Thu Aug 25 10:31:13 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.148835	100.135991	0.000000
1.209547	90.100572	0.005005
1.238386	90.061288	0.010010
1.152160	90.600018	0.015014
1.207359	90.733775	0.020019
0.705392	82.918893	0.025024
0.905268	67.359914	0.030029
0.659824	70.701364	0.035034
0.659817	47.840145	0.040038
0.079353	44.988844	0.045043
-0.148712	34.986047	0.050048
-0.213771	24.669814	0.055053
-0.751090	20.543097	0.060058
-1.324509	7.035216	0.065062
-1.337778	-6.218737	0.070067
-1.709374	-5.597332	0.075072
-2.308599	-9.458080	0.080077
-2.648102	-15.203980	0.085082
-2.970195	-15.514143	0.090086
-2.905322	-21.241142	0.095091
-3.218378	-14.570355	0.100096
-3.098604	-21.963754	0.105101
-3.685872	-27.031755	0.110106
-4.176948	-18.273486	0.115110
-4.482310	-20.775575	0.120115
-5.180022	-17.575249	0.125120
-5.288331	-23.398498	0.130125
-5.659151	-27.956250	0.135130
-5.766090	-16.818928	0.140134
-5.702319	-20.558928	0.145139
-5.861300	-15.184104	0.150144
-5.889688	-19.396880	0.155149
-5.399061	-22.694400	0.160154
-6.873880	-14.262880	0.165158
-7.060175	-26.205230	0.170163
-7.113229	-19.628967	0.175168
-7.596713	-22.612509	0.180173
-7.216726	-20.049273	0.185178
-7.967158	-15.666941	0.190182
-8.451600	-16.514811	0.195187
-8.535214	-14.767946	0.200192
-8.652989	-15.144923	0.205197
-8.757488	-15.093713	0.210202
-9.561973	-10.297951	0.215206
-10.050064	-17.757459	0.220211
-10.260494	-13.541993	0.225216
-9.872231	-17.263233	0.230221
-9.921612	-32.162978	0.235226
-10.063386	-19.656631	0.240230
-10.275549	-23.109789	0.245235
-11.296272	-23.060552	0.250240
-11.424797	-21.632516	0.255245
-11.693160	-26.595460	0.260250
-11.791369	-15.567073	0.265254
-11.694922	-21.068066	0.270259
-12.012622	-13.646746	0.275264
-12.145896	-24.774833	0.280269
-12.834846	-19.772551	0.285274
-13.455331	-11.231282	0.290278
-13.100693	-16.234896	0.295283
-13.672720	-15.749765	0.300288
-13.584246	-12.802333	0.305293
-13.703120	-17.184428	0.310298
-14.305376	-19.617853	0.315302
-14.532535	-20.689532	0.320307
-14.522639	-17.318504	0.325312
-14.652503	-14.922154	0.330317
-15.852461	-21.852508	0.335322
-16.347918	-23.540206	0.340326
-15.427713	-24.658781	0.345331
-15.943274	-26.393948	0.350336
-16.169471	-25.532735	0.355341
-16.424830	-18.377448	0.360346
-16.420152	-14.635445	0.365350
-16.821766	-21.580156	0.370355
-17.336610	-10.609872	0.375360
-17.785131	-14.307570	0.380365
-17.672082	-18.333700	0.385370
-18.145163	-7.167478	0.390374
-17.823424	-9.552692	0.395379
-18.317697	-3.963979	0.400384
-18.951502	-13.925320	0.405389
-18.927736	-14.530117	0.410394
-19.607923	-13.300379	0.415398
-19.288779	-21.636172	0.420403
-19.383696	-3.268427	0.425408
-19.940072	-17.775534	0.430413
-19.903725	-13.779066	0.435418
-20.235507	-11.781346	0.440422
-20.251386	-20.238652	0.445427
-21.258715	-9.830277	0.450432
-21.799631	-22.273882	0.455437
-21.783148	-19.232915	0.460442
-22.067063	-18.324693	0.465446
-21.765776	-17.501837	0.470451
-21.962388	-20.343666	0.475456
-22.226656	-23.187549	0.480461
-22.695072	-21.756876	0.485466
-23.413551	-16.500031	0.490470
-23.263430	-25.733149	0.495475
-23.746164	-13.217668	0.500480
-23.568139	-26.232659	0.505485
-23.356557	-21.358822	0.510490
-24.513310	-12.458284	0.515494
-24.810111	-12.535129	0.520499
-24.900601	-12.223523	0.525504
-24.478122	-15.279413	0.530509
-24.875144	-18.314466	0.535514
-25.725369	-18.250814	0.540518
-25.803906	-24.072400	0.545523
-26.090296	-12.422908	0.550528
-26.099464	-20.384558	0.555533
-26.149798	-18.595452	0.560538
-26.825577	-7.717009	0.565542
-27.294624	-25.129447	0.570547
-27.282561	-14.105684	0.575552
-27.954184	-15.386130	0.580557
-27.913976	-25.538492	0.585562
-28.174163	-20.685647	0.590566
-27.914158	-18.676250	0.595571
-28.316209	-19.132070	0.600576
-28.833316	-16.421946	0.605581
-29.392386	-13.923545	0.610586
-29.271298	-14.344275	0.615590
-29.417099	-14.308739	0.620595
-29.365805	-20.729632	0.625600
-29.798911	-13.878685	0.630605
-30.135820	-19.147262	0.635610
-30.857605	-9.362591	0.640614
-30.879826	-21.406579	0.645619
-31.301057	-18.600747	0.650624
-31.017288	-16.278699	0.655629
-31.486913	-17.419954	0.660634
-31.900820	-20.053730	0.665638
-31.999769	-25.619017	0.670643
-32.691639	-13.776281	0.675648
-32.479361	-24.338416	0.680653
-32.318867	-14.400925	0.685658
-33.061108	-11.003795	0.690662
-33.500364	-26.949761	0.695667
-33.880775	-17.459026	0.700672
-34.149079	-18.941871	0.705677
-34.014798	-19.418452	0.710682
-34.451792	-17.723785	0.715686
-33.819789	-19.708361	0.720691
-34.824051	-23.426545	0.725696
-35.625778	-18.574269	0.730701
-35.490031	-14.492137	0.735706
-35.777516	-11.008075	0.740710
-35.387098	-13.147786	0.745715
-35.690392	-14.976323	0.750720
-35.792434	-12.318578	0.755725
-36.271911	-12.999547	0.760730
-37.082115	-11.306513	0.765734
-36.855069	-20.156219	0.770739
-36.996946	-19.501205	0.775744
-37.320977	-8.861374	0.780749
-37.936240	-5.468320	0.785754
-38.357662	-13.276793	0.790758
-38.181386	-21.106148	0.795763
-38.808870	-19.384797	0.800768
-38.712159	-19.659340	0.805773
-38.826405	-12.500852	0.810778
-39.453736	-12.687257	0.815782
-40.015436	-16.962001	0.820787
-39.682036	-7.311025	0.825792
-39.998310	-11.962745	0.830797
-39.547898	-17.857720	0.835802
-40.481315	-18.480216	0.840806
-40.782877	-17.335113	0.845811
-41.365118	-15.953043	0.850816
-41.193139	-10.161843	0.855821
-41.257856	-22.737005	0.860826
-42.312636	-11.723250	0.865830
-42.499479	-16.183279	0.870835
-42.678506	-12.618135	0.875840
-42.727211	-17.931870	0.880845
-42.948150	-19.279767	0.885850
-43.341862	-4.664855	0.890854
-42.344649	-18.336550	0.895859
-42.789594	-11.404654	0.900864
