Thu Aug 25 10:16:36 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.530014	103.917963	0.000000
1.433848	108.416111	0.005005
1.579989	107.526381	0.010010
1.635431	105.299937	0.015014
1.462994	101.666525	0.020019
1.380211	99.534506	0.025024
1.272997	79.853809	0.030029
1.255362	79.176402	0.035034
1.203421	86.698490	0.040038
1.129946	69.163871	0.045043
0.917852	64.723596	0.050048
0.248893	52.625868	0.055053
0.323831	45.467259	0.060058
-0.298179	30.090877	0.065062
-0.692616	26.156907	0.070067
-1.001584	16.454701	0.075072
-1.743114	26.331065	0.080077
-1.337862	10.645052	0.085082
-1.707380	15.360011	0.090086
-2.128790	13.322187	0.095091
-2.716892	14.765286	0.100096
-3.211766	9.489812	0.105101
-2.953877	7.674584	0.110106
-2.932565	14.365756	0.115110
-3.344347	13.212271	0.120115
-3.911183	7.691810	0.125120
-4.270547	13.104364	0.130125
-4.006139	-2.822160	0.135130
-4.414724	10.415702	0.140134
-5.077157	12.079254	0.145139
-5.715632	13.603011	0.150144
-6.195440	10.770747	0.155149
-6.062015	15.166461	0.160154
-5.678243	10.503126	0.165158
-6.069876	10.409501	0.170163
-6.111485	12.693950	0.175168
-6.667011	9.633106	0.180173
-6.378431	8.765356	0.185178
-7.030925	7.488236	0.190182
-7.359009	14.616964	0.195187
-7.453302	11.306683	0.200192
-7.819402	18.849492	0.205197
-7.537613	1.142219	0.210202
-8.514132	12.339871	0.215206
-8.649729	3.594432	0.220211
-8.601819	11.284340	0.225216
-8.946742	16.321311	0.230221
-9.812681	2.381548	0.235226
-10.116903	25.632122	0.240230
-9.866269	8.961103	0.245235
-10.034349	7.560629	0.250240
-10.059455	19.684888	0.255245
-10.033140	10.369914	0.260250
-10.951204	23.358583	0.265254
-11.421652	11.258255	0.270259
-11.456219	16.812909	0.275264
-11.678348	15.120347	0.280269
-11.617362	4.797037	0.285274
-11.918875	14.708856	0.290278
-12.105543	22.853136	0.295283
-12.643431	25.253310	0.300288
-13.159474	17.810824	0.305293
-13.163430	14.410459	0.310298
-13.528080	24.860520	0.315302
-13.678668	19.328621	0.320307
-13.399473	13.216859	0.325312
-14.539101	20.380995	0.330317
-14.574814	18.589622	0.335322
-14.871679	15.573672	0.340326
-14.709871	25.096527	0.345331
-14.794866	19.690392	0.350336
-15.325237	20.137359	0.355341
-15.738718	12.368759	0.360346
-16.024922	16.523338	0.365350
-16.151232	8.494611	0.370355
-16.143512	12.375347	0.375360
-16.208322	14.799472	0.380365
-16.693328	10.420955	0.385370
-17.396774	22.436366	0.390374
-17.594214	15.934213	0.395379
-17.250538	13.444321	0.400384
-17.776680	23.011691	0.405389
-18.118842	19.347943	0.410394
-18.861168	28.806819	0.415398
-19.067811	23.577930	0.420403
-19.001155	10.906233	0.425408
-19.140728	19.125389	0.430413
-19.286479	6.069362	0.435418
-19.128087	20.275084	0.440422
-19.723803	17.986163	0.445427
-20.229450	7.783271	0.450432
-20.474462	8.609469	0.455437
-20.582781	10.442463	0.460442
-21.057985	14.971502	0.465446
-20.884594	8.601074	0.470451
-21.245562	10.002258	0.475456
-21.569606	17.880160	0.480461
-21.904018	15.436402	0.485466
-22.294030	16.237862	0.490470
-22.214273	18.702612	0.495475
-22.281911	7.722414	0.500480
-23.062856	14.124835	0.505485
-23.346957	8.313304	0.510490
-23.702963	12.649660	0.515494
-23.944007	9.830608	0.520499
-23.881443	18.192098	0.525504
-23.936622	13.996170	0.530509
-24.223654	12.763029	0.535514
-24.892561	11.232219	0.540518
-25.302400	20.211891	0.545523
-25.173731	6.461137	0.550528
-25.617722	22.270346	0.555533
-25.455885	15.866924	0.560538
-25.642033	19.142125	0.565542
-26.483444	9.203814	0.570547
-26.416828	13.742870	0.575552
-26.841832	6.792325	0.580557
-26.778412	9.585497	0.585562
-26.623904	15.265548	0.590566
-27.192903	13.782359	0.595571
-27.808561	12.015417	0.600576
-28.130751	17.922018	0.605581
-27.950844	12.430088	0.610586
-27.970998	14.223959	0.615590
-28.284995	16.598543	0.620595
-28.770508	16.937243	0.625600
-29.619309	17.522688	0.630605
-29.473124	14.570197	0.635610
-29.696356	13.627615	0.640614
-29.959931	14.333335	0.645619
-30.314445	10.355151	0.650624
-30.677391	14.676777	0.655629
-30.546134	10.521240	0.660634
-31.039976	16.818566	0.665638
-31.005565	12.725660	0.670643
-30.997891	14.341165	0.675648
-31.607924	18.913477	0.680653
-32.072268	11.630574	0.685658
-32.139002	17.911599	0.690662
-32.490524	15.454705	0.695667
-32.267224	11.414460	0.700672
-33.169058	20.642061	0.705677
-33.658975	5.181736	0.710682
-33.514018	12.818472	0.715686
-33.852196	11.738878	0.720691
-33.513071	4.798320	0.725696
-33.717914	16.564761	0.730701
-33.928863	-0.154146	0.735706
-34.706663	14.191928	0.740710
-35.230434	20.611003	0.745715
-34.993086	9.029365	0.750720
-35.591211	7.803840	0.755725
-35.502405	5.866409	0.760730
-36.275232	6.851237	0.765734
-36.802148	15.286105	0.770739
-36.872148	4.970666	0.775744
-36.801939	8.528399	0.780749
-36.686734	5.625056	0.785754
-36.991091	13.806753	0.790758
-36.618207	14.517154	0.795763
-37.236428	16.009266	0.800768
-38.024698	15.338714	0.805773
-38.066347	13.434378	0.810778
-37.995456	12.841179	0.815782
-38.796640	13.586843	0.820787
-39.176188	6.164107	0.825792
-39.636212	16.837912	0.830797
-39.376520	10.463453	0.835802
-39.805116	6.041300	0.840806
-39.857819	13.822900	0.845811
-39.822686	13.852234	0.850816
-40.628246	9.014583	0.855821
-40.885085	12.557122	0.860826
-40.765797	14.120338	0.865830
-41.207627	15.398152	0.870835
-41.126966	15.183071	0.875840
-42.092391	20.383705	0.880845
-42.358993	10.684360	0.885850
-42.362147	13.181081	0.890854
-42.482790	15.914510	0.895859
-42.374564	22.465514	0.900864
-42.549678	18.269395	0.905869
-42.822790	15.167467	0.910874
-43.785038	7.177975	0.915878
-44.181267	10.435471	0.920883
-44.231652	13.581831	0.925888
-44.146936	21.746863	0.930893
-43.988688	14.992829	0.935898
-44.390036	16.495253	0.940902
-44.894979	17.438108	0.945907
-45.115964	8.396003	0.950912
-45.662171	11.768747	0.955917
-45.582602	13.733654	0.960922
-45.814449	16.778734	0.965926
-46.323955	21.072705	0.970931
-46.815772	8.409424	0.975936
-47.039318	20.343311	0.980941
-47.356666	12.774787	0.985946
-47.336719	9.974953	0.990950
-47.319717	11.566851	0.995955
-47.065643	12.125024	1.000960
-47.728272	9.976304	1.005965
-48.545930	15.909918	1.010970
-49.012931	12.310026	1.015974
-49.094255	11.158549	1.020979
-49.160057	7.236370	1.025984
-49.094337	16.334513	1.030989
-48.440933	8.522139	1.035994
-49.148521	8.278707	1.040998
-49.710213	18.443262	1.046003
-50.257572	15.365323	1.051008
-50.282829	6.811404	1.056013
-51.210886	10.614137	1.061018
-51.578593	8.900095	1.066022
-51.685481	17.332425	1.071027
-51.812330	7.215718	1.076032
-51.724249	16.139516	1.081037
-51.823164	15.262877	1.086042
-51.730334	19.399195	1.091046
-51.998350	19.624724	1.096051
-52.545931	15.290815	1.101056
-53.058005	21.970648	1.106061
-52.989286	15.217988	1.111066
-53.029124	12.054201	1.116070
-54.250425	15.127766	1.121075
-54.750116	11.615254	1.126080
-54.791906	18.139142	1.131085
-54.070581	13.653868	1.136090
-54.312781	10.654666	1.141094
-54.286030	17.376620	1.146099
-54.778479	9.231260	1.151104
-55.452864	9.020591	1.156109
-55.603336	7.819838	1.161114
-55.913321	0.117289	1.166118
-56.476841	22.759915	1.171123
-56.840291	14.480445	1.176128
-57.369633	23.380766	1.181133
-57.098796	17.156418	1.186138
-57.111739	12.887435	1.191142
-57.223180	25.290975	1.196147
-57.285747	16.401214	1.201152
-57.726629	22.500420	1.206157
-58.336812	24.114661	1.211162
-58.656573	27.192500	1.216166
-58.860416	23.946841	1.221171
-58.912918	16.131175	1.226176
-59.268802	16.073080	1.231181
-59.422489	14.455217	1.236186
-59.984204	16.375073	1.241190
-60.221894	21.075705	1.246195
-60.435227	17.752441	1.251200
-60.607590	21.152032	1.256205
-60.602955	10.853371	1.261210
-60.780788	19.410713	1.266214
-61.143989	25.428146	1.271219
-61.697215	23.012347	1.276224
-61.987156	20.643881	1.281229
-61.987612	3.610421	1.286234
-62.040212	12.695463	1.291238
-62.185874	20.947210	1.296243
-62.753033	8.498216	1.301248
-63.198917	13.917999	1.306253
-63.487100	4.611181	1.311258
-63.769713	8.578535	1.316262
-63.729563	18.908215	1.321267
-63.983080	15.012283	1.326272
-63.947544	12.083458	1.331277
-64.307258	11.352087	1.336282
-65.143201	12.878314	1.341286
-65.275004	18.258377	1.346291
-65.262983	4.323427	1.351296
-65.535250	8.592878	1.356301
-65.470353	8.832682	1.361306
-65.677907	11.737914	1.366310
-66.565076	15.505769	1.371315
-66.517672	0.619319	1.376320
-67.003408	4.596353	1.381325
-67.095625	9.827842	1.386330
-67.100110	3.206880	1.391334
-67.271344	17.638246	1.396339
-68.044779	0.608849	1.401344
-68.409548	13.855662	1.406349
-68.562736	12.756575	1.411354
-68.385258	7.549764	1.416358
-68.488889	9.271293	1.421363
-68.141697	8.346901	1.426368
-68.849910	11.640627	1.431373
-69.380741	19.304158	1.436378
-69.684580	5.137127	1.441382
-70.152718	7.981949	1.446387
-70.522599	9.406677	1.451392
-71.225946	12.193443	1.456397
-71.263013	10.348501	1.461402
-71.004913	12.639772	1.466406
-71.478270	9.442673	1.471411
-71.302928	0.794053	1.476416
-71.238491	2.163382	1.481421
-71.423371	4.919529	1.486426
-72.118014	0.583359	1.491430
-72.472471	6.286205	1.496435
-72.328809	8.959236	1.501440
-73.283827	18.498890	1.506445
-73.755687	11.033673	1.511450
-73.957970	8.341427	1.516454
-74.396517	6.632159	1.521459
-74.093800	3.841804	1.526464
-74.290666	11.086008	1.531469
-74.355123	14.769245	1.536474
-74.199898	8.661092	1.541478
-74.788678	18.111722	1.546483
-75.112981	6.346012	1.551488
-75.783664	16.217597	1.556493
-75.618658	11.531592	1.561498
-75.502021	7.432132	1.566502
-76.527423	13.012321	1.571507
-76.733471	8.219943	1.576512
-77.089535	5.804893	1.581517
-77.424708	7.005885	1.586522
-77.414696	9.937137	1.591526
-77.433449	10.224849	1.596531
-77.095466	9.058292	1.601536
-77.955719	7.709329	1.606541
-78.430651	2.127021	1.611546
-78.462486	6.096208	1.616550
-79.200334	21.410458	1.621555
-78.654982	2.725427	1.626560
-78.853513	12.026322	1.631565
-79.429405	7.507030	1.636570
-79.962587	14.791278	1.641574
-80.399229	16.153702	1.646579
-80.261747	12.756488	1.651584
-80.737161	8.794088	1.656589
-80.508499	5.480664	1.661594
-80.533724	-0.558083	1.666598
-81.316142	8.195224	1.671603
-81.133568	8.834202	1.676608
-81.764598	9.037519	1.681613
-82.525461	15.803789	1.686618
-82.566467	13.703201	1.691622
-83.124916	17.362602	1.696627
-83.074053	8.828395	1.701632
-83.007927	13.449783	1.706637
-82.968152	8.460701	1.711642
-82.935625	3.621451	1.716646
-83.487822	2.701944	1.721651
-84.180191	13.393169	1.726656
-84.427664	11.808985	1.731661
-84.550864	4.719408	1.736666
-84.666893	2.560975	1.741670
-84.707674	8.148234	1.746675
-85.323056	9.200144	1.751680
-85.837463	10.872144	1.756685
-85.930275	18.166485	1.761690
-85.728910	12.478206	1.766694
-86.194134	3.151676	1.771699
-86.326800	3.004822	1.776704
-87.249569	10.498809	1.781709
-87.448543	9.568247	1.786714
-87.537613	5.314360	1.791718
-87.691959	5.275306	1.796723
-87.320396	-5.916063	1.801728
-87.742863	5.457362	1.806733
-88.467181	0.208360	1.811738
-88.629841	6.735362	1.816742
-88.868444	10.335154	1.821747
-88.795898	4.040642	1.826752
-88.992574	4.511256	1.831757
-89.664136	9.602570	1.836762
-90.424941	3.040006	1.841766
-90.663388	0.549580	1.846771
-90.651129	0.057317	1.851776
-90.873623	3.989940	1.856781
-90.561520	9.354227	1.861786
-90.354971	4.209300	1.866790
-90.837691	13.194059	1.871795
-91.694613	5.093160	1.876800
-92.136656	10.031453	1.881805
-92.374320	14.545418	1.886810
-91.631869	1.141424	1.891814
-92.426878	8.188287	1.896819
-92.768182	-3.989199	1.901824
-93.203555	17.589303	1.906829
-93.191323	4.302889	1.911834
-93.324701	6.446693	1.916838
-93.857817	12.819774	1.921843
-94.243530	9.811423	1.926848
-94.872546	11.425452	1.931853
-94.888959	8.751539	1.936858
-94.746860	7.663131	1.941862
-95.285520	6.073955	1.946867
-95.202138	0.157395	1.951872
-95.072700	6.619645	1.956877
-95.695804	6.907141	1.961882
-96.145490	13.659454	1.966886
-96.482855	9.890558	1.971891
-96.588720	3.905575	1.976896
-96.588762	5.743749	1.981901
-96.782498	9.773106	1.986906
-97.446444	0.113887	1.991910
-97.749496	6.947624	1.996915
-97.624675	4.250970	2.006912
-98.038941	5.744628	2.016909
-97.222408	4.067710	2.026906
-96.961966	10.669825	2.036902
-95.707321	10.289574	2.046899
-95.366140	7.638602	2.056896
-95.591877	6.609670	2.066893
-94.662170	4.576065	2.076890
-94.084936	6.424377	2.086886
-93.427172	9.083695	2.096883
-92.708157	12.525364	2.106880
-92.586951	11.394552	2.116877
-92.416260	15.916825	2.126874
-91.573115	14.663388	2.136870
-91.082498	7.737828	2.146867
-90.801627	11.878540	2.156864
-89.960689	4.974115	2.166861
-89.943170	12.685008	2.176858
-89.007389	13.352575	2.186854
-88.455159	12.499514	2.196851
-88.408270	11.640106	2.206848
-87.317374	8.903337	2.216845
-86.995761	12.400940	2.226842
-86.753015	5.111911	2.236838
-85.866263	10.602198	2.246835
-85.675177	7.151119	2.256832
-85.156561	12.439332	2.266829
-84.156118	14.189655	2.276826
-84.037970	5.247556	2.286822
-83.946519	5.531072	2.296819
-82.820124	7.318680	2.306816
-82.367917	2.429692	2.316813
-82.617609	8.329297	2.326810
-81.996945	3.150987	2.336806
-80.945577	12.217257	2.346803
-80.062151	13.691311	2.356800
-80.006584	11.348018	2.366797
-79.979184	13.450378	2.376794
-79.099134	13.752879	2.386790
-78.683795	7.789451	2.396787
-77.637358	17.962055	2.406784
-77.581274	6.866079	2.416781
-77.090405	11.303337	2.426778
-76.636232	9.584997	2.436774
-76.119554	9.364730	2.446771
-75.826956	13.896411	2.456768
-74.717587	6.731349	2.466765
-74.429266	2.023262	2.476762
-74.519540	2.116676	2.486758
-73.413270	5.453318	2.496755
-72.964278	8.325914	2.506752
-72.460491	13.752667	2.516749
-71.703001	4.513987	2.526746
-71.302574	18.969296	2.536742
-71.377310	12.211513	2.546739
-70.673490	11.474084	2.556736
-70.028510	10.058464	2.566733
-69.696261	4.564218	2.576730
-69.053292	6.747521	2.586726
-68.704287	14.061187	2.596723
-67.796449	9.281369	2.606720
-67.272975	13.742030	2.616717
-67.287265	18.391491	2.626714
-66.526455	17.990421	2.636710
-65.911628	14.083307	2.646707
-65.692195	9.300482	2.656704
-64.761187	9.886437	2.666701
-64.211734	14.083269	2.676698
-64.289684	12.891797	2.686694
-63.607658	18.696102	2.696691
-63.082000	17.739501	2.706688
-62.662335	15.199774	2.716685
-61.943425	17.795664	2.726682
-61.604418	19.183964	2.736678
-61.201711	15.829604	2.746675
-60.525882	11.963618	2.756672
-59.920158	12.790609	2.766669
-59.188450	10.182983	2.776666
-58.632603	9.557438	2.786662
-58.328631	14.553004	2.796659
-58.331567	13.432140	2.806656
-57.843278	8.116182	2.816653
-57.484152	9.596362	2.826650
-56.481424	9.208073	2.836646
-55.954681	6.550200	2.846643
-55.337560	10.559034	2.856640
-54.388871	13.841177	2.866637
-54.401830	10.247839	2.876634
-53.986962	7.477617	2.886630
-53.863660	10.350562	2.896627
-53.188581	7.178440	2.906624
-52.544831	0.190875	2.916621
-51.784255	7.668133	2.926618
-51.322007	6.002381	2.936614
-51.315465	12.945224	2.946611
-50.466865	9.505161	2.956608
-50.010202	8.724097	2.966605
-49.555707	10.135483	2.976602
-48.501043	9.751728	2.986598
-48.398587	11.221441	2.996595
-48.166493	10.320343	3.006592
-47.490423	17.215302	3.016589
-47.206630	14.782395	3.026586
-46.522964	13.997440	3.036582
-45.597280	11.264388	3.046579
-45.234522	6.383080	3.056576
-45.280183	8.148431	3.066573
-44.895819	17.959114	3.076570
-44.104218	14.271391	3.086566
-42.835404	15.194057	3.096563
-42.645287	12.265814	3.106560
-42.295756	12.404357	3.116557
-42.243737	5.382794	3.126554
-41.620749	9.970415	3.136550
-41.091664	13.432345	3.146547
-40.453267	9.512037	3.156544
-39.766536	8.865986	3.166541
-39.457134	12.283143	3.176538
-39.295998	11.136572	3.186534
-38.120639	10.740242	3.196531
-38.016985	-1.113952	3.206528
-37.629660	-2.343480	3.216525
-36.603970	3.451325	3.226522
-36.386706	7.576664	3.236518
-36.304895	3.382438	3.246515
-35.558046	2.197947	3.256512
-35.104954	1.765900	3.266509
-34.364353	6.867281	3.276506
-34.289192	3.320326	3.286502
-33.284185	8.269406	3.296499
-32.773524	5.303611	3.306496
-32.603859	8.771173	3.316493
-31.676873	0.779389	3.326490
-31.119134	7.467974	3.336486
-31.188033	3.373389	3.346483
-30.692127	5.909188	3.356480
-29.840832	5.196172	3.366477
-29.763443	5.561087	3.376474
-28.671449	9.660243	3.386470
-28.161453	5.690363	3.396467
-28.162902	6.526960	3.406464
-27.688974	2.204772	3.416461
-26.899824	4.846678	3.426458
-26.172289	6.547902	3.436454
-25.539358	6.151033	3.446451
-25.076386	6.167265	3.456448
-25.200150	2.417062	3.466445
-24.869943	8.453889	3.476442
-23.786041	2.195642	3.486438
-23.510734	0.932981	3.496435
-22.566956	-2.591682	3.506432
-22.336237	1.465024	3.516429
-22.324816	8.733385	3.526426
-21.399408	1.422923	3.536422
-20.857311	3.637874	3.546419
-20.709409	4.324359	3.556416
-19.554488	-0.221736	3.566413
-19.342399	11.288531	3.576410
-18.916095	5.313882	3.586406
-17.997992	-0.864533	3.596403
-17.713617	5.705328	3.606400
-17.553151	-2.217039	3.616397
-17.328640	1.184909	3.626394
-16.206385	-0.619099	3.636390
-15.980889	3.175500	3.646387
-15.243340	2.733731	3.656384
-14.768304	-2.025785	3.666381
-14.525917	0.163267	3.676378
-14.070519	7.444426	3.686374
-13.308946	6.799322	3.696371
-13.183605	6.504159	3.706368
-12.196271	10.128709	3.716365
-12.204674	3.639298	3.726362
-11.312229	8.301911	3.736358
-10.381150	7.557389	3.746355
-10.672891	2.135568	3.756352
-9.820769	1.020116	3.766349
-8.988826	2.733492	3.776346
-9.021222	3.688979	3.786342
-8.848849	3.069668	3.796339
-7.328839	9.556802	3.806336
-7.433786	6.757153	3.816333
-7.179720	8.985558	3.826330
-6.372616	5.704054	3.836326
-5.908349	2.149985	3.846323
-5.188372	0.893680	3.856320
-4.637528	8.229578	3.866317
-4.595210	8.188176	3.876314
-4.046131	12.834898	3.886310
-3.442896	14.492245	3.896307
-2.978646	12.059575	3.906304
-2.438542	23.727534	3.916301
-2.498598	36.674289	3.926298
-1.986861	56.386580	3.936294
-1.443666	65.526179	3.946291
-0.779069	84.542977	3.956288
-0.234161	95.839598	3.966285
0.149147	113.091682	3.976282
0.000000	117.930409	3.981286
0.656462	125.971109	3.986291
0.513922	132.384276	3.991296
1.028582	146.822184	3.996301
1.070855	155.294487	4.001306
0.979758	168.077760	4.006310
0.895694	164.436816	4.011315
1.233188	156.809917	4.016320
1.224559	162.113779	4.021325
1.285280	167.751627	4.026330
1.560509	178.186943	4.031334
1.265901	175.104171	4.036339
1.753037	182.253933	4.041344
1.336268	180.987322	4.046349
1.963776	180.534699	4.051354
1.786019	171.261105	4.056358
1.413974	160.024784	4.061363
1.316844	166.449832	4.066368
1.297501	168.544150	4.071373
1.738821	170.066416	4.076378
1.855201	171.500388	4.081382
1.588818	170.238689	4.086387
1.760442	158.657758	4.091392
1.398337	160.533695	4.096397
1.455803	167.753936	4.101402
1.328688	172.022831	4.106406
1.929479	184.729348	4.111411
1.666953	183.679016	4.116416
1.753737	193.748396	4.121421
2.123506	186.913698	4.126426
1.855052	174.797427	4.131430
1.605315	165.307323	4.136435
1.874452	160.718858	4.141440
1.628074	174.073797	4.146445
1.430335	166.631995	4.151450
1.802787	188.492271	4.156454
1.757585	185.534937	4.161459
1.752688	177.376377	4.166464
1.661432	182.550821	4.171469
1.844392	189.858977	4.176474
2.014556	190.411323	4.181478
2.146898	189.485786	4.186483
2.010737	174.355860	4.191488
1.706950	178.275948	4.196493
1.588034	170.644623	4.201498
1.640978	180.270042	4.206502
1.968436	190.146686	4.211507
2.142944	192.080920	4.216512
1.807645	192.184112	4.221517
2.217904	181.280789	4.226522
2.291439	186.141511	4.231526
1.982237	178.397627	4.236531
1.972068	171.783816	4.241536
1.398787	163.483363	4.246541
2.087427	178.302162	4.251546
2.244508	188.097932	4.256550
2.461792	180.315850	4.261555
2.031012	171.720981	4.266560
1.971339	172.641533	4.271565
2.196176	166.250332	4.276570
1.910819	168.443277	4.281574
1.830733	169.699223	4.286579
2.082098	183.090077	4.291584
2.155582	194.692806	4.296589
2.244287	187.209279	4.301594
1.919471	189.699476	4.306598
1.699968	190.651399	4.311603
2.185858	184.655890	4.316608
2.279746	193.370062	4.321613
2.132960	183.851163	4.326618
2.065900	190.761892	4.331622
1.944610	192.163501	4.336627
1.811166	191.523217	4.341632
1.830053	198.135744	4.346637
1.863626	182.662840	4.351642
2.089063	206.346358	4.356646
2.019247	218.983963	4.361651
2.393121	220.222570	4.366656
2.223107	220.312520	4.371661
2.330640	210.092530	4.376666
2.877837	219.235567	4.381670
2.489389	223.662479	4.386675
2.643753	214.469705	4.391680
2.262538	206.360602	4.396685
2.233519	196.959286	4.401690
2.275449	205.903070	4.406694
2.727819	209.109900	4.411699
2.318067	208.800812	4.416704
2.019111	213.340250	4.421709
2.243609	216.196804	4.426714
2.915323	219.027581	4.431718
2.655137	226.148919	4.436723
2.848612	218.427499	4.441728
2.498565	204.109349	4.446733
2.187158	196.704326	4.451738
2.554576	212.997182	4.456742
2.544641	212.343874	4.461747
2.727538	217.209616	4.466752
2.527291	220.351021	4.471757
2.451562	214.392876	4.476762
2.619248	220.545496	4.481766
2.191004	223.159471	4.486771
2.654537	219.676329	4.491776
2.472037	225.029598	4.496781
2.808563	222.129508	4.501786
2.622664	229.780213	4.506790
2.590495	227.962954	4.511795
2.780662	222.573755	4.516800
2.629508	222.860069	4.521805
2.681785	219.466673	4.526810
2.275052	221.688133	4.531814
2.203345	226.967095	4.536819
2.486122	220.807244	4.541824
2.054858	225.177589	4.546829
2.209634	228.228568	4.551834
2.476093	234.353062	4.556838
3.016605	236.302722	4.561843
3.267354	231.432380	4.566848
2.794917	242.092446	4.571853
2.824923	240.822270	4.576858
2.669133	244.168686	4.581862
2.774687	243.475135	4.586867
2.665705	242.324812	4.591872
2.623190	241.277971	4.596877
2.901913	243.442657	4.601882
2.882803	249.355632	4.606886
2.713309	242.190950	4.611891
2.844669	240.661282	4.616896
2.886297	239.711990	4.621901
2.884933	240.553806	4.626906
3.139084	240.232446	4.631910
3.039832	244.901956	4.636915
3.134348	253.217423	4.641920
3.107692	247.017459	4.646925
3.094262	255.495374	4.651930
2.957677	251.922753	4.656934
2.815654	241.874724	4.661939
3.058879	252.909890	4.666944
2.957893	252.476492	4.671949
3.074739	253.837631	4.676954
3.004380	248.065297	4.681958
2.865124	247.691680	4.686963
3.072128	243.976641	4.691968
2.927536	250.633784	4.696973
3.097378	246.690447	4.701978
2.961144	253.770228	4.706982
3.024958	261.150866	4.711987
3.278557	255.935218	4.716992
3.106261	256.088802	4.721997
2.912572	261.323610	4.727002
3.164755	276.935384	4.732006
3.023901	273.331790	4.737011
3.154610	281.673237	4.742016
3.130299	283.420330	4.747021
3.322498	271.396336	4.752026
3.619782	275.646216	4.757030
3.538355	275.298340	4.762035
3.774637	277.298835	4.767040
3.582826	269.349855	4.772045
3.386860	263.068844	4.777050
3.133998	256.182976	4.782054
3.282364	249.775253	4.787059
3.224147	250.996140	4.792064
3.465464	260.063736	4.797069
3.209022	253.697290	4.802074
3.387719	268.248047	4.807078
3.433690	272.967578	4.812083
3.679484	265.367655	4.817088
3.204310	265.647789	4.822093
3.086781	265.739007	4.827098
3.678135	272.049893	4.832102
3.299159	280.025103	4.837107
3.483803	266.616557	4.842112
3.525180	280.094169	4.847117
3.743294	274.725886	4.852122
3.397855	281.822638	4.857126
3.275453	279.877140	4.862131
3.614486	275.606729	4.867136
3.580718	277.845690	4.872141
3.538998	279.279132	4.877146
3.656762	276.875222	4.882150
3.679255	273.707948	4.887155
3.639602	270.148610	4.892160
3.402543	282.429646	4.897165
3.408652	282.036416	4.902170
3.445495	273.089817	4.907174
3.375988	288.536866	4.912179
3.689313	277.626525	4.917184
3.653102	281.324376	4.922189
3.931944	276.826111	4.927194
3.763297	279.747437	4.932198
3.560471	281.617413	4.937203
3.857543	275.151580	4.942208
3.750093	279.933116	4.947213
3.686989	277.430993	4.952218
3.748551	291.243977	4.957222
3.714130	278.078555	4.962227
3.755260	276.411159	4.967232
3.709930	277.993864	4.972237
4.020244	277.821893	4.977242
3.889781	284.283844	4.982246
3.853658	284.805238	4.987251
4.134026	278.756477	4.992256
4.072527	278.614288	4.997261
3.993030	283.404100	5.002266
4.065519	279.646854	5.007270
3.792208	285.593342	5.012275
3.682041	276.527405	5.017280
3.880781	283.557877	5.022285
4.089411	277.877865	5.027290
4.207229	284.152216	5.032294
3.620043	284.582779	5.037299
4.077101	283.989179	5.042304
4.017849	291.778257	5.047309
3.779010	284.051777	5.052314
3.776216	284.539475	5.057318
3.659273	287.313494	5.062323
4.046742	280.222885	5.067328
3.650703	290.614743	5.072333
3.969464	308.895843	5.077338
3.965063	307.672182	5.082342
4.071079	305.627617	5.087347
4.280744	301.734977	5.092352
3.957894	318.066478	5.097357
4.439094	307.753084	5.102362
4.008396	304.982681	5.107366
3.961197	309.659871	5.112371
4.210843	302.499096	5.117376
3.739129	312.137187	5.122381
3.929294	315.967257	5.127386
3.896461	310.549696	5.132390
3.894794	311.356761	5.137395
4.125724	312.064107	5.142400
3.981985	312.513777	5.147405
4.215254	316.900250	5.152410
4.374128	335.323488	5.157414
4.325619	338.763846	5.162419
4.702957	334.797471	5.167424
4.209951	319.321531	5.172429
4.119502	317.949997	5.177434
4.211612	325.724866	5.182438
3.977696	327.432037	5.187443
4.275600	330.656764	5.192448
4.496357	334.143519	5.197453
4.470302	330.597858	5.202458
4.365207	331.525534	5.207462
3.954419	333.924816	5.212467
4.261967	338.856484	5.217472
4.060821	328.580385	5.222477
4.179918	335.082347	5.227482
4.328141	333.888555	5.232486
4.427745	339.099580	5.237491
4.856593	332.160657	5.242496
4.664620	326.034024	5.247501
4.990096	337.315786	5.252506
4.819192	332.967068	5.257510
4.788856	335.411146	5.262515
5.033083	330.519652	5.267520
4.931273	333.876611	5.272525
4.472441	325.029795	5.277530
4.546218	319.769536	5.282534
4.336292	324.269743	5.287539
4.652427	323.381842	5.292544
4.445042	342.507888	5.297549
4.636447	332.290506	5.302554
4.478080	329.433137	5.307558
4.255437	333.660089	5.312563
4.221198	330.840219	5.317568
4.418557	337.206532	5.322573
4.500334	329.227315	5.327578
4.327799	334.569564	5.332582
4.342816	337.354553	5.337587
4.766858	353.309631	5.342592
5.004293	359.432388	5.347597
5.138498	364.210885	5.352602
4.845609	341.398352	5.357606
4.614068	342.424936	5.362611
4.785201	332.903602	5.367616
4.653410	345.449765	5.372621
5.096133	349.537669	5.377626
5.053045	347.706289	5.382630
4.875879	336.600677	5.387635
4.694464	341.491896	5.392640
4.595058	338.755003	5.397645
5.034079	353.246059	5.402650
5.144700	349.919429	5.407654
4.661494	343.547351	5.412659
4.650080	351.850987	5.417664
4.925885	368.212123	5.422669
4.967691	360.052491	5.427674
5.307818	353.171753	5.432678
4.863583	363.333920	5.437683
5.306579	353.807945	5.442688
5.107253	363.884283	5.447693
4.727464	350.342643	5.452698
5.114238	358.140961	5.457702
5.230905	359.005420	5.462707
5.274838	348.520065	5.467712
4.922529	342.143297	5.472717
4.803430	348.157394	5.477722
4.841641	346.759373	5.482726
4.946664	359.129234	5.487731
5.211587	355.693004	5.492736
5.205437	355.396607	5.497741
5.186968	366.669001	5.502746
5.135625	354.569212	5.507750
5.029152	362.751703	5.512755
5.182130	357.621395	5.517760
5.317540	356.347350	5.522765
5.366088	357.627448	5.527770
5.432118	359.933042	5.532774
5.339790	361.678145	5.537779
5.699640	361.412989	5.542784
5.049156	340.181439	5.547789
5.060705	345.191124	5.552794
5.170289	358.721385	5.557798
4.901096	361.354752	5.562803
5.049051	358.556953	5.567808
5.083051	370.080560	5.572813
5.039137	363.475129	5.577818
5.718746	362.960554	5.582822
4.916455	351.845308	5.587827
5.198252	351.725261	5.592832
4.705537	357.943435	5.597837
4.673746	362.010774	5.602842
5.178721	376.561119	5.607846
5.110705	383.668229	5.612851
5.394788	385.616953	5.617856
5.306171	390.863812	5.622861
5.706568	393.914301	5.627866
5.842582	386.935815	5.632870
5.377905	395.772404	5.637875
5.784411	390.032879	5.642880
5.474684	393.824228	5.647885
5.484585	382.205215	5.652890
5.506768	383.299617	5.657894
5.728802	380.594613	5.662899
5.853559	381.989324	5.667904
5.683382	384.540742	5.672909
5.671012	390.256552	5.677914
5.925407	385.170458	5.682918
5.655546	380.356335	5.687923
5.313510	367.571243	5.692928
5.516649	393.656668	5.697933
5.542905	393.889876	5.702938
5.985309	389.191947	5.707942
5.495195	397.703487	5.712947
5.810195	382.379308	5.717952
5.698620	381.270512	5.722957
5.711757	387.602430	5.727962
6.045666	391.232822	5.732966
5.500812	391.182183	5.737971
5.600305	388.047117	5.742976
5.504155	393.149621	5.747981
5.760811	386.968495	5.752986
5.938563	391.205494	5.757990
5.631942	388.570664	5.762995
5.932456	385.508508	5.768000
5.846297	384.769059	5.773005
5.627802	381.981214	5.778010
5.735257	383.489370	5.783014
5.645203	386.898281	5.788019
5.544699	382.285416	5.793024
5.925710	386.617119	5.798029
5.872171	390.048784	5.803034
6.001690	391.347835	5.808038
5.810870	389.337114	5.813043
5.782388	387.430674	5.818048
5.723276	393.011437	5.823053
5.596327	394.584794	5.828058
5.723003	376.717951	5.833062
5.803769	400.326317	5.838067
6.289587	401.136102	5.843072
6.304226	402.965691	5.848077
6.081880	394.167211	5.853082
5.873329	392.700279	5.858086
5.884163	395.498588	5.863091
5.908687	400.050667	5.868096
6.159281	413.922715	5.873101
6.518426	414.214500	5.878106
6.439553	396.974639	5.883110
6.119945	394.604439	5.888115
5.983129	383.777217	5.893120
5.922712	388.538758	5.898125
5.894455	386.610136	5.903130
6.150682	398.855093	5.908134
6.113238	409.516708	5.913139
6.033018	410.181059	5.918144
6.235710	417.024300	5.923149
6.528960	417.566859	5.928154
6.461322	409.348420	5.933158
6.066048	406.632563	5.938163
6.016892	396.800855	5.943168
6.026526	407.780965	5.948173
6.081204	409.654902	5.953178
6.164137	406.864120	5.958182
6.080368	420.196927	5.963187
6.147978	425.128247	5.968192
5.934745	422.526237	5.973197
6.135490	418.483107	5.978202
6.249951	419.047351	5.983206
5.949111	420.916880	5.988211
5.979780	424.319538	5.993216
6.404109	428.138254	5.998221
6.376111	431.904453	6.003226
6.585869	417.545878	6.008230
6.572053	426.368790	6.013235
6.467618	412.692210	6.018240
6.379068	418.233300	6.023245
6.159964	416.021359	6.028250
6.459092	413.161900	6.033254
6.303041	418.738877	6.038259
6.267989	419.687222	6.043264
6.260367	421.906286	6.048269
6.551177	409.762342	6.053274
6.363535	409.108396	6.058278
6.208583	416.558176	6.063283
6.368709	406.772767	6.068288
6.167023	414.498792	6.073293
6.159758	411.503838	6.078298
6.547713	412.876296	6.083302
6.314651	422.081577	6.088307
6.230176	413.688600	6.093312
6.453046	417.668595	6.098317
6.423944	420.213733	6.103322
6.225601	415.682629	6.108326
6.265214	416.837579	6.113331
6.523686	413.452969	6.118336
6.480493	424.473005	6.123341
6.270369	419.080024	6.128346
6.154680	419.129826	6.133350
6.169213	417.741836	6.138355
6.361741	429.060305	6.143360
6.736961	428.909802	6.148365
6.345826	428.841406	6.153370
6.502610	417.170882	6.158374
6.103782	424.775936	6.163379
6.269597	422.465720	6.168384
6.218630	423.967063	6.173389
6.199152	419.904652	6.178394
6.294372	429.814652	6.183398
6.284081	433.729940	6.188403
6.377972	437.730148	6.193408
6.398889	444.139963	6.198413
6.481411	443.456341	6.203418
6.246129	426.895867	6.208422
6.246972	435.536150	6.213427
6.597526	432.444000	6.218432
6.464535	424.248448	6.223437
6.184626	419.818710	6.228442
6.162662	414.943590	6.233446
6.423148	434.955064	6.238451
6.157990	434.870093	6.243456
6.073749	430.722912	6.248461
6.561047	434.145778	6.253466
6.645103	436.391609	6.258470
6.473273	433.893844	6.263475
6.447696	418.249666	6.268480
6.062517	417.408366	6.273485
6.203381	427.295395	6.278490
6.325203	434.989725	6.283494
6.445634	430.041669	6.288499
6.353975	433.017397	6.293504
6.419819	435.054106	6.298509
6.285381	438.109306	6.303514
6.278325	428.055845	6.308518
6.311520	444.401279	6.313523
6.606664	441.156454	6.318528
6.439197	426.290652	6.323533
6.214572	427.192769	6.328538
6.220028	423.177071	6.333542
6.541541	440.034159	6.338547
6.307191	421.610056	6.343552
6.397909	421.886950	6.348557
6.179367	432.260572	6.353562
6.362053	423.629575	6.358566
6.431346	446.189413	6.363571
6.373701	439.408931	6.368576
6.358624	419.903252	6.373581
6.312173	414.301128	6.378586
6.375118	416.135805	6.383590
5.920747	427.068402	6.388595
6.537193	429.275111	6.393600
6.484168	434.035505	6.398605
6.507124	438.511908	6.403610
6.786092	426.056591	6.408614
6.342310	417.523752	6.413619
6.262578	410.999847	6.418624
6.365674	420.155621	6.423629
6.323620	424.825707	6.428634
6.635794	412.371525	6.433638
6.286031	412.467492	6.438643
6.353805	411.713414	6.443648
6.410958	413.137703	6.448653
6.457380	416.955515	6.453658
6.145800	417.165725	6.458662
6.403135	415.628959	6.463667
6.441993	417.435772	6.468672
6.393334	420.319338	6.473677
6.150679	418.291425	6.478682
6.210173	416.959667	6.483686
6.396077	411.105999	6.488691
6.523373	413.851263	6.493696
6.567081	414.527835	6.498701
6.182490	420.222879	6.503706
6.589144	414.619366	6.508710
6.295242	414.393364	6.513715
6.356906	417.291282	6.518720
6.394801	421.025008	6.523725
6.450458	423.297434	6.528730
6.475206	411.764662	6.533734
6.276058	415.269766	6.538739
6.284485	416.454912	6.543744
6.139615	423.020411	6.548749
6.328479	426.028118	6.553754
6.626436	413.300910	6.558758
6.449375	422.548038	6.563763
6.324182	409.042395	6.568768
6.230430	412.347484	6.573773
6.271357	414.729786	6.578778
6.498443	419.702558	6.583782
6.590968	424.506585	6.588787
6.410376	426.034564	6.593792
6.315812	418.753665	6.598797
6.347177	416.265195	6.603802
6.416544	413.827720	6.608806
6.324659	425.181257	6.613811
6.470257	416.388393	6.618816
6.650265	424.253939	6.623821
6.161313	422.511392	6.628826
6.406307	419.518042	6.633830
6.506232	419.375870	6.638835
6.565402	420.834646	6.643840
6.386951	419.796437	6.648845
6.546054	414.200073	6.653850
6.427062	410.997994	6.658854
6.398858	421.604383	6.663859
6.200805	405.139339	6.668864
6.491156	395.839742	6.673869
6.204093	415.573146	6.678874
6.515249	410.509790	6.683878
6.502110	407.480954	6.688883
6.538776	398.888667	6.693888
6.575418	397.630095	6.698893
5.979260	394.566057	6.703898
6.009978	398.943156	6.708902
6.061673	415.136965	6.713907
6.271013	414.041162	6.718912
6.546697	415.652679	6.723917
6.540207	414.964021	6.728922
6.440090	414.932287	6.733926
6.169710	404.511965	6.738931
6.334202	409.776120	6.743936
6.452791	413.867368	6.748941
6.225591	418.205786	6.753946
6.544536	409.132661	6.758950
6.554362	404.091208	6.763955
6.217687	398.363716	6.768960
6.198452	397.243614	6.773965
6.152538	410.061110	6.778970
6.509385	406.809788	6.783974
6.102866	414.156611	6.788979
6.382754	408.645730	6.793984
6.862663	413.566232	6.798989
6.272754	403.572468	6.803994
6.040031	392.820380	6.808998
6.283720	408.933482	6.814003
6.755096	407.138550	6.819008
6.472265	402.551083	6.824013
6.298229	398.038322	6.829018
6.538276	394.014350	6.834022
6.531328	392.528486	6.839027
6.081618	384.496474	6.844032
6.223881	387.087525	6.849037
6.317151	401.110764	6.854042
6.521873	388.470950	6.859046
6.550939	397.866106	6.864051
6.499266	388.566316	6.869056
6.338969	389.138807	6.874061
6.241365	392.650144	6.879066
6.636240	385.539350	6.884070
6.030815	398.007896	6.889075
6.205451	386.625665	6.894080
6.534561	391.500185	6.899085
6.153769	390.028602	6.904090
6.246275	387.157227	6.909094
6.276342	386.193919	6.914099
6.045815	399.328239	6.919104
6.145956	392.326897	6.924109
6.308824	412.192286	6.929114
6.810589	408.320297	6.934118
6.233423	407.547044	6.939123
6.201220	401.297275	6.944128
5.964165	398.996399	6.949133
5.932916	413.763670	6.954138
6.033185	417.430673	6.959142
6.289816	417.729029	6.964147
6.800655	419.060088	6.969152
6.549685	430.232907	6.974157
6.382226	426.491078	6.979162
6.962056	420.737042	6.984166
6.319149	407.907311	6.989171
6.117432	404.126562	6.994176
6.466082	402.698879	6.999181
6.070203	403.763870	7.004186
6.405158	407.875000	7.009190
6.497095	408.284583	7.014195
6.433537	406.475387	7.019200
6.493221	394.266425	7.024205
6.438465	403.987934	7.029210
6.375403	389.403203	7.034214
6.218092	393.857218	7.039219
6.084852	392.802437	7.044224
6.380024	394.856995	7.049229
6.351476	414.505600	7.054234
6.460211	406.813195	7.059238
6.418197	404.117921	7.064243
6.233510	408.266175	7.069248
6.305092	397.327198	7.074253
6.155403	402.820915	7.079258
6.472700	407.111985	7.084262
6.500562	419.557254	7.089267
6.234695	410.180280	7.094272
6.237855	413.758092	7.099277
6.380889	417.162126	7.104282
6.603944	411.774046	7.109286
6.630028	414.063759	7.114291
6.284391	401.193785	7.119296
6.300270	394.544172	7.124301
6.035751	399.609781	7.129306
6.082471	394.261989	7.134310
6.410940	406.846816	7.139315
6.345262	420.202100	7.144320
6.157165	418.317501	7.149325
6.074008	415.644491	7.154330
6.314963	412.373359	7.159334
6.245728	422.347088	7.164339
6.216892	416.220175	7.169344
6.110323	415.594655	7.174349
6.349746	419.673299	7.179354
6.442193	420.990816	7.184358
6.466090	423.157485	7.189363
6.101847	418.149327	7.194368
6.318760	413.262091	7.199373
6.183308	418.130310	7.204378
6.486606	411.002216	7.209382
6.127320	422.647589	7.214387
6.433248	423.754485	7.219392
6.158623	417.754668	7.224397
5.986702	415.010142	7.229402
6.250386	406.986570	7.234406
6.337688	417.736214	7.239411
6.241407	418.387262	7.244416
6.475030	421.213946	7.249421
6.698439	424.757251	7.254426
6.364657	422.455708	7.259430
6.396834	420.485976	7.264435
6.603443	424.424227	7.269440
6.502170	416.635005	7.274445
6.516874	421.761278	7.279450
6.739245	411.741483	7.284454
6.671603	415.099431	7.289459
6.528522	421.943065	7.294464
6.407862	411.581540	7.299469
6.244907	417.469651	7.304474
6.319527	406.881376	7.309478
5.960396	418.216669	7.314483
6.228826	414.197736	7.319488
6.254654	423.425731	7.324493
6.248468	422.129574	7.329498
6.571961	413.603073	7.334502
6.521197	411.054704	7.339507
6.596316	412.324315	7.344512
6.484988	424.857836	7.349517
6.322441	418.362723	7.354522
6.188240	419.870778	7.359526
6.315234	429.861223	7.364531
6.543472	419.248872	7.369536
6.458734	422.093798	7.374541
6.359631	411.678274	7.379546
6.272202	405.981331	7.384550
6.335582	417.658556	7.389555
6.212385	417.298238	7.394560
6.428793	417.704138	7.399565
6.511648	412.926492	7.404570
6.175570	402.791716	7.409574
6.293691	407.819523	7.414579
6.305963	417.166699	7.419584
6.425471	415.993220	7.424589
6.351021	414.328102	7.429594
5.957662	419.138652	7.434598
6.159017	432.297080	7.439603
6.112889	417.478714	7.444608
6.490938	420.880729	7.449613
6.239065	416.936990	7.454618
6.302846	416.243650	7.459622
6.156452	428.428321	7.464627
6.191612	418.779546	7.469632
6.662635	409.976827	7.474637
6.204440	427.914703	7.479642
6.193110	422.123572	7.484646
6.320833	433.654682	7.489651
6.202871	433.964272	7.494656
6.298896	430.912002	7.499661
6.560858	422.047118	7.504666
6.393810	421.339324	7.509670
6.251808	426.240210	7.514675
6.191634	424.088790	7.519680
6.346452	417.850842	7.524685
6.348861	421.859052	7.529690
6.506564	422.704428	7.534694
6.274481	417.526865	7.539699
6.578809	415.194947	7.544704
6.613910	423.443871	7.549709
6.513347	423.662148	7.554714
6.428025	420.391516	7.559718
6.356255	426.221050	7.564723
6.356409	421.029245	7.569728
6.820340	412.271930	7.574733
6.721099	419.700327	7.579738
6.523001	405.465777	7.584742
6.161920	399.919281	7.589747
6.068452	398.801319	7.594752
6.471276	402.142500	7.599757
6.041979	408.344427	7.604762
6.567328	417.715620	7.609766
6.509288	411.295886	7.614771
6.218822	406.342612	7.619776
6.412096	395.818012	7.624781
6.215370	404.334207	7.629786
6.274102	397.886690	7.634790
6.427342	411.084279	7.639795
6.369735	406.369772	7.644800
6.315233	399.088932	7.649805
6.163285	410.170291	7.654810
6.583572	407.934103	7.659814
6.327829	407.015576	7.664819
6.431912	400.273045	7.669824
6.501445	391.931880	7.674829
6.006309	403.415025	7.679834
6.389772	407.556521	7.684838
6.514139	399.020096	7.689843
6.183448	401.463786	7.694848
6.410987	407.458393	7.699853
6.043712	413.014678	7.704858
6.175923	419.641169	7.709862
6.189275	421.901240	7.714867
6.174561	419.236488	7.719872
6.594235	420.154716	7.724877
6.227497	422.923602	7.729882
6.743070	420.783216	7.734886
6.514570	426.434823	7.739891
6.038821	427.208603	7.744896
6.370288	418.585936	7.749901
6.504953	422.231733	7.754906
6.398131	414.187113	7.759910
6.279540	416.398252	7.764915
6.041259	415.046709	7.769920
5.972561	412.377762	7.774925
6.210682	415.845993	7.779930
6.484866	418.315137	7.784934
6.306630	414.274438	7.789939
6.143024	415.894670	7.794944
6.192148	416.023054	7.799949
5.858644	422.592798	7.804954
6.552516	420.123915	7.809958
6.350928	424.439339	7.814963
6.480873	425.529515	7.819968
6.259866	422.621833	7.824973
6.446873	433.627953	7.829978
6.174409	426.947574	7.834982
6.486772	419.042922	7.839987
6.377031	419.620147	7.844992
6.409090	412.531387	7.849997
6.104404	425.949433	7.855002
6.282640	418.505566	7.860006
6.268047	417.099993	7.865011
6.500742	418.566382	7.870016
6.343744	420.467159	7.875021
6.424102	418.755638	7.880026
6.365910	416.496339	7.885030
6.496848	409.385759	7.890035
6.247792	417.802591	7.895040
6.502162	415.981547	7.900045
6.126552	422.355404	7.905050
6.464612	411.472745	7.910054
6.596050	411.075695	7.915059
6.116127	420.838518	7.920064
6.449438	405.957548	7.925069
6.726230	414.994354	7.930074
