Thu Aug 25 10:25:32 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.236297	100.431365	0.000000
0.608109	104.542998	0.005005
0.248881	95.092245	0.010010
0.135963	90.544692	0.015014
0.199555	77.791179	0.020019
0.185950	88.572278	0.025024
0.088223	76.559051	0.030029
0.117730	76.291891	0.035034
-0.344978	70.340659	0.040038
-0.678583	50.556267	0.045043
-1.237591	54.095559	0.050048
-1.298244	34.540501	0.055053
-1.421655	41.342965	0.060058
-1.699485	23.947985	0.065062
-1.856341	17.540725	0.070067
-2.190239	7.984811	0.075072
-2.585116	7.736690	0.080077
-2.916382	-1.727883	0.085082
-3.802337	-1.987646	0.090086
-4.107074	-10.535722	0.095091
-3.980623	-7.230391	0.100096
-4.419814	-13.935085	0.105101
-4.245231	-13.731431	0.110106
-4.651788	-4.533963	0.115110
-5.216894	-16.831400	0.120115
-5.785478	-8.889862	0.125120
-5.578456	-12.532068	0.130125
-5.690185	-10.670048	0.135130
-5.975486	-11.824348	0.140134
-6.303192	-8.264361	0.145139
-6.856684	-13.154143	0.150144
-6.741096	-11.900376	0.155149
-6.801411	-5.354587	0.160154
-7.069755	-4.869564	0.165158
-7.958000	0.774570	0.170163
-8.371596	-5.488050	0.175168
-8.320144	-13.883126	0.180173
-8.381454	-13.057221	0.185178
-9.096022	2.250232	0.190182
-8.647710	-4.900404	0.195187
-8.544732	-7.124773	0.200192
-8.965797	-0.588898	0.205197
-10.105318	-9.357354	0.210202
-10.358952	-8.513969	0.215206
-9.940614	-16.327453	0.220211
-10.131082	-5.825583	0.225216
-10.418517	-14.904711	0.230221
-10.759746	-21.333688	0.235226
-11.475451	-11.872652	0.240230
-11.579240	-16.032468	0.245235
-11.527956	-8.675267	0.250240
-11.604195	-10.754497	0.255245
-12.135493	-10.959097	0.260250
-13.175271	-9.517976	0.265254
-12.472465	-10.412645	0.270259
-12.914088	-11.786060	0.275264
-13.209588	-9.866772	0.280269
-13.216032	-17.474495	0.285274
-13.521812	-0.775776	0.290278
-13.953389	-18.165606	0.295283
-14.332141	-13.996513	0.300288
-14.542127	-17.987830	0.305293
-14.395914	-15.672682	0.310298
-14.791329	-8.799145	0.315302
-15.350851	-8.433014	0.320307
-15.631422	-9.809516	0.325312
-16.146959	-17.100193	0.330317
-16.280254	-5.288002	0.335322
-16.289746	-6.798727	0.340326
-16.032679	-9.901448	0.345331
-15.846502	-6.567510	0.350336
-17.121178	0.000872	0.355341
-17.015331	-8.826669	0.360346
-17.571375	-4.053995	0.365350
-17.224306	-7.275222	0.370355
-17.897669	-4.499466	0.375360
-18.610117	-6.210096	0.380365
-18.719398	-6.018912	0.385370
-19.202992	-4.367544	0.390374
-18.906715	-5.163717	0.395379
-19.186558	-5.629177	0.400384
-18.978728	-11.343758	0.405389
-18.882792	-17.483729	0.410394
-19.719512	-5.137383	0.415398
-20.158587	-7.931715	0.420403
-20.266507	-7.674307	0.425408
-20.749944	-9.113935	0.430413
-21.433313	-2.790061	0.435418
-22.073657	2.717156	0.440422
-20.931102	-10.872897	0.445427
-21.579031	-10.328398	0.450432
-22.019768	-8.076308	0.455437
-21.789556	-16.372841	0.460442
-22.266697	-8.341226	0.465446
-22.896415	-12.728684	0.470451
-23.461542	-9.242229	0.475456
-23.394122	-4.396399	0.480461
-23.550635	-13.594116	0.485466
-23.289233	-4.400068	0.490470
-23.583660	-14.231070	0.495475
-24.324439	1.146927	0.500480
-24.963559	-4.767146	0.505485
-24.976451	-8.900076	0.510490
-25.028862	-7.661115	0.515494
-24.734800	-10.038809	0.520499
-24.881668	-12.828305	0.525504
-25.661791	-4.837801	0.530509
-26.101724	-15.310388	0.535514
-26.638879	-5.649536	0.540518
-26.146973	-13.983910	0.545523
-26.496118	-10.733774	0.550528
-26.745184	-12.558136	0.555533
-27.189043	-12.817563	0.560538
-27.545850	-17.795107	0.565542
-27.662938	-8.402553	0.570547
-28.058484	-10.634232	0.575552
-28.406623	-7.890451	0.580557
-28.133802	-9.125872	0.585562
-28.763234	-9.764345	0.590566
-29.082119	-9.635232	0.595571
-29.702110	-6.238256	0.600576
-29.728284	-8.002629	0.605581
-29.718236	-2.768161	0.610586
-30.191801	-3.987874	0.615590
-29.882451	-12.761878	0.620595
-29.898652	-7.491662	0.625600
-30.110746	-8.945331	0.630605
-30.421825	-7.292519	0.635610
-31.259675	-8.217874	0.640614
-31.864924	-14.801635	0.645619
-32.051923	-0.915108	0.650624
-32.315452	0.075360	0.655629
-32.200219	-9.554077	0.660634
-32.355377	-7.742199	0.665638
-32.360559	-11.661202	0.670643
-33.066604	-7.655960	0.675648
-33.592037	-13.904215	0.680653
-33.556721	-19.803734	0.685658
-33.676657	-0.853083	0.690662
-33.579621	-2.570323	0.695667
-33.781450	-11.055426	0.700672
-34.290627	-3.559789	0.705677
-34.692456	-9.257940	0.710682
-35.204157	-0.989955	0.715686
-35.283956	-8.136936	0.720691
-35.495297	-3.162007	0.725696
-35.687705	-5.216708	0.730701
-35.861839	-6.562431	0.735706
-36.493032	-1.056648	0.740710
-36.472190	-3.919878	0.745715
-36.693306	-5.302532	0.750720
-36.326178	-1.816613	0.755725
-36.967658	-5.926983	0.760730
-37.921211	-6.432414	0.765734
-37.890089	-7.158567	0.770739
-38.075522	-1.532804	0.775744
-38.406064	-3.967656	0.780749
-38.407110	-5.239260	0.785754
-38.430475	6.438654	0.790758
-38.770474	-4.704491	0.795763
-39.437461	-1.252693	0.800768
-39.594564	-4.961233	0.805773
-39.065848	-9.897193	0.810778
-40.028192	3.133226	0.815782
-40.643676	-7.122034	0.820787
-40.511301	1.842297	0.825792
-40.921085	-0.551665	0.830797
-40.663661	-5.505230	0.835802
-41.056295	-6.655366	0.840806
-40.808287	-13.331691	0.845811
-41.782501	-11.018157	0.850816
-41.467178	-8.008175	0.855821
-42.152681	-9.045984	0.860826
-43.068260	-1.081710	0.865830
-43.143057	-10.947124	0.870835
-43.658309	4.253169	0.875840
-43.605950	-5.331617	0.880845
-43.466714	-5.166718	0.885850
-43.658990	-4.472150	0.890854
-43.787836	-7.302434	0.895859
-43.863149	3.137103	0.900864
-43.980651	0.529666	0.905869
-44.418193	-14.426311	0.910874
-45.074155	-1.295205	0.915878
-44.820654	-10.402142	0.920883
-45.986829	-12.326412	0.925888
-46.445243	-2.228646	0.930893
-46.047041	-6.543047	0.935898
-46.332351	-1.562856	0.940902
-46.072885	-7.614558	0.945907
-46.798062	1.139292	0.950912
-46.738392	1.126834	0.955917
-46.889718	-10.055360	0.960922
-47.768066	-3.922397	0.965926
-48.183461	-9.839882	0.970931
-48.192687	-3.741859	0.975936
-48.394945	-7.269317	0.980941
-48.317450	-5.677390	0.985946
-48.914809	2.471142	0.990950
-48.748308	-9.292360	0.995955
-49.132547	-8.570878	1.000960
-49.728330	-5.924335	1.005965
-49.528703	-4.933672	1.010970
-50.048980	6.217826	1.015974
-49.952863	-7.167138	1.020979
-50.563270	-6.527277	1.025984
-50.943300	-8.650655	1.030989
-51.343989	-7.565930	1.035994
-51.384835	5.459309	1.040998
-51.226246	-8.254980	1.046003
-51.339786	-5.930770	1.051008
-52.068333	-2.387069	1.056013
-52.197494	-2.221244	1.061018
-52.476556	-0.725307	1.066022
-52.657097	1.141169	1.071027
-52.967263	4.679427	1.076032
-53.757795	6.951528	1.081037
-53.709362	-2.278304	1.086042
-54.180136	0.459383	1.091046
-54.264066	-6.974850	1.096051
-54.021563	-2.675308	1.101056
-54.200811	-1.036824	1.106061
-54.187101	1.153554	1.111066
-54.692739	11.100540	1.116070
-54.823915	-1.612902	1.121075
-55.216941	3.216490	1.126080
-56.252798	-4.426091	1.131085
-56.421181	-5.459505	1.136090
-56.864765	-4.418678	1.141094
-56.930480	-8.454746	1.146099
-57.000292	-7.080181	1.151104
-57.127660	2.139981	1.156109
-56.906530	-0.495205	1.161114
-57.127292	-0.182150	1.166118
-57.354817	2.523751	1.171123
-57.775903	0.109415	1.176128
-58.486272	-0.323387	1.181133
-58.285221	-1.341920	1.186138
-58.767459	8.930427	1.191142
-58.960129	1.880223	1.196147
-59.642959	1.401977	1.201152
-59.968064	1.443482	1.206157
-59.618907	-1.183291	1.211162
-60.154388	2.962908	1.216166
-60.020799	-7.656491	1.221171
-60.132287	4.705940	1.226176
-60.907197	7.266657	1.231181
-61.426016	-2.206486	1.236186
-61.662407	6.037347	1.241190
-61.410107	-6.492569	1.246195
-61.481298	-2.570979	1.251200
-61.477328	-3.596597	1.256205
-62.281865	-1.932903	1.261210
-62.805003	7.516952	1.266214
-62.937679	-0.687925	1.271219
-63.159202	-3.120875	1.276224
-62.924922	3.470503	1.281229
-62.906592	-7.219421	1.286234
-64.014351	7.738357	1.291238
-64.267864	-0.830399	1.296243
-64.610150	8.217799	1.301248
-64.879026	2.973376	1.306253
-64.544886	0.709622	1.311258
-65.040532	-5.204780	1.316262
-64.999746	-9.210079	1.321267
-65.490368	6.837400	1.326272
-65.951409	7.830344	1.331277
-66.423355	-0.837063	1.336282
-66.079385	0.355609	1.341286
-65.806534	-9.611732	1.346291
-66.967551	-3.181378	1.351296
-67.287949	7.059282	1.356301
-67.548845	-1.612719	1.361306
-68.036231	5.942782	1.366310
-67.545908	0.025747	1.371315
-67.742683	0.455266	1.376320
-68.245981	-2.983894	1.381325
-68.975463	-3.862950	1.386330
-69.244444	-3.640416	1.391334
-69.328518	-9.593995	1.396339
-69.180415	-9.003381	1.401344
-69.398931	-6.944295	1.406349
-69.077624	-1.647869	1.411354
-69.866492	1.282029	1.416358
-70.371944	-4.795350	1.421363
-70.459805	1.644023	1.426368
-70.506869	-4.467216	1.431373
-71.299504	-2.767422	1.436378
-71.599003	-3.694869	1.441382
-71.591439	-1.310541	1.446387
-71.987048	-4.412236	1.451392
-71.967329	-5.142930	1.456397
-72.114487	-6.100575	1.461402
-72.162684	-1.594133	1.466406
-72.964842	2.894407	1.471411
-72.852656	-4.007410	1.476416
-73.394361	3.135824	1.481421
-73.541013	-1.507655	1.486426
-73.808071	8.047607	1.491430
-74.618450	-2.158129	1.496435
-74.631930	-2.858312	1.501440
-74.930819	-2.533014	1.506445
-74.760304	-1.496661	1.511450
-75.040332	-3.354135	1.516454
-75.336334	-4.734544	1.521459
-75.203128	1.983400	1.526464
-75.476741	-1.355708	1.531469
-76.263400	-4.180994	1.536474
-76.511860	7.149373	1.541478
-76.473607	-7.314847	1.546483
-76.512795	0.262172	1.551488
-77.013715	-1.785316	1.556493
-77.120856	-5.697834	1.561498
-77.775052	-1.014181	1.566502
-77.804943	-5.713919	1.571507
-77.724102	-0.133043	1.576512
-78.019049	11.049588	1.581517
-78.890324	-2.674175	1.586522
-79.271827	5.007102	1.591526
-79.558951	2.261730	1.596531
-79.459268	8.798269	1.601536
-79.175311	-2.866580	1.606541
-79.061397	-6.914975	1.611546
-80.224829	1.293781	1.616550
-80.334521	-3.507349	1.621555
-80.526519	-3.401279	1.626560
-80.664266	-3.686523	1.631565
-80.504935	-4.160684	1.636570
-81.878069	3.017915	1.641574
-82.025631	-12.850358	1.646579
-82.168559	-2.985524	1.651584
-82.120087	-0.319706	1.656589
-82.033911	0.046495	1.661594
-82.396435	1.251792	1.666598
-82.497551	-11.387256	1.671603
-83.333004	-12.151631	1.676608
-83.529919	-5.631898	1.681613
-83.748372	-7.625568	1.686618
-83.584037	-4.199626	1.691622
-83.918766	-7.307694	1.696627
-84.248772	-8.299963	1.701632
-85.188567	-4.378313	1.706637
-84.933787	-10.049630	1.711642
-85.797823	1.203183	1.716646
-85.589815	-13.999471	1.721651
-85.407289	-11.421098	1.726656
-85.700471	0.855902	1.731661
-85.576353	-8.300363	1.736666
-85.986946	-4.388868	1.741670
-86.596094	-5.501912	1.746675
-86.815012	0.717552	1.751680
-86.849711	0.498419	1.756685
-87.044632	-2.527153	1.761690
-88.066330	1.249145	1.766694
-88.285252	-6.647985	1.771699
-88.443941	-1.108671	1.776704
-88.374015	-3.998574	1.781709
-88.447724	-2.193130	1.786714
-88.303989	8.708791	1.791718
-88.686280	-4.259525	1.796723
-89.469072	-6.360919	1.801728
-89.555209	-9.239022	1.806733
-89.196137	-6.115675	1.811738
-90.234548	-5.497332	1.816742
-90.663356	-13.728565	1.821747
-90.939483	-4.076977	1.826752
-91.091811	-3.334885	1.831757
-91.064756	-9.536828	1.836762
-91.395636	-6.080747	1.841766
-91.050376	-10.662097	1.846771
-91.980826	-9.307701	1.851776
-92.363608	-13.895194	1.856781
-92.271893	-14.554912	1.861786
-93.092251	-9.139711	1.866790
-92.907433	-7.627876	1.871795
-92.810242	-6.823642	1.876800
-93.516599	-8.702896	1.881805
-93.537000	-11.828579	1.886810
-94.267504	-1.264239	1.891814
-94.425892	-6.807542	1.896819
-94.393371	-2.642778	1.901824
-94.750419	-3.137266	1.906829
-94.146835	-12.764124	1.911834
-94.814107	-5.999849	1.916838
-95.388715	-19.301847	1.921843
-95.973733	-17.561819	1.926848
-95.820025	-13.881115	1.931853
-95.706077	-11.165448	1.936858
-96.348048	-7.043692	1.941862
-96.610874	-13.595679	1.946867
-97.192652	-10.834271	1.951872
-97.127110	-6.459548	1.956877
-96.980886	-12.430228	1.961882
-97.759583	-6.812748	1.966886
-98.077809	-11.729894	1.971891
-98.436186	-16.938138	1.976896
-98.674717	-14.062837	1.981901
-98.526449	-9.995305	1.986906
-98.923060	-7.234437	1.991910
-99.012346	-11.406013	1.996915
-99.080247	-6.093543	2.006912
-98.980397	-6.340327	2.016909
-98.921370	-13.673387	2.026906
-98.347820	-14.174960	2.036902
-97.557255	-13.281866	2.046899
-97.388527	-10.355817	2.056896
-96.521492	-1.640767	2.066893
-96.142784	-13.576030	2.076890
-95.511733	-14.178479	2.086886
-95.006332	-9.752969	2.096883
-94.950926	-8.877728	2.106880
-94.278318	-14.995467	2.116877
-93.671637	-11.748405	2.126874
-93.112329	-11.170698	2.136870
-92.469215	-7.907169	2.146867
-91.913825	-18.026462	2.156864
-92.030436	-13.383113	2.166861
-91.197555	-14.977025	2.176858
-90.678507	-18.422433	2.186854
-90.207259	-14.146794	2.196851
-89.310806	-10.615686	2.206848
-89.146319	-9.161993	2.216845
-88.882215	-10.492554	2.226842
-88.228511	-14.019250	2.236838
-87.678657	-4.576595	2.246835
-87.007861	-6.804010	2.256832
-86.508898	-7.246378	2.266829
-86.219714	-16.503503	2.276826
-85.621917	-13.229705	2.286822
-85.317278	-10.416818	2.296819
-84.804765	-10.835967	2.306816
-84.323710	-11.890079	2.316813
-83.112719	-12.010029	2.326810
-82.922159	-13.389254	2.336806
-82.559657	-7.328948	2.346803
-82.552493	-12.100647	2.356800
-81.552948	-8.154872	2.366797
-80.976657	-5.888227	2.376794
-80.803736	-8.531804	2.386790
-79.597339	-8.530657	2.396787
-79.408517	-7.498925	2.406784
-79.006558	-12.709451	2.416781
-78.773439	-13.883103	2.426778
-78.131693	-7.252001	2.436774
-78.153529	-6.006697	2.446771
-77.094540	-9.004521	2.456768
-76.922752	-4.982896	2.466765
-75.715715	-3.638707	2.476762
-75.144189	-10.671939	2.486758
-75.378623	-1.911007	2.496755
-75.071107	-5.035004	2.506752
-74.175158	-11.929002	2.516749
-73.258425	-6.044235	2.526746
-72.633992	-4.298314	2.536742
-72.613924	-7.440626	2.546739
-72.463142	-11.236976	2.556736
-71.556900	-9.326138	2.566733
-71.299951	-3.372834	2.576730
-70.624866	0.405206	2.586726
-69.770732	1.617794	2.596723
-69.406271	-4.442163	2.606720
-69.402839	-1.749970	2.616717
-68.300624	-8.036395	2.626714
-67.586782	-6.614927	2.636710
-67.727885	-3.500946	2.646707
-67.660138	-8.000206	2.656704
-66.804489	-2.074188	2.666701
-65.357529	-7.758899	2.676698
-65.514460	1.604441	2.686694
-65.061599	-3.953016	2.696691
-64.921457	-3.715106	2.706688
-63.971760	-3.857467	2.716685
-63.538110	-3.142860	2.726682
-63.361652	-0.610826	2.736678
-62.156421	-4.059215	2.746675
-62.077812	1.985390	2.756672
-61.772997	-7.910915	2.766669
-60.799824	3.977476	2.776666
-60.663078	-5.277945	2.786662
-60.000409	-0.924588	2.796659
-59.542794	0.435660	2.806656
-59.428647	-1.137499	2.816653
-58.243278	-2.007364	2.826650
-57.937544	-4.082543	2.836646
-57.756745	-7.972296	2.846643
-56.900447	0.174243	2.856640
-56.330060	3.465012	2.866637
-56.145057	-10.115665	2.876634
-55.715487	-9.245198	2.886630
-55.414282	-2.684276	2.896627
-54.546885	-2.351243	2.906624
-54.011441	-5.482443	2.916621
-53.636138	-4.546452	2.926618
-52.936320	-8.625233	2.936614
-52.481604	-5.294166	2.946611
-52.123866	-4.380765	2.956608
-51.155577	-3.205070	2.966605
-50.998609	-7.227303	2.976602
-50.685309	-3.189836	2.986598
-50.329844	-3.083865	2.996595
-49.567727	-8.677106	3.006592
-49.042883	-6.446747	3.016589
-48.087493	-12.887560	3.026586
-47.944682	-8.956427	3.036582
-47.983400	-11.579514	3.046579
-46.819993	-11.904244	3.056576
-46.717524	-12.832512	3.066573
-45.858105	-14.259518	3.076570
-45.225777	-12.581356	3.086566
-45.017620	-9.202154	3.096563
-44.956674	-4.906568	3.106560
-43.643961	-15.230056	3.116557
-43.597075	-13.257425	3.126554
-42.998748	-5.308050	3.136550
-42.123514	-5.742849	3.146547
-42.085750	-5.251313	3.156544
-41.943107	-3.119456	3.166541
-41.130520	-6.461972	3.176538
-40.478561	-8.423506	3.186534
-39.355931	-5.146407	3.196531
-39.546321	-7.590508	3.206528
-38.798017	-4.983347	3.216525
-38.888990	-7.085066	3.226522
-37.730067	-10.123887	3.236518
-37.391477	-7.522222	3.246515
-37.254630	-10.730348	3.256512
-36.615414	-7.979384	3.266509
-35.969715	-5.752121	3.276506
-35.589190	-6.613083	3.286502
-34.749149	-3.703518	3.296499
-34.509391	-7.114669	3.306496
-34.337407	-0.403618	3.316493
-32.887722	-8.369560	3.326490
-33.122112	-6.875542	3.336486
-32.839060	-8.319944	3.346483
-32.032659	-3.713508	3.356480
-31.536789	-9.261864	3.366477
-30.528785	-13.765897	3.376474
-30.325396	-5.105243	3.386470
-30.270356	-5.069408	3.396467
-29.800899	-7.312790	3.406464
-29.037614	-7.574825	3.416461
-28.259659	-8.653280	3.426458
-27.490800	-2.685147	3.436454
-27.416448	-4.176044	3.446451
-27.134558	-6.709983	3.456448
-26.722372	-6.964523	3.466445
-25.759419	-9.868101	3.476442
-25.571506	-3.694902	3.486438
-24.667447	-6.085574	3.496435
-24.400770	-9.491439	3.506432
-24.421624	-7.112220	3.516429
-23.031389	-12.886238	3.526426
-22.735713	-10.816372	3.536422
-23.032607	-7.630465	3.546419
-21.895746	-7.092562	3.556416
-21.556395	-5.530050	3.566413
-21.022004	-3.798526	3.576410
-20.127597	-12.358537	3.586406
-19.779115	-10.825966	3.596403
-19.822349	-1.854238	3.606400
-18.857331	-9.250064	3.616397
-18.647793	-12.219325	3.626394
-17.896929	-7.493314	3.636390
-17.028470	-1.224005	3.646387
-16.848992	-7.324669	3.656384
-16.858106	-6.771935	3.666381
-16.229095	-7.703508	3.676378
-15.394727	-15.791614	3.686374
-14.223281	-5.638555	3.696371
-14.729278	-9.268644	3.706368
-13.827784	-5.570422	3.716365
-13.348913	-3.830199	3.726362
-12.838762	-9.754591	3.736358
-12.440235	-9.002801	3.746355
-12.066058	-4.794306	3.756352
-11.349892	-9.531378	3.766349
-11.152332	-5.469438	3.776346
-10.343485	-8.789192	3.786342
-9.390698	-9.853857	3.796339
-9.224569	-6.182966	3.806336
-8.887300	-12.634633	3.816333
-8.929868	-10.575126	3.826330
-8.296308	-10.902364	3.836326
-7.527998	-10.965614	3.846323
-7.023563	-11.431009	3.856320
-6.156457	-11.148611	3.866317
-5.403891	-9.942278	3.876314
-5.407396	-6.453882	3.886310
-5.091049	-9.645784	3.896307
-4.807625	-11.967722	3.906304
-3.896886	-5.435775	3.916301
-3.803499	7.129001	3.926298
-3.344373	14.957650	3.936294
-2.529560	29.148526	3.946291
-2.457687	35.206874	3.956288
-1.885445	53.553913	3.966285
-1.592760	61.883831	3.976282
-1.109468	90.869656	3.986278
-0.495700	107.018122	3.996275
0.000000	113.420736	4.001280
0.199636	119.637939	4.006285
0.556468	129.721943	4.011290
0.537333	144.496612	4.016294
0.673120	143.054861	4.021299
0.683911	152.376845	4.026304
0.715343	145.690101	4.031309
0.811401	139.110293	4.036314
0.488106	149.031951	4.041318
0.903863	142.569730	4.046323
0.619448	147.119550	4.051328
0.924409	138.656208	4.056333
0.825570	140.215667	4.061338
0.786642	145.745756	4.066342
0.867542	153.633060	4.071347
1.168462	163.102582	4.076352
1.168956	151.469385	4.081357
0.991597	157.577990	4.086362
0.971185	151.133486	4.091366
0.778119	143.039240	4.096371
0.845559	157.072688	4.101376
1.324119	157.364759	4.106381
1.456269	159.770719	4.111386
0.943002	150.847111	4.116390
1.229938	155.089114	4.121395
1.102465	151.379060	4.126400
1.237778	140.392302	4.131405
0.974211	141.154992	4.136410
0.681886	144.820196	4.141414
1.070326	162.365755	4.146419
1.057801	181.268137	4.151424
1.394631	174.176026	4.156429
1.204685	172.690396	4.161434
1.227127	171.560633	4.166438
1.511110	166.716754	4.171443
1.451650	170.048084	4.176448
1.340546	158.872132	4.181453
1.100208	154.724179	4.186458
1.240422	147.643902	4.191462
1.147362	146.854941	4.196467
1.041458	160.403022	4.201472
1.008702	169.864716	4.206477
1.421109	167.534896	4.211482
1.487232	169.210880	4.216486
1.448608	173.918350	4.221491
1.538842	165.279830	4.226496
1.152210	161.376261	4.231501
1.329948	167.486180	4.236506
1.318389	176.745239	4.241510
1.407635	174.152837	4.246515
1.182331	181.059905	4.251520
1.348189	179.660897	4.256525
1.353059	179.191951	4.261530
1.494866	181.134490	4.266534
1.381794	170.680179	4.271539
1.332741	176.756032	4.276544
1.804759	161.435924	4.281549
1.675960	175.367255	4.286554
1.312600	175.892480	4.291558
1.647593	173.546315	4.296563
1.339972	183.386442	4.301568
1.229959	177.095173	4.306573
1.516564	178.144987	4.311578
1.489869	186.621808	4.316582
1.764792	171.841939	4.321587
1.588761	179.149412	4.326592
1.365636	176.343360	4.331597
1.496372	180.935710	4.336602
1.766653	178.011222	4.341606
1.528984	168.740702	4.346611
1.543703	172.775422	4.351616
1.429120	175.197896	4.356621
1.579997	179.986408	4.361626
1.363703	193.931463	4.366630
1.758164	188.301472	4.371635
2.120269	195.556274	4.376640
2.120831	182.287375	4.381645
1.737579	181.044004	4.386650
1.411379	188.634440	4.391654
1.500524	182.603032	4.396659
1.680703	192.398372	4.401664
1.625683	194.343278	4.406669
1.979908	203.007197	4.411674
1.863063	205.455340	4.416678
2.211974	196.690853	4.421683
1.952143	201.543721	4.426688
2.021981	199.216951	4.431693
1.782679	191.281788	4.436698
1.702372	193.901376	4.441702
2.159647	198.429913	4.446707
1.804895	199.298642	4.451712
1.910289	199.535286	4.456717
1.890923	201.063315	4.461722
1.547450	211.073591	4.466726
1.844649	203.785196	4.471731
1.831594	208.327316	4.476736
1.820724	203.358781	4.481741
1.996128	202.360075	4.486746
1.731724	203.293742	4.491750
1.938960	192.602569	4.496755
1.626414	205.436410	4.501760
1.992342	199.048416	4.506765
2.160508	206.741737	4.511770
1.766212	199.314913	4.516774
1.985336	203.611844	4.521779
1.804374	211.356705	4.526784
2.140822	221.523049	4.531789
2.240472	219.966731	4.536794
2.200823	227.366751	4.541798
2.404839	213.904599	4.546803
2.272392	213.501460	4.551808
2.300496	206.831033	4.556813
2.234314	207.970926	4.561818
2.377665	205.110613	4.566822
2.350247	206.896171	4.571827
1.819199	208.684707	4.576832
2.345449	204.410305	4.581837
1.927195	199.496109	4.586842
1.924675	215.736226	4.591846
2.317001	224.659944	4.596851
2.376110	230.082948	4.601856
2.424268	230.850584	4.606861
2.373310	217.175277	4.611866
2.244385	228.148537	4.616870
2.304295	219.761517	4.621875
2.213579	235.271981	4.626880
2.133902	227.419361	4.631885
2.104731	232.925802	4.636890
2.180424	224.884322	4.641894
2.215379	226.356386	4.646899
2.360258	225.795899	4.651904
2.355935	228.723128	4.656909
2.200314	231.190005	4.661914
1.960062	228.155672	4.666918
2.241216	232.398599	4.671923
2.524218	240.228966	4.676928
2.749253	242.557109	4.681933
2.465933	238.700611	4.686938
2.432726	236.643083	4.691942
2.700683	228.944804	4.696947
2.522170	234.360748	4.701952
2.896146	233.938374	4.706957
2.561446	232.396324	4.711962
2.706538	226.697824	4.716966
2.666982	226.843283	4.721971
2.351261	228.677178	4.726976
2.577754	228.945469	4.731981
2.421866	229.162940	4.736986
2.521381	235.803999	4.741990
2.696318	238.949918	4.746995
2.581185	252.322343	4.752000
2.570137	258.417579	4.757005
2.794819	260.381944	4.762010
2.948640	253.717112	4.767014
2.901086	238.589078	4.772019
2.697871	236.653101	4.777024
2.168528	237.599806	4.782029
3.016005	238.536437	4.787034
2.865282	256.264642	4.792038
2.702500	256.347150	4.797043
2.879945	253.408721	4.802048
2.879613	252.636864	4.807053
2.783319	253.389169	4.812058
2.834075	251.745595	4.817062
3.148791	251.620410	4.822067
2.799260	238.830269	4.827072
2.637371	241.412025	4.832077
3.055792	240.125302	4.837082
3.010672	250.541274	4.842086
3.150604	235.674935	4.847091
2.981354	240.339613	4.852096
2.754609	238.132073	4.857101
2.887751	234.915848	4.862106
2.856238	242.105790	4.867110
3.251976	246.564887	4.872115
2.902090	246.692530	4.877120
2.916568	241.574479	4.882125
2.950251	240.022167	4.887130
3.080402	247.715134	4.892134
2.999831	241.865323	4.897139
3.080702	249.597649	4.902144
3.269797	249.061872	4.907149
3.074092	241.527984	4.912154
2.950485	239.291629	4.917158
3.086067	243.405505	4.922163
3.155969	251.658412	4.927168
3.097579	249.636466	4.932173
2.871774	247.688208	4.937178
3.289528	253.520103	4.942182
3.325220	250.306489	4.947187
3.051953	256.971162	4.952192
2.855601	248.589478	4.957197
3.171147	266.722369	4.962202
3.179318	267.363393	4.967206
3.337538	253.187043	4.972211
3.021149	262.139563	4.977216
3.372867	255.048251	4.982221
3.237051	253.671194	4.987226
3.137920	259.239224	4.992230
3.555903	250.264571	4.997235
3.176370	255.069768	5.002240
3.124062	256.517542	5.007245
3.109686	263.916782	5.012250
3.222665	256.907168	5.017254
3.223422	260.811216	5.022259
3.028598	261.582123	5.027264
3.238844	253.652427	5.032269
3.196505	254.437408	5.037274
3.167170	259.200393	5.042278
3.124253	255.571982	5.047283
3.364916	268.838053	5.052288
3.683750	271.616579	5.057293
3.390573	262.626793	5.062298
3.147781	263.598206	5.067302
3.183365	273.451048	5.072307
3.368527	276.497295	5.077312
3.859123	274.360857	5.082317
3.383545	279.570256	5.087322
3.678894	282.627713	5.092326
3.773132	277.762914	5.097331
3.713934	290.205940	5.102336
3.567431	286.429237	5.107341
3.450268	293.793973	5.112346
3.199206	293.526477	5.117350
3.774340	283.802676	5.122355
3.565314	288.347047	5.127360
3.551294	274.900028	5.132365
3.706772	291.909569	5.137370
3.523779	294.931243	5.142374
3.670658	285.875661	5.147379
3.562398	289.784141	5.152384
3.367467	289.482540	5.157389
3.854550	278.737978	5.162394
3.670229	291.912463	5.167398
3.681349	286.013469	5.172403
3.725393	290.511862	5.177408
3.801119	287.117960	5.182413
3.527492	288.075223	5.187418
3.243072	287.917358	5.192422
3.214550	288.269900	5.197427
3.731790	292.384101	5.202432
3.611009	299.059699	5.207437
4.094501	305.779829	5.212442
4.249848	292.853597	5.217446
3.960345	284.654172	5.222451
3.582387	285.880885	5.227456
3.653728	287.401037	5.232461
3.675769	287.074932	5.237466
3.914721	298.838492	5.242470
4.022468	302.507485	5.247475
3.872882	299.971468	5.252480
4.007699	303.259728	5.257485
3.978306	299.569078	5.262490
3.825580	311.450963	5.267494
4.047565	314.741387	5.272499
4.179020	315.758571	5.277504
3.630582	313.338830	5.282509
4.110920	304.518896	5.287514
3.956383	306.530027	5.292518
3.942824	301.584033	5.297523
3.943612	305.212837	5.302528
4.110647	305.746712	5.307533
4.291365	304.617452	5.312538
3.952037	303.544363	5.317542
4.361385	300.063385	5.322547
4.164878	308.266308	5.327552
3.872907	310.143947	5.332557
4.375832	312.052067	5.337562
4.497071	310.372134	5.342566
4.280587	298.130588	5.347571
4.206352	295.456214	5.352576
3.691293	290.316713	5.357581
4.032879	303.491065	5.362586
4.075412	308.226984	5.367590
4.387393	308.007313	5.372595
4.194403	306.607571	5.377600
4.166775	313.094571	5.382605
4.266791	308.026375	5.387610
4.063836	310.064075	5.392614
3.980379	307.628429	5.397619
3.741275	308.931465	5.402624
4.484718	304.202226	5.407629
4.238803	309.274408	5.412634
3.930916	315.783173	5.417638
4.562143	310.603272	5.422643
3.982416	311.216185	5.427648
3.933778	315.390580	5.432653
4.480236	320.829004	5.437658
4.202573	328.358109	5.442662
4.454558	329.691772	5.447667
4.505225	337.008083	5.452672
4.449127	332.755290	5.457677
4.758157	327.730272	5.462682
4.739355	326.417133	5.467686
4.232064	316.018175	5.472691
4.167487	321.226466	5.477696
4.413623	321.194284	5.482701
4.575761	323.598732	5.487706
4.617415	336.304403	5.492710
4.594672	334.093362	5.497715
4.545948	335.654477	5.502720
4.497052	334.346053	5.507725
4.459095	332.577164	5.512730
4.455206	341.490253	5.517734
4.476965	332.732665	5.522739
4.866638	332.621045	5.527744
4.875621	334.423058	5.532749
4.898261	338.466066	5.537754
4.954437	331.765884	5.542758
4.509965	320.164329	5.547763
4.557719	325.168357	5.552768
4.607336	335.227846	5.557773
4.574336	337.893827	5.562778
4.645982	333.880450	5.567782
4.741886	329.110290	5.572787
4.800365	325.086323	5.577792
4.724342	335.412273	5.582797
4.647888	328.179208	5.587802
4.574937	333.860220	5.592806
4.805857	329.135345	5.597811
4.891179	340.603460	5.602816
4.560961	331.160691	5.607821
4.577121	329.101746	5.612826
4.427189	335.823055	5.617830
4.996703	329.849212	5.622835
4.507077	345.159679	5.627840
4.726256	322.580160	5.632845
4.734967	333.705928	5.637850
4.666290	337.905615	5.642854
4.686233	327.854320	5.647859
4.889307	350.121020	5.652864
5.108800	353.902231	5.657869
5.213748	346.893840	5.662874
4.976517	347.446765	5.667878
5.031814	338.222004	5.672883
4.807016	336.396967	5.677888
4.780881	333.044326	5.682893
5.319685	343.087285	5.687898
4.846548	343.408248	5.692902
5.251435	349.495295	5.697907
4.691604	350.791637	5.702912
5.006674	355.747463	5.707917
5.526147	353.264801	5.712922
5.182478	348.876724	5.717926
5.170079	338.185075	5.722931
4.994143	338.228515	5.727936
5.172012	333.587882	5.732941
4.910797	337.988580	5.737946
4.762977	361.689690	5.742950
5.228543	355.219590	5.747955
5.268790	369.668761	5.752960
4.993219	372.154451	5.757965
5.464242	354.771532	5.762970
5.303989	359.216529	5.767974
5.324942	364.705665	5.772979
5.492649	362.186366	5.777984
5.235444	354.282410	5.782989
5.156557	348.704387	5.787994
5.168937	347.566697	5.792998
5.287944	361.914935	5.798003
5.463764	361.374907	5.803008
5.435652	367.545622	5.808013
5.420946	358.683002	5.813018
4.818626	358.856524	5.818022
5.263451	355.104217	5.823027
5.324672	370.869408	5.828032
5.355713	356.184547	5.833037
5.586575	360.144315	5.838042
5.353180	368.871910	5.843046
5.527559	365.646037	5.848051
5.613589	371.416049	5.853056
5.580643	363.480115	5.858061
5.775260	353.831715	5.863066
5.188534	348.731899	5.868070
5.394781	353.302972	5.873075
5.280973	357.810295	5.878080
5.639279	357.039191	5.883085
5.223182	365.358805	5.888090
5.360000	362.505819	5.893094
5.062986	362.900429	5.898099
5.505292	359.901501	5.903104
5.638598	362.573067	5.908109
5.775785	361.982143	5.913114
5.654598	366.468478	5.918118
5.808061	357.740864	5.923123
5.565580	361.081922	5.928128
5.627673	366.536139	5.933133
5.833305	365.054953	5.938138
5.419993	373.586110	5.943142
5.230735	369.218128	5.948147
5.395770	372.042914	5.953152
5.347641	358.490443	5.958157
5.723235	356.985792	5.963162
5.344270	367.501597	5.968166
5.540826	360.399753	5.973171
5.505356	379.144586	5.978176
5.714711	382.212370	5.983181
6.129276	378.585024	5.988186
5.648740	391.556053	5.993190
5.795055	383.418014	5.998195
5.859516	387.134936	6.003200
6.205695	393.487465	6.008205
5.658795	387.334177	6.013210
5.312857	376.346746	6.018214
5.819806	376.210423	6.023219
5.849556	398.589764	6.028224
5.868622	393.075474	6.033229
5.632797	395.956744	6.038234
6.007217	393.373415	6.043238
6.081801	386.910777	6.048243
5.843902	389.226049	6.053248
5.848669	374.614893	6.058253
5.754977	365.233126	6.063258
5.516724	375.967338	6.068262
6.065854	378.213081	6.073267
5.911656	373.972484	6.078272
5.819133	375.103860	6.083277
5.967538	367.712159	6.088282
5.334714	371.490871	6.093286
5.719660	376.125702	6.098291
5.744906	382.882858	6.103296
5.729663	382.591067	6.108301
6.098695	379.432771	6.113306
5.949912	388.137627	6.118310
5.892764	380.414289	6.123315
5.776440	372.820451	6.128320
5.592401	369.577966	6.133325
5.809211	370.157830	6.138330
5.933679	384.938673	6.143334
5.695789	366.673379	6.148339
5.882636	375.778067	6.153344
5.532433	373.317766	6.158349
6.181280	377.028546	6.163354
5.841272	376.667416	6.168358
5.494084	369.033820	6.173363
5.859780	369.334088	6.178368
5.782510	375.512507	6.183373
5.894926	377.984865	6.188378
5.620652	374.661604	6.193382
5.660360	369.201036	6.198387
6.412935	376.850322	6.203392
6.193259	375.059279	6.208397
5.794087	359.163644	6.213402
5.479788	366.711160	6.218406
5.665711	354.317940	6.223411
5.752374	355.180790	6.228416
5.670626	353.823727	6.233421
5.923766	355.207831	6.238426
5.875930	371.483664	6.243430
5.717392	363.073855	6.248435
5.419216	364.933488	6.253440
5.751345	374.325465	6.258445
5.555632	390.577027	6.263450
5.846327	386.029436	6.268454
5.981506	380.028715	6.273459
5.960315	384.350688	6.278464
6.015015	390.027537	6.283469
5.695814	380.178049	6.288474
5.584345	381.078271	6.293478
5.856907	375.957711	6.298483
5.916676	384.133171	6.303488
5.745937	395.840761	6.308493
6.063621	386.147751	6.313498
5.601023	385.305946	6.318502
6.022774	375.229634	6.323507
5.658508	364.058417	6.328512
5.626249	367.170383	6.333517
6.163243	374.840790	6.338522
5.776883	376.799664	6.343526
5.742841	357.347652	6.348531
5.662961	359.536920	6.353536
5.893932	357.925212	6.358541
5.905911	353.949654	6.363546
5.681346	363.650314	6.368550
5.742384	358.151606	6.373555
5.885768	368.509638	6.378560
5.490826	380.138449	6.383565
5.961346	377.685600	6.388570
5.959378	387.895572	6.393574
5.934057	368.350431	6.398579
5.631775	368.998971	6.403584
5.787046	362.223139	6.408589
5.984078	351.384771	6.413594
5.805584	371.964864	6.418598
5.729180	362.918917	6.423603
5.916467	363.645777	6.428608
5.417975	366.697913	6.433613
5.809892	368.313379	6.438618
5.845321	372.696082	6.443622
6.000647	373.519700	6.448627
5.418411	360.082551	6.453632
5.738721	368.910055	6.458637
6.035533	382.971020	6.463642
5.757913	389.551001	6.468646
6.052501	377.431809	6.473651
5.559033	377.075739	6.478656
5.667061	382.326608	6.483661
5.727850	383.750344	6.488666
5.657369	387.488408	6.493670
6.038977	381.879354	6.498675
5.931059	385.316394	6.503680
5.714160	387.824531	6.508685
5.880873	381.723954	6.513690
5.937447	389.649977	6.518694
5.851065	380.855524	6.523699
5.473104	374.368882	6.528704
5.640618	379.518679	6.533709
5.492008	386.590983	6.538714
5.370113	395.494113	6.543718
5.995178	391.507911	6.548723
5.908141	389.806819	6.553728
5.656256	397.392026	6.558733
5.923813	396.499095	6.563738
5.747255	400.782139	6.568742
6.185450	388.447446	6.573747
6.223160	392.336242	6.578752
6.186970	381.037680	6.583757
6.435173	370.662690	6.588762
5.755960	370.411655	6.593766
5.681568	362.694190	6.598771
5.637924	364.374736	6.603776
5.569631	361.595017	6.608781
5.575379	357.231286	6.613786
5.604591	357.982913	6.618790
5.885443	364.339340	6.623795
5.919425	373.971022	6.628800
5.920934	369.304228	6.633805
5.760441	366.731945	6.638810
5.898294	369.731835	6.643814
5.420240	358.037440	6.648819
5.663430	368.825931	6.653824
5.904489	376.166212	6.658829
6.046170	375.580911	6.663834
5.518260	378.571218	6.668838
6.269296	376.017470	6.673843
5.969192	371.236577	6.678848
5.688074	365.965485	6.683853
5.781259	366.422347	6.688858
5.695925	362.813216	6.693862
5.865510	370.674067	6.698867
5.523835	364.865125	6.703872
5.545527	369.949180	6.708877
5.983206	379.634675	6.713882
5.637831	383.795466	6.718886
5.859554	386.114655	6.723891
5.832514	392.924300	6.728896
6.153409	392.874078	6.733901
6.120643	374.725336	6.738906
5.698165	375.886262	6.743910
6.038756	363.215698	6.748915
5.794664	373.846417	6.753920
5.623285	363.062602	6.758925
5.898004	363.908643	6.763930
5.494130	364.487678	6.768934
5.694562	370.622585	6.773939
6.039127	370.350352	6.778944
5.660637	366.635289	6.783949
5.771911	355.971709	6.788954
5.975162	365.250994	6.793958
5.755090	368.322783	6.798963
5.701012	361.529131	6.803968
5.552401	369.889097	6.808973
5.942054	365.110868	6.813978
6.050907	373.212193	6.818982
5.850180	367.792461	6.823987
6.006276	366.220958	6.828992
6.155555	369.930915	6.833997
6.156360	366.456986	6.839002
5.782969	369.891324	6.844006
5.762630	369.296607	6.849011
6.010512	375.841704	6.854016
5.890063	377.353948	6.859021
6.123156	359.932372	6.864026
5.410491	383.965625	6.869030
6.101428	364.320920	6.874035
6.182681	378.788984	6.879040
5.814679	374.015565	6.884045
5.820371	367.193563	6.889050
5.512803	364.277323	6.894054
5.745063	366.085486	6.899059
5.751892	362.341691	6.904064
5.806579	378.968468	6.909069
5.698023	368.687343	6.914074
5.741203	371.059814	6.919078
5.701576	361.707543	6.924083
5.998930	362.904384	6.929088
5.707538	362.760266	6.934093
5.980707	365.422574	6.939098
5.632774	366.132052	6.944102
5.829228	363.519662	6.949107
5.765888	362.612138	6.954112
5.493969	358.007170	6.959117
5.536900	365.160187	6.964122
5.899548	370.057942	6.969126
5.727706	362.982179	6.974131
6.003945	361.002705	6.979136
5.907474	371.100921	6.984141
6.109367	363.178814	6.989146
5.822611	364.258363	6.994150
5.942143	359.566751	6.999155
5.797749	363.348029	7.004160
5.705522	371.597919	7.009165
6.061967	366.198459	7.014170
5.977687	361.766574	7.019174
5.851593	363.858678	7.024179
5.851452	362.491992	7.029184
5.709659	364.497969	7.034189
6.040195	357.587109	7.039194
6.067196	361.047298	7.044198
5.742234	350.512184	7.049203
5.614904	346.080720	7.054208
5.401940	363.638447	7.059213
5.641826	357.902906	7.064218
5.473896	362.494642	7.069222
5.460177	361.724878	7.074227
5.416158	362.013409	7.079232
5.373378	366.035035	7.084237
5.561216	362.661518	7.089242
5.555526	370.249269	7.094246
6.052852	371.155347	7.099251
5.531948	370.199289	7.104256
5.829641	383.782382	7.109261
6.188002	374.336109	7.114266
5.944419	378.167733	7.119270
5.813209	375.714250	7.124275
5.785307	360.902577	7.129280
5.403263	371.365081	7.134285
5.642449	358.890744	7.139290
5.753153	387.920359	7.144294
6.215220	381.384357	7.149299
6.000124	367.864367	7.154304
5.926489	371.485862	7.159309
6.029146	357.922421	7.164314
6.029990	360.367965	7.169318
6.022962	359.065634	7.174323
5.944718	363.766706	7.179328
5.804091	368.151682	7.184333
5.700491	366.592394	7.189338
5.397041	367.864387	7.194342
5.488005	359.054814	7.199347
5.750487	373.023071	7.204352
5.805460	372.584236	7.209357
5.866798	362.200564	7.214362
5.774024	373.687113	7.219366
6.060863	366.998234	7.224371
5.991093	350.038578	7.229376
5.865772	365.791864	7.234381
6.180145	359.937082	7.239386
5.850439	369.170157	7.244390
5.918102	364.125997	7.249395
5.954121	366.686254	7.254400
6.030128	365.943562	7.259405
6.144232	354.760675	7.264410
5.806245	364.922040	7.269414
5.683694	363.568205	7.274419
6.027237	366.624454	7.279424
5.880336	373.278862	7.284429
5.955234	364.259829	7.289434
5.572982	357.362571	7.294438
5.619030	360.209162	7.299443
5.796337	360.336463	7.304448
5.448323	363.994618	7.309453
5.938571	368.347188	7.314458
5.842425	373.297845	7.319462
5.883582	366.650623	7.324467
5.926583	375.379209	7.329472
5.734850	370.176370	7.334477
6.015645	359.941815	7.339482
5.965784	362.063104	7.344486
5.641366	350.439555	7.349491
5.722816	357.874441	7.354496
5.643847	364.666901	7.359501
6.013724	361.530622	7.364506
5.622848	357.744735	7.369510
5.607443	357.990817	7.374515
5.550503	359.489945	7.379520
5.432475	361.087231	7.384525
5.825948	363.230808	7.389530
6.034944	362.521064	7.394534
5.765803	358.997681	7.399539
5.540778	353.341312	7.404544
5.729000	351.128853	7.409549
5.420261	348.842395	7.414554
5.641329	358.254928	7.419558
5.697559	363.868253	7.424563
5.459015	369.189238	7.429568
5.452652	360.132318	7.434573
5.879470	358.341226	7.439578
6.136349	365.954276	7.444582
5.663873	366.018867	7.449587
6.066011	369.040625	7.454592
5.849784	369.776924	7.459597
6.194575	359.415282	7.464602
5.612524	367.665985	7.469606
5.855403	363.011995	7.474611
6.178001	363.195627	7.479616
6.075790	362.926954	7.484621
5.795437	356.127628	7.489626
5.889917	356.992417	7.494630
5.770030	355.451501	7.499635
5.849544	354.977183	7.504640
5.731797	360.937310	7.509645
5.609105	358.795711	7.514650
5.344003	368.828597	7.519654
5.682762	360.033983	7.524659
5.581641	351.589873	7.529664
5.825993	358.126025	7.534669
5.627249	357.736434	7.539674
5.243128	356.932955	7.544678
5.683541	369.715380	7.549683
6.425006	372.810525	7.554688
6.155821	369.802848	7.559693
5.860572	356.599150	7.564698
5.878825	361.921027	7.569702
5.938438	365.695652	7.574707
5.683186	358.598158	7.579712
5.787263	362.327850	7.584717
5.897098	356.255176	7.589722
6.147960	365.837055	7.594726
6.045802	361.607290	7.599731
6.167548	365.125404	7.604736
5.758285	355.277385	7.609741
6.001153	354.071945	7.614746
5.717305	360.902832	7.619750
6.003935	356.773507	7.624755
5.935365	364.399582	7.629760
5.808151	363.163539	7.634765
5.826305	359.474918	7.639770
5.823405	368.979497	7.644774
5.545995	363.147831	7.649779
5.877274	365.671318	7.654784
5.652284	358.660833	7.659789
6.292961	352.796058	7.664794
5.679702	358.352923	7.669798
5.523670	348.357662	7.674803
6.087780	355.982683	7.679808
5.678279	371.669766	7.684813
5.958805	364.542108	7.689818
5.776036	362.188455	7.694822
5.744072	362.781986	7.699827
5.922422	361.251290	7.704832
5.995102	364.593591	7.709837
5.936285	344.575989	7.714842
5.549455	349.831615	7.719846
5.797028	352.282793	7.724851
6.027529	355.037208	7.729856
5.910712	345.858393	7.734861
5.550071	328.292589	7.739866
5.382923	349.525785	7.744870
5.851949	346.418267	7.749875
6.104871	359.375596	7.754880
6.158138	355.709948	7.759885
5.702576	343.578597	7.764890
5.615303	353.700673	7.769894
5.833111	342.431942	7.774899
5.593989	350.407441	7.779904
5.846736	350.434336	7.784909
5.689426	363.984297	7.789914
5.979296	366.441505	7.794918
6.055711	355.460680	7.799923
5.918272	354.112342	7.804928
5.783805	339.969126	7.809933
5.915732	326.122709	7.814938
5.657324	334.117042	7.819942
5.751666	328.831427	7.824947
6.002997	340.257712	7.829952
5.169935	338.009114	7.834957
5.752395	354.765152	7.839962
5.765916	365.051779	7.844966
5.696084	360.209499	7.849971
5.754003	362.019667	7.854976
5.811102	369.322329	7.859981
6.145114	353.318151	7.864986
5.723487	365.628188	7.869990
5.882368	365.125615	7.874995
5.724638	360.025021	7.880000
