Thu Aug 25 10:22:33 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.748735	106.197009	0.000000
1.206243	102.596289	0.005005
1.641312	100.468576	0.010010
1.370485	95.645211	0.015014
1.256553	86.102252	0.020019
1.632904	88.321249	0.025024
1.505904	89.277679	0.030029
0.867987	66.627138	0.035034
0.824213	65.627984	0.040038
0.716495	62.506480	0.045043
-0.048586	58.371170	0.050048
-0.131350	49.250454	0.055053
-0.376384	40.180478	0.060058
-0.429788	40.236361	0.065062
-1.173373	30.171994	0.070067
-1.337507	23.797516	0.075072
-1.455901	23.183377	0.080077
-1.851312	20.796654	0.085082
-2.399345	5.595380	0.090086
-2.235937	7.246619	0.095091
-2.221094	4.460262	0.100096
-2.810985	10.864411	0.105101
-3.342434	0.624454	0.110106
-3.215620	4.141706	0.115110
-3.812255	-4.446053	0.120115
-4.356550	-8.691869	0.125120
-4.658268	-7.404350	0.130125
-4.607158	-22.326154	0.135130
-4.649961	-8.130027	0.140134
-4.982781	-3.964960	0.145139
-4.765891	-11.186896	0.150144
-5.656247	-4.393991	0.155149
-6.184184	-7.933693	0.160154
-6.329132	-2.554713	0.165158
-6.418001	-5.027427	0.170163
-6.404707	-4.074000	0.175168
-7.177079	-5.351296	0.180173
-7.116795	-4.781717	0.185178
-7.773719	-8.636564	0.190182
-7.951667	-2.363403	0.195187
-7.433794	-5.867650	0.200192
-7.704608	-11.975464	0.205197
-8.436866	-10.370552	0.210202
-8.955259	-13.706104	0.215206
-9.166952	-11.262108	0.220211
-9.012038	-15.978142	0.225216
-9.156055	-6.246006	0.230221
-9.098788	-9.709721	0.235226
-9.645800	-9.990947	0.240230
-10.418709	-3.099385	0.245235
-10.388061	-21.219686	0.250240
-10.524301	-12.475858	0.255245
-10.512507	-22.016311	0.260250
-11.488243	-15.747868	0.265254
-12.174582	-11.929207	0.270259
-12.109077	-10.240483	0.275264
-12.329106	-8.035624	0.280269
-12.070411	-10.002813	0.285274
-12.213305	-13.862269	0.290278
-12.181493	-16.964492	0.295283
-12.299809	-12.152832	0.300288
-13.273969	-8.804763	0.305293
-13.428121	-11.349504	0.310298
-13.613723	-10.317458	0.315302
-13.933442	-11.763751	0.320307
-14.390858	-13.447896	0.325312
-14.943621	-1.127052	0.330317
-15.288760	-1.414598	0.335322
-14.897894	-2.377446	0.340326
-15.415525	-2.704403	0.345331
-15.057087	-13.343208	0.350336
-15.043564	-7.280381	0.355341
-15.324526	-5.493079	0.360346
-15.975499	-14.553206	0.365350
-16.802328	-4.926055	0.370355
-16.555801	-8.055594	0.375360
-16.624746	1.889408	0.380365
-17.208077	-5.808258	0.385370
-17.828194	1.173260	0.390374
-18.060366	-10.230380	0.395379
-18.102937	-2.061206	0.400384
-18.156926	-1.682529	0.405389
-18.412832	-4.167036	0.410394
-18.107284	-13.332742	0.415398
-19.085706	3.952265	0.420403
-18.998175	-10.788593	0.425408
-19.579934	-0.842336	0.430413
-19.652989	1.690671	0.435418
-19.451572	-9.954912	0.440422
-20.032004	-11.654582	0.445427
-20.402863	-19.164072	0.450432
-21.218544	-12.949179	0.455437
-20.890417	-5.818847	0.460442
-20.781819	-10.439040	0.465446
-21.392695	-8.638011	0.470451
-22.015417	-1.773144	0.475456
-22.438571	-8.337978	0.480461
-22.437218	-5.778666	0.485466
-22.293822	-6.753358	0.490470
-22.537630	-6.439852	0.495475
-22.225454	-12.385911	0.500480
-23.253475	-6.365535	0.505485
-23.746391	-12.175958	0.510490
-24.011257	-9.574934	0.515494
-23.940860	0.525404	0.520499
-23.570769	-7.751916	0.525504
-24.147333	-0.672819	0.530509
-24.827724	-5.659771	0.535514
-25.128408	-7.017298	0.540518
-25.031366	-8.661767	0.545523
-24.973688	-11.246027	0.550528
-25.572498	-2.069051	0.555533
-25.772133	-5.929109	0.560538
-26.446054	-3.501272	0.565542
-26.820279	-2.325777	0.570547
-26.930665	-11.214342	0.575552
-26.820301	-0.528649	0.580557
-26.704563	-2.517732	0.585562
-26.848844	2.415057	0.590566
-28.098308	-4.564470	0.595571
-28.172104	-8.893495	0.600576
-28.217060	-2.802523	0.605581
-28.170302	-9.675100	0.610586
-28.630333	-6.489842	0.615590
-29.366113	-4.533201	0.620595
-29.248408	-11.100520	0.625600
-29.498284	-7.840623	0.630605
-29.826034	-1.952113	0.635610
-30.021869	2.659726	0.640614
-29.891759	9.827417	0.645619
-30.232976	-8.743990	0.650624
-30.774054	-3.853434	0.655629
-31.022018	2.867295	0.660634
-30.713456	-5.514279	0.665638
-31.764054	-0.078818	0.670643
-32.113730	-12.432148	0.675648
-32.326121	3.451519	0.680653
-32.458894	3.152845	0.685658
-32.498067	5.816584	0.690662
-32.666622	4.270676	0.695667
-31.946760	-5.456658	0.700672
-32.913873	-2.723455	0.705677
-33.778849	8.390310	0.710682
-33.691629	-0.171720	0.715686
-33.971392	9.122950	0.720691
-33.894260	1.461002	0.725696
-34.599209	-9.805285	0.730701
-35.110630	-12.167497	0.735706
-34.920777	-6.926398	0.740710
-35.343666	-3.471714	0.745715
-35.234178	-13.100242	0.750720
-35.417289	-5.231751	0.755725
-35.758947	-17.760338	0.760730
-36.311534	-11.877731	0.765734
-36.672991	-7.932803	0.770739
-36.888863	-9.490278	0.775744
-37.230498	-5.785736	0.780749
-37.114423	-17.025637	0.785754
-37.100152	-8.393976	0.790758
-37.877108	-13.103204	0.795763
-38.027139	-14.854492	0.800768
-38.323898	-6.889100	0.805773
-38.316225	-15.470296	0.810778
-38.216557	-13.600266	0.815782
-39.210705	-1.491837	0.820787
-39.508241	-12.524565	0.825792
-39.644297	-10.747313	0.830797
-39.877487	-4.427533	0.835802
-39.820553	-6.173286	0.840806
-40.217888	-4.551246	0.845811
-40.318892	-10.989383	0.850816
-40.741509	-9.338073	0.855821
-41.372535	-7.796475	0.860826
-41.507277	-8.857301	0.865830
-41.390577	-1.010474	0.870835
-41.543079	-5.738453	0.875840
-41.714623	-3.860728	0.880845
-41.894920	-11.457024	0.885850
-42.541433	-18.119731	0.890854
-42.874415	-9.430498	0.895859
-42.698094	0.374832	0.900864
-43.275389	-4.245459	0.905869
-43.755249	-14.651672	0.910874
-44.073154	-12.342892	0.915878
-44.694373	-8.550251	0.920883
-44.129176	-6.041321	0.925888
-44.519929	-7.074688	0.930893
-44.726826	-3.008445	0.935898
-44.781961	-14.240503	0.940902
-44.657758	5.149627	0.945907
-44.701926	-15.167242	0.950912
-45.477640	2.968683	0.955917
-46.243891	-8.091846	0.960922
-46.565689	-12.976793	0.965926
-47.308340	-5.061758	0.970931
-46.749561	-16.927841	0.975936
-46.895525	-3.031925	0.980941
-47.053034	-6.730905	0.985946
-47.348965	-1.891413	0.990950
-47.380882	-4.740044	0.995955
-48.046019	-11.377688	1.000960
-48.943183	-7.696833	1.005965
-48.926047	-10.578458	1.010970
-48.900275	-15.957623	1.015974
-49.103976	-15.919318	1.020979
-49.129818	-5.864018	1.025984
-49.032020	-10.115525	1.030989
-49.484551	-1.916918	1.035994
-49.791422	-8.379747	1.040998
-50.153576	-7.487715	1.046003
-50.002818	-13.380008	1.051008
-50.768068	-9.488869	1.056013
-51.346106	-9.575406	1.061018
-51.531686	-3.161847	1.066022
-52.110698	-0.226862	1.071027
-51.730761	-6.461949	1.076032
-51.824347	-9.307243	1.081037
-52.185906	-6.599320	1.086042
-52.237468	-12.981928	1.091046
-52.875263	-1.894275	1.096051
-53.369902	-8.599763	1.101056
-53.341876	-6.069941	1.106061
-53.434361	-7.260773	1.111066
-53.181154	-11.210766	1.116070
-53.995920	-3.335050	1.121075
-54.555547	-12.817607	1.126080
-54.857272	0.634484	1.131085
-54.855005	1.795281	1.136090
-54.581125	-5.603263	1.141094
-54.803023	4.504908	1.146099
-55.753259	-0.806754	1.151104
-56.186532	0.384323	1.156109
-56.499536	-2.999229	1.161114
-56.294811	-2.066307	1.166118
-56.499825	2.970911	1.171123
-56.334414	-8.254578	1.176128
-56.781736	3.692243	1.181133
-57.089936	-3.728991	1.186138
-57.362309	3.270807	1.191142
-58.214554	-0.363608	1.196147
-57.909496	-10.174640	1.201152
-57.943933	-6.480267	1.206157
-58.846881	-11.052692	1.211162
-59.030701	-11.356022	1.216166
-59.435987	4.320586	1.221171
-59.268765	-0.897250	1.226176
-59.401934	-9.146333	1.231181
-59.546606	-4.238794	1.236186
-59.500241	-2.202224	1.241190
-60.680402	-5.611252	1.246195
-60.630336	-12.047749	1.251200
-60.814880	-5.760902	1.256205
-61.246151	3.010176	1.261210
-61.120589	-6.677820	1.266214
-60.972310	-5.701253	1.271219
-61.384010	-17.228612	1.276224
-62.064287	-5.049144	1.281229
-62.177735	-7.343999	1.286234
-62.244420	-16.875317	1.291238
-62.941853	-10.204390	1.296243
-63.511408	-16.050254	1.301248
-63.652178	-11.231914	1.306253
-63.719334	-3.334136	1.311258
-63.740464	-14.903712	1.316262
-63.954650	-6.495682	1.321267
-63.690911	-11.624235	1.326272
-64.736891	-10.780078	1.331277
-65.346632	-15.891986	1.336282
-65.035662	-13.140746	1.341286
-65.275731	-7.348233	1.346291
-65.011618	-14.299156	1.351296
-65.251726	-12.711243	1.356301
-66.309886	-8.470489	1.361306
-66.495920	-10.542000	1.366310
-66.718281	-11.041769	1.371315
-66.699104	-12.227951	1.376320
-66.804643	-10.423843	1.381325
-67.220213	-10.330194	1.386330
-67.628828	-14.511841	1.391334
-68.410998	-3.831835	1.396339
-68.225942	-16.898527	1.401344
-68.202422	-4.076367	1.406349
-68.681973	-14.115631	1.411354
-68.405540	-12.314427	1.416358
-69.187612	-5.250587	1.421363
-69.394650	-14.551107	1.426368
-69.782440	-7.273803	1.431373
-70.186834	-11.965473	1.436378
-69.778244	-17.768450	1.441382
-70.376800	-4.538772	1.446387
-69.774021	-8.831439	1.451392
-70.643094	-13.383860	1.456397
-70.930944	-11.788467	1.461402
-71.180105	-13.704554	1.466406
-71.358275	-8.370992	1.471411
-71.576266	-8.178587	1.476416
-72.319912	-9.855844	1.481421
-72.676222	-2.580306	1.486426
-72.537334	-18.594693	1.491430
-73.052483	0.405228	1.496435
-72.515996	-1.282789	1.501440
-73.046931	-2.737113	1.506445
-73.569714	-7.432380	1.511450
-73.858689	-7.219363	1.516454
-74.104609	-10.040786	1.521459
-74.087266	-13.770324	1.526464
-74.607222	4.790595	1.531469
-75.497372	4.968098	1.536474
-75.547127	7.402542	1.541478
-75.397245	-0.201200	1.546483
-75.831192	-10.418452	1.551488
-75.739773	-1.295845	1.556493
-75.817022	4.101001	1.561498
-75.588672	-8.001213	1.566502
-76.767561	-9.366662	1.571507
-76.848646	-9.784165	1.576512
-76.863875	-11.635668	1.581517
-77.069450	-12.071629	1.586522
-77.500894	-14.335638	1.591526
-78.134271	-9.452766	1.596531
-78.321555	-21.097541	1.601536
-78.608901	-13.098828	1.606541
-78.865495	-12.761171	1.611546
-78.306746	-5.695454	1.616550
-78.666203	-14.798085	1.621555
-79.066928	-20.043982	1.626560
-79.519779	-12.775467	1.631565
-79.936517	-8.366299	1.636570
-79.977079	-12.539178	1.641574
-79.970352	-13.021060	1.646579
-80.449026	-15.869287	1.651584
-81.253997	-13.756269	1.656589
-81.398272	-1.901229	1.661594
-81.110180	-11.573560	1.666598
-81.430942	-0.750717	1.671603
-81.588644	-8.072143	1.676608
-82.224999	-0.312965	1.681613
-83.030860	-9.035605	1.686618
-82.787063	-14.047137	1.691622
-83.013122	-6.257339	1.696627
-83.112078	-7.966010	1.701632
-83.071067	-3.688677	1.706637
-83.135783	-5.583045	1.711642
-83.607622	-10.416006	1.716646
-83.942381	-9.914242	1.721651
-84.096178	-4.382019	1.726656
-84.765230	-9.139786	1.731661
-85.157296	-0.207175	1.736666
-84.981478	-21.055207	1.741670
-85.655854	-8.092060	1.746675
-85.702000	-12.441233	1.751680
-85.638314	-5.560535	1.756685
-85.940290	-5.854841	1.761690
-85.997634	-8.788070	1.766694
-86.329244	-10.185040	1.771699
-86.690680	-7.379060	1.776704
-87.129401	-7.889219	1.781709
-87.490306	-12.457989	1.786714
-87.829169	-18.289378	1.791718
-88.530787	-22.330199	1.796723
-88.705195	-19.455450	1.801728
-88.431287	-16.195371	1.806733
-88.621011	-13.090432	1.811738
-88.684943	-16.120703	1.816742
-88.949101	-16.895495	1.821747
-88.924792	-17.645885	1.826752
-89.323839	-15.821097	1.831757
-89.920008	-10.241706	1.836762
-90.048389	-16.675548	1.841766
-90.459699	-11.514262	1.846771
-90.363167	-16.486900	1.851776
-90.883934	-12.273403	1.856781
-91.749993	-20.733503	1.861786
-91.566310	-20.180098	1.866790
-91.707143	-12.305582	1.871795
-92.094689	-8.638138	1.876800
-92.096407	-7.002157	1.881805
-91.899443	-14.812584	1.886810
-92.125480	-17.535882	1.891814
-92.943772	-6.771125	1.896819
-93.048727	-9.209678	1.901824
-93.467513	-10.706882	1.906829
-93.442743	-13.877602	1.911834
-93.550917	-22.079972	1.916838
-94.605433	-7.367826	1.921843
-94.784820	-7.798399	1.926848
-94.844082	-16.951229	1.931853
-95.237826	-11.365592	1.936858
-94.801344	-15.685984	1.941862
-94.981476	-12.699607	1.946867
-95.429537	-6.801738	1.951872
-95.968787	-8.517347	1.956877
-96.349364	-7.745813	1.961882
-96.287554	-16.386106	1.966886
-96.927441	-6.816722	1.971891
-96.799278	-14.901104	1.976896
-96.832216	-25.215981	1.981901
-97.739607	0.017841	1.986906
-97.565948	-7.649733	1.991910
-97.801838	-1.892676	1.996915
-97.901800	-6.885548	2.006912
-98.198764	-11.920025	2.016909
-97.248086	-12.711929	2.026906
-96.941800	-14.669976	2.036902
-96.775468	-13.555516	2.046899
-95.626830	-14.559003	2.056896
-95.450793	-12.273983	2.066893
-95.130015	-10.201710	2.076890
-94.424634	-1.698905	2.086886
-93.938980	-7.844363	2.096883
-92.742963	-7.540643	2.106880
-92.548822	-9.839078	2.116877
-92.546921	-12.427337	2.126874
-92.407760	-13.659116	2.136870
-91.657018	-10.330080	2.146867
-90.835713	-13.718303	2.156864
-90.014832	-5.426832	2.166861
-89.930626	-11.211614	2.176858
-89.517223	-6.594282	2.186854
-88.869795	-15.365839	2.196851
-88.272914	-18.218386	2.206848
-87.982886	-4.781613	2.216845
-87.553404	-9.483261	2.226842
-87.077771	-12.057052	2.236838
-86.329027	-10.799434	2.246835
-85.288642	-5.998412	2.256832
-85.561813	-8.176106	2.266829
-85.345216	-7.034676	2.276826
-84.595876	-6.847863	2.286822
-83.481737	-10.839502	2.296819
-82.940933	-9.007610	2.306816
-82.745334	-3.808121	2.316813
-82.818517	-9.498551	2.326810
-81.932826	-10.498848	2.336806
-81.513602	-10.947719	2.346803
-80.282210	-10.282076	2.356800
-80.377972	-7.796077	2.366797
-80.181318	-3.414043	2.376794
-79.633783	-6.772041	2.386790
-78.515203	-4.048666	2.396787
-78.552596	-8.328703	2.406784
-77.760952	-5.769510	2.416781
-77.237707	-11.768803	2.426778
-76.991336	1.015917	2.436774
-76.232110	-1.567465	2.446771
-75.791935	-12.704565	2.456768
-75.422218	-6.936816	2.466765
-75.133298	-7.324087	2.476762
-74.753827	1.660608	2.486758
-73.738816	-5.261542	2.496755
-73.243253	-7.860630	2.506752
-72.781369	-9.127138	2.516749
-71.845537	-6.663396	2.526746
-71.770524	-9.804803	2.536742
-71.610689	-8.299686	2.546739
-70.786566	-8.149933	2.556736
-70.222918	-6.270934	2.566733
-70.123774	-0.432276	2.576730
-69.404009	-4.862631	2.586726
-68.917825	-6.902719	2.596723
-68.051925	-0.886432	2.606720
-67.314524	-6.269886	2.616717
-67.526399	1.825454	2.626714
-67.203338	-3.040084	2.636710
-66.286539	-8.762091	2.646707
-65.500157	-1.257155	2.656704
-65.680032	-4.212907	2.666701
-64.743540	-4.498907	2.676698
-64.383427	-8.638491	2.686694
-63.679260	-9.914451	2.696691
-62.788930	-9.401272	2.706688
-62.823623	-7.083230	2.716685
-62.880638	-9.431010	2.726682
-61.873776	-11.077514	2.736678
-61.412778	-11.805359	2.746675
-60.563608	-9.134802	2.756672
-59.896861	-1.145455	2.766669
-59.933299	-5.200730	2.776666
-59.362600	-4.067265	2.786662
-58.766204	-5.012728	2.796659
-58.440540	-11.839533	2.806656
-57.613134	-5.490932	2.816653
-57.336141	-12.522353	2.826650
-56.961967	-7.236804	2.836646
-56.393408	-7.379622	2.846643
-55.917363	-7.514280	2.856640
-55.166867	-8.765822	2.866637
-54.636784	-8.487631	2.876634
-54.338572	-11.207850	2.886630
-54.077339	-4.073622	2.896627
-53.311724	-11.751806	2.906624
-52.769575	-7.078617	2.916621
-51.833754	-9.756190	2.926618
-51.654682	-10.458867	2.936614
-51.508405	-10.963170	2.946611
-51.151566	-10.863741	2.956608
-50.422042	-6.796448	2.966605
-49.478291	-4.942159	2.976602
-48.771300	-3.608304	2.986598
-48.376473	-7.648790	2.996595
-48.417742	-1.832479	3.006592
-48.302717	-5.220909	3.016589
-47.565007	-3.996404	3.026586
-46.629172	-3.436500	3.036582
-46.022967	-6.125783	3.046579
-45.958390	-10.459811	3.056576
-45.544044	-4.426621	3.066573
-44.286070	-3.825326	3.076570
-44.144795	0.540046	3.086566
-43.848851	-8.331663	3.096563
-43.663189	-6.117840	3.106560
-42.747516	-3.790318	3.116557
-41.965138	-7.593756	3.126554
-41.266909	-5.406392	3.136550
-41.385885	-1.985425	3.146547
-41.050617	-2.874133	3.156544
-40.073758	-0.033512	3.166541
-39.797106	-0.114753	3.176538
-39.598214	-5.055869	3.186534
-38.687053	-0.310616	3.196531
-37.940272	-11.150470	3.206528
-37.947413	-4.123077	3.216525
-37.096446	-3.337632	3.226522
-36.553144	-0.020434	3.236518
-36.599918	-5.711837	3.246515
-35.400063	1.677635	3.256512
-35.078138	-8.313208	3.266509
-34.915107	-3.919567	3.276506
-34.006928	-8.819764	3.286502
-33.342872	-8.556228	3.296499
-33.319999	-7.523825	3.306496
-33.416891	-6.897140	3.316493
-32.214595	-7.566906	3.326490
-31.495663	0.246377	3.336486
-30.871364	2.419984	3.346483
-30.549989	-1.095812	3.356480
-30.624872	-5.680421	3.366477
-29.960588	-8.207742	3.376474
-29.219953	-9.904394	3.386470
-28.794951	-10.959215	3.396467
-28.136296	-5.648546	3.406464
-28.134823	-10.273628	3.416461
-27.120214	-4.534059	3.426458
-26.815423	-8.319685	3.436454
-26.079278	-6.588087	3.446451
-25.333844	-3.270881	3.456448
-24.837515	-6.294572	3.466445
-25.011090	-3.701346	3.476442
-24.542537	-10.354138	3.486438
-23.690567	-9.524500	3.496435
-23.373649	-9.463163	3.506432
-22.317847	-11.437277	3.516429
-22.188758	0.820967	3.526426
-21.939263	-5.791168	3.536422
-21.228452	-2.674443	3.546419
-20.564116	-9.101320	3.556416
-20.238319	-4.913746	3.566413
-19.549010	1.763777	3.576410
-19.193473	-3.132193	3.586406
-18.963152	-3.770040	3.596403
-18.057636	-7.054246	3.606400
-17.446329	-6.472001	3.616397
-17.278741	-2.155100	3.626394
-16.434214	-3.744486	3.636390
-16.368796	-3.092548	3.646387
-15.797230	-6.650712	3.656384
-14.695995	-10.843060	3.666381
-14.651014	-3.412019	3.676378
-14.647135	-4.701797	3.686374
-14.216105	-0.378655	3.696371
-12.954218	-5.046003	3.706368
-12.203578	-4.533105	3.716365
-12.191681	-4.275090	3.726362
-11.875325	-4.121799	3.736358
-11.156304	2.807661	3.746355
-10.295985	-3.076555	3.756352
-10.208591	-6.485998	3.766349
-9.837451	-8.672784	3.776346
-8.910012	-5.748389	3.786342
-8.763165	-5.612888	3.796339
-8.371307	-6.982462	3.806336
-7.334923	-7.052859	3.816333
-7.070758	-9.086668	3.826330
-6.943501	-7.082269	3.836326
-6.040080	-8.633365	3.846323
-5.510228	-2.687960	3.856320
-5.690201	-0.629087	3.866317
-4.811699	2.632426	3.876314
-4.511607	3.811463	3.886310
-4.016049	18.305783	3.896307
-3.200462	20.455760	3.906304
-2.919324	32.740890	3.916301
-2.567744	40.538893	3.926298
-2.077078	56.035035	3.936294
-1.393458	67.788293	3.946291
-1.047861	71.256861	3.956288
-0.699031	77.484081	3.966285
-0.347784	101.824445	3.976282
0.000000	110.381882	3.981286
0.516057	131.327442	3.986291
0.511027	122.881045	3.991296
0.156854	134.180609	3.996301
0.834975	137.285641	4.001306
1.075844	150.871134	4.006310
1.101528	150.177469	4.011315
1.308521	151.625740	4.016320
1.359553	161.064814	4.021325
1.463226	160.320964	4.026330
1.223623	157.947774	4.031334
1.303351	152.405078	4.036339
1.375211	157.455906	4.041344
1.196164	158.629304	4.046349
1.366889	154.005661	4.051354
1.383384	152.199789	4.056358
0.817594	145.935656	4.061363
0.949125	142.808290	4.066368
1.005590	158.086822	4.071373
1.096341	154.700088	4.076378
1.240980	155.984121	4.081382
1.221612	153.509987	4.086387
1.643296	150.520657	4.091392
1.005296	156.309132	4.096397
1.417173	151.514828	4.101402
1.273086	148.522394	4.106406
1.104303	163.222453	4.111411
1.156017	147.522125	4.116416
1.430210	163.858047	4.121421
1.340960	161.711237	4.126426
1.334652	160.532200	4.131430
1.198103	163.239695	4.136435
1.203677	152.004343	4.141440
1.415672	157.583710	4.146445
1.553098	169.654162	4.151450
1.283436	165.928424	4.156454
1.393177	173.823878	4.161459
1.790827	175.210641	4.166464
1.512458	180.759279	4.171469
1.678557	180.034121	4.176474
1.710679	155.968681	4.181478
1.870931	173.578481	4.186483
1.564325	154.422504	4.191488
1.304706	157.598535	4.196493
1.440876	154.404002	4.201498
1.043740	163.166647	4.206502
1.535643	176.095893	4.211507
1.992235	175.689054	4.216512
1.995536	181.421351	4.221517
1.766206	161.500281	4.226522
1.394914	170.622714	4.231526
1.386510	172.348346	4.236531
1.720996	174.336630	4.241536
1.825181	175.782029	4.246541
1.980638	181.348116	4.251546
2.200813	179.137004	4.256550
1.320315	166.578811	4.261555
1.767668	164.942714	4.266560
1.878051	178.624604	4.271565
2.106631	178.879917	4.276570
1.493903	168.605141	4.281574
1.684868	172.979248	4.286579
2.149984	175.443777	4.291584
1.858164	174.265181	4.296589
1.629867	166.844006	4.301594
1.735279	165.834126	4.306598
1.708561	185.554992	4.311603
2.022313	182.104838	4.316608
1.821692	183.158231	4.321613
2.098638	174.927058	4.326618
1.873663	183.134389	4.331622
1.752734	185.016859	4.336627
2.075628	185.985062	4.341632
2.051310	193.623118	4.346637
1.898618	194.346296	4.351642
2.082153	191.520824	4.356646
1.987529	187.270944	4.361651
2.102530	187.003047	4.366656
1.696518	185.886635	4.371661
1.648212	175.102638	4.376666
2.312189	176.520440	4.381670
1.842472	181.368227	4.386675
2.023515	173.031858	4.391680
1.676632	175.313563	4.396685
1.972862	182.917209	4.401690
2.281076	175.978283	4.406694
2.014186	183.841004	4.411699
1.957433	187.168753	4.416704
1.817859	179.217976	4.421709
2.383781	180.549901	4.426714
2.133861	181.889429	4.431718
2.018888	190.063709	4.436723
2.222233	179.746485	4.441728
1.906905	189.600482	4.446733
1.780324	180.296738	4.451738
2.258082	197.315808	4.456742
2.134430	209.139290	4.461747
2.324990	209.400560	4.466752
2.129136	214.199120	4.471757
2.231276	202.385453	4.476762
2.777192	202.606865	4.481766
2.330508	211.507012	4.486771
2.470336	200.997246	4.491776
2.529964	198.599313	4.496781
2.479019	184.955672	4.501786
2.027537	186.317290	4.506790
2.103879	184.761468	4.511795
2.502572	197.344664	4.516800
2.245007	205.190113	4.521805
2.415460	206.254970	4.526810
2.557553	206.207456	4.531814
2.578446	214.025100	4.536819
2.504616	204.599182	4.541824
2.385674	204.219242	4.546829
2.223304	202.020608	4.551834
2.612407	210.865734	4.556838
2.371830	200.371277	4.561843
2.567839	204.940756	4.566848
2.088027	204.490807	4.571853
2.142572	200.049872	4.576858
2.365856	205.330090	4.581862
2.016220	197.696958	4.586867
2.501478	193.720053	4.591872
2.753818	208.142194	4.596877
2.616513	210.432195	4.601882
2.675376	198.856268	4.606886
2.482417	207.716659	4.611891
3.069358	196.785661	4.616896
2.607722	205.602727	4.621901
2.635660	199.115833	4.626906
2.953899	197.832159	4.631910
2.722268	203.072922	4.636915
2.807559	199.683870	4.641920
2.569014	210.183913	4.646925
2.589220	214.663880	4.651930
2.535531	206.079534	4.656934
2.483683	200.237897	4.661939
2.672581	200.610160	4.666944
2.752661	206.570882	4.671949
2.872220	208.542225	4.676954
2.992967	211.348619	4.681958
2.845441	207.091204	4.686963
3.002731	197.214623	4.691968
2.801968	209.043858	4.696973
2.725187	214.301491	4.701978
2.814314	205.381555	4.706982
2.926906	209.505358	4.711987
2.955761	202.898096	4.716992
2.924883	208.449094	4.721997
2.726633	203.902232	4.727002
2.502443	206.041330	4.732006
2.859667	215.888042	4.737011
3.377320	227.661675	4.742016
3.189823	217.456287	4.747021
2.665639	213.216757	4.752026
2.699120	211.708777	4.757030
2.795851	232.561968	4.762035
3.365662	229.549416	4.767040
3.271139	241.159545	4.772045
2.714503	214.648921	4.777050
2.603279	216.608967	4.782054
2.706834	232.168089	4.787059
3.098191	227.724995	4.792064
2.779334	238.636274	4.797069
3.012778	245.231047	4.802074
3.037377	234.714004	4.807078
2.888981	239.264687	4.812083
2.960694	237.329932	4.817088
3.038864	241.114283	4.822093
3.279360	234.676331	4.827098
3.542873	227.826648	4.832102
3.481131	243.699582	4.837107
3.251092	227.334642	4.842112
3.223771	237.766805	4.847117
3.426701	237.064348	4.852122
3.578764	238.926197	4.857126
3.317080	232.731445	4.862131
3.514345	237.575985	4.867136
3.579385	248.987110	4.872141
3.337973	239.732965	4.877146
3.247159	230.429918	4.882150
3.077828	242.153009	4.887155
3.557193	240.116417	4.892160
3.388343	243.164345	4.897165
3.513680	233.365517	4.902170
3.671704	232.515071	4.907174
3.420508	229.764035	4.912179
3.182269	215.662494	4.917184
3.360129	225.474039	4.922189
3.391198	223.650058	4.927194
3.451919	221.637932	4.932198
3.505327	228.896826	4.937203
3.426236	215.425252	4.942208
3.552313	237.131234	4.947213
3.219556	232.146691	4.952218
3.500924	234.567252	4.957222
3.294867	233.637808	4.962227
3.609736	224.315494	4.967232
3.457531	233.701028	4.972237
3.453451	229.993776	4.977242
3.466622	236.977402	4.982246
3.162721	232.111725	4.987251
3.647528	243.393802	4.992256
3.182344	241.954460	4.997261
3.499663	244.654129	5.002266
3.570932	237.609935	5.007270
3.217374	231.818723	5.012275
3.281748	234.494747	5.017280
3.223664	245.621439	5.022285
3.550627	239.957720	5.027290
3.684619	250.544951	5.032294
3.765917	254.072548	5.037299
4.017911	249.271630	5.042304
3.713921	243.725751	5.047309
3.537426	241.288878	5.052314
3.742835	241.411780	5.057318
3.620881	252.836387	5.062323
4.104293	249.562120	5.067328
3.736638	253.969988	5.072333
3.689431	249.984749	5.077338
3.948747	253.244007	5.082342
3.869893	257.932496	5.087347
3.664952	255.841767	5.092352
3.624361	255.544464	5.097357
3.936317	257.191435	5.102362
3.938407	262.348139	5.107366
3.788014	257.825402	5.112371
4.058427	256.454304	5.117376
4.265437	260.658239	5.122381
4.135319	251.358175	5.127386
3.851681	246.875301	5.132390
3.615449	239.895104	5.137395
3.889877	247.628745	5.142400
3.921016	262.800603	5.147405
4.280896	266.483873	5.152410
3.833260	258.859741	5.157414
3.830385	267.307561	5.162419
4.144859	267.131798	5.167424
4.348090	262.401792	5.172429
3.455443	265.126527	5.177434
3.787378	259.155135	5.182438
3.868453	260.344731	5.187443
3.869883	261.894823	5.192448
4.077325	264.377591	5.197453
4.126290	262.316682	5.202458
4.266154	266.730457	5.207462
4.305890	269.419838	5.212467
4.152732	260.575801	5.217472
4.180799	268.610646	5.222477
3.978729	270.844363	5.227482
4.294314	271.016442	5.232486
4.296339	269.234972	5.237491
4.297977	259.873131	5.242496
4.233949	269.181592	5.247501
3.887563	260.181167	5.252506
4.161300	263.514098	5.257510
4.028558	262.244132	5.262515
4.277818	265.697958	5.267520
4.427891	273.254939	5.272525
4.097245	266.830532	5.277530
4.142939	261.672789	5.282534
3.964738	263.288990	5.287539
3.966347	261.482277	5.292544
4.030408	261.358403	5.297549
4.504267	278.476240	5.302554
4.754848	285.928894	5.307558
4.287553	274.568235	5.312563
4.372912	265.474851	5.317568
4.229348	271.283972	5.322573
4.304807	272.781336	5.327578
4.529816	274.615940	5.332582
4.172049	287.093094	5.337587
4.787005	279.688447	5.342592
4.636095	288.194273	5.347597
4.752699	281.725095	5.352602
4.474649	265.209454	5.357606
4.284256	270.861395	5.362611
4.336078	263.943624	5.367616
4.389078	279.944147	5.372621
4.623224	273.785590	5.377626
4.871425	287.281453	5.382630
4.612091	284.095080	5.387635
4.464390	269.476268	5.392640
4.430332	270.250465	5.397645
4.291113	274.651020	5.402650
4.753940	276.565424	5.407654
4.383196	278.797095	5.412659
4.297548	273.941504	5.417664
4.679832	288.723005	5.422669
4.714786	286.196047	5.427674
5.129367	275.583076	5.432678
4.782233	286.280514	5.437683
4.573823	270.563886	5.442688
4.806528	276.497554	5.447693
4.846014	282.901265	5.452698
4.885563	281.680233	5.457702
4.512095	291.287129	5.462707
4.512247	287.468469	5.467712
4.753033	287.092277	5.472717
4.634690	287.439914	5.477722
4.913399	290.683484	5.482726
4.526308	286.197827	5.487731
4.558375	283.234719	5.492736
4.689847	278.943064	5.497741
4.681912	285.730697	5.502746
4.743191	281.317160	5.507750
4.534167	288.462171	5.512755
4.751195	296.192172	5.517760
4.500664	300.673450	5.522765
4.655592	310.301971	5.527770
5.172148	310.784252	5.532774
4.740376	317.692089	5.537779
5.261626	309.644042	5.542784
4.954539	318.215482	5.547789
4.975659	319.582157	5.552794
5.232598	309.392504	5.557798
4.888788	304.232500	5.562803
4.664570	306.637373	5.567808
5.105874	311.117825	5.572813
5.055503	309.388854	5.577818
5.147036	311.510135	5.582822
5.195215	319.589308	5.587827
5.082059	312.346186	5.592832
5.230012	320.074365	5.597837
5.036281	312.910307	5.602842
5.113769	306.921819	5.607846
5.053455	324.436610	5.612851
5.241171	304.902460	5.617856
5.035546	316.599649	5.622861
5.309703	318.667006	5.627866
4.727707	309.450368	5.632870
5.221284	313.909976	5.637875
4.887501	314.398937	5.642880
5.243516	314.678579	5.647885
5.025259	316.513036	5.652890
5.192966	317.075286	5.657894
5.169425	315.876792	5.662899
5.288338	309.075044	5.667904
5.155218	312.845059	5.672909
5.361677	311.727589	5.677914
5.152900	310.450550	5.682918
5.278840	317.653822	5.687923
5.612717	315.089517	5.692928
5.394788	310.697573	5.697933
5.033665	315.316407	5.702938
5.306625	315.495165	5.707942
5.076296	324.551297	5.712947
5.525418	316.182350	5.717952
5.147737	317.934217	5.722957
5.159272	323.478605	5.727962
5.573449	323.954781	5.732966
5.224903	327.622508	5.737971
5.256013	330.857424	5.742976
5.500230	339.045097	5.747981
5.392166	339.609426	5.752986
5.527114	339.290946	5.757990
5.580525	344.831943	5.762995
5.786223	341.809983	5.768000
5.657825	335.277932	5.773005
5.384838	350.399437	5.778010
5.622833	341.471927	5.783014
5.486965	349.023121	5.788019
5.534411	339.505363	5.793024
5.629728	341.341311	5.798029
5.614111	352.780960	5.803034
5.447286	352.848288	5.808038
5.529112	345.039921	5.813043
5.183534	345.986318	5.818048
5.454344	348.323126	5.823053
5.398965	338.403857	5.828058
5.528123	339.813718	5.833062
5.202049	332.809596	5.838067
5.237213	340.359299	5.843072
5.677538	352.154623	5.848077
5.473205	359.767170	5.853082
5.596901	359.463107	5.858086
5.550304	363.681491	5.863091
5.628299	368.674470	5.868096
5.852493	358.863248	5.873101
5.798639	359.814560	5.878106
6.013468	350.526838	5.883110
5.979520	360.289384	5.888115
5.696288	365.484495	5.893120
5.768185	365.539730	5.898125
5.962434	367.638596	5.903130
6.164404	368.005651	5.908134
5.907534	360.743897	5.913139
6.294051	356.997567	5.918144
6.426976	361.156184	5.923149
6.227372	342.388207	5.928154
6.356281	336.799781	5.933158
5.777690	344.970841	5.938163
5.903470	335.573691	5.943168
5.735976	334.837519	5.948173
5.849316	344.108737	5.953178
5.914504	339.375030	5.958182
5.927711	347.143315	5.963187
6.052168	339.749056	5.968192
5.899130	337.944418	5.973197
6.257517	342.909277	5.978202
6.050353	338.404906	5.983206
5.959000	342.386685	5.988211
6.245838	331.733584	5.993216
6.106774	343.961372	5.998221
5.992063	343.682008	6.003226
5.894696	334.417899	6.008230
6.152265	327.898144	6.013235
6.284766	329.048049	6.018240
6.115743	330.510956	6.023245
5.887503	334.318025	6.028250
6.054903	330.140953	6.033254
5.972963	329.862782	6.038259
6.269976	325.418627	6.043264
6.388673	336.612592	6.048269
6.251133	336.583581	6.053274
6.255866	330.242647	6.058278
5.875085	336.478103	6.063283
6.033299	335.466269	6.068288
5.896413	340.125907	6.073293
5.789842	344.986443	6.078298
6.208690	338.694519	6.083302
5.929017	342.338803	6.088307
6.340348	338.015941	6.093312
5.888816	340.959478	6.098317
5.726948	339.251138	6.103322
5.977329	337.253576	6.108326
6.123783	344.766862	6.113331
5.784234	346.291290	6.118336
5.694228	340.082257	6.123341
5.716997	353.360387	6.128346
6.202728	355.309176	6.133350
6.349688	370.595858	6.138355
5.898831	351.626789	6.143360
6.037505	354.139327	6.148365
6.246252	353.587817	6.153370
6.424816	358.998477	6.158374
6.026739	357.415730	6.163379
6.184934	352.800327	6.168384
6.217310	354.361397	6.173389
6.177817	344.797144	6.178394
6.263721	348.754316	6.183398
5.767092	340.150719	6.188403
6.001177	343.970775	6.193408
5.799950	344.084623	6.198413
6.096687	347.046965	6.203418
6.384262	346.055991	6.208422
6.037136	346.240155	6.213427
5.901133	343.350827	6.218432
5.934081	345.266152	6.223437
5.972484	345.266523	6.228442
5.938601	346.116627	6.233446
5.690234	346.054360	6.238451
5.850501	351.002805	6.243456
5.973875	361.196291	6.248461
5.618369	367.003848	6.253466
6.380981	354.526605	6.258470
6.388595	365.342516	6.263475
6.039188	359.591742	6.268480
6.029057	349.352160	6.273485
6.123553	363.324587	6.278490
6.534271	355.730444	6.283494
6.108322	355.272051	6.288499
5.865068	351.836369	6.293504
5.920609	350.546388	6.298509
6.019020	348.765627	6.303514
5.866510	349.545732	6.308518
6.148557	354.256795	6.313523
5.955955	363.895503	6.318528
6.145528	369.563873	6.323533
6.006778	361.672998	6.328538
6.269061	358.575729	6.333542
5.910238	350.453581	6.338547
5.786288	363.083980	6.343552
5.971637	362.634214	6.348557
6.127454	371.129987	6.353562
6.163335	371.247813	6.358566
6.121781	367.521094	6.363571
6.214926	367.917855	6.368576
6.379955	350.491140	6.373581
5.862428	350.698839	6.378586
6.116769	345.492561	6.383590
5.987993	348.069149	6.388595
5.808207	352.210321	6.393600
5.886124	343.437607	6.398605
6.228235	360.819778	6.403610
6.605360	363.437329	6.408614
6.250284	360.455771	6.413619
6.341374	342.259189	6.418624
6.236414	349.894127	6.423629
5.834606	346.135271	6.428634
6.340200	340.060712	6.433638
5.967070	342.773663	6.438643
6.113465	341.197360	6.443648
6.408679	339.066222	6.448653
6.248863	345.890329	6.453658
6.305501	341.550272	6.458662
5.940455	344.372690	6.463667
6.112377	354.928730	6.468672
6.090552	341.729666	6.473677
6.162725	345.945256	6.478682
6.206901	335.472544	6.483686
5.869323	348.259793	6.488691
5.899185	345.423572	6.493696
6.141563	342.724900	6.498701
5.812655	341.599560	6.503706
6.251234	345.324300	6.508710
6.227251	348.865248	6.513715
5.948462	349.456327	6.518720
6.014870	352.565491	6.523725
5.793145	355.764094	6.528730
6.481633	351.454752	6.533734
5.832806	353.160518	6.538739
5.848236	353.699171	6.543744
6.176230	344.267169	6.548749
6.118662	350.078661	6.553754
6.523818	343.754078	6.558758
6.477497	351.275424	6.563763
6.095001	345.732322	6.568768
5.962817	330.921200	6.573773
5.560231	334.287344	6.578778
5.889278	337.314225	6.583782
5.671545	350.949579	6.588787
5.716513	347.886361	6.593792
5.940291	341.691440	6.598797
5.714122	351.851100	6.603802
6.051995	342.366931	6.608806
6.187772	353.029874	6.613811
5.955387	358.270800	6.618816
6.133373	345.989568	6.623821
5.735470	347.700313	6.628826
6.256476	346.356384	6.633830
5.933871	355.544051	6.638835
6.091926	351.637361	6.643840
5.877801	352.487232	6.648845
5.828720	351.390815	6.653850
5.945492	337.091183	6.658854
5.963266	345.580098	6.663859
6.087363	339.334355	6.668864
6.009250	338.255143	6.673869
5.841051	350.066715	6.678874
5.952520	351.941264	6.683878
5.942571	356.115938	6.688883
5.804787	356.147078	6.693888
6.165646	367.945372	6.698893
6.227581	380.641573	6.703898
6.307967	355.581195	6.708902
6.130051	355.552182	6.713907
5.587029	349.132546	6.718912
6.245361	358.011494	6.723917
6.046980	363.572965	6.728922
5.970420	364.527835	6.733926
6.065873	366.306816	6.738931
5.990708	367.043165	6.743936
6.193347	367.356330	6.748941
5.920020	365.165569	6.753946
5.993675	366.201309	6.758950
5.990067	368.831056	6.763955
5.920154	353.067345	6.768960
6.222652	360.999121	6.773965
6.026716	364.883394	6.778970
5.969237	359.377950	6.783974
6.028534	363.643018	6.788979
5.834768	365.328108	6.793984
6.624350	364.454634	6.798989
6.280109	376.644988	6.803994
6.403322	364.242608	6.808998
5.961834	356.737696	6.814003
5.674610	344.212974	6.819008
6.078176	347.278802	6.824013
5.878129	359.598414	6.829018
5.886161	359.511793	6.834022
5.797479	361.151943	6.839027
6.109840	364.779403	6.844032
6.182579	363.578476	6.849037
5.937690	359.984859	6.854042
6.277153	361.029571	6.859046
6.174695	371.372343	6.864051
5.925767	366.219602	6.869056
6.307137	362.486732	6.874061
6.143601	358.972119	6.879066
6.111382	359.923204	6.884070
6.007473	353.890354	6.889075
5.974913	356.163962	6.894080
6.359582	353.329097	6.899085
6.041413	346.576835	6.904090
6.027735	348.784207	6.909094
5.900516	343.321333	6.914099
5.723373	345.816913	6.919104
6.490989	350.107042	6.924109
5.920536	348.855029	6.929114
5.908825	348.413992	6.934118
6.178218	359.369221	6.939123
5.990292	357.728237	6.944128
6.254181	352.703962	6.949133
6.040921	358.036806	6.954138
6.124857	339.581915	6.959142
6.289546	345.969196	6.964147
5.936360	347.135088	6.969152
6.238628	337.105998	6.974157
5.879811	342.679945	6.979162
6.258849	346.395032	6.984166
5.877474	345.037463	6.989171
5.722201	342.562449	6.994176
6.256156	346.806929	6.999181
5.849722	347.373714	7.004186
6.123999	349.846022	7.009190
6.016959	350.717080	7.014195
5.905403	348.412389	7.019200
6.083740	348.707215	7.024205
6.099166	364.248622	7.029210
6.369209	353.984123	7.034214
6.126383	347.764229	7.039219
5.890640	348.797823	7.044224
5.908946	338.231085	7.049229
5.752140	345.247712	7.054234
6.316736	353.967335	7.059238
6.045741	350.536000	7.064243
6.237280	352.701729	7.069248
6.143338	343.655380	7.074253
6.105033	348.853240	7.079258
5.972628	341.980123	7.084262
5.762934	348.533632	7.089267
5.985183	354.820147	7.094272
6.398893	360.304697	7.099277
5.853500	355.198409	7.104282
5.862178	355.532473	7.109286
5.965358	358.993386	7.114291
5.779468	357.564059	7.119296
6.243153	361.838534	7.124301
6.138167	369.527270	7.129306
6.233834	363.380887	7.134310
6.173694	363.839631	7.139315
6.031756	354.614133	7.144320
6.214741	349.254516	7.149325
5.885729	351.337287	7.154330
6.067605	353.121709	7.159334
5.852411	345.401009	7.164339
5.857665	355.581360	7.169344
6.195099	360.470411	7.174349
6.067442	367.662817	7.179354
6.351295	363.192241	7.184358
6.153244	360.809349	7.189363
5.839916	356.584204	7.194368
6.314235	352.444461	7.199373
5.741580	348.528872	7.204378
6.109813	359.930530	7.209382
6.356605	372.822392	7.214387
5.912096	365.147104	7.219392
6.001985	360.061502	7.224397
6.011701	361.104095	7.229402
5.883242	362.832737	7.234406
5.994687	364.542773	7.239411
5.970471	376.259035	7.244416
6.373908	378.942068	7.249421
6.048917	374.481461	7.254426
5.590909	366.175525	7.259430
5.798011	363.343170	7.264435
5.917865	369.440086	7.269440
5.516870	373.479878	7.274445
5.784981	373.077256	7.279450
6.379680	372.139402	7.284454
6.754823	384.289815	7.289459
6.675204	373.798511	7.294464
6.752882	367.218341	7.299469
6.197260	364.363118	7.304474
6.368751	352.434081	7.309478
6.131228	357.884623	7.314483
6.041334	364.090332	7.319488
6.119035	350.394770	7.324493
6.045042	359.711167	7.329498
5.808853	352.212055	7.334502
5.979151	345.025750	7.339507
5.750512	353.056560	7.344512
6.239065	351.075465	7.349517
5.884295	357.765605	7.354522
6.310143	355.465298	7.359526
6.114648	364.892485	7.364531
6.171443	364.950086	7.369536
6.069910	350.096180	7.374541
5.794199	365.952128	7.379546
6.087925	355.443468	7.384550
5.857759	359.889932	7.389555
5.668909	348.960170	7.394560
5.759291	351.454964	7.399565
5.586825	364.516915	7.404570
6.356511	365.092417	7.409574
6.369275	374.176926	7.414579
5.973265	365.247499	7.419584
6.238064	355.189468	7.424589
5.738447	358.561328	7.429594
6.424102	356.489238	7.434598
6.327045	351.315869	7.439603
5.837501	356.388275	7.444608
6.063348	345.412522	7.449613
5.778708	351.923991	7.454618
6.022378	356.707507	7.459622
6.019299	354.638923	7.464627
6.075282	367.244297	7.469632
6.194131	353.504320	7.474637
6.209805	365.334549	7.479642
6.144355	354.780924	7.484646
6.305507	356.245886	7.489651
6.029873	349.243345	7.494656
6.052684	353.226222	7.499661
6.141880	357.666941	7.504666
6.353972	352.995636	7.509670
6.269861	349.990608	7.514675
5.945707	353.923442	7.519680
6.064108	354.999627	7.524685
5.791506	363.995962	7.529690
6.001536	363.235440	7.534694
5.888381	356.416250	7.539699
5.835741	357.940019	7.544704
6.238979	359.091800	7.549709
6.145253	363.751010	7.554714
6.084615	358.138492	7.559718
6.028257	349.320373	7.564723
5.934459	349.411061	7.569728
6.106525	346.827810	7.574733
6.119718	361.050259	7.579738
5.944392	348.558623	7.584742
5.959574	363.087651	7.589747
5.928075	361.741702	7.594752
6.342083	353.561740	7.599757
5.884096	356.351265	7.604762
6.019704	350.429586	7.609766
6.177576	358.668763	7.614771
5.993138	360.333408	7.619776
6.402955	344.687532	7.624781
5.898610	355.156538	7.629786
6.295463	357.084451	7.634790
6.433003	356.082183	7.639795
5.996852	360.178101	7.644800
6.047831	350.878085	7.649805
6.038196	366.205118	7.654810
5.915779	364.202688	7.659814
5.831009	352.234707	7.664819
5.697192	356.112409	7.669824
6.348040	360.895406	7.674829
6.084040	353.327884	7.679834
5.923908	357.358408	7.684838
5.837621	353.350794	7.689843
5.976552	353.208862	7.694848
5.824447	345.253647	7.699853
5.907018	348.379261	7.704858
5.912011	346.872569	7.709862
6.171635	355.946865	7.714867
5.778628	364.572918	7.719872
6.342722	369.369510	7.724877
5.973143	365.624583	7.729882
6.029295	355.830200	7.734886
6.281911	351.718867	7.739891
5.853333	360.802915	7.744896
6.201279	355.161183	7.749901
6.215556	361.005714	7.754906
5.923735	356.176076	7.759910
6.352444	362.718151	7.764915
6.073051	356.807709	7.769920
6.174969	356.579826	7.774925
5.923212	357.084411	7.779930
6.025794	360.026554	7.784934
5.779123	356.572425	7.789939
5.600166	366.980964	7.794944
6.316289	364.802857	7.799949
6.175425	376.347568	7.804954
6.327351	365.206212	7.809958
6.211912	356.103113	7.814963
6.246824	362.014015	7.819968
6.641758	348.933149	7.824973
6.157626	351.103500	7.829978
5.970459	344.732516	7.834982
6.307447	352.225443	7.839987
5.957999	352.555506	7.844992
6.282713	349.897717	7.849997
6.261515	362.220947	7.855002
6.319769	359.146154	7.860006