6.472964	419.618436	7.935078
6.028449	420.694212	7.940083
6.232719	418.811414	7.945088
6.484947	422.989294	7.950093
6.185991	421.732680	7.955098
6.678334	425.347747	7.960102
6.669230	414.035417	7.965107
6.486003	409.691775	7.970112
6.694396	416.916944	7.975117
6.490213	425.136919	7.980122
6.447286	404.681924	7.985139
6.442752	395.632014	7.990157
6.004096	394.949715	7.995174
6.368636	392.450095	8.000192
6.312768	416.833813	8.005210
6.536286	414.312105	8.010227
6.456977	403.733906	8.015245
6.401884	396.437041	8.020262
6.596792	394.935966	8.025280
6.354197	393.604423	8.030298
6.516546	394.825540	8.035315
6.416427	394.027083	8.040333
6.511966	390.398833	8.045350
6.635082	387.387942	8.050368
5.982914	397.039420	8.055386
6.438230	392.698406	8.060403
6.540783	384.442748	8.065421
6.057596	391.407462	8.070438
6.313065	391.225464	8.075456
6.439953	415.287062	8.080474
6.356745	423.407236	8.085491
6.316082	421.012124	8.090509
6.663743	422.355683	8.095526
6.550144	413.474329	8.100544
6.627718	425.902145	8.105562
6.729215	399.030929	8.110579
6.703611	397.289855	8.115597
6.125347	394.824347	8.120614
6.496869	386.693800	8.125632
6.386103	395.865984	8.130650
6.064936	391.842284	8.135667
6.637393	404.088408	8.140685
6.441853	414.637163	8.145702
6.737188	413.574778	8.150720
6.458362	418.247973	8.155738
6.574564	428.637442	8.160755
6.760476	416.282022	8.165773
6.431952	413.509144	8.170790
6.697528	403.583794	8.175808
6.267461	409.441995	8.180826
6.457580	418.800573	8.185843
6.648517	419.471268	8.190861
6.405064	428.831513	8.195878
6.506996	419.894295	8.200896
6.592768	420.628804	8.205914
6.363100	421.223392	8.210931
6.545424	419.888385	8.215949
6.718555	425.614214	8.220966
6.407473	424.069341	8.225984
6.358583	422.530725	8.231002
6.355267	431.130680	8.236019
6.838218	424.942374	8.241037
6.452003	421.304394	8.246054
6.198570	419.854628	8.251072
6.159964	429.586712	8.256090
6.714884	421.563112	8.261107
6.669765	422.737843	8.266125
6.604285	422.751295	8.271142
6.437460	421.385788	8.276160
6.352252	424.744262	8.281178
6.392411	424.176285	8.286195
6.757226	435.871151	8.291213
6.718036	451.899050	8.296230
6.894561	446.137437	8.301248
6.567826	426.323255	8.306266
6.646725	432.467786	8.311283
7.069650	424.745726	8.316301
6.811057	426.774397	8.321318
6.376732	421.916370	8.326336
6.519441	422.244335	8.331354
6.831647	439.365856	8.336371
6.814687	427.815371	8.341389
6.304500	434.074290	8.346406
7.039506	440.472624	8.351424
6.782598	438.493236	8.356442
6.678482	432.441090	8.361459
6.784751	414.616623	8.366477
6.454387	428.986023	8.371494
6.866920	437.132670	8.376512
6.640647	448.030235	8.381530
6.733930	441.221336	8.386547
7.080976	451.915470	8.391565
6.628258	441.746042	8.396582
6.695453	444.373754	8.401600
6.579562	444.136333	8.406618
6.613938	444.664305	8.411635
6.808262	446.681975	8.416653
6.792479	459.487352	8.421670
6.519865	447.677114	8.426688
6.532148	445.166409	8.431706
6.651876	440.811692	8.436723
6.852941	442.809371	8.441741
6.442338	444.356941	8.446758
6.975868	433.812090	8.451776
7.103489	438.030296	8.456794
6.911152	453.283788	8.461811
7.016821	445.207492	8.466829
6.907488	452.795296	8.471846
6.819900	454.929718	8.476864
6.773933	446.902425	8.481882
6.683302	452.985164	8.486899
6.918672	442.146203	8.491917
6.805256	457.472538	8.496934
6.775140	458.130533	8.501952
7.013889	455.704262	8.506970
6.724966	449.800983	8.511987
6.859074	442.114701	8.517005
7.005245	449.195420	8.522022
7.003584	455.980574	8.527040
6.953185	452.757022	8.532058
6.812470	455.369975	8.537075
6.809188	454.928722	8.542093
6.599831	454.431395	8.547110
6.613817	453.858051	8.552128
7.054302	449.263731	8.557146
6.634052	456.856070	8.562163
6.957009	465.297627	8.567181
6.826745	472.863472	8.572199
7.025011	481.955723	8.577216
7.076803	482.269533	8.582234
7.079786	479.125973	8.587251
7.151509	477.827225	8.592269
6.845611	474.675258	8.597287
7.045401	474.735509	8.602304
7.358939	481.076819	8.607322
6.858679	468.974036	8.612339
7.022113	456.486413	8.617357
6.743466	461.229018	8.622375
6.806752	474.454355	8.627392
7.262046	467.595037	8.632410
6.821686	485.916937	8.637427
7.136045	476.725505	8.642445
7.431653	485.376480	8.647463
7.099385	476.838619	8.652480
6.922930	468.875941	8.657498
6.984094	481.003415	8.662515
7.180998	477.861029	8.667533
7.232843	488.752913	8.672551
7.316893	479.468179	8.677568
7.353228	457.059853	8.682586
7.231270	461.689547	8.687603
7.052045	457.129206	8.692621
6.900416	459.131655	8.697639
7.125938	458.159100	8.702656
7.524338	458.888808	8.707674
6.982645	460.630486	8.712691
7.124465	458.462393	8.717709
6.779379	455.048331	8.722727
6.961775	457.418159	8.727744
7.344863	454.151934	8.732762
7.092099	463.968083	8.737779
7.221963	451.949618	8.742797
6.976445	458.814005	8.747815
7.069098	467.581975	8.752832
7.139308	469.309830	8.757850
7.044627	482.209635	8.762867
7.302075	482.560649	8.767885
7.317220	488.428014	8.772903
6.945741	475.191068	8.777920
7.135849	487.563426	8.782938
7.210020	482.865549	8.787955
7.267589	480.171021	8.792973
7.551729	479.706824	8.797991
7.274631	484.982514	8.803008
7.391279	478.453957	8.808026
7.013652	477.938814	8.813043
7.204786	483.986883	8.818061
7.075278	483.417086	8.823079
7.144934	489.884971	8.828096
7.212942	483.622805	8.833114
6.979068	488.566681	8.838131
7.223759	482.592409	8.843149
7.130399	477.037171	8.848167
6.974999	478.677301	8.853184
7.331066	477.526503	8.858202
6.997848	483.284349	8.863219
7.244790	486.483498	8.868237
7.348377	488.556414	8.873255
7.193060	485.327204	8.878272
7.352084	481.445995	8.883290
7.144522	492.315410	8.888307
7.288683	491.450274	8.893325
7.397348	482.723405	8.898343
7.040954	490.387804	8.903360
7.063454	482.400259	8.908378
7.005325	504.679564	8.913395
7.323257	505.437661	8.918413
7.577364	507.341831	8.923431
7.385330	507.671753	8.928448
7.730179	510.581015	8.933466
7.315426	513.372610	8.938483
7.552870	501.378281	8.943501
7.921830	503.933476	8.948519
7.485260	498.217414	8.953536
7.508620	477.613031	8.958554
7.548869	480.497431	8.963571
7.312165	481.058409	8.968589
7.494165	487.426642	8.973607
7.531146	483.170085	8.978624
7.271968	473.977000	8.983642
7.271240	482.314648	8.988659
7.042461	479.848018	8.993677
7.529071	494.338771	8.998695
7.380958	502.557511	9.003712
7.778167	495.199207	9.008730
7.548170	503.074177	9.013747
7.297413	487.293703	9.018765
7.405649	489.470030	9.023783
7.323897	500.016786	9.028800
7.710532	506.968336	9.033818
8.004294	512.902507	9.038835
7.745321	499.663694	9.043853
7.513887	488.187799	9.048871
7.587611	497.419490	9.053888
7.530997	481.409791	9.058906
7.954011	490.608842	9.063923
7.397229	484.703339	9.068941
7.446729	482.335117	9.073959
7.594372	493.950441	9.078976
7.614273	486.887938	9.083994
7.517380	495.878121	9.089011
7.673161	486.089847	9.094029
7.926870	484.731028	9.099047
7.323490	486.119462	9.104064
7.804390	484.466275	9.109082
7.394244	487.231898	9.114099
7.522056	487.650559	9.119117
7.427812	483.010627	9.124135
7.446917	481.600205	9.129152
7.570717	482.136257	9.134170
7.319759	484.280501	9.139187
8.023336	500.122640	9.144205
7.824520	494.997324	9.149223
7.240894	488.076717	9.154240
7.653905	501.894209	9.159258
7.708605	506.007094	9.164275
7.873272	506.653507	9.169293
7.866782	497.026349	9.174311
7.702316	487.521776	9.179328
7.770484	481.152290	9.184346
7.542953	487.300670	9.189363
7.513248	479.444381	9.194381
7.788188	489.900531	9.199399
7.743974	501.444936	9.204416
8.095460	503.049830	9.209434
7.726018	485.306138	9.214451
7.380790	481.961520	9.219469
7.857047	503.484921	9.224487
7.832615	501.535373	9.229504
7.608206	495.883898	9.234522
7.411469	502.412461	9.239539
7.782635	509.315943	9.244557
7.701081	501.518260	9.249575
7.635622	511.746894	9.254592
8.162666	501.360808	9.259610
7.673554	497.088847	9.264627
8.066587	507.485480	9.269645
8.140468	504.434948	9.274663
8.016255	506.310031	9.279680
7.621535	490.615226	9.284698
8.012979	481.752535	9.289715
7.748314	487.376567	9.294733
7.747856	486.628762	9.299751
8.030517	501.302952	9.304768
7.978301	492.096365	9.309786
7.607905	484.381814	9.314803
7.760535	493.503312	9.319821
7.899568	500.755581	9.324839
7.763776	506.343648	9.329856
7.651013	511.388474	9.334874
7.791797	514.070938	9.339891
7.829934	515.409352	9.344909
7.931748	511.840054	9.349927
7.591273	511.382203	9.354944
8.137217	506.787125	9.359962
8.297034	514.995493	9.364979
8.114816	510.864791	9.369997
8.255949	513.490397	9.375015
8.259230	506.118070	9.380032
7.969265	491.397758	9.385050
7.831152	486.666869	9.390067
7.966164	490.637781	9.395085
7.950717	474.350243	9.400103
7.860452	487.394525	9.405120
8.010016	503.074164	9.410138
8.400708	503.196022	9.415155
7.745732	495.159987	9.420173
8.433396	480.860856	9.425191
7.576860	492.589333	9.430208
7.860020	491.519385	9.435226
8.088381	502.607679	9.440243
7.993534	511.565992	9.445261
8.144726	505.398081	9.450279
8.353810	505.892370	9.455296
7.751914	496.617273	9.460314
8.207715	502.854251	9.465331
7.923470	501.052706	9.470349
8.102909	500.791102	9.475367
8.029188	509.165445	9.480384
8.268065	511.829383	9.485402
8.357469	505.727957	9.490419
7.952618	496.191616	9.495437
8.266010	486.157745	9.500455
7.969206	490.669676	9.505472
8.130723	492.701959	9.510490
8.355016	488.848391	9.515507
8.089866	484.755935	9.520525
8.088326	479.120039	9.525543
7.728224	489.281218	9.530560
7.860904	504.326042	9.535578
8.086815	505.783356	9.540595
8.076303	517.022693	9.545613
8.139959	502.796069	9.550631
8.185971	509.968244	9.555648
8.308950	505.739233	9.560666
8.609807	499.620456	9.565683
8.270785	511.214214	9.570701
8.432195	503.201740	9.575719
8.303792	519.653926	9.580736
8.369743	515.796760	9.585754
8.396839	503.958460	9.590771
8.250572	498.013880	9.595789
8.306400	487.477573	9.600807
8.033130	482.745771	9.605824
8.251841	493.046634	9.610842
8.241692	498.431979	9.615859
8.060954	505.014839	9.620877
8.605923	502.799355	9.625895
8.432677	511.066218	9.630912
8.256902	508.793248	9.635930
8.283876	499.122977	9.640947
8.437023	511.270772	9.645965
8.307550	505.500280	9.650983
8.292127	508.825746	9.656000
8.462652	508.013282	9.661018
8.498403	501.304890	9.666035
8.074914	496.135881	9.671053
8.365517	499.413397	9.676071
8.302882	507.413622	9.681088
7.706751	509.902281	9.686106
8.462386	501.550556	9.691123
8.174838	512.552434	9.696141
8.572930	507.062195	9.701159
8.169272	508.387780	9.706176
8.098269	514.319143	9.711194
8.553640	505.389622	9.716211
8.208316	520.184310	9.721229
8.373351	511.975607	9.726247
8.362273	520.071900	9.731264
8.250176	510.322428	9.736282
8.400395	506.101772	9.741299
8.758049	515.459397	9.746317
8.684110	505.893294	9.751335
8.403145	504.368942	9.756352
8.215385	508.756497	9.761370
8.789186	509.351431	9.766387
8.733651	501.868402	9.771405
8.861735	508.797347	9.776423
8.315127	503.909554	9.781440
8.128011	507.650078	9.786458
8.584833	498.382667	9.791475
8.383382	510.065320	9.796493
8.324254	503.570606	9.801511
8.570744	499.984953	9.806528
8.365151	505.419857	9.811546
8.346082	508.130521	9.816563
8.297556	507.570125	9.821581
8.331368	499.183175	9.826599
8.307294	514.681751	9.831616
8.569008	524.881222	9.836634
8.722483	523.979911	9.841651
8.720866	532.601740	9.846669
8.857771	530.008381	9.851687
8.508291	516.572301	9.856704
8.432364	525.511878	9.861722
8.883100	524.358868	9.866739
8.490894	524.789580	9.871757
8.544466	531.799635	9.876775
8.785671	530.878267	9.881792
8.672330	532.590706	9.886810
8.645333	526.368656	9.891827
8.929618	531.385992	9.896845
8.831954	524.821570	9.901863
8.477863	507.574061	9.906880
8.370375	514.675616	9.911898
8.723523	521.077004	9.916915
8.480552	537.802774	9.921933
8.644477	541.642936	9.926951
8.841276	535.723486	9.931968
8.370375	542.680022	9.936986
8.431466	531.660033	9.942003
8.189206	539.912476	9.947021
8.475526	533.593997	9.952039
8.919192	526.493485	9.957056
8.485752	532.462706	9.962074
8.876104	522.795447	9.967091
8.819206	535.989168	9.972109
8.614129	534.408742	9.977127
9.125706	533.164150	9.982144
8.786922	537.439677	9.987162
8.827959	524.860731	9.992179
8.813383	543.371595	9.997197
8.618326	534.572369	10.002215
8.670648	530.193479	10.007232
8.551839	531.089432	10.012250
8.801112	533.262602	10.017267
8.882334	556.987568	10.022285
8.713568	559.712227	10.027303
9.010179	556.746708	10.032320
9.043290	563.438093	10.037338
9.041691	550.439781	10.042355
9.001746	551.310757	10.047373
8.831512	550.987176	10.052391
8.876594	526.257905	10.057408
8.515293	538.599930	10.062426
8.953461	551.899131	10.067443
8.979063	555.871420	10.072461
9.300343	566.607530	10.077479
9.305839	558.010397	10.082496
8.781994	543.919970	10.087514
9.100518	530.679014	10.092531
8.453313	547.269315	10.097549
8.812334	557.311549	10.102567
9.078239	560.413067	10.107584
8.461176	566.508898	10.112602
9.248920	562.112603	10.117619
8.963237	566.818469	10.122637
9.013831	569.101666	10.127655
8.931247	569.559606	10.132672
8.996778	571.670051	10.137690
9.178138	567.352984	10.142707
9.241553	570.492542	10.147725
8.966242	568.557048	10.152743
9.145412	568.620530	10.157760
8.943861	568.961411	10.162778
9.444522	554.505332	10.167795
9.345926	560.488370	10.172813
9.043374	561.750781	10.177831
9.177648	558.864344	10.182848
9.200264	558.336980	10.187866
9.228695	565.414103	10.192883
8.966544	552.971003	10.197901
8.958857	566.895485	10.202919
9.354733	558.148827	10.207936
9.327824	561.365650	10.212954
9.154630	552.859632	10.217971
9.190087	555.072616	10.222989
9.306190	556.048529	10.228007
9.666495	538.524959	10.233024
9.026841	543.428288	10.238042
8.948727	538.151505	10.243059
9.357924	536.099299	10.248077
9.339294	530.879469	10.253095
9.217111	530.829223	10.258112
8.998736	537.039301	10.263130
8.774307	537.835040	10.268147
8.937854	552.688878	10.273165
9.183789	553.205797	10.278183
9.175894	557.287476	10.283200
9.000505	561.931879	10.288218
9.164266	553.066958	10.293235
9.558982	559.461847	10.298253
8.948852	560.665153	10.303271
9.149454	557.610536	10.308288
9.238408	558.391889	10.313306
9.064287	551.312423	10.318323
9.186976	557.279724	10.323341
9.109869	555.758140	10.328359
9.615460	553.024963	10.333376
9.134337	552.213612	10.338394
9.296498	553.387432	10.343411
9.230139	552.807738	10.348429
9.143952	555.983356	10.353447
9.513686	560.630710	10.358464
9.410037	566.248473	10.363482
9.358915	579.428698	10.368499
9.541475	562.882840	10.373517
9.231580	559.810378	10.378535
9.547642	563.888638	10.383552
9.424169	571.544978	10.388570
9.245299	566.911971	10.393587
9.047242	578.215445	10.398605
9.254050	577.921151	10.403623
9.571759	577.849319	10.408640
9.354673	578.700713	10.413658
9.211496	584.312052	10.418675
9.285344	576.414250	10.423693
9.403021	584.711303	10.428711
9.651925	582.283423	10.433728
9.295801	590.039339	10.438746
9.158453	585.273591	10.443763
9.827140	592.698529	10.448781
9.465598	587.141094	10.453799
9.428049	581.081623	10.458816
9.318555	587.921592	10.463834
9.591063	581.450628	10.468851
9.804284	576.450076	10.473869
9.360918	583.676865	10.478887
9.460112	570.602787	10.483904
9.544489	584.386628	10.488922
9.693873	587.607392	10.493939
9.699109	579.530992	10.498957
9.595700	582.961774	10.503975
9.767360	582.231179	10.508992
9.760662	588.834138	10.514010
9.635321	588.689713	10.519027
9.990422	585.847567	10.524045
9.396144	588.894517	10.529063
9.856991	582.908434	10.534080
9.333090	595.424295	10.539098
9.100255	583.970649	10.544115
9.495370	584.438948	10.549133
9.654963	609.338275	10.554151
10.172758	607.417367	10.559168
9.684260	594.855068	10.564186
9.624643	585.491804	10.569203
9.843358	596.430192	10.574221
9.458032	592.072520	10.579239
9.751052	601.632819	10.584256
10.164241	614.462614	10.589274
10.026638	598.452876	10.594291
9.854258	593.446464	10.599309
9.738265	584.006827	10.604327
9.677854	582.643570	10.609344
9.785634	585.946590	10.614362
9.529620	584.948491	10.619379
9.825767	589.963985	10.624397
9.789712	604.423111	10.629415
9.883290	622.241775	10.634432
9.874178	613.372352	10.639450
9.877823	611.468885	10.644467
9.837279	612.040158	10.649485
9.792851	621.662807	10.654503
10.113308	610.968201	10.659520
10.148753	611.922040	10.664538
9.410917	614.028976	10.669555
9.871943	605.975824	10.674573
9.881696	614.507549	10.679591
9.939280	608.796078	10.684608
9.916220	609.443506	10.689626
9.884877	624.949628	10.694643
10.010085	618.186151	10.699661
9.744447	623.400127	10.704679
10.105172	619.354743	10.709696
10.053671	623.676797	10.714714
9.892424	620.764069	10.719731
10.177934	613.505268	10.724749
10.004040	624.347397	10.729767
10.014286	612.663144	10.734784
10.128325	623.535898	10.739802
10.266823	618.827906	10.744819
9.839675	615.199454	10.749837
9.960734	613.741490	10.754855
9.916060	615.522073	10.759872
9.952570	616.270620	10.764890
10.242306	619.365259	10.769907
9.965281	615.511316	10.774925
10.042472	627.639534	10.779943
9.988647	615.028051	10.784960
9.817718	613.101444	10.789978
10.193958	609.012607	10.794995
9.876686	611.290331	10.800013
10.009800	624.400698	10.805031
9.648961	609.530449	10.810048
10.051772	617.262140	10.815066
10.057733	616.923575	10.820083
10.045724	618.762155	10.825101
9.912442	615.908162	10.830119
9.881692	626.806760	10.835136
10.088451	627.468673	10.840154
9.921137	639.467952	10.845171
10.496285	634.173994	10.850189
10.093007	651.612946	10.855207
10.172350	649.820691	10.860224
10.519978	645.474398	10.865242
10.148204	641.575335	10.870259
10.652714	641.436366	10.875277
10.260082	647.411854	10.880295
10.553802	649.164667	10.885312
10.301232	624.182098	10.890330
10.125803	631.897097	10.895347
10.265244	617.181985	10.900365
10.191625	638.813794	10.905383
10.268341	639.499239	10.910400
10.459707	639.747002	10.915418
10.265859	648.399005	10.920435
10.606149	633.298963	10.925453
10.414720	640.959669	10.930471
10.066784	634.472289	10.935488
10.634151	634.058386	10.940506
10.397663	636.102551	10.945523
10.204311	628.590570	10.950541
10.159516	632.321445	10.955559
10.398139	639.772760	10.960576
10.579444	642.193276	10.965594
10.010504	641.783841	10.970611
10.422640	633.643663	10.975629
10.265303	638.723911	10.980647
9.974908	630.412943	10.985664
10.289536	642.702784	10.990682
10.294472	635.226004	10.995699
10.289202	633.844635	11.000717
10.130251	637.665979	11.005735
10.419253	643.938608	11.010752
10.300849	650.858892	11.015770
10.430336	662.890578	11.020787
10.409753	659.867443	11.025805
10.623693	662.835110	11.030823
10.373412	664.045157	11.035840
10.771179	670.326001	11.040858
10.652407	666.870127	11.045875
11.118527	665.945071	11.050893
10.669936	654.553585	11.055911
10.368784	655.146757	11.060928
10.786165	639.296178	11.065946
10.441112	637.728207	11.070963
10.374937	640.411558	11.075981
10.235576	648.218743	11.080999
10.221307	659.919503	11.086016
10.414746	663.073418	11.091034
10.796616	668.454197	11.096051
10.564570	662.469353	11.101069
10.482099	671.889708	11.106087
10.612787	671.689389	11.111104
10.703818	668.746594	11.116122
10.408196	673.024858	11.121139
10.679056	670.492541	11.126157
10.629752	669.566191	11.131175
10.533634	662.045273	11.136192
10.493095	666.024794	11.141210
10.558320	670.031927	11.146227
10.689573	665.710064	11.151245
10.729963	676.007413	11.156263
10.822596	687.811362	11.161280
11.046394	685.807123	11.166298
11.007537	682.790002	11.171315
11.033975	673.766657	11.176333
10.941845	669.167370	11.181351
10.548373	662.078047	11.186368
10.640328	667.116088	11.191386
10.980085	669.751621	11.196403
10.875560	676.694987	11.201421
10.944307	669.170325	11.206439
10.605925	665.370166	11.211456
11.196534	668.692226	11.216474
10.646445	668.828943	11.221491
11.093556	661.686813	11.226509
10.887369	667.235467	11.231527
10.671523	674.581279	11.236544
11.308064	682.841264	11.241562
11.160488	670.749357	11.246579
11.104397	661.385500	11.251597
10.790012	664.723122	11.256615
11.156126	669.778169	11.261632
11.532381	664.808853	11.266650
11.341004	667.448709	11.271667
10.839131	669.023221	11.276685
11.229113	662.028896	11.281703
11.025671	672.986137	11.286720
11.344995	661.783598	11.291738
10.635815	671.103330	11.296755
10.777602	669.219238	11.301773
10.918260	664.252121	11.306791
10.854027	674.376515	11.311808
11.434532	669.274211	11.316826
11.362762	670.112308	11.321843
10.955409	656.805110	11.326861
10.972722	665.389323	11.331879
10.870161	667.762801	11.336896
10.987937	663.471452	11.341914
11.071546	662.123492	11.346931
11.198262	672.432561	11.351949
11.123096	666.814453	11.356967
11.110598	674.759561	11.361984
11.481618	662.523291	11.367002
11.407099	671.210257	11.372019
11.273820	662.792606	11.377037
11.066227	663.244888	11.382055
11.131538	665.585752	11.387072
11.040171	658.177699	11.392090
10.966988	653.294583	11.397107
11.250898	659.924619	11.402125
11.232380	666.447408	11.407143
10.999588	677.125230	11.412160
11.710390	681.536142	11.417178
11.385488	687.744028	11.422195
10.902365	675.322840	11.427213
11.282004	678.330821	11.432231
11.237911	676.384334	11.437248
11.365037	687.583279	11.442266
11.587482	685.935855	11.447283
11.429204	686.058521	11.452301
11.425565	682.269026	11.457319
11.082597	683.793396	11.462336
11.540626	682.169022	11.467354
11.527100	680.845747	11.472371
11.184322	688.826831	11.477389
11.258594	685.211320	11.482407
11.350718	691.836703	11.487424
11.318270	683.052952	11.492442
11.501235	693.053420	11.497459
11.376697	699.633858	11.502477
11.558125	690.056048	11.507495
11.317424	700.738278	11.512512
11.426499	685.428268	11.517530
11.423203	694.201915	11.522547
11.411873	685.493749	11.527565
11.508535	689.880967	11.532583
11.584421	685.387894	11.537600
11.808861	685.734616	11.542618
11.572020	685.276302	11.547635
11.036727	687.231591	11.552653
11.640127	685.915798	11.557671
11.365945	686.630976	11.562688
11.291878	680.523545	11.567706
11.701954	687.193783	11.572723
11.436506	690.741492	11.577741
11.698103	675.540137	11.582759
11.661820	688.743363	11.587776
11.612289	680.363075	11.592794
11.497024	688.270643	11.597811
11.296477	684.461507	11.602829
11.631610	685.450446	11.607847
11.453671	685.787629	11.612864
11.668789	684.049836	11.617882
11.344230	688.503050	11.622899
11.534696	707.007203	11.627917
11.734740	706.997988	11.632935
11.568578	712.843341	11.637952
11.815967	710.885895	11.642970
11.665092	708.596375	11.647987
11.642278	708.751465	11.653005
11.997979	713.694547	11.658023
11.975342	714.136786	11.663040
11.779238	716.187256	11.668058
11.709120	719.704367	11.673075
11.992793	722.108855	11.678093
11.942476	697.350114	11.683111
11.879558	721.085258	11.688128
12.098441	707.118172	11.693146
11.999704	708.039392	11.698163
11.656034	706.477509	11.703181
11.769980	698.948909	11.708199
11.675982	711.760410	11.713216
12.025576	715.240162	11.718234
12.054115	713.127657	11.723251
11.908674	710.225061	11.728269
11.700788	707.632050	11.733287
11.932916	727.007007	11.738304
11.757661	708.087115	11.743322
11.931782	722.099997	11.748339
11.833405	715.677627	11.753357
12.008577	718.184321	11.758375
11.721242	713.792331	11.763392
11.979055	705.303917	11.768410
12.060055	709.176044	11.773427
11.804990	721.018713	11.778445
11.975064	708.933815	11.783463
11.873081	712.500097	11.788480
11.736860	714.238229	11.793498
12.165405	712.820442	11.798515
11.581617	709.617299	11.803533
12.110339	712.990089	11.808551
11.418589	724.412032	11.813568
12.125359	732.190823	11.818586
12.512785	737.791659	11.823603
12.186133	729.117097	11.828621
12.388025	721.779835	11.833639
11.949305	714.574504	11.838656
12.318415	713.427960	11.843674
11.881682	711.650285	11.848691
12.198357	730.324036	11.853709
11.963335	731.784161	11.858727
11.808081	748.509007	11.863744
12.209418	747.228024	11.868762
12.476676	739.085252	11.873779
12.423692	748.081305	11.878797
12.321887	734.410596	11.883815
12.097921	744.743092	11.888832
12.416545	743.490848	11.893850
12.449125	745.047901	11.898867
12.376388	742.692485	11.903885
12.497786	740.559117	11.908903
12.376255	733.859502	11.913920
12.351297	734.456739	11.918938
12.136204	727.683424	11.923955
12.317448	737.709432	11.928973
12.416890	736.535711	11.933991
12.291531	738.133288	11.939008
12.362775	743.565915	11.944026
12.649253	743.994436	11.949043
12.130947	739.749081	11.954061
12.693291	739.563181	11.959079
12.352905	743.611790	11.964096
12.106982	736.527722	11.969114
12.258220	745.021563	11.974131
12.478065	746.438822	11.979149
12.610115	741.166920	11.984167
12.683881	747.113548	11.989184
12.197758	743.251313	11.994202
12.575311	737.827339	11.999219
12.322446	747.833006	12.004237
12.252745	745.174158	12.009255
12.519938	736.090969	12.014272
12.446380	739.649648	12.019290
12.569096	739.157088	12.024307
12.261847	740.398156	12.029325
12.248643	740.993552	12.034343
12.354997	739.032954	12.039360
12.119067	750.856866	12.044378
12.443805	749.770921	12.049395
12.253704	769.303596	12.054413
12.340222	766.411985	12.059431
12.398260	767.270775	12.064448
12.240590	774.083649	12.069466
12.586345	766.010617	12.074483
12.487653	772.183089	12.079501
13.107799	767.942392	12.084519
12.740187	764.042649	12.089536
13.076681	769.152858	12.094554
12.817318	771.424685	12.099571
12.991994	768.516106	12.104589
12.646779	770.681463	12.109607
12.803657	768.536221	12.114624
12.757451	775.729262	12.119642
13.299281	774.262164	12.124659
12.805123	770.868241	12.129677
12.991470	768.551124	12.134695
13.119420	770.197378	12.139712
12.855785	780.157414	12.144730
12.981484	769.638395	12.149747
12.935915	776.411616	12.154765
13.028460	766.809821	12.159783
12.748651	741.806109	12.164800
12.776363	755.876670	12.169818
13.200601	755.813394	12.174835
12.753401	752.954915	12.179853
12.797139	761.686513	12.184871
12.965481	771.446318	12.189888
12.633265	771.974933	12.194906
12.734403	770.829346	12.199923
12.652539	779.675306	12.204941
12.884851	769.622422	12.209959
12.919917	780.311985	12.214976
12.803953	777.221724	12.219994
13.070742	772.581954	12.225011
12.997762	769.428154	12.230029
12.944170	767.672494	12.235047
13.113269	762.669336	12.240064
13.080107	773.476883	12.245082
12.959148	772.684830	12.250099
12.979048	772.890032	12.255117
13.014026	767.728006	12.260135
13.046528	759.397944	12.265152
12.956342	772.278319	12.270170
13.243215	772.987646	12.275187
12.675585	775.285682	12.280205
12.919324	774.007299	12.285223
13.201604	789.458113	12.290240
13.029177	793.515132	12.295258
13.453438	788.490923	12.300275
13.203342	793.169181	12.305293
13.104655	789.287259	12.310311
13.378931	796.815105	12.315328
13.416975	803.685688	12.320346
13.616622	796.566498	12.325363
13.258277	783.106359	12.330381
13.112334	775.223971	12.335399
13.383342	782.660804	12.340416
13.258744	788.502826	12.345434
13.448426	785.500374	12.350451
13.082701	775.048881	12.355469
13.311159	785.954300	12.360487
13.581733	785.072499	12.365504
13.405425	793.683955	12.370522
13.382438	784.996501	12.375539
13.220887	786.533481	12.380557
13.320191	795.467828	12.385575
13.350794	795.636640	12.390592
12.996936	799.273961	12.395610
13.593381	795.854326	12.400627
13.404640	795.353759	12.405645
13.407395	801.857486	12.410663
13.549728	795.466801	12.415680
13.753118	802.658616	12.420698
13.708974	799.957886	12.425715
13.485725	797.954249	12.430733
13.222127	793.523806	12.435751
13.277289	797.355819	12.440768
13.268015	798.212533	12.445786
13.399710	795.361176	12.450803
13.199835	791.700234	12.455821
13.159631	797.361778	12.460839
13.484064	797.957924	12.465856
13.305104	797.771405	12.470874
13.844683	797.816290	12.475891
13.667536	796.354541	12.480909
13.513043	793.390233	12.485927
13.846048	800.350301	12.490944
13.586276	802.584326	12.495962
13.531349	803.498686	12.500979
13.582727	795.882019	12.505997
13.767446	827.379664	12.511015
14.283727	814.618756	12.516032
13.752172	810.792027	12.521050
13.603844	782.889557	12.526067
13.835603	786.125853	12.531085
13.614817	793.728108	12.536103
14.075072	787.666311	12.541120
13.789105	786.941136	12.546138
13.790680	785.546060	12.551155
13.915651	787.808164	12.556173
13.714700	792.923691	12.561191
13.939839	787.176443	12.566208
13.911227	785.893394	12.571226
13.686280	783.438745	12.576243
13.803932	788.800998	12.581261
13.954761	791.702836	12.586279
13.964351	793.724243	12.591296
13.982292	801.267007	12.596314
13.719876	793.402859	12.601331
14.160849	793.422168	12.606349
13.987733	801.846934	12.611367
14.103659	792.282488	12.616384
13.774499	791.611418	12.621402
13.903999	793.150134	12.626419
14.090594	798.460562	12.631437
14.115880	804.989162	12.636455
13.848431	791.590515	12.641472
14.200651	812.262720	12.646490
13.994671	817.606261	12.651507
14.089517	807.035250	12.656525
14.040372	814.550660	12.661543
14.156787	826.019614	12.666560
14.529339	819.065829	12.671578
14.113771	809.780308	12.676595
14.241355	804.468062	12.681613
13.705283	796.640478	12.686631
14.025822	805.240365	12.691648
13.858502	820.878415	12.696666
14.137448	823.555058	12.701683
14.237140	829.791141	12.706701
14.121304	821.954508	12.711719
14.268696	816.986294	12.716736
13.986553	821.221455	12.721754
13.977154	820.405610	12.726771
14.265585	821.206213	12.731789
14.388581	826.993675	12.736807
14.399626	814.564393	12.741824
14.629129	816.545035	12.746842
14.376536	818.736912	12.751859
14.689679	814.777835	12.756877
14.334100	833.178324	12.761895
14.365863	819.915813	12.766912
14.298209	824.486599	12.771930
14.551481	823.806323	12.776947
14.650201	819.379067	12.781965
14.577894	831.332030	12.786983
14.633525	810.722207	12.792000
14.512596	806.875324	12.797018
14.084895	800.059552	12.802035
14.417707	808.903672	12.807053
14.478327	820.842113	12.812071
14.549997	816.662093	12.817088
14.406603	820.133899	12.822106
14.562633	816.268866	12.827123
14.701639	815.893673	12.832141
14.448036	813.692818	12.837159
14.343868	809.019642	12.842176
14.307544	812.474671	12.847194
14.225010	812.187837	12.852211
14.776968	819.962521	12.857229
14.609028	827.436589	12.862247
14.752338	821.657969	12.867264
14.864620	816.818333	12.872282
14.600930	820.047055	12.877299
14.538568	819.589802	12.882317
14.192146	828.010176	12.887335
14.477151	810.236207	12.892352
14.343288	820.289542	12.897370
14.241944	812.532693	12.902387
14.664481	823.783269	12.907405
14.173832	825.116194	12.912423
14.977600	844.707829	12.917440
15.202104	838.310566	12.922458
14.512161	827.076705	12.927475
14.875250	827.297565	12.932493
14.586420	832.082888	12.937511
14.869132	839.410614	12.942528
14.862961	840.042781	12.947546
14.908555	847.413974	12.952563
14.763189	840.512925	12.957581
14.658992	850.214489	12.962599
15.036363	844.736862	12.967616
14.659608	848.002239	12.972634
14.882490	844.849408	12.977651
15.298331	841.713682	12.982669
14.989781	853.028329	12.987687
15.036197	844.011235	12.992704
14.911811	847.076124	12.997722
14.966872	840.642292	13.002739
15.369113	840.560371	13.007757
15.084390	848.668130	13.012775
15.152590	840.105218	13.017792
14.807554	828.441775	13.022810
14.914896	840.107820	13.027827
15.071489	839.818234	13.032845
14.849500	850.251468	13.037863
15.127001	839.364640	13.042880
15.324756	844.581815	13.047898
15.002190	859.139687	13.052915
15.165003	843.631772	13.057933
14.771559	840.957361	13.062951
14.957525	844.106168	13.067968
14.916627	845.384407	13.072986
14.912865	840.130599	13.078003
14.994779	834.910706	13.083021
14.744803	837.635508	13.088039
14.946071	839.885665	13.093056
15.275669	857.298354	13.098074
15.348870	870.787520	13.103091
15.584630	854.914715	13.108109
15.138580	865.345193	13.113127
14.908695	849.043574	13.118144
15.124529	854.857525	13.123162
15.030294	864.081008	13.128179
15.129798	862.146716	13.133197
15.214377	864.632911	13.138215
15.091440	872.279828	13.143232
15.544963	871.353580	13.148250
15.408648	869.853869	13.153267
15.762178	874.024160	13.158285
15.702781	877.467038	13.163303
15.414239	859.662961	13.168320
15.393745	862.443330	13.173338
15.334226	870.190764	13.178355
15.691705	861.759244	13.183373
15.570220	873.981874	13.188391
15.682460	873.500419	13.193408
15.637758	867.000157	13.198426
15.630349	872.246330	13.203443
16.040092	866.564807	13.208461
15.624377	869.321893	13.213479
15.372998	862.030345	13.218496
15.818586	863.298636	13.223514
15.926426	868.413140	13.228531
15.565508	855.814888	13.233549
15.515708	846.475196	13.238567
15.605037	860.829677	13.243584
15.632009	859.074008	13.248602
15.442418	875.656030	13.253619
15.730715	855.574593	13.258637
15.336270	868.575292	13.263655
15.497629	864.952412	13.268672
15.572058	866.367219	13.273690
15.547458	868.813715	13.278707
15.542684	870.925744	13.283725
15.628058	861.779461	13.288743
15.669027	860.876826	13.293760
15.801336	858.937395	13.298778
15.503793	865.759595	13.303795
15.577227	862.327218	13.308813
15.504588	864.686566	13.313831
15.987125	878.607068	13.318848
16.080447	883.906889	13.323866
15.974897	894.391334	13.328883
16.313532	886.893723	13.333901
16.224432	884.351503	13.338919
15.720570	876.629290	13.343936
15.972764	865.926293	13.348954
15.626620	883.829893	13.353971
16.167580	880.273767	13.358989
16.118724	886.567859	13.364007
16.031634	887.910143	13.369024
16.029153	889.071912	13.374042
16.325319	895.779012	13.379059
16.210324	878.566267	13.384077
15.542397	875.436236	13.389095
15.563097	875.966363	13.394112
16.196744	890.046236	13.399130
16.007312	892.420731	13.404147
16.229905	886.427695	13.409165
16.054433	888.235110	13.414183
16.140224	889.152673	13.419200
16.126367	892.121357	13.424218
15.845452	881.927914	13.429235
16.081135	878.391217	13.434253
15.949588	881.460389	13.439271
16.175092	884.817605	13.444288
16.302852	874.241397	13.449306
15.954461	879.755592	13.454323
16.052185	891.426334	13.459341
15.971312	890.593281	13.464359
16.236255	905.680837	13.469376
16.438426	904.418425	13.474394
16.635802	922.363138	13.479411
16.612067	917.734136	13.484429
16.298510	900.167469	13.489447
16.011375	889.163949	13.494464
16.853266	903.043946	13.499482
16.404403	908.624385	13.504499
16.545927	893.599448	13.509517
16.524008	893.246311	13.514535
16.314327	884.616463	13.519552
16.268160	886.173242	13.524570
16.241081	903.619770	13.529587
16.620023	901.417628	13.534605
16.641095	908.041601	13.539623
16.542458	914.741137	13.544640
17.040434	911.892334	13.549658
16.718245	904.747563	13.554675
16.321588	897.592373	13.559693
16.687428	895.310233	13.564711
16.676632	893.225961	13.569728
16.722246	890.728905	13.574746
16.608250	896.518808	13.579763
16.293952	892.184647	13.584781
16.759615	896.902267	13.589799
16.286903	907.441090	13.594816
16.886885	901.669789	13.599834
16.897713	908.266965	13.604851
16.891544	909.322015	13.609869
17.095204	913.417966	13.614887
16.861894	899.688838	13.619904
16.996018	891.983425	13.624922
16.912114	892.937044	13.629939
16.687122	889.926961	13.634957
16.699068	888.517629	13.639975
16.693063	900.359264	13.644992
17.016311	904.619514	13.650010
16.768882	915.280836	13.655027
16.914995	913.730559	13.660045
17.047150	918.083869	13.665063
16.761528	913.669470	13.670080
16.999991	908.847909	13.675098
17.021314	910.697077	13.680115
16.814878	913.099485	13.685133
16.936901	913.354961	13.690151
16.703945	916.654624	13.695168
17.134128	910.487044	13.700186
16.921852	907.901003	13.705203
16.757270	909.081859	13.710221
17.084885	915.294885	13.715239
16.597907	915.683649	13.720256
17.009521	912.463366	13.725274
16.865943	912.025147	13.730291
16.835710	910.562461	13.735309
16.801379	927.341112	13.740327
16.990883	938.804999	13.745344
17.135801	927.036323	13.750362
17.088734	933.812993	13.755379
17.185460	934.230224	13.760397
17.552877	938.414134	13.765415
17.186507	939.920101	13.770432
17.562389	941.918849	13.775450
17.363136	942.773777	13.780467
17.411631	946.054595	13.785485
17.428110	937.717493	13.790503
17.425206	934.593711	13.795520
17.181487	919.884734	13.800538
17.197048	917.442877	13.805555
17.333009	925.298564	13.810573
17.508810	931.901458	13.815591
17.431022	940.923586	13.820608
17.679781	934.746552	13.825626
17.436872	931.663530	13.830643
17.536425	926.642820	13.835661
17.357749	913.056601	13.840679
17.363273	931.971820	13.845696
17.613669	935.555521	13.850714
17.927990	933.313007	13.855731
17.594808	917.592404	13.860749
17.603933	907.078946	13.865767
17.399621	912.712589	13.870784
17.393719	906.395583	13.875802
17.582951	914.132465	13.880819
17.548830	932.413263	13.885837
17.824344	935.765808	13.890855
17.723480	936.447529	13.895872
17.576249	931.134121	13.900890
17.713835	932.961919	13.905907
18.037967	932.895393	13.910925
17.880492	918.791447	13.915943
17.082432	926.742983	13.920960
17.716497	928.458278	13.925978
17.801923	929.893457	13.930995
17.561070	936.164000	13.936013
17.829944	941.471047	13.941031
17.568948	937.166394	13.946048
17.589820	941.625509	13.951066
17.753692	934.903193	13.956083
17.570242	936.421526	13.961101
17.650417	924.852345	13.966119
17.381037	932.828349	13.971136
17.678543	944.338434	13.976154
17.583965	948.904003	13.981171
17.819265	956.393841	13.986189
18.014298	966.632415	13.991207
17.674455	959.105377	13.996224
18.123672	962.317102	14.001242
18.001987	964.463239	14.006259
18.177872	960.856999	14.011277
18.119128	974.531020	14.016295
17.830740	961.113434	14.021312
18.083947	964.204390	14.026330
18.174865	952.305301	14.031347
18.190167	967.050167	14.036365
18.230358	960.438738	14.041383
18.260066	960.689744	14.046400
18.296087	955.155111	14.051418
18.477335	960.053011	14.056435
18.055847	961.308837	14.061453
18.142988	962.734283	14.066471
18.028630	968.606317	14.071488
18.199889	971.684866	14.076506
18.289089	966.214483	14.081523
18.283375	967.430413	14.086541
18.538033	961.637458	14.091559
18.378210	971.461413	14.096576
18.312623	967.195565	14.101594
18.430027	959.808326	14.106611
18.153687	959.050078	14.111629
18.341255	954.943386	14.116647
18.066441	962.670943	14.121664
18.037990	962.561828	14.126682
18.417598	959.034123	14.131699
18.252023	966.899202	14.136717
18.508984	963.980855	14.141735
18.060688	965.212479	14.146752
18.420483	956.007372	14.151770
18.342575	963.773507	14.156787
18.099491	977.709944	14.161805
18.342360	982.885377	14.166823
18.480382	986.407799	14.171840
18.787805	978.302808	14.176858
18.846401	980.827804	14.181875
18.738196	986.146607	14.186893
18.549745	989.543454	14.191911
18.765571	986.407483	14.196928
19.093262	990.550292	14.201946
18.908596	982.746463	14.206963
18.603841	976.627736	14.211981
18.820848	978.181161	14.216999
18.808097	982.143775	14.222016
18.847997	976.330815	14.227034
18.555711	974.337974	14.232051
18.607541	977.574094	14.237069
18.977461	976.329576	14.242087
18.603894	987.521950	14.247104
18.557857	983.688541	14.252122
19.164320	978.645200	14.257139
18.629784	982.676944	14.262157
18.917487	984.522253	14.267175
18.933692	982.288571	14.272192
19.020333	989.842741	14.277210
19.056407	987.833167	14.282227
18.962926	988.920836	14.287245
19.114802	978.624815	14.292263
18.847052	987.610456	14.297280
18.974512	984.901745	14.302298
18.963707	978.348794	14.307315
18.933942	984.497917	14.312333
19.045477	969.831069	14.317351
18.844706	985.689101	14.322368
18.697188	983.938668	14.327386
18.862925	982.249609	14.332403
18.279442	989.507982	14.337421
18.954971	993.571046	14.342439
19.133667	1003.790110	14.347456
19.099521	1007.803420	14.352474
19.143853	1003.381484	14.357491
18.912778	1006.119129	14.362509
18.971102	1003.632689	14.367527
19.050600	1006.025024	14.372544
19.190941	1013.031142	14.377562
19.170089	1006.697507	14.382579
19.003566	1019.021968	14.387597
19.264755	1022.821749	14.392615
19.266640	1035.552186	14.397632
19.405082	1036.524625	14.402650
19.679112	1029.387377	14.407667
19.874363	1043.040590	14.412685
19.821950	1029.308266	14.417703
19.825432	1013.840947	14.422720
19.351851	1007.723414	14.427738
19.766833	1007.607939	14.432755
19.420128	1008.242973	14.437773
19.795455	1003.238995	14.442791
19.782413	993.038233	14.447808
19.601738	1011.869099	14.452826
19.649844	998.831115	14.457843
19.236440	1007.634457	14.462861
19.371962	1010.601847	14.467879
19.520894	1005.125248	14.472896
19.429314	1012.454884	14.477914
19.565900	1006.667791	14.482931
19.512753	1028.808111	14.487949
19.741679	1027.468915	14.492967
19.661497	1033.584927	14.497984
19.630575	1036.063995	14.503002
19.868200	1029.506816	14.508019
19.784738	1048.808491	14.513037
20.033164	1038.386853	14.518055
20.333880	1030.879344	14.523072
19.722513	1019.099711	14.528090
19.720158	1011.674410	14.533107
19.729034	1026.237292	14.538125
19.819600	1020.599418	14.543143
20.030320	1027.461968	14.548160
19.961998	1038.066897	14.553178
19.752923	1025.438423	14.558195
20.112033	1034.278535	14.563213
19.581986	1025.051863	14.568231
19.883999	1026.061791	14.573248
19.853488	1038.617422	14.578266
19.824135	1028.343455	14.583283
19.688672	1046.289948	14.588301
19.985101	1035.602010	14.593319
20.186662	1027.232712	14.598336
19.996759	1031.608107	14.603354
19.876020	1023.740595	14.608371
19.996755	1027.218396	14.613389
20.335329	1040.587216	14.618407
20.080148	1033.835844	14.623424
20.151313	1043.920298	14.628442
20.675578	1044.500923	14.633459
20.510566	1040.338998	14.638477
19.955567	1034.000680	14.643495