5.564266	363.849932	7.885005
6.032033	354.696581	7.890010
5.640665	363.458416	7.895014
6.012794	369.098178	7.900019
6.002064	360.636737	7.905024
5.962685	358.070790	7.910029
5.984932	344.266854	7.915034
5.245701	335.549402	7.920038
6.018819	350.298189	7.925043
6.003530	335.747156	7.930048
5.397625	343.732662	7.935053
5.839485	350.623850	7.940058
5.799201	357.577928	7.945062
5.828477	366.340298	7.950067
5.668801	371.130062	7.955072
5.706076	363.679844	7.960077
5.868906	357.636832	7.965082
5.801446	362.614629	7.970086
6.016584	359.470957	7.975091
6.034436	354.029637	7.980096
5.755505	346.739702	7.985101
5.920330	333.707550	7.990106
5.721689	338.680583	7.995110
5.306648	335.891920	8.000115
5.772957	352.644693	8.005133
5.990111	363.397019	8.010150
5.910843	358.571755	8.015168
5.368308	359.748699	8.020186
5.871471	357.978446	8.025203
5.921167	357.137602	8.030221
5.909515	361.708984	8.035238
6.066494	359.292398	8.040256
6.103529	360.059805	8.045274
5.362659	348.802683	8.050291
5.786121	352.835685	8.055309
5.462959	361.539392	8.060326
5.413669	360.205983	8.065344
5.782323	367.040400	8.070362
5.551460	360.342292	8.075379
6.073192	369.289156	8.080397
6.002980	361.092149	8.085414
5.836838	355.052918	8.090432
5.506878	365.815229	8.095450
5.319357	362.799382	8.100467
5.795143	351.695607	8.105485
5.615252	363.753500	8.110502
5.997787	365.684888	8.115520
6.155498	377.611001	8.120538
6.151694	364.991869	8.125555
5.958694	362.036839	8.130573
5.821594	364.564028	8.135590
5.772840	368.570037	8.140608
6.109113	364.326591	8.145626
6.361688	360.635889	8.150643
5.926395	364.374264	8.155661
5.770041	368.239346	8.160678
5.978579	356.915513	8.165696
5.679024	361.771840	8.170714
5.953624	363.805344	8.175731
5.891954	360.741377	8.180749
5.855097	381.328910	8.185766
6.173765	383.030470	8.190784
5.949460	371.758668	8.195802
5.945986	371.083941	8.200819
6.032913	375.677750	8.205837
5.769264	385.842717	8.210854
6.273004	382.494502	8.215872
6.188854	378.247498	8.220890
5.963162	366.332146	8.225907
5.954082	370.887349	8.230925
6.220335	383.847320	8.235942
5.811303	361.982259	8.240960
6.160590	375.506713	8.245978
6.020293	383.787313	8.250995
6.343607	386.024621	8.256013
6.236967	381.039541	8.261030
6.385786	362.684615	8.266048
5.880877	365.086400	8.271066
5.658086	358.263954	8.276083
5.782960	364.940910	8.281101
6.132749	384.297089	8.286118
6.631102	384.032874	8.291136
6.160353	372.802840	8.296154
5.946459	365.704448	8.301171
6.359697	363.484391	8.306189
6.252810	372.880036	8.311206
5.831015	363.721967	8.316224
5.848921	367.285196	8.321242
6.071025	380.100606	8.326259
6.191075	385.102630	8.331277
5.951050	392.026113	8.336294
6.122375	390.825390	8.341312
6.290570	393.961143	8.346330
6.432553	373.896866	8.351347
6.169645	383.219134	8.356365
6.101155	375.211194	8.361382
6.327344	377.078719	8.366400
6.197541	361.594988	8.371418
5.987236	360.138489	8.376435
6.149542	368.002448	8.381453
6.412091	370.425996	8.386470
6.122462	377.432982	8.391488
5.955838	373.211524	8.396506
6.310699	385.842040	8.401523
6.389128	389.487307	8.406541
6.393234	377.924099	8.411558
6.725655	376.262645	8.416576
6.482002	372.069035	8.421594
6.057975	376.345278	8.426611
6.227886	370.496380	8.431629
5.922303	369.676488	8.436646
5.994675	362.792015	8.441664
6.448691	372.371171	8.446682
5.924879	375.407065	8.451699
6.565931	376.865614	8.456717
6.374916	381.689161	8.461734
5.940911	365.546204	8.466752
6.152653	373.449756	8.471770
6.242668	391.309802	8.476787
6.571331	390.112829	8.481805
6.717774	387.404407	8.486822
5.958694	367.913652	8.491840
6.302847	369.917324	8.496858
6.238411	377.939887	8.501875
6.315183	368.022061	8.506893
6.290718	392.451350	8.511910
6.361299	396.839447	8.516928
6.703881	394.081358	8.521946
6.012207	371.802988	8.526963
6.415741	371.471580	8.531981
6.551517	381.981052	8.536998
6.242087	370.268162	8.542016
5.923614	369.377707	8.547034
5.879794	383.383472	8.552051
6.493578	387.891581	8.557069
6.222280	393.059062	8.562087
6.609359	398.293800	8.567104
6.471578	401.329175	8.572122
6.277639	401.533182	8.577139
6.346652	393.248076	8.582157
6.154093	395.178056	8.587175
6.410305	395.109567	8.592192
6.356289	385.070215	8.597210
6.190433	393.197036	8.602227
6.495358	386.067840	8.607245
6.293592	386.544467	8.612263
6.302454	383.627233	8.617280
6.687712	390.796721	8.622298
6.333513	389.791944	8.627315
6.686457	392.371742	8.632333
6.585418	383.235988	8.637351
6.363575	395.025927	8.642368
6.317928	387.475140	8.647386
6.543540	388.575913	8.652403
6.440535	377.603831	8.657421
6.448413	385.627690	8.662439
6.348066	389.846911	8.667456
6.241949	388.090068	8.672474
6.458671	395.860309	8.677491
6.880957	389.432231	8.682509
6.528390	394.776545	8.687527
6.563478	395.165570	8.692544
6.745319	391.946683	8.697562
6.372904	398.105132	8.702579
6.576807	394.343156	8.707597
6.475471	398.190156	8.712615
6.309982	391.484949	8.717632
6.268239	385.312610	8.722650
6.546564	405.106033	8.727667
6.472225	404.950482	8.732685
6.580434	411.630067	8.737703
6.533471	418.034170	8.742720
7.061751	411.327551	8.747738
6.549796	412.862617	8.752755
6.441121	399.130136	8.757773
6.899859	419.990350	8.762791
6.720601	411.554790	8.767808
6.814340	398.465924	8.772826
6.396424	389.666988	8.777843
6.624527	387.920894	8.782861
6.436413	402.750840	8.787879
6.107206	411.793183	8.792896
6.936890	412.622589	8.797914
6.546437	417.471082	8.802931
6.888713	421.093950	8.807949
6.945278	417.623293	8.812967
6.976722	416.327723	8.817984
6.670187	401.815214	8.823002
6.396337	402.899571	8.828019
6.463151	404.138831	8.833037
6.447788	413.141469	8.838055
6.731332	421.216825	8.843072
6.868331	416.247210	8.848090
6.843946	427.270943	8.853107
6.803963	419.286919	8.858125
6.942518	419.965841	8.863143
6.723199	423.288544	8.868160
6.869484	416.411405	8.873178
6.837924	425.123102	8.878195
7.085665	404.824474	8.883213
6.475413	400.003500	8.888231
6.622791	407.816168	8.893248
6.856038	402.620042	8.898266
6.489568	411.415764	8.903283
6.643870	415.421526	8.908301
6.821418	417.157824	8.913319
6.669654	415.685835	8.918336
6.845337	415.383815	8.923354
6.701994	418.006662	8.928371
6.721338	414.847943	8.933389
6.820533	403.238262	8.938407
6.920108	413.728180	8.943424
7.160327	406.766900	8.948442
6.762537	419.878276	8.953459
7.153406	409.633509	8.958477
6.965164	407.413014	8.963495
6.899583	414.094583	8.968512
7.298199	410.573490	8.973530
6.576932	406.031835	8.978547
6.626872	397.651887	8.983565
6.806460	405.349057	8.988583
6.732362	411.760565	8.993600
6.727271	405.560387	8.998618
6.849707	406.857203	9.003635
6.739208	413.864539	9.008653
6.765438	412.528762	9.013671
6.657463	420.681240	9.018688
6.942596	410.838039	9.023706
6.596381	410.314839	9.028723
6.996612	413.174403	9.033741
6.957744	413.215262	9.038759
6.595586	413.385667	9.043776
7.429540	403.756276	9.048794
6.733943	413.458772	9.053811
6.835379	417.236137	9.058829
7.219749	418.491915	9.063847
6.873607	419.956821	9.068864
6.852228	416.637228	9.073882
6.838444	413.508947	9.078899
7.045071	416.477739	9.083917
7.052765	414.614701	9.088935
6.614985	412.856173	9.093952
7.241694	404.549952	9.098970
7.176672	418.660050	9.103987
7.093388	423.788615	9.109005
7.222769	412.906331	9.114023
6.840349	416.428154	9.119040
6.838224	410.063410	9.124058
7.020686	415.431196	9.129075
7.107863	411.195210	9.134093
6.924456	406.569283	9.139111
6.834543	423.460337	9.144128
7.276121	436.130949	9.149146
7.113287	440.776531	9.154163
7.485803	426.861340	9.159181
7.237330	423.760361	9.164199
7.227701	424.500369	9.169216
7.216705	417.076682	9.174234
6.973538	413.192249	9.179251
7.153115	410.443919	9.184269
7.124900	419.300253	9.189287
6.639538	420.843776	9.194304
7.356957	421.678149	9.199322
7.289269	422.960575	9.204339
6.926591	416.907935	9.209357
6.875857	424.016363	9.214375
7.101123	437.986322	9.219392
7.434954	446.965822	9.224410
7.438468	444.917246	9.229427
7.503040	439.747537	9.234445
7.076344	417.099395	9.239463
6.803952	418.685287	9.244480
7.232113	431.058203	9.249498
7.192116	439.979508	9.254515
7.124063	446.689878	9.259533
7.731407	441.015413	9.264551
7.319188	437.479347	9.269568
7.364141	420.917321	9.274586
7.398727	421.028720	9.279603
6.740821	420.507019	9.284621
6.969705	431.727754	9.289639
7.492549	441.662229	9.294656
7.308724	443.641338	9.299674
7.375386	443.476317	9.304691
7.663221	441.477867	9.309709
7.450570	419.285326	9.314727
6.797088	418.033956	9.319744
7.349480	426.338585	9.324762
7.150234	438.437430	9.329779
7.102780	439.628326	9.334797
7.518285	442.277222	9.339815
7.367703	452.967300	9.344832
7.187524	439.110295	9.349850
7.361776	445.729052	9.354867
7.725448	449.503206	9.359885
7.370509	443.992134	9.364903
7.153585	452.136450	9.369920
7.361514	441.393318	9.374938
7.382146	448.048769	9.379955
7.060176	444.751022	9.384973
7.245959	440.912981	9.389991
6.812505	448.658885	9.395008
6.867021	444.374360	9.400026
7.170155	442.963637	9.405043
6.933295	446.973891	9.410061
7.391220	446.605558	9.415079
7.260863	458.504278	9.420096
7.373913	461.699175	9.425114
7.834878	460.591920	9.430131
7.830588	460.479040	9.435149
7.389823	447.382368	9.440167
7.323741	452.075909	9.445184
7.547635	434.182509	9.450202
7.261828	437.600837	9.455219
7.566218	449.276803	9.460237
7.689433	454.145809	9.465255
7.269704	461.785428	9.470272
7.326080	453.565388	9.475290
7.469730	462.000347	9.480307
7.835305	472.221408	9.485325
7.724869	448.551702	9.490343
7.383094	448.971374	9.495360
7.586249	442.861628	9.500378
7.355294	451.724498	9.505395
7.893869	461.817463	9.510413
7.405345	453.231526	9.515431
7.336756	450.547318	9.520448
7.647130	461.790017	9.525466
7.806824	470.396033	9.530483
7.709016	457.144634	9.535501
7.596107	449.102597	9.540519
7.180156	457.091910	9.545536
7.593234	456.478144	9.550554
7.785862	464.586699	9.555571
7.751410	466.261545	9.560589
7.723565	449.597291	9.565607
7.387877	451.944172	9.570624
7.735800	458.800806	9.575642
7.734738	468.255659	9.580659
7.681763	471.729030	9.585677
7.569106	463.182026	9.590695
7.590201	474.466902	9.595712
7.880930	467.961580	9.600730
8.114078	462.112212	9.605747
7.468843	458.887202	9.610765
7.546589	452.579355	9.615783
7.579397	465.219362	9.620800
7.599972	461.735400	9.625818
7.858498	471.354705	9.630835
7.971687	474.271877	9.635853
7.580353	461.864870	9.640871
7.514004	466.877187	9.645888
7.801363	468.820343	9.650906
7.929215	465.483671	9.655923
7.781489	473.453056	9.660941
7.912283	463.378393	9.665959
7.786950	466.724248	9.670976
7.972363	465.975741	9.675994
7.854762	450.654120	9.681011
7.605035	456.042298	9.686029
8.051468	452.595754	9.691047
7.681047	448.567153	9.696064
7.589069	443.526111	9.701082
7.968580	453.006532	9.706099
8.009208	460.476194	9.711117
7.794035	450.376850	9.716135
7.521316	445.136912	9.721152
7.626544	463.761493	9.726170
7.919296	463.677811	9.731187
7.839218	468.376705	9.736205
7.908168	461.287607	9.741223
8.213466	482.257140	9.746240
7.700263	472.396981	9.751258
7.885558	466.971668	9.756275
7.423388	473.825848	9.761293
8.003768	472.516849	9.766311
7.747094	470.436454	9.771328
7.741703	464.835895	9.776346
7.595504	465.691975	9.781363
7.294356	467.320246	9.786381
8.141556	469.658516	9.791399
7.681994	475.994745	9.796416
7.707462	468.492741	9.801434
7.817261	473.704676	9.806451
8.145765	484.793072	9.811469
8.008191	474.167169	9.816487
7.968321	477.278732	9.821504
7.712623	477.732254	9.826522
8.245014	477.551066	9.831539
8.277551	479.411074	9.836557
8.460700	478.277920	9.841575
8.121785	474.256999	9.846592
8.298419	480.600846	9.851610
8.128914	474.233903	9.856627
8.001422	478.479488	9.861645
8.035385	473.854199	9.866663
8.066498	477.708866	9.871680
7.871125	474.795214	9.876698
7.955372	474.498052	9.881715
8.214322	484.978819	9.886733
8.142690	468.299318	9.891751
8.285749	471.293858	9.896768
8.295367	471.778392	9.901786
8.195563	475.764022	9.906803
7.943905	480.742262	9.911821
7.981175	481.039431	9.916839
8.560992	478.297807	9.921856
8.315161	472.687581	9.926874
8.052180	469.333250	9.931891
8.332969	476.512830	9.936909
7.901995	477.587096	9.941927
8.168883	478.173330	9.946944
8.069466	477.968060	9.951962
7.902580	482.383917	9.956979
8.144145	481.490914	9.961997
8.247468	475.728153	9.967015
8.138731	467.243648	9.972032
7.510647	473.940790	9.977050
7.942693	471.496871	9.982067
8.397367	486.178837	9.987085
8.446231	487.430383	9.992103
7.742650	484.252379	9.997120
7.772999	502.238647	10.002138
8.162458	500.584024	10.007155
8.148875	505.386116	10.012173
8.672881	498.904192	10.017191
8.405802	496.481447	10.022208
8.093036	498.483921	10.027226
8.338858	483.736482	10.032243
7.860217	502.594593	10.037261
8.194790	492.358599	10.042279
8.368957	496.799917	10.047296
8.461313	498.656866	10.052314
8.602364	491.569083	10.057331
8.285198	496.390336	10.062349
8.686664	504.049628	10.067367
8.916140	501.274531	10.072384
8.291079	501.492440	10.077402
8.327939	498.551866	10.082419
8.268633	507.848610	10.087437
8.269754	503.537723	10.092455
8.218730	498.622791	10.097472
8.151484	505.642321	10.102490
8.326333	497.397388	10.107507
8.274885	499.952200	10.112525
8.365115	500.720746	10.117543
8.427362	507.890399	10.122560
8.116123	499.791052	10.127578
8.507028	496.100739	10.132595
8.215809	499.658781	10.137613
8.510538	499.467493	10.142631
8.547993	497.473553	10.147648
8.498242	493.644003	10.152666
8.778698	497.645797	10.157683
8.409542	494.289163	10.162701
8.405031	485.431718	10.167719
8.637205	497.339934	10.172736
8.455730	500.385327	10.177754
8.673668	498.038065	10.182771
8.241973	500.766062	10.187789
8.425258	501.497938	10.192807
8.716774	497.479220	10.197824
8.190088	496.637160	10.202842
8.364892	493.823294	10.207859
8.553607	502.282769	10.212877
8.362691	506.263746	10.217895
8.841607	520.531694	10.222912
8.572172	520.255233	10.227930
8.650100	516.146901	10.232947
8.852977	507.818677	10.237965
8.665419	495.682672	10.242983
8.888023	492.763489	10.248000
8.759373	498.470375	10.253018
8.605071	493.312854	10.258035
8.764981	499.564655	10.263053
8.496717	493.743346	10.268071
8.726710	486.726833	10.273088
8.677501	495.700102	10.278106
8.706913	490.778881	10.283123
8.318687	495.866884	10.288141
8.388708	502.230598	10.293159
8.950470	515.305308	10.298176
8.543716	515.148191	10.303194
8.732428	514.212975	10.308211
8.687229	514.737657	10.313229
8.651938	525.356067	10.318247
8.820599	515.815076	10.323264
8.816701	524.531955	10.328282
8.990266	517.360173	10.333299
8.752321	528.022959	10.338317
8.982815	517.869528	10.343335
8.834005	502.795746	10.348352
8.455922	504.688535	10.353370
8.813248	514.535378	10.358387
8.695521	514.418181	10.363405
8.764061	523.530802	10.368423
8.782533	511.861116	10.373440
8.615475	518.542845	10.378458
9.083516	515.894467	10.383475
8.814993	519.136536	10.388493
8.459072	515.585322	10.393511
8.910032	523.599781	10.398528
8.717603	523.128220	10.403546
8.810678	523.334596	10.408563
8.641127	522.184118	10.413581
8.983624	523.235027	10.418599
9.034793	528.636042	10.423616
9.078240	523.630563	10.428634
8.951281	521.040695	10.433651
8.504676	522.609712	10.438669
8.740147	522.156313	10.443687
8.841870	518.097900	10.448704
8.471939	523.552268	10.453722
8.390394	517.938378	10.458739
8.632550	538.510778	10.463757
8.891940	533.799661	10.468775
8.900028	540.763221	10.473792
8.860800	544.300724	10.478810
9.103010	537.632568	10.483827
9.009177	546.767486	10.488845
8.932817	544.456862	10.493863
9.254003	546.044437	10.498880
8.908164	552.877264	10.503898
9.119165	546.889329	10.508915
9.326914	548.898615	10.513933
9.264684	552.935179	10.518951
9.411020	540.406006	10.523968
9.103164	552.026490	10.528986
8.954802	558.702148	10.534003
9.332109	554.865633	10.539021
9.275921	548.528245	10.544039
8.859115	535.787511	10.549056
9.173058	543.529961	10.554074
9.229104	556.907996	10.559091
9.057251	548.398628	10.564109
9.013724	561.173738	10.569127
9.385997	544.973717	10.574144
9.411069	555.996093	10.579162
9.604306	544.731343	10.584179
9.222395	530.776487	10.589197
9.123753	527.951811	10.594215
8.954167	523.667666	10.599232
8.917643	526.283260	10.604250
8.810451	530.945393	10.609267
9.491554	543.969868	10.614285
9.101335	538.514786	10.619303
9.254266	542.274642	10.624320
9.357862	548.143969	10.629338
9.384747	542.721362	10.634355
9.660923	548.450042	10.639373
9.156762	537.802643	10.644391
9.408999	530.949884	10.649408
9.214151	526.556089	10.654426
9.443931	528.940612	10.659443
9.295437	520.926208	10.664461
9.124545	523.739576	10.669479
9.164967	537.173693	10.674496
9.266929	542.251177	10.679514
9.419663	535.937864	10.684531
9.597849	545.588732	10.689549
9.496656	546.156901	10.694567
9.558217	537.610967	10.699584
9.080900	534.160820	10.704602
9.437496	537.137693	10.709619
9.505934	548.377328	10.714637
9.288745	553.631051	10.719655
9.458108	539.482518	10.724672
9.634055	549.979485	10.729690
9.348011	537.843103	10.734707
9.477782	532.593725	10.739725
9.351884	531.726737	10.744743
9.717561	542.178193	10.749760
8.940622	551.760965	10.754778
9.270429	541.446796	10.759795
9.567594	552.410759	10.764813
9.272481	554.353669	10.769831
9.514051	551.743925	10.774848
9.473836	552.769594	10.779866
9.222748	555.961601	10.784883
9.498680	553.419056	10.789901
9.186982	557.769259	10.794919
9.298714	543.733893	10.799936
9.210900	555.143180	10.804954
9.188538	553.149138	10.809971
9.282014	550.843461	10.814989
8.991399	577.331238	10.820007
9.808615	575.562251	10.825024
9.903585	577.106378	10.830042
9.762486	574.809049	10.835059
10.109970	565.249481	10.840077
10.056697	558.422489	10.845095
9.423098	553.917551	10.850112
9.649720	553.004796	10.855130
9.461190	551.784707	10.860147
9.673748	552.508843	10.865165
9.181187	552.415662	10.870183
9.499981	557.721106	10.875200
9.947175	572.842967	10.880218
9.636010	576.767063	10.885235
9.845364	577.917731	10.890253
9.939242	573.314586	10.895271
9.849571	555.110437	10.900288
9.496992	554.058060	10.905306
9.469279	550.587959	10.910323
10.087626	563.511829	10.915341
9.433939	572.693453	10.920359
9.918896	573.602126	10.925376
9.542685	569.183088	10.930394
10.000434	574.946443	10.935411
10.225380	578.455185	10.940429
9.703099	574.775392	10.945447
9.789205	559.011511	10.950464
9.835010	554.845088	10.955482
9.715302	550.998085	10.960499
9.941482	548.832560	10.965517
9.871376	552.598962	10.970535
9.621691	553.625893	10.975552
9.958184	569.251085	10.980570
10.124673	573.030914	10.985587
9.852456	554.602905	10.990605
9.524439	568.729081	10.995623
9.923263	562.238347	11.000640
10.201477	577.351975	11.005658
10.064663	570.970408	11.010675
9.766831	554.424096	11.015693
9.824354	565.703321	11.020711
10.062406	576.111678	11.025728
9.470187	574.301592	11.030746
10.148595	578.408309	11.035763
10.274702	574.718445	11.040781
9.944296	575.679130	11.045799
10.350803	567.495697	11.050816
10.364206	559.556894	11.055834
9.863140	560.446489	11.060851
9.908922	552.906554	11.065869
9.774995	555.493231	11.070887
10.142986	562.387787	11.075904
9.924574	550.430146	11.080922
10.168011	558.830582	11.085939
10.400016	567.876590	11.090957
10.396237	549.438085	11.095975
9.716209	554.044810	11.100992
10.009411	551.998170	11.106010
9.927527	558.171113	11.111027
10.001457	568.040298	11.116045
9.739656	569.372082	11.121063
10.297908	572.809666	11.126080
10.231407	573.852077	11.131098
10.069784	581.198846	11.136115
10.228844	569.497627	11.141133
10.006743	570.472901	11.146151
10.223078	574.541562	11.151168
10.228752	578.214046	11.156186
10.211833	576.228617	11.161203
10.163877	570.943958	11.166221
9.957036	574.514041	11.171239
10.142759	580.200099	11.176256
10.467793	562.347528	11.181274
10.375898	578.071405	11.186291
10.045985	576.977606	11.191309
10.284721	577.047553	11.196327
10.096371	573.328063	11.201344
10.530721	572.909774	11.206362
10.122181	575.037713	11.211379
10.490251	577.075531	11.216397
10.313252	580.350608	11.221415
10.589885	573.203680	11.226432
10.446674	574.703074	11.231450
10.048052	575.579774	11.236467
10.874046	572.499768	11.241485
10.425778	578.240978	11.246503
10.401403	580.270858	11.251520
10.827802	574.179738	11.256538
10.299053	555.233350	11.261555
10.264750	552.979251	11.266573
10.292049	561.896385	11.271591
10.450907	568.546002	11.276608
10.121220	568.708165	11.281626
10.014998	570.788737	11.286643
9.958554	570.302180	11.291661
10.194150	575.156766	11.296679
10.280491	574.518451	11.301696
10.343574	565.277996	11.306714
10.233069	574.428163	11.311731
10.876176	576.504939	11.316749
10.644397	580.170446	11.321767
10.699397	579.193063	11.326784
10.901861	571.480249	11.331802
10.197471	577.166916	11.336819
10.561587	577.712674	11.341837
10.381245	577.419096	11.346855
10.134627	573.591972	11.351872
10.238194	576.529603	11.356890
10.264487	591.733206	11.361907
10.574976	591.432152	11.366925
10.545558	600.130976	11.371943
11.194479	596.990347	11.376960
11.137907	592.275072	11.381978
10.543994	578.678439	11.386995
10.596022	570.825097	11.392013
10.382535	574.011216	11.397031
10.424896	572.887491	11.402048
10.852441	584.585276	11.407066
10.896274	586.500329	11.412083
10.884619	576.763498	11.417101
10.430567	573.136131	11.422119
10.446508	576.144294	11.427136
10.990509	595.482897	11.432154
10.751262	588.236911	11.437171
10.613779	580.627850	11.442189
9.979732	588.338971	11.447207
10.455552	595.989809	11.452224
10.744980	595.086147	11.457242
10.404398	609.558304	11.462259
10.445954	600.431655	11.467277
10.396439	601.042221	11.472295
10.754538	596.959401	11.477312
10.777185	592.963853	11.482330
10.895571	595.744532	11.487347
10.834659	595.435398	11.492365
10.740466	602.083651	11.497383
10.737047	609.629703	11.502400
11.121299	613.059844	11.507418
10.917891	613.180131	11.512435
10.879084	600.064548	11.517453
11.121206	598.278368	11.522471
10.871536	597.989341	11.527488
10.793453	592.286523	11.532506
10.516108	598.853019	11.537523
10.832261	602.394812	11.542541
11.163411	612.902212	11.547559
10.914719	621.553351	11.552576
10.773246	622.992517	11.557594
10.781962	621.864594	11.562611
11.118696	623.768473	11.567629
11.222540	628.927738	11.572647
11.340594	616.563888	11.577664
11.467644	617.399253	11.582682
10.850145	606.536043	11.587699
11.363260	588.950620	11.592717
11.256034	589.406128	11.597735
11.002118	596.540147	11.602752
10.829629	595.494265	11.607770
10.800820	598.701946	11.612787
11.450474	604.138599	11.617805
11.290612	597.706985	11.622823
10.772265	603.244591	11.627840
10.950930	604.248592	11.632858
11.119699	610.947165	11.637875
11.242452	616.103463	11.642893
11.496935	621.854500	11.647911
11.019388	605.396258	11.652928
10.844077	599.099606	11.657946
10.708108	615.808712	11.662963
10.950137	617.411851	11.667981
11.141243	616.394206	11.672999
11.101421	619.196520	11.678016
11.623639	619.083197	11.683034
11.398604	615.454652	11.688051
11.236829	616.265843	11.693069
11.058888	618.218803	11.698087
10.973262	629.312216	11.703104
11.094350	620.706423	11.708122
11.120014	622.640106	11.713139
11.196647	611.510347	11.718157
11.077557	622.448055	11.723175
11.114687	624.736544	11.728192
11.302236	616.091938	11.733210
11.047932	624.857567	11.738227
11.261935	631.668979	11.743245
11.547032	635.796309	11.748263
11.582732	642.440004	11.753280
11.683910	627.724576	11.758298
11.269184	630.683462	11.763315
11.306050	624.527126	11.768333
11.865329	620.365442	11.773351
11.602551	615.953866	11.778368
11.660753	616.048943	11.783386
11.669590	625.360318	11.788403
11.558342	620.186546	11.793421
11.613062	615.494853	11.798439
11.719965	623.724209	11.803456
11.815632	619.818200	11.808474
11.511375	621.456439	11.813491
11.483890	618.809946	11.818509
11.444218	618.535353	11.823527
11.287634	619.860123	11.828544
11.464174	618.705905	11.833562
11.517775	624.371653	11.838579
11.866201	626.179027	11.843597
11.421587	624.607739	11.848615
11.379988	630.323119	11.853632
11.774458	623.574271	11.858650
11.533229	623.066172	11.863667
11.450773	620.980554	11.868685
11.323605	618.592675	11.873703
11.377890	623.529330	11.878720
11.348798	622.388396	11.883738
11.398003	630.222855	11.888755
11.785043	644.530544	11.893773
11.958607	648.902568	11.898791
11.559663	652.127226	11.903808
12.040712	647.618034	11.908826
11.742596	639.109470	11.913843
11.400738	627.931663	11.918861
11.524877	636.297178	11.923879
11.801540	646.399727	11.928896
11.962924	642.445547	11.933914
11.521939	645.793554	11.938931
11.498205	647.182718	11.943949
11.970129	651.949805	11.948967
11.516830	646.810683	11.953984
11.582851	641.949956	11.959002
11.328667	646.843432	11.964019
11.481174	656.154402	11.969037
11.944805	645.462602	11.974055
11.536688	652.292602	11.979072
11.503728	658.675663	11.984090
11.603499	663.649384	11.989107
11.973369	672.348799	11.994125
12.409698	667.979151	11.999143
11.981937	664.104650	12.004160
12.212461	651.975617	12.009178
11.686528	644.481039	12.014195
11.890344	649.021891	12.019213
12.158410	657.519499	12.024231
11.998579	664.481014	12.029248
12.095351	648.964690	12.034266
12.127346	654.472888	12.039283
12.215149	649.630836	12.044301
12.375958	654.304659	12.049319
11.772614	647.383938	12.054336
11.804202	638.539697	12.059354
12.010136	642.903491	12.064371
11.707845	650.221835	12.069389
12.365398	652.899111	12.074407
12.211209	650.288245	12.079424
11.890130	643.055058	12.084442
12.454925	654.570439	12.089459
12.066961	650.787535	12.094477
12.157415	639.573544	12.099495
12.114127	647.810663	12.104512
12.096420	635.865700	12.109530
12.256100	653.904440	12.114547
12.399310	654.254440	12.119565
11.904654	654.918974	12.124583
12.193282	656.259197	12.129600
12.340461	660.206171	12.134618
12.213181	658.894427	12.139635
12.474138	655.546332	12.144653
12.062860	643.486304	12.149671
12.005661	653.268784	12.154688
12.382387	657.230285	12.159706
12.553110	670.274859	12.164723
12.264567	667.401020	12.169741
12.192563	648.256739	12.174759
12.048513	651.431992	12.179776
12.464255	658.328571	12.184794
12.701000	661.532526	12.189811
12.628582	660.092266	12.194829
12.625094	642.994828	12.199847
11.895432	650.288614	12.204864
12.370869	640.768919	12.209882
12.262515	647.324734	12.214899
11.934732	657.345269	12.219917
12.469632	651.953486	12.224935
12.430021	667.792326	12.229952
12.082691	664.564783	12.234970
12.541941	664.988341	12.239987
12.539254	665.515834	12.245005
12.640907	657.326476	12.250023
12.388588	667.887457	12.255040
12.279439	678.381831	12.260058
12.643416	673.231415	12.265075
12.511790	676.127017	12.270093
12.674060	666.769983	12.275111
12.467304	663.539350	12.280128
12.812308	652.541086	12.285146
12.459975	665.512976	12.290163
12.751086	665.095037	12.295181
12.778981	664.917154	12.300199
12.817791	667.265345	12.305216
12.863556	661.685111	12.310234
12.528683	664.517882	12.315251
12.877620	659.540240	12.320269
13.036753	658.167842	12.325287
12.599908	658.570855	12.330304
12.542577	656.225677	12.335322
12.480558	655.992454	12.340339
12.617974	660.026164	12.345357
12.576792	653.582246	12.350375
12.658480	659.688571	12.355392
12.977813	658.158530	12.360410
12.801807	650.470268	12.365427
12.317089	655.396710	12.370445
12.757989	662.185207	12.375463
12.987458	663.275925	12.380480
12.491335	659.607795	12.385498
13.176492	663.483102	12.390515
13.167932	659.091645	12.395533
12.907831	652.741988	12.400551
12.987930	662.026437	12.405568
13.027135	661.660590	12.410586
13.235077	662.439103	12.415603
12.832572	657.825348	12.420621
13.099946	652.112565	12.425639
12.695859	646.391381	12.430656
12.815018	651.901700	12.435674
13.213324	663.765063	12.440691
12.830582	650.816938	12.445709
12.940400	654.072336	12.450727
12.920665	662.204787	12.455744
12.893215	670.597226	12.460762
13.157813	668.514029	12.465779
12.729800	671.336148	12.470797
12.619815	656.584355	12.475815
13.069935	663.519730	12.480832
13.024622	659.569530	12.485850
13.213893	666.498439	12.490867
12.698740	664.998159	12.495885
12.948799	663.150770	12.500903
12.886574	661.835145	12.505920
13.009350	662.888931	12.510938
12.984612	660.516555	12.515955
13.098978	668.990914	12.520973
13.118028	662.149394	12.525991
13.475875	667.552894	12.531008
13.034333	660.256524	12.536026
12.832860	665.687696	12.541043
12.739392	665.970638	12.546061
13.118686	669.284803	12.551079
13.336167	687.945679	12.556096
13.025151	694.978231	12.561114
13.198822	688.241862	12.566131
13.462793	693.609585	12.571149
13.549349	684.425351	12.576167
13.193174	680.725821	12.581184
13.277655	688.296004	12.586202
13.350889	685.460153	12.591219
12.918140	678.951345	12.596237
13.455171	682.335472	12.601255
13.417982	696.962134	12.606272
13.478219	694.696360	12.611290
13.546666	688.617104	12.616307
13.393908	692.967684	12.621325
13.603409	688.920748	12.626343
13.344649	683.306169	12.631360
13.464868	674.091419	12.636378
13.474366	666.699131	12.641395
13.126822	675.858088	12.646413
13.236705	677.702843	12.651431
13.533598	686.445256	12.656448
13.213484	685.823283	12.661466
13.420655	690.707601	12.666483
13.460293	695.886412	12.671501
13.278506	690.572194	12.676519
13.303546	697.387993	12.681536
13.560118	694.479233	12.686554
13.552790	692.539625	12.691571
13.544980	695.620957	12.696589
13.698960	695.155076	12.701607
13.704624	703.334059	12.706624
13.553259	697.421784	12.711642
13.544187	688.927869	12.716659
13.478689	694.798492	12.721677
13.774803	690.999916	12.726695
13.314730	693.845996	12.731712
13.559472	692.381288	12.736730
13.898746	686.221730	12.741747
13.552114	694.626319	12.746765
13.353123	694.023238	12.751783
13.710617	693.938880	12.756800
13.587690	714.256260	12.761818
13.642893	711.164455	12.766835
13.866378	710.340546	12.771853
14.108982	714.433526	12.776871
13.791099	707.423874	12.781888
13.719411	714.993291	12.786906
13.787699	705.811907	12.791923
13.806523	710.959270	12.796941
13.813463	714.877735	12.801959
13.993118	721.599891	12.806976
13.349349	722.455047	12.811994
13.878368	717.297695	12.817011
13.537661	722.182657	12.822029
14.088986	717.492024	12.827047
14.069178	713.380025	12.832064
13.639528	714.984270	12.837082
13.578982	722.059640	12.842099
13.818314	719.235628	12.847117
13.688962	707.753077	12.852135
13.790542	715.307969	12.857152
13.512306	726.854497	12.862170
14.006655	722.245373	12.867187
13.898095	737.328219	12.872205
14.409422	739.785423	12.877223
14.344577	725.335768	12.882240
14.240764	720.028259	12.887258
14.103300	705.968694	12.892275
14.277935	716.749986	12.897293
14.274880	710.322165	12.902311
13.997553	706.588186	12.907328
14.036801	713.187170	12.912346
14.524887	711.706423	12.917363
14.020423	714.243883	12.922381
14.152754	710.717116	12.927399
14.218346	711.842981	12.932416
13.829292	710.660610	12.937434
14.125123	706.145709	12.942451
14.320795	719.501991	12.947469
14.368885	711.409363	12.952487
14.395761	712.844250	12.957504
14.307555	708.582023	12.962522
14.650785	709.042696	12.967539
14.439280	701.634528	12.972557
14.702180	707.652517	12.977575
14.372098	711.365011	12.982592
14.250378	703.204318	12.987610
14.293154	701.039109	12.992627
14.299365	705.989632	12.997645
14.649689	715.761944	13.002663
14.437660	702.992161	13.007680
13.894200	711.951459	13.012698
13.811785	713.201499	13.017715
14.067035	721.057364	13.022733
14.408711	726.760059	13.027751
14.878394	733.888057	13.032768
14.661080	736.175402	13.037786
14.772333	722.676456	13.042803
14.753200	725.330379	13.047821
14.460558	710.992166	13.052839
14.733613	711.441744	13.057856
14.500617	709.414415	13.062874
14.495458	711.466546	13.067891
14.524699	708.811152	13.072909
14.179046	710.768308	13.077927
14.560283	703.579693	13.082944
14.204414	729.598238	13.087962
14.813992	727.618774	13.092979
14.702852	739.315855	13.097997
14.360519	738.261861	13.103015
14.881034	739.436371	13.108032
14.731676	737.200275	13.113050
14.792124	738.787694	13.118067
14.548405	741.113890	13.123085
14.630187	743.401710	13.128103
14.797882	732.172403	13.133120
14.630061	741.224339	13.138138
14.800005	734.895635	13.143155
14.537488	731.023631	13.148173
14.477489	736.789265	13.153191
14.751688	739.223662	13.158208
14.699108	746.174716	13.163226
14.662420	734.803861	13.168243
14.330416	744.711498	13.173261
14.779316	731.449977	13.178279
15.321488	734.602935	13.183296
14.538790	737.284976	13.188314
14.588630	729.536048	13.193331
14.634674	744.550495	13.198349
14.910926	756.549808	13.203367
15.177377	759.313625	13.208384
14.983238	759.044296	13.213402
15.000576	773.144926	13.218419
15.103819	772.248336	13.223437
15.200905	756.747648	13.228455
14.990992	754.271729	13.233472
15.097947	757.060536	13.238490
14.987104	748.080766	13.243507
15.161852	758.638003	13.248525
15.375069	748.228373	13.253543
14.748531	740.891528	13.258560
14.816821	748.584193	13.263578
15.034102	742.652013	13.268595
15.343027	755.110108	13.273613
15.246328	759.502413	13.278631
15.541834	756.284587	13.283648
15.354113	759.416209	13.288666
15.410240	739.948796	13.293683
15.241108	745.428575	13.298701
14.659323	732.117102	13.303719
15.175500	736.842565	13.308736
15.404800	757.505595	13.313754
15.604677	744.510299	13.318771
14.973858	752.142089	13.323789
14.842410	750.616397	13.328807
15.245149	755.545831	13.333824
15.229370	752.774408	13.338842
15.240465	750.519482	13.343859
15.587946	752.308083	13.348877
15.449568	760.796839	13.353895
15.378473	745.814816	13.358912
15.413495	761.506346	13.363930
15.355882	759.511493	13.368947
15.544873	758.459457	13.373965
15.322218	762.025742	13.378983
15.731252	757.998021	13.384000
15.611506	765.328836	13.389018
15.715525	766.511799	13.394035
15.577520	759.085780	13.399053
15.400754	762.313516	13.404071
15.671745	757.278631	13.409088
15.507293	762.369518	13.414106
15.382052	753.770697	13.419123
15.526785	763.256511	13.424141
15.367780	753.179753	13.429159
15.486218	758.854320	13.434176
15.233334	756.009593	13.439194
15.415132	762.718805	13.444211
15.692809	763.754639	13.449229
15.307818	766.402775	13.454247
15.549261	759.791461	13.459264
15.635079	762.766617	13.464282
15.651561	766.828766	13.469299
15.796094	757.487087	13.474317
15.434358	769.598991	13.479335
15.880477	772.157935	13.484352
15.931883	783.283622	13.489370
15.856384	766.427722	13.494387
15.858833	762.021891	13.499405
15.796747	760.854559	13.504423
15.757123	760.267532	13.509440
15.883020	767.045464	13.514458
16.115005	767.599308	13.519475
16.042897	758.701826	13.524493
15.839033	752.030898	13.529511
15.792832	751.779416	13.534528
16.001188	753.659243	13.539546
15.918772	757.897831	13.544563
15.796168	753.426389	13.549581
15.790180	766.110557	13.554599
16.121941	769.217593	13.559616
16.168165	781.306612	13.564634
16.266789	766.575691	13.569651
16.178746	755.578941	13.574669
15.814363	759.524038	13.579687
15.809365	751.427086	13.584704
15.719590	760.558322	13.589722
15.927443	766.433477	13.594739
16.076669	773.343456	13.599757
16.422375	783.384772	13.604775
16.350376	774.480954	13.609792
16.228895	767.336365	13.614810
16.524948	776.912086	13.619827
16.306840	761.555453	13.624845
15.984017	759.718917	13.629863
16.211549	757.430079	13.634880
16.457043	764.722603	13.639898
15.962984	751.138595	13.644915
16.289427	768.513851	13.649933
16.446416	771.222237	13.654951
16.893444	765.771605	13.659968
16.167750	759.971384	13.664986
16.135405	751.875562	13.670003
16.261713	748.005749	13.675021
16.230325	744.192203	13.680039
16.431067	761.514563	13.685056
16.693424	761.785937	13.690074
16.576354	754.362951	13.695091
16.552779	752.656255	13.700109
16.079322	753.415301	13.705127
16.264627	743.928386	13.710144
16.532399	755.802794	13.715162
16.388928	771.699024	13.720179
16.404014	774.707355	13.725197
16.310585	775.122836	13.730215
16.872323	778.250646	13.735232
16.915991	771.310553	13.740250
16.507721	769.452690	13.745267
16.891620	754.598188	13.750285
16.040635	751.982871	13.755303
16.503471	766.831049	13.760320
16.450373	775.031895	13.765338
16.213011	774.040347	13.770355
16.542266	774.683092	13.775373
16.336574	784.059720	13.780391
16.544360	788.574739	13.785408
16.538213	782.349348	13.790426
16.318816	784.097382	13.795443
16.872061	774.729527	13.800461
16.380753	783.415602	13.805479
16.793661	772.712739	13.810496
16.392862	786.036292	13.815514
16.541574	799.314784	13.820531
17.006682	804.278641	13.825549
16.786374	799.516381	13.830567
16.855243	801.354952	13.835584
17.169116	811.186676	13.840602
16.938095	800.502636	13.845619
17.061628	797.911350	13.850637
16.852511	803.454216	13.855655
16.966821	803.925512	13.860672
17.287983	807.084708	13.865690
16.677471	795.882615	13.870707
17.095856	789.395046	13.875725
16.626783	788.433490	13.880743
17.193040	797.480894	13.885760
17.346477	799.388265	13.890778
17.045829	786.954199	13.895795
16.872056	786.328229	13.900813
17.233944	791.996221	13.905831
17.009728	786.076395	13.910848
17.001559	789.877324	13.915866
17.310866	802.430067	13.920883
17.554258	792.779390	13.925901
16.719268	790.000615	13.930919
17.034763	787.401345	13.935936
17.358416	795.833506	13.940954
17.218973	809.867211	13.945971
17.333086	803.256896	13.950989
17.213114	801.423288	13.956007
17.537273	797.519309	13.961024
17.485513	791.294751	13.966042
16.856974	774.058434	13.971059
17.377515	786.303514	13.976077
17.409664	803.469293	13.981095
17.638705	795.174707	13.986112
17.628632	775.648200	13.991130
17.284242	779.340859	13.996147
17.093891	772.134474	14.001165
17.300747	777.870934	14.006183
17.516247	784.051009	14.011200
17.598563	789.119019	14.016218
17.322380	792.703164	14.021235
17.260656	798.071456	14.026253
17.330385	801.181683	14.031271
17.248556	795.059664	14.036288
17.918063	794.588748	14.041306
17.229305	809.980310	14.046323
17.360469	801.312891	14.051341
17.178501	803.190762	14.056359
17.071424	789.669169	14.061376
17.648134	800.671538	14.066394
17.147551	805.471118	14.071411
17.409482	799.333107	14.076429
17.381290	812.415263	14.081447
17.791052	819.117182	14.086464
18.059373	816.866127	14.091482
17.712928	816.333482	14.096499
17.688580	808.267939	14.101517
17.542033	808.095295	14.106535
17.571700	815.484771	14.111552
17.881443	825.247723	14.116570
17.935484	827.899664	14.121587
18.051588	813.888647	14.126605
17.849548	811.471447	14.131623
17.570082	816.492007	14.136640
17.440574	827.106422	14.141658
17.587825	818.954028	14.146675
18.411769	824.524390	14.151693
18.043071	815.941593	14.156711
17.897925	832.620781	14.161728
18.121032	819.104238	14.166746
18.177243	830.876144	14.171763
18.082257	819.662691	14.176781
18.044936	822.799162	14.181799
17.707857	832.164842	14.186816
17.980773	822.004593	14.191834
17.757816	824.674687	14.196851
17.874353	818.770889	14.201869
17.911487	817.635345	14.206887
18.111435	812.621044	14.211904
18.033907	818.619824	14.216922
17.961846	818.385017	14.221939
18.129577	810.077938	14.226957
18.183682	817.517235	14.231975
17.698751	830.961302	14.236992
18.069783	822.404613	14.242010
17.994467	827.825536	14.247027
18.306109	819.047780	14.252045
18.208147	818.059635	14.257063
18.092180	831.928733	14.262080
18.385079	836.496701	14.267098
17.935657	836.819637	14.272115
18.315310	844.349951	14.277133
18.165419	852.786905	14.282151
18.379939	842.771494	14.287168
18.083279	848.422764	14.292186
18.133821	844.826734	14.297203
18.754503	840.532304	14.302221
18.728608	843.035824	14.307239
18.290930	841.447650	14.312256
18.633354	842.037842	14.317274
18.712369	842.599876	14.322291
18.622987	850.942142	14.327309
18.733146	838.781348	14.332327
18.341679	852.447472	14.337344
18.660785	839.853151	14.342362
18.796205	846.818971	14.347379
19.168783	836.027714	14.352397
18.696536	818.331363	14.357415
18.358623	823.165421	14.362432
18.558455	824.364935	14.367450
18.552800	832.750879	14.372467
18.814419	831.513890	14.377485
19.103105	833.614669	14.382503
18.556472	826.890120	14.387520
18.650503	822.201680	14.392538
18.440391	836.568372	14.397555
18.484747	835.942937	14.402573
18.649306	835.478551	14.407591
18.731325	840.713881	14.412608
18.933201	839.962780	14.417626
18.890177	838.483186	14.422643
18.681252	838.509664	14.427661
18.608884	838.035062	14.432679
18.841299	844.998307	14.437696
18.951070	835.750397	14.442714
18.761237	841.817274	14.447731
18.571048	832.360742	14.452749
18.804141	839.891926	14.457767
18.504634	840.554292	14.462784
18.920308	850.606775	14.467802
18.933210	862.685291	14.472819
19.216015	858.601585	14.477837
19.222361	862.640097	14.482855
19.209460	873.766449	14.487872
19.402612	864.401318	14.492890
18.956643	865.932393	14.497907
18.937853	867.257682	14.502925
19.208079	868.250508	14.507943
19.446348	869.491340	14.512960
19.466108	861.229513	14.517978
19.243455	846.836043	14.522995
18.944713	838.917620	14.528013
18.957963	844.744396	14.533031
19.244134	858.070822	14.538048
19.312560	852.890923	14.543066
19.360417	862.357254	14.548083
19.329042	865.353945	14.553101
19.498160	867.735396	14.558119
19.026976	867.780873	14.563136
19.490472	865.085820	14.568154
19.473609	864.694040	14.573171
19.148899	869.185213	14.578189
19.341339	865.516454	14.583207
19.418173	861.679615	14.588224
19.416777	864.539063	14.593242
19.542841	867.997084	14.598259
18.947732	862.936922	14.603277
19.386227	861.959398	14.608295
18.910023	862.857734	14.613312
19.430911	859.891757	14.618330