6.451699	359.296388	7.865011
6.204672	350.982714	7.870016
6.009659	338.671342	7.875021
5.969170	335.169093	7.880026
5.667252	336.611693	7.885030
6.318523	354.043496	7.890035
6.242342	357.883694	7.895040
6.054402	343.631799	7.900045
5.917129	338.357166	7.905050
6.102277	353.090513	7.910054
6.397061	335.111963	7.915059
6.070390	341.079512	7.920064
6.245017	336.584926	7.925069
5.643832	333.613459	7.930074
5.822842	340.058606	7.935078
5.943328	348.531429	7.940083
5.904372	352.460708	7.945088
6.217256	348.830321	7.950093
6.123773	354.717045	7.955098
6.237622	357.401155	7.960102
6.190828	342.949973	7.965107
5.672289	346.252027	7.970112
6.236363	337.380998	7.975117
5.938760	352.683535	7.980122
5.803211	347.663638	7.985139
5.775782	363.342516	7.990157
6.174602	363.153860	7.995174
6.292934	354.365599	8.000192
6.282937	360.602953	8.005210
6.255185	355.990525	8.010227
5.879066	352.694974	8.015245
6.024321	357.573127	8.020262
6.325411	352.019260	8.025280
6.100140	348.482329	8.030298
5.921510	354.212783	8.035315
6.110585	356.054568	8.040333
5.843999	364.645277	8.045350
5.962894	363.702079	8.050368
5.860004	366.009323	8.055386
6.077204	361.806629	8.060403
6.105306	355.298322	8.065421
5.974813	359.613779	8.070438
6.463590	358.334924	8.075456
6.334009	363.174091	8.080474
6.354789	362.337782	8.085491
6.264179	359.098479	8.090509
5.853255	363.883899	8.095526
6.140266	364.697350	8.100544
6.280983	364.549133	8.105562
6.301589	359.361096	8.110579
6.448083	354.497311	8.115597
5.900254	360.695859	8.120614
6.094746	355.761438	8.125632
6.104213	362.380742	8.130650
5.772817	368.558004	8.135667
6.223870	357.268762	8.140685
6.187685	363.324032	8.145702
6.027929	372.327186	8.150720
6.046556	366.609293	8.155738
6.162992	359.904112	8.160755
6.206641	360.970282	8.165773
6.179607	360.690562	8.170790
6.056616	358.974240	8.175808
5.963150	373.410648	8.180826
5.888093	367.694810	8.185843
6.416590	371.364233	8.190861
6.248707	380.169854	8.195878
6.239679	364.386343	8.200896
6.521976	369.287208	8.205914
6.415799	371.970500	8.210931
6.377173	371.585301	8.215949
6.298812	362.221954	8.220966
6.219650	354.887873	8.225984
6.131826	369.364418	8.231002
5.945475	367.676956	8.236019
6.337248	373.892389	8.241037
6.339395	382.548297	8.246054
6.617047	376.228095	8.251072
6.412266	385.336139	8.256090
6.326730	368.529530	8.261107
6.467894	366.421533	8.266125
6.123305	362.878048	8.271142
6.449640	364.947630	8.276160
6.655473	365.959988	8.281178
6.238590	369.843804	8.286195
6.406368	354.458625	8.291213
6.169915	367.730876	8.296230
6.335231	371.583432	8.301248
6.866973	374.321406	8.306266
6.270027	366.159595	8.311283
6.373007	367.992781	8.316301
6.285191	364.506891	8.321318
6.651560	369.189461	8.326336
6.551583	371.650880	8.331354
6.149100	365.749664	8.336371
6.387761	363.490695	8.341389
6.295857	361.558067	8.346406
6.735474	367.586125	8.351424
6.530492	364.490970	8.356442
6.149759	367.431869	8.361459
6.747408	356.927526	8.366477
6.183853	371.289267	8.371494
6.072406	360.157582	8.376512
6.628748	362.831740	8.381530
6.471660	368.849152	8.386547
6.554109	373.500470	8.391565
6.469876	383.359624	8.396582
6.354139	381.875687	8.401600
6.284820	380.065749	8.406618
6.279022	390.723642	8.411635
6.520630	375.948556	8.416653
6.403923	374.054527	8.421670
6.453648	380.276218	8.426688
6.476666	381.585459	8.431706
6.356031	380.925937	8.436723
6.585628	388.889817	8.441741
6.565242	387.917949	8.446758
6.771960	381.179679	8.451776
6.812002	379.848057	8.456794
6.564417	384.402768	8.461811
6.721718	379.291135	8.466829
6.686180	389.180532	8.471846
6.666469	384.721468	8.476864
6.641778	380.181136	8.481882
6.467106	383.335899	8.486899
6.807248	382.575781	8.491917
6.752448	379.286683	8.496934
6.570375	369.254787	8.501952
6.212134	368.660896	8.506970
6.044151	382.367389	8.511987
6.512353	377.371142	8.517005
6.239010	379.392677	8.522022
6.373993	375.332246	8.527040
6.410858	378.857799	8.532058
6.777613	385.758795	8.537075
6.832896	377.232861	8.542093
6.616987	382.315928	8.547110
6.693290	381.101697	8.552128
6.792269	384.099978	8.557146
6.820498	386.951557	8.562163
6.830037	384.242501	8.567181
6.941837	385.313774	8.572199
6.741860	378.402546	8.577216
6.750902	381.171926	8.582234
6.340463	382.637442	8.587251
6.758766	380.659586	8.592269
6.791323	392.374953	8.597287
6.687050	386.124056	8.602304
6.667499	380.702468	8.607322
6.520186	385.755854	8.612339
6.737183	386.233145	8.617357
6.698156	389.000590	8.622375
6.521623	389.040933	8.627392
6.510416	385.946971	8.632410
6.696962	387.079114	8.637427
6.953208	374.861039	8.642445
6.275353	386.230129	8.647463
6.685080	379.400094	8.652480
6.874637	367.886735	8.657498
6.738326	378.495643	8.662515
6.795580	379.913126	8.667533
6.533868	381.317469	8.672551
6.625184	376.995643	8.677568
6.710271	380.860771	8.682586
6.852856	395.992343	8.687603
7.115124	396.942213	8.692621
6.775828	390.500925	8.697639
6.507047	378.911052	8.702656
6.825816	381.158543	8.707674
6.910204	391.761282	8.712691
6.984500	389.218800	8.717709
6.635876	397.803444	8.722727
6.869498	403.914281	8.727744
6.970717	396.880118	8.732762
6.676294	405.165945	8.737779
7.359070	397.892342	8.742797
7.298729	397.993373	8.747815
6.877664	390.368871	8.752832
6.951088	371.839567	8.757850
6.621227	387.550073	8.762867
6.810186	380.009873	8.767885
6.603077	386.293898	8.772903
6.361115	392.637033	8.777920
6.967564	400.854292	8.782938
7.017905	399.647283	8.787955
7.118486	409.483806	8.792973
6.987365	408.216869	8.797991
6.579669	415.946104	8.803008
7.176666	402.475439	8.808026
6.640136	414.059084	8.813043
6.843720	406.538672	8.818061
6.945844	408.375152	8.823079
6.592368	409.358383	8.828096
7.057795	410.342693	8.833114
7.060258	408.111259	8.838131
6.827969	411.770505	8.843149
7.071846	408.055916	8.848167
6.994283	414.827728	8.853184
7.108969	399.659107	8.858202
6.704060	406.939787	8.863219
6.974556	406.174801	8.868237
7.320019	400.326795	8.873255
6.912350	406.717989	8.878272
7.132317	408.734816	8.883290
6.891105	404.174755	8.888307
6.856134	405.240624	8.893325
7.321002	406.916129	8.898343
6.893045	405.386437	8.903360
7.124597	409.869239	8.908378
7.042342	412.993748	8.913395
7.046292	411.418475	8.918413
6.921810	403.709629	8.923431
7.023353	402.223205	8.928448
7.120155	400.175802	8.933466
7.148265	397.924571	8.938483
7.046367	401.023755	8.943501
7.219915	397.386457	8.948519
6.831025	407.239711	8.953536
7.050395	394.853835	8.958554
6.627645	404.914359	8.963571
6.892435	417.697866	8.968589
7.016042	422.074510	8.973607
7.054718	428.174875	8.978624
7.025782	431.698125	8.983642
7.119655	436.148858	8.988659
7.224969	433.528927	8.993677
7.400356	429.632564	8.998695
6.955145	445.089799	9.003712
7.317281	425.126675	9.008730
7.426852	432.793806	9.013747
7.550336	427.589630	9.018765
7.362911	437.875229	9.023783
7.183049	428.335250	9.028800
7.382008	421.733878	9.033818
7.104984	415.945530	9.038835
7.091853	411.785224	9.043853
7.405376	423.245155	9.048871
7.156579	424.240387	9.053888
7.408769	423.768598	9.058906
7.121462	416.113660	9.063923
7.311661	421.477085	9.068941
7.270029	417.277063	9.073959
7.218468	411.355562	9.078976
7.637868	411.460320	9.083994
6.840032	416.240106	9.089011
7.146320	420.802717	9.094029
7.435068	424.342461	9.099047
7.208346	434.599502	9.104064
7.487403	431.027717	9.109082
7.239133	437.807349	9.114099
7.527545	431.548557	9.119117
7.654762	431.269914	9.124135
7.431184	423.702816	9.129152
7.423076	411.207406	9.134170
7.334315	416.447282	9.139187
6.993614	409.611739	9.144205
7.352148	412.020259	9.149223
7.416717	426.154242	9.154240
7.674728	426.432608	9.159258
7.097092	414.685980	9.164275
7.168776	420.358301	9.169293
7.475218	419.060674	9.174311
7.232782	423.999589	9.179328
7.542093	431.704850	9.184346
7.400864	437.407381	9.189363
7.368771	431.220897	9.194381
7.620246	430.682948	9.199399
7.507100	440.253179	9.204416
7.598293	428.701545	9.209434
7.236079	428.357578	9.214451
7.372479	434.922307	9.219469
7.527378	436.324495	9.224487
7.694559	432.176958	9.229504
7.613152	419.929706	9.234522
7.303708	414.888038	9.239539
7.182119	414.638911	9.244557
7.530679	428.450695	9.249575
7.570282	434.191163	9.254592
7.381819	430.102504	9.259610
7.438211	429.399465	9.264627
7.443301	430.033033	9.269645
7.737572	433.635028	9.274663
7.252452	428.709241	9.279680
7.543640	426.085435	9.284698
7.719759	435.253742	9.289715
7.449739	432.547455	9.294733
7.788211	428.294186	9.299751
7.671733	427.223765	9.304768
7.609914	433.485042	9.309786
7.842436	427.058287	9.314803
7.279890	421.021189	9.319821
7.647891	419.451989	9.324839
7.736635	429.675379	9.329856
7.733033	429.319404	9.334874
7.953138	431.061663	9.339891
7.471320	427.006345	9.344909
7.427912	395.806077	9.349927
7.402318	415.505125	9.354944
7.793014	423.667838	9.359962
8.010120	426.066960	9.364979
7.503510	423.097948	9.369997
7.497505	413.019507	9.375015
7.503789	418.954534	9.380032
7.808756	413.772419	9.385050
7.685556	435.758917	9.390067
7.781717	440.550112	9.395085
7.996216	426.369357	9.400103
7.655212	424.198047	9.405120
7.252100	402.243655	9.410138
7.672871	412.427636	9.415155
7.720216	429.177275	9.420173
7.795555	417.713337	9.425191
7.398453	433.305033	9.430208
7.374692	429.042249	9.435226
7.818980	425.946339	9.440243
7.600161	431.720984	9.445261
7.533523	421.557365	9.450279
7.766005	435.933286	9.455296
7.562956	433.027161	9.460314
7.923949	426.674950	9.465331
7.387748	425.417831	9.470349
7.533074	432.293580	9.475367
7.606988	426.456554	9.480384
7.651229	430.826701	9.485402
7.546212	429.694524	9.490419
7.211135	442.161790	9.495437
7.613950	443.389437	9.500455
7.877487	454.409104	9.505472
7.868351	456.146258	9.510490
8.093199	444.983920	9.515507
7.962673	456.627054	9.520525
8.106834	458.567403	9.525543
7.751029	457.581814	9.530560
7.894947	454.880094	9.535578
7.807590	453.678878	9.540595
7.900690	450.278233	9.545613
8.236578	452.261124	9.550631
8.098645	449.660368	9.555648
7.856797	434.194136	9.560666
7.940842	433.306887	9.565683
7.796710	425.159307	9.570701
7.842854	435.124291	9.575719
7.919232	439.315839	9.580736
8.170820	455.430755	9.585754
8.042601	431.053822	9.590771
7.653779	431.367263	9.595789
8.186863	432.495605	9.600807
7.687937	440.863983	9.605824
8.046243	453.986308	9.610842
8.258709	453.060002	9.615859
7.849882	438.689727	9.620877
8.461140	440.929268	9.625895
7.763313	436.683734	9.630912
7.745817	423.094742	9.635930
8.129576	433.382362	9.640947
7.971336	453.663958	9.645965
8.253601	454.146803	9.650983
7.895407	443.410326	9.656000
7.559501	453.047024	9.661018
7.991406	443.098765	9.666035
7.627604	461.954623	9.671053
7.450144	456.368409	9.676071
7.909968	451.471283	9.681088
7.674260	464.317463	9.686106
8.020906	455.253544	9.691123
7.629408	460.704965	9.696141
8.182271	470.773610	9.701159
8.253912	469.269775	9.706176
8.121331	473.699194	9.711194
8.447384	462.877588	9.716211
8.107064	473.651059	9.721229
7.982561	462.350945	9.726247
8.212116	458.439777	9.731264
7.938213	464.567040	9.736282
8.061987	453.228032	9.741299
8.151705	464.710433	9.746317
8.267854	474.389920	9.751335
7.955707	472.400272	9.756352
8.359861	481.637014	9.761370
8.446537	483.179281	9.766387
8.110686	481.808718	9.771405
8.170529	464.161901	9.776423
8.289862	470.252799	9.781440
8.187114	461.376051	9.786458
8.154354	458.872423	9.791475
8.184063	478.635458	9.796493
8.520606	470.122215	9.801511
8.463138	469.178242	9.806528
8.152969	466.437216	9.811546
8.347856	462.212748	9.816563
8.229575	463.465239	9.821581
8.149290	461.366682	9.826599
8.520974	454.356389	9.831616
8.111626	459.614951	9.836634
8.000073	454.248780	9.841651
8.323111	467.190451	9.846669
8.392812	468.284104	9.851687
8.510084	470.806170	9.856704
8.381308	461.428580	9.861722
8.067742	453.944995	9.866739
8.679011	468.769670	9.871757
8.394918	466.431650	9.876775
8.216588	454.467800	9.881792
8.089606	456.030917	9.886810
8.381628	459.645893	9.891827
8.500600	482.910453	9.896845
8.614523	475.037993	9.901863
8.530936	465.227294	9.906880
8.420396	462.107858	9.911898
8.374812	449.359520	9.916915
8.404659	457.948009	9.921933
8.447660	462.021717	9.926951
8.255462	459.846022	9.931968
8.322884	470.413597	9.936986
8.917691	461.332883	9.942003
8.524241	469.189294	9.947021
8.323731	453.726036	9.952039
8.516644	457.296581	9.957056
8.469149	456.275308	9.962074
8.079502	455.459120	9.967091
8.204325	471.079525	9.972109
8.341472	479.143136	9.977127
8.772121	476.626857	9.982144
8.510284	485.753358	9.987162
8.411717	480.265227	9.992179
8.280031	486.322878	9.997197
8.349252	480.685382	10.002215
8.313635	482.401442	10.007232
8.140156	484.448366	10.012250
8.618961	478.554196	10.017267
8.258672	485.894188	10.022285
8.521326	487.569826	10.027303
8.619426	489.552109	10.032320
8.508882	479.603617	10.037338
8.739890	487.314860	10.042355
8.508188	489.156315	10.047373
8.348089	483.671512	10.052391
8.555019	482.067585	10.057408
8.481006	496.267518	10.062426
8.490497	495.574981	10.067443
8.657141	507.244169	10.072461
8.802296	512.538940	10.077479
8.811308	495.499651	10.082496
8.421093	501.159164	10.087514
8.829362	493.622424	10.092531
8.396696	499.793508	10.097549
8.949563	506.652768	10.102567
8.896034	491.207473	10.107584
8.705077	495.308378	10.112602
8.293623	483.838619	10.117619
8.644954	492.326262	10.122637
8.442377	501.935784	10.127655
8.821208	509.475555	10.132672
8.533181	503.897182	10.137690
9.068613	500.761733	10.142707
8.875229	516.125925	10.147725
8.718985	515.535093	10.152743
8.840734	503.975466	10.157760
8.907072	507.950856	10.162778
8.829841	510.853692	10.167795
8.942628	506.534782	10.172813
8.916336	508.615451	10.177831
8.531870	488.889152	10.182848
8.676941	502.256358	10.187866
8.963107	503.912535	10.192883
8.771999	499.770627	10.197901
9.189603	510.311760	10.202919
9.232135	499.512464	10.207936
8.957516	501.515277	10.212954
8.481232	486.388684	10.217971
8.881502	485.448730	10.222989
8.738356	502.032627	10.228007
8.964303	497.008034	10.233024
8.872478	497.476910	10.238042
8.907103	499.289262	10.243059
8.897773	508.464573	10.248077
8.672216	514.252923	10.253095
9.071000	506.029708	10.258112
8.509186	508.137480	10.263130
8.591872	504.413413	10.268147
8.863395	509.290758	10.273165
8.886758	515.892163	10.278183
8.968969	516.750332	10.283200
9.080394	499.773887	10.288218
8.865489	508.186156	10.293235
8.912210	503.751367	10.298253
8.795563	515.196708	10.303271
8.918176	512.163806	10.308288
8.798582	520.955618	10.313306
8.934446	511.290388	10.318323
9.089674	502.420536	10.323341
9.027527	513.611187	10.328359
9.322996	507.559544	10.333376
8.786654	510.849889	10.338394
9.029543	499.287065	10.343411
8.971326	509.028605	10.348429
9.032124	511.477475	10.353447
9.116873	509.823263	10.358464
9.078300	512.537008	10.363482
9.268088	511.033593	10.368499
9.294988	515.905087	10.373517
8.892899	511.127212	10.378535
9.171208	509.054513	10.383552
8.760502	518.308496	10.388570
8.919382	522.644924	10.393587
9.511614	527.478338	10.398605
9.242635	526.318197	10.403623
9.015434	524.069083	10.408640
9.073581	523.703432	10.413658
9.261837	535.946757	10.418675
9.371347	532.414139	10.423693
9.299316	522.992912	10.428711
9.082909	504.284822	10.433728
9.110623	518.636090	10.438746
9.297339	520.929535	10.443763
9.462919	526.394678	10.448781
9.285196	517.914652	10.453799
9.265182	520.470858	10.458816
9.010108	522.050895	10.463834
9.190249	525.528782	10.468851
9.179448	529.528885	10.473869
9.420262	530.876595	10.478887
9.592523	534.731254	10.483904
9.688253	520.089357	10.488922
9.147992	511.988024	10.493939
9.484364	513.008340	10.498957
9.208904	511.776633	10.503975
9.175965	507.922361	10.508992
9.323625	507.353339	10.514010
9.216145	509.222670	10.519027
9.439708	509.818854	10.524045
9.600708	518.891745	10.529063
9.460093	504.135416	10.534080
9.277661	501.866668	10.539098
9.155402	513.211902	10.544115
9.634246	512.584679	10.549133
9.375503	504.625431	10.554151
9.537576	512.192853	10.559168
9.485986	514.018714	10.564186
9.539839	505.148966	10.569203
9.435916	501.826517	10.574221
8.842635	506.829892	10.579239
9.908625	512.747236	10.584256
9.588417	503.800399	10.589274
9.488204	507.372700	10.594291
9.357581	501.046997	10.599309
9.456163	510.183311	10.604327
9.274047	516.043749	10.609344
9.495685	522.200686	10.614362
9.503218	529.271628	10.619379
9.766636	528.141678	10.624397
9.874197	533.420256	10.629415
9.722144	520.174160	10.634432
9.547695	508.137084	10.639450
9.191980	508.246526	10.644467
9.654288	506.081883	10.649485
9.485545	514.679425	10.654503
9.430539	521.416185	10.659520
9.853365	524.079730	10.664538
9.531489	523.382307	10.669555
9.533703	514.170355	10.674573
9.682602	522.661328	10.679591
9.623002	524.911317	10.684608
9.907189	527.325190	10.689626
9.360336	528.774220	10.694643
9.795859	523.562151	10.699661
9.820654	532.429174	10.704679
9.818863	527.168859	10.709696
9.682513	512.427633	10.714714
9.673856	514.275170	10.719731
9.353613	515.013362	10.724749
9.727212	523.620605	10.729767
9.560192	535.821767	10.734784
9.637400	529.166849	10.739802
9.818217	527.876274	10.744819
9.804859	525.451646	10.749837
9.548653	540.405986	10.754855
9.650120	537.789798	10.759872
9.950217	533.807602	10.764890
9.759665	528.977643	10.769907
9.707725	536.417664	10.774925
9.561015	537.270677	10.779943
9.686050	531.103720	10.784960
9.730436	534.116891	10.789978
9.579273	538.318867	10.794995
9.645422	536.263628	10.800013
9.452087	542.555017	10.805031
9.597818	528.539588	10.810048
9.807295	529.321014	10.815066
9.789285	531.286781	10.820083
9.294928	533.289313	10.825101
9.629577	547.368453	10.830119
9.563852	559.519046	10.835136
9.849223	557.640894	10.840154
9.718816	554.515086	10.845171
10.009411	560.348811	10.850189
9.720202	569.094639	10.855207
9.637539	567.690711	10.860224
10.218920	563.251031	10.865242
9.621419	570.707117	10.870259
9.693792	558.341004	10.875277
9.548998	561.983416	10.880295
9.456589	557.425248	10.885312
10.041704	576.280870	10.890330
10.144218	588.023274	10.895347
10.518199	589.460576	10.900365
10.254650	578.078034	10.905383
10.281523	562.064664	10.910400
10.248082	561.776478	10.915418
9.685564	561.438645	10.920435
10.444032	552.142897	10.925453
10.170307	557.907250	10.930471
10.395819	559.522444	10.935488
10.352982	552.176278	10.940506
10.208321	568.583752	10.945523
10.395848	556.650872	10.950541
10.010547	561.662701	10.955559
10.089565	559.507614	10.960576
10.163118	555.677672	10.965594
10.359611	559.781001	10.970611
10.536631	546.644271	10.975629
10.439786	559.288883	10.980647
10.064605	549.829934	10.985664
10.405947	543.048421	10.990682
9.909339	547.626411	10.995699
10.040639	544.525872	11.000717
10.316631	561.407067	11.005735
9.859969	564.287311	11.010752
10.146394	557.738456	11.015770
10.069333	565.640011	11.020787
10.112836	554.395566	11.025805
10.088791	562.023728	11.030823
10.262495	558.080265	11.035840
10.502170	556.152468	11.040858
10.192606	561.168209	11.045875
10.276988	553.199359	11.050893
10.434413	556.816509	11.055911
10.298894	561.991172	11.060928
10.676150	555.383906	11.065946
10.260982	567.570320	11.070963
10.067949	568.556823	11.075981
10.328436	560.686608	11.080999
10.097740	561.151999	11.086016
10.535988	553.698898	11.091034
10.263019	560.087976	11.096051
10.470237	559.408637	11.101069
10.410880	554.763240	11.106087
10.226412	563.615730	11.111104
10.294346	556.921230	11.116122
10.005589	564.335251	11.121139
10.233640	552.326598	11.126157
10.443097	548.664709	11.131175
10.113352	551.954251	11.136192
10.320801	548.674524	11.141210
10.523324	553.111419	11.146227
10.545316	565.232493	11.151245
10.357906	558.817838	11.156263
9.636686	562.888233	11.161280
10.233996	567.184381	11.166298
10.392067	574.424257	11.171315
10.329316	583.402851	11.176333
10.732521	584.933402	11.181351
10.383268	583.012670	11.186368
10.792282	574.418596	11.191386
10.827679	585.369949	11.196403
10.692136	584.823208	11.201421
10.930495	581.683798	11.206439
10.734767	589.127435	11.211456
10.643531	580.725345	11.216474
10.752077	581.686688	11.221491
10.599877	584.544478	11.226509
10.694908	581.982941	11.231527
10.262608	586.986362	11.236544
10.831983	583.059793	11.241562
10.636223	588.859278	11.246579
10.481911	585.042940	11.251597
10.767660	583.265711	11.256615
10.544090	584.862907	11.261632
10.930463	588.223288	11.266650
10.562979	586.015081	11.271667
10.407385	588.608319	11.276685
10.833411	591.713182	11.281703
10.426052	589.564870	11.286720
10.780564	584.860932	11.291738
10.744712	596.445142	11.296755
10.824472	588.748397	11.301773
10.924242	585.255164	11.306791
10.547922	591.105030	11.311808
10.783205	583.219819	11.316826
10.712256	590.435625	11.321843
11.118474	588.718414	11.326861
10.921418	583.435028	11.331879
10.510817	585.847316	11.336896
11.009542	592.894972	11.341914
11.041661	594.805555	11.346931
10.890678	588.176900	11.351949
10.923314	589.692930	11.356967
10.717440	594.140174	11.361984
11.135977	591.073517	11.367002
10.986115	602.928057	11.372019
10.897682	590.202111	11.377037
11.271212	589.979547	11.382055
10.830972	594.409863	11.387072
10.857480	588.526564	11.392090
11.024083	592.164374	11.397107
10.788900	590.920039	11.402125
10.876889	588.343826	11.407143
11.037874	588.687888	11.412160
11.035909	586.766391	11.417178
10.753049	595.416564	11.422195
11.073390	592.822879	11.427213
11.150885	585.382108	11.432231
10.600315	589.987499	11.437248
10.839340	586.582899	11.442266
10.911637	583.554713	11.447283
10.929331	594.660323	11.452301
10.931195	583.157298	11.457319
10.616773	592.759147	11.462336
10.712645	588.944635	11.467354
10.677805	601.068327	11.472371
10.636183	602.400334	11.477389
11.264679	607.572067	11.482407
11.032935	608.422628	11.487424
10.832909	623.178887	11.492442
10.994975	611.748573	11.497459
10.938964	620.066572	11.502477
11.166112	619.478782	11.507495
10.713792	622.004908	11.512512
11.052746	609.959905	11.517530
10.996627	609.735231	11.522547
11.113759	608.479874	11.527565
11.381343	620.174346	11.532583
11.323693	626.214133	11.537600
11.205240	614.562684	11.542618
11.251199	612.507444	11.547635
11.184360	615.134116	11.552653
11.562851	616.741125	11.557671
11.284337	618.836079	11.562688
11.141624	615.535465	11.567706
11.250606	606.865310	11.572723
11.282211	614.077680	11.577741
11.223089	611.524512	11.582759
11.356238	616.480372	11.587776
11.668612	618.072494	11.592794
11.553405	621.505158	11.597811
10.952271	616.777375	11.602829
11.378816	615.214765	11.607847
11.319420	627.525357	11.612864
11.412139	634.504100	11.617882
11.567547	624.851526	11.622899
11.150068	627.129198	11.627917
11.776500	633.225906	11.632935
11.546049	631.917711	11.637952
11.113731	611.100563	11.642970
11.427469	614.024209	11.647987
11.567013	631.614808	11.653005
11.895794	626.031273	11.658023
11.310551	622.421300	11.663040
11.384675	621.295757	11.668058
11.342762	627.055370	11.673075
11.507332	627.067514	11.678093
11.875254	628.237527	11.683111
11.500477	637.833077	11.688128
11.382948	636.510345	11.693146
11.718008	636.101305	11.698163
11.530731	634.546506	11.703181
11.859980	633.582959	11.708199
11.684277	620.630826	11.713216
11.424680	613.732004	11.718234
11.625421	621.094600	11.723251
11.608969	624.218304	11.728269
11.764746	628.356431	11.733287
11.504354	626.465952	11.738304
11.423259	630.044750	11.743322
11.890543	633.319879	11.748339
11.746451	637.691183	11.753357
11.860956	631.437479	11.758375
11.421809	624.491046	11.763392
11.616614	629.197410	11.768410
11.688346	633.282434	11.773427
11.055774	639.298696	11.778445
11.525674	633.282796	11.783463
11.625669	634.895573	11.788480
11.999201	628.263617	11.793498
11.776988	623.511176	11.798515
11.513211	641.209158	11.803533
11.760196	631.930393	11.808551
11.729364	631.124248	11.813568
11.682243	633.413321	11.818586
11.643052	636.079846	11.823603
11.681039	643.559469	11.828621
11.601017	633.025445	11.833639
11.476264	647.646856	11.838656
11.606449	650.624513	11.843674
12.021950	661.323855	11.848691
12.082440	677.210138	11.853709
12.185000	670.062048	11.858727
12.001352	649.070195	11.863744
11.670175	637.698211	11.868762
12.075256	645.309666	11.873779
11.970984	643.110704	11.878797
12.227101	631.378466	11.883815
11.961967	639.612475	11.888832
11.602813	637.191519	11.893850
11.981573	636.766165	11.898867
11.982514	654.671991	11.903885
12.072790	662.048756	11.908903
12.338595	657.860468	11.913920
12.074129	642.539609	11.918938
12.202679	642.592111	11.923955
11.993618	644.010316	11.928973
11.924503	639.009823	11.933991
11.816738	643.154531	11.939008
11.908369	643.550487	11.944026
12.017869	657.986881	11.949043
12.235298	662.740202	11.954061
12.490995	655.053731	11.959079
12.283498	651.633874	11.964096
12.011289	643.679829	11.969114
12.134684	644.427411	11.974131
12.187356	660.141336	11.979149
12.210789	656.776814	11.984167
11.800432	655.275900	11.989184
12.418330	657.719554	11.994202
12.672090	653.694099	11.999219
12.590907	649.541244	12.004237
12.299181	635.966655	12.009255
12.107559	643.955621	12.014272
12.214816	635.957904	12.019290
12.452621	634.358593	12.024307
12.232554	646.678594	12.029325
12.267797	638.067313	12.034343
12.545024	634.751392	12.039360
12.568460	633.731619	12.044378
11.992034	625.730574	12.049395
11.861079	634.593649	12.054413
11.700641	629.995628	12.059431
12.028204	648.427780	12.064448
11.920748	667.978988	12.069466
12.463771	658.013201	12.074483
12.294324	665.449596	12.079501
12.169840	663.720854	12.084519
12.485258	660.509397	12.089536
12.273083	661.745056	12.094554
12.478319	659.478664	12.099571
12.405284	665.950061	12.104589
12.552911	656.478569	12.109607
12.396233	654.401425	12.114624
12.308813	658.662869	12.119642
12.337354	652.987512	12.124659
12.247572	663.043348	12.129677
12.582650	663.883996	12.134695
12.447308	663.573904	12.139712
12.251344	665.289858	12.144730
12.296696	668.081996	12.149747
12.611073	684.900489	12.154765
12.670692	686.933005	12.159783
13.049249	682.859588	12.164800
12.758431	679.645283	12.169818
12.565132	665.562947	12.174835
12.450040	667.910010	12.179853
12.613627	667.540459	12.184871
12.826985	667.402949	12.189888
12.659402	671.112071	12.194906
12.871047	659.232148	12.199923
12.842501	661.758153	12.204941
12.329337	656.918747	12.209959
12.430195	665.139606	12.214976
12.594594	679.810412	12.219994
13.037454	687.286578	12.225011
12.733287	681.073209	12.230029
12.908779	681.462337	12.235047
13.274042	670.221054	12.240064
12.775471	670.378125	12.245082
12.400205	658.088390	12.250099
12.553173	664.215110	12.255117
12.865914	669.991753	12.260135
12.839889	680.722415	12.265152
12.542449	680.712274	12.270170
12.977061	678.618223	12.275187
12.981584	684.872350	12.280205
12.827631	685.676012	12.285223
13.196312	681.913410	12.290240
12.968282	680.459665	12.295258
12.710735	673.730912	12.300275
12.855673	674.765452	12.305293
12.947436	679.383833	12.310311
12.993918	680.342282	12.315328
12.959443	690.881771	12.320346
13.342367	677.649568	12.325363
12.973334	666.778955	12.330381
12.729396	667.016051	12.335399
12.854396	670.111288	12.340416
12.593111	680.900902	12.345434
12.805746	677.509887	12.350451
12.835745	678.960066	12.355469
13.000538	684.510586	12.360487
13.110610	680.927358	12.365504
12.943737	681.291234	12.370522
12.941374	688.070301	12.375539
12.944219	685.715696	12.380557
12.779558	683.579840	12.385575
12.908543	684.900902	12.390592
13.011982	687.317869	12.395610
12.914602	685.007370	12.400627
12.935202	688.163149	12.405645
13.178858	697.936389	12.410663
13.620829	703.774845	12.415680
13.014821	712.415745	12.420698
13.096270	709.032656	12.425715
13.379975	708.145668	12.430733
13.134603	707.190098	12.435751
13.473356	703.889771	12.440768
13.019189	712.020889	12.445786
13.537192	706.379279	12.450803
13.275767	703.772588	12.455821
13.093682	710.418878	12.460839
13.161241	704.904648	12.465856
13.085771	712.398921	12.470874
13.411170	715.080917	12.475891
13.543014	710.471794	12.480909
13.415910	717.825837	12.485927
13.565613	710.613541	12.490944
13.235265	717.235725	12.495962
13.585552	709.881549	12.500979
13.720362	709.166212	12.505997
13.294051	709.444506	12.511015
13.461078	689.375957	12.516032
13.139080	688.056855	12.521050
13.217952	698.588058	12.526067
13.649567	703.986326	12.531085
13.384602	708.673229	12.536103
14.004412	709.440865	12.541120
13.322358	700.102500	12.546138
13.579364	705.184145	12.551155
13.696983	708.299480	12.556173
13.534008	703.004408	12.561191
13.796460	693.347648	12.566208
13.734710	693.486770	12.571226
13.382315	690.572444	12.576243
13.395631	682.873446	12.581261
13.255509	700.454283	12.586279
13.687456	707.111661	12.591296
13.557590	708.239753	12.596314
13.423319	705.360676	12.601331
13.931907	714.063627	12.606349
13.561902	719.663237	12.611367
13.897644	705.933478	12.616384
13.956855	722.457472	12.621402
14.010033	722.417643	12.626419
13.652988	698.464360	12.631437
13.256001	703.121455	12.636455
13.591694	697.820836	12.641472
13.562444	707.097199	12.646490
13.517488	701.849907	12.651507
13.650692	704.562014	12.656525
13.264074	715.399688	12.661543
13.570625	702.365624	12.666560
13.441579	709.546400	12.671578
13.358433	714.233220	12.676595
13.761587	714.596146	12.681613
13.474542	738.230766	12.686631
13.627041	735.682293	12.691648
13.659437	746.227117	12.696666
13.695161	747.764767	12.701683
13.965710	733.237316	12.706701
13.826492	738.968030	12.711719
13.945237	734.704935	12.716736
13.868699	736.430587	12.721754
13.903177	743.238617	12.726771
13.924025	724.319554	12.731789
13.879570	744.776155	12.736807
14.259116	735.953092	12.741824
14.318367	740.646010	12.746842
14.531470	736.964578	12.751859
14.369649	732.136374	12.756877
14.058098	740.257782	12.761895
13.761528	736.580465	12.766912
13.678989	738.344927	12.771930
13.901585	744.517569	12.776947
14.200468	741.908291	12.781965
14.228470	731.328881	12.786983
13.911228	730.536049	12.792000
14.118750	740.580061	12.797018
13.901060	733.400072	12.802035
14.408336	728.918314	12.807053
14.281647	731.383967	12.812071
13.949049	730.751331	12.817088
14.272053	727.115797	12.822106
13.888212	741.370780	12.827123
14.272501	733.957617	12.832141
14.132899	745.583426	12.837159
13.899105	740.700225	12.842176
14.405849	741.343567	12.847194
14.029743	747.392265	12.852211
14.319888	747.302684	12.857229
14.491249	760.230464	12.862247
14.446181	759.480192	12.867264
14.106671	743.186394	12.872282
14.200219	762.396943	12.877299
14.777874	753.899438	12.882317
14.618468	761.760332	12.887335
14.354431	754.120538	12.892352
14.477021	746.439105	12.897370
14.092789	739.042211	12.902387
14.175622	742.292390	12.907405
14.036443	766.961073	12.912423
14.442127	767.607627	12.917440
15.050787	763.974666	12.922458
14.716724	774.602169	12.927475
14.903454	759.570278	12.932493
14.386577	747.189060	12.937511
14.338343	740.165555	12.942528
14.556596	739.216237	12.947546
14.593738	764.412712	12.952563
14.790720	758.146041	12.957581
14.728640	757.663523	12.962599
14.402923	741.771508	12.967616
14.480661	749.443763	12.972634
14.588412	762.681312	12.977651
14.730338	761.838626	12.982669
14.827709	759.301944	12.987687
14.351862	767.414392	12.992704
14.850623	762.874000	12.997722
14.749824	769.321383	13.002739
14.880325	761.203203	13.007757
14.517594	762.080605	13.012775
14.638821	757.766623	13.017792
14.370779	763.905692	13.022810
14.405824	763.808744	13.027827
14.215928	753.812571	13.032845
14.469703	775.614190	13.037863
14.747191	764.945178	13.042880
14.619817	768.139934	13.047898
14.766580	764.030233	13.052915
14.763799	761.818511	13.057933
14.866827	767.410293	13.062951
14.785751	769.237644	13.067968
15.144177	771.677788	13.072986
14.859292	768.983245	13.078003
14.924258	762.674141	13.083021
14.812989	767.841908	13.088039
14.871164	770.840335	13.093056
14.990144	774.012273	13.098074
15.135923	779.565803	13.103091
15.007107	757.653203	13.108109
14.684154	769.989408	13.113127
14.928161	774.366209	13.118144
15.397861	774.750269	13.123162
15.177729	778.647527	13.128179
15.152785	776.319354	13.133197
14.812123	766.173227	13.138215
15.071387	768.237587	13.143232
15.132311	769.159065	13.148250
14.846075	787.539208	13.153267
15.430413	775.294702	13.158285
14.995673	789.216871	13.163303
15.202052	785.309263	13.168320
15.716368	770.816173	13.173338
14.870539	765.968898	13.178355
14.938082	766.684211	13.183373
15.289413	772.631565	13.188391
15.715101	777.074576	13.193408
15.320247	772.115615	13.198426
15.163462	770.246757	13.203443
14.819338	760.400977	13.208461
15.257879	768.408029	13.213479
15.341292	774.772903	13.218496
15.609155	770.322334	13.223514
15.429670	772.619541	13.228531
15.455280	767.250720	13.233549
14.970713	763.744864	13.238567
14.903824	770.101728	13.243584
15.506613	770.307145	13.248602
15.220813	780.551549	13.253619
15.480180	776.430514	13.258637
15.223976	781.750381	13.263655
15.516237	787.047432	13.268672
15.567088	786.960630	13.273690
15.347413	790.371824	13.278707
15.642581	781.735529	13.283725
15.748664	777.799456	13.288743
15.787942	779.494342	13.293760
15.760871	777.147568	13.298778
15.447359	793.032593	13.303795
15.515388	778.035063	13.308813
15.793777	781.163091	13.313831
15.414272	777.126375	13.318848
15.867495	769.017588	13.323866
15.715010	770.726740	13.328883
15.328156	760.663592	13.333901
15.618958	773.578979	13.338919
15.550202	779.396496	13.343936
16.182230	779.243881	13.348954
15.587236	781.221182	13.353971
15.671726	772.185554	13.358989
16.021961	785.883745	13.364007
15.714047	772.197979	13.369024
15.847601	769.939648	13.374042
15.401111	772.748904	13.379059
15.709598	775.717581	13.384077
15.908126	777.687317	13.389095
15.835289	778.632908	13.394112
15.924036	771.338620	13.399130
15.558683	771.045629	13.404147
15.801615	780.137374	13.409165
15.759009	785.146064	13.414183
15.759174	780.030535	13.419200
16.015059	776.465468	13.424218
15.918997	777.711344	13.429235
15.458649	772.554361	13.434253
15.760569	771.992720	13.439271
15.685913	779.139755	13.444288
15.885311	773.387097	13.449306
15.928736	773.197317	13.454323
15.607479	780.430327	13.459341
15.942617	779.667822	13.464359
16.057507	789.098369	13.469376
16.048153	778.237605	13.474394
15.936094	783.061517	13.479411
15.851916	778.060190	13.484429
15.899780	787.580133	13.489447
16.075052	797.389388	13.494464
16.232906	787.553306	13.499482
16.286240	806.858566	13.504499
16.215653	791.125349	13.509517
16.179864	780.148806	13.514535
16.022906	789.735556	13.519552
16.490594	786.885228	13.524570
16.083261	783.591330	13.529587
16.002358	785.286111	13.534605
16.321283	791.311134	13.539623
16.280123	807.314445	13.544640
16.456043	802.155593	13.549658
16.314695	795.048825	13.554675
16.423085	788.423639	13.559693
16.286207	790.752041	13.564711
16.113451	780.229304	13.569728
16.166441	785.267198	13.574746
16.394039	794.263522	13.579763
16.214579	795.011225	13.584781
16.597474	792.530788	13.589799
16.457760	803.951524	13.594816
16.409516	793.100001	13.599834
16.178167	808.104318	13.604851
16.391873	801.083929	13.609869
16.590585	799.055228	13.614887
16.349434	798.622856	13.619904
16.624192	800.470197	13.624922
16.788465	800.018485	13.629939
16.337030	801.600909	13.634957
16.542207	791.129404	13.639975
16.532361	796.208704	13.644992
16.394043	792.443465	13.650010
16.535259	793.450194	13.655027
16.472596	792.421811	13.660045
16.671542	788.641600	13.665063
16.453582	792.251341	13.670080
16.374060	782.209457	13.675098
16.522208	784.736198	13.680115
16.581920	790.003414	13.685133
16.888160	784.009950	13.690151
16.883553	802.115609	13.695168
17.085137	798.401255	13.700186
16.738970	797.975869	13.705203
16.772631	793.385264	13.710221
16.635109	792.087744	13.715239
16.639218	797.461504	13.720256
16.791723	795.118149	13.725274
16.720095	803.687990	13.730291
16.665303	803.583026	13.735309
16.786522	802.705713	13.740327
16.547143	789.757123	13.745344
16.970150	802.345703	13.750362
16.957612	798.494483	13.755379
16.513834	795.231540	13.760397
17.162821	803.685319	13.765415
16.849350	813.501731	13.770432
17.204879	811.060293	13.775450
16.988588	815.818494	13.780467
17.166240	819.801759	13.785485
17.034134	799.552737	13.790503
17.125300	814.983055	13.795520
17.297281	803.816153	13.800538
17.344365	799.728373	13.805555
16.965939	796.303711	13.810573
17.295639	786.765753	13.815591
17.253261	796.015817	13.820608
17.011269	791.711399	13.825626
17.058321	789.182596	13.830643
17.053039	793.465917	13.835661
17.143450	789.895215	13.840679
16.944349	790.399842	13.845696
17.120853	791.123330	13.850714
17.179928	813.476210	13.855731
17.178024	819.551509	13.860749
17.304843	809.183789	13.865767
17.228911	812.900670	13.870784
17.393245	807.412272	13.875802
17.532331	810.117162	13.880819
17.229599	809.991085	13.885837
17.483468	798.495774	13.890855
17.460709	806.540407	13.895872
17.283063	804.299272	13.900890
17.525716	805.621469	13.905907
17.142812	804.529651	13.910925
17.722750	799.389550	13.915943
17.419885	802.094256	13.920960
17.419686	811.596496	13.925978
17.430028	812.620575	13.930995
17.648126	813.271275	13.936013
17.827106	801.352195	13.941031
17.484882	801.371161	13.946048
17.286429	792.032715	13.951066
17.661319	784.841911	13.956083
17.392207	801.871857	13.961101
17.819270	798.018033	13.966119
17.514460	796.068223	13.971136
17.413456	806.340493	13.976154
17.734676	807.568329	13.981171
17.216626	817.173799	13.986189
17.750078	808.430729	13.991207
17.426669	821.884199	13.996224
17.709179	815.922845	14.001242
17.797854	808.773720	14.006259
17.624887	814.695938	14.011277
17.713706	814.309696	14.016295
17.604168	814.730863	14.021312
17.664311	813.367657	14.026330
17.567947	812.865262	14.031347
17.402549	825.656504	14.036365
17.426929	815.484712	14.041383
17.737525	829.413210	14.046400
17.597777	839.189794	14.051418
18.154355	838.039140	14.056435
18.014025	841.715624	14.061453
18.232386	837.140250	14.066471
17.962345	830.599588	14.071488
17.926495	829.358718	14.076506
18.045570	839.823744	14.081523
17.874120	838.436861	14.086541
18.391782	837.349109	14.091559
17.834647	836.240406	14.096576
17.835245	830.686136	14.101594
18.245817	826.702346	14.106611
17.759816	841.860199	14.111629
18.160445	847.717804	14.116647
18.022088	846.805420	14.121664
18.069624	840.104542	14.126682
18.308458	838.170536	14.131699
18.124994	847.136618	14.136717
18.114007	841.252799	14.141735
18.019442	838.859787	14.146752
18.108345	836.598976	14.151770
18.241547	832.911108	14.156787
18.246350	851.422443	14.161805
18.192288	838.533145	14.166823
18.068657	834.450014	14.171840
18.017191	830.254591	14.176858
18.399276	828.121415	14.181875
18.527166	834.416226	14.186893
18.328285	836.826932	14.191911
18.172607	838.508188	14.196928
18.248922	833.860397	14.201946
18.378906	835.967112	14.206963
18.318377	837.933262	14.211981
18.427338	841.277196	14.216999
18.499777	829.639878	14.222016
18.228762	837.653993	14.227034
18.428806	834.672022	14.232051
18.055696	840.909631	14.237069
18.389578	855.487755	14.242087
18.642328	850.291606	14.247104
18.702469	864.104737	14.252122
18.934502	849.065672	14.257139
18.522301	843.746490	14.262157
18.675869	842.700004	14.267175
18.617748	835.150989	14.272192
18.582962	838.618430	14.277210
18.825857	844.159920	14.282227
18.443482	842.859733	14.287245
18.990390	859.985943	14.292263
18.741594	844.498353	14.297280
18.530412	840.744519	14.302298
18.617625	842.930520	14.307315
18.685738	857.676520	14.312333
19.176712	859.332200	14.317351
19.060872	867.867973	14.322368
19.004318	846.928557	14.327386
18.699836	837.906503	14.332403
18.437152	837.805709	14.337421
18.893029	848.546176	14.342439
19.083423	851.618575	14.347456
19.147318	860.915139	14.352474
19.559693	851.619814	14.357491
18.905966	850.112832	14.362509
18.910535	838.113756	14.367527
18.689602	836.340149	14.372544
18.988531	845.404219	14.377562
19.251345	849.566652	14.382579
19.105021	839.803446	14.387597
18.941141	833.530173	14.392615
19.115915	841.991997	14.397632
18.978443	835.676716	14.402650
19.192092	838.392018	14.407667
18.889646	853.287592	14.412685
19.013488	847.168050	14.417703
19.276780	858.494121	14.422720
19.212314	854.660492	14.427738
19.503894	856.842877	14.432755
19.382101	857.628885	14.437773
19.163833	850.950714	14.442791
19.322549	857.770880	14.447808
19.114727	858.617704	14.452826
19.092284	860.262308	14.457843
19.271282	863.267067	14.462861
19.112861	851.416596	14.467879
19.291143	857.776103	14.472896
19.444919	865.928803	14.477914
19.216884	863.616660	14.482931
19.173929	858.851849	14.487949
19.374434	856.232722	14.492967
19.387857	856.224368	14.497984
19.285516	862.545793	14.503002
19.541365	860.984661	14.508019
19.046622	867.124571	14.513037
19.239084	855.380068	14.518055
19.058110	852.741816	14.523072
19.072665	869.698979	14.528090
19.671045	875.118508	14.533107
19.722773	883.321919	14.538125
19.553587	876.976878	14.543143
19.392030	883.149797	14.548160
19.514433	874.568928	14.553178
19.533189	884.405910	14.558195
19.886690	878.979371	14.563213
19.805056	879.781177	14.568231
19.985049	872.677679	14.573248
19.721782	881.217622	14.578266
19.652300	881.859734	14.583283
19.925347	870.686423	14.588301
20.191752	878.139824	14.593319