-43.311907	-13.831620	0.905869
-44.071994	-10.517115	0.910874
-44.115334	-6.435394	0.915878
-44.716835	-21.210668	0.920883
-45.340909	-7.322123	0.925888
-45.580474	-14.013817	0.930893
-45.664818	-15.484357	0.935898
-45.810178	-17.590738	0.940902
-45.375233	-6.601595	0.945907
-45.810946	-5.704388	0.950912
-46.073595	-8.510561	0.955917
-46.619446	-23.250260	0.960922
-47.295366	-12.374962	0.965926
-47.144605	-10.079529	0.970931
-47.329324	-7.538543	0.975936
-47.550448	-8.184062	0.980941
-47.764175	-15.490405	0.985946
-47.588867	-10.803870	0.990950
-48.152481	-13.237020	0.995955
-49.002416	-7.443885	1.000960
-48.508581	-8.922762	1.005965
-48.588617	-11.941044	1.010970
-49.501517	-5.555915	1.015974
-49.787777	-7.156168	1.020979
-50.266149	-15.329036	1.025984
-50.277904	-18.753483	1.030989
-50.149509	-12.727666	1.035994
-50.200090	-8.932712	1.040998
-50.340418	-20.882262	1.046003
-51.105533	-6.171193	1.051008
-51.689218	-4.298516	1.056013
-51.628098	-19.250381	1.061018
-51.819455	-10.703586	1.066022
-51.918904	-11.070779	1.071027
-52.526968	-16.524658	1.076032
-53.154371	-11.446595	1.081037
-53.101012	-11.625761	1.086042
-53.379644	-7.168654	1.091046
-53.402168	-7.361240	1.096051
-53.287868	-13.178241	1.101056
-53.698633	-14.297079	1.106061
-53.407293	-19.047166	1.111066
-54.080797	-13.063380	1.116070
-54.751887	-9.120580	1.121075
-54.953690	-6.111847	1.126080
-54.861162	-7.135540	1.131085
-54.939694	-11.017758	1.136090
-55.543771	-7.085458	1.141094
-56.147138	-14.950840	1.146099
-55.873261	-12.507021	1.151104
-56.111966	-7.192470	1.156109
-56.411143	-12.264481	1.161114
-57.252524	-12.695754	1.166118
-57.557316	-10.173919	1.171123
-57.621605	-9.037519	1.176128
-57.657102	-14.321687	1.181133
-57.548633	-15.439626	1.186138
-57.749720	-5.081647	1.191142
-57.960201	-5.583302	1.196147
-58.676320	-8.527227	1.201152
-59.185145	-11.940228	1.206157
-59.111135	-19.174595	1.211162
-59.547276	-11.899231	1.216166
-58.991165	-24.315405	1.221171
-60.194479	-12.626647	1.226176
-60.528427	-7.869810	1.231181
-60.666064	-6.133462	1.236186
-60.770944	-10.615824	1.241190
-60.326200	-9.660424	1.246195
-60.678757	-11.781796	1.251200
-61.248395	-11.509007	1.256205
-61.556093	-25.102780	1.261210
-62.042314	-17.411450	1.266214
-62.375014	-24.775075	1.271219
-62.104647	-7.837638	1.276224
-62.337672	-13.973538	1.281229
-62.598150	-13.904213	1.286234
-63.310855	-7.907955	1.291238
-63.463523	-21.700028	1.296243
-63.715910	-14.048500	1.301248
-63.966813	-12.468410	1.306253
-63.970405	-18.732006	1.311258
-64.546355	-17.695767	1.316262
-65.009974	-16.661311	1.321267
-65.178289	-10.930687	1.326272
-65.196309	-12.636244	1.331277
-65.367212	-14.251407	1.336282
-65.529206	-10.780680	1.341286
-65.494854	-11.270078	1.346291
-65.772622	-20.920201	1.351296
-66.524781	-14.873471	1.356301
-66.505827	-18.173016	1.361306
-66.539437	-20.164029	1.366310
-66.538427	-21.717544	1.371315
-67.521954	-14.223535	1.376320
-67.882086	-21.823306	1.381325
-67.735602	-7.261405	1.386330
-67.829984	-13.466484	1.391334
-68.174695	-17.980867	1.396339
-68.779727	-11.732564	1.401344
-69.299965	-9.819208	1.406349
-69.279945	-14.181936	1.411354
-69.506268	-18.506063	1.416358
-69.048647	-7.384436	1.421363
-69.421534	-11.625489	1.426368
-70.611594	-7.905089	1.431373
-70.457851	-7.758301	1.436378
-70.734564	-14.687779	1.441382
-70.964378	-25.835532	1.446387
-71.057587	-15.760217	1.451392
-71.148617	-12.503089	1.456397
-71.153992	-16.592919	1.461402
-71.861044	-12.419859	1.466406
-71.995350	-14.654521	1.471411
-72.091600	-16.904637	1.476416
-72.937845	-20.204653	1.481421
-73.191096	-17.864900	1.486426
-73.449329	-16.903754	1.491430
-73.433269	-22.015664	1.496435
-73.386474	-19.564739	1.501440
-74.016460	-12.502610	1.506445
-73.639702	-19.265561	1.511450
-74.559253	-12.075803	1.516454
-75.134048	-17.886066	1.521459
-75.161745	-12.756440	1.526464
-75.285753	-8.611461	1.531469
-75.404994	-19.460170	1.536474
-75.799379	-12.359028	1.541478
-74.803433	-16.767106	1.546483
-75.468520	-16.229425	1.551488
-76.421183	-14.931679	1.556493
-76.344514	-27.174650	1.561498
-77.153288	-15.266142	1.566502
-77.375816	-18.493048	1.571507
-78.155448	-22.477376	1.576512
-78.212972	-14.951294	1.581517
-77.790295	-25.381879	1.586522
-78.138481	-25.264010	1.591526
-78.239524	-16.851592	1.596531
-78.418372	-14.539315	1.601536
-78.512025	-11.167882	1.606541
-78.531412	-13.132651	1.611546
-79.321307	-19.057904	1.616550
-79.451695	-15.202991	1.621555
-79.859495	-18.498942	1.626560
-80.535732	-17.564046	1.631565
-80.855114	-26.457839	1.636570
-81.078545	-21.341838	1.641574
-80.852243	-20.244645	1.646579
-81.254805	-15.923144	1.651584
-81.444640	-14.855657	1.656589
-81.340540	-21.284821	1.661594
-81.428261	-16.288158	1.666598
-82.353635	-23.919581	1.671603
-82.752488	-27.330825	1.676608
-82.905691	-18.296472	1.681613
-82.753190	-28.206996	1.686618
-83.054329	-29.377811	1.691622
-83.092532	-19.928046	1.696627
-83.854593	-15.452139	1.701632
-83.932200	-14.630026	1.706637
-83.794339	-24.047880	1.711642
-84.421919	-15.521321	1.716646
-84.225447	-16.950440	1.721651
-84.965757	-8.450506	1.726656
-85.622097	-14.099296	1.731661
-85.759349	-28.399974	1.736666
-85.957708	-10.598165	1.741670
-85.841007	-18.367564	1.746675
-85.765266	-22.982627	1.751680
-86.357347	-11.383316	1.756685
-86.925810	-20.582929	1.761690
-87.149140	-14.157156	1.766694
-87.492003	-14.913312	1.771699
-87.338923	-22.027189	1.776704
-87.388103	-14.059492	1.781709
-87.412528	-10.227509	1.786714
-88.131867	-7.473039	1.791718
-88.592589	-19.929199	1.796723
-88.427835	-15.614336	1.801728
-88.776799	-19.786367	1.806733