20.306818	1031.632446	14.648512
19.948114	1033.395998	14.653530
20.380105	1040.937108	14.658547
20.202936	1051.685333	14.663565
20.313457	1061.700514	14.668583
20.797486	1054.710237	14.673600
20.448851	1057.917596	14.678618
20.188367	1053.436107	14.683635
20.224939	1060.903476	14.688653
20.669856	1057.125675	14.693671
20.764564	1050.041762	14.698688
20.525850	1065.489236	14.703706
20.718591	1064.076810	14.708723
20.376839	1063.562338	14.713741
20.672582	1056.598406	14.718759
20.633711	1064.077597	14.723776
20.574099	1064.954834	14.728794
20.532866	1057.923775	14.733811
20.416572	1058.904568	14.738829
20.679848	1053.618326	14.743847
20.835635	1048.112238	14.748864
20.817951	1063.222118	14.753882
20.477198	1058.787918	14.758899
20.623793	1044.951818	14.763917
20.564947	1047.716133	14.768935
20.477272	1059.201435	14.773952
20.726282	1055.520601	14.778970
20.673548	1051.618798	14.783987
20.607065	1067.092939	14.789005
20.605163	1060.683732	14.794023
20.868659	1059.017219	14.799040
20.747776	1063.833096	14.804058
21.126075	1068.917906	14.809075
20.703361	1068.766419	14.814093
20.755115	1067.240381	14.819111
21.104959	1063.628956	14.824128
20.985212	1080.061365	14.829146
21.322411	1073.103554	14.834163
21.339730	1080.397221	14.839181
20.938176	1065.706541	14.844199
20.708312	1069.223502	14.849216
20.655263	1074.925016	14.854234
20.786871	1073.541103	14.859251
20.837035	1068.569118	14.864269
20.752980	1074.310204	14.869287
21.026649	1070.464556	14.874304
20.638267	1082.643937	14.879322
20.934913	1081.354087	14.884339
21.262243	1092.424087	14.889357
21.454318	1105.380400	14.894375
21.648487	1094.061498	14.899392
21.288221	1079.711483	14.904410
21.004402	1075.950024	14.909427
21.373767	1086.937694	14.914445
21.252948	1089.913701	14.919463
21.420528	1095.656395	14.924480
21.436882	1098.254299	14.929498
21.637081	1098.809960	14.934515
21.260503	1086.308674	14.939533
21.273695	1096.086654	14.944551
21.865855	1094.662139	14.949568
21.545564	1089.262188	14.954586
21.416221	1089.837922	14.959603
21.651782	1085.064107	14.964621
21.571109	1101.562999	14.969639
21.694830	1088.812909	14.974656
21.729616	1093.654897	14.979674
21.856611	1075.425730	14.984691
21.762033	1073.360875	14.989709
21.828116	1073.950171	14.994727
21.899674	1069.145250	14.999744
21.235702	1073.238320	15.004762
21.172844	1071.206366	15.009779
21.592410	1083.940826	15.014797
21.700015	1089.531965	15.019815
21.787423	1091.708474	15.024832
21.583115	1099.459758	15.029850
21.564689	1101.738058	15.034867
21.720001	1094.404786	15.039885
21.502515	1103.723443	15.044903
21.865949	1101.141848	15.049920
21.736667	1096.254776	15.054938
21.959845	1102.569440	15.059955
21.824335	1103.512220	15.064973
21.474350	1095.951998	15.069991
21.989908	1115.024189	15.075008
21.805200	1123.750729	15.080026
21.775109	1126.706216	15.085043
21.953678	1114.531349	15.090061
22.201449	1128.933807	15.095079
22.199761	1122.309945	15.100096
22.241669	1124.875447	15.105114
22.333630	1126.066616	15.110131
22.449589	1121.362024	15.115149
22.332668	1124.233283	15.120167
22.470363	1115.163881	15.125184
22.262797	1108.061031	15.130202
22.373371	1100.021541	15.135219
22.213001	1097.256923	15.140237
21.894680	1098.600737	15.145255
22.213902	1103.025771	15.150272
22.475027	1119.783558	15.155290
22.336347	1127.493012	15.160307
22.585638	1119.835731	15.165325
22.360804	1123.118380	15.170343
22.235455	1106.945316	15.175360
22.405896	1117.866341	15.180378
22.067331	1114.605766	15.185395
22.333643	1117.357018	15.190413
22.058476	1114.667188	15.195431
22.311010	1129.801061	15.200448
22.665828	1116.888508	15.205466
22.297205	1130.147287	15.210483
22.567674	1107.275420	15.215501
22.231436	1122.438417	15.220519
22.317695	1118.366496	15.225536
22.650160	1124.727162	15.230554
22.730449	1126.611295	15.235571
22.571521	1120.961986	15.240589
22.559157	1123.081545	15.245607
22.734108	1137.378652	15.250624
22.884545	1145.140648	15.255642
22.661746	1138.368383	15.260659
22.976749	1140.121067	15.265677
22.880477	1132.252829	15.270695
22.942428	1116.744701	15.275712
22.791897	1114.603400	15.280730
22.628191	1115.519040	15.285747
23.471819	1124.917612	15.290765
22.878779	1121.769491	15.295783
22.884887	1115.583076	15.300800
22.902259	1108.236696	15.305818
22.916387	1119.775515	15.310835
23.067206	1121.216243	15.315853
23.116945	1137.398085	15.320871
22.906700	1127.531106	15.325888
22.994170	1142.832866	15.330906
22.839988	1139.445565	15.335923
23.079758	1144.208112	15.340941
22.997036	1145.142624	15.345959
23.156465	1149.453847	15.350976
23.274336	1148.832645	15.355994
22.640325	1148.556469	15.361011
23.143138	1145.040984	15.366029
23.096310	1149.412926	15.371047
23.197906	1139.882099	15.376064
23.084194	1138.899542	15.381082
23.128274	1143.746399	15.386099
23.636608	1141.372474	15.391117
22.985181	1143.658437	15.396135
23.138755	1143.435592	15.401152
23.383760	1150.977642	15.406170
23.524352	1167.530292	15.411187
23.358720	1163.535698	15.416205
23.245134	1172.131196	15.421223
23.533436	1168.090726	15.426240
23.499204	1172.915146	15.431258
23.424415	1173.157279	15.436275
23.792030	1165.427790	15.441293
23.574576	1164.846502	15.446311
23.503097	1161.247419	15.451328
23.672318	1163.070284	15.456346
23.627878	1166.299431	15.461363
23.485163	1165.195181	15.466381
23.418814	1172.492526	15.471399
23.735357	1173.089922	15.476416
23.791195	1171.304454	15.481434
23.702442	1172.119988	15.486451
23.813916	1168.905659	15.491469
23.544442	1163.589244	15.496487
23.862879	1167.452672	15.501504
23.608105	1167.142324	15.506522
23.283518	1167.120632	15.511539
23.459704	1157.578108	15.516557
23.600276	1176.522920	15.521575
23.841270	1195.079625	15.526592
23.819094	1187.332301	15.531610
23.850210	1186.478532	15.536627
23.924454	1187.631455	15.541645
23.894575	1188.024346	15.546663
24.035327	1191.861969	15.551680
23.974121	1197.848829	15.556698
24.021679	1189.115412	15.561715
24.034397	1187.873196	15.566733
24.116396	1189.116425	15.571751
24.118605	1190.940213	15.576768
24.229698	1182.506120	15.581786
23.882373	1193.126452	15.586803
24.088405	1182.875478	15.591821
24.140820	1185.584513	15.596839
24.074291	1178.282808	15.601856
24.388510	1182.888531	15.606874
24.540408	1205.041126	15.611891
24.522945	1183.378794	15.616909
24.246706	1185.820578	15.621927
24.786286	1175.668830	15.626944
24.448182	1176.820085	15.631962
24.382347	1175.823713	15.636979
24.699203	1179.431765	15.641997
24.953930	1177.577264	15.647015
24.589134	1181.891733	15.652032
24.549424	1176.728667	15.657050
24.829706	1185.524399	15.662067
24.838867	1177.292476	15.667085
24.593290	1184.229734	15.672103
24.731578	1182.740622	15.677120
24.479865	1175.237554	15.682138
24.393302	1182.998828	15.687155
24.664521	1180.217071	15.692173
24.347953	1181.036740	15.697191
24.423312	1187.011668	15.702208
24.532015	1192.334419	15.707226
24.800712	1213.402037	15.712243
24.669345	1207.123518	15.717261
24.625234	1212.684816	15.722279
24.815720	1206.172829	15.727296
25.175128	1201.827714	15.732314
24.551019	1206.526808	15.737331
24.806010	1203.930631	15.742349
25.071539	1202.484698	15.747367
25.033852	1209.304186	15.752384
25.048331	1211.163924	15.757402
25.223634	1219.846730	15.762419
25.034422	1213.640389	15.767437
24.869412	1213.527420	15.772455
24.831716	1211.816564	15.777472
24.951713	1198.823976	15.782490
25.145043	1210.988044	15.787507
25.000247	1209.981950	15.792525
25.081261	1211.698717	15.797543
24.838008	1209.073302	15.802560
25.071716	1213.353968	15.807578
25.106825	1227.597316	15.812595
25.484662	1231.271565	15.817613
25.368219	1228.269665	15.822631
25.555811	1244.215404	15.827648
25.789637	1219.626021	15.832666
25.273973	1213.660180	15.837683
25.419591	1212.469726	15.842701
25.333556	1205.070078	15.847719
25.416492	1206.149056	15.852736
25.417755	1205.804904	15.857754
25.614893	1209.712593	15.862771
25.424952	1205.178986	15.867789
25.456080	1215.841024	15.872807
25.422601	1228.349916	15.877824
25.622742	1226.677536	15.882842
25.664746	1226.487950	15.887859
25.671199	1234.783797	15.892877
25.755945	1230.961403	15.897895
25.650775	1232.767305	15.902912
25.749858	1226.556816	15.907930
25.574029	1234.401528	15.912947
25.939437	1227.675929	15.917965
25.696820	1230.614237	15.922983
25.552094	1235.023630	15.928000
25.789974	1231.817887	15.933018
25.519435	1238.670713	15.938035
25.540394	1242.104226	15.943053
25.844372	1228.729332	15.948071
25.835361	1235.897796	15.953088
25.701680	1237.663982	15.958106
25.629174	1239.108152	15.963123
25.922043	1252.654710	15.968141
26.003362	1251.411209	15.973159
25.941442	1262.886294	15.978176
26.123245	1261.560776	15.983194
26.149822	1256.964829	15.988211
26.034025	1251.813663	15.993229
26.072210	1251.141825	15.998247
26.246786	1251.449034	16.003264
26.053300	1246.736086	16.008282
25.825969	1256.501345	16.013299
25.847505	1253.010750	16.018317
26.008703	1251.009945	16.023335
25.794461	1257.462627	16.028352
26.367279	1272.312903	16.033370
26.156402	1277.591073	16.038387
26.207016	1277.065614	16.043405
26.346177	1268.276779	16.048423
26.677969	1280.700074	16.053440
26.866759	1273.310990	16.058458
26.631134	1284.488247	16.063475
26.557533	1281.710006	16.068493
26.827302	1273.926370	16.073511
26.875024	1281.537256	16.078528
26.667720	1267.273580	16.083546
26.488860	1255.321881	16.088563
26.514845	1270.500836	16.093581
26.754395	1282.550411	16.098599
26.632781	1281.338703	16.103616
26.541400	1276.082716	16.108634
26.744656	1284.638093	16.113651
26.755192	1275.579065	16.118669
26.973353	1273.559865	16.123687
26.790885	1284.637273	16.128704
27.005126	1274.217698	16.133722
27.007177	1278.922850	16.138739
26.726537	1278.831154	16.143757
26.760810	1275.726734	16.148775
26.664635	1276.423512	16.153792
26.700436	1274.748473	16.158810
27.101000	1267.812218	16.163827
26.814167	1273.480994	16.168845
26.904765	1267.145586	16.173863
26.640056	1271.737892	16.178880
26.920875	1266.644505	16.183898
26.910515	1276.296883	16.188915
27.150082	1294.724523	16.193933
27.271572	1303.112834	16.198951
27.457355	1301.524750	16.203968
27.124300	1296.413922	16.208986
27.257465	1298.122526	16.214003
27.290693	1305.227594	16.219021
27.759355	1294.597727	16.224039
27.107230	1291.196893	16.229056
27.060690	1292.214108	16.234074
27.171179	1301.872812	16.239091
27.321751	1299.968344	16.244109
27.596992	1298.981643	16.249127
27.279636	1297.308283	16.254144
26.920963	1295.351054	16.259162
27.025853	1308.302240	16.264179
27.072129	1304.056655	16.269197
27.359369	1297.450578	16.274215
27.563853	1317.231306	16.279232
27.672158	1313.307370	16.284250
27.856974	1318.141692	16.289267
27.774276	1321.162259	16.294285
27.773389	1314.860103	16.299303
27.620320	1319.924095	16.304320
27.678994	1319.949654	16.309338
27.706925	1321.832543	16.314355
27.436883	1325.548359	16.319373
28.072883	1319.402042	16.324391
27.972787	1325.376103	16.329408
27.695507	1322.623455	16.334426
28.419004	1325.703909	16.339443
27.852202	1328.393214	16.344461
28.060248	1317.542226	16.349479
28.069762	1313.305555	16.354496
27.957967	1322.588831	16.359514
28.107166	1330.483649	16.364531
27.726721	1332.316910	16.369549
27.960221	1322.916802	16.374567
27.883501	1327.444954	16.379584
27.912775	1313.608093	16.384602
28.033092	1318.357843	16.389619
27.720134	1322.421219	16.394637
28.485899	1322.604245	16.399655
28.195200	1338.565043	16.404672
28.203807	1336.783802	16.409690
28.147604	1342.378595	16.414707
28.108414	1354.553944	16.419725
28.406771	1340.674901	16.424743
28.278341	1349.247563	16.429760
28.513252	1343.438644	16.434778
28.418039	1346.483268	16.439795
27.971989	1348.307874	16.444813
28.665318	1349.322784	16.449831
28.213851	1342.958665	16.454848
28.360161	1347.016364	16.459866
28.486924	1347.637189	16.464883
28.418062	1353.546403	16.469901
28.444504	1340.243313	16.474919
28.715342	1365.590182	16.479936
28.699404	1373.147962	16.484954
28.850735	1372.505731	16.489971
28.741287	1365.980716	16.494989
28.553889	1368.108794	16.500007
28.326094	1373.238159	16.505024
28.615008	1364.782431	16.510042
28.859457	1369.178221	16.515059
28.959501	1374.511850	16.520077
29.054746	1367.645485	16.525095
29.025889	1367.489092	16.530112
28.914947	1364.379005	16.535130
28.862437	1366.861502	16.540147
28.602864	1366.946391	16.545165
29.309249	1370.064248	16.550183
28.837835	1370.251758	16.555200
28.760768	1365.643619	16.560218
29.480450	1359.907070	16.565235
28.957576	1364.277908	16.570253
29.134806	1365.480981	16.575271
29.344933	1364.788511	16.580288
29.079465	1364.909039	16.585306
29.626778	1356.627432	16.590323
29.340187	1355.823433	16.595341
29.563524	1355.425548	16.600359
29.293693	1360.422636	16.605376
29.104152	1369.399370	16.610394
29.476514	1363.739329	16.615411
29.626598	1383.544433	16.620429
29.541924	1368.289442	16.625447
29.344606	1366.104946	16.630464
29.382778	1375.718215	16.635482
29.715200	1385.825047	16.640499
29.423567	1389.547414	16.645517
29.977929	1389.182875	16.650535
29.418816	1398.069199	16.655552
29.484292	1389.405463	16.660570
29.993012	1389.499370	16.665587
30.194501	1396.041606	16.670605
30.108197	1379.985258	16.675623
30.116102	1365.716188	16.680640
29.269699	1369.165698	16.685658
29.859074	1369.086017	16.690675
30.024830	1375.286693	16.695693
30.048068	1379.505698	16.700711
30.069676	1379.931553	16.705728
29.861111	1375.236714	16.710746
30.006567	1376.943400	16.715763
30.210069	1386.297233	16.720781
30.323072	1369.777308	16.725799
29.954310	1365.546241	16.730816
29.908106	1367.383944	16.735834
30.001614	1368.694813	16.740851
29.895257	1383.127712	16.745869
30.116217	1381.287948	16.750887
30.149314	1392.931272	16.755904
29.566144	1392.868039	16.760922
30.115809	1369.630190	16.765939
29.850070	1387.385990	16.770957
30.254473	1383.254696	16.775975
30.442321	1395.280888	16.780992
30.517382	1420.235616	16.786010
30.481575	1408.760036	16.791027
30.449075	1421.445641	16.796045
30.293252	1416.411155	16.801063
30.673741	1421.644053	16.806080
30.306056	1416.538616	16.811098
30.887057	1406.500174	16.816115
30.402730	1413.913600	16.821133
30.254898	1413.201470	16.826151
30.602119	1413.588934	16.831168
30.406880	1415.793987	16.836186
30.578577	1411.607625	16.841203
30.515200	1412.529651	16.846221
30.412162	1415.622851	16.851239
30.366795	1421.342207	16.856256
30.625719	1429.702734	16.861274
30.980969	1435.832715	16.866291
30.672594	1429.862727	16.871309
31.210804	1434.670115	16.876327
31.040091	1427.785434	16.881344
31.133668	1436.866172	16.886362
31.291191	1429.188422	16.891379
30.970149	1431.454215	16.896397
31.151141	1421.289082	16.901415
31.443031	1434.245774	16.906432
31.091693	1424.656367	16.911450
31.204868	1415.697956	16.916467
31.113189	1403.552611	16.921485
31.334600	1412.354523	16.926503
31.252168	1413.986461	16.931520
31.249942	1423.612396	16.936538
31.743202	1430.484485	16.941555
31.015827	1414.919882	16.946573
31.010968	1418.698313	16.951591
31.088156	1427.005258	16.956608
30.721032	1432.317422	16.961626
31.253930	1431.078899	16.966643
31.361680	1424.851204	16.971661
31.390546	1429.353372	16.976679
31.542959	1425.271017	16.981696
31.187784	1429.337875	16.986714
31.528372	1439.787454	16.991731
31.677910	1450.216477	16.996749
31.709380	1451.221479	17.001767
31.729520	1452.019965	17.006784
31.495122	1462.013669	17.011802
32.030342	1458.912785	17.016819
32.004154	1451.494191	17.021837
31.807677	1454.248574	17.026855
31.766873	1442.079452	17.031872
31.725604	1456.915639	17.036890
32.024834	1446.858203	17.041907
31.657888	1444.119585	17.046925
32.001040	1452.861416	17.051943
32.157235	1448.481806	17.056960
31.871860	1456.776140	17.061978
32.251354	1444.556946	17.066995
32.054869	1444.975946	17.072013
31.991005	1449.006634	17.077031
31.913398	1449.536402	17.082048
31.651571	1459.035766	17.087066
32.150346	1467.702727	17.092083
32.203355	1473.075314	17.097101
32.364460	1477.683012	17.102119
32.504297	1469.686111	17.107136
32.518601	1474.676584	17.112154
32.592277	1473.124985	17.117171
32.605627	1469.550420	17.122189
32.604724	1460.928609	17.127207
32.519782	1456.678299	17.132224
32.127262	1451.014989	17.137242
32.661826	1457.350422	17.142259
32.496324	1462.482676	17.147277
32.211669	1467.627289	17.152295
32.817444	1471.953868	17.157312
32.683398	1467.815395	17.162330
32.798085	1468.873635	17.167347
33.157715	1467.318261	17.172365
32.583846	1469.579487	17.177383
32.867858	1464.744330	17.182400
32.584381	1466.249975	17.187418
32.896450	1465.566777	17.192435
32.788913	1462.695990	17.197453
32.830968	1464.971172	17.202471
33.160117	1468.384847	17.207488
33.014983	1469.752047	17.212506
32.914541	1471.711873	17.217523
33.033333	1471.825847	17.222541
32.832159	1473.072435	17.227559
33.093216	1463.923566	17.232576
32.940015	1463.259614	17.237594
33.052836	1470.399616	17.242611
33.114256	1470.705622	17.247629
33.173128	1465.848932	17.252647
32.911213	1460.774249	17.257664
32.863374	1477.422984	17.262682
33.236793	1492.102706	17.267699
33.057921	1484.007404	17.272717
33.105266	1495.793735	17.277735
33.247500	1484.927710	17.282752
33.261586	1498.262503	17.287770
33.505134	1486.304431	17.292787
33.383004	1497.015896	17.297805
33.126064	1492.890360	17.302823
33.372196	1499.700206	17.307840
33.566023	1515.162352	17.312858
33.921695	1507.207361	17.317875
34.136012	1517.809318	17.322893
33.716508	1500.280750	17.327911
33.873680	1501.215566	17.332928
33.704571	1498.385980	17.337946
33.850989	1511.636931	17.342963
34.518427	1505.277335	17.347981
33.866289	1504.423300	17.352999
33.651879	1488.541566	17.358016
33.732566	1497.971507	17.363034
33.804011	1509.858218	17.368051
34.381639	1504.450006	17.373069
34.008275	1506.629327	17.378087
34.184623	1512.168802	17.383104
34.397309	1508.294745	17.388122
34.479667	1497.286608	17.393139
34.423466	1488.342074	17.398157
34.226304	1490.537970	17.403175
33.914724	1481.778624	17.408192
33.828411	1502.709695	17.413210
34.294361	1496.466881	17.418227
34.667802	1502.559320	17.423245
34.395750	1513.054433	17.428263
34.700022	1504.249082	17.433280
34.707211	1503.165507	17.438298
34.532262	1501.327799	17.443315
34.844147	1498.669015	17.448333
34.702132	1493.370402	17.453351
34.597598	1481.924478	17.458368
34.533626	1484.888488	17.463386
34.695105	1490.887896	17.468403
35.038811	1491.481048	17.473421
34.702914	1489.251974	17.478439
34.584440	1480.894736	17.483456
34.449138	1485.037615	17.488474
34.878098	1498.919659	17.493491
34.751292	1494.404489	17.498509
34.807919	1504.725020	17.503527
34.710034	1493.874519	17.508544
34.626064	1494.944949	17.513562
34.497727	1499.048870	17.518579
34.839026	1498.686152	17.523597
34.832670	1500.328269	17.528615
34.795416	1504.140198	17.533632
34.746147	1521.723354	17.538650
35.003270	1523.440962	17.543667
35.433186	1517.247970	17.548685
35.269103	1521.032434	17.553703
35.542903	1527.651755	17.558720
35.371192	1531.304867	17.563738
35.238475	1523.435855	17.568755
35.744416	1520.569932	17.573773
35.562750	1529.813767	17.578791
35.434408	1527.299694	17.583808
35.472230	1527.571528	17.588826
35.363006	1525.505759	17.593843
35.333848	1526.804299	17.598861
35.535849	1525.494532	17.603879
35.777496	1522.045142	17.608896
35.836019	1519.811075	17.613914
35.768354	1525.032164	17.618931
35.895103	1521.843782	17.623949
35.870378	1522.611430	17.628967
35.811243	1518.464364	17.633984
35.821716	1530.688858	17.639002
36.088210	1520.292514	17.644019
35.986941	1520.481994	17.649037
35.869896	1523.157667	17.654055
35.623648	1518.374015	17.659072
35.897607	1521.042078	17.664090
35.721800	1513.224005	17.669107
35.850469	1518.165012	17.674125
35.413682	1522.800123	17.679143
35.891298	1516.741674	17.684160
35.827523	1522.088391	17.689178
35.896654	1527.278580	17.694195
36.135619	1537.529535	17.699213
36.333296	1547.007447	17.704231
36.289907	1549.409641	17.709248
36.751801	1550.435577	17.714266
36.301233	1555.486284	17.719283
36.112514	1545.921827	17.724301
36.176185	1551.772471	17.729319
36.292538	1544.372532	17.734336
36.410950	1547.816084	17.739354
36.381872	1546.387879	17.744371
36.424959	1548.312602	17.749389
36.235115	1546.767568	17.754407
36.474915	1536.542661	17.759424
36.690073	1546.750012	17.764442
36.581399	1565.169374	17.769459
36.571291	1564.056947	17.774477
36.578083	1575.950675	17.779495
36.596571	1577.061864	17.784512
36.949596	1566.077553	17.789530
36.617968	1575.392246	17.794547
37.040201	1570.680578	17.799565
36.923699	1571.415268	17.804583
36.862584	1575.287757	17.809600
37.148127	1574.883278	17.814618
36.905064	1578.897889	17.819635
36.980114	1571.823162	17.824653
36.854712	1573.259865	17.829671
36.880126	1571.419161	17.834688
37.193211	1588.380695	17.839706
37.146248	1594.725235	17.844723
37.308381	1596.643934	17.849741
37.416007	1601.569326	17.854759
37.330132	1590.631674	17.859776
37.617455	1589.873450	17.864794
37.609614	1589.357140	17.869811
37.525605	1583.238333	17.874829
37.307519	1591.796754	17.879847
37.512974	1596.407001	17.884864
37.459732	1590.731516	17.889882
37.436064	1591.521093	17.894899
37.699407	1591.277890	17.899917
37.659357	1600.679462	17.904935
37.472577	1592.364433	17.909952
37.719377	1589.728457	17.914970
37.514740	1595.968307	17.919987
38.003734	1588.749818	17.925005
38.092600	1593.154260	17.930023
38.107553	1588.512710	17.935040
38.335475	1586.659211	17.940058
37.787592	1587.998000	17.945075
38.017616	1590.704516	17.950093
38.005060	1595.771818	17.955111
37.873411	1585.977482	17.960128
37.798756	1579.314388	17.965146
37.831327	1583.677152	17.970163
38.033085	1589.698686	17.975181
38.289967	1602.591556	17.980199
38.067624	1607.694886	17.985216
38.598736	1608.785724	17.990234
38.375212	1616.464498	17.995251
38.464051	1619.000626	18.000269
38.082220	1604.543108	18.005287
37.875367	1607.946109	18.010304
38.337125	1606.261109	18.015322
38.336011	1607.678342	18.020339
38.481588	1602.315702	18.025357
38.620398	1611.130654	18.030375
38.387716	1608.699193	18.035392
38.614625	1596.904607	18.040410
38.768617	1616.176002	18.045427
38.637524	1615.742121	18.050445
38.917563	1626.990285	18.055463
38.877271	1632.175557	18.060480
38.842668	1637.094839	18.065498
38.946519	1627.986297	18.070515
38.962584	1625.395934	18.075533
39.239993	1633.785220	18.080551
39.124311	1629.883685	18.085568
39.174770	1628.177912	18.090586
38.989369	1622.444224	18.095603
39.079848	1622.982377	18.100621
38.723733	1628.046709	18.105639
39.330475	1618.938279	18.110656
39.546089	1621.830103	18.115674
39.385616	1629.713609	18.120691
39.667648	1619.027581	18.125709
39.539499	1622.961078	18.130727
39.522035	1618.608635	18.135744
39.689052	1615.679028	18.140762
39.699662	1614.165702	18.145779
39.656096	1614.784819	18.150797
39.736914	1611.562590	18.155815
39.613928	1601.325055	18.160832
39.644290	1603.052952	18.165850
39.741252	1612.852806	18.170867
39.779050	1606.121588	18.175885
40.003642	1606.017006	18.180903
39.863803	1601.273467	18.185920
39.832984	1595.632339	18.190938
39.353127	1596.411335	18.195955
39.814468	1598.772328	18.200973
39.823518	1610.211268	18.205991
39.748948	1612.993914	18.211008
39.810877	1610.790862	18.216026
39.652871	1617.588328	18.221043
39.671531	1604.036941	18.226061
40.001804	1614.415652	18.231079
39.954358	1636.899830	18.236096
40.136934	1635.126018	18.241114
39.976979	1640.478371	18.246131
40.169823	1639.539278	18.251149
40.363160	1638.682163	18.256167
40.500997	1634.485274	18.261184
40.477522	1636.382563	18.266202
40.434723	1631.406051	18.271219
40.343628	1638.600160	18.276237
40.386740	1642.399527	18.281255
40.306926	1644.343515	18.286272
40.289744	1639.000052	18.291290
40.232201	1638.718757	18.296307
40.118718	1637.900246	18.301325
40.474336	1646.962127	18.306343
40.495821	1667.513565	18.311360
41.124088	1658.111395	18.316378
40.868220	1665.072542	18.321395
41.018887	1662.571544	18.326413
41.161883	1659.169143	18.331431
41.005742	1656.252288	18.336448
41.239144	1659.901918	18.341466
41.029552	1651.252748	18.346483
41.371636	1652.975994	18.351501
41.094226	1655.572666	18.356519
40.947404	1654.961358	18.361536
41.224165	1645.630047	18.366554
41.157053	1655.723887	18.371571
41.436563	1655.856865	18.376589
41.496815	1650.595946	18.381607
41.099447	1657.582416	18.386624
41.401273	1666.513873	18.391642
41.340736	1654.694854	18.396659
41.348715	1650.537243	18.401677
41.471453	1658.584682	18.406695
41.060366	1658.387182	18.411712
41.142209	1653.116567	18.416730
41.663647	1665.665061	18.421747
41.278378	1679.229825	18.426765
41.710223	1677.754642	18.431783
41.535744	1681.162053	18.436800
41.931747	1679.989147	18.441818
41.742296	1686.838906	18.446835
41.564586	1683.029132	18.451853
41.768713	1684.534142	18.456871
41.680586	1679.378517	18.461888
42.133772	1680.320615	18.466906
42.219451	1685.120074	18.471923
41.737508	1683.860647	18.476941
42.344950	1692.179316	18.481959
42.292071	1703.943616	18.486976
42.182599	1697.876099	18.491994
42.444763	1701.713745	18.497011
42.528291	1697.348616	18.502029
42.327604	1693.113229	18.507047
42.111142	1696.918561	18.512064
42.281884	1702.998644	18.517082
42.181246	1702.133933	18.522099
42.259225	1700.960357	18.527117
42.633214	1701.927488	18.532135
42.493290	1701.409777	18.537152
42.425887	1700.543016	18.542170
42.743305	1706.720046	18.547187
42.675412	1702.347080	18.552205
42.821193	1693.377110	18.557223
42.747699	1702.342141	18.562240
42.872881	1697.809531	18.567258
42.995099	1698.137576	18.572275
42.913249	1692.823165	18.577293
42.982511	1700.961057	18.582311
43.024885	1691.489710	18.587328
42.902476	1679.453139	18.592346
43.292952	1685.918533	18.597363
42.909076	1703.317595	18.602381
43.028898	1682.362178	18.607399
42.651084	1701.101573	18.612416
43.449091	1717.068868	18.617434
43.364606	1720.657857	18.622451
43.442628	1719.825117	18.627469
43.309184	1716.604880	18.632487
43.465855	1718.344558	18.637504
43.741422	1714.400641	18.642522
43.981736	1722.186678	18.647539
43.375839	1703.803441	18.652557
43.538605	1707.031780	18.657575
43.603512	1719.178443	18.662592
43.782087	1713.015295	18.667610
43.830667	1710.580780	18.672627
43.408188	1716.485554	18.677645
43.630573	1707.980126	18.682663
43.470218	1728.661116	18.687680
43.574888	1709.797295	18.692698
43.626223	1713.181956	18.697715
43.376658	1716.506459	18.702733
43.638490	1724.431144	18.707751
43.680976	1732.260805	18.712768
44.049676	1727.140895	18.717786
44.329313	1734.936557	18.722803
44.055090	1734.569281	18.727821
44.187174	1726.279975	18.732839
44.285975	1728.132868	18.737856
44.455460	1720.061779	18.742874
44.739229	1720.661174	18.747891
44.266213	1725.901647	18.752909
44.629501	1715.363785	18.757927
44.237321	1726.922470	18.762944
44.502272	1726.044663	18.767962
44.507018	1721.300531	18.772979
44.293682	1719.916962	18.777997
44.333859	1722.747922	18.783015
44.389517	1732.020954	18.788032
44.794524	1741.491734	18.793050
44.847812	1746.526670	18.798067
44.639148	1746.057600	18.803085
44.917991	1736.848998	18.808103
44.933067	1744.357893	18.813120
45.019975	1737.723078	18.818138
45.088823	1741.348011	18.823155
45.116062	1751.247232	18.828173
45.394812	1733.034648	18.833191
45.351044	1737.687136	18.838208
44.863247	1737.861434	18.843226
44.864587	1739.287761	18.848243
45.148313	1748.095856	18.853261
45.479172	1739.797492	18.858279
45.793277	1752.182860	18.863296
45.647699	1740.528596	18.868314
45.699598	1743.427154	18.873331
45.778798	1747.934140	18.878349
45.619378	1742.802290	18.883367
45.584693	1739.336189	18.888384
45.499064	1739.011953	18.893402
45.736271	1736.134448	18.898419
45.307274	1736.899169	18.903437
45.611367	1737.034608	18.908455
45.831793	1740.146617	18.913472
45.787550	1731.215867	18.918490
45.546511	1738.856410	18.923507
45.421449	1747.936846	18.928525
45.741393	1758.904271	18.933543
45.770258	1761.920057	18.938560
45.596360	1759.028060	18.943578
46.169874	1758.070347	18.948595
45.749532	1766.957202	18.953613
46.152842	1755.463096	18.958631
46.046401	1770.473865	18.963648
46.087481	1773.850676	18.968666
46.393182	1787.231520	18.973683
46.126806	1788.264270	18.978701
46.629503	1787.453359	18.983719
46.457254	1783.828911	18.988736
46.575085	1785.880811	18.993754
46.916758	1785.240304	18.998771
46.437909	1789.310839	19.003789
46.515771	1784.097617	19.008807
46.868873	1789.666294	19.013824
46.766871	1787.463656	19.018842
46.592750	1792.070305	19.023859
46.680920	1795.095740	19.028877
46.633955	1788.617589	19.033895
46.926211	1787.852273	19.038912
47.035406	1777.467800	19.043930
46.990375	1791.058241	19.048947
46.897026	1791.640980	19.053965
46.792679	1794.128501	19.058983
47.130575	1802.110736	19.064000
46.876981	1812.416929	19.069018
46.833340	1811.685302	19.074035
47.153011	1816.792139	19.079053
47.050934	1806.402879	19.084071
47.067849	1807.028307	19.089088
47.413692	1816.429496	19.094106
47.513188	1820.529354	19.099123
47.369328	1817.831468	19.104141
48.001768	1821.929882	19.109159
47.636410	1816.593577	19.114176
47.745395	1823.942617	19.119194
47.856069	1826.633153	19.124211
47.873463	1824.803147	19.129229
47.592078	1825.285952	19.134247
47.815211	1823.202793	19.139264
47.585665	1827.944375	19.144282
47.825472	1816.235992	19.149299
47.959061	1822.467113	19.154317
47.795117	1828.732227	19.159335
48.089498	1832.271347	19.164352
47.340592	1825.230933	19.169370
48.042439	1839.061020	19.174387
48.170112	1847.079367	19.179405
48.308345	1849.793993	19.184423
48.293311	1849.771138	19.189440
48.559233	1853.803900	19.194458
48.446644	1850.116440	19.199475
48.547366	1849.201238	19.204493
48.513039	1838.817124	19.209511
48.567369	1829.801450	19.214528
48.504112	1834.532760	19.219546
48.516765	1838.980763	19.224563
48.467724	1844.988025	19.229581
48.937749	1836.222818	19.234599
48.854269	1836.728269	19.239616
48.578565	1839.526683	19.244634
48.686663	1837.963348	19.249651
49.064219	1833.959242	19.254669
49.091407	1839.474848	19.259687
49.024690	1834.880746	19.264704
48.981959	1840.022277	19.269722
48.912824	1830.861834	19.274739
48.920988	1845.996730	19.279757
49.237580	1861.970150	19.284775
49.486187	1861.735565	19.289792
49.619531	1868.244467	19.294810
49.638574	1860.127453	19.299827
49.578512	1852.909672	19.304845
49.171266	1844.139888	19.309863
49.639256	1849.065696	19.314880
49.718908	1852.887786	19.319898
49.840742	1848.219956	19.324915
49.517143	1854.683673	19.329933
49.605344	1852.520658	19.334951
49.725828	1857.393611	19.339968
49.417583	1868.203889	19.344986
49.596546	1856.785897	19.350003
49.736529	1854.292858	19.355021
49.931419	1861.038283	19.360039
49.728728	1851.176032	19.365056
49.743761	1857.703467	19.370074
49.493825	1869.236801	19.375091
49.836899	1883.116821	19.380109
49.929120	1884.027117	19.385127
50.275209	1878.200608	19.390144
49.906009	1892.507830	19.395162
50.315138	1882.644385	19.400179
50.212414	1884.232204	19.405197
50.261435	1881.990113	19.410215
50.289220	1885.668849	19.415232
49.986315	1907.170846	19.420250
50.456155	1908.400700	19.425267
50.439162	1913.790700	19.430285
50.448699	1913.142262	19.435303
50.758119	1901.359797	19.440320
50.676831	1901.969055	19.445338
51.015038	1906.990957	19.450355
50.826271	1897.492595	19.455373
50.892481	1910.885806	19.460391
51.087510	1904.530654	19.465408
51.328994	1910.211536	19.470426
51.223465	1909.713678	19.475443
51.067555	1907.598372	19.480461
51.396696	1904.892641	19.485479
51.437265	1904.807422	19.490496
51.089200	1899.282178	19.495514
51.396467	1907.196671	19.500531
51.820257	1923.159663	19.505549
51.741205	1919.937178	19.510567
51.506712	1898.440536	19.515584
51.702376	1895.304411	19.520602
51.839550	1893.304143	19.525619
51.955394	1888.649865	19.530637
51.580928	1898.949797	19.535655
51.972997	1890.723829	19.540672
51.617647	1890.362949	19.545690
51.876331	1887.933364	19.550707
51.672699	1903.035215	19.555725
51.849327	1909.758271	19.560743
52.321901	1910.659473	19.565760
52.188518	1914.786370	19.570778
52.338396	1917.941023	19.575795
52.290081	1920.785879	19.580813
51.989412	1920.280722	19.585831
52.180781	1921.462683	19.590848
52.484840	1923.826271	19.595866
52.489807	1912.653268	19.600883
52.683412	1914.705936	19.605901
52.199440	1915.955833	19.610919
52.364825	1921.869562	19.615936
52.023129	1907.878910	19.620954
52.486351	1917.438499	19.625971
52.584025	1907.447101	19.630989
52.383088	1911.811814	19.636007
52.072924	1908.710753	19.641024
52.583266	1922.779206	19.646042
52.947934	1933.023318	19.651059
52.686280	1935.068415	19.656077
52.769487	1943.964831	19.661095
52.992631	1937.595795	19.666112
52.548543	1935.595067	19.671130
52.670557	1933.991671	19.676147
52.985235	1942.690865	19.681165
52.861202	1940.939813	19.686183
53.015267	1957.096583	19.691200
53.034627	1964.163057	19.696218
53.075426	1969.815436	19.701235
53.325046	1962.006256	19.706253
53.444726	1967.636808	19.711271
53.610039	1968.352608	19.716288
53.422941	1966.838667	19.721306
53.384221	1960.109837	19.726323
53.342708	1972.860364	19.731341
53.806872	1975.413484	19.736359
54.074447	1983.207988	19.741376
53.933447	1986.323014	19.746394
53.897670	1983.967955	19.751411
53.468102	1972.159204	19.756429
53.526256	1976.230858	19.761447
54.070785	1977.505824	19.766464
54.237626	1977.088376	19.771482
54.250866	1975.448366	19.776499
54.179467	1975.513242	19.781517
54.176000	1966.247761	19.786535
54.458748	1972.338792	19.791552
54.665090	1975.424644	19.796570
54.239065	1977.899468	19.801587
54.608117	1974.253294	19.806605
54.702268	1995.462799	19.811623
54.874640	1987.832980	19.816640
54.821013	1990.827013	19.821658
54.406379	1985.908659	19.826675
54.948241	1982.263813	19.831693
54.778642	1995.978074	19.836711
55.050450	1995.736696	19.841728
55.345398	2000.942140	19.846746
55.229867	1982.399730	19.851763
54.945257	1973.919957	19.856781
54.773733	1984.860374	19.861799
55.110481	1990.037173	19.866816
55.082331	1996.366283	19.871834
55.041908	1997.745522	19.876851
55.157858	1986.043810	19.881869
54.938930	1990.263028	19.886887
55.239197	1982.266012	19.891904
55.404411	1993.014810	19.896922
55.333385	1994.042213	19.901939
55.838067	2005.340633	19.906957
55.729762	2014.024076	19.911975
55.719952	2024.711946	19.916992
55.779701	2015.550153	19.922010
55.370097	2021.512972	19.927027
55.650914	2017.363025	19.932045
55.569525	2014.964612	19.937063
55.595546	2015.547593	19.942080
55.933282	2014.263866	19.947098
55.991359	2008.659176	19.952115
56.047960	2008.786054	19.957133
55.896165	2011.685010	19.962151
55.945493	2010.326541	19.967168
56.367620	2022.155493	19.972186
56.500825	2029.810113	19.977203
56.559183	2029.842035	19.982221
56.372646	2038.102215	19.987239
56.538786	2038.237179	19.992256
56.701450	2034.635953	19.997274
56.608831	2031.185184	20.002291
57.129056	2025.296628	20.007309
56.706069	2026.174035	20.012327
56.917285	2031.061224	20.017344
56.911053	2027.325503	20.022362
56.933356	2036.840620	20.027379
57.132736	2030.131268	20.032397
56.897954	2030.145997	20.037415
57.108752	2037.791619	20.042432
57.161514	2032.130946	20.047450
56.818322	2029.022415	20.052467
57.234088	2030.708906	20.057485
57.191835	2031.258400	20.062503
56.880791	2024.556431	20.067520
57.245433	2036.580605	20.072538
57.171945	2032.697619	20.077555
57.324462	2031.439754	20.082573
57.403944	2054.415846	20.087591
57.660817	2053.914858	20.092608
57.657554	2057.065124	20.097626
57.521152	2056.108162	20.102643
57.954032	2047.721084	20.107661
57.499219	2056.673446	20.112679
57.668948	2060.961185	20.117696
57.896107	2051.063037	20.122714
57.609283	2046.790564	20.127731
58.236469	2056.763228	20.132749
58.414573	2078.287906	20.137767
58.048176	2077.553183	20.142784
58.337275	2076.510619	20.147802
58.334490	2079.989042	20.152819
58.671051	2073.368642	20.157837
58.674847	2074.371703	20.162855
58.732863	2070.600659	20.167872
58.765011	2055.083764	20.172890
58.545153	2054.742679	20.177907
58.625787	2064.087715	20.182925
58.708363	2068.480635	20.187943
58.553777	2062.423218	20.192960
58.724090	2072.385414	20.197978
58.517000	2074.295736	20.202995
58.945487	2061.446709	20.208013
58.707161	2069.614024	20.213031
58.785232	2068.696048	20.218048
58.958727	2068.659435	20.223066
58.802099	2080.579102	20.228083
58.954221	2085.882693	20.233101
58.933984	2083.225362	20.238119
59.103335	2101.737426	20.243136
59.235916	2089.054670	20.248154
58.871922	2095.909838	20.253171
59.514892	2105.315126	20.258189
59.651121	2115.901269	20.263207
59.822574	2117.386188	20.268224
59.777131	2114.483475	20.273242
60.056276	2118.605751	20.278259
59.793869	2112.517869	20.283277
59.885844	2113.074739	20.288295
59.890415	2105.259706	20.293312
59.967569	2103.612827	20.298330
59.861330	2105.381110	20.303347
60.384900	2103.295033	20.308365
60.161294	2109.806296	20.313383
60.032987	2106.121245	20.318400
60.477235	2102.368582	20.323418
60.259882	2108.983014	20.328435
60.382760	2105.447972	20.333453
60.447910	2104.509926	20.338471
60.450164	2105.390145	20.343488
60.705758	2099.975403	20.348506
60.446877	2100.085433	20.353523
60.511184	2098.266985	20.358541
60.425179	2104.882929	20.363559
60.581066	2099.026184	20.368576
60.753606	2107.315350	20.373594
60.734781	2119.147176	20.378611
60.558063	2127.210183	20.383629
60.697724	2129.653208	20.388647
60.710329	2123.938833	20.393664
61.079773	2119.320508	20.398682
60.873198	2131.096543	20.403699
61.401877	2136.110761	20.408717
61.506706	2147.942169	20.413735
61.544565	2147.080986	20.418752
61.812596	2152.274911	20.423770
61.553740	2155.967051	20.428787
62.064778	2151.380186	20.433805
61.661059	2137.853542	20.438823
61.639359	2142.395371	20.443840
62.186866	2136.477257	20.448858
61.453887	2148.559857	20.453875
61.702849	2141.448190	20.458893
61.700429	2146.334165	20.463911
61.988948	2139.408819	20.468928
62.071034	2134.952284	20.473946
62.018053	2139.641036	20.478963
62.075967	2140.566189	20.483981
61.995486	2147.459015	20.488999
61.847744	2140.532587	20.494016
62.466234	2146.978205	20.499034
62.073474	2169.671800	20.504051
62.013256	2178.575023	20.509069
62.450232	2168.855394	20.514087
62.631626	2172.052495	20.519104
62.914186	2174.056539	20.524122
62.581150	2175.197592	20.529139
62.289787	2175.928141	20.534157
62.534703	2186.528858	20.539175
62.641560	2209.267312	20.544192
62.749239	2189.319988	20.549210
62.630867	2195.473940	20.554227
62.754121	2200.807337	20.559245
63.098146	2198.512674	20.564263
62.934433	2218.396272	20.569280
63.437354	2206.113040	20.574298
63.507150	2218.328709	20.579315
63.450611	2225.643882	20.584333
63.966926	2220.560672	20.589351
63.780937	2225.358654	20.594368
64.033161	2224.126184	20.599386
63.870938	2216.447696	20.604403
63.639805	2217.269804	20.609421
63.508075	2226.837560	20.614439
63.566099	2220.061914	20.619456
63.887004	2213.137778	20.624474
63.534673	2215.885134	20.629491
63.622066	2212.999466	20.634509
63.852606	2214.737088	20.639527
63.920446	2237.276546	20.644544
64.233586	2229.425739	20.649562
64.051222	2238.730012	20.654579
64.291726	2231.439739	20.659597
64.782165	2224.675245	20.664615
64.371015	2238.395975	20.669632
64.484730	2233.312716	20.674650
64.422021	2229.027179	20.679667
64.884986	2226.978988	20.684685
64.857907	2225.392613	20.689703
64.836664	2235.432252	20.694720
64.913357	2226.160390	20.699738
65.032081	2230.083746	20.704755
65.114400	2222.171267	20.709773
65.173746	2216.386418	20.714791
64.703924	2214.708451	20.719808
65.107626	2226.234288	20.724826
65.515944	2249.692485	20.729843
65.364126	2250.912456	20.734861
65.289011	2245.574733	20.739879
65.321744	2248.769891	20.744896
65.487755	2243.407015	20.749914
65.583248	2250.401708	20.754931
65.317057	2252.078292	20.759949
65.830019	2244.732702	20.764967
65.113664	2250.472234	20.769984
65.505368	2244.527999	20.775002
65.701063	2263.162344	20.780019
66.181637	2262.026650	20.785037
66.423619	2268.673325	20.790055
66.031230	2267.522909	20.795072
66.189990	2262.555672	20.800090
66.136240	2270.277558	20.805107
66.424538	2278.343523	20.810125
66.459989	2269.261153	20.815143
66.524772	2277.611466	20.820160
66.430442	2276.288108	20.825178
66.497386	2272.193704	20.830195
66.187131	2280.129366	20.835213
66.639894	2271.133104	20.840231
66.403573	2273.133241	20.845248
66.818802	2288.545589	20.850266
67.179070	2292.468988	20.855283
67.195944	2303.869273	20.860301
67.300923	2291.465277	20.865319
67.054641	2292.438097	20.870336
67.151153	2287.562663	20.875354
67.329928	2283.823152	20.880371
67.179429	2288.173741	20.885389
67.498992	2285.226438	20.890407
67.657625	2284.150650	20.895424
67.389175	2281.576364	20.900442
67.886455	2289.360262	20.905459
67.506819	2290.701143	20.910477
67.700444	2279.277429	20.915495
67.208791	2281.491154	20.920512
67.568092	2272.601061	20.925530
67.827409	2287.119420	20.930547
67.918425	2296.229400	20.935565
68.243800	2294.486805	20.940583
68.049049	2309.960022	20.945600
68.264067	2309.620233	20.950618
68.130546	2311.648453	20.955635
67.997983	2305.562254	20.960653
68.362990	2297.876875	20.965671
68.098063	2302.362170	20.970688
68.124998	2309.885224	20.975706
68.368643	2311.071645	20.980723
68.073308	2302.628113	20.985741
68.297388	2310.669437	20.990759
68.152049	2323.723684	20.995776
68.239673	2323.372292	21.000794
68.837312	2321.754310	21.005811
68.860673	2330.013299	21.010829