19.986065	868.733044	14.598336
19.839928	875.045556	14.603354
19.927481	875.912374	14.608371
19.923170	873.341113	14.613389
20.101073	882.383139	14.618407
19.954136	872.134014	14.623424
19.830493	874.267848	14.628442
20.373898	869.136607	14.633459
20.049469	867.742132	14.638477
19.894219	850.617786	14.643495
20.202205	852.040204	14.648512
19.675509	848.799709	14.653530
20.076294	858.412718	14.658547
20.220186	872.660861	14.663565
20.123868	874.629467	14.668583
20.234997	868.511910	14.673600
19.505132	864.586872	14.678618
20.244447	869.315285	14.683635
19.997492	872.364693	14.688653
20.133960	874.751265	14.693671
20.144970	878.287279	14.698688
20.043901	880.143020	14.703706
20.104835	869.507875	14.708723
19.876653	874.324759	14.713741
20.130096	870.952561	14.718759
20.165278	871.654013	14.723776
20.126445	869.113409	14.728794
20.111464	872.924895	14.733811
20.193830	876.686415	14.738829
20.336800	892.992316	14.743847
20.757586	899.998657	14.748864
20.578455	890.253187	14.753882
20.195482	880.741632	14.758899
20.372692	873.222001	14.763917
20.231830	885.649678	14.768935
20.858286	880.647433	14.773952
20.630684	891.993633	14.778970
20.591806	867.535834	14.783987
20.364847	873.109923	14.789005
20.555220	884.135008	14.794023
20.994119	887.177946	14.799040
20.324085	886.440382	14.804058
20.963488	886.097262	14.809075
20.779432	878.507999	14.814093
20.222771	873.233532	14.819111
20.761143	875.393031	14.824128
20.657819	886.028630	14.829146
20.858367	892.088014	14.834163
20.392475	889.450215	14.839181
20.832479	894.127699	14.844199
20.710960	886.030013	14.849216
20.684373	900.446901	14.854234
20.904077	905.799538	14.859251
20.830269	890.521177	14.864269
20.516712	901.779864	14.869287
20.664975	888.486441	14.874304
20.582606	891.825648	14.879322
20.515800	891.602644	14.884339
20.752406	891.780230	14.889357
20.875928	903.181877	14.894375
20.900151	900.590363	14.899392
20.858113	902.108652	14.904410
21.001830	901.111044	14.909427
21.003466	896.045744	14.914445
21.176302	910.737509	14.919463
21.223150	904.131390	14.924480
20.996353	892.929082	14.929498
20.918808	901.149600	14.934515
21.000960	907.691445	14.939533
20.968691	912.960486	14.944551
21.157017	911.842278	14.949568
21.531096	924.022042	14.954586
21.749915	922.384655	14.959603
21.602664	911.053106	14.964621
21.341660	902.667996	14.969639
21.312599	895.325843	14.974656
21.404442	897.015660	14.979674
21.128376	891.621484	14.984691
21.437557	897.708030	14.989709
21.257229	904.243662	14.994727
21.200205	891.291673	14.999744
21.368495	905.674876	15.004762
21.605260	916.859972	15.009779
21.903561	896.849518	15.014797
21.191024	906.542313	15.019815
21.531236	891.805002	15.024832
21.324780	896.965629	15.029850
21.418549	899.289466	15.034867
21.370121	903.118822	15.039885
21.423768	904.710483	15.044903
21.581599	913.730422	15.049920
21.513676	916.167958	15.054938
21.728714	916.109080	15.059955
21.445960	911.912006	15.064973
21.506846	916.330157	15.069991
21.790767	912.899527	15.075008
21.841708	913.705810	15.080026
21.311731	910.393233	15.085043
21.880843	918.168456	15.090061
21.341400	915.201347	15.095079
21.725104	915.182315	15.100096
22.169049	916.684422	15.105114
21.948152	920.174728	15.110131
22.005983	914.037103	15.115149
21.751468	917.886129	15.120167
21.866533	917.360072	15.125184
21.991663	916.359064	15.130202
21.986826	928.942184	15.135219
21.889311	912.575601	15.140237
21.728811	913.639076	15.145255
22.003254	916.559462	15.150272
22.234890	918.561897	15.155290
21.875723	917.409548	15.160307
22.054433	913.944909	15.165325
21.590719	909.722539	15.170343
22.055619	927.429713	15.175360
22.229728	932.312970	15.180378
22.357597	933.741524	15.185395
22.299970	911.312648	15.190413
22.015071	912.471354	15.195431
21.790174	906.011953	15.200448
22.223838	918.889283	15.205466
22.262681	931.500276	15.210483
22.413032	927.705559	15.215501
22.044561	937.256099	15.220519
22.276376	933.559071	15.225536
22.398866	932.924553	15.230554
22.164089	934.473042	15.235571
22.615622	921.229910	15.240589
22.411997	929.274533	15.245607
22.429631	926.400022	15.250624
22.460895	936.859929	15.255642
22.497628	926.768189	15.260659
22.472113	927.504401	15.265677
22.500814	934.117747	15.270695
22.555553	932.455574	15.275712
22.544614	936.515751	15.280730
22.612201	938.215684	15.285747
22.938352	930.880979	15.290765
22.667950	936.373531	15.295783
22.729831	933.249087	15.300800
22.905210	938.368835	15.305818
22.849829	930.036703	15.310835
22.878391	938.638248	15.315853
22.423307	933.388874	15.320871
22.535853	930.638349	15.325888
22.888903	931.892764	15.330906
22.449185	938.431180	15.335923
22.540382	937.353435	15.340941
22.317367	931.616417	15.345959
22.475993	930.073668	15.350976
22.943229	940.550476	15.355994
22.692701	941.337722	15.361011
22.964727	940.547229	15.366029
22.925883	953.198812	15.371047
22.958171	950.287287	15.376064
23.017262	960.007537	15.381082
23.086906	958.447169	15.386099
23.251584	953.564593	15.391117
22.992984	957.887643	15.396135
22.915781	959.439848	15.401152
23.090983	948.890896	15.406170
22.753127	958.316729	15.411187
23.156102	946.469755	15.416205
23.267618	954.752194	15.421223
23.185771	957.261346	15.426240
23.064830	953.345026	15.431258
23.143383	958.754508	15.436275
23.482393	949.631575	15.441293
23.208116	963.942153	15.446311
23.410754	961.127015	15.451328
23.253530	949.866432	15.456346
23.528102	950.183238	15.461363
23.056736	949.932101	15.466381
23.170946	954.322972	15.471399
22.850834	951.122674	15.476416
23.111958	955.256995	15.481434
23.227653	966.505273	15.486451
23.624314	961.305479	15.491469
23.499906	981.203671	15.496487
23.333651	981.810456	15.501504
23.757668	971.042623	15.506522
23.944211	972.427272	15.511539
23.660886	964.023540	15.516557
23.458023	951.097513	15.521575
23.540185	960.397578	15.526592
23.945895	967.655619	15.531610
23.815005	962.914026	15.536627
23.740794	956.345790	15.541645
23.419878	956.673845	15.546663
23.432638	955.854544	15.551680
23.849752	970.003151	15.556698
23.664880	968.529997	15.561715
23.977566	967.401769	15.566733
23.919784	972.845240	15.571751
23.786212	965.986496	15.576768
23.998104	971.157338	15.581786
23.768266	978.208844	15.586803
24.034959	975.481498	15.591821
24.160495	974.313163	15.596839
24.252688	973.595026	15.601856
24.473147	969.325407	15.606874
23.784834	969.439624	15.611891
23.983523	958.284220	15.616909
24.245592	966.514674	15.621927
24.074115	964.102137	15.626944
23.987598	968.685409	15.631962
24.178876	980.470970	15.636979
24.256937	966.992826	15.641997
24.159395	970.549022	15.647015
24.190446	967.549325	15.652032
24.533081	961.436489	15.657050
24.317686	973.787541	15.662067
24.247358	972.485791	15.667085
24.173234	978.562992	15.672103
24.456433	962.695297	15.677120
24.316371	963.689300	15.682138
24.148302	968.137025	15.687155
24.481644	974.626916	15.692173
24.213372	970.301325	15.697191
24.482508	969.527062	15.702208
24.440509	965.197579	15.707226
24.280105	968.416481	15.712243
24.374700	972.081431	15.717261
24.576717	963.885681	15.722279
24.067109	963.195561	15.727296
24.279343	961.486618	15.732314
24.429067	969.204495	15.737331
24.529740	977.807384	15.742349
24.888931	992.855032	15.747367
24.640182	992.856196	15.752384
25.105967	988.084226	15.757402
24.769868	975.399965	15.762419
24.820930	965.924504	15.767437
24.900410	964.779165	15.772455
24.276732	970.014650	15.777472
24.881049	977.052228	15.782490
25.225720	982.896555	15.787507
24.858886	978.264508	15.792525
24.722320	969.061442	15.797543
24.993724	976.785504	15.802560
25.033373	980.948220	15.807578
24.686313	984.202681	15.812595
24.636500	985.245663	15.817613
25.257798	985.672249	15.822631
25.126687	990.985202	15.827648
24.964377	974.082752	15.832666
25.141229	974.768324	15.837683
24.870486	985.423902	15.842701
25.265085	984.355423	15.847719
25.128129	990.032213	15.852736
25.212757	989.703430	15.857754
25.123864	988.139496	15.862771
25.049741	988.018624	15.867789
25.218735	981.768884	15.872807
25.041026	990.323876	15.877824
25.535193	974.729233	15.882842
25.278126	983.031565	15.887859
25.225693	980.767634	15.892877
25.524869	981.664416	15.897895
25.120301	982.204396	15.902912
25.037994	978.367225	15.907930
24.949384	989.698021	15.912947
25.067062	997.196866	15.917965
25.679463	1001.531783	15.922983
25.615415	1018.223689	15.928000
25.981029	1007.824751	15.933018
25.713166	1005.452557	15.938035
25.788338	1008.224297	15.943053
25.773701	1001.946515	15.948071
25.660907	991.562582	15.953088
25.706594	982.580266	15.958106
25.520537	986.677359	15.963123
25.941975	998.171247	15.968141
26.097275	984.911364	15.973159
25.486070	980.790982	15.978176
25.775370	979.221443	15.983194
25.384560	993.480874	15.988211
26.003072	999.058237	15.993229
26.002471	998.894287	15.998247
26.048102	1002.203992	16.003264
26.264370	996.704244	16.008282
26.224648	1004.912571	16.013299
26.129115	989.066321	16.018317
26.222153	974.481279	16.023335
25.952169	975.924834	16.028352
25.563400	970.078072	16.033370
25.687833	985.004703	16.038387
25.959022	991.453845	16.043405
26.035679	1002.793470	16.048423
25.614903	1009.679242	16.053440
25.878794	1005.510108	16.058458
26.111730	1007.913142	16.063475
25.847132	1002.002733	16.068493
26.116369	999.962959	16.073511
26.345655	1010.947312	16.078528
26.403206	1012.424760	16.083546
25.641747	1015.232907	16.088563
25.743300	1021.437235	16.093581
26.257031	1022.909483	16.098599
26.398119	1032.948290	16.103616
26.614817	1036.417394	16.108634
26.552880	1032.220408	16.113651
26.548393	1021.453409	16.118669
26.922728	1016.478006	16.123687
26.581737	1019.340198	16.128704
26.753435	1021.146906	16.133722
26.512411	1015.949176	16.138739
26.355167	1017.330888	16.143757
26.622803	1015.502805	16.148775
26.417172	1018.362724	16.153792
26.669310	1019.326840	16.158810
26.665049	1017.295201	16.163827
26.490864	1025.209021	16.168845
26.631078	1024.603280	16.173863
26.418693	1018.321762	16.178880
26.685269	1021.391723	16.183898
26.817337	1032.590140	16.188915
26.903174	1040.526343	16.193933
27.162135	1032.119666	16.198951
27.259039	1028.819302	16.203968
27.168600	1022.013740	16.208986
26.869434	1009.172188	16.214003
26.800771	1020.777593	16.219021
27.152153	1005.299970	16.224039
26.877582	1006.299271	16.229056
27.011060	1020.659619	16.234074
26.992527	1018.327255	16.239091
27.417406	1026.791008	16.244109
27.309925	1019.880817	16.249127
27.310524	1011.975383	16.254144
27.137043	1013.353327	16.259162
27.140184	1006.987551	16.264179
27.048622	1013.111678	16.269197
27.304579	1029.942807	16.274215
27.678216	1034.911598	16.279232
27.434328	1027.533620	16.284250
27.807549	1013.677831	16.289267
27.273828	1017.393896	16.294285
27.359011	1000.998606	16.299303
27.048500	1011.701456	16.304320
27.444862	1019.080906	16.309338
27.427182	1024.871565	16.314355
27.518904	1031.721229	16.319373
27.490578	1038.078458	16.324391
27.684934	1037.091844	16.329408
27.598788	1041.141737	16.334426
27.802888	1034.769712	16.339443
27.738637	1036.695441	16.344461
28.157506	1031.757238	16.349479
27.796411	1030.166520	16.354496
28.027544	1023.572510	16.359514
27.779009	1006.257499	16.364531
27.554748	1007.274165	16.369549
27.849236	1010.929894	16.374567
27.634986	1023.975088	16.379584
27.485988	1022.537335	16.384602
27.721462	1029.269801	16.389619
27.709631	1035.753834	16.394637
27.810420	1028.530138	16.399655
28.198141	1025.206302	16.404672
27.932906	1023.341785	16.409690
27.803432	1020.461905	16.414707
27.893270	1029.158037	16.419725
27.879475	1030.810769	16.424743
28.200125	1026.588555	16.429760
27.978690	1027.292350	16.434778
28.285625	1020.374035	16.439795
28.261021	1022.703811	16.444813
28.043923	1039.520703	16.449831
28.183181	1020.529124	16.454848
28.472798	1036.281997	16.459866
28.483105	1030.754546	16.464883
28.202185	1028.636863	16.469901
27.978212	1023.307069	16.474919
28.563872	1046.742246	16.479936
28.317689	1053.995162	16.484954
28.485239	1053.631294	16.489971
28.643666	1058.479174	16.494989
28.671973	1045.157091	16.500007
28.833330	1055.044410	16.505024
28.590952	1045.283517	16.510042
28.560661	1032.920536	16.515059
28.304616	1030.625383	16.520077
28.528671	1043.103294	16.525095
28.595458	1058.158941	16.530112
28.630418	1057.812691	16.535130
28.601090	1054.847686	16.540147
28.858292	1057.868629	16.545165
28.669170	1049.926630	16.550183
29.064947	1050.577904	16.555200
28.874979	1052.447592	16.560218
28.841103	1050.032419	16.565235
28.972638	1053.110920	16.570253
28.984272	1048.135531	16.575271
29.185401	1055.185817	16.580288
28.991905	1048.513158	16.585306
28.955203	1042.989913	16.590323
28.921360	1047.773238	16.595341
29.429068	1043.149323	16.600359
29.304770	1049.357487	16.605376
29.066444	1046.235878	16.610394
29.186802	1042.183900	16.615411
29.275127	1053.480704	16.620429
29.030995	1040.390661	16.625447
29.202661	1034.146796	16.630464
29.075656	1048.333380	16.635482
29.021439	1049.635835	16.640499
29.187274	1049.925498	16.645517
29.088601	1050.398618	16.650535
28.831343	1050.953389	16.655552
28.807701	1048.369353	16.660570
28.940320	1042.870072	16.665587
29.130460	1059.291813	16.670605
29.105517	1061.018879	16.675623
29.082138	1066.027792	16.680640
29.130126	1074.238189	16.685658
29.158896	1063.409149	16.690675
29.554515	1072.496056	16.695693
29.815601	1086.340993	16.700711
30.006366	1076.515375	16.705728
29.659370	1078.557993	16.710746
29.652741	1060.535987	16.715763
29.584088	1060.366920	16.720781
29.440452	1083.458810	16.725799
29.656380	1077.791829	16.730816
29.528740	1086.840805	16.735834
29.842426	1074.329226	16.740851
30.407874	1073.458040	16.745869
29.834441	1073.680491	16.750887
30.079782	1077.135648	16.755904
29.794376	1085.694936	16.760922
30.027285	1082.392189	16.765939
30.025444	1082.143225	16.770957
29.853801	1079.411956	16.775975
30.283965	1084.368749	16.780992
29.927877	1085.150448	16.786010
30.110800	1081.820819	16.791027
30.388673	1081.537497	16.796045
30.338479	1082.697311	16.801063
30.460852	1075.470214	16.806080
30.158820	1077.111305	16.811098
30.007551	1077.860914	16.816115
30.021143	1076.448176	16.821133
30.368398	1075.431292	16.826151
30.327439	1073.720982	16.831168
30.257698	1088.548733	16.836186
30.170091	1079.066535	16.841203
30.241962	1083.101147	16.846221
30.381336	1088.239203	16.851239
30.523412	1092.887679	16.856256
30.590519	1099.400394	16.861274
30.634877	1103.761220	16.866291
30.760242	1104.653683	16.871309
30.676235	1105.279143	16.876327
30.710997	1099.987685	16.881344
30.570236	1110.701868	16.886362
31.002573	1106.402176	16.891379
30.532534	1108.375712	16.896397
31.020328	1107.264222	16.901415
30.810572	1098.706885	16.906432
31.062973	1100.437839	16.911450
31.103651	1089.723684	16.916467
30.800503	1090.815831	16.921485
30.655606	1094.846539	16.926503
31.459053	1093.830763	16.931520
31.067429	1085.551240	16.936538
30.808202	1082.562290	16.941555
31.133825	1097.249206	16.946573
31.002662	1096.247317	16.951591
31.100705	1095.588221	16.956608
30.903798	1100.434979	16.961626
30.654337	1102.484410	16.966643
30.924797	1102.498901	16.971661
30.917766	1086.562957	16.976679
31.043915	1093.580824	16.981696
30.477824	1105.608210	16.986714
30.978597	1111.229302	16.991731
31.359411	1121.943825	16.996749
31.354764	1123.677185	17.001767
31.666609	1118.913521	17.006784
31.596402	1125.056431	17.011802
31.568557	1116.562104	17.016819
31.437610	1126.665677	17.021837
31.261000	1124.676809	17.026855
31.605998	1121.555312	17.031872
31.249073	1128.065045	17.036890
31.616286	1121.112000	17.041907
31.432179	1117.022499	17.046925
31.461096	1121.070162	17.051943
31.396959	1121.484222	17.056960
31.769577	1136.413122	17.061978
32.198765	1135.639023	17.066995
31.849753	1129.312598	17.072013
31.927897	1126.785188	17.077031
31.866769	1118.188775	17.082048
31.935741	1124.177333	17.087066
32.029541	1124.099580	17.092083
31.874808	1125.364139	17.097101
32.105733	1138.854074	17.102119
32.056681	1134.525655	17.107136
32.383725	1145.520021	17.112154
32.454721	1132.289017	17.117171
32.558835	1122.694705	17.122189
32.096442	1120.053166	17.127207
32.500963	1120.750411	17.132224
32.086576	1119.319516	17.137242
32.252416	1116.399663	17.142259
32.041139	1118.572503	17.147277
32.047519	1117.268191	17.152295
32.261647	1121.618202	17.157312
32.345873	1140.900049	17.162330
32.325597	1139.274857	17.167347
32.584184	1141.673890	17.172365
32.264913	1143.169362	17.177383
32.700653	1141.258123	17.182400
32.657712	1146.929701	17.187418
32.882672	1144.786392	17.192435
32.589159	1142.629642	17.197453
32.560887	1139.260506	17.202471
32.970345	1140.556594	17.207488
32.290433	1139.407145	17.212506
32.339565	1135.716607	17.217523
32.321736	1137.956972	17.222541
32.303750	1141.794234	17.227559
32.668005	1130.290883	17.232576
32.717106	1130.295874	17.237594
32.858608	1139.514151	17.242611
32.789266	1136.877300	17.247629
32.681784	1134.236958	17.252647
33.015544	1140.348140	17.257664
33.054643	1162.067101	17.262682
32.931828	1154.622763	17.267699
33.354427	1168.953710	17.272717
33.040209	1162.691251	17.277735
32.945463	1160.433927	17.282752
33.042822	1157.726773	17.287770
32.923174	1155.700573	17.292787
33.368670	1162.699992	17.297805
33.192607	1154.058452	17.302823
33.347105	1165.704729	17.307840
33.158283	1153.735740	17.312858
33.206812	1156.593730	17.317875
33.471859	1148.851934	17.322893
33.287775	1159.670766	17.327911
33.512689	1149.716678	17.332928
33.672732	1159.462247	17.337946
33.630927	1164.568750	17.342963
33.541064	1152.972430	17.347981
33.386540	1148.474335	17.352999
33.625754	1143.040376	17.358016
33.730007	1154.536724	17.363034
33.556815	1145.493942	17.368051
33.630440	1145.810678	17.373069
33.678337	1145.872663	17.378087
33.796152	1159.519194	17.383104
33.734649	1171.328707	17.388122
33.818907	1168.541552	17.393139
34.034197	1172.922951	17.398157
33.914299	1173.957989	17.403175
33.886054	1175.237449	17.408192
34.002387	1171.119799	17.413210
33.880558	1169.608348	17.418227
34.443916	1172.941112	17.423245
34.425891	1175.572842	17.428263
34.079702	1166.582402	17.433280
34.129706	1174.183444	17.438298
34.199131	1178.840170	17.443315
34.465000	1171.593708	17.448333
34.245423	1170.918099	17.453351
34.193717	1173.605599	17.458368
34.398175	1171.872608	17.463386
34.340878	1166.084302	17.468403
34.369822	1169.863722	17.473421
34.198830	1179.071019	17.478439
34.311567	1176.377232	17.483456
34.309319	1174.379974	17.488474
34.298638	1171.298417	17.493491
34.672168	1162.192059	17.498509
34.235403	1169.181385	17.503527
34.444197	1167.965279	17.508544
34.468708	1170.782852	17.513562
34.222313	1178.872158	17.518579
34.426923	1191.791887	17.523597
34.839660	1195.299737	17.528615
34.714897	1191.535444	17.533632
34.727527	1198.883571	17.538650
34.694082	1196.244244	17.543667
35.011496	1184.413674	17.548685
34.686703	1192.032421	17.553703
34.812465	1187.648196	17.558720
34.886245	1186.585789	17.563738
34.798178	1191.696392	17.568755
35.082741	1187.874280	17.573773
34.840115	1190.134094	17.578791
35.159802	1191.065545	17.583808
35.074550	1188.620532	17.588826
35.372616	1206.941119	17.593843
35.415425	1209.487581	17.598861
35.125876	1198.111871	17.603879
35.459126	1205.466572	17.608896
35.547298	1204.468183	17.613914
35.148407	1199.380342	17.618931
35.481240	1201.373266	17.623949
35.353574	1207.045513	17.628967
35.472863	1213.045153	17.633984
35.571828	1207.339650	17.639002
35.573260	1224.264492	17.644019
35.959214	1206.127179	17.649037
35.512855	1213.067531	17.654055
35.677975	1211.381726	17.659072
36.112920	1207.015328	17.664090
35.540308	1208.339054	17.669107
35.553696	1192.163126	17.674125
35.785664	1213.192352	17.679143
36.072052	1208.287482	17.684160
36.051817	1208.076113	17.689178
36.163300	1209.387333	17.694195
36.404060	1193.816423	17.699213
35.576749	1195.129559	17.704231
35.748848	1197.005652	17.709248
35.859689	1196.609640	17.714266
35.857459	1199.276769	17.719283
36.103387	1197.941231	17.724301
35.914558	1200.511361	17.729319
35.791218	1204.368298	17.734336
36.183883	1193.965015	17.739354
36.110624	1203.646172	17.744371
36.093476	1206.874231	17.749389
36.307282	1199.484432	17.754407
36.410554	1196.492317	17.759424
36.657855	1194.121435	17.764442
36.485482	1200.529693	17.769459
36.580345	1203.244728	17.774477
36.383269	1210.556287	17.779495
36.029387	1207.115075	17.784512
36.122851	1214.336931	17.789530
36.570868	1230.197705	17.794547
36.681923	1222.536810	17.799565
36.501280	1233.307810	17.804583
36.734761	1226.312560	17.809600
36.933193	1222.106294	17.814618
36.570491	1240.148579	17.819635
36.732655	1234.972823	17.824653
37.168508	1234.781516	17.829671
36.487552	1236.971153	17.834688
36.747649	1233.152864	17.839706
36.911608	1225.243832	17.844723
36.833162	1230.125715	17.849741
36.719612	1233.419377	17.854759
36.773664	1238.267880	17.859776
37.173585	1252.245832	17.864794
37.257238	1256.868790	17.869811
37.666630	1251.051519	17.874829
37.495855	1247.853017	17.879847
37.031468	1240.414820	17.884864
37.237440	1226.897504	17.889882
36.890652	1250.078245	17.894899
37.196514	1245.760465	17.899917
37.404134	1242.196556	17.904935
37.416110	1248.717963	17.909952
37.487799	1245.001777	17.914970
37.126221	1247.974531	17.919987
37.500241	1248.370439	17.925005
37.645686	1245.437981	17.930023
37.528557	1250.546843	17.935040
37.527910	1249.193128	17.940058
37.355290	1247.333012	17.945075
37.609135	1244.699160	17.950093
37.649607	1251.279221	17.955111
37.629087	1249.714019	17.960128
38.097567	1259.913104	17.965146
37.646714	1263.439505	17.970163
38.048374	1266.463097	17.975181
38.025868	1271.434060	17.980199
37.814908	1266.550291	17.985216
38.239932	1257.678821	17.990234
38.007661	1266.570706	17.995251
38.057671	1259.203390	18.000269
38.024287	1264.775675	18.005287
38.116387	1265.111609	18.010304
38.287558	1265.002798	18.015322
38.290341	1268.540178	18.020339
38.271690	1261.313011	18.025357
38.452176	1263.301408	18.030375
38.289914	1265.510769	18.035392
38.693976	1259.460795	18.040410
38.724786	1263.997356	18.045427
38.748973	1255.497967	18.050445
38.409839	1265.290244	18.055463
38.274313	1270.439865	18.060480
38.357231	1260.719407	18.065498
38.159517	1260.327556	18.070515
38.358098	1258.604945	18.075533
38.270025	1259.022759	18.080551
38.034032	1270.443098	18.085568
38.430250	1272.814275	18.090586
38.701378	1294.165674	18.095603
38.877265	1274.581089	18.100621
38.993479	1280.966252	18.105639
38.705849	1285.827275	18.110656
39.194612	1279.612540	18.115674
39.113989	1282.437135	18.120691
39.097842	1284.304859	18.125709
39.130919	1284.094604	18.130727
39.268640	1286.780846	18.135744
39.237424	1276.264041	18.140762
39.076466	1288.900280	18.145779
39.554493	1279.584980	18.150797
39.222734	1280.179834	18.155815
38.796530	1291.027213	18.160832
39.294896	1279.922489	18.165850
39.369190	1278.478132	18.170867
39.422908	1270.747303	18.175885
39.418159	1274.178564	18.180903
39.050550	1277.881279	18.185920
39.457433	1292.688173	18.190938
39.520648	1298.229554	18.195955
39.755084	1306.426625	18.200973
39.919164	1305.116526	18.205991
39.650342	1298.215727	18.211008
39.588089	1290.581956	18.216026
39.818857	1298.208381	18.221043
39.865232	1296.402313	18.226061
39.614026	1292.518951	18.231079
39.611360	1298.834381	18.236096
40.004108	1291.485938	18.241114
39.781825	1296.636535	18.246131
39.810221	1296.600588	18.251149
40.081511	1297.971986	18.256167
40.216004	1292.159901	18.261184
40.176273	1288.202380	18.266202
40.080289	1283.925460	18.271219
39.518055	1289.470154	18.276237
40.246749	1284.824178	18.281255
39.952032	1301.719751	18.286272
40.175525	1305.733814	18.291290
40.550561	1315.647762	18.296307
40.213026	1325.010618	18.301325
40.404693	1317.034086	18.306343
40.234186	1327.825646	18.311360
40.587356	1318.220610	18.316378
40.408351	1318.441226	18.321395
40.172171	1321.044040	18.326413
40.726790	1313.256803	18.331431
40.307631	1310.434887	18.336448
40.654650	1310.569931	18.341466
40.721051	1309.313008	18.346483
40.613799	1312.400563	18.351501
40.971901	1311.523983	18.356519
40.906175	1322.374864	18.361536
40.819840	1323.587694	18.366554
41.163702	1338.158340	18.371571
41.172624	1332.410100	18.376589
41.392429	1318.161533	18.381607
41.465224	1304.971146	18.386624
41.164068	1304.611279	18.391642
41.025411	1308.540068	18.396659
41.136214	1311.432509	18.401677
41.177912	1316.844719	18.406695
41.046813	1307.580658	18.411712
41.469236	1321.873887	18.416730
41.556182	1332.520967	18.421747
41.429528	1326.118607	18.426765
41.575124	1328.017801	18.431783
41.484950	1333.703150	18.436800
41.512959	1329.952763	18.441818
41.374845	1335.787639	18.446835
41.555828	1332.941121	18.451853
41.409615	1332.108839	18.456871
41.593613	1327.718612	18.461888
41.544236	1332.794790	18.466906
41.864932	1336.004655	18.471923
41.347549	1342.438616	18.476941
41.436442	1327.610930	18.481959
41.472251	1339.458959	18.486976
41.751032	1344.871903	18.491994
41.999807	1341.276279	18.497011
41.540797	1341.865824	18.502029
41.574450	1346.487171	18.507047
41.676188	1346.354523	18.512064
41.807839	1347.296508	18.517082
41.889619	1354.173103	18.522099
42.149003	1367.182210	18.527117
42.216325	1366.862443	18.532135
42.504629	1369.686056	18.537152
42.869502	1371.727630	18.542170
42.636889	1367.831870	18.547187
42.286296	1349.241749	18.552205
42.449135	1352.340645	18.557223
42.420905	1367.689160	18.562240
42.696006	1357.600857	18.567258
42.833317	1367.523676	18.572275
42.693336	1348.670176	18.577293
42.983698	1337.121464	18.582311
42.680242	1348.407252	18.587328
42.664728	1339.819365	18.592346
42.587772	1345.136562	18.597363
42.641339	1360.147196	18.602381
42.918993	1364.824996	18.607399
43.094662	1361.285005	18.612416
43.133721	1371.548279	18.617434
43.128901	1366.146175	18.622451
43.235048	1370.872939	18.627469
42.960492	1341.241005	18.632487
43.136328	1352.751513	18.637504
43.037560	1362.159033	18.642522
43.317215	1361.342081	18.647539
43.282193	1366.554880	18.652557
43.528262	1363.246864	18.657575
43.206290	1357.073916	18.662592
43.148856	1364.587728	18.667610
43.005974	1355.808343	18.672627
42.809543	1372.073182	18.677645
43.305860	1362.524593	18.682663
43.272319	1362.211161	18.687680
43.851406	1369.827226	18.692698
43.862688	1369.188025	18.697715
43.402542	1369.903985	18.702733
43.893367	1367.068878	18.707751
43.747144	1369.029578	18.712768
43.520276	1378.854822	18.717786
43.853878	1382.116324	18.722803
43.728647	1375.215088	18.727821
44.194761	1383.552627	18.732839
43.916417	1375.596058	18.737856
44.023621	1377.996751	18.742874
44.308013	1382.878634	18.747891
44.192378	1377.727426	18.752909
44.632455	1376.386704	18.757927
44.518309	1388.128867	18.762944
44.181430	1378.644538	18.767962
43.932631	1384.465212	18.772979
44.235364	1387.068809	18.777997
43.824110	1386.158126	18.783015
43.960935	1387.866190	18.788032
43.959886	1377.486615	18.793050
44.486917	1378.742209	18.798067
44.488188	1398.980951	18.803085
44.597221	1403.066620	18.808103
44.719514	1401.359105	18.813120
44.773789	1401.278075	18.818138
45.100793	1402.994215	18.823155
44.828210	1408.301053	18.828173
44.963849	1401.485172	18.833191
44.793883	1402.853127	18.838208
44.885866	1404.284186	18.843226
44.815326	1400.826945	18.848243
44.989584	1397.760556	18.853261
44.971390	1399.234124	18.858279
45.025282	1409.536123	18.863296
44.679343	1403.638323	18.868314
45.238070	1397.065435	18.873331
44.778094	1409.827506	18.878349
45.093072	1397.773108	18.883367
44.913417	1399.073150	18.888384
45.200003	1410.253907	18.893402
45.514771	1418.066045	18.898419
45.505740	1426.642157	18.903437
45.666433	1418.440050	18.908455
45.036829	1418.084302	18.913472
45.331315	1427.783706	18.918490
45.703603	1418.213493	18.923507
45.371661	1418.297121	18.928525
45.623221	1411.276874	18.933543
45.947933	1419.718639	18.938560
45.665705	1420.592925	18.943578
45.831203	1425.644932	18.948595
45.721371	1421.493229	18.953613
46.159134	1420.727244	18.958631
45.970823	1416.256466	18.963648
45.908278	1423.307184	18.968666
45.983269	1408.292254	18.973683
45.806038	1417.349166	18.978701
46.284881	1413.061051	18.983719
45.828908	1414.820968	18.988736
45.961750	1422.147197	18.993754
46.197360	1436.772755	18.998771
46.097305	1438.495846	19.003789
46.306329	1446.460269	19.008807
46.211831	1443.265560	19.013824
46.348015	1446.687397	19.018842
46.351719	1438.768664	19.023859
46.425793	1445.674904	19.028877
46.322431	1446.319188	19.033895
46.443498	1437.451069	19.038912
46.520279	1435.738057	19.043930
47.011203	1447.464357	19.048947
46.601432	1455.541514	19.053965
46.715791	1451.970084	19.058983
46.834816	1460.860677	19.064000
46.725171	1463.172275	19.069018
46.878473	1455.864437	19.074035
46.924029	1462.753060	19.079053
47.507345	1463.214016	19.084071
47.603567	1459.588620	19.089088
47.275356	1468.015936	19.094106
47.003354	1461.042985	19.099123
47.477461	1467.728761	19.104141
47.325318	1459.941738	19.109159
47.234399	1468.606441	19.114176
47.243963	1463.498711	19.119194
47.371396	1451.943894	19.124211
47.133472	1470.408691	19.129229
47.120692	1463.404593	19.134247
47.250539	1464.542535	19.139264
47.067937	1468.099532	19.144282
47.372335	1476.143703	19.149299
47.722226	1482.312439	19.154317
47.732180	1483.049428	19.159335
47.749860	1486.925358	19.164352
47.684317	1482.874004	19.169370
47.957304	1481.729874	19.174387
48.294335	1479.856157	19.179405
48.184081	1474.622024	19.184423
48.143040	1474.136190	19.189440
48.224727	1474.366458	19.194458
48.464930	1474.896952	19.199475
48.211094	1482.873947	19.204493
48.429573	1481.763605	19.209511
48.781990	1470.489119	19.214528
48.401809	1478.785721	19.219546
48.699155	1470.808343	19.224563
48.636791	1477.707569	19.229581
48.504895	1473.445697	19.234599
48.524233	1466.954138	19.239616
48.532235	1471.595316	19.244634
48.586005	1466.543778	19.249651
48.524008	1473.562870	19.254669
48.790569	1469.244882	19.259687
48.908830	1455.520220	19.264704
48.676512	1475.593667	19.269722
48.922236	1470.212240	19.274739
48.679023	1473.822918	19.279757
48.865224	1469.956195	19.284775
49.061755	1477.698519	19.289792
48.808627	1480.196708	19.294810
48.616065	1467.555881	19.299827
48.479687	1473.112808	19.304845
48.887365	1484.662819	19.309863
49.264438	1487.545130	19.314880
48.820659	1504.009794	19.319898
49.243652	1490.698128	19.324915
49.514914	1508.180590	19.329933
49.133635	1505.207534	19.334951
49.546682	1494.908185	19.339968
49.148963	1500.240968	19.344986
49.116063	1490.737355	19.350003
49.543368	1502.353734	19.355021
49.578093	1510.389677	19.360039
49.720847	1521.192235	19.365056
49.532051	1518.324724	19.370074
49.645300	1514.412615	19.375091
49.837260	1513.988108	19.380109
49.792120	1517.211140	19.385127
50.180725	1516.907308	19.390144
49.739874	1521.312698	19.395162
49.978931	1523.071032	19.400179
50.007003	1511.077289	19.405197
50.050081	1520.358523	19.410215
50.085634	1510.285574	19.415232
49.990227	1515.529969	19.420250
50.281867	1520.679010	19.425267
50.373271	1537.164000	19.430285
50.189601	1537.293827	19.435303
50.134812	1540.796098	19.440320
50.253317	1546.672891	19.445338
50.821381	1534.064331	19.450355
50.575040	1536.662455	19.455373
50.516413	1530.744845	19.460391
50.745226	1536.964129	19.465408
50.612055	1542.088211	19.470426
50.364035	1531.374840	19.475443
50.607986	1539.160256	19.480461
50.804282	1557.418249	19.485479
50.959469	1550.621340	19.490496
50.815781	1557.760567	19.495514
50.925223	1552.914886	19.500531
51.149656	1552.081329	19.505549
50.660164	1557.176032	19.510567
51.089592	1558.784618	19.515584
51.203797	1566.423108	19.520602
51.361093	1557.546098	19.525619
51.267984	1558.406539	19.530637
51.423693	1566.805422	19.535655
51.586439	1569.039641	19.540672
51.686363	1577.459893	19.545690
51.706400	1577.904958	19.550707
51.819648	1561.387987	19.555725
51.555918	1557.515996	19.560743
51.793288	1565.217244	19.565760
51.978102	1563.490450	19.570778
51.997780	1564.866575	19.575795
51.787966	1546.547694	19.580813
51.751878	1563.933192	19.585831
52.055012	1558.495404	19.590848
52.217450	1566.473492	19.595866
52.527068	1564.307403	19.600883
52.388560	1554.460525	19.605901
52.216346	1545.136508	19.610919
51.920658	1543.851088	19.615936
52.123352	1540.341544	19.620954
52.147560	1546.974757	19.625971
52.049523	1563.246445	19.630989
51.836438	1563.223083	19.636007
51.985182	1565.039755	19.641024
52.236191	1568.541460	19.646042
52.336222	1560.935799	19.651059
52.496996	1564.123422	19.656077
52.666957	1586.759713	19.661095
53.049759	1582.473982	19.666112
52.755385	1584.754575	19.671130
52.568053	1584.297970	19.676147
52.870159	1585.831828	19.681165
53.183916	1592.059915	19.686183
53.021186	1584.280807	19.691200
53.143674	1583.049792	19.696218
53.283879	1585.918736	19.701235
52.837223	1575.422661	19.706253
53.067249	1583.068259	19.711271
53.012824	1577.080545	19.716288
53.304267	1580.708467	19.721306
53.496054	1586.195078	19.726323
53.515584	1575.685926	19.731341
53.350958	1581.957401	19.736359
53.645069	1587.090294	19.741376
53.713565	1586.994412	19.746394
53.284258	1577.057377	19.751411
53.826316	1584.852913	19.756429
53.235959	1586.299370	19.761447
53.718731	1601.116724	19.766464
53.812779	1615.736205	19.771482
53.724913	1614.869520	19.776499
54.299379	1612.557784	19.781517
53.813879	1613.498642	19.786535
54.232401	1612.142345	19.791552
53.864417	1609.700544	19.796570
53.947321	1613.698833	19.801587
54.179389	1612.990316	19.806605
54.255781	1618.258319	19.811623
54.367951	1612.875683	19.816640
54.468950	1612.739993	19.821658
54.124425	1607.400507	19.826675
53.999675	1612.772610	19.831693
54.170864	1626.972896	19.836711
54.407151	1636.204983	19.841728
54.494671	1635.459149	19.846746
54.612690	1629.491739	19.851763
54.777539	1627.951112	19.856781
54.548926	1635.258316	19.861799
54.701013	1628.468176	19.866816
54.943590	1633.028460	19.871834
54.887483	1629.546822	19.876851
54.903682	1631.043424	19.881869
55.024094	1648.925218	19.886887
54.901078	1639.716526	19.891904
55.231067	1652.594853	19.896922
55.201724	1646.445388	19.901939
55.402933	1649.118582	19.906957
55.266194	1656.244134	19.911975
55.396543	1643.779819	19.916992
55.090279	1640.343685	19.922010
55.186657	1640.259214	19.927027
55.902229	1633.768970	19.932045
55.691229	1642.174847	19.937063
55.658657	1640.775609	19.942080
55.927037	1645.234019	19.947098
55.743304	1640.563642	19.952115
56.058711	1634.524277	19.957133
55.696425	1645.254551	19.962151
55.798268	1643.644896	19.967168
55.695269	1640.347336	19.972186
55.720931	1641.296476	19.977203
55.747819	1653.897229	19.982221
55.952277	1662.894463	19.987239
55.993975	1664.254523	19.992256
55.849625	1668.007548	19.997274
55.901973	1678.199485	20.002291
56.273794	1661.480955	20.007309
56.290242	1666.325998	20.012327
56.595016	1673.436035	20.017344
56.615996	1683.320449	20.022362
56.674599	1691.687265	20.027379
56.885693	1679.936146	20.032397
56.688531	1688.873235	20.037415
57.190115	1676.126661	20.042432
57.141309	1674.925633	20.047450
56.411355	1661.065451	20.052467
56.461817	1660.710450	20.057485
56.954916	1677.328303	20.062503
57.121197	1675.919999	20.067520
57.205578	1676.111977	20.072538
56.709933	1682.583679	20.077555
57.303149	1673.562571	20.082573
56.899696	1688.834443	20.087591
57.081912	1681.840736	20.092608
57.337892	1688.450313	20.097626
57.387836	1699.175997	20.102643
57.892301	1702.896807	20.107661
57.615665	1704.947407	20.112679
57.755138	1696.890516	20.117696
57.759005	1698.048212	20.122714
57.413555	1703.735801	20.127731
57.327125	1705.766068	20.132749
57.561195	1701.487832	20.137767
57.613687	1701.776329	20.142784
57.587205	1700.802188	20.147802
57.375861	1720.364511	20.152819
57.941946	1713.039236	20.157837
57.799020	1723.558454	20.162855
58.023106	1726.856115	20.167872
58.115131	1723.300754	20.172890
58.432471	1724.731247	20.177907
58.424613	1717.069836	20.182925
58.124620	1724.161030	20.187943
58.189260	1717.674905	20.192960
58.447735	1732.975659	20.197978
58.837645	1741.637748	20.202995
59.043402	1743.555965	20.208013
59.227832	1738.550155	20.213031
58.902848	1726.592646	20.218048
58.956969	1715.503605	20.223066
58.658687	1715.108563	20.228083
58.829730	1718.711193	20.233101
59.021753	1731.642753	20.238119
58.964853	1734.233317	20.243136
59.351969	1734.381020	20.248154
59.139380	1741.041938	20.253171
59.469892	1728.312661	20.258189
59.223480	1736.799874	20.263207
59.556505	1728.232936	20.268224
59.513947	1732.058394	20.273242
59.413118	1729.757766	20.278259
60.010161	1721.007448	20.283277
59.837176	1720.905216	20.288295
59.744886	1730.804247	20.293312
59.929223	1712.950489	20.298330
59.334007	1714.460836	20.303347
59.725804	1723.198364	20.308365
59.738283	1734.485390	20.313383
59.858809	1729.707357	20.318400
59.729499	1718.334611	20.323418
59.674853	1727.956329	20.328435
59.886306	1721.049549	20.333453
59.551360	1727.732788	20.338471
59.735878	1739.434700	20.343488
60.462473	1747.261360	20.348506
60.084916	1751.117215	20.353523
60.185819	1755.668169	20.358541
59.921963	1758.436335	20.363559
60.231043	1752.243278	20.368576
60.245225	1749.867821	20.373594
60.706113	1771.729735	20.378611
60.478457	1777.323148	20.383629
60.425349	1774.891955	20.388647
60.768829	1772.988795	20.393664
61.072495	1772.496285	20.398682
60.818275	1779.498273	20.403699
61.084452	1767.435493	20.408717
61.412047	1767.384228	20.413735
61.140299	1773.540001	20.418752
61.355441	1768.447315	20.423770
61.403228	1770.453405	20.428787
61.292030	1764.954232	20.433805
61.137909	1766.016757	20.438823
60.914156	1767.648800	20.443840
61.241712	1770.453704	20.448858
61.479965	1790.302290	20.453875
61.620654	1790.933597	20.458893
61.595631	1799.010590	20.463911
61.895408	1799.033115	20.468928
62.089007	1797.920340	20.473946
61.727599	1805.589265	20.478963
61.920965	1799.171311	20.483981
62.038184	1806.992480	20.488999
61.793081	1799.819510	20.494016
62.182449	1792.480861	20.499034
62.137430	1788.404130	20.504051
62.146537	1791.691300	20.509069
62.130270	1794.221854	20.514087
62.027406	1796.204210	20.519104
62.208258	1806.480234	20.524122
61.765401	1809.500528	20.529139
62.029805	1816.799995	20.534157
62.490187	1821.518719	20.539175
62.545101	1819.742821	20.544192
62.653677	1818.779073	20.549210
62.639380	1832.756104	20.554227
62.846535	1839.367075	20.559245
63.156068	1828.004405	20.564263
63.095628	1838.311939	20.569280
63.204638	1838.831440	20.574298
63.145809	1835.448024	20.579315
63.480137	1829.418253	20.584333
63.431281	1830.663117	20.589351
63.511331	1834.393643	20.594368
63.564299	1821.764592	20.599386
63.610247	1833.860683	20.604403
63.602628	1826.148692	20.609421
63.198202	1810.643615	20.614439
63.313868	1824.350955	20.619456
63.508279	1815.632114	20.624474
63.393699	1830.145594	20.629491
63.624684	1828.847068	20.634509
63.953022	1825.396683	20.639527
64.093956	1828.959869	20.644544
63.853393	1821.890326	20.649562
63.678471	1831.852855	20.654579
63.520772	1830.236507	20.659597
63.781844	1829.245710	20.664615
64.192102	1847.240091	20.669632
63.814435	1839.122139	20.674650
63.824400	1844.324873	20.679667
63.890088	1846.646923	20.684685
64.160675	1848.210991	20.689703
64.288480	1863.500769	20.694720
64.329418	1870.443925	20.699738
64.644222	1869.914952	20.704755
64.482120	1873.683425	20.709773
64.634497	1868.894052	20.714791
64.518666	1876.290988	20.719808
64.485177	1868.172752	20.724826
65.038825	1881.915663	20.729843
64.916030	1895.761411	20.734861
65.511138	1895.614581	20.739879
65.190032	1904.091483	20.744896
65.476639	1894.348237	20.749914
65.309546	1897.199101	20.754931
65.406516	1896.155111	20.759949
65.631960	1895.472869	20.764967
65.469607	1891.193577	20.769984
65.558654	1897.021449	20.775002
65.469219	1895.220819	20.780019
65.652854	1892.459010	20.785037
65.799091	1890.974929	20.790055
65.605539	1900.154570	20.795072
65.567209	1891.033472	20.800090
65.638039	1899.313257	20.805107
66.040284	1902.355805	20.810125
66.568457	1906.577906	20.815143
66.222810	1903.864303	20.820160
66.631381	1901.095655	20.825178
66.450831	1887.474286	20.830195
66.085038	1883.166906	20.835213
66.694484	1887.691869	20.840231
66.017184	1899.241714	20.845248
66.280181	1907.229447	20.850266
66.730023	1907.190589	20.855283
66.761954	1913.769077	20.860301
66.791310	1906.477319	20.865319
66.637567	1909.553324	20.870336
66.785168	1901.498225	20.875354
66.503515	1899.879199	20.880371
66.477134	1909.600733	20.885389
67.322864	1917.926389	20.890407
66.996825	1933.697614	20.895424
67.291461	1934.188034	20.900442
67.140363	1940.094573	20.905459
67.178424	1930.781594	20.910477
67.402455	1935.278585	20.915495
67.218654	1936.279494	20.920512
67.523889	1927.328627	20.925530
67.382173	1926.009586	20.930547
67.441607	1933.148698	20.935565
67.966657	1929.733750	20.940583
67.587356	1935.552956	20.945600
67.944457	1936.566956	20.950618
67.906376	1937.844855	20.955635
68.164544	1945.877546	20.960653
68.532025	1936.604476	20.965671
68.161105	1932.285263	20.970688
68.258456	1928.773212	20.975706
68.270207	1930.191636	20.980723
68.224499	1925.995053	20.985741
68.875502	1927.562647	20.990759
68.580012	1933.734819	20.995776
68.478594	1931.535249	21.000794