19.338372	863.652271	14.623347
19.906028	874.189043	14.628365
19.937411	875.156175	14.633383
19.506927	873.487975	14.638400
19.690756	862.044617	14.643418
19.715072	859.626660	14.648435
19.709322	861.151878	14.653453
19.550362	856.320030	14.658471
19.625518	873.359217	14.663488
19.775167	881.137024	14.668506
20.023049	877.039851	14.673523
19.600723	871.662280	14.678541
19.941359	871.773067	14.683559
19.649925	886.622758	14.688576
20.207735	885.661253	14.693594
20.003368	880.842824	14.698611
19.886908	858.309616	14.703629
20.253925	850.952755	14.708647
19.812185	857.696582	14.713664
20.162904	847.470479	14.718682
20.200366	857.430744	14.723699
19.636860	858.806664	14.728717
20.126312	851.847188	14.733735
19.856733	855.032678	14.738752
19.857552	852.820375	14.743770
20.089132	858.893815	14.748787
19.788315	875.632148	14.753805
20.081986	875.456803	14.758823
20.150860	885.831887	14.763840
20.142918	884.690778	14.768858
20.078579	885.676064	14.773875
20.038839	888.522589	14.778893
20.181315	885.009978	14.783911
19.777912	887.291784	14.788928
20.198130	881.210997	14.793946
20.039222	874.349941	14.798963
19.905203	889.070828	14.803981
19.963348	889.071240	14.808999
19.718652	887.358151	14.814016
20.588599	891.311855	14.819034
20.551837	901.877070	14.824051
19.995643	910.847929	14.829069
20.723627	898.344140	14.834087
20.214008	912.013043	14.839104
21.020149	898.304104	14.844122
20.468512	896.235159	14.849139
20.114798	886.091001	14.854157
20.917572	891.932947	14.859175
20.666923	876.912674	14.864192
20.233395	877.911622	14.869210
20.532932	874.551131	14.874227
20.524248	869.339127	14.879245
20.415446	879.559008	14.884263
20.784624	896.299684	14.889280
20.639252	890.995480	14.894298
20.624612	888.722478	14.899315
20.655630	907.084592	14.904333
20.865879	899.632352	14.909351
20.525108	896.501569	14.914368
20.449070	902.724208	14.919386
20.652783	904.071443	14.924403
20.405962	901.052172	14.929421
21.126537	896.104600	14.934439
20.477648	899.674578	14.939456
20.445839	898.837011	14.944474
20.806177	898.218871	14.949491
20.479880	903.742257	14.954509
20.935213	894.307629	14.959527
20.441846	900.254825	14.964544
20.772820	898.328462	14.969562
21.208919	903.006556	14.974579
20.865560	905.692370	14.979597
20.891122	898.218574	14.984615
20.991499	919.296469	14.989632
21.073992	921.663097	14.994650
21.330954	921.414607	14.999667
21.218039	920.630773	15.004685
20.935912	902.336501	15.009703
20.763414	913.254352	15.014720
21.375848	912.653519	15.019738
21.569797	923.488715	15.024755
21.101943	916.221608	15.029773
21.191504	904.452163	15.034791
21.081246	898.997287	15.039808
21.340021	907.300810	15.044826
21.495640	911.473737	15.049843
21.457986	917.838691	15.054861
21.474813	892.797760	15.059879
20.875069	899.130854	15.064896
21.065915	912.753126	15.069914
21.240248	920.732212	15.074931
21.528289	916.439388	15.079949
21.689134	915.287610	15.084967
21.676182	914.125194	15.089984
21.390063	904.879314	15.095002
21.599978	908.352607	15.100019
21.379948	911.356773	15.105037
21.359121	915.260698	15.110055
21.364797	927.905284	15.115072
21.656503	924.826879	15.120090
21.444079	917.317778	15.125107
21.478207	928.392614	15.130125
21.841278	921.670665	15.135143
21.212710	926.042201	15.140160
21.423820	918.151158	15.145178
21.701001	916.776024	15.150195
21.258725	925.012668	15.155213
21.867424	917.996614	15.160231
21.804074	919.350979	15.165248
21.522715	921.951341	15.170266
21.749153	916.093409	15.175283
22.256683	918.494429	15.180301
21.769213	923.323544	15.185319
21.302560	921.560019	15.190336
21.413960	916.105123	15.195354
21.629971	913.369942	15.200371
21.919071	932.382774	15.205389
22.243185	936.062244	15.210407
22.033859	927.056788	15.215424
22.055183	920.795486	15.220442
22.292254	916.961932	15.225459
21.845331	912.910496	15.230477
21.803598	907.779398	15.235495
21.839353	915.385715	15.240512
21.969775	924.659261	15.245530
22.354977	936.490145	15.250547
22.115593	941.665406	15.255565
22.689706	936.100136	15.260583
22.259503	919.757262	15.265600
22.164784	920.397013	15.270618
22.421549	906.871974	15.275635
21.936270	908.172524	15.280653
22.251096	912.270014	15.285671
21.887597	920.620546	15.290688
22.455596	932.410164	15.295706
22.698289	914.768961	15.300723
21.930867	919.739768	15.305741
22.448100	915.982240	15.310759
21.896530	922.743299	15.315776
22.346833	934.911124	15.320794
22.487138	932.752697	15.325811
22.747954	942.318249	15.330829
22.526701	944.773497	15.335847
22.789210	958.861107	15.340864
22.354827	942.758711	15.345882
22.672812	928.573961	15.350899
22.460417	932.542619	15.355917
22.418496	926.931859	15.360935
22.630439	933.614321	15.365952
22.589288	934.583354	15.370970
22.438007	936.822508	15.375987
22.514447	942.109234	15.381005
22.763632	930.497801	15.386023
22.360051	935.474723	15.391040
22.285007	937.143350	15.396058
22.816335	931.262890	15.401075
22.476182	939.066970	15.406093
22.442625	933.180339	15.411111
22.431784	937.836949	15.416128
22.715537	948.531857	15.421146
22.903097	953.561333	15.426163
23.083480	953.716165	15.431181
23.063016	957.964029	15.436199
22.980320	961.047672	15.441216
22.833580	947.794108	15.446234
23.033897	952.947819	15.451251
22.778609	956.172113	15.456269
22.991865	952.967139	15.461287
23.137232	951.155058	15.466304
23.008750	964.410831	15.471322
23.089685	956.221427	15.476339
23.323392	960.612507	15.481357
23.446506	952.672119	15.486375
23.219906	940.822797	15.491392
22.849874	945.570401	15.496410
23.231713	945.330748	15.501427
23.173059	959.938898	15.506445
22.984312	958.485282	15.511463
23.252830	952.863744	15.516480
23.339112	955.557990	15.521498
23.242817	962.339251	15.526515
23.453686	964.550070	15.531533
23.192106	949.379968	15.536551
23.384784	951.009805	15.541568
23.264652	954.402273	15.546586
23.587225	948.137945	15.551603
23.493642	954.407532	15.556621
23.413869	954.211801	15.561639
23.597654	958.459223	15.566656
23.096015	950.812382	15.571674
23.282860	947.444288	15.576691
23.573874	950.882792	15.581709
23.488851	948.153746	15.586727
23.271347	948.664411	15.591744
23.214142	956.957503	15.596762
23.631415	948.661756	15.601779
23.435526	963.199892	15.606797
23.722535	950.935572	15.611815
23.689896	957.526976	15.616832
23.503017	971.991122	15.621850
24.046937	969.349726	15.626867
23.726463	974.540858	15.631885
24.000419	980.049117	15.636903
23.855172	961.884818	15.641920
23.661303	972.383170	15.646938
23.905027	964.433348	15.651955
23.619836	976.186256	15.656973
23.786583	970.498606	15.661991
24.074586	964.580519	15.667008
24.151819	967.427665	15.672026
24.231109	972.357344	15.677043
24.354121	972.738918	15.682061
24.447544	968.845807	15.687079
24.116656	947.005653	15.692096
23.927672	951.365127	15.697114
24.241752	945.635466	15.702131
24.073130	948.155052	15.707149
24.054797	949.208873	15.712167
24.518513	955.498443	15.717184
23.932064	949.752083	15.722202
24.170326	949.307705	15.727219
23.911430	955.259207	15.732237
24.111256	970.584270	15.737255
24.466902	964.620870	15.742272
24.512616	970.471003	15.747290
24.377437	967.636202	15.752307
24.672973	973.784869	15.757325
24.177870	976.349300	15.762343
24.483198	970.179185	15.767360
24.629954	977.127500	15.772378
24.389507	973.526543	15.777395
24.479401	967.289196	15.782413
24.585585	965.221318	15.787431
24.618694	969.574402	15.792448
24.580551	976.491726	15.797466
24.776278	965.403048	15.802483
24.704195	964.354036	15.807501
24.633427	958.536344	15.812519
24.716591	965.759709	15.817536
24.793993	968.057712	15.822554
24.857260	964.652171	15.827571
24.693034	959.874769	15.832589
24.703049	957.645234	15.837607
24.804359	962.334772	15.842624
24.643312	967.649248	15.847642
24.747012	967.771913	15.852659
24.610555	973.047823	15.857677
24.483344	961.754122	15.862695
24.804081	954.464431	15.867712
24.555620	966.249448	15.872730
24.615125	964.602299	15.877747
24.404106	965.171910	15.882765
24.441676	964.449703	15.887783
24.653211	980.072744	15.892800
24.713592	987.782531	15.897818
24.926823	988.904217	15.902835
24.711740	992.687114	15.907853
24.833656	994.621536	15.912871
25.149554	997.652202	15.917888
24.584323	998.176324	15.922906
25.139949	995.416324	15.927923
25.340506	1004.581092	15.932941
25.097881	1002.984432	15.937959
24.994187	998.282744	15.942976
25.043748	1013.318958	15.947994
25.340592	1003.820741	15.953011
25.310686	1010.074059	15.958029
25.248153	1010.434212	15.963047
25.818622	1003.629244	15.968064
25.546557	1008.781243	15.973082
25.451509	1008.152397	15.978099
25.380292	1000.668474	15.983117
25.552283	1008.423901	15.988135
25.726836	1003.366187	15.993152
25.674566	1007.770527	15.998170
25.527658	1006.812132	16.003187
25.436077	1003.307766	16.008205
25.538696	1010.720608	16.013223
25.510742	1005.164440	16.018240
25.524071	1015.535679	16.023258
25.826393	1013.670599	16.028275
26.094927	1001.188230	16.033293
25.966832	1007.043516	16.038311
26.361217	1005.438571	16.043328
25.894831	991.367198	16.048346
25.732926	981.303388	16.053363
25.744025	972.206568	16.058381
25.651871	981.171030	16.063399
25.953726	989.429971	16.068416
26.207093	993.180499	16.073434
25.835539	990.919223	16.078451
25.773899	993.551443	16.083469
25.315822	1003.460040	16.088487
25.414687	1001.500604	16.093504
25.420553	1001.373507	16.098522
25.255394	1001.879128	16.103539
25.674546	1010.987559	16.108557
26.058109	1018.845543	16.113575
26.185938	1015.792799	16.118592
26.031588	1020.531877	16.123610
26.151763	1028.298586	16.128627
26.043083	1032.500329	16.133645
26.073452	1035.070801	16.138663
26.167424	1015.123781	16.143680
26.246326	1023.610177	16.148698
26.068977	1026.487753	16.153715
26.226047	1021.142435	16.158733
26.416757	1022.655821	16.163751
26.515916	1011.992505	16.168768
26.205094	1019.877233	16.173786
26.490277	1021.101258	16.178803
26.159748	1023.318013	16.183821
26.253287	1040.133570	16.188839
26.636688	1035.286126	16.193856
26.573990	1049.434229	16.198874
26.775257	1046.713962	16.203891
26.790494	1040.661858	16.208909
26.608084	1038.920060	16.213927
26.879337	1024.846699	16.218944
26.601562	1030.091118	16.223962
26.850880	1014.806199	16.228979
26.824428	1016.072739	16.233997
26.606222	1020.329509	16.239015
26.550881	1025.106724	16.244032
26.594757	1035.488968	16.249050
26.694173	1045.035683	16.254067
27.347089	1039.568489	16.259085
26.687628	1051.421113	16.264103
26.952583	1036.698623	16.269120
27.322187	1045.988408	16.274138
26.922891	1038.742067	16.279155
26.925554	1027.715159	16.284173
27.274019	1035.910014	16.289191
27.043827	1025.894748	16.294208
26.760107	1017.604657	16.299226
26.890913	1029.535422	16.304243
27.524886	1039.307654	16.309261
27.103590	1035.255329	16.314279
26.936884	1032.870433	16.319296
27.113047	1036.131286	16.324314
27.286093	1040.711774	16.329331
27.600304	1038.150540	16.334349
27.352280	1052.261409	16.339367
27.201385	1039.191467	16.344384
27.317210	1044.336352	16.349402
27.020704	1046.020751	16.354419
27.245698	1033.021311	16.359437
27.283178	1046.367908	16.364455
27.309290	1038.650966	16.369472
27.235158	1041.483970	16.374490
27.366013	1045.626094	16.379507
27.573103	1039.805867	16.384525
26.963306	1047.620683	16.389543
27.312953	1039.991907	16.394560
27.183966	1053.184708	16.399578
27.369033	1057.652862	16.404595
27.751816	1063.232460	16.409613
27.698188	1066.078034	16.414631
28.086614	1071.057137	16.419648
27.931488	1071.362368	16.424666
27.923854	1065.973414	16.429683
28.051364	1058.218486	16.434701
27.879551	1064.121666	16.439719
27.755274	1048.664875	16.444736
28.266991	1056.824694	16.449754
27.525940	1051.313965	16.454771
27.907978	1054.324811	16.459789
27.843008	1062.975781	16.464807
28.146930	1058.560513	16.469824
28.079065	1053.559702	16.474842
27.770478	1063.378637	16.479859
27.918319	1062.392993	16.484877
27.787496	1068.147739	16.489895
27.921023	1064.169428	16.494912
28.027326	1059.942915	16.499930
27.591181	1064.861857	16.504947
27.675734	1053.926245	16.509965
27.724104	1071.130767	16.514983
27.727687	1075.141357	16.520000
28.121501	1083.445896	16.525018
28.168503	1084.798763	16.530035
28.482723	1083.932220	16.535053
28.524108	1088.400802	16.540071
28.419022	1087.546304	16.545088
28.589213	1085.875491	16.550106
28.611352	1090.378648	16.555123
28.306341	1086.207105	16.560141
28.419114	1086.347284	16.565159
28.094104	1090.339933	16.570176
28.452838	1088.898359	16.575194
28.212424	1087.572750	16.580211
28.634783	1083.015841	16.585229
28.689638	1086.182098	16.590247
28.318227	1083.412694	16.595264
28.842116	1087.316520	16.600282
28.843589	1083.368362	16.605299
28.787906	1081.562522	16.610317
28.450971	1088.892784	16.615335
29.171685	1092.062016	16.620352
29.179720	1085.458749	16.625370
29.047214	1089.875681	16.630387
29.146988	1079.480477	16.635405
28.939531	1081.677956	16.640423
28.825992	1082.775105	16.645440
28.831902	1074.439608	16.650458
28.712801	1077.686769	16.655475
28.899336	1075.590510	16.660493
29.027272	1084.078720	16.665511
29.411046	1087.682601	16.670528
28.991210	1083.263957	16.675546
28.933193	1090.828235	16.680563
29.185977	1091.905860	16.685581
29.323573	1109.490922	16.690599
28.975489	1111.555801	16.695616
29.345836	1110.178679	16.700634
29.128795	1107.400864	16.705651
29.346288	1105.135647	16.710669
29.139928	1101.078034	16.715687
29.078621	1102.829732	16.720704
29.297889	1101.501529	16.725722
29.269131	1093.064155	16.730739
29.398344	1098.784481	16.735757
29.351976	1096.724711	16.740775
29.512456	1103.794004	16.745792
29.463656	1091.853607	16.750810
29.045480	1101.636084	16.755827
29.383015	1108.623989	16.760845
29.373324	1112.049677	16.765863
29.636240	1119.569996	16.770880
29.899221	1127.819313	16.775898
29.977371	1133.538182	16.780915
30.117242	1119.437994	16.785933
30.081104	1114.649950	16.790951
29.828803	1108.036970	16.795968
30.031892	1090.354461	16.800986
29.620273	1097.276698	16.806003
30.151601	1095.921693	16.811021
30.042550	1091.031468	16.816039
29.776418	1081.955937	16.821056
29.909742	1105.092823	16.826074
29.946363	1104.989309	16.831091
30.351900	1113.572897	16.836109
30.283885	1110.150027	16.841127
30.045411	1098.103641	16.846144
29.985518	1104.289106	16.851162
29.786020	1111.077125	16.856179
30.283704	1110.992893	16.861197
29.999988	1117.639473	16.866215
30.094546	1118.959645	16.871232
29.748572	1114.024482	16.876250
30.023505	1116.102203	16.881267
30.469134	1115.221381	16.886285
29.974208	1115.264266	16.891303
30.440402	1125.387886	16.896320
30.354014	1123.672061	16.901338
30.481807	1121.550286	16.906355
30.492276	1120.762891	16.911373
30.551146	1114.618717	16.916391
30.920554	1114.273711	16.921408
30.901886	1111.720439	16.926426
30.419111	1115.021430	16.931443
30.556100	1114.592916	16.936461
30.690024	1105.123327	16.941479
30.332261	1118.636048	16.946496
30.661853	1118.013252	16.951514
30.436251	1124.448753	16.956531
30.660936	1129.380943	16.961549
30.965391	1136.301457	16.966567
31.037453	1139.240961	16.971584
31.302800	1126.736913	16.976602
30.757503	1119.406115	16.981619
30.953872	1111.747674	16.986637
30.863175	1110.101955	16.991655
30.916733	1122.915905	16.996672
30.898754	1113.003043	17.001690
31.232372	1133.173630	17.006707
31.490866	1125.401306	17.011725
31.431536	1119.565990	17.016743
31.240283	1109.004923	17.021760
31.105318	1106.801240	17.026778
30.841999	1113.889599	17.031795
30.989794	1108.940192	17.036813
31.201932	1124.654785	17.041831
31.514085	1126.436337	17.046848
32.038847	1124.978215	17.051866
31.531362	1114.021714	17.056883
31.447155	1107.088903	17.061901
31.171308	1093.508313	17.066919
31.051163	1106.317908	17.071936
31.529542	1116.433303	17.076954
31.509535	1132.370471	17.081971
31.553600	1133.616503	17.086989
31.942301	1123.318019	17.092007
31.829475	1129.609619	17.097024
31.784895	1113.073601	17.102042
31.327887	1111.841887	17.107059
31.484902	1117.299081	17.112077
31.380136	1125.416663	17.117095
31.079162	1131.750365	17.122112
31.409402	1127.911637	17.127130
31.147401	1132.146892	17.132147
31.890488	1136.953679	17.137165
31.867086	1142.802074	17.142183
31.860139	1152.488590	17.147200
32.195884	1152.170948	17.152218
32.070489	1162.232641	17.157235
32.082277	1154.533672	17.162253
32.542163	1148.011070	17.167271
31.793824	1142.728677	17.172288
32.132207	1134.782882	17.177306
32.193497	1142.388451	17.182323
32.081083	1144.435344	17.187341
32.067853	1140.836624	17.192359
31.994197	1156.387735	17.197376
32.346193	1152.198446	17.202394
32.330158	1153.141464	17.207411
32.159791	1157.640085	17.212429
32.449517	1158.128090	17.217447
32.058874	1145.307077	17.222464
32.453966	1144.449951	17.227482
32.500952	1150.751233	17.232499
32.168782	1151.743782	17.237517
32.353086	1143.219353	17.242535
32.030211	1149.979380	17.247552
32.207202	1144.542540	17.252570
32.350242	1163.209266	17.257587
32.467510	1165.261202	17.262605
32.744694	1175.663780	17.267623
33.049583	1172.321330	17.272640
32.913164	1165.545003	17.277658
33.090445	1168.502741	17.282675
32.887999	1160.029431	17.287693
32.981894	1146.012166	17.292711
32.645672	1148.482298	17.297728
32.789643	1140.929887	17.302746
32.674524	1155.010545	17.307763
33.192901	1159.704220	17.312781
33.289320	1160.509696	17.317799
33.187171	1163.820489	17.322816
32.915480	1150.254985	17.327834
33.002364	1154.318815	17.332851
32.901952	1157.361086	17.337869
32.951867	1170.838375	17.342887
33.053716	1167.193216	17.347904
33.460192	1161.733039	17.352922
33.397489	1163.068386	17.357939
33.166890	1155.132833	17.362957
33.257517	1159.404366	17.367975
33.190164	1162.987424	17.372992
33.213226	1160.304529	17.378010
33.122650	1161.407552	17.383027
33.108724	1163.685175	17.388045
33.022507	1167.394269	17.393063
33.100220	1174.631196	17.398080
33.493678	1186.019131	17.403098
33.591618	1191.261537	17.408115
33.440468	1188.306123	17.413133
33.394350	1179.975573	17.418151
33.492212	1188.364401	17.423168
33.413796	1190.358634	17.428186
33.475720	1192.637001	17.433203
33.253189	1186.726244	17.438221
33.682123	1188.912394	17.443239
34.072950	1206.205405	17.448256
33.771904	1205.624607	17.453274
34.177474	1213.731700	17.458291
34.390356	1206.597665	17.463309
34.361960	1192.735226	17.468327
33.689905	1192.764836	17.473344
33.945104	1191.803391	17.478362
33.751622	1185.054931	17.483379
34.398478	1202.225772	17.488397
34.277250	1209.506507	17.493415
34.508759	1209.987855	17.498432
34.385562	1195.139853	17.503450
33.991364	1187.924211	17.508467
34.306057	1190.617421	17.513485
34.753163	1191.077613	17.518503
34.578821	1194.762649	17.523520
34.139327	1177.717231	17.528538
34.065106	1186.918833	17.533555
34.227252	1192.160647	17.538573
34.854358	1208.665542	17.543591
34.561728	1208.130763	17.548608
34.627205	1199.243063	17.553626
34.570889	1201.906039	17.558643
34.913109	1211.294877	17.563661
34.550389	1185.565057	17.568679
34.715240	1194.798635	17.573696
34.960150	1199.459425	17.578714
34.589508	1194.487078	17.583731
34.564466	1192.717452	17.588749
34.935508	1197.023957	17.593767
34.949971	1205.769850	17.598784
35.115936	1194.401665	17.603802
34.832876	1201.218590	17.608819
34.781212	1201.627537	17.613837
35.133506	1195.784510	17.618855
34.901455	1199.295547	17.623872
34.786804	1198.120643	17.628890
35.127610	1200.298510	17.633907
34.899686	1204.528443	17.638925
35.099795	1190.466099	17.643943
35.247178	1197.458585	17.648960
34.949073	1195.693871	17.653978
35.149261	1191.941778	17.658995
34.949747	1198.537325	17.664013
35.117451	1193.733101	17.669031
35.191401	1202.728455	17.674048
35.332801	1196.902691	17.679066
35.094962	1202.589038	17.684083
34.928980	1220.534205	17.689101
35.252367	1221.439827	17.694119
35.493094	1228.701730	17.699136
35.294496	1217.226542	17.704154
35.601384	1214.593846	17.709171
35.297647	1225.800700	17.714189
35.380053	1217.670907	17.719207
35.512643	1238.011968	17.724224
35.763506	1237.606635	17.729242
35.977954	1240.593277	17.734259
35.840100	1244.158994	17.739277
35.965924	1245.341730	17.744295
35.884701	1240.983605	17.749312
35.974321	1245.346837	17.754330
36.433493	1244.757385	17.759347
36.041359	1240.457440	17.764365
36.318066	1240.287906	17.769383
36.093909	1221.170004	17.774400
36.113371	1214.577523	17.779418
36.119427	1221.333379	17.784435
36.091762	1238.057657	17.789453
36.458100	1239.385750	17.794471
36.177092	1236.539040	17.799488
36.304907	1238.655606	17.804506
36.505406	1229.371186	17.809523
36.028236	1236.388955	17.814541
36.464491	1234.629103	17.819559
36.159176	1244.927320	17.824576
36.125846	1243.282068	17.829594
36.298896	1236.974792	17.834611
36.340521	1239.044900	17.839629
36.602181	1241.405591	17.844647
36.542877	1241.496991	17.849664
36.323833	1239.502129	17.854682
36.530870	1228.894367	17.859699
36.528142	1243.389843	17.864717
36.872995	1245.169440	17.869735
36.634342	1260.172121	17.874752
36.738244	1268.023538	17.879770
37.356769	1261.750602	17.884787
36.992160	1262.009760	17.889805
37.174996	1248.524449	17.894823
36.812991	1242.080090	17.899840
37.005073	1246.212669	17.904858
37.140608	1243.572101	17.909875
37.105299	1243.107461	17.914893
36.935167	1234.521753	17.919911
37.025439	1249.974677	17.924928
37.000389	1253.349148	17.929946
37.477234	1248.827843	17.934963
36.875316	1258.127939	17.939981
37.132288	1248.714737	17.944999
36.871722	1258.185419	17.950016
37.124632	1260.954593	17.955034
36.842399	1254.147427	17.960051
37.063460	1270.188964	17.965069
37.495192	1272.778640	17.970087
37.441901	1284.558534	17.975104
37.825065	1283.435019	17.980122
38.148852	1278.208676	17.985139
37.419295	1269.076265	17.990157
37.153061	1260.824347	17.995175
37.403930	1273.231940	18.000192
37.636198	1286.305195	18.005210
37.751265	1274.178050	18.010227
37.996185	1291.648644	18.015245
37.869461	1283.848241	18.020263
37.715140	1285.945899	18.025280
37.814480	1292.879676	18.030298
37.684079	1278.547145	18.035315
37.732649	1281.468261	18.040333
37.596800	1286.150860	18.045351
37.778957	1285.349181	18.050368
37.933352	1302.467885	18.055386
38.424040	1302.315319	18.060403
38.395054	1308.218293	18.065421
38.267848	1291.767641	18.070439
38.692367	1307.505927	18.075456
38.518760	1296.253998	18.080474
38.428791	1279.257865	18.085491
37.903677	1272.330951	18.090509
38.512998	1286.825245	18.095527
38.585886	1291.323657	18.100544
38.551278	1293.727617	18.105562
38.943197	1286.423484	18.110579
38.397647	1285.751599	18.115597
38.695506	1287.513316	18.120615
38.713979	1281.829863	18.125632
38.443484	1284.658955	18.130650
38.425162	1294.448319	18.135667
38.645257	1299.179298	18.140685
38.823797	1295.998637	18.145703
38.953799	1298.017035	18.150720
38.813789	1299.481272	18.155738
39.121312	1293.241273	18.160755
39.145049	1297.968301	18.165773
38.706442	1290.879499	18.170791
39.015445	1287.448019	18.175808
38.950364	1293.107328	18.180826
39.134597	1296.490044	18.185843
38.828592	1294.272108	18.190861
38.707427	1297.361837	18.195879
38.937920	1288.991053	18.200896
39.347777	1292.177468	18.205914
38.994046	1295.243671	18.210931
38.796229	1302.283972	18.215949
39.047149	1318.011595	18.220967
39.402301	1306.468525	18.225984
39.368664	1316.758933	18.231002
39.791839	1302.071398	18.236019
39.571613	1315.682643	18.241037
39.689207	1308.544561	18.246055
39.701340	1308.489065	18.251072
39.729365	1317.248668	18.256090
39.750150	1306.726848	18.261107
39.409533	1315.613637	18.266125
39.092691	1307.719931	18.271143
39.341208	1300.693887	18.276160
39.598089	1313.476119	18.281178
40.152560	1323.368265	18.286195
39.918011	1322.461454	18.291213
40.233946	1321.193831	18.296231
39.822237	1311.370950	18.301248
40.020194	1323.203027	18.306266
40.329076	1325.572110	18.311283
40.255468	1323.074755	18.316301
40.202935	1307.483418	18.321319
40.341174	1300.294766	18.326336
39.879294	1303.851300	18.331354
40.084164	1312.968213	18.336371
40.358246	1321.263220	18.341389
40.400453	1325.589718	18.346407
40.414722	1324.467192	18.351424
40.199592	1334.508326	18.356442
40.629550	1318.437429	18.361459
40.266595	1327.980996	18.366477
40.246539	1319.229718	18.371495
40.648566	1321.202342	18.376512
40.245138	1333.703023	18.381530
40.737948	1328.677408	18.386547
40.501266	1338.018154	18.391565
40.871335	1329.978945	18.396583
40.855913	1330.120276	18.401600
40.796595	1336.220522	18.406618
41.052104	1319.485813	18.411635
40.840154	1333.635434	18.416653
40.817396	1325.799788	18.421671
40.674915	1327.075061	18.426688
40.962376	1331.691348	18.431706
40.957198	1343.823517	18.436723
40.992673	1347.084378	18.441741
40.553405	1342.804417	18.446759
41.031311	1345.579380	18.451776
40.789360	1350.502688	18.456794
40.996048	1340.387237	18.461811
41.120596	1341.778469	18.466829
41.130957	1356.164685	18.471847
41.318643	1363.756856	18.476864
41.636668	1373.269495	18.481882
41.860045	1368.027299	18.486899
41.955707	1366.080949	18.491917
41.493236	1357.137028	18.496935
41.990800	1341.112324	18.501952
41.612102	1337.908506	18.506970
41.813456	1333.976315	18.511987
41.700486	1337.339330	18.517005
41.574319	1341.240917	18.522023
41.655575	1350.800108	18.527040
41.766764	1360.319900	18.532058
41.986982	1358.830578	18.537075
42.163693	1362.306007	18.542093
41.807269	1360.064403	18.547111
42.185618	1369.229907	18.552128
42.103609	1360.668202	18.557146
42.242870	1351.652098	18.562163
42.199681	1362.669887	18.567181
42.328846	1361.239014	18.572199
42.248460	1360.330138	18.577216
42.365905	1360.330728	18.582234
42.379729	1354.543836	18.587251
41.951696	1360.906993	18.592269
42.358832	1358.223855	18.597287
42.477999	1356.917629	18.602304
42.249345	1360.027365	18.607322
42.426080	1350.421546	18.612339
42.312927	1351.370323	18.617357
42.244059	1345.372320	18.622375
42.426920	1353.855209	18.627392
42.459290	1355.207234	18.632410
42.812737	1353.495060	18.637427
42.784834	1349.753425	18.642445
42.357581	1342.590237	18.647463
42.774960	1350.190598	18.652480
42.695342	1372.101987	18.657498
42.711449	1372.219443	18.662515
43.091308	1375.590460	18.667533
42.723882	1382.742575	18.672551
43.219908	1368.520116	18.677568
42.866765	1381.079225	18.682586
43.191098	1381.615465	18.687603
43.207707	1387.353526	18.692621
43.041988	1368.649202	18.697639
43.041401	1366.897819	18.702656
43.068378	1379.249044	18.707674
43.209876	1367.041953	18.712691
43.224353	1367.642519	18.717709
42.827176	1385.365290	18.722727
43.425182	1390.684046	18.727744
43.317737	1396.883375	18.732762
43.696883	1401.254934	18.737779
43.818092	1397.789738	18.742797
43.929118	1400.802078	18.747815
44.509063	1393.531560	18.752832
43.881393	1389.975406	18.757850
43.955884	1375.247765	18.762867
44.075781	1373.124042	18.767885
43.728474	1368.880160	18.772903
43.733365	1362.157360	18.777920
43.829299	1385.524538	18.782938
44.021497	1381.745255	18.787955
44.536665	1388.219430	18.792973
43.829514	1391.063301	18.797991
43.907322	1386.367788	18.803008
44.306545	1401.226465	18.808026
44.229240	1393.938997	18.813043
44.324599	1396.663447	18.818061
44.021922	1401.662558	18.823079
44.249585	1392.339083	18.828096
44.161447	1397.314047	18.833114
44.202999	1391.626944	18.838131
44.176882	1394.783851	18.843149
43.919265	1397.481550	18.848167
44.462521	1407.394436	18.853184
44.793194	1418.972245	18.858202
44.994460	1422.702624	18.863219
44.897733	1411.309184	18.868237
44.690242	1410.335011	18.873255
44.649840	1409.154771	18.878272
44.530215	1414.071555	18.883290
44.834455	1414.200674	18.888307
45.011399	1416.360059	18.893325
44.854026	1426.688852	18.898343
45.058811	1420.600610	18.903360
44.952490	1420.917136	18.908378
45.001932	1416.544808	18.913395
45.235929	1410.366782	18.918413
45.237679	1414.197849	18.923431
45.165698	1413.357084	18.928448
45.082831	1412.278175	18.933466
44.805054	1406.363377	18.938483
45.343574	1416.349597	18.943501
45.285968	1410.902093	18.948519
45.209674	1403.728076	18.953536
45.080368	1419.673158	18.958554
45.414698	1429.069660	18.963571
45.769546	1436.531527	18.968589
45.314163	1446.297929	18.973607
46.098772	1432.273211	18.978624
45.847969	1430.740911	18.983642
45.653313	1428.666465	18.988659
45.799160	1430.628744	18.993677
45.914120	1430.904289	18.998695
46.015775	1429.370419	19.003712
46.036022	1436.165160	19.008730
45.599860	1440.607661	19.013747
46.106053	1427.645931	19.018765
45.535408	1438.875800	19.023783
45.911267	1430.813547	19.028800
46.116095	1432.334225	19.033818
46.055872	1437.677226	19.038835
45.972762	1423.621201	19.043853
46.023604	1445.935134	19.048871
46.345232	1444.199534	19.053888
46.494498	1440.821456	19.058906
46.171164	1450.374660	19.063923
46.484280	1453.484739	19.068941
46.474214	1458.939813	19.073959
46.339507	1446.154226	19.078976
46.457153	1446.826997	19.083994
46.597974	1448.584931	19.089011
46.536334	1446.290818	19.094029
46.291997	1451.056732	19.099047
46.277366	1453.034689	19.104064
46.572961	1467.253224	19.109082
46.751767	1471.675125	19.114099
47.062435	1478.828338	19.119117
46.945968	1480.844346	19.124135
46.961253	1469.572180	19.129152
46.947406	1475.965163	19.134170
46.735538	1480.748088	19.139187
46.921343	1466.473165	19.144205
46.939061	1496.275059	19.149223
47.525333	1495.384808	19.154240
47.741978	1495.713853	19.159258
47.453439	1496.570191	19.164275
47.680476	1490.431100	19.169293
47.215861	1498.138152	19.174311
47.430101	1491.950571	19.179328
47.525890	1493.390504	19.184346
47.715422	1491.745026	19.189363
47.781108	1490.570251	19.194381
47.600955	1489.187830	19.199399
47.910453	1497.827679	19.204416
48.056748	1490.350499	19.209434
47.685389	1491.888870	19.214451
48.016466	1490.063420	19.219469
47.957017	1484.240626	19.224487
48.061277	1489.251747	19.229504
48.061262	1481.440873	19.234522
47.807239	1480.574976	19.239539
48.147629	1489.184733	19.244557
48.161874	1488.967953	19.249575
48.383824	1486.806136	19.254592
48.416439	1488.950271	19.259610
48.504390	1500.723959	19.264627
48.742854	1487.971397	19.269645
48.291264	1491.633657	19.274663
48.717416	1477.229547	19.279680
48.616045	1486.230421	19.284698
48.254847	1478.343588	19.289715
48.231578	1478.792275	19.294733
48.353081	1493.975419	19.299751
48.347193	1479.323404	19.304768
48.581213	1480.372435	19.309786
48.836666	1480.651216	19.314803
48.741276	1483.247768	19.319821
48.880253	1493.612223	19.324839
48.741052	1505.838087	19.329856
49.160920	1505.497793	19.334874
49.021078	1516.868505	19.339891
48.912303	1510.763086	19.344909
49.134126	1511.848744	19.349927
49.072645	1514.790298	19.354944
49.418449	1511.081599	19.359962
49.258167	1501.364394	19.364979
49.289074	1509.063245	19.369997
49.299877	1503.977396	19.375015
48.984181	1505.510203	19.380032
49.154666	1505.638188	19.385050
49.355137	1502.845391	19.390067
49.167653	1500.738253	19.395085
49.327350	1518.809426	19.400103
49.492706	1533.682763	19.405120
49.708491	1529.751424	19.410138
49.240284	1526.899280	19.415155
49.591374	1525.225332	19.420173
49.794533	1531.161439	19.425191
49.704446	1532.125546	19.430208
50.030039	1530.805902	19.435226
49.440575	1525.160814	19.440243
49.824105	1536.601024	19.445261
49.734854	1547.004424	19.450279
50.181086	1554.625600	19.455296
50.378722	1554.301188	19.460314
49.977558	1545.353878	19.465331
50.046324	1541.010051	19.470349
49.897796	1546.887650	19.475367
50.141573	1545.950068	19.480384
50.768618	1552.425710	19.485402
50.581726	1564.728516	19.490419
51.035715	1557.054771	19.495437
50.804191	1553.275564	19.500455
50.487687	1548.515550	19.505472
50.888810	1529.687532	19.510490
50.725399	1541.185034	19.515507
50.679766	1531.872746	19.520525
50.656569	1547.350017	19.525543
51.074837	1556.629289	19.530560
51.185325	1563.930670	19.535578
50.926230	1564.653004	19.540595
51.136761	1565.462712	19.545613
51.106928	1562.160010	19.550631
51.532151	1552.401538	19.555648
51.882438	1555.761443	19.560666
51.788217	1547.684422	19.565683
51.332911	1536.968802	19.570701
51.106910	1537.742757	19.575719
51.164877	1533.416403	19.580736
51.699028	1537.220890	19.585754
51.188260	1541.700352	19.590771
51.832290	1540.068872	19.595789
51.863975	1557.109212	19.600807
51.477153	1563.702679	19.605824
52.172104	1549.123848	19.610842
51.350688	1543.467756	19.615859
51.786717	1542.014038	19.620877
51.853056	1551.929140	19.625895
51.534185	1553.607621	19.630912
51.944666	1551.113288	19.635930
52.048411	1547.754945	19.640947
52.047634	1545.530183	19.645965
51.736026	1548.921203	19.650983
51.650734	1550.765069	19.656000
52.038595	1550.773787	19.661018
52.229793	1558.627435	19.666035
52.070006	1563.086628	19.671053
51.903973	1575.979491	19.676071
52.491721	1580.930667	19.681088
52.398051	1586.493557	19.686106
52.387708	1574.338518	19.691123
52.411323	1573.971940	19.696141
52.305651	1573.196409	19.701159
52.373933	1570.676788	19.706176
52.436384	1580.248517	19.711194
52.468224	1586.082090	19.716211
52.649913	1592.226717	19.721229
52.844595	1593.114653	19.726247
52.968541	1591.665643	19.731264
53.112529	1589.023700	19.736282
52.973101	1594.644257	19.741299
52.977955	1588.849227	19.746317
53.121380	1582.846287	19.751335
52.710459	1584.640183	19.756352
52.757740	1593.352721	19.761370
53.171273	1607.410873	19.766387
53.497878	1613.479152	19.771405
53.631232	1614.370385	19.776423
53.477285	1611.636256	19.781440
53.614606	1608.010697	19.786458
53.503258	1610.893804	19.791475
53.627067	1613.777940	19.796493
53.767562	1611.499476	19.801511
53.558926	1607.025517	19.806528
53.552433	1601.702498	19.811546
53.734945	1605.776697	19.816563
53.809406	1597.739499	19.821581
53.904978	1609.234340	19.826599
53.716128	1607.925859	19.831616
53.728564	1616.669116	19.836634
54.025012	1628.564863	19.841651
53.911747	1629.510516	19.846669
54.212698	1634.538200	19.851687
54.187802	1635.249091	19.856704
54.526753	1638.213137	19.861722
54.555730	1631.183490	19.866739
54.669005	1636.120652	19.871757
54.629730	1630.117917	19.876775
54.447323	1636.862430	19.881792
54.716663	1633.317173	19.886810
54.658093	1629.577127	19.891827
54.718609	1623.574539	19.896845
54.779922	1620.891893	19.901863
54.777865	1628.706419	19.906880
54.992155	1624.144103	19.911898
54.617779	1632.329403	19.916915
54.682670	1629.756654	19.921933
55.190048	1633.063559	19.926951
55.024492	1646.278306	19.931968
55.086656	1651.296067	19.936986
55.098488	1653.127883	19.942003
55.169772	1649.522130	19.947021
55.590277	1657.551344	19.952039
55.275171	1654.466899	19.957056
55.421581	1645.487398	19.962074
55.375678	1646.757029	19.967091
55.668730	1647.288712	19.972109
55.236396	1639.116292	19.977127
55.087113	1649.273524	19.982144
55.541007	1647.365696	19.987162
55.736457	1642.235098	19.992179
55.312591	1641.487325	19.997197
55.724916	1653.270256	20.002215
55.903839	1666.449982	20.007232
56.131231	1674.149680	20.012250
56.071622	1675.052213	20.017267
56.083779	1662.985112	20.022285
56.195993	1675.174857	20.027303
56.183087	1663.231609	20.032320
56.333560	1666.641777	20.037338
56.121008	1674.053779	20.042355
56.140927	1671.892034	20.047373
56.148476	1671.392264	20.052391
55.952198	1669.548429	20.057408
56.326499	1669.130061	20.062426
55.876163	1669.393186	20.067443
56.176188	1683.118869	20.072461
56.806902	1696.827468	20.077479
56.586222	1698.698872	20.082496
56.690087	1687.841903	20.087514
56.741964	1696.979827	20.092531
56.765578	1696.616402	20.097549
56.737109	1685.669708	20.102567
56.916474	1700.531521	20.107584
57.245487	1707.994395	20.112602
57.486133	1706.498688	20.117619
57.186471	1701.366746	20.122637
57.575670	1702.142156	20.127655
57.191189	1711.724014	20.132672
57.607801	1695.923128	20.137690
57.580211	1710.353447	20.142707
57.819950	1702.766859	20.147725
57.893868	1681.714491	20.152743
57.668516	1686.518520	20.157760
57.770690	1674.342629	20.162778
57.910522	1669.548957	20.167795
57.857683	1678.277223	20.172813
57.593426	1677.766387	20.177831
58.036185	1686.814661	20.182848
57.849982	1686.187448	20.187866
57.921491	1696.663583	20.192883
57.826567	1699.600938	20.197901
57.839637	1704.298185	20.202919
57.770996	1705.101144	20.207936
58.156436	1696.942592	20.212954
58.550693	1708.974556	20.217971
58.265245	1699.343128	20.222989
58.265371	1694.243117	20.228007
58.335881	1699.666704	20.233024
58.047284	1699.326947	20.238042
58.467664	1718.730327	20.243059
58.380918	1726.681248	20.248077
58.753671	1717.186541	20.253095
58.180145	1720.640721	20.258112
58.585021	1720.410076	20.263130
58.823281	1724.115787	20.268147
59.050972	1731.865959	20.273165
58.691456	1726.131127	20.278183
58.696134	1735.431109	20.283200
58.959707	1740.224825	20.288218
59.049057	1743.442602	20.293235
58.958711	1751.539273	20.298253
59.235498	1740.162846	20.303271
59.281890	1745.315656	20.308288
59.142938	1746.984902	20.313306
59.168011	1740.072595	20.318323
59.291811	1735.076279	20.323341
59.562189	1732.032640	20.328359
59.234702	1733.608341	20.333376
59.340239	1752.530881	20.338394
59.677132	1768.816665	20.343411
59.612910	1770.609913	20.348429
59.946764	1763.914320	20.353447
59.956895	1770.429891	20.358464
60.148696	1762.989651	20.363482
60.043864	1768.645870	20.368499
59.575135	1762.511547	20.373517
60.020426	1759.241673	20.378535
59.935330	1758.759572	20.383552
60.292816	1761.001172	20.388570
60.195764	1772.040277	20.393587
60.225729	1781.412064	20.398605
60.626203	1787.642409	20.403623
60.534192	1792.229903	20.408640
60.776338	1790.733955	20.413658
61.007882	1777.748729	20.418675
60.931017	1790.507849	20.423693
61.134621	1779.123927	20.428711
61.262371	1782.045345	20.433728
60.921364	1758.728779	20.438746
60.998072	1746.414810	20.443763
60.834809	1752.897576	20.448781
60.927193	1762.442621	20.453799
60.963773	1773.542845	20.458816
61.432260	1782.224199	20.463834
60.928612	1780.958714	20.468851
61.179836	1779.044755	20.473869
60.923856	1777.355437	20.478887
61.083144	1776.819266	20.483904
61.281031	1775.589044	20.488922
61.636524	1777.761528	20.493939
61.057799	1790.741296	20.498957
61.558014	1795.800926	20.503975
61.765860	1806.918522	20.508992
62.014686	1812.367858	20.514010
61.920712	1799.938574	20.519027
61.792251	1809.256297	20.524045
61.835673	1797.698633	20.529063
61.913598	1806.671577	20.534080
61.948671	1797.709444	20.539098
62.430469	1800.073592	20.544115
61.880028	1802.425887	20.549133
61.993564	1801.294090	20.554151
62.009549	1808.922821	20.559168
62.057674	1823.218284	20.564186
62.275914	1819.321214	20.569203
62.539854	1829.587386	20.574221
62.611632	1823.289459	20.579239
62.506932	1820.986265	20.584256
62.599168	1816.723906	20.589274
62.871654	1814.601472	20.594291
62.615956	1821.960331	20.599309
62.841524	1820.075635	20.604327
63.204532	1837.995350	20.609344
63.066946	1851.672954	20.614362
63.125884	1846.052414	20.619379
62.902007	1846.826048	20.624397
63.187854	1839.992774	20.629415
63.302530	1843.206601	20.634432
63.116066	1845.867970	20.639450
63.438838	1839.764258	20.644467
63.326574	1836.348180	20.649485
63.473259	1831.745908	20.654503
63.556540	1832.572409	20.659520
63.257601	1831.959698	20.664538
63.500792	1832.439235	20.669555
63.380967	1842.648768	20.674573
63.956188	1844.944634	20.679591
63.654563	1858.676347	20.684608
64.102356	1862.598583	20.689626
64.410673	1843.311377	20.694643
64.074022	1858.711787	20.699661
64.133412	1849.837342	20.704679
64.430385	1851.955883	20.709696
64.167439	1853.931761	20.714714
64.475421	1850.273104	20.719731
64.320054	1848.435464	20.724749
64.514562	1844.993413	20.729767
64.733469	1847.673328	20.734784
64.564901	1846.809803	20.739802
64.703141	1837.515887	20.744819
64.456546	1844.399930	20.749837
65.314842	1848.131607	20.754855
64.875088	1847.275854	20.759872
65.129974	1848.091250	20.764890
64.692374	1843.356441	20.769907
64.442688	1838.257656	20.774925
65.056153	1844.849151	20.779943
65.000974	1853.126561	20.784960
65.100654	1866.034811	20.789978
65.228667	1866.724910	20.794995
64.900461	1871.642938	20.800013
65.260319	1867.449098	20.805031
65.209205	1868.451301	20.810048
65.274838	1870.385169	20.815066
65.391815	1872.418298	20.820083
65.608029	1882.411094	20.825101
65.968344	1881.366869	20.830119
65.671471	1888.151501	20.835136
65.836495	1894.103172	20.840154
66.022902	1887.206559	20.845171
66.051695	1890.377043	20.850189
66.233218	1885.340082	20.855207
66.220861	1882.555323	20.860224
66.057262	1883.502563	20.865242
66.053211	1880.558703	20.870259
66.078718	1900.346060	20.875277
66.220932	1892.935627	20.880295
66.454186	1896.844143	20.885312
66.338076	1906.030586	20.890330
66.702636	1902.268373	20.895347
66.177705	1905.503521	20.900365
66.411275	1907.710903	20.905383
66.672390	1909.535248	20.910400
66.602268	1912.011131	20.915418
66.775338	1923.241553	20.920435
66.613609	1926.003207	20.925453
67.033713	1932.536660	20.930471
67.042396	1922.717009	20.935488
67.260051	1928.546829	20.940506
67.365950	1922.180402	20.945523
67.631597	1931.398570	20.950541
67.751800	1924.632243	20.955559
67.789132	1922.265755	20.960576
67.577075	1914.560502	20.965594
67.689957	1915.811587	20.970611
67.519331	1925.255905	20.975629
67.636567	1923.782672	20.980647
67.610327	1914.142077	20.985664
67.520244	1919.568800	20.990682
67.528524	1913.545895	20.995699
67.826249	1929.771686	21.000717
67.726174	1942.572423	21.005735
67.932664	1934.833146	21.010752
67.896268	1941.018375	21.015770
68.007845	1942.743068	21.020787