-88.914839	-23.304918	1.811738
-90.045947	-13.962309	1.816742
-90.021667	-14.326743	1.821747
-90.201206	-5.474917	1.826752
-90.233717	-12.651465	1.831757
-89.866573	-18.014540	1.836762
-90.572193	-13.999890	1.841766
-90.665521	-16.617456	1.846771
-90.993086	-13.282137	1.851776
-91.749799	-11.625953	1.856781
-91.412197	-20.515126	1.861786
-91.625547	-13.704941	1.866790
-91.827731	-13.068951	1.871795
-92.296280	-8.996535	1.876800
-92.881126	-4.551557	1.881805
-92.676605	-18.564111	1.886810
-93.162723	-9.316238	1.891814
-93.850936	-6.379983	1.896819
-94.311816	-4.580330	1.901824
-94.290693	-5.909209	1.906829
-94.614295	-14.663141	1.911834
-94.764138	-12.222532	1.916838
-94.507288	-11.256674	1.921843
-94.719916	-14.339599	1.926848
-94.661804	-13.345765	1.931853
-94.731285	-23.522063	1.936858
-95.621982	-16.798731	1.941862
-96.158352	-14.686696	1.946867
-96.118011	-16.141970	1.951872
-96.071721	-21.682557	1.956877
-96.955973	-13.818126	1.961882
-97.473390	-10.864343	1.966886
-97.258384	-17.178009	1.971891
-97.665367	-11.223328	1.976896
-97.528660	-10.327229	1.981901
-97.462353	-18.449397	1.986906
-98.061193	-11.025155	1.991910
-98.427632	-14.776836	1.996915
-98.970328	-12.911600	2.006912
-98.358607	-8.683353	2.016909
-97.734483	-11.039708	2.026906
-97.674692	-10.757568	2.036902
-97.070408	-15.860451	2.046899
-96.585946	-11.152934	2.056896
-96.130570	-10.631840	2.066893
-95.797036	-11.691386	2.076890
-94.798986	-9.044210	2.086886
-93.925371	-3.428326	2.096883
-93.787929	-11.755726	2.106880
-93.874323	-8.729551	2.116877
-93.303341	-12.997257	2.126874
-92.496935	-14.926012	2.136870
-91.844499	-10.434882	2.146867
-91.167069	-8.995078	2.156864
-91.013796	-14.904768	2.166861
-90.783248	-15.492015	2.176858
-90.238141	-23.604522	2.186854
-89.463732	-22.484022	2.196851
-88.633508	-19.297369	2.206848
-88.641187	-15.653141	2.216845
-87.956823	-20.556328	2.226842
-87.252077	-9.107436	2.236838
-87.087516	-14.870008	2.246835
-86.259676	-16.966846	2.256832
-85.509922	-17.081086	2.266829
-85.058814	-19.008020	2.276826
-84.891790	-16.084911	2.286822
-85.071328	-18.910880	2.296819
-84.051432	-16.659933	2.306816
-83.400956	-8.940522	2.316813
-82.233046	-16.909868	2.326810
-82.273131	-3.855403	2.336806
-82.098987	-14.738621	2.346803
-81.869551	-16.510445	2.356800
-81.346883	-16.554257	2.366797
-80.234110	-19.348304	2.376794
-79.627686	-19.728354	2.386790
-79.840660	-16.663339	2.396787
-79.077294	-23.270502	2.406784
-78.199159	-20.015329	2.416781
-77.888058	-21.901318	2.426778
-77.243039	-18.872543	2.436774
-76.723470	-21.266364	2.446771
-76.685410	-14.265115	2.456768
-76.057616	-20.284002	2.466765
-75.492111	-23.885612	2.476762
-74.619976	-20.597820	2.486758
-74.097953	-20.492644	2.496755
-74.013912	-22.184665	2.506752
-73.840344	-22.363842	2.516749
-72.587461	-18.736569	2.526746
-72.187110	-16.714825	2.536742
-72.185730	-23.151907	2.546739
-71.282920	-19.137162	2.556736
-70.899470	-13.849951	2.566733
-70.503816	-20.535712	2.576730
-69.528444	-17.599881	2.586726
-69.429796	-23.640391	2.596723
-69.093353	-15.314245	2.606720
-68.557718	-20.754826	2.616717
-68.151628	-20.549121	2.626714
-67.082119	-18.214080	2.636710
-66.767353	-22.359274	2.646707
-67.013946	-19.599435	2.656704
-65.748665	-22.673968	2.666701
-65.415311	-21.766289	2.676698
-64.711210	-13.038421	2.686694
-63.928341	-16.198922	2.696691
-64.052632	-19.388341	2.706688
-63.958333	-23.264573	2.716685
-63.333293	-16.725928	2.726682
-61.902003	-19.116889	2.736678
-61.476500	-16.234279	2.746675
-61.352081	-11.974023	2.756672
-61.337684	-17.225227	2.766669
-60.314050	-15.979050	2.776666
-59.852264	-26.818635	2.786662
-59.467874	-18.005827	2.796659
-58.266104	-14.633467	2.806656
-58.142910	-22.385261	2.816653
-58.029826	-22.564465	2.826650
-57.782848	-19.495494	2.836646
-57.206242	-20.754681	2.846643
-55.957785	-21.453906	2.856640
-55.560611	-24.367072	2.866637
-55.452029	-18.539449	2.876634
-55.111054	-17.297179	2.886630
-54.104984	-19.225538	2.896627
-54.018313	-22.840817	2.906624
-53.430107	-11.481364	2.916621
-52.668602	-19.729149	2.926618
-52.515395	-22.981055	2.936614
-51.652966	-22.257645	2.946611
-51.192780	-18.173544	2.956608
-50.948151	-14.996499	2.966605
-50.545255	-19.152334	2.976602
-49.638973	-21.125245	2.986598
-49.730631	-18.757146	2.996595
-48.630302	-16.978125	3.006592
-47.990446	-16.070954	3.016589
-48.043913	-18.599900	3.026586
-47.630097	-23.790144	3.036582
-47.094170	-22.407360	3.046579
-46.071213	-26.406927	3.056576
-45.602888	-24.319806	3.066573
-45.140094	-22.957240	3.076570
-45.134381	-26.059324	3.086566
-44.264907	-23.816480	3.096563
-43.822988	-21.639691	3.106560
-43.481018	-19.881227	3.116557
-42.516377	-25.110261	3.126554
-42.467070	-17.863686	3.136550
-42.059837	-19.403609	3.146547
-41.184630	-16.810039	3.156544
-40.845554	-16.650853	3.166541
-40.110012	-23.674970	3.176538
-39.697784	-19.225394	3.186534
-39.455703	-23.463736	3.196531
-38.957158	-17.044650	3.206528
-38.289008	-17.462878	3.216525
-37.990654	-17.842171	3.226522
-37.009118	-17.039220	3.236518
-36.969333	-27.939395	3.246515
-36.524947	-17.159287	3.256512
-35.554802	-26.358418	3.266509
-35.063549	-22.377385	3.276506
-34.865346	-23.308019	3.286502
-34.445922	-21.865798	3.296499
-33.789825	-23.441547	3.306496
-33.613751	-25.772042	3.316493
-32.568974	-20.962249	3.326490
-32.297507	-22.857865	3.336486
-31.577132	-23.065699	3.346483
-31.055385	-18.421040	3.356480
-30.642062	-27.805354	3.366477
-30.306008	-25.957265	3.376474
-30.133059	-25.141660	3.386470
-29.072848	-24.579117	3.396467
-28.779836	-24.213142	3.406464
-27.950923	-22.271217	3.416461