68.706236	1941.851361	21.005811
68.898053	1934.272189	21.010829
68.810243	1928.150723	21.015847
68.744623	1931.077218	21.020864
69.064279	1931.115565	21.025882
69.033117	1932.660640	21.030899
68.614565	1936.194733	21.035917
69.126808	1925.273643	21.040935
68.804503	1935.707474	21.045952
69.178458	1937.425780	21.050970
69.082292	1928.995422	21.055987
68.997090	1932.404699	21.061005
69.002003	1930.829140	21.066023
68.783456	1944.042944	21.071040
69.211718	1952.553952	21.076058
69.216994	1959.013547	21.081075
68.958420	1960.812020	21.086093
69.535838	1960.595374	21.091111
69.819439	1975.684102	21.096128
69.805797	1977.024451	21.101146
69.664250	1967.244098	21.106163
69.740464	1974.377441	21.111181
70.063543	1975.908048	21.116199
70.285691	1976.700181	21.121216
70.229012	1973.284841	21.126234
70.193996	1982.752132	21.131251
70.127501	1992.770350	21.136269
70.529647	1990.899005	21.141287
70.378004	1999.387273	21.146304
70.337929	1995.035146	21.151322
70.724705	2000.396655	21.156339
70.623246	2001.267893	21.161357
70.920139	1993.410284	21.166375
70.631291	1995.055702	21.171392
70.591435	1997.959235	21.176410
71.123971	1998.396605	21.181427
70.827297	2012.487450	21.186445
71.349944	2010.262685	21.191463
71.554373	2017.429609	21.196480
71.646634	2014.483268	21.201498
71.398534	2017.125919	21.206515
71.042524	2009.474745	21.211533
71.656383	2008.198277	21.216551
71.705669	2016.187982	21.221568
71.852945	2011.781249	21.226586
71.957757	2012.370845	21.231603
71.803268	2012.442450	21.236621
71.976684	2008.116836	21.241639
72.153861	2014.435902	21.246656
72.387306	2013.581978	21.251674
72.509198	2008.222948	21.256691
72.077793	2010.518751	21.261709
72.508958	2005.543642	21.266727
72.131110	2005.233646	21.271744
72.252837	2013.884234	21.276762
72.578793	2004.967954	21.281779
71.955587	2005.744199	21.286797
72.117405	2007.943903	21.291815
72.102677	2021.501399	21.296832
72.607558	2028.315120	21.301850
72.707477	2019.885559	21.306867
72.475796	2035.635777	21.311885
72.513449	2024.148310	21.316903
72.553778	2034.878858	21.321920
72.898907	2047.243822	21.326938
73.250518	2055.624867	21.331955
73.278079	2060.474587	21.336973
73.693397	2048.729104	21.341991
73.658878	2052.925782	21.347008
73.618251	2050.530468	21.352026
73.679417	2041.387393	21.357043
73.492989	2057.673378	21.362061
73.644684	2054.903923	21.367079
73.333838	2057.793114	21.372096
73.667409	2052.457715	21.377114
73.646141	2047.891175	21.382131
73.748532	2051.403636	21.387149
73.902189	2044.496319	21.392167
73.958159	2052.582830	21.397184
73.847329	2057.659374	21.402202
74.119007	2067.327984	21.407219
73.972551	2067.360459	21.412237
74.364815	2082.277607	21.417255
74.281853	2073.507416	21.422272
74.378724	2075.449042	21.427290
74.626012	2084.102083	21.432307
74.424247	2090.240688	21.437325
74.561519	2089.603814	21.442343
74.694403	2092.827462	21.447360
74.760451	2097.428148	21.452378
74.711357	2098.717252	21.457395
75.050205	2095.656519	21.462413
74.865223	2097.935817	21.467431
74.835798	2096.431900	21.472448
74.918310	2114.054990	21.477466
75.358093	2115.579950	21.482483
75.425667	2126.107453	21.487501
75.233074	2118.601055	21.492519
75.564497	2123.125453	21.497536
75.681226	2122.327683	21.502554
75.803990	2113.092863	21.507571
76.021314	2115.851973	21.512589
75.645981	2114.771506	21.517607
75.985320	2113.509637	21.522624
76.114759	2125.548660	21.527642
76.182254	2130.676187	21.532659
76.080285	2141.965620	21.537677
75.883205	2137.663305	21.542695
76.609831	2131.445730	21.547712
76.438491	2142.130604	21.552730
76.720435	2132.555231	21.557747
76.577236	2135.045754	21.562765
76.505071	2136.524683	21.567783
76.728725	2130.471123	21.572800
76.881829	2132.154617	21.577818
76.800904	2131.491962	21.582835
76.757648	2133.070510	21.587853
77.076678	2122.419432	21.592871
77.285753	2130.137982	21.597888
77.145197	2136.317509	21.602906
77.405788	2145.514492	21.607923
77.337334	2156.669287	21.612941
77.338400	2158.300858	21.617959
77.467627	2152.170560	21.622976
77.163586	2160.458701	21.627994
77.453025	2150.645441	21.633011
77.557258	2151.759036	21.638029
77.738265	2151.923257	21.643047
77.669687	2154.563051	21.648064
77.467841	2159.360370	21.653082
77.822840	2161.835965	21.658099
77.443597	2169.425781	21.663117
77.697434	2170.544343	21.668135
77.754063	2180.735896	21.673152
77.848142	2183.135598	21.678170
78.412114	2189.346786	21.683187
78.146971	2205.326475	21.688205
78.538390	2205.066379	21.693223
78.656544	2205.268852	21.698240
78.709778	2211.351766	21.703258
79.007520	2202.673358	21.708275
79.021501	2207.755638	21.713293
78.961211	2199.802409	21.718311
78.939063	2197.208504	21.723328
78.686730	2199.536240	21.728346
78.743998	2183.870133	21.733363
79.018635	2200.459582	21.738381
78.998726	2210.057179	21.743399
79.379615	2226.800433	21.748416
78.967228	2220.095351	21.753434
79.499224	2220.163553	21.758451
79.509770	2219.505500	21.763469
79.738440	2230.784217	21.768487
79.789470	2242.769325	21.773504
79.683536	2252.582411	21.778522
79.983723	2238.591943	21.783539
79.937973	2249.860012	21.788557
80.206090	2246.150718	21.793575
80.110898	2245.591288	21.798592
80.098970	2246.281239	21.803610
80.094955	2240.761971	21.808627
80.101749	2248.035697	21.813645
80.271333	2252.030017	21.818663
80.686578	2254.780232	21.823680
80.667300	2252.217430	21.828698
80.535014	2257.240583	21.833715
80.905207	2261.184538	21.838733
80.704470	2259.697980	21.843751
81.122700	2254.128333	21.848768
80.605025	2262.216443	21.853786
81.028020	2271.482729	21.858803
80.966779	2279.537209	21.863821
81.305422	2280.967567	21.868839
81.336524	2272.753813	21.873856
81.017705	2281.091667	21.878874
81.362102	2269.518111	21.883891
81.644662	2283.306961	21.888909
81.420400	2292.961868	21.893927
81.814075	2291.836654	21.898944
81.845084	2296.417631	21.903962
81.740482	2294.373164	21.908979
81.952653	2292.705136	21.913997
81.888360	2300.876879	21.919015
82.258368	2298.142617	21.924032
82.080758	2304.258574	21.929050
82.440687	2302.662078	21.934067
82.583730	2304.388194	21.939085
82.563470	2311.694589	21.944103
82.967186	2313.149472	21.949120
83.166797	2318.221637	21.954138
83.051963	2306.716850	21.959155
83.265823	2298.894210	21.964173
82.731650	2301.067282	21.969191
83.086946	2293.137271	21.974208
83.215573	2299.116877	21.979226
82.967503	2305.515295	21.984243
83.164047	2298.983047	21.989261
83.166083	2308.719283	21.994279
83.598297	2309.175536	21.999296
83.468278	2312.011187	22.004314
83.230690	2300.011196	22.009331
83.539848	2292.454519	22.014349
83.405019	2301.489452	22.019367
83.769164	2304.932550	22.024384
83.831314	2317.335724	22.029402
83.902688	2323.261186	22.034419
83.817553	2312.203062	22.039437
84.090879	2322.452271	22.044455
84.138529	2314.056010	22.049472
83.928321	2319.962466	22.054490
84.428914	2317.034158	22.059507
84.554296	2324.374551	22.064525
84.485891	2337.350507	22.069543
84.514309	2339.848889	22.074560
84.781689	2343.610137	22.079578
85.056829	2339.760856	22.084595
85.288575	2339.342722	22.089613
84.751568	2335.418692	22.094631
85.112758	2333.234966	22.099648
85.144569	2330.443223	22.104666
85.049059	2331.370354	22.109683
85.159741	2333.486585	22.114701
85.315180	2348.895535	22.119719
85.686706	2358.315110	22.124736
85.525239	2357.784997	22.129754
85.513732	2357.632212	22.134771
85.794721	2361.751126	22.139789
85.895239	2358.121720	22.144807
85.949495	2352.116719	22.149824
85.743357	2361.421653	22.154842
86.033559	2351.816465	22.159859
86.057113	2357.203428	22.164877
86.200968	2372.270201	22.169895
86.725292	2380.883139	22.174912
86.864311	2382.325844	22.179930
86.655247	2385.296979	22.184947
86.607839	2389.833457	22.189965
86.584451	2383.733302	22.194983
86.433334	2386.013643	22.200000
86.490385	2387.885795	22.205018
86.568449	2388.126112	22.210035
86.826267	2395.843452	22.215053
86.847093	2402.411235	22.220071
87.076208	2405.550429	22.225088
87.106067	2414.572242	22.230106
86.900146	2413.821853	22.235123
87.527958	2420.007339	22.240141
87.606415	2427.585521	22.245159
87.994376	2427.654199	22.250176
87.619493	2440.375261	22.255194
87.801791	2429.855887	22.260211
87.843292	2433.974466	22.265229
87.609147	2432.388976	22.270247
87.862329	2432.494550	22.275264
87.968183	2448.545731	22.280282
88.176116	2449.381142	22.285299
88.569472	2454.050571	22.290317
88.611776	2453.999819	22.295335
88.647214	2452.504647	22.300352
88.493385	2447.381206	22.305370
88.704913	2454.493540	22.310387
88.735357	2444.818536	22.315405
88.550328	2449.089385	22.320423
88.850774	2445.507541	22.325440
89.077072	2466.469697	22.330458
89.110838	2468.531716	22.335475
89.128568	2467.399113	22.340493
88.935145	2480.975483	22.345511
89.042831	2471.348329	22.350528
88.947259	2474.320634	22.355546
89.227028	2474.690312	22.360563
89.678834	2476.387007	22.365581
89.940627	2490.696873	22.370599
90.113932	2490.259487	22.375616
89.897199	2491.461263	22.380634
89.705502	2497.096607	22.385651
89.869847	2481.022108	22.390669
89.925230	2494.354361	22.395687
89.821877	2487.878498	22.400704
90.180099	2498.916159	22.405722
90.492535	2503.206922	22.410739
90.580798	2518.749631	22.415757
90.789193	2526.146535	22.420775
90.643107	2520.283329	22.425792
90.422228	2520.371649	22.430810
90.433838	2524.854729	22.435827
90.892368	2518.666402	22.440845
91.158284	2540.550335	22.445863
91.195111	2528.582945	22.450880
91.285193	2543.478387	22.455898
91.152823	2538.610360	22.460915
91.773158	2536.692152	22.465933
91.503867	2535.497205	22.470951
91.419188	2532.496441	22.475968
91.868449	2533.095212	22.480986
91.904141	2548.191702	22.486003
92.035707	2547.877631	22.491021
92.179422	2545.494399	22.496039
92.330778	2540.865970	22.501056
92.295021	2544.327582	22.506074
92.267363	2551.467960	22.511091
92.808847	2544.389226	22.516109
92.366528	2545.335986	22.521127
92.681868	2553.871285	22.526144
92.727345	2539.781620	22.531162
92.674260	2549.684428	22.536179
92.591797	2540.326893	22.541197
92.791526	2544.755256	22.546215
93.021166	2555.409114	22.551232
93.420385	2559.916690	22.556250
93.217013	2557.474215	22.561267
93.350684	2558.081401	22.566285
93.082300	2561.478466	22.571303
93.124398	2564.618583	22.576320
93.439410	2556.928322	22.581338
93.183326	2563.725758	22.586355
93.740483	2572.115872	22.591373
93.767309	2584.426926	22.596391
93.844962	2576.092120	22.601408
94.039888	2582.648473	22.606426
94.313103	2587.377790	22.611443
94.225689	2581.723145	22.616461
93.830746	2584.095364	22.621479
94.230899	2596.357405	22.626496
94.530587	2601.789551	22.631514
94.529580	2606.284096	22.636531
94.778910	2600.434661	22.641549
94.807078	2606.641570	22.646567
94.678914	2608.315521	22.651584
94.665644	2605.915846	22.656602
94.530652	2622.102756	22.661619
95.024237	2617.856236	22.666637
95.211223	2628.327452	22.671655
95.268934	2626.106022	22.676672
95.405982	2624.875812	22.681690
94.992407	2628.172547	22.686707
95.443030	2635.042346	22.691725
95.487101	2652.192254	22.696743
95.723845	2651.423000	22.701760
95.676871	2655.729079	22.706778
95.443399	2662.396764	22.711795
95.923065	2656.495443	22.716813
96.181643	2669.770742	22.721831
96.313966	2673.505879	22.726848
96.263193	2669.805429	22.731866
96.330055	2670.442022	22.736883
96.522368	2671.115772	22.741901
95.931206	2679.894151	22.746919
96.538366	2685.120343	22.751936
96.708527	2696.541078	22.756954
96.882137	2701.061944	22.761971
96.902524	2700.815787	22.766989
96.968055	2701.124351	22.772007
97.075052	2695.663298	22.777024
97.315104	2703.244684	22.782042
97.377521	2712.987459	22.787059
97.781965	2710.055217	22.792077
97.964114	2714.599998	22.797095
98.138066	2717.798389	22.802112
98.057641	2713.338788	22.807130
98.136950	2720.077424	22.812147
98.169681	2709.249925	22.817165
97.993423	2712.847202	22.822183
98.272678	2719.614480	22.827200
98.353129	2705.686481	22.832218
98.544465	2700.196432	22.837235
98.304407	2701.218820	22.842253
98.271285	2717.790686	22.847271
98.226138	2731.265110	22.852288
98.727234	2731.893641	22.857306
98.636903	2732.709516	22.862323
98.530477	2727.455479	22.867341
98.902063	2753.050530	22.872359
98.999874	2760.193426	22.877376
99.187951	2758.869997	22.882394
98.937761	2752.795782	22.887411
99.520629	2769.646770	22.892429
99.737322	2780.346977	22.897447
99.784278	2781.684204	22.902464
100.130643	2779.281817	22.907482
99.990924	2773.707898	22.912499
99.955216	2773.647273	22.917517
100.044297	2770.461438	22.922535
100.237250	2776.061855	22.927552
100.349070	2768.652674	22.932570
100.248546	2775.959209	22.937587
100.623448	2775.906846	22.942605
100.980167	2789.349915	22.947623
100.986442	2800.442902	22.952640
101.149480	2790.418697	22.957658
100.878294	2790.208752	22.962675
100.710289	2795.461737	22.967693
101.007421	2797.050138	22.972711
101.019993	2789.564969	22.977728
101.094154	2788.432974	22.982746
101.300067	2785.001589	22.987763
101.511476	2794.304452	22.992781
101.483511	2813.384747	22.997799
101.515272	2807.064346	23.002816
101.895325	2801.844535	23.007834
101.998781	2804.539532	23.012851
101.950957	2809.899939	23.017869
101.812189	2805.200119	23.022887
102.023421	2804.810439	23.027904
102.291919	2804.462286	23.032922
102.378093	2809.871135	23.037939
102.657152	2820.037671	23.042957
102.637969	2827.539790	23.047975
102.465794	2838.992156	23.052992
103.030925	2820.588434	23.058010
103.149430	2823.110642	23.063027
102.906986	2814.788002	23.068045
103.257846	2818.795078	23.073063
102.731477	2824.060031	23.078080
103.247556	2824.458975	23.083098
103.257645	2839.038953	23.088115
103.525703	2838.719274	23.093133
103.924716	2851.590809	23.098151
103.937515	2840.870507	23.103168
104.214487	2824.863273	23.108186
104.069472	2839.707421	23.113203
103.940753	2832.433741	23.118221
104.111047	2830.560762	23.123239
104.201654	2833.734358	23.128256
104.511972	2828.626463	23.133274
104.346041	2835.924332	23.138291
104.457451	2853.281658	23.143309
104.825601	2850.718040	23.148327
104.817996	2855.797573	23.153344
104.822321	2851.551904	23.158362
104.905437	2867.569148	23.163379
105.245707	2857.495046	23.168397
105.221031	2855.889324	23.173415
105.056094	2865.260655	23.178432
105.272051	2866.116923	23.183450
105.277418	2871.970847	23.188467
105.175266	2874.193078	23.193485
105.483741	2874.271057	23.198503
105.432507	2876.617871	23.203520
105.957609	2883.993710	23.208538
105.732372	2891.695416	23.213555
106.234008	2898.765632	23.218573
106.232325	2895.420405	23.223591
105.830975	2897.733701	23.228608
106.203759	2905.357502	23.233626
106.641258	2912.665017	23.238643
106.712688	2917.426035	23.243661
106.750865	2917.726264	23.248679
106.528704	2917.136206	23.253696
106.998279	2913.303684	23.258714
106.869052	2926.494747	23.263731
107.100149	2934.055540	23.268749
107.500669	2934.523091	23.273767
107.611417	2943.800772	23.278784
107.832531	2934.136663	23.283802
107.615390	2941.673000	23.288819
107.603195	2933.487822	23.293837
107.862066	2930.818222	23.298855
107.683153	2932.225566	23.303872
108.261927	2934.019193	23.308890
108.179314	2954.875664	23.313907
108.173545	2950.296997	23.318925
108.866470	2954.010643	23.323943
108.566789	2949.847297	23.328960
108.514609	2950.448896	23.333978
108.838336	2951.670183	23.338995
108.719643	2947.424827	23.344013
108.792696	2949.370280	23.349031
108.573977	2947.662390	23.354048
109.139497	2956.944578	23.359066
109.237549	2971.952750	23.364083
109.141964	2976.638952	23.369101
109.298917	2976.021058	23.374119
108.894864	2976.245387	23.379136
109.207145	2970.433314	23.384154
109.713573	2983.114525	23.389171
109.728224	3004.176748	23.394189
109.700972	2990.833518	23.399207
109.876516	2996.856506	23.404224
109.965925	2994.734219	23.409242
109.965714	2997.423393	23.414259
110.086975	3007.696819	23.419277
110.403236	3014.237476	23.424295
110.398491	3021.718477	23.429312
110.815551	3018.620087	23.434330
110.809788	3027.281669	23.439347
110.838772	3035.069855	23.444365
110.842587	3040.393835	23.449383
110.428432	3042.646030	23.454400
110.431267	3048.648750	23.459418
110.896592	3065.306967	23.464435
110.723327	3080.420860	23.469453
111.917046	3083.402739	23.474471
111.782531	3097.330152	23.479488
112.182938	3098.043910	23.484506
112.483017	3089.071183	23.489523
111.898277	3100.083356	23.494541
112.560204	3092.928730	23.499559
112.350242	3101.701244	23.504576
112.507859	3095.484116	23.509594
112.370191	3084.720962	23.514611
112.163157	3092.340996	23.519629
112.605692	3109.697192	23.524647
112.662261	3111.051875	23.529664
112.593056	3117.485682	23.534682
112.679048	3120.704238	23.539699
113.070990	3140.915300	23.544717
113.396414	3133.415693	23.549735
113.370996	3138.207724	23.554752
113.810628	3135.295152	23.559770
113.669231	3138.186370	23.564787
113.717311	3148.184125	23.569805
113.680758	3138.478214	23.574823
114.178065	3153.180957	23.579840
114.099820	3145.842429	23.584858
114.317946	3163.117054	23.589875
114.109837	3155.353841	23.594893
114.515132	3157.629167	23.599911
114.759176	3160.264317	23.604928
114.474370	3153.693549	23.609946
114.998828	3165.829194	23.614963
114.710145	3177.912336	23.619981
115.154856	3172.543416	23.624999
114.857448	3181.127670	23.630016
114.967627	3178.301425	23.635034
115.181319	3175.373745	23.640051
114.991344	3199.103705	23.645069
115.735020	3194.783153	23.650087
115.741885	3196.786346	23.655104
115.603878	3194.178886	23.660122
115.902689	3199.936444	23.665139
116.078494	3212.931583	23.670157
116.343564	3215.415104	23.675175
116.284886	3223.879915	23.680192
116.284656	3217.201414	23.685210
116.740858	3214.510327	23.690227
116.133472	3223.332539	23.695245
116.804451	3207.935516	23.700263
116.421486	3220.248081	23.705280
116.953069	3226.695113	23.710298
117.348507	3235.230815	23.715315
117.081655	3242.550971	23.720333
117.240802	3231.359323	23.725351
117.237774	3242.034260	23.730368
117.484915	3247.673678	23.735386
117.451220	3235.672680	23.740403
117.275810	3254.637667	23.745421
117.702236	3255.924948	23.750439
117.645521	3258.323170	23.755456
117.873085	3263.785754	23.760474
118.439414	3267.658176	23.765491
118.350508	3289.118861	23.770509
118.463022	3286.756202	23.775527
118.488079	3284.871213	23.780544
118.641331	3288.890418	23.785562
118.947092	3294.012511	23.790579
118.864889	3295.442606	23.795597
119.070613	3288.577157	23.800615
119.305779	3304.918155	23.805632
119.532795	3318.107347	23.810650
119.545837	3306.903824	23.815667
119.617318	3315.420879	23.820685
119.772977	3301.802576	23.825703
119.896793	3303.771676	23.830720
119.633332	3305.586826	23.835738
120.197363	3306.369646	23.840755
120.348098	3314.785910	23.845773
120.087305	3320.028334	23.850791
120.300830	3328.134923	23.855808
120.156352	3322.855110	23.860826
119.985564	3327.442716	23.865843
120.350274	3345.714021	23.870861
120.558401	3341.316370	23.875879
120.821728	3347.726567	23.880896
120.664777	3359.056940	23.885914
121.032559	3371.185708	23.890931
121.239012	3371.207080	23.895949
121.425083	3364.319431	23.900967
121.621125	3375.114759	23.905984
121.791393	3394.489707	23.911002
121.701140	3388.500688	23.916019
121.806668	3402.251853	23.921037
122.276736	3391.948806	23.926055
122.071755	3392.877360	23.931072
122.084002	3400.150698	23.936090
122.305386	3396.606305	23.941107
122.392789	3405.562786	23.946125
122.507887	3420.909538	23.951143
122.415618	3422.372783	23.956160
122.436085	3430.522289	23.961178
123.177908	3439.369948	23.966195
123.000964	3445.789187	23.971213
123.374689	3438.774266	23.976231
123.316689	3443.953392	23.981248
123.453264	3449.269319	23.986266
123.596053	3459.047250	23.991283
123.935119	3458.287184	23.996301
123.494185	3451.403045	24.001319
124.228363	3449.896165	24.006336
123.957039	3462.721658	24.011354
124.459981	3474.759883	24.016371
124.268049	3470.961444	24.021389
124.756731	3479.454247	24.026407
124.579446	3475.861828	24.031424
124.621772	3479.844797	24.036442
124.950001	3476.820217	24.041459
124.478903	3480.448056	24.046477
124.981506	3489.746692	24.051495
125.238862	3496.568195	24.056512
125.358317	3499.570105	24.061530
125.409921	3496.326889	24.066547
125.372771	3501.278668	24.071565
125.749366	3501.358605	24.076583
125.943698	3519.003428	24.081600
125.953367	3519.677420	24.086618
126.389453	3520.922176	24.091635
126.072490	3527.963076	24.096653
126.078645	3513.859872	24.101671
126.226434	3520.480766	24.106688
126.528864	3545.544899	24.111706
126.714082	3545.932572	24.116723
126.616271	3552.702426	24.121741
126.973298	3549.809043	24.126759
127.106637	3544.286794	24.131776
127.335925	3557.011830	24.136794
127.602467	3561.928673	24.141811
127.758350	3565.404644	24.146829
127.482307	3562.004432	24.151847
127.554321	3558.347689	24.156864
127.487763	3567.385184	24.161882
127.781788	3571.638058	24.166899
127.785194	3580.775069	24.171917
128.067349	3580.977117	24.176935
128.080278	3584.964715	24.181952
128.286956	3609.134922	24.186970
128.657784	3607.719675	24.191987
128.655891	3608.856302	24.197005
128.651753	3613.840816	24.202023
129.142901	3620.417422	24.207040
129.060091	3626.256999	24.212058
129.547920	3623.867059	24.217075
129.543695	3628.813716	24.222093
129.375612	3634.815001	24.227111
129.723372	3638.920595	24.232128
129.451582	3653.946244	24.237146
130.119908	3647.582634	24.242163
130.346942	3653.064358	24.247181
130.350817	3652.498831	24.252199
130.361896	3640.304327	24.257216
130.420355	3648.365915	24.262234
130.873534	3657.132651	24.267251
130.874593	3674.599590	24.272269
131.015304	3670.799496	24.277287
131.067147	3675.203963	24.282304
130.772512	3676.910405	24.287322
131.063231	3672.607050	24.292339
131.287596	3686.207248	24.297357
131.472295	3690.849723	24.302375
131.714685	3688.498228	24.307392
131.240337	3698.808546	24.312410
131.669743	3700.609874	24.317427
132.255719	3706.960183	24.322445
132.195160	3715.542302	24.327463
132.631747	3717.310944	24.332480
132.412955	3717.616726	24.337498
132.629268	3713.334486	24.342515
132.575137	3717.184272	24.347533
132.803376	3732.876542	24.352551
132.984342	3726.601883	24.357568
132.808730	3737.821787	24.362586
133.053321	3735.987578	24.367603
133.217989	3737.937702	24.372621
133.385885	3746.045315	24.377639
133.529679	3750.833093	24.382656
133.817740	3749.929502	24.387674
133.479233	3753.214676	24.392691
133.789010	3757.622943	24.397709
133.515692	3766.285764	24.402727
134.440545	3774.738781	24.407744
134.596817	3786.212885	24.412762
134.505735	3777.594640	24.417779
134.542247	3774.394770	24.422797
134.470780	3779.992738	24.427815
134.828916	3790.090621	24.432832
134.685431	3812.520004	24.437850
134.978842	3801.774107	24.442867
135.182479	3810.876710	24.447885
135.249644	3829.106744	24.452903
135.492711	3825.839785	24.457920
135.783860	3832.447803	24.462938
136.031412	3827.052767	24.467955
135.796696	3840.387275	24.472973
136.003769	3846.894842	24.477991
136.238325	3849.105473	24.483008
136.124231	3856.364068	24.488026
136.257840	3859.294382	24.493043
136.696394	3867.621624	24.498061
136.773022	3869.494020	24.503079
137.079851	3880.663682	24.508096
136.964178	3878.036842	24.513114
137.417390	3878.433039	24.518131
137.609791	3900.178639	24.523149
137.324407	3903.673306	24.528167
137.501289	3900.656586	24.533184
137.654806	3897.978101	24.538202
138.025648	3895.716927	24.543219
138.203098	3899.902921	24.548237
138.124486	3917.010125	24.553255
138.849385	3911.511873	24.558272
138.503014	3922.597669	24.563290
138.700343	3906.911280	24.568307
138.675545	3913.878149	24.573325
138.439199	3930.678660	24.578343
138.732496	3927.227058	24.583360
138.990094	3936.595874	24.588378
139.061339	3942.395635	24.593395
139.231659	3957.850977	24.598413
139.400811	3954.049525	24.603431
139.830956	3959.114446	24.608448
139.799051	3972.385714	24.613466
140.106823	3980.181133	24.618483
140.171132	3977.832249	24.623501
140.129249	3984.760789	24.628519
140.822584	3984.254525	24.633536
140.645815	3986.015126	24.638554
141.114718	3991.604255	24.643571
140.962153	4004.177953	24.648589
141.239839	4014.638923	24.653607
141.459554	4007.206020	24.658624
141.228188	4013.400414	24.663642
141.463007	4003.339042	24.668659
141.492782	3995.443506	24.673677
141.417879	4016.246335	24.678695
141.735194	4018.431397	24.683712
141.862826	4024.342293	24.688730
141.995286	4026.799357	24.693747
142.059586	4025.750896	24.698765
142.482088	4047.182863	24.703783
142.500340	4054.209325	24.708800
142.164687	4059.239586	24.713818
142.226204	4057.771760	24.718835
142.353741	4064.086701	24.723853
142.659364	4073.624821	24.728871
143.045751	4072.576399	24.733888
142.852849	4089.922618	24.738906
143.459506	4093.889909	24.743923
143.679986	4099.470645	24.748941
143.553586	4101.829393	24.753959
144.040352	4113.826391	24.758976
144.167178	4128.408059	24.763994
143.915157	4128.226655	24.769011
144.153370	4122.930843	24.774029
144.412752	4137.510690	24.779047
144.508121	4135.687194	24.784064
144.721809	4147.799594	24.789082
144.742291	4155.283424	24.794099
145.212481	4142.284370	24.799117
145.117784	4158.415838	24.804135
145.320225	4173.781110	24.809152
145.334070	4179.574158	24.814170
145.300471	4172.285034	24.819187
145.737000	4171.878971	24.824205
145.696126	4186.622685	24.829223
146.288946	4198.186479	24.834240
146.335260	4203.608304	24.839258
146.246031	4201.532802	24.844275
147.006276	4214.989473	24.849293
147.060150	4213.630150	24.854311
146.789797	4224.022436	24.859328
147.056896	4212.914275	24.864346
147.294168	4208.224616	24.869363
147.374289	4209.320024	24.874381
147.457493	4231.187290	24.879399
147.554391	4230.799714	24.884416
147.615001	4232.646250	24.889434
148.110662	4233.499799	24.894451
148.074835	4232.163997	24.899469
148.161748	4241.483957	24.904487
147.830617	4252.201422	24.909504
148.236190	4261.121107	24.914522
148.350877	4258.508625	24.919539
148.469194	4263.818183	24.924557
148.542908	4274.093466	24.929575
148.954751	4273.470319	24.934592
148.993243	4284.915845	24.939610
149.143885	4298.909982	24.944627
149.228789	4297.924562	24.949645
149.304524	4301.378512	24.954663
149.658722	4307.863196	24.959680
149.981764	4314.870417	24.964698
150.012779	4313.691428	24.969715
150.395894	4320.499855	24.974733
150.254093	4341.676526	24.979751
150.628229	4338.436289	24.984768
150.842587	4338.317544	24.989786
150.772835	4341.756417	24.994803
150.845064	4351.583763	24.999821
150.989168	4358.129787	25.004839
151.417151	4349.824505	25.009856
151.441293	4358.330530	25.014874
151.608151	4363.414718	25.019891
151.731881	4385.054871	25.024909
151.815346	4385.878311	25.029927
152.086827	4381.628307	25.034944
152.475555	4388.123392	25.039962
152.442949	4402.578750	25.044979
152.826369	4409.002077	25.049997
152.924543	4407.777839	25.055015
152.746011	4404.703085	25.060032
153.318145	4407.864649	25.065050
152.910073	4395.198707	25.070067
153.155700	4397.761195	25.075085
153.246409	4408.687275	25.080103
153.603321	4410.613667	25.085120
153.839310	4427.533182	25.090138
153.626707	4428.671306	25.095155
153.672391	4423.383474	25.100173
153.552665	4443.597246	25.105191
153.801564	4443.463619	25.110208
154.126241	4455.341042	25.115226
154.328949	4473.398980	25.120243
154.816857	4475.898270	25.125261
154.503712	4479.700415	25.130279
154.536930	4489.297213	25.135296
154.867785	4504.642648	25.140314
155.088806	4508.954529	25.145331
155.250204	4525.819536	25.150349
155.449191	4532.934658	25.155367
155.957524	4539.489972	25.160384
156.379264	4545.831590	25.165402
155.922445	4552.819039	25.170419
156.202227	4552.077688	25.175437
156.374763	4562.277679	25.180455
156.429721	4570.731629	25.185472
156.791872	4581.220729	25.190490
156.666736	4585.094449	25.195507
157.202659	4576.674302	25.200525
157.150008	4595.296342	25.205543
157.429114	4600.400890	25.210560
157.721488	4595.004918	25.215578
157.684292	4609.660017	25.220595
158.293943	4607.948451	25.225613
158.256698	4617.995106	25.230631
158.587016	4620.102450	25.235648
158.623813	4615.699769	25.240666
158.774924	4613.378239	25.245683
159.131938	4615.976968	25.250701
159.333135	4610.768882	25.255719
159.111139	4608.013394	25.260736
159.341609	4616.102125	25.265754
159.558861	4628.391051	25.270771
159.558706	4628.829887	25.275789
159.567653	4637.152191	25.280807
159.942645	4640.786590	25.285824
160.216090	4632.205524	25.290842
160.161212	4651.004732	25.295859
160.383148	4651.787553	25.300877
160.444665	4652.683888	25.305895
160.472602	4654.242032	25.310912
160.599122	4662.189245	25.315930
160.779469	4674.310377	25.320947
161.379240	4673.989208	25.325965
161.607107	4680.661113	25.330983
161.552551	4673.586556	25.336000
161.561248	4682.193003	25.341018
161.557110	4700.220442	25.346035
161.674761	4704.097186	25.351053
162.071876	4716.096005	25.356071
162.255240	4721.329220	25.361088
162.241051	4723.323254	25.366106
162.301358	4734.765646	25.371123
162.515502	4739.163885	25.376141
162.370099	4739.732800	25.381159
162.410841	4748.823516	25.386176
162.770804	4756.443800	25.391194
163.180608	4784.548324	25.396211
163.671914	4770.888962	25.401229
163.587589	4775.239274	25.406247
163.754791	4786.286171	25.411264
163.916598	4791.232385	25.416282
163.909137	4801.151372	25.421299
164.445185	4793.589679	25.426317
164.464308	4799.306341	25.431335
164.452565	4810.520174	25.436352
164.555329	4823.007090	25.441370
164.564603	4827.680497	25.446387
164.783517	4838.368952	25.451405
164.941527	4843.211610	25.456423
165.413426	4843.784828	25.461440
165.237951	4854.459322	25.466458
165.580586	4863.174522	25.471475
165.848529	4870.102209	25.476493
165.713336	4883.387167	25.481511
165.782700	4899.383112	25.486528
166.388350	4894.821802	25.491546
166.589048	4909.228386	25.496563
166.938767	4908.485534	25.501581
167.178179	4912.608396	25.506599
167.173373	4920.639426	25.511616
167.334702	4915.428030	25.516634
167.388296	4932.815349	25.521651
167.759047	4938.334924	25.526669
168.413341	4927.588646	25.531687
168.405582	4929.764774	25.536704
168.695418	4927.554046	25.541722
168.775762	4931.001081	25.546739
168.650918	4927.646364	25.551757
168.723336	4923.638908	25.556775
168.797035	4934.388048	25.561792
169.629594	4938.108651	25.566810
169.368243	4945.614863	25.571827
169.645414	4942.437061	25.576845
169.642390	4948.400293	25.581863
169.627917	4952.244127	25.586880
169.942376	4963.230185	25.591898
170.075168	4965.273819	25.596915
170.189123	4969.283773	25.601933
170.435238	4977.329180	25.606951
170.128612	4979.375369	25.611968
170.899017	4981.896762	25.616986
170.821809	4993.818560	25.622003
170.816205	4989.760181	25.627021
171.453922	4996.150193	25.632039
171.032327	5016.866435	25.637056
171.688387	5008.168434	25.642074
171.752830	5027.596431	25.647091
171.685921	5028.970604	25.652109
172.168144	5041.429788	25.657127
172.311624	5030.441507	25.662144
172.538003	5035.412394	25.667162
172.360499	5050.986290	25.672180
172.753553	5053.402670	25.677197
172.892121	5054.589983	25.682215
172.593756	5064.055951	25.687232
172.829542	5071.594813	25.692250
173.352326	5087.832389	25.697268
173.371982	5094.836938	25.702285
173.643709	5102.130283	25.707303
173.586685	5109.604553	25.712320
174.408643	5114.254884	25.717338
174.031091	5132.192893	25.722356
174.417565	5124.682905	25.727373
174.887003	5120.174445	25.732391
174.576063	5123.777513	25.737408
175.199459	5134.244947	25.742426
175.316310	5138.027212	25.747444
175.332585	5139.820811	25.752461
175.500181	5144.968236	25.757479
175.571979	5146.696319	25.762496
175.612896	5147.958911	25.767514
175.343377	5159.169150	25.772532
175.932108	5162.631282	25.777549
176.046805	5169.655693	25.782567
176.219459	5180.938720	25.787584
176.961970	5186.267555	25.792602
176.748423	5197.153391	25.797620
176.927411	5209.884314	25.802637
177.292658	5219.820898	25.807655
177.265076	5214.597976	25.812672
177.315584	5222.768834	25.817690
177.665717	5237.916162	25.822708
177.600213	5239.681547	25.827725
178.415250	5248.158784	25.832743
178.446141	5265.840384	25.837760
178.794705	5262.746040	25.842778
179.093307	5265.060452	25.847796
178.857683	5259.791194	25.852813
179.124342	5259.275991	25.857831
178.761732	5277.675820	25.862848
179.560883	5285.429546	25.867866
179.241484	5293.105981	25.872884
179.637456	5308.959578	25.877901
180.159435	5304.177688	25.882919
179.780633	5317.535849	25.887936
180.261413	5317.741527	25.892954
180.813211	5340.142785	25.897972
180.504377	5337.804834	25.902989
181.088338	5333.944425	25.908007
181.121061	5350.315829	25.913024
181.499640	5360.335630	25.918042
181.657012	5360.923419	25.923060
181.156915	5358.331334	25.928077
181.854893	5356.962562	25.933095
181.812828	5380.492272	25.938112
182.436306	5383.784860	25.943130
182.133259	5387.828668	25.948148
182.590186	5390.418172	25.953165
182.771296	5398.489733	25.958183
182.848564	5414.942602	25.963200
182.692398	5406.213827	25.968218
183.219694	5416.260867	25.973236
183.522788	5429.064043	25.978253
183.657965	5433.629497	25.983271
183.600703	5430.668147	25.988288
184.082068	5437.849870	25.993306
184.623800	5454.103747	25.998324
184.270796	5451.346556	26.003341
184.625699	5444.576878	26.008359
184.601980	5452.797347	26.013376
184.926865	5462.866653	26.018394
185.192005	5471.392263	26.023412
185.215607	5476.710701	26.028429
185.617667	5481.483731	26.033447
185.647138	5499.655058	26.038464
185.572068	5499.805771	26.043482
185.799728	5505.666757	26.048500
185.866390	5511.685546	26.053517
185.936989	5523.518245	26.058535
186.259057	5515.917176	26.063552
186.036195	5548.620203	26.068570
186.350698	5548.665692	26.073588
186.670473	5572.385182	26.078605
186.978583	5568.324878	26.083623
187.080339	5582.425518	26.088640
187.284412	5596.544863	26.093658
187.365705	5601.958470	26.098676
187.335132	5607.847318	26.103693
188.221644	5613.314711	26.108711
187.964168	5628.204007	26.113728
188.266998	5634.280538	26.118746
188.539465	5642.704068	26.123764
188.162931	5656.838658	26.128781
189.049354	5664.203234	26.133799
188.996685	5676.219489	26.138816
189.355629	5676.996677	26.143834
189.646886	5685.051109	26.148852
189.886575	5697.018421	26.153869
190.153484	5694.962714	26.158887
190.427044	5692.650275	26.163904
190.652726	5709.323223	26.168922
191.161237	5715.496983	26.173940
191.023336	5715.774337	26.178957
191.287462	5705.814764	26.183975
191.186293	5719.022396	26.188992
191.261558	5722.596644	26.194010
191.655005	5734.997610	26.199028
191.663641	5736.461015	26.204045
191.811277	5727.880205	26.209063
192.120341	5753.366189	26.214080
192.076379	5756.305689	26.219098
192.478085	5754.118375	26.224116
192.601308	5786.025789	26.229133
193.011178	5772.428947	26.234151
193.219664	5780.515329	26.239168
193.108614	5803.646023	26.244186
193.688149	5796.099204	26.249204
193.575226	5809.930610	26.254221
193.982261	5814.841844	26.259239
194.328842	5823.468501	26.264256
194.255070	5827.643792	26.269274
194.707945	5821.073282	26.274292
194.938810	5837.227838	26.279309
194.986678	5842.561522	26.284327
195.042425	5844.326910	26.289344
195.152236	5847.245492	26.294362
195.535414	5865.232347	26.299380
195.868309	5873.649674	26.304397
196.026160	5863.678254	26.309415
195.809016	5871.878706	26.314432
196.216061	5897.949314	26.319450
196.532315	5892.602886	26.324468
196.641643	5908.893343	26.329485
197.050335	5913.709642	26.334503
196.954936	5927.134333	26.339520
197.270488	5922.981241	26.344538
197.492647	5933.884488	26.349556
197.477141	5942.571084	26.354573
197.676585	5947.363352	26.359591
198.149022	5960.282425	26.364608
197.869374	5980.140990	26.369626
198.072096	5976.453815	26.374644
198.313935	5990.343423	26.379661
198.877619	5994.213702	26.384679
198.768581	6005.828631	26.389696
199.136492	6022.498523	26.394714
199.177009	6024.572517	26.399732
199.500476	6023.843208	26.404749
199.568240	6034.511851	26.409767
199.921082	6052.023821	26.414784
199.901500	6057.314469	26.419802
200.822264	6056.841984	26.424820
200.416717	6082.547706	26.429837
200.695710	6086.295297	26.434855
200.928176	6080.870395	26.439872
200.903175	6095.714182	26.444890
201.171251	6097.130658	26.449908
201.172463	6109.164010	26.454925
201.375291	6120.244017	26.459943
201.839946	6123.081800	26.464960
201.921652	6128.110376	26.469978
202.186257	6137.968528	26.474996
202.159540	6153.462919	26.480013
202.346590	6165.732362	26.485031
202.771565	6170.943930	26.490048
202.827072	6183.887439	26.495066
203.393720	6186.346228	26.500084
203.600134	6197.744553	26.505101
203.872726	6196.338192	26.510119
204.393211	6211.784789	26.515136
204.036801	6230.522375	26.520154
204.221621	6215.388396	26.525172
204.616359	6238.951798	26.530189
204.733982	6253.416655	26.535207
205.243082	6255.496187	26.540224
205.407341	6251.117338	26.545242
205.309822	6254.873440	26.550260
205.622978	6276.069471	26.555277
206.040587	6266.726374	26.560295
205.979039	6285.370472	26.565312
206.569412	6296.004748	26.570330
206.532861	6298.659065	26.575348
206.224863	6313.812530	26.580365
206.424982	6321.979383	26.585383
206.765127	6326.629752	26.590400
207.244344	6355.761251	26.595418
207.733517	6352.581563	26.600436
207.766478	6362.498223	26.605453
207.755817	6375.395411	26.610471
208.362431	6377.084024	26.615488
208.213148	6383.417884	26.620506
208.668474	6388.479548	26.625524
208.896335	6400.411293	26.630541
208.692715	6396.077414	26.635559
208.849806	6412.670202	26.640576
209.487949	6427.018928	26.645594
209.684743	6424.948871	26.650612
209.522163	6442.046343	26.655629
209.758855	6449.364659	26.660647
210.221565	6456.133012	26.665664
210.398197	6471.074944	26.670682
210.770297	6474.921674	26.675700
210.940768	6484.649548	26.680717
211.425980	6488.554325	26.685735
211.383175	6497.725294	26.690752
211.625887	6494.505272	26.695770
211.765654	6493.779470	26.700788
211.869636	6505.168779	26.705805
212.082158	6510.997736	26.710823
212.373644	6518.667372	26.715840
212.413692	6532.377497	26.720858
212.648360	6525.998763	26.725876
212.901272	6534.248988	26.730893
213.037957	6543.754895	26.735911
213.451653	6551.680042	26.740928
213.226306	6573.039699	26.745946
213.648489	6569.125460	26.750964
213.816537	6593.757112	26.755981
214.156193	6603.688992	26.760999
214.396937	6609.330464	26.766016
214.312920	6611.525052	26.771034
214.596760	6633.635256	26.776052
214.981859	6637.167459	26.781069
215.008586	6635.600702	26.786087
215.640289	6648.328002	26.791104
215.999134	6668.437694	26.796122
215.888401	6656.478076	26.801140
215.905500	6663.900329	26.806157
215.984950	6688.426027	26.811175
216.200486	6690.163309	26.816192
215.699098	6710.931844	26.821210
216.619022	6712.934444	26.826228
216.897778	6725.331955	26.831245
216.944522	6733.567215	26.836263
217.780110	6744.911512	26.841280
218.022788	6763.164339	26.846298
218.144752	6755.919263	26.851316
218.348642	6770.686699	26.856333
218.567443	6778.090028	26.861351
218.940478	6779.029216	26.866368
218.930539	6785.777030	26.871386
219.426423	6804.738407	26.876404
219.651510	6797.647630	26.881421
219.501984	6805.519062	26.886439
220.031747	6815.115061	26.891456
220.103667	6827.968063	26.896474
220.175594	6823.054249	26.901492
220.399376	6845.098352	26.906509
220.687226	6853.860974	26.911527
220.983253	6856.324369	26.916544
220.933205	6881.902908	26.921562
221.173798	6887.651824	26.926580
221.576627	6889.969060	26.931597
221.654087	6902.224597	26.936615
221.854368	6912.026949	26.941632
222.061675	6918.257777	26.946650
222.213907	6924.699275	26.951668
222.715467	6936.818946	26.956685
222.758177	6950.772047	26.961703
223.103430	6969.861369	26.966720
223.075498	6978.585127	26.971738
223.569206	6982.671781	26.976756
223.991205	7005.906741	26.981773
224.332432	7008.243114	26.986791
224.496597	7002.374049	26.991808
224.584159	7028.221668	26.996826
224.746300	7025.759205	27.001844
225.281797	7042.312225	27.006861
225.252357	7054.906613	27.011879
225.639149	7050.603206	27.016896
225.556478	7058.009679	27.021914
226.171108	7070.730478	27.026932
226.295147	7079.023236	27.031949
226.213204	7075.134199	27.036967
227.006760	7083.571471	27.041984
227.072035	7095.390236	27.047002
227.101380	7081.103853	27.052020
227.515878	7096.258427	27.057037
227.800716	7115.774078	27.062055
228.034763	7107.251698	27.067072
228.163829	7118.968935	27.072090
228.047706	7111.997785	27.077108
228.539856	7132.914215	27.082125
228.643875	7133.980802	27.087143
228.923253	7142.173488	27.092160
228.990362	7150.538335	27.097178
229.585152	7165.532132	27.102196
229.472653	7175.693002	27.107213
229.744148	7175.912556	27.112231
230.270580	7179.608984	27.117248
230.043092	7191.094842	27.122266
230.353615	7204.807295	27.127284
230.771724	7201.632284	27.132301
230.966987	7222.131257	27.137319
231.029633	7211.403731	27.142336
230.757162	7230.716372	27.147354
231.138306	7230.672509	27.152372
230.886850	7252.444287	27.157389
231.555434	7271.300170	27.162407
231.672767	7275.474264	27.167424
232.002048	7293.385731	27.172442
232.427273	7306.145836	27.177460
232.628086	7312.766120	27.182477
232.356983	7340.248838	27.187495
233.157973	7341.998647	27.192512
233.043981	7358.565305	27.197530
233.525398	7377.658977	27.202548
234.076618	7380.142448	27.207565
234.041586	7400.283077	27.212583
234.502679	7411.260268	27.217600
234.566836	7426.817264	27.222618
234.771112	7428.442730	27.227636
