264	43.873012
3501.836060	337096.283801	43.878017
3501.619508	337078.796465	43.883021
3501.664717	337068.871776	43.888026
3501.601747	337059.904908	43.893031
3501.909147	337047.091059	43.898036
3501.539257	337030.187133	43.903041
3501.619729	337018.629394	43.908045
3501.821536	337014.681703	43.913050
3501.599583	336987.938622	43.918055
3501.497546	336978.621821	43.923060
3501.341660	336979.332894	43.928065
3501.782620	336962.759911	43.933069
3501.284524	336951.114592	43.938074
3501.098380	336930.367377	43.943079
3501.516117	336929.717264	43.948084
3501.495216	336938.646593	43.953089
3501.550847	336915.725441	43.958093
3501.309077	336903.327989	43.963098
3501.525410	336892.130422	43.968103
3501.716330	336885.539683	43.973108
3501.754289	336871.801551	43.978113
3501.468957	336848.857371	43.983117
3501.118266	336852.853964	43.988122
3501.151196	336853.535520	43.993127
3501.279036	336845.784847	43.998132
3501.045955	336843.914112	44.003137
3501.436381	336829.866557	44.008141
3501.406069	336815.757624	44.013146
3501.572486	336798.871466	44.018151
3501.560585	336801.136705	44.023156
3501.730449	336798.287483	44.028161
3501.561817	336775.655606	44.033165
3501.558754	336772.451964	44.038170
3501.462252	336767.762546	44.043175
3501.640698	336756.469140	44.048180
3501.547996	336740.691535	44.053185
3501.572574	336717.088496	44.058189
3501.515834	336727.930750	44.063194
3501.445429	336719.880450	44.068199
3501.467807	336688.470642	44.073204
3501.350735	336687.420961	44.078209
3501.601943	336679.727258	44.083213
3501.826628	336671.885117	44.088218
3501.794009	336655.411464	44.093223
3501.814677	336637.886830	44.098228
3501.550432	336621.601956	44.103233
3501.697850	336603.472591	44.108237
3501.548517	336598.053931	44.113242
3501.637800	336598.523238	44.118247
3501.964910	336582.044173	44.123252
3501.759366	336577.422639	44.128257
3501.581136	336547.824199	44.133261
3501.556861	336526.873434	44.138266
3501.476651	336526.224872	44.143271
3501.484096	336517.704610	44.148276
3501.468151	336519.334738	44.153281
3501.593150	336498.080886	44.158285
3501.541420	336484.076895	44.163290
3501.281402	336472.419632	44.168295
3501.411526	336467.949050	44.173300
3501.571794	336449.410713	44.178305
3501.732067	336435.220976	44.183309
3501.758702	336427.562329	44.188314
3501.660470	336420.228368	44.193319
3501.923886	336400.326064	44.198324
3501.689391	336391.691014	44.203329
3501.622872	336365.406357	44.208333
3501.827904	336356.753445	44.213338
3501.425491	336340.362894	44.218343
3502.027978	336336.479641	44.223348
3501.567812	336323.098915	44.228353
3501.485365	336305.997131	44.233357
3501.788550	336303.355903	44.238362
3501.312475	336288.655262	44.243367
3501.344270	336261.083631	44.248372
3501.321593	336265.715632	44.253377
3501.427965	336255.552285	44.258381
3501.256355	336256.316691	44.263386
3501.054392	336240.174493	44.268391
3501.114297	336214.810895	44.273396
3501.514640	336210.577773	44.278401
3501.563150	336216.724488	44.283405
3501.310429	336216.636934	44.288410
3501.034300	336216.273302	44.293415
3501.313236	336196.724491	44.298420
3501.368048	336185.907990	44.303425
3501.202052	336185.908599	44.308429
3501.389901	336174.995004	44.313434
3501.194422	336169.430910	44.318439
3501.642025	336164.859795	44.323444
3500.901743	336151.853398	44.328449
3501.351396	336131.845541	44.333453
3501.554397	336128.126444	44.338458
3501.408158	336123.495581	44.343463
3501.447265	336123.158957	44.348468
3501.264582	336113.803682	44.353473
3501.089718	336091.426662	44.358477
3500.510492	336092.051351	44.363482
3500.681108	336091.185553	44.368487
3501.180453	336087.776152	44.373492
3501.607529	336093.736550	44.378497
3501.284892	336083.487642	44.383501
3501.470440	336095.487448	44.388506
3501.265836	336085.499825	44.393511
3501.510733	336068.626492	44.398516
3501.588581	336055.339570	44.403521
3501.352385	336044.873692	44.408525
3501.606063	336047.936671	44.413530
3501.416973	336033.953983	44.418535
3501.486381	336011.386141	44.423540
3501.198297	336010.515761	44.428545
3501.114796	335999.008766	44.433549
3501.251300	336001.835761	44.438554
3501.150124	335989.924634	44.443559
3501.205058	335992.815243	44.448564
3501.341984	335977.357441	44.453569
3501.289731	335973.118758	44.458573
3501.052774	335955.456058	44.463578
3501.001665	335951.547794	44.468583
3501.097263	335947.235131	44.473588
3500.790540	335945.274138	44.478593
3501.197662	335945.795487	44.483597
3501.401799	335952.884287	44.488602
3501.185177	335954.723829	44.493607
3501.463757	335935.886998	44.498612
3501.167592	335925.888215	44.503617
3501.268386	335912.928255	44.508621
3501.320015	335913.708628	44.513626
3501.231091	335902.583914	44.518631
3501.472553	335901.300142	44.523636
3501.008154	335890.284987	44.528641
3501.239389	335864.106005	44.533645
3501.390065	335869.982498	44.538650
3501.322417	335870.374625	44.543655
3501.415324	335863.595580	44.548660
3501.188900	335867.598282	44.553665
3501.523525	335854.398298	44.558669
3501.296632	335835.793025	44.563674
3501.025002	335831.664915	44.568679
3501.428867	335820.386842	44.573684
3501.366997	335822.303920	44.578689
3501.390894	335825.351980	44.583693
3501.396644	335804.523264	44.588698
3501.168282	335793.216869	44.593703
3501.554381	335778.228646	44.598708
3501.194351	335784.337581	44.603713
3501.319540	335783.631463	44.608717
3501.045027	335780.037847	44.613722
3501.044556	335768.161767	44.618727
3501.304233	335749.632967	44.623732
3500.950976	335750.044316	44.628737
3501.095923	335735.983861	44.633741
3501.178239	335741.667614	44.638746
3501.252601	335737.968589	44.643751
3501.362397	335736.654534	44.648756
3501.251923	335733.747334	44.653761
3501.444113	335727.232483	44.658765
3501.596020	335706.228275	44.663770
3501.287973	335700.808864	44.668775
3501.790911	335694.576027	44.673780
3501.364940	335690.421169	44.678785
3501.455162	335664.594694	44.683789