-27.362604	-27.482466	3.426458
-27.210826	-17.762066	3.436454
-27.418842	-20.764139	3.446451
-26.598419	-25.840696	3.456448
-26.046849	-23.361140	3.466445
-24.683622	-26.698100	3.476442
-24.576450	-28.520457	3.486438
-24.597044	-19.631520	3.496435
-23.717112	-21.074447	3.506432
-22.939043	-27.592045	3.516429
-22.943587	-23.362267	3.526426
-22.468557	-22.993134	3.536422
-22.167171	-24.351747	3.546419
-21.341843	-19.897204	3.556416
-20.617195	-16.025597	3.566413
-20.699024	-21.230047	3.576410
-19.755162	-18.865809	3.586406
-19.086097	-16.582057	3.596403
-18.751625	-21.715520	3.606400
-17.862658	-19.735486	3.616397
-17.321295	-17.371537	3.626394
-17.768610	-22.027714	3.636390
-16.606111	-19.339772	3.646387
-15.957701	-17.746529	3.656384
-15.814080	-23.851109	3.666381
-15.546165	-18.916422	3.676378
-14.504491	-20.888369	3.686374
-14.196253	-15.769932	3.696371
-14.078778	-15.889635	3.706368
-13.093024	-18.131586	3.716365
-13.021072	-21.535486	3.726362
-11.694352	-21.569060	3.736358
-11.445811	-23.540279	3.746355
-11.397289	-23.177178	3.756352
-11.363905	-17.407461	3.766349
-10.292339	-18.227849	3.776346
-9.765140	-23.942704	3.786342
-8.990776	-21.434699	3.796339
-8.721599	-25.867353	3.806336
-8.426864	-16.666692	3.816333
-7.428365	-13.680622	3.826330
-7.333723	-24.941020	3.836326
-7.286014	-21.448019	3.846323
-6.396679	-13.024762	3.856320
-5.393250	-14.518716	3.866317
-4.874985	-13.057134	3.876314
-4.803316	-10.100073	3.886310
-4.994971	0.437586	3.896307
-4.129766	7.616525	3.906304
-3.110817	19.703633	3.916301
-3.348993	30.226424	3.926298
-2.632753	41.831954	3.936294
-2.241886	48.964854	3.946291
-1.927200	68.670026	3.956288
-1.277816	80.637683	3.966285
-0.664472	99.722722	3.976282
-0.236850	115.472666	3.986278
0.000000	125.389400	3.991283
0.686412	126.057009	3.996288
0.446711	146.820417	4.001293
0.885890	152.446421	4.006298
0.859932	142.943409	4.011302
0.844458	152.085989	4.016307
1.067431	139.158746	4.021312
0.858857	146.275131	4.026317
0.965588	148.697708	4.031322
1.209448	139.819977	4.036326
0.537674	155.772570	4.041331
1.155159	144.618496	4.046336
0.769446	158.045879	4.051341
1.108380	165.873756	4.056346
1.366726	169.993671	4.061350
0.864841	173.577801	4.066355
1.173070	178.790894	4.071360
1.017646	183.462863	4.076365
1.169589	177.475384	4.081370
1.321101	180.916010	4.086374
1.110113	175.516910	4.091379
1.400859	179.505200	4.096384
1.654935	179.962139	4.101389
1.122762	183.949652	4.106394
1.347533	177.703987	4.111398
1.389142	184.888757	4.116403
1.387992	170.522290	4.121408
1.385113	173.961795	4.126413
1.443390	168.795756	4.131418
0.998750	164.527933	4.136422
1.120981	176.208438	4.141427
1.378530	174.643183	4.146432
1.621315	180.122796	4.151437
1.387824	166.836780	4.156442
1.009812	176.425319	4.161446
0.974805	176.452987	4.166451
1.039167	177.961549	4.171456
1.345500	181.612037	4.176461
1.211580	177.966246	4.181466
1.586799	180.036710	4.186470
1.043849	184.377090	4.191475
1.173468	179.570031	4.196480
1.320905	182.808815	4.201485
1.386179	191.271207	4.206490
1.987847	203.832071	4.211494
1.625195	194.046425	4.216499
1.589923	183.042059	4.221504
1.060198	192.625903	4.226509
1.295500	208.787600	4.231514
1.628002	205.283859	4.236518
1.787778	208.900368	4.241523
2.164133	209.129340	4.246528
1.780648	199.679152	4.251533
1.536565	190.874684	4.256538
1.509207	182.672181	4.261542
1.421355	187.105772	4.266547
1.654793	197.788098	4.271552
1.597144	205.627510	4.276557
1.854719	206.795751	4.281562
2.020764	209.651972	4.286566
1.916621	212.189856	4.291571
1.531112	190.088051	4.296576
1.728859	190.781608	4.301581
1.747458	205.869935	4.306586
1.790395	195.837241	4.311590
1.531136	206.890999	4.316595
2.028626	203.823320	4.321600
2.064707	206.646119	4.326605
1.610759	209.428637	4.331610
2.061819	205.431754	4.336614
1.859192	208.361558	4.341619
1.852179	201.225215	4.346624
1.688679	202.133562	4.351629
1.890644	205.528323	4.356634
2.038438	206.340440	4.361638
2.007986	214.390732	4.366643
2.294870	200.624521	4.371648
1.615214	193.574590	4.376653
1.707524	194.860474	4.381658
1.908835	190.997639	4.386662
1.662542	213.378846	4.391667
2.047250	205.250975	4.396672
2.032825	206.515619	4.401677
2.005015	215.062210	4.406682
2.085776	210.326073	4.411686
2.156118	204.585490	4.416691
1.980579	207.087103	4.421696
2.014842	203.481394	4.426701
1.836215	207.448319	4.431706
2.277174	199.242035	4.436710
1.723277	209.626947	4.441715
2.293416	209.230766	4.446720
2.002667	218.381709	4.451725
1.846967	212.255757	4.456730
2.241386	214.044805	4.461734
1.985317	217.005129	4.466739
2.443114	205.958295	4.471744
2.008877	202.508251	4.476749
1.762394	215.205176	4.481754
2.130165	204.121828	4.486758
1.639378	218.268077	4.491763
2.171901	223.509316	4.496768
2.493869	238.078735	4.501773
2.337142	235.505863	4.506778
2.155293	227.286417	4.511782
2.300898	238.688052	4.516787
2.413442	244.475995	4.521792
2.286657	232.340647	4.526797
2.275217	231.488255	4.531802
2.513405	236.955951	4.536806
2.427649	229.487082	4.541811
2.463964	226.703630	4.546816
2.262657	226.349227	4.551821
2.137115	233.142586	4.556826
2.390151	229.255820	4.561830
2.482911	247.202111	4.566835
2.517674	238.527936	4.571840
2.927845	239.438151	4.576845
2.424321	229.589136	4.581850
2.397045	225.932953	4.586854
1.992548	222.532029	4.591859
2.653938	228.933168	4.596864
2.796928	240.211826	4.601869
2.692336	231.869540	4.606874
2.633742	218.685798	4.611878
2.237738	225.065947	4.616883
2.660181	219.203751	4.621888
2.393642	236.677976	4.626893
2.607222	235.043675	4.631898
2.796521	239.145951	4.636902
2.585834	227.786223	4.641907
2.295916	223.924417	4.646912
2.242566	243.080014	4.651917