235.036951	7445.764461	27.232653
234.768065	7462.175529	27.237671
235.470238	7466.927326	27.242688
235.811738	7480.736156	27.247706
236.123532	7504.118447	27.252724
236.490503	7498.217455	27.257741
236.292148	7526.288878	27.262759
236.932259	7522.343459	27.267776
237.035772	7546.033088	27.272794
237.472228	7557.958166	27.277812
238.002990	7560.097599	27.282829
237.752548	7577.257243	27.287847
238.616064	7574.643793	27.292864
238.515915	7573.999731	27.297882
238.929002	7591.598446	27.302900
239.317315	7597.356014	27.307917
238.926678	7609.767434	27.312935
239.607415	7613.787048	27.317952
239.600973	7620.383085	27.322970
239.644693	7628.473997	27.327988
240.277878	7635.193986	27.333005
240.462952	7653.630357	27.338023
240.623471	7649.520110	27.343040
240.868893	7673.039293	27.348058
240.796476	7667.197609	27.353076
241.412595	7686.024254	27.358093
241.616266	7699.356032	27.363111
241.761718	7701.637925	27.368128
241.704473	7708.232481	27.373146
241.817908	7715.081275	27.378164
242.231238	7726.647029	27.383181
242.369105	7748.803542	27.388199
242.799105	7758.264129	27.393216
242.958017	7771.915517	27.398234
243.605463	7776.874862	27.403252
243.968575	7797.973273	27.408269
243.632316	7805.141952	27.413287
244.341193	7813.024565	27.418304
244.335219	7821.464306	27.423322
244.070507	7834.421257	27.428340
244.642201	7845.858096	27.433357
245.031838	7857.762290	27.438375
245.184867	7865.002724	27.443392
245.648721	7875.004236	27.448410
245.697624	7880.862420	27.453428
245.930099	7897.561551	27.458445
245.756581	7908.240667	27.463463
246.121514	7918.216657	27.468480
246.533326	7932.838802	27.473498
246.535772	7964.014385	27.478516
246.876595	7949.482799	27.483533
247.091833	7974.560367	27.488551
247.526722	7973.835632	27.493568
248.224841	7994.064110	27.498586
248.413141	8002.429301	27.503604
248.567501	8003.162876	27.508621
248.801357	8026.305474	27.513639
248.788623	8028.798456	27.518656
248.918020	8054.003233	27.523674
249.372877	8061.909961	27.528692
249.583106	8065.993912	27.533709
249.504249	8088.213197	27.538727
249.918197	8097.935354	27.543744
250.486796	8111.106080	27.548762
250.574853	8126.366313	27.553780
250.888362	8127.756892	27.558797
251.417141	8147.626902	27.563815
251.561228	8155.648652	27.568832
251.831326	8163.218145	27.573850
252.238814	8179.665961	27.578868
252.739007	8182.700560	27.583885
252.675705	8187.070484	27.588903
252.524652	8192.382341	27.593920
253.148708	8201.617018	27.598938
253.566036	8213.580247	27.603956
253.479837	8220.103750	27.608973
253.376523	8238.822666	27.613991
253.864636	8254.898010	27.619008
254.798131	8260.721925	27.624026
254.854436	8268.252338	27.629044
254.538237	8283.822283	27.634061
255.188784	8288.007791	27.639079
255.484807	8298.929289	27.644096
255.803992	8311.662506	27.649114
255.494008	8323.357730	27.654132
256.066292	8328.764684	27.659149
256.098163	8351.150051	27.664167
256.335182	8358.358580	27.669184
256.723529	8368.826815	27.674202
257.223118	8391.274719	27.679220
257.536322	8402.711355	27.684237
257.553950	8411.441282	27.689255
257.938964	8421.947956	27.694272
258.367946	8428.166671	27.699290
258.262132	8440.114127	27.704308
258.862622	8453.520046	27.709325
258.909386	8467.726230	27.714343
258.874664	8472.265387	27.719360
259.314081	8478.798199	27.724378
259.479889	8498.794906	27.729396
259.901675	8515.348125	27.734413
260.089014	8521.380569	27.739431
260.674662	8527.470590	27.744448
260.938010	8535.303337	27.749466
261.341925	8554.015728	27.754484
262.172142	8555.104396	27.759501
262.031589	8557.585900	27.764519
262.057622	8553.998509	27.769536
262.623890	8559.924248	27.774554
262.745268	8572.947519	27.779572
262.945771	8569.986326	27.784589
262.998901	8579.806304	27.789607
263.165741	8581.488254	27.794624
263.315284	8593.591551	27.799642
263.227966	8600.203763	27.804660
263.481525	8608.581107	27.809677
263.796853	8623.064214	27.814695
264.114471	8634.894950	27.819712
264.559084	8645.818633	27.824730
264.785701	8666.794191	27.829748
265.388650	8673.825547	27.834765
265.360879	8690.345161	27.839783
265.405592	8704.166672	27.844800
265.892169	8701.981512	27.849818
265.875198	8731.346050	27.854836
266.422577	8730.360564	27.859853
266.487425	8757.183420	27.864871
266.859006	8768.705855	27.869888
267.605721	8783.453015	27.874906
267.758758	8794.564537	27.879924
268.340277	8805.321638	27.884941
268.276152	8811.541957	27.889959
268.375816	8810.879178	27.894976
268.758027	8821.260231	27.899994
268.623113	8839.624783	27.905012
269.017805	8850.932116	27.910029
269.509540	8856.421304	27.915047
269.559194	8878.119408	27.920064
270.056409	8876.074636	27.925082
270.108109	8897.317804	27.930100
270.161918	8915.198227	27.935117
270.736989	8918.543257	27.940135
271.002189	8930.827561	27.945152
271.589730	8939.190623	27.950170
271.549819	8962.232047	27.955188
272.034045	8973.553845	27.960205
272.146411	8983.434218	27.965223
272.402297	8997.020804	27.970240
272.735441	8999.863860	27.975258
272.816216	9022.649661	27.980276
273.157541	9030.527233	27.985293
273.295953	9057.632622	27.990311
273.257274	9074.788893	27.995328
274.112062	9091.022220	28.000346
274.158443	9104.291249	28.005364
274.366504	9116.189971	28.010381
274.488470	9129.551368	28.015399
274.742945	9152.385891	28.020416
275.275697	9158.241301	28.025434
275.392754	9182.275046	28.030452
276.162084	9203.421934	28.035469
276.326321	9213.755264	28.040487
276.299580	9221.368534	28.045504
277.036165	9232.916170	28.050522
277.328064	9259.214806	28.055540
277.362557	9259.035813	28.060557
277.571002	9271.243987	28.065575
277.938307	9289.224054	28.070592
278.309042	9294.568149	28.075610
278.325706	9314.857469	28.080628
278.997379	9320.170216	28.085645
279.219905	9325.187079	28.090663
279.150968	9340.810735	28.095680
280.111508	9354.410334	28.100698
279.730609	9361.728681	28.105716
280.364185	9374.353393	28.110733
280.534877	9391.897079	28.115751
280.893124	9389.921382	28.120768
281.058003	9406.682982	28.125786
281.045457	9416.712602	28.130804
281.276068	9428.030205	28.135821
281.693283	9440.770945	28.140839
282.062133	9450.115691	28.145856
282.317244	9457.151320	28.150874
282.299762	9471.276775	28.155892
282.761390	9492.118575	28.160909
283.079998	9499.466320	28.165927
283.023677	9520.449278	28.170944
283.633608	9532.247426	28.175962
283.626325	9548.654087	28.180980
284.138661	9559.233027	28.185997
284.853876	9575.924357	28.191015
284.743631	9586.651356	28.196032
285.405781	9599.502232	28.201050
285.699884	9612.647570	28.206068
285.632117	9618.224633	28.211085
285.956465	9629.079333	28.216103
286.071306	9643.866176	28.221120
286.750429	9667.070525	28.226138
286.865416	9683.066640	28.231156
287.138963	9702.880428	28.236173
287.660975	9702.685051	28.241191
287.537627	9718.860613	28.246208
288.096045	9730.155466	28.251226
288.120671	9743.510451	28.256244
289.013408	9745.388218	28.261261
289.305883	9757.735103	28.266279
289.669898	9762.016356	28.271296
289.857242	9765.529630	28.276314
290.116616	9783.959643	28.281332
290.447456	9790.187880	28.286349
290.554797	9806.715736	28.291367
290.930772	9820.887173	28.296384
291.280140	9822.373303	28.301402
291.561855	9836.562674	28.306420
291.658489	9844.336843	28.311437
292.220387	9860.250473	28.316455
292.136191	9875.573860	28.321472
292.875246	9879.521699	28.326490
293.015938	9898.248266	28.331508
292.926253	9917.699250	28.336525
293.204540	9926.126993	28.341543
293.632569	9937.192964	28.346560
294.163044	9959.050657	28.351578
293.762267	9955.785603	28.356596
293.880466	9979.914922	28.361613
294.299107	10008.262860	28.366631
294.789258	10038.664586	28.371648
294.982751	10044.011404	28.376666
295.466512	10078.209402	28.381684
295.941424	10079.824286	28.386701
296.232733	10096.879287	28.391719
296.589987	10119.844141	28.396736
297.075315	10133.796611	28.401754
297.224489	10146.693492	28.406772
297.588796	10155.126809	28.411789
297.883545	10165.307613	28.416807
297.972634	10173.199925	28.421824
298.401162	10188.639012	28.426842
298.873326	10209.031611	28.431860
299.188032	10226.376708	28.436877
299.357319	10219.804876	28.441895
299.861459	10239.800977	28.446912
299.857176	10248.923564	28.451930
300.253332	10271.342588	28.456948
300.431219	10279.669393	28.461965
300.723714	10279.816240	28.466983
301.072958	10298.062181	28.472000
301.492310	10314.750004	28.477018
301.628279	10325.817754	28.482036
301.659207	10330.422858	28.487053
302.092450	10348.646218	28.492071
302.543520	10354.754773	28.497088
302.746318	10371.037682	28.502106
303.124563	10388.420338	28.507124
303.193507	10404.297986	28.512141
303.512944	10405.135257	28.517159
303.774415	10436.097593	28.522176
303.895519	10438.598349	28.527194
304.341802	10452.576120	28.532212
304.671831	10480.806044	28.537229
305.401103	10483.022090	28.542247
305.041529	10507.290081	28.547264
305.918684	10532.358985	28.552282
306.227625	10532.155933	28.557300
306.479352	10557.152337	28.562317
306.753454	10565.217914	28.567335
307.386095	10578.181447	28.572352
307.259659	10599.868093	28.577370
307.480106	10616.170554	28.582388
307.781053	10628.109371	28.587405
308.382775	10642.148188	28.592423
308.559995	10660.383541	28.597440
308.938211	10676.992880	28.602458
309.199685	10680.362100	28.607476
309.310467	10700.944463	28.612493
309.951639	10707.778003	28.617511
310.075915	10720.631819	28.622528
310.379595	10740.593551	28.627546
310.789811	10762.328937	28.632564
311.329477	10783.662008	28.637581
311.812562	10789.124712	28.642599
311.803956	10802.826674	28.647616
312.075695	10815.846907	28.652634
312.539034	10835.556389	28.657652
312.635661	10851.925814	28.662669
313.208593	10851.460379	28.667687
313.542465	10873.747794	28.672704
313.780141	10885.352514	28.677722
314.261221	10902.328005	28.682740
314.111281	10915.376471	28.687757
314.778748	10925.076193	28.692775
314.928891	10955.535832	28.697792
315.026872	10960.212684	28.702810
315.643340	10969.415208	28.707828
315.670139	10993.838019	28.712845
316.315599	11008.830163	28.717863
316.223478	11025.431392	28.722880
316.524769	11040.348013	28.727898
317.262018	11051.524090	28.732916
317.284821	11073.026869	28.737933
317.899829	11084.522084	28.742951
318.177110	11102.524320	28.747968
318.596444	11115.900554	28.752986
318.697367	11121.546367	28.758004
319.008492	11142.483058	28.763021
319.707061	11139.446600	28.768039
319.595616	11167.301495	28.773056
319.880740	11178.396907	28.778074
320.363975	11193.875622	28.783092
320.500334	11213.608303	28.788109
320.836530	11224.853623	28.793127
321.125785	11250.375552	28.798144
321.529406	11263.305971	28.803162
321.696872	11279.674147	28.808180
322.319352	11290.378915	28.813197
322.415822	11292.735237	28.818215
322.818715	11318.040527	28.823232
322.839289	11332.448771	28.828250
323.182664	11348.176871	28.833268
323.311845	11363.865912	28.838285
324.186637	11372.646097	28.843303
324.393306	11395.358236	28.848320
324.604420	11406.828505	28.853338
325.312356	11416.342160	28.858356
325.475284	11424.889697	28.863373
325.973280	11440.407353	28.868391
325.671195	11457.266046	28.873408
326.123725	11462.064314	28.878426
326.429876	11491.903590	28.883444
326.812701	11504.932164	28.888461
327.252810	11517.459179	28.893479
327.527028	11554.670376	28.898496
327.787766	11557.209405	28.903514
328.043584	11581.145559	28.908532
328.398217	11610.330107	28.913549
328.958915	11609.604487	28.918567
328.951688	11638.097392	28.923584
329.303374	11657.556827	28.928602
330.018831	11668.544071	28.933620
330.065878	11691.215260	28.938637
330.500212	11714.877322	28.943655
330.736096	11734.389711	28.948672
331.103160	11748.567166	28.953690
331.481282	11767.811009	28.958708
331.752003	11799.617256	28.963725
332.484724	11808.410430	28.968743
332.742594	11822.264014	28.973760
332.736861	11839.209249	28.978778
333.223322	11860.501360	28.983796
333.535227	11876.929531	28.988813
334.075442	11888.736943	28.993831
334.432723	11904.517014	28.998848
334.979632	11928.834306	29.003866
335.367960	11938.382504	29.008884
335.341928	11955.476280	29.013901
335.730529	11961.055178	29.018919
336.196114	11987.305187	29.023936
336.197203	11995.527826	29.028954
336.620194	12012.586052	29.033972
337.141225	12040.519999	29.038989
337.430828	12048.918510	29.044007
337.870037	12075.280137	29.049024
337.887992	12089.578849	29.054042
338.469279	12103.801960	29.059060
338.662375	12119.238472	29.064077
339.335725	12133.611389	29.069095
339.755361	12160.175140	29.074112
340.037337	12162.647770	29.079130
340.540833	12182.011341	29.084148
340.587246	12199.747648	29.089165
341.405848	12208.492824	29.094183
341.268634	12221.729668	29.099200
341.431052	12235.604823	29.104218
341.837923	12245.118696	29.109236
342.151816	12273.439108	29.114253
342.742095	12286.397836	29.119271
343.034279	12302.065284	29.124288
343.036362	12316.221395	29.129306
343.563442	12336.374036	29.134324
343.871325	12355.316862	29.139341
344.222671	12347.904217	29.144359
344.756544	12374.380904	29.149376
344.540444	12380.158857	29.154394
345.109084	12399.171405	29.159412
345.274848	12420.915427	29.164429
345.560024	12440.332409	29.169447
345.971577	12449.703550	29.174464
346.360054	12470.342245	29.179482
346.751159	12473.738853	29.184500
347.104738	12502.751271	29.189517
347.144324	12510.816529	29.194535
347.753061	12544.465781	29.199552
348.058111	12555.820987	29.204570
348.294858	12564.234324	29.209588
348.680372	12589.951411	29.214605
348.868923	12612.358389	29.219623
349.447631	12631.379068	29.224640
349.835923	12651.973781	29.229658
350.159656	12673.270198	29.234676
350.320671	12695.103701	29.239693
351.233791	12713.089986	29.244711
351.274013	12741.504495	29.249728
351.629335	12752.491948	29.254746
352.204016	12764.603985	29.259764
352.370417	12781.232579	29.264781
352.612469	12798.525122	29.269799
353.206211	12827.955154	29.274816
353.420785	12842.201532	29.279834
354.154911	12857.127587	29.284852
354.638332	12873.052922	29.289869
355.071524	12895.049284	29.294887
355.453907	12906.509430	29.299904
355.472090	12922.283471	29.304922
355.921865	12939.584659	29.309940
356.278230	12954.071016	29.314957
356.358691	12965.578492	29.319975
357.040132	12984.229750	29.324992
357.208264	13002.970906	29.330010
357.821317	13020.562382	29.335028
358.398027	13032.933223	29.340045
358.250412	13045.758585	29.345063
358.661904	13073.073324	29.350080
359.063148	13082.143237	29.355098
359.245696	13099.240111	29.360116
359.624932	13129.424220	29.365133
360.161334	13134.879265	29.370151
360.960449	13144.881633	29.375168
361.490478	13162.233612	29.380186
361.941613	13155.225028	29.385204
362.244886	13172.533588	29.390221
362.318296	13176.103249	29.395239
362.774673	13190.293066	29.400256
362.674708	13212.907004	29.405274
363.061023	13213.752881	29.410292
363.464958	13223.880351	29.415309
363.831884	13249.165452	29.420327
364.255118	13268.858508	29.425344
364.536825	13283.287338	29.430362
364.990405	13301.583018	29.435380
365.211292	13316.716151	29.440397
365.415389	13341.028965	29.445415
365.897537	13350.140019	29.450432
366.108083	13377.395093	29.455450
366.477238	13383.463791	29.460468
366.621822	13413.145097	29.465485
366.721566	13437.038579	29.470503
367.356602	13456.319696	29.475520
367.531718	13486.798462	29.480538
368.333179	13503.944023	29.485556
368.390998	13519.649194	29.490573
368.782570	13541.895994	29.495591
369.607976	13559.325234	29.500608
369.722802	13585.594515	29.505626
370.035061	13601.439904	29.510644
370.384297	13603.479018	29.515661
371.118336	13615.929813	29.520679
371.515372	13637.108463	29.525696
371.673021	13656.935107	29.530714
372.145459	13666.875236	29.535732
372.388769	13682.987293	29.540749
372.914362	13705.636468	29.545767
373.252283	13717.903052	29.550784
373.656763	13736.617387	29.555802
373.911405	13755.115200	29.560820
374.393952	13771.177226	29.565837
374.470298	13790.931478	29.570855
374.903585	13814.327907	29.575872
374.811439	13847.836623	29.580890
375.398214	13854.095607	29.585908
375.764418	13877.448934	29.590925
376.023400	13909.746913	29.595943
376.485963	13924.261592	29.600960
376.596463	13951.059453	29.605978
376.977900	13973.917854	29.610996
377.950943	13999.469035	29.616013
378.173661	14032.805593	29.621031
378.694230	14051.195721	29.626048
379.363885	14075.171273	29.631066
379.794266	14091.557550	29.636084
379.831738	14100.441761	29.641101
380.304579	14128.670575	29.646119
380.559852	14146.350725	29.651136
381.238402	14169.462842	29.656154
381.489561	14184.885630	29.661172
381.744104	14206.813599	29.666189
382.228676	14227.000183	29.671207
382.671625	14245.238436	29.676224
383.102580	14271.197023	29.681242
383.674201	14282.126222	29.686260
383.906141	14290.825313	29.691277
384.294209	14316.294855	29.696295
385.045606	14335.880772	29.701312
385.066938	14357.352776	29.706330
385.549492	14370.247703	29.711348
386.078160	14383.823890	29.716365
386.490342	14411.595222	29.721383
386.807872	14418.237647	29.726400
387.014944	14443.498850	29.731418
387.532372	14454.303995	29.736436
387.938840	14476.596931	29.741453
388.110403	14500.521556	29.746471
388.400738	14518.746079	29.751488
388.988144	14537.956806	29.756506
389.357365	14552.972946	29.761524
389.573255	14572.592457	29.766541
389.789354	14608.707090	29.771559
390.590604	14613.404177	29.776576
390.656584	14640.418420	29.781594
391.061075	14656.831348	29.786612
391.617545	14678.630456	29.791629
391.825673	14718.488995	29.796647
392.370157	14714.812906	29.801664
392.690901	14750.156607	29.806682
392.845695	14778.515159	29.811700
393.520008	14795.201763	29.816717
394.180032	14816.710045	29.821735
394.147907	14833.990543	29.826752
394.740303	14842.829235	29.831770
395.227608	14862.971852	29.836788
395.338863	14874.794640	29.841805
395.794587	14897.945706	29.846823
396.495065	14914.773595	29.851840
396.354425	14932.004857	29.856858
397.139053	14948.380602	29.861876
397.605438	14967.557029	29.866893
397.397033	14992.078688	29.871911
398.279752	14998.534882	29.876928
398.412755	15019.746956	29.881946
399.035661	15042.306686	29.886964
399.634765	15061.951948	29.891981
399.417050	15087.962723	29.896999
399.973042	15093.854268	29.902016
400.216682	15128.648579	29.907034
400.898223	15145.703876	29.912052
401.441288	15164.401068	29.917069
401.515384	15192.318084	29.922087
402.406553	15202.679807	29.927104
402.833566	15234.258891	29.932122
403.062988	15239.478390	29.937140
403.571705	15273.786127	29.942157
403.725723	15296.650157	29.947175
404.364928	15310.841350	29.952192
404.552838	15337.000533	29.957210
405.046552	15363.001311	29.962228
405.612781	15378.426247	29.967245
405.651041	15405.227990	29.972263
406.326639	15414.726636	29.977280
406.889908	15445.713074	29.982298
407.236933	15467.725915	29.987316
407.651164	15481.431353	29.992333
407.915361	15507.673569	29.997351
408.638578	15529.428583	30.002368
408.819427	15550.235801	30.007386
409.180382	15570.515815	30.012404
409.978715	15588.706007	30.017421
409.912834	15609.264528	30.022439
410.502326	15633.216702	30.027456
411.125552	15659.071263	30.032474
411.386294	15672.750346	30.037492
411.812086	15684.976012	30.042509
412.094038	15711.904248	30.047527
412.752501	15725.960084	30.052544
413.801986	15745.443914	30.057562
413.566935	15766.487063	30.062580
413.638853	15778.433431	30.067597
414.074295	15811.834527	30.072615
414.714309	15826.831363	30.077632
415.098825	15847.329067	30.082650
415.703832	15863.620034	30.087668
415.844719	15893.283669	30.092685
416.329405	15903.785247	30.097703
416.637967	15935.317716	30.102720
417.132882	15954.054809	30.107738
417.069193	15976.865316	30.112756
417.602760	16005.870681	30.117773
418.013696	16028.995391	30.122791
418.826988	16058.234960	30.127808
419.331477	16085.457338	30.132826
419.468474	16103.637907	30.137844
420.341891	16122.265343	30.142861
420.392515	16143.617902	30.147879
420.693035	16164.053298	30.152896
421.115208	16184.415968	30.157914
421.862606	16212.080561	30.162932
422.084490	16218.931262	30.167949
422.389968	16237.594076	30.172967
423.010747	16257.502485	30.177984
423.168033	16269.581075	30.183002
423.557826	16293.691693	30.188020
424.543937	16312.004770	30.193037
424.753105	16344.080940	30.198055
425.114792	16354.823125	30.203072
425.243651	16367.875877	30.208090
425.672556	16386.570039	30.213108
426.177281	16408.432922	30.218125
426.612145	16432.985159	30.223143
427.257443	16447.135185	30.228160
427.571969	16479.621473	30.233178
427.906858	16497.935660	30.238196
428.628385	16516.372495	30.243213
428.646099	16541.454508	30.248231
428.788244	16565.837986	30.253248
429.670018	16586.896609	30.258266
429.916953	16617.106963	30.263284
430.410630	16636.893542	30.268301
430.610579	16666.438571	30.273319
431.043426	16691.405219	30.278336
431.946456	16717.293187	30.283354
432.160935	16745.616873	30.288372
432.437483	16762.430674	30.293389
432.500415	16781.015141	30.298407
433.196103	16817.118827	30.303424
433.717620	16843.553138	30.308442
434.382338	16870.944204	30.313460
434.478687	16894.213987	30.318477
434.975222	16920.513340	30.323495
435.531051	16950.066233	30.328512
436.320968	16980.599563	30.333530
436.430076	17005.977403	30.338548
436.986621	17036.888501	30.343565
437.321240	17060.272775	30.348583
437.605330	17086.217126	30.353600
438.435926	17115.708284	30.358618
438.736323	17144.587643	30.363636
439.358394	17160.093711	30.368653
439.932213	17186.453970	30.373671
439.996190	17218.156354	30.378688
440.307001	17244.627377	30.383706
440.770081	17268.276057	30.388724
441.886179	17295.960268	30.393741
442.235117	17311.281820	30.398759
442.626378	17328.466657	30.403776
443.014572	17352.645184	30.408794
443.450634	17378.307116	30.413812
443.964415	17394.360985	30.418829
444.256514	17428.289562	30.423847
444.724486	17447.313452	30.428864
445.283924	17464.137253	30.433882
445.746970	17497.085265	30.438900
446.342474	17510.523704	30.443917
446.479845	17547.054184	30.448935
447.003746	17563.441426	30.453952
447.507707	17581.809128	30.458970
447.901078	17608.931038	30.463988
448.342808	17634.415538	30.469005
448.747650	17657.871662	30.474023
449.141881	17680.066006	30.479040
449.205041	17692.425561	30.484058
449.827359	17729.562702	30.489076
450.700433	17753.867940	30.494093
451.142657	17776.023291	30.499111
451.348580	17799.232778	30.504128
451.866464	17823.612690	30.509146
451.894694	17840.305231	30.514164
452.627449	17859.382816	30.519181
453.303911	17882.480798	30.524199
453.673886	17893.244656	30.529216
454.296483	17920.646972	30.534234
454.060590	17946.490716	30.539252
454.947574	17962.075969	30.544269
455.584837	17969.790900	30.549287
455.943016	18007.153153	30.554304
456.280404	18019.071963	30.559322
456.446329	18045.838428	30.564340
457.140536	18062.812215	30.569357
457.729120	18100.441799	30.574375
458.215071	18116.765963	30.579392
458.957373	18137.358527	30.584410
459.173116	18149.940857	30.589428
459.620257	18176.221230	30.594445
460.281827	18199.599896	30.599463
460.937915	18223.238467	30.604480
461.134951	18249.040075	30.609498
461.340547	18275.926994	30.614516
461.719896	18290.246386	30.619533
462.010463	18319.160627	30.624551
462.217146	18341.732571	30.629568
462.822422	18368.923437	30.634586
463.243351	18399.459950	30.639604
463.945103	18438.658180	30.644621
464.277452	18461.324297	30.649639
465.007084	18484.389402	30.654656
465.539454	18507.927664	30.659674
466.472274	18528.749828	30.664692
466.685813	18548.970780	30.669709
467.370101	18572.150491	30.674727
467.680670	18603.911282	30.679744
468.253271	18609.109536	30.684762
468.483246	18636.296383	30.689780
469.042649	18663.185282	30.694797
469.618129	18685.763039	30.699815
470.356589	18712.845080	30.704832
470.527368	18724.360817	30.709850
470.516928	18752.008768	30.714868
471.212684	18774.340352	30.719885
471.603924	18804.111391	30.724903
471.995637	18832.081848	30.729920
472.459552	18854.645687	30.734938
472.905059	18891.111480	30.739956
473.337440	18922.348291	30.744973
474.041236	18950.680692	30.749991
474.341675	18978.520346	30.755008
475.227412	18998.503808	30.760026
475.658318	19035.913509	30.765044
476.142038	19052.510478	30.770061
476.988682	19079.803527	30.775079
477.138045	19100.325724	30.780096
477.878698	19118.367193	30.785114
478.069298	19151.082705	30.790132
478.156739	19166.301372	30.795149
478.780836	19205.001567	30.800167
478.946064	19225.066525	30.805184
479.713192	19250.142065	30.810202
480.082864	19288.174674	30.815220
480.416042	19313.526754	30.820237
481.044239	19349.396180	30.825255
481.589147	19372.579725	30.830272
481.950508	19395.116029	30.835290
482.841509	19429.485003	30.840308
482.915702	19457.070153	30.845325
483.805629	19488.457336	30.850343
484.009357	19510.778381	30.855360
484.734724	19525.177166	30.860378
484.908233	19544.969484	30.865396
485.514137	19561.200262	30.870413
485.676761	19595.266626	30.875431
485.794587	19616.975767	30.880448
486.570630	19639.700123	30.885466
487.243292	19666.787481	30.890484
487.827315	19697.022493	30.895501
488.347508	19733.907790	30.900519
488.791163	19765.586448	30.905536
489.026278	19781.047822	30.910554
489.449687	19816.596373	30.915572
489.880902	19837.176288	30.920589
490.486366	19881.307953	30.925607
490.836667	19906.936117	30.930624
491.604355	19946.196555	30.935642
492.040867	19971.615440	30.940660
492.665229	20002.811276	30.945677
493.353268	20028.317201	30.950695
493.682451	20061.492707	30.955712
494.121313	20081.364051	30.960730
494.637813	20115.818165	30.965748
495.016348	20138.327364	30.970765
495.622034	20170.910069	30.975783
495.870640	20211.882428	30.980800
496.676318	20229.826291	30.985818
497.264414	20267.396958	30.990836
497.837070	20291.941979	30.995853
498.607837	20337.097603	31.000871
498.642339	20359.041755	31.005888
499.308230	20377.696334	31.010906
499.794091	20410.696255	31.015924
500.565308	20439.759495	31.020941
501.326734	20453.925864	31.025959
501.743704	20482.273824	31.030976
502.322077	20507.835462	31.035994
502.734604	20529.865917	31.041012
502.720872	20552.531805	31.046029
503.274932	20579.815918	31.051047
503.465864	20620.703389	31.056064
504.009641	20640.925331	31.061082
504.528077	20681.628950	31.066100
504.843374	20717.341390	31.071117
505.852496	20744.459683	31.076135
506.022681	20786.361684	31.081152
506.594019	20821.737249	31.086170
507.420922	20843.589424	31.091188
507.718100	20875.065357	31.096205
508.195238	20909.489120	31.101223
508.828829	20945.682868	31.106240
509.486006	20976.053722	31.111258
509.725941	21013.629801	31.116276
510.310299	21041.838620	31.121293
511.027077	21067.834238	31.126311
511.611364	21094.905824	31.131328
512.340678	21117.474939	31.136346
513.032123	21138.457756	31.141364
513.258718	21171.234186	31.146381
513.841850	21204.485582	31.151399
514.400197	21233.545430	31.156416
514.758319	21259.900763	31.161434
515.536718	21280.295129	31.166452
515.898732	21307.224902	31.171469
516.507944	21324.966757	31.176487
517.255324	21355.355662	31.181504
517.582375	21364.605396	31.186522
518.315911	21394.200393	31.191540
518.816491	21410.929416	31.196557
519.280063	21420.701191	31.201575
519.246768	21439.434698	31.206592
519.859760	21460.133174	31.211610
520.492360	21481.466778	31.216628
521.282788	21499.483701	31.221645
521.977783	21512.574447	31.226663
522.179144	21540.357437	31.231680
522.458125	21560.501746	31.236698
523.241657	21575.189913	31.241716
523.373255	21600.469106	31.246733
524.248098	21625.562418	31.251751
524.568339	21663.664242	31.256768
525.132390	21675.594020	31.261786
525.292487	21710.504827	31.266804
525.754240	21743.441256	31.271821
526.518767	21754.391882	31.276839
527.022375	21802.170735	31.281856
527.643069	21826.368944	31.286874
527.858244	21857.170551	31.291892
528.183720	21889.957964	31.296909
528.914327	21916.710785	31.301927
529.334588	21951.884569	31.306944
529.841347	21982.236305	31.311962
530.627891	22020.954528	31.316980
530.812439	22060.316846	31.321997
531.763504	22074.429414	31.327015
532.340958	22121.938405	31.332032
532.553793	22154.219438	31.337050
533.484562	22180.233562	31.342068
533.826654	22211.729869	31.347085
534.624333	22235.281615	31.352103
535.153271	22268.865555	31.357120
536.044928	22297.716798	31.362138
536.602996	22322.538352	31.367156
536.404679	22344.167320	31.372173
537.662388	22378.130176	31.377191
537.641324	22406.246206	31.382208
538.167687	22428.715917	31.387226
538.721488	22458.871450	31.392244
539.492491	22499.823616	31.397261
540.464851	22523.708527	31.402279
540.573939	22551.185123	31.407296
541.277881	22592.798835	31.412314
541.715422	22613.393305	31.417332
542.059190	22644.997460	31.422349
542.714793	22670.606682	31.427367
542.990899	22706.632169	31.432384
543.487544	22738.648540	31.437402
544.066660	22767.694756	31.442420
544.660568	22805.086103	31.447437
545.688324	22835.427058	31.452455
545.993341	22871.915924	31.457472
546.730049	22901.816000	31.462490
547.410076	22932.388498	31.467508
547.403375	22957.274025	31.472525
548.363464	22988.213485	31.477543
548.467160	23024.127531	31.482560
549.106356	23054.099981	31.487578
549.936675	23078.279530	31.492596
550.252164	23121.263241	31.497613
550.750464	23147.434840	31.502631
551.065387	23181.913246	31.507648
552.323215	23216.907544	31.512666
552.557966	23251.682988	31.517684
552.592990	23282.464470	31.522701
553.437481	23320.537925	31.527719
553.824743	23345.545491	31.532736
554.292633	23366.350842	31.537754
554.724549	23399.970851	31.542772
555.323015	23425.956511	31.547789
556.293558	23464.351736	31.552807
556.756210	23501.215179	31.557824
556.855869	23522.931461	31.562842
557.620914	23557.738131	31.567860
557.946048	23594.743350	31.572877
558.756315	23623.963152	31.577895
558.902914	23669.432692	31.582912
559.805603	23700.230590	31.587930
560.488835	23739.271677	31.592948
561.162373	23771.135620	31.597965
561.839298	23810.588590	31.602983
562.366898	23841.647671	31.608000
563.156129	23866.694045	31.613018
563.349542	23897.609653	31.618036
563.730994	23936.635198	31.623053
564.421499	23961.160008	31.628071
565.250641	23997.897456	31.633088
565.847406	24029.280925	31.638106
566.336043	24070.147844	31.643124
566.991765	24102.760798	31.648141
567.850760	24124.813807	31.653159
568.207665	24166.453567	31.658176
569.155310	24192.922693	31.663194
569.500069	24223.505449	31.668212
569.992777	24257.964190	31.673229
570.521674	24286.262154	31.678247
571.115674	24311.851543	31.683264
571.639287	24355.437266	31.688282
572.548089	24379.700900	31.693300
572.529279	24416.805746	31.698317
573.339733	24442.778490	31.703335
573.868928	24480.783473	31.708352
574.606600	24518.831712	31.713370
575.253397	24539.780897	31.718388
575.559566	24576.424370	31.723405
576.392206	24614.192495	31.728423
577.315610	24647.440610	31.733440
577.224683	24678.136533	31.738458
578.004684	24708.910968	31.743476
578.540598	24759.434574	31.748493
579.110110	24778.335916	31.753511
579.626989	24812.077707	31.758528
580.040442	24852.098528	31.763546
581.118794	24879.350691	31.768564
581.491692	24920.130039	31.773581
581.934172	24950.749159	31.778599
582.466815	24980.835989	31.783616
583.121817	25025.931958	31.788634
583.645309	25057.612903	31.793652
584.155449	25100.355514	31.798669
584.770595	25133.241932	31.803687
585.449076	25173.183967	31.808704
586.083871	25221.639330	31.813722
586.422419	25241.778038	31.818740
587.116849	25286.476591	31.823757
587.725285	25312.444187	31.828775
588.439096	25353.107823	31.833792
588.907597	25389.367127	31.838810
589.712899	25421.282582	31.843828
590.142523	25466.724510	31.848845
590.759795	25496.685103	31.853863
591.675881	25530.138065	31.858880
592.032681	25571.439484	31.863898
592.929419	25597.311736	31.868916
593.162307	25632.919512	31.873933
594.005444	25657.138103	31.878951
594.256128	25677.088772	31.883968
594.844508	25706.782446	31.888986
595.311313	25740.034365	31.894004
595.533076	25773.470075	31.899021
596.552819	25812.677382	31.904039
596.986424	25850.832648	31.909056
597.370596	25879.414645	31.914074
598.211974	25920.476568	31.919092
598.752540	25954.311368	31.924109
599.186854	25994.059434	31.929127
599.883454	26028.729443	31.934144
600.678878	26077.066908	31.939162
601.219383	26105.681622	31.944180
601.543975	26145.643092	31.949197
602.193466	26177.034304	31.954215
602.797746	26229.200430	31.959232
603.354705	26264.139197	31.964250
603.940040	26298.264606	31.969268
604.549107	26345.797647	31.974285
605.494757	26378.767062	31.979303
605.847968	26420.013898	31.984320
606.115195	26460.275700	31.989338
607.381123	26503.806704	31.994356
608.070253	26548.976581	31.999373
608.833114	26582.139280	32.004391
609.308247	26625.383583	32.009408
609.730590	26657.405216	32.014426
610.589585	26698.491245	32.019444
611.266777	26734.126180	32.024461
611.982483	26774.823989	32.029479
612.657032	26798.394091	32.034496
612.917994	26840.060727	32.039514
613.790623	26869.983369	32.044532
614.592675	26913.758553	32.049549
615.209534	26950.920191	32.054567
615.852864	26990.871332	32.059584
616.482341	27024.668719	32.064602
616.967894	27056.542036	32.069620
617.373676	27088.497421	32.074637
617.810487	27127.627928	32.079655
618.877171	27167.930261	32.084672
619.684593	27202.294190	32.089690
620.674730	27232.603471	32.094708
621.063255	27262.223285	32.099725
621.660567	27294.155319	32.104743
622.052812	27333.059346	32.109760
622.280712	27369.075464	32.114778
623.292573	27378.897030	32.119796
623.778668	27434.586295	32.124813
624.547067	27473.520167	32.129831
625.377989	27507.444822	32.134848
625.641420	27549.782498	32.139866
626.505135	27575.788873	32.144884
627.603692	27615.461376	32.149901
627.948337	27646.061981	32.154919
628.518212	27672.038652	32.159936
628.796955	27717.199557	32.164954
630.029032	27742.143490	32.169972
630.703877	27771.251485	32.174989
631.524247	27795.040092	32.180007
632.231567	27814.725416	32.185024
632.834960	27854.716116	32.190042
633.574348	27859.359785	32.195060
633.807054	27900.154457	32.200077
634.390147	27925.882880	32.205095
634.949265	27947.260184	32.210112
635.215276	27980.610435	32.215130
635.959506	28002.382289	32.220148
636.542194	28041.365296	32.225165
636.965658	28062.694439	32.230183
637.504129	28091.299636	32.235200
637.722116	28123.816995	32.240218
638.863756	28153.977514	32.245236
639.174412	28194.722643	32.250253
639.650578	28239.272282	32.255271
640.465784	28262.961115	32.260288
641.138415	28314.793220	32.265306
641.586712	28346.497414	32.270324
642.276653	28379.579662	32.275341
643.143939	28420.459295	32.280359
643.619296	28455.288199	32.285376
644.130171	28514.042108	32.290394
644.746347	28545.265223	32.295412
645.540241	28588.685007	32.300429
645.905023	28632.026708	32.305447
646.480129	28665.443445	32.310464
647.236311	28722.351775	32.315482
647.893722	28764.586024	32.320500
648.668753	28804.817182	32.325517
649.311522	28847.192955	32.330535
650.452765	28884.718464	32.335552
650.531766	28930.065032	32.340570
651.403288	28969.624028	32.345588
652.270336	29024.998813	32.350605
652.531756	29060.292075	32.355623
653.505343	29097.250061	32.360640
654.145396	29146.162764	32.365658
654.989549	29180.682307	32.370676
655.852072	29224.560447	32.375693
656.579020	29267.770922	32.380711
657.170464	29295.800618	32.385728
657.408583	29340.623811	32.390746
658.214106	29370.971513	32.395764
659.212510	29414.304132	32.400781
659.828254	29456.350380	32.405799
660.649067	29493.010631	32.410816
661.183506	29524.671554	32.415834
662.060376	29552.991920	32.420852
663.118110	29601.189222	32.425869
663.251237	29631.339197	32.430887
664.032000	29673.739315	32.435904
664.446797	29711.026123	32.440922
665.468243	29730.423900	32.445940
666.161416	29769.866986	32.450957
666.759956	29803.275588	32.455975
667.446595	29844.862724	32.460992
668.677373	29881.908273	32.466010
669.586681	29911.880214	32.471028
670.133099	29935.929144	32.476045
670.654274	29970.589096	32.481063
671.049387	30010.825228	32.486080
671.547444	30037.486208	32.491098
672.219441	30063.797597	32.496116
673.196494	30086.736255	32.501133
673.680098	30134.809798	32.506151
674.440859	30157.270383	32.511168
674.792325	30205.706135	32.516186
675.226703	30233.464607	32.521204
676.106225	30264.326712	32.526221
676.324023	30310.394180	32.531239
677.348916	30339.533191	32.536256
677.896194	30382.489686	32.541274
678.492820	30414.869199	32.546292
679.109373	30455.425517	32.551309
679.171008	30492.010479	32.556327
680.120246	30536.775481	32.561344
680.905909	30568.657846	32.566362
681.299966	30610.835991	32.571380
682.270356	30646.122087	32.576397
682.744405	30688.053969	32.581415
683.402093	30723.553526	32.586432
684.070565	30761.504191	32.591450
684.562655	30803.167978	32.596468
685.620197	30853.934772	32.601485
686.060761	30890.170306	32.606503
686.590014	30929.774034	32.611520
687.341409	30984.363048	32.616538
688.009002	31027.744551	32.621556
689.046440	31063.438085	32.626573
689.603048	31116.749386	32.631591
690.216871	31157.693127	32.636608
691.124597	31208.831942	32.641626
691.504264	31249.818856	32.646644
692.619442	31291.310189	32.651661
693.119729	31332.708249	32.656679
693.875414	31379.629465	32.661696
694.347609	31434.762801	32.666714
695.190156	31474.571375	32.671732
696.331654	31517.930264	32.676749
696.875652	31566.699385	32.681767
697.540189	31601.680994	32.686784
698.142519	31647.223406	32.691802
698.633842	31699.073459	32.696820
699.741103	31735.686518	32.701837
700.637766	31780.955545	32.706855
701.657590	31822.639885	32.711872
702.418567	31868.480349	32.716890
703.000159	31905.138098	32.721908
703.812926	31937.682121	32.726925
703.932610	31981.486480	32.731943
705.072967	32015.654616	32.736960
705.550943	32062.715693	32.741978
706.279000	32102.379033	32.746996
707.285295	32150.811608	32.752013
707.957112	32194.036840	32.757031
708.668058	32229.555924	32.762048
708.951943	32271.761018	32.767066
710.036269	32309.118349	32.772084
710.676474	32356.831134	32.777101
710.929970	32391.631886	32.782119
712.039079	32431.767226	32.787136
712.668737	32475.284133	32.792154
713.611708	32520.914196	32.797172
714.511700	32558.585332	32.802189
714.887628	32608.002771	32.807207
715.935732	32637.457489	32.812224
716.278957	32693.316101	32.817242
717.096344	32736.462763	32.822260
717.883748	32766.887837	32.827277
718.364450	32813.709942	32.832295
719.099260	32846.615311	32.837312
720.186089	32890.447140	32.842330
720.526291	32935.641445	32.847348
721.188385	32983.181535	32.852365
721.848069	33030.399681	32.857383
722.712444	33069.259563	32.862400
723.702755	33111.020650	32.867418
724.535089	33146.212498	32.872436
725.548022	33181.780746	32.877453
725.827117	33234.477092	32.882471
726.586352	33269.415062	32.887488
727.522008	33306.437095	32.892506
727.680859	33336.063669	32.897524
728.523413	33369.509349	32.902541
728.977912	33417.538139	32.907559
729.249411	33442.974514	32.912576
730.536050	33489.627665	32.917594
731.212512	33536.382796	32.922612
731.528537	33569.708935	32.927629
732.246278	33620.984581	32.932647
733.238203	33665.623191	32.937664
734.118869	33705.246709	32.942682
734.428741	33756.251471	32.947700
735.717311	33807.046192	32.952717
735.987374	33839.450563	32.957735
737.229942	33890.265334	32.962752
737.911760	33933.005768	32.967770
738.345138	33968.849462	32.972788
739.255273	34004.485786	32.977805
740.089698	34060.726334	32.982823
740.960900	34104.543893	32.987840
741.719449	34140.545601	32.992858
742.346232	34191.729401	32.997876
743.098054	34232.189695	33.002893
743.960422	34275.256612	33.007911
744.388603	34320.022830	33.012928
745.382645	34369.132653	33.017946
746.139077	34410.907665	33.022964
746.957061	34455.050417	33.027981
747.378258	34494.279503	33.032999
748.260400	34542.022602	33.038016
749.156214	34591.812202	33.043034
750.017119	34631.427916	33.048052
751.020107	34681.795275	33.053069
751.770259	34728.238028	33.058087
752.452000	34775.956134	33.063104
753.159889	34811.492720	33.068122
753.902978	34854.705955	33.073140
754.787998	34890.746045	33.078157
755.474787	34947.694934	33.083175
756.434414	34986.821651	33.088192
756.980318	35038.570250	33.093210
757.792079	35078.738259	33.098228
758.802070	35109.176134	33.103245
759.457465	35167.812395	33.108263
760.301291	35201.785586	33.113280
761.020850	35247.930776	33.118298
761.548869	35289.787556	33.123316
762.599604	35332.296015	33.128333
763.340489	35373.771870	33.133351
763.993153	35409.375016	33.138368
764.868473	35442.818864	33.143386
765.599238	35502.835286	33.148404
766.182480	35535.300706	33.153421
767.168217	35586.880602	33.158439
767.640375	35623.163636	33.163456
768.779104	35672.936714	33.168474
769.146493	35718.423582	33.173492
769.975366	35755.789119	33.178509
770.765766	35793.103840	33.183527
771.425998	35848.156086	33.188544
772.267254	35885.444036	33.193562
772.888722	35947.679244	33.198580
773.820572	35986.337932	33.203597
774.860715	36039.870557	33.208615
775.860053	36076.994982	33.213632
776.896968	36116.630178	33.218650
777.203801	36147.261860	33.223668
778.215285	36187.147772	33.228685
778.575747	36230.866349	33.233703
779.376763	36265.467616	33.238720
779.971561	36299.146437	33.243738
780.423366	36329.009548	33.248756
781.161937	36368.603409	33.253773