3501.686925	335662.651224	44.688794
3501.351043	335662.322359	44.693799
3501.276564	335651.958241	44.698804
3501.469010	335627.489033	44.703809
3501.563020	335617.632616	44.708813
3501.459914	335619.174686	44.713818
3500.936325	335622.766114	44.718823
3501.535848	335607.362991	44.723828
3501.247620	335587.597354	44.728833
3501.231639	335565.754658	44.733837
3501.546467	335568.604669	44.738842
3501.080319	335565.447889	44.743847
3501.475610	335561.724104	44.748852
3501.167099	335567.697865	44.753857
3501.754511	335545.125047	44.758861
3501.365926	335543.812608	44.763866
3501.157148	335526.475901	44.768871
3501.334780	335522.913297	44.773876
3501.213097	335525.856986	44.778881
3501.439637	335514.301368	44.783885
3501.240709	335499.938549	44.788890
3501.106315	335490.804446	44.793895
3501.273852	335483.886507	44.798900
3501.099396	335487.728539	44.803905
3501.326959	335484.590454	44.808909
3501.200101	335489.162546	44.813914
3501.373435	335467.163040	44.818919
3501.635604	335458.475553	44.823924
3501.353739	335451.271832	44.828929
3501.416110	335450.626391	44.833933
3501.325820	335450.081110	44.838938
3501.368825	335431.484300	44.843943
3501.648808	335416.817696	44.848948
3501.275020	335420.792622	44.853953
3501.552205	335411.721310	44.858957
3501.214966	335402.771485	44.863962
3501.171412	335387.239927	44.868967
3501.526396	335369.077504	44.873972
3501.176228	335372.031495	44.878977
3501.333506	335368.192314	44.883981
3501.549027	335368.209571	44.888986
3501.340954	335347.719201	44.893991
3501.316238	335334.626073	44.898996
3501.370836	335333.829258	44.904001
3501.152576	335336.330298	44.909005
3501.390364	335318.847385	44.914010
3501.043754	335319.918912	44.919015
3501.648105	335308.812789	44.924020
3501.384855	335296.647034	44.929025
3501.509990	335286.455055	44.934029
3501.505772	335282.946289	44.939034
3501.052957	335278.414111	44.944039
3501.075390	335259.973019	44.949044
3501.098435	335252.518139	44.954049
3501.337661	335250.471756	44.959053
3501.179307	335237.806387	44.964058
3501.029545	335242.839855	44.969063
3501.111783	335230.365751	44.974068
3501.085933	335236.982019	44.979073
3501.259812	335231.334607	44.984077
3501.481680	335236.971189	44.989082
3501.200027	335222.366881	44.994087
3501.324415	335202.333079	44.999092
3501.177923	335204.314282	45.004097
3501.293335	335193.513447	45.009101
3501.398653	335188.944863	45.014106
3501.270240	335195.755192	45.019111
3501.393143	335161.251174	45.024116
3501.046590	335166.569731	45.029121
3501.262193	335155.956672	45.034125
3501.434821	335160.660003	45.039130
3501.111814	335147.664306	45.044135
3501.330115	335149.969951	45.049140
3501.252415	335145.175661	45.054145
3501.288822	335128.436220	45.059149
3501.195404	335121.940482	45.064154
3501.170411	335118.994438	45.069159
3501.088330	335112.496926	45.074164
3501.162783	335112.103904	45.079169
3501.104412	335110.510942	45.084173
3501.077083	335107.005772	45.089178
3501.234133	335107.108465	45.094183
3501.425565	335079.434699	45.099188
3501.199455	335075.833447	45.104193
3501.340993	335071.208323	45.109197
3501.434050	335054.536286	45.114202
3501.306214	335058.447368	45.119207
3501.661958	335050.101196	45.124212
3501.327425	335032.249858	45.129217
3501.479980	335024.774685	45.134221
3501.361812	335018.944016	45.139226
3501.257450	335017.765143	45.144231
3501.401790	334993.582783	45.149236
3501.355643	334989.343032	45.154241
3501.060335	334984.608173	45.159245
3501.416222	334982.950440	45.164250
3501.348396	334977.595092	45.169255
3501.307197	334966.945833	45.174260
3501.111012	334967.154613	45.179265
3501.156892	334940.190149	45.184269
3501.400747	334943.712524	45.189274
3501.128447	334941.796958	45.194279
3501.250032	334929.113150	45.199284
3501.280983	334938.111153	45.204289
3501.405049	334932.674935	45.209293
3501.521089	334918.873004	45.214298
3501.348138	334905.752037	45.219303
3501.072472	334905.337455	45.224308
3501.185213	334905.981138	45.229313
3501.554135	334884.357612	45.234317
3501.408901	334892.543929	45.239322
3501.247600	334874.436548	45.244327
3501.469070	334859.066788	45.249332
3501.411680	334858.999555	45.254337
3501.266113	334858.259454	45.259341
3501.465529	334844.266440	45.264346
3501.651413	334826.816841	45.269351
3501.259521	334813.806365	45.274356
3501.043339	334810.406987	45.279361
3501.222529	334814.193800	45.284365
3501.226618	334815.871734	45.289370
3501.452890	334819.676617	45.294375
3501.355395	334786.452855	45.299380
3501.314400	334775.396603	45.304385
3501.246647	334772.508080	45.309389
3501.552644	334767.730049	45.314394
3501.205888	334764.732555	45.319399
3501.521688	334749.068254	45.324404
3501.087075	334742.142591	45.329409
3501.429936	334732.526781	45.334413
3501.538898	334731.136526	45.339418
3501.451151	334734.227562	45.344423
3501.628466	334716.474072	45.349428
3501.467042	334705.589217	45.354433
3501.351177	334698.639144	45.359437
3501.271902	334694.379107	45.364442
3501.207533	334690.828825	45.369447
3501.406695	334671.240818	45.374452
3501.543528	334661.199429	45.379457
3501.217471	334657.791783	45.384461
3501.454362	334652.566771	45.389466
3501.321411	334651.010880	45.394471
3501.440758	334636.699694	45.399476
3501.216607	334629.181608	45.404481
3501.271600	334618.873254	45.409485
3501.179242	334608.511639	45.414490
3501.442422	334614.370743	45.419495
3501.412001	334604.838690	45.424500
3501.106477	334589.144301	45.429505
3501.222024	334571.095217	45.434509
3501.183464	334571.737128	45.439514
3501.295068	334570.295591	45.444519
3501.496702	334564.948920	45.449524
3501.289912	334565.439109	45.454529
3501.301317	334565.564574	45.459533
3501.063760	334536.024658	45.464538
3501.239758	334531.368648	45.469543
3501.435223	334520.046467	45.474548
3501.175532	334530.412459	45.479553
3501.402899	334529.410594	45.484557
3501.404779	334524.171442	45.489562
3501.101038	334499.677337	45.494567