2.931029	247.584976	4.656922
2.879356	250.323454	4.661926
2.383320	246.484446	4.666931
2.804918	247.237846	4.671936
2.691052	246.952000	4.676941
2.851803	239.624840	4.681946
3.016470	237.957073	4.686950
2.914024	245.025232	4.691955
2.845819	226.651222	4.696960
2.586981	230.437729	4.701965
2.463316	221.269526	4.706970
2.729406	238.385051	4.711974
2.609231	237.442127	4.716979
2.696743	247.682270	4.721984
2.644459	243.935089	4.726989
2.630861	251.467060	4.731994
2.620472	242.303244	4.736998
2.792514	240.874769	4.742003
2.759483	248.944464	4.747008
2.989936	249.968260	4.752013
2.808617	251.179961	4.757018
3.167265	244.214101	4.762022
2.631412	246.772174	4.767027
3.031514	253.258554	4.772032
3.097500	255.159177	4.777037
3.012853	249.968052	4.782042
3.262150	239.001322	4.787046
3.101101	249.568316	4.792051
2.988443	241.512030	4.797056
3.263261	241.174776	4.802061
3.222221	249.628543	4.807066
2.981980	237.204081	4.812070
3.095838	248.503128	4.817075
3.108993	244.714055	4.822080
2.831022	234.301345	4.827085
2.969817	239.196152	4.832090
3.062614	244.648664	4.837094
2.410232	250.926622	4.842099
2.874300	249.395443	4.847104
2.993730	254.688761	4.852109
2.919951	247.249646	4.857114
2.983124	245.996418	4.862118
3.055204	256.052321	4.867123
3.112503	253.914152	4.872128
2.797920	262.334854	4.877133
2.816263	266.157034	4.882138
2.815972	267.204329	4.887142
3.073191	279.366794	4.892147
3.428535	271.942691	4.897152
3.010983	282.227188	4.902157
2.944525	287.555968	4.907162
3.235747	282.033855	4.912166
2.769836	285.182095	4.917171
3.296862	275.082999	4.922176
3.183203	273.313304	4.927181
3.010564	282.217981	4.932186
3.293740	286.150532	4.937190
3.077684	291.740037	4.942195
3.716787	295.610496	4.947200
3.867720	291.647964	4.952205
3.563820	289.620169	4.957210
3.478260	275.121309	4.962214
3.539740	284.321502	4.967219
3.299052	276.857906	4.972224
3.273335	282.291034	4.977229
3.630822	277.647565	4.982234
3.540029	275.969200	4.987238
3.232278	285.072220	4.992243
3.398194	286.473129	4.997248
3.734006	291.561710	5.002253
3.469905	294.735280	5.007258
3.631668	277.891263	5.012262
3.492422	287.464597	5.017267
3.769774	281.204330	5.022272
3.539752	282.815974	5.027277
3.181670	285.298742	5.032282
3.745189	292.797256	5.037286
3.741766	303.962851	5.042291
3.864151	296.923256	5.047296
3.485394	284.223069	5.052301
3.367618	294.539697	5.057306
3.757346	294.795049	5.062310
3.662580	301.703837	5.067315
3.845688	301.700494	5.072320
4.039021	286.601100	5.077325
3.522147	279.035242	5.082330
3.561481	278.994314	5.087334
3.546422	286.450598	5.092339
3.665908	287.991662	5.097344
3.512355	297.269847	5.102349
3.411281	302.876141	5.107354
3.554470	299.411536	5.112358
3.486885	299.070981	5.117363
3.982172	299.990009	5.122368
3.686432	300.273667	5.127373
3.578871	299.797005	5.132378
3.607704	303.196765	5.137382
3.562159	295.607672	5.142387
3.532651	293.631798	5.147392
3.758897	303.071944	5.152397
3.731817	329.430639	5.157402
3.863571	324.423888	5.162406
4.058011	327.025738	5.167411
4.215077	327.070769	5.172416
4.235822	327.374443	5.177421
3.831249	319.193015	5.182426
3.964648	313.894939	5.187430
3.871757	321.980373	5.192435
4.069177	324.189445	5.197440
4.173052	334.898481	5.202445
3.965389	324.553797	5.207450
3.980555	324.238242	5.212454
4.029298	331.931324	5.217459
4.224865	317.717417	5.222464
4.152159	313.271058	5.227469
3.603233	310.063591	5.232474
3.868215	321.047936	5.237478
3.871783	333.863957	5.242483
4.130751	328.612642	5.247488
3.965328	332.077646	5.252493
3.705304	335.877016	5.257498
4.389192	329.413829	5.262502
4.197189	332.506505	5.267507
4.361716	336.688616	5.272512
4.353321	329.318317	5.277517
4.104682	329.831880	5.282522
4.355660	327.498840	5.287526
4.383926	332.888723	5.292531
4.606898	325.539124	5.297536
4.507324	320.220600	5.302541
4.625749	323.672766	5.307546
4.385194	312.728958	5.312550
4.119955	314.751089	5.317555
4.071079	317.890940	5.322560
4.293001	325.060170	5.327565
4.432556	316.872583	5.332570
4.260952	319.851328	5.337574
4.269690	327.038141	5.342579
4.299377	319.522673	5.347584
4.609018	321.922973	5.352589
4.502177	328.783042	5.357594
4.745345	326.653709	5.362598
4.361864	324.894646	5.367603
4.223577	332.120317	5.372608
4.565480	333.594898	5.377613
4.528610	332.423778	5.382618
4.195759	319.985295	5.387622
4.047439	328.218623	5.392627
4.252826	318.135098	5.397632
4.336242	323.506845	5.402637
4.031059	324.045087	5.407642
4.486947	322.394960	5.412646
4.391863	328.655230	5.417651
4.381743	327.517884	5.422656
4.205903	328.048516	5.427661
4.403620	332.019778	5.432666
4.706077	340.435587	5.437670
4.676700	349.975921	5.442675
4.911887	349.031097	5.447680
4.286776	345.079412	5.452685
4.693001	354.744490	5.457690
4.876345	349.131689	5.462694
4.752583	346.794086	5.467699
4.410676	346.686339	5.472704
4.492270	342.639745	5.477709
4.570936	343.380441	5.482714
5.203975	352.750548	5.487718
4.781949	343.496150	5.492723
4.831260	345.127309	5.497728
4.825493	355.628907	5.502733
4.511891	354.159454	5.507738
4.731769	348.284661	5.512742
4.443954	351.987148	5.517747
4.455066	356.139515	5.522752
4.612606	351.812097	5.527757
4.693541	347.800408	5.532762
4.965339	354.579015	5.537766
4.753540	356.573794	5.542771
4.691995	367.065154	5.547776
5.082794	348.695033	5.552781
5.109813	361.292260	5.557786
4.762733	352.257073	5.562790
4.792480	358.326949	5.567795
4.720604	356.500078	5.572800
5.007659	352.680722	5.577805
4.722095	358.518423	5.582810
5.530365	351.058125	5.587814
4.913939	356.501570	5.592819
5.088448	365.560707	5.597824
5.167905	354.440181	5.602829
4.951586	354.983483	5.607834
5.138713	354.653639	5.612838
5.091861	357.169912	5.617843