781.788009	36401.095062	33.258791
782.805136	36447.550361	33.263808
783.672794	36499.707407	33.268826
784.346115	36542.188868	33.273844
785.126062	36588.087232	33.278861
785.636507	36632.194156	33.283879
786.287510	36678.138199	33.288896
787.841816	36717.952751	33.293914
788.714236	36772.645350	33.298932
789.315628	36813.146780	33.303949
790.049723	36840.095624	33.308967
791.093872	36891.587337	33.313984
791.819208	36934.782295	33.319002
792.298954	36980.684250	33.324020
793.233675	37027.520472	33.329037
793.742780	37064.698095	33.334055
794.411326	37129.243734	33.339072
795.687140	37169.469499	33.344090
796.124415	37219.672209	33.349108
796.967921	37278.208946	33.354125
797.715727	37321.774250	33.359143
798.504113	37369.355009	33.364160
799.380410	37423.903229	33.369178
800.152278	37481.364101	33.374196
801.271921	37517.567940	33.379213
802.112606	37574.499758	33.384231
802.619280	37620.449456	33.389248
803.886063	37661.898005	33.394266
804.649130	37725.842550	33.399284
805.722498	37776.769022	33.404301
806.664580	37809.232304	33.409319
807.203794	37860.495562	33.414336
808.215236	37899.714381	33.419354
808.537801	37945.326834	33.424372
809.591799	37984.836356	33.429389
810.795475	38028.369653	33.434407
811.243941	38081.791369	33.439424
812.298180	38122.565842	33.444442
813.252007	38171.507363	33.449460
814.352193	38206.659357	33.454477
814.991321	38241.795073	33.459495
815.752152	38293.138487	33.464512
816.424042	38334.422220	33.469530
817.162249	38372.666567	33.474548
817.995398	38409.410029	33.479565
818.937795	38454.667228	33.484583
819.611862	38509.211930	33.489600
820.481863	38548.226426	33.494618
821.271997	38598.509904	33.499636
821.819486	38644.038025	33.504653
822.547902	38698.473514	33.509671
823.177170	38749.952447	33.514688
824.343779	38795.270111	33.519706
825.225901	38854.715736	33.524724
825.978795	38906.567766	33.529741
827.016879	38943.766991	33.534759
827.691195	38990.148684	33.539776
828.541152	39028.990120	33.544794
829.279400	39084.841608	33.549812
829.933455	39131.422820	33.554829
830.989475	39180.856550	33.559847
831.363308	39227.437580	33.564864
832.424746	39275.922079	33.569882
833.197991	39337.340203	33.574900
834.079182	39375.987650	33.579917
835.028825	39410.773095	33.584935
835.381928	39447.764246	33.589952
836.396701	39487.485040	33.594970
837.227326	39541.463961	33.599988
837.839708	39584.757819	33.605005
838.581504	39628.866283	33.610023
839.462779	39683.704033	33.615040
840.202078	39731.101649	33.620058
840.899006	39792.008107	33.625076
841.751296	39849.045301	33.630093
843.310657	39893.171739	33.635111
843.500157	39940.674877	33.640128
844.502104	39994.975932	33.645146
845.567060	40054.168549	33.650164
846.333743	40100.493886	33.655181
847.790508	40155.040336	33.660199
848.384298	40207.261904	33.665216
849.240236	40254.926993	33.670234
849.905410	40303.014165	33.675252
850.668862	40352.831571	33.680269
851.700446	40399.868663	33.685287
852.618689	40456.429122	33.690304
853.654071	40499.753433	33.695322
854.274800	40558.220110	33.700340
855.102780	40621.081579	33.705357
855.972863	40660.688042	33.710375
856.478405	40725.934015	33.715392
857.878008	40777.360380	33.720410
858.804844	40830.960620	33.725428
859.909536	40877.367497	33.730445
860.603800	40925.293375	33.735463
861.253482	40987.279415	33.740480
861.998989	41031.016995	33.745498
863.140604	41085.596154	33.750516
863.973462	41143.069850	33.755533
864.945776	41191.186782	33.760551
865.351432	41257.101412	33.765568
866.744510	41301.104960	33.770586
867.740947	41353.797490	33.775604
868.318666	41410.818519	33.780621
869.574893	41452.149504	33.785639
870.134376	41501.014823	33.790656
870.967169	41543.228165	33.795674
871.837196	41598.116767	33.800692
873.018411	41650.875950	33.805709
873.829001	41707.905562	33.810727
874.624496	41759.074649	33.815744
875.322932	41801.771234	33.820762
876.074563	41856.122442	33.825780
877.283740	41904.520093	33.830797
878.443560	41959.357898	33.835815
879.347653	42011.857753	33.840832
880.151455	42052.040025	33.845850
881.431891	42095.329131	33.850868
882.180021	42142.996246	33.855885
883.335131	42183.705637	33.860903
883.807963	42242.408689	33.865920
884.844030	42273.111953	33.870938
885.640546	42325.338458	33.875956
886.304867	42382.259900	33.880973
887.236481	42419.285672	33.885991
887.894740	42476.322155	33.891008
888.593655	42516.869573	33.896026
889.471248	42573.530417	33.901044
890.336581	42617.372574	33.906061
891.258690	42674.735106	33.911079
892.158556	42727.224680	33.916096
893.131893	42766.717586	33.921114
893.942662	42814.977226	33.926132
894.295879	42863.555293	33.931149
895.420252	42897.629511	33.936167
896.094132	42962.975946	33.941184
896.903933	43003.323469	33.946202
897.517559	43068.559475	33.951220
898.349387	43119.384480	33.956237
899.634587	43173.996952	33.961255
900.271974	43228.647742	33.966272
901.302492	43275.779728	33.971290
902.431209	43329.582163	33.976308
903.127303	43392.193907	33.981325
904.440650	43446.385181	33.986343
904.997547	43497.627293	33.991360
906.389243	43554.418888	33.996378
907.012813	43605.410449	34.001396
907.895220	43657.765812	34.006413
909.006316	43718.555068	34.011431
910.064156	43769.523286	34.016448
910.793707	43839.550651	34.021466
911.988447	43884.203989	34.026484
912.780547	43945.492915	34.031501
913.883378	43994.531694	34.036519
914.543219	44052.887673	34.041536
915.646590	44099.149751	34.046554
916.669840	44157.550309	34.051572
917.745481	44215.936492	34.056589
918.929156	44255.759674	34.061607
919.668436	44325.717467	34.066624
920.483327	44366.389275	34.071642
921.400606	44410.524150	34.076660
922.190002	44477.729307	34.081677
923.616983	44524.738617	34.086695
924.127667	44590.811207	34.091712
925.221785	44630.788247	34.096730
926.065296	44677.813332	34.101748
927.208993	44736.297759	34.106765
928.079729	44782.559732	34.111783
928.816421	44838.014935	34.116800
929.993219	44893.875787	34.121818
931.508670	44936.235425	34.126836
931.879846	44995.840945	34.131853
933.098012	45044.142856	34.136871
933.637713	45098.604791	34.141888
934.751720	45148.719733	34.146906
935.840197	45199.673782	34.151924
936.591653	45242.836805	34.156941
937.323540	45289.937590	34.161959
938.344887	45345.077474	34.166976
938.870673	45402.066305	34.171994
940.083971	45453.324002	34.177012
940.600949	45513.768379	34.182029
942.025113	45573.128326	34.187047
943.151984	45638.835521	34.192064
943.533694	45691.590353	34.197082
944.913445	45739.343421	34.202100
945.718836	45792.791257	34.207117
946.840320	45844.412150	34.212135
947.526830	45902.047631	34.217152
948.280007	45958.179900	34.222170
949.899977	46017.225700	34.227188
950.604503	46078.787229	34.232205
951.521599	46127.012100	34.237223
952.320783	46183.915826	34.242240
953.427937	46235.932075	34.247258
954.436357	46288.330814	34.252276
955.219725	46349.836458	34.257293
956.315593	46392.682075	34.262311
956.911469	46437.560815	34.267328
957.674305	46474.448968	34.272346
958.956618	46524.471049	34.277364
959.503279	46579.334029	34.282381
960.240547	46639.468590	34.287399
961.320483	46690.617148	34.292416
962.263898	46748.575161	34.297434
963.289330	46803.117002	34.302452
964.176236	46859.882177	34.307469
965.527793	46910.210583	34.312487
966.242242	46961.062713	34.317504
966.979288	47037.153089	34.322522
968.235597	47087.775159	34.327540
969.206928	47144.078666	34.332557
970.054379	47207.664283	34.337575
971.361654	47260.322151	34.342592
972.132369	47316.784025	34.347610
973.018880	47366.692811	34.352628
973.775163	47427.984211	34.357645
975.279402	47485.729779	34.362663
976.006994	47549.879191	34.367680
976.946782	47619.531158	34.372698
978.475467	47661.931836	34.377716
979.374989	47733.121448	34.382733
980.870698	47785.681446	34.387751
981.416879	47833.474576	34.392768
982.698574	47884.619553	34.397786
984.154607	47938.419780	34.402804
984.882467	47990.935989	34.407821
985.364278	48036.500043	34.412839
986.483704	48098.286803	34.417856
987.215290	48161.836298	34.422874
988.691245	48207.213407	34.427892
989.678773	48277.290123	34.432909
990.498183	48318.974304	34.437927
991.547536	48378.375018	34.442944
992.357219	48433.087423	34.447962
993.558721	48489.288640	34.452980
994.090895	48549.707118	34.457997
995.266224	48611.461213	34.463015
996.315377	48670.027598	34.468032
997.212573	48736.589577	34.473050
998.485802	48798.866622	34.478068
999.019337	48861.316591	34.483085
1000.423281	48910.875705	34.488103
1001.626301	48971.443336	34.493120
1002.709608	49020.186122	34.498138
1004.478365	49066.493430	34.503156
1005.121653	49131.963819	34.508173
1005.952015	49190.964386	34.513191
1006.887147	49236.725589	34.518208
1007.991054	49293.292044	34.523226
1008.935923	49345.372476	34.528244
1009.988705	49397.689206	34.533261
1010.982945	49450.268298	34.538279
1012.046697	49497.851015	34.543296
1012.493169	49557.962902	34.548314
1013.981305	49614.159973	34.553332
1014.757796	49669.298114	34.558349
1016.065732	49719.525694	34.563367
1016.951179	49777.557447	34.568384
1018.051696	49832.860367	34.573402
1019.114345	49878.001821	34.578420
1019.745212	49939.635957	34.583437
1020.710759	49990.423901	34.588455
1021.644377	50036.351442	34.593472
1022.754492	50102.580356	34.598490
1023.645297	50155.974474	34.603508
1024.465875	50205.494863	34.608525
1025.380205	50258.246496	34.613543
1026.489410	50312.163569	34.618560
1027.149531	50369.036264	34.623578
1028.505393	50422.813744	34.628596
1029.281059	50477.144074	34.633613
1030.245660	50533.786016	34.638631
1031.147882	50585.034419	34.643648
1032.223278	50661.963378	34.648666
1033.300461	50705.686881	34.653684
1034.066702	50779.336501	34.658701
1035.758775	50826.222505	34.663719
1036.893653	50885.622657	34.668736
1037.912497	50960.157090	34.673754
1038.710681	51002.608755	34.678772
1039.814390	51060.799389	34.683789
1040.994021	51120.098227	34.688807
1041.982073	51183.229967	34.693824
1043.039743	51251.912762	34.698842
1044.321713	51309.778726	34.703860
1045.327551	51370.453155	34.708877
1046.472051	51432.630948	34.713895
1047.561047	51489.837884	34.718912
1048.135678	51548.998426	34.723930
1049.633110	51609.065005	34.728948
1050.650255	51669.093041	34.733965
1051.781938	51727.755536	34.738983
1052.615632	51787.806274	34.744000
1053.738971	51853.728089	34.749018
1054.814313	51916.841833	34.754036
1056.112143	51973.219989	34.759053
1057.004576	52040.855300	34.764071
1058.272534	52104.160862	34.769088
1059.270285	52163.541467	34.774106
1060.405253	52227.766713	34.779124
1061.532636	52282.685305	34.784141
1062.881817	52356.754879	34.789159
1063.632241	52408.144981	34.794176
1064.650971	52475.034092	34.799194
1066.136496	52531.675293	34.804212
1067.293651	52584.261325	34.809229
1067.781951	52649.069887	34.814247
1068.948989	52711.127344	34.819264
1070.389846	52767.801425	34.824282
1071.573993	52825.749760	34.829300
1072.709260	52882.218849	34.834317
1073.352998	52945.972460	34.839335
1074.547260	53005.640835	34.844352
1075.856307	53061.336461	34.849370
1076.815224	53122.516380	34.854388
1077.586513	53173.107582	34.859405
1078.691199	53223.779582	34.864423
1080.316601	53285.336504	34.869440
1081.244126	53350.907204	34.874458
1082.452999	53408.093756	34.879476
1083.564428	53465.529840	34.884493
1084.466263	53519.347615	34.889511
1085.527783	53576.507024	34.894528
1086.334831	53636.864106	34.899546
1088.109825	53682.970886	34.904564
1089.005749	53746.933987	34.909581
1090.077642	53795.859483	34.914599
1091.192605	53842.019286	34.919616
1092.127509	53905.831171	34.924634
1092.855714	53968.802306	34.929652
1094.366761	54013.938561	34.934669
1095.345819	54067.682221	34.939687
1096.567445	54115.439544	34.944704
1097.664233	54173.531455	34.949722
1098.568162	54208.252015	34.954740
1099.059670	54251.339804	34.959757
1100.206904	54308.266087	34.964775
1101.356297	54360.028326	34.969792
1102.653040	54409.324905	34.974810
1103.585623	54452.964177	34.979828
1104.653444	54520.509579	34.984845
1105.739190	54577.572705	34.989863
1106.603707	54629.740850	34.994880
1107.831195	54702.444662	34.999898
1109.163599	54753.134939	35.004916
1110.102637	54813.581955	35.009933
1111.168210	54878.818882	35.014951
1112.403432	54919.785361	35.019968
1113.092129	54991.447962	35.024986
1114.703188	55060.352735	35.030004
1115.980582	55118.874346	35.035021
1116.673578	55175.089108	35.040039
1118.119307	55238.634769	35.045056
1119.259544	55302.905577	35.050074
1120.337310	55355.035608	35.055092
1121.439522	55419.743023	35.060109
1122.781212	55490.729006	35.065127
1123.799764	55547.861951	35.070144
1124.918061	55601.929046	35.075162
1126.413319	55668.398234	35.080180
1127.439936	55732.219678	35.085197
1128.585343	55790.130749	35.090215
1129.576810	55856.369233	35.095232
1130.872227	55905.688128	35.100250
1131.971227	55961.467799	35.105268
1133.484020	56024.353214	35.110285
1134.616782	56087.424867	35.115303
1135.685994	56146.519545	35.120320
1136.740960	56210.907419	35.125338
1137.951550	56269.227149	35.130356
1139.367392	56330.970393	35.135373
1140.375102	56388.904479	35.140391
1141.354468	56442.931950	35.145408
1142.118212	56505.695411	35.150426
1143.171428	56565.059441	35.155444
1144.530520	56634.641113	35.160461
1145.855233	56704.658734	35.165479
1146.867998	56770.174932	35.170496
1148.443051	56828.268091	35.175514
1149.778755	56893.980898	35.180532
1151.204853	56948.711702	35.185549
1152.187145	57004.733597	35.190567
1153.501688	57053.931626	35.195584
1154.285375	57117.744177	35.200602
1155.867524	57177.242106	35.205620
1156.732117	57217.675649	35.210637
1157.653728	57282.922716	35.215655
1158.879403	57330.249180	35.220672
1160.308659	57390.404478	35.225690
1161.481960	57449.232921	35.230708
1162.455855	57504.959834	35.235725
1163.483747	57563.608791	35.240743
1164.796801	57624.966408	35.245760
1165.835692	57690.443057	35.250778
1166.686893	57745.284672	35.255796
1167.980778	57788.278562	35.260813
1168.572183	57866.218218	35.265831
1170.124318	57919.773272	35.270848
1171.212324	57988.534218	35.275866
1172.079407	58049.918433	35.280884
1173.489906	58099.204853	35.285901
1174.893694	58156.347014	35.290919
1175.758649	58207.833030	35.295936
1176.918466	58271.893563	35.300954
1177.643991	58325.832100	35.305972
1178.892605	58370.954432	35.310989
1180.495096	58443.908411	35.316007
1181.459099	58500.696174	35.321024
1182.412523	58551.998182	35.326042
1183.524489	58606.940179	35.331060
1185.003362	58671.837936	35.336077
1186.156137	58744.072053	35.341095
1187.068134	58797.020380	35.346112
1188.550556	58859.601521	35.351130
1189.445813	58926.705356	35.356148
1191.298944	58995.982335	35.361165
1191.997037	59062.332558	35.366183
1193.278773	59120.932902	35.371200
1194.839379	59191.477827	35.376218
1196.051411	59258.393740	35.381236
1197.115413	59305.375953	35.386253
1198.063141	59373.814674	35.391271
1199.344768	59439.163117	35.396288
1200.856015	59509.203998	35.401306
1201.699183	59572.254171	35.406324
1203.144494	59635.330506	35.411341
1204.153737	59704.197270	35.416359
1206.012995	59763.221457	35.421376
1207.108676	59838.968074	35.426394
1208.277611	59903.227713	35.431412
1209.642910	59960.456117	35.436429
1210.771518	60032.735828	35.441447
1212.328008	60085.997504	35.446464
1213.480108	60152.602442	35.451482
1214.598861	60224.858946	35.456500
1216.085983	60273.302269	35.461517
1217.145962	60343.599760	35.466535
1218.451688	60404.864295	35.471552
1219.434381	60465.502260	35.476570
1220.911084	60533.139823	35.481588
1222.067046	60585.674060	35.486605
1223.208080	60644.857131	35.491623
1224.548678	60707.838696	35.496640
1226.074366	60765.733841	35.501658
1227.518974	60830.148992	35.506676
1228.108573	60886.279322	35.511693
1229.498732	60946.101427	35.516711
1230.766840	61009.664814	35.521728
1232.072482	61064.398471	35.526746
1233.193896	61132.409810	35.531764
1234.629132	61193.744666	35.536781
1235.813004	61262.006118	35.541799
1237.149029	61308.506503	35.546816
1238.379666	61380.888164	35.551834
1239.723150	61446.479168	35.556852
1241.013968	61500.019731	35.561869
1242.237518	61549.209486	35.566887
1243.592306	61606.437058	35.571904
1245.037543	61651.363782	35.576922
1246.179221	61724.583300	35.581940
1247.332187	61766.637782	35.586957
1248.266099	61831.812837	35.591975
1249.453795	61888.294939	35.596992
1250.871892	61950.172434	35.602010
1251.965749	62012.879463	35.607028
1253.254654	62069.548703	35.612045
1254.716094	62127.798954	35.617063
1256.092594	62176.611525	35.622080
1257.337338	62228.331433	35.627098
1258.075019	62267.603148	35.632116
1259.285323	62310.814360	35.637133
1260.469567	62370.893728	35.642151
1261.730374	62419.788194	35.647168
1262.600119	62471.940807	35.652186
1263.635370	62520.813809	35.657204
1264.943243	62590.452210	35.662221
1266.166001	62652.279749	35.667239
1267.427779	62722.102987	35.672256
1268.570964	62765.907901	35.677274
1269.913554	62833.275255	35.682292
1271.398530	62889.865040	35.687309
1272.607635	62954.563172	35.692327
1273.862489	63018.963108	35.697344
1275.660555	63079.979978	35.702362
1276.614347	63155.993248	35.707380
1278.086310	63208.603893	35.712397
1279.362971	63275.482655	35.717415
1280.554176	63334.360461	35.722432
1281.661627	63399.892310	35.727450
1282.944058	63460.870554	35.732468
1284.386467	63526.230019	35.737485
1285.606374	63601.747186	35.742503
1287.047297	63666.246284	35.747520
1288.237342	63736.571061	35.752538
1289.883335	63806.058649	35.757556
1291.374399	63864.112092	35.762573
1292.633234	63931.115688	35.767591
1293.978803	63994.149170	35.772608
1295.339833	64057.250030	35.777626
1296.490245	64133.387437	35.782644
1297.930489	64188.651387	35.787661
1299.049475	64260.134635	35.792679
1300.484852	64322.160950	35.797696
1301.745222	64374.167767	35.802714
1302.982647	64454.445561	35.807732
1304.579193	64513.813484	35.812749
1305.792329	64583.339338	35.817767
1306.889478	64649.547152	35.822784
1308.009416	64708.046836	35.827802
1309.461735	64777.187585	35.832820
1310.675791	64846.657046	35.837837
1312.256341	64923.514558	35.842855
1313.578011	64981.704739	35.847872
1314.971184	65047.474741	35.852890
1316.365297	65123.431391	35.857908
1317.699478	65189.350281	35.862925
1319.265082	65254.486052	35.867943
1320.427335	65316.690532	35.872960
1322.033189	65379.237247	35.877978
1323.316603	65437.060936	35.882996
1324.665386	65497.533596	35.888013
1326.039105	65565.802460	35.893031
1326.866145	65628.655310	35.898048
1328.443970	65691.865629	35.903066
1329.625032	65763.887915	35.908084
1331.012311	65822.747207	35.913101
1332.524833	65891.862600	35.918119
1333.659951	65942.239822	35.923136
1335.375646	66003.884520	35.928154
1336.464259	66084.918898	35.933172
1337.824623	66138.331917	35.938189
1338.969235	66197.318705	35.943207
1340.384454	66264.107768	35.948224
1342.202048	66324.724288	35.953242
1343.074529	66389.768885	35.958260
1344.473563	66445.101227	35.963277
1345.702144	66493.704799	35.968295
1346.913932	66544.071217	35.973312
1348.531533	66591.303485	35.978330
1349.440642	66643.388968	35.983348
1350.385549	66695.741205	35.988365
1352.223819	66753.487383	35.993383
1353.550241	66808.736914	35.998400
1355.079945	66854.596845	36.003418
1356.367321	66924.725344	36.008436
1357.705810	66975.693271	36.013453
1359.041765	67030.454268	36.018471
1359.990022	67083.085365	36.023488
1361.629085	67144.409265	36.028506
1362.673056	67209.600066	36.033524
1364.268254	67269.626836	36.038541
1365.451027	67336.081541	36.043559
1366.488955	67393.606217	36.048576
1368.377556	67464.161281	36.053594
1369.311512	67539.032185	36.058612
1370.931455	67607.337649	36.063629
1372.058475	67683.824984	36.068647
1373.214124	67756.857298	36.073664
1374.892134	67829.586445	36.078682
1376.336594	67897.369295	36.083700
1378.145661	67973.985008	36.088717
1379.575696	68044.847731	36.093735
1380.796369	68108.848122	36.098752
1382.470509	68183.421426	36.103770
1383.579339	68248.224813	36.108788
1385.182355	68316.623466	36.113805
1386.380226	68386.706668	36.118823
1388.135022	68453.701587	36.123840
1389.386963	68520.686747	36.128858
1390.682634	68597.492327	36.133876
1392.242428	68663.365912	36.138893
1393.812427	68735.538333	36.143911
1395.014273	68811.548752	36.148928
1396.909583	68874.831252	36.153946
1397.845862	68952.219698	36.158964
1399.634995	69017.887330	36.163981
1401.264871	69089.209214	36.168999
1402.411898	69145.834259	36.174016
1403.948127	69214.695327	36.179034
1405.413082	69282.807889	36.184052
1406.775999	69343.262129	36.189069
1407.846818	69416.363089	36.194087
1409.352084	69475.357973	36.199104
1410.910984	69545.470131	36.204122
1412.638125	69624.313495	36.209140
1414.137013	69676.768736	36.214157
1415.502826	69742.314509	36.219175
1416.836801	69819.472329	36.224192
1418.554042	69871.304894	36.229210
1419.484178	69943.542853	36.234228
1420.863022	70001.608893	36.239245
1422.273189	70071.942056	36.244263
1423.777486	70149.884727	36.249280
1425.404678	70210.622573	36.254298
1426.595605	70266.679624	36.259316
1428.242550	70337.457700	36.264333
1429.617226	70397.956887	36.269351
1430.598348	70466.901841	36.274368
1432.265357	70537.651991	36.279386
1433.658917	70613.384393	36.284404
1435.059265	70671.258592	36.289421
1436.521807	70745.954733	36.294439
1437.413249	70813.964779	36.299456
1439.188474	70874.161744	36.304474
1440.542966	70944.619965	36.309492
1442.222022	70990.584219	36.314509
1443.225077	71043.341468	36.319527
1444.228022	71107.522669	36.324544
1445.675856	71175.180601	36.329562
1447.310033	71241.251738	36.334580
1448.474140	71303.001831	36.339597
1450.223848	71362.773305	36.344615
1451.255418	71439.945261	36.349632
1452.750536	71503.974406	36.354650
1454.539009	71576.266179	36.359668
1455.717607	71642.270319	36.364685
1457.225072	71712.238048	36.369703
1458.711693	71785.172912	36.374720
1460.100998	71845.685828	36.379738
1461.725421	71928.491167	36.384756
1463.285934	72011.712063	36.389773
1464.961026	72081.489887	36.394791
1466.169367	72162.182627	36.399808
1467.782851	72216.594530	36.404826
1469.505088	72303.666690	36.409844
1470.787250	72374.545371	36.414861
1472.518564	72440.072368	36.419879
1473.801955	72515.422206	36.424896
1475.290284	72588.637675	36.429914
1476.874452	72672.984205	36.434932
1478.503486	72742.112370	36.439949
1480.159678	72815.074207	36.444967
1481.635637	72886.861201	36.449984
1483.050254	72962.521087	36.455002
1485.102972	73023.984141	36.460020
1486.446875	73092.575219	36.465037
1488.166844	73164.704753	36.470055
1489.987471	73235.336804	36.475072
1491.517268	73291.739924	36.480090
1493.172551	73354.684552	36.485108
1494.312376	73426.791609	36.490125
1495.850231	73477.912097	36.495143
1497.167122	73548.573163	36.500160
1498.992669	73619.433459	36.505178
1499.948245	73677.738545	36.510196
1501.613533	73749.232250	36.515213
1503.162430	73822.302320	36.520231
1504.816587	73905.349854	36.525248
1506.466021	73970.741462	36.530266
1508.168806	74031.514310	36.535284
1509.554855	74088.473612	36.540301
1511.468193	74148.479121	36.545319
1512.510473	74217.804301	36.550336
1513.792300	74285.610186	36.555354
1515.314250	74358.508612	36.560372
1516.499354	74430.319967	36.565389
1518.425432	74501.154210	36.570407
1519.724810	74567.526735	36.575424
1521.566836	74634.270491	36.580442
1522.894285	74709.568988	36.585460
1524.209336	74787.288987	36.590477
1526.172832	74848.035557	36.595495
1527.190507	74921.508450	36.600512
1528.826104	75005.043647	36.605530
1530.236904	75070.931306	36.610548
1531.644383	75147.358525	36.615565
1533.461741	75205.950070	36.620583
1535.002584	75293.047741	36.625600
1536.505942	75357.806922	36.630618
1538.174781	75434.878072	36.635636
1539.553046	75503.520636	36.640653
1540.879071	75566.838693	36.645671
1542.284655	75630.410457	36.650688
1543.253907	75687.197719	36.655706
1544.963183	75736.914982	36.660724
1546.359814	75810.698339	36.665741
1547.785403	75886.884146	36.670759
1549.128555	75963.437756	36.675776
1550.798608	76023.650220	36.680794
1552.539495	76090.388092	36.685812
1553.907396	76177.376346	36.690829
1555.599439	76242.361470	36.695847
1557.103035	76316.002790	36.700864
1558.726767	76382.848394	36.705882
1560.267389	76465.186901	36.710900
1561.774930	76549.532314	36.715917
1563.405712	76615.706007	36.720935
1564.766429	76698.694094	36.725952
1566.163567	76769.591761	36.730970
1568.347599	76845.826242	36.735988
1569.794708	76933.133883	36.741005
1571.846352	77014.051292	36.746023
1573.326486	77095.235739	36.751040
1575.088901	77165.405875	36.756058
1576.619304	77230.532677	36.761076
1578.214776	77312.865168	36.766093
1580.108629	77384.307426	36.771111
1581.071168	77462.647677	36.776128
1582.806556	77547.809280	36.781146
1584.671254	77636.726000	36.786164
1586.014618	77716.375528	36.791181
1587.663346	77788.845323	36.796199
1589.304657	77869.284764	36.801216
1591.287234	77949.164300	36.806234
1592.486087	78026.278365	36.811252
1594.417578	78104.570149	36.816269
1595.574570	78178.853496	36.821287
1597.271151	78260.894315	36.826304
1599.382331	78339.196652	36.831322
1601.452596	78414.503195	36.836340
1602.902944	78490.654408	36.841357
1604.304261	78567.092213	36.846375
1605.794403	78653.309118	36.851392
1607.544352	78728.742667	36.856410
1609.404065	78801.384816	36.861428
1610.897494	78871.626765	36.866445
1612.840196	78949.830526	36.871463
1614.286521	79023.855505	36.876480
1616.141507	79094.446835	36.881498
1617.901260	79168.549836	36.886516
1619.088338	79254.892067	36.891533
1620.958530	79315.840608	36.896551
1622.705425	79392.910736	36.901568
1623.839497	79459.080365	36.906586
1625.823234	79533.453345	36.911604
1627.150255	79602.405627	36.916621
1629.002307	79679.966857	36.921639
1630.001942	79759.574741	36.926656
1631.809720	79841.716883	36.931674
1633.899979	79919.076804	36.936692
1635.143425	79994.998496	36.941709
1636.682701	80070.886765	36.946727
1638.377882	80145.661287	36.951744
1639.964255	80217.032338	36.956762
1642.106172	80290.787141	36.961780
1643.677804	80371.878250	36.966797
1645.114187	80436.938673	36.971815
1646.957756	80512.413113	36.976832
1648.904579	80591.267006	36.981850
1650.645193	80642.609980	36.986868
1651.747793	80706.545011	36.991885
1653.089068	80766.299904	36.996903
1654.876034	80818.953578	37.001920
1656.159601	80889.879633	37.006938
1657.663717	80955.830206	37.011956
1658.855975	81026.694881	37.016973
1660.605665	81095.394670	37.021991
1662.393911	81160.705786	37.027008
1663.787586	81234.314126	37.032026
1665.440985	81314.685674	37.037044
1666.990506	81406.755265	37.042061
1668.811686	81476.990519	37.047079
1670.013932	81559.903993	37.052096
1671.961845	81648.237765	37.057114
1673.634287	81722.982062	37.062132
1675.205104	81809.221465	37.067149
1677.124158	81896.762326	37.072167
1678.688717	81991.694905	37.077184
1680.487412	82079.964695	37.082202
1682.048076	82157.312341	37.087220
1683.753042	82252.515238	37.092237
1686.015765	82339.458872	37.097255
1687.676983	82431.717058	37.102272
1689.165799	82517.540672	37.107290
1691.044829	82597.044331	37.112308
1692.729000	82699.081299	37.117325
1694.846756	82778.763505	37.122343
1696.877061	82856.242293	37.127360
1698.528043	82945.019381	37.132378
1700.354740	83014.712775	37.137396
1701.988172	83101.149051	37.142413
1703.813430	83171.197831	37.147431
1706.086426	83252.706984	37.152448
1707.954285	83329.008778	37.157466
1709.488461	83399.420443	37.162484
1710.773835	83478.652032	37.167501
1712.297534	83545.923359	37.172519
1714.610279	83626.147617	37.177536
1715.907829	83712.993101	37.182554
1717.546705	83791.384646	37.187572
1718.930727	83876.025033	37.192589
1721.111639	83958.843054	37.197607
1722.867484	84043.919917	37.202624
1724.434563	84130.661135	37.207642
1726.210319	84215.634025	37.212660
1727.871121	84296.899856	37.217677
1729.707405	84382.015821	37.222695
1731.752783	84452.045975	37.227712
1733.113004	84540.949564	37.232730
1735.031389	84622.758884	37.237748
1736.750095	84709.072646	37.242765
1738.207290	84787.317955	37.247783
1740.317387	84871.214090	37.252800
1741.958272	84956.336995	37.257818
1743.867880	85045.092810	37.262836
1745.288168	85122.673222	37.267853
1747.086023	85208.659311	37.272871
1748.953349	85294.127923	37.277888
1750.599243	85374.550144	37.282906
1752.649737	85466.250355	37.287924
1754.056582	85546.697794	37.292941
1755.861903	85633.000771	37.297959
1757.431843	85705.059822	37.302976
1759.303580	85797.853484	37.307994
1760.789271	85875.919883	37.313012
1762.534207	85970.153180	37.318029
1764.515289	86050.879639	37.323047
1766.226509	86125.515359	37.328064
1767.881494	86209.169811	37.333082
1769.550651	86271.406675	37.338100
1771.316988	86345.413410	37.343117
1772.532800	86414.957232	37.348135
1774.650490	86488.706597	37.353152
1776.307762	86566.633955	37.358170
1778.008447	86640.981191	37.363188
1779.163297	86717.834417	37.368205
1781.050439	86793.166635	37.373223
1783.330813	86883.238660	37.378240
1784.801879	86971.511431	37.383258
1786.465224	87056.003378	37.388276
1787.959802	87158.960228	37.393293
1790.297768	87241.382928	37.398311
1792.215293	87338.520965	37.403328
1794.019939	87428.162222	37.408346
1796.229050	87504.523051	37.413364
1797.638749	87594.974301	37.418381
1799.430109	87690.156334	37.423399
1801.205069	87780.652377	37.428416
1802.652749	87883.619110	37.433434
1804.729914	87975.234344	37.438452
1806.437953	88070.722120	37.443469
1808.305450	88164.297009	37.448487
1810.307391	88265.454845	37.453504
1812.153525	88359.565956	37.458522
1814.051774	88453.846632	37.463540
1815.890943	88556.779799	37.468557
1817.614053	88650.353479	37.473575
1819.232518	88751.408241	37.478592
1821.228502	88859.526534	37.483610
1823.615785	88945.444065	37.488628
1825.792045	89042.876738	37.493645
1827.402449	89140.347587	37.498663
1829.905622	89231.418476	37.503680
1831.232490	89323.256690	37.508698
1833.222634	89410.948610	37.513716
1834.978901	89511.401425	37.518733
1836.906366	89601.169470	37.523751
1838.632006	89699.105707	37.528768
1840.130163	89794.834660	37.533786
1841.965058	89887.393543	37.538804
1844.402127	89977.754674	37.543821
1845.746329	90084.724737	37.548839
1848.233830	90182.581362	37.553856
1849.665012	90277.397167	37.558874
1851.474076	90363.992271	37.563892
1853.306037	90472.116740	37.568909
1855.328154	90565.320134	37.573927
1857.304582	90655.045664	37.578944
1858.775895	90768.512624	37.583962
1860.935157	90849.376434	37.588980
1863.018216	90963.635576	37.593997
1864.390353	91051.226235	37.599015
1866.690469	91145.566610	37.604032
1868.222891	91247.821968	37.609050
1870.117987	91343.873973	37.614068
1871.629702	91435.829153	37.619085
1873.669642	91540.350804	37.624103
1875.634981	91639.244452	37.629120
1877.448356	91744.005049	37.634138
1879.762990	91834.200815	37.639156
1881.561206	91936.999932	37.644173
1883.527964	92041.408022	37.649191
1885.474651	92132.067835	37.654208
1887.026702	92231.598439	37.659226
1888.925750	92327.868416	37.664244
1890.736753	92421.655584	37.669261
1892.318992	92503.171799	37.674279
1894.280310	92586.314640	37.679296
1895.549682	92667.601411	37.684314
1897.332575	92756.894504	37.689332
1899.188264	92855.517755	37.694349
1900.881101	92950.250299	37.699367
1902.785818	93042.782586	37.704384
1904.527531	93144.238416	37.709402
1906.412860	93239.372680	37.714420
1908.162430	93342.868598	37.719437
1909.715775	93466.054489	37.724455
1912.033788	93567.066640	37.729472
1913.674680	93673.571989	37.734490
1915.498603	93786.842937	37.739508
1917.741224	93898.109483	37.744525
1919.433060	94018.031068	37.749543
1921.549946	94138.355594	37.754560
1923.388962	94252.221629	37.759578
1925.247942	94355.970018	37.764596
1927.421261	94483.512017	37.769613
1929.559671	94596.343790	37.774631
1931.673403	94708.951677	37.779648
1933.806740	94836.767574	37.784666
1935.411932	94939.087265	37.789684
1938.152950	95046.958955	37.794701
1939.959342	95165.105146	37.799719
1942.385862	95273.774702	37.804736
1944.215789	95384.198519	37.809754
1946.334898	95494.564801	37.814772
1948.037673	95599.140368	37.819789
1949.862294	95718.553393	37.824807
1951.900773	95827.602499	37.829824
1953.599398	95947.048788	37.834842
1956.045371	96065.047606	37.839860
1957.975494	96178.171229	37.844877
1959.635801	96288.041681	37.849895
1961.520380	96402.985931	37.854912
1963.236243	96531.710726	37.859930
1965.502000	96634.034019	37.864948
1967.290982	96763.331430	37.869965
1969.592988	96888.632092	37.874983
1971.887182	96995.946612	37.880000
1973.700011	97123.416363	37.885018
1975.884978	97234.767232	37.890036
1978.081569	97349.247789	37.895053
1979.707197	97464.933643	37.900071
1981.769896	97579.245834	37.905088
1983.745777	97704.943035	37.910106
1985.483431	97821.119728	37.915124
1987.381477	97945.879304	37.920141
1989.418519	98076.271502	37.925159
1991.490687	98182.204977	37.930176
1992.919328	98309.650870	37.935194
1994.899887	98439.166004	37.940212
1997.028608	98565.489216	37.945229
1998.662886	98699.585298	37.950247
2001.019163	98823.693462	37.955264
2002.468953	98964.234163	37.960282
2004.381597	99097.679849	37.965300
2006.597445	99229.963043	37.970317
2008.440867	99374.589432	37.975335
2010.566749	99509.905072	37.980352
2012.548558	99642.023742	37.985370
2014.312824	99784.914866	37.990388
2016.742330	99925.686795	37.995405
2018.285720	100061.007145	38.000423
2020.653677	100196.325819	38.005440
2022.432786	100333.423336	38.010458
2024.356713	100449.440946	38.015476
2026.670951	100560.238017	38.020493
2027.693318	100689.113425	38.025511
2030.005331	100804.437685	38.030528
2032.137624	100937.324127	38.035546
2033.898422	101074.554415	38.040564
2035.796485	101201.507227	38.045581
2037.464494	101343.913149	38.050599
2039.641233	101468.376513	38.055616
2041.594120	101615.315869	38.060634
2043.334874	101770.352480	38.065652
2045.689802	101909.445768	38.070669
2047.321672	102064.716338	38.075687
2049.369958	102207.966678	38.080704
2051.911661	102361.815764	38.085722
2053.850056	102507.328701	38.090740
2056.074100	102666.211598	38.095757
2057.798624	102815.537595	38.100775
2060.039431	102965.163848	38.105792
2061.949687	103121.346734	38.110810
2064.125473	103277.615598	38.115828
2066.179366	103426.411013	38.120845
2068.441129	103598.656084	38.125863
2070.620326	103762.064973	38.130880
2072.924898	103918.747784	38.135898
2075.145927	104075.457082	38.140916
2077.186254	104239.955089	38.145933
2079.188241	104402.152267	38.150951
2081.348215	104548.539694	38.155968
2083.756637	104713.261375	38.160986
2085.508920	104876.222639	38.166004
2087.971331	105031.960355	38.171021
2089.906887	105205.025495	38.176039
2092.211186	105353.638134	38.181056
2094.382490	105513.062683	38.186074
2096.683033	105672.746718	38.191092
2098.740778	105841.725784	38.196109
2101.119603	105985.739431	38.201127
2103.214634	106154.955140	38.206144
2105.014104	106310.269902	38.211162
2107.018598	106470.612647	38.216180
2109.579658	106633.874260	38.221197
2111.527483	106794.924802	38.226215
2113.709139	106951.349261	38.231232
2115.833692	107112.322924	38.236250
2117.425634	107270.451506	38.241268
2120.031729	107437.640821	38.246285
2122.129084	107596.997913	38.251303
2124.536522	107759.502729	38.256320
2126.754174	107923.699164	38.261338
2128.617902	108086.125737	38.266356
2131.059058	108238.368861	38.271373
2132.799439	108400.068041	38.276391
2134.787005	108562.439427	38.281408
2137.136512	108738.741994	38.286426
2139.165886	108903.112015	38.291444
2141.526895	109061.267941	38.296461
2143.718715	109226.970944	38.301479
2145.709480	109385.325757	38.306496
2147.810986	109549.890435	38.311514
2149.935658	109720.868985	38.316532
2152.340674	109878.527151	38.321549
2154.178946	110050.452489	38.326567
2156.334641	110210.928378	38.331584
2158.333343	110385.201679	38.336602
2159.904049	110555.827102	38.341620
2162.608476	110714.963954	38.346637
2164.386480	110884.062093	38.351655
2166.545094	111043.678950	38.356672
2168.507407	111189.846482	38.361690
2170.121644	111350.906842	38.366708
2172.343067	111507.725947	38.371725
2173.937800	111684.529122	38.376743
2176.143333	111851.611943	38.381760
2178.226380	112012.703397	38.386778
2179.892909	112194.634106	38.391796
2181.776939	112368.453134	38.396813
2184.195437	112560.413821	38.401831
2186.161628	112738.926912	38.406848
2188.691569	112928.893681	38.411866
2190.641192	113130.696219	38.416884
2193.010120	113305.788244	38.421901
2195.406702	113508.588293	38.426919
2197.092938	113706.275344	38.431936
2199.521198	113904.151763	38.436954
2201.400001	114097.879157	38.441972
2203.625857	114297.526922	38.446989
2205.718443	114520.495229	38.452007
2208.132845	114723.400706	38.457024
2210.778386	114917.367602	38.462042
2212.903244	115135.578431	38.467060
2215.549074	115344.653202	38.472077
2217.645830	115545.279186	38.477095
2220.457697	115746.073413	38.482112
2222.605881	115946.363755	38.487130
2224.897211	116155.561984	38.492148
2227.139009	116348.496086	38.497165
2229.484128	116564.740276	38.502183
2231.336456	116769.216204	38.507200
2234.290011	116967.496157	38.512218
2236.181865	117176.851390	38.517236
2238.525524	117377.220294	38.522253
2240.598018	117587.107642	38.527271
2242.629170	117798.473980	38.532288
2245.179040	118011.840548	38.537306
2247.328509	118223.939117	38.542324
2249.622558	118439.085852	38.547341
2252.187146	118648.267880	38.552359
2254.188849	118868.206730	38.557376
2256.663763	119072.737243	38.562394
2258.612629	119290.390893	38.567412
2260.765756	119505.844747	38.572429
2263.233936	119720.552862	38.577447
2265.619899	119938.535028	38.582464
2267.943045	120159.889742	38.587482
2269.911874	120381.504115	38.592500
2272.300881	120589.240048	38.597517
2274.797424	120811.053387	38.602535
2276.625775	121036.257980	38.607552
2278.700788	121260.943246	38.612570
2280.832203	121490.010092	38.617588
2282.999250	121714.861161	38.622605
2285.464762	121957.515246	38.627623
2287.954587	122181.430507	38.632640
2290.131570	122409.912053	38.637658
2292.408055	122633.102118	38.642676
2295.002699	122853.757263	38.647693
2296.882434	123093.300474	38.652711
2299.264616	123330.914383	38.657728
2301.466078	123552.193093	38.662746
2303.944468	123786.420198	38.667764
2306.389832	124002.893298	38.672781
2309.221142	124233.921655	38.677799
2311.547885	124458.205076	38.682816
2313.804045	124680.179193	38.687834
2316.054068	124896.319753	38.692852
2318.757869	125087.791464	38.697869
2320.927078	125274.146247	38.702887
2322.841585	125474.052916	38.707904
2325.332244	125673.477146	38.712922
2327.385470	125873.173771	38.717940
2329.514104	126071.692394	38.722957
2331.592343	126281.549183	38.727975
2333.968937	126491.411117	38.732992
2336.317009	126692.220110	38.738010
2338.094448	126922.705441	38.743028
2340.283381	127134.033635	38.748045
2342.318973	127369.746204	38.753063
2344.382586	127600.913705	38.758080
2346.469546	127841.645050	38.763098
2348.531229	128081.518997	38.768116
2350.894391	128329.467114	38.773133
2353.270606	128577.313154	38.778151
2355.163149	128835.627452	38.783168
2357.874777	129093.815197	38.788186
2360.095775	129355.189767	38.793204
2362.626675	129603.081069	38.798221
2365.217982	129882.874424	38.803239
2367.386640	130135.799152	38.808256
2370.313521	130396.701740	38.813274
2372.460318	130669.248773	38.818292
2374.637298	130916.505210	38.823309
2377.374395	131183.113889	38.828327
2379.836222	131458.458805	38.833344
2382.610130	131716.462301	38.838362
2385.108727	131980.245607	38.843380
2387.810168	132234.558464	38.848397
2390.206049	132498.475167	38.853415
2392.560287	132760.534727	38.858432
2395.325651	133007.444534	38.863450
2397.864859	133283.753190	38.868468
2400.298704	133528.649484	38.873485
2402.674614	133796.485281	38.878503
2404.894733	134060.654529	38.883520
2406.992972	134329.882016	38.888538
2409.754892	134591.875934	38.893556
2411.732708	134868.485268	38.898573
2414.261351	135129.592491	38.903591
2416.396965	135412.081054	38.908608
2419.130047	135679.681875	38.913626
2420.947739	135959.672977	38.918644
2423.602198	136234.547841	38.923661
2426.287111	136531.207986	38.928679
2428.254480	136825.165141	38.933696
2430.565297	137099.730940	38.938714
2432.841867	137382.285763	38.943732
2435.892634	137672.944400	38.948749
2438.435097	137952.897703	38.953767
2440.485160	138234.427165	38.958784
2443.106724	138521.554198	38.963802
2445.356308	138807.332540	38.968820
2447.970583	139095.327168	38.973837
2450.585588	139384.097564	38.978855
2452.619837	139669.394492	38.983872
2455.093315	139958.406261	38.988890
2457.869729	140252.055303	38.993908
2460.325539	140545.388262	38.998925
2462.700751	140821.729726	39.003943
2464.834897	141125.548510	39.008960
2467.457379	141414.533039	39.013978
2469.762564	141711.259787	39.018996
2472.012408	142002.336691	39.024013
2474.609547	142292.447224	39.029031
2476.464158	142590.531614	39.034048
2479.346837	142856.588647	39.039066
2481.734856	143139.375819	39.044084
2484.122913	143415.653791	39.049101
2486.343350	143688.431223	39.054119
2488.176491	143969.977286	39.059136
2490.938384	144259.870495	39.064154
2492.936015	144550.468755	39.069172
2495.105522	144843.529434	39.074189