68.291843	1942.828025	21.025805
68.153347	1948.915636	21.030823
68.480618	1954.987085	21.035840
68.391686	1962.812212	21.040858
68.693276	1965.753763	21.045875
68.659589	1965.449807	21.050893
68.701073	1972.730607	21.055911
69.170059	1969.766273	21.060928
68.960621	1972.847854	21.065946
69.052349	1974.095946	21.070963
68.917236	1964.866883	21.075981
68.976653	1963.421642	21.080999
69.212170	1966.442978	21.086016
68.706936	1967.241762	21.091034
68.588437	1963.252242	21.096051
69.086366	1982.110392	21.101069
69.135631	1981.736631	21.106087
69.616401	1978.928250	21.111104
69.544768	1989.124005	21.116122
69.751843	1987.270593	21.121139
69.560130	1982.468818	21.126157
69.322273	1981.695043	21.131175
69.734014	1986.800150	21.136192
69.416116	2004.422741	21.141210
69.981681	2006.407695	21.146227
70.064452	2009.755948	21.151245
70.192426	2012.027228	21.156263
70.398871	2014.854297	21.161280
70.592515	2017.427735	21.166298
70.499884	2000.592290	21.171315
70.589253	2006.988227	21.176333
70.875735	1999.548836	21.181351
71.269910	1995.983950	21.186368
70.749506	1989.712467	21.191386
70.932162	1990.968406	21.196403
71.153958	1997.501393	21.201421
70.878333	2000.454484	21.206439
71.310700	1988.037287	21.211456
71.324140	2000.116487	21.216474
71.530369	1992.481375	21.221491
71.097918	1970.365523	21.226509
70.983410	1965.015134	21.231527
71.132545	1976.681713	21.236544
71.109996	1990.432924	21.241562
71.275700	1990.331273	21.246579
71.316860	1985.224751	21.251597
71.258310	1988.487837	21.256615
71.471672	1984.749296	21.261632
70.901208	1990.551125	21.266650
71.429736	2001.438707	21.271667
71.304342	2008.243859	21.276685
71.064949	2014.596626	21.281703
72.230152	2027.095040	21.286720
72.122149	2037.369108	21.291738
72.342281	2040.181414	21.296755
72.422393	2038.594059	21.301773
72.423400	2044.767151	21.306791
72.627127	2038.716739	21.311808
72.418915	2027.797997	21.316826
72.346896	2017.179838	21.321843
72.539111	2019.409493	21.326861
72.754912	2036.866443	21.331879
72.878531	2038.876458	21.336896
72.533979	2044.617661	21.341914
72.815865	2038.255181	21.346931
72.927859	2037.442371	21.351949
72.652875	2036.330402	21.356967
73.107714	2033.257813	21.361984
72.644707	2035.703743	21.367002
72.831190	2033.156070	21.372019
72.950858	2036.441739	21.377037
72.653265	2042.080904	21.382055
73.431726	2046.131268	21.387072
73.283400	2052.422440	21.392090
73.331998	2052.743109	21.397107
73.403865	2054.824354	21.402125
73.220271	2056.428034	21.407143
73.826615	2057.870080	21.412160
73.580152	2077.289958	21.417178
73.449095	2078.749699	21.422195
73.647332	2083.253921	21.427213
74.007168	2088.326161	21.432231
73.905196	2083.118951	21.437248
73.976518	2079.664595	21.442266
74.202339	2087.131172	21.447283
74.459368	2099.500504	21.452301
74.610617	2104.592804	21.457319
74.844095	2105.509404	21.462336
74.621006	2102.113795	21.467354
74.557823	2096.689049	21.472371
74.701442	2094.602553	21.477389
74.787212	2091.316358	21.482407
74.851484	2101.749679	21.487424
74.755980	2098.990538	21.492442
74.665209	2098.092719	21.497459
75.034166	2095.614287	21.502477
74.839779	2097.001894	21.507495
75.068482	2106.614134	21.512512
75.248705	2115.520709	21.517530
75.198089	2117.018347	21.522547
75.600464	2120.152434	21.527565
75.233462	2120.989531	21.532583
75.732203	2111.762079	21.537600
75.606130	2114.148918	21.542618
75.505200	2114.975889	21.547635
75.766573	2128.064138	21.552653
75.820896	2135.740655	21.557671
76.374735	2137.279303	21.562688
76.047925	2144.068722	21.567706
76.295396	2138.585823	21.572723
76.529868	2138.801627	21.577741
76.321030	2140.879520	21.582759
76.559844	2134.760458	21.587776
76.547771	2133.114949	21.592794
76.202013	2135.271102	21.597811
76.516258	2133.015847	21.602829
76.781481	2131.566753	21.607847
76.711588	2124.173677	21.612864
76.447628	2130.495617	21.617882
76.739443	2138.693546	21.622899
77.042265	2149.881689	21.627917
77.053673	2162.822919	21.632935
77.123694	2158.339880	21.637952
77.035401	2159.108065	21.642970
77.316809	2154.569816	21.647987
77.639368	2141.033539	21.653005
77.777908	2154.024277	21.658023
77.680771	2150.896126	21.663040
77.519744	2151.382193	21.668058
77.505295	2145.085039	21.673075
77.291896	2147.094215	21.678093
77.634405	2162.470537	21.683111
77.661059	2137.012880	21.688128
77.675263	2157.610240	21.693146
77.941669	2169.826661	21.698163
78.306744	2171.918791	21.703181
78.082673	2183.088511	21.708199
78.167028	2174.086908	21.713216
78.374926	2173.170697	21.718234
78.322707	2171.247429	21.723251
78.091800	2171.084830	21.728269
78.243682	2176.413756	21.733287
78.264213	2181.365600	21.738304
78.531841	2181.737168	21.743322
78.607697	2185.673564	21.748339
78.690875	2188.216993	21.753357
78.277502	2195.016837	21.758375
78.760874	2201.370051	21.763392
79.010989	2220.526076	21.768410
79.112605	2215.258525	21.773427
79.449855	2199.059344	21.778445
79.121495	2212.571436	21.783463
79.625863	2200.442637	21.788480
79.330188	2207.997280	21.793498
79.381116	2211.353716	21.798515
79.882219	2214.734305	21.803533
79.444522	2226.366745	21.808551
79.656840	2233.283187	21.813568
79.830192	2230.724920	21.818586
79.954210	2234.293989	21.823603
79.952515	2220.653807	21.828621
79.880212	2227.908353	21.833639
79.938370	2237.108691	21.838656
80.244667	2251.831145	21.843674
80.479243	2241.802344	21.848691
80.598005	2239.643981	21.853709
80.642515	2243.443277	21.858727
80.671086	2237.445489	21.863744
80.464176	2242.710717	21.868762
80.658775	2244.034236	21.873779
81.145259	2240.754667	21.878797
80.468275	2245.610665	21.883815
80.898979	2258.360030	21.888832
81.440809	2262.147692	21.893850
81.336972	2271.774248	21.898867
81.541311	2267.083930	21.903885
80.968672	2267.984811	21.908903
81.406229	2267.458684	21.913920
81.244246	2266.859216	21.918938
81.730732	2267.423734	21.923955
81.967335	2264.672501	21.928973
81.556722	2272.778554	21.933991
81.712757	2276.860212	21.939008
81.624428	2293.298309	21.944026
81.951451	2285.379038	21.949043
81.858554	2286.804412	21.954061
81.529181	2290.365625	21.959079
82.149033	2284.294120	21.964096
82.217728	2315.806295	21.969114
82.386665	2311.607548	21.974131
83.035728	2308.883213	21.979149
82.962844	2311.956082	21.984167
82.944008	2311.652949	21.989184
83.135183	2316.196210	21.994202
83.051815	2316.086240	21.999219
83.142861	2297.126103	22.004237
82.813040	2300.725261	22.009255
83.135859	2296.303575	22.014272
82.980871	2309.921132	22.019290
83.439120	2304.136894	22.024307
83.423749	2304.596989	22.029325
82.917387	2302.233574	22.034343
83.068032	2300.641458	22.039360
83.516354	2300.605991	22.044378
83.288595	2305.461058	22.049395
83.868117	2311.669848	22.054413
83.681434	2329.477345	22.059431
84.194625	2323.236330	22.064448
84.036892	2325.031658	22.069466
83.716855	2328.506201	22.074483
84.214851	2325.085946	22.079501
83.809571	2335.125869	22.084519
84.016172	2329.762935	22.089536
84.338053	2324.230449	22.094554
84.071810	2341.507577	22.099571
84.464484	2343.137772	22.104589
84.720583	2346.708263	22.109607
84.817092	2347.598995	22.114624
84.869195	2353.524326	22.119642
84.734215	2344.648527	22.124659
85.021827	2344.395221	22.129677
84.955633	2346.693807	22.134695
84.851062	2346.886987	22.139712
85.213956	2350.374470	22.144730
85.441995	2360.697070	22.149747
85.823524	2367.523932	22.154765
85.703995	2374.334615	22.159783
85.907264	2375.641006	22.164800
86.336529	2363.937312	22.169818
85.922190	2369.430753	22.174835
85.899785	2367.502793	22.179853
86.179858	2368.866584	22.184871
85.451092	2359.279005	22.189888
85.725287	2357.437133	22.194906
86.096609	2366.938799	22.199923
86.084626	2360.836860	22.204941
86.153689	2377.723789	22.209959
85.944746	2383.838364	22.214976
86.825425	2388.945865	22.219994
86.291266	2392.788513	22.225011
86.475899	2389.265849	22.230029
86.441827	2387.374431	22.235047
86.781893	2399.765679	22.240064
86.960515	2401.211645	22.245082
86.475441	2413.100958	22.250099
86.940850	2404.983212	22.255117
86.848571	2410.508266	22.260135
87.175343	2427.689412	22.265152
87.482881	2434.180721	22.270170
87.185572	2436.215699	22.275187
87.614950	2429.634295	22.280205
87.736530	2431.679391	22.285223
87.447612	2425.908023	22.290240
88.022444	2424.426180	22.295258
87.821710	2430.574202	22.300275
88.459454	2432.358532	22.305293
87.870166	2435.313494	22.310311
87.867401	2440.054444	22.315328
88.233931	2452.738255	22.320346
87.932321	2448.625822	22.325363
88.318275	2438.276521	22.330381
88.783498	2451.484563	22.335399
88.606816	2444.363729	22.340416
88.723216	2449.076544	22.345434
88.452224	2454.683264	22.350451
88.903001	2471.349516	22.355469
88.874719	2473.907292	22.360487
89.179078	2470.094429	22.365504
89.444476	2463.841690	22.370522
89.080335	2470.233098	22.375539
89.465342	2472.896553	22.380557
89.173646	2463.057388	22.385575
89.549648	2471.977654	22.390592
89.797424	2466.775502	22.395610
90.040367	2461.621450	22.400627
89.870946	2457.715543	22.405645
89.677272	2458.288792	22.410663
89.646588	2456.674573	22.415680
90.418902	2448.366701	22.420698
90.156115	2455.509157	22.425715
90.133575	2458.766686	22.430733
89.949261	2474.816006	22.435751
90.029594	2478.997941	22.440768
90.473462	2479.569145	22.445786
90.109322	2484.029021	22.450803
90.279365	2474.641422	22.455821
90.677684	2493.645120	22.460839
90.794156	2502.277826	22.465856
90.990092	2498.810179	22.470874
91.005237	2506.843321	22.475891
90.744812	2492.164078	22.480909
91.035154	2499.077867	22.485927
90.993792	2511.980275	22.490944
91.276839	2524.080711	22.495962
91.288574	2522.478778	22.500979
91.420836	2522.612761	22.505997
91.395072	2526.546216	22.511015
91.429700	2532.161889	22.516032
91.864148	2527.640599	22.521050
91.822575	2547.805289	22.526067
92.263311	2542.680192	22.531085
91.913785	2550.391752	22.536103
92.032375	2543.675944	22.541120
92.295139	2542.271389	22.546138
92.062871	2548.430704	22.551155
92.120703	2562.138197	22.556173
92.714441	2565.829422	22.561191
92.863864	2571.613333	22.566208
92.857723	2568.145771	22.571226
93.194861	2572.094971	22.576243
92.958605	2563.143404	22.581261
93.348041	2565.727276	22.586279
92.938271	2565.046686	22.591296
93.043188	2560.671700	22.596314
93.321423	2560.388299	22.601331
93.422336	2561.029017	22.606349
93.427924	2564.452589	22.611367
93.824996	2581.903764	22.616384
93.803179	2579.224532	22.621402
93.626938	2583.181575	22.626419
93.625419	2583.721565	22.631437
93.863195	2580.149508	22.636455
93.666822	2588.250542	22.641472
94.285352	2594.090367	22.646490
94.173339	2606.805075	22.651507
94.468499	2607.298586	22.656525
94.731699	2606.099106	22.661543
94.579461	2617.832256	22.666560
94.541781	2602.423676	22.671578
94.381341	2608.546509	22.676595
94.794969	2604.643908	22.681613
94.688634	2599.588725	22.686631
94.693816	2603.397415	22.691648
95.209922	2615.537147	22.696666
94.955959	2638.575731	22.701683
95.380167	2630.186600	22.706701
95.641640	2630.947348	22.711719
95.305660	2629.936425	22.716736
95.711343	2621.196713	22.721754
95.553852	2625.479065	22.726771
95.705457	2620.490773	22.731789
95.881466	2623.546794	22.736807
95.340057	2621.747461	22.741824
96.188810	2629.880454	22.746842
96.214796	2640.597826	22.751859
96.517505	2640.108597	22.756877
96.923537	2636.873124	22.761895
96.343984	2636.761986	22.766912
96.558112	2640.525324	22.771930
96.374047	2634.264040	22.776947
96.548526	2636.105192	22.781965
96.683051	2631.081699	22.786983
96.180013	2638.669008	22.792000
96.598981	2643.542776	22.797018
96.522420	2655.882697	22.802035
96.835627	2660.043971	22.807053
96.965888	2672.525088	22.812071
97.172434	2684.186290	22.817088
97.465877	2680.857983	22.822106
97.018187	2688.458735	22.827123
97.292485	2693.067973	22.832141
97.618716	2697.688012	22.837159
97.574242	2709.757827	22.842176
97.964868	2714.898014	22.847194
97.797871	2720.450650	22.852211
98.028936	2713.852871	22.857229
98.297737	2719.627596	22.862247
98.235068	2734.531343	22.867264
98.388775	2728.122424	22.872282
98.306668	2731.247308	22.877299
98.445074	2740.905597	22.882317
99.260115	2737.836426	22.887335
98.604024	2729.846898	22.892352
99.029460	2730.130633	22.897370
99.035284	2744.625984	22.902387
99.209729	2750.601714	22.907405
99.411690	2751.346542	22.912423
99.524970	2747.137477	22.917440
99.884125	2754.097396	22.922458
99.471645	2752.823864	22.927475
99.812674	2760.556727	22.932493
99.875383	2748.484132	22.937511
99.863059	2749.473995	22.942528
99.863599	2745.254188	22.947546
100.305342	2750.335879	22.952563
100.170750	2751.133435	22.957581
100.212325	2751.193256	22.962599
100.147030	2764.721357	22.967616
100.552061	2766.068758	22.972634
100.523303	2766.155379	22.977651
100.439534	2772.389346	22.982669
100.833171	2778.144531	22.987687
100.704972	2771.713483	22.992704
100.805208	2765.808444	22.997722
101.048496	2786.922962	23.002739
101.073161	2792.376156	23.007757
101.731157	2787.942870	23.012775
101.317705	2796.298938	23.017792
101.760656	2792.985062	23.022810
101.663436	2794.701520	23.027827
101.513979	2798.723849	23.032845
101.841196	2792.407657	23.037863
101.709323	2792.469403	23.042880
101.843306	2791.526868	23.047898
101.626876	2792.703362	23.052915
101.475836	2797.114147	23.057933
101.860705	2800.317378	23.062951
101.869473	2815.550866	23.067968
102.277855	2819.820357	23.072986
102.381490	2819.087726	23.078003
102.843672	2828.187194	23.083021
102.576205	2830.763557	23.088039
102.487642	2832.049423	23.093056
102.915720	2825.572234	23.098074
102.780619	2829.093646	23.103091
102.999552	2834.162927	23.108109
102.760905	2835.740581	23.113127
103.131150	2845.539351	23.118144
103.211413	2847.095449	23.123162
103.579898	2838.187871	23.128179
103.464688	2853.866898	23.133197
103.517439	2861.285165	23.138215
103.544234	2872.097234	23.143232
103.892805	2870.745491	23.148250
104.103943	2870.245354	23.153267
104.026281	2876.017598	23.158285
104.227909	2882.995934	23.163303
104.383002	2891.136725	23.168320
104.646560	2890.745153	23.173338
104.665913	2885.234644	23.178355
104.517046	2887.858714	23.183373
104.785659	2888.684635	23.188391
104.682535	2891.304694	23.193408
105.156704	2900.165608	23.198426
105.323904	2912.095085	23.203443
105.266422	2910.421901	23.208461
105.712615	2903.421076	23.213479
105.544164	2909.516860	23.218496
105.194652	2919.289562	23.223514
105.695191	2912.819926	23.228531
105.395374	2916.180946	23.233549
105.876836	2916.017198	23.238567
105.754814	2933.774131	23.243584
106.048735	2931.225283	23.248602
106.334909	2928.781802	23.253619
106.300240	2932.139159	23.258637
106.499832	2932.934865	23.263655
106.633828	2935.394690	23.268672
106.645898	2926.284102	23.273690
106.600198	2937.382156	23.278707
106.474210	2954.735739	23.283725
106.890721	2946.827408	23.288743
106.734715	2948.764556	23.293760
106.926423	2946.733552	23.298778
107.184963	2948.476350	23.303795
107.477018	2969.542412	23.308813
107.608742	2971.204081	23.313831
107.654253	2969.379039	23.318848
107.649445	2966.236280	23.323866
108.020203	2971.824678	23.328883
108.081437	2970.830408	23.333901
108.459227	2963.423659	23.338919
108.264092	2972.225345	23.343936
108.402528	2967.516766	23.348954
108.295546	2962.032339	23.353971
108.220589	2973.718894	23.358989
108.459163	2975.212327	23.364007
109.156698	2983.021993	23.369024
108.911682	2988.558528	23.374042
109.021204	2986.104841	23.379059
108.976286	2992.219174	23.384077
109.357816	2989.520875	23.389095
109.194176	2989.622316	23.394112
109.465211	2991.173788	23.399130
109.621218	2981.251572	23.404147
109.357147	2978.941634	23.409165
109.691896	2990.077958	23.414183
109.558840	2986.721729	23.419200
109.540083	2975.567574	23.424218
109.683118	2986.885429	23.429235
109.708831	2997.940770	23.434253
109.746902	3005.225680	23.439271
109.772179	3004.969279	23.444288
109.839277	3025.164821	23.449306
110.017166	3027.478910	23.454323
110.129281	3033.521311	23.459341
110.065126	3036.854901	23.464359
110.660992	3045.381200	23.469376
110.556263	3058.044586	23.474394
110.719412	3047.303757	23.479411
110.816384	3072.304730	23.484429
110.984089	3074.683545	23.489447
110.961761	3072.809153	23.494464
111.297672	3076.496692	23.499482
111.376505	3085.836254	23.504499
111.511507	3105.954967	23.509517
111.855822	3097.540263	23.514535
111.995293	3102.094981	23.519552
111.916404	3103.903283	23.524570
112.058439	3093.285670	23.529587
112.417017	3116.838049	23.534605
112.771083	3121.201340	23.539623
112.894367	3119.443004	23.544640
112.839591	3125.606269	23.549658
112.960595	3118.148158	23.554675
113.052540	3127.769747	23.559693
113.180047	3116.283280	23.564711
113.212592	3121.583841	23.569728
113.208239	3115.180611	23.574746
113.120209	3115.175520	23.579763
113.205982	3114.268928	23.584781
113.579197	3110.476707	23.589799
113.873265	3132.025545	23.594816
113.634261	3143.908348	23.599834
113.797379	3139.861819	23.604851
113.840239	3136.074005	23.609869
113.762096	3142.373499	23.614887
114.000401	3134.373070	23.619904
114.261626	3152.354236	23.624922
114.708103	3153.591020	23.629939
114.512078	3161.594412	23.634957
114.308740	3158.359630	23.639975
114.417714	3155.726102	23.644992
114.366383	3165.259690	23.650010
114.831647	3172.102149	23.655027
114.673002	3185.288536	23.660045
115.366199	3176.168954	23.665063
115.239534	3175.412421	23.670080
115.585619	3192.755399	23.675098
115.723226	3199.122110	23.680115
115.987394	3202.243325	23.685133
115.978011	3194.998139	23.690151
116.208153	3193.709115	23.695168
116.181381	3202.004788	23.700186
116.267018	3196.029303	23.705203
116.106138	3196.796278	23.710221
116.114101	3189.273784	23.715239
115.759849	3190.746488	23.720256
116.272655	3207.678300	23.725274
116.338315	3212.585483	23.730291
116.453233	3223.929985	23.735309
116.350300	3221.452740	23.740327
116.743738	3240.710493	23.745344
116.794621	3240.759390	23.750362
117.031636	3238.765443	23.755379
117.169767	3254.559784	23.760397
117.420243	3260.915147	23.765415
117.252924	3263.015068	23.770432
117.460783	3273.379231	23.775450
117.500353	3268.477750	23.780467
117.637944	3278.726674	23.785485
117.993719	3288.240735	23.790503
118.128320	3285.445360	23.795520
118.045500	3292.118076	23.800538
118.375648	3285.555066	23.805555
118.966303	3298.141239	23.810573
118.771144	3311.459689	23.815591
118.922296	3314.466067	23.820608
118.842475	3314.497565	23.825626
119.187358	3307.326239	23.830643
119.052899	3312.747708	23.835661
119.281609	3307.917584	23.840679
119.614148	3314.960798	23.845696
119.625832	3326.927539	23.850714
120.083893	3329.819556	23.855731
119.981179	3340.364976	23.860749
119.967843	3326.062966	23.865767
120.156363	3330.647932	23.870784
120.181411	3323.583520	23.875802
120.176344	3320.317646	23.880819
120.069557	3323.190842	23.885837
120.229016	3329.465801	23.890855
120.681181	3342.654453	23.895872
120.587228	3347.009083	23.900890
120.748858	3347.018535	23.905907
120.816642	3351.742360	23.910925
121.301852	3354.421814	23.915943
121.290227	3365.981920	23.920960
121.095496	3373.521233	23.925978
121.440709	3368.047901	23.930995
121.146389	3375.328222	23.936013
121.479501	3378.665918	23.941031
121.822269	3380.007342	23.946048
121.826797	3404.578226	23.951066
121.789141	3395.307908	23.956083
121.938073	3404.898624	23.961101
122.099171	3413.455338	23.966119
122.575569	3422.650727	23.971136
122.475249	3430.544557	23.976154
122.856461	3419.983969	23.981171
122.727377	3421.920105	23.986189
122.627263	3417.002593	23.991207
122.972269	3436.104017	23.996224
122.950023	3441.116566	24.001242
123.021223	3442.857200	24.006259
123.464548	3439.966091	24.011277
123.665286	3445.559180	24.016295
123.946282	3460.150872	24.021312
123.721494	3472.650293	24.026330
123.798371	3470.091186	24.031347
123.981871	3467.196591	24.036365
123.952217	3466.503754	24.041383
124.091137	3464.910218	24.046400
124.145283	3466.132740	24.051418
124.457631	3474.454316	24.056435
124.450169	3486.667197	24.061453
124.482968	3489.752116	24.066471
124.969122	3483.508629	24.071488
124.893653	3489.580572	24.076506
125.087631	3489.458706	24.081523
124.823174	3495.787511	24.086541
125.147669	3504.615361	24.091559
125.640340	3504.579263	24.096576
125.495126	3504.352722	24.101594
125.352273	3500.903243	24.106611
126.063907	3517.406506	24.111629
126.207880	3523.238922	24.116647
126.365374	3522.340011	24.121664
126.151670	3521.641287	24.126682
126.426288	3513.726535	24.131699
126.496937	3518.282672	24.136717
126.565557	3514.285584	24.141735
126.801245	3520.315102	24.146752
127.012292	3524.962871	24.151770
127.006409	3534.016091	24.156787
127.079399	3540.304670	24.161805
126.997741	3538.445837	24.166823
127.355509	3535.031548	24.171840
127.303965	3543.700545	24.176858
127.582900	3554.088453	24.181875
127.647653	3559.750228	24.186893
127.969556	3563.938758	24.191911
128.141580	3555.784400	24.196928
128.119498	3564.956956	24.201946
128.419453	3564.518638	24.206963
128.691025	3578.733146	24.211981
128.752969	3577.186379	24.216999
129.093767	3576.296624	24.222016
128.971090	3580.157115	24.227034
128.981890	3574.657205	24.232051
129.254456	3571.922236	24.237069
128.858960	3575.670809	24.242087
129.361487	3578.173988	24.247104
129.084382	3595.678113	24.252122
129.337682	3595.562734	24.257139
129.654386	3590.273711	24.262157
129.269814	3610.651141	24.267175
129.807114	3618.003276	24.272192
129.418203	3623.328980	24.277210
129.756820	3622.313312	24.282227
130.196487	3640.450075	24.287245
129.948352	3648.108339	24.292263
130.493954	3653.609589	24.297280
130.540592	3668.140320	24.302298
130.658341	3665.076084	24.307315
131.139248	3667.219687	24.312333
130.737904	3666.411477	24.317351
130.890003	3684.217734	24.322368
131.206616	3696.004383	24.327386
131.130788	3687.825670	24.332403
131.482002	3690.481980	24.337421
131.536328	3716.358514	24.342439
131.991892	3713.610636	24.347456
131.796980	3728.760021	24.352474
132.417702	3716.570951	24.357491
132.769090	3709.262726	24.362509
132.615774	3724.374028	24.367527
132.549938	3724.002482	24.372544
132.568904	3738.297723	24.377562
132.757103	3737.349803	24.382579
133.074797	3726.458106	24.387597
132.978403	3727.559039	24.392615
133.156085	3725.413364	24.397632
133.559707	3740.835123	24.402650
133.451814	3743.127794	24.407667
133.685754	3748.608461	24.412685
133.903387	3751.004795	24.417703
134.177834	3756.491744	24.422720
133.848468	3752.806305	24.427738
134.332761	3745.414117	24.432755
134.440736	3738.387052	24.437773
133.936697	3756.971630	24.442791
134.449695	3763.144008	24.447808
134.349853	3771.994280	24.452826
134.686275	3770.682253	24.457843
134.778597	3770.377462	24.462861
135.163583	3790.584028	24.467879
135.163999	3796.659967	24.472896
134.964361	3804.152883	24.477914
135.015311	3789.966687	24.482931
135.665624	3801.773722	24.487949
135.849496	3824.666315	24.492967
136.054493	3817.065347	24.497984
136.104850	3825.443914	24.503002
136.181068	3818.440731	24.508019
135.953492	3818.315466	24.513037
136.394842	3825.420743	24.518055
136.664437	3829.289270	24.523072
136.741512	3839.172390	24.528090
136.968350	3836.419295	24.533107
136.913755	3840.070325	24.538125
137.402723	3858.190115	24.543143
137.421634	3855.706318	24.548160
137.581914	3864.004554	24.553178
137.871023	3858.135853	24.558195
137.939084	3860.394660	24.563213
137.659555	3864.765862	24.568231
137.611069	3856.623821	24.573248
137.531589	3878.405674	24.578266
137.670407	3882.809187	24.583283
138.023190	3888.122930	24.588301
138.158127	3900.073898	24.593319
138.479455	3902.883271	24.598336
138.660586	3912.450274	24.603354
139.137350	3924.202514	24.608371
139.061137	3933.462645	24.613389
139.233272	3930.664448	24.618407
139.584379	3925.868644	24.623424
139.783495	3930.464729	24.628442
139.611705	3924.365203	24.633459
139.831015	3921.711122	24.638477
139.810910	3953.435766	24.643495
139.931729	3948.732848	24.648512
140.448097	3953.115106	24.653530
139.981645	3952.503307	24.658547
140.772134	3954.213368	24.663565
140.725978	3958.087203	24.668583
141.053764	3970.434114	24.673600
140.856998	3968.536455	24.678618
141.052686	3969.945157	24.683635
141.526239	3962.904921	24.688653
141.370795	3968.364593	24.693671
141.580005	3962.183270	24.698688
141.450299	3967.900888	24.703706
141.769163	3988.903971	24.708723
141.858544	3981.021192	24.713741
142.023382	3984.271735	24.718759
141.987232	3981.812329	24.723776
142.283596	3987.103377	24.728794
142.056177	4001.614183	24.733811
142.505727	3999.615266	24.738829
142.504905	4012.228320	24.743847
142.909475	4008.263715	24.748864
142.522222	4015.779797	24.753882
143.001460	4025.596857	24.758899
143.242480	4031.051251	24.763917
143.265937	4035.299273	24.768935
143.394015	4026.984301	24.773952
143.555113	4045.414468	24.778970
143.206095	4056.627012	24.783987
143.790311	4056.595513	24.789005
143.681819	4067.129636	24.794023
144.338577	4084.705719	24.799040
144.213103	4075.328868	24.804058
144.132079	4083.731293	24.809075
145.156350	4093.159990	24.814093
145.151601	4106.786926	24.819111
144.948087	4105.335361	24.824128
145.252956	4104.312330	24.829146
145.362711	4110.841547	24.834163
145.734476	4101.737142	24.839181
145.456648	4114.226376	24.844199
145.350325	4108.662587	24.849216
146.209956	4119.859419	24.854234
146.463844	4116.688557	24.859251
146.337524	4109.215126	24.864269
146.074642	4120.673039	24.869287
146.326864	4117.199424	24.874304
146.693542	4132.810378	24.879322
146.451945	4144.239720	24.884339
146.754014	4146.256736	24.889357
147.052094	4143.426150	24.894375
146.882740	4167.504505	24.899392
147.068873	4165.799351	24.904410
147.385265	4172.097364	24.909427
147.675292	4176.609829	24.914445
147.676592	4191.605761	24.919463
147.957996	4184.289372	24.924480
147.752426	4189.510764	24.929498
147.823395	4186.172849	24.934515
148.352547	4196.029529	24.939533
148.519008	4208.872182	24.944551
148.642141	4218.366367	24.949568
149.008039	4204.758632	24.954586
149.170350	4213.504921	24.959603
149.221664	4228.527769	24.964621
149.467137	4234.069906	24.969639
149.379251	4233.316722	24.974656
149.478892	4228.866407	24.979674
149.587130	4227.744760	24.984691
150.142766	4234.882798	24.989709
150.310914	4246.494212	24.994727
150.103155	4248.603738	24.999744
150.453970	4244.003594	25.004762
150.491342	4239.449401	25.009779
150.627690	4244.109059	25.014797
150.687918	4256.056185	25.019815
150.794738	4258.413131	25.024832
151.398858	4256.674049	25.029850
150.991831	4265.007687	25.034867
151.229970	4276.245168	25.039885
151.090198	4287.545016	25.044903
151.308062	4293.366106	25.049920
151.885591	4303.764484	25.054938
151.420207	4320.844279	25.059955
152.042153	4316.166920	25.064973
151.964386	4327.242442	25.069991
152.144577	4327.384716	25.075008
152.851589	4333.451142	25.080026
152.559877	4341.192279	25.085043
152.935559	4340.742081	25.090061
152.925808	4338.076479	25.095079
153.143774	4349.257193	25.100096
153.222198	4357.524290	25.105114
153.583180	4366.381568	25.110131
153.828646	4378.362883	25.115149
153.581247	4373.799609	25.120167
153.573228	4370.448784	25.125184
153.739930	4381.751181	25.130202
153.945048	4391.049539	25.135219
154.171267	4396.844102	25.140237
154.459158	4410.993581	25.145255
154.597201	4416.757773	25.150272
154.827134	4421.967820	25.155290
154.463635	4422.548793	25.160307
154.847818	4426.699361	25.165325
155.130022	4436.616955	25.170343
155.345757	4437.940486	25.175360
155.984420	4432.139940	25.180378
156.184263	4444.510377	25.185395
156.673000	4442.880891	25.190413
156.889102	4452.666810	25.195431
156.871177	4442.831017	25.200448
157.227330	4435.060914	25.205466
157.438251	4416.512207	25.210483
157.146876	4407.530478	25.215501
157.033688	4415.897062	25.220519
157.378897	4427.878566	25.225536
157.473312	4433.886333	25.230554
157.144859	4435.774898	25.235571
157.367020	4437.078483	25.240589
157.378919	4427.244339	25.245607
157.505124	4447.709977	25.250624
157.632851	4453.800913	25.255642
157.492477	4464.797946	25.260659
158.202765	4482.953134	25.265677
158.236229	4503.963650	25.270695
158.263577	4500.219015	25.275712
158.913617	4513.589010	25.280730
158.430677	4526.407367	25.285747
158.672080	4519.589519	25.290765
158.472181	4531.403973	25.295783
158.730533	4542.000846	25.300800
159.314658	4558.067354	25.305818
159.548394	4569.151039	25.310835
159.824098	4557.447898	25.315853
160.052923	4585.624655	25.320871
159.901481	4590.320019	25.325888
160.619497	4583.844135	25.330906
160.760802	4585.018357	25.335923
161.001396	4596.501857	25.340941
161.063352	4604.572788	25.345959
161.319389	4602.916615	25.350976
161.651374	4598.174136	25.355994
161.759571	4604.631176	25.361011
161.908944	4599.506963	25.366029
161.730176	4592.357196	25.371047
161.764164	4593.933322	25.376064
162.189021	4605.280640	25.381082
162.216525	4615.976851	25.386099
162.086927	4623.803187	25.391117
162.104801	4621.688756	25.396135
162.319806	4636.888312	25.401152
162.694185	4640.794261	25.406170
162.411676	4650.197554	25.411187
163.166738	4652.819149	25.416205
163.341295	4659.972867	25.421223
163.066173	4664.220466	25.426240
163.782674	4669.565842	25.431258
163.440315	4668.669429	25.436275
163.342107	4680.849983	25.441293
163.630040	4681.688748	25.446311
163.737943	4696.646301	25.451328
164.014169	4712.347682	25.456346
164.359208	4726.191744	25.461363
164.401732	4723.098081	25.466381
164.629880	4739.384657	25.471399
164.674363	4742.209126	25.476416
165.372174	4738.548796	25.481434
165.229216	4762.188207	25.486451
165.467436	4772.229667	25.491469
165.770126	4769.859113	25.496487
165.656525	4773.055568	25.501504
166.003413	4773.585233	25.506522
165.812393	4784.303152	25.511539
166.152310	4790.225228	25.516557
166.150573	4795.689476	25.521575
166.319863	4814.665218	25.526592
166.802281	4813.327091	25.531610
166.783505	4823.790780	25.536627
166.831761	4832.539453	25.541645
167.114755	4832.362601	25.546663
167.752402	4841.287247	25.551680
168.261268	4857.189047	25.556698
168.494748	4861.325447	25.561715
168.380532	4850.781674	25.566733
168.601209	4846.526890	25.571751
168.609459	4848.908826	25.576768
169.197850	4846.881756	25.581786
168.848912	4845.869573	25.586803
169.164578	4831.880988	25.591821
169.364390	4844.984015	25.596839
169.264139	4862.742583	25.601856
169.854537	4877.018644	25.606874
169.597888	4864.827375	25.611891
169.883632	4865.145665	25.616909
170.376342	4862.483339	25.621927
169.985919	4877.724284	25.626944
170.404248	4875.010479	25.631962
170.365887	4888.936825	25.636979
170.413412	4884.396662	25.641997
170.737107	4899.257446	25.647015
170.841220	4904.913475	25.652032
170.884016	4916.459730	25.657050
170.828368	4923.053031	25.662067
171.197035	4929.863949	25.667085
171.446658	4929.944846	25.672103
171.134026	4945.685019	25.677120
171.385131	4956.699934	25.682138
171.370418	4982.342880	25.687156
171.912030	4981.951901	25.692173
172.715843	4992.772927	25.697191
172.650585	5007.038171	25.702208
172.924091	5004.899431	25.707226
172.845833	5010.312600	25.712244
172.576242	5010.099210	25.717261
173.236604	5023.878317	25.722279
173.429002	5032.146806	25.727296
173.649525	5040.398266	25.732314
173.770624	5047.794096	25.737332
174.089516	5054.739121	25.742349
174.315023	5043.832671	25.747367
174.342879	5066.871224	25.752384
174.770225	5068.164808	25.757402
175.021960	5090.331829	25.762420
174.890166	5083.717439	25.767437
174.870941	5074.550698	25.772455
174.802975	5077.553820	25.777472
175.450833	5085.779389	25.782490
175.547347	5096.588177	25.787508
175.386845	5090.941033	25.792525
175.869315	5097.027116	25.797543
175.694919	5115.533025	25.802560
176.331138	5127.156902	25.807578
176.289099	5122.138287	25.812596
176.818952	5145.290846	25.817613
176.959996	5142.307942	25.822631
176.146982	5146.134867	25.827648
177.021563	5161.925979	25.832666
177.164371	5178.721901	25.837684
177.389857	5185.609007	25.842701
177.689384	5184.684610	25.847719
177.593157	5199.731374	25.852736
177.976044	5197.158808	25.857754
178.203275	5207.615743	25.862772
178.743732	5227.105110	25.867789
178.604603	5233.872587	25.872807
178.542935	5234.753522	25.877824
178.798024	5240.386003	25.882842
178.668237	5248.783979	25.887860
178.939408	5259.028882	25.892877
179.503303	5269.281594	25.897895
179.341631	5278.154911	25.902912
179.605403	5279.253174	25.907930
179.795595	5289.166711	25.912948
180.051082	5297.428594	25.917965
180.363645	5298.449770	25.922983
180.293093	5317.312093	25.928000
180.768632	5321.249692	25.933018
180.914700	5319.342373	25.938036
180.663577	5328.996782	25.943053
181.506449	5339.180576	25.948071
181.632130	5352.175632	25.953088
181.659605	5350.321611	25.958106
181.708753	5366.062288	25.963124
181.827985	5375.062102	25.968141
182.312029	5374.184547	25.973159
182.042023	5386.108392	25.978176
182.697626	5401.773032	25.983194
182.607978	5397.670904	25.988212
182.765961	5405.080041	25.993229
183.199334	5414.671455	25.998247
183.306065	5421.520436	26.003264
183.605328	5413.443170	26.008282
183.890802	5428.455579	26.013300
183.841229	5442.564032	26.018317
184.287111	5438.475854	26.023335
184.357728	5437.795643	26.028352
184.557177	5443.316953	26.033370
184.794345	5449.097511	26.038388
184.951492	5453.264946	26.043405
185.282341	5444.459851	26.048423
185.194080	5455.329366	26.053440
185.340572	5466.051628	26.058458
185.379167	5476.812897	26.063476
185.473509	5481.498394	26.068493
186.144948	5483.265144	26.073511
186.748026	5497.091467	26.078528
186.551220	5503.091548	26.083546
186.887379	5498.853244	26.088564
186.465924	5505.529316	26.093581
186.990727	5504.200286	26.098599
187.125557	5498.049036	26.103616
186.726101	5502.849777	26.108634
187.181034	5508.043829	26.113652
187.323041	5531.589088	26.118669
187.854722	5522.708300	26.123687
188.168372	5539.117933	26.128704
187.976455	5543.033879	26.133722
188.023077	5548.219305	26.138740
188.056278	5546.247571	26.143757
188.744314	5566.585417	26.148775
188.571647	5574.125338	26.153792
188.783186	5574.294280	26.158810
189.212909	5583.517027	26.163828
188.723420	5601.154206	26.168845
189.286442	5607.224685	26.173863
189.733901	5631.227285	26.178880
190.119369	5634.661372	26.183898
190.192663	5634.189073	26.188916
190.092221	5649.315785	26.193933
190.480940	5652.449483	26.198951
190.316961	5653.302272	26.203968
190.535201	5670.866525	26.208986
190.825914	5664.728679	26.214004
191.277536	5688.967453	26.219021
191.514652	5694.656555	26.224039
191.955569	5701.601652	26.229056
191.650514	5706.614937	26.234074
192.097407	5715.295271	26.239092
192.190428	5722.203333	26.244109
192.225849	5724.132880	26.249127
192.664885	5739.762293	26.254144
192.714280	5743.681514	26.259162
192.570593	5746.715548	26.264180
193.304933	5768.782538	26.269197
193.354651	5766.281028	26.274215
193.578964	5776.625107	26.279232
193.722890	5784.153398	26.284250
193.949907	5783.101437	26.289268
193.999118	5797.440910	26.294285
194.599318	5814.506685	26.299303
194.314260	5819.718896	26.304320
194.692548	5832.826241	26.309338
194.679167	5836.559602	26.314356
195.171355	5844.693108	26.319373
195.573908	5850.545744	26.324391
195.467676	5854.366258	26.329408
195.786679	5863.944260	26.334426
196.592778	5870.396589	26.339444
196.676796	5877.564970	26.344461
196.842056	5882.419392	26.349479
196.625453	5882.229255	26.354496
197.208907	5875.707712	26.359514
197.051262	5874.788611	26.364532
197.218566	5887.957459	26.369549
197.539015	5904.700967	26.374567
197.702129	5912.993385	26.379584
197.850744	5911.363396	26.384602
198.315145	5919.914817	26.389620
198.445385	5928.092436	26.394637
198.414154	5926.680023	26.399655
198.523387	5930.681455	26.404672
198.314216	5939.786659	26.409690
198.842689	5944.227489	26.414708
199.051904	5958.049575	26.419725
199.104199	5963.442574	26.424743
199.338331	5970.413856	26.429760
199.731036	5974.809672	26.434778
199.804964	5986.550601	26.439796
199.831348	6009.338037	26.444813
200.312883	5995.606685	26.449831
200.261487	6003.301404	26.454848
200.718579	6021.349436	26.459866
201.269842	6022.566858	26.464884
200.776745	6010.364510	26.469901
201.391046	6028.356354	26.474919
201.269554	6029.328773	26.479936
201.184811	6044.481762	26.484954
202.006670	6041.486758	26.489972
201.930806	6060.694765	26.494989
202.572760	6059.956593	26.500007
202.594027	6065.177706	26.505024
202.389618	6084.639473	26.510042
202.987371	6084.413303	26.515060
203.323754	6089.196779	26.520077
203.648878	6106.233316	26.525095
203.462536	6108.592236	26.530112
203.614999	6120.232559	26.535130
203.958055	6114.237888	26.540148
203.750029	6139.647578	26.545165
204.210926	6137.914983	26.550183
204.738743	6155.248114	26.555200
205.028687	6168.442147	26.560218
205.142309	6158.325966	26.565236
205.224851	6169.311201	26.570253
205.184821	6175.230119	26.575271
205.136096	6182.712992	26.580288
205.605925	6193.274543	26.585306
205.958961	6201.543653	26.590324
205.792997	6221.738223	26.595341
205.887478	6232.368068	26.600359
206.495039	6237.569988	26.605376
206.296839	6254.657079	26.610394
206.685013	6259.375664	26.615412
207.045900	6280.175938	26.620429
207.318319	6292.713042	26.625447
207.633818	6294.156825	26.630464
207.783258	6317.196848	26.635482
208.079837	6311.998587	26.640500
208.018733	6330.551112	26.645517
208.195497	6344.924696	26.650535
208.850106	6338.167713	26.655552
208.869914	6353.149897	26.660570
209.321694	6367.751900	26.665588
209.327474	6366.523061	26.670605
209.317509	6370.480127	26.675623
209.833264	6386.303268	26.680640
210.011697	6391.995468	26.685658
210.289200	6391.166011	26.690676
210.701176	6399.195531	26.695693
211.077745	6405.541719	26.700711
211.134752	6406.865009	26.705728
211.180451	6407.492420	26.710746
211.525946	6422.309995	26.715764
211.629510	6429.964834	26.720781
211.795818	6421.630157	26.725799
211.988074	6416.359819	26.730816
212.106536	6434.211922	26.735834
212.213698	6438.519999	26.740852
212.211604	6452.612321	26.745869
212.518306	6461.400209	26.750887
212.981402	6471.991388	26.755904
212.734473	6482.586472	26.760922
213.172122	6494.456999	26.765940
213.502119	6502.638307	26.770957
213.698492	6511.380366	26.775975
214.138218	6519.958034	26.780992
213.989520	6532.766466	26.786010
214.215907	6525.536685	26.791028
214.397181	6545.872936	26.796045
214.619880	6549.869356	26.801063
214.722403	6544.426788	26.806080
214.872102	6566.532667	26.811098
215.367432	6578.324763	26.816116
215.613656	6588.100800	26.821133
215.714032	6598.714150	26.826151
215.933381	6601.928214	26.831168
216.074893	6616.244398	26.836186
216.792606	6626.195982	26.841204
216.814485	6630.624797	26.846221
216.469959	6640.288212	26.851239
216.800844	6648.201116	26.856256
217.075272	6659.958420	26.861274
217.408307	6671.485572	26.866292
217.705246	6682.279685	26.871309
217.776466	6695.388404	26.876327
217.841210	6690.864037	26.881344
218.180664	6709.234234	26.886362
218.614851	6720.142614	26.891380
218.835294	6735.718734	26.896397
219.090517	6746.538362	26.901415
219.462830	6753.946040	26.906432
219.702968	6762.643481	26.911450
220.042543	6771.795720	26.916468
220.099166	6776.029715	26.921485
220.021846	6778.674699	26.926503
220.347083	6777.793552	26.931520
220.599252	6796.436372	26.936538
220.926585	6797.139638	26.941556
221.210468	6810.956986	26.946573
221.261181	6813.752388	26.951591
221.765165	6825.593797	26.956608
221.749757	6842.147701	26.961626
221.788358	6843.502318	26.966644
222.341835	6856.668191	26.971661
222.407621	6859.903201	26.976679
222.781607	6867.184388	26.981696
222.660664	6878.366082	26.986714
222.828025	6892.965708	26.991732
223.446885	6906.478102	26.996749
223.211272	6923.713734	27.001767
223.809301	6933.333823	27.006784
224.139928	6943.071572	27.011802
224.465962	6946.171121	27.016820
224.838838	6960.173524	27.021837
224.672146	6976.230361	27.026855
225.264699	6977.990683	27.031872
225.023551	6984.263370	27.036890
225.252235	7003.692989	27.041908
225.438902	7003.853216	27.046925
225.490038	7024.412426	27.051943
225.943365	7028.514882	27.056960
226.114358	7041.204135	27.061978
226.475421	7050.605699	27.066996
226.558899	7057.597840	27.072013
226.751715	7077.118392	27.077031
226.922278	7087.888346	27.082048
227.052766	7099.245456	27.087066
227.270955	7104.808531	27.092084
228.166535	7120.781163	27.097101
228.050236	7133.363954	27.102119
228.380299	7129.915463	27.107136
228.411664	7148.097596	27.112154
228.777889	7155.099148	27.117172
228.725762	7167.021583	27.122189
229.039026	7176.642214	27.127207
229.343090	7190.974422	27.132224
229.587990	7187.179373	27.137242
230.404558	7202.283673	27.142260
229.895923	7196.620960	27.147277
230.314999	7207.004791	27.152295
230.371038	7202.361699	27.157312
230.589158	7213.844057	27.162330
230.771248	7224.239767	27.167348
230.873084	7246.066683	27.172365
230.807579	7248.170047	27.177383
231.151914	7258.322532	27.182400
231.749685	7276.851719	27.187418
232.118913	7297.964380	27.192436
232.380734	7303.965809	27.197453
232.595175	7317.036750	27.202471
233.084752	7318.185007	27.207488
232.920376	7320.827921	27.212506
233.503477	7343.040473	27.217524
233.920172	7348.578840	27.222541
233.752809	7357.621369	27.227559
234.299644	7363.180393	27.232576
234.579157	7382.570881	27.237594
234.370590	7375.633049	27.242612
234.887381	7386.955076	27.247629