69.085611	2323.729060	21.015847
69.130845	2314.105445	21.020864
69.244625	2329.845948	21.025882
69.416241	2335.724122	21.030899
69.362525	2339.955409	21.035917
69.854197	2335.238977	21.040935
69.167800	2334.472320	21.045952
69.347730	2327.784841	21.050970
69.597739	2335.699027	21.055987
69.505458	2338.825416	21.061005
69.995685	2333.578990	21.066023
69.413942	2343.245717	21.071040
69.652302	2337.691581	21.076058
69.926320	2331.791003	21.081075
69.987996	2345.930085	21.086093
70.129931	2330.159045	21.091111
69.903000	2345.432190	21.096128
69.874751	2342.122768	21.101146
70.027964	2347.830244	21.106163
70.130959	2352.649262	21.111181
70.316446	2359.645679	21.116199
70.133014	2359.743889	21.121216
70.453086	2359.425512	21.126234
70.342160	2357.088490	21.131251
70.232274	2363.146488	21.136269
70.766336	2379.894257	21.141287
70.646576	2380.904069	21.146304
70.771156	2393.000811	21.151322
70.927765	2383.366022	21.156339
70.665397	2391.063836	21.161357
71.072958	2375.872890	21.166375
70.929914	2384.546173	21.171392
71.113477	2390.902218	21.176410
71.130272	2400.323709	21.181427
71.008402	2404.483631	21.186445
71.259251	2398.539321	21.191463
71.345346	2407.233525	21.196480
71.375163	2415.620941	21.201498
71.413595	2410.410559	21.206515
71.677089	2414.446986	21.211533
71.864827	2426.776875	21.216551
72.091616	2434.966168	21.221568
71.972782	2429.846698	21.226586
72.521302	2428.375271	21.231603
72.066542	2429.030434	21.236621
72.434120	2419.422538	21.241639
72.418627	2425.443675	21.246656
72.285351	2421.203864	21.251674
72.452073	2421.487078	21.256691
72.397394	2426.573838	21.261709
72.282249	2423.909234	21.266727
72.421512	2422.034825	21.271744
72.335560	2422.761606	21.276762
72.496785	2416.720868	21.281779
72.241195	2419.623526	21.286797
72.508394	2433.351744	21.291815
72.696899	2448.853406	21.296832
72.873510	2441.756112	21.301850
72.892290	2439.083148	21.306867
72.753814	2448.664703	21.311885
72.944688	2439.333813	21.316903
72.715301	2440.275588	21.321920
73.135605	2460.102671	21.326938
73.538809	2464.110909	21.331955
73.462542	2468.765521	21.336973
73.886623	2462.658337	21.341991
73.942703	2465.546889	21.347008
73.732203	2467.404133	21.352026
74.041294	2462.122926	21.357043
73.689702	2465.921185	21.362061
74.171382	2456.415325	21.367079
73.954798	2467.659768	21.372096
74.033652	2460.271640	21.377114
74.127426	2452.328860	21.382131
74.005746	2459.954164	21.387149
73.961081	2450.357185	21.392167
74.353672	2460.202713	21.397184
74.377172	2483.576327	21.402202
74.740182	2472.425783	21.407219
74.552611	2481.863554	21.412237
74.849706	2477.704640	21.417255
74.945163	2482.856265	21.422272
74.716931	2486.827724	21.427290
75.229906	2482.713889	21.432307
75.197964	2483.369088	21.437325
75.060755	2474.379943	21.442343
75.211413	2475.158026	21.447360
74.956598	2482.273972	21.452378
75.156442	2475.955739	21.457395
75.013134	2473.393379	21.462413
75.207060	2477.415471	21.467431
75.123323	2474.992115	21.472448
75.454229	2492.567157	21.477466
75.566828	2489.942609	21.482483
75.409799	2499.432414	21.487501
75.832599	2495.894492	21.492519
75.904239	2498.660680	21.497536
75.808909	2506.597485	21.502554
75.818575	2498.424842	21.507571
75.737137	2503.159176	21.512589
76.241309	2521.145800	21.517607
76.157129	2529.655282	21.522624
76.143677	2525.393517	21.527642
76.365055	2528.597043	21.532659
75.964717	2534.539642	21.537677
76.025951	2531.396064	21.542695
76.314561	2541.434670	21.547712
76.433880	2547.816617	21.552730
76.634565	2546.658479	21.557747
76.832402	2552.482117	21.562765
76.586051	2542.452738	21.567783
77.161332	2540.926612	21.572800
76.996608	2546.990107	21.577818
77.121291	2546.920112	21.582835
77.232384	2550.516498	21.587853
77.428557	2566.509414	21.592871
77.504536	2567.011995	21.597888
77.615881	2572.883909	21.602906
77.915354	2567.184414	21.607923
77.397543	2569.717883	21.612941
77.428098	2565.726953	21.617959
77.714416	2569.450540	21.622976
77.945917	2559.680834	21.627994
78.242302	2559.517660	21.633011
77.970785	2563.903056	21.638029
78.014172	2568.024500	21.643047
78.302220	2558.457396	21.648064
77.946317	2556.966694	21.653082
77.994651	2562.738013	21.658099
78.197489	2559.202978	21.663117
78.125827	2557.210108	21.668135
78.591304	2565.595617	21.673152
78.539446	2576.366151	21.678170
78.772961	2575.180774	21.683187
78.898493	2584.746288	21.688205
78.777202	2581.110537	21.693223
78.985302	2574.749946	21.698240
78.818268	2587.141841	21.703258
78.932551	2582.007897	21.708275
78.849276	2582.933101	21.713293
78.978508	2584.241618	21.718311
78.858927	2578.898138	21.723328
78.923698	2592.838093	21.728346
79.604656	2583.695460	21.733363
79.507642	2597.559770	21.738381
79.620431	2610.592720	21.743399
79.683745	2597.093552	21.748416
79.666883	2595.376143	21.753434
79.652371	2596.442068	21.758451
79.960940	2599.278459	21.763469
79.804606	2594.758169	21.768487
80.294960	2612.611337	21.773504
80.222187	2626.733830	21.778522
80.672584	2612.489125	21.783539
80.520904	2621.318526	21.788557
80.295269	2628.420489	21.793575
80.307235	2618.640960	21.798592
80.524859	2625.301053	21.803610
80.153997	2622.723825	21.808627
80.572333	2628.348824	21.813645
80.747409	2615.785284	21.818663
80.874347	2621.683176	21.823680
80.883070	2631.431133	21.828698
80.840045	2638.217283	21.833715
81.071206	2638.326286	21.838733
80.992788	2647.276778	21.843751
81.067074	2644.756050	21.848768
81.240584	2644.302825	21.853786
81.039731	2642.027197	21.858803
81.087418	2647.596651	21.863821
81.335181	2661.318621	21.868839
81.425130	2660.603903	21.873856
81.531034	2662.398971	21.878874
81.559928	2657.243666	21.883891
81.605559	2670.987844	21.888909
81.820862	2680.154295	21.893927
81.961430	2682.950742	21.898944
82.259019	2685.738370	21.903962
82.380438	2684.933505	21.908979
82.310978	2685.373659	21.913997
82.500522	2687.487020	21.919015
83.023261	2684.836060	21.924032
82.751127	2695.145662	21.929050
82.766713	2684.753238	21.934067
82.701316	2677.494930	21.939085
82.643255	2686.347569	21.944103
82.927804	2677.592078	21.949120
82.837691	2692.831457	21.954138
82.585654	2697.576789	21.959155
83.204038	2699.452533	21.964173
83.192316	2713.963204	21.969191
83.499532	2707.119928	21.974208
82.919816	2711.152815	21.979226
82.965889	2708.835335	21.984243
83.292141	2710.308676	21.989261
83.314220	2720.493294	21.994279
83.465471	2731.213162	21.999296
83.415978	2737.252355	22.004314
83.422297	2727.438934	22.009331
83.906350	2721.786221	22.014349
83.698966	2734.276066	22.019367
84.238378	2749.805071	22.024384
84.099334	2757.300663	22.029402
83.821631	2750.526917	22.034419
84.121316	2754.043299	22.039437
84.276831	2755.167811	22.044455
84.502852	2752.096218	22.049472
84.460537	2751.474810	22.054490
84.616692	2761.581634	22.059507
85.104527	2768.679182	22.064525
84.635705	2772.814642	22.069543
85.264559	2765.520121	22.074560
85.216541	2769.678026	22.079578
84.967007	2760.220287	22.084595
85.399979	2762.033558	22.089613
85.205375	2759.008927	22.094631
85.549322	2762.082826	22.099648
85.119618	2761.515798	22.104666
85.415910	2764.341515	22.109683
85.667456	2761.957120	22.114701
85.716212	2773.087590	22.119719
86.227396	2784.798943	22.124736
86.148449	2780.481100	22.129754
86.229255	2771.763797	22.134771
86.117671	2760.892581	22.139789
85.985215	2770.814228	22.144807
86.298664	2776.310523	22.149824
86.236557	2782.777789	22.154842
86.023259	2780.156915	22.159859
86.502455	2774.183018	22.164877
85.879872	2774.148037	22.169895
86.686299	2782.404484	22.174912
86.503103	2795.682779	22.179930
86.772931	2805.049058	22.184947
86.690802	2810.515810	22.189965
86.566599	2807.350738	22.194983
86.704339	2809.399638	22.200000
86.998074	2817.341905	22.205018
87.250668	2822.699409	22.210035
87.338505	2819.374868	22.215053
87.168239	2823.466721	22.220071
87.579172	2818.702847	22.225088
87.321619	2828.697780	22.230106
87.352704	2831.132664	22.235123
87.746930	2834.773121	22.240141
87.713234	2848.122716	22.245159
87.845005	2849.497136	22.250176
87.507392	2847.946733	22.255194
87.551372	2841.908441	22.260211
87.904751	2857.122662	22.265229
88.173718	2872.066066	22.270247
88.178165	2864.711523	22.275264
88.616759	2871.971479	22.280282
88.604919	2871.326356	22.285299
88.911216	2869.971749	22.290317
88.690570	2871.350885	22.295335
88.969468	2865.364153	22.300352
88.945540	2864.522085	22.305370
88.710653	2862.744123	22.310387
89.164533	2874.922158	22.315405
89.128194	2879.876770	22.320423
89.540930	2877.287203	22.325440
89.620661	2879.701847	22.330458
89.704261	2876.302211	22.335475
90.224880	2872.158687	22.340493
90.075292	2858.405467	22.345511
90.110911	2842.366580	22.350528
89.667651	2842.170945	22.355546
89.570952	2843.637969	22.360563
90.159725	2843.640448	22.365581
90.220016	2863.129860	22.370599
90.178023	2868.060105	22.375616
90.651302	2861.970329	22.380634
90.109041	2871.646931	22.385651
90.631633	2867.619877	22.390669
90.374683	2861.221579	22.395687
90.431735	2871.583861	22.400704
90.420850	2868.599863	22.405722
90.240946	2871.651700	22.410739
90.465276	2869.625046	22.415757
90.332596	2888.967973	22.420775
90.722198	2888.613446	22.425792
90.676910	2897.782961	22.430810
90.585803	2897.686806	22.435827
91.182833	2906.619978	22.440845
91.185557	2914.898249	22.445863
91.407439	2918.840313	22.450880
91.719298	2922.190699	22.455898
91.594515	2930.012370	22.460915
91.589397	2913.143415	22.465933
91.817473	2934.411952	22.470951
92.089887	2944.181891	22.475968
92.551540	2946.814452	22.480986
92.223324	2951.467632	22.486003
92.521689	2937.981882	22.491021
92.399809	2939.569638	22.496039
92.381654	2940.222694	22.501056
92.569279	2942.131234	22.506074
92.219527	2937.050953	22.511091
92.396598	2927.144391	22.516109
92.310447	2927.823881	22.521127
92.741818	2948.265226	22.526144
92.895672	2951.015447	22.531162
92.811418	2956.451015	22.536179
93.113909	2961.440939	22.541197
93.150482	2964.231630	22.546215
93.216428	2952.530812	22.551232
93.439936	2957.072305	22.556250
93.345727	2961.893977	22.561267
93.829054	2959.239685	22.566285
93.500088	2969.662501	22.571303
93.527374	2974.995382	22.576320
93.831829	2966.224009	22.581338
93.685545	2969.371592	22.586355
94.007514	2969.185470	22.591373
93.514806	2978.504029	22.596391
94.203818	2989.486982	22.601408
94.601682	2993.360460	22.606426
94.731385	2992.680532	22.611443
95.033765	2987.207697	22.616461
94.829109	2992.936728	22.621479
94.954553	2993.504164	22.626496
94.989809	2988.884321	22.631514
94.733170	2985.698935	22.636531
94.961172	2976.339858	22.641549
95.020799	2975.781376	22.646567
94.989795	2982.890859	22.651584
95.246888	2985.044172	22.656602
94.907984	2992.034620	22.661619
95.169579	3002.286026	22.666637
95.082954	3009.255893	22.671655
95.274789	3013.224779	22.676672
95.769907	3005.812242	22.681690
95.748571	3013.895488	22.686707
95.671552	3018.326270	22.691725
95.946243	3029.112195	22.696743
96.106566	3034.108631	22.701760
96.394440	3031.355545	22.706778
96.551224	3030.605093	22.711795
96.770030	3023.179027	22.716813
96.679706	3025.143747	22.721831
96.577783	3029.142878	22.726848
96.768375	3016.147385	22.731866
96.437179	3027.384883	22.736883
96.441321	3029.407396	22.741901
96.614081	3036.254574	22.746919
96.921106	3053.139544	22.751936
97.158983	3051.827206	22.756954
97.137290	3053.140467	22.761971
97.479757	3046.174761	22.766989
96.985662	3057.822856	22.772007
97.339867	3062.230276	22.777024
97.499001	3067.896023	22.782042
97.886349	3071.651231	22.787059
97.654104	3065.422580	22.792077
97.959887	3073.034828	22.797095
97.423024	3076.148936	22.802112
97.814194	3079.101869	22.807130
98.123016	3098.808251	22.812147
98.043076	3095.184855	22.817165
98.138068	3104.496621	22.822183
98.218438	3095.378390	22.827200
98.773029	3109.068414	22.832218
98.502527	3112.860414	22.837235
98.768877	3118.742940	22.842253
98.940168	3114.849776	22.847271
99.130723	3113.904656	22.852288
99.374897	3104.707102	22.857306
99.276562	3114.140692	22.862323
99.469216	3114.770195	22.867341
99.188004	3113.687520	22.872359
99.381590	3118.438896	22.877376
99.891165	3124.248600	22.882394
99.553052	3130.282642	22.887411
99.592187	3141.850407	22.892429
99.640043	3138.541539	22.897447
99.615186	3149.175624	22.902464
100.011512	3129.639688	22.907482
99.821156	3145.239182	22.912499
100.260768	3156.504341	22.917517
100.235493	3160.276869	22.922535
100.228101	3163.775161	22.927552
100.626699	3149.531837	22.932570
100.383420	3152.962928	22.937587
100.502553	3166.588657	22.942605
100.847808	3170.950163	22.947623
101.026699	3183.502895	22.952640
101.048577	3172.714675	22.957658
100.892849	3178.919002	22.962675
100.985777	3189.155910	22.967693
101.235768	3196.335079	22.972711
101.222422	3213.238829	22.977728
101.654801	3202.843932	22.982746
101.499771	3203.161787	22.987763
101.593188	3201.303950	22.992781
101.886263	3209.117089	22.997799
101.299055	3224.175984	23.002816
101.825811	3221.076134	23.007834
102.011492	3232.450561	23.012851
102.085448	3232.527386	23.017869
102.405394	3229.573560	23.022887
102.365100	3241.150675	23.027904
102.723141	3243.250329	23.032922
102.876309	3253.162212	23.037939
102.626569	3254.757402	23.042957
102.849855	3249.931284	23.047975
102.767779	3255.492850	23.052992
103.469925	3250.534898	23.058010
102.978623	3252.931743	23.063027
103.317564	3252.825022	23.068045
103.515237	3239.364293	23.073063
103.410192	3249.171440	23.078080
103.580607	3267.349978	23.083098
103.468329	3275.374995	23.088115
103.493830	3279.789779	23.093133
103.634599	3271.315340	23.098151
103.732538	3287.352695	23.103168
103.951093	3284.294807	23.108186
104.326493	3297.646924	23.113203
104.505719	3299.702006	23.118221
104.490449	3290.734380	23.123239
104.291331	3298.836137	23.128256
104.586003	3297.477009	23.133274
104.549430	3299.259744	23.138291
104.722786	3305.144276	23.143309
104.930512	3317.973490	23.148327
105.062278	3314.676694	23.153344
105.292838	3319.251893	23.158362
105.224116	3307.297350	23.163379
105.096177	3309.226962	23.168397
105.393694	3300.472295	23.173415
105.445992	3315.219607	23.178432
105.913282	3316.692998	23.183450
105.558426	3335.026491	23.188467
105.811768	3342.785945	23.193485
106.098611	3335.282811	23.198503
106.170052	3345.097079	23.203520
106.254142	3328.759791	23.208538
106.176087	3331.192903	23.213555
105.960472	3350.050629	23.218573
106.589940	3345.943602	23.223591
106.415328	3359.119965	23.228608
106.486374	3360.532344	23.233626
106.624712	3353.074563	23.238643
106.868469	3363.758222	23.243661
107.081569	3377.388326	23.248679
106.742029	3388.816731	23.253696
107.487185	3377.403760	23.258714
107.624088	3374.740557	23.263731
107.383301	3375.523196	23.268749
107.657538	3377.629683	23.273767
107.574944	3390.422370	23.278784
107.857865	3399.319781	23.283802
108.054007	3395.129131	23.288819
107.936727	3401.823044	23.293837
107.811335	3408.489824	23.298855
107.955732	3405.165783	23.303872
108.083059	3408.185358	23.308890
108.195396	3425.151678	23.313907
108.018366	3427.767592	23.318925
108.565032	3415.672377	23.323943
108.623392	3422.360875	23.328960
109.121788	3439.462415	23.333978
109.094593	3446.432608	23.338995
109.243205	3453.706669	23.344013
109.398858	3439.204491	23.349031
109.105048	3450.458487	23.354048
109.111484	3444.258593	23.359066
109.334586	3439.173640	23.364083
109.050107	3442.882679	23.369101
109.596834	3443.286284	23.374119
109.972153	3463.238306	23.379136
110.249225	3458.185924	23.384154
110.639556	3461.798714	23.389171
110.424525	3464.512119	23.394189
110.357710	3457.717691	23.399207
110.294251	3457.039602	23.404224
110.716182	3452.188622	23.409242
110.886019	3459.563518	23.414259
110.706191	3462.852162	23.419277
110.969725	3461.359024	23.424295
111.018387	3457.084152	23.429312
110.642424	3454.113065	23.434330
110.943539	3462.338527	23.439347
111.030354	3468.135670	23.444365
111.173922	3473.100134	23.449383
111.171610	3476.272594	23.454400
111.020997	3479.499851	23.459418
111.447146	3488.665246	23.464435
111.614513	3504.616166	23.469453
111.744321	3517.217852	23.474471
111.624803	3504.863974	23.479488
111.843053	3515.046714	23.484506
112.230522	3522.040348	23.489523
112.372466	3528.971449	23.494541
112.365402	3521.122905	23.499559
112.180780	3533.997960	23.504576
112.483401	3527.243472	23.509594
112.697592	3541.056594	23.514611
112.417464	3558.504314	23.519629
112.997599	3552.189252	23.524647
112.786667	3548.624162	23.529664
112.947322	3562.821287	23.534682
113.110679	3565.412299	23.539699
113.426974	3570.012006	23.544717
113.794894	3566.293100	23.549735
113.992734	3573.897221	23.554752
113.482226	3579.800606	23.559770
114.423932	3586.278178	23.564787
114.223974	3591.978255	23.569805
114.748356	3592.843028	23.574823
114.176241	3592.815914	23.579840
114.489439	3593.136170	23.584858
114.925299	3582.895170	23.589875
114.556933	3592.721663	23.594893
114.774027	3585.554453	23.599911
114.999222	3588.268345	23.604928
114.884666	3588.223203	23.609946
115.235264	3584.301847	23.614963
115.022556	3607.587673	23.619981
115.099033	3595.793256	23.624999
115.624532	3608.967430	23.630016
115.420294	3611.464537	23.635034
115.556373	3613.027719	23.640051
115.748474	3615.437483	23.645069
116.026303	3624.708248	23.650087
115.976519	3630.886662	23.655104
116.048730	3630.616569	23.660122
116.452760	3629.521196	23.665139
116.582838	3635.175893	23.670157
116.695039	3626.980362	23.675175
116.731413	3621.627919	23.680192
116.600362	3626.988956	23.685210
117.002764	3619.101470	23.690227
116.585801	3620.707108	23.695245
116.908602	3618.292500	23.700263
116.905608	3635.015114	23.705280
117.240059	3640.303226	23.710298
117.378079	3635.635555	23.715315
116.943125	3642.218354	23.720333
117.488216	3646.794861	23.725351
117.331555	3648.637476	23.730368
117.397970	3660.816780	23.735386
117.811093	3663.135109	23.740403
117.415121	3659.958806	23.745421
117.988202	3672.914100	23.750439
118.217408	3689.638262	23.755456
118.336261	3695.080107	23.760474
118.209111	3692.208878	23.765491
118.298426	3694.723132	23.770509
118.406204	3711.412681	23.775527
118.859988	3724.351982	23.780544
119.185479	3725.118513	23.785562
119.057324	3722.544130	23.790579
118.759522	3724.648745	23.795597
119.210453	3727.046381	23.800615
119.189394	3744.406347	23.805632
119.513644	3744.876378	23.810650
119.821402	3741.340460	23.815667
119.721980	3744.588151	23.820685
119.739184	3750.636171	23.825703
119.963194	3760.865492	23.830720
119.920851	3765.843382	23.835738
120.257193	3760.305025	23.840755
120.233746	3773.031901	23.845773
120.477639	3776.210030	23.850791
120.797113	3790.297232	23.855808
120.637437	3790.896738	23.860826
121.091597	3785.775488	23.865843
120.766833	3784.923694	23.870861
120.949342	3793.912784	23.875879
121.516969	3805.183546	23.880896
121.329296	3821.149336	23.885914
121.347160	3814.972775	23.890931
121.376066	3813.011354	23.895949
121.655544	3817.077159	23.900967
122.104832	3826.624175	23.905984
121.801009	3841.828564	23.911002
122.294911	3832.493671	23.916019
122.420978	3839.124370	23.921037
122.766783	3831.987400	23.926055
122.807073	3822.439507	23.931072
122.127454	3833.605835	23.936090
122.262511	3833.373239	23.941107
122.505875	3851.297898	23.946125
122.779657	3853.716992	23.951143
123.105186	3860.619459	23.956160
123.163242	3865.146071	23.961178
123.399940	3874.167745	23.966195
123.044391	3875.435522	23.971213
123.454292	3885.932488	23.976231
124.370845	3884.655802	23.981248
123.769056	3887.044787	23.986266
123.746185	3886.218286	23.991283
124.005251	3896.476912	23.996301
123.926608	3899.857099	24.001319
124.363307	3896.960627	24.006336
124.377242	3903.346940	24.011354
124.628863	3896.638182	24.016371
124.321067	3905.028683	24.021389
124.857564	3914.647304	24.026407
125.018204	3918.630747	24.031424
124.995070	3919.186771	24.036442
125.301097	3918.488654	24.041459
125.278690	3914.597258	24.046477
125.386807	3922.919451	24.051495
125.332804	3918.499579	24.056512
125.569615	3935.639417	24.061530
125.873895	3941.645682	24.066547
125.748206	3943.540288	24.071565
125.719790	3941.616241	24.076583
125.697584	3939.886915	24.081600
125.962513	3964.723895	24.086618
126.449280	3963.479817	24.091635
126.491159	3970.000656	24.096653
126.526132	3971.087317	24.101671
126.583364	3972.132614	24.106688
126.753684	3986.053953	24.111706
127.416330	3986.931807	24.116723
127.133904	3980.922177	24.121741
127.319464	3995.582883	24.126759
127.558973	3992.363776	24.131776
127.319755	3994.661251	24.136794
127.665208	4002.359213	24.141811
127.798388	4008.240801	24.146829
127.719452	4008.998108	24.151847
128.088611	4001.784816	24.156864
128.301708	4013.761464	24.161882
128.131955	4002.854422	24.166899
128.246800	4023.595932	24.171917
128.446458	4030.161514	24.176935
128.589437	4026.282060	24.181952
128.741361	4038.296715	24.186970
128.730128	4034.722337	24.191987
129.043039	4047.636596	24.197005
129.102617	4046.342653	24.202023
129.393376	4046.044627	24.207040
128.969958	4050.457334	24.212058
129.357867	4061.557560	24.217075
129.441936	4080.561635	24.222093
129.452747	4080.367439	24.227111
130.017407	4081.585756	24.232128
130.326771	4099.033177	24.237146
130.448270	4100.270421	24.242163
130.816719	4087.858636	24.247181
130.773304	4096.472941	24.252199
130.951955	4084.974681	24.257216
130.809512	4094.923869	24.262234
130.973549	4092.979124	24.267251
131.164978	4084.789912	24.272269
131.114829	4091.691353	24.277287
131.314935	4099.932932	24.282304
131.024922	4111.009984	24.287322
131.816282	4107.448734	24.292339
131.599393	4114.470997	24.297357
131.668045	4117.269467	24.302375
132.153527	4113.920268	24.307392
131.802320	4133.412391	24.312410
132.303368	4133.785296	24.317427
132.086969	4136.407478	24.322445
132.128752	4145.687084	24.327463
132.594123	4152.839206	24.332480
132.556070	4158.854986	24.337498
132.626641	4162.732651	24.342515
133.023991	4166.941045	24.347533
132.697191	4168.835618	24.352551
133.214369	4179.293854	24.357568
133.404992	4187.688466	24.362586
133.153901	4183.567701	24.367603
133.236268	4186.092582	24.372621
133.426972	4206.727726	24.377639
133.815091	4197.327153	24.382656
134.020083	4208.847521	24.387674
133.888658	4209.799288	24.392691
134.308459	4201.615279	24.397709
134.343599	4214.986664	24.402727
134.887626	4211.527271	24.407744
134.874228	4224.682162	24.412762
134.664512	4230.181957	24.417779
135.289985	4219.715197	24.422797
135.148467	4226.312207	24.427815
135.357057	4220.588558	24.432832
134.963766	4230.151004	24.437850
135.150264	4241.027226	24.442867
135.381447	4249.134592	24.447885
135.433556	4252.304974	24.452903
135.928726	4254.831478	24.457920
136.078842	4273.894849	24.462938
136.143258	4269.771982	24.467955
136.446620	4275.510207	24.472973
136.018312	4271.066823	24.477991
136.475997	4281.850082	24.483008
136.551426	4292.481752	24.488026
136.721731	4297.256027	24.493043
136.646148	4293.224528	24.498061
136.832548	4306.436557	24.503079
137.313044	4315.224558	24.508096
137.175574	4323.345522	24.513114
137.440691	4326.242658	24.518131
137.730149	4322.157120	24.523149
137.715857	4345.226579	24.528167
137.867868	4345.534226	24.533184
138.004522	4354.533936	24.538202
138.033391	4341.531266	24.543219
138.449297	4358.046881	24.548237
138.337453	4369.440228	24.553255
138.524511	4361.668226	24.558272
138.700069	4359.791089	24.563290
138.748551	4367.223246	24.568307
139.181320	4378.455523	24.573325
138.906582	4387.185117	24.578343
138.792856	4391.009636	24.583360
139.507007	4391.175557	24.588378
139.545779	4399.212128	24.593395
139.800269	4410.967917	24.598413
139.638843	4410.971148	24.603431
139.708235	4416.357831	24.608448
139.741075	4417.012420	24.613466
139.893967	4428.392737	24.618483
140.354141	4422.456007	24.623501
140.877869	4439.100000	24.628519
140.949769	4437.545271	24.633536
141.197224	4446.483478	24.638554
141.422623	4443.506393	24.643571
141.473346	4438.760656	24.648589
141.341288	4435.195658	24.653607
141.895749	4438.492541	24.658624
141.841082	4427.478833	24.663642
141.541927	4436.067079	24.668659
142.150870	4440.955747	24.673677
142.120397	4464.311972	24.678695
142.345247	4451.742518	24.683712
142.620319	4464.896580	24.688730
142.554560	4465.162592	24.693747
142.730144	4461.956575	24.698765
142.745908	4456.774406	24.703783
142.574014	4470.011122	24.708800
142.994330	4465.538904	24.713818
142.871247	4481.015374	24.718835
143.448864	4487.193639	24.723853
143.172927	4487.189559	24.728871
143.255696	4482.931197	24.733888
143.412112	4485.558151	24.738906
143.412792	4496.432073	24.743923
143.972363	4513.471390	24.748941
143.619037	4517.699621	24.753959
143.594077	4516.557774	24.758976
143.953460	4534.518595	24.763994
143.803799	4543.061376	24.769011
143.990168	4552.501614	24.774029
144.520312	4557.402658	24.779047
144.301608	4571.448524	24.784064
144.880166	4579.602623	24.789082
144.872764	4585.683185	24.794099
145.201788	4594.441394	24.799117
145.286359	4608.607069	24.804135
145.377823	4609.413460	24.809152
145.686680	4620.229707	24.814170
145.438768	4631.101621	24.819187
146.334885	4629.209422	24.824205
146.417773	4639.470819	24.829223
146.109210	4635.854522	24.834240
146.665556	4642.680095	24.839258
146.638713	4658.772936	24.844275
147.172112	4660.387598	24.849293
147.005494	4667.768351	24.854311
147.504529	4667.971135	24.859328
147.544589	4658.678513	24.864346
147.154252	4668.486931	24.869363
147.677795	4674.418057	24.874381
147.869232	4688.484984	24.879399
148.052438	4676.887785	24.884416
148.366351	4684.871908	24.889434
147.927298	4689.675465	24.894451
148.179404	4683.982732	24.899469
148.146786	4698.154210	24.904487
148.494433	4701.111077	24.909504
148.743194	4705.317626	24.914522
148.590770	4721.303936	24.919539
148.905791	4723.009633	24.924557
149.191681	4721.389790	24.929575
148.795946	4736.855532	24.934592
149.170158	4749.129389	24.939610
149.658034	4750.489201	24.944627
149.982937	4748.045710	24.949645
150.154758	4751.311060	24.954663
150.514575	4760.730547	24.959680
150.636320	4762.782177	24.964698
151.046432	4770.413521	24.969715
151.144862	4771.408219	24.974733
150.965645	4768.481845	24.979751
150.875762	4756.255043	24.984768
151.334789	4759.936249	24.989786
151.218854	4763.672810	24.994803
151.476582	4760.646418	24.999821
151.369192	4763.330524	25.004839
151.286016	4767.415482	25.009856
151.779224	4788.919284	25.014874
151.611328	4789.438039	25.019891
152.102069	4797.271406	25.024909
152.188176	4806.875840	25.029927
152.327355	4811.699317	25.034944
152.175703	4812.878396	25.039962
152.258878	4819.790792	25.044979
152.499057	4828.553563	25.049997
152.668420	4832.033955	25.055015
152.583569	4837.542779	25.060032
153.390427	4845.506565	25.065050
153.155466	4859.542573	25.070067
153.405888	4860.866995	25.075085
153.308459	4863.088703	25.080103
153.708154	4869.538027	25.085120
154.041856	4883.724861	25.090138
153.748678	4889.515703	25.095155
153.856178	4884.991381	25.100173
154.162611	4898.544881	25.105191
153.754214	4913.649756	25.110208
154.044181	4915.652954	25.115226
154.002260	4935.170080	25.120243
154.597031	4941.323719	25.125261
154.896030	4956.273615	25.130279
154.994984	4961.144469	25.135296
155.637259	4960.832397	25.140314
155.705541	4981.067781	25.145331
156.335798	4976.994996	25.150349
156.342015	4978.720687	25.155367
156.227878	4989.120470	25.160384
156.628919	4975.781266	25.165402
156.518615	4987.496725	25.170419
156.917783	4991.806040	25.175437
157.283451	5000.243050	25.180455
157.319646	4990.130163	25.185472
157.339382	4997.964806	25.190490
157.051576	5006.046495	25.195507
157.605664	4992.430777	25.200525
157.667979	4997.657758	25.205543
157.417827	5009.770770	25.210560
157.805097	5013.927282	25.215578
157.660634	5024.028808	25.220595
158.417908	5034.112177	25.225613
158.429419	5039.792203	25.230631
158.306968	5052.276649	25.235648
158.314059	5042.843796	25.240666
158.661443	5058.982529	25.245683
159.030506	5061.491027	25.250701
158.992755	5072.453385	25.255719
158.723641	5073.300504	25.260736
159.300967	5086.571807	25.265754
159.238767	5081.417458	25.270771
160.019233	5093.034471	25.275789
159.948625	5100.633943	25.280807
159.918122	5111.213244	25.285824
160.382090	5104.413959	25.290842
160.206464	5115.461073	25.295859
160.406841	5127.285779	25.300877
160.860762	5126.255108	25.305895
161.115715	5136.717103	25.310912
161.019338	5133.405216	25.315930
161.031488	5147.431141	25.320947
161.193110	5158.280245	25.325965
161.521684	5158.370853	25.330983
161.772406	5164.679479	25.336000
162.147086	5164.734455	25.341018
161.820129	5186.089437	25.346035
161.945118	5181.669626	25.351053
162.100112	5186.317114	25.356071
162.331993	5202.290989	25.361088
162.454775	5203.569145	25.366106
162.938591	5218.891189	25.371123
163.027666	5217.437870	25.376141
163.600500	5226.887360	25.381159
163.312880	5232.440696	25.386176
163.630111	5230.203521	25.391194
163.833243	5225.190646	25.396211
164.271471	5226.050065	25.401229
163.939711	5226.850186	25.406247
164.227778	5235.463606	25.411264
164.634513	5244.560336	25.416282
164.566141	5250.249785	25.421299
164.615400	5249.512933	25.426317
164.693107	5256.893527	25.431335
164.508682	5253.664856	25.436352
164.770001	5265.517984	25.441370
164.789875	5276.929143	25.446387
164.539035	5276.712792	25.451405
165.111225	5293.236343	25.456423
165.002188	5298.130402	25.461440
165.422754	5311.862040	25.466458
165.759846	5322.519610	25.471475
165.709836	5344.951984	25.476493
166.099309	5349.654322	25.481511
166.087482	5357.314138	25.486528
166.674038	5354.738035	25.491546
166.468176	5365.291293	25.496563
166.690778	5384.009874	25.501581
167.183889	5394.024347	25.506599
167.173282	5398.388485	25.511616
167.877406	5405.134379	25.516634
167.991825	5412.023165	25.521651
168.257679	5422.729834	25.526669
168.455623	5414.845197	25.531687
168.314255	5427.935777	25.536704
168.593353	5419.214548	25.541722
168.758104	5415.479750	25.546739
168.629862	5428.410444	25.551757
169.043101	5427.297745	25.556775
169.089428	5440.554640	25.561792
169.377028	5433.864936	25.566810
170.055755	5442.016362	25.571827
170.202715	5449.913340	25.576845
170.411578	5453.984266	25.581863
170.082329	5455.301689	25.586880
170.375476	5449.498121	25.591898
170.413950	5451.512369	25.596915
170.457010	5453.551152	25.601933
170.568580	5452.454145	25.606951
170.509909	5473.385483	25.611968
170.944154	5486.518507	25.616986
170.935297	5485.241497	25.622003
171.317357	5497.735596	25.627021
171.632271	5508.497762	25.632039
171.848496	5504.906400	25.637056
171.678704	5513.032957	25.642074
171.839053	5525.593375	25.647091
171.895378	5531.045568	25.652109
172.336917	5531.307880	25.657127
172.168762	5546.852292	25.662144
172.420622	5557.968439	25.667162
172.484971	5568.119626	25.672180
173.030937	5585.594544	25.677197
172.972428	5592.725142	25.682215
172.928681	5600.702568	25.687232
173.268796	5603.632355	25.692250
173.523081	5612.469055	25.697268
173.281533	5619.524169	25.702285
174.001311	5631.365689	25.707303
174.338790	5639.356012	25.712320
174.450628	5646.068518	25.717338
174.554484	5653.773468	25.722356
174.795407	5667.094742	25.727373
174.917037	5666.842132	25.732391
175.007724	5666.666972	25.737408
174.978629	5659.455444	25.742426
175.045364	5677.239120	25.747444
175.338677	5685.447878	25.752461
175.705361	5683.370206	25.757479
175.617131	5694.975335	25.762496
176.185196	5705.057155	25.767514
176.290560	5713.383758	25.772532
176.119107	5717.981510	25.777549
176.455748	5719.955391	25.782567
176.929559	5736.753604	25.787584
176.893306	5737.441162	25.792602
176.906131	5740.924156	25.797620
177.018580	5748.555196	25.802637
177.436543	5750.008115	25.807655
177.408346	5752.335882	25.812672
177.611739	5773.138121	25.817690
178.037107	5773.901726	25.822708
177.803667	5781.413350	25.827725
178.303221	5797.421573	25.832743
178.411917	5808.711822	25.837760
178.856387	5803.569437	25.842778
179.203487	5814.364622	25.847796
179.181990	5825.321729	25.852813
179.386121	5823.263193	25.857831
179.457826	5831.752957	25.862848
179.591321	5840.286708	25.867866
179.845325	5846.708698	25.872884
179.706808	5856.863416	25.877901
180.051546	5862.333660	25.882919
180.080745	5875.416779	25.887936
180.375543	5881.526191	25.892954
180.904082	5885.136763	25.897972
181.000708	5894.904272	25.902989
180.997329	5897.856352	25.908007
181.349269	5897.697083	25.913024
181.319217	5916.351620	25.918042
181.716779	5915.635937	25.923060
182.040221	5918.574702	25.928077
182.201936	5917.084694	25.933095
182.418962	5933.089948	25.938112
182.690538	5940.307865	25.943130
182.953860	5942.646808	25.948148
182.856025	5942.655858	25.953165
182.949679	5945.750580	25.958183
183.363460	5955.594704	25.963200
183.555978	5966.291084	25.968218
183.339325	5968.234873	25.973236
183.440156	5964.888783	25.978253
183.691046	5980.115378	25.983271
184.164875	5984.507936	25.988288
184.085726	5982.436941	25.993306
184.076926	6000.081242	25.998324
184.310994	6021.361936	26.003341
184.474789	6016.358164	26.008359
184.569877	6041.609711	26.013376
184.626045	6042.251234	26.018394
184.896090	6061.307161	26.023412
184.849117	6068.887548	26.028429
185.540393	6080.285573	26.033447
185.706791	6092.321416	26.038464
185.411725	6095.161387	26.043482
186.310379	6105.040117	26.048500
186.113165	6118.790228	26.053517
186.493129	6118.213035	26.058535
186.523575	6138.001059	26.063552
186.796740	6142.267254	26.068570
187.071919	6141.223495	26.073588
187.070498	6161.007066	26.078605
187.662854	6150.809567	26.083623
187.610494	6163.814124	26.088640
187.652215	6168.754246	26.093658
188.482586	6180.897632	26.098676
188.479920	6186.274031	26.103693
188.514646	6184.456653	26.108711
188.886686	6178.987740	26.113728
188.840275	6182.233871	26.118746
189.013371	6194.568624	26.123764
188.852591	6209.667341	26.128781
189.526707	6212.207131	26.133799
189.940627	6211.536227	26.138816
189.773038	6210.946952	26.143834
189.730970	6224.969571	26.148852
190.036744	6232.258009	26.153869
190.308628	6240.378830	26.158887
190.629567	6248.782391	26.163904
190.511813	6250.335061	26.168922
191.030844	6243.927640	26.173940
191.239674	6257.952018	26.178957
191.385215	6274.066628	26.183975
191.550952	6280.376329	26.188992
191.464035	6284.635833	26.194010
191.764908	6285.905107	26.199028
191.551881	6297.261843	26.204045
191.914908	6312.183882	26.209063
192.311426	6321.942519	26.214080
192.066580	6334.904746	26.219098
192.585933	6343.476145	26.224116
192.823177	6354.149962	26.229133
193.135001	6362.823330	26.234151
193.711943	6373.011463	26.239168
193.804480	6378.136244	26.244186
194.435496	6371.086193	26.249204
194.105944	6369.931967	26.254221
194.252954	6394.664469	26.259239
194.567521	6396.146267	26.264256
194.822681	6407.353962	26.269274
194.745710	6403.912532	26.274292
194.780945	6416.051213	26.279309
195.129597	6413.534335	26.284327
195.584790	6418.895897	26.289344
195.235780	6425.636691	26.294362
195.773029	6441.642733	26.299380
195.613251	6440.821780	26.304397
195.809493	6455.432288	26.309415
196.292736	6460.738959	26.314432
196.252609	6466.812647	26.319450
196.652631	6485.409859	26.324468
196.954399	6499.022105	26.329485
197.150662	6499.048218	26.334503
197.543466	6510.054475	26.339520
197.333436	6531.231710	26.344538
197.269683	6533.009547	26.349556
197.661776	6547.147493	26.354573
198.047424	6551.077326	26.359591
197.791859	6557.014326	26.364608
198.301391	6585.901483	26.369626
198.405451	6575.900204	26.374644
198.514081	6592.693280	26.379661
199.227150	6605.739237	26.384679
199.021347	6604.556139	26.389696
198.955368	6624.473439	26.394714
199.082403	6631.411219	26.399732
200.000415	6647.837630	26.404749
200.037166	6649.460834	26.409767
200.243921	6653.964845	26.414784
200.288315	6668.965504	26.419802
200.808117	6673.688810	26.424820
201.338706	6677.163478	26.429837
201.184288	6683.794961	26.434855
201.280115	6672.721595	26.439872
201.351122	6690.540312	26.444890
201.478290	6699.353257	26.449908
201.715727	6696.828510	26.454925
202.055343	6703.423644	26.459943
202.544573	6710.049009	26.464960
202.222751	6727.632558	26.469978
202.362217	6725.539858	26.474996
202.937011	6742.219004	26.480013
203.022424	6752.831604	26.485031
203.193890	6743.425790	26.490048
203.165704	6763.905553	26.495066
203.728380	6768.890500	26.500084
203.889365	6772.318911	26.505101
203.557877	6783.988092	26.510119
203.838561	6795.725535	26.515136
203.980370	6811.623380	26.520154
204.537243	6824.368808	26.525172
204.788246	6837.073769	26.530189
204.859008	6845.115876	26.535207
205.109064	6853.511879	26.540224
205.381038	6868.770638	26.545242
205.599534	6876.969557	26.550260
205.774583	6882.223613	26.555277
206.025579	6897.940271	26.560295
206.401462	6900.470058	26.565312
206.200224	6906.398659	26.570330
206.839676	6911.223245	26.575348
207.082473	6930.290659	26.580365
207.139052	6927.557448	26.585383
207.631234	6928.304326	26.590400
207.382960	6933.754145	26.595418
207.834921	6940.931573	26.600436
208.202841	6952.548116	26.605453
208.567397	6955.707906	26.610471
208.881098	6961.107578	26.615488
208.920216	6972.759859	26.620506
209.154586	6968.044678	26.625524
209.411275	6981.370755	26.630541
209.392662	6988.050523	26.635559
210.112351	6979.167985	26.640576
209.767951	6990.542571	26.645594
209.822112	6986.228129	26.650612
210.219121	6994.866355	26.655629
210.367286	7004.051828	26.660647
210.494811	7007.671782	26.665664
210.115220	7027.818592	26.670682
210.652382	7037.877583	26.675700
210.829543	7056.671290	26.680717
211.049992	7066.325319	26.685735
211.425548	7067.390380	26.690752
211.718997	7086.993009	26.695770
212.215877	7088.850389	26.700788
212.022650	7096.072127	26.705805
212.243114	7113.615288	26.710823
212.822993	7112.697373	26.715840
212.315319	7123.314705	26.720858
212.563520	7136.724304	26.725876
213.228736	7144.398766	26.730893
213.048378	7166.310800	26.735911
213.549754	7172.233596	26.740928
213.759163	7179.802691	26.745946
213.968862	7184.865147	26.750964
214.221085	7194.514266	26.755981
214.578502	7213.257797	26.760999
214.742280	7212.831247	26.766016
214.777351	7215.038795	26.771034
214.873825	7226.429698	26.776052
215.115209	7237.864202	26.781069
215.213449	7248.077306	26.786087
215.569749	7254.297509	26.791104
215.989606	7264.753834	26.796122
215.531909	7261.826484	26.801140
215.799505	7280.735687	26.806157
216.486264	7300.753628	26.811175
216.680305	7302.911028	26.816192
216.732992	7325.080338	26.821210
216.971041	7321.797744	26.826228
217.537017	7341.869378	26.831245
217.666045	7349.978345	26.836263
217.832319	7359.325320	26.841280
218.305220	7364.463401	26.846298
218.446581	7366.092379	26.851316
218.975467	7377.349340	26.856333
218.890893	7381.390900	26.861351
219.220875	7384.641418	26.866368
219.493243	7392.093401	26.871386
219.442537	7400.277902	26.876404
219.981619	7405.696067	26.881421
219.855863	7400.112203	26.886439
220.126627	7408.419980	26.891456
220.637883	7423.499652	26.896474
220.710129	7424.523855	26.901492
221.156587	7426.726965	26.906509
220.813203	7448.008224	26.911527
221.284072	7446.955838	26.916544
221.517120	7458.606459	26.921562
221.463319	7465.064611	26.926580
221.948099	7477.269320	26.931597
222.031982	7492.242365	26.936615
222.389874	7504.290179	26.941632
222.636984	7498.729955	26.946650
222.675630	7503.844552	26.951668
223.193915	7511.299100	26.956685
223.370082	7521.834788	26.961703
223.585745	7537.027157	26.966720
223.530780	7552.230363	26.971738
223.752065	7563.665062	26.976756
224.307765	7561.115596	26.981773
224.329499	7572.673114	26.986791
224.611134	7573.370924	26.991808
224.817901	7593.950555	26.996826
224.804105	7602.975437	27.001844
225.238713	7618.199870	27.006861
225.253692	7629.360700	27.011879
225.764738	7629.271208	27.016896
226.032596	7646.403358	27.021914
226.065014	7659.698764	27.026932
226.501288	7663.254696	27.031949
226.557345	7678.690017	27.036967
226.263114	7680.374633	27.041984
227.163352	7694.534887	27.047002
227.036663	7716.050854	27.052020
227.215027	7727.549205	27.057037
227.166010	7737.700410	27.062055
228.100136	7755.119757	27.067072
227.869446	7770.060225	27.072090
228.090826	7778.322236	27.077108
228.733814	7784.778684	27.082125
228.679591	7802.987467	27.087143
229.186573	7807.406847	27.092160
229.543580	7810.984697	27.097178
229.555750	7817.495779	27.102196
229.624523	7813.276722	27.107213
229.795459	7830.222176	27.112231
230.108053	7830.848849	27.117248
230.333023	7841.774861	27.122266
230.390600	7859.521045	27.127284
230.920901	7857.534315	27.132301
230.823537	7882.651218	27.137319
231.089652	7886.811589	27.142336
231.413975	7889.870505	27.147354
231.541213	7916.982248	27.152372
232.035769	7915.891399	27.157389
232.029292	7927.819776	27.162407
232.317164	7933.182741	27.167424
232.789408	7948.477322	27.172442
232.680211	7963.029538	27.177460
233.246741	7970.322021	27.182477
233.103589	7982.398126	27.187495
233.047483	7996.241184	27.192512
233.577154	8007.507881	27.197530
234.018398	8024.906828	27.202548
234.187774	8028.934003	27.207565
234.532819	8050.891063	27.212583
234.971281	8051.179162	27.217600
235.288645	8067.741990	27.222618
235.134592	8079.365247	27.227636
235.492567	8076.534138	27.232653
235.675826	8095.589988	27.237671