3501.476283	334481.104405	45.499572
3501.576168	334486.531286	45.504577
3501.375259	334485.723535	45.509581
3501.425036	334476.255207	45.514586
3501.362605	334467.084169	45.519591
3501.526765	334438.142599	45.524596
3501.375501	334442.693204	45.529601
3501.369495	334434.912088	45.534605
3501.637446	334432.098215	45.539610
3501.301641	334413.305799	45.544615
3501.584990	334403.241436	45.549620
3501.924202	334400.925056	45.554625
3501.703882	334386.616013	45.559629
3501.827880	334368.234896	45.564634
3501.708565	334367.312658	45.569639
3501.650637	334340.414853	45.574644
3501.851618	334323.293274	45.579649
3501.648497	334312.084208	45.584653
3501.939056	334296.321936	45.589658
3501.261457	334287.018140	45.594663
3501.784343	334279.256034	45.599668
3501.640850	334265.647028	45.604673
3501.217198	334251.624041	45.609677
3501.597235	334240.908719	45.614682
3501.483138	334236.526913	45.619687
3500.986175	334233.959770	45.624692
3501.246873	334232.571207	45.629697
3501.119887	334219.086763	45.634701
3501.327334	334199.497213	45.639706
3500.941926	334190.961537	45.644711
3501.381073	334185.857432	45.649716
3501.145203	334185.207732	45.654721
3501.105615	334185.290305	45.659725
3501.445807	334184.499681	45.664730
3500.925099	334186.692033	45.669735
3501.448071	334169.163996	45.674740
3500.933271	334161.284343	45.679745
3501.325359	334152.627106	45.684749
3501.325069	334143.878618	45.689754
3501.274758	334155.814199	45.694759
3501.469206	334158.734004	45.699764
3501.168293	334141.665374	45.704769
3501.016399	334118.698635	45.709773
3501.254119	334106.581328	45.714778
3501.056305	334112.665175	45.719783
3501.048349	334116.633909	45.724788
3500.990455	334115.829223	45.729793
3501.145701	334104.716660	45.734797
3501.249193	334102.055634	45.739802
3501.146600	334103.445094	45.744807
3501.028104	334101.759759	45.749812
3501.061514	334097.990678	45.754817
3500.851139	334090.826379	45.759821
3500.885589	334030.038363	45.764826
3501.220347	333939.829141	45.769831
3501.009309	333791.846633	45.774836
3500.943843	333599.512116	45.779841
3500.830188	333351.817462	45.784845
3500.959058	333067.307496	45.789850
3500.398659	332727.688145	45.794855
3500.305472	332336.159756	45.799860
3499.974784	331900.766181	45.804865
3499.611931	331412.851754	45.809869
3499.078387	330874.776101	45.814874
3498.494073	330302.211565	45.819879
3498.151423	329667.513950	45.824884
3497.458186	329002.363722	45.829889
3497.051807	328283.233267	45.834893
3496.761013	327514.318073	45.839898
3495.696601	326702.953030	45.844903
3495.367315	325837.503818	45.849908
3494.532895	324929.811651	45.854913
3493.639896	323965.761942	45.859917
3493.060740	322968.747716	45.864922
3491.905987	321921.326944	45.869927
3491.522455	320823.463650	45.874932
3490.597843	319668.083227	45.879937
3489.935007	318476.605202	45.884941
3488.942517	317222.455601	45.889946
3487.599963	315936.877229	45.894951
3486.594753	314593.120417	45.899956
3485.508343	313212.110850	45.904961
3484.512678	311787.406629	45.909965
3483.307871	310307.549554	45.914970
3482.079467	308780.751180	45.919975
3481.239206	307224.070126	45.924980
3479.731260	305618.175719	45.929985
3478.125420	303955.263906	45.934989
3477.229910	302257.193184	45.939994
3475.842665	300514.655924	45.944999
3474.539458	298723.537617	45.950004
3472.861952	296904.218093	45.955009
3471.185755	295044.852239	45.960013
3469.933879	293128.546093	45.965018
3467.853847	291185.936445	45.970023
3466.347366	289200.918705	45.975028
3464.838892	287177.221127	45.980033
3462.821407	285122.813329	45.985037
3461.149650	283007.341582	45.990042
3459.333979	280875.509503	45.995047
3457.247448	278696.149207	46.000052
3455.478389	276483.450635	46.005057
3453.274666	274244.864128	46.010061
3451.092652	271966.442026	46.015066
3448.882571	269660.566784	46.020071
3446.997874	267317.711593	46.025076
3445.139200	264957.760212	46.030081
3442.761163	262540.030927	46.035085
3440.969326	260102.370022	46.040090
3438.679048	257621.775484	46.045095
3436.254890	255107.461134	46.050100
3433.659099	252580.903266	46.055105
3431.214560	250020.433096	46.060109
3428.846313	247429.528367	46.065114
3426.120037	244820.917401	46.070119
3423.600953	242176.331191	46.075124
3421.183735	239511.172373	46.080129
3418.294082	236808.776373	46.085133
3415.846116	234092.078877	46.090138
3413.110316	231350.705349	46.095143
3409.774191	228582.187874	46.100148
3407.156534	225794.831848	46.105153
3404.126973	222992.206600	46.110157
3401.405621	220158.949025	46.115162
3398.211763	217323.610233	46.120167
3395.194067	214455.073521	46.125172
3392.027812	211574.483982	46.130177
3389.113744	208669.840518	46.135181
3385.748715	205753.229737	46.140186
3382.243882	202824.533115	46.145191
3378.703683	199864.844438	46.150196
3374.852701	196927.490798	46.155201
3371.378117	193972.082391	46.160205
3368.244298	191000.134721	46.165210
3364.514740	188024.508734	46.170215
3360.682754	185039.659270	46.175220
3357.025917	182052.374379	46.180225
3353.204787	179059.378304	46.185229
3349.508890	176067.061949	46.190234
3345.406262	173073.058034	46.195239
3341.403028	170077.421495	46.200244
3336.886444	167086.084933	46.205249
3332.869580	164099.977934	46.210253
3328.301937	161118.175972	46.215258
3322.955593	158167.193914	46.220263
3318.199299	155201.053692	46.225268
3313.131480	152268.659232	46.230273
3307.890782	149361.896401	46.235277
3302.893807	146482.801645	46.240282
3297.013282	143630.254711	46.245287
3290.820693	140782.257738	46.250292
3285.003497	137955.552991	46.255297
3278.418175	135233.089931	46.260301
3271.989689	132541.474586	46.265306
3264.549590	129917.065731	46.270311
3257.431914	127361.605918	46.275316
3250.095153	124847.050015	46.280321
3242.079715	122433.304955	46.285325
3234.367338	120075.857191	46.290330
3226.149030	117814.273151	46.295335
3217.339701	115646.479404	46.300340
3208.738923	113556.901075	46.305345