234.988441	7399.431387	27.252647
235.306467	7404.252813	27.257664
235.179551	7424.799323	27.262682
235.597548	7429.665076	27.267700
236.213617	7441.571408	27.272717
236.096625	7461.945928	27.277735
236.403753	7463.327979	27.282752
236.600049	7485.105653	27.287770
236.613083	7487.764997	27.292788
237.348225	7496.382086	27.297805
236.998957	7515.454493	27.302823
237.513223	7526.496031	27.307840
237.308736	7532.138078	27.312858
237.677796	7547.192802	27.317876
237.939251	7562.498013	27.322893
238.115439	7575.515147	27.327911
239.196418	7583.983391	27.332928
239.023407	7596.183913	27.337946
239.263450	7605.121701	27.342964
240.014582	7618.355027	27.347981
240.303265	7628.194422	27.352999
240.603444	7622.098644	27.358016
240.818705	7636.328302	27.363034
241.114775	7633.106034	27.368052
241.154446	7622.489200	27.373069
241.181171	7635.627658	27.378087
241.425389	7639.428369	27.383104
241.293152	7641.305457	27.388122
241.570134	7664.497669	27.393140
242.200995	7667.177063	27.398157
242.347437	7674.667854	27.403175
242.423764	7682.074921	27.408192
242.773275	7705.445243	27.413210
243.045094	7717.149965	27.418228
243.134042	7719.847962	27.423245
243.237077	7731.377085	27.428263
243.558630	7733.666118	27.433280
244.136499	7754.430917	27.438298
244.145464	7757.741284	27.443316
244.362673	7773.432444	27.448333
244.274147	7774.084086	27.453351
244.775251	7780.900584	27.458368
244.863696	7798.083111	27.463386
245.218826	7808.941385	27.468404
245.736371	7824.591854	27.473421
245.314971	7827.473996	27.478439
245.925739	7836.783178	27.483456
246.393763	7847.952122	27.488474
246.059310	7853.191583	27.493492
246.850758	7863.492198	27.498509
246.859669	7874.613111	27.503527
246.955063	7886.882276	27.508544
247.433151	7900.815245	27.513562
247.511180	7907.388676	27.518580
248.025145	7921.442323	27.523597
248.246745	7930.070611	27.528615
248.650872	7950.114627	27.533632
248.785767	7964.881200	27.538650
249.068417	7959.646777	27.543668
249.386405	7967.158169	27.548685
249.640468	7972.040278	27.553703
249.691670	7975.798684	27.558720
249.811156	7999.994678	27.563738
249.814868	8000.338272	27.568756
250.696181	8015.540443	27.573773
250.453977	8032.418237	27.578791
250.826298	8042.285793	27.583808
251.211236	8050.879078	27.588826
251.156129	8072.387437	27.593844
251.365607	8080.026372	27.598861
252.061209	8104.094368	27.603879
252.513919	8100.143454	27.608896
252.360509	8115.046866	27.613914
252.191450	8127.878536	27.618932
252.580525	8139.539902	27.623949
253.151751	8158.244620	27.628967
253.236507	8169.338045	27.633984
253.766935	8188.999470	27.639002
253.569599	8203.193173	27.644020
254.042526	8218.071164	27.649037
254.486860	8229.171438	27.654055
254.614975	8243.816169	27.659072
255.246968	8254.801819	27.664090
255.277176	8260.764074	27.669108
255.712323	8274.842967	27.674125
256.080629	8283.776778	27.679143
256.576039	8287.926599	27.684160
257.421516	8303.204080	27.689178
257.145068	8297.640406	27.694196
257.464119	8301.555817	27.699213
257.827530	8307.238579	27.704231
257.748667	8300.317964	27.709248
258.106435	8308.517830	27.714266
258.141589	8319.562287	27.719284
258.517957	8314.521453	27.724301
258.704562	8338.615820	27.729319
259.201433	8339.428348	27.734336
259.125234	8345.789312	27.739354
259.165165	8359.901767	27.744372
259.559203	8358.671960	27.749389
259.857433	8373.006003	27.754407
260.089450	8389.705649	27.759424
260.318542	8398.995980	27.764442
260.683129	8409.395343	27.769460
260.513621	8411.344646	27.774477
261.157658	8431.010634	27.779495
261.302008	8443.357742	27.784512
261.379581	8443.367746	27.789530
261.620113	8471.280291	27.794548
261.800060	8463.346672	27.799565
262.486070	8486.352715	27.804583
262.268190	8499.261747	27.809600
262.883846	8502.755037	27.814618
263.033024	8522.776472	27.819636
263.670188	8528.609005	27.824653
263.669580	8535.024492	27.829671
263.833793	8547.226486	27.834688
264.204418	8550.698184	27.839706
263.952168	8561.109018	27.844724
264.308469	8573.334610	27.849741
264.435620	8593.773160	27.854759
264.411282	8607.431769	27.859776
264.678828	8632.451518	27.864794
265.012133	8648.314666	27.869812
265.319258	8657.927564	27.874829
265.881224	8683.677926	27.879847
266.043894	8697.686168	27.884864
266.684846	8709.011663	27.889882
266.895019	8739.897122	27.894900
267.092752	8741.324824	27.899917
267.627971	8757.901533	27.904935
267.647749	8775.102038	27.909952
268.239011	8773.721337	27.914970
268.031488	8795.854278	27.919988
268.702718	8809.745052	27.925005
269.299482	8815.767124	27.930023
269.176885	8822.498597	27.935040
269.248481	8825.698312	27.940058
269.548166	8846.138528	27.945076
269.949724	8853.444603	27.950093
270.275542	8867.828381	27.955111
270.705456	8878.325121	27.960128
271.158092	8889.800202	27.965146
271.541039	8899.464492	27.970164
271.575461	8902.351166	27.975181
271.921282	8922.945258	27.980199
271.928547	8931.800180	27.985216
272.682752	8933.371203	27.990234
273.005624	8948.311177	27.995252
273.414057	8950.649900	28.000269
273.313922	8965.081536	28.005287
273.240138	8967.884139	28.010304
273.649333	8968.060044	28.015322
273.642650	8984.058827	28.020340
274.122805	8996.988304	28.025357
274.289320	9020.647851	28.030375
274.725086	9036.359521	28.035392
274.986628	9042.610985	28.040410
275.404665	9048.856881	28.045428
275.566076	9065.397706	28.050445
275.920482	9076.537836	28.055463
276.386022	9091.540822	28.060480
276.804766	9094.026339	28.065498
276.699171	9106.321483	28.070516
277.000378	9112.191045	28.075533
277.046936	9126.536682	28.080551
277.312657	9141.122680	28.085568
277.897361	9146.928900	28.090586
277.789046	9167.872243	28.095604
278.178480	9181.277021	28.100621
278.372031	9196.013287	28.105639
278.764708	9200.365690	28.110656
279.099494	9211.392156	28.115674
279.427124	9227.749224	28.120692
279.768700	9236.109904	28.125709
280.080908	9251.648518	28.130727
279.912827	9272.746576	28.135744
280.522634	9275.214818	28.140762
281.026607	9283.332227	28.145780
280.950708	9299.986211	28.150797
281.547753	9309.159371	28.155815
281.558331	9318.449665	28.160832
281.698832	9332.322938	28.165850
281.998537	9333.936780	28.170868
282.282706	9352.504555	28.175885
282.617773	9366.192668	28.180903
282.657896	9381.429868	28.185920
282.938096	9379.696876	28.190938
282.947688	9407.432311	28.195956
283.334083	9422.656346	28.200973
283.694731	9438.670597	28.205991
283.649460	9465.309655	28.211008
284.141126	9475.165599	28.216026
284.630890	9500.808432	28.221044
284.910636	9515.821923	28.226061
285.654031	9528.205364	28.231079
285.667836	9545.375945	28.236096
286.019561	9551.433488	28.241114
286.417419	9567.277840	28.246132
286.500352	9575.843370	28.251149
287.102474	9597.575747	28.256167
287.298883	9609.397675	28.261184
287.998447	9620.458805	28.266202
288.123471	9629.781844	28.271220
288.173798	9642.157108	28.276237
288.827424	9643.049337	28.281255
288.661144	9646.194895	28.286272
288.800989	9657.968881	28.291290
289.419378	9668.790170	28.296308
289.672523	9691.234051	28.301325
290.497527	9696.620764	28.306343
290.210880	9717.775787	28.311360
290.649489	9712.042841	28.316378
290.904448	9726.583625	28.321396
291.018188	9748.206399	28.326413
291.546068	9753.068190	28.331431
291.466662	9765.817484	28.336448
291.610447	9776.561628	28.341466
292.481495	9794.071758	28.346484
292.751500	9820.674566	28.351501
293.068917	9819.207239	28.356519
293.294075	9839.439208	28.361536
293.697982	9844.500414	28.366554
293.660471	9854.546806	28.371572
294.120642	9871.174159	28.376589
294.601068	9871.045281	28.381607
294.440166	9900.866772	28.386624
294.682739	9898.040857	28.391642
294.335033	9920.203407	28.396660
295.112030	9943.335936	28.401677
295.236632	9966.349672	28.406695
295.647378	9983.628976	28.411712
296.089785	10006.056220	28.416730
296.533631	10024.321802	28.421748
296.551453	10041.378544	28.426765
297.188202	10061.104242	28.431783
297.482983	10073.258370	28.436800
297.738273	10083.303222	28.441818
298.104422	10101.637885	28.446836
298.581244	10125.638592	28.451853
298.797651	10124.875383	28.456871
299.325336	10146.645323	28.461888
299.817144	10141.535399	28.466906
299.789210	10163.449228	28.471924
299.927921	10169.805566	28.476941
300.278430	10176.422370	28.481959
300.294055	10198.086294	28.486976
300.545655	10200.756018	28.491994
301.019231	10217.353163	28.497012
301.007295	10229.738571	28.502029
301.974635	10243.467216	28.507047
302.009501	10257.888177	28.512064
302.456768	10261.638681	28.517082
303.009232	10276.878450	28.522100
302.580759	10273.753442	28.527117
302.957468	10287.890385	28.532135
302.949948	10308.130894	28.537152
303.390434	10318.386830	28.542170
303.573104	10347.021685	28.547188
304.081475	10368.933840	28.552205
304.197683	10380.288885	28.557223
304.682276	10403.758279	28.562240
305.116569	10415.922351	28.567258
305.252796	10447.794732	28.572276
305.544330	10461.762015	28.577293
305.951518	10463.093892	28.582311
306.248650	10481.913363	28.587328
306.919987	10502.069844	28.592346
306.945040	10519.858428	28.597364
307.656303	10542.758873	28.602381
307.764916	10545.132139	28.607399
307.960678	10565.565266	28.612416
308.366573	10572.063022	28.617434
308.685856	10587.671110	28.622452
308.807908	10593.764972	28.627469
309.256964	10607.448774	28.632487
309.806197	10629.190643	28.637504
309.770866	10644.285976	28.642522
310.471817	10660.229027	28.647540
310.685696	10679.740604	28.652557
311.261562	10695.299118	28.657575
311.361596	10701.566970	28.662592
311.829441	10710.208501	28.667610
312.145652	10723.199597	28.672628
312.274357	10740.599566	28.677645
312.921609	10738.783694	28.682663
312.942129	10764.141815	28.687680
313.491320	10761.810838	28.692698
313.497147	10776.754583	28.697716
314.010114	10797.659269	28.702733
314.635060	10794.249173	28.707751
314.407096	10806.239377	28.712768
314.597061	10825.656969	28.717786
314.873513	10847.991235	28.722804
315.197365	10864.539788	28.727821
315.715943	10870.379016	28.732839
315.878793	10889.892491	28.737856
316.197414	10909.845746	28.742874
316.404462	10922.490963	28.747892
316.812167	10936.102545	28.752909
317.031381	10948.597468	28.757927
317.295082	10971.404356	28.762944
317.850177	10985.106558	28.767962
318.343475	10994.015785	28.772980
318.418152	11014.629407	28.777997
319.140718	11026.139310	28.783015
319.239413	11047.718581	28.788032
319.482063	11067.055546	28.793050
319.682185	11065.742275	28.798068
320.054791	11087.512346	28.803085
320.518994	11108.617631	28.808103
320.476564	11122.928221	28.813120
320.441288	11136.625128	28.818138
320.577570	11155.359958	28.823156
321.457009	11173.476336	28.828173
322.130084	11186.626572	28.833191
321.984943	11200.719648	28.838208
322.733622	11217.164075	28.843226
322.804975	11232.659974	28.848244
323.245901	11250.901955	28.853261
323.788184	11248.537268	28.858279
323.938611	11273.436820	28.863296
323.977150	11283.089994	28.868314
324.412341	11303.821130	28.873332
324.741575	11320.767104	28.878349
325.063340	11331.039038	28.883367
325.474962	11345.629170	28.888384
325.476522	11357.125915	28.893402
326.022344	11371.019312	28.898420
326.162228	11393.470351	28.903437
326.540912	11399.259034	28.908455
326.778468	11427.091219	28.913472
327.230933	11441.962374	28.918490
327.800716	11458.873951	28.923508
327.727154	11483.660459	28.928525
328.440578	11504.322972	28.933543
328.887359	11516.874199	28.938560
328.771372	11529.570427	28.943578
329.242792	11550.409836	28.948596
329.748537	11563.374986	28.953613
330.393445	11567.650547	28.958631
330.431262	11593.730185	28.963648
330.554475	11609.085649	28.968666
331.342111	11623.440268	28.973684
331.490705	11639.394897	28.978701
331.873686	11650.519464	28.983719
332.100971	11676.010628	28.988736
332.418609	11684.290904	28.993754
332.777574	11705.574389	28.998772
332.780556	11732.417522	29.003789
333.464962	11737.324790	29.008807
333.397246	11751.699815	29.013824
333.682428	11769.256216	29.018842
334.199416	11791.645503	29.023860
334.574622	11813.409695	29.028877
335.188245	11822.294155	29.033895
335.464381	11845.965372	29.038912
335.929293	11863.588439	29.043930
336.690377	11871.600399	29.048948
337.002982	11893.813413	29.053965
337.385453	11886.506587	29.058983
337.540662	11903.792963	29.064000
337.622824	11928.284099	29.069018
337.757405	11926.693683	29.074036
338.102002	11951.052166	29.079053
338.275386	11968.799941	29.084071
339.098815	11986.104873	29.089088
339.516214	11993.697060	29.094106
340.318422	12001.453173	29.099124
340.412143	12020.163955	29.104141
340.919840	12022.866456	29.109159
341.298220	12038.738064	29.114176
341.254081	12051.537068	29.119194
341.593082	12054.787026	29.124212
341.787693	12068.821216	29.129229
342.111819	12072.717690	29.134247
342.155497	12094.142577	29.139264
342.761792	12111.525846	29.144282
343.327057	12136.071047	29.149300
343.212468	12149.165351	29.154317
343.531965	12167.247253	29.159335
343.662429	12163.409132	29.164352
343.847321	12191.108598	29.169370
344.593988	12197.626174	29.174388
344.745688	12225.795083	29.179405
345.102767	12239.128187	29.184423
345.034706	12240.702005	29.189440
345.324760	12262.461109	29.194458
346.384199	12287.626970	29.199476
346.548704	12313.943541	29.204493
346.544877	12323.376524	29.209511
347.148517	12347.382322	29.214528
347.192397	12363.698169	29.219546
347.982270	12393.406263	29.224564
347.874340	12402.808225	29.229581
348.145268	12419.596961	29.234599
348.816639	12448.973188	29.239616
349.260154	12463.230783	29.244634
350.092315	12477.509613	29.249652
350.312962	12487.643288	29.254669
350.742508	12505.875642	29.259687
351.147953	12504.896419	29.264704
351.350255	12532.034725	29.269722
351.980768	12536.783284	29.274740
352.495845	12554.534929	29.279757
352.238896	12567.478141	29.284775
353.070139	12581.905613	29.289792
353.174505	12596.462745	29.294810
353.810093	12602.202087	29.299828
353.810151	12621.840754	29.304845
354.303490	12642.415842	29.309863
354.563853	12659.165395	29.314880
354.733176	12671.580860	29.319898
355.719116	12684.616830	29.324916
355.824169	12698.229734	29.329933
356.303849	12717.026012	29.334951
356.315418	12724.344175	29.339968
356.450183	12742.957667	29.344986
356.817464	12767.392601	29.350004
357.269242	12780.357573	29.355021
357.721808	12800.737117	29.360039
358.093549	12820.324085	29.365056
358.097359	12841.020280	29.370074
358.879792	12854.025088	29.375092
359.047487	12882.975628	29.380109
359.063015	12897.786907	29.385127
359.212335	12920.254077	29.390144
359.704824	12943.412784	29.395162
359.968829	12967.232573	29.400180
360.529983	12989.831107	29.405197
361.109061	13007.617365	29.410215
361.248871	13028.346146	29.415232
361.565094	13050.042060	29.420250
361.870072	13069.829219	29.425268
362.705276	13096.752355	29.430285
363.031193	13115.118375	29.435303
363.420341	13142.076709	29.440320
363.638934	13163.626991	29.445338
364.673485	13178.417819	29.450356
364.507164	13194.568358	29.455373
364.994652	13209.779644	29.460391
365.562640	13215.100285	29.465408
365.371230	13242.901291	29.470426
366.136254	13259.108108	29.475444
366.458417	13279.641229	29.480461
366.726634	13290.348948	29.485479
367.127768	13312.401344	29.490496
367.248607	13324.420614	29.495514
368.307897	13331.082256	29.500532
368.488585	13357.394588	29.505549
369.000155	13359.562984	29.510567
368.945655	13368.031771	29.515584
369.189954	13384.844485	29.520602
369.461972	13395.447455	29.525620
369.849039	13419.103271	29.530637
369.961436	13438.380968	29.535655
370.328784	13457.385058	29.540672
370.690386	13474.397378	29.545690
370.923527	13491.057194	29.550708
371.474300	13519.285524	29.555725
371.688030	13546.729820	29.560743
372.326337	13557.000760	29.565760
372.600274	13577.260697	29.570778
373.314761	13601.275994	29.575796
373.252165	13626.789935	29.580813
373.244941	13653.290013	29.585831
373.897741	13665.194593	29.590848
374.427687	13700.633054	29.595866
374.943536	13710.544296	29.600884
375.434654	13736.527465	29.605901
375.625091	13761.979847	29.610919
376.490799	13775.749126	29.615936
376.621913	13799.341294	29.620954
377.290530	13817.092184	29.625972
377.583375	13828.876401	29.630989
377.787137	13848.017039	29.636007
378.442383	13874.325231	29.641024
378.552467	13889.248795	29.646042
379.155376	13909.359657	29.651060
379.426077	13931.401623	29.656077
379.701608	13936.294572	29.661095
380.456373	13952.800451	29.666112
380.911673	13969.751169	29.671130
380.998602	13982.613057	29.676148
381.573633	14000.486153	29.681165
381.572326	14025.855232	29.686183
382.128355	14041.280676	29.691200
382.319093	14068.069289	29.696218
382.705993	14081.411656	29.701236
383.085859	14104.968397	29.706253
383.510805	14121.207119	29.711271
384.131924	14147.097851	29.716288
384.512360	14171.020924	29.721306
384.729533	14185.188950	29.726324
385.242084	14203.678381	29.731341
385.352669	14231.307203	29.736359
386.292776	14246.637913	29.741376
386.193332	14267.923456	29.746394
386.879936	14282.734917	29.751412
387.054636	14311.427573	29.756429
387.312081	14327.256887	29.761447
388.164387	14343.106729	29.766464
388.610031	14356.932758	29.771482
388.766106	14368.293437	29.776500
389.352339	14385.002948	29.781517
389.936539	14399.359979	29.786535
390.405111	14419.353467	29.791552
390.396659	14438.035269	29.796570
390.977349	14442.722643	29.801588
391.437533	14470.079139	29.806605
391.162208	14487.561639	29.811623
391.906961	14498.495423	29.816640
392.352371	14517.087263	29.821658
392.650659	14542.650123	29.826676
392.893778	14562.956995	29.831693
393.197343	14579.464617	29.836711
393.751740	14597.366774	29.841728
394.206979	14624.351602	29.846746
394.287256	14634.688431	29.851764
394.849171	14647.621644	29.856781
395.081982	14673.564443	29.861799
395.419257	14680.459677	29.866816
395.886582	14713.465400	29.871834
396.326206	14729.304411	29.876852
396.682656	14753.083538	29.881869
396.668437	14765.317525	29.886887
397.307480	14791.841128	29.891904
397.336363	14810.135304	29.896922
397.533632	14835.881765	29.901940
398.211426	14858.334772	29.906957
398.474458	14897.272360	29.911975
399.299497	14915.738804	29.916992
399.874911	14952.438925	29.922010
400.072149	14965.625286	29.927028
400.427073	14983.050576	29.932045
400.346772	15008.423860	29.937063
401.204736	15039.192932	29.942080
401.707429	15052.656808	29.947098
402.131719	15076.286749	29.952116
402.765696	15100.133377	29.957133
403.294949	15131.557313	29.962151
403.958065	15143.590700	29.967168
404.510894	15167.045865	29.972186
404.583199	15186.486367	29.977204
405.383977	15203.219843	29.982221
405.491626	15225.614149	29.987239
405.940613	15239.901406	29.992256
406.308395	15254.968854	29.997274
406.758942	15260.144243	30.002292
407.401780	15274.435903	30.007309
407.438267	15302.573733	30.012327
408.035652	15312.081417	30.017344
408.652873	15328.591091	30.022362
408.989424	15352.181426	30.027380
409.060701	15359.766023	30.032397
409.484812	15385.285037	30.037415
409.930681	15402.399585	30.042432
410.408492	15420.715618	30.047450
410.359391	15444.268566	30.052468
411.213955	15473.579732	30.057485
411.470649	15493.117997	30.062503
411.815113	15507.529208	30.067520
412.088699	15527.538610	30.072538
412.769795	15558.693116	30.077556
413.186377	15576.380907	30.082573
413.529718	15602.250804	30.087591
413.694458	15619.232713	30.092608
414.087704	15647.201468	30.097626
414.731860	15662.759710	30.102644
415.345233	15687.223020	30.107661
415.532117	15714.513567	30.112679
416.234872	15725.710467	30.117696
416.682520	15748.506933	30.122714
416.702849	15779.421036	30.127732
417.175532	15789.400138	30.132749
417.760121	15816.426401	30.137767
418.268322	15831.807099	30.142784
418.954449	15856.799312	30.147802
418.981188	15874.466323	30.152820
419.703800	15890.293558	30.157837
419.678178	15919.335844	30.162855
420.362145	15933.672091	30.167872
420.431604	15953.034857	30.172890
420.707156	15983.482928	30.177908
421.700510	16006.358463	30.182925
421.804381	16031.192591	30.187943
422.426726	16036.473937	30.192960
422.427916	16050.216050	30.197978
422.770276	16078.938791	30.202996
422.715723	16095.405906	30.208013
423.366203	16134.130560	30.213031
424.339739	16151.065217	30.218048
425.071785	16168.833639	30.223066
425.182034	16184.769668	30.228084
425.877222	16192.973834	30.233101
426.049933	16224.010072	30.238119
426.310662	16238.731844	30.243136
426.759965	16268.114024	30.248154
427.155757	16286.336347	30.253172
428.168431	16299.329577	30.258189
428.297796	16323.496815	30.263207
428.932375	16335.184838	30.268224
429.476435	16357.913235	30.273242
429.303851	16380.059046	30.278260
429.684238	16406.192696	30.283277
430.347730	16433.930761	30.288295
430.938355	16444.899287	30.293312
431.336299	16462.688729	30.298330
431.561938	16494.933129	30.303348
431.868836	16509.398357	30.308365
432.481499	16539.462866	30.313383
432.935447	16556.160260	30.318400
433.379499	16585.799586	30.323418
433.632673	16609.442431	30.328436
434.197286	16625.993053	30.333453
434.437920	16649.236781	30.338471
434.625422	16669.121883	30.343488
435.610144	16696.560491	30.348506
435.835569	16721.322776	30.353524
436.421283	16743.858753	30.358541
436.788483	16772.843957	30.363559
437.402644	16797.589671	30.368576
437.880900	16826.930268	30.373594
438.036735	16841.640506	30.378612
438.584441	16869.119384	30.383629
439.335697	16892.472938	30.388647
439.694006	16914.413025	30.393664
440.002811	16941.578826	30.398682
440.359103	16962.843352	30.403700
441.174354	16979.411876	30.408717
441.383587	17006.381742	30.413735
441.970181	17031.476359	30.418752
442.245407	17054.933099	30.423770
442.792352	17070.684595	30.428788
443.056449	17081.072915	30.433805
443.466687	17115.437274	30.438823
444.066320	17139.089674	30.443840
444.795986	17164.983290	30.448858
444.747388	17193.083515	30.453876
445.238852	17217.030910	30.458893
445.851851	17232.380526	30.463911
446.199549	17265.289354	30.468928
446.850778	17288.548506	30.473946
447.192333	17309.979972	30.478964
447.819065	17332.990325	30.483981
447.932952	17356.668537	30.488999
448.177547	17374.381765	30.494016
449.057455	17400.460635	30.499034
449.393590	17428.456721	30.504052
449.589605	17450.189098	30.509069
450.565849	17471.401303	30.514087
450.693685	17497.162208	30.519104
451.103200	17520.800634	30.524122
451.528097	17534.234223	30.529140
452.228226	17547.953212	30.534157
452.433959	17572.526996	30.539175
453.031784	17594.499832	30.544192
453.500602	17612.607737	30.549210
453.603519	17630.608720	30.554228
454.489278	17650.388625	30.559245
454.435559	17672.880545	30.564263
454.648603	17701.250078	30.569280
455.385283	17718.336936	30.574298
455.376425	17755.604576	30.579316
456.233929	17774.523553	30.584333
456.410090	17797.219672	30.589351
457.219191	17823.657662	30.594368
457.529417	17848.682918	30.599386
458.261833	17879.460424	30.604404
458.941402	17901.799851	30.609421
459.328863	17930.395098	30.614439
459.544189	17959.996552	30.619456
460.115862	17978.000247	30.624474
460.508516	17998.571616	30.629492
461.494186	18021.387587	30.634509
461.385656	18054.135470	30.639527
461.884086	18082.871498	30.644544
462.444005	18099.341997	30.649562
462.682078	18138.062623	30.654580
463.332220	18164.469120	30.659597
463.776095	18189.897157	30.664615
464.128129	18210.133967	30.669632
464.705444	18236.798354	30.674650
464.925549	18269.703605	30.679668
465.770065	18283.204660	30.684685
466.696994	18317.553402	30.689703
466.238009	18343.874844	30.694720
467.078016	18369.190531	30.699738
467.532930	18400.612500	30.704756
468.219725	18417.347689	30.709773
468.752213	18441.606057	30.714791
468.702148	18469.632550	30.719808
469.675191	18496.159500	30.724826
469.963964	18521.302702	30.729844
470.499137	18555.833261	30.734861
471.455793	18575.533518	30.739879
471.314711	18604.206225	30.744896
472.168840	18617.169008	30.749914
472.567906	18648.524315	30.754932
472.877373	18664.838675	30.759949
473.528926	18697.487544	30.764967
474.259912	18723.111383	30.769984
474.904801	18744.042052	30.775002
474.868527	18769.754538	30.780020
475.845120	18793.956423	30.785037
475.934151	18805.061722	30.790055
476.353153	18840.463876	30.795072
476.962059	18857.988728	30.800090
477.468622	18882.321203	30.805108
477.801730	18902.125775	30.810125
478.503848	18916.774139	30.815143
478.833199	18940.028835	30.820160
479.607140	18954.526987	30.825178
479.797103	18990.356989	30.830196
480.183404	19010.652445	30.835213
480.893058	19031.661730	30.840231
481.262927	19044.991268	30.845248
481.617833	19068.760175	30.850266
481.733636	19097.001667	30.855284
482.280267	19133.527889	30.860301
482.688808	19147.047293	30.865319
483.138983	19179.886460	30.870336
483.211298	19210.725244	30.875354
484.095719	19236.243597	30.880372
484.453810	19258.578082	30.885389
485.044648	19281.665872	30.890407
485.472456	19314.060199	30.895424
486.081802	19333.550275	30.900442
486.561051	19364.369791	30.905460
486.764378	19386.551761	30.910477
487.457299	19414.734912	30.915495
487.763125	19434.740154	30.920512
488.112598	19468.328459	30.925530
488.437290	19502.862077	30.930548
489.141915	19531.637450	30.935565
489.631573	19568.640940	30.940583
490.124828	19607.450879	30.945600
490.986329	19633.895769	30.950618
491.455434	19670.466730	30.955636
491.883493	19700.890443	30.960653
492.574456	19731.955372	30.965671
492.617125	19745.203959	30.970688
493.300141	19769.895306	30.975706
494.032850	19806.576868	30.980724
494.755505	19834.459020	30.985741
495.135325	19863.923880	30.990759
495.867042	19888.898381	30.995776
496.354329	19907.548892	31.000794
496.594235	19948.048207	31.005812
497.251094	19967.038665	31.010829
497.761338	19992.686115	31.015847
498.173420	20028.963408	31.020864
498.606564	20047.104447	31.025882
498.637880	20083.706840	31.030900
498.953077	20103.212167	31.035917
500.090890	20142.781483	31.040935
500.218182	20176.342621	31.045952
501.388669	20200.269483	31.050970
501.424506	20240.036865	31.055988
501.985293	20268.930627	31.061005
502.717737	20297.431090	31.066023
502.770896	20326.973083	31.071040
503.628440	20352.667701	31.076058
503.534564	20400.618868	31.081076
504.513663	20421.606407	31.086093
505.181079	20445.239587	31.091111
505.413860	20481.166705	31.096128
505.977710	20508.670324	31.101146
506.282021	20547.189488	31.106164
506.845182	20574.149933	31.111181
507.529431	20612.969862	31.116199
507.944649	20641.090866	31.121216
508.687962	20667.606215	31.126234
509.082518	20705.568180	31.131252
510.069195	20738.016336	31.136269
509.971510	20762.521614	31.141287
510.739141	20791.396387	31.146304
510.969672	20823.697744	31.151322
511.773236	20856.111592	31.156340
512.010578	20886.358510	31.161357
512.763797	20918.584477	31.166375
513.477872	20948.990605	31.171392
514.035318	20962.791230	31.176410
514.547157	21003.332270	31.181428
514.893393	21023.149572	31.186445
515.590622	21053.419495	31.191463
515.763488	21076.183127	31.196480
516.807473	21101.830574	31.201498
517.491575	21130.308228	31.206516
517.859655	21156.143748	31.211533
518.072778	21170.156409	31.216551
518.420352	21194.807316	31.221568
519.040459	21219.548258	31.226586
519.547127	21238.329690	31.231604
520.087702	21268.984636	31.236621
520.669586	21282.787977	31.241639
521.009251	21315.768086	31.246656
521.374893	21334.925536	31.251674
521.980549	21367.383863	31.256692
522.323853	21392.876053	31.261709
522.914031	21425.020971	31.266727
523.031947	21448.021108	31.271744
523.495681	21476.647513	31.276762
524.250356	21511.407976	31.281780
524.860225	21553.666091	31.286797
525.262948	21582.005230	31.291815
525.992585	21624.870283	31.296832
526.500262	21653.237317	31.301850
527.324746	21682.717405	31.306868
527.579087	21717.354397	31.311885
528.080053	21747.156954	31.316903
528.302186	21773.591140	31.321920
529.180286	21801.894054	31.326938
529.956683	21842.098406	31.331956
530.378304	21874.864415	31.336973
530.892877	21897.392234	31.341991
531.517207	21939.048632	31.347008
532.420025	21963.145951	31.352026
532.575825	21991.581220	31.357044
533.389522	22028.551232	31.362061
533.777627	22049.531980	31.367079
534.295435	22087.028669	31.372096
534.789079	22120.371452	31.377114
535.683186	22139.857637	31.382132
535.959810	22169.797069	31.387149
537.025811	22194.482038	31.392167
537.381767	22218.292509	31.397184
537.471335	22246.593186	31.402202
538.483419	22272.872724	31.407220
538.839474	22310.414127	31.412237
539.629679	22326.510912	31.417255
539.702798	22357.935837	31.422272
540.462471	22390.757177	31.427290
541.114476	22413.548410	31.432308
541.094908	22444.179172	31.437325
542.296866	22471.655102	31.442343
542.476035	22503.714495	31.447360
543.035706	22532.302130	31.452378
543.606524	22555.738135	31.457396
543.678514	22597.994260	31.462413
544.809417	22628.786344	31.467431
545.079521	22662.796946	31.472448
545.909033	22687.311046	31.477466
546.743871	22727.318478	31.482484
546.500812	22749.890101	31.487501
547.477118	22765.768529	31.492519
547.908327	22806.218476	31.497536
548.344752	22842.882596	31.502554
548.995185	22869.301717	31.507572
549.551893	22908.139822	31.512589
550.222154	22932.830825	31.517607
550.643671	22967.184739	31.522624
551.066216	22997.127842	31.527642
551.830170	23027.263964	31.532660
551.988604	23067.605507	31.537677
552.805637	23092.286360	31.542695
553.183137	23125.345707	31.547712
553.783487	23158.338611	31.552730
554.494929	23184.040856	31.557748
554.844694	23210.874032	31.562765
555.497607	23228.092585	31.567783
556.105455	23260.888592	31.572800
556.575243	23281.213299	31.577818
556.904026	23319.380159	31.582836
557.389538	23353.895336	31.587853
557.980127	23377.942177	31.592871
558.664088	23413.645981	31.597888
558.880361	23452.089804	31.602906
559.980427	23472.322313	31.607924
560.506739	23516.954772	31.612941
561.205775	23529.167852	31.617959
561.512963	23567.477593	31.622976
562.091157	23604.127233	31.627994
562.783013	23628.569269	31.633012
563.346270	23655.249542	31.638029
564.580485	23673.344290	31.643047
564.650384	23700.304108	31.648064
565.373403	23730.359238	31.653082
565.935153	23754.069809	31.658100
566.633127	23787.086384	31.663117
567.535857	23818.124592	31.668135
567.708434	23845.207550	31.673152
567.919083	23865.996836	31.678170
568.875449	23912.117385	31.683188
569.213127	23930.182158	31.688205
570.229671	23963.307116	31.693223
570.239713	23996.640318	31.698240
570.938520	24022.667916	31.703258
571.590869	24043.268141	31.708276
572.141508	24082.381222	31.713293
573.163049	24113.900518	31.718311
573.509331	24131.698710	31.723328
573.753523	24154.195608	31.728346
574.136381	24176.411716	31.733364
574.673120	24220.627034	31.738381
575.416614	24266.377297	31.743399
576.073145	24283.785784	31.748416
576.643574	24330.700804	31.753434
576.936404	24352.779540	31.758452
577.712559	24393.008059	31.763469
578.209217	24428.054189	31.768487
579.145614	24465.793145	31.773504
579.689973	24508.939906	31.778522
580.344026	24517.621697	31.783540
580.710330	24560.973404	31.788557
581.329716	24584.998234	31.793575
582.139043	24626.201560	31.798592
582.248243	24656.215189	31.803610
583.231794	24683.254426	31.808628
583.824413	24721.831337	31.813645
584.478539	24754.609915	31.818663
585.155592	24783.966035	31.823680
585.741973	24811.889201	31.828698
586.295581	24834.862934	31.833716
586.527500	24872.940498	31.838733
587.544181	24898.691947	31.843751
588.131190	24921.944935	31.848768
588.558103	24962.393606	31.853786
589.285011	24978.856366	31.858804
589.892852	25024.098752	31.863821
590.399676	25044.451055	31.868839
590.944377	25077.335775	31.873856
591.097076	25107.791967	31.878874
592.070684	25141.096238	31.883892
592.449866	25174.594776	31.888909
592.962931	25210.549749	31.893927
593.666892	25220.652299	31.898944
593.925672	25260.527525	31.903962
594.500242	25279.340070	31.908980
595.044538	25311.561659	31.913997
595.414803	25347.905791	31.919015
595.961145	25388.254459	31.924032
596.357738	25420.164404	31.929050
597.522483	25447.549168	31.934068
597.969716	25484.905308	31.939085
598.615456	25527.482236	31.944103
598.863147	25557.406002	31.949120
599.844432	25603.507588	31.954138
600.333710	25631.788378	31.959156
601.041816	25664.085996	31.964173
601.747479	25698.703459	31.969191
602.621568	25730.355836	31.974208
603.163546	25766.187197	31.979226
603.719129	25799.456911	31.984244
604.164173	25839.291472	31.989261
604.760059	25866.753260	31.994279
605.840838	25897.160096	31.999296
606.404223	25940.344873	32.004314
607.207385	25965.164176	32.009332
607.904194	25998.677542	32.014349
607.959781	26030.938901	32.019367
608.634493	26061.504381	32.024384
609.258345	26097.140227	32.029402
609.639571	26125.122630	32.034420
610.246220	26159.383509	32.039437
610.870722	26198.659789	32.044455
611.622723	26225.971216	32.049472
611.683232	26274.538015	32.054490
613.096483	26305.304206	32.059508
613.497829	26342.997769	32.064525
614.141487	26391.776887	32.069543
614.942561	26428.125019	32.074560
615.414768	26455.050805	32.079578
616.197460	26490.668790	32.084596
616.642365	26524.197200	32.089613
617.338608	26575.629321	32.094631
617.814690	26592.246452	32.099648
618.353705	26642.451968	32.104666
619.089040	26669.077702	32.109684
619.244544	26710.476180	32.114701
620.072505	26755.245563	32.119719
620.864399	26790.502382	32.124736
620.841103	26833.945276	32.129754
622.040561	26869.789391	32.134772
623.021843	26914.427671	32.139789
623.510647	26952.993514	32.144807
624.389590	26983.711695	32.149824
624.673152	27025.337252	32.154842
625.399964	27054.056858	32.159860
625.957438	27096.537152	32.164877
626.712587	27145.964265	32.169895
627.506431	27169.446592	32.174912
627.972614	27206.126666	32.179930
628.851066	27227.794500	32.184948
629.705487	27271.170394	32.189965
630.053433	27308.140947	32.194983
630.823019	27338.800949	32.200000
631.045515	27372.694256	32.205018
632.070346	27403.200613	32.210036
632.578819	27438.698881	32.215053
632.656648	27474.719728	32.220071
633.829577	27507.832366	32.225088
634.038659	27544.553316	32.230106
634.925170	27567.737171	32.235124
635.221078	27607.636490	32.240141
635.414962	27641.319828	32.245159
636.396464	27668.938572	32.250176
637.005701	27710.413399	32.255194
637.725073	27741.890904	32.260212
638.430318	27785.980201	32.265229
638.966415	27806.134770	32.270247
639.719337	27850.260983	32.275264
640.449626	27894.220181	32.280282
641.109533	27910.044813	32.285300
641.683893	27957.858856	32.290317
642.264542	27984.952990	32.295335
642.997819	28019.740758	32.300352
643.167037	28060.760596	32.305370
644.303744	28103.430391	32.310388
645.001886	28139.696582	32.315405
644.985960	28172.256970	32.320423
645.886444	28213.895794	32.325440
646.572451	28265.871059	32.330458
647.309903	28304.988352	32.335476
647.931861	28328.808657	32.340493
648.572925	28382.586346	32.345511
649.902415	28419.803407	32.350528
649.843900	28465.947940	32.355546
650.890736	28493.804085	32.360564
651.275763	28541.364711	32.365581
651.892974	28577.707563	32.370599
652.925487	28610.009643	32.375616
653.530466	28657.965910	32.380634
653.975699	28697.022264	32.385652
654.589002	28736.697100	32.390669
655.318144	28792.497391	32.395687
655.810547	28824.037397	32.400704
656.638825	28862.711714	32.405722
657.129896	28907.639731	32.410740
657.973176	28952.335701	32.415757
658.827043	28994.084553	32.420775
659.810657	29027.368376	32.425792
660.412351	29065.003999	32.430810
661.251661	29096.230937	32.435828
661.888149	29132.672893	32.440845
662.177207	29170.926560	32.445863
663.136904	29200.845321	32.450880
663.523558	29243.919410	32.455898
664.437260	29286.095637	32.460916
665.393813	29320.395541	32.465933
665.614076	29349.836142	32.470951
666.307935	29390.112771	32.475968
667.159151	29425.876872	32.480986
668.100211	29465.893698	32.486004
668.515151	29493.148527	32.491021
669.373175	29531.181019	32.496039
670.077687	29562.398173	32.501056
670.627617	29588.936667	32.506074
671.258259	29627.700271	32.511092
671.967988	29655.572869	32.516109
672.194356	29697.686912	32.521127
672.933415	29729.290822	32.526144
673.957756	29767.234494	32.531162
674.555351	29811.016315	32.536180
674.948578	29840.348356	32.541197
675.340025	29879.029791	32.546215
676.575576	29921.416091	32.551232
677.381238	29959.198407	32.556250
677.886140	29993.083432	32.561268
678.627422	30024.143821	32.566285
679.009019	30064.963732	32.571303
680.154755	30074.569690	32.576320
680.482979	30108.084333	32.581338
680.844727	30144.659609	32.586356
681.628951	30172.186214	32.591373
682.239587	30202.369707	32.596391
683.029679	30238.751643	32.601408
683.352996	30267.728604	32.606426
683.918410	30320.834196	32.611444
684.778670	30356.250827	32.616461
685.423061	30401.056956	32.621479
686.098912	30444.480193	32.626496
686.776196	30480.109012	32.631514
687.070955	30516.689117	32.636532
688.214209	30556.012655	32.641549
688.735172	30609.290306	32.646567
689.329218	30640.968898	32.651584
689.964123	30692.345129	32.656602
690.721695	30745.807329	32.661620
691.551765	30786.349826	32.666637
692.040746	30833.716149	32.671655
692.802452	30865.634332	32.676672
693.645323	30919.829563	32.681690
694.309949	30963.464260	32.686708
695.309192	31005.953017	32.691725
695.876170	31057.720085	32.696743
696.490649	31095.104555	32.701760
697.460240	31145.677230	32.706778
698.025396	31176.444535	32.711796
698.968999	31214.043186	32.716813
699.794053	31258.045321	32.721831
700.795262	31289.155413	32.726848
701.594046	31315.815201	32.731866
702.106789	31357.091249	32.736884
703.342085	31384.043101	32.741901
703.912525	31424.646474	32.746919
704.799451	31450.654142	32.751936
705.559257	31482.187953	32.756954
705.906189	31516.972611	32.761972
706.870915	31544.137731	32.766989
707.442330	31580.240190	32.772007
708.351429	31618.540371	32.777024
708.744696	31644.290538	32.782042
709.610021	31678.166137	32.787060
710.398582	31710.764170	32.792077
710.732155	31756.633392	32.797095
711.711370	31781.887376	32.802112
712.053418	31820.460063	32.807130
712.544780	31867.461710	32.812148
713.472867	31899.785318	32.817165
713.895501	31940.583535	32.822183
714.213748	31992.031541	32.827200
715.242448	32032.640200	32.832218
715.397249	32081.623206	32.837236
716.729581	32122.456334	32.842253
716.906606	32171.809063	32.847271
718.059585	32223.778079	32.852288
718.268196	32270.218008	32.857306
719.219889	32319.715296	32.862324
720.191284	32361.768656	32.867341
720.848977	32405.091370	32.872359
721.168496	32459.808796	32.877376
722.237964	32510.090986	32.882394
722.780553	32554.190676	32.887412
723.570585	32597.897676	32.892429
724.274305	32655.122196	32.897447
725.193339	32689.155405	32.902464
725.936389	32735.493709	32.907482
726.627356	32789.079074	32.912500
726.976432	32817.511859	32.917517
727.821978	32869.454764	32.922535
728.947376	32906.168202	32.927552
729.338318	32949.091268	32.932570
729.852612	32996.426940	32.937588
731.268885	33025.483157	32.942605
731.641759	33072.170997	32.947623
731.795638	33110.807145	32.952640
732.904059	33150.855470	32.957658
733.520926	33195.716191	32.962676
734.737001	33235.570798	32.967693
735.458776	33282.931526	32.972711
736.158105	33317.076032	32.977728
736.981591	33369.257556	32.982746
737.080279	33409.344375	32.987764
738.138528	33444.716307	32.992781
738.936669	33499.785092	32.997799
739.851346	33544.176329	33.002816
740.374189	33587.124302	33.007834
741.377854	33646.776596	33.012852
742.300164	33687.506296	33.017869
742.806318	33729.749070	33.022887
743.529252	33770.352093	33.027904
744.550236	33809.125603	33.032922
745.278318	33863.466592	33.037940
746.116871	33904.039124	33.042957
747.031012	33950.644156	33.047975
747.740533	33982.075819	33.052992
748.346323	34025.599689	33.058010
749.423635	34064.149886	33.063028
750.266061	34092.937073	33.068045
750.999036	34140.968168	33.073063
751.682842	34162.737021	33.078080
752.418679	34216.635133	33.083098
752.932445	34261.937888	33.088116
753.680015	34290.664330	33.093133
754.598456	34346.114815	33.098151
755.279229	34385.340987	33.103168
756.152438	34423.177741	33.108186
756.541040	34469.398349	33.113204
757.589462	34508.984471	33.118221
758.030214	34554.501612	33.123239
758.797783	34608.041688	33.128256
759.779002	34643.724871	33.133274
760.340081	34699.320764	33.138292
761.139544	34738.851464	33.143309
761.887197	34783.562317	33.148327
763.242574	34832.578705	33.153344
763.750597	34875.057423	33.158362
764.192983	34922.269591	33.163380
764.819775	34950.061112	33.168397
766.082360	35010.327969	33.173415
766.905380	35045.688853	33.178432
767.481581	35079.450846	33.183450
768.264938	35139.243033	33.188468
768.994000	35174.005533	33.193485
769.750815	35222.332530	33.198503
770.754217	35275.963826	33.203520
771.186420	35312.688863	33.208538
771.919588	35356.423154	33.213556
773.035605	35398.908881	33.218573
773.807697	35450.819081	33.223591
774.301719	35485.751681	33.228608
775.491919	35532.190523	33.233626
776.157970	35578.920202	33.238644
777.134527	35611.450607	33.243661
777.524693	35653.987282	33.248679
778.384813	35698.688781	33.253696
779.417984	35740.277660	33.258714
779.730736	35767.126724	33.263732
780.283802	35797.687729	33.268749