4.965233	360.777541	5.622848
5.124172	357.721751	5.627853
4.451592	358.554843	5.632858
5.011895	351.721864	5.637862
4.666803	364.836149	5.642867
4.934740	370.343517	5.647872
5.239985	370.615272	5.652877
5.320657	378.692520	5.657882
5.348633	377.811799	5.662886
5.101894	366.172889	5.667891
4.893475	360.551864	5.672896
5.236292	374.760618	5.677901
5.274273	378.067208	5.682906
5.244939	380.454187	5.687910
5.360464	386.494814	5.692915
5.056005	384.296251	5.697920
5.136626	380.483923	5.702925
5.301202	391.851045	5.707930
5.320687	375.829672	5.712934
4.733581	383.021279	5.717939
4.719761	378.363193	5.722944
5.115506	388.646874	5.727949
5.040494	385.814400	5.732954
5.063934	377.088148	5.737958
4.917379	377.721762	5.742963
5.424398	396.514472	5.747968
5.572518	394.324091	5.752973
5.394616	401.761645	5.757978
5.298691	405.206282	5.762982
5.288285	407.852895	5.767987
5.455871	410.844951	5.772992
5.765205	404.867537	5.777997
5.907478	404.522573	5.783002
5.412875	393.732417	5.788006
5.035087	390.649984	5.793011
5.057058	398.353617	5.798016
5.494894	400.689548	5.803021
5.565721	415.181401	5.808026
5.937838	408.697430	5.813030
5.743272	420.124005	5.818035
5.408247	407.103660	5.823040
5.800602	413.464760	5.828045
5.367738	408.752098	5.833050
5.943926	412.553346	5.838054
5.509171	408.195327	5.843059
5.809566	415.387100	5.848064
5.776437	395.596360	5.853069
5.493654	395.656522	5.858074
5.729930	393.607356	5.863078
5.383462	397.907510	5.868083
5.391517	405.603836	5.873088
5.871133	401.045605	5.878093
5.413936	409.235615	5.883098
5.972055	399.710556	5.888102
5.477403	408.504395	5.893107
5.398018	406.707170	5.898112
6.037245	407.562522	5.903117
5.526733	411.246128	5.908122
5.894851	403.335907	5.913126
5.681997	411.294642	5.918131
5.646080	405.004320	5.923136
5.640685	403.198666	5.928141
5.962720	418.929341	5.933146
6.285523	409.358888	5.938150
6.008845	412.411060	5.943155
5.731816	409.527975	5.948160
5.643772	410.914901	5.953165
5.816941	412.162821	5.958170
5.645585	411.003277	5.963174
5.732172	409.822300	5.968179
5.662728	416.407620	5.973184
5.976655	404.459372	5.978189
5.485887	415.549533	5.983194
6.149598	423.756917	5.988198
6.270443	417.014914	5.993203
6.006875	413.120464	5.998208
6.371362	410.548161	6.003213
6.032165	416.577785	6.008218
6.200893	409.578342	6.013222
5.880523	416.715515	6.018227
5.694869	412.030559	6.023232
5.767747	407.216510	6.028237
5.637805	411.881382	6.033242
5.875622	415.745138	6.038246
6.233609	432.596510	6.043251
5.935381	418.146674	6.048256
6.278326	418.399867	6.053261
5.769208	416.508617	6.058266
6.072373	412.591810	6.063270
5.685604	409.482306	6.068275
6.212722	421.058404	6.073280
5.823032	413.725666	6.078285
5.405696	423.140160	6.083290
5.633391	434.396178	6.088294
5.859977	438.451528	6.093299
6.270687	440.010252	6.098304
6.393857	433.543131	6.103309
6.010907	442.708634	6.108314
6.047219	448.711072	6.113318
6.082787	443.782635	6.118323
6.307706	446.889102	6.123328
6.274726	434.295985	6.128333
6.054172	426.174261	6.133338
5.768285	414.240892	6.138342
5.558547	420.250234	6.143347
6.225993	424.413679	6.148352
6.473008	419.945673	6.153357
5.839644	422.212158	6.158362
6.210801	417.433631	6.163366
6.126758	411.033787	6.168371
5.739119	410.733885	6.173376
6.007184	415.773003	6.178381
5.889586	418.664208	6.183386
6.011409	421.957670	6.188390
5.904496	417.399583	6.193395
5.686780	418.591687	6.198400
6.230647	411.660019	6.203405
6.084028	420.557524	6.208410
6.195574	416.354357	6.213414
6.108649	414.431760	6.218419
6.002374	407.310887	6.223424
6.037624	416.724070	6.228429
5.877523	417.252238	6.233434
5.679588	418.498192	6.238438
5.496429	413.964707	6.243443
6.140060	412.864134	6.248448
5.713645	407.030472	6.253453
5.864028	430.507754	6.258458
5.870390	430.671312	6.263462
5.963652	432.412654	6.268467
6.446622	441.062824	6.273472
6.401539	423.339900	6.278477
5.991486	417.971915	6.283482
6.074337	418.692975	6.288486
5.868467	402.191186	6.293491
5.838460	410.206694	6.298496
5.652327	415.044889	6.303501
5.747021	429.555160	6.308506
6.134685	424.312128	6.313510
6.019106	433.230086	6.318515
6.141744	441.962025	6.323520
6.401184	431.702283	6.328525
6.063186	429.553262	6.333530
5.997225	425.105818	6.338534
6.064106	415.154673	6.343539
5.704046	420.083396	6.348544
6.329660	417.758086	6.353549
5.970984	410.711561	6.358554
5.783951	418.849754	6.363558
6.044915	413.892337	6.368563
5.816112	411.561690	6.373568
6.139513	414.285720	6.378573
6.013201	416.188016	6.383578
5.926750	412.889085	6.388582
6.039098	411.150405	6.393587
6.336712	412.556001	6.398592
6.010255	414.306154	6.403597
6.174762	417.675187	6.408602
6.264659	410.302110	6.413606
5.918928	416.551061	6.418611
5.967817	410.035475	6.423616
5.744183	411.500594	6.428621
5.855041	414.669220	6.433626
5.827099	407.203874	6.438630
5.871188	413.714456	6.443635
5.750739	416.096733	6.448640
5.996448	411.027809	6.453645
5.831783	417.257882	6.458650
6.105232	416.455759	6.463654
5.685466	414.240456	6.468659
5.760363	415.665128	6.473664
6.378323	428.220435	6.478669
5.961446	422.154315	6.483674
6.114371	416.350103	6.488678
6.455608	419.805344	6.493683
6.372714	409.393605	6.498688
6.333229	415.379433	6.503693
5.624988	427.566716	6.508698
6.118471	409.193099	6.513702
6.016750	411.167474	6.518707
5.850442	412.117401	6.523712
6.193727	417.043492	6.528717
6.201862	415.586900	6.533722
6.039662	420.098638	6.538726
6.145279	420.044160	6.543731
6.185490	419.746825	6.548736
6.256112	410.880284	6.553741
5.968600	425.535859	6.558746
6.314618	411.076838	6.563750
6.335076	417.309544	6.568755
5.502564	402.870665	6.573760
6.025006	400.241977	6.578765