2497.461412	145147.262067	39.079207
2499.594471	145463.126988	39.084224
2502.177768	145762.195082	39.089242
2504.541084	146086.303164	39.094260
2506.879588	146401.240577	39.099277
2509.034274	146730.754222	39.104295
2511.702085	147069.632947	39.109312
2514.191538	147401.357750	39.114330
2516.456765	147737.587562	39.119348
2518.708670	148085.803601	39.124365
2521.054352	148427.851225	39.129383
2523.390038	148797.738271	39.134400
2525.593814	149158.420673	39.139418
2528.164809	149527.806324	39.144436
2530.924077	149886.858168	39.149453
2533.440759	150264.609499	39.154471
2536.408959	150634.422925	39.159488
2539.453742	150990.962197	39.164506
2541.896093	151362.220998	39.169524
2544.622891	151728.614220	39.174541
2547.469989	152088.644185	39.179559
2550.183116	152456.136006	39.184576
2552.867573	152816.119940	39.189594
2555.494981	153186.397220	39.194612
2557.741998	153557.447293	39.199629
2560.114721	153916.941153	39.204647
2562.648353	154300.962724	39.209664
2565.445596	154672.073605	39.214682
2568.249123	155046.283319	39.219700
2570.714636	155419.583538	39.224717
2573.746761	155798.205393	39.229735
2576.255572	156175.096217	39.234752
2578.660588	156550.990106	39.239770
2581.316689	156931.264889	39.244788
2583.964644	157301.933354	39.249805
2586.589415	157672.290363	39.254823
2589.140143	158055.737105	39.259840
2591.684228	158440.418736	39.264858
2594.535353	158830.170927	39.269876
2596.653395	159211.610602	39.274893
2599.258569	159604.199124	39.279911
2601.806378	159993.828371	39.284928
2604.227756	160386.145881	39.289946
2606.664783	160781.865808	39.294964
2609.262317	161178.756499	39.299981
2611.854539	161581.147753	39.304999
2614.348236	161983.226856	39.310016
2617.159465	162383.316327	39.315034
2619.565930	162779.015289	39.320052
2621.286395	163199.327343	39.325069
2623.864904	163619.088902	39.330087
2626.567614	164039.925573	39.335104
2629.327979	164455.512312	39.340122
2631.662002	164886.429361	39.345140
2634.013831	165307.773241	39.350157
2636.906646	165732.348910	39.355175
2639.047127	166166.884765	39.360192
2641.583726	166590.416842	39.365210
2644.205495	167029.885330	39.370228
2646.744008	167456.660043	39.375245
2649.295894	167885.339785	39.380263
2651.418214	168301.925568	39.385280
2653.879786	168713.889761	39.390298
2656.413906	169141.056149	39.395316
2659.085788	169569.930322	39.400333
2661.579989	169995.660472	39.405351
2664.051877	170432.303612	39.410368
2666.879761	170872.474314	39.415386
2669.751043	171304.755649	39.420404
2672.406894	171734.025729	39.425421
2674.912088	172170.178530	39.430439
2677.233669	172634.068997	39.435456
2679.687910	173093.433764	39.440474
2682.257912	173542.231174	39.445492
2685.002238	174015.802997	39.450509
2687.903730	174479.181924	39.455527
2690.427325	174953.454119	39.460544
2693.917782	175417.216143	39.465562
2696.874226	175877.521504	39.470580
2698.979475	176344.083156	39.475597
2701.952746	176816.810059	39.480615
2705.060370	177290.356701	39.485632
2707.345953	177767.234584	39.490650
2710.048182	178242.576908	39.495668
2712.532720	178725.397310	39.500685
2715.570589	179207.117925	39.505703
2718.355188	179707.700426	39.510720
2720.702948	180191.388327	39.515738
2723.416575	180686.780824	39.520756
2725.688863	181187.248444	39.525773
2728.347766	181688.267857	39.530791
2731.066225	182202.817944	39.535808
2734.051394	182716.033787	39.540826
2736.820269	183221.768219	39.545844
2739.544392	183780.697246	39.550861
2742.364679	184324.146483	39.555879
2744.793534	184837.765255	39.560896
2747.828458	185367.166314	39.565914
2750.493726	185897.694697	39.570932
2752.954093	186421.298401	39.575949
2755.923171	186944.012365	39.580967
2758.220879	187484.588257	39.585984
2761.011422	188014.447262	39.591002
2764.240364	188555.848019	39.596020
2766.671090	189094.912449	39.601037
2769.636697	189622.414929	39.606055
2772.476024	190175.517656	39.611072
2775.384134	190715.937460	39.616090
2778.135314	191257.451100	39.621108
2780.813100	191803.703174	39.626125
2784.029551	192341.313401	39.631143
2786.916689	192885.911890	39.636160
2789.688719	193423.342265	39.641178
2792.932812	193958.846785	39.646196
2795.484593	194500.126237	39.651213
2798.576789	195035.404883	39.656231
2801.509187	195573.149171	39.661248
2804.044917	196111.237015	39.666266
2807.087040	196646.402753	39.671284
2809.917819	197191.764208	39.676301
2812.505178	197729.113426	39.681319
2815.343880	198281.336155	39.686336
2817.541862	198817.454677	39.691354
2820.475110	199370.581020	39.696372
2822.926367	199926.451903	39.701389
2825.846693	200470.921968	39.706407
2828.687456	201034.178551	39.711424
2831.124172	201582.080978	39.716442
2833.571298	202109.229731	39.721460
2836.093009	202645.919735	39.726477
2838.694150	203170.329466	39.731495
2841.002455	203717.852086	39.736512
2843.665069	204262.501172	39.741530
2846.787164	204821.102264	39.746548
2849.206453	205384.412749	39.751565
2851.530863	205949.416209	39.756583
2854.248781	206516.417278	39.761600
2856.886935	207092.170950	39.766618
2859.835998	207680.833068	39.771636
2862.421924	208274.507091	39.776653
2865.295618	208858.890788	39.781671
2868.490982	209458.975604	39.786688
2871.510566	210051.773131	39.791706
2874.526207	210637.815271	39.796724
2876.874178	211256.073055	39.801741
2879.863831	211862.190519	39.806759
2882.697807	212479.739742	39.811776
2885.518090	213089.213944	39.816794
2888.345304	213711.796464	39.821812
2891.283930	214344.905197	39.826829
2894.274909	214980.064518	39.831847
2896.919684	215610.528483	39.836864
2899.638457	216260.441153	39.841882
2902.646866	216893.974765	39.846900
2905.424944	217544.260988	39.851917
2908.059506	218195.484993	39.856935
2911.068846	218860.394663	39.861952
2913.876888	219509.992495	39.866970
2917.355165	220168.656950	39.871988
2920.306741	220840.131732	39.877005
2923.268606	221491.993467	39.882023
2926.758911	222156.449577	39.887040
2929.577867	222821.138030	39.892058
2932.877852	223468.375129	39.897076
2935.881688	224132.984309	39.902093
2938.666050	224802.099050	39.907111
2941.735607	225456.892141	39.912128
2944.609210	226122.919056	39.917146
2948.158191	226789.678591	39.922164
2950.545535	227465.612661	39.927181
2953.887136	228125.799157	39.932199
2956.771023	228802.010667	39.937216
2959.900654	229483.873851	39.942234
2962.845706	230140.310596	39.947252
2965.804990	230818.693647	39.952269
2968.771297	231488.336006	39.957287
2972.022352	232145.510623	39.962304
2975.296731	232816.881649	39.967322
2978.477490	233469.137359	39.972340
2981.620980	234147.462382	39.977357
2984.341021	234812.185375	39.982375
2987.148427	235481.847404	39.987392
2990.057168	236159.748670	39.992410
2993.600068	236811.815619	39.997428
2996.744477	237479.287467	40.002445
2998.977307	238149.771135	40.007463
3001.891649	238819.460913	40.012480
3004.569452	239501.608480	40.017498
3008.187564	240173.877878	40.022516
3011.021557	240863.136054	40.027533
3013.761324	241537.901885	40.032551
3016.783225	242220.293543	40.037568
3019.504836	242901.180634	40.042586
3022.768422	243576.773344	40.047604
3025.663456	244273.709320	40.052621
3028.718243	244938.458005	40.057639
3031.993780	245598.292702	40.062656
3034.795787	246250.756280	40.067674
3037.814228	246898.255714	40.072692
3040.635970	247550.483152	40.077709
3043.830033	248194.927701	40.082727
3046.992271	248844.988812	40.087744
3049.678262	249509.525033	40.092762
3052.617811	250166.906377	40.097780
3055.630203	250825.365980	40.102797
3058.388181	251497.198672	40.107815
3061.514566	252165.668615	40.112832
3064.683979	252853.205574	40.117850
3067.489729	253520.906750	40.122868
3070.306508	254216.976568	40.127885
3073.062424	254903.806373	40.132903
3075.853515	255595.885304	40.137920
3078.696997	256311.727902	40.142938
3082.044670	257018.318018	40.147956
3085.040729	257729.531375	40.152973
3088.084247	258449.217107	40.157991
3091.405094	259177.694638	40.163008
3094.120946	259908.853197	40.168026
3097.243159	260645.938119	40.173044
3100.182244	261378.728962	40.178061
3103.341978	262121.716694	40.183079
3106.183416	262870.311742	40.188096
3109.044926	263630.074270	40.193114
3112.668896	264384.200493	40.198132
3115.765466	265148.918976	40.203149
3118.361276	265912.567093	40.208167
3122.002376	266672.744113	40.213184
3124.797753	267456.769759	40.218202
3128.044383	268211.764376	40.223220
3131.057375	268995.718008	40.228237
3134.609547	269766.703997	40.233255
3138.120629	270544.471116	40.238272
3141.517115	271331.036969	40.243290
3145.008814	272099.218730	40.248308
3148.147946	272874.585414	40.253325
3151.458134	273657.867534	40.258343
3154.914838	274420.014920	40.263360
3157.716657	275197.419319	40.268378
3161.276038	275964.590224	40.273396
3164.263606	276744.084021	40.278413
3167.709928	277526.622077	40.283431
3171.231488	278289.941650	40.288448
3174.047615	279078.327317	40.293466
3177.395005	279847.220078	40.298484
3180.681481	280631.249607	40.303501
3183.868172	281402.208342	40.308519
3186.933106	282177.977404	40.313536
3190.227126	282961.168006	40.318554
3193.739537	283728.901960	40.323572
3196.657754	284517.060302	40.328589
3199.949830	285290.601048	40.333607
3203.350201	286064.801655	40.338624
3206.559597	286845.879105	40.343642
3210.058818	287624.997629	40.348660
3213.431278	288394.604810	40.353677
3216.361866	289173.438202	40.358695
3219.995897	289936.942849	40.363712
3222.752581	290708.548131	40.368730
3226.180783	291483.542745	40.373748
3229.767731	292266.906915	40.378765
3232.753099	293037.482438	40.383783
3235.981333	293808.873362	40.388800
3238.931856	294589.412406	40.393818
3241.878949	295342.166281	40.398836
3245.239752	296091.113626	40.403853
3248.097660	296837.413326	40.408871
3251.043164	297568.456864	40.413888
3253.995739	298332.366611	40.418906
3257.046523	299081.526010	40.423924
3260.404626	299844.259900	40.428941
3263.154981	300606.341966	40.433959
3266.387783	301379.253876	40.438976
3269.262504	302153.429134	40.443994
3272.247859	302940.141523	40.449012
3275.284767	303723.762483	40.454029
3278.596796	304520.249343	40.459047
3281.848884	305323.790034	40.464064
3284.737674	306127.679452	40.469082
3287.925771	306951.689001	40.474100
3291.307062	307757.835935	40.479117
3294.443875	308598.629655	40.484135
3297.628989	309427.217989	40.489152
3301.290348	310268.814594	40.494170
3304.502545	311102.573112	40.499188
3308.038183	311942.154743	40.504205
3311.125201	312788.415769	40.509223
3314.467417	313635.357529	40.514240
3318.012023	314479.993330	40.519258
3321.729756	315331.337214	40.524276
3324.976951	316181.875781	40.529293
3328.113727	317048.276645	40.534311
3331.701248	317899.744358	40.539328
3335.453661	318766.598952	40.544346
3339.148893	319618.473174	40.549364
3342.713328	320479.181842	40.554381
3345.924753	321345.536342	40.559399
3349.626536	322199.515047	40.564416
3352.952881	323072.692710	40.569434
3356.003439	323924.784190	40.574452
3359.618246	324801.026705	40.579469
3362.885514	325663.222934	40.584487
3366.489148	326528.189931	40.589504
3369.517013	327412.231689	40.594522
3372.992405	328275.785544	40.599540
3376.219156	329149.101682	40.604557
3379.753254	330036.329143	40.609575
3383.206089	330921.925414	40.614592
3386.448762	331802.891707	40.619610
3389.678558	332688.000085	40.624628
3393.299551	333566.278854	40.629645
3396.338186	334458.402420	40.634663
3399.935915	335350.442595	40.639680
3403.176466	336252.790221	40.644698
3406.450029	337152.700797	40.649716
3409.848205	338046.938710	40.654733
3413.446755	338949.188844	40.659751
3417.329337	339830.396440	40.664768
3420.574314	340741.051739	40.669786
3423.919209	341645.885365	40.674804
3427.582224	342549.327051	40.679821
3431.342949	343447.049154	40.684839
3435.318054	344342.229052	40.689856
3438.358340	345241.208736	40.694874
3441.397594	346140.621204	40.699892
3444.616151	347029.356630	40.704909
3448.057314	347940.829779	40.709927
3451.840619	348848.167331	40.714944
3455.130991	349767.575597	40.719962
3458.538646	350649.946508	40.724980
3462.115096	351554.883190	40.729997
3465.201461	352463.521992	40.735015
3468.887272	353344.143344	40.740020
3472.158769	354205.158672	40.745024
3475.535984	355013.547229	40.750029
3478.883590	355777.518015	40.755034
3481.712284	356491.254324	40.760039
3484.922703	357141.809679	40.765044
3487.348849	357735.673031	40.770048
3490.167112	358290.910836	40.775053
3492.973853	358784.690772	40.780058
3495.497869	359238.837173	40.785063
3497.851333	359619.077934	40.790068
3499.970803	359972.057567	40.795072
3502.201703	360268.778571	40.800077
3504.434461	360523.465014	40.805082
3505.899654	360735.806250	40.810087
3507.731329	360891.039604	40.815092
3509.199979	361036.342182	40.820096
3510.557403	361132.032945	40.825101
3512.080077	361188.513231	40.830106
3513.400557	361215.979842	40.835111
3514.084716	361202.760676	40.840116
3515.425291	361183.086036	40.845120
3516.066354	361124.387145	40.850125
3517.223017	361046.980903	40.855130
3517.732499	360948.838141	40.860135
3518.350823	360834.465390	40.865140
3518.916949	360704.141758	40.870144
3519.676327	360544.004578	40.875149
3520.273151	360378.453776	40.880154
3520.517119	360209.602816	40.885159
3520.706294	359996.846890	40.890164
3520.980959	359806.718695	40.895168
3521.255584	359588.762376	40.900173
3521.771819	359368.987812	40.905178
3521.786402	359140.878344	40.910183
3522.446855	358890.810742	40.915188
3522.337011	358650.798201	40.920192
3522.344172	358403.522568	40.925197
3522.982078	358136.628419	40.930202
3522.506542	357871.888320	40.935207
3522.745800	357592.980029	40.940212
3522.830783	357329.596247	40.945216
3522.464881	357054.894855	40.950221
3523.029664	356775.521637	40.955226
3522.822022	356497.384928	40.960231
3522.996564	356201.395098	40.965236
3522.666175	355919.332989	40.970240
3522.674069	355622.626649	40.975245
3522.703043	355329.980793	40.980250
3522.545144	355048.290506	40.985255
3522.158668	354753.696313	40.990260
3521.875751	354467.394512	40.995264
3522.011954	354180.058732	41.000269
3522.217801	353892.099431	41.005274
3522.452265	353604.463466	41.010279
3522.088595	353313.969928	41.015284
3521.721938	353025.965175	41.020288
3521.696566	352729.516410	41.025293
3521.879792	352444.063944	41.030298
3521.960956	352162.158101	41.035303
3521.720698	351867.285489	41.040308
3521.273736	351579.432784	41.045312
3521.155115	351291.577014	41.050317
3520.821160	351005.328364	41.055322
3520.771224	350723.125389	41.060327
3520.733667	350435.351011	41.065332
3520.763684	350151.961247	41.070336
3520.203208	349873.999660	41.075341
3520.505209	349593.435052	41.080346
3520.288703	349326.066350	41.085351
3519.918487	349047.813792	41.090356
3519.872656	348783.566223	41.095360
3519.656011	348498.167006	41.100365
3519.587398	348221.055133	41.105370
3519.417706	347969.073753	41.110375
3519.592899	347695.325925	41.115380
3519.393105	347431.167898	41.120384
3519.150537	347160.989289	41.125389
3518.928825	346893.576328	41.130394
3518.852183	346640.375477	41.135399
3518.594099	346381.175765	41.140404
3518.426332	346133.197106	41.145408
3518.287022	345872.780006	41.150413
3518.325803	345608.494053	41.155418
3518.042178	345361.138007	41.160423
3517.824047	345106.625709	41.165428
3517.312700	344856.886286	41.170432
3517.446485	344607.527240	41.175437
3517.643869	344363.521060	41.180442
3517.155226	344125.061332	41.185447
3517.262993	343885.006620	41.190452
3516.948962	343656.610116	41.195456
3516.707861	343411.419872	41.200461
3516.816613	343170.266722	41.205466
3516.485559	342948.885672	41.210471
3516.666440	342709.980934	41.215476
3516.199242	342478.346051	41.220480
3515.780182	342247.236051	41.225485
3515.659268	342030.265898	41.230490
3515.886607	341812.680563	41.235495
3515.845096	341584.278651	41.240500
3515.558610	341369.694976	41.245504
3515.267906	341149.592957	41.250509
3515.264262	340930.919464	41.255514
3514.819184	340722.204907	41.260519
3514.792588	340510.194384	41.265524
3515.103484	340315.598693	41.270528
3514.497882	340090.453744	41.275533
3514.441831	339887.648999	41.280538
3514.281823	339691.318111	41.285543
3514.073613	339487.619458	41.290548
3514.412659	339292.530625	41.295552
3513.818295	339098.985228	41.300557
3513.831537	338889.272816	41.305562
3513.507349	338708.244874	41.310567
3513.546747	338511.622043	41.315572
3513.646528	338321.549422	41.320576
3513.542600	338129.041004	41.325581
3513.210383	337937.915008	41.330586
3512.907179	337759.396531	41.335591
3513.060860	337574.016019	41.340596
3512.928627	337392.773459	41.345600
3512.767331	337213.848663	41.350605
3512.569413	337027.070820	41.355610
3511.891242	336854.658874	41.360615
3512.300615	336690.696965	41.365620
3512.515094	336512.778055	41.370624
3512.334637	336339.039773	41.375629
3512.099297	336148.626724	41.380634
3511.657305	335989.575747	41.385639
3511.832986	335816.872842	41.390644
3511.977736	335662.433441	41.395648
3511.460095	335488.998169	41.400653
3511.604135	335333.362239	41.405658
3510.895646	335179.740857	41.410663
3511.280674	335008.654485	41.415668
3511.447636	334856.878555	41.420672
3510.528161	334697.947532	41.425677
3511.201494	334543.217377	41.430682
3510.821770	334395.670415	41.435687
3510.678556	334232.038305	41.440692
3510.554980	334096.275993	41.445696
3510.370425	333942.949077	41.450701
3510.502584	333800.609637	41.455706
3509.990580	333653.411048	41.460711
3510.252780	333510.846721	41.465716
3510.031372	333382.396244	41.470720
3510.279386	333233.322345	41.475725
3510.236078	333090.498998	41.480730
3509.678202	332952.206309	41.485735
3509.748287	332811.932902	41.490740
3509.740802	332675.943855	41.495744
3509.850529	332535.739528	41.500749
3509.834897	332402.090623	41.505754
3509.741243	332277.990941	41.510759
3509.588770	332143.345188	41.515764
3509.762259	332011.649152	41.520768
3509.794226	331882.212942	41.525773
3509.826837	331744.510250	41.530778
3509.231315	331612.627860	41.535783
3509.111876	331473.828880	41.540788
3509.502094	331349.904876	41.545792
3509.165310	331236.827283	41.550797
3509.081840	331100.208655	41.555802
3508.843710	330976.432550	41.560807
3508.183092	330852.671229	41.565812
3508.824067	330738.218468	41.570816
3508.313903	330623.105997	41.575821
3508.671359	330487.967767	41.580826
3508.689486	330381.852104	41.585831
3508.349384	330259.717458	41.590836
3508.032244	330157.061838	41.595840
3508.195364	330047.844992	41.600845
3508.210093	329935.446246	41.605850
3507.881125	329822.439600	41.610855
3508.007531	329704.681392	41.615860
3507.639289	329602.210342	41.620864
3507.332374	329493.930221	41.625869
3507.652971	329386.289318	41.630874
3507.270862	329288.881223	41.635879
3507.141693	329189.601996	41.640884
3507.496445	329098.233583	41.645888
3507.108772	328998.002305	41.650893
3507.430819	328899.669222	41.655898
3507.138703	328812.369217	41.660903
3507.103994	328693.335943	41.665908
3507.554023	328603.248704	41.670912
3507.310119	328501.492976	41.675917
3507.063523	328409.479340	41.680922
3506.836075	328311.434184	41.685927
3506.853831	328213.910042	41.690932
3506.992577	328121.174156	41.695936
3506.783210	328034.927809	41.700941
3507.256072	327946.259926	41.705946
3506.803818	327848.757493	41.710951
3506.745834	327754.474461	41.715956
3507.091512	327655.091704	41.720960
3506.769957	327562.146675	41.725965
3506.629612	327473.014005	41.730970
3506.519751	327393.542242	41.735975
3506.468538	327298.799216	41.740980
3506.597887	327212.650751	41.745984
3506.559893	327129.835031	41.750989
3506.476170	327038.199743	41.755994
3506.213813	326957.657175	41.760999
3506.079483	326865.215427	41.766004
3506.006369	326795.962340	41.771008
3505.782391	326711.038132	41.776013
3505.773510	326634.525197	41.781018
3505.645084	326577.362948	41.786023
3505.799046	326495.177270	41.791028
3505.747536	326418.467092	41.796032
3505.637450	326342.936035	41.801037
3505.791738	326261.843629	41.806042
3505.207437	326200.860221	41.811047
3505.206449	326125.998508	41.816052
3505.219501	326059.681412	41.821056
3504.880087	325994.614868	41.826061
3505.054333	325930.281913	41.831066
3504.943971	325868.384473	41.836071
3504.993357	325796.541334	41.841076
3505.307780	325734.373779	41.846080
3505.285801	325669.231648	41.851085
3505.511975	325602.193669	41.856090
3505.327786	325534.482042	41.861095
3505.034178	325471.976703	41.866100
3505.143948	325408.416133	41.871104
3504.605772	325345.872522	41.876109
3505.208112	325272.034174	41.881114
3505.028058	325217.854304	41.886119
3504.840538	325150.702192	41.891124
3504.853116	325090.565002	41.896128
3504.625511	325036.443201	41.901133
3504.643331	324969.309564	41.906138
3504.625898	324905.539155	41.911143
3504.730412	324851.619567	41.916148
3504.433924	324793.132858	41.921152
3504.276673	324751.769626	41.926157
3504.439427	324686.876864	41.931162
3504.301493	324649.606060	41.936167
3503.930716	324587.976332	41.941172
3504.217696	324544.940830	41.946176
3503.988125	324499.111508	41.951181
3504.000736	324440.652288	41.956186
3503.946636	324397.898901	41.961191
3504.068482	324342.449631	41.966196
3503.997743	324291.990893	41.971200
3503.929619	324250.257083	41.976205
3504.175827	324193.719754	41.981210
3504.090990	324151.403371	41.986215
3503.816585	324101.942905	41.991220
3503.865642	324056.044092	41.996224
3503.888681	324016.839653	42.001229
3503.892392	323970.947834	42.006234
3503.731294	323919.841362	42.011239
3503.971142	323876.023931	42.016244
3503.739545	323829.888918	42.021248
3503.632709	323792.332649	42.026253
3503.864587	323731.319706	42.031258
3503.628314	323698.896787	42.036263
3503.858052	323650.883293	42.041268
3504.144564	323615.758376	42.046272
3504.120842	323562.823826	42.051277
3504.113821	323507.876922	42.056282
3503.704083	323464.007977	42.061287
3503.858497	323410.562044	42.066292
3503.628135	323371.549244	42.071296
3503.665454	323330.815582	42.076301
3503.630319	323293.730994	42.081306
3503.914989	323253.569124	42.086311
3503.639533	323207.084127	42.091316
3503.784833	323164.018460	42.096320
3503.593191	323126.042381	42.101325
3503.707432	323073.594423	42.106330
3503.860035	323038.591711	42.111335
3503.800534	322991.818319	42.116340
3503.442849	322957.200587	42.121344
3503.413255	322920.369193	42.126349
3503.780273	322868.975348	42.131354
3503.569592	322835.072273	42.136359
3503.218607	322786.181876	42.141364
3503.533339	322746.930636	42.146368
3503.560563	322705.460199	42.151373
3503.663911	322673.924643	42.156378
3503.421812	322633.971728	42.161383
3503.365186	322597.144276	42.166388
3503.373269	322563.435734	42.171392
3503.089753	322524.354133	42.176397
3503.186012	322486.943012	42.181402
3503.027104	322450.640212	42.186407
3503.064933	322418.478718	42.191412
3503.110118	322391.658369	42.196416
3502.983844	322354.612635	42.201421
3503.120373	322321.239973	42.206426
3503.095300	322285.831935	42.211431
3503.182968	322255.138025	42.216436
3502.968905	322231.487186	42.221440
3502.789635	322192.312659	42.226445
3503.128825	322169.542001	42.231450
3502.851859	322129.568616	42.236455
3503.151858	322091.005941	42.241460
3503.031513	322067.391237	42.246464
3502.731483	322035.180511	42.251469
3502.729305	321991.475260	42.256474
3502.497271	321975.866081	42.261479
3502.661757	321945.872253	42.266484
3502.966980	321917.789833	42.271488
3502.633000	321900.288571	42.276493
3502.929366	321863.761448	42.281498
3502.790687	321841.065322	42.286503
3502.911372	321806.244652	42.291508
3502.593427	321780.218443	42.296512
3502.652664	321746.221410	42.301517
3503.173358	321716.197169	42.306522
3502.697294	321699.481238	42.311527
3502.535983	321667.986305	42.316532
3502.720875	321635.546821	42.321536
3502.719595	321610.971965	42.326541
3502.714958	321577.417263	42.331546
3502.360496	321565.134286	42.336551
3502.606884	321534.389598	42.341556
3502.681647	321512.066968	42.346560
3502.261639	321489.618156	42.351565
3502.443616	321469.110434	42.356570
3502.446979	321441.354732	42.361575
3502.620041	321416.879708	42.366580
3502.582626	321389.588271	42.371584
3502.495810	321367.799631	42.376589
3502.545414	321336.500439	42.381594
3502.763011	321327.587832	42.386599
3502.730756	321301.313142	42.391604
3502.460181	321268.613860	42.396608
3502.711620	321243.465036	42.401613
3502.490102	321212.055497	42.406618
3501.949656	321202.905210	42.411623
3502.386049	321174.064022	42.416628
3502.319556	321157.843532	42.421632
3502.204791	321134.405518	42.426637
3502.171150	321104.798234	42.431642
3502.603593	321091.705205	42.436647
3502.692061	321071.618956	42.441652
3502.521020	321053.481300	42.446656
3502.124941	321018.053881	42.451661
3501.953009	320998.211832	42.456666
3502.196698	320985.071958	42.461671
3502.325239	320961.570370	42.466676
3502.168895	320940.199428	42.471680
3502.493542	320936.917791	42.476685
3502.206790	320908.672848	42.481690
3502.584662	320887.879814	42.486695
3502.187707	320867.284226	42.491700
3502.426076	320848.217499	42.496704
3502.405747	320825.120718	42.501709
3502.637318	320805.698866	42.506714
3502.099573	320782.428548	42.511719
3502.487151	320767.510713	42.516724
3502.464802	320739.733132	42.521728
3502.408511	320718.804368	42.526733
3502.317147	320694.777319	42.531738
3502.335136	320671.776227	42.536743
3502.471151	320654.251853	42.541748
3502.324334	320639.112231	42.546752
3502.045762	320619.795491	42.551757
3502.117054	320601.797841	42.556762
3502.156240	320575.638738	42.561767
3502.260387	320560.816023	42.566772
3502.394149	320534.718431	42.571776
3502.115586	320533.693531	42.576781
3502.112329	320505.225913	42.581786
3502.158931	320486.036360	42.586791
3502.338089	320479.012202	42.591796
3502.215005	320456.516424	42.596800
3502.035855	320443.264405	42.601805
3502.419285	320407.867257	42.606810
3502.077396	320400.084999	42.611815
3501.872134	320370.173306	42.616820
3502.184831	320351.552672	42.621824
3501.637414	320352.859474	42.626829
3502.106258	320328.871842	42.631834
3501.883706	320314.354526	42.636839
3502.229820	320304.760151	42.641844
3502.377504	320280.466530	42.646848
3501.766251	320262.957059	42.651853
3502.391223	320244.974462	42.656858
3502.250578	320240.162739	42.661863
3502.103463	320217.772356	42.666868
3502.416311	320195.360934	42.671872
3502.257667	320175.974361	42.676877
3502.171533	320154.566609	42.681882
3502.277957	320144.780703	42.686887
3502.013210	320116.124740	42.691892
3502.352452	320097.601609	42.696896
3502.240801	320095.838255	42.701901
3502.427704	320062.863001	42.706906
3502.459872	320051.613105	42.711911
3502.791558	320029.020563	42.716916
3502.568759	319997.559450	42.721920
3502.201075	319968.995804	42.726925
3502.090914	319958.149751	42.731930
3501.780823	319942.577469	42.736935
3502.098514	319925.304247	42.741940
3502.123417	319905.914299	42.746944
3502.103344	319895.384879	42.751949
3502.175986	319872.069521	42.756954
3502.195680	319845.658610	42.761959
3502.099808	319835.878819	42.766964
3502.072432	319817.285679	42.771968
3501.749739	319802.503993	42.776973
3501.765214	319798.481930	42.781978
3501.598546	319786.423491	42.786983
3501.714740	319766.688472	42.791988
3501.868674	319753.435049	42.796993
3501.894824	319754.219697	42.801997
3502.142014	319721.870787	42.807002
3501.925594	319720.378209	42.812007
3501.919094	319692.292179	42.817012
3502.076409	319680.997179	42.822017
3501.774706	319678.296753	42.827021
3502.032690	319654.875978	42.832026
3501.892558	319640.320107	42.837031
3501.773336	319621.435947	42.842036
3502.057067	319616.277954	42.847041
3502.123437	319592.429158	42.852045
3502.121484	319578.792992	42.857050
3502.244053	319562.873077	42.862055
3502.119935	319538.087263	42.867060
3502.359142	319533.037986	42.872065
3501.801500	319513.815259	42.877069
3502.117906	319499.111643	42.882074
3502.022418	319485.948014	42.887079
3501.946727	319465.454175	42.892084
3502.032817	319463.201936	42.897089
3501.985712	319436.979307	42.902093
3501.956793	319411.008233	42.907098
3501.596643	319409.232818	42.912103
3501.847629	319377.137471	42.917108
3501.939432	319376.538026	42.922113
3501.714470	319374.690591	42.927117
3501.879688	319358.051574	42.932122
3502.052569	319336.552039	42.937127
3502.011620	319332.894934	42.942132
3501.834497	319316.462071	42.947137
3501.769266	319295.101506	42.952141
3502.122295	319286.498042	42.957146
3501.811596	319275.632286	42.962151
3501.746801	319260.377590	42.967156
3501.504573	319257.311658	42.972161
3501.463006	319249.660329	42.977165
3501.733399	319247.633681	42.982170
3501.468091	319228.823071	42.987175
3501.417323	319200.336578	42.992180
3501.685400	319202.940645	42.997185
3501.385019	319200.214541	43.002189
3502.004157	319189.534134	43.007194
3501.876213	319173.271618	43.012199
3501.823098	319160.813629	43.017204
3501.807608	319148.095339	43.022209
3501.600156	319144.362482	43.027213
3501.796831	319121.485277	43.032218
3501.603513	319118.259040	43.037223
3501.470187	319118.865100	43.042228
3501.519905	319112.624203	43.047233
3501.410714	319097.223741	43.052237
3501.453022	319078.772039	43.057242
3501.832945	319067.823701	43.062247
3501.831887	319066.348314	43.067252
3501.980270	319059.837569	43.072257
3501.438379	319037.889916	43.077261
3501.939873	319030.560714	43.082266
3501.679210	319028.617079	43.087271
3501.446710	319011.327743	43.092276
3501.688423	318991.674514	43.097281
3501.560457	318985.919328	43.102285
3501.781499	318976.217005	43.107290
3501.401592	318987.801525	43.112295
3501.387773	318969.994592	43.117300
3501.553144	318953.050097	43.122305
3501.471323	318951.790865	43.127309
3501.619061	318937.851237	43.132314
3501.524655	318941.707748	43.137319
3501.583810	318938.391143	43.142324
3502.003278	318913.748964	43.147329
3501.649363	318909.097642	43.152333
3501.749685	318900.177427	43.157338
3501.795882	318898.363904	43.162343
3501.433000	318870.663800	43.167348
3501.298429	318867.657335	43.172353
3501.266059	318866.899204	43.177357
3501.911438	318850.820969	43.182362
3501.779986	318861.628868	43.187367
3501.911837	318838.481790	43.192372
3502.166427	318822.719056	43.197377
3501.978499	318813.945654	43.202381
3502.110544	318781.690370	43.207386
3502.051105	318778.392294	43.212391
3501.947877	318772.862187	43.217396
3502.060174	318737.378853	43.222401
3501.726889	318738.550457	43.227405
3501.666272	318722.786083	43.232410
3501.216924	318708.456334	43.237415
3501.473864	318700.198521	43.242420
3501.817211	318691.774547	43.247425
3501.727637	318678.991376	43.252429
3501.917950	318681.047913	43.257434
3501.617498	318667.127383	43.262439
3501.755319	318655.580746	43.267444
3501.993839	318642.313760	43.272449
3501.723827	318624.190554	43.277453
3502.136452	318616.722525	43.282458
3501.854515	318611.983592	43.287463
3501.735425	318593.709569	43.292468
3502.109576	318585.586061	43.297473
3501.616776	318583.169861	43.302477
3501.738034	318556.793170	43.307482
3501.763029	318547.681124	43.312487
3501.705950	318528.328819	43.317492
3501.601977	318528.650437	43.322497
3501.414392	318528.781591	43.327501
3501.645691	318499.436401	43.332506
3501.707543	318490.725651	43.337511
3501.652442	318484.857239	43.342516
3501.649189	318486.028137	43.347521
3501.563047	318475.101631	43.352525
3502.236244	318446.984859	43.357530
3501.700168	318455.261038	43.362535
3501.637882	318445.450241	43.367540
3501.821000	318431.377710	43.372545
3501.673030	318419.417735	43.377549
3501.738087	318410.401165	43.382554
3501.411587	318404.982244	43.387559
3501.772386	318396.530043	43.392564
3501.452515	318371.748725	43.397569
3501.225455	318364.507871	43.402573
3501.863161	318360.286628	43.407578
3501.435578	318356.486351	43.412583
3501.625532	318346.178140	43.417588
3501.617928	318333.382054	43.422593
3501.284854	318322.799419	43.427597
3501.549170	318318.102265	43.432602
3501.603123	318319.086129	43.437607
3501.783135	318307.736341	43.442612
3502.021857	318290.576585	43.447617
3501.309197	318282.317627	43.452621
3501.560974	318268.692266	43.457626
3501.511411	318265.697911	43.462631
3501.673740	318260.940370	43.467636
3502.087545	318240.649290	43.472641
3501.628581	318236.828466	43.477645
3501.799165	318231.255483	43.482650
3501.761887	318208.923217	43.487655
3501.603399	318196.201564	43.492660
3501.847162	318189.014283	43.497665
3501.828176	318184.157869	43.502669
3502.122058	318158.695309	43.507674
3501.721976	318150.463784	43.512679
3501.700403	318146.421918	43.517684
3501.793640	318132.490553	43.522689
3501.850509	318115.435486	43.527693
3501.850688	318108.871443	43.532698
3501.680940	318105.590561	43.537703
3501.481563	318081.349969	43.542708
3501.713841	318069.228683	43.547713
3501.699359	318064.956721	43.552717
3501.430018	318063.803107	43.557722
3501.649210	318063.031076	43.562727
3501.409979	318042.638462	43.567732
3501.571578	318034.980600	43.572737
3501.650662	318031.915232	43.577741
3501.697486	318029.719943	43.582746
3501.712895	318018.853774	43.587751
3501.601395	318000.222125	43.592756
3501.717211	317995.191962	43.597761
3501.669982	317995.377501	43.602765
3501.681482	317981.865943	43.607770
3501.728685	317962.344431	43.612775
3501.591600	317949.543033	43.617780
3501.694484	317939.858954	43.622785
3501.582793	317940.792397	43.627789
3501.655447	317923.556691	43.632794
3501.707514	317917.849545	43.637799
3501.670285	317920.704959	43.642804
3501.729621	317914.411503	43.647809
3501.415365	317901.943097	43.652813
3501.302693	317878.681086	43.657818
3501.785890	317875.679741	43.662823
3501.635460	317870.385880	43.667828
3501.760039	317860.036893	43.672833
3501.534137	317860.072270	43.677837
3501.868874	317840.963713	43.682842
3502.046622	317834.142888	43.687847
3501.757733	317822.382878	43.692852
3501.861514	317799.570389	43.697857
3501.268557	317792.564740	43.702861
3501.714059	317794.326999	43.707866
3501.453673	317790.958494	43.712871
3501.454305	317779.127767	43.717876
3501.762300	317758.573142	43.722881
3501.482653	317745.768530	43.727885
3501.767229	317731.069297	43.732890
3502.015471	317737.594678	43.737895
3501.935570	317719.415933	43.742900
3501.738625	317706.878247	43.747905
3501.617450	317705.854113	43.752909
3501.884959	317685.178571	43.757914
3501.947960	317675.042707	43.762919
3501.585729	317668.713353	43.767924
3501.816629	317654.989297	43.772929
3501.653070	317656.770455	43.777933
3501.795774	317618.889876	43.782938
3501.834312	317632.393843	43.787943
3501.872945	317615.188778	43.792948
3502.009833	317591.556848	43.797953
3501.712880	317586.336745	43.802957
3501.882919	317579.237219	43.807962
3501.835869	317559.882919	43.812967
3501.519528	317545.481110	43.817972
3502.079219	317539.465571	43.822977
3501.843780	317534.159517	43.827981
3501.804566	317508.723215	43.832986
3501.854766	317504.135777	43.837991
3501.272217	317498.985756	43.842996
3501.508457	317486.787364	43.848001
3501.654283	317469.692696	43.853005
3501.893563	317457.519263	43.858010
3501.614640	317455.476642	43.863015
3501.485848	317460.966981	43.868020
3501.385524	317437.422939	43.873025
3501.209616	317416.816595	43.878029
3501.525917	317418.013890	43.883034
3501.588815	317417.673364	43.888039
3501.786174	317415.225527	43.893044
3501.869668	317408.572026	43.898049
3501.884927	317395.390454	43.903053
3501.876215	317381.322136	43.908058
3501.739657	317375.313655	43.913063
3501.829313	317360.695657	43.918068
3501.713105	317334.915096	43.923073
3501.404547	317336.337296	43.928077
3501.693038	317326.013443	43.933082
3501.724352	317332.165717	43.938087
3501.788029	317304.983116	43.943092
3501.663411	317296.021414	43.948097
3501.703694	317293.827111	43.953101
3501.426203	317281.072912	43.958106
3501.366978	317276.477115	43.963111
3501.536356	317251.516907	43.968116
3501.249907	317253.190079	43.973121
3501.599609	317246.876576	43.978125
3502.025009	317246.988228	43.983130
3501.749952	317233.724782	43.988135
3501.782373	317214.993974	43.993140
3501.951251	317209.344802	43.998145
3501.621339	317203.773609	44.003149
3501.918408	317173.679416	44.008154
3501.945169	317173.242767	44.013159
3501.500823	317165.475945	44.018164
3502.208713	317155.162812	44.023169
3501.492778	317148.227171	44.028173
3501.708654	317129.671187	44.033178
3501.693205	317127.332933	44.038183
3501.409194	317106.692459	44.043188
3501.579659	317096.997631	44.048193
3501.323830	317101.083081	44.053197
3501.945389	317087.297775	44.058202
3501.607290	317092.871768	44.063207
3501.751384	317072.266120	44.068212
3501.754240	317058.602974	44.073217
3501.446836	317053.359000	44.078221
3501.439205	317046.719692	44.083226
3501.538195	317050.927775	44.088231
3501.713893	317035.125851	44.093236
3501.600208	317018.249681	44.098241
3501.483534	317010.838688	44.103245
3501.803952	317009.033103	44.108250
3501.512468	317008.569877	44.113255
3501.716680	316988.056563	44.118260
3501.687228	316976.230325	44.123265
3501.734060	316973.144484	44.128269
3502.120943	316955.248648	44.133274
3501.937550	316945.252908	44.138279
3501.810853	316923.010300	44.143284
3501.948112	316915.203393	44.148289
3501.806814	316913.444544	44.153293
3501.429518	316894.523227	44.158298
3501.839024	316883.696937	44.163303
3501.954515	316867.980696	44.168308
3502.031464	316853.491732	44.173313
3501.403738	316845.397323	44.178317
3501.470017	316833.937723	44.183322
3501.469316	316844.827447	44.188327
3501.473490	316830.273525	44.193332
3501.819347	316802.003342	44.198337
3501.786630	316801.067129	44.203341
3501.736173	316798.988759	44.208346
3501.558705	316785.862580	44.213351
3501.379039	316764.925762	44.218356
3501.528641	316762.078269	44.223361
3500.956842	316770.309459	44.228365
3501.211214	316764.570536	44.233370
3501.255892	316761.434131	44.238375
3501.108701	316751.407245	44.243380
3501.517586	316761.876754	44.248385
3501.037378	316764.801497	44.253389
3501.386818	316751.160402	44.258394
3501.399670	316745.408349	44.263399
3501.463064	316730.997793	44.268404
3501.487245	316723.513847	44.273409
3501.599749	316730.340471	44.278413
3501.604845	316715.684595	44.283418
3501.269951	316720.952817	44.288423
3501.334417	316714.861933	44.293428
3501.647370	316690.489595	44.298433
3501.298286	316677.924516	44.303437
3501.423423	316669.076299	44.308442
3501.172021	316673.898943	44.313447
3501.233426	316668.699036	44.318452
3501.496118	316665.503097	44.323457
3501.441385	316668.488543	44.328461
3501.581501	316666.304044	44.333466
3501.706962	316648.957816	44.338471
3501.530269	316640.385767	44.343476
3501.606485	316635.208983	44.348481
3501.468110	316639.810416	44.353485
3501.578190	316630.557458	44.358490
3501.515318	316605.353324	44.363495
3501.428727	316613.635902	44.368500
3501.294606	316601.011751	44.373505
3501.376064	316598.429331	44.378509
3501.226910	316601.047898	44.383514
3501.491242	316591.083854	44.388519
3501.036819	316596.497993	44.393524
3501.617859	316587.018738	44.398529
3501.456829	316582.871317	44.403533
3501.596382	316555.650952	44.408538
3501.330304	316552.334128	44.413543
3501.357347	316558.309076	44.418548
3501.805767	316552.488903	44.423553
3501.314738	316546.535727	44.428557
3501.411523	316522.018991	44.433562
3501.433538	316517.995605	44.438567
3501.323839	316503.612037	44.443572
3501.670399	316507.069061	44.448577
3501.236708	316505.025148	44.453581
3501.681062	316505.591816	44.458586
3501.477119	316503.562871	44.463591
3501.396351	316486.248820	44.468596
3501.695692	316479.510550	44.473601
3501.207703	316473.582332	44.478605
3501.587834	316473.548407	44.483610
3501.342765	316474.426402	44.488615
3501.556110	316474.011462	44.493620
3501.703689	316442.947867	44.498625
3501.713456	316435.517011	44.503629
3501.994646	316433.692093	44.508634
3501.613107	316434.591425	44.513639
3501.796827	316404.488991	44.518644
3501.671648	316399.267336	44.523649
3501.627488	316394.185673	44.528653
3501.384279	316379.135973	44.533658
3501.215640	316377.126946	44.538663
3501.001296	316358.408913	44.543668
3501.611326	316354.598901	44.548673
3501.467943	316350.906676	44.553677
3501.556068	316334.990979	44.558682
3501.661816	316345.736967	44.563687
3501.344182	316344.387312	44.568692
3501.597727	316330.710194	44.573697
3501.401018	316315.958521	44.578701
3501.600838	316306.844125	44.583706
3501.535066	316310.111195	44.588711
3501.630045	316302.285348	44.593716
3501.924975	316295.649513	44.598721
3501.633367	316283.227996	44.603725
3501.869540	316270.291429	44.608730
3501.702291	316266.373939	44.613735
3501.453121	316251.910322	44.618740
3501.694122	316227.574424	44.623745
3501.558132	316235.254157	44.628749
3501.349106	316218.977784	44.633754
3501.439482	316230.820261	44.638759
3501.289785	316225.805965	44.643764
3501.617156	316215.323118	44.648769
3501.303789	316200.207996	44.653773
3501.859730	316186.865207	44.658778
3501.476336	316185.373168	44.663783
3501.286694	316177.413694	44.668788
3501.366335	316175.849264	44.673793
3501.766609	316178.254742	44.678797
3501.775038	316153.446299	44.683802
3501.595502	316152.304037	44.688807
3501.384831	316148.037119	44.693812
3501.614829	316143.090669	44.698817
3501.515988	316137.508660	44.703821
3501.819865	316113.849839	44.708826
3501.637276	316109.222322	44.713831
3501.547045	316108.218756	44.718836