235.845272	8095.844461	27.242688
236.330638	8116.791452	27.247706
236.224942	8127.333757	27.252724
236.602872	8129.525590	27.257741
236.735139	8150.439535	27.262759
236.818545	8159.320021	27.267776
237.389526	8164.581877	27.272794
237.458012	8182.980179	27.277812
238.054809	8190.526890	27.282829
237.520796	8209.830976	27.287847
237.947123	8217.928481	27.292864
238.329822	8224.283791	27.297882
238.631872	8248.164180	27.302900
238.764836	8266.830291	27.307917
239.374877	8280.847033	27.312935
239.563958	8282.916928	27.317952
239.844477	8300.868551	27.322970
239.796553	8303.266029	27.327988
240.075488	8321.391561	27.333005
240.370211	8327.624933	27.338023
240.585553	8346.066692	27.343040
240.951054	8352.809910	27.348058
240.908595	8366.739506	27.353076
241.608562	8386.627121	27.358093
241.929229	8399.814762	27.363111
241.917076	8412.397866	27.368128
242.202948	8409.596945	27.373146
242.423079	8429.802874	27.378164
242.770297	8428.188894	27.383181
242.836600	8439.616843	27.388199
243.398048	8461.840420	27.393216
243.528424	8477.776223	27.398234
243.731633	8483.689327	27.403252
243.935475	8486.628304	27.408269
244.058512	8495.417500	27.413287
244.405086	8516.064658	27.418304
244.811975	8513.004821	27.423322
245.054825	8529.286121	27.428340
244.922114	8534.156332	27.433357
245.189406	8533.861925	27.438375
245.723382	8556.058347	27.443392
245.861220	8561.564972	27.448410
245.961442	8571.055510	27.453428
246.622467	8575.580390	27.458445
246.953939	8579.156077	27.463463
247.017356	8585.447871	27.468480
247.315977	8582.837514	27.473498
247.668694	8605.119219	27.478516
247.331349	8601.607664	27.483533
248.011629	8607.212443	27.488551
248.091258	8621.732439	27.493568
248.314683	8628.520115	27.498586
248.464528	8637.403052	27.503604
248.631154	8649.311091	27.508621
248.823674	8655.860516	27.513639
248.917999	8674.795136	27.518656
249.340833	8676.452754	27.523674
249.838652	8701.019739	27.528692
249.907424	8705.375384	27.533709
250.397439	8715.815232	27.538727
250.427377	8728.729776	27.543744
251.318280	8734.617319	27.548762
251.016960	8744.199262	27.553780
251.106652	8756.997121	27.558797
251.798178	8772.873688	27.563815
251.401395	8782.527435	27.568832
251.760129	8795.570479	27.573850
252.323800	8811.476580	27.578868
252.872588	8814.573105	27.583885
252.797440	8827.977760	27.588903
253.088392	8842.007031	27.593920
253.282421	8841.695681	27.598938
253.450565	8869.405438	27.603956
253.271333	8871.236319	27.608973
253.783891	8897.799771	27.613991
254.002880	8906.624647	27.619008
254.649476	8912.247426	27.624026
254.919925	8928.988866	27.629044
255.175492	8938.480515	27.634061
255.431175	8947.953207	27.639079
255.457955	8973.604655	27.644096
256.039711	8973.690364	27.649114
256.052315	8997.096120	27.654132
256.272774	9012.187920	27.659149
256.793882	9020.813976	27.664167
256.630734	9034.545131	27.669184
257.252881	9042.438677	27.674202
257.366236	9054.134315	27.679220
257.446200	9059.220769	27.684237
257.975760	9074.485206	27.689255
258.084941	9087.040289	27.694272
258.516309	9090.928781	27.699290
258.247865	9112.620123	27.704308
258.738391	9131.496302	27.709325
258.854382	9144.981747	27.714343
259.175240	9156.348161	27.719360
259.611668	9170.020222	27.724378
259.791573	9183.419909	27.729396
260.238140	9201.636863	27.734413
260.071506	9210.781188	27.739431
260.572299	9230.530422	27.744448
261.008537	9236.243085	27.749466
261.146689	9257.618320	27.754484
261.227277	9273.442631	27.759501
261.633147	9279.340029	27.764519
261.765673	9289.716227	27.769536
262.271427	9308.110294	27.774554
262.258273	9325.262763	27.779572
262.699052	9326.822912	27.784589
263.362301	9332.364280	27.789607
263.268626	9350.290292	27.794624
263.435559	9353.907693	27.799642
263.851770	9369.944722	27.804660
263.999760	9375.929908	27.809677
264.601186	9385.086608	27.814695
264.443122	9401.049446	27.819712
264.760634	9405.432593	27.824730
264.816083	9428.314383	27.829748
265.210970	9436.935149	27.834765
265.338625	9446.147152	27.839783
265.864963	9460.196849	27.844800
266.379741	9477.468826	27.849818
266.789635	9481.758587	27.854836
267.219576	9491.106383	27.859853
267.724289	9495.135023	27.864871
267.418716	9496.909980	27.869888
267.696552	9521.383065	27.874906
268.099019	9532.187553	27.879924
267.753934	9537.877467	27.884941
268.632013	9553.100334	27.889959
268.381327	9554.655157	27.894976
268.890821	9567.959288	27.899994
269.072299	9585.507748	27.905012
269.018013	9599.970553	27.910029
269.582873	9615.100456	27.915047
269.985983	9629.763165	27.920064
270.443397	9641.743112	27.925082
270.555769	9652.211075	27.930100
270.706327	9667.835320	27.935117
271.249228	9670.828723	27.940135
271.210294	9687.114137	27.945152
271.462085	9700.777625	27.950170
272.122794	9710.177789	27.955188
272.007978	9730.361828	27.960205
272.726716	9731.341720	27.965223
272.814662	9754.288282	27.970240
273.300639	9754.518454	27.975258
273.795550	9762.991095	27.980276
273.841898	9771.341407	27.985293
274.497325	9769.495908	27.990311
274.447169	9782.543710	27.995328
274.768064	9793.891567	28.000346
275.123496	9801.644093	28.005364
274.992195	9803.653840	28.010381
275.506787	9817.067860	28.015399
275.577821	9835.107462	28.020416
275.829452	9849.317310	28.025434
276.172655	9859.278782	28.030452
276.194621	9873.382543	28.035469
276.333900	9866.850247	28.040487
276.565927	9891.593058	28.045504
276.908782	9907.389454	28.050522
277.413336	9916.924693	28.055540
277.649490	9925.071685	28.060557
278.204222	9946.170910	28.065575
278.072141	9967.283026	28.070592
278.661108	9974.484386	28.075610
279.007261	9999.954609	28.080628
278.955371	10004.913579	28.085645
279.257489	10016.166634	28.090663
279.494501	10026.883663	28.095680
279.520903	10043.670653	28.100698
280.041766	10063.828094	28.105716
280.364683	10070.079741	28.110733
280.580976	10087.784249	28.115751
280.929120	10109.708532	28.120768
280.994968	10119.934611	28.125786
281.588271	10139.026208	28.130804
281.156412	10142.096605	28.135821
281.843196	10154.625077	28.140839
281.863165	10174.864261	28.145856
282.407156	10196.713763	28.150874
282.753247	10206.488681	28.155892
282.806174	10223.726348	28.160909
283.007692	10237.388634	28.165927
283.435425	10256.790458	28.170944
283.800265	10265.021636	28.175962
284.150772	10286.939443	28.180980
284.365519	10311.597110	28.185997
284.730680	10315.979325	28.191015
284.745616	10329.165713	28.196032
285.444757	10337.549790	28.201050
285.476094	10356.669650	28.206068
285.631360	10380.878894	28.211085
286.154201	10390.051561	28.216103
286.245479	10411.697534	28.221120
286.615992	10430.849590	28.226138
287.023054	10437.896493	28.231156
286.910121	10465.854735	28.236173
287.753142	10471.333557	28.241191
287.673002	10496.621795	28.246208
288.067110	10511.390807	28.251226
288.493786	10527.578757	28.256244
288.926067	10542.190254	28.261261
289.623551	10551.780851	28.266279
289.519204	10571.553684	28.271296
289.928116	10578.764541	28.276314
290.003858	10597.887164	28.281332
290.668479	10605.370568	28.286349
290.770218	10615.515515	28.291367
291.511996	10621.919603	28.296384
291.728480	10649.753895	28.301402
291.855502	10639.080597	28.306420
291.678902	10649.913296	28.311437
292.112687	10659.390538	28.316455
292.594024	10679.914795	28.321472
292.659054	10692.430514	28.326490
293.091447	10710.259637	28.331508
293.248405	10728.744482	28.336525
294.117755	10735.981157	28.341543
294.246484	10743.084407	28.346560
294.046007	10765.070141	28.351578
294.272347	10767.207103	28.356596
294.386483	10789.585637	28.361613
295.093344	10797.154071	28.366631
295.285987	10820.461289	28.371648
295.548944	10838.822282	28.376666
295.971423	10856.163678	28.381684
296.289822	10863.587750	28.386701
296.695748	10873.375748	28.391719
297.377524	10893.894103	28.396736
297.415776	10905.179556	28.401754
297.578476	10907.266510	28.406772
297.626659	10926.940043	28.411789
298.271046	10933.425805	28.416807
298.814729	10946.570850	28.421824
298.963844	10950.147148	28.426842
299.208289	10967.020798	28.431860
299.473756	10974.595296	28.436877
299.733082	10984.823116	28.441895
300.099343	11002.688138	28.446912
300.314012	11007.207765	28.451930
300.283442	11014.244501	28.456948
300.741176	11037.500992	28.461965
301.197382	11039.633554	28.466983
301.603463	11054.053788	28.472000
301.606818	11060.444239	28.477018
301.863328	11073.097570	28.482036
302.351081	11084.906344	28.487053
302.401705	11099.060220	28.492071
303.074781	11109.624309	28.497088
303.010735	11125.614938	28.502106
303.064781	11131.425949	28.507124
303.579535	11155.371482	28.512141
303.977894	11165.770235	28.517159
304.224949	11177.010514	28.522176
304.275228	11195.278868	28.527194
304.883877	11197.093913	28.532212
305.012059	11218.147723	28.537229
305.253785	11230.844525	28.542247
305.840352	11261.419396	28.547264
306.064107	11269.824685	28.552282
306.540292	11279.750299	28.557300
306.932754	11303.026818	28.562317
307.198869	11308.258396	28.567335
307.468270	11323.824361	28.572352
307.744927	11347.567458	28.577370
308.030572	11354.406380	28.582388
307.874258	11372.792526	28.587405
308.569582	11384.916315	28.592423
308.947341	11405.931240	28.597440
309.186156	11416.756145	28.602458
309.245757	11430.937284	28.607476
309.542036	11454.822694	28.612493
310.218579	11468.348316	28.617511
310.442057	11491.872575	28.622528
310.611205	11510.192084	28.627546
310.672085	11518.177770	28.632564
311.370426	11542.694995	28.637581
311.608543	11560.485894	28.642599
312.242045	11577.706489	28.647616
312.074197	11595.611536	28.652634
312.517536	11593.353861	28.657652
312.550900	11620.416232	28.662669
312.970611	11639.302891	28.667687
313.636998	11657.756219	28.672704
313.706798	11689.641075	28.677722
314.378573	11700.319381	28.682740
314.552730	11719.544566	28.687757
314.834601	11726.245277	28.692775
315.049728	11751.927874	28.697792
315.321232	11769.732686	28.702810
315.869348	11775.608600	28.707828
316.011016	11802.666899	28.712845
316.208381	11815.077379	28.717863
317.049963	11826.048086	28.722880
316.980722	11844.929444	28.727898
318.051491	11860.496634	28.732916
317.702050	11869.367748	28.737933
318.073458	11874.226170	28.742951
318.539032	11891.950176	28.747968
318.586817	11904.728337	28.752986
319.426240	11919.611856	28.758004
319.110836	11933.391088	28.763021
319.977040	11948.867244	28.768039
320.315969	11956.837981	28.773056
320.516790	11981.607390	28.778074
320.746393	11990.978354	28.783092
320.722421	12009.429649	28.788109
321.072394	12021.854253	28.793127
321.478464	12032.744889	28.798144
321.675512	12043.658800	28.803162
322.160152	12067.149185	28.808180
322.447406	12080.016264	28.813197
322.413281	12100.363889	28.818215
322.985157	12106.706692	28.823232
323.245355	12130.023901	28.828250
323.723436	12134.319389	28.833268
323.663798	12143.407330	28.838285
324.043201	12169.971041	28.843303
324.432504	12176.522460	28.848320
324.534813	12200.334996	28.853338
325.103310	12217.942138	28.858356
324.967542	12250.434860	28.863373
325.448907	12268.933562	28.868391
325.565211	12294.935526	28.873408
325.811446	12322.641327	28.878426
326.407619	12339.915838	28.883444
326.987978	12369.770353	28.888461
327.096984	12385.757049	28.893479
327.617784	12410.587422	28.898496
327.643246	12433.768098	28.903514
328.285371	12458.254275	28.908532
328.963309	12467.627878	28.913549
329.536879	12480.895634	28.918567
329.613237	12490.688738	28.923584
329.983608	12505.589356	28.928602
330.683592	12524.609841	28.933620
330.769617	12539.469765	28.938637
331.231497	12558.009698	28.943655
331.436343	12563.623849	28.948672
331.758115	12575.124835	28.953690
332.039287	12592.480500	28.958708
332.400391	12618.646666	28.963725
332.616622	12628.891607	28.968743
333.016380	12650.529732	28.973760
333.392778	12675.222024	28.978778
333.368347	12682.817362	28.983796
333.877454	12706.664708	28.988813
333.815982	12730.118309	28.993831
334.658748	12734.170497	28.998848
334.797484	12764.341128	29.003866
335.378052	12786.980551	29.008884
335.847339	12796.510160	29.013901
335.940396	12814.435492	29.018919
336.799234	12815.260992	29.023936
337.228300	12841.448400	29.028954
337.497886	12844.532508	29.033972
337.782948	12847.276300	29.038989
337.932463	12864.668628	29.044007
338.631814	12870.672778	29.049024
338.536087	12888.782488	29.054042
338.944522	12906.579559	29.059060
339.451724	12916.501184	29.064077
339.556229	12930.158522	29.069095
339.938608	12927.932348	29.074112
340.303057	12948.508979	29.079130
340.526556	12965.214021	29.084148
340.779360	12991.596616	29.089165
340.855868	13006.878400	29.094183
341.219517	13024.351017	29.099200
341.563572	13044.191996	29.104218
342.454271	13059.264180	29.109236
342.523385	13079.059841	29.114253
342.587651	13095.066777	29.119271
343.107115	13111.738220	29.124288
343.497446	13136.649988	29.129306
343.444704	13152.056347	29.134324
343.978887	13163.483367	29.139341
343.831081	13190.914266	29.144359
344.252862	13201.522063	29.149376
344.580276	13225.758531	29.154394
345.148398	13243.382483	29.159412
346.129991	13256.732140	29.164429
346.230123	13279.785312	29.169447
346.618734	13282.247680	29.174464
346.942386	13305.025866	29.179482
347.166945	13310.637153	29.184500
347.375719	13326.195324	29.189517
347.538145	13342.831317	29.194535
348.068244	13357.098102	29.199552
348.885646	13377.537932	29.204570
348.482889	13386.534949	29.209588
349.203358	13400.901425	29.214605
349.255027	13430.761485	29.219623
349.687681	13450.045840	29.224640
350.154091	13475.675631	29.229658
350.295993	13492.046541	29.234676
351.069685	13509.799599	29.239693
351.122925	13524.959126	29.244711
351.875295	13539.980731	29.249728
352.503039	13562.354740	29.254746
352.784172	13582.847214	29.259764
353.093278	13587.213719	29.264781
353.522881	13597.845778	29.269799
353.986483	13602.993378	29.274816
354.227753	13617.586666	29.279834
354.628183	13633.692984	29.284852
355.143913	13642.912579	29.289869
355.268357	13657.599989	29.294887
355.973130	13664.876227	29.299904
356.352493	13677.309953	29.304922
356.247148	13689.377490	29.309940
356.890971	13694.822161	29.314957
356.915185	13725.435437	29.319975
357.651813	13736.448973	29.324992
357.748761	13750.256515	29.330010
357.686648	13756.781297	29.335028
358.047753	13771.700158	29.340045
358.202746	13794.227444	29.345063
358.691400	13812.233866	29.350080
358.844029	13844.200965	29.355098
359.217891	13870.218436	29.360116
359.656329	13883.760994	29.365133
359.983698	13912.422780	29.370151
360.501620	13933.987021	29.375168
360.958048	13964.220331	29.380186
360.907350	13989.019136	29.385204
361.541145	14009.627366	29.390221
361.625904	14025.123427	29.395239
362.480053	14049.044744	29.400256
362.735159	14074.951616	29.405274
362.899601	14093.789136	29.410292
364.047072	14110.404146	29.415309
363.832140	14118.127799	29.420327
364.359038	14145.312276	29.425344
364.969380	14173.885918	29.430362
365.239070	14190.540592	29.435380
365.908967	14196.350824	29.440397
366.146004	14214.302298	29.445415
366.467812	14224.566306	29.450432
366.862904	14241.766683	29.455450
367.117612	14246.002906	29.460468
367.820752	14270.333447	29.465485
368.149540	14283.985052	29.470503
368.308403	14290.440665	29.475520
368.449009	14310.930672	29.480538
368.755801	14310.127862	29.485556
369.444955	14334.612266	29.490573
369.312482	14343.545288	29.495591
369.552321	14359.541580	29.500608
369.897402	14377.008880	29.505626
370.341073	14396.191412	29.510644
370.659740	14413.179689	29.515661
370.731241	14440.855955	29.520679
370.802324	14461.019092	29.525696
371.335296	14488.512608	29.530714
371.737990	14510.654546	29.535732
371.972157	14533.719826	29.540749
372.381249	14569.403023	29.545767
372.901842	14596.399644	29.550784
373.352865	14612.239899	29.555802
373.661547	14645.140825	29.560820
374.395036	14660.851606	29.565837
374.466992	14683.980373	29.570855
374.953591	14705.540923	29.575872
375.493890	14726.966758	29.580890
375.759056	14741.140285	29.585908
376.447828	14769.866764	29.590925
376.422021	14799.043144	29.595943
376.953102	14822.428617	29.600960
377.532421	14843.118925	29.605978
377.727893	14864.797895	29.610996
378.036975	14872.932453	29.616013
378.353589	14904.973550	29.621031
378.887526	14931.649576	29.626048
379.692827	14952.153011	29.631066
379.577098	14981.965926	29.636084
380.120379	14997.883641	29.641101
380.595561	15018.754680	29.646119
381.064276	15028.367622	29.651136
381.290866	15051.835811	29.656154
381.429542	15081.346898	29.661172
381.906533	15097.107692	29.666189
382.297944	15120.878608	29.671207
382.919338	15148.662419	29.676224
383.328178	15166.913181	29.681242
384.005716	15188.188549	29.686260
384.533495	15198.736648	29.691277
384.452392	15225.452574	29.696295
384.792060	15237.315577	29.701312
385.942447	15258.854895	29.706330
386.092980	15278.788529	29.711348
386.250204	15290.051644	29.716365
386.672313	15305.546436	29.721383
387.214140	15323.984965	29.726400
387.587591	15338.091441	29.731418
387.743776	15355.718718	29.736436
388.323476	15368.005315	29.741453
388.862088	15386.245435	29.746471
388.820178	15409.086561	29.751488
389.092708	15417.991387	29.756506
389.629030	15446.597484	29.761524
390.142620	15463.928846	29.766541
390.829874	15474.597401	29.771559
390.639402	15505.073451	29.776576
391.337202	15520.348369	29.781594
391.454874	15534.927746	29.786612
391.895065	15550.252513	29.791629
392.081593	15584.712297	29.796647
392.230904	15599.820526	29.801664
393.155120	15622.636909	29.806682
393.375326	15650.553775	29.811700
393.621973	15657.280352	29.816717
394.223787	15684.900619	29.821735
394.449297	15704.352359	29.826752
394.981167	15722.837050	29.831770
395.168776	15744.432973	29.836788
395.675712	15760.758131	29.841805
396.058876	15783.523645	29.846823
396.609833	15796.389845	29.851840
397.086373	15813.556776	29.856858
397.116148	15835.847099	29.861876
397.271915	15851.541972	29.866893
397.891286	15880.903197	29.871911
398.447060	15905.558957	29.876928
399.005778	15915.549891	29.881946
398.816101	15954.269921	29.886964
399.523131	15959.711669	29.891981
400.098268	15978.840460	29.896999
400.427430	16007.489320	29.902016
400.693010	16026.473984	29.907034
400.989074	16050.655791	29.912052
401.403068	16059.535600	29.917069
401.836097	16082.808480	29.922087
402.253046	16119.399805	29.927104
402.706332	16146.273348	29.932122
402.876246	16174.154636	29.937140
403.542051	16195.909890	29.942157
403.959662	16213.626503	29.947175
404.398283	16240.717249	29.952192
404.842181	16264.749832	29.957210
405.443463	16284.727614	29.962228
406.053348	16304.205034	29.967245
406.329418	16324.281173	29.972263
406.641863	16354.266036	29.977280
407.360834	16356.654958	29.982298
407.841015	16376.231729	29.987316
408.350371	16388.855326	29.992333
408.975193	16399.035142	29.997351
409.348558	16425.394131	30.002368
409.618523	16425.140265	30.007386
409.940518	16458.092758	30.012404
410.750635	16456.165572	30.017421
411.273659	16473.802745	30.022439
411.146942	16487.441996	30.027456
411.832974	16505.634827	30.032474
412.131674	16519.226417	30.037492
412.494312	16538.357467	30.042509
412.726662	16550.383386	30.047527
412.788326	16579.356104	30.052544
412.965184	16596.794931	30.057562
413.409069	16621.109070	30.062580
413.760615	16642.512925	30.067597
414.244024	16676.653376	30.072615
414.307609	16701.785227	30.077632
414.915840	16727.412969	30.082650
415.135477	16761.872837	30.087668
415.498365	16779.658556	30.092685
415.980233	16817.532880	30.097703
416.410144	16847.538016	30.102720
417.179692	16870.054787	30.107738
417.434300	16893.899867	30.112756
418.256398	16931.462123	30.117773
418.563834	16947.949042	30.122791
418.866119	16967.456365	30.127808
419.578541	16995.029610	30.132826
419.926509	17019.542472	30.137844
420.292377	17038.026007	30.142861
420.775030	17062.789466	30.147879
420.902345	17082.106369	30.152896
421.472626	17096.514962	30.157914
421.541203	17132.227840	30.162932
422.449649	17153.677696	30.167949
422.666571	17174.957935	30.172967
423.042397	17194.735083	30.177984
423.253987	17207.191075	30.183002
423.796533	17240.037712	30.188020
424.124717	17255.735152	30.193037
424.868623	17277.987937	30.198055
425.035999	17306.490348	30.203072
425.569928	17329.167749	30.208090
426.060703	17347.354058	30.213108
426.142423	17371.561622	30.218125
426.222559	17393.154120	30.223143
426.721700	17422.236463	30.228160
427.294178	17459.058664	30.233178
427.610150	17492.983572	30.238196
427.904176	17515.332365	30.243213
428.734240	17548.406137	30.248231
429.009722	17576.152888	30.253248
429.410976	17593.715401	30.258266
430.023481	17629.097625	30.263284
429.973782	17657.009137	30.268301
431.181155	17678.419075	30.273319
431.311381	17719.126723	30.278336
432.026216	17742.824957	30.283354
432.609642	17762.923945	30.288372
432.980786	17795.747835	30.293389
433.983173	17814.467237	30.298407
433.676968	17836.676673	30.303424
434.466927	17855.991637	30.308442
434.913474	17886.864427	30.313460
435.600435	17894.375674	30.318477
435.585262	17909.773651	30.323495
436.210470	17944.206848	30.328512
436.953463	17957.243420	30.333530
437.152873	17975.886592	30.338548
437.523186	18003.751769	30.343565
438.260849	18014.824486	30.348583
438.585532	18042.501025	30.353600
438.752343	18056.524993	30.358618
439.386974	18087.766645	30.363636
439.675309	18100.975608	30.368653
440.640560	18121.646913	30.373671
441.141532	18138.151916	30.378688
441.406374	18151.661516	30.383706
442.096333	18171.643164	30.388724
442.593819	18192.128793	30.393741
443.281683	18206.456625	30.398759
443.201397	18220.146681	30.403776
443.799729	18239.631031	30.408794
444.007009	18257.755204	30.413812
444.460080	18279.479802	30.418829
444.891280	18298.901944	30.423847
445.427157	18322.294090	30.428864
445.740482	18334.159975	30.433882
445.953980	18360.628775	30.438900
446.465371	18374.529509	30.443917
446.696784	18391.727661	30.448935
447.271960	18425.847355	30.453952
447.815307	18448.878381	30.458970
448.288449	18466.462016	30.463988
448.489233	18497.589073	30.469005
449.359471	18508.969826	30.474023
449.766167	18535.869791	30.479040
449.900709	18555.123856	30.484058
449.902977	18579.117937	30.489076
450.595678	18609.315242	30.494093
450.953023	18630.827792	30.499111
451.507131	18651.418756	30.504128
452.184736	18673.266570	30.509146
452.273965	18696.830209	30.514164
452.786398	18720.460262	30.519181
453.074924	18737.826670	30.524199
453.583808	18773.271439	30.529216
454.234749	18789.342858	30.534234
454.776769	18813.568573	30.539252
454.891573	18832.680696	30.544269
455.847639	18856.456232	30.549287
455.826384	18892.799241	30.554304
456.320847	18899.696625	30.559322
456.965552	18934.684489	30.564340
457.185379	18957.305596	30.569357
457.788111	18972.361239	30.574375
457.953260	19004.524485	30.579392
458.684821	19033.099010	30.584410
458.856168	19057.793744	30.589428
459.503618	19102.946824	30.594445
460.266796	19119.708533	30.599463
460.376862	19149.587277	30.604480
460.957782	19172.518510	30.609498
461.600326	19203.293200	30.614516
461.416959	19228.852393	30.619533
462.079461	19260.198971	30.624551
462.786280	19289.024145	30.629568
463.344966	19318.738113	30.634586
463.856962	19345.016188	30.639604
463.941748	19376.409215	30.644621
464.541556	19393.929626	30.649639
464.768240	19436.698035	30.654656
465.450001	19464.251172	30.659674
466.197547	19504.398340	30.664692
466.818231	19529.876215	30.669709
467.241635	19549.142879	30.674727
467.625855	19568.162981	30.679744
468.061126	19602.256108	30.684762
468.706221	19626.049704	30.689780
468.910601	19665.239810	30.694797
469.735287	19683.729822	30.699815
470.387930	19714.718550	30.704832
470.384639	19731.411298	30.709850
471.078517	19759.405216	30.714868
471.517467	19792.581985	30.719885
472.533501	19808.622338	30.724903
472.680325	19831.192711	30.729920
473.205286	19863.939139	30.734938
473.198247	19884.916249	30.739956
473.972558	19915.721970	30.744973
474.236457	19949.634048	30.749991
474.057098	19977.651326	30.755008
474.536980	20012.521625	30.760026
475.726411	20040.823736	30.765044
475.819195	20081.080960	30.770061
476.761886	20104.613713	30.775079
477.286063	20138.308443	30.780096
477.596444	20173.091850	30.785114
478.191485	20195.093305	30.790132
478.428383	20229.035368	30.795149
479.190078	20247.845373	30.800167
479.265962	20267.066086	30.805184
479.853430	20305.508788	30.810202
480.731611	20331.711883	30.815220
481.026332	20365.480852	30.820237
481.405434	20393.082705	30.825255
482.083741	20409.669274	30.830272
482.587382	20436.266038	30.835290
483.499123	20464.568030	30.840308
483.430690	20491.583019	30.845325
484.468618	20504.878393	30.850343
484.706751	20525.015368	30.855360
485.098813	20551.560263	30.860378
485.643795	20564.471652	30.865396
485.789347	20587.466420	30.870413
486.294432	20597.913627	30.875431
487.010220	20631.048457	30.880448
487.063164	20653.741892	30.885466
487.414896	20676.123185	30.890484
487.758985	20699.011168	30.895501
488.215240	20720.794856	30.900519
488.515954	20755.239619	30.905536
489.304516	20786.379353	30.910554
489.845618	20813.716328	30.915572
490.184965	20843.953483	30.920589
490.771976	20882.523756	30.925607
491.003773	20903.135989	30.930624
491.429593	20945.743814	30.935642
492.109323	20970.911037	30.940660
492.612134	21016.148053	30.945677
493.554322	21039.783107	30.950695
494.138927	21079.971665	30.955712
494.404754	21107.086788	30.960730
495.054778	21124.632482	30.965748
495.293388	21162.695529	30.970765
495.980904	21183.672655	30.975783
496.569035	21216.183982	30.980800
496.989262	21253.719599	30.985818
497.515508	21274.393519	30.990836
497.876494	21308.728714	30.995853
498.623144	21331.434331	31.000871
499.130717	21365.038990	31.005888
499.704481	21386.880835	31.010906
500.293113	21417.983381	31.015924
500.905374	21445.967220	31.020941
501.545143	21467.356517	31.025959
501.851169	21497.865275	31.030976
502.288734	21527.102397	31.035994
502.995769	21549.157337	31.041012
503.344875	21576.209514	31.046029
503.638680	21598.600930	31.051047
504.258165	21628.011905	31.056064
504.443848	21651.759865	31.061082
505.600243	21681.807152	31.066100
505.402010	21710.240561	31.071117
506.575345	21725.486982	31.076135
506.882869	21758.801394	31.081152
507.470310	21795.117624	31.086170
508.187412	21813.361120	31.091188
508.463098	21850.364467	31.096205
509.067671	21876.422920	31.101223
509.607438	21903.117111	31.106240
510.050273	21930.850152	31.111258
510.696700	21953.768066	31.116276
510.910719	21978.706221	31.121293
511.454063	22006.183514	31.126311
511.969430	22034.556173	31.131328
512.249812	22068.393495	31.136346
512.678403	22101.487322	31.141364
513.418869	22135.606552	31.146381
513.640179	22156.253333	31.151399
514.259508	22178.329033	31.156416
514.504969	22224.380021	31.161434
515.046244	22251.516764	31.166452
515.865527	22291.285586	31.171469
516.588731	22323.101468	31.176487
517.040568	22347.219303	31.181504
517.179965	22386.431322	31.186522
517.906033	22403.530246	31.191540
518.374952	22427.771881	31.196557
518.772761	22458.179283	31.201575
519.579439	22477.553084	31.206592
519.756652	22503.274889	31.211610
520.375581	22527.689038	31.216628
520.584104	22561.285701	31.221645
521.227971	22591.755873	31.226663
521.919245	22620.619974	31.231680
522.076530	22659.204155	31.236698
522.541209	22678.448468	31.241716
523.071343	22719.129136	31.246733
523.729435	22748.377758	31.251751
524.372049	22780.946320	31.256768
524.680911	22813.358680	31.261786
525.517790	22849.302871	31.266804
525.717134	22881.770410	31.271821
526.226991	22925.525723	31.276839
527.379386	22955.057418	31.281856
527.497760	22986.406700	31.286874
528.252761	23018.357739	31.291892
528.714729	23047.340523	31.296909
529.338971	23067.830359	31.301927
529.833476	23099.885519	31.306944
530.379851	23142.194836	31.311962
530.490322	23166.215475	31.316980
531.003625	23203.961382	31.321997
532.039425	23240.247956	31.327015
532.703342	23263.910309	31.332032
532.797872	23312.742607	31.337050
533.414649	23341.335063	31.342068
534.004192	23377.470609	31.347085
534.402990	23412.182681	31.352103
535.572561	23446.887840	31.357120
535.577501	23483.980872	31.362138
536.600785	23511.277658	31.367156
537.209401	23541.217675	31.372173
537.546992	23568.501867	31.377191
538.180761	23590.140853	31.382208
538.803305	23640.875502	31.387226
539.172343	23647.914278	31.392244
539.840764	23687.475716	31.397261
540.016959	23720.630731	31.402279
541.009684	23739.237274	31.407296
541.290494	23783.024026	31.412314
541.933617	23811.695183	31.417332
542.235069	23845.058282	31.422349
542.783137	23876.556523	31.427367
543.518783	23912.411065	31.432384
543.985252	23954.323864	31.437402
544.445856	23974.113538	31.442420
545.530941	24006.482102	31.447437
545.792134	24039.156698	31.452455
546.505872	24072.777895	31.457472
546.839853	24099.172343	31.462490
547.188131	24129.545822	31.467508
547.760538	24165.969856	31.472525
548.435047	24200.488452	31.477543
548.705590	24225.616475	31.482560
549.156695	24265.282609	31.487578
549.813465	24295.431079	31.492596
550.887371	24326.645451	31.497613
551.540232	24371.266269	31.502631
552.306618	24385.567374	31.507648
552.568420	24426.261957	31.512666
553.357353	24446.910688	31.517684
554.041416	24469.004078	31.522701
554.287187	24490.331958	31.527719
554.887017	24504.741388	31.532736
555.381493	24536.773586	31.537754
555.750069	24545.872926	31.542772
556.220362	24579.128653	31.547789
556.120369	24593.571917	31.552807
557.256586	24627.747199	31.557824
557.553298	24653.282433	31.562842
558.083833	24685.005881	31.567860
558.993611	24715.393422	31.572877
559.102603	24748.194127	31.577895
559.576333	24782.094253	31.582912
559.937612	24811.588303	31.587930
560.561543	24845.768355	31.592948
561.156701	24880.490143	31.597965
562.044900	24928.563797	31.602983
562.482771	24958.975060	31.608000
562.784002	25005.706260	31.613018
563.496729	25029.691690	31.618036
564.039271	25065.509028	31.623053
564.720945	25110.032185	31.628071
565.578704	25135.435926	31.633088
565.661984	25179.591613	31.638106
566.298266	25212.468488	31.643124
566.864882	25250.089836	31.648141
567.410574	25285.199258	31.653159
568.515689	25318.919249	31.658176
569.063164	25363.975890	31.663194
569.218595	25393.281839	31.668212
570.009235	25429.301123	31.673229
570.486080	25484.032116	31.678247
571.302393	25505.581392	31.683264
571.607472	25547.434321	31.688282
572.154258	25578.240255	31.693300
573.130730	25615.330427	31.698317
573.239168	25648.827874	31.703335
574.192419	25682.003469	31.708352
574.949880	25722.054257	31.713370
575.354406	25750.632843	31.718388
575.965036	25777.011451	31.723405
576.718116	25817.050474	31.728423
577.341543	25847.421381	31.733440
577.688417	25886.506646	31.738458
578.546929	25913.522849	31.743476
579.244207	25941.303778	31.748493
579.273320	25976.571151	31.753511
580.039926	26005.017551	31.758528
580.778505	26044.300895	31.763546
580.791172	26079.880705	31.768564
581.919729	26106.526232	31.773581
582.510025	26150.680480	31.778599
582.973020	26182.808713	31.783616
583.561830	26231.444297	31.788634
584.085362	26254.171525	31.793652
584.767720	26286.973419	31.798669
585.413738	26329.014738	31.803687
585.860363	26361.961114	31.808704
586.491234	26404.080802	31.813722
586.843533	26434.280171	31.818740
587.651985	26468.263439	31.823757
588.001150	26502.805347	31.828775
588.789470	26535.907058	31.833792
589.292888	26569.742343	31.838810
590.062799	26606.879334	31.843828
590.822453	26643.531342	31.848845
591.281886	26674.681283	31.853863
591.528292	26705.769831	31.858880
592.514700	26743.764319	31.863898
593.101094	26786.574356	31.868916
593.551871	26799.036862	31.873933
594.222118	26832.979186	31.878951
594.584008	26863.531628	31.883968
595.627514	26886.393023	31.888986
595.808109	26927.149615	31.894004
596.521809	26944.722078	31.899021
596.991061	26969.550633	31.904039
597.852549	26998.293270	31.909056
598.588824	27030.108277	31.914074
599.113520	27053.164879	31.919092
599.905571	27071.395137	31.924109
600.436666	27108.241793	31.929127
600.838115	27131.937182	31.934144
601.535115	27155.295575	31.939162
601.773693	27192.207155	31.944180
602.321327	27217.636816	31.949197
602.976969	27265.417486	31.954215
603.581580	27294.794893	31.959232
604.312674	27329.727145	31.964250
604.635936	27352.904122	31.969268
605.187525	27397.661273	31.974285
605.824162	27442.101821	31.979303
606.247839	27473.454523	31.984320
606.990306	27510.313048	31.989338
607.601053	27547.166987	31.994356
608.483122	27588.434455	31.999373
609.304664	27624.503381	32.004391
609.866612	27653.932233	32.009408
610.633689	27684.687916	32.014426
611.135035	27719.998131	32.019444
611.724358	27745.921248	32.024461
612.324234	27781.822911	32.029479
612.966496	27811.846188	32.034496
613.314774	27852.761671	32.039514
614.151185	27900.079402	32.044532
614.504652	27932.549913	32.049549
615.613162	27972.038209	32.054567
616.310360	27998.538893	32.059584
616.930669	28039.481674	32.064602
617.379357	28078.744839	32.069620
617.783469	28096.973571	32.074637
618.233029	28138.569038	32.079655
618.888064	28173.527295	32.084672
619.624462	28222.195102	32.089690
620.139618	28256.518055	32.094708
620.909759	28295.592238	32.099725
621.402881	28331.113384	32.104743
622.139040	28377.278588	32.109760
622.848036	28402.741348	32.114778
623.227828	28452.913007	32.119796
624.296521	28478.452265	32.124813
624.510316	28522.759127	32.129831
625.149464	28562.094526	32.134848
625.926246	28601.003914	32.139866
626.036587	28636.124117	32.144884
626.851627	28678.921292	32.149901
627.376298	28721.479592	32.154919
627.854146	28764.001067	32.159936
628.958752	28802.663552	32.164954
629.118069	28844.027791	32.169972
630.218364	28884.467276	32.174989
631.005598	28930.385537	32.180007
631.638065	28972.409162	32.185024
632.387650	28994.162239	32.190042
632.831284	29029.243561	32.195060
633.636577	29067.580486	32.200077
634.194182	29095.122131	32.205095
634.758295	29139.021489	32.210112
635.607059	29163.540446	32.215130
636.036997	29199.445933	32.220148
636.789225	29226.451595	32.225165
636.784885	29266.047148	32.230183
637.757433	29286.785861	32.235200
638.634234	29323.222080	32.240218
638.817145	29357.080586	32.245236
639.679889	29379.404210	32.250253
640.555996	29420.891235	32.255271
641.186981	29455.223344	32.260288
642.071672	29478.055645	32.265306
642.394559	29511.974660	32.270324
643.236243	29552.866840	32.275341
643.551124	29578.576099	32.280359
643.740678	29624.886611	32.285376
644.576292	29662.922809	32.290394
644.962381	29701.661593	32.295412
645.382839	29740.489884	32.300429
645.869094	29794.377639	32.305447
646.841759	29840.490140	32.310464
647.634026	29883.343966	32.315482
648.170003	29931.282356	32.320500
648.874227	29973.132441	32.325517
650.070525	30014.336636	32.330535
650.421272	30062.247447	32.335552
651.163184	30093.706039	32.340570
651.965144	30138.866146	32.345588
652.586872	30180.211225	32.350605
653.494546	30223.009758	32.355623
654.230706	30266.638049	32.360640
654.764918	30297.560560	32.365658
655.551138	30346.358356	32.370676
656.087659	30364.309196	32.375693
656.615775	30421.156750	32.380711
657.357303	30459.006872	32.385728
658.230175	30486.115405	32.390746
658.452532	30531.392427	32.395764
658.964911	30573.627774	32.400781
659.899919	30612.851233	32.405799
660.385325	30657.151763	32.410816
661.268037	30703.634286	32.415834
661.420370	30746.805055	32.420852
662.337370	30789.476874	32.425869
663.283947	30830.468952	32.430887
663.789058	30880.620584	32.435904
664.854727	30926.815775	32.440922
665.564424	30958.919207	32.445940
666.171217	30997.847114	32.450957
666.667885	31038.739381	32.455975
667.235379	31076.504101	32.460992
668.107421	31118.658950	32.466010
668.780237	31165.579964	32.471028
669.636841	31203.887550	32.476045
669.924557	31250.135756	32.481063
670.529661	31283.678439	32.486080
671.113668	31328.110360	32.491098
671.928040	31376.710208	32.496116
672.516807	31429.214370	32.501133
673.339644	31460.681338	32.506151
673.733778	31507.039885	32.511168
674.689622	31541.836651	32.516186
675.130749	31586.639196	32.521204
676.017152	31626.308389	32.526221
676.776110	31672.338338	32.531239
677.158360	31718.250372	32.536256
678.064273	31751.297858	32.541274
678.629184	31799.229722	32.546292
679.254104	31842.733356	32.551309
680.003312	31876.981438	32.556327
680.692124	31905.720080	32.561344
681.254717	31944.580824	32.566362
682.046160	31979.081656	32.571380
682.700921	32018.680404	32.576397
683.682063	32058.727544	32.581415
683.740640	32083.367405	32.586432
684.806718	32124.039879	32.591450
685.328731	32164.095904	32.596468
685.714362	32200.064117	32.601485
686.942171	32246.692037	32.606503
687.563812	32282.225151	32.611520
688.309332	32313.193443	32.616538
689.046929	32352.508011	32.621556
689.746978	32388.863527	32.626573
690.673172	32423.931940	32.631591
691.216679	32466.924903	32.636608
691.819025	32499.901002	32.641626
692.408368	32530.792924	32.646644
693.065313	32570.601006	32.651661
693.703431	32615.039847	32.656679
694.702822	32655.805991	32.661696
695.500930	32683.308436	32.666714
696.051025	32725.807780	32.671732
696.770684	32766.529439	32.676749
697.257341	32809.595232	32.681767
697.976668	32858.282969	32.686784
698.709239	32900.646616	32.691802
699.152937	32944.926942	32.696820
699.996970	32982.487440	32.701837
700.785580	33025.601224	32.706855
701.659560	33068.050543	32.711872
702.089609	33108.331413	32.716890
702.823588	33158.206126	32.721908
703.753321	33199.622784	32.726925
704.632367	33232.398653	32.731943
705.144574	33285.956325	32.736960
706.129304	33317.988720	32.741978
706.622007	33363.596252	32.746996
707.045884	33409.379040	32.752013
707.988513	33453.569663	32.757031
708.794068	33499.963042	32.762048
709.573474	33529.385190	32.767066
710.133372	33572.308313	32.772084
710.718231	33610.783008	32.777101
711.567217	33659.559783	32.782119
712.227018	33706.874219	32.787136
712.962576	33747.879804	32.792154
713.237860	33795.539162	32.797172
714.457723	33843.404762	32.802189
715.399172	33886.812505	32.807207
716.002682	33934.989797	32.812224
716.729975	33969.605125	32.817242
717.357694	34019.991678	32.822260
718.205509	34059.159421	32.827277
719.199867	34092.019738	32.832295
719.489175	34129.024269	32.837312
720.509580	34169.214725	32.842330
721.026469	34219.290341	32.847348
721.581667	34255.810880	32.852365
722.802119	34289.521255	32.857383
723.258628	34341.111382	32.862400
724.215829	34380.129820	32.867418
724.971545	34411.371494	32.872436
725.537056	34448.952947	32.877453
726.368246	34490.988234	32.882471
727.219095	34518.592317	32.887488
727.917456	34547.883165	32.892506
728.492623	34582.472744	32.897524
728.970759	34618.721462	32.902541
729.757849	34649.244118	32.907559
729.980981	34687.575103	32.912576
730.827801	34716.406674	32.917594
731.714060	34766.539555	32.922612
732.416864	34800.919824	32.927629
732.905488	34850.963430	32.932647
733.363209	34893.317235	32.937664
734.538663	34939.523086	32.942682
735.059080	34977.902885	32.947700
735.666441	35020.435840	32.952717
736.474298	35053.238346	32.957735
736.929813	35096.161952	32.962752
738.189752	35139.686797	32.967770
738.808284	35191.000715	32.972788
739.541640	35248.632252	32.977805
740.128343	35287.463799	32.982823
740.309218	35332.896802	32.987840
741.556579	35384.890428	32.992858
742.044988	35434.341096	32.997876
742.922002	35495.346198	33.002893
743.646834	35532.733911	33.007911
744.419708	35586.876252	33.012928
745.218858	35636.740305	33.017946
746.400973	35685.861625	33.022964
746.727788	35745.328604	33.027981
748.024785	35769.785169	33.032999
748.501499	35828.286782	33.038016
749.218760	35890.083119	33.043034
750.176575	35930.065426	33.048052
750.691929	35978.229565	33.053069
751.799984	36023.013006	33.058087
752.290164	36084.206838	33.063104
753.278363	36123.090858	33.068122
754.477017	36174.417478	33.073140
754.600153	36214.581612	33.078157
755.856419	36252.601886	33.083175
756.742875	36300.860398	33.088192
757.400301	36337.798495	33.093210
758.199601	36374.385635	33.098228
758.429513	36421.324519	33.103245
759.942045	36473.753529	33.108263
760.581528	36514.204116	33.113280
761.433678	36554.102973	33.118298
762.472296	36593.504786	33.123316
763.086342	36630.140345	33.128333
764.054009	36665.576084	33.133351
764.557488	36712.681437	33.138368
765.280339	36746.258667	33.143386
766.307970	36781.931817	33.148404
766.938530	36824.825180	33.153421
767.773166	36856.899104	33.158439
768.372145	36898.602455	33.163456
768.952612	36938.715306	33.168474
769.765138	36980.701544	33.173492
770.532128	37030.523312	33.178509
771.655102	37067.370803	33.183527
772.203097	37117.094276	33.188544
772.964635	37145.657956	33.193562
773.809933	37185.211281	33.198580
774.167572	37226.472485	33.203597
775.054727	37263.850469	33.208615
775.776001	37316.323256	33.213632
776.385763	37357.538909	33.218650
777.466391	37393.324929	33.223668
777.998059	37454.712219	33.228685
778.948793	37494.129459	33.233703
779.314244	37538.665612	33.238720
780.094334	37569.661506	33.243738
780.884277	37607.991195	33.248756