781.249093	35840.994645	33.273767
781.939782	35874.310012	33.278784
782.978392	35916.429519	33.283802
783.436926	35970.906661	33.288820
783.857902	35996.253151	33.293837
784.933603	36045.720825	33.298855
785.514953	36091.174988	33.303872
786.668721	36127.390089	33.308890
787.108343	36180.669341	33.313908
788.022338	36223.030279	33.318925
789.016437	36262.855827	33.323943
789.515665	36321.993970	33.328960
790.247563	36362.189566	33.333978
790.870172	36424.476580	33.338996
791.592087	36467.272767	33.344013
792.585670	36511.815968	33.349031
793.445819	36565.605743	33.354048
794.310316	36619.287477	33.359066
794.679837	36680.236403	33.364084
795.856813	36723.132573	33.369101
796.614105	36776.300335	33.374119
797.045285	36832.567129	33.379136
797.967747	36879.114076	33.384154
799.453520	36943.942206	33.389172
800.442613	36988.322699	33.394189
801.052124	37034.615470	33.399207
802.034348	37083.739761	33.404224
802.944179	37122.132058	33.409242
803.214917	37169.161095	33.414260
804.001628	37215.894442	33.419277
805.195978	37266.421353	33.424295
805.563080	37319.379658	33.429312
806.922114	37368.142074	33.434330
807.433845	37427.901018	33.439348
808.633982	37473.330787	33.444365
809.528169	37515.400191	33.449383
810.205159	37564.307796	33.454400
811.421591	37598.207502	33.459418
812.202402	37650.589637	33.464436
813.300759	37691.754767	33.469453
813.930541	37715.609860	33.474471
814.727422	37764.834299	33.479488
815.445772	37798.211577	33.484506
816.091403	37842.944836	33.489524
816.938749	37888.873383	33.494541
817.841838	37942.609309	33.499559
818.402925	37989.961449	33.504576
819.314103	38027.103077	33.509594
820.133127	38081.649295	33.514612
820.862400	38122.183766	33.519629
821.474145	38166.499318	33.524647
822.387341	38222.378095	33.529664
823.079513	38265.043413	33.534682
824.352925	38312.803269	33.539700
824.648952	38367.248718	33.544717
825.606295	38418.536367	33.549735
826.278036	38469.476786	33.554752
827.456672	38507.728294	33.559770
827.907868	38567.664304	33.564788
828.918687	38619.740860	33.569805
829.698315	38667.768540	33.574823
830.191108	38722.190396	33.579840
831.188875	38765.637280	33.584858
832.086538	38821.779323	33.589876
832.556369	38866.782545	33.594893
833.184564	38911.318389	33.599911
834.076635	38970.939850	33.604928
835.675529	39001.265780	33.609946
836.404207	39058.130532	33.614964
837.115634	39098.865679	33.619981
837.826068	39141.593112	33.624999
838.465794	39184.129334	33.630016
839.301987	39236.260019	33.635034
840.241130	39284.618238	33.640052
841.024251	39328.327530	33.645069
841.944281	39378.023323	33.650087
842.762463	39437.025234	33.655104
843.617835	39474.437384	33.660122
844.665361	39527.509587	33.665140
845.390085	39565.745513	33.670157
846.669824	39616.599757	33.675175
847.283826	39670.733082	33.680192
848.293907	39711.618666	33.685210
849.247958	39753.423780	33.690228
850.486881	39801.420004	33.695245
851.426076	39842.487688	33.700263
851.816054	39884.216951	33.705280
852.766578	39926.674345	33.710298
853.277731	39981.836424	33.715316
854.364348	40034.511647	33.720333
855.683747	40079.125064	33.725351
856.313259	40125.901986	33.730368
857.085212	40163.328389	33.735386
857.958957	40202.319990	33.740404
858.962206	40247.969849	33.745421
859.816539	40285.459455	33.750439
860.170332	40342.512763	33.755456
861.012749	40387.966748	33.760474
862.232626	40447.597860	33.765492
863.132007	40494.162560	33.770509
863.960068	40545.178249	33.775527
864.664659	40603.227159	33.780544
866.046690	40640.318527	33.785562
866.317484	40696.867156	33.790580
867.113067	40736.472775	33.795597
868.755406	40792.478019	33.800615
869.572185	40845.077293	33.805632
870.122216	40885.670305	33.810650
870.928715	40940.813864	33.815668
871.752575	40988.713268	33.820685
872.853709	41037.031051	33.825703
873.516459	41080.111290	33.830720
874.173090	41131.572614	33.835738
875.260290	41190.189306	33.840756
876.370618	41230.031145	33.845773
877.084918	41273.476844	33.850791
877.824600	41339.560787	33.855808
878.974626	41382.445155	33.860826
880.058939	41423.284387	33.865844
880.928205	41481.316170	33.870861
882.206828	41521.574915	33.875879
882.610943	41582.804190	33.880896
882.995155	41605.291620	33.885914
883.981145	41665.550881	33.890932
884.870599	41709.855481	33.895949
885.874001	41762.781925	33.900967
886.972815	41815.472191	33.905984
887.472718	41866.283032	33.911002
888.446510	41913.212268	33.916020
888.913103	41968.411639	33.921037
890.417783	42018.957983	33.926055
891.063177	42071.979180	33.931072
891.851915	42120.329297	33.936090
892.984591	42164.603056	33.941108
893.582988	42210.333060	33.946125
894.733817	42252.662420	33.951143
895.065890	42299.205945	33.956160
895.735127	42340.630523	33.961178
897.049999	42388.860900	33.966196
897.901240	42430.731518	33.971213
898.988273	42484.804072	33.976231
899.658373	42532.256554	33.981248
900.696506	42581.125231	33.986266
901.441416	42633.936125	33.991284
902.202545	42678.781422	33.996301
903.467421	42740.808916	34.001319
903.904735	42796.261622	34.006336
904.758408	42835.906217	34.011354
905.742076	42892.880180	34.016372
906.747704	42953.595302	34.021389
907.643611	43009.248715	34.026407
908.415954	43069.494674	34.031424
909.586925	43119.798524	34.036442
910.598402	43174.864996	34.041460
911.592153	43237.062841	34.046477
912.719998	43284.793152	34.051495
913.278861	43337.596908	34.056512
914.304032	43394.078626	34.061530
915.399703	43451.669014	34.066548
915.803925	43514.548193	34.071565
917.412900	43569.433539	34.076583
918.152499	43624.410870	34.081600
919.408296	43667.890365	34.086618
920.722225	43722.626206	34.091636
921.086402	43784.051274	34.096653
922.129976	43823.130253	34.101671
923.561661	43883.667361	34.106688
924.284134	43919.710018	34.111706
924.909010	43981.373128	34.116724
925.423676	44034.204439	34.121741
926.591086	44086.256852	34.126759
927.481760	44142.691958	34.131776
928.833038	44201.408150	34.136794
929.474330	44249.589925	34.141812
930.272990	44302.889769	34.146829
931.664308	44346.823788	34.151847
932.602616	44402.062903	34.156864
933.602431	44451.934817	34.161882
934.880078	44501.288927	34.166900
935.476543	44549.003955	34.171917
936.456528	44601.213432	34.176935
937.358212	44654.611848	34.181952
938.230067	44695.117202	34.186970
939.315700	44751.162767	34.191988
940.083662	44818.713897	34.197005
941.074635	44855.007009	34.202023
942.336501	44907.685445	34.207040
943.105546	44954.204075	34.212058
944.430544	45007.309331	34.217076
944.730110	45052.497376	34.222093
945.803388	45093.825884	34.227111
946.716920	45159.255122	34.232128
947.466279	45207.396743	34.237146
948.694275	45262.206763	34.242164
949.779428	45311.175309	34.247181
950.481758	45357.648293	34.252199
951.439996	45419.585796	34.257216
952.204343	45461.406160	34.262234
953.242558	45509.395666	34.267252
953.798520	45570.390768	34.272269
954.764090	45622.851599	34.277287
955.864529	45673.950354	34.282304
956.461647	45731.656332	34.287322
957.502694	45774.458748	34.292340
958.456830	45834.367431	34.297357
959.257693	45879.212964	34.302375
960.468389	45929.700404	34.307392
960.864842	45980.410336	34.312410
961.941927	46031.912099	34.317428
963.227413	46092.161798	34.322445
963.764228	46149.429147	34.327463
965.067529	46199.839435	34.332480
965.916563	46254.034336	34.337498
966.668587	46315.892732	34.342516
967.629514	46373.903980	34.347533
968.765936	46428.762822	34.352551
969.641877	46491.443665	34.357568
970.691781	46562.194857	34.362586
971.824728	46609.868231	34.367604
972.542599	46685.542909	34.372621
973.610158	46745.923374	34.377639
974.738223	46806.402072	34.382656
975.840896	46867.865467	34.387674
976.952640	46923.222820	34.392692
977.939864	46976.841116	34.397709
979.116854	47030.992863	34.402727
980.446151	47091.459797	34.407744
980.934645	47149.274980	34.412762
981.827749	47206.084344	34.417780
983.086795	47273.104143	34.422797
984.119750	47326.798351	34.427815
985.004923	47391.770375	34.432832
985.988294	47451.033493	34.437850
986.874848	47511.115373	34.442868
987.970016	47569.690701	34.447885
989.047077	47615.964167	34.452903
990.109713	47675.639330	34.457920
991.238495	47731.445170	34.462938
992.394224	47784.475946	34.467956
993.216328	47845.536749	34.472973
994.306886	47901.380625	34.477991
995.275524	47957.136178	34.483008
996.438545	48005.940232	34.488026
998.079193	48060.249602	34.493044
998.854309	48108.393388	34.498061
1000.016585	48155.293594	34.503079
1001.326143	48198.836739	34.508096
1001.828192	48249.838899	34.513114
1003.052233	48293.933375	34.518132
1003.754355	48350.237747	34.523149
1004.801457	48403.780453	34.528167
1006.042284	48459.437683	34.533184
1006.704734	48502.336185	34.538202
1007.927684	48546.956434	34.543220
1008.638169	48607.619201	34.548237
1009.547614	48657.350093	34.553255
1010.915348	48707.509148	34.558272
1011.539703	48762.637296	34.563290
1012.786584	48821.305979	34.568308
1013.820298	48880.248606	34.573325
1014.500372	48925.751766	34.578343
1015.813382	48981.057324	34.583360
1016.892562	49029.421175	34.588378
1017.857245	49081.719347	34.593396
1018.333865	49138.567116	34.598413
1019.800727	49188.180257	34.603431
1020.848293	49243.546991	34.608448
1021.672696	49298.537554	34.613466
1023.032192	49346.446942	34.618484
1023.440210	49400.927197	34.623501
1024.332541	49452.813644	34.628519
1025.684517	49491.746634	34.633536
1026.225035	49550.989651	34.638554
1027.383456	49593.046989	34.643572
1028.167938	49654.485489	34.648589
1028.891217	49700.021386	34.653607
1029.768829	49754.334052	34.658624
1030.996704	49810.876056	34.663642
1031.985630	49873.251164	34.668660
1032.995961	49935.351027	34.673677
1034.125819	49998.533252	34.678695
1035.336444	50061.279092	34.683712
1036.227200	50124.587677	34.688730
1036.985636	50178.053193	34.693748
1038.094560	50250.932519	34.698765
1039.499003	50318.292826	34.703783
1040.743267	50383.419612	34.708800
1041.506632	50449.830366	34.713818
1042.825254	50499.868171	34.718836
1043.695761	50571.526728	34.723853
1044.929155	50627.519410	34.728871
1045.713339	50688.840500	34.733888
1046.923467	50749.721756	34.738906
1048.077886	50803.468398	34.743924
1049.048840	50869.746623	34.748941
1050.342819	50936.955197	34.753959
1051.072479	50991.806459	34.758976
1052.315970	51059.921776	34.763994
1053.721855	51123.316964	34.769012
1054.494127	51181.471216	34.774029
1055.767127	51249.468579	34.779047
1056.991084	51307.305662	34.784064
1057.891591	51372.368838	34.789082
1059.363449	51430.635647	34.794100
1060.246028	51488.184947	34.799117
1061.299001	51549.080259	34.804135
1062.701574	51596.462413	34.809152
1063.669157	51655.023873	34.814170
1065.024317	51707.045415	34.819188
1065.730752	51763.351143	34.824205
1066.998890	51823.606046	34.829223
1068.292612	51878.681147	34.834240
1069.245265	51936.657191	34.839258
1069.783766	51990.737141	34.844276
1071.313286	52047.718300	34.849293
1072.456604	52109.353924	34.854311
1073.605002	52159.985136	34.859328
1074.488012	52209.500046	34.864346
1075.841353	52267.888759	34.869364
1076.838554	52320.195515	34.874381
1077.915324	52374.926098	34.879399
1078.802018	52434.299476	34.884416
1079.945010	52493.240560	34.889434
1081.479698	52543.483087	34.894452
1082.658033	52598.369143	34.899469
1083.331578	52646.683863	34.904487
1084.349377	52689.667407	34.909504
1085.335612	52757.979851	34.914522
1086.548207	52814.000057	34.919540
1087.773603	52872.789988	34.924557
1088.618346	52922.059289	34.929575
1090.220435	52972.127665	34.934592
1090.889605	53033.972854	34.939610
1091.829793	53079.291601	34.944628
1092.871079	53140.705468	34.949645
1093.915581	53193.550978	34.954663
1095.246111	53238.106521	34.959680
1095.697676	53291.753812	34.964698
1096.881994	53335.705965	34.969716
1098.062868	53385.271656	34.974733
1098.849595	53437.651837	34.979751
1100.259368	53480.632423	34.984768
1101.138064	53533.435051	34.989786
1102.132977	53583.707374	34.994804
1103.219764	53649.197031	34.999821
1103.776511	53704.796822	35.004839
1105.422609	53765.073506	35.009856
1106.227738	53816.806188	35.014874
1107.405206	53871.581464	35.019892
1108.408111	53929.567243	35.024909
1109.689508	53997.818107	35.029927
1111.135962	54054.829830	35.034944
1111.938154	54129.674105	35.039962
1113.307088	54181.040880	35.044980
1114.581432	54244.553750	35.049997
1115.488463	54307.428191	35.055015
1116.565544	54361.112885	35.060032
1117.690853	54433.952113	35.065050
1119.171496	54500.489925	35.070068
1120.552538	54554.386931	35.075085
1121.282695	54605.348374	35.080103
1122.402369	54678.771444	35.085120
1123.745605	54733.117761	35.090138
1124.857650	54794.752692	35.095156
1126.064109	54863.112721	35.100173
1126.794570	54922.535839	35.105191
1128.149770	54976.222689	35.110208
1129.685542	55034.520125	35.115226
1130.381540	55094.132593	35.120244
1132.099655	55157.382264	35.125261
1133.086549	55220.575712	35.130279
1134.499166	55276.848930	35.135296
1135.367582	55339.782792	35.140314
1136.269318	55399.692901	35.145332
1137.657513	55458.868836	35.150349
1139.074263	55523.274160	35.155367
1140.161584	55577.371369	35.160384
1141.184758	55639.864113	35.165402
1142.076030	55691.960802	35.170420
1143.606345	55757.095755	35.175437
1144.483590	55823.086236	35.180455
1145.664472	55871.929364	35.185472
1146.712308	55935.874614	35.190490
1147.893747	55996.096843	35.195508
1148.961564	56053.197982	35.200525
1150.198475	56120.702496	35.205543
1151.514329	56176.904397	35.210560
1152.570528	56240.089707	35.215578
1154.071656	56301.439807	35.220596
1155.081455	56356.873637	35.225613
1156.201135	56430.251495	35.230631
1157.692326	56459.953298	35.235648
1158.633605	56536.840253	35.240666
1160.079307	56589.643211	35.245684
1161.651166	56645.907402	35.250701
1162.692027	56703.343419	35.255719
1163.990910	56748.094086	35.260736
1165.172838	56806.261403	35.265754
1166.055454	56854.830469	35.270772
1167.288439	56909.774963	35.275789
1168.063121	56961.025617	35.280807
1169.384888	57013.380575	35.285824
1170.184710	57062.083274	35.290842
1171.343044	57113.350140	35.295860
1172.681311	57168.861012	35.300877
1173.446713	57223.240199	35.305895
1174.330115	57273.322623	35.310912
1175.366410	57320.254677	35.315930
1176.547127	57377.543837	35.320948
1178.201338	57428.423626	35.325965
1178.736929	57492.820320	35.330983
1180.255311	57540.702645	35.336000
1181.279346	57594.592819	35.341018
1182.234604	57646.766034	35.346036
1183.890123	57711.462673	35.351053
1184.787244	57773.752884	35.356071
1185.777032	57833.851519	35.361088
1186.502318	57896.776549	35.366106
1188.037826	57965.555991	35.371124
1189.161720	58033.900061	35.376141
1190.612296	58095.895598	35.381159
1191.549456	58156.414676	35.386176
1193.003764	58223.878427	35.391194
1194.208958	58290.039559	35.396212
1195.552353	58357.533706	35.401229
1196.703459	58417.545249	35.406247
1198.057965	58485.208905	35.411264
1199.177133	58550.656345	35.416282
1200.176481	58612.420042	35.421300
1202.013867	58672.248830	35.426317
1203.055249	58744.126962	35.431335
1204.667264	58805.902841	35.436352
1205.369516	58875.055840	35.441370
1206.785448	58937.793179	35.446388
1207.940584	58992.457135	35.451405
1209.257969	59054.551940	35.456423
1210.269300	59130.290576	35.461440
1211.415202	59186.697028	35.466458
1212.789189	59248.283437	35.471476
1214.378459	59310.564198	35.476493
1215.423168	59382.804488	35.481511
1216.751630	59442.626239	35.486528
1218.494117	59503.383400	35.491546
1219.655276	59562.908830	35.496564
1221.017418	59628.093277	35.501581
1222.188997	59689.168143	35.506599
1223.596322	59733.679522	35.511616
1224.969113	59783.209485	35.516634
1225.793798	59857.036397	35.521652
1227.074188	59903.498513	35.526669
1228.053138	59963.781363	35.531687
1229.077511	60027.823441	35.536704
1230.836471	60087.243911	35.541722
1231.875461	60150.891581	35.546740
1233.249281	60208.802858	35.551757
1234.200471	60268.337563	35.556775
1235.991181	60323.259486	35.561792
1237.145852	60376.622688	35.566810
1238.435429	60438.832990	35.571828
1239.448214	60490.041188	35.576845
1240.524041	60559.659536	35.581863
1241.713374	60606.536030	35.586880
1243.263031	60660.793832	35.591898
1244.325413	60728.104353	35.596916
1245.793999	60777.266867	35.601933
1246.939849	60836.778813	35.606951
1247.970374	60895.169566	35.611968
1249.538991	60956.331039	35.616986
1250.663235	61010.073856	35.622004
1252.135951	61061.825260	35.627021
1253.335121	61123.139934	35.632039
1254.805052	61174.050120	35.637056
1256.205169	61217.103101	35.642074
1256.721573	61270.004795	35.647092
1257.986838	61301.108909	35.652109
1258.823882	61350.073925	35.657127
1260.451198	61410.125911	35.662144
1261.547727	61457.499649	35.667162
1262.342526	61513.573977	35.672180
1263.362351	61559.554634	35.677197
1264.425484	61622.145216	35.682215
1265.549613	61686.612795	35.687232
1266.886594	61747.287099	35.692250
1268.136489	61817.432491	35.697268
1269.544511	61880.995231	35.702285
1271.103843	61950.320276	35.707303
1272.248867	62010.923995	35.712320
1273.827770	62078.999280	35.717338
1274.843723	62141.016181	35.722356
1276.252235	62206.706657	35.727373
1277.810508	62267.505858	35.732391
1279.071900	62331.143355	35.737408
1280.527868	62396.174884	35.742426
1281.792985	62456.697594	35.747444
1282.889502	62514.657723	35.752461
1284.303245	62576.024720	35.757479
1285.708798	62640.026599	35.762496
1287.306301	62704.239151	35.767514
1288.787869	62764.215967	35.772532
1290.213876	62815.332668	35.777549
1291.741772	62871.301649	35.782567
1292.683383	62931.217793	35.787584
1294.103449	62985.671937	35.792602
1295.625692	63046.124185	35.797620
1296.885800	63088.904825	35.802637
1298.001329	63155.036174	35.807655
1299.170781	63220.437576	35.812672
1300.526884	63265.267251	35.817690
1301.279035	63342.869987	35.822708
1303.025379	63393.982051	35.827725
1304.198385	63459.649410	35.832743
1305.630707	63519.869995	35.837760
1307.103028	63586.142888	35.842778
1308.142828	63647.273531	35.847796
1309.713957	63715.563443	35.852813
1311.057945	63785.630039	35.857831
1312.165620	63840.103303	35.862848
1313.360561	63905.027709	35.867866
1314.657422	63974.760354	35.872884
1316.255147	64034.272570	35.877901
1317.329249	64101.318213	35.882919
1318.658408	64171.464182	35.887936
1320.266120	64231.285514	35.892954
1321.077340	64306.628229	35.897972
1322.852195	64363.878723	35.902989
1324.217951	64428.448546	35.908007
1325.422154	64489.194655	35.913024
1326.633393	64551.801090	35.918042
1328.036785	64626.760850	35.923060
1329.404734	64684.436635	35.928077
1330.621766	64752.715170	35.933095
1331.997033	64821.602216	35.938112
1333.430500	64882.952818	35.943130
1335.133830	64948.819635	35.948148
1336.712643	65003.468591	35.953165
1337.809630	65059.820158	35.958183
1339.120115	65120.272594	35.963200
1340.380461	65178.624785	35.968218
1341.775276	65246.845178	35.973236
1343.099840	65298.122132	35.978253
1344.365468	65363.602716	35.983271
1345.167797	65410.897088	35.988288
1346.800080	65472.350960	35.993306
1347.627794	65515.361720	35.998324
1348.887730	65573.784534	36.003341
1350.252825	65619.389426	36.008359
1351.573845	65692.928087	36.013376
1352.675931	65743.120155	36.018394
1354.310799	65801.250553	36.023412
1355.514880	65864.766738	36.028429
1356.731402	65939.126537	36.033447
1358.093879	65999.110762	36.038464
1359.540341	66050.775366	36.043482
1361.049007	66127.787107	36.048500
1362.573824	66181.984890	36.053517
1363.627937	66252.952134	36.058535
1365.121535	66320.146955	36.063552
1366.772385	66371.045787	36.068570
1367.637870	66450.989298	36.073588
1369.377830	66516.050395	36.078605
1370.966588	66578.469811	36.083623
1372.138768	66654.788719	36.088640
1374.263605	66709.653480	36.093658
1375.230821	66779.838039	36.098676
1376.907326	66845.004885	36.103693
1378.193506	66908.118283	36.108711
1379.665624	66975.894367	36.113728
1381.228062	67039.053489	36.118746
1382.837528	67101.990134	36.123764
1384.032990	67161.579040	36.128781
1385.165606	67222.083335	36.133799
1386.371163	67288.623003	36.138816
1388.408291	67348.371853	36.143834
1389.255297	67404.793095	36.148852
1390.835265	67480.379496	36.153869
1392.547687	67544.554780	36.158887
1393.531258	67610.186621	36.163904
1394.866138	67675.098815	36.168922
1396.278290	67752.029275	36.173940
1397.923686	67814.791100	36.178957
1399.314556	67878.384385	36.183975
1400.466192	67947.074328	36.188992
1402.064957	68010.641732	36.194010
1403.352683	68081.754788	36.199028
1405.224926	68147.559160	36.204045
1406.435008	68201.854835	36.209063
1407.588283	68277.250777	36.214080
1409.017787	68339.458824	36.219098
1410.114717	68420.841252	36.224116
1411.274662	68485.523276	36.229133
1413.135170	68561.176597	36.234151
1414.584851	68634.760596	36.239168
1416.162820	68696.249759	36.244186
1417.569109	68773.595773	36.249204
1419.183282	68843.640399	36.254221
1420.533439	68911.921930	36.259239
1421.994246	68982.731780	36.264256
1423.597224	69045.541249	36.269274
1424.916523	69117.063805	36.274292
1426.363665	69181.265713	36.279309
1428.089961	69243.708101	36.284327
1429.426438	69319.243049	36.289344
1430.972055	69368.201390	36.294362
1432.509678	69436.182686	36.299380
1434.213736	69491.986787	36.304397
1435.430518	69554.332380	36.309415
1436.718209	69614.767381	36.314432
1438.412422	69668.382485	36.319450
1439.359171	69730.644126	36.324468
1440.428918	69769.457596	36.329485
1442.084785	69820.628465	36.334503
1443.326623	69875.144323	36.339520
1444.792269	69931.018351	36.344538
1446.076376	69981.956448	36.349556
1447.135153	70041.060513	36.354573
1448.728094	70108.857615	36.359591
1449.788954	70178.029961	36.364608
1451.620024	70226.337350	36.369626
1453.018908	70289.302101	36.374644
1454.547440	70362.036478	36.379661
1455.940945	70423.748597	36.384679
1457.487531	70496.581842	36.389696
1458.995922	70557.579737	36.394714
1460.164055	70625.406685	36.399732
1461.512261	70693.851528	36.404749
1463.091699	70770.378520	36.409767
1464.483921	70838.652211	36.414784
1465.901061	70899.728514	36.419802
1467.687804	70980.162459	36.424820
1468.922861	71053.299320	36.429837
1470.645899	71128.171102	36.434855
1472.275301	71209.098984	36.439872
1473.301700	71275.556648	36.444890
1475.499256	71340.855956	36.449908
1476.610932	71419.332501	36.454925
1477.981552	71481.493983	36.459943
1479.348626	71565.832967	36.464960
1480.950900	71638.306053	36.469978
1482.572936	71713.904574	36.474996
1484.375088	71799.556728	36.480013
1485.894917	71863.063617	36.485031
1487.355369	71934.267851	36.490048
1488.849132	72012.065758	36.495066
1490.596741	72089.380870	36.500084
1492.025015	72166.024258	36.505101
1494.102505	72233.345736	36.510119
1495.255890	72309.994572	36.515136
1496.818512	72387.972795	36.520154
1498.100043	72450.340498	36.525172
1499.528461	72519.917462	36.530189
1500.985531	72589.908093	36.535207
1502.254106	72668.769107	36.540224
1504.022650	72732.441817	36.545242
1505.893999	72813.577420	36.550260
1507.215344	72882.982112	36.555277
1509.255718	72950.792536	36.560295
1510.390036	73021.835433	36.565312
1511.970403	73085.234465	36.570330
1513.294423	73163.581637	36.575348
1514.778143	73232.581851	36.580365
1516.629968	73302.588579	36.585383
1517.832705	73373.811701	36.590400
1519.727921	73441.063462	36.595418
1521.522129	73516.158887	36.600436
1522.816075	73584.594411	36.605453
1524.564656	73649.805063	36.610471
1525.926551	73716.305025	36.615488
1527.676901	73784.922955	36.620506
1528.994845	73850.657489	36.625524
1530.362807	73923.604175	36.630541
1531.943593	73983.471378	36.635559
1533.153764	74057.671766	36.640576
1534.882245	74117.617485	36.645594
1536.516998	74184.177242	36.650612
1537.671366	74265.391502	36.655629
1539.293411	74329.850970	36.660647
1540.804718	74400.483880	36.665664
1542.048069	74460.113636	36.670682
1543.759900	74516.908876	36.675700
1545.155984	74576.451653	36.680717
1546.634609	74636.741646	36.685735
1548.022055	74701.112061	36.690752
1549.604040	74764.033508	36.695770
1550.701251	74829.222329	36.700788
1551.967581	74898.577552	36.705805
1553.779436	74968.683585	36.710823
1555.202106	75038.939382	36.715840
1556.668594	75121.931419	36.720858
1558.144017	75183.629172	36.725876
1559.472769	75268.213918	36.730893
1561.398958	75341.077100	36.735911
1562.905931	75428.902549	36.740928
1564.389711	75507.142921	36.745946
1566.167424	75585.464187	36.750964
1567.705770	75670.055394	36.755981
1569.686846	75742.708398	36.760999
1571.588550	75833.728859	36.766016
1573.061481	75901.496261	36.771034
1574.503990	75974.994221	36.776052
1575.868479	76061.982654	36.781069
1577.690625	76130.899375	36.786087
1579.296002	76220.738782	36.791104
1581.170259	76289.736424	36.796122
1582.961964	76374.834885	36.801140
1584.218011	76454.836426	36.806157
1586.353271	76527.011379	36.811175
1587.512189	76610.486828	36.816192
1589.208695	76687.949936	36.821210
1591.341347	76752.956013	36.826228
1592.443695	76831.601942	36.831245
1594.080709	76912.685302	36.836263
1595.895204	76983.024178	36.841280
1597.485023	77067.231660	36.846298
1599.426373	77138.083132	36.851316
1600.742257	77225.272919	36.856333
1602.745044	77285.322114	36.861351
1604.173851	77364.691233	36.866368
1606.196389	77427.955315	36.871386
1607.644513	77505.788995	36.876404
1608.762468	77577.530561	36.881421
1610.499534	77656.092199	36.886439
1612.501287	77738.653772	36.891456
1613.762012	77812.261161	36.896474
1615.760343	77879.330531	36.901492
1617.363011	77953.239493	36.906509
1618.780150	78026.860985	36.911527
1620.089198	78102.564524	36.916544
1621.756607	78178.896277	36.921562
1623.598526	78262.966643	36.926580
1625.122484	78340.613471	36.931597
1627.033550	78410.104798	36.936615
1628.473799	78494.948172	36.941632
1630.104968	78559.023567	36.946650
1631.930433	78645.998771	36.951668
1633.205560	78725.953302	36.956685
1634.901573	78791.399967	36.961703
1636.605948	78869.020051	36.966720
1638.316687	78946.436660	36.971738
1639.922179	79020.234034	36.976756
1641.648066	79099.295636	36.981773
1643.182345	79172.521800	36.986791
1644.837572	79250.771423	36.991808
1646.305255	79324.527834	36.996826
1648.060918	79398.011333	37.001844
1649.554156	79468.533561	37.006861
1651.142216	79534.721015	37.011879
1652.668443	79603.084701	37.016896
1654.453919	79662.298959	37.021914
1655.682488	79721.043064	37.026932
1657.306972	79787.732184	37.031949
1658.813038	79862.472211	37.036967
1660.359560	79933.886793	37.041984
1661.815379	80004.023498	37.047002
1663.508861	80077.607217	37.052020
1664.975657	80158.156682	37.057037
1666.994815	80238.037148	37.062055
1668.945139	80310.833801	37.067072
1670.076010	80393.210223	37.072090
1671.782092	80469.314208	37.077108
1673.702830	80554.836193	37.082125
1675.543200	80631.768456	37.087143
1677.236838	80711.739235	37.092160
1679.108393	80791.872442	37.097178
1680.463846	80863.053251	37.102196
1682.176555	80948.494975	37.107213
1684.005436	81027.875361	37.112231
1686.424099	81117.628823	37.117248
1687.574208	81206.554855	37.122266
1689.457678	81274.689364	37.127284
1691.517397	81360.141387	37.132301
1692.847253	81437.003726	37.137319
1694.711613	81512.426952	37.142336
1696.330436	81598.404815	37.147354
1698.488454	81673.161692	37.152372
1700.125468	81756.869277	37.157389
1701.919308	81832.963240	37.162407
1703.709342	81913.682565	37.167424
1705.185296	81991.600510	37.172442
1706.938802	82066.561111	37.177460
1709.250498	82152.280194	37.182477
1710.328270	82233.998815	37.187495
1711.937569	82309.970905	37.192512
1713.346269	82390.624573	37.197530
1715.601346	82466.458012	37.202548
1717.058774	82561.345941	37.207565
1719.230278	82640.613914	37.212583
1721.142801	82729.260721	37.217600
1723.069849	82806.134699	37.222618
1724.420910	82873.342769	37.227636
1726.050150	82959.234457	37.232653
1727.602521	83038.537085	37.237671
1729.568231	83127.873696	37.242688
1731.218794	83207.414841	37.247706
1732.846097	83288.670386	37.252724
1734.670355	83376.078635	37.257741
1736.337477	83464.398694	37.262759
1737.967956	83530.335531	37.267776
1739.739260	83624.595039	37.272794
1741.317255	83716.667713	37.277812
1743.301836	83807.764753	37.282829
1745.157061	83884.298106	37.287847
1747.034770	83966.340007	37.292864
1748.537947	84049.086976	37.297882
1750.309258	84128.434403	37.302900
1752.397712	84215.018277	37.307917
1754.016206	84303.031766	37.312935
1756.024273	84382.330176	37.317952
1757.674377	84466.246445	37.322970
1759.669714	84534.003836	37.327988
1761.335110	84618.006855	37.333005
1762.891463	84691.624072	37.338023
1764.652610	84770.430005	37.343040
1766.377460	84851.586032	37.348058
1768.108010	84908.437714	37.353076
1769.555994	84982.465448	37.358093
1770.875548	85044.336232	37.363111
1772.398577	85116.629254	37.368128
1773.849098	85193.406839	37.373146
1775.706798	85262.974172	37.378164
1777.430562	85340.457009	37.383181
1778.917886	85436.401545	37.388199
1781.020392	85522.645032	37.393216
1782.688897	85610.705384	37.398234
1784.471034	85682.807217	37.403252
1786.115155	85773.127443	37.408269
1788.104344	85872.720382	37.413287
1789.775222	85958.310423	37.418304
1791.566674	86043.387645	37.423322
1793.413810	86133.119661	37.428340
1795.220008	86222.402172	37.433357
1796.884291	86316.991379	37.438375
1798.981384	86414.871249	37.443392
1800.725907	86518.939900	37.448410
1802.621942	86610.224402	37.453428
1804.624784	86707.423040	37.458445
1806.681156	86796.782214	37.463463
1808.785690	86881.711520	37.468480
1810.492577	86973.685716	37.473498
1812.284275	87067.268984	37.478516
1814.103424	87156.438281	37.483533
1816.265277	87259.278412	37.488551
1817.878504	87345.502499	37.493568
1819.755864	87435.651988	37.498586
1821.323031	87528.232725	37.503604
1823.250285	87624.749256	37.508621
1824.852448	87719.416089	37.513639
1827.125865	87809.390696	37.518656
1828.702386	87911.412282	37.523674
1830.796141	87997.664472	37.528692
1832.639351	88099.429541	37.533709
1834.245495	88191.461340	37.538727
1836.418072	88284.938200	37.543744
1838.363605	88380.985458	37.548762
1840.146275	88478.465208	37.553780
1842.063229	88569.207604	37.558797
1843.933531	88666.598224	37.563815
1845.588712	88763.389176	37.568832
1847.399901	88859.167533	37.573850
1849.552961	88963.066860	37.578868
1851.404363	89053.973078	37.583885
1853.166919	89149.215037	37.588903
1855.165338	89236.436256	37.593920
1856.944117	89347.606569	37.598938
1858.771467	89433.270976	37.603956
1860.914534	89531.952454	37.608973
1862.663906	89621.811814	37.613991
1864.763964	89706.521850	37.619008
1866.270517	89805.443246	37.624026
1868.396368	89910.680860	37.629044
1869.879492	90004.321725	37.634061
1871.919457	90097.216720	37.639079
1873.786056	90185.323152	37.644096
1875.369410	90285.640893	37.649114
1877.647379	90379.741544	37.654132
1879.707012	90481.341499	37.659149
1881.068610	90582.670814	37.664167
1883.043633	90676.262155	37.669184
1885.255432	90767.421374	37.674202
1886.848540	90866.966426	37.679220
1888.885786	90962.627446	37.684237
1890.708282	91040.464713	37.689255
1892.268797	91128.925989	37.694272
1894.198731	91212.399507	37.699290
1895.668997	91286.414263	37.704308
1897.716877	91371.339961	37.709325
1899.445707	91459.357624	37.714343
1900.942233	91540.466430	37.719360
1902.667058	91633.529560	37.724378
1904.172173	91735.043079	37.729396
1906.163213	91843.223645	37.734413
1908.053622	91947.339195	37.739431
1910.094230	92042.749626	37.744448
1911.531043	92143.349969	37.749466
1913.327313	92257.658903	37.754484
1915.466696	92351.939494	37.759501
1917.394853	92476.089406	37.764519
1919.573559	92581.987161	37.769536
1921.417233	92694.832736	37.774554
1923.243034	92807.643501	37.779572
1925.335070	92912.694085	37.784589
1927.242876	93035.886177	37.789607
1929.799917	93144.743294	37.794624
1931.299925	93246.528824	37.799642
1933.579282	93369.334572	37.804660
1935.699848	93482.266476	37.809677
1937.522291	93596.880527	37.814695
1939.804198	93707.392428	37.819712
1941.543616	93827.179095	37.824730
1943.648489	93930.241162	37.829748
1945.219626	94035.833410	37.834765
1947.427662	94170.416141	37.839783
1949.303715	94278.141657	37.844800
1951.335329	94390.228890	37.849818
1953.625162	94502.035291	37.854836
1955.714143	94614.266465	37.859853
1957.272353	94741.157947	37.864871
1959.409118	94853.268431	37.869888
1961.601725	94971.125312	37.874906
1963.277790	95085.514280	37.879924
1965.403942	95203.014846	37.884941
1967.250165	95317.656908	37.889959
1969.433783	95438.128173	37.894976
1971.544444	95557.825418	37.899994
1973.227317	95675.599941	37.905012
1975.454903	95785.088337	37.910029
1977.077285	95909.540757	37.915047
1979.337030	96017.377056	37.920064
1981.282413	96147.167198	37.925082
1983.663070	96264.467149	37.930100
1985.689365	96370.629914	37.935117
1987.498613	96489.680697	37.940135
1989.687204	96616.620603	37.945152
1991.408669	96738.233995	37.950170
1992.991063	96855.306121	37.955188
1995.081794	96967.456747	37.960205
1996.926221	97090.560752	37.965223
1999.260847	97204.905120	37.970240
2001.299007	97337.297017	37.975258
2002.791208	97470.028426	37.980276
2004.856848	97586.381139	37.985293
2006.289837	97713.278886	37.990311
2008.789845	97837.652304	37.995328
2010.897989	97975.309452	38.000346
2012.432943	98099.948990	38.005364
2014.936301	98228.570169	38.010381
2016.468041	98367.472801	38.015399
2018.491896	98493.000829	38.020416
2020.912432	98619.925146	38.025434
2022.633432	98744.740925	38.030452
2024.959562	98856.823362	38.035469
2026.571429	98974.633959	38.040487
2028.602165	99074.086158	38.045504
2030.354102	99201.054008	38.050522
2031.815977	99317.608925	38.055540
2034.045797	99431.711464	38.060557
2036.109717	99552.584768	38.065575
2037.896031	99680.005518	38.070592
2039.781951	99824.538559	38.075610
2041.340119	99949.397171	38.080628
2043.239340	100083.368847	38.085645
2045.112232	100222.543057	38.090663
2047.388866	100364.202925	38.095680
2049.507691	100511.542412	38.100698
2051.473559	100669.099518	38.105716
2053.764400	100810.987314	38.110733
2055.708833	100966.165760	38.115751
2057.611296	101117.243819	38.120768
2060.057541	101261.061681	38.125786
2062.138382	101416.423774	38.130804
2064.384388	101560.147502	38.135821
2066.160262	101718.462059	38.140839
2068.524607	101872.577520	38.145856
2070.471761	102026.061667	38.150874
2072.661180	102188.586409	38.155892
2074.895035	102331.808278	38.160909
2076.708965	102496.244353	38.165927
2078.812666	102646.828858	38.170944
2081.135027	102810.946054	38.175962
2083.255053	102977.339865	38.180980
2085.392764	103130.431647	38.185997
2087.676857	103297.397299	38.191015
2089.644108	103451.227248	38.196032
2091.702201	103602.190917	38.201050
2093.526841	103767.975595	38.206068
2095.958548	103925.779691	38.211085
2098.111800	104090.386111	38.216103
2100.312801	104258.434629	38.221120
2102.434703	104419.332549	38.226138
2104.191864	104585.106473	38.231156
2106.791472	104742.926188	38.236173
2108.809496	104918.677704	38.241191
2111.239089	105076.335391	38.246208
2113.358787	105234.967915	38.251226
2115.382318	105393.793746	38.256244
2117.668317	105560.237824	38.261261
2119.600305	105725.596926	38.266279
2121.981669	105893.600018	38.271296
2123.903413	106057.073036	38.276314
2125.899243	106223.578447	38.281332
2128.077994	106376.285512	38.286349
2130.106242	106556.646778	38.291367
2132.105710	106722.482008	38.296384
2134.264565	106898.272457	38.301402
2136.823192	107070.171807	38.306420
2138.846356	107227.192959	38.311437
2140.644879	107390.374621	38.316455
2142.946999	107564.472250	38.321472
2145.097054	107734.777703	38.326490
2146.958429	107903.683573	38.331508
2149.575388	108060.323965	38.336525
2151.303649	108233.779273	38.341543
2153.734825	108410.485886	38.346560
2156.228849	108575.593257	38.351578
2158.085873	108748.663247	38.356596
2160.382240	108908.756117	38.361613
2162.393189	109083.781922	38.366631
2164.387048	109244.646483	38.371648
2166.498507	109391.962588	38.376666
2168.563654	109540.364462	38.381684
2170.800431	109686.394079	38.386701
2172.549627	109840.388367	38.391719
2174.385376	109984.605132	38.396736
2176.409896	110150.490874	38.401754
2178.493814	110313.831806	38.406772
2181.072292	110475.688466	38.411789
2183.217860	110633.771074	38.416807
2184.696789	110805.337838	38.421824
2186.891621	110971.251513	38.426842
2189.005317	111143.088369	38.431860
2191.911495	111312.138883	38.436877
2193.914989	111497.970091	38.441895
2196.290782	111659.039538	38.446912
2199.130189	111824.019335	38.451930
2201.072631	111983.040143	38.456948
2203.368084	112158.924405	38.461965
2205.574686	112337.575470	38.466983
2207.627368	112517.342179	38.472000
2209.745007	112694.702662	38.477018
2211.635310	112876.982308	38.482036
2213.870870	113052.778850	38.487053
2215.812667	113241.900807	38.492071
2217.993188	113440.587125	38.497088
2220.053951	113622.171675	38.502106
2222.429922	113821.539727	38.507124
2224.543449	114012.198801	38.512141
2226.943602	114216.029571	38.517159
2229.119572	114418.881915	38.522176
2231.189489	114619.989038	38.527194
2233.553636	114829.016201	38.532212
2236.086159	115025.017987	38.537229
2237.939325	115232.821021	38.542247
2240.073199	115445.350225	38.547264
2242.285288	115644.538205	38.552282
2244.343180	115854.418140	38.557300
2246.858394	116062.413974	38.562317
2248.934296	116273.536441	38.567335
2251.206699	116490.159430	38.572352
2253.462837	116706.519862	38.577370
2256.065477	116924.006929	38.582388
2258.012796	117135.775888	38.587405
2260.224985	117359.808019	38.592423
2262.324082	117577.123966	38.597440
2265.110088	117793.318975	38.602458
2267.352751	118016.208669	38.607476
2269.770349	118232.451140	38.612493
2272.083086	118453.176122	38.617511
2273.792503	118671.256946	38.622528
2276.502966	118886.290355	38.627546
2278.616043	119110.145382	38.632564
2280.950976	119333.802110	38.637581
2283.539613	119555.390906	38.642599
2285.788865	119772.010918	38.647616
2288.528236	119972.788258	38.652634
2290.563290	120205.553921	38.657652
2293.009300	120416.121450	38.662669
2295.727343	120626.469976	38.667687
2297.825979	120862.768759	38.672704
2300.176025	121062.712016	38.677722
2302.513290	121269.254615	38.682740
2304.870741	121474.818381	38.687757
2307.159021	121695.578427	38.692775
2309.260693	121912.652075	38.697792
2311.706642	122113.435621	38.702810
2314.060874	122333.440487	38.707828
2316.379093	122539.066699	38.712845
2318.707225	122727.084681	38.717863
2320.529081	122917.390078	38.722880
2322.621651	123102.808055	38.727898
2324.759721	123302.326474	38.732916
2326.706109	123493.997908	38.737933
2328.846193	123698.224476	38.742951
2330.673794	123909.655915	38.747968
2333.039838	124115.574568	38.752986
2335.259890	124346.344019	38.758004
2337.545279	124568.845803	38.763021
2339.686487	124786.195339	38.768039
2341.797760	125012.443903	38.773056
2344.252318	125235.303481	38.778074
2346.581925	125476.376354	38.783092
2348.885727	125714.638259	38.788109
2351.245884	125953.958420	38.793127
2353.468825	126201.420990	38.798144
2355.602723	126432.012769	38.803162
2357.951648	126698.285924	38.808180
2360.417164	126941.147696	38.813197
2362.727335	127202.456854	38.818215
2365.111746	127445.930568	38.823232
2367.436431	127699.945465	38.828250
2369.625383	127962.141093	38.833268
2371.944716	128211.402193	38.838285
2374.556331	128480.690645	38.843303
2376.885146	128754.782899	38.848320
2379.476738	129011.491818	38.853338
2381.926725	129286.393266	38.858356
2384.232164	129544.710775	38.863373
2386.981130	129819.429340	38.868391
2389.529842	130087.786270	38.873408
2391.967128	130349.856360	38.878426
2394.099179	130618.294485	38.883444
2396.296448	130886.521072	38.888461
2398.921684	131165.556234	38.893479
2401.468701	131445.836206	38.898496
2403.832638	131714.346377	38.903514
2406.431739	131985.739779	38.908532
2408.871909	132261.930644	38.913549
2411.347347	132526.038116	38.918567
2413.395706	132803.562556	38.923584
2415.904841	133075.649288	38.928602
2418.651598	133363.472848	38.933620
2420.573578	133645.209690	38.938637
2423.345402	133921.092603	38.943655
2425.663776	134215.523572	38.948672
2428.292418	134486.382095	38.953690
2430.824125	134755.671255	38.958708
2433.092781	135039.418324	38.963725
2436.023862	135316.807646	38.968743
2438.694340	135595.115015	38.973760
2441.040124	135876.190462	38.978778
2443.393093	136161.555641	38.983796
2445.910840	136443.153341	38.988813
2448.574025	136714.692342	38.993831
2450.724400	137001.388809	38.998848
2453.559795	137266.064250	39.003866
2455.554280	137548.854598	39.008884
2458.403901	137823.289676	39.013901
2461.097240	138085.479363	39.018919
2463.334386	138359.848437	39.023936
2466.085587	138629.316360	39.028954
2468.382676	138898.996461	39.033972
2470.304919	139174.726669	39.038989
2472.880445	139460.013841	39.044007
2475.303105	139736.570073	39.049024
2477.868528	140011.912651	39.054042
2480.219837	140265.589007	39.059060
2482.609016	140523.626449	39.064077
2484.230448	140782.559519	39.069095
2486.305364	141037.095406	39.074112
2488.799438	141308.319304	39.079130
2490.979642	141578.667362	39.084148
2493.326669	141862.862345	39.089165
2495.924096	142145.204957	39.094183