6.054467	410.095833	6.583770
6.340097	410.199816	6.588774
6.164727	404.219252	6.593779
5.856038	395.703220	6.598784
5.983393	395.642172	6.603789
5.690314	391.239813	6.608794
5.677086	388.824773	6.613798
5.949223	408.847054	6.618803
5.664212	417.646016	6.623808
5.855271	415.233765	6.628813
6.000530	422.408718	6.633818
6.288261	417.668573	6.638822
6.320485	410.646224	6.643827
5.877889	422.826684	6.648832
5.969832	408.790295	6.653837
5.834936	410.301623	6.658842
6.030664	412.257866	6.663846
5.975309	412.295050	6.668851
6.192560	413.605668	6.673856
6.235303	419.167319	6.678861
5.920792	413.515442	6.683866
5.929204	420.711836	6.688870
6.182740	414.765308	6.693875
5.718917	406.656399	6.698880
6.126171	406.560988	6.703885
5.679957	409.487860	6.708890
6.327250	408.560722	6.713894
5.940541	412.822892	6.718899
6.068298	412.173312	6.723904
5.793863	395.321597	6.728909
6.199152	413.503831	6.733914
6.100598	398.864534	6.738918
5.706311	382.737139	6.743923
5.779202	406.378394	6.748928
5.784635	405.399961	6.753933
5.952094	418.066975	6.758938
6.108071	409.800841	6.763942
5.939651	411.763519	6.768947
5.931389	417.617903	6.773952
6.276435	410.885069	6.778957
5.942832	416.863196	6.783962
6.175140	412.685403	6.788966
6.451373	399.676860	6.793971
6.112553	404.738295	6.798976
6.052248	392.190618	6.803981
5.635803	404.534651	6.808986
5.997560	389.646066	6.813990
6.287771	396.219321	6.818995
5.754120	391.788215	6.824000
6.007729	385.908125	6.829005
5.829132	394.734696	6.834010
5.837909	393.278005	6.839014
5.845024	397.930891	6.844019
6.338977	404.529174	6.849024
6.447760	392.575111	6.854029
5.839508	391.942773	6.859034
6.163374	391.164390	6.864038
5.888314	393.767045	6.869043
5.697955	395.065594	6.874048
5.607356	386.787483	6.879053
5.568542	394.427871	6.884058
5.862094	403.740464	6.889062
6.038261	407.987207	6.894067
5.760465	418.417566	6.899072
5.948217	414.911155	6.904077
5.806884	417.948450	6.909082
5.835871	415.688146	6.914086
6.183383	421.581703	6.919091
5.910077	417.033868	6.924096
6.112723	417.574803	6.929101
6.160853	423.711425	6.934106
5.722699	409.875153	6.939110
5.987228	407.853197	6.944115
6.098540	417.608810	6.949120
6.645535	412.774259	6.954125
6.298446	416.815082	6.959130
6.237082	402.957745	6.964134
5.938157	398.040599	6.969139
5.818203	391.725483	6.974144
5.974558	391.482719	6.979149
5.832210	398.047817	6.984154
5.859823	405.817009	6.989158
6.149686	412.444109	6.994163
5.975253	405.232674	6.999168
6.135382	403.651026	7.004173
6.136697	394.206884	7.009178
6.034009	385.908521	7.014182
5.627039	385.725545	7.019187
5.934186	391.188811	7.024192
6.041551	402.843320	7.029197
5.745021	405.556910	7.034202
6.134397	414.234387	7.039206
6.358518	402.233772	7.044211
5.952097	397.953575	7.049216
6.049930	388.412054	7.054221
5.998850	390.821424	7.059226
6.232301	385.855670	7.064230
5.760718	382.133026	7.069235
5.600693	380.367421	7.074240
6.034396	391.186166	7.079245
5.860441	404.431856	7.084250
6.129338	405.237663	7.089254
6.204752	405.630851	7.094259
6.120531	399.158272	7.099264
5.994418	393.381968	7.104269
5.436551	396.911637	7.109274
5.707299	404.933805	7.114278
6.091196	405.939896	7.119283
5.910607	411.897211	7.124288
6.327710	422.297790	7.129293
6.270052	415.805223	7.134298
6.222016	405.058989	7.139302
6.057828	394.058872	7.144307
5.671549	398.963224	7.149312
6.117616	391.907678	7.154317
5.910107	393.670831	7.159322
5.729025	384.767809	7.164326
5.867751	397.084963	7.169331
6.026893	407.972048	7.174336
6.306681	410.551047	7.179341
6.056370	405.411143	7.184346
5.929068	393.234637	7.189350
5.928462	394.911588	7.194355
6.028689	389.362418	7.199360
6.097067	392.904699	7.204365
5.953348	397.502122	7.209370
6.257930	384.327793	7.214374
5.826257	391.150196	7.219379
5.783390	390.622265	7.224384
6.243389	388.038164	7.229389
5.830607	390.912338	7.234394
5.779406	389.066405	7.239398
5.664689	391.549022	7.244403
5.842126	402.891990	7.249408
5.993609	404.042066	7.254413
6.072114	409.386134	7.259418
6.404014	403.892413	7.264422
6.070498	404.555320	7.269427
5.825073	396.924734	7.274432
6.095675	403.956652	7.279437
5.983851	400.867347	7.284442
6.063127	394.179324	7.289446
6.125902	393.938567	7.294451
5.925474	395.460161	7.299456
5.701347	387.848388	7.304461
5.251617	393.955436	7.309466
5.774247	408.294234	7.314470
5.997050	416.703577	7.319475
5.983614	417.487180	7.324480
6.314697	415.979988	7.329485
6.147682	415.560095	7.334490
6.281329	412.767691	7.339494
6.158780	422.563113	7.344499
6.348484	409.371963	7.349504
6.201135	402.168941	7.354509
5.765052	402.822609	7.359514
5.889821	405.577759	7.364518
5.852043	392.732318	7.369523
5.591522	388.097064	7.374528
5.905229	400.785445	7.379533
5.592004	411.619991	7.384538
6.152472	410.459680	7.389542
6.320768	407.108181	7.394547
6.506249	411.356630	7.399552
5.917837	411.303324	7.404557
5.779843	400.808473	7.409562
6.138392	404.972855	7.414566
6.115747	394.409313	7.419571
5.812776	393.944283	7.424576
6.243397	395.294235	7.429581
5.670347	397.924597	7.434586
6.143285	393.231371	7.439590
6.138635	394.858334	7.444595
5.654475	383.098423	7.449600
6.211986	392.562644	7.454605
6.037105	394.168822	7.459610
6.072525	397.459998	7.464614
5.713042	392.884542	7.469619
5.863571	394.870012	7.474624
5.906871	396.533756	7.479629
6.060362	409.943284	7.484634
5.910819	411.197474	7.489638
6.292422	406.085113	7.494643
5.898399	404.204306	7.499648
5.795321	393.688169	7.504653
5.626782	407.667016	7.509658
6.178333	417.274556	7.514662
6.315001	409.081051	7.519667
6.129110	418.788317	7.524672
6.012056	395.751998	7.529677
5.683574	395.129610	7.534682
6.045711	401.751710	7.539686
5.790429	408.052926	7.544691