3199.600669	111565.592724	46.310349
3191.015543	109673.602811	46.315354
3181.489081	107888.664303	46.320359
3172.682821	106201.311321	46.325364
3163.876770	104630.126410	46.330369
3153.945612	103161.313353	46.335373
3145.474246	101797.950800	46.340378
3136.433026	100528.218089	46.345383
3127.900470	99361.011075	46.350388
3120.381858	98284.521976	46.355393
3112.593150	97295.498633	46.360397
3105.820100	96390.008462	46.365402
3098.928179	95554.814574	46.370407
3092.454330	94787.019082	46.375412
3086.073335	94094.063906	46.380417
3079.794437	93450.476849	46.385421
3074.066045	92864.139516	46.390426
3069.208104	92330.093735	46.395431
3064.136833	91824.541209	46.400436
3059.322558	91375.882566	46.405441
3054.878391	90941.391201	46.410445
3050.732319	90534.571854	46.415450
3046.617888	90155.973337	46.420455
3042.915776	89790.516609	46.425460
3039.154987	89443.395303	46.430465
3035.509295	89108.012780	46.435469
3032.335937	88776.994398	46.440474
3028.814272	88467.773109	46.445479
3025.338583	88145.867995	46.450484
3022.335278	87836.864448	46.455489
3018.881065	87528.760474	46.460493
3015.661935	87234.153649	46.465498
3012.377807	86933.105929	46.470503
3009.436726	86634.840780	46.475508
3005.918839	86333.645206	46.480513
3002.547409	86028.377147	46.485517
2999.244806	85729.923689	46.490522
2996.248518	85432.886362	46.495527
2992.924150	85132.079489	46.500532
2989.101503	84814.889507	46.505537
2985.907005	84530.227853	46.510541
2982.856819	84217.039639	46.515546
2979.356818	83928.823897	46.520551
2976.064279	83623.175083	46.525556
2972.365785	83325.253025	46.530561
2969.027172	83034.594742	46.535565
2965.555854	82724.270675	46.540570
2961.765309	82436.941112	46.545575
2958.251162	82136.881295	46.550580
2955.358995	81839.750581	46.555585
2951.240730	81550.093196	46.560589
2947.882406	81256.953846	46.565594
2943.902793	80971.104107	46.570599
2940.178525	80680.695439	46.575604
2936.746192	80397.712813	46.580609
2932.598557	80130.163201	46.585613
2929.316167	79850.947778	46.590618
2925.554900	79588.995149	46.595623
2921.671729	79313.676817	46.600628
2918.281013	79035.883666	46.605633
2915.034351	78772.600840	46.610637
2911.237833	78519.961041	46.615642
2907.753471	78263.781994	46.620647
2904.140308	78005.428241	46.625652
2900.502167	77745.874261	46.630657
2896.785653	77492.824958	46.635661
2893.233294	77245.365901	46.640666
2889.602874	76994.225505	46.645671
2886.184209	76744.718025	46.650676
2882.777308	76504.824937	46.655681
2878.767515	76259.275174	46.660685
2875.726054	76006.629379	46.665690
2871.678866	75768.354212	46.670695
2868.015096	75530.795856	46.675700
2864.922221	75286.571961	46.680705
2861.250933	75060.816749	46.685709
2857.809468	74816.143656	46.690714
2854.528645	74590.090038	46.695719
2850.745055	74337.296548	46.700724
2847.532916	74100.975477	46.705729
2843.803185	73871.937678	46.710733
2840.504560	73636.751730	46.715738
2836.786686	73397.290503	46.720743
2833.239568	73164.026983	46.725748
2829.867557	72934.319065	46.730753
2826.403607	72694.837146	46.735757
2822.912035	72441.203269	46.740762
2819.416136	72223.279374	46.745767
2816.047799	71984.944443	46.750772
2812.864143	71743.141671	46.755777
2809.130963	71505.756977	46.760781
2805.736717	71260.499705	46.765786
2802.523350	71026.314017	46.770791
2798.852170	70773.905140	46.775796
2795.420345	70539.859544	46.780801
2792.216876	70306.186635	46.785805
2788.753359	70057.561329	46.790810
2785.124430	69821.051697	46.795815
2781.358050	69570.288199	46.800820
2778.136469	69324.634839	46.805825
2774.369900	69094.488974	46.810829
2770.990859	68846.909502	46.815834
2767.481693	68601.701566	46.820839
2763.918153	68360.256180	46.825844
2760.345398	68116.516512	46.830849
2757.019576	67880.231131	46.835853
2753.697963	67627.817232	46.840858
2750.298611	67385.936351	46.845863
2746.336980	67154.346592	46.850868
2743.227797	66903.017470	46.855873
2739.757735	66652.648631	46.860877
2736.298924	66404.216510	46.865882
2732.810770	66162.475362	46.870887
2729.259878	65911.713862	46.875892
2725.940774	65669.957309	46.880897
2722.387212	65426.513252	46.885901
2719.251290	65166.871390	46.890906
2715.185840	64925.276772	46.895911
2711.838540	64667.424945	46.900916
2708.367857	64418.506389	46.905921
2704.783419	64171.429692	46.910925
2701.413796	63924.702646	46.915930
2697.824831	63675.638589	46.920935
2694.393393	63425.993849	46.925940
2690.755735	63171.230265	46.930945
2687.112568	62927.614996	46.935949
2683.793990	62661.877647	46.940954
2680.227191	62419.467620	46.945959
2676.808546	62171.750123	46.950964
2673.867378	61917.347394	46.955969
2669.999391	61665.541958	46.960973
2666.379960	61406.459037	46.965978
2662.717902	61158.961109	46.970983
2659.603477	60915.486009	46.975988
2655.937311	60656.481748	46.980993
2652.826971	60410.256786	46.985997
2649.111561	60152.750527	46.991002
2645.503092	59889.855231	46.996007
2642.123813	59634.034301	47.001012
2638.610352	59376.701352	47.006017
2634.953462	59126.818083	47.011021
2631.593820	58867.670607	47.016026
2628.135855	58612.564395	47.021031
2624.681859	58356.584560	47.026036
2620.864116	58102.523553	47.031041
2617.406747	57854.405267	47.036045
2613.668252	57593.160557	47.041050
2610.371946	57346.932248	47.046055
2606.864369	57084.146760	47.051060
2603.574285	56823.094077	47.056065
2600.167709	56566.859334	47.061069
2596.886864	56311.851287	47.066074
2593.524045	56051.649582	47.071079
2589.655803	55799.086516	47.076084
2586.137704	55541.579510	47.081089
2582.721595	55273.324040	47.086093
2579.299927	55009.792897	47.091098
2575.372867	54751.305208	47.096103
2572.395185	54495.241371	47.101108
2569.083726	54224.265937	47.106113
2565.248477	53967.402979	47.111117
2561.882480	53696.829137	47.116122
2558.159688	53443.989278	47.121127
2554.786354	53178.783429	47.126132
2551.742317	52915.901760	47.131137
2547.952254	52661.742245	47.136141