2497.674353	142439.649690	39.099200
2500.424471	142718.748106	39.104218
2502.438050	143017.559038	39.109236
2504.295967	143327.869339	39.114253
2507.333585	143629.734753	39.119271
2509.131882	143955.097941	39.124288
2511.815574	144266.985607	39.129306
2514.353416	144586.779713	39.134324
2516.465065	144917.798789	39.139341
2519.371858	145245.421087	39.144359
2521.621440	145573.744829	39.149376
2524.296840	145909.924042	39.154394
2526.602964	146260.302493	39.159412
2528.567989	146604.415848	39.164429
2531.262265	146948.480880	39.169447
2533.546919	147306.916823	39.174464
2536.665336	147662.762424	39.179482
2539.283727	148016.442031	39.184500
2542.131960	148374.022845	39.189517
2544.564312	148729.894113	39.194535
2547.169375	149086.210385	39.199552
2549.789362	149451.703819	39.204570
2552.593818	149816.650462	39.209588
2554.235313	150178.633546	39.214605
2557.048823	150553.306796	39.219623
2559.774114	150931.804458	39.224640
2562.435006	151298.509807	39.229658
2565.071257	151667.823646	39.234676
2567.516559	152042.539257	39.239693
2570.166577	152415.194362	39.244711
2572.756209	152794.424133	39.249728
2575.104761	153186.667410	39.254746
2577.947999	153563.539688	39.259764
2580.264319	153956.313787	39.264781
2583.074324	154333.145575	39.269799
2585.370698	154731.310457	39.274816
2587.570472	155122.739769	39.279834
2590.526277	155519.004311	39.284852
2592.747735	155921.733692	39.289869
2595.594593	156311.812988	39.294887
2598.000630	156714.341185	39.299904
2600.647921	157114.092286	39.304922
2603.663886	157521.189530	39.309940
2605.991000	157921.592752	39.314957
2608.731010	158325.755260	39.319975
2611.281163	158729.594682	39.324992
2613.982287	159130.290118	39.330010
2616.654067	159533.468339	39.335028
2619.157234	159951.833883	39.340045
2622.112553	160353.525789	39.345063
2624.445358	160757.729795	39.350080
2627.370444	161161.170874	39.355098
2630.027445	161572.642068	39.360116
2632.156695	161984.947505	39.365133
2634.871654	162388.886237	39.370151
2637.572738	162802.465907	39.375168
2640.103218	163222.194386	39.380186
2642.527228	163633.232641	39.385204
2644.932220	164052.059208	39.390221
2647.920860	164459.802120	39.395239
2650.107657	164859.623422	39.400256
2652.585975	165253.243715	39.405274
2655.295851	165644.557391	39.410292
2657.916625	166033.144777	39.415309
2660.570977	166429.131262	39.420327
2663.044281	166821.796387	39.425344
2665.908116	167223.353892	39.430362
2668.356182	167618.135100	39.435380
2670.911556	168038.282945	39.440397
2673.453282	168450.283906	39.445415
2675.946257	168868.910047	39.450432
2678.669818	169281.166653	39.455450
2680.995840	169709.892618	39.460468
2683.383362	170130.878795	39.465485
2685.977569	170563.859476	39.470503
2688.333188	170999.406784	39.475520
2691.022924	171459.753458	39.480538
2693.310462	171906.858720	39.485556
2695.764769	172372.174409	39.490573
2698.819965	172828.599362	39.495591
2701.371874	173305.028639	39.500608
2704.102519	173774.029957	39.505626
2706.745203	174237.981305	39.510644
2709.222808	174722.900293	39.515661
2712.250607	175197.310955	39.520679
2714.621906	175675.814301	39.525696
2717.492432	176159.131192	39.530714
2720.460342	176651.362622	39.535732
2722.897824	177147.591021	39.540749
2725.672625	177645.014019	39.545767
2728.178436	178135.548540	39.550784
2730.854569	178644.192901	39.555802
2733.833023	179153.021509	39.560820
2736.448249	179660.614572	39.565837
2739.358046	180162.246760	39.570855
2741.733364	180676.740473	39.575872
2744.576083	181191.392556	39.580890
2747.753102	181702.109289	39.585908
2750.153376	182238.831198	39.590925
2753.072389	182753.657713	39.595943
2755.674593	183345.037198	39.600960
2758.472992	183887.242943	39.605978
2761.270929	184411.393111	39.610996
2764.003782	184947.950941	39.616013
2767.459406	185455.849898	39.621031
2770.088607	185984.987440	39.626048
2772.581311	186520.295686	39.631066
2775.168006	187042.739773	39.636084
2777.843200	187587.575092	39.641101
2780.375039	188126.288816	39.646119
2783.803394	188657.270384	39.651136
2786.493140	189209.655242	39.656154
2789.477787	189748.636179	39.661172
2792.235012	190291.897058	39.666189
2795.142350	190820.150745	39.671207
2797.555835	191360.320665	39.676224
2800.486234	191908.489565	39.681242
2803.354770	192450.472811	39.686260
2805.713528	192998.913760	39.691277
2808.501441	193546.299327	39.696295
2811.439287	194092.927140	39.701312
2814.205945	194646.594732	39.706330
2816.866828	195201.271814	39.711348
2820.055586	195744.742794	39.716365
2822.894567	196293.579523	39.721383
2825.856502	196853.169430	39.726400
2828.224330	197407.469272	39.731418
2831.334929	197951.621341	39.736436
2833.753042	198483.512981	39.741453
2836.970947	198997.881055	39.746471
2839.714286	199518.345331	39.751488
2842.121316	200044.020540	39.756506
2844.816417	200567.493215	39.761524
2847.960308	201095.037929	39.766541
2850.345309	201625.979879	39.771559
2852.792508	202170.427826	39.776576
2855.331281	202712.119655	39.781594
2858.020535	203258.082605	39.786612
2860.921785	203815.343594	39.791629
2863.112157	204375.232258	39.796647
2866.056558	204952.126093	39.801664
2868.748389	205523.599461	39.806682
2871.877136	206102.195112	39.811700
2874.416801	206698.996813	39.816717
2877.490590	207294.929102	39.821735
2879.896085	207884.515065	39.826752
2882.962951	208472.805122	39.831770
2885.612717	209069.087652	39.836788
2888.537805	209687.073789	39.841805
2891.062048	210298.722412	39.846823
2893.829805	210915.059362	39.851840
2897.041098	211542.734454	39.856858
2899.872024	212166.456590	39.861876
2902.444432	212819.104303	39.866893
2905.284688	213442.548024	39.871911
2908.689855	214088.717047	39.876928
2911.216080	214727.327329	39.881946
2914.076705	215377.953163	39.886964
2917.056460	216035.826883	39.891981
2919.947609	216686.297507	39.896999
2922.767792	217345.239611	39.902016
2925.702040	218007.695862	39.907034
2928.668509	218679.521910	39.912052
2931.668904	219338.234923	39.917069
2934.976813	219998.653348	39.922087
2937.642453	220666.209688	39.927104
2941.022751	221342.520775	39.932122
2944.241568	222003.665926	39.937140
2947.246551	222671.068859	39.942157
2949.927695	223344.416462	39.947175
2952.699277	224013.914114	39.952192
2955.669067	224705.152207	39.957210
2959.061162	225377.626912	39.962228
2962.138083	226066.460312	39.967245
2964.875082	226743.051198	39.972263
2967.802618	227427.258744	39.977280
2971.023889	228110.480154	39.982298
2974.231470	228778.689583	39.987316
2976.781433	229465.393984	39.992333
2980.241951	230143.216522	39.997351
2983.455641	230828.164821	40.002368
2986.400258	231510.919007	40.007386
2989.382988	232178.271729	40.012404
2992.860043	232868.613140	40.017421
2996.181278	233531.516440	40.022439
2999.307147	234202.680242	40.027456
3001.875889	234866.436057	40.032474
3005.702040	235531.442216	40.037492
3008.615602	236186.809538	40.042509
3011.658017	236856.127577	40.047527
3015.067398	237523.024419	40.052544
3017.901378	238186.021543	40.057562
3020.973905	238845.753724	40.062580
3023.838361	239501.782683	40.067597
3026.585587	240156.355075	40.072615
3029.455174	240811.846690	40.077632
3032.185148	241455.977833	40.082650
3035.336567	242091.175707	40.087668
3038.710671	242715.845596	40.092685
3041.462788	243342.871952	40.097703
3043.951661	243973.214716	40.102720
3046.872492	244617.891566	40.107738
3049.605276	245256.067319	40.112756
3052.375241	245920.628729	40.117773
3055.005457	246573.194291	40.122791
3057.723243	247247.691766	40.127808
3060.250383	247924.325008	40.132826
3063.443931	248604.687259	40.137844
3065.687747	249309.200536	40.142861
3068.255967	250012.390051	40.147879
3071.417968	250723.155140	40.152896
3074.589918	251444.508135	40.157914
3076.966574	252170.910108	40.162932
3080.065771	252908.651786	40.167949
3083.182892	253645.370911	40.172967
3086.246424	254379.148071	40.177984
3089.419593	255135.917832	40.183002
3092.283146	255886.229117	40.188020
3095.290252	256655.056474	40.193037
3098.243450	257418.096315	40.198055
3101.405223	258183.334215	40.203072
3104.505655	258965.468351	40.208090
3108.081127	259743.789295	40.213108
3111.433203	260529.810917	40.218125
3114.563552	261301.942646	40.223143
3118.578835	262076.064323	40.228160
3121.483705	262856.678747	40.233178
3124.667622	263634.881770	40.238196
3128.042796	264409.188494	40.243213
3130.892303	265188.854682	40.248231
3134.553888	265974.839268	40.253248
3137.400901	266758.836966	40.258266
3140.703873	267544.331826	40.263284
3143.915862	268326.989907	40.268301
3147.153997	269132.140152	40.273319
3150.185142	269907.727263	40.278336
3153.198234	270705.635161	40.283354
3157.022778	271492.208817	40.288372
3160.237002	272281.410615	40.293389
3162.988953	273068.823540	40.298407
3166.774499	273860.004077	40.303424
3170.183212	274650.448788	40.308442
3173.177534	275446.639492	40.313460
3176.669135	276238.274947	40.318477
3179.834339	277027.236262	40.323495
3183.291685	277809.490380	40.328512
3186.417846	278598.619718	40.333530
3190.010366	279396.480049	40.338548
3193.205211	280184.820312	40.343565
3196.438303	280967.991157	40.348583
3199.644098	281745.952093	40.353600
3203.517439	282511.585810	40.358618
3207.746960	283284.113456	40.363636
3211.007039	284041.624372	40.368653
3214.338848	284793.884833	40.373671
3217.790265	285553.710773	40.378688
3220.582543	286314.393016	40.383706
3223.735010	287066.986344	40.388724
3226.670573	287823.566143	40.393741
3229.799782	288593.361304	40.398759
3232.424921	289360.382254	40.403776
3235.602134	290126.444343	40.408794
3238.234684	290899.666263	40.413812
3241.841707	291654.089665	40.418829
3244.279743	292417.827000	40.423847
3247.049918	293151.466737	40.428864
3250.120112	293915.797202	40.433882
3253.021205	294664.022196	40.438900
3256.640062	295415.349809	40.443917
3259.449298	296176.365741	40.448935
3263.053338	296945.422298	40.453952
3265.939667	297714.910715	40.458970
3269.146359	298489.238290	40.463988
3272.422902	299263.848820	40.469005
3275.206237	300048.502542	40.474023
3278.551914	300843.186187	40.479040
3281.447886	301642.548678	40.484058
3284.669630	302447.280771	40.489076
3288.153226	303254.929726	40.494093
3291.337231	304078.910060	40.499111
3294.507954	304893.944052	40.504128
3297.609594	305723.013191	40.509146
3300.254649	306554.780039	40.514164
3303.957282	307396.774808	40.519181
3306.769385	308244.808686	40.524199
3310.425349	309091.782225	40.529216
3313.371110	309952.507445	40.534234
3317.046989	310816.402687	40.539252
3320.037104	311690.313392	40.544269
3323.231076	312569.379005	40.549287
3326.606637	313460.785057	40.554304
3329.295497	314354.438525	40.559322
3332.281882	315256.225400	40.564340
3335.869602	316165.133135	40.569357
3338.705990	317083.834251	40.574375
3342.389008	318004.033506	40.579392
3345.897586	318911.729999	40.584410
3349.056959	319834.002749	40.589428
3352.789777	320757.587137	40.594445
3356.272158	321696.365025	40.599463
3359.896377	322614.952451	40.604480
3363.125206	323563.091520	40.609498
3366.456410	324494.344926	40.614516
3370.100403	325423.346234	40.619533
3373.491115	326354.928517	40.624551
3377.188369	327291.566413	40.629568
3381.260974	328223.455363	40.634586
3385.209885	329153.438902	40.639604
3388.728472	330066.292230	40.644621
3392.225544	330991.888231	40.649639
3395.561252	331910.891354	40.654656
3399.129153	332825.498111	40.659674
3402.406754	333744.491356	40.664692
3406.206891	334673.907637	40.669709
3409.868645	335595.103685	40.674727
3412.821225	336511.644243	40.679744
3416.042426	337428.322766	40.684762
3419.493742	338365.664773	40.689780
3423.159825	339287.451616	40.694797
3426.459412	340205.974763	40.699815
3429.774701	341127.996986	40.704832
3433.119368	342060.946634	40.709850
3436.221514	343000.858112	40.714868
3439.852038	343920.550737	40.719885
3442.817676	344862.436187	40.724903
3446.270490	345796.104559	40.729920
3449.037274	346742.026270	40.734938
3452.405285	347705.552110	40.739956
3455.634332	348655.835539	40.744973
3458.989402	349622.020764	40.749991
3462.498390	350582.245620	40.755008
3465.929554	351530.620704	40.760013
3469.095551	352441.623599	40.765018
3472.427227	353304.738198	40.770023
3475.318077	354134.169612	40.775028
3478.627711	354894.253557	40.780032
3481.858374	355617.096968	40.785037
3484.938468	356282.838626	40.790042
3487.403857	356897.247641	40.795047
3490.037664	357445.184602	40.800052
3492.416943	357954.674660	40.805056
3494.991806	358410.502753	40.810061
3497.249068	358817.986641	40.815066
3499.569941	359175.035603	40.820071
3501.506005	359490.819302	40.825076
3503.278195	359750.717648	40.830080
3504.963196	359966.155683	40.835085
3506.260296	360153.445220	40.840090
3508.048002	360311.763315	40.845095
3509.128240	360431.412445	40.850100
3510.563178	360490.448962	40.855104
3511.958243	360549.898186	40.860109
3512.377115	360573.542077	40.865114
3513.858771	360560.985719	40.870119
3514.705177	360534.450455	40.875124
3515.469678	360481.626579	40.880128
3516.467730	360421.269549	40.885133
3517.071228	360318.103859	40.890138
3517.571397	360195.742333	40.895143
3518.037375	360078.976368	40.900148
3518.190768	359923.758974	40.905152
3519.179334	359768.156090	40.910157
3519.465529	359603.716935	40.915162
3519.699816	359413.160569	40.920167
3519.757808	359225.502240	40.925172
3520.298735	359024.247428	40.930176
3520.614336	358808.845844	40.935181
3520.700697	358598.459635	40.940186
3520.833357	358357.390338	40.945191
3521.195006	358123.145111	40.950196
3521.552708	357883.714222	40.955200
3521.551942	357640.906568	40.960205
3521.840665	357383.336705	40.965210
3521.934961	357126.557528	40.970215
3521.927354	356865.166616	40.975220
3521.884943	356590.537606	40.980224
3521.689731	356320.657324	40.985229
3521.938446	356052.408142	40.990234
3521.680043	355778.974841	40.995239
3521.882620	355508.822000	41.000244
3521.535350	355229.119995	41.005248
3521.239948	354952.076120	41.010253
3521.487761	354689.991607	41.015258
3521.469075	354398.437442	41.020263
3521.267222	354129.632221	41.025268
3521.266507	353849.228329	41.030272
3521.383103	353568.778195	41.035277
3521.287606	353286.960756	41.040282
3521.414454	352998.217745	41.045287
3521.229401	352724.593963	41.050292
3520.923949	352437.133536	41.055296
3521.029778	352165.137116	41.060301
3520.547142	351884.104962	41.065306
3520.812217	351604.936156	41.070311
3520.752145	351329.882877	41.075316
3520.647900	351048.123366	41.080320
3520.626711	350763.323450	41.085325
3520.109395	350482.767495	41.090330
3520.030027	350210.554781	41.095335
3519.841710	349932.128791	41.100340
3519.742758	349656.355636	41.105344
3519.540708	349394.933702	41.110349
3519.465972	349124.795739	41.115354
3519.355520	348854.584876	41.120359
3519.184760	348591.626376	41.125364
3519.017883	348330.495543	41.130368
3518.947469	348064.797032	41.135373
3518.678938	347802.050916	41.140378
3519.308259	347532.984714	41.145383
3518.616996	347272.461405	41.150388
3518.487943	347019.398737	41.155392
3518.494418	346753.398088	41.160397
3518.156228	346493.067737	41.165402
3518.065915	346238.391453	41.170407
3517.452956	345994.803355	41.175412
3517.468675	345750.428770	41.180416
3517.592841	345500.187959	41.185421
3517.116315	345259.293589	41.190426
3517.000075	345004.154421	41.195431
3516.389863	344773.396376	41.200436
3516.604039	344544.567282	41.205440
3517.043968	344307.209470	41.210445
3516.444311	344078.885862	41.215450
3516.557963	343827.871661	41.220455
3516.744980	343601.913561	41.225460
3516.348181	343372.485676	41.230464
3516.133308	343150.680953	41.235469
3515.986736	342916.100351	41.240474
3516.226917	342682.347607	41.245479
3515.688452	342458.961774	41.250484
3515.472129	342226.980886	41.255488
3515.487246	342017.820712	41.260493
3515.066280	341799.243312	41.265498
3515.495379	341573.946098	41.270503
3515.002893	341361.505010	41.275508
3514.820518	341143.598171	41.280512
3515.111563	340938.914447	41.285517
3514.861605	340735.839757	41.290522
3514.950913	340516.945751	41.295527
3514.670270	340299.379613	41.300532
3514.400957	340094.905739	41.305536
3514.451661	339886.947869	41.310541
3513.844004	339693.840060	41.315546
3513.928669	339485.976249	41.320551
3513.701390	339291.611660	41.325556
3513.658965	339098.132545	41.330560
3513.762021	338898.831883	41.335565
3513.438435	338701.758270	41.340570
3513.261928	338515.722209	41.345575
3512.858995	338329.110284	41.350580
3512.842159	338135.901703	41.355584
3512.731671	337958.218679	41.360589
3512.362477	337782.609590	41.365594
3512.692560	337594.887521	41.370599
3512.208413	337422.473366	41.375604
3512.221487	337235.714472	41.380608
3512.075543	337067.034816	41.385613
3512.001892	336902.005021	41.390618
3512.126506	336719.752613	41.395623
3511.852127	336547.225229	41.400628
3511.775732	336385.067164	41.405632
3511.858586	336222.680040	41.410637
3511.504440	336061.454039	41.415642
3511.765608	335882.507548	41.420647
3511.521155	335717.270243	41.425652
3511.308373	335550.603105	41.430656
3511.274989	335390.493851	41.435661
3510.932567	335229.364103	41.440666
3511.013942	335068.192831	41.445671
3510.909768	334913.636634	41.450676
3510.551903	334757.237514	41.455680
3510.842665	334607.170563	41.460685
3510.256948	334454.798577	41.465690
3510.614476	334302.863440	41.470695
3510.393751	334170.397306	41.475700
3510.343016	334003.138390	41.480704
3509.955556	333864.949575	41.485709
3509.986157	333717.259493	41.490714
3510.090630	333574.414879	41.495719
3510.054197	333435.228604	41.500724
3509.913215	333284.537175	41.505728
3509.845304	333140.293637	41.510733
3509.465135	333011.943017	41.515738
3509.561775	332869.071524	41.520743
3509.174798	332737.770819	41.525748
3509.374329	332605.360643	41.530752
3509.556185	332462.957525	41.535757
3509.242067	332335.916816	41.540762
3509.325287	332200.700320	41.545767
3509.048045	332072.279564	41.550772
3509.113817	331937.955035	41.555776
3509.404460	331808.172932	41.560781
3509.001777	331689.104638	41.565786
3508.764445	331557.598434	41.570791
3508.514498	331426.907635	41.575796
3508.907919	331305.195734	41.580800
3508.958840	331179.645584	41.585805
3508.509999	331058.725865	41.590810
3508.892580	330936.022560	41.595815
3508.438077	330819.452224	41.600820
3508.499897	330696.518528	41.605824
3508.462772	330574.413812	41.610829
3508.210900	330458.039616	41.615834
3508.071359	330343.707712	41.620839
3507.732980	330233.806753	41.625844
3507.887177	330124.922170	41.630848
3507.992233	330003.581905	41.635853
3507.869929	329901.861673	41.640858
3508.021594	329772.755761	41.645863
3507.452972	329673.419290	41.650868
3507.660767	329560.226228	41.655872
3507.652457	329452.865844	41.660877
3507.143166	329355.198010	41.665882
3507.464452	329239.112093	41.670887
3507.320964	329158.835204	41.675892
3506.800640	329043.999441	41.680896
3506.995178	328946.856440	41.685901
3506.700279	328856.377529	41.690906
3507.052303	328752.926843	41.695911
3506.864082	328661.845787	41.700916
3506.621588	328566.830464	41.705920
3507.071643	328471.350539	41.710925
3506.718870	328377.165946	41.715930
3506.883556	328286.537568	41.720935
3506.360845	328192.175615	41.725940
3506.120314	328084.517134	41.730944
3506.503873	328009.547952	41.735949
3506.312288	327917.346517	41.740954
3505.992595	327827.632210	41.745959
3505.946543	327750.415006	41.750964
3505.867185	327669.183920	41.755968
3506.324898	327583.671701	41.760973
3506.271202	327506.048236	41.765978
3505.894958	327413.467519	41.770983
3505.884092	327341.738303	41.775988
3505.738647	327246.195914	41.780992
3506.113203	327164.816527	41.785997
3505.963958	327096.059156	41.791002
3506.190280	327006.842683	41.796007
3505.450263	326930.317430	41.801012
3505.309367	326849.221480	41.806016
3505.682019	326766.417118	41.811021
3505.547676	326694.884106	41.816026
3505.974683	326614.105889	41.821031
3505.351450	326543.793705	41.826036
3505.533147	326467.098033	41.831040
3505.407695	326389.992365	41.836045
3505.371910	326323.632461	41.841050
3505.433104	326249.905928	41.846055
3505.423733	326183.032919	41.851060
3505.034897	326105.179328	41.856064
3505.227029	326027.667196	41.861069
3505.098029	325957.658282	41.866074
3505.434120	325890.425532	41.871079
3505.250621	325823.909838	41.876084
3505.090047	325759.501767	41.881088
3505.161275	325690.122464	41.886093
3504.842293	325622.533805	41.891098
3504.830460	325549.249853	41.896103
3504.390733	325487.734011	41.901108
3504.628284	325431.861123	41.906112
3504.745396	325363.135469	41.911117
3504.835362	325310.338021	41.916122
3504.696833	325236.717184	41.921127
3504.370590	325174.063860	41.926132
3504.461860	325120.401073	41.931136
3504.396896	325061.827675	41.936141
3503.819643	325010.304296	41.941146
3504.140319	324939.892635	41.946151
3504.220182	324896.839003	41.951156
3503.867787	324829.813890	41.956160
3504.163094	324796.189449	41.961165
3503.889581	324739.683244	41.966170
3503.888536	324679.700206	41.971175
3503.763511	324627.902139	41.976180
3503.904544	324588.934178	41.981184
3504.114673	324528.612645	41.986189
3504.059194	324487.691122	41.991194
3503.649144	324435.708428	41.996199
3504.259669	324381.988933	42.001204
3504.178984	324329.573037	42.006208
3503.783264	324285.550140	42.011213
3503.492137	324236.372270	42.016218
3503.491439	324192.262077	42.021223
3503.643193	324144.057837	42.026228
3503.494844	324098.800455	42.031232
3503.805361	324043.473915	42.036237
3503.739596	324002.197377	42.041242
3503.647271	323950.393345	42.046247
3503.891109	323901.996356	42.051252
3503.494255	323859.372308	42.056256
3503.900543	323812.170875	42.061261
3503.912968	323772.331891	42.066266
3503.897741	323715.427757	42.071271
3503.777091	323676.677916	42.076276
3503.411248	323628.706628	42.081280
3503.566523	323572.589686	42.086285
3503.514417	323538.000977	42.091290
3503.433582	323489.374436	42.096295
3503.636706	323463.115175	42.101300
3503.461631	323401.554831	42.106304
3503.592456	323365.563674	42.111309
3503.245972	323316.367925	42.116314
3503.750029	323273.297159	42.121319
3503.304237	323242.229467	42.126324
3503.195840	323185.949711	42.131328
3503.819253	323136.093334	42.136333
3503.381370	323104.032175	42.141338
3503.317731	323068.096601	42.146343
3503.026948	323024.335787	42.151348
3503.420183	322980.569747	42.156352
3503.597591	322940.348023	42.161357
3502.789760	322899.211839	42.166362
3503.055497	322862.817567	42.171367
3502.924876	322822.211417	42.176372
3502.967662	322790.532778	42.181376
3502.971659	322756.214482	42.186381
3503.048540	322730.457844	42.191386
3503.252939	322683.337573	42.196391
3503.000999	322652.569847	42.201396
3502.886266	322605.473941	42.206400
3503.146031	322573.176107	42.211405
3502.888428	322537.168643	42.216410
3503.007823	322493.521224	42.221415
3503.129743	322465.747657	42.226420
3502.749222	322424.467883	42.231424
3503.157990	322401.075918	42.236429
3503.222786	322364.610869	42.241434
3503.288929	322318.478509	42.246439
3502.882240	322291.169063	42.251444
3503.005589	322261.410844	42.256448
3503.123231	322228.244575	42.261453
3502.552468	322190.784829	42.266458
3502.724513	322159.543420	42.271463
3502.874743	322130.951135	42.276468
3502.767040	322090.722290	42.281472
3502.785709	322056.706406	42.286477
3502.624291	322035.845602	42.291482
3502.816062	321999.156867	42.296487
3502.644503	321966.315443	42.301492
3502.462186	321927.090261	42.306496
3503.101005	321901.347024	42.311501
3502.495206	321879.029221	42.316506
3502.477104	321840.083565	42.321511
3502.705714	321812.547288	42.326516
3502.589607	321793.485518	42.331520
3502.386952	321753.958076	42.336525
3502.442908	321735.174659	42.341530
3502.496133	321697.438841	42.346535
3502.493428	321670.421996	42.351540
3502.284351	321641.122350	42.356544
3502.625795	321611.126055	42.361549
3502.381834	321596.663400	42.366554
3502.410852	321572.465382	42.371559
3502.525187	321539.807891	42.376564
3502.278899	321520.410188	42.381568
3502.493813	321486.261404	42.386573
3502.342463	321472.293030	42.391578
3502.725679	321440.712794	42.396583
3502.676091	321413.296071	42.401588
3502.311170	321386.157590	42.406592
3502.792506	321357.131414	42.411597
3502.371840	321332.494758	42.416602
3502.196223	321304.283579	42.421607
3502.716519	321279.296261	42.426612
3502.427494	321251.204538	42.431616
3502.835678	321226.361919	42.436621
3502.577444	321202.081397	42.441626
3502.466118	321162.997051	42.446631
3502.457907	321144.376046	42.451636
3502.252117	321112.862210	42.456640
3502.457523	321080.291889	42.461645
3502.735714	321060.837421	42.466650
3502.620057	321026.053055	42.471655
3502.824445	320995.518064	42.476660
3502.394759	320966.252442	42.481664
3502.470219	320934.618182	42.486669
3502.489257	320919.045678	42.491674
3502.618124	320890.455896	42.496679
3502.439090	320873.438791	42.501684
3502.450979	320833.800628	42.506688
3502.346708	320814.609365	42.511693
3502.354383	320782.527660	42.516698
3502.172058	320753.782912	42.521703
3502.084869	320728.330552	42.526708
3502.087057	320706.349570	42.531712
3502.346552	320680.690337	42.536717
3502.243465	320668.723965	42.541722
3502.037259	320638.914367	42.546727
3502.422937	320626.820689	42.551732
3502.332365	320605.515614	42.556736
3502.473343	320571.886469	42.561741
3502.036322	320558.165982	42.566746
3502.070230	320528.547734	42.571751
3502.134186	320509.457237	42.576756
3502.166013	320482.256153	42.581760
3502.180817	320459.458967	42.586765
3502.241029	320446.983628	42.591770
3502.546142	320416.407035	42.596775
3502.349904	320387.587894	42.601780
3501.895727	320374.175319	42.606784
3502.352285	320341.514289	42.611789
3502.054491	320319.630889	42.616794
3502.199591	320300.425849	42.621799
3502.083889	320289.275451	42.626804
3501.910299	320257.883153	42.631808
3502.324550	320243.571543	42.636813
3502.055824	320224.583812	42.641818
3502.151998	320203.834482	42.646823
3501.791994	320177.330486	42.651828
3502.007082	320164.627325	42.656832
3502.358488	320140.861472	42.661837
3502.141693	320124.384232	42.666842
3501.613647	320099.153066	42.671847
3501.762525	320081.982618	42.676852
3502.004707	320075.253828	42.681856
3501.842757	320045.869395	42.686861
3501.501097	320053.300759	42.691866
3501.733299	320026.424234	42.696871
3502.157032	320000.993329	42.701876
3502.216049	319990.909503	42.706880
3502.058752	319964.424567	42.711885
3501.921690	319944.551131	42.716890
3502.172359	319924.337217	42.721895
3502.167218	319900.448886	42.726900
3501.802533	319873.716464	42.731904
3502.133960	319853.286363	42.736909
3502.295186	319835.834033	42.741914
3502.557228	319815.541967	42.746919
3502.178941	319789.854707	42.751924
3501.826459	319771.846634	42.756928
3502.525906	319753.877627	42.761933
3502.417153	319726.214660	42.766938
3502.441027	319685.276061	42.771943
3502.012778	319665.346255	42.776948
3502.207221	319655.571915	42.781952
3502.274577	319630.552685	42.786957
3502.466759	319606.989519	42.791962
3502.381883	319579.526256	42.796967
3501.946933	319560.793190	42.801972
3501.837271	319546.283402	42.806977
3502.030844	319524.297336	42.811981
3501.812273	319515.732393	42.816986
3501.752539	319493.785912	42.821991
3501.728862	319471.223191	42.826996
3501.944372	319455.059730	42.832001
3501.905893	319441.174813	42.837005
3502.232041	319421.712105	42.842010
3502.488168	319403.659613	42.847015
3501.925656	319372.378356	42.852020
3502.068036	319355.997319	42.857025
3502.064932	319331.523202	42.862029
3501.810710	319315.789306	42.867034
3501.808013	319290.500976	42.872039
3502.226674	319276.086591	42.877044
3501.729367	319260.874066	42.882049
3501.934606	319238.224553	42.887053
3501.763348	319228.329198	42.892058
3502.328716	319194.276449	42.897063
3502.269615	319192.861019	42.902068
3501.975310	319161.385030	42.907073
3502.459017	319142.431837	42.912077
3502.192050	319126.903398	42.917082
3501.956871	319101.854836	42.922087
3502.038383	319076.426008	42.927092
3501.528110	319063.606951	42.932097
3501.778566	319038.584195	42.937101
3501.469956	319024.385193	42.942106
3501.975374	319022.169137	42.947111
3501.458107	318991.949079	42.952116
3501.586724	318987.400415	42.957121
3501.582606	318969.312103	42.962125
3501.457457	318958.747996	42.967130
3501.774200	318938.039901	42.972135
3501.968214	318933.481007	42.977140
3501.956542	318918.294206	42.982145
3501.489242	318899.744003	42.987149
3501.288034	318887.843359	42.992154
3501.819968	318878.804774	42.997159
3501.802203	318866.213961	43.002164
3501.807252	318850.719222	43.007169
3501.917969	318827.041161	43.012173
3501.554432	318827.657769	43.017178
3501.848730	318809.115669	43.022183
3501.624534	318791.748618	43.027188
3501.445102	318764.197854	43.032193
3501.569858	318759.522560	43.037197
3501.526000	318744.188080	43.042202
3501.497526	318727.731750	43.047207
3501.649936	318721.805481	43.052212
3501.640433	318710.129236	43.057217
3501.749663	318686.807517	43.062221
3501.408800	318681.314546	43.067226
3501.432018	318672.202799	43.072231
3501.798622	318662.503087	43.077236
3501.941168	318649.276545	43.082241
3501.724183	318639.286437	43.087245
3501.652409	318610.904606	43.092250
3501.266149	318604.655467	43.097255
3501.604631	318598.013161	43.102260
3501.609181	318586.131151	43.107265
3501.609164	318560.714768	43.112269
3501.239033	318557.083614	43.117274
3501.895405	318555.505424	43.122279
3501.689712	318531.647693	43.127284
3501.555070	318510.424800	43.132289
3502.073610	318502.889305	43.137293
3501.501353	318484.126356	43.142298
3501.868133	318467.099296	43.147303
3501.718542	318453.104225	43.152308
3501.396735	318438.271046	43.157313
3501.526693	318429.295212	43.162317
3501.588806	318420.864265	43.167322
3501.634567	318405.032257	43.172327
3501.550706	318397.336502	43.177332
3501.128655	318380.712595	43.182337
3501.865304	318367.672948	43.187341
3501.609349	318360.640142	43.192346
3501.561149	318340.039703	43.197351
3501.520067	318339.206594	43.202356
3501.564049	318324.316190	43.207361
3501.696212	318302.211898	43.212365
3501.612867	318295.228421	43.217370
3501.720574	318275.824796	43.222375
3501.798145	318259.148174	43.227380
3501.401492	318254.503459	43.232385
3501.544014	318244.813245	43.237389
3501.567534	318221.148489	43.242394
3501.812529	318206.175734	43.247399
3501.767061	318201.908626	43.252404
3501.773967	318192.290487	43.257409
3501.808048	318177.147159	43.262413
3501.384760	318165.611786	43.267418
3501.428652	318137.822175	43.272423
3501.688113	318129.665625	43.277428
3501.350597	318134.043610	43.282433
3501.044442	318121.039711	43.287437
3501.205077	318096.920934	43.292442
3501.667573	318084.636446	43.297447
3501.576840	318093.301022	43.302452
3501.351322	318091.657151	43.307457
3501.725763	318069.769286	43.312461
3501.407473	318055.749577	43.317466
3501.721191	318041.961805	43.322471
3501.455254	318030.478123	43.327476
3501.400252	318014.763496	43.332481
3501.440301	318000.764074	43.337485
3501.255693	318000.131493	43.342490
3501.246758	317992.551164	43.347495
3501.618848	317985.827185	43.352500
3500.967976	317976.947890	43.357505
3501.638344	317957.837793	43.362509
3501.293075	317956.797810	43.367514
3501.769714	317947.615026	43.372519
3501.460228	317929.065180	43.377524
3501.414458	317922.788153	43.382529
3501.454307	317913.546437	43.387533
3501.345086	317912.978395	43.392538
3501.321415	317888.659338	43.397543
3501.665654	317875.731780	43.402548
3501.529629	317867.738780	43.407553
3501.851425	317860.462915	43.412557
3501.831149	317854.639854	43.417562
3502.116938	317837.421674	43.422567
3501.860052	317806.091512	43.427572
3501.738135	317802.141624	43.432577
3502.091127	317777.814504	43.437581
3501.655351	317763.355107	43.442586
3501.723122	317742.736257	43.447591
3502.020887	317728.594688	43.452596
3501.803405	317706.519317	43.457601
3501.773300	317695.940045	43.462605
3501.662158	317680.030537	43.467610
3501.809692	317669.906893	43.472615
3501.354900	317662.090903	43.477620
3501.360118	317637.538209	43.482625
3501.396099	317629.060311	43.487629
3501.330534	317624.007572	43.492634
3501.478647	317614.469001	43.497639
3501.483625	317606.962758	43.502644
3501.210950	317587.160334	43.507649
3501.572239	317569.777591	43.512653
3501.300488	317579.513709	43.517658
3501.632610	317566.409858	43.522663
3501.597286	317546.214113	43.527668
3501.386421	317537.062399	43.532673
3501.590642	317529.524994	43.537677
3501.374306	317527.828782	43.542682
3501.307737	317515.194326	43.547687
3501.265302	317509.222028	43.552692
3501.387002	317503.682035	43.557697
3501.557821	317493.198515	43.562701
3501.583196	317481.516490	43.567706
3501.564316	317462.437607	43.572711
3501.579883	317457.295838	43.577716
3501.338184	317449.650036	43.582721
3501.734617	317434.348034	43.587725
3501.553772	317415.726975	43.592730
3501.654288	317413.319716	43.597735
3501.489415	317393.271367	43.602740
3500.857836	317385.915490	43.607745
3501.420063	317365.982439	43.612749
3501.338785	317372.304961	43.617754
3501.287009	317364.960205	43.622759
3501.653952	317353.708156	43.627764
3501.277400	317341.122112	43.632769
3501.349127	317341.365380	43.637773
3501.068637	317336.320767	43.642778
3501.708900	317331.208533	43.647783
3501.604898	317298.403880	43.652788
3501.446384	317294.408783	43.657793
3501.358820	317287.145937	43.662797
3501.288025	317275.987746	43.667802
3501.477210	317247.080827	43.672807
3501.392141	317251.393989	43.677812
3501.056381	317248.775058	43.682817
3501.456278	317243.980261	43.687821
3501.082645	317229.918056	43.692826
3500.821439	317217.695584	43.697831
3501.022309	317212.499374	43.702836
3500.712926	317203.337550	43.707841
3501.050083	317195.855634	43.712845
3501.035931	317208.299370	43.717850
3500.960439	317196.073300	43.722855
3501.235972	317199.363270	43.727860
3501.046324	317198.349825	43.732865
3501.164675	317189.044799	43.737869
3501.332313	317207.591800	43.742874
3501.515905	317175.047406	43.747879
3501.201292	317159.780145	43.752884
3501.248987	317166.235189	43.757889
3501.394189	317163.388404	43.762893
3501.165096	317175.000701	43.767898
3501.302784	317146.203538	43.772903
3501.307491	317125.288947	43.777908
3501.317884	317125.261935	43.782913
3501.631218	317105.265908	43.787917
3501.023927	317107.752522	43.792922
3501.343155	317093.403854	43.797927
3501.426233	317081.407390	43.802932
3501.264775	317075.453642	43.807937
3501.821039	317064.833433	43.812941
3501.646872	317065.115145	43.817946
3501.897045	317039.785984	43.822951
3501.575933	317028.794078	43.827956
3501.294902	317010.010412	43.832961
3501.464321	316992.733769	43.837965
3501.209419	317001.907638	43.842970
3501.426179	316987.600398	43.847975
3501.688215	316985.625834	43.852980
3501.316667	316960.419270	43.857985
3501.316763	316950.471169	43.862989
3501.057824	316944.176444	43.867994
3501.453139	316941.570414	43.872999
3501.298909	316941.212938	43.878004
3501.178155	316916.628654	43.883009
3501.194530	316911.613910	43.888013
3501.377304	316912.094247	43.893018
3501.351483	316905.152443	43.898023
3501.648203	316899.203369	43.903028
3501.235478	316886.597408	43.908033
3501.572183	316865.198263	43.913037
3501.778046	316870.941664	43.918042
3501.552501	316858.891618	43.923047
3501.452171	316837.051927	43.928052
3501.474438	316836.819515	43.933057
3501.596800	316820.364334	43.938061
3501.240964	316809.072488	43.943066
3501.574670	316798.029038	43.948071
3501.655837	316779.392193	43.953076
3501.092280	316793.804713	43.958081
3501.445078	316775.965016	43.963085
3501.182201	316762.724963	43.968090
3501.220304	316743.026232	43.973095
3501.247319	316747.245591	43.978100
3501.354192	316737.357078	43.983105
3501.244996	316736.738131	43.988109
3501.272917	316723.452603	43.993114
3501.575856	316711.167238	43.998119
3501.709439	316704.531240	44.003124
3501.220896	316705.803492	44.008129
3500.898970	316676.390920	44.013133
3501.347096	316675.404969	44.018138
3501.066773	316663.923179	44.023143
3501.075984	316669.748237	44.028148
3501.148060	316667.548928	44.033153
3501.455464	316655.924367	44.038157
3501.861875	316660.771381	44.043162
3501.388737	316637.336081	44.048167
3501.500128	316625.385954	44.053172
3501.395183	316623.239761	44.058177
3501.782706	316611.806206	44.063181
3501.400008	316591.460791	44.068186
3501.537581	316595.154019	44.073191
3501.697195	316585.282670	44.078196
3501.499956	316558.471159	44.083201
3501.757096	316541.002526	44.088205
3501.835906	316539.285575	44.093210
3501.577618	316515.994724	44.098215
3501.764641	316507.976417	44.103220
3501.455154	316501.638645	44.108225
3501.311598	316476.447049	44.113229
3501.542206	316464.961660	44.118234
3501.390203	316460.151290	44.123239
3501.893148	316455.900047	44.128244
3501.527907	316430.285107	44.133249
3501.766016	316431.698194	44.138253
3501.443698	316417.017074	44.143258
3501.423632	316386.361292	44.148263
3501.810378	316376.479831	44.153268
3501.607390	316381.218602	44.158273
3501.530311	316359.960234	44.163277
3501.310864	316349.664675	44.168282
3501.397772	316333.494733	44.173287
3501.658778	316337.066913	44.178292
3501.338522	316318.263644	44.183297
3501.385889	316300.089860	44.188301
3501.589244	316303.874601	44.193306
3501.493599	316302.312132	44.198311
3501.547055	316277.191396	44.203316
3501.462842	316271.072804	44.208321
3501.499217	316252.213753	44.213325
3501.524961	316249.385586	44.218330
3501.538161	316235.898669	44.223335
3501.427098	316213.729589	44.228340
3501.368713	316221.346300	44.233345
3501.845333	316204.352087	44.238349
3501.331988	316195.069283	44.243354
3501.201876	316187.456704	44.248359
3501.353746	316187.840108	44.253364
3501.538133	316187.709563	44.258369
3501.312627	316165.990886	44.263373
3501.809449	316140.851645	44.268378
3501.429463	316141.241870	44.273383
3501.427651	316125.518258	44.278388
3501.211116	316115.502066	44.283393
3501.435859	316096.562613	44.288397
3501.315310	316101.212196	44.293402
3501.381526	316095.909692	44.298407
3501.196989	316093.394267	44.303412
3501.113402	316070.330304	44.308417
3501.319024	316057.373004	44.313421
3500.959446	316056.182552	44.318426
3501.566500	316055.578835	44.323431
3501.481232	316055.057911	44.328436
3501.292820	316045.469843	44.333441
3501.389187	316012.124051	44.338445
3501.166232	316019.308545	44.343450
3500.989075	316009.006295	44.348455
3501.354271	316003.860585	44.353460
3500.943049	315997.843967	44.358465
3501.133420	316003.182809	44.363469
3501.484457	315994.095591	44.368474
3501.475274	315975.676082	44.373479
3501.532514	315973.504502	44.378484
3501.159940	315964.301415	44.383489
3501.639558	315953.514823	44.388493
3501.405809	315938.692482	44.393498
3501.232350	315929.712693	44.398503
3501.353990	315938.242713	44.403508
3501.375044	315926.484626	44.408513
3501.330251	315907.790780	44.413517
3501.312502	315892.553004	44.418522
3501.272575	315888.539240	44.423527
3501.415706	315874.141382	44.428532
3501.229117	315878.343331	44.433537
3501.793541	315862.734651	44.438541
3501.533944	315849.035833	44.443546
3501.434757	315846.710597	44.448551
3501.603995	315842.002600	44.453556
3501.280555	315828.695408	44.458561
3501.616729	315816.201054	44.463565
3501.461583	315810.704133	44.468570
3501.395232	315791.530183	44.473575
3501.832133	315776.373949	44.478580
3501.545089	315773.976305	44.483585
3501.385755	315756.801469	44.488589
3501.367802	315751.562970	44.493594
3501.435562	315737.940157	44.498599
3501.536950	315732.046911	44.503604
3501.245301	315729.268332	44.508609
3501.309695	315717.147206	44.513613
3501.180974	315694.548090	44.518618
3501.568403	315685.913104	44.523623
3501.539220	315681.337884	44.528628
3501.571462	315677.719916	44.533633
3501.533247	315649.356387	44.538637
3501.646985	315644.046400	44.543642
3501.240190	315638.766905	44.548647
3501.194535	315635.746313	44.553652
3501.328471	315617.940373	44.558657
3501.616730	315606.242203	44.563661
3501.240978	315600.779745	44.568666
3501.299030	315590.008087	44.573671
3501.459188	315581.663048	44.578676
3501.588991	315579.098450	44.583681
3501.572262	315559.204223	44.588685
3501.303662	315551.307864	44.593690
3501.467742	315549.068672	44.598695
3501.482914	315535.123252	44.603700
3501.331049	315529.167798	44.608705
3501.687223	315512.421148	44.613709
3501.522572	315509.368265	44.618714
3501.383806	315485.930975	44.623719
3501.294845	315478.846159	44.628724
3501.317594	315483.753283	44.633729
3501.584113	315471.066174	44.638733
3501.594649	315445.468254	44.643738
3501.384980	315440.030699	44.648743
3501.603687	315447.985875	44.653748
3501.457487	315421.979903	44.658753
3501.292235	315409.665604	44.663757
3501.548479	315408.811400	44.668762
3500.931308	315396.186094	44.673767
3501.349090	315397.469350	44.678772
3501.137730	315385.823789	44.683777
3501.380394	315372.020860	44.688781
3501.348222	315354.240785	44.693786
3500.976494	315364.272894	44.698791
3501.149213	315357.834129	44.703796
3501.297628	315363.383156	44.708801
3501.145155	315346.436085	44.713805
3501.216090	315341.285416	44.718810
3500.878161	315321.212307	44.723815
3501.307738	315318.957040	44.728820
3501.342038	315323.429832	44.733825
3501.354103	315314.828015	44.738829