781.294467	37649.738220	33.253773
782.073864	37686.425580	33.258791
782.617054	37731.231507	33.263808
783.475163	37791.164809	33.268826
784.285077	37834.639174	33.273844
785.100315	37882.918737	33.278861
786.036858	37928.902909	33.283879
786.792024	37975.902069	33.288896
787.496491	38032.470634	33.293914
788.507687	38076.362949	33.298932
789.263047	38124.709346	33.303949
790.060111	38166.896365	33.308967
790.568026	38217.501334	33.313984
791.380263	38264.972791	33.319002
792.687031	38313.404007	33.324020
793.328876	38373.815461	33.329037
793.933889	38417.348386	33.334055
794.539446	38470.095064	33.339072
795.699353	38524.766032	33.344090
796.486079	38562.794387	33.349108
796.998143	38621.013523	33.354125
797.983820	38670.988247	33.359143
798.668975	38722.919951	33.364160
799.722070	38774.117510	33.369178
800.821849	38829.374139	33.374196
801.613926	38885.924903	33.379213
801.953959	38932.036246	33.384231
802.837160	38984.449804	33.389248
803.729576	39040.327571	33.394266
804.534791	39083.931675	33.399284
805.187904	39142.490594	33.404301
806.578746	39183.473604	33.409319
807.445323	39236.990753	33.414336
808.412270	39282.903492	33.419354
809.174241	39331.491871	33.424372
809.698376	39387.529389	33.429389
810.366355	39433.558827	33.434407
811.362698	39492.811188	33.439424
811.960330	39532.338049	33.444442
813.115275	39589.852010	33.449460
813.966465	39630.427093	33.454477
815.310567	39674.030216	33.459495
815.750033	39711.027220	33.464512
816.749520	39753.318451	33.469530
818.157627	39802.002759	33.474548
818.516775	39849.858533	33.479565
819.430180	39880.647154	33.484583
820.190367	39921.306598	33.489600
821.206157	39966.232886	33.494618
822.060485	40007.042179	33.499636
822.576563	40056.948184	33.504653
823.282165	40095.637013	33.509671
824.160830	40139.725034	33.514688
824.858653	40190.121476	33.519706
826.161019	40225.928082	33.524724
826.626345	40271.345953	33.529741
827.200944	40322.697995	33.534759
828.250213	40356.969694	33.539776
828.707219	40414.316860	33.544794
829.740412	40460.152152	33.549812
829.907492	40515.767838	33.554829
830.778459	40571.020470	33.559847
831.829227	40615.208994	33.564864
832.494145	40672.239684	33.569882
833.675387	40725.483552	33.574900
834.586710	40761.010754	33.579917
835.270603	40799.856021	33.584935
836.068268	40843.376302	33.589952
836.451962	40879.985584	33.594970
837.287054	40930.646846	33.599988
838.210413	40979.909336	33.605005
839.135784	41019.147249	33.610023
839.918993	41076.160471	33.615040
840.489703	41127.217762	33.620058
841.201038	41174.749341	33.625076
842.005359	41235.054772	33.630093
842.745639	41288.666319	33.635111
844.083406	41334.613873	33.640128
844.789765	41388.262598	33.645146
845.684864	41438.314801	33.650164
846.311375	41494.563069	33.655181
847.066876	41558.545340	33.660199
848.257708	41606.957802	33.665216
849.271768	41665.947665	33.670234
849.905722	41724.933959	33.675252
851.073744	41774.355994	33.680269
851.955494	41826.270648	33.685287
852.797530	41874.769942	33.690304
853.829565	41938.210362	33.695322
854.823663	41977.945218	33.700340
855.569500	42029.128982	33.705357
856.306730	42085.083135	33.710375
857.404149	42137.135525	33.715392
858.203628	42192.669090	33.720410
859.004274	42228.703023	33.725428
859.742886	42287.073575	33.730445
861.258130	42328.175862	33.735463
862.511590	42375.144462	33.740480
862.683549	42430.511241	33.745498
863.662393	42472.083609	33.750516
864.510239	42533.967030	33.755533
865.341879	42581.476493	33.760551
866.227536	42630.002249	33.765568
866.937618	42692.255560	33.770586
868.184550	42735.184274	33.775604
868.919957	42794.454825	33.780621
869.651101	42834.352580	33.785639
870.770811	42883.190122	33.790656
871.555025	42941.890496	33.795674
872.170699	42980.490980	33.800692
873.143223	43033.083703	33.805709
873.823283	43088.461122	33.810727
875.177963	43138.369332	33.815744
875.570929	43196.094323	33.820762
876.560314	43246.768394	33.825780
877.434286	43301.167208	33.830797
878.314756	43358.892191	33.835815
879.020087	43404.981060	33.840832
879.991897	43471.952142	33.845850
880.785735	43512.771114	33.850868
881.540655	43574.330437	33.855885
882.540780	43625.914532	33.860903
883.467641	43678.490639	33.865920
884.492514	43733.834656	33.870938
885.782162	43777.859314	33.875956
886.588902	43835.426300	33.880973
887.607443	43874.275203	33.885991
888.918892	43922.395557	33.891008
889.823102	43967.524629	33.896026
890.805316	44000.490524	33.901044
891.429878	44047.630739	33.906061
891.951759	44093.186805	33.911079
893.259403	44132.231258	33.916096
894.059215	44171.089629	33.921114
894.969071	44204.117761	33.926132
895.541271	44242.657672	33.931149
895.958585	44274.959700	33.936167
897.256247	44314.701838	33.941184
897.816115	44367.185230	33.946202
898.818728	44406.663783	33.951220
899.790595	44457.836756	33.956237
900.427220	44498.087561	33.961255
901.637721	44535.737345	33.966272
901.959746	44583.887548	33.971290
902.907314	44638.176908	33.976308
903.607025	44685.382614	33.981325
904.756521	44748.471125	33.986343
905.841752	44791.966828	33.991360
906.539449	44843.651711	33.996378
907.470940	44904.377390	34.001396
908.260057	44957.016044	34.006413
908.923852	45015.120841	34.011431
910.137822	45064.403879	34.016448
910.827902	45135.219492	34.021466
911.689054	45188.954410	34.026484
912.485949	45241.099109	34.031501
913.400611	45305.054633	34.036519
914.548391	45364.824138	34.041536
915.222977	45429.304692	34.046554
916.785750	45484.866152	34.051572
917.327100	45547.021036	34.056589
918.312521	45615.078147	34.061607
919.222620	45670.609420	34.066624
919.869999	45739.295491	34.071642
920.743941	45797.160658	34.076660
922.249936	45862.878670	34.081677
922.750170	45927.425910	34.086695
924.349805	45990.548659	34.091712
925.515046	46048.596598	34.096730
926.024364	46101.863740	34.101748
927.021810	46158.413677	34.106765
928.008858	46228.901573	34.111783
929.096295	46285.425087	34.116800
929.896203	46335.130013	34.121818
930.850508	46386.531559	34.126836
931.867497	46445.274297	34.131853
932.578387	46507.272442	34.136871
933.549331	46567.509338	34.141888
934.586184	46624.775453	34.146906
935.450207	46684.150072	34.151924
936.433833	46736.661227	34.156941
937.302929	46800.507946	34.161959
938.790159	46846.899017	34.166976
939.732371	46911.411503	34.171994
940.740269	46969.106882	34.177012
941.457371	47016.169265	34.182029
941.914440	47073.097114	34.187047
943.270009	47124.342622	34.192064
944.318492	47181.216100	34.197082
945.016159	47237.543654	34.202100
946.157687	47287.437588	34.207117
947.024143	47347.205800	34.212135
948.056491	47405.467833	34.217152
949.068296	47457.584020	34.222170
950.262500	47518.136445	34.227188
950.979128	47562.783367	34.232205
951.996456	47616.771664	34.237223
953.410788	47664.877633	34.242240
953.796124	47717.155770	34.247258
954.882001	47763.782382	34.252276
956.229807	47808.830752	34.257293
956.879965	47850.742972	34.262311
957.431993	47894.783675	34.267328
958.310243	47942.233972	34.272346
959.249847	47980.374812	34.277364
960.688232	48025.150045	34.282381
961.436507	48072.298314	34.287399
962.458512	48115.323207	34.292416
963.955912	48155.078843	34.297434
964.291682	48195.718677	34.302452
965.237847	48240.982631	34.307469
966.094167	48294.137336	34.312487
966.979672	48344.339402	34.317504
967.454730	48390.329056	34.322522
968.307775	48452.202713	34.327540
969.470319	48504.582401	34.332557
970.551918	48568.103475	34.337575
971.822616	48625.844169	34.342592
972.474621	48674.046333	34.347610
973.263818	48740.814974	34.352628
974.221837	48790.380325	34.357645
974.973381	48863.311119	34.362663
976.035560	48934.807948	34.367680
977.285988	48994.501392	34.372698
978.169892	49049.298501	34.377716
979.296680	49114.465313	34.382733
980.024454	49185.578735	34.387751
981.144926	49250.943056	34.392768
981.963667	49305.516888	34.397786
983.153875	49372.325816	34.402804
984.333045	49429.867762	34.407821
984.901160	49507.188558	34.412839
985.873919	49565.623623	34.417856
987.073516	49633.032900	34.422874
988.270937	49706.959496	34.427892
989.363941	49761.200432	34.432909
990.118900	49830.432481	34.437927
991.594609	49884.360707	34.442944
992.346759	49950.208601	34.447962
992.808736	50024.637318	34.452980
994.538681	50083.056382	34.457997
995.376214	50155.579215	34.463015
996.278598	50216.114897	34.468032
997.436536	50275.902087	34.473050
998.634139	50348.736126	34.478068
999.765994	50392.412460	34.483085
1000.773469	50455.026606	34.488103
1001.845387	50519.364484	34.493120
1002.728043	50573.450455	34.498138
1003.997208	50641.560445	34.503156
1004.997507	50698.810887	34.508173
1005.812412	50759.545182	34.513191
1006.637117	50816.582973	34.518208
1007.960937	50869.518601	34.523226
1009.004020	50934.469572	34.528244
1010.259393	50978.690810	34.533261
1010.775705	51049.798809	34.538279
1012.255131	51100.046793	34.543296
1012.972116	51155.621686	34.548314
1014.029357	51216.800121	34.553332
1015.640317	51266.534338	34.558349
1016.602878	51325.057721	34.563367
1017.593394	51374.079402	34.568384
1018.455793	51418.559161	34.573402
1019.510093	51480.523356	34.578420
1020.263320	51524.678729	34.583437
1021.299603	51586.177795	34.588455
1022.380930	51634.078499	34.593472
1023.408960	51690.194432	34.598490
1023.942176	51734.871869	34.603508
1025.129416	51778.067591	34.608525
1026.012296	51831.922351	34.613543
1026.658253	51878.417404	34.618560
1027.519453	51927.954054	34.623578
1028.869281	51991.461567	34.628596
1029.951263	52039.426282	34.633613
1030.392979	52096.134874	34.638631
1031.383235	52158.281752	34.643648
1032.529308	52217.734129	34.648666
1033.477282	52282.400039	34.653684
1034.490209	52343.063185	34.658701
1035.724164	52419.283362	34.663719
1036.636296	52464.573613	34.668736
1037.809311	52528.641806	34.673754
1039.053766	52602.380463	34.678772
1039.905432	52659.924784	34.683789
1040.954060	52728.315889	34.688807
1041.939985	52789.351435	34.693824
1043.498389	52850.563281	34.698842
1044.460394	52908.761689	34.703860
1045.803255	52960.661345	34.708877
1046.964056	53029.934327	34.713895
1047.811724	53089.530564	34.718912
1049.265927	53152.550310	34.723930
1050.099536	53205.479427	34.728948
1050.992799	53264.581721	34.733965
1052.221246	53324.099956	34.738983
1053.408544	53383.428617	34.744000
1054.462984	53441.632863	34.749018
1055.365652	53501.734106	34.754036
1056.278962	53558.606545	34.759053
1057.356979	53617.389715	34.764071
1058.899606	53686.339081	34.769088
1059.768920	53744.864154	34.774106
1060.373112	53805.076184	34.779124
1061.607810	53872.410020	34.784141
1062.369656	53936.616050	34.789159
1063.558296	53999.401214	34.794176
1064.859975	54060.447590	34.799194
1065.616145	54130.445300	34.804212
1066.955947	54184.461757	34.809229
1068.296640	54260.778796	34.814247
1069.120912	54317.078486	34.819264
1070.471515	54378.763507	34.824282
1071.636917	54442.572339	34.829300
1072.915691	54509.572028	34.834317
1073.948541	54561.321259	34.839335
1075.257769	54623.741153	34.844352
1076.338330	54674.211172	34.849370
1076.725992	54733.098883	34.854388
1078.389128	54791.698454	34.859405
1079.618821	54853.802334	34.864423
1080.428500	54919.617285	34.869440
1081.420993	54974.373394	34.874458
1082.451301	55034.737014	34.879476
1083.720776	55084.804958	34.884493
1084.391019	55150.598082	34.889511
1085.394349	55208.650157	34.894528
1086.649449	55262.150754	34.899546
1087.539800	55331.289326	34.904564
1088.504345	55392.157774	34.909581
1089.847414	55463.168705	34.914599
1091.056824	55515.272094	34.919616
1092.789886	55578.248350	34.924634
1093.483907	55632.223667	34.929652
1094.598072	55682.741206	34.934669
1095.880829	55732.194568	34.939687
1096.564411	55783.001233	34.944704
1097.669459	55819.553243	34.949722
1098.712776	55872.126423	34.954740
1099.633054	55919.345957	34.959757
1100.767935	55974.493447	34.964775
1101.977174	56018.908642	34.969792
1103.041804	56072.314314	34.974810
1104.041660	56127.622529	34.979828
1105.250802	56172.272188	34.984845
1106.420556	56216.624319	34.989863
1107.418379	56276.034215	34.994880
1108.703485	56317.520540	34.999898
1109.507006	56392.460274	35.004916
1110.680216	56441.558865	35.009933
1111.909319	56496.230812	35.014951
1112.674553	56562.664835	35.019968
1113.913904	56615.778561	35.024986
1114.778456	56678.741814	35.030004
1116.261161	56730.906343	35.035021
1117.291629	56791.755393	35.040039
1118.523731	56855.129906	35.045056
1119.577976	56914.013587	35.050074
1120.730354	56981.685591	35.055092
1121.547309	57041.037101	35.060109
1122.586342	57114.043540	35.065127
1123.899526	57177.811267	35.070144
1125.538312	57238.635836	35.075162
1126.686589	57308.562530	35.080180
1127.754833	57360.603450	35.085197
1128.861058	57419.657448	35.090215
1129.847481	57489.204948	35.095232
1131.386557	57556.102850	35.100250
1132.438069	57624.463343	35.105268
1133.467002	57678.669330	35.110285
1134.679238	57735.125229	35.115303
1135.573173	57806.143825	35.120320
1136.675732	57866.604568	35.125338
1137.886038	57932.979036	35.130356
1138.658598	58000.447548	35.135373
1139.914049	58068.125465	35.140391
1141.528687	58141.836065	35.145408
1142.601551	58205.865668	35.150426
1143.437297	58278.983420	35.155444
1144.567330	58346.922267	35.160461
1145.860204	58408.190039	35.165479
1146.985766	58480.800991	35.170496
1148.142889	58541.033356	35.175514
1149.209015	58610.014630	35.180532
1150.351042	58676.819571	35.185549
1151.727887	58740.043476	35.190567
1152.912024	58803.487598	35.195584
1154.607933	58863.630089	35.200602
1155.693258	58936.419602	35.205620
1156.839619	58993.344480	35.210637
1158.015150	59049.556024	35.215655
1158.903130	59107.768527	35.220672
1160.005779	59163.586658	35.225690
1161.174372	59240.161749	35.230708
1162.599107	59302.778322	35.235725
1163.609196	59361.459691	35.240743
1164.787476	59420.855432	35.245760
1166.332405	59475.744220	35.250778
1167.181491	59531.849748	35.255796
1168.000646	59599.239464	35.260813
1169.339039	59662.655355	35.265831
1170.366343	59729.544453	35.270848
1171.837983	59796.091997	35.275866
1172.961290	59855.889846	35.280884
1174.164110	59899.427065	35.285901
1174.928355	59952.002215	35.290919
1175.747128	60009.474476	35.295936
1176.943919	60059.943973	35.300954
1177.842863	60117.043142	35.305972
1179.077956	60177.792732	35.310989
1180.886530	60228.920047	35.316007
1181.540883	60300.527815	35.321024
1182.521986	60365.780143	35.326042
1183.835466	60426.334516	35.331060
1184.939667	60494.815121	35.336077
1186.077882	60554.618678	35.341095
1187.481468	60625.072006	35.346112
1188.636156	60674.321368	35.351130
1190.054814	60746.918521	35.356148
1190.971515	60814.638134	35.361165
1192.329235	60884.010639	35.366183
1193.800096	60941.269067	35.371200
1195.230956	61008.459298	35.376218
1196.199706	61076.627245	35.381236
1197.315832	61139.891868	35.386253
1199.102058	61204.229138	35.391271
1199.813777	61269.171562	35.396288
1201.087559	61324.638684	35.401306
1201.888942	61387.870928	35.406324
1203.135296	61464.250914	35.411341
1204.423849	61532.794178	35.416359
1205.973871	61607.804077	35.421376
1207.494228	61664.328479	35.426394
1208.665317	61736.062102	35.431412
1209.641871	61806.389436	35.436429
1211.189099	61864.277411	35.441447
1212.313582	61937.664769	35.446464
1213.150461	61992.359874	35.451482
1215.045088	62068.551625	35.456500
1216.176415	62142.058793	35.461517
1217.562708	62181.735206	35.466535
1218.932654	62248.963683	35.471552
1220.184410	62312.178434	35.476570
1221.641243	62368.670085	35.481588
1222.611028	62432.454703	35.486605
1224.035909	62481.064005	35.491623
1225.102612	62545.865591	35.496640
1226.460925	62605.500412	35.501658
1227.775034	62663.243175	35.506676
1228.980142	62728.257796	35.511693
1230.394984	62773.811654	35.516711
1231.637817	62835.237627	35.521728
1232.830793	62888.435627	35.526746
1233.984534	62940.120569	35.531764
1235.293369	62999.479212	35.536781
1236.881081	63049.494833	35.541799
1237.760355	63114.238619	35.546816
1239.027184	63166.045600	35.551834
1240.207713	63217.562333	35.556852
1241.162657	63271.646710	35.561869
1242.642226	63320.401034	35.566887
1244.000043	63380.411300	35.571904
1245.180143	63441.019286	35.576922
1246.416962	63500.466369	35.581940
1247.130689	63567.339013	35.586957
1248.579384	63615.991130	35.591975
1249.526679	63677.712345	35.596992
1250.958387	63744.029921	35.602010
1252.408902	63798.563311	35.607028
1253.088696	63861.941184	35.612045
1254.718159	63922.948470	35.617063
1255.789142	63989.424459	35.622080
1256.903030	64037.205523	35.627098
1257.966413	64092.236979	35.632116
1259.080973	64152.894939	35.637133
1260.329475	64193.026639	35.642151
1261.736822	64261.337272	35.647168
1262.642451	64323.066604	35.652186
1263.886177	64378.817497	35.657204
1264.902310	64442.391090	35.662221
1266.238118	64490.809353	35.667239
1267.418288	64570.045482	35.672256
1268.658140	64635.325537	35.677274
1270.042207	64712.890496	35.682292
1271.143450	64780.965572	35.687309
1272.550631	64849.334812	35.692327
1273.714801	64916.767310	35.697344
1274.743023	64987.671660	35.702362
1276.427057	65050.458492	35.707380
1277.407129	65138.534169	35.712397
1278.881473	65212.484182	35.717415
1280.208457	65290.357416	35.722432
1281.589035	65357.428003	35.727450
1283.055482	65426.587251	35.732468
1284.481304	65499.577044	35.737485
1285.657705	65564.204675	35.742503
1287.194238	65642.109505	35.747520
1288.376472	65710.592271	35.752538
1290.293516	65777.402725	35.757556
1291.123181	65854.089311	35.762573
1292.768909	65920.201862	35.767591
1294.377576	65983.882861	35.772608
1295.628220	66047.284508	35.777626
1297.044114	66113.642475	35.782644
1297.840384	66182.313562	35.787661
1299.575348	66237.003993	35.792679
1300.635981	66306.609055	35.797696
1302.026448	66373.984696	35.802714
1303.527797	66442.489134	35.807732
1304.654665	66514.768892	35.812749
1305.723505	66571.026865	35.817767
1307.008438	66642.585792	35.822784
1308.583506	66706.577775	35.827802
1309.915686	66788.665202	35.832820
1311.038450	66860.623682	35.837837
1312.681237	66929.081967	35.842855
1314.079592	66995.482975	35.847872
1315.556277	67062.296106	35.852890
1316.987884	67111.717445	35.857908
1318.718783	67167.562858	35.862925
1320.117172	67232.261296	35.867943
1321.592114	67280.276908	35.872960
1322.952977	67346.918970	35.877978
1324.257508	67394.999463	35.882996
1325.737265	67446.357715	35.888013
1326.915633	67494.641762	35.893031
1327.988132	67551.141930	35.898048
1329.267130	67610.769389	35.903066
1330.621627	67658.836227	35.908084
1332.157384	67729.105276	35.913101
1333.128416	67781.183334	35.918119
1334.257425	67846.083788	35.923136
1335.420696	67895.833580	35.928154
1337.120638	67959.695195	35.933172
1337.885129	68023.405808	35.938189
1339.662303	68095.081709	35.943207
1341.052891	68149.431262	35.948224
1342.007128	68216.683775	35.953242
1343.600188	68281.405052	35.958260
1344.759648	68340.179132	35.963277
1346.124174	68381.742978	35.968295
1346.744453	68441.741421	35.973312
1348.008980	68490.102506	35.978330
1349.836769	68548.094938	35.983348
1350.809350	68615.326627	35.988365
1351.877524	68670.842166	35.993383
1352.982067	68726.364796	35.998400
1353.910446	68792.084204	36.003418
1355.729909	68856.511882	36.008436
1356.931781	68930.021455	36.013453
1358.393660	68998.260318	36.018471
1359.787928	69068.757806	36.023488
1361.262374	69149.779418	36.028506
1362.522006	69213.282496	36.033524
1363.774761	69297.441970	36.038541
1365.278741	69360.774190	36.043559
1367.320413	69435.489815	36.048576
1368.105333	69510.661992	36.053594
1369.529122	69569.600129	36.058612
1371.359083	69650.763957	36.063629
1372.809927	69713.744427	36.068647
1373.949997	69786.252963	36.073664
1375.330383	69854.608158	36.078682
1376.822553	69934.850593	36.083700
1378.106890	69998.212422	36.088717
1379.185120	70083.414923	36.093735
1380.959337	70157.022026	36.098752
1382.596379	70233.842281	36.103770
1383.854691	70304.997644	36.108788
1385.222746	70381.366520	36.113805
1386.467438	70457.412984	36.118823
1387.725819	70525.466092	36.123840
1389.158497	70610.386870	36.128858
1390.725485	70680.671734	36.133876
1391.870503	70765.448072	36.138893
1393.770264	70836.137200	36.143911
1395.532599	70897.615323	36.148928
1396.383696	70980.563963	36.153946
1397.891205	71056.279739	36.158964
1399.559148	71145.623502	36.163981
1400.887811	71206.296348	36.168999
1402.390081	71280.075842	36.174016
1403.749332	71364.415306	36.179034
1405.795242	71417.250652	36.184052
1406.970029	71500.783529	36.189069
1408.265016	71566.921177	36.194087
1409.833878	71632.040899	36.199104
1411.271867	71704.083845	36.204122
1412.771427	71759.766434	36.209140
1414.321507	71833.248700	36.214157
1415.895172	71901.344695	36.219175
1417.363635	71963.757900	36.224192
1418.301661	72021.137445	36.229210
1419.941535	72081.725609	36.234228
1421.412711	72156.854975	36.239245
1422.659116	72221.760658	36.244263
1424.287515	72283.845616	36.249280
1425.687207	72361.659189	36.254298
1427.048884	72411.766550	36.259316
1428.468818	72494.339620	36.264333
1429.823852	72555.188775	36.269351
1431.081174	72622.474884	36.274368
1432.477571	72699.226048	36.279386
1434.330197	72749.586516	36.284404
1435.644099	72826.046981	36.289421
1436.981292	72898.564941	36.294439
1438.293752	72951.252200	36.299456
1439.766648	73020.202807	36.304474
1440.909697	73068.597741	36.309492
1442.146086	73138.282301	36.314509
1443.635814	73173.627886	36.319527
1445.069794	73242.990476	36.324544
1446.251075	73301.525333	36.329562
1447.985147	73365.356877	36.334580
1449.230725	73433.115530	36.339597
1450.444002	73499.182150	36.344615
1452.105452	73562.366896	36.349632
1453.366691	73622.967198	36.354650
1454.780009	73686.431735	36.359668
1456.049453	73762.952525	36.364685
1457.245142	73837.154480	36.369703
1458.743150	73909.992023	36.374720
1460.439453	73984.128697	36.379738
1461.886436	74065.195125	36.384756
1463.199685	74150.221997	36.389773
1464.398907	74224.766471	36.394791
1466.019010	74300.689259	36.399808
1467.537432	74388.382744	36.404826
1469.489078	74459.681463	36.409844
1470.652651	74539.286365	36.414861
1472.373838	74621.996226	36.419879
1473.909585	74711.740059	36.424896
1475.758277	74788.401123	36.429914
1477.090037	74854.680556	36.434932
1478.472826	74938.204366	36.439949
1480.020350	75022.576665	36.444967
1481.788031	75098.161946	36.449984
1483.119090	75187.027390	36.455002
1484.730842	75252.833305	36.460020
1486.155050	75334.591157	36.465037
1487.892067	75412.614187	36.470055
1489.457577	75495.186435	36.475072
1490.469481	75571.309353	36.480090
1492.776374	75643.163641	36.485108
1493.940218	75714.322994	36.490125
1494.996831	75798.407214	36.495143
1496.061886	75879.830250	36.500160
1497.669797	75964.728074	36.505178
1499.821584	76051.517144	36.510196
1501.302363	76128.454959	36.515213
1503.057907	76211.899040	36.520231
1504.648596	76293.456396	36.525248
1506.287563	76363.757711	36.530266
1507.701114	76430.534918	36.535284
1509.217843	76510.204375	36.540301
1510.621356	76586.332193	36.545319
1512.019165	76660.104940	36.550336
1513.705424	76754.823057	36.555354
1515.214198	76819.914187	36.560372
1517.248073	76895.678189	36.565389
1518.623131	76970.253407	36.570407
1520.404238	77037.772649	36.575424
1521.799830	77121.719241	36.580442
1523.088786	77182.918616	36.585460
1524.701408	77261.422492	36.590477
1526.004224	77335.858002	36.595495
1527.602673	77401.835914	36.600512
1529.317109	77480.527172	36.605530
1530.821935	77547.292838	36.610548
1532.118539	77621.742769	36.615565
1533.318941	77700.375766	36.620583
1535.147338	77761.023289	36.625600
1536.603054	77843.822559	36.630618
1538.466622	77916.461684	36.635636
1540.078907	77998.907545	36.640653
1541.455606	78063.629602	36.645671
1543.063992	78110.845965	36.650688
1544.374848	78172.892908	36.655706
1545.765147	78227.706597	36.660724
1547.343075	78293.259150	36.665741
1548.157234	78355.371576	36.670759
1550.050213	78419.810976	36.675776
1551.576331	78493.416575	36.680794
1553.067672	78559.059326	36.685812
1554.213657	78632.623445	36.690829
1555.352420	78709.875445	36.695847
1557.427875	78774.819199	36.700864
1558.631981	78866.604967	36.705882
1560.407390	78947.102511	36.710900
1562.352998	79021.543344	36.715917
1563.697147	79105.149338	36.720935
1565.542031	79175.172288	36.725952
1567.028890	79258.173646	36.730970
1568.423037	79338.351939	36.735988
1570.311230	79422.659214	36.741005
1571.778471	79505.765736	36.746023
1573.201418	79580.543258	36.751040
1575.309294	79664.170770	36.756058
1576.406016	79740.013300	36.761076
1577.950094	79820.764969	36.766093
1579.291498	79913.090159	36.771111
1581.266397	80001.275045	36.776128
1582.862231	80080.271025	36.781146
1584.358580	80164.806584	36.786164
1586.209032	80252.517646	36.791181
1587.549344	80335.937912	36.796199
1589.453529	80416.634953	36.801216
1591.370064	80499.382735	36.806234
1592.683182	80589.434105	36.811252
1594.855840	80676.627306	36.816269
1596.395268	80744.130125	36.821287
1598.208631	80818.773858	36.826304
1599.926085	80898.690670	36.831322
1601.223535	80971.502450	36.836340
1603.154517	81047.129283	36.841357
1604.254873	81121.619354	36.846375
1606.337525	81194.739595	36.851392
1608.097383	81272.294275	36.856410
1609.669394	81346.369043	36.861428
1611.456856	81422.640172	36.866445
1612.819901	81508.340944	36.871463
1614.861693	81571.142646	36.876480
1616.148651	81651.775147	36.881498
1617.632856	81736.976198	36.886516
1619.421086	81810.562235	36.891533
1620.878580	81889.331580	36.896551
1622.453677	81960.455373	36.901568
1624.010110	82038.766201	36.906586
1625.656606	82125.729511	36.911604
1627.060263	82213.579995	36.916621
1628.670142	82291.084939	36.921639
1630.235205	82367.317417	36.926656
1632.058644	82450.009508	36.931674
1633.669271	82544.201772	36.936692
1635.527866	82612.672759	36.941709
1636.985519	82701.707321	36.946727
1638.379966	82769.782526	36.951744
1640.068783	82859.833050	36.956762
1641.887648	82942.375252	36.961780
1643.772095	83025.236864	36.966797
1644.892296	83104.885969	36.971815
1646.841595	83181.795400	36.976832
1648.477029	83266.267840	36.981850
1649.783564	83342.670111	36.986868
1651.471693	83408.432838	36.991885
1653.044757	83481.955537	36.996903
1654.595398	83547.765445	37.001920
1655.595426	83611.862428	37.006938
1656.918212	83693.356750	37.011956
1658.704919	83770.267878	37.016973
1660.339457	83864.486119	37.021991
1661.953440	83935.190645	37.027008
1663.614609	84022.322194	37.032026
1665.062758	84116.988579	37.037044
1667.113197	84204.946734	37.042061
1668.728781	84299.283414	37.047079
1670.308553	84386.821615	37.052096
1671.734993	84477.589884	37.057114
1673.684414	84574.612195	37.062132
1675.638084	84653.691688	37.067149
1677.005239	84751.464627	37.072167
1679.015042	84835.160854	37.077184
1680.548110	84927.472430	37.082202
1681.991337	85025.335764	37.087220
1683.846315	85128.241584	37.092237
1685.328703	85226.289544	37.097255
1687.973087	85325.182379	37.102272
1689.313041	85405.538439	37.107290
1690.590681	85502.770385	37.112308
1692.994728	85591.032250	37.117325
1694.995929	85690.964699	37.122343
1696.491477	85780.535118	37.127360
1698.244373	85862.842630	37.132378
1700.488915	85957.745242	37.137396
1702.379399	86036.977811	37.142413
1704.083342	86123.310700	37.147431
1705.704929	86202.801227	37.152448
1707.476167	86290.403945	37.157466
1709.159968	86382.620545	37.162484
1711.311338	86464.930767	37.167501
1712.513174	86550.659215	37.172519
1714.476537	86625.776238	37.177536
1716.507577	86706.990832	37.182554
1718.161270	86795.766633	37.187572
1719.404565	86879.715456	37.192589
1720.998239	86969.147459	37.197607
1722.853561	87053.127723	37.202624
1724.701616	87140.467532	37.207642
1726.608236	87229.281103	37.212660
1728.323162	87304.844271	37.217677
1729.901914	87402.707080	37.222695
1731.048910	87494.859133	37.227712
1733.367124	87580.276496	37.232730
1734.994082	87670.199662	37.237748
1736.681256	87752.687542	37.242765
1738.082674	87840.568221	37.247783
1740.083074	87930.940649	37.252800
1741.807638	88031.874866	37.257818
1743.662787	88120.471082	37.262836
1745.538140	88212.245273	37.267853
1747.592949	88295.716313	37.272871
1749.152164	88381.647644	37.277888
1751.474083	88472.148839	37.282906
1753.139514	88547.520184	37.287924
1754.822177	88623.814151	37.292941
1756.303349	88715.879709	37.297959
1757.954203	88795.474078	37.302976
1759.497861	88869.559979	37.307994
1761.759935	88963.988025	37.313012
1763.548636	89049.581231	37.318029
1764.862808	89140.267523	37.323047
1766.397944	89214.254235	37.328064
1768.278349	89288.592643	37.333082
1769.870797	89364.877292	37.338100
1771.249520	89438.673595	37.343117
1773.045746	89509.388491	37.348135
1774.531337	89578.656710	37.353152
1776.301568	89666.054202	37.358170
1777.831463	89751.994095	37.363188
1779.246493	89832.211127	37.368205
1781.193967	89936.969689	37.373223
1782.589445	90027.012282	37.378240
1784.304708	90125.293636	37.383258
1786.335087	90221.333461	37.388276
1788.362588	90318.425960	37.393293
1790.029000	90412.292787	37.398311
1791.863272	90518.528579	37.403328
1793.498410	90613.757024	37.408346
1795.601887	90723.804252	37.413364
1797.507427	90815.277583	37.418381
1799.356920	90903.287309	37.423399
1801.119432	91010.879508	37.428416
1803.354728	91114.088942	37.433434
1804.912116	91217.062614	37.438452
1806.753415	91312.539840	37.443469
1808.396467	91411.166228	37.448487
1810.702146	91512.667679	37.453504
1812.897121	91605.289491	37.458522
1814.566706	91711.339802	37.463540
1816.188514	91798.234412	37.468557
1818.011032	91896.542791	37.473575
1819.728473	91996.262115	37.478592
1821.657660	92103.451892	37.483610
1823.873975	92205.831514	37.488628
1825.766466	92308.414250	37.493645
1827.325788	92402.696937	37.498663
1829.320472	92510.613025	37.503680
1831.342244	92601.921481	37.508698
1833.137266	92702.442158	37.513716
1834.848613	92804.256407	37.518733
1836.836442	92909.209096	37.523751
1838.888103	92999.132516	37.528768
1840.856025	93093.936443	37.533786
1842.507749	93188.295823	37.538804
1844.155589	93290.451177	37.543821
1846.294128	93401.339184	37.548839
1847.952961	93509.184607	37.553856
1849.868797	93593.148424	37.558874
1851.698220	93699.839743	37.563892
1853.241247	93805.118609	37.568909
1855.246515	93906.193395	37.573927
1857.022632	94017.343142	37.578944
1859.142562	94112.227832	37.583962
1860.866472	94222.156988	37.588980
1862.965979	94319.136936	37.593997
1864.794775	94429.050416	37.599015
1866.483954	94538.212934	37.604032
1868.675669	94633.404880	37.609050
1870.471335	94730.294234	37.614068
1871.911384	94836.011021	37.619085
1874.097887	94933.980654	37.624103
1875.432280	95039.638614	37.629120
1877.136768	95151.589536	37.634138
1879.485914	95256.633119	37.639156
1881.356348	95362.106889	37.644173
1883.215999	95468.039033	37.649191
1884.950615	95580.278326	37.654208
1887.059731	95680.987733	37.659226
1888.750470	95792.588185	37.664244
1890.585421	95890.235563	37.669261
1892.076601	95983.310293	37.674279
1893.736921	96075.572917	37.679296
1895.375880	96166.140560	37.684314
1897.080409	96274.470141	37.689332
1898.948714	96376.765961	37.694349
1900.691016	96484.266405	37.699367
1902.354668	96583.818831	37.704384
1904.209829	96696.968631	37.709402
1905.791764	96815.447631	37.714420
1907.750872	96928.772144	37.719437
1909.722765	97045.479675	37.724455
1911.573104	97164.526456	37.729472
1914.021924	97294.584688	37.734490
1915.678271	97409.403429	37.739508
1917.721991	97528.484704	37.744525
1919.732798	97648.268794	37.749543
1921.296979	97780.926728	37.754560
1923.588293	97897.802926	37.759578
1925.448316	98021.478439	37.764596
1927.340638	98142.309757	37.769613
1929.585527	98270.172771	37.774631
1931.338999	98412.412834	37.779648
1933.204953	98526.530931	37.784666
1935.461327	98654.000699	37.789684
1937.230729	98789.090071	37.794701
1938.861537	98916.531998	37.799719
1940.780793	99047.200026	37.804736
1943.189868	99182.799472	37.809754
1944.879691	99319.209290	37.814772
1946.672836	99455.324616	37.819789
1948.859688	99596.107604	37.824807
1950.721019	99726.280357	37.829824
1952.894893	99872.391136	37.834842
1954.684111	100010.030725	37.839860
1956.640752	100148.253232	37.844877
1958.759385	100287.997664	37.849895
1960.586059	100430.691595	37.854912
1963.044103	100565.528525	37.859930
1965.295870	100712.822624	37.864948
1966.520028	100854.142056	37.869965
1968.726292	100970.789181	37.874983
1970.858734	101126.775573	37.880000
1972.927696	101262.132681	37.885018
1975.238961	101399.442907	37.890036
1977.463326	101533.179375	37.895053
1979.311972	101664.655056	37.900071
1980.821096	101800.456982	37.905088
1983.236491	101931.299885	37.910106
1985.398935	102069.472979	37.915124
1987.409438	102205.489732	37.920141
1989.303948	102344.289114	37.925159
1991.431677	102474.748122	37.930176
1993.128875	102602.422323	37.935194
1995.637139	102749.013477	37.940212
1997.413688	102870.894822	37.945229
1999.571125	103002.986825	37.950247
2001.502418	103131.057516	37.955264
2003.819758	103265.952925	37.960282
2005.603328	103398.548763	37.965300
2007.274493	103527.587247	37.970317
2009.686718	103655.914365	37.975335
2011.240495	103788.801294	37.980352
2013.180165	103927.980613	37.985370
2015.244339	104064.300896	37.990388
2017.046881	104207.953230	37.995405
2019.068588	104338.182564	38.000423
2020.739372	104484.620784	38.005440
2022.639130	104620.474563	38.010458
2024.696148	104745.831070	38.015476
2026.358779	104874.559099	38.020493
2028.650466	104996.570479	38.025511
2030.339865	105124.940250	38.030528
2032.152477	105246.571030	38.035546
2033.949165	105384.536157	38.040564
2035.581266	105532.595304	38.045581
2038.125864	105666.323646	38.050599
2039.509016	105804.520026	38.055616
2041.835429	105958.431918	38.060634
2043.513470	106101.972321	38.065652
2045.334300	106255.774466	38.070669
2047.469547	106416.451422	38.075687
2049.258661	106581.507212	38.080704
2051.353072	106740.594388	38.085722
2053.545819	106894.797706	38.090740
2055.540271	107074.672307	38.095757
2057.793941	107225.887712	38.100775
2059.632013	107394.274692	38.105792
2061.708072	107571.717166	38.110810
2063.676923	107740.770124	38.115828
2065.525553	107914.496504	38.120845
2067.647349	108091.287781	38.125863
2069.577329	108282.058791	38.130880
2071.587879	108462.026872	38.135898
2073.924373	108646.205661	38.140916
2076.483711	108836.957333	38.145933
2078.119952	109019.776672	38.150951
2080.185347	109195.187478	38.155968
2082.492019	109382.202703	38.160986
2084.496972	109556.787823	38.166004
2086.695139	109758.342018	38.171021
2088.767338	109935.010910	38.176039
2090.873365	110136.936769	38.181056
2093.146682	110330.011296	38.186074
2095.676994	110506.319702	38.191092
2097.576520	110698.085116	38.196109
2099.782449	110879.658281	38.201127
2102.109681	111070.077939	38.206144
2104.450272	111243.769214	38.211162
2106.727336	111432.258344	38.216180
2108.958884	111602.975509	38.221197
2110.818286	111790.580735	38.226215
2113.003552	111968.421493	38.231232
2115.181824	112155.978744	38.236250
2117.441930	112347.962942	38.241268
2119.143262	112526.579705	38.246285
2121.882281	112705.618385	38.251303
2123.806341	112889.871103	38.256320
2125.932527	113073.839486	38.261338
2128.482314	113255.244074	38.266356
2130.048277	113438.667836	38.271373
2132.348411	113612.288116	38.276391
2134.593632	113795.125463	38.281408
2136.927871	113977.112739	38.286426
2139.259526	114160.001808	38.291444
2140.948085	114348.128984	38.296461
2143.449136	114528.025594	38.301479
2145.423082	114699.343050	38.306496
2147.599231	114872.861893	38.311514
2149.900639	115050.826424	38.316532
2151.763640	115237.637185	38.321549
2153.978160	115409.300804	38.326567
2155.614009	115598.977300	38.331584
2158.112678	115781.417073	38.336602
2160.515396	115967.868047	38.341620
2162.396824	116148.706614	38.346637
2164.538661	116319.066733	38.351655
2166.554911	116490.461971	38.356672
2168.055932	116656.611455	38.361690
2170.542928	116817.343664	38.366708
2172.150174	116985.862535	38.371725
2174.286277	117164.015259	38.376743
2176.131542	117346.146347	38.381760
2177.973678	117533.276296	38.386778
2180.149222	117713.049000	38.391796
2182.107811	117916.689948	38.396813
2184.462508	118095.624661	38.401831
2186.648674	118276.337010	38.406848
2188.776497	118483.468061	38.411866
2191.143971	118675.037076	38.416884
2193.054123	118878.107278	38.421901
2194.973349	119080.783921	38.426919
2196.991296	119285.285455	38.431936
2199.535808	119492.483635	38.436954
2202.106720	119691.027833	38.441972
2204.488670	119903.670033	38.446989
2206.651347	120120.140479	38.452007
2209.057601	120315.402912	38.457024
2211.481787	120526.291415	38.462042
2213.613958	120728.727771	38.467060
2215.588624	120941.084209	38.472077
2217.837722	121149.200076	38.477095
2220.084415	121356.556314	38.482112
2222.235270	121574.977557	38.487130
2224.648734	121792.077708	38.492148
2226.690571	122006.903076	38.497165
2229.011608	122222.244100	38.502183
2231.334421	122449.218716	38.507200
2233.363245	122670.760419	38.512218
2235.608855	122895.339395	38.517236
2237.793818	123124.559452	38.522253
2239.816040	123352.093696	38.527271
2242.000835	123577.421818	38.532288
2243.701396	123811.643759	38.537306
2246.257618	124054.131407	38.542324
2248.553076	124294.733016	38.547341
2250.728840	124540.048705	38.552359
2253.200261	124777.682456	38.557376
2255.457488	125018.395852	38.562394
2257.920108	125253.001717	38.567412
2259.897867	125497.694487	38.572429
2262.173564	125739.233888	38.577447
2264.555016	125981.582810	38.582464
2266.926285	126224.467605	38.587482
2269.495452	126471.509542	38.592500
2271.523415	126715.897252	38.597517
2273.889360	126960.525336	38.602535
2276.148986	127208.165652	38.607552
2278.509958	127454.205698	38.612570
2280.428627	127689.963610	38.617588
2282.514577	127933.182197	38.622605
2284.794338	128191.342994	38.627623
2287.387843	128445.091812	38.632640
2289.524829	128691.021933	38.637658
2291.556949	128941.791189	38.642676
2293.667299	129204.767941	38.647693
2296.383636	129453.923359	38.652711
2298.688410	129696.978336	38.657728
2300.824640	129963.698655	38.662746
2303.858023	130207.657595	38.667764
2306.167409	130459.826176	38.672781
2308.832436	130695.636346	38.677799
2311.181542	130941.127581	38.682816
2313.166903	131182.096651	38.687834
2315.819086	131415.248230	38.692852
2317.736092	131631.729307	38.697869
2319.765641	131860.996528	38.702887
2322.210073	132081.724106	38.707904
2323.967489	132301.837026	38.712922
2326.352718	132523.020197	38.717940
2328.251147	132770.812786	38.722957
2330.312350	133005.752919	38.727975
2332.379550	133242.584010	38.732992
2334.738586	133489.547248	38.738010
2337.142227	133729.525926	38.743028
2339.210934	133997.220506	38.748045
2341.501045	134247.269498	38.753063
2343.822648	134501.857708	38.758080
2345.770646	134764.601588	38.763098
2348.512966	135033.313645	38.768116
2350.284445	135311.417106	38.773133
2352.847286	135565.973596	38.778151
2355.071186	135851.889800	38.783168
2357.134748	136131.995625	38.788186
2359.650705	136404.811920	38.793204
2361.982407	136691.972808	38.798221
2364.614871	136968.923814	38.803239
2366.877540	137268.839784	38.808256
2369.272714	137557.265135	38.813274
2371.861140	137860.204974	38.818292
2374.314639	138144.563993	38.823309
2376.875587	138432.524676	38.828327
2379.437391	138727.492094	38.833344
2381.368937	139022.141171	38.838362
2384.368878	139306.079102	38.843380
2386.478140	139601.833450	38.848397
2389.197091	139886.427963	38.853415
2391.522131	140181.149591	38.858432
2393.619188	140474.220814	38.863450
2396.208251	140776.544703	38.868468
2398.324376	141080.467396	38.873485
2400.921170	141379.138835	38.878503
2403.633414	141681.017614	38.883520
2406.102492	141992.137469	38.888538
2408.924880	142275.473457	38.893556
2410.960028	142575.509215	38.898573
2413.036585	142880.160026	38.903591
2415.749475	143188.012981	38.908608
2417.681532	143495.799619	38.913626
2420.143433	143808.226598	38.918644
2422.559325	144116.690191	38.923661
2424.988950	144437.985029	38.928679
2427.370157	144740.226158	38.933696
2429.805474	145066.702429	38.938714
2432.018449	145381.462673	38.943732
2434.407051	145696.349693	38.948749
2436.965974	146017.659686	38.953767
2439.608224	146341.129047	38.958784
2441.923906	146667.481936	38.963802
2444.171533	146985.914701	38.968820
2446.570374	147313.515201	38.973837
2449.374539	147627.130485	38.978855
2452.287538	147925.232776	38.983872
2455.156014	148238.042006	38.988890
2458.052167	148544.045366	38.993908
2461.273419	148832.584890	38.998925
2463.748830	149134.697262	39.003943
2466.835590	149421.077805	39.008960
2469.229862	149699.964992	39.013978
2471.779716	149983.652715	39.018996
2473.705734	150272.212191	39.024013
2476.192136	150562.183359	39.029031
2479.226137	150825.947324	39.034048
2481.437801	151081.730056	39.039066
2484.001252	151344.173840	39.044084
2486.555781	151593.799724	39.049101
2488.267981	151851.111229	39.054119
2490.268179	152115.855481	39.059136
2492.098295	152383.661413	39.064154
2494.414782	152669.430510	39.069172