2544.474625	52375.956374	47.141146
2540.425502	52121.729062	47.146151
2537.330332	51849.617986	47.151156
2533.604297	51592.459473	47.156161
2530.128080	51326.041025	47.161165
2526.815968	51059.942517	47.166170
2523.063711	50813.105091	47.171175
2519.601104	50537.184623	47.176180
2515.781187	50266.727903	47.181185
2512.711039	50011.710868	47.186189
2508.806958	49745.872325	47.191194
2505.306853	49482.111310	47.196199
2502.073269	49222.447329	47.201204
2498.961595	48961.549356	47.206209
2495.423361	48695.012423	47.211213
2491.927384	48427.368326	47.216218
2488.138964	48166.109573	47.221223
2484.899134	47896.941069	47.226228
2481.215121	47630.991188	47.231233
2477.767505	47360.808650	47.236237
2474.216646	47090.778672	47.241242
2470.585619	46828.546614	47.246247
2467.622436	46564.836831	47.251252
2463.994957	46288.809512	47.256257
2460.544933	46019.702524	47.261261
2457.150242	45756.710250	47.266266
2453.203101	45484.617835	47.271271
2450.009842	45206.278095	47.276276
2446.478934	44941.572633	47.281281
2443.145831	44671.670771	47.286285
2439.649397	44392.031428	47.291290
2435.785157	44125.250611	47.296295
2432.198209	43854.745146	47.301300
2429.068944	43578.318154	47.306305
2425.841006	43309.843173	47.311309
2422.118276	43038.087922	47.316314
2418.423891	42760.947824	47.321319
2415.119716	42488.766047	47.326324
2411.928214	42210.311309	47.331329
2407.885882	41936.146571	47.336333
2404.853712	41659.240109	47.341338
2401.499197	41379.800480	47.346343
2397.777181	41099.293236	47.351348
2394.424509	40810.336689	47.356353
2390.690132	40545.278135	47.361357
2387.555932	40255.324626	47.366362
2383.414291	39982.645521	47.371367
2380.029597	39701.431367	47.376372
2376.795854	39419.290569	47.381377
2373.460334	39149.634261	47.386381
2370.097864	38857.693537	47.391386
2366.381843	38575.043197	47.396391
2362.519082	38289.509459	47.401396
2359.404944	38010.614380	47.406401
2355.679530	37729.815156	47.411405
2352.550216	37443.778475	47.416410
2349.259058	37163.806271	47.421415
2345.751464	36870.361958	47.426420
2342.116396	36577.125452	47.431425
2338.738450	36294.236675	47.436429
2335.152902	36001.475778	47.441434
2331.663307	35712.412339	47.446439
2327.992124	35424.313087	47.451444
2324.791027	35136.670341	47.456449
2321.184039	34850.457872	47.461453
2317.835810	34557.394492	47.466458
2314.389690	34256.103718	47.471463
2310.932089	33970.095310	47.476468
2307.534250	33663.493610	47.481473
2304.162515	33371.971635	47.486477
2300.584517	33069.273281	47.491482
2297.050242	32766.794294	47.496487
2293.710620	32465.575887	47.501492
2290.656582	32160.970588	47.506497
2286.668812	31866.257423	47.511501
2283.204265	31561.319463	47.516506
2280.091343	31263.017427	47.521511
2276.339926	30956.193825	47.526516
2273.233662	30636.997704	47.531521
2269.274694	30331.749536	47.536525
2266.187194	30029.411538	47.541530
2262.690716	29711.507546	47.546535
2259.296734	29402.337915	47.551540
2255.842846	29083.986992	47.556545
2252.495671	28771.993112	47.561549
2249.001807	28455.419906	47.566554
2245.318566	28143.843036	47.571559
2241.839025	27817.943153	47.576564
2238.773904	27484.284510	47.581569
2235.442333	27170.696748	47.586573
2231.886669	26837.112778	47.591578
2228.381453	26520.159502	47.596583
2224.971607	26186.734487	47.601588
2221.776066	25855.410402	47.606593
2218.068897	25526.877313	47.611597
2214.990608	25189.558174	47.616602
2211.538436	24858.094193	47.621607
2208.078429	24526.396139	47.626612
2204.336327	24175.126057	47.631617
2200.591242	23852.923923	47.636621
2197.431156	23513.003799	47.641626
2193.930918	23156.157547	47.646631
2190.328079	22822.729842	47.651636
2186.945562	22473.676102	47.656641
2183.239470	22139.990916	47.661645
2180.366049	21788.607954	47.666650
2176.212409	21455.511109	47.671655
2172.450415	21112.780510	47.676660
2169.528706	20759.123892	47.681665
2165.828869	20417.928618	47.686669
2162.766415	20066.643884	47.691674
2159.030631	19719.220667	47.696679
2155.651193	19372.907007	47.701684
2152.048523	19021.085779	47.706689
2148.531485	18678.277007	47.711693
2145.059528	18321.646817	47.716698
2141.950911	17980.648559	47.721703
2138.156338	17630.370891	47.726708
2134.725410	17267.831712	47.731713
2130.967831	16920.056483	47.736717
2127.425404	16574.676315	47.741722
2123.847781	16227.075406	47.746727
2119.860941	15874.538547	47.751732
2116.775155	15520.306110	47.756737
2112.953372	15183.442707	47.761741
2109.189165	14828.125969	47.766746
2105.955889	14497.768529	47.771751
2101.977905	14153.801402	47.776756
2098.614786	13806.733252	47.781761
2094.437259	13481.192266	47.786765
2090.881930	13157.766251	47.791770
2086.696023	12835.894444	47.796775
2081.936652	12551.210162	47.801780
2076.430732	12286.772685	47.806785
2071.577572	12041.251006	47.811789
2067.589138	11789.275064	47.816794
2063.241805	11547.552493	47.821799
2058.962747	11327.457090	47.826804
2055.351136	11115.288091	47.831809
2051.268215	10907.510063	47.836813
2047.813761	10709.379869	47.841818
2043.756370	10509.712658	47.846823
2040.406499	10327.300095	47.851828
2037.266930	10127.756099	47.856833
2033.802888	9954.915508	47.861837
2030.515794	9755.044045	47.866842
2027.134870	9571.564304	47.871847
2023.511267	9374.149002	47.876852
2020.115893	9187.351621	47.881857
2016.805685	9007.332489	47.886861
2013.600777	8827.134031	47.891866
2010.097339	8633.078884	47.896871
2006.796884	8446.435545	47.901876
2003.397328	8251.263469	47.906881
1999.679784	8070.807579	47.911885
1996.590119	7883.089263	47.916890
1993.558972	7688.767556	47.921895
1990.136797	7496.018835	47.926900
1986.600671	7293.744117	47.931905
1983.001207	7112.266314	47.936909
1979.606979	6918.503293	47.941914
1976.489040	6729.981418	47.946919
1972.818371	6537.686744	47.951924
1969.222087	6337.368911	47.956929
1965.793604	6138.172694	47.961933
1962.167324	5941.857947	47.966938
1958.509613	5749.268868	47.971943
1954.822251	5560.740529	47.976948