3501.433719	315315.858817	44.743834
3501.180692	315293.380709	44.748839
3501.403593	315285.102138	44.753844
3501.192655	315283.074226	44.758849
3501.666611	315283.610834	44.763853
3501.620210	315286.442401	44.768858
3501.294914	315254.179723	44.773863
3501.861934	315240.351488	44.778868
3501.488350	315238.399889	44.783873
3501.878324	315211.597546	44.788877
3501.755336	315195.841667	44.793882
3501.495339	315194.279409	44.798887
3501.762884	315158.616283	44.803892
3501.767520	315158.768277	44.808897
3501.857063	315153.894560	44.813901
3501.633277	315135.711811	44.818906
3501.497392	315123.952607	44.823911
3501.633112	315113.041474	44.828916
3501.801928	315089.123346	44.833921
3501.471623	315084.315260	44.838925
3501.237834	315085.267845	44.843930
3501.533393	315065.070139	44.848935
3501.244925	315042.851887	44.853940
3501.524443	315039.042545	44.858945
3501.529720	315029.194985	44.863949
3501.612046	315024.805817	44.868954
3501.125903	314993.382304	44.873959
3501.204215	314989.171868	44.878964
3500.871681	315001.029893	44.883969
3500.625763	314982.646991	44.888973
3501.038919	314991.436942	44.893978
3501.003749	314984.012868	44.898983
3501.117496	314990.890445	44.903988
3501.034995	314983.092111	44.908993
3501.290564	314983.586534	44.913997
3501.137657	314986.689210	44.919002
3501.065554	314958.966645	44.924007
3501.847757	314948.972160	44.929012
3501.390954	314953.903425	44.934017
3501.350788	314947.752324	44.939021
3501.101250	314934.865862	44.944026
3501.207322	314907.395293	44.949031
3501.302007	314912.291232	44.954036
3500.807662	314911.223594	44.959041
3501.833166	314904.625998	44.964045
3501.600951	314905.044017	44.969050
3501.238299	314888.205965	44.974055
3501.509085	314874.831035	44.979060
3501.513525	314877.120356	44.984065
3501.436654	314869.397455	44.989069
3501.172582	314858.548763	44.994074
3501.196752	314846.662689	44.999079
3501.289971	314834.435044	45.004084
3501.443921	314845.479177	45.009089
3501.431292	314837.440899	45.014093
3501.344564	314811.069062	45.019098
3501.168200	314800.053980	45.024103
3501.375737	314798.087843	45.029108
3501.191709	314798.040336	45.034113
3501.530963	314795.951830	45.039117
3501.223279	314778.163715	45.044122
3501.377977	314764.170801	45.049127
3501.342002	314740.920608	45.054132
3501.280105	314752.074840	45.059137
3501.475654	314747.057287	45.064141
3501.089098	314726.584411	45.069146
3501.150254	314719.196123	45.074151
3501.107043	314714.775663	45.079156
3500.953583	314707.649922	45.084161
3501.277088	314708.286392	45.089165
3501.172301	314710.185691	45.094170
3500.943186	314709.636352	45.099175
3500.672599	314704.844334	45.104180
3500.830764	314708.330946	45.109185
3501.241011	314704.628359	45.114189
3501.332486	314701.993372	45.119194
3501.500769	314686.115448	45.124199
3501.211371	314671.861161	45.129204
3501.284775	314661.773873	45.134209
3501.490947	314658.179520	45.139213
3501.325561	314644.389275	45.144218
3501.071879	314627.584979	45.149223
3501.015579	314624.057102	45.154228
3501.306004	314625.462068	45.159233
3501.144146	314618.566623	45.164237
3501.220125	314624.254286	45.169242
3501.546158	314618.961878	45.174247
3501.258740	314592.901177	45.179252
3501.441174	314585.341241	45.184257
3501.390027	314581.100119	45.189261
3501.339279	314574.314517	45.194266
3501.400196	314564.788932	45.199271
3501.330593	314543.401320	45.204276
3501.256007	314536.339553	45.209281
3501.239987	314523.747241	45.214285
3501.360784	314533.091872	45.219290
3501.324946	314528.746574	45.224295
3501.364945	314505.255386	45.229300
3501.415702	314501.227322	45.234305
3501.146732	314487.097005	45.239309
3500.997899	314492.514501	45.244314
3500.656627	314489.590937	45.249319
3501.183435	314496.022349	45.254324
3501.016143	314493.020698	45.259329
3501.371732	314471.337581	45.264333
3501.491682	314454.474808	45.269338
3501.191078	314446.939478	45.274343
3501.348696	314438.441962	45.279348
3501.041085	314445.792604	45.284353
3501.349380	314439.357958	45.289357
3501.518365	314415.973780	45.294362
3501.282781	314417.028435	45.299367
3501.524907	314403.428851	45.304372
3501.367437	314406.939387	45.309377
3501.272131	314387.260486	45.314381
3501.256974	314375.558547	45.319386
3501.406835	314373.855851	45.324391
3501.473126	314364.914602	45.329396
3501.328507	314368.881130	45.334401
3501.343043	314343.129298	45.339405
3501.149842	314331.785959	45.344410
3501.206973	314328.087660	45.349415
3501.389641	314331.392360	45.354420
3501.329940	314326.821775	45.359425
3501.689805	314300.074493	45.364429
3501.564230	314294.725430	45.369434
3501.405016	314288.643739	45.374439
3501.399675	314285.209646	45.379444
3501.178388	314266.390051	45.384449
3501.264291	314252.229625	45.389453
3501.281220	314247.850607	45.394458
3501.001318	314241.635113	45.399463
3501.415711	314239.229503	45.404468
3501.257973	314252.866942	45.409473
3501.145766	314232.987062	45.414477
3501.399082	314208.342820	45.419482
3501.430194	314204.368690	45.424487
3501.209927	314207.049396	45.429492
3501.188335	314209.088376	45.434497
3501.187446	314202.854700	45.439501
3501.261000	314182.004315	45.444506
3500.853498	314169.422220	45.449511
3501.329776	314157.465285	45.454516
3501.130908	314166.172967	45.459521
3501.368657	314157.840982	45.464525
3501.578259	314156.103494	45.469530
3501.276698	314136.533063	45.474535
3501.351023	314119.371967	45.479540
3501.313201	314118.996269	45.484545
3501.142929	314111.491397	45.489549
3501.466830	314121.796691	45.494554
3501.167946	314104.719381	45.499559
3501.316358	314086.732468	45.504564
3501.175948	314084.897031	45.509569
3501.096699	314075.825812	45.514573
3501.120702	314070.377005	45.519578
3500.837347	314076.299025	45.524583
3501.368651	314068.506352	45.529588
3501.019235	314052.225699	45.534593
3501.113305	314044.399601	45.539597
3500.953739	314036.409598	45.544602
3501.139272	314044.446540	45.549607
3501.307773	314035.107581	45.554612
3500.700580	314038.281343	45.559617
3500.733569	314032.296793	45.564621
3501.078399	314026.899600	45.569626
3500.743305	314026.443154	45.574631
3501.547445	314023.136933	45.579636
3501.249646	314021.326100	45.584641
3501.361970	313998.790235	45.589645
3501.270768	313998.804548	45.594650
3501.408824	313988.452560	45.599655
3501.238178	313990.413074	45.604660
3501.270177	313993.385131	45.609665
3501.287486	313981.270905	45.614669
3501.621662	313950.100093	45.619674
3501.403428	313947.844261	45.624679
3501.545468	313949.577781	45.629684
3501.390253	313936.370956	45.634689
3501.417636	313919.802348	45.639693
3501.086433	313917.665954	45.644698
3500.999428	313918.875504	45.649703
3501.121390	313904.963779	45.654708
3501.128203	313917.328810	45.659713
3501.020523	313904.089100	45.664717
3501.153249	313898.292496	45.669722
3501.272836	313883.897690	45.674727
3501.398619	313866.703010	45.679732
3501.479759	313883.865450	45.684737
3501.230487	313863.472503	45.689741
3501.303776	313866.692559	45.694746
3501.361039	313844.419671	45.699751
3501.308935	313828.143348	45.704756
3500.917308	313822.174264	45.709761
3500.971830	313820.206563	45.714765
3501.184409	313825.593079	45.719770
3500.964581	313825.652946	45.724775
3501.011145	313815.188000	45.729780
3501.110874	313821.330052	45.734785
3501.186407	313801.751413	45.739789
3501.344455	313795.009387	45.744794
3501.334562	313784.985818	45.749799
3501.287928	313770.845965	45.754804
3501.175075	313792.364351	45.759809
3501.318892	313776.591715	45.764813
3501.186892	313757.936064	45.769818
3501.543214	313697.296748	45.774823
3501.201513	313591.474925	45.779828
3500.688645	313446.978118	45.784833
3500.653786	313253.221179	45.789837
3500.404926	313019.268327	45.794842
3500.477977	312728.266803	45.799847
3500.687694	312394.112231	45.804852
3500.183241	312008.717794	45.809857
3499.864994	311568.277280	45.814861
3499.199184	311092.338861	45.819866
3498.890251	310558.296794	45.824871
3498.865339	309989.800500	45.829876
3498.181460	309379.998309	45.834881
3497.447954	308696.831613	45.839885
3497.057403	307986.016454	45.844890
3496.454114	307232.496992	45.849895
3495.810976	306420.059110	45.854900
3495.256172	305567.843075	45.859905
3494.713728	304651.681997	45.864909
3493.921235	303703.807722	45.869914
3493.186884	302702.435946	45.874919
3492.319399	301648.255473	45.879924
3491.026937	300573.097818	45.884929
3490.209825	299431.287864	45.889933
3489.588288	298247.070806	45.894938
3488.429956	297018.802580	45.899943
3487.497906	295736.409122	45.904948
3486.271728	294425.066453	45.909953
3485.096190	293041.242640	45.914957
3484.090777	291634.527012	45.919962
3482.839926	290179.960493	45.924967
3481.932589	288694.835186	45.929972
3480.539230	287146.134317	45.934977
3479.557027	285551.890796	45.939981
3478.006648	283923.278922	45.944986
3476.459883	282249.133279	45.949991
3475.565086	280532.481937	45.954996
3473.661808	278781.679043	45.960001
3471.841461	276974.045624	45.965005
3470.537024	275142.331062	45.970010
3469.095508	273265.784054	45.975015
3467.291600	271360.072344	45.980020
3465.492544	269417.703099	45.985025
3463.777597	267425.727906	45.990029
3461.735419	265397.069209	45.995034
3460.059950	263336.736673	46.000039
3458.321381	261244.033815	46.005044
3456.092846	259121.141406	46.010049
3454.481568	256960.527381	46.015053
3452.525463	254761.858804	46.020058
3450.262225	252538.678797	46.025063
3448.137720	250256.895157	46.030068
3446.043545	247960.736654	46.035073
3443.937313	245615.576148	46.040077
3441.516708	243275.250744	46.045082
3439.204978	240871.544419	46.050087
3437.015804	238454.654985	46.055092
3434.563949	236019.424701	46.060097
3431.909104	233534.520695	46.065101
3429.309789	231029.322072	46.070106
3426.731555	228505.620629	46.075111
3424.736222	225953.450301	46.080116
3421.624841	223382.631565	46.085121
3418.811544	220775.246538	46.090125
3415.839861	218152.790489	46.095130
3413.000044	215505.519011	46.100135
3410.013761	212842.878466	46.105140
3407.594828	210164.482044	46.110145
3404.640133	207459.887138	46.115149
3401.172340	204735.233628	46.120154
3398.115389	201984.576204	46.125159
3395.018798	199214.918545	46.130164
3391.755205	196446.634438	46.135169
3388.442178	193664.150905	46.140173
3385.256609	190870.884263	46.145178
3381.836388	188044.437252	46.150183
3377.985616	185234.274297	46.155188
3374.337343	182411.374169	46.160193
3371.162549	179561.645745	46.165197
3367.675729	176727.257336	46.170202
3364.103518	173872.226832	46.175207
3360.133947	171011.632231	46.180212
3356.341377	168143.098789	46.185217
3352.218234	165276.590245	46.190221
3347.887541	162416.089621	46.195226
3343.415540	159569.368242	46.200231
3339.047198	156716.829859	46.205236
3334.283082	153890.591981	46.210241
3329.736772	151058.440028	46.215245
3324.893866	148244.142722	46.220250
3319.951419	145458.589698	46.225255
3315.208825	142669.047060	46.230260
3309.817721	139904.611485	46.235265
3304.440731	137106.262573	46.240269
3298.256660	134416.953845	46.245274
3292.429809	131763.406918	46.250279
3285.885054	129146.920173	46.255284
3279.211124	126601.271008	46.260289
3272.091942	124094.347342	46.265293
3264.834754	121647.285835	46.270298
3257.302201	119275.399207	46.275303
3250.015075	116947.847607	46.280308
3242.056670	114716.076488	46.285313
3233.645905	112554.124479	46.290317
3225.507800	110483.939914	46.295322
3216.991891	108502.534187	46.300327
3208.183556	106601.121911	46.305332
3198.987266	104803.732164	46.310337
3190.025525	103113.405021	46.315341
3181.209061	101518.903217	46.320346
3172.282287	100022.287519	46.325351
3163.215878	98642.194877	46.330356
3154.252080	97350.969047	46.335361
3145.311324	96158.054734	46.340365
3136.992146	95053.969053	46.345370
3128.862499	94050.906405	46.350375
3121.709026	93119.736077	46.355380
3114.657461	92279.318594	46.360385
3107.768838	91504.986131	46.365389
3101.577416	90792.063222	46.370394
3095.132106	90148.889790	46.375399
3089.781375	89549.864257	46.380404
3083.995903	89002.973609	46.385409
3078.925407	88493.817882	46.390413
3074.134512	88045.002300	46.395418
3069.072317	87621.506262	46.400423
3064.524006	87218.530523	46.405428
3060.323449	86856.910536	46.410433
3056.566447	86500.675901	46.415437
3052.712068	86161.916680	46.420442
3049.383279	85853.137491	46.425447
3045.771476	85533.035637	46.430452
3041.959704	85242.530785	46.435457
3038.717259	84939.693283	46.440461
3035.447806	84653.581300	46.445466
3031.651326	84378.098579	46.450471
3029.106620	84084.510809	46.455476
3025.851169	83815.923087	46.460481
3022.797663	83534.857111	46.465485
3019.556688	83241.869574	46.470490
3016.257587	82969.587313	46.475495
3013.170212	82674.815861	46.480500
3009.730448	82391.039632	46.485505
3006.440804	82106.251960	46.490509
3003.346000	81817.943498	46.495514
2999.886473	81540.987411	46.500519
2996.503486	81251.053093	46.505524
2992.931031	80955.003575	46.510529
2989.271775	80670.097675	46.515533
2985.962959	80388.670979	46.520538
2982.357157	80105.782055	46.525543
2978.956504	79825.683667	46.530548
2975.114658	79547.409893	46.535553
2971.766156	79265.835614	46.540557
2968.424694	78995.503657	46.545562
2964.936839	78712.064314	46.550567
2961.221885	78436.982514	46.555572
2957.386469	78168.247309	46.560577
2953.523902	77904.408744	46.565581
2950.360302	77639.701368	46.570586
2946.565311	77374.841279	46.575591
2943.271876	77104.901380	46.580596
2939.102387	76860.018980	46.585601
2935.258865	76601.371687	46.590605
2932.288247	76357.182621	46.595610
2928.549753	76109.509072	46.600615
2925.057520	75866.612479	46.605620
2921.202820	75607.379511	46.610625
2917.379713	75367.675953	46.615629
2914.133598	75130.932147	46.620634
2910.472723	74899.893777	46.625639
2906.959669	74660.148022	46.630644
2902.969815	74435.514692	46.635649
2899.461445	74200.559866	46.640653
2896.027256	73968.579734	46.645658
2892.195959	73741.844813	46.650663
2888.587240	73511.559482	46.655668
2885.133601	73296.248869	46.660673
2882.088638	73083.161803	46.665677
2877.517173	72860.893012	46.670682
2874.270415	72632.780892	46.675687
2871.138263	72422.341302	46.680692
2867.061805	72218.501672	46.685697
2863.658708	71995.803460	46.690701
2860.773932	71785.342952	46.695706
2857.025105	71579.184113	46.700711
2853.737543	71354.263849	46.705716
2850.086332	71145.147301	46.710721
2846.491400	70926.995757	46.715725
2843.237893	70716.842726	46.720730
2839.565012	70506.261781	46.725735
2836.085137	70285.989851	46.730740
2832.540849	70080.851982	46.735745
2829.229165	69865.864645	46.740749
2825.637610	69650.376894	46.745754
2821.779061	69434.723193	46.750759
2818.514883	69229.319695	46.755764
2815.304222	69013.415811	46.760769
2811.741077	68799.797071	46.765773
2808.477312	68581.727669	46.770778
2804.544245	68376.765663	46.775783
2801.624450	68149.409657	46.780788
2797.664608	67931.372101	46.785793
2793.990286	67718.351036	46.790797
2791.174804	67499.827119	46.795802
2787.559086	67296.645939	46.800807
2784.418645	67072.431716	46.805812
2780.651860	66857.197866	46.810817
2777.176635	66641.786932	46.815821
2773.917246	66417.806536	46.820826
2770.389382	66199.335339	46.825831
2766.812140	65974.653203	46.830836
2763.273460	65756.346197	46.835841
2759.466099	65532.719559	46.840845
2756.314219	65312.273944	46.845850
2752.675305	65099.396206	46.850855
2749.461025	64871.956808	46.855860
2746.022387	64650.432020	46.860865
2742.422698	64435.890799	46.865869
2738.994662	64210.769419	46.870874
2735.347120	63978.423435	46.875879
2732.099916	63762.671341	46.880884
2728.400414	63545.049705	46.885889
2724.656373	63312.439389	46.890893
2721.653157	63088.372356	46.895898
2717.950385	62868.986383	46.900903
2714.566271	62633.254306	46.905908
2710.909142	62413.141699	46.910913
2707.403734	62191.877631	46.915917
2703.974148	61957.142803	46.920922
2700.214404	61734.259830	46.925927
2697.089347	61501.944101	46.930932
2693.362070	61275.157185	46.935937
2689.955465	61051.368398	46.940941
2686.771494	60831.278381	46.945946
2682.626528	60605.064324	46.950951
2679.228082	60375.733899	46.955956
2676.227957	60148.570769	46.960961
2672.650294	59921.087593	46.965965
2669.628665	59687.643269	46.970970
2665.689128	59459.275460	46.975975
2662.694762	59220.995814	46.980980
2658.531544	58998.410240	46.985985
2655.427463	58765.362050	46.990989
2651.469820	58528.616869	46.995994
2647.832272	58305.460479	47.000999
2644.664656	58076.553446	47.006004
2641.237453	57844.383226	47.011009
2637.469524	57611.545165	47.016013
2634.181438	57374.795401	47.021018
2630.946752	57155.469951	47.026023
2627.248989	56919.816674	47.031028
2623.988115	56681.051726	47.036033
2620.309897	56446.485058	47.041037
2616.822907	56210.171289	47.046042
2613.427049	55982.214550	47.051047
2610.010519	55740.171297	47.056052
2606.162333	55512.359597	47.061057
2602.823601	55276.818645	47.066061
2599.630993	55034.220934	47.071066
2596.574081	54808.449402	47.076071
2592.716847	54560.193255	47.081076
2589.101436	54320.904698	47.086081
2585.663214	54071.871212	47.091085
2582.289508	53833.634681	47.096090
2578.366421	53598.316043	47.101095
2574.755837	53360.298996	47.106100
2571.376078	53120.649528	47.111105
2567.757497	52878.920940	47.116109
2564.275201	52641.975955	47.121114
2560.538237	52399.528586	47.126119
2557.022059	52173.765363	47.131124
2553.587449	51926.847569	47.136129
2550.183751	51687.635232	47.141133
2547.046030	51454.499077	47.146138
2543.428592	51220.901091	47.151143
2540.084361	50971.111987	47.156148
2536.429224	50740.721899	47.161153
2532.864156	50502.967966	47.166157
2529.380462	50251.806545	47.171162
2525.741109	50016.695399	47.176167
2522.304540	49772.598274	47.181172
2519.163611	49534.172695	47.186177
2515.287229	49293.340075	47.191181
2511.931697	49045.838091	47.196186
2508.285716	48809.433676	47.201191
2505.146599	48566.089389	47.206196
2501.531856	48317.766851	47.211201
2498.092418	48083.272210	47.216205
2494.771901	47840.477803	47.221210
2490.764546	47592.345102	47.226215
2487.799134	47344.749805	47.231220
2484.309193	47105.915803	47.236225
2480.699377	46845.887634	47.241229
2477.481606	46607.637872	47.246234
2473.560133	46356.251649	47.251239
2470.416313	46103.459110	47.256244
2466.787168	45861.774329	47.261249
2463.185819	45605.393190	47.266253
2459.626550	45350.403637	47.271258
2456.273867	45103.407219	47.276263
2452.973338	44855.416035	47.281268
2449.373756	44610.740408	47.286273
2445.536378	44360.498572	47.291277
2442.364384	44105.969962	47.296282
2438.778979	43856.303171	47.301287
2435.170475	43600.497868	47.306292
2431.577085	43354.484334	47.311297
2428.121016	43104.063819	47.316301
2424.864977	42846.062355	47.321306
2421.052432	42603.021134	47.326311
2417.216145	42359.054153	47.331316
2413.898270	42098.059051	47.336321
2410.519243	41856.302554	47.341325
2407.194492	41601.046698	47.346330
2403.737080	41355.459022	47.351335
2400.233774	41096.869959	47.356340
2397.380988	40840.439481	47.361345
2393.823479	40581.243598	47.366349
2390.167030	40319.790004	47.371354
2386.488096	40066.598389	47.376359
2383.058575	39798.889177	47.381364
2380.032254	39554.097594	47.386369
2376.013904	39292.231095	47.391373
2372.648870	39029.409630	47.396378
2369.142276	38771.127664	47.401383
2365.977220	38508.636285	47.406388
2362.238455	38259.843417	47.411393
2358.476399	37987.561420	47.416397
2355.749818	37727.401091	47.421402
2351.502902	37473.783450	47.426407
2348.464179	37195.388252	47.431412
2344.702702	36939.805425	47.436417
2341.135374	36679.168050	47.441421
2337.545808	36406.796716	47.446426
2333.604485	36149.032683	47.451431
2330.735640	35884.181505	47.456436
2327.185271	35628.264393	47.461441
2323.425334	35355.673243	47.466445
2320.647047	35087.236223	47.471450
2316.820623	34824.804749	47.476455
2313.600058	34556.716216	47.481460
2309.956805	34281.794264	47.486465
2306.482387	34016.408254	47.491469
2303.039251	33747.509090	47.496474
2299.432239	33484.552866	47.501479
2296.170940	33207.512475	47.506484
2292.938428	32933.665781	47.511489
2288.923755	32666.232628	47.516493
2285.815073	32387.588281	47.521498
2281.876920	32117.741650	47.526503
2278.272750	31831.677883	47.531508
2275.058493	31569.565267	47.536513
2271.601303	31286.116258	47.541517
2268.481111	31018.044602	47.546522
2264.648080	30744.852974	47.551527
2261.618212	30451.442655	47.556532
2258.363041	30168.604741	47.561537
2254.927158	29890.349266	47.566541
2251.486207	29602.858447	47.571546
2247.539058	29318.587791	47.576551
2244.285591	29035.841198	47.581556
2240.639522	28744.858308	47.586561
2237.148558	28468.233980	47.591565
2233.588722	28171.377660	47.596570
2229.967030	27890.947748	47.601575
2226.790452	27591.879023	47.606580
2222.889928	27308.902668	47.611585
2219.420970	27017.916667	47.616589
2216.542215	26732.063754	47.621594
2212.842578	26446.172212	47.626599
2209.671111	26153.466578	47.631604
2206.143886	25857.354930	47.636609
2202.539000	25566.848228	47.641613
2198.977634	25268.684980	47.646618
2195.797392	24967.564660	47.651623
2192.108245	24666.243355	47.656628
2188.839349	24366.406742	47.661633
2185.506061	24070.316382	47.666637
2181.933791	23761.241893	47.671642
2178.269106	23465.649484	47.676647
2175.068446	23153.649957	47.681652
2171.282131	22855.627501	47.686657
2167.726449	22558.498360	47.691661
2164.336738	22246.080171	47.696666
2160.842738	21946.644571	47.701671
2157.312446	21633.757562	47.706676
2153.659106	21337.618567	47.711681
2149.745431	21037.964654	47.716685
2146.508703	20729.340960	47.721690
2142.495046	20438.573895	47.726695
2139.385077	20144.667238	47.731700
2135.522395	19850.534364	47.736705
2131.601410	19566.226717	47.741709
2128.110075	19270.866287	47.746714
2123.962244	18990.320636	47.751719
2120.359569	18712.715012	47.756724
2116.409378	18451.496374	47.761729
2112.375183	18191.782825	47.766733
2108.363341	17928.649065	47.771738
2104.125020	17681.008287	47.776743
2100.156519	17439.744314	47.781748
2095.776508	17220.448790	47.786753
2092.086218	16998.343491	47.791757
2088.344823	16776.869409	47.796762
2084.527757	16568.807666	47.801767
2081.039588	16356.219163	47.806772
2077.594804	16156.533075	47.811777
2073.779026	15951.498701	47.816781
2070.210990	15749.277589	47.821786
2066.942138	15549.959764	47.826791
2063.617265	15355.028766	47.831796
2059.831795	15153.531915	47.836801
2056.425284	14952.038054	47.841805
2052.642142	14755.680859	47.846810
2049.243321	14562.852954	47.851815
2045.947689	14366.290506	47.856820
2042.741956	14176.548728	47.861825
2039.236372	13977.759295	47.866829
2036.066179	13773.410352	47.871834
2032.125647	13581.050770	47.876839
2028.383801	13397.786731	47.881844
2025.333201	13202.103493	47.886849
2021.453667	13004.566882	47.891853
2018.417659	12810.633055	47.896858
2014.647255	12621.831016	47.901863
2011.405594	12416.691079	47.906868
2008.042381	12218.961593	47.911873
2004.282714	12033.738062	47.916877
2001.073899	11840.259146	47.921882
1997.489313	11649.953000	47.926887
1994.347783	11445.859018	47.931892
1991.092880	11249.699326	47.936897
1987.233242	11051.344345	47.941901
1983.947907	10847.931505	47.946906
1980.437709	10650.497951	47.951911
1976.710121	10445.854443	47.956916
1973.536659	10256.970123	47.961921
1969.773923	10052.801762	47.966925
1966.404492	9855.079192	47.971930
1962.639965	9660.389750	47.976935
1959.800324	9451.427138	47.981940
1956.097847	9257.029760	47.986945
1952.613219	9057.026124	47.991949
1949.729315	8855.996871	47.996954
1945.564945	8653.220340	48.001959
1942.486811	8444.664055	48.006964
1938.855283	8240.070946	48.011969
1934.900113	8041.481301	48.016973
1931.416119	7832.739045	48.021978
1927.516764	7642.184457	48.026983
1924.380972	7430.141692	48.031988
1921.050364	7235.466831	48.036993
1917.479551	7038.242633	48.041997
1914.154200	6827.663894	48.047002
1910.837919	6640.142791	48.052007
1906.867779	6428.935255	48.057012
1903.711317	6230.350956	48.062017
1900.076566	6029.305448	48.067021
1896.893839	5828.118626	48.072026
1893.227111	5620.360564	48.077031
1889.986161	5412.171130	48.082036
1886.082796	5199.704617	48.087041
1883.009520	5001.025718	48.092045
1879.624672	4788.242349	48.097050
1875.598774	4588.628392	48.102055
1872.006034	4375.505799	48.107060
1868.685331	4173.602507	48.112065
1865.009281	3960.029481	48.117069
1862.178435	3769.170877	48.122074
1858.158389	3574.560677	48.127079
1854.769446	3363.041446	48.132084
1851.086044	3154.317422	48.137089
1847.504646	2961.774787	48.142093
1844.034620	2744.187362	48.147098
1840.105701	2542.280389	48.152103
1836.747745	2339.444656	48.157108
1833.218148	2132.008895	48.162113
1829.847040	1938.852598	48.167117
1826.298235	1722.963680	48.172122
1822.457273	1536.048905	48.177127
1818.847338	1335.485121	48.182132
1815.679795	1141.147532	48.187137
1812.084955	955.165329	48.192141
1808.297619	751.889537	48.197146
1805.001182	560.663258	48.202151
1801.180130	361.987990	48.207156
1797.294830	185.633094	48.212161
1793.140637	8.682941	48.217165
1783.193280	2.741515	48.222170
1772.302177	58.053314	48.227175
1767.048608	51.054621	48.232180
1763.969395	54.649739	48.237185
1761.602029	59.408468	48.242189
1759.461568	57.240933	48.247194
1757.113330	55.824098	48.252199
1754.546624	58.405693	48.257204
1751.539813	58.869979	48.262209
1747.983081	56.939908	48.267213
1744.203877	51.985264	48.272218
1740.717448	57.912560	48.277223
1737.252388	62.267271	48.282228
1734.467906	56.277420	48.287233
1731.204991	50.175782	48.292237
1727.821561	53.616037	48.297242
1724.131935	56.028521	48.302247
1720.495520	51.089505	48.307252
1716.997822	55.294302	48.312257
1713.720089	49.568318	48.317261
1710.208965	51.908578	48.322266
1707.045896	53.387600	48.327271
1703.598006	53.908274	48.332276
1700.490753	48.937072	48.337281
1696.778423	57.123884	48.342285
1693.563477	50.018157	48.347290
1689.531268	50.655594	48.352295
1686.134595	53.866976	48.357300
1682.859073	55.929924	48.362305
1679.361117	61.058602	48.367309
1676.162309	53.320759	48.372314
1672.835274	55.920126	48.377319
1669.216080	54.199179	48.382324
1665.728206	48.265653	48.387329
1662.006274	55.308683	48.392333
1658.449218	56.245095	48.397338
1655.441356	67.653147	48.402343
1651.687280	59.881989	48.407348
1648.498713	54.980478	48.412353
1644.792380	65.997967	48.417357
1641.941280	54.940679	48.422362
1638.053505	61.114320	48.427367
1634.451765	61.981802	48.432372
1631.105172	60.993335	48.437377
1627.071740	74.722780	48.442381
1623.838399	61.235409	48.447386
1620.457154	62.527138	48.452391
1617.175412	67.024039	48.457396
1613.909305	57.629430	48.462401
1610.107269	54.019862	48.467405
1606.300654	59.275965	48.472410
1602.704621	58.478410	48.477415
1599.538657	58.249467	48.482420
1595.903259	57.831403	48.487425
1592.677373	57.618169	48.492429
1589.731481	54.947138	48.497434
1585.972632	59.553521	48.502439
1582.126153	54.327894	48.507444
1578.471988	51.906929	48.512449
1574.788819	54.084332	48.517453
1571.636060	55.938272	48.522458
1568.439790	58.991773	48.527463
1564.580933	61.047980	48.532468
1561.117348	58.005562	48.537473
1557.694698	58.256575	48.542477
1554.478759	53.163227	48.547482
1550.875798	57.242180	48.552487
1547.403245	54.466930	48.557492
1543.901245	51.563412	48.562497
1540.220805	61.178477	48.567501
1537.069183	52.753086	48.572506
1533.298606	63.315581	48.577511
1529.659931	63.594088	48.582516
1526.432459	63.887330	48.587521
1522.839373	63.443686	48.592525
1519.689735	49.427571	48.597530
1515.759040	61.460984	48.602535
1512.341461	59.126400	48.607540
1508.876900	59.368171	48.612545
1505.164490	61.670400	48.617549
1502.210622	49.411192	48.622554
1498.315264	62.653976	48.627559
1494.924767	52.054500	48.632564
1491.372412	58.431954	48.637569
1487.518983	51.236414	48.642573
1484.422121	48.415039	48.647578
1480.737956	65.456123	48.652583
1477.682327	55.462306	48.657588
1474.133039	51.990405	48.662593
1470.296690	65.657401	48.667597
1466.823360	53.359290	48.672602
1463.397733	66.598164	48.677607
1459.599120	59.995173	48.682612
1456.549394	57.815005	48.687617
1453.132854	56.242754	48.692621
1449.685951	58.123788	48.697626
1445.744911	65.055649	48.702631
1442.378346	65.721871	48.707636
1439.459405	60.069540	48.712641
1435.905843	61.296550	48.717645
1432.386608	56.984720	48.722650
1428.351789	60.147372	48.727655
1424.946439	53.966901	48.732660
1421.125104	50.233881	48.737665
1417.332284	52.602510	48.742669
1414.630128	46.805527	48.747674
1411.014038	54.452168	48.752679
1407.646161	55.007873	48.757684
1404.173498	59.901718	48.762689
1400.313184	59.414527	48.767693
1397.163797	56.012937	48.772698
1393.797303	57.710558	48.777703
1390.039502	63.525411	48.782708
1386.418676	56.929425	48.787713
1383.282206	65.649458	48.792717
1379.452002	53.612896	48.797722
1375.847442	61.874684	48.802727
1372.433857	64.430743	48.807732
1369.223027	66.164118	48.812737
1365.422883	62.684068	48.817741
1361.996546	60.901408	48.822746
1358.831257	68.923599	48.827751
1354.670229	57.862658	48.832756
1351.823084	52.161155	48.837761
1348.142626	52.332372	48.842765
1344.777123	50.650930	48.847770
1340.948291	64.490791	48.852775
1337.289710	51.057465	48.857780
1333.496608	53.230014	48.862785
1330.169944	55.857902	48.867789
1326.904543	55.518061	48.872794
1323.463902	59.492583	48.877799
1319.955307	59.349002	48.882804
1316.234872	53.094511	48.887809
1312.963329	56.862230	48.892813
1309.879929	56.136396	48.897818
1306.008461	59.975883	48.902823
1302.410064	61.962940	48.907828
1298.968902	57.461768	48.912833
1295.320085	57.061733	48.917837
1292.305244	59.878104	48.922842
1288.644885	63.830085	48.927847
1285.395413	51.506506	48.932852
1281.903047	53.416859	48.937857
1278.034735	60.204511	48.942861
1274.393953	50.090406	48.947866
1270.663216	53.610479	48.952871
1267.213700	53.963874	48.957876
1264.315595	50.899485	48.962881
1260.249805	49.814922	48.967885
1256.714411	48.122142	48.972890
1253.277772	60.268115	48.977895
1250.106808	54.145935	48.982900
1246.608329	49.239303	48.987905
1243.032445	54.000657	48.992909
1239.876754	44.807223	48.997914
1236.066060	56.496059	49.002919
1232.601933	56.215833	49.007924
1229.048897	51.548704	49.012929
1225.232549	60.299276	49.017933
1221.698461	52.908328	49.022938
1218.316239	58.259475	49.027943
1214.699358	54.643231	49.032948
1211.411331	60.609228	49.037953
1207.981266	55.109762	49.042957
1204.979177	57.000336	49.047962
1200.933236	59.544714	49.052967
1197.307848	54.173909	49.057972
1194.078248	62.361231	49.062977
1190.685972	59.440667	49.067981
1187.341897	54.604798	49.072986
1183.549938	57.087274	49.077991
1179.993762	50.085786	49.082996
1176.297450	58.906166	49.088001
1172.766378	53.229537	49.093005
1169.368286	50.591470	49.098010
1165.614784	63.875414	49.103015
1162.573322	58.302473	49.108020
1158.926786	60.844451	49.113025
1155.143346	57.266961	49.118029
1152.023127	61.311598	49.123034
1148.264852	64.105193	49.128039
1144.810850	56.926367	49.133044
1141.644253	54.954427	49.138049
1137.842598	61.314071	49.143053
1134.482096	57.483713	49.148058
1130.978237	55.283001	49.153063
1127.541109	53.290144	49.158068
1124.427896	51.072569	49.163073
1120.746043	58.425872	49.168077
1117.116199	51.065780	49.173082
1112.973437	53.916419	49.178087
1109.654630	54.970747	49.183092
1106.052790	54.895627	49.188097
1102.987617	56.334195	49.193101
1099.169892	56.663039	49.198106
1095.476083	58.699907	49.203111
1092.435717	58.226835	49.208116
1089.095581	55.238035	49.213121
1085.492669	55.460486	49.218125
1081.960731	63.745793	49.223130
1078.496085	53.430193	49.228135
1075.028087	50.369668	49.233140
1071.494052	55.035941	49.238145
1067.674763	59.259654	49.243149
1064.625682	58.538017	49.248154
1060.780296	52.771440	49.253159
1056.882507	50.755820	49.258164
1054.013572	50.521678	49.263169
1049.930189	59.513432	49.268173
1046.896602	47.722478	49.273178
1043.506204	52.037237	49.278183
1039.931713	51.739559	49.283188
1036.446007	49.687903	49.288193
1032.678080	52.419775	49.293197
1029.386327	43.788737	49.298202
1025.807322	54.315052	49.303207
1021.965094	51.901603	49.308212
1018.962997	49.884968	49.313217
1015.294331	57.546290	49.318221
1011.994786	51.292473	49.323226
1008.578147	43.826284	49.328231
1004.992076	44.685210	49.333236
1001.652610	46.714089	49.338241
997.793702	51.466053	49.343245
994.297844	49.229340	49.348250
990.764090	49.719410	49.353255
987.414673	53.613316	49.358260
984.021961	55.527151	49.363265
980.225327	57.807954	49.368269
976.883276	55.933146	49.373274
973.241973	52.596073	49.378279
969.888522	56.534910	49.383284
966.680509	48.646926	49.388289
962.715178	53.228904	49.393293
959.084089	42.464859	49.398298
955.746666	50.979171	49.403303
952.322430	50.730766	49.408308
948.948753	50.629471	49.413313
945.166840	46.751276	49.418317
941.847912	51.880622	49.423322
938.014648	41.224174	49.428327
934.424595	41.387720	49.433332
931.487721	40.667541	49.438337
927.550473	52.885648	49.443341
924.229306	47.587550	49.448346
921.246527	40.423627	49.453351
917.435099	44.554413	49.458356
914.028330	42.101301	49.463361
910.109044	48.776833	49.468365
906.817593	47.884389	49.473370
903.157702	55.449459	49.478375
899.745458	56.689333	49.483380
895.887941	45.381800	49.488385
892.670606	47.761753	49.493389
889.308855	37.015683	49.498394
885.897637	44.421592	49.503399
882.299432	38.673345	49.508404
879.124638	46.766740	49.513409
874.838855	40.879385	49.518413
871.775549	39.638017	49.523418
868.125195	48.777160	49.528423
864.677033	50.342212	49.533428
861.311764	43.276169	49.538433
857.528411	52.059654	49.543437
854.024549	44.072512	49.548442
850.630469	41.642748	49.553447
847.364452	48.206517	49.558452
843.836305	35.373124	49.563457
839.871304	42.030527	49.568461
836.213005	39.192887	49.573466
832.908568	43.703061	49.578471
829.576458	47.749331	49.583476
826.366572	38.880934	49.588481
822.811701	50.994904	49.593485
818.960885	45.618433	49.598490
815.441019	50.570475	49.603495
812.208385	49.159488	49.608500
808.809598	43.810316	49.613505
805.204716	53.992732	49.618509
801.816632	43.174890	49.623514
798.309216	48.995024	49.628519
794.411733	36.191016	49.633524
791.042997	42.097002	49.638529
787.820157	53.504088	49.643533
784.398701	44.225909	49.648538
780.841504	42.925870	49.653543
777.174344	40.203538	49.658548
773.671462	47.933886	49.663553
769.717866	56.943379	49.668557
766.465870	48.015157	49.673562
763.209428	50.667033	49.678567
759.484070	44.375598	49.683572
756.298173	44.627783	49.688577
752.772048	50.561594	49.693581
749.193691	48.641618	49.698586
745.750643	43.251947	49.703591
741.558861	46.031320	49.708596
738.746537	55.589767	49.713601
734.976784	62.264097	49.718605
731.868906	47.428708	49.723610
728.295085	42.784026	49.728615
724.387905	47.404444	49.733620
721.124665	51.493749	49.738625
717.337578	55.674583	49.743629
714.140560	50.936096	49.748634
710.560769	39.958494	49.753639
706.809184	44.257156	49.758644
703.406705	43.679568	49.763649
699.968605	46.325111	49.768653
696.735431	40.953215	49.773658
692.878167	46.072030	49.778663
689.623345	46.186334	49.783668
686.406917	37.537322	49.788673
682.247574	43.076771	49.793677
678.998179	36.555813	49.798682
675.555494	43.204246	49.803687
671.942376	43.115239	49.808692
668.680582	36.159627	49.813697
665.086660	40.911342	49.818701
661.605265	44.446369	49.823706
658.023339	32.339667	49.828711
654.315541	43.680360	49.833716
651.364033	40.982045	49.838721
647.475544	39.199267	49.843725
644.192928	39.672282	49.848730
640.403123	44.290168	49.853735
636.834169	46.763236	49.858740
633.714087	37.089917	49.863745
629.844401	54.691756	49.868749
626.259336	47.657071	49.873754
622.618234	50.555897	49.878759
619.819217	37.314193	49.883764
616.264430	39.914764	49.888769
612.195652	49.470696	49.893773
608.863855	43.566948	49.898778
605.696533	45.689224	49.903783
601.598014	53.721722	49.908788
598.775748	45.900029	49.913793
594.994329	40.867138	49.918797
591.477722	51.140196	49.923802
588.099019	51.030328	49.928807
584.608771	51.795312	49.933812
581.016053	41.740452	49.938817
577.457321	47.619315	49.943821
574.209785	42.347794	49.948826
570.437962	48.924424	49.953831
566.499868	48.813589	49.958836
563.551297	44.596238	49.963841
559.590040	51.566374	49.968845
556.555400	50.232039	49.973850
553.075791	44.585582	49.978855
549.463433	57.999451	49.983860
546.126436	44.221933	49.988865
542.042928	49.844477	49.993869
538.761164	48.055305	49.998874
535.207033	43.686034	50.003879
531.698546	52.315846	50.008884
528.313736	45.003068	50.013889
524.924479	56.151548	50.018893
521.376638	53.663735	50.023898
517.880113	54.325323	50.028903
514.361875	59.669520	50.033908
510.905763	43.958633	50.038913
507.328451	55.399163	50.043917
503.613833	55.996838	50.048922
500.212933	47.911470	50.053927
496.870668	52.791510	50.058932
493.456886	53.528733	50.063937
489.644323	52.578856	50.068941
486.538053	48.095165	50.073946
483.346020	52.059498	50.078951
479.401650	51.041685	50.083956
475.923998	40.146276	50.088961
472.034212	48.981360	50.093965
468.703859	57.194151	50.098970
465.106773	54.119287	50.103975
461.581055	56.784967	50.108980
458.567990	54.194435	50.113985
454.574564	49.030297	50.118989
451.932881	51.152552	50.123994
447.883477	47.234216	50.128999
444.059485	55.467385	50.134004
440.828458	49.940228	50.139009
437.033979	46.861494	50.144013
433.918671	39.373670	50.149018
429.985732	40.885096	50.154023
426.939811	50.464381	50.159028
423.525093	41.564964	50.164033
419.525007	54.160073	50.169037
416.406661	45.154124	50.174042
413.028742	47.802998	50.179047
409.332772	55.038524	50.184052
406.117084	55.827008	50.189057
402.079106	54.567627	50.194061
398.795233	43.024968	50.199066
395.129863	44.326819	50.204071
391.508570	51.177329	50.209076
388.231710	45.707995	50.214081
384.444043	44.789065	50.219085
380.998805	41.124142	50.224090
377.873169	48.577225	50.229095
374.070767	46.629223	50.234100
371.074886	43.918974	50.239105
367.082363	48.261833	50.244109
363.860743	47.289049	50.249114
360.318488	44.847886	50.254119
356.587659	56.214432	50.259124
353.101304	48.661371	50.264129
349.342386	58.981953	50.269133
346.446366	51.266821	50.274138
343.177244	53.082428	50.279143
339.612940	56.447060	50.284148
335.948368	48.083528	50.289153
331.836771	52.593752	50.294157
328.790187	51.118998	50.299162
325.235016	55.624321	50.304167
321.426959	56.318966	50.309172
318.503339	54.227003	50.314177
314.447966	48.278535	50.319181
311.132921	43.055660	50.324186
307.547945	58.050351	50.329191
304.102172	55.394779	50.334196
300.750691	52.183437	50.339201
296.828657	67.512512	50.344205
293.804168	52.116933	50.349210
290.557024	58.937345	50.354215
286.442775	63.381567	50.359220
283.101997	56.318260	50.364225
279.401201	62.485240	50.369229
276.036970	53.669725	50.374234
272.684729	42.868663	50.379239
269.365374	56.486649	50.384244
265.889820	46.552792	50.389249
261.955366	55.746129	50.394253
258.629943	54.204348	50.399258
255.175798	55.666157	50.404263
251.483695	45.297994	50.409268
248.274337	52.805360	50.414273
244.224357	66.677020	50.419277
240.926024	41.583165	50.424282
237.572858	55.722147	50.429287
234.206819	47.261278	50.434292
230.683199	54.745114	50.439297
227.119502	48.808252	50.444301
223.668547	44.587470	50.449306
220.352906	47.954320	50.454311
216.303769	45.225628	50.459316
212.937004	49.464195	50.464321
209.538822	54.479641	50.469325
206.035542	44.050285	50.474330
202.547746	44.156971	50.479335
198.846893	50.516975	50.484340
195.633371	46.230534	50.489345
191.806454	49.013102	50.494349
188.356670	43.283040	50.499354
184.969175	42.795053	50.504359
181.542345	47.995330	50.509364
178.364403	44.294944	50.514369
174.549371	43.070346	50.519373
171.080227	40.023025	50.524378
167.583199	34.778104	50.529383
163.785101	37.195500	50.534388
160.552203	45.393111	50.539393
157.041146	43.940565	50.544397
153.260123	37.699266	50.549402
150.080340	42.686843	50.554407
146.664531	44.446406	50.559412
142.964420	44.393389	50.564417
139.713456	43.985270	50.569421
136.034634	38.484105	50.574426
132.402733	49.009481	50.579431
129.157062	46.515624	50.584436
125.568645	41.269219	50.589441
121.998549	41.303409	50.594445
118.487890	38.961803	50.599450
114.923051	42.459479	50.604455
111.154102	40.512683	50.609460
107.858546	41.006903	50.614465
104.402596	49.546362	50.619469
101.040242	47.798459	50.624474
97.627501	41.306499	50.629479
93.837867	42.624777	50.634484
90.387597	38.166665	50.639489
87.151658	37.553732	50.644493
83.484177	31.095366	50.649498
79.827327	42.080244	50.654503
76.267150	48.187299	50.659508
72.987900	32.904525	50.664513
69.129094	47.350554	50.669517
65.635369	41.994428	50.674522
62.635889	46.833562	50.679527
59.016708	43.901544	50.684532
55.677608	34.727863	50.689537
51.893531	51.224957	50.694541
48.154555	45.790203	50.699546
44.763710	45.799504	50.704551
40.994146	56.621730	50.709556
37.992311	41.877631	50.714561
34.516828	51.511667	50.719565
31.088533	44.221744	50.724570
27.695099	44.016323	50.729575
24.282101	42.361808	50.734580
20.325974	39.643951	50.739585
16.961866	44.780674	50.744589
13.432384	34.880706	50.749594
9.697171	47.624277	50.754599
6.104025	45.811334	50.759604
3.104762	42.440527	50.764609