2496.390398	152953.172580	39.074189
2498.313996	153248.805783	39.079207
2500.314245	153548.719130	39.084224
2502.182489	153862.516686	39.089242
2504.407071	154193.410080	39.094260
2507.116740	154520.675111	39.099277
2508.872213	154861.052180	39.104295
2511.144506	155205.755370	39.109312
2513.135348	155553.322805	39.114330
2515.317049	155898.387010	39.119348
2517.962596	156267.640149	39.124365
2520.099448	156645.810696	39.129383
2522.332003	157026.545726	39.134400
2524.193543	157430.814070	39.139418
2526.824621	157805.017314	39.144436
2529.535695	158206.301606	39.149453
2531.821742	158613.609052	39.154471
2534.328520	159029.707864	39.159488
2537.185088	159437.185440	39.164506
2539.662668	159848.622464	39.169524
2542.285589	160256.890993	39.174541
2544.858632	160680.138047	39.179559
2547.234514	161096.905913	39.184576
2549.247420	161521.046027	39.189594
2552.315452	161945.899923	39.194612
2554.852830	162383.611702	39.199629
2557.568462	162827.684633	39.204647
2559.853685	163257.252819	39.209664
2562.557351	163708.951235	39.214682
2565.180123	164145.874264	39.219700
2567.961940	164591.231028	39.224717
2570.312652	165034.690233	39.229735
2573.439514	165477.662740	39.234752
2576.072413	165927.546145	39.239770
2578.594044	166354.976822	39.244788
2581.362172	166796.071355	39.249805
2584.090095	167241.453792	39.254823
2586.798964	167677.395544	39.259840
2589.526248	168125.081797	39.264858
2592.155442	168564.647391	39.269876
2595.012001	169002.491391	39.274893
2597.714503	169442.825390	39.279911
2601.046315	169881.260597	39.284928
2603.738339	170315.875005	39.289946
2605.886438	170746.298002	39.294964
2608.431503	171186.565434	39.299981
2610.645405	171624.068372	39.304999
2613.655824	172060.496917	39.310016
2615.883782	172524.578993	39.315034
2618.275779	172961.185559	39.320052
2620.978715	173416.056257	39.325069
2623.467534	173870.493252	39.330087
2626.304763	174308.116977	39.335104
2628.324568	174766.124389	39.340122
2631.048943	175219.122706	39.345140
2633.475854	175669.452647	39.350157
2635.686273	176148.313888	39.355175
2638.567318	176614.755578	39.360192
2640.845298	177073.827507	39.365210
2643.832831	177537.083038	39.370228
2646.638457	177991.759900	39.375245
2649.391810	178436.720176	39.380263
2651.976103	178868.172351	39.385280
2654.398888	179303.055174	39.390298
2656.723090	179745.447852	39.395316
2659.342954	180177.002415	39.400333
2661.844223	180640.502744	39.405351
2664.295406	181082.958290	39.410368
2667.414176	181533.134170	39.415386
2669.897492	181985.976837	39.420404
2672.325521	182433.369673	39.425421
2674.544442	182977.616477	39.430439
2677.591158	183443.153405	39.435456
2679.950748	183922.794752	39.440474
2682.441053	184394.925308	39.445492
2684.610767	184868.022603	39.450509
2686.732200	185371.888025	39.455527
2689.526282	185860.487358	39.460544
2692.232666	186369.473021	39.465562
2694.816909	186886.277906	39.470580
2697.286041	187381.234222	39.475597
2699.926199	187915.459478	39.480615
2702.458679	188430.298679	39.485632
2705.174325	188954.941422	39.490650
2707.826660	189487.572150	39.495668
2710.754334	190021.584713	39.500685
2713.155996	190571.328623	39.505703
2716.177527	191104.975857	39.510720
2718.781293	191643.212117	39.515738
2721.433180	192202.271804	39.520756
2724.586806	192751.044424	39.525773
2727.055966	193306.556134	39.530791
2729.776683	193852.124514	39.535808
2732.864474	194413.259470	39.540826
2735.408984	194976.894892	39.545844
2738.163309	195523.099936	39.550861
2740.623721	196096.481863	39.555879
2743.579365	196659.678867	39.560896
2746.215010	197232.021931	39.565914
2748.592739	197803.721734	39.570932
2751.971280	198373.362069	39.575949
2754.728643	198955.599449	39.580967
2757.467884	199524.759799	39.585984
2760.534133	200092.651745	39.591002
2763.572366	200662.937869	39.596020
2766.867804	201224.244118	39.601037
2769.856872	201802.924561	39.606055
2772.485447	202360.706277	39.611072
2775.554545	202915.601159	39.616090
2778.335508	203487.765763	39.621108
2780.919538	204041.266532	39.626125
2783.694506	204616.051949	39.631143
2786.384162	205177.769918	39.636160
2789.039538	205753.517204	39.641178
2791.521156	206337.041156	39.646196
2794.247603	206909.503474	39.651213
2796.697356	207500.554808	39.656231
2799.369225	208080.903590	39.661248
2802.463647	208671.018755	39.666266
2805.220983	209255.726345	39.671284
2808.969817	209820.313176	39.676301
2811.684289	210395.579992	39.681319
2815.125157	210961.665374	39.686336
2818.323699	211525.274830	39.691354
2821.425065	212087.401744	39.696372
2824.335342	212637.315029	39.701389
2827.191747	213198.821733	39.706407
2830.366350	213751.769372	39.711424
2832.942942	214286.088859	39.716442
2835.848104	214814.514865	39.721460
2838.454681	215324.570538	39.726477
2841.169249	215843.298060	39.731495
2843.758282	216368.650835	39.736512
2846.351177	216887.220772	39.741530
2848.876980	217407.376795	39.746548
2851.818952	217939.865367	39.751565
2854.513656	218477.905775	39.756583
2857.051345	219011.804968	39.761600
2859.738837	219559.221494	39.766618
2861.886145	220113.505788	39.771636
2864.926744	220663.357487	39.776653
2867.623583	221233.942175	39.781671
2869.915980	221802.634321	39.786688
2872.765842	222371.722237	39.791706
2875.165636	222971.187825	39.796724
2877.691952	223570.913273	39.801741
2880.122660	224166.792400	39.806759
2883.068627	224779.027486	39.811776
2885.370013	225402.998493	39.816794
2888.254868	226028.351676	39.821812
2890.630521	226657.442606	39.826829
2893.358732	227308.300365	39.831847
2896.597397	227948.789437	39.836864
2899.846769	228594.865456	39.841882
2902.594259	229258.624620	39.846900
2905.482819	229899.675500	39.851917
2908.184757	230559.300019	39.856935
2911.318207	231220.787194	39.861952
2914.521140	231883.939524	39.866970
2916.752026	232568.201390	39.871988
2920.176382	233228.497737	39.877005
2923.013794	233918.632937	39.882023
2925.816729	234591.066058	39.887040
2928.963621	235271.395738	39.892058
2931.547527	235972.617982	39.897076
2934.446902	236663.247073	39.902093
2937.484306	237363.328802	39.907111
2939.871423	238059.319182	39.912128
2943.257679	238760.257903	39.917146
2945.781161	239480.382517	39.922164
2949.020028	240184.821172	39.927181
2951.792908	240894.767196	39.932199
2954.829288	241617.447923	39.937216
2957.844802	242331.645158	39.942234
2960.686650	243056.638335	39.947252
2963.727595	243781.775907	39.952269
2966.689147	244518.304026	39.957287
2969.478514	245241.824852	39.962304
2973.050079	245968.929599	39.967322
2975.924893	246690.958480	39.972340
2979.125851	247409.834510	39.977357
2982.448440	248136.334858	39.982375
2985.971172	248857.491858	39.987392
2989.391318	249563.547555	39.992410
2992.922565	250281.826744	39.997428
2995.963711	250982.499600	40.002445
2999.224933	251691.771600	40.007463
3001.839916	252394.536933	40.012480
3004.943509	253097.324184	40.017498
3007.827236	253795.620973	40.022516
3010.639428	254506.905671	40.027533
3013.410024	255209.480605	40.032551
3016.533322	255925.332376	40.037568
3019.567653	256648.255696	40.042586
3022.265025	257360.432316	40.047604
3025.078630	258070.224504	40.052621
3028.413273	258773.454014	40.057639
3031.220422	259459.032438	40.062656
3034.627550	260122.541838	40.067674
3037.170692	260808.610927	40.072692
3040.044171	261483.321258	40.077709
3043.056624	262167.479964	40.082727
3045.540229	262853.952310	40.087744
3048.539096	263543.768681	40.092762
3051.138336	264252.591006	40.097780
3054.341997	264953.135479	40.102797
3057.051095	265657.689364	40.107815
3059.772730	266389.336930	40.112832
3062.444743	267109.201895	40.117850
3065.329912	267855.975972	40.122868
3068.096357	268587.676236	40.127885
3071.392591	269348.495730	40.132903
3073.696391	270102.835326	40.137920
3076.957160	270861.869977	40.142938
3079.779684	271639.786197	40.147956
3083.156000	272410.167572	40.152973
3086.263921	273186.145993	40.157991
3088.894730	273976.210935	40.163008
3091.851727	274764.261895	40.168026
3094.785019	275567.699141	40.173044
3097.798578	276365.249413	40.178061
3101.349251	277171.367671	40.183079
3103.982879	277993.594796	40.188096
3107.428674	278806.543929	40.193114
3110.327732	279632.089568	40.198132
3113.203585	280451.179526	40.203149
3116.808983	281281.319841	40.208167
3119.703494	282118.011942	40.213184
3122.802952	282946.079159	40.218202
3126.072550	283795.212029	40.223220
3129.173716	284636.590598	40.228237
3132.957932	285476.201529	40.233255
3135.914708	286321.771713	40.238272
3139.430792	287160.387857	40.243290
3142.630246	288016.690175	40.248308
3145.896239	288858.142171	40.253325
3149.447936	289690.194503	40.258343
3152.871405	290529.593907	40.263360
3156.402322	291371.351944	40.268378
3159.616181	292211.624667	40.273396
3162.884698	293031.286127	40.278413
3166.748234	293872.627540	40.283431
3169.590618	294694.516336	40.288448
3173.219938	295528.609516	40.293466
3176.749563	296347.701771	40.298484
3180.123464	297170.030960	40.303501
3183.360928	297980.462757	40.308519
3186.395730	298813.280718	40.313536
3189.663754	299624.496239	40.318554
3192.489419	300444.958846	40.323572
3195.726495	301274.864514	40.328589
3198.884201	302085.552757	40.333607
3202.285346	302927.211439	40.338624
3205.671880	303752.181017	40.343642
3208.635364	304577.254413	40.348660
3211.694893	305397.984252	40.353677
3214.900366	306226.648516	40.358695
3217.509644	307064.581114	40.363712
3220.817687	307894.217092	40.368730
3224.186543	308728.322301	40.373748
3227.242407	309556.928931	40.378765
3230.637023	310399.707448	40.383783
3233.335817	311245.016514	40.388800
3236.458625	312079.939673	40.393818
3239.152996	312919.508789	40.398836
3242.582613	313742.273303	40.403853
3245.961438	314566.832993	40.408871
3249.071304	315376.827013	40.413888
3251.992407	316193.434417	40.418906
3255.230684	316996.197147	40.423924
3258.355325	317808.251286	40.428941
3261.785145	318628.744022	40.433959
3264.985769	319463.721767	40.438976
3267.841706	320287.800234	40.443994
3271.187015	321129.955213	40.449012
3274.474215	321978.091089	40.454029
3277.616412	322801.771555	40.459047
3281.076981	323660.579714	40.464064
3284.521535	324502.017123	40.469082
3288.106798	325350.697315	40.474100
3291.059652	326213.743343	40.479117
3294.271490	327071.681424	40.484135
3297.403659	327935.245993	40.489152
3300.814176	328813.234935	40.494170
3303.863346	329683.979537	40.499188
3307.192909	330566.812898	40.504205
3310.363769	331449.067432	40.509223
3313.290599	332345.799826	40.514240
3316.837273	333244.139175	40.519258
3319.939072	334157.087452	40.524276
3322.729611	335054.664591	40.529293
3326.112308	335977.112898	40.534311
3329.371918	336885.961499	40.539328
3333.092241	337804.480824	40.544346
3336.701171	338732.099928	40.549364
3340.252540	339653.287109	40.554381
3344.028234	340576.266846	40.559399
3347.284212	341507.825349	40.564416
3351.082287	342430.676806	40.569434
3354.355383	343357.821056	40.574452
3357.585768	344280.965516	40.579469
3361.298634	345208.625014	40.584487
3364.694467	346127.154243	40.589504
3368.558847	347054.637936	40.594522
3372.027622	347990.145250	40.599540
3375.208831	348900.137112	40.604557
3379.135911	349834.835886	40.609575
3382.323953	350757.503718	40.614592
3385.760678	351675.922935	40.619610
3389.152982	352612.019710	40.624628
3392.035403	353544.594006	40.629645
3395.657022	354471.853468	40.634663
3398.958229	355426.185615	40.639680
3401.955097	356364.109006	40.644698
3405.394737	357306.168230	40.649716
3408.806124	358255.300779	40.654733
3412.016585	359204.663404	40.659751
3415.357039	360168.956352	40.664768
3418.791256	361110.214377	40.669786
3422.041608	362073.218265	40.674804
3425.508085	363032.836950	40.679821
3428.890227	364008.201678	40.684839
3432.035568	364969.404023	40.689856
3435.500765	365938.938304	40.694874
3439.207892	366903.967428	40.699892
3442.480121	367874.429656	40.704909
3446.157524	368834.836890	40.709927
3449.683325	369819.408672	40.714944
3453.416784	370789.774797	40.719962
3456.780995	371758.593994	40.724980
3460.551021	372729.190780	40.729997
3464.631824	373683.794070	40.735015
3468.032367	374623.564170	40.740020
3471.421486	375537.525387	40.745024
3474.772111	376390.811897	40.750029
3478.092854	377201.078881	40.755034
3481.250839	377957.608257	40.760039
3483.895988	378672.420551	40.765044
3486.656043	379330.183936	40.770048
3489.573728	379919.595419	40.775053
3491.496524	380479.793919	40.780058
3494.255850	380970.043344	40.785063
3496.792781	381417.607424	40.790068
3499.285274	381819.794301	40.795072
3501.238913	382147.558502	40.800077
3503.009389	382442.210729	40.805082
3505.159827	382700.921773	40.810087
3506.831971	382914.939874	40.815092
3508.025670	383092.391382	40.820096
3509.611556	383214.681571	40.825101
3510.632870	383314.766087	40.830106
3512.123172	383376.182586	40.835111
3513.346012	383420.400290	40.840116
3514.247943	383425.210562	40.845120
3515.251501	383419.543869	40.850125
3516.003957	383369.177498	40.855130
3516.869473	383306.402510	40.860135
3517.448799	383214.142197	40.865140
3518.227164	383114.588536	40.870144
3518.934137	382982.493899	40.875149
3519.170941	382855.651961	40.880154
3519.839140	382694.691734	40.885159
3520.286038	382534.958518	40.890164
3520.818985	382339.204987	40.895168
3521.279708	382148.336573	40.900173
3521.613660	381955.429786	40.905178
3521.864273	381734.678900	40.910183
3521.751296	381511.875373	40.915188
3522.137596	381272.714927	40.920192
3522.438641	381036.587416	40.925197
3522.438359	380804.720202	40.930202
3522.838262	380535.738851	40.935207
3523.023588	380273.720856	40.940212
3522.996001	380010.108292	40.945216
3523.009665	379745.115326	40.950221
3523.044118	379473.437603	40.955226
3523.196129	379188.203118	40.960231
3523.115102	378911.966545	40.965236
3522.907449	378634.273937	40.970240
3523.576248	378346.511601	40.975245
3523.478318	378060.465972	40.980250
3523.224129	377758.086377	40.985255
3523.060170	377468.895550	40.990260
3523.011777	377170.134244	40.995264
3523.170999	376877.457894	41.000269
3523.057270	376590.738654	41.005274
3522.911674	376285.760279	41.010279
3522.698225	375997.856603	41.015284
3522.919778	375698.274774	41.020288
3522.672573	375401.124985	41.025293
3522.796075	375105.742703	41.030298
3522.589992	374806.598844	41.035303
3522.401147	374508.744371	41.040308
3522.377368	374213.096018	41.045312
3522.290899	373912.856846	41.050317
3521.959923	373615.776846	41.055322
3521.542451	373314.617643	41.060327
3521.509746	373030.718402	41.065332
3521.404765	372746.573518	41.070336
3521.692354	372447.504496	41.075341
3521.209599	372170.499736	41.080346
3521.245391	371881.319807	41.085351
3521.151973	371604.578745	41.090356
3520.769479	371311.978171	41.095360
3520.730145	371026.509848	41.100365
3520.531282	370744.340529	41.105370
3520.415051	370467.871172	41.110375
3520.367977	370193.522168	41.115380
3520.400482	369917.024124	41.120384
3519.908739	369642.307385	41.125389
3519.686926	369376.386441	41.130394
3519.975455	369100.729503	41.135399
3519.595046	368824.031244	41.140404
3519.500245	368559.657850	41.145408
3519.391734	368279.964796	41.150413
3519.004425	368028.411006	41.155418
3519.152012	367757.259813	41.160423
3519.173566	367505.281808	41.165428
3518.867925	367245.654675	41.170432
3519.211160	366977.463423	41.175437
3518.287638	366730.707624	41.180442
3518.763251	366460.305882	41.185447
3517.973871	366212.178099	41.190452
3517.772608	365949.651942	41.195456
3518.109508	365709.829796	41.200461
3517.408611	365464.425766	41.205466
3517.620988	365218.953106	41.210471
3517.389029	364974.208450	41.215476
3517.395602	364733.007021	41.220480
3517.138023	364489.786801	41.225485
3516.932893	364266.400597	41.230490
3516.963322	364021.098750	41.235495
3516.874910	363791.058933	41.240500
3516.574644	363558.204584	41.245504
3516.408430	363327.639704	41.250509
3516.105524	363102.684537	41.255514
3516.302305	362866.596204	41.260519
3516.025240	362639.676902	41.265524
3515.710950	362426.152932	41.270528
3515.751073	362202.458628	41.275533
3515.609006	361984.660998	41.280538
3515.605579	361771.312417	41.285543
3515.334417	361559.630475	41.290548
3515.188307	361351.662936	41.295552
3514.913308	361136.319371	41.300557
3514.577935	360924.846262	41.305562
3514.940793	360715.956153	41.310567
3514.927885	360509.359592	41.315572
3514.447286	360304.867699	41.320576
3514.420947	360105.944934	41.325581
3514.150141	359902.281531	41.330586
3514.113552	359700.308197	41.335591
3514.008378	359509.907070	41.340596
3513.847582	359321.724371	41.345600
3513.875754	359131.528738	41.350605
3513.396000	358941.055536	41.355610
3513.450378	358742.060372	41.360615
3513.272770	358556.976009	41.365620
3513.241577	358379.974624	41.370624
3513.046267	358186.682140	41.375629
3512.807541	358007.830416	41.380634
3512.689971	357820.419529	41.385639
3512.569112	357653.542821	41.390644
3512.369039	357480.247723	41.395648
3512.673369	357311.650745	41.400653
3512.165305	357132.454812	41.405658
3512.244695	356964.551887	41.410663
3512.508055	356795.907667	41.415668
3512.294700	356629.116120	41.420672
3512.355850	356461.060823	41.425677
3512.101743	356302.508458	41.430682
3511.855748	356117.267624	41.435687
3511.974679	355955.757789	41.440692
3511.570871	355793.083461	41.445696
3511.833817	355628.753669	41.450701
3511.254891	355474.416093	41.455706
3511.524651	355324.367505	41.460711
3511.240334	355164.314512	41.465716
3511.338661	355012.613749	41.470720
3511.154220	354849.925634	41.475725
3511.328730	354703.726882	41.480730
3511.251819	354545.773317	41.485735
3511.079051	354391.138159	41.490740
3510.917347	354240.541838	41.495744
3510.953071	354092.811501	41.500749
3510.666627	353940.504876	41.505754
3510.769165	353791.720574	41.510759
3510.551457	353657.194088	41.515764
3510.022752	353500.983492	41.520768
3510.394805	353357.416488	41.525773
3510.001874	353227.948310	41.530778
3509.971533	353095.474424	41.535783
3509.792627	352957.482051	41.540788
3509.828902	352819.989224	41.545792
3509.862535	352682.547054	41.550797
3509.483738	352563.190483	41.555802
3509.479619	352425.371832	41.560807
3509.326361	352304.987712	41.565812
3508.941865	352181.334847	41.570816
3509.268973	352046.538457	41.575821
3509.026937	351925.785509	41.580826
3508.942737	351804.219440	41.585831
3508.760987	351688.489155	41.590836
3508.902456	351563.887434	41.595840
3508.769685	351446.140498	41.600845
3508.555449	351325.609726	41.605850
3508.519593	351217.252004	41.610855
3508.360210	351100.397651	41.615860
3508.267419	350987.294585	41.620864
3508.456587	350875.443455	41.625869
3507.859797	350766.460163	41.630874
3507.812817	350662.906686	41.635879
3507.633505	350563.237417	41.640884
3507.745531	350462.632590	41.645888
3507.991881	350355.905599	41.650893
3507.973731	350256.616918	41.655898
3507.605644	350140.274721	41.660903
3507.949711	350044.818087	41.665908
3507.628302	349942.398301	41.670912
3507.866393	349830.383406	41.675917
3507.526485	349741.413395	41.680922
3507.401278	349644.300348	41.685927
3507.286028	349553.438986	41.690932
3506.963288	349448.450353	41.695936
3507.258737	349357.778451	41.700941
3507.110309	349267.862061	41.705946
3507.099908	349171.390612	41.710951
3506.787304	349083.634761	41.715956
3507.225083	348984.779367	41.720960
3507.185329	348895.556765	41.725965
3506.941640	348809.518060	41.730970
3507.156294	348716.467407	41.735975
3506.929906	348629.840835	41.740980
3507.030119	348537.163469	41.745984
3507.278490	348442.962801	41.750989
3506.856672	348351.230864	41.755994
3506.911933	348265.601597	41.760999
3506.590987	348173.599179	41.766004
3506.554274	348095.737535	41.771008
3506.856322	348000.586603	41.776013
3506.058168	347918.445569	41.781018
3506.435546	347831.366605	41.786023
3506.462753	347753.875499	41.791028
3506.521943	347671.726931	41.796032
3506.453330	347596.614712	41.801037
3505.946387	347519.892971	41.806042
3505.927365	347445.026881	41.811047
3506.160938	347362.977401	41.816052
3506.059408	347281.310602	41.821056
3506.198277	347195.919734	41.826061
3506.036456	347138.896564	41.831066
3506.205373	347057.949619	41.836071
3505.622691	346973.103173	41.841076
3505.474090	346906.213479	41.846080
3505.925837	346838.721336	41.851085
3505.656245	346773.096014	41.856090
3505.510768	346707.807083	41.861095
3505.589538	346635.339079	41.866100
3505.474616	346576.095809	41.871104
3505.673646	346496.846151	41.876109
3505.270165	346439.096873	41.881114
3505.516012	346356.915894	41.886119
3505.715971	346304.588901	41.891124
3505.416338	346232.763924	41.896128
3505.664523	346171.200491	41.901133
3505.399514	346103.386728	41.906138
3505.488325	346036.127678	41.911143
3505.336869	345975.821274	41.916148
3505.548973	345900.076622	41.921152
3505.292592	345836.811806	41.926157
3505.405170	345777.836649	41.931162
3505.025445	345708.336635	41.936167
3504.863827	345650.039716	41.941172
3505.184015	345592.735176	41.946176
3504.945717	345525.577097	41.951181
3504.934482	345464.790228	41.956186
3505.137056	345415.080117	41.961191
3504.642257	345358.563617	41.966196
3504.654438	345296.298190	41.971200
3505.555691	345243.809069	41.976205
3504.933776	345184.235830	41.981210
3505.175908	345108.611835	41.986215
3504.970742	345061.532800	41.991220
3504.813906	344999.776313	41.996224
3504.822610	344931.383499	42.001229
3504.813526	344881.120937	42.006234
3504.786773	344823.462548	42.011239
3504.534704	344774.254793	42.016244
3504.526625	344713.262690	42.021248
3504.746809	344663.218208	42.026253
3504.548050	344617.281662	42.031258
3504.385136	344561.576387	42.036263
3504.544632	344513.422597	42.041268
3504.404341	344459.569621	42.046272
3504.485587	344412.673734	42.051277
3504.508733	344364.235954	42.056282
3504.805590	344309.983877	42.061287
3504.431001	344258.124925	42.066292
3504.046219	344210.081223	42.071296
3504.213072	344157.679823	42.076301
3503.747589	344110.563896	42.081306
3503.821090	344075.669348	42.086311
3503.712422	344025.726196	42.091316
3504.086626	343989.462447	42.096320
3504.405586	343941.588024	42.101325
3504.187911	343902.086026	42.106330
3504.322046	343861.918778	42.111335
3504.017334	343808.980364	42.116340
3503.990257	343767.668649	42.121344
3503.872369	343715.234813	42.126349
3503.825528	343674.205753	42.131354
3503.998668	343631.031951	42.136359
3503.935164	343584.081285	42.141364
3503.510162	343542.348428	42.146368
3503.827694	343505.177714	42.151373
3503.730013	343476.869081	42.156378
3504.053823	343432.374776	42.161383
3503.937250	343393.008940	42.166388
3503.696145	343362.866573	42.171392
3503.644502	343314.871239	42.176397
3503.498881	343282.145890	42.181402
3503.750480	343232.933457	42.186407
3503.756532	343199.497826	42.191412
3503.654935	343161.578647	42.196416
3503.640081	343122.857668	42.201421
3503.604480	343085.512878	42.206426
3503.853902	343039.783837	42.211431
3503.623662	343009.715740	42.216436
3503.389470	342967.494691	42.221440
3503.722843	342924.803472	42.226445
3503.607809	342891.081363	42.231450
3503.480086	342859.191870	42.236455
3503.425840	342825.994138	42.241460
3503.226944	342791.674820	42.246464
3503.304221	342757.947942	42.251469
3503.206738	342722.265124	42.256474
3503.646517	342681.311365	42.261479
3503.284045	342659.298262	42.266484
3503.332752	342621.660106	42.271488
3503.561870	342587.756767	42.276493
3503.336822	342559.518147	42.281498
3503.317525	342534.044213	42.286503
3503.245397	342488.644402	42.291508
3503.258619	342458.308928	42.296512
3503.429003	342424.134925	42.301517
3503.233243	342402.731252	42.306522
3503.346232	342355.141095	42.311527
3503.379958	342329.150196	42.316532
3503.049623	342299.554805	42.321536
3503.524642	342263.120928	42.326541
3503.537958	342233.471755	42.331546
3503.241719	342195.861639	42.336551
3503.065831	342169.598274	42.341556
3503.156673	342137.521390	42.346560
3503.089373	342116.478854	42.351565
3503.369967	342094.746256	42.356570
3503.431898	342056.825730	42.361575
3503.443751	342023.998295	42.366580
3503.096161	341987.921574	42.371584
3503.165794	341957.271726	42.376589
3503.356601	341926.730040	42.381594
3503.339199	341897.466783	42.386599
3503.165945	341863.320526	42.391604
3503.391566	341836.409327	42.396608
3503.346224	341806.336708	42.401613
3503.430399	341771.895850	42.406618
3503.157765	341735.044347	42.411623
3503.340210	341704.656335	42.416628
3502.973202	341680.380341	42.421632
3503.322641	341639.566616	42.426637
3503.161770	341618.157007	42.431642
3503.064762	341585.015630	42.436647
3503.231115	341558.901716	42.441652
3503.127477	341532.041759	42.446656
3503.134012	341491.535739	42.451661
3502.634394	341468.221124	42.456666
3503.210935	341443.288916	42.461671
3503.473119	341420.872250	42.466676
3502.986040	341393.411031	42.471680
3503.209006	341360.473688	42.476685
3503.021120	341332.914793	42.481690
3503.285469	341300.937152	42.486695
3503.240010	341276.330910	42.491700
3502.600276	341244.570839	42.496704
3503.073166	341222.858492	42.501709
3502.817997	341196.428801	42.506714
3502.974513	341155.975227	42.511719
3502.879308	341141.903505	42.516724
3502.839270	341116.050373	42.521728
3503.264857	341086.030648	42.526733
3502.928202	341065.588989	42.531738
3502.990408	341037.583928	42.536743
3503.174025	341017.060903	42.541748
3503.043129	340989.772529	42.546752
3502.915495	340942.879180	42.551757
3502.587491	340929.555732	42.556762
3503.046409	340898.284699	42.561767
3503.175436	340877.922691	42.566772
3502.713364	340860.628084	42.571776
3502.961473	340822.753399	42.576781
3502.457074	340805.516236	42.581786
3502.733109	340779.816862	42.586791
3503.122124	340763.635094	42.591796
3502.803045	340741.181731	42.596800
3502.681939	340705.653112	42.601805
3502.781838	340691.220151	42.606810
3502.842045	340663.723655	42.611815
3502.843457	340639.567336	42.616820
3502.726230	340619.828511	42.621824
3502.764118	340595.107052	42.626829
3502.665834	340574.983827	42.631834
3502.917311	340550.432366	42.636839
3502.611974	340525.789945	42.641844
3502.506758	340507.320559	42.646848
3502.866405	340483.591252	42.651853
3502.527426	340471.286452	42.656858
3502.653533	340448.915870	42.661863
3502.529151	340420.812352	42.666868
3502.586006	340398.274571	42.671872
3502.833106	340372.884557	42.676877
3502.676567	340359.381521	42.681882
3502.698327	340336.391488	42.686887
3502.659075	340314.199239	42.691892
3502.318135	340287.502569	42.696896
3502.838255	340272.495186	42.701901
3502.549530	340251.257300	42.706906
3502.412401	340229.461716	42.711911
3502.740282	340201.236463	42.716916
3502.586571	340189.055167	42.721920
3502.688093	340161.780673	42.726925
3502.274096	340144.274775	42.731930
3502.722646	340124.142087	42.736935
3502.602639	340102.114897	42.741940
3502.657131	340090.409576	42.746944
3502.717435	340064.463702	42.751949
3502.602222	340047.673883	42.756954
3502.857749	340025.486224	42.761959
3503.036622	339999.623479	42.766964
3502.589609	339970.527495	42.771968
3502.661000	339948.572000	42.776973
3502.517897	339933.490164	42.781978
3502.315346	339916.078236	42.786983
3502.738432	339898.034500	42.791988
3502.772746	339874.355648	42.796993
3502.597387	339854.015210	42.801997
3502.193999	339830.989603	42.807002
3502.455308	339811.191148	42.812007
3502.101461	339791.997416	42.817012
3502.210328	339775.325005	42.822017
3502.449146	339756.903156	42.827021
3502.224290	339730.899907	42.832026
3502.438025	339722.526088	42.837031
3502.617321	339714.132222	42.842036
3502.351242	339697.314967	42.847041
3502.740723	339679.327231	42.852045
3502.470113	339655.873901	42.857050
3502.525227	339628.097688	42.862055
3502.337521	339608.903312	42.867060
3502.272361	339595.792551	42.872065
3502.285125	339595.154886	42.877069
3502.045903	339563.000119	42.882074
3502.088182	339539.090943	42.887079
3502.218181	339538.587519	42.892084
3502.326305	339533.866414	42.897089
3502.770571	339504.859564	42.902093
3502.146506	339500.202067	42.907098
3502.191961	339475.173505	42.912103
3502.008024	339455.419032	42.917108
3502.342217	339459.918500	42.922113
3502.134846	339431.216892	42.927117
3502.244973	339418.129519	42.932122
3502.216054	339415.387810	42.937127
3502.370374	339388.918178	42.942132
3502.202088	339381.468569	42.947137
3502.263470	339358.598852	42.952141
3502.034377	339340.199082	42.957146
3502.084553	339324.044205	42.962151
3502.068724	339325.648709	42.967156
3501.939147	339314.912763	42.972161
3502.240360	339298.159201	42.977165
3502.100432	339293.298845	42.982170
3502.318635	339280.347097	42.987175
3502.291601	339262.500553	42.992180
3502.470666	339257.183466	42.997185
3502.362593	339230.475025	43.002189
3502.116901	339214.747781	43.007194
3502.300492	339202.996557	43.012199
3502.249160	339190.137771	43.017204
3502.152631	339166.504332	43.022209
3502.454527	339147.512879	43.027213
3502.265661	339138.489864	43.032218
3502.205896	339130.285807	43.037223
3502.228183	339121.941778	43.042228
3501.999711	339098.812066	43.047233
3502.300559	339074.938441	43.052237
3502.427115	339067.366386	43.057242
3502.603253	339049.589688	43.062247
3502.366302	339029.461838	43.067252
3502.106551	339019.178441	43.072257
3502.285566	338996.518960	43.077261
3502.437007	338994.995028	43.082266
3502.473441	338974.926121	43.087271
3502.693705	338957.854483	43.092276
3502.017199	338936.854436	43.097281
3502.441053	338912.910617	43.102285
3502.385473	338902.442694	43.107290
3502.091700	338887.816260	43.112295
3502.284381	338860.501091	43.117300
3502.449766	338853.762070	43.122305
3502.228316	338834.903127	43.127309
3502.182055	338825.857739	43.132314
3502.346873	338818.508509	43.137319
3502.330042	338793.336635	43.142324
3502.321919	338779.530079	43.147329
3502.379770	338755.872234	43.152333
3502.176831	338737.493494	43.157338
3502.152187	338729.690717	43.162343
3502.014965	338724.651859	43.167348
3502.324739	338709.091841	43.172353
3502.414405	338675.003119	43.177357
3502.411470	338674.367892	43.182362
3502.191344	338650.244857	43.187367
3502.054120	338647.825169	43.192372
3501.865397	338642.006053	43.197377
3502.122347	338625.691389	43.202381
3502.147399	338607.454942	43.207386
3502.266746	338605.580006	43.212391
3502.155733	338589.984005	43.217396
3502.089609	338576.186439	43.222401
3502.241059	338556.328179	43.227405
3501.974934	338557.920990	43.232410
3502.033662	338541.230414	43.237415
3502.284665	338522.856883	43.242420
3501.920848	338520.116605	43.247425
3501.786486	338503.252766	43.252429
3501.918902	338495.298238	43.257434
3501.865147	338476.819755	43.262439
3501.616496	338470.501398	43.267444
3501.787135	338480.290377	43.272449
3501.858038	338461.054954	43.277453
3502.168622	338463.930778	43.282458
3502.155218	338427.543890	43.287463
3502.105425	338420.329846	43.292468
3501.739477	338420.107374	43.297473
3501.896641	338395.798039	43.302477
3501.920794	338380.231674	43.307482
3501.807722	338383.580605	43.312487
3501.918264	338371.408234	43.317492
3501.702057	338381.308576	43.322497
3501.957418	338359.450489	43.327501
3501.819489	338339.255913	43.332506
3501.925214	338331.483526	43.337511
3502.394019	338324.035813	43.342516
3502.134019	338321.228430	43.347521
3502.304012	338297.425606	43.352525
3502.058996	338295.175320	43.357530
3502.283064	338280.086243	43.362535
3502.383063	338268.068060	43.367540
3502.089601	338251.076401	43.372545
3502.349316	338218.766137	43.377549
3502.061308	338208.308920	43.382554
3502.115929	338208.554710	43.387559
3502.022231	338198.448552	43.392564
3502.150390	338178.949734	43.397569
3502.277254	338156.806463	43.402573
3502.016690	338171.697937	43.407578
3501.994160	338139.609732	43.412583
3502.308111	338126.159443	43.417588
3501.919418	338125.203074	43.422593
3502.069916	338110.735731	43.427597
3502.107196	338093.336279	43.432602
3502.105912	338077.188886	43.437607
3502.125542	338071.540539	43.442612
3501.685059	338056.428115	43.447617
3501.997566	338041.503117	43.452621
3502.018279	338031.073872	43.457626
3502.128651	338027.089671	43.462631
3502.280922	338016.054979	43.467636
3502.087275	338007.871596	43.472641
3502.160915	337992.755057	43.477645
3502.518168	337985.146708	43.482650
3501.815358	337973.152219	43.487655
3501.928907	337959.326327	43.492660
3502.255068	337960.699421	43.497665
3502.266449	337942.769928	43.502669
3502.153181	337933.429638	43.507674
3501.934625	337919.248780	43.512679
3501.928182	337914.291079	43.517684
3501.851393	337884.321776	43.522689
3502.081355	337876.631586	43.527693
3501.458035	337873.982686	43.532698
3501.787882	337861.877577	43.537703
3502.200894	337866.593790	43.542708
3502.241969	337845.964080	43.547713
3502.565090	337826.383734	43.552717
3502.247245	337830.247889	43.557722
3502.203669	337804.494627	43.562727
3502.475526	337791.508526	43.567732
3502.096792	337788.948530	43.572737
3502.372529	337756.864214	43.577741
3502.192038	337747.661533	43.582746
3502.040038	337721.594578	43.587751
3502.406955	337709.483622	43.592756
3502.314778	337698.080176	43.597761
3502.444436	337693.024879	43.602765
3502.085754	337667.803944	43.607770
3501.836755	337663.926745	43.612775
3502.106818	337654.526454	43.617780
3502.017484	337639.180950	43.622785
3502.373956	337626.156132	43.627789
3502.142180	337630.566305	43.632794
3502.245132	337607.409250	43.637799
3502.185521	337598.899664	43.642804
3502.156947	337586.748778	43.647809
3502.349020	337555.414825	43.652813
3502.038879	337549.105920	43.657818
3501.943466	337539.813596	43.662823
3502.373218	337521.513331	43.667828
3502.147273	337509.901871	43.672833
3502.115023	337490.275182	43.677837
3502.082904	337479.981187	43.682842
3502.285822	337467.946649	43.687847
3502.598878	337458.030991	43.692852
3502.303523	337442.209017	43.697857
3502.313411	337429.009444	43.702861
3502.182633	337416.315023	43.707866
3502.133324	337390.689512	43.712871
3502.047463	337380.607330	43.717876
3501.918649	337377.067328	43.722881
3502.082992	337363.691005	43.727885
3502.111662	337342.579782	43.732890
3501.660169	337332.046150	43.737895
3502.043526	337328.044624	43.742900
3502.273991	337329.814152	43.747905
3501.940077	337307.386380	43.752909
3501.981882	337292.274526	43.757914
3501.945111	337294.772441	43.762919
3502.023886	337280.722858	43.767924
3502.041008	337261.774935	43.772929
3502.263083	337254.162137	43.777933
3502.397072	337257.014807	43.782938
3502.088091	337228.327328	43.787943
3501.864123	337211.019155	43.792948
3502.150291	337209.524946	43.797953
3501.866182	337201.736973	43.802957
3501.989478	337178.881624	43.807962
3502.050861	337162.113707	43.812967
3502.085772	337163.405215	43.817972
3501.848598	337153.321195	43.822977
3502.082616	337131.414846	43.827981
3501.808424	337121.234884	43.832986
3501.923711	337117.885565	43.837991
3502.002749	337117.262925	43.842996
3502.248866	337105.170654	43.848001
3502.153373	337080.340475	43.853005
3501.866839	337078.274614	43.858010
3502.248527	337082.843247	43.863015
3501.846972	337052.669729	43.868020
3502.005225	337048.855945	43.873025
3502.343040	337031.281850	43.878029
3502.411792	337027.685497	43.883034
3502.164699	336999.064451	43.888039
3502.397461	336989.262939	43.893044
3502.073311	336976.089994	43.898049
3502.144097	336959.701965	43.903053
3502.122447	336967.715876	43.908058
3502.112076	336953.171501	43.913063
3502.378876	336927.623396	43.918068
3502.130166	336913.574009	43.923073
3502.196376	336897.618981	43.928077
3502.157541	336873.720720	43.933082
3502.340801	336868.733220	43.938087
3502.222787	336859.291674	43.943092
3502.318762	336842.238470	43.948097
3502.328130	336827.462087	43.953101
3502.062995	336808.761497	43.958106
3502.402692	336796.145889	43.963111
3502.257700	336785.716763	43.968116
3502.263517	336768.448747	43.973121
3502.190469	336749.311212	43.978125
3502.270970	336745.763855	43.983130
3502.227548	336731.911177	43.988135
3502.455285	336713.845532	43.993140
3501.781019	336708.432606	43.998145
3501.991063	336695.226906	44.003149
3501.823316	336681.469936	44.008154
3501.797270	336669.496361	44.013159
3502.074191	336668.181588	44.018164
3501.779069	336661.488725	44.023169
3502.061418	336645.830391	44.028173
3501.904559	336649.542351	44.033178
3501.776349	336634.329652	44.038183
3502.024512	336635.587840	44.043188
3502.004621	336623.511567	44.048193
3501.683786	336596.732720	44.053197
3502.026225	336592.584929	44.058202
3501.949240	336579.576643	44.063207
3502.233281	336581.464983	44.068212
3501.746026	336561.349460	44.073217
3501.858471	336544.496985	44.078221
3501.904506	336543.599761	44.083226
3501.748397	336545.811219	44.088231
3501.766748	336540.976607	44.093236
3501.738046	336537.802329	44.098241
3501.957629	336517.728859	44.103245
3502.036515	336493.862806	44.108250
3501.667643	336502.109116	44.113255
3501.983481	336495.346137	44.118260
3501.618787	336482.153922	44.123265
3502.048322	336464.285480	44.128269
3501.883133	336463.726441	44.133274
3501.729857	336465.505143	44.138279
3501.975459	336450.081345	44.143284
3501.864408	336443.283373	44.148289
3502.139234	336419.996971	44.153293
3502.217162	336420.722310	44.158298
3502.246795	336411.639023	44.163303
3502.240278	336380.665706	44.168308
3501.786829	336371.429058	44.173313
3501.841510	336361.960385	44.178317
3502.117311	336371.606340	44.183322
3502.287345	336342.487248	44.188327
3502.228311	336324.974856	44.193332
3501.960245	336331.323582	44.198337
3502.008740	336308.937133	44.203341
3502.262273	336291.604735	44.208346
3502.087954	336285.757557	44.213351
3502.445656	336275.504001	44.218356
3501.996872	336253.449567	44.223361
3502.364389	336241.007434	44.228365
3502.152198	336233.284302	44.233370
3501.779494	336218.669128	44.238375
3502.085693	336210.254612	44.243380
3502.070202	336212.927289	44.248385
3502.143945	336194.987186	44.253389
3502.143557	336175.303948	44.258394
3501.922921	336166.158005	44.263399
3502.223196	336164.356380	44.268404
3502.002850	336151.141478	44.273409
3502.553744	336117.308849	44.278413
3502.142432	336129.325623	44.283418
3502.418206	336105.886290	44.288423
3502.007934	336082.681350	44.293428
3502.377577	336084.302027	44.298433
3502.472275	336050.616949	44.303437
3502.278338	336049.121460	44.308442
3501.956076	336036.532788	44.313447
3501.986294	336011.453354	44.318452
3502.178847	335999.216508	44.323457
3502.159430	335995.786423	44.328461
3502.153948	335975.824135	44.333466
3501.877434	335971.162701	44.338471
3501.824667	335967.280073	44.343476
3502.022413	335966.460839	44.348481
3502.507015	335949.219309	44.353485
3502.070736	335930.061840	44.358490
3501.799724	335928.349518	44.363495
3502.189445	335913.360719	44.368500
3501.675453	335894.393397	44.373505
3502.043067	335874.779620	44.378509
3502.052055	335872.972659	44.383514
3501.651409	335871.509479	44.388519
3501.954992	335845.649699	44.393524
3501.486782	335848.494902	44.398529
3501.786893	335829.578289	44.403533
3501.688593	335828.678181	44.408538
3501.781358	335825.891745	44.413543
3501.619538	335821.212361	44.418548
3501.468759	335818.870895	44.423553
3501.432540	335818.520561	44.428557
3501.686932	335816.039459	44.433562
3501.606433	335805.701694	44.438567
3501.597847	335794.564325	44.443572
3501.755122	335790.089360	44.448577
3501.548969	335784.247078	44.453581
3501.432140	335784.646844	44.458586
3501.375180	335783.918289	44.463591
3501.546694	335785.849694	44.468596
3501.530517	335781.172966	44.473601
3501.555340	335772.115705	44.478605
3501.293181	335773.631722	44.483610
3501.835959	335770.851221	44.488615
3502.165429	335760.373058	44.493620
3501.764115	335755.883693	44.498625
3501.725796	335741.419500	44.503629
3501.656699	335737.056211	44.508634
3501.694112	335738.576258	44.513639
3502.020118	335728.047765	44.518644
3501.575647	335724.404365	44.523649
3501.541708	335699.436472	44.528653
3501.381166	335696.562474	44.533658
3501.767389	335694.671097	44.538663
3501.809620	335689.171434	44.543668
3501.715690	335687.380554	44.548673
3501.509330	335681.080531	44.553677
3501.570983	335688.191612	44.558682
3501.466611	335686.351502	44.563687
3501.636027	335686.375915	44.568692
3501.340031	335670.095515	44.573697
3501.511673	335656.946308	44.578701
3501.397780	335654.090444	44.583706
3501.377040	335655.924757	44.588711
3501.490009	335647.616616	44.593716
3501.563163	335650.911250	44.598721
3501.671489	335633.575813	44.603725
3501.653568	335635.002790	44.608730
3501.718362	335644.554769	44.613735
3501.656060	335648.404633	44.618740
3501.661983	335646.623571	44.623745
3501.745697	335641.880347	44.628749
3501.841520	335631.235226	44.633754
3501.575918	335619.578502	44.638759
3501.908526	335605.437732	44.643764
3501.566003	335605.465887	44.648769
3501.828613	335602.245984	44.653773
3501.563928	335607.068442	44.658778
3501.431988	335607.165399	44.663783
3501.840892	335600.031672	44.668788
3501.554907	335582.045786	44.673793
3501.964256	335567.918435	44.678797
3501.903207	335571.005178	44.683802
3501.515434	335574.321017	44.688807
3501.748765	335565.994040	44.693812
3501.627014	335564.029486	44.698817
3501.683906	335552.754652	44.703821
3501.608463	335540.152654	44.708826
3501.442915	335530.718197	44.713831