1951.515796	5360.248799	47.981953
1948.009919	5182.348472	47.986957
1944.624207	4978.806741	47.991962
1941.142421	4778.921647	47.996967
1937.932310	4600.328813	48.001972
1934.503533	4403.237064	48.006977
1930.620233	4217.734323	48.011981
1927.342872	4021.287581	48.016986
1924.039846	3829.995574	48.021991
1920.079159	3642.229256	48.026996
1916.864371	3436.905985	48.032001
1912.871637	3245.180650	48.037005
1909.290495	3062.601157	48.042010
1906.477836	2869.094002	48.047015
1902.416991	2686.419350	48.052020
1899.138235	2486.344277	48.057025
1895.272590	2299.782640	48.062029
1892.006072	2111.800236	48.067034
1888.323327	1928.184993	48.072039
1884.677254	1740.990455	48.077044
1881.305116	1562.636552	48.082049
1877.500117	1391.268756	48.087053
1873.564948	1211.835762	48.092058
1870.087509	1026.080921	48.097063
1866.315395	871.962973	48.102068
1862.962189	687.935546	48.107073
1858.878483	537.191369	48.112077
1854.892492	384.465256	48.117082
1850.996414	234.111918	48.122087
1846.589271	102.034914	48.127092
1840.426773	27.896924	48.132097
1831.339189	55.651469	48.137101
1825.091688	61.637545	48.142106
1821.330534	49.406489	48.147111
1818.225665	69.713707	48.152116
1815.615755	57.792877	48.157121
1812.823625	51.984565	48.162125
1810.387806	52.998604	48.167130
1807.366176	52.408521	48.172135
1803.997256	56.969676	48.177140
1800.832104	60.458052	48.182145
1796.913563	71.654302	48.187149
1793.119522	63.968459	48.192154
1790.300669	58.610431	48.197159
1786.995397	62.649095	48.202164
1783.366180	56.354849	48.207169
1779.913402	59.967339	48.212173
1776.796236	55.962652	48.217178
1773.493025	68.410390	48.222183
1770.010564	69.474338	48.227188
1766.968046	51.325259	48.232193
1763.165918	65.230494	48.237197
1759.284554	57.517205	48.242202
1756.048613	65.642154	48.247207
1752.292506	74.345230	48.252212
1749.537838	55.822070	48.257217
1746.261190	60.093550	48.262221
1742.667625	54.796668	48.267226
1739.079080	61.192417	48.272231
1735.170241	67.413666	48.277236
1732.049458	59.454804	48.282241
1728.697131	58.334358	48.287245
1725.093561	59.398292	48.292250
1722.110800	50.101695	48.297255
1718.189503	49.899215	48.302260
1714.764254	51.178857	48.307265
1711.213609	51.446725	48.312269
1707.526362	55.842588	48.317274
1704.232832	57.180714	48.322279
1700.477520	67.895856	48.327284
1697.376153	52.397793	48.332289
1694.018314	53.056278	48.337293
1690.331346	47.134950	48.342298
1687.213299	43.266477	48.347303
1683.318971	53.528802	48.352308
1680.481275	51.258466	48.357313
1676.634207	58.412876	48.362317
1673.123670	56.671794	48.367322
1669.719270	60.947471	48.372327
1666.129739	61.904822	48.377332
1662.642954	60.106242	48.382337
1659.290568	65.674105	48.387341
1655.436113	59.016524	48.392346
1651.732908	57.141086	48.397351
1648.412222	69.642207	48.402356
1645.696940	60.651789	48.407361
1641.925831	61.457230	48.412365
1638.102703	58.018667	48.417370
1634.845175	50.036954	48.422375
1631.537035	52.674547	48.427380
1627.793925	56.310375	48.432385
1623.966631	51.360175	48.437389
1620.532652	51.625634	48.442394
1617.754373	50.159114	48.447399
1613.238624	60.271946	48.452404
1610.074484	53.743628	48.457409
1606.688249	55.295613	48.462413
1603.328659	52.901336	48.467418
1600.032466	54.249403	48.472423
1596.307239	59.540273	48.477428
1592.811190	55.310207	48.482433
1589.511480	58.414736	48.487437
1585.934879	53.577176	48.492442
1582.305598	53.174016	48.497447
1578.352368	53.055682	48.502452
1575.636191	48.567519	48.507457
1572.349046	51.274611	48.512461
1568.720673	56.012485	48.517466
1565.222317	52.583232	48.522471
1561.509613	62.152772	48.527476
1557.874195	57.615498	48.532481
1554.463980	62.641939	48.537485
1551.008072	63.315820	48.542490
1547.239976	54.221301	48.547495
1543.427877	57.282654	48.552500
1540.377081	55.039386	48.557505
1536.887266	55.354742	48.562509
1533.183515	54.517161	48.567514
1530.350175	52.417033	48.572519
1526.746659	56.410701	48.577524
1523.267741	48.346625	48.582529
1519.494761	51.765698	48.587533
1515.952445	54.183712	48.592538
1512.244637	52.286902	48.597543
1508.880266	54.771980	48.602548
1505.788079	53.889306	48.607553
1501.941046	55.836157	48.612557
1498.269553	47.859182	48.617562
1494.838972	50.705809	48.622567
1491.158750	60.441129	48.627572
1487.783927	62.076789	48.632577
1484.829659	60.941576	48.637581
1481.253316	63.551593	48.642586
1478.039455	53.921094	48.647591
1474.008534	53.071470	48.652596
1470.631245	58.045325	48.657601
1466.825322	64.547948	48.662605
1463.450243	62.317497	48.667610
1459.969131	60.359912	48.672615
1456.464928	60.680711	48.677620
1453.299108	54.146387	48.682625
1449.652160	59.241552	48.687629
1445.778352	58.155372	48.692634
1442.759363	53.464708	48.697639
1439.020194	57.818164	48.702644
1435.918538	50.796071	48.707649
1432.195808	50.572111	48.712653
1428.542078	54.450283	48.717658
1425.155670	47.662595	48.722663
1421.029331	56.344618	48.727668
1417.774945	55.443068	48.732673
1414.186719	56.979277	48.737677
1410.917617	61.132611	48.742682
1407.760450	57.687975	48.747687
1404.227791	53.286540	48.752692
1400.437101	52.934023	48.757697
1397.492880	52.781205	48.762701
1393.561535	58.297397	48.767706
1390.226692	52.222995	48.772711
1386.340332	64.689329	48.777716
1383.009779	56.307850	48.782721
1379.669549	48.408788	48.787725
1375.848622	69.755142	48.792730
1372.452320	58.188527	48.797735
1368.994779	56.622760	48.802740
1365.425998	53.337486	48.807745
1362.139163	53.538870	48.812749
1358.369800	55.233167	48.817754
1355.551300	52.020278	48.822759
1351.748309	53.922325	48.827764
1348.189427	59.911745	48.832769
1344.669571	56.555544	48.837773
1340.876401	50.869286	48.842778
1337.658954	48.952732	48.847783
1334.169284	52.011142	48.852788
1330.418272	40.465282	48.857793
1326.496782	49.561361	48.862797
1323.508317	48.599233	48.867802
1320.160975	46.525847	48.872807
1316.701686	43.764462	48.877812