3501.688709	316102.064833	44.723841
3501.340570	316088.481708	44.728845
3501.589163	316070.759799	44.733850
3501.436145	316062.794578	44.738855
3501.757682	316049.157632	44.743860
3501.860641	316045.426869	44.748865
3501.528996	316038.965284	44.753869
3501.717685	316026.824813	44.758874
3501.703419	316018.634346	44.763879
3501.597018	316021.195375	44.768884
3501.961284	316011.037476	44.773889
3501.330956	315995.946395	44.778893
3501.590217	315981.301430	44.783898
3501.508362	315980.983523	44.788903
3501.553091	315977.745282	44.793908
3501.825999	315963.708819	44.798913
3501.680897	315959.965943	44.803917
3501.805409	315948.878664	44.808922
3501.595361	315952.957062	44.813927
3501.369083	315925.844395	44.818932
3501.459062	315905.348444	44.823937
3501.331437	315907.632920	44.828941
3501.524760	315906.279699	44.833946
3501.510063	315905.925849	44.838951
3501.534025	315901.495009	44.843956
3501.560244	315896.911154	44.848961
3501.621670	315877.717269	44.853965
3501.494289	315863.819685	44.858970
3501.753709	315869.783839	44.863975
3501.512386	315861.425293	44.868980
3501.774842	315843.879231	44.873985
3501.592701	315826.148236	44.878989
3501.520977	315825.625197	44.883994
3501.364418	315820.382937	44.888999
3501.471322	315825.327758	44.894004
3501.770341	315818.360449	44.899009
3501.781745	315799.810437	44.904013
3501.296029	315784.976555	44.909018
3501.432050	315788.364776	44.914023
3501.523993	315781.378948	44.919028
3501.551240	315777.354677	44.924033
3501.300036	315770.447938	44.929037
3501.433007	315748.545802	44.934042
3501.511675	315737.592856	44.939047
3501.302205	315735.284861	44.944052
3501.316576	315734.341265	44.949057
3501.254239	315743.816055	44.954061
3501.468660	315733.401642	44.959066
3501.409026	315735.726384	44.964071
3501.545753	315726.367300	44.969076
3501.553267	315706.876448	44.974081
3501.197159	315701.385492	44.979085
3501.223973	315694.740598	44.984090
3501.297981	315695.721386	44.989095
3501.305800	315694.804257	44.994100
3501.567502	315690.972316	44.999105
3501.231560	315693.976347	45.004109
3501.268526	315699.288326	45.009114
3501.480712	315675.032965	45.014119
3501.213378	315662.022280	45.019124
3501.485226	315649.232618	45.024129
3500.991847	315654.958282	45.029133
3501.430776	315652.421696	45.034138
3501.641277	315655.950944	45.039143
3501.569034	315647.744030	45.044148
3501.709677	315642.760607	45.049153
3501.533249	315623.196702	45.054157
3501.621757	315613.488922	45.059162
3501.591088	315618.048178	45.064167
3501.439671	315609.497424	45.069172
3501.496747	315602.491575	45.074177
3501.608032	315589.955992	45.079181
3501.589170	315574.387519	45.084186
3501.946749	315572.372519	45.089191
3501.517858	315571.192894	45.094196
3501.814740	315545.830148	45.099201
3501.527551	315538.521901	45.104205
3501.369870	315525.061491	45.109210
3501.646952	315519.242528	45.114215
3501.344834	315530.459574	45.119220
3501.877142	315520.784166	45.124225
3501.763282	315501.642968	45.129229
3501.563297	315495.186164	45.134234
3501.294399	315488.791021	45.139239
3501.405328	315490.045921	45.144244
3501.256580	315484.878731	45.149249
3501.240317	315474.576654	45.154253
3501.248154	315462.286200	45.159258
3501.461710	315453.602027	45.164263
3501.072240	315445.953544	45.169268
3501.703989	315451.019903	45.174273
3501.015786	315451.407436	45.179277
3501.530611	315450.538255	45.184282
3501.713060	315449.135833	45.189287
3501.464179	315442.813884	45.194292
3501.587625	315421.650946	45.199297
3501.567216	315423.129930	45.204301
3501.691826	315410.973869	45.209306
3501.289139	315404.472411	45.214311
3500.905186	315413.692228	45.219316
3501.312952	315414.188300	45.224321
3501.512636	315409.704495	45.229325
3501.303687	315393.275149	45.234330
3501.154449	315368.160155	45.239335
3501.431534	315372.798540	45.244340
3501.518708	315372.734084	45.249345
3501.338863	315377.443904	45.254349
3501.375955	315369.423395	45.259354
3501.466035	315367.908193	45.264359
3501.526986	315358.382773	45.269364
3501.465627	315336.256381	45.274369
3501.487211	315326.991546	45.279373
3501.540090	315325.762040	45.284378
3501.654564	315325.158997	45.289383
3501.303484	315329.666599	45.294388
3501.691425	315320.115494	45.299393
3501.630315	315312.313877	45.304397
3501.694217	315293.399238	45.309402
3501.473016	315291.881811	45.314407
3500.967761	315296.947838	45.319412
3501.457690	315297.914498	45.324417
3501.464640	315288.270286	45.329421
3501.449085	315268.706521	45.334426
3501.338196	315268.036935	45.339431
3501.390908	315260.166628	45.344436
3501.477766	315254.631808	45.349441
3501.420575	315252.070988	45.354445
3501.563712	315255.178255	45.359450
3501.567097	315242.201456	45.364455
3501.358721	315224.626988	45.369460
3501.541489	315206.889588	45.374465
3501.245651	315220.370227	45.379469
3501.234532	315213.731193	45.384474
3501.210096	315211.928564	45.389479
3501.190174	315216.791505	45.394484
3501.319333	315210.359534	45.399489
3501.264667	315210.597134	45.404493
3501.144277	315203.644413	45.409498
3501.532311	315201.751854	45.414503
3501.002847	315194.201546	45.419508
3501.629987	315188.429589	45.424513
3501.465279	315175.071948	45.429517
3501.227410	315167.654155	45.434522
3501.369343	315167.937352	45.439527
3501.198488	315172.976557	45.444532
3501.424604	315162.712847	45.449537
3501.376618	315172.261845	45.454541
3501.143652	315159.398305	45.459546
3501.220492	315146.867983	45.464551
3501.264403	315131.314988	45.469556
3501.466365	315125.762158	45.474561
3501.196814	315129.391943	45.479565
3501.596813	315121.009327	45.484570
3501.473516	315121.613872	45.489575
3500.934364	315135.183464	45.494580
3501.289164	315115.180074	45.499585
3501.084403	315129.613368	45.504589
3501.060380	315115.648507	45.509594
3501.343832	315128.478844	45.514599
3501.062600	315135.418155	45.519604
3501.314810	315131.384101	45.524609
3501.174188	315105.606074	45.529613
3501.100750	315090.198630	45.534618
3501.147697	315086.883647	45.539623
3500.619407	315090.935544	45.544628
3500.776642	315095.490919	45.549633
3501.139938	315116.043712	45.554637
3501.116282	315117.039781	45.559642
3500.951277	315122.586955	45.564647
3501.013185	315121.610470	45.569652
3501.125333	315123.043297	45.574657
3501.016638	315122.347922	45.579661
3501.086957	315121.115684	45.584666
3501.180427	315124.154394	45.589671
3500.924804	315118.240555	45.594676
3501.356798	315116.493783	45.599681
3501.272567	315108.721190	45.604685
3500.829540	315089.605836	45.609690
3501.110555	315095.973818	45.614695
3501.115160	315099.738851	45.619700
3501.147440	315090.879397	45.624705
3501.189572	315089.346238	45.629709
3501.206276	315088.096937	45.634714
3501.388729	315091.045406	45.639719
3501.398511	315090.560503	45.644724
3501.281526	315082.029710	45.649729
3501.214038	315082.625531	45.654733
3501.181273	315092.248498	45.659738
3501.023585	315086.650115	45.664743
3501.145201	315079.608651	45.669748
3501.397218	315075.091189	45.674753
3501.523433	315089.370976	45.679757
3501.392213	315070.944738	45.684762
3501.377482	315052.347618	45.689767
3500.961125	315039.181944	45.694772
3501.488576	315030.499503	45.699777
3501.134687	315038.009954	45.704781
3501.113165	315043.458374	45.709786
3501.503958	315042.150587	45.714791
3501.261025	315041.374422	45.719796
3501.432579	315038.218062	45.724801
3501.019394	315045.737781	45.729805
3501.382764	315042.602321	45.734810
3501.351071	315037.874770	45.739815
3501.496726	315035.943766	45.744820
3501.739450	314996.824026	45.749825
3501.572304	314947.361755	45.754829
3501.290187	314840.973738	45.759834
3501.010971	314699.141413	45.764839
3501.142273	314511.419491	45.769844
3501.109617	314262.732400	45.774849
3500.780336	313989.968966	45.779853
3500.374866	313647.243019	45.784858
3500.300557	313256.906276	45.789863
3499.937959	312831.929626	45.794868
3499.943302	312350.301071	45.799873
3499.025177	311824.409261	45.804877
3498.649525	311252.038773	45.809882
3498.137594	310633.981132	45.814887
3497.717896	309973.583299	45.819892
3497.258033	309260.990845	45.824897
3496.404327	308498.190852	45.829901
3495.932083	307692.668768	45.834906
3495.563150	306840.089009	45.839911
3494.810618	305944.724475	45.844916
3494.317957	304996.089176	45.849921
3493.192019	304004.448963	45.854925
3492.146068	302953.121985	45.859930
3491.367623	301862.028988	45.864935
3490.262488	300729.453691	45.869940
3489.639124	299557.532638	45.874945
3488.491737	298333.389315	45.879949
3487.503703	297059.968224	45.884954
3486.269405	295748.147703	45.889959
3484.918802	294390.854558	45.894964
3483.798994	292986.122864	45.899969
3482.813874	291543.077990	45.904973
3481.396550	290050.809612	45.909978
3480.418924	288517.859377	45.914983
3479.109468	286931.108129	45.919988
3477.762573	285308.556480	45.924993
3476.189816	283645.217033	45.929997
3474.643040	281945.656671	45.935002
3473.421170	280203.080459	45.940007
3471.582194	278420.256303	45.945012
3470.528395	276599.662348	45.950017
3468.752684	274747.083650	45.955021
3467.120307	272835.420050	45.960026
3465.247061	270897.346833	45.965031
3463.472335	268923.567861	45.970036
3461.735594	266907.013280	45.975041
3459.734448	264868.432029	45.980045
3458.126851	262781.136875	45.985050
3456.101288	260659.921962	45.990055
3453.949792	258509.987950	45.995060
3452.204476	256319.181616	46.000065
3449.831227	254105.644415	46.005069
3447.417370	251855.763170	46.010074
3445.554386	249563.232525	46.015079
3442.849538	247255.801763	46.020084
3441.017081	244908.501471	46.025089
3438.763311	242545.424745	46.030093
3436.645271	240131.493681	46.035098
3434.192040	237707.380797	46.040103
3431.770981	235250.415645	46.045108
3429.194883	232743.719114	46.050113
3426.449380	230237.826955	46.055117
3423.766830	227691.574193	46.060122
3421.348504	225126.811035	46.065127
3418.539383	222554.239091	46.070132
3415.943948	219936.124887	46.075137
3413.119656	217316.628954	46.080141
3410.022617	214652.847775	46.085146
3407.210400	211980.763016	46.090151
3404.056133	209291.487241	46.095156
3401.205739	206572.343524	46.100161
3397.995133	203851.456047	46.105165
3394.641298	201093.956668	46.110170
3391.305703	198329.801398	46.115175
3387.814331	195554.158884	46.120180
3384.509020	192769.044303	46.125185
3381.204368	189984.551284	46.130189
3377.587999	187178.121367	46.135194
3374.378252	184355.811564	46.140199
3370.527309	181548.526506	46.145204
3367.121360	178713.069109	46.150209
3363.167478	175871.703418	46.155213
3359.387782	173034.150540	46.160218
3355.748771	170190.733508	46.165223
3351.710021	167352.604898	46.170228
3348.335194	164490.861754	46.175233
3343.571538	161658.006802	46.180237
3339.023476	158812.387914	46.185242
3334.258258	155983.326964	46.190247
3329.491566	153188.037827	46.195252
3324.648091	150381.177898	46.200257
3319.933756	147589.852210	46.205261
3315.220640	144818.193694	46.210266
3310.096929	142065.123681	46.215271
3304.722704	139257.868819	46.220276
3299.117468	136569.947495	46.225281
3293.179702	133908.365102	46.230285
3287.181721	131285.838057	46.235290
3280.779919	128719.996672	46.240295
3273.405998	126199.082172	46.245300
3266.889739	123723.974404	46.250305
3259.387733	121318.586523	46.255309
3252.207734	118970.687328	46.260314
3244.409036	116699.490982	46.265319
3236.799809	114506.220839	46.270324
3228.320065	112378.113329	46.275329
3219.655641	110356.436255	46.280333
3211.218278	108402.854963	46.285338
3202.786611	106550.955848	46.290343
3193.598349	104799.610313	46.295348
3185.374678	103131.247670	46.300353
3176.036913	101588.394058	46.305357
3167.049614	100116.544159	46.310362
3158.405742	98767.088000	46.315367
3149.577559	97504.240933	46.320372
3141.129273	96330.764443	46.325377
3133.009951	95250.100906	46.330381
3125.302245	94254.336584	46.335386
3117.850869	93346.829927	46.340391
3111.058184	92510.127123	46.345396
3104.496078	91739.931051	46.350401
3098.315349	91037.331385	46.355405
3092.289267	90393.794986	46.360410
3086.928645	89790.636734	46.365415
3081.155210	89244.438667	46.370420
3076.466956	88734.990388	46.375425
3071.303468	88281.185457	46.380429
3066.848385	87834.696491	46.385434
3062.408387	87438.256696	46.390439
3057.972488	87057.296031	46.395444
3054.341191	86686.797443	46.400449
3050.393988	86338.560368	46.405453
3046.708910	86009.800310	46.410458
3043.040565	85681.625738	46.415463
3039.371852	85367.365870	46.420468
3035.850437	85067.378287	46.425473
3032.405252	84768.982572	46.430477
3028.969543	84474.361448	46.435482
3025.983082	84190.128095	46.440487
3022.813158	83909.406978	46.445492
3019.733616	83612.376154	46.450497
3016.253020	83324.481182	46.455501
3013.156115	83041.508697	46.460506
3009.979376	82750.472457	46.465511
3006.528266	82477.850317	46.470516
3003.547346	82182.330595	46.475521
2999.944678	81883.494209	46.480525
2996.500101	81592.930915	46.485530
2993.079386	81304.323029	46.490535
2989.845938	81022.128792	46.495540
2986.389599	80724.132856	46.500545
2982.872351	80430.696878	46.505549
2979.254127	80147.187117	46.510554
2976.168979	79855.747278	46.515559
2972.658898	79577.891304	46.520564
2969.184605	79297.263615	46.525569
2965.506919	79014.930505	46.530573
2961.924331	78735.532052	46.535578
2958.329648	78444.809061	46.540583
2954.385943	78170.692890	46.545588
2951.516530	77888.422701	46.550593
2947.407014	77616.725714	46.555597
2943.512105	77350.624156	46.560602
2940.046258	77081.918018	46.565607
2936.612230	76822.709299	46.570612
2932.629740	76550.507732	46.575617
2928.782182	76309.351885	46.580621
2924.944366	76042.771561	46.585626
2921.721851	75799.122226	46.590631
2917.974039	75552.712521	46.595636
2914.530645	75308.632260	46.600641
2911.056391	75060.330137	46.605645
2907.075038	74820.745111	46.610650
2903.613788	74580.585613	46.615655
2900.103684	74346.125074	46.620660
2896.541478	74114.303414	46.625665
2893.097076	73879.912874	46.630669
2889.222377	73651.064832	46.635674
2885.985611	73416.188735	46.640679
2882.098837	73190.902141	46.645684
2878.546563	72963.304830	46.650689
2874.752900	72742.388423	46.655693
2871.041784	72517.283247	46.660698
2867.763798	72296.772437	46.665703
2864.504505	72085.034838	46.670708
2860.993420	71867.776650	46.675713
2857.328479	71642.925661	46.680717
2853.764595	71431.583787	46.685722
2850.878262	71203.389578	46.690727
2846.463426	71004.170716	46.695732
2843.327861	70777.644463	46.700737
2839.910423	70572.787645	46.705741
2836.507246	70352.553970	46.710746
2832.982266	70131.896806	46.715751
2829.262992	69922.007146	46.720756
2826.166084	69704.708473	46.725761
2822.474353	69480.813480	46.730765
2819.048451	69262.300291	46.735770
2816.011668	69049.295501	46.740775
2812.054910	68825.879298	46.745780
2808.638897	68609.655424	46.750785
2805.328924	68388.224041	46.755789
2801.692362	68175.491662	46.760794
2798.418165	67949.621179	46.765799
2795.055666	67731.936270	46.770804
2791.654888	67508.393761	46.775809
2788.029449	67296.485801	46.780813
2784.591013	67063.367864	46.785818
2781.044313	66836.686514	46.790823
2777.465935	66619.628821	46.795828
2774.070531	66390.268112	46.800833
2770.644076	66177.087854	46.805837
2767.099888	65948.471672	46.810842
2763.389808	65722.581154	46.815847
2760.014636	65500.124975	46.820852
2756.571264	65284.771372	46.825857
2753.430137	65057.369659	46.830861
2749.990748	64832.536486	46.835866
2746.094404	64599.398556	46.840871
2742.525885	64375.135519	46.845876
2738.624680	64149.396885	46.850881
2735.395844	63931.228614	46.855885
2732.117992	63720.007096	46.860890
2728.958995	63482.207135	46.865895
2725.219430	63258.488599	46.870900
2721.897973	63029.730824	46.875905
2718.024702	62807.960311	46.880909
2714.674868	62584.091677	46.885914
2711.673221	62345.605208	46.890919
2707.575951	62128.508800	46.895924
2704.517612	61898.552528	46.900929
2701.052962	61685.080090	46.905933
2697.460960	61445.108030	46.910938
2694.056858	61206.289325	46.915943
2690.505362	60978.455915	46.920948
2686.955602	60746.404145	46.925953
2683.614904	60512.234000	46.930957
2680.285667	60278.692556	46.935962
2676.770504	60040.315051	46.940967
2673.391789	59816.533186	46.945972
2669.810085	59574.305968	46.950977
2666.245198	59334.166293	46.955981
2662.641742	59096.630426	46.960986
2659.329359	58867.402262	46.965991
2655.548536	58619.371328	46.970996
2652.089544	58393.647968	46.976001
2648.733498	58154.864277	46.981005
2645.144856	57929.121113	46.986010
2641.679936	57695.644737	46.991015
2638.179229	57460.075922	46.996020
2634.357907	57217.446542	47.001025
2630.885644	56982.531515	47.006029
2627.640899	56744.055314	47.011034
2624.165719	56507.394144	47.016039
2620.468540	56270.452789	47.021044
2617.117068	56033.986339	47.026049
2613.650405	55799.748264	47.031053
2609.837709	55566.829234	47.036058
2606.772428	55322.907993	47.041063
2603.244682	55084.911387	47.046068
2599.708208	54848.872674	47.051073
2596.105929	54617.858805	47.056077
2592.663822	54373.847652	47.061082
2589.460138	54124.776940	47.066087
2585.870703	53896.210720	47.071092
2582.200924	53651.861983	47.076097
2578.744605	53409.848792	47.081101
2575.357020	53162.821796	47.086106
2571.890321	52925.750979	47.091111
2568.658243	52679.897436	47.096116
2564.720655	52434.232961	47.101121
2561.618768	52197.220309	47.106125
2557.599640	51949.613424	47.111130
2554.313213	51704.457444	47.116135
2551.138206	51471.707591	47.121140
2547.616140	51224.297111	47.126145
2543.908729	50981.555414	47.131149
2540.680497	50741.056686	47.136154
2536.857876	50490.396092	47.141159
2533.096424	50245.945155	47.146164
2529.660108	50010.294861	47.151169
2526.362395	49758.259738	47.156173
2522.723294	49515.453001	47.161178
2519.418113	49266.437445	47.166183
2515.663437	49026.869910	47.171188
2512.520727	48781.500482	47.176193
2508.861157	48536.322365	47.181197
2505.322629	48294.692619	47.186202
2501.769485	48047.720769	47.191207
2498.022373	47803.661523	47.196212
2494.974357	47551.617995	47.201217
2491.591275	47303.619145	47.206221
2487.884225	47062.219133	47.211226
2484.652941	46807.079356	47.216231
2481.320865	46550.226762	47.221236
2477.871909	46295.659564	47.226241
2474.027930	46048.469595	47.231245
2470.476854	45791.533056	47.236250
2467.121762	45533.484303	47.241255
2463.357304	45298.523981	47.246260
2459.681038	45041.698053	47.251265
2456.276413	44792.880386	47.256269
2453.045653	44547.691157	47.261274
2449.665126	44293.833561	47.266279
2446.142954	44044.998225	47.271284
2442.667685	43791.370449	47.276289
2439.199900	43538.505375	47.281293
2435.521327	43292.385383	47.286298
2432.108168	43033.277560	47.291303
2428.731733	42779.316142	47.296308
2425.164594	42514.493284	47.301313
2421.787805	42271.882171	47.306317
2418.119772	42015.730392	47.311322
2414.793911	41754.309435	47.316327
2410.826089	41489.295262	47.321332
2407.685586	41242.384768	47.326337
2404.038578	40986.317796	47.331341
2400.940354	40727.029328	47.336346
2397.241539	40471.648599	47.341351
2393.478007	40215.786421	47.346356
2390.090327	39958.315036	47.351361
2386.750539	39713.551691	47.356365
2383.125500	39449.859148	47.361370
2379.725466	39186.673530	47.366375
2375.866756	38933.269655	47.371380
2372.979451	38672.184754	47.376385
2369.427531	38408.398351	47.381389
2366.241977	38147.138211	47.386394
2362.480510	37880.950165	47.391399
2359.250546	37630.715573	47.396404
2355.489417	37362.815807	47.401409
2352.135454	37103.357130	47.406413
2348.383001	36824.007031	47.411418
2344.990438	36559.641492	47.416423
2341.375460	36301.190635	47.421428
2338.049162	36034.120654	47.426433
2334.859202	35770.550967	47.431437
2330.887775	35501.629767	47.436442
2327.629087	35234.901555	47.441447
2323.988057	34970.252310	47.446452
2320.486703	34693.762444	47.451457
2317.034038	34432.253575	47.456461
2313.784941	34164.136468	47.461466
2310.553508	33887.665632	47.466471
2306.667224	33618.862810	47.471476
2303.008667	33346.706418	47.476481
2299.880003	33084.738910	47.481485
2295.684781	32815.474954	47.486490
2292.422848	32539.071006	47.491495
2288.814352	32263.941860	47.496500
2285.768442	31998.533366	47.501505
2282.178041	31721.253588	47.506509
2278.780701	31462.219570	47.511514
2275.616264	31177.686834	47.516519
2272.306163	30903.403602	47.521524
2268.914882	30620.029445	47.526529
2265.649363	30342.590495	47.531533
2261.995822	30054.125326	47.536538
2258.321999	29765.204731	47.541543
2254.596151	29479.965640	47.546548
2251.500341	29198.022360	47.551553
2247.961203	28923.870968	47.556557
2244.431494	28626.654811	47.561562
2241.048046	28334.210839	47.566567
2237.361311	28053.706505	47.571572
2233.800868	27762.895292	47.576577
2230.424516	27473.954100	47.581581
2226.928477	27189.300280	47.586586
2223.639877	26900.518250	47.591591
2219.940801	26609.396696	47.596596
2216.318742	26324.641646	47.601601
2212.949269	26031.208415	47.606605
2209.639677	25732.042173	47.611610
2206.436777	25444.819851	47.616615
2202.763395	25157.966685	47.621620
2199.248361	24855.557211	47.626625
2195.513657	24566.022990	47.631629
2191.885403	24262.512385	47.636634
2188.817130	23972.096845	47.641639
2185.182295	23676.369957	47.646644
2181.789164	23378.930741	47.651649
2178.130916	23091.750002	47.656653
2174.538974	22803.739448	47.661658
2170.707728	22504.272202	47.666663
2167.226989	22221.035735	47.671668
2163.360163	21927.195630	47.676673
2159.165321	21655.177849	47.681677
2154.677778	21399.344336	47.686682
2150.396633	21159.578375	47.691687
2145.675842	20936.784963	47.696692
2140.873556	20719.600263	47.701697
2136.611080	20508.896064	47.706701
2132.798938	20303.013862	47.711706
2129.073103	20105.633730	47.716711
2125.248484	19924.125852	47.721716
2121.769225	19736.940796	47.726721
2118.601096	19565.316339	47.731725
2114.143207	19376.672634	47.736730
2111.571114	19195.494957	47.741735
2107.898527	19022.712722	47.746740
2104.736514	18838.862689	47.751745
2100.997527	18662.768705	47.756749
2097.858707	18486.861104	47.761754
2094.556595	18298.262374	47.766759
2090.611894	18124.054936	47.771764
2087.405711	17941.221042	47.776769
2084.238630	17764.260358	47.781773
2080.769361	17584.061454	47.786778
2077.329743	17399.217131	47.791783
2073.812735	17228.168266	47.796788
2070.803371	17036.153970	47.801793
2067.968331	16860.447955	47.806797
2064.380597	16669.309974	47.811802
2060.853383	16480.609038	47.816807
2057.172403	16288.818109	47.821812
2053.679013	16098.510182	47.826817
2050.373590	15901.984209	47.831821
2046.725634	15714.208986	47.836826
2043.345220	15513.832459	47.841831
2039.748822	15333.551042	47.846836
2036.530156	15141.404781	47.851841
2032.828558	14951.501799	47.856845
2029.358892	14759.170681	47.861850
2025.929306	14562.529082	47.866855
2022.820485	14380.483248	47.871860
2018.994592	14184.379337	47.876865
2015.773062	13992.574390	47.881869
2011.706085	13792.554508	47.886874
2008.586283	13598.733443	47.891879
2005.054278	13414.236516	47.896884
2001.699866	13216.925868	47.901889
1998.124713	13015.561308	47.906893
1994.190314	12827.143875	47.911898
1990.795599	12629.468910	47.916903
1987.550527	12435.910471	47.921908
1984.341271	12242.646009	47.926913
1980.516348	12039.159142	47.931917
1976.960596	11859.024698	47.936922
1973.950086	11669.217442	47.941927
1970.051972	11468.885512	47.946932
1966.456251	11263.940248	47.951937
1963.268871	11073.030197	47.956941
1959.698904	10875.657511	47.961946
1956.511036	10672.098446	47.966951
1952.700484	10479.873753	47.971956
1949.447372	10278.557766	47.976961
1945.904145	10074.054170	47.981965
1942.019234	9874.804035	47.986970
1939.197535	9671.777864	47.991975
1935.435258	9474.934401	47.996980
1931.956614	9275.851853	48.001985
1928.593390	9072.692214	48.006989
1924.833970	8874.430256	48.011994
1921.399711	8675.182609	48.016999
1917.685014	8478.573340	48.022004
1913.716424	8269.167723	48.027009
1910.740987	8075.583797	48.032013
1907.047287	7878.898491	48.037018
1903.819774	7674.163049	48.042023
1900.407846	7481.584203	48.047028
1896.672893	7287.351952	48.052033
1893.119496	7083.892614	48.057037
1890.431722	6887.294699	48.062042
1886.659924	6672.859921	48.067047
1882.988876	6475.445476	48.072052
1879.781993	6265.699758	48.077057
1876.042770	6063.926547	48.082061
1872.358791	5863.795785	48.087066
1869.219089	5658.834874	48.092071
1865.401281	5457.242062	48.097076
1862.032586	5241.355836	48.102081
1858.693046	5047.696256	48.107085
1854.608211	4842.268981	48.112090
1851.585673	4642.643067	48.117095
1847.872017	4446.576877	48.122100
1844.593216	4230.925912	48.127105
1840.836142	4036.788651	48.132109
1836.906074	3837.300954	48.137114
1833.298808	3634.790379	48.142119
1830.162622	3430.100867	48.147124
1827.020420	3227.601183	48.152129
1823.092092	3028.641094	48.157133
1819.541343	2826.431347	48.162138
1816.353014	2624.882275	48.167143
1811.606191	2418.965923	48.172148
1808.833985	2224.026388	48.177153
1805.118959	2041.386837	48.182157
1801.237800	1839.733499	48.187162
1798.077646	1643.807322	48.192167
1794.534423	1468.512700	48.197172
1790.966171	1269.490433	48.202177
1787.563512	1090.377540	48.207181
1783.490980	898.728133	48.212186
1779.981553	708.229754	48.217191
1776.093081	537.750497	48.222196
1772.568722	368.734541	48.227201
1768.543393	197.824363	48.232205
1763.408664	61.248960	48.237210
1754.678908	44.480313	48.242215
1745.780666	59.467770	48.247220
1740.482392	48.030960	48.252225
1737.278848	51.009625	48.257229
1734.616845	57.763374	48.262234
1731.810668	52.621661	48.267239
1729.038514	57.719001	48.272244
1726.262438	62.092447	48.277249
1723.688169	55.693216	48.282253
1720.396306	60.837091	48.287258
1717.269014	58.839831	48.292263
1713.250413	59.870610	48.297268
1709.666399	49.519640	48.302273
1706.715438	51.626705	48.307277
1703.366167	70.595877	48.312282
1699.562730	64.803475	48.317287
1696.637993	52.337154	48.322292
1692.563426	60.688234	48.327297
1689.551225	56.157752	48.332301
1686.176487	59.653614	48.337306
1682.738844	53.854596	48.342311
1679.348857	68.198344	48.347316
1675.943079	59.806352	48.352321
1672.297582	53.625411	48.357325
1668.918668	55.669749	48.362330
1665.647272	52.290334	48.367335
1662.116393	61.726938	48.372340
1658.357678	54.399445	48.377345
1655.126415	63.960005	48.382349
1651.564498	51.602917	48.387354
1648.654778	58.841548	48.392359
1644.853932	61.976999	48.397364
1641.276457	60.790548	48.402369
1638.144004	59.417389	48.407373
1634.296064	69.884404	48.412378
1630.891329	57.439445	48.417383
1627.563344	60.905861	48.422388
1623.662182	66.353936	48.427393
1620.523001	59.970382	48.432397
1617.293643	47.469513	48.437402
1613.981038	50.844938	48.442407
1610.080426	53.116480	48.447412
1606.840614	55.806627	48.452417
1603.724619	49.337195	48.457421
1599.707791	55.129250	48.462426
1596.486564	52.498153	48.467431
1592.419008	61.572678	48.472436
1588.998953	51.360615	48.477441
1585.951550	52.470394	48.482445
1581.977990	57.480554	48.487450
1578.859013	52.549201	48.492455
1575.437072	51.740233	48.497460
1571.661330	55.295728	48.502465
1568.570329	48.695846	48.507469
1564.565482	59.529123	48.512474
1561.446630	57.033877	48.517479
1558.013066	52.850967	48.522484
1554.424926	63.495641	48.527489
1551.080816	60.238378	48.532493
1547.052980	64.627451	48.537498
1543.966725	54.888349	48.542503
1540.289180	54.018159	48.547508
1537.135163	65.607303	48.552513
1533.789653	54.921680	48.557517
1529.962533	57.865128	48.562522
1526.848683	53.755576	48.567527
1522.844367	59.972812	48.572532
1519.650617	58.754819	48.577537
1516.160965	58.076694	48.582541
1512.505931	58.936748	48.587546
1509.352775	56.706319	48.592551
1505.401369	60.513962	48.597556
1502.207231	57.163639	48.602561
1498.469402	52.326015	48.607565
1494.841429	55.804622	48.612570
1491.596833	49.250956	48.617575
1487.946313	57.928039	48.622580
1484.707212	56.141346	48.627585
1481.300500	56.500629	48.632589
1477.510900	58.001862	48.637594
1474.152736	57.312662	48.642599
1470.431364	62.878181	48.647604
1466.866681	59.013224	48.652609
1463.921487	50.504937	48.657613
1460.247425	55.898535	48.662618
1456.881809	46.513251	48.667623
1452.983181	53.805473	48.672628
1449.362385	49.718352	48.677633
1446.096980	46.097629	48.682637
1442.470258	51.518624	48.687642
1439.004262	45.857020	48.692647
1435.569230	51.735235	48.697652
1432.350206	55.896505	48.702657
1429.085863	48.539187	48.707661
1425.062150	59.834210	48.712666
1421.858697	59.070190	48.717671
1418.273147	61.099495	48.722676
1414.740246	53.303322	48.727681
1411.202192	57.229795	48.732685
1407.523748	62.927822	48.737690
1404.264019	50.586822	48.742695
1400.699150	53.286782	48.747700
1397.340725	53.916949	48.752705
1393.812012	55.295116	48.757709
1390.003931	66.376063	48.762714
1386.659795	52.583447	48.767719
1382.905098	51.633643	48.772724
1379.761391	53.486229	48.777729
1376.601561	54.464970	48.782733
1372.914439	51.160225	48.787738
1369.512610	53.246210	48.792743
1365.775557	52.578391	48.797748
1362.384423	43.000988	48.802753
1358.794464	42.136139	48.807757
1354.731241	56.721375	48.812762
1351.686813	50.658452	48.817767
1347.926011	57.169826	48.822772
1344.244740	43.202219	48.827777
1341.441682	45.514024	48.832781
1337.698454	52.190329	48.837786
1334.504662	40.889422	48.842791
1330.776950	50.426525	48.847796
1327.228414	49.336901	48.852801
1323.697004	46.033113	48.857805
1320.368508	51.011988	48.862810
1316.996734	54.684669	48.867815
1313.145014	56.300091	48.872820
1309.646837	45.233504	48.877825
1306.168821	53.042067	48.882829
1302.531807	52.545276	48.887834
1298.930345	36.698569	48.892839
1296.223852	50.650648	48.897844
1292.413937	48.782535	48.902849
1289.030676	46.173747	48.907853
1285.431271	52.564960	48.912858
1281.789176	53.056073	48.917863
1277.946165	68.337700	48.922868
1274.517060	61.756048	48.927873
1271.400566	53.489785	48.932877
1267.423269	61.816288	48.937882
1264.209099	47.788250	48.942887
1260.489145	55.163297	48.947892
1257.032485	53.844179	48.952897
1254.048125	38.783584	48.957901
1250.297337	59.055877	48.962906
1246.607476	44.691025	48.967911
1243.014254	50.135312	48.972916
1239.693359	46.437929	48.977921
1236.500988	43.144375	48.982925
1233.014017	53.694196	48.987930
1229.392318	38.986489	48.992935
1225.751658	51.983827	48.997940
1221.952973	50.132967	49.002945
1218.822977	38.594331	49.007949
1215.584514	50.130315	49.012954
1211.678968	51.187885	49.017959
1208.263481	46.337886	49.022964
1204.445963	50.485348	49.027969
1201.377832	41.607264	49.032973
1197.799041	53.411671	49.037978
1194.222991	40.895663	49.042983
1190.542590	50.602572	49.047988
1186.895627	51.746221	49.052993
1183.736469	49.197301	49.057997
1180.234245	46.392040	49.063002
1176.902258	51.858727	49.068007
1173.263955	43.500191	49.073012
1169.489796	44.986464	49.078017
1166.302692	49.753423	49.083021
1162.466860	55.055383	49.088026
1159.020111	47.606506	49.093031
1155.683888	46.733646	49.098036
1152.014690	38.452726	49.103041
1148.576981	42.151599	49.108045
1144.845486	47.560617	49.113050
1141.432983	42.453912	49.118055
1138.194882	55.742595	49.123060
1134.825377	48.449315	49.128065
1131.962146	51.526741	49.133069
1127.809066	56.726520	49.138074
1124.322644	49.245903	49.143079
1120.490389	51.576528	49.148084
1116.935256	49.513572	49.153089
1113.668327	42.409889	49.158093
1109.819000	53.440420	49.163098
1106.412928	46.997606	49.168103
1102.855813	61.889662	49.173108
1099.281190	48.601508	49.178113
1096.175732	42.200221	49.183117
1092.618131	45.933703	49.188122
1089.404028	41.223067	49.193127
1086.090676	46.019305	49.198132
1082.349483	47.725078	49.203137
1078.251580	40.669253	49.208141
1075.121930	44.535056	49.213146
1071.523950	34.585205	49.218151
1068.089048	41.017167	49.223156
1064.501861	51.079681	49.228161
1061.067235	44.707797	49.233165
1057.357255	54.691464	49.238170
1054.425041	49.788007	49.243175
1050.612138	47.515497	49.248180
1046.921481	48.520504	49.253185
1043.775028	48.643036	49.258189
1040.102058	62.328865	49.263194
1036.828871	53.875254	49.268199
1033.074377	47.414255	49.273204
1029.906555	53.244428	49.278209
1026.369179	52.893493	49.283213
1022.453042	60.077871	49.288218
1018.788867	44.465748	49.293223
1015.728733	52.816411	49.298228
1012.103426	52.719697	49.303233
1008.758469	51.370526	49.308237
1004.892057	60.973741	49.313242
1001.854026	48.794364	49.318247
997.968771	45.115832	49.323252
994.248073	43.990015	49.328257
991.305085	47.415326	49.333261
987.498392	44.594537	49.338266
984.110424	48.288840	49.343271
980.538429	51.632306	49.348276
976.736154	49.427765	49.353281
973.458169	46.185675	49.358285
970.068293	56.324894	49.363290
966.874555	54.417383	49.368295
963.351395	53.690920	49.373300
959.257998	57.125525	49.378305
956.224923	52.348627	49.383309
952.507646	46.796169	49.388314
948.713228	45.008028	49.393319
945.366845	50.350487	49.398324
941.802737	55.230327	49.403329
938.575230	42.568117	49.408333
935.023212	62.676479	49.413338
931.696424	46.935641	49.418343
928.015798	55.933981	49.423348
924.473106	57.336649	49.428353
921.202100	45.725302	49.433357
917.326629	56.171525	49.438362
913.965836	44.476164	49.443367
910.545312	51.219139	49.448372
906.559226	57.803900	49.453377
903.726320	56.665656	49.458381
899.943573	54.046799	49.463386
896.617200	54.140603	49.468391
893.022914	53.985293	49.473396
889.210858	56.600748	49.478401
886.258962	51.671958	49.483405
882.154418	57.326145	49.488410
878.885248	39.991266	49.493415
875.930305	49.638457	49.498420
871.874997	51.475754	49.503425
868.347390	41.053064	49.508429
864.563743	47.172701	49.513434
861.669231	39.213536	49.518439
858.096648	45.961353	49.523444
854.311084	47.269198	49.528449
851.140197	42.089976	49.533453
847.466377	55.076790	49.538458
844.091570	48.815852	49.543463
840.452472	53.280359	49.548468
836.618217	48.100611	49.553473
833.486482	41.327052	49.558477
829.573091	45.413731	49.563482
826.628937	45.270537	49.568487
823.046893	47.464019	49.573492
819.243572	52.925526	49.578497
816.127889	44.921915	49.583501
812.429939	47.025982	49.588506
809.248282	44.506029	49.593511
805.466977	56.361239	49.598516
801.610215	59.265304	49.603521
798.456888	58.499974	49.608525
794.745003	48.700959	49.613530
791.128942	45.024658	49.618535
787.457143	55.325133	49.623540
784.303469	44.521219	49.628545
780.595756	41.099722	49.633549
777.467950	44.794482	49.638554
774.226480	51.851147	49.643559
770.699267	44.756725	49.648564
766.856669	49.284762	49.653569
763.338253	47.007386	49.658573
759.622936	51.407926	49.663578
756.433488	44.020171	49.668583
752.751812	52.781447	49.673588
749.231068	51.361823	49.678593
746.230483	46.921602	49.683597
742.508087	49.997637	49.688602
738.853647	48.450257	49.693607
735.526997	59.433858	49.698612
731.787959	49.544212	49.703617
728.762578	36.967509	49.708621
724.613166	56.739187	49.713626
721.281070	49.642703	49.718631
717.603327	42.815489	49.723636
714.154193	46.035403	49.728641
710.684207	48.945372	49.733645
707.190368	56.690152	49.738650
704.123046	48.353143	49.743655
700.644853	47.610249	49.748660
696.778356	46.551677	49.753665
693.464433	39.300503	49.758669
689.562915	45.587358	49.763674
686.234378	48.247392	49.768679
682.723695	48.202457	49.773684
679.334046	50.805625	49.778689
676.054936	47.589134	49.783693
672.248415	52.627251	49.788698
668.585276	42.491636	49.793703
665.128339	43.254543	49.798708
661.435720	45.278738	49.803713
658.376884	30.204771	49.808717
654.824647	45.491631	49.813722
651.476537	36.031194	49.818727
647.990178	36.067885	49.823732
643.992782	42.505813	49.828737
641.041951	48.128106	49.833741
637.130971	46.187509	49.838746
633.971133	45.853528	49.843751
630.015186	37.003988	49.848756
626.410234	40.988655	49.853761
623.457538	34.108049	49.858765
619.794889	45.865632	49.863770
616.311241	33.866953	49.868775
613.183229	40.807815	49.873780
608.665300	40.806762	49.878785
605.699478	30.416442	49.883789
602.079917	44.315476	49.888794
598.364453	40.895272	49.893799
595.140473	38.824953	49.898804
591.626918	34.449313	49.903809
588.591182	37.221710	49.908813
584.278355	38.896978	49.913818
581.043841	36.442336	49.918823
577.844396	41.293658	49.923828
574.380650	42.105122	49.928833
571.144158	48.015783	49.933837
567.021153	45.864814	49.938842
563.579816	43.268563	49.943847
560.307180	41.702588	49.948852
556.842912	43.532872	49.953857
553.421247	41.041112	49.958861
549.525235	42.720718	49.963866
545.917525	47.654977	49.968871
542.619596	40.989821	49.973876
538.761579	46.146783	49.978881
535.066984	44.836731	49.983885
531.401798	42.835539	49.988890
528.946341	44.071231	49.993895
525.399210	46.509292	49.998900
521.828443	52.750735	50.003905
518.463302	48.386679	50.008909
514.959786	40.424954	50.013914
511.224881	46.116303	50.018919
507.940425	44.811627	50.023924
503.796461	46.438339	50.028929
500.401386	49.523311	50.033933
496.682667	58.182907	50.038938
493.601106	48.392883	50.043943
490.094673	46.297239	50.048948
486.829598	52.032070	50.053953
483.176242	53.297210	50.058957
479.259171	52.651616	50.063962
476.333328	52.749277	50.068967
472.821470	49.240288	50.073972
468.864544	51.426180	50.078977
465.348133	47.414870	50.083981
462.273625	50.914718	50.088986
458.583919	49.154678	50.093991
454.956214	45.474017	50.098996
451.535426	48.654783	50.104001
448.488668	44.962225	50.109005
444.240933	49.702538	50.114010
441.168685	43.979677	50.119015
437.508942	50.067406	50.124020
433.907188	49.362952	50.129025
430.574734	48.337907	50.134029
426.845764	48.599346	50.139034
423.637520	52.041060	50.144039
419.931967	45.227830	50.149044
416.429550	45.899878	50.154049
413.266379	41.744676	50.159053
409.777058	48.444800	50.164058
405.960845	52.067171	50.169063
402.385084	41.750321	50.174068
398.726648	49.897466	50.179073
395.254173	35.230096	50.184077
391.988971	39.879803	50.189082
388.609600	43.984248	50.194087
385.225700	37.307317	50.199092
381.162990	47.520450	50.204097
377.898003	35.686953	50.209101
374.777520	48.052549	50.214106
371.217919	38.106510	50.219111
367.609916	39.260187	50.224116
363.704691	46.598113	50.229121
360.512560	47.142484	50.234125
356.824587	45.553060	50.239130
353.207327	40.649598	50.244135
350.161370	44.866345	50.249140
346.324197	47.043021	50.254145
343.141030	42.245573	50.259149
339.540026	43.958150	50.264154
336.017064	35.831877	50.269159
332.354194	40.107299	50.274164
328.841918	48.199934	50.279169
325.572213	42.628273	50.284173
321.884635	51.874669	50.289178
318.471032	49.644331	50.294183
315.329542	42.856690	50.299188
311.142673	40.649410	50.304193
307.858184	40.357217	50.309197
304.460130	43.135840	50.314202
300.999026	45.781972	50.319207
297.284094	39.447999	50.324212
293.702964	43.226577	50.329217
290.701395	48.480429	50.334221
287.188327	52.156600	50.339226
283.541749	44.992511	50.344231
279.568543	40.881997	50.349236
275.879085	49.413694	50.354241
272.970092	36.720885	50.359245
269.306621	38.354690	50.364250
266.197889	38.636094	50.369255
262.645513	38.385883	50.374260
258.835189	45.012956	50.379265
255.457963	37.234050	50.384269
251.627132	35.831566	50.389274
248.243634	43.419998	50.394279
245.102071	32.193654	50.399284
241.030543	41.449600	50.404289
237.705844	40.749282	50.409293
233.880880	44.613536	50.414298
230.602717	49.084996	50.419303
227.279028	43.721149	50.424308
223.729483	43.527458	50.429313
220.595126	45.916789	50.434317
216.395804	62.418789	50.439322
213.334286	47.377076	50.444327
209.855897	42.822083	50.449332
206.116181	50.320802	50.454337
202.646112	43.106955	50.459341
199.495095	49.054962	50.464346
196.189443	44.707031	50.469351
192.481631	49.600152	50.474356
189.169143	48.660657	50.479361
185.401762	46.042872	50.484365
181.805085	41.104626	50.489370
177.684480	38.200497	50.494375
174.769888	46.098308	50.499380
170.602293	51.512722	50.504385
167.863062	42.456987	50.509389
164.304597	44.280028	50.514394
161.139274	41.934929	50.519399
157.730468	43.073303	50.524404
153.737140	53.297800	50.529409
150.159352	46.917099	50.534413
146.681356	52.213996	50.539418
143.173789	48.188785	50.544423
139.469985	45.387054	50.549428
136.029462	49.425238	50.554433
133.121627	44.638523	50.559437
129.638073	48.376566	50.564442
125.748560	38.381093	50.569447
122.362892	51.930414	50.574452
118.394518	43.073594	50.579457
115.019708	37.951924	50.584461
111.800633	46.365689	50.589466
108.816737	51.493440	50.594471
105.477925	49.716544	50.599476
101.340892	46.504977	50.604481
97.583911	47.951023	50.609485
93.820984	39.150615	50.614490
90.433683	51.089852	50.619495
87.047060	46.147212	50.624500
83.634809	43.726935	50.629505
80.431063	45.459633	50.634509
76.955018	47.443802	50.639514
73.075953	44.397477	50.644519
69.659850	40.108034	50.649524
65.665518	45.922452	50.654529
62.678006	38.715325	50.659533
59.096958	46.958028	50.664538
55.683152	44.357673	50.669543
52.277830	40.762573	50.674548
48.769392	43.425706	50.679553
44.901482	36.347034	50.684557
41.547599	49.366213	50.689562
37.822088	41.841289	50.694567
34.784207	50.767691	50.699572
31.434520	44.610736	50.704577
27.839320	41.621198	50.709581
24.247802	38.688033	50.714586
20.734732	47.783802	50.719591
17.061818	44.901358	50.724596
13.432092	47.244987	50.729601
10.103424	37.924167	50.734605
6.507927	50.465522	50.739610
3.064884	36.031027	50.744615