3502.070328	335526.118838	44.718836
3501.480963	335523.591609	44.723841
3501.468943	335528.043971	44.728845
3501.517010	335525.696830	44.733850
3501.347998	335518.831455	44.738855
3501.521984	335522.796978	44.743860
3501.555099	335524.190550	44.748865
3501.642779	335516.750991	44.753869
3501.730248	335520.195986	44.758874
3501.675952	335503.674276	44.763879
3501.855478	335480.859941	44.768884
3501.825780	335481.424106	44.773889
3501.551237	335472.820471	44.778893
3501.661546	335475.066636	44.783898
3501.697527	335477.705888	44.788903
3501.879368	335465.089072	44.793908
3501.797831	335446.359084	44.798913
3501.955980	335439.264529	44.803917
3501.826057	335437.072365	44.808922
3501.919140	335427.546586	44.813927
3502.026101	335426.894121	44.818932
3501.723050	335413.386710	44.823937
3501.927953	335394.764502	44.828941
3501.555842	335395.534787	44.833946
3501.759746	335389.374024	44.838951
3502.011506	335386.054074	44.843956
3501.848659	335369.472981	44.848961
3501.917516	335351.711251	44.853965
3501.625178	335350.790604	44.858970
3501.538138	335346.557231	44.863975
3502.051692	335339.432525	44.868980
3501.925578	335340.088059	44.873985
3501.569052	335320.154867	44.878989
3501.827189	335314.545101	44.883994
3501.760304	335314.479300	44.888999
3501.535908	335313.726049	44.894004
3501.703180	335316.293924	44.899009
3501.700383	335303.171863	44.904013
3501.878195	335302.101419	44.909018
3501.821968	335292.929555	44.914023
3501.683854	335280.082953	44.919028
3501.648671	335275.917759	44.924033
3501.886197	335276.643600	44.929037
3501.682790	335274.030583	44.934042
3501.612133	335273.660196	44.939047
3501.691152	335268.714208	44.944052
3501.846060	335265.485683	44.949057
3501.728564	335248.032782	44.954061
3501.475271	335241.409413	44.959066
3501.486434	335241.356842	44.964071
3501.887324	335231.935479	44.969076
3501.897582	335238.927526	44.974081
3501.807110	335230.218763	44.979085
3502.041148	335201.292215	44.984090
3501.528751	335200.940026	44.989095
3501.970582	335194.233407	44.994100
3501.408896	335197.398449	44.999105
3501.587817	335188.876443	45.004109
3501.827788	335200.410227	45.009114
3501.370901	335196.310951	45.014119
3501.925267	335179.948254	45.019124
3501.734053	335164.287033	45.024129
3500.995361	335157.790398	45.029133
3501.746287	335155.587665	45.034138
3501.475880	335148.305739	45.039143
3501.758962	335151.236991	45.044148
3501.523152	335150.638109	45.049153
3501.779752	335151.589854	45.054157
3501.772053	335158.737311	45.059162
3501.454329	335151.030450	45.064167
3501.943911	335120.334554	45.069172
3501.825276	335118.242332	45.074177
3501.847886	335113.610319	45.079181
3501.923394	335112.199824	45.084186
3501.878153	335110.706480	45.089191
3502.135298	335086.150432	45.094196
3501.828433	335086.376463	45.099201
3502.194055	335069.000536	45.104205
3501.933547	335069.829675	45.109210
3501.500885	335053.036308	45.114215
3501.898226	335029.780739	45.119220
3501.860900	335034.262549	45.124225
3501.869312	335032.735383	45.129229
3501.861920	335030.549470	45.134234
3501.572045	335038.656597	45.139239
3502.059612	335016.353310	45.144244
3501.880694	335005.750962	45.149249
3502.110201	334993.736890	45.154253
3502.007960	334989.378695	45.159258
3502.098035	334984.125763	45.164263
3502.306563	334964.358355	45.169268
3502.039069	334957.355683	45.174273
3501.935519	334946.894124	45.179277
3501.899638	334920.578139	45.184282
3502.031098	334917.149798	45.189287
3502.026964	334903.213995	45.194292
3501.740138	334904.352430	45.199297
3501.918334	334876.349895	45.204301
3501.715458	334877.907543	45.209306
3501.581096	334872.384504	45.214311
3502.134566	334859.556794	45.219316
3501.632100	334862.890627	45.224321
3502.036409	334857.970024	45.229325
3501.944747	334843.793567	45.234330
3501.941920	334823.753948	45.239335
3502.009162	334824.048651	45.244340
3501.773922	334824.924708	45.249345
3501.802310	334809.610479	45.254349
3501.870552	334786.101029	45.259354
3501.647067	334785.271330	45.264359
3501.883714	334775.544918	45.269364
3501.688586	334777.304812	45.274369
3501.794530	334778.687025	45.279373
3501.831840	334768.203395	45.284378
3501.779289	334749.061617	45.289383
3502.197929	334739.026995	45.294388
3501.811092	334748.319200	45.299393
3501.668264	334739.669371	45.304397
3501.639848	334710.630883	45.309402
3501.432828	334696.930175	45.314407
3501.865116	334696.226837	45.319412
3501.637638	334703.383309	45.324417
3501.768388	334710.966978	45.329421
3501.764153	334697.234567	45.334426
3501.874699	334704.236467	45.339431
3502.251380	334687.418131	45.344436
3502.090415	334675.795614	45.349441
3502.043791	334659.628373	45.354445
3502.050570	334648.284803	45.359450
3501.831111	334647.251017	45.364455
3501.979238	334627.060534	45.369460
3501.919848	334625.086180	45.374465
3502.090237	334624.906988	45.379469
3501.804943	334606.411885	45.384474
3501.590501	334590.982939	45.389479
3501.806430	334592.169943	45.394484
3501.446418	334590.547766	45.399489
3501.577206	334591.951535	45.404493
3501.852561	334587.661419	45.409498
3501.708313	334588.828437	45.414503
3501.928277	334574.094523	45.419508
3501.832760	334555.417134	45.424513
3501.572426	334542.818271	45.429517
3501.693586	334545.164523	45.434522
3501.428139	334536.686407	45.439527
3501.518008	334534.459828	45.444532
3501.542232	334535.320759	45.449537
3501.502438	334538.633150	45.454541
3501.658156	334539.015752	45.459546
3501.721126	334539.133103	45.464551
3501.705981	334508.846225	45.469556
3501.617784	334513.030868	45.474561
3501.936224	334500.188915	45.479565
3501.842532	334488.326936	45.484570
3501.660975	334496.086633	45.489575
3501.973234	334483.398232	45.494580
3501.937909	334482.132200	45.499585
3501.675663	334466.380062	45.504589
3501.828684	334459.947350	45.509594
3501.554996	334461.846699	45.514599
3501.696127	334449.541087	45.519604
3501.244558	334459.224962	45.524609
3501.349030	334464.422195	45.529613
3501.746011	334455.840499	45.534618
3501.583976	334436.766540	45.539623
3501.888560	334420.239106	45.544628
3501.572138	334416.906171	45.549633
3501.945814	334411.329070	45.554637
3501.822775	334402.345454	45.559642
3501.677823	334412.769794	45.564647
3501.819682	334408.602256	45.569652
3501.541252	334381.611717	45.574657
3501.577457	334370.721237	45.579661
3501.508234	334372.715785	45.584666
3501.322090	334369.591366	45.589671
3501.598876	334370.285656	45.594676
3501.669396	334369.257392	45.599681
3501.760081	334368.887204	45.604685
3501.699730	334367.091010	45.609690
3501.331371	334369.081461	45.614695
3501.678303	334360.304112	45.619700
3501.329386	334355.679224	45.624705
3501.538994	334354.680078	45.629709
3501.634277	334340.753954	45.634714
3501.614968	334350.192256	45.639719
3501.551364	334328.737684	45.644724
3501.675486	334333.881000	45.649729
3501.494725	334326.966377	45.654733
3501.670178	334326.252321	45.659738
3501.438367	334328.119699	45.664743
3501.922496	334317.922134	45.669748
3501.862423	334326.909039	45.674753
3501.736597	334313.907591	45.679757
3501.250199	334289.467261	45.684762
3501.374624	334290.515988	45.689767
3501.884526	334284.586956	45.694772
3501.555597	334280.976212	45.699777
3501.122420	334278.297318	45.704781
3501.405129	334287.205211	45.709786
3501.411417	334283.821812	45.714791
3501.999380	334277.880575	45.719796
3501.844399	334279.583352	45.724801
3501.927624	334271.457576	45.729805
3502.120435	334244.749314	45.734810
3501.664242	334249.729046	45.739815
3501.972372	334237.448119	45.744820
3501.830776	334214.123707	45.749825
3501.904198	334160.196347	45.754829
3501.771160	334050.859185	45.759834
3501.434584	333906.431634	45.764839
3501.218995	333718.876796	45.769844
3500.972203	333475.120073	45.774849
3500.846359	333188.310737	45.779853
3500.696794	332860.861126	45.784858
3500.299622	332476.578821	45.789863
3500.347552	332039.321437	45.794868
3500.203822	331568.516411	45.799873
3499.263685	331031.777677	45.804877
3499.425582	330460.776923	45.809882
3498.689480	329853.485350	45.814887
3498.058173	329166.555295	45.819892
3497.623053	328450.051544	45.824897
3496.916803	327672.326538	45.829901
3496.444689	326876.336954	45.834906
3495.841791	326019.251477	45.839911
3495.340207	325098.206463	45.844916
3494.764026	324144.972582	45.849921
3494.045157	323130.913952	45.854925
3493.174015	322076.074440	45.859930
3491.893906	320983.696884	45.864935
3491.434775	319834.785404	45.869940
3490.805218	318636.054830	45.874945
3489.667911	317399.410434	45.879949
3488.883228	316094.132114	45.884954
3487.382860	314759.590735	45.889959
3486.482323	313363.416352	45.894964
3485.459886	311945.971834	45.899969
3483.553653	310474.523767	45.904973
3482.902773	308950.591115	45.909978
3481.626864	307394.033299	45.914983
3480.395949	305775.426351	45.919988
3478.783170	304135.805989	45.924993
3477.381817	302444.843372	45.929997
3476.068235	300704.819211	45.935002
3474.381392	298942.297750	45.940007
3473.245308	297115.925394	45.945012
3471.523983	295269.884584	45.950017
3470.038510	293384.675667	45.955021
3468.591062	291430.442851	45.960026
3466.628420	289470.831940	45.965031
3464.794012	287451.876719	45.970036
3462.979557	285397.444506	45.975041
3461.933803	283309.657447	45.980045
3460.171917	281180.727224	45.985050
3457.585161	279011.967988	45.990055
3455.898027	276813.904502	45.995060
3453.731039	274588.713092	46.000065
3451.697434	272326.138947	46.005069
3449.545730	270024.362444	46.010074
3447.319480	267703.518291	46.015079
3445.335937	265330.633533	46.020084
3443.006052	262941.781307	46.025089
3440.695603	260514.166276	46.030093
3438.824893	258049.277113	46.035098
3436.010043	255577.636314	46.040103
3433.991062	253052.956925	46.045108
3431.414541	250515.485852	46.050113
3428.779624	247936.293801	46.055117
3426.773932	245343.519351	46.060122
3424.120080	242711.795952	46.065127
3421.394912	240057.234340	46.070132
3418.844411	237387.313145	46.075137
3416.244935	234679.506242	46.080141
3413.415001	231945.536274	46.085146
3410.356344	229206.368537	46.090151
3407.726900	226429.075516	46.095156
3404.420702	223635.381980	46.100161
3401.517854	220815.191481	46.105165
3398.744185	217988.672959	46.110170
3395.542180	215142.267929	46.115175
3392.427469	212265.255915	46.120180
3388.883796	209392.335599	46.125185
3385.728869	206480.242053	46.130189
3382.767721	203573.785294	46.135194
3379.037867	200651.219782	46.140199
3375.383672	197714.381345	46.145204
3372.045384	194779.435910	46.150209
3368.602935	191805.557463	46.155213
3364.795685	188845.279162	46.160218
3360.937239	185893.540840	46.165223
3357.513759	182915.514394	46.170228
3353.682741	179937.286834	46.175233
3350.051617	176945.478612	46.180237
3345.873519	173969.290799	46.185242
3341.276904	170983.630059	46.190247
3337.725426	167991.852145	46.195252
3333.473479	165028.312545	46.200257
3328.820752	162057.353322	46.205261
3323.739666	159104.581705	46.210266
3319.155079	156167.896897	46.215271
3314.335839	153236.574131	46.220276
3309.528881	150318.495632	46.225281
3304.428459	147428.512549	46.230285
3298.652015	144567.080552	46.235290
3293.088103	141702.583343	46.240295
3287.267761	138856.704093	46.245300
3280.891354	136110.583135	46.250305
3274.291315	133394.251748	46.255309
3267.529786	130741.091466	46.260314
3260.393321	128146.982136	46.265319
3253.313863	125607.550712	46.270324
3245.681984	123148.742832	46.275329
3238.092414	120742.717532	46.280333
3229.880117	118423.132172	46.285338
3221.273847	116194.045800	46.290343
3213.072619	114041.969169	46.295348
3204.646907	111983.582268	46.300353
3195.519185	110031.227620	46.305357
3186.461403	108159.266309	46.310362
3177.519877	106405.601379	46.315367
3168.405790	104748.994254	46.320372
3159.164842	103207.741813	46.325377
3149.682430	101759.552279	46.330381
3140.925491	100430.446195	46.335386
3131.994266	99196.605096	46.340391
3123.972195	98048.393420	46.345396
3115.858877	97002.416848	46.350401
3108.372029	96043.303121	46.355405
3101.493856	95147.333862	46.360410
3094.368995	94344.119792	46.365415
3088.478529	93598.374844	46.370420
3082.340953	92918.281380	46.375425
3076.482564	92305.722421	46.380429
3071.087030	91728.250270	46.385434
3065.912103	91206.599824	46.390439
3060.903509	90707.486101	46.395444
3055.893897	90262.852027	46.400449
3051.414992	89838.331326	46.405453
3047.368781	89439.376572	46.410458
3043.284751	89074.471477	46.415463
3039.936240	88713.953576	46.420468
3036.073880	88377.457279	46.425473
3032.851738	88048.005012	46.430477
3029.228596	87716.954760	46.435482
3025.613212	87400.962353	46.440487
3022.392034	87087.312899	46.445492
3018.851055	86784.528477	46.450497
3015.924725	86496.312104	46.455501
3012.811786	86189.147360	46.460506
3009.488033	85891.458096	46.465511
3006.202123	85589.510069	46.470516
3002.880564	85291.127882	46.475521
2999.559665	84992.405659	46.480525
2996.673080	84689.616919	46.485530
2993.208422	84395.979441	46.490535
2989.991960	84087.849569	46.495540
2986.165168	83777.785913	46.500545
2983.111041	83486.100665	46.505549
2979.826874	83186.743589	46.510554
2976.004770	82893.774447	46.515559
2972.840122	82584.306155	46.520564
2969.453130	82292.672469	46.525569
2966.003725	81998.155359	46.530573
2962.624956	81698.130117	46.535578
2958.880452	81408.860590	46.540583
2955.589288	81112.981523	46.545588
2951.728555	80823.405936	46.550593
2947.888801	80533.753846	46.555597
2944.678319	80242.062971	46.560602
2940.894663	79963.941218	46.565607
2937.147369	79675.833163	46.570612
2933.689345	79408.348005	46.575617
2929.805056	79120.635470	46.580621
2926.585937	78838.969242	46.585626
2922.493761	78576.087491	46.590631
2919.608007	78300.801321	46.595636
2915.515924	78036.273588	46.600641
2911.881401	77776.528486	46.605645
2908.107753	77509.161888	46.610650
2904.475618	77250.119927	46.615655
2900.770734	76991.536307	46.620660
2897.195576	76741.367753	46.625665
2893.540243	76496.078151	46.630669
2889.902671	76242.342530	46.635674
2886.286025	76005.992053	46.640679
2882.726983	75757.125418	46.645684
2879.064168	75529.053830	46.650689
2875.576494	75291.546457	46.655693
2872.323166	75047.858029	46.660698
2868.285575	74815.292016	46.665703
2864.959340	74575.111567	46.670708
2861.456126	74346.567863	46.675713
2858.010775	74113.661326	46.680717
2854.677328	73883.025100	46.685722
2851.059077	73647.647994	46.690727
2847.253455	73415.184851	46.695732
2842.108493	73184.901472	46.700737
2838.864316	72973.510070	46.705741
2835.648458	72757.722314	46.710746
2832.017001	72545.950447	46.715751
2828.673777	72331.367014	46.720756
2825.544767	72110.783771	46.725761
2822.293936	71886.285083	46.730765
2819.611395	71678.396984	46.735770
2815.760666	71459.976401	46.740775
2812.962062	71222.841958	46.745780
2809.556984	70997.041737	46.750785
2805.711027	70764.240004	46.755789
2802.651864	70531.520442	46.760794
2798.914180	70307.466920	46.765799
2795.576366	70059.685593	46.770804
2792.218594	69845.848481	46.775809
2788.647592	69610.271515	46.780813
2785.387864	69364.776357	46.785818
2781.471914	69135.599625	46.790823
2778.386797	68901.654436	46.795828
2775.012974	68660.538668	46.800833
2771.369035	68434.175930	46.805837
2768.115820	68185.764470	46.810842
2764.608926	67955.728035	46.815847
2761.068582	67718.005212	46.820852
2757.601934	67466.790213	46.825857
2753.970043	67230.850929	46.830861
2750.806953	66990.378037	46.835866
2747.216354	66752.881510	46.840871
2743.695909	66508.101849	46.845876
2739.905640	66263.684121	46.850881
2736.149556	66028.340319	46.855885
2733.146288	65778.865808	46.860890
2729.453340	65545.179643	46.865895
2726.156248	65298.142436	46.870900
2722.839482	65054.950809	46.875905
2718.925988	64813.701892	46.880909
2715.482173	64570.369784	46.885914
2711.855565	64328.839453	46.890919
2708.790140	64077.601600	46.895924
2705.276203	63848.930005	46.900929
2701.686396	63603.637160	46.905933
2698.184046	63361.588965	46.910938
2694.494777	63117.471573	46.915943
2691.055607	62867.415018	46.920948
2687.962726	62620.486479	46.925953
2684.138561	62373.858824	46.930957
2680.913758	62132.210740	46.935962
2677.503619	61886.208601	46.940967
2673.914249	61632.342033	46.945972
2670.550018	61377.249751	46.950977
2667.005534	61134.582545	46.955981
2663.783825	60876.008100	46.960986
2659.816207	60634.135481	46.965991
2656.410702	60380.443444	46.970996
2652.877590	60125.079611	46.976001
2649.041874	59875.090013	46.981005
2646.114142	59624.738846	46.986010
2642.276506	59382.318874	46.991015
2638.677859	59132.629787	46.996020
2635.380426	58880.554593	47.001025
2631.628842	58630.520191	47.006029
2627.914272	58377.785722	47.011034
2624.550858	58131.274645	47.016039
2621.294281	57879.552474	47.021044
2617.876574	57630.732575	47.026049
2614.421822	57379.725570	47.031053
2610.978925	57131.168583	47.036058
2607.405900	56882.564725	47.041063
2603.992666	56632.212585	47.046068
2600.405068	56380.018553	47.051073
2596.660849	56126.100472	47.056077
2593.290106	55864.043289	47.061082
2589.720347	55615.610711	47.066087
2586.097659	55361.193214	47.071092
2583.013809	55107.239799	47.076097
2579.341152	54859.262658	47.081101
2576.187177	54598.219689	47.086106
2572.564706	54339.949283	47.091111
2569.352983	54088.298114	47.096116
2565.330236	53828.459057	47.101121
2561.845353	53577.465124	47.106125
2558.441098	53313.303379	47.111130
2554.866202	53067.702510	47.116135
2551.521967	52810.008059	47.121140
2548.193463	52548.735969	47.126145
2544.136565	52299.900641	47.131149
2540.870101	52037.584158	47.136154
2537.085919	51792.911214	47.141159
2533.771019	51537.884263	47.146164
2530.509144	51290.591070	47.151169
2527.200725	51039.742698	47.156173
2523.646927	50759.127257	47.161178
2519.859611	50494.905119	47.166183
2516.457099	50238.231506	47.171188
2512.977425	49989.793731	47.176193
2509.495622	49731.419130	47.181197
2505.988091	49463.885597	47.186202
2502.367601	49205.919188	47.191207
2498.926923	48950.255438	47.196212
2495.047849	48687.419483	47.201217
2491.765332	48447.536877	47.206221
2488.713677	48171.580883	47.211226
2484.576936	47914.350427	47.216231
2481.543306	47656.785413	47.221236
2477.911861	47394.287167	47.226241
2474.282714	47135.565388	47.231245
2471.455967	46877.913423	47.236250
2467.826163	46613.800297	47.241255
2464.211783	46338.487369	47.246260
2460.667167	46075.584933	47.251265
2456.864877	45814.197250	47.256269
2454.024207	45547.588527	47.261274
2450.614290	45286.716385	47.266279
2446.867695	45023.179262	47.271284
2443.416061	44756.643805	47.276289
2439.926950	44485.817672	47.281293
2436.688514	44212.926271	47.286298
2433.040884	43940.628575	47.291303
2429.525087	43671.065811	47.296308
2425.926361	43400.530024	47.301313
2422.545344	43124.015268	47.306317
2419.206285	42861.701906	47.311322
2415.470024	42588.217142	47.316327
2412.053816	42319.130840	47.321332
2408.636169	42042.635339	47.326337
2404.889815	41762.415504	47.331341
2401.922699	41491.335061	47.336346
2398.114126	41218.734641	47.341351
2394.748797	40941.712179	47.346356
2391.223282	40665.624996	47.351361
2387.384422	40385.938141	47.356365
2384.169887	40114.222329	47.361370
2380.768182	39843.223952	47.366375
2377.150960	39568.521858	47.371380
2373.489259	39287.965449	47.376385
2369.877640	39022.266234	47.381389
2366.519398	38730.295273	47.386394
2362.711409	38463.086659	47.391399
2359.615867	38193.487517	47.396404
2356.138907	37909.109788	47.401409
2352.562137	37635.034555	47.406413
2349.550582	37343.002780	47.411418
2345.842624	37073.183818	47.416423
2342.478348	36789.766900	47.421428
2338.654574	36505.633188	47.426433
2335.611705	36215.105118	47.431437
2332.281367	35934.813197	47.436442
2328.509249	35653.960156	47.441447
2325.161428	35368.131635	47.446452
2321.737274	35078.179518	47.451457
2317.983454	34794.938826	47.456461
2314.686229	34506.229789	47.461466
2311.164601	34219.588206	47.466471
2307.757799	33921.858875	47.471476
2304.347714	33635.581761	47.476481
2300.628704	33342.321129	47.481485
2297.313438	33055.175047	47.486490
2293.475344	32764.159570	47.491495
2290.239858	32466.772664	47.496500
2286.827180	32168.955022	47.501505
2282.971701	31877.149665	47.506509
2280.065190	31586.480203	47.511514
2276.293706	31288.154521	47.516519
2272.929288	30997.000861	47.521524
2269.394380	30699.850801	47.526529
2265.928067	30395.634170	47.531533
2262.544344	30095.351028	47.536538
2259.322902	29797.765620	47.541543
2255.509874	29500.131298	47.546548
2252.246491	29196.103394	47.551553
2249.024123	28894.646450	47.556557
2245.344536	28580.527982	47.561562
2242.053123	28283.076836	47.566567
2238.702136	27972.306563	47.571572
2235.333469	27659.319576	47.576577
2231.402149	27358.319356	47.581581
2228.239734	27039.023645	47.586586
2224.590248	26726.139291	47.591591
2221.178429	26412.867739	47.596596
2217.663469	26086.792532	47.601601
2213.968989	25784.150184	47.606605
2210.592010	25457.886119	47.611610
2207.148227	25146.223215	47.616615
2203.945912	24827.380476	47.621620
2200.722148	24508.660193	47.626625
2196.926684	24189.876023	47.631629
2193.725672	23867.468665	47.636634
2189.949319	23550.586024	47.641639
2186.854351	23216.002123	47.646644
2183.534029	22892.590163	47.651649
2179.792657	22562.882487	47.656653
2176.582763	22232.387601	47.661658
2172.782840	21911.771709	47.666663
2169.377507	21580.855808	47.671668
2165.836682	21247.755815	47.676673
2161.919228	20926.585155	47.681677
2158.491775	20595.682891	47.686682
2154.676972	20265.258533	47.691687
2150.975240	19937.501463	47.696692
2147.495199	19626.418535	47.701697
2143.527370	19324.455670	47.706701
2139.619316	19018.725704	47.711706
2135.639832	18726.534654	47.716711
2131.535728	18429.123065	47.721716
2127.463056	18141.332065	47.726721
2123.365681	17858.514779	47.731725
2119.492936	17590.354008	47.736730
2115.145129	17336.768619	47.741735
2111.066254	17094.531939	47.746740
2106.729734	16867.665264	47.751745
2102.193304	16649.401437	47.756749
2098.372776	16434.365664	47.761754
2094.311674	16234.335100	47.766759
2090.600511	16029.464077	47.771764
2087.268678	15828.905652	47.776769
2083.452513	15644.244753	47.781773
2080.173269	15446.544585	47.786778
2076.781593	15267.314664	47.791783
2073.229034	15078.359174	47.796788
2070.098628	14879.422528	47.801793
2065.997341	14692.510347	47.806797
2063.503816	14503.113047	47.811802
2059.627850	14319.484362	47.816807
2056.380996	14122.286777	47.821812
2052.979269	13941.889896	47.826817
2049.364979	13748.252316	47.831821
2046.394160	13565.486631	47.836826
2042.900348	13366.166747	47.841831
2039.408907	13178.240053	47.846836
2036.230884	12986.007883	47.851841
2032.355001	12785.525481	47.856845
2029.602000	12591.356554	47.861850
2026.027286	12398.619393	47.866855
2022.794088	12197.279690	47.871860
2019.139677	11996.688706	47.876865
2015.388432	11795.579988	47.881869
2012.261549	11596.183393	47.886874
2008.727016	11396.843202	47.891879
2004.826148	11204.124996	47.896884
2001.602429	11004.857470	47.901889
1998.124027	10819.133448	47.906893
1994.690740	10606.911085	47.911898
1991.320246	10406.400316	47.916903
1987.395184	10210.391261	47.921908
1984.334596	10011.267075	47.926913
1980.620675	9823.798120	47.931917
1977.453740	9619.060191	47.936922
1973.715363	9415.423700	47.941927
1970.328512	9217.618891	47.946932
1967.173526	9014.841955	47.951937
1963.647838	8813.264755	47.956941
1960.362083	8600.956707	47.961946
1956.273866	8405.821524	47.966951
1952.619310	8193.256171	47.971956
1949.288126	7995.164503	47.976961
1946.169803	7798.905924	47.981965
1942.829587	7581.889371	47.986970
1938.990633	7385.165579	47.991975
1936.198298	7179.259747	47.996980
1932.401410	6967.879701	48.001985
1928.591092	6761.871976	48.006989
1925.072298	6561.289951	48.011994
1921.712618	6351.472201	48.016999
1917.892524	6151.587448	48.022004
1914.594871	5945.999225	48.027009
1911.006309	5739.677130	48.032013
1907.675839	5533.342298	48.037018
1904.662695	5327.881075	48.042023
1901.004123	5118.769845	48.047028
1897.556006	4909.738847	48.052033
1893.483811	4700.282581	48.057037
1890.577728	4486.149390	48.062042
1886.958002	4282.044896	48.067047
1883.257629	4068.528261	48.072052
1879.539426	3849.722780	48.077057
1875.930968	3658.518745	48.082061
1872.511213	3438.187418	48.087066
1868.699972	3233.738654	48.092071
1865.126893	3036.178475	48.097076
1861.803747	2827.556971	48.102081
1858.366919	2629.755259	48.107085
1855.076064	2420.782179	48.112090
1851.424878	2216.898957	48.117095
1847.785037	2012.082851	48.122100
1844.443614	1803.846281	48.127105
1840.752098	1613.129426	48.132109
1837.591659	1397.737429	48.137114
1833.824066	1202.901454	48.142119
1830.036113	1000.932881	48.147124
1826.743514	802.451660	48.152129
1822.617597	609.529132	48.157133
1819.152737	419.434981	48.162138
1815.267838	229.032095	48.167143
1811.388596	54.275337	48.172148
1802.642086	-5.306336	48.177153
1790.030926	80.267370	48.182157
1784.435988	77.052184	48.187162
1781.069421	78.585158	48.192167
1778.911927	82.428323	48.197172
1777.434566	69.574077	48.202177
1774.904792	81.021167	48.207181
1772.279637	75.803625	48.212186
1769.143568	86.171831	48.217191
1765.624507	82.394504	48.222196
1762.610053	81.417269	48.227201
1759.139693	87.224971	48.232205
1755.962989	70.333900	48.237210
1751.991296	78.852340	48.242215
1748.576690	87.179196	48.247220
1745.680123	79.564845	48.252225
1742.050452	79.107846	48.257229
1738.841901	74.139804	48.262234
1735.202182	80.619430	48.267239
1731.133492	82.094619	48.272244
1728.083094	79.674000	48.277249
1724.910935	76.687134	48.282253
1721.713418	83.024793	48.287258
1718.276934	85.973456	48.292263
1714.383841	72.700010	48.297268
1711.243838	78.851496	48.302273
1707.727958	90.123892	48.307277
1704.100042	75.385238	48.312282
1700.833503	86.450930	48.317287
1697.781346	83.685740	48.322292
1693.839251	68.939317	48.327297
1690.327269	81.214026	48.332301
1686.804245	74.643715	48.337306
1683.807648	67.465831	48.342311
1679.901108	81.520234	48.347316
1676.972774	81.462868	48.352321
1672.928573	86.366969	48.357325
1669.724455	78.130052	48.362330
1666.461055	81.409151	48.367335
1662.662637	80.772943	48.372340
1659.510444	73.556141	48.377345
1655.683832	81.175533	48.382349
1652.626452	81.979940	48.387354
1648.804284	76.646051	48.392359
1645.218632	82.266180	48.397364
1641.900517	84.724935	48.402369
1638.301871	82.443933	48.407373
1634.927464	73.730639	48.412378
1631.532034	72.613751	48.417383
1627.868624	82.295716	48.422388
1625.068340	78.583120	48.427393
1620.753800	85.389863	48.432397
1617.543382	77.549427	48.437402
1614.201772	79.078547	48.442407
1610.896769	70.132937	48.447412
1607.697960	67.026895	48.452417
1603.583730	83.394921	48.457421
1599.950774	74.624029	48.462426
1596.317800	78.539965	48.467431
1593.022673	81.080559	48.472436
1589.446580	73.404938	48.477441
1586.156181	81.392850	48.482445
1582.967168	69.395017	48.487450
1579.202386	76.248607	48.492455
1575.859220	77.812784	48.497460
1572.542354	78.275008	48.502465
1568.735803	73.609434	48.507469
1565.269941	74.325938	48.512474
1561.389261	73.955747	48.517479
1557.952677	74.661344	48.522484
1555.226369	66.099752	48.527489
1551.222791	78.296409	48.532493
1547.795350	68.395539	48.537498
1544.258151	76.909313	48.542503
1540.702838	75.137264	48.547508
1537.873198	74.650034	48.552513
1533.916010	82.821419	48.557517
1530.336664	82.843843	48.562522
1526.785273	81.052203	48.567527
1523.159317	79.126700	48.572532
1520.246981	74.836882	48.577537
1516.288398	81.296878	48.582541
1513.024522	77.429085	48.587546
1509.594775	77.301550	48.592551
1505.868863	87.236945	48.597556
1502.517751	77.289341	48.602561
1498.707456	82.704228	48.607565
1495.371512	76.756454	48.612570
1492.003513	82.794985	48.617575
1488.092766	74.099261	48.622580
1484.744642	74.297484	48.627585
1481.186498	79.385003	48.632589
1478.076638	75.078660	48.637594
1474.722833	69.266571	48.642599
1470.931085	82.648156	48.647604
1467.585808	69.510554	48.652609
1464.043355	79.205268	48.657613
1460.260495	76.067305	48.662618
1457.087604	72.859180	48.667623
1453.620411	78.277324	48.672628
1450.501171	71.125046	48.677633
1446.686467	71.320383	48.682637
1443.085953	74.427685	48.687642
1439.221041	76.918305	48.692647
1435.660164	78.263501	48.697652
1432.333263	73.978491	48.702657
1428.757979	83.232260	48.707661
1425.723403	81.853312	48.712666
1422.263564	80.961715	48.717671
1418.262477	78.683677	48.722676
1415.242998	77.628240	48.727681
1411.150814	84.783073	48.732685
1407.987489	72.594627	48.737690
1404.322329	76.474534	48.742695
1400.738305	77.864494	48.747700
1397.689299	68.638452	48.752705
1393.910286	80.540573	48.757709
1390.560222	73.459249	48.762714
1387.229689	67.551802	48.767719
1383.300910	70.881352	48.772724
1380.105337	66.240444	48.777729
1376.471536	80.021277	48.782733
1373.011414	71.872008	48.787738
1369.621304	70.071000	48.792743
1365.874960	87.991874	48.797748
1362.783723	79.281821	48.802753
1359.035824	78.995329	48.807757
1355.415777	81.545727	48.812762
1352.129102	75.349848	48.817767
1348.431888	66.829577	48.822772
1345.317855	71.888747	48.827777
1341.546392	80.116543	48.832781
1337.838166	75.457820	48.837786
1334.664869	74.274624	48.842791
1330.427831	83.641502	48.847796
1327.319433	86.175094	48.852801
1323.861510	85.650232	48.857805
1320.855961	79.369227	48.862810
1317.176687	76.218271	48.867815
1313.404553	77.770588	48.872820
1310.195644	73.096989	48.877825
1306.386201	79.226823	48.882829
1303.302267	67.639771	48.887834
1299.466936	69.736665	48.892839
1295.435721	65.255075	48.897844
1292.414344	69.477170	48.902849
1288.715124	74.903212	48.907853
1285.622617	72.802543	48.912858
1282.121871	66.194111	48.917863
1278.614420	85.191258	48.922868
1275.198452	67.527938	48.927873
1271.296973	79.221471	48.932877
1268.135357	72.708652	48.937882
1264.586372	78.664847	48.942887
1260.916046	68.280099	48.947892
1257.774163	69.623040	48.952897
1253.784704	76.850430	48.957901
1250.377464	67.145846	48.962906
1246.972813	59.706132	48.967911
1243.208161	65.284799	48.972916
1240.077913	68.052792	48.977921
1236.131623	65.949755	48.982925
1232.947194	68.650300	48.987930
1229.165495	70.473067	48.992935
1225.883210	78.118112	48.997940
1223.015133	68.810029	49.002945
1219.138770	74.092980	49.007949
1215.517985	64.130775	49.012954
1211.767699	70.165954	49.017959
1208.043050	74.640540	49.022964
1205.039385	63.281414	49.027969
1201.555427	72.435522	49.032973
1198.263255	74.884025	49.037978
1194.225167	74.377268	49.042983
1191.013780	71.963044	49.047988
1187.916067	78.082735	49.052993
1183.976009	73.738784	49.057997
1180.485002	78.749448	49.063002
1176.972704	73.446345	49.068007
1173.168348	73.969201	49.073012
1169.918519	77.132426	49.078017
1166.389477	75.084319	49.083021
1163.093722	73.344544	49.088026
1159.848619	70.394603	49.093031
1155.813820	70.447337	49.098036
1152.619931	63.563128	49.103041
1148.571094	72.157111	49.108045
1145.088851	71.202683	49.113050
1141.991361	71.387094	49.118055
1138.501790	76.267831	49.123060
1135.267627	70.329575	49.128065
1131.327516	70.728166	49.133069
1127.823308	73.795186	49.138074
1124.293078	66.115751	49.143079
1120.765975	71.264962	49.148084
1117.935425	56.677026	49.153089
1114.097236	71.505489	49.158093
1110.496178	66.788957	49.163098
1107.045330	72.869041	49.168103
1103.272051	71.175575	49.173108
1099.539506	69.586465	49.178113
1096.195635	79.231207	49.183117
1092.885843	64.775254	49.188122
1089.438330	69.526033	49.193127
1085.824865	74.565389	49.198132
1082.395722	64.358104	49.203137
1078.732669	65.864955	49.208141
1075.662641	61.843589	49.213146
1071.989415	70.584436	49.218151
1068.320778	64.682593	49.223156
1064.806444	61.328747	49.228161
1061.226858	69.710085	49.233165
1057.883731	67.076088	49.238170
1054.420965	60.455480	49.243175
1050.665176	66.244798	49.248180
1047.366446	54.856009	49.253185
1043.821619	70.578202	49.258189
1040.351691	68.859413	49.263194
1036.785188	74.340690	49.268199
1033.332414	64.829994	49.273204
1030.278235	67.968956	49.278209
1026.600652	68.990880	49.283213
1022.839436	70.737750	49.288218
1019.443426	64.464211	49.293223
1015.701514	61.462394	49.298228
1012.529970	69.463481	49.303233
1008.585950	68.271354	49.308237
1004.782140	70.613362	49.313242
1001.655603	67.319046	49.318247
998.061558	81.457584	49.323252
995.056469	71.032078	49.328257
991.370987	78.806756	49.333261
987.460585	73.651486	49.338266
983.989087	69.699337	49.343271
980.636399	72.397831	49.348276
977.746566	70.528127	49.353281
974.021857	71.709310	49.358285
970.261405	60.981308	49.363290
966.698215	68.354025	49.368295
963.408975	74.332920	49.373300
960.089987	62.846095	49.378305
956.244007	61.382374	49.383309
952.730692	56.471837	49.388314
949.247572	62.762665	49.393319
945.811117	69.267653	49.398324
941.883782	63.162762	49.403329
938.514999	77.503324	49.408333
935.039131	68.923273	49.413338
932.324434	64.213564	49.418343
928.323777	67.098955	49.423348
925.167286	72.291441	49.428353
921.352376	71.158229	49.433357
917.569727	68.495027	49.438362
914.050194	63.604460	49.443367
910.355388	68.903385	49.448372
906.974617	71.691722	49.453377
903.752719	76.230064	49.458381
899.787898	74.870395	49.463386
897.293812	63.327201	49.468391
893.668459	62.904643	49.473396
890.045733	67.258974	49.478401
886.015531	74.543493	49.483405
882.289096	70.969827	49.488410
879.093822	72.979314	49.493415
875.775419	76.469746	49.498420
872.817706	72.661819	49.503425
869.012011	66.718248	49.508429
865.201090	72.231525	49.513434
861.403439	64.261884	49.518439
857.901579	67.749409	49.523444
854.803275	63.792661	49.528449
850.797787	63.521393	49.533453
847.537506	66.600933	49.538458
844.539872	60.426439	49.543463
841.009307	74.583546	49.548468
837.643981	57.867990	49.553473
834.027170	57.159378	49.558477
830.136619	66.652506	49.563482
826.666761	67.471134	49.568487
822.791860	71.766901	49.573492
819.478215	62.879926	49.578497
815.964481	63.192898	49.583501
812.540360	68.974656	49.588506
809.291276	58.226771	49.593511
805.426909	64.931687	49.598516
802.056740	67.712071	49.603521
798.369586	63.145196	49.608525
795.319832	63.746189	49.613530
792.013255	54.978346	49.618535
788.278399	61.871796	49.623540
784.924014	58.401267	49.628545
780.888816	62.722149	49.633549
777.395643	59.624535	49.638554
774.127273	57.627513	49.643559
770.382736	61.757350	49.648564
767.278219	53.596958	49.653569
763.628474	56.797623	49.658573
759.899732	64.357681	49.663578
756.715282	60.259435	49.668583
752.989146	64.158606	49.673588
749.585934	62.546542	49.678593
746.376705	56.297653	49.683597
742.711076	65.369607	49.688602
739.100333	58.130062	49.693607
735.500504	62.955427	49.698612
732.121108	63.339142	49.703617
728.473831	62.252527	49.708621
725.213007	57.096900	49.713626
721.752284	59.866181	49.718631
717.810596	66.368101	49.723636
714.435366	53.865141	49.728641
711.038530	63.831485	49.733645
707.366817	63.802241	49.738650
704.092761	62.799557	49.743655
700.503052	61.985514	49.748660
697.404382	58.943211	49.753665
693.472569	58.486467	49.758669
689.851059	64.473182	49.763674
686.504162	54.949231	49.768679
682.502964	56.755960	49.773684
679.696883	56.189365	49.778689
676.236000	64.096647	49.783693
672.708324	58.457645	49.788698
669.138481	57.960043	49.793703
665.199016	62.322927	49.798708
661.804361	53.711305	49.803713
658.158772	47.325148	49.808717
654.789861	52.595267	49.813722
651.861392	52.126942	49.818727
648.142237	57.828404	49.823732
645.073240	43.078708	49.828737
641.169503	59.265322	49.833741
637.711673	54.460124	49.838746
634.184337	52.098749	49.843751
630.400035	55.295226	49.848756
626.950393	63.722783	49.853761
623.211697	59.154566	49.858765
620.107741	58.577693	49.863770
616.553407	57.115898	49.868775
612.588755	55.284931	49.873780
609.461849	53.879586	49.878785
605.534821	57.240795	49.883789
602.410094	60.296019	49.888794
598.621046	54.220257	49.893799
595.780434	66.652681	49.898804
592.000456	51.501823	49.903809
588.371071	55.686458	49.908813
584.747784	59.411394	49.913818
581.134254	57.291331	49.918823
577.794345	61.332558	49.923828
574.516564	61.551719	49.928833
571.052104	66.330630	49.933837
567.430811	61.547897	49.938842
564.307523	53.697414	49.943847
560.507381	69.557786	49.948852
557.207099	53.265627	49.953857
553.139801	64.260842	49.958861
549.465365	60.084392	49.963866
546.263748	58.652805	49.968871
542.891206	67.273958	49.973876
539.506160	58.698848	49.978881
536.284735	62.193184	49.983885
532.534408	64.356155	49.988890
528.767130	63.187176	49.993895
525.131143	56.701495	49.998900
522.000294	59.090150	50.003905
518.527060	62.003833	50.008909
515.183964	62.729956	50.013914
511.136943	58.320812	50.018919
507.462241	67.201274	50.023924
504.404579	55.654751	50.028929
500.849383	66.541305	50.033933
497.383704	64.543651	50.038938
493.882703	54.920537	50.043943
490.721378	68.785779	50.048948
486.980893	64.603882	50.053953
483.060996	70.188151	50.058957
479.929629	62.285180	50.063962
476.213811	63.939730	50.068967
472.746210	72.025301	50.073972
469.051033	64.239116	50.078977
465.632308	66.521019	50.083981
462.190250	58.037132	50.088986
458.843095	60.643185	50.093991
455.388305	66.053374	50.098996
452.158239	56.308748	50.104001
448.061509	67.390870	50.109005
444.659170	60.390901	50.114010
441.266375	59.973226	50.119015
437.625607	65.225889	50.124020
434.484898	71.020326	50.129025
430.986901	69.878813	50.134029
427.323938	71.594707	50.139034
423.773827	65.658769	50.144039
419.959626	67.195874	50.149044
416.871493	52.990277	50.154049
413.008563	62.947455	50.159053
409.947797	62.927039	50.164058
406.473774	68.599686	50.169063
402.698689	70.719131	50.174068
399.393775	60.002321	50.179073
395.755966	58.746680	50.184077
392.406142	57.803437	50.189082
388.694220	69.587773	50.194087
385.158919	61.624726	50.199092
381.735383	52.634940	50.204097
378.427431	59.436352	50.209101
374.796325	68.525165	50.214106
371.023767	61.880611	50.219111
367.335257	66.716834	50.224116
364.131933	58.989700	50.229121
360.515001	61.508332	50.234125
357.190871	70.909736	50.239130
354.146222	56.716337	50.244135
350.198632	66.139469	50.249140
346.920683	53.922005	50.254145
343.257336	61.278972	50.259149
340.037018	56.354438	50.264154
336.113493	53.413003	50.269159
332.295663	61.344667	50.274164
328.996549	65.022083	50.279169
324.861360	62.262504	50.284173
322.102767	58.486861	50.289178
319.500864	52.975082	50.294183
315.302326	67.028148	50.299188
311.760528	65.282939	50.304193
307.902313	55.380511	50.309197
304.155096	67.160909	50.314202
301.358495	59.313142	50.319207
297.854993	65.161286	50.324212
294.430998	64.239190	50.329217
290.987551	60.289263	50.334221
287.417328	62.218476	50.339226
283.542958	55.985385	50.344231
279.663858	71.810751	50.349236
276.329545	62.503311	50.354241
272.580025	62.299770	50.359245
269.368824	64.653640	50.364250
265.823083	64.104968	50.369255
262.905142	64.932262	50.374260
259.580534	64.893118	50.379265
255.803500	65.450032	50.384269
252.074247	63.901892	50.389274
248.474456	64.405733	50.394279
244.755999	62.783139	50.399284
242.019052	59.817218	50.404289
238.709739	59.503603	50.409293
234.850011	65.398081	50.414298
231.015982	62.730575	50.419303
227.467357	60.986471	50.424308
224.066635	58.254254	50.429313
220.380581	52.814272	50.434317
216.988451	64.671947	50.439322
213.685820	63.857421	50.444327
209.672650	65.384655	50.449332
206.219780	54.339940	50.454337
203.171421	60.888770	50.459341
199.655321	60.307007	50.464346
196.409687	55.671236	50.469351
192.410827	56.955790	50.474356
189.490097	53.993369	50.479361
185.631902	64.573144	50.484365
181.725406	62.764900	50.489370
178.609626	61.478191	50.494375
174.707328	63.779009	50.499380
171.254192	56.448599	50.504385
167.743174	54.154464	50.509389
164.451127	61.083167	50.514394
161.392525	53.842815	50.519399
157.585054	67.005768	50.524404
154.389628	63.703578	50.529409
150.689051	69.171360	50.534413
146.543409	62.768862	50.539418
143.451915	71.282833	50.544423
139.879299	75.930144	50.549428
136.340581	61.792101	50.554433
133.056802	71.048044	50.559437
129.762269	68.267590	50.564442
125.997081	63.064673	50.569447
122.551735	62.690156	50.574452
119.044347	56.836251	50.579457
115.638948	70.489885	50.584461
111.580735	55.354408	50.589466
108.353693	55.508844	50.594471
105.099574	68.556649	50.599476
101.386309	62.064289	50.604481
97.473017	55.397628	50.609485
94.650211	63.717654	50.614490
90.695224	53.055384	50.619495
87.002730	65.374606	50.624500
83.835467	67.025632	50.629505
81.119314	51.676750	50.634509
77.686198	55.451176	50.639514
73.836382	55.238124	50.644519
69.773803	64.745813	50.649524
66.533709	58.758305	50.654529
62.812011	66.766757	50.659533
59.324077	59.970196	50.664538
55.560698	58.617315	50.669543
52.414193	61.571727	50.674548
48.694393	57.544980	50.679553
45.426242	62.742570	50.684557
42.005549	65.442553	50.689562
38.467697	49.963005	50.694567
34.561159	60.632663	50.699572
31.024175	53.546411	50.704577
28.050506	59.368581	50.709581
24.828954	58.841982	50.714586
21.104946	55.515096	50.719591
17.259484	60.644960	50.724596
13.849953	55.734388	50.729601
10.505014	66.373014	50.734605
6.711791	61.066980	50.739610
3.518425	56.084578	50.744615