1313.655459	49.069354	48.882817
1309.682479	41.468695	48.887821
1306.115227	47.124073	48.892826
1302.593643	42.211578	48.897831
1299.091553	51.476132	48.902836
1295.423022	47.032737	48.907841
1291.869402	42.742199	48.912845
1287.956125	49.834327	48.917850
1284.898394	43.650149	48.922855
1281.079574	58.292114	48.927860
1278.072220	42.111970	48.932865
1274.849372	44.793267	48.937869
1270.881221	47.164128	48.942874
1267.528827	41.408904	48.947879
1264.087148	49.629452	48.952884
1260.663692	47.821106	48.957889
1257.040448	52.495001	48.962893
1253.199289	56.813866	48.967898
1250.160265	42.717301	48.972903
1246.547344	51.265223	48.977908
1243.347903	40.468297	48.982913
1239.456432	48.066396	48.987917
1235.810287	62.656034	48.992922
1232.876530	48.925811	48.997927
1229.135626	57.987326	49.002932
1225.370591	51.214699	49.007937
1221.859396	51.176004	49.012941
1218.300660	50.644874	49.017946
1215.183932	55.068643	49.022951
1211.467989	63.135994	49.027956
1208.516072	54.537122	49.032961
1204.592252	46.704185	49.037965
1200.996181	47.741817	49.042970
1197.262084	46.089695	49.047975
1193.220730	50.927145	49.052980
1190.450336	48.326879	49.057985
1187.066740	48.160652	49.062989
1183.621343	46.292493	49.067994
1180.004896	51.332349	49.072999
1176.483834	49.760779	49.078004
1173.186345	49.375430	49.083009
1169.409619	46.091151	49.088013
1165.737356	52.949435	49.093018
1162.484363	55.714582	49.098023
1158.711832	53.059244	49.103028
1155.472806	50.526029	49.108033
1152.539814	44.496379	49.113037
1148.407280	47.756736	49.118042
1145.144636	46.682564	49.123047
1140.898911	59.021728	49.128052
1137.922096	44.111870	49.133057
1134.795426	57.968460	49.138061
1130.952877	55.488612	49.143066
1127.479358	37.666751	49.148071
1123.438473	48.667202	49.153076
1120.367895	41.700478	49.158081
1117.231379	45.203546	49.163085
1113.112983	42.314473	49.168090
1110.077986	47.222188	49.173095
1106.212481	47.220024	49.178100
1102.978664	41.557033	49.183105
1099.566260	51.104997	49.188109
1095.816228	50.179916	49.193114
1092.630664	33.641784	49.198119
1089.163854	48.532402	49.203124
1085.093349	47.505639	49.208129
1081.721962	41.531997	49.213133
1078.006357	49.956838	49.218138
1074.778917	41.923186	49.223143
1071.465425	45.855776	49.228148
1068.276298	47.987688	49.233153
1064.835469	34.150275	49.238157
1060.738570	54.160475	49.243162
1057.274114	52.086537	49.248167
1054.082560	50.906353	49.253172
1050.681503	49.322369	49.258177
1046.889611	47.369305	49.263181
1042.918069	52.983663	49.268186
1039.807888	45.422051	49.273191
1036.016666	45.987257	49.278196
1032.465138	57.407837	49.283201
1029.547825	46.003672	49.288205
1025.941597	46.900589	49.293210
1022.753856	36.937165	49.298215
1018.988245	46.350624	49.303220
1015.557269	44.214514	49.308225
1012.076064	43.608047	49.313229
1008.325501	37.538780	49.318234
1004.455927	33.655338	49.323239
1001.092176	47.416190	49.328244
997.596897	42.303546	49.333249
994.535606	46.016337	49.338253
990.986398	46.084919	49.343258
987.426808	46.373429	49.348263
984.026018	49.528772	49.353268
980.161310	45.464240	49.358273
976.894058	39.692638	49.363277
972.908530	48.495135	49.368282
970.039811	35.925450	49.373287
966.361170	46.451613	49.378292
962.692182	42.970218	49.383297
959.350629	37.412738	49.388301
955.184898	45.265849	49.393306
952.060601	46.707434	49.398311
948.849450	45.881534	49.403316
945.214868	46.555128	49.408321
942.027013	43.697601	49.413325
938.328408	43.954112	49.418330
934.582776	48.435305	49.423335
931.392539	51.972151	49.428340
927.994328	44.126650	49.433345
924.209598	41.963708	49.438349
920.481828	50.849251	49.443354
917.259966	47.066907	49.448359
914.110421	44.235029	49.453364
910.493198	44.595868	49.458369
906.947917	42.803566	49.463373
903.137905	47.241066	49.468378
899.287350	44.683477	49.473383
896.091894	53.760927	49.478388
892.486221	45.444885	49.483393
889.511587	46.040472	49.488397
885.968932	44.045286	49.493402
882.383834	41.854265	49.498407
878.386589	41.708306	49.503412
875.217484	39.202211	49.508417
872.012186	38.182432	49.513421
868.602407	44.740279	49.518426
864.878584	47.376763	49.523431
860.921570	49.227183	49.528436
857.679859	55.657478	49.533441
853.878695	43.420508	49.538445
850.475755	43.804763	49.543450
847.657538	43.477358	49.548455
843.615156	45.502505	49.553460
839.773713	41.219257	49.558465
836.598372	41.659627	49.563469
832.985394	50.109605	49.568474
830.012849	47.012757	49.573479
826.606538	50.222801	49.578484
822.926110	49.812118	49.583489
819.448399	47.211997	49.588493
815.480288	43.378869	49.593498
812.259130	42.016743	49.598503
808.438481	45.108176	49.603508
805.005699	39.837128	49.608513
801.529262	42.627887	49.613517
798.050245	36.506702	49.618522
794.736368	31.017724	49.623527
791.108716	37.214238	49.628532
787.612962	44.715722	49.633537
784.414703	46.634017	49.638541
780.578840	47.889690	49.643546
776.986196	39.426130	49.648551
773.312352	40.805132	49.653556
770.261194	41.453869	49.658561
766.299400	47.383179	49.663565
763.018566	41.382833	49.668570
760.058586	48.366988	49.673575
756.254505	49.146292	49.678580
752.625022	46.433923	49.683585
749.407673	46.804971	49.688589
745.571415	42.248869	49.693594
742.102122	46.164834	49.698599
738.490840	46.271706	49.703604
735.046528	40.252680	49.708609
731.925796	41.469148	49.713613
728.086093	48.996041	49.718618
724.632364	40.026694	49.723623
721.180211	40.067524	49.728628
717.628694	47.609401	49.733633
714.355211	42.924052	49.738637
710.308476	39.305768	49.743642
707.017848	43.785389	49.748647
703.343201	48.505487	49.753652
700.090293	46.354266	49.758657
696.770739	41.524279	49.763661
693.180776	43.855125	49.768666
689.546710	33.920615	49.773671
685.922467	39.512351	49.778676
682.392493	34.038278	49.783681
679.329527	43.692983	49.788685
675.198191	44.555208	49.793690
672.405789	41.642177	49.798695
668.811792	42.825216	49.803700
665.112291	44.293700	49.808705
661.746512	34.649382	49.813709
657.816433	49.622148	49.818714
654.684107	32.405172	49.823719
650.892806	39.832759	49.828724
647.164425	43.852607	49.833729
644.402510	44.158692	49.838733
640.310609	37.244539	49.843738
637.356377	38.121750	49.848743
633.123853	43.255110	49.853748
629.541520	44.676784	49.858753
626.400774	41.976512	49.863757
622.542566	35.813548	49.868762
619.522718	47.258537	49.873767
615.920176	44.035804	49.878772
612.559841	44.954478	49.883777
609.047159	40.613519	49.888781
605.272344	47.548159	49.893786
602.126665	45.389672	49.898791
598.485831	49.342044	49.903796
595.037115	53.580706	49.908801
591.608540	46.233655	49.913805
588.004252	46.665359	49.918810
584.855704	43.491759	49.923815
580.948820	43.496293	49.928820
577.204422	39.656713	49.933825
573.801270	42.885329	49.938829
570.247882	51.091939	49.943834
566.768147	39.943737	49.948839
563.533854	40.947092	49.953844
559.906699	44.318365	49.958849
556.543048	46.477776	49.963853
552.772225	43.145384	49.968858
549.345848	43.618842	49.973863
545.903782	38.428452	49.978868
542.128004	47.777219	49.983873
538.915422	49.128361	49.988877
535.331062	42.353067	49.993882
531.938795	49.319567	49.998887
528.893630	48.663972	50.003892
525.105505	42.765324	50.008897
521.599376	38.328463	50.013901
517.283603	44.835331	50.018906
513.873809	37.007647	50.023911
510.955334	42.760988	50.028916
507.551201	53.038655	50.033921
504.235650	44.335667	50.038925
500.676097	42.261024	50.043930
496.948322	41.740830	50.048935
493.154566	39.965466	50.053940
489.250807	41.450192	50.058945
486.369261	42.151551	50.063949
482.748712	46.113442	50.068954
479.621944	30.888857	50.073959
475.847933	31.524360	50.078964
472.607107	41.719504	50.083969
469.223270	38.073436	50.088973
464.742607	53.515317	50.093978
461.663004	36.865980	50.098983
457.994452	41.987009	50.103988
455.050227	41.429525	50.108993
451.577735	32.988430	50.113997
447.718213	41.480308	50.119002
444.644294	35.469832	50.124007
440.744218	45.907453	50.129012
436.860525	34.683384	50.134017
433.939726	34.928998	50.139021
430.385605	32.704839	50.144026
427.279256	33.064940	50.149031
423.404442	39.825480	50.154036
419.681846	36.830445	50.159041
416.405856	29.911996	50.164045
412.651839	39.580097	50.169050
409.401558	36.431991	50.174055
405.795350	35.168292	50.179060
402.065232	40.378079	50.184065
398.392730	34.385452	50.189069
394.664900	34.871386	50.194074
391.711578	35.099961	50.199079
388.595964	36.976969	50.204084
384.760584	34.442543	50.209089
381.408246	41.886889	50.214093
377.800037	36.216395	50.219098
374.072046	32.447105	50.224103
370.510176	33.523986	50.229108
367.329569	42.662522	50.234113
363.913229	34.921354	50.239117
360.228366	42.642421	50.244122
356.684662	41.587251	50.249127
353.104211	39.259679	50.254132
349.724371	44.854380	50.259137
346.359897	37.861233	50.264141
342.632171	38.628747	50.269146
339.236504	37.831970	50.274151
335.761442	29.217327	50.279156
332.027512	37.433306	50.284161
328.792136	38.493862	50.289165
325.325174	36.366824	50.294170
321.660269	37.817369	50.299175
318.421354	38.362790	50.304180
314.828987	40.678337	50.309185
311.491667	38.084906	50.314189
307.746961	43.040749	50.319194
303.711415	45.621877	50.324199
300.191284	38.953691	50.329204
296.955821	44.465682	50.334209
293.722977	39.698207	50.339213
290.162594	41.173521	50.344218
286.454200	38.040279	50.349223
283.425872	37.540321	50.354228
279.581590	41.942296	50.359233
275.968472	43.438532	50.364237
272.773652	42.904547	50.369242
269.552408	39.982901	50.374247
265.771011	43.147493	50.379252
261.752915	45.605683	50.384257
258.548548	44.687220	50.389261
255.220063	48.881854	50.394266
251.719472	41.571549	50.399271
247.984092	38.116684	50.404276
244.579202	47.708008	50.409281
241.103727	46.958572	50.414285
237.410166	44.775319	50.419290
234.512777	41.502395	50.424295
230.920343	36.335698	50.429300
227.327229	46.174813	50.434305
223.621720	39.247800	50.439309
220.093865	33.998226	50.444314
216.561241	36.054515	50.449319
212.824152	32.656883	50.454324
209.553296	40.461840	50.459329
205.960825	31.365777	50.464333
202.658106	37.084485	50.469338
199.005515	34.622748	50.474343
195.594754	41.383442	50.479348
192.414887	39.113406	50.484353
188.853329	38.083248	50.489357
184.736008	50.930977	50.494362
181.307664	42.116091	50.499367
177.805903	43.041263	50.504372
174.624144	42.995651	50.509377
171.173260	40.600402	50.514381
167.628872	43.534913	50.519386
163.817995	35.675312	50.524391
160.390622	41.312323	50.529396
156.939457	37.417505	50.534401
153.751311	33.041720	50.539405
150.151176	43.280591	50.544410
146.430617	40.905455	50.549415
142.964506	32.030071	50.554420
139.179235	35.669883	50.559425
136.236038	31.145000	50.564429
132.569372	40.701436	50.569434
129.045611	38.308131	50.574439
125.268432	35.527424	50.579444
121.802188	44.400733	50.584449
118.603114	36.464286	50.589453
114.803883	34.689949	50.594458
111.478356	34.486550	50.599463
107.824940	36.058769	50.604468
104.474959	39.997393	50.609473
101.281281	29.991016	50.614477
97.482047	34.262619	50.619482
94.159473	37.538893	50.624487
90.536276	33.977940	50.629492
86.791898	43.397873	50.634497
83.517575	33.046633	50.639501
79.792795	38.474004	50.644506
76.102733	40.396826	50.649511
72.969483	35.193061	50.654516
69.591578	34.694164	50.659521
65.771626	37.940808	50.664525
62.029395	38.245640	50.669530
58.931914	35.456548	50.674535
55.728890	26.587445	50.679540
51.666866	38.439459	50.684545
48.465835	31.183559	50.689549
44.710506	40.788718	50.694554
41.601373	39.368199	50.699559
38.020721	38.182909	50.704564
34.381408	38.335587	50.709569
31.268163	29.620106	50.714573
27.630130	34.537195	50.719578
24.275839	31.680786	50.724583
20.276843	39.628361	50.729588
16.851046	34.157245	50.734593
13.418671	35.321547	50.739597
9.733673	39.948610	50.744602
5.953897	42.341099	50.749607
2.978123	35.505503	50.754612