6.192678	414.327054	7.549696
6.341099	408.539369	7.554701
6.105005	399.806313	7.559706
6.006594	388.305503	7.564710
5.917581	392.701361	7.569715
5.692905	388.114276	7.574720
5.864592	378.621301	7.579725
5.517459	397.313720	7.584730
6.097368	411.877669	7.589734
6.304518	408.763696	7.594739
5.970484	414.317939	7.599744
6.217438	414.684250	7.604749
5.936019	405.591291	7.609754
6.106704	398.316294	7.614758
5.903575	391.536475	7.619763
5.742902	391.922360	7.624768
6.181741	399.965646	7.629773
5.857305	403.670717	7.634778
6.311076	411.828730	7.639782
5.980891	399.835871	7.644787
5.475118	403.034670	7.649792
6.040606	399.972123	7.654797
6.191904	406.203308	7.659802
6.237806	412.726260	7.664806
6.525012	397.472856	7.669811
6.002379	397.769919	7.674816
5.642215	385.563464	7.679821
5.818209	394.223743	7.684826
6.121745	383.355997	7.689830
6.173937	388.862373	7.694835
6.093493	400.960765	7.699840
6.137596	390.310836	7.704845
6.016737	401.222805	7.709850
5.822863	386.424445	7.714854
6.044465	383.744817	7.719859
6.157970	392.968553	7.724864
6.508527	388.490659	7.729869
5.674819	390.361417	7.734874
5.882186	381.245671	7.739878
6.115253	385.828349	7.744883
5.761510	391.401492	7.749888
6.071922	389.691893	7.754893
5.937389	396.689207	7.759898
5.871943	393.779302	7.764902
5.789017	386.645288	7.769907
5.733740	391.665458	7.774912
5.977771	388.023681	7.779917
5.617813	390.823138	7.784922
5.897720	391.450046	7.789926
5.798482	394.240292	7.794931
6.104292	411.587045	7.799936
6.637319	409.633753	7.804941
5.967827	401.927237	7.809946
5.948368	394.628248	7.814950
5.913295	393.501136	7.819955
5.604462	393.198379	7.824960
6.140451	399.451546	7.829965
5.839589	386.631511	7.834970
5.937191	397.037841	7.839974
6.373305	400.895835	7.844979
5.673590	401.600300	7.849984
5.826082	398.162693	7.854989
6.003777	407.275137	7.859994
6.115203	411.234627	7.864998
5.837021	393.098993	7.870003
5.953412	414.110644	7.875008
6.146022	412.451139	7.880013
6.112892	418.575180	7.885018
6.064276	411.986284	7.890022
5.970438	396.909644	7.895027
5.451399	404.799289	7.900032
6.052067	410.605720	7.905037
5.972867	410.580200	7.910042
5.724734	422.926348	7.915046
6.485591	422.288307	7.920051
6.022675	419.858297	7.925056
5.777458	408.813918	7.930061
6.006940	415.855447	7.935066
6.058813	420.074211	7.940070
6.064127	421.690124	7.945075
5.870910	420.995921	7.950080
6.121001	412.088604	7.955085
5.978367	421.795421	7.960090
5.771678	413.782264	7.965094
6.202922	423.095440	7.970099
5.941037	415.407312	7.975104
5.819494	419.336866	7.980109
6.255438	423.533419	7.985114
6.028975	415.880871	7.990118
5.800597	410.844703	7.995136
5.742587	415.836744	8.000154
5.939717	412.277775	8.005171
5.812905	424.794421	8.010189
5.846760	423.552102	8.015206
6.231304	424.722628	8.020224
6.164696	420.636945	8.025242
6.046639	415.644160	8.030259
6.064120	422.798682	8.035277
6.276057	425.511009	8.040294
6.136802	413.787190	8.045312
6.026113	414.776538	8.050330
6.316856	409.606096	8.055347
6.136958	404.623003	8.060365
5.632901	395.430454	8.065382
5.740143	399.064878	8.070400
5.897317	412.408004	8.075418
6.100582	414.522097	8.080435
6.106756	419.087525	8.085453
5.918182	420.136413	8.090470
6.186798	416.503127	8.095488
6.019901	413.711236	8.100506
6.510193	414.631667	8.105523
6.233994	426.890860	8.110541
6.058844	418.606112	8.115558
6.032153	420.977137	8.120576
6.154579	424.148449	8.125594
6.029692	415.300415	8.130611
6.091045	414.167395	8.135629
6.283453	418.347045	8.140646
6.451238	417.945259	8.145664
5.882089	426.797970	8.150682
6.036611	415.757097	8.155699
6.321288	419.941224	8.160717
6.244821	420.622259	8.165734
6.413879	413.403871	8.170752
5.850492	414.363165	8.175770
5.971798	418.279405	8.180787
6.055047	419.705417	8.185805
6.058157	419.076973	8.190822
6.248223	408.929922	8.195840
6.133649	428.368350	8.200858
6.117945	422.223458	8.205875
6.004204	429.957110	8.210893
5.867917	424.257136	8.215910
6.033249	414.877647	8.220928
5.750303	416.282141	8.225946
6.010101	418.321106	8.230963
6.051739	417.317404	8.235981
6.116710	424.328789	8.240998
6.537267	425.670394	8.246016
5.888509	439.953997	8.251034
6.470723	436.448294	8.256051
6.719898	437.308677	8.261069
6.393064	434.213644	8.266086
6.438418	427.058813	8.271104
6.187656	435.221026	8.276122
6.171153	424.692929	8.281139
6.136487	426.995778	8.286157
6.319684	423.110793	8.291174
6.193076	414.499710	8.296192
6.164320	409.682279	8.301210
6.090577	420.294007	8.306227
6.678811	428.245869	8.311245
6.473144	428.663131	8.316262
6.205915	416.359769	8.321280
6.115880	415.768010	8.326298
6.274770	416.923399	8.331315
6.461481	427.371249	8.336333
6.245122	427.600841	8.341350
6.425227	418.578790	8.346368
6.340461	423.896912	8.351386
6.120792	429.037360	8.356403
6.473441	432.911046	8.361421
6.257397	441.266634	8.366438
6.556568	433.339899	8.371456
6.493818	446.528164	8.376474
6.548430	436.878838	8.381491
6.223515	421.829545	8.386509
5.997527	428.075493	8.391526
6.523261	427.743853	8.396544
6.672087	441.978230	8.401562
6.329248	445.048877	8.406579
6.551850	439.248486	8.411597
6.491633	430.283018	8.416614
6.386033	428.141071	8.421632
6.394482	423.245225	8.426650
6.761817	425.942671	8.431667
6.457783	422.528493	8.436685
6.115431	419.499009	8.441702
6.703571	428.921462	8.446720
6.455743	428.436475	8.451738
6.240619	423.417871	8.456755
6.395980	433.340472	8.461773
6.432673	446.500533	8.466790
6.728327	444.112682	8.471808
6.555622	443.966212	8.476826
6.551832	436.847478	8.481843
6.523123	424.244813	8.486861
6.299180	422.127720	8.491878
6.623324	425.128573	8.496896
6.686625	428.217632	8.501914
6.521486	431.522362	8.506931
6.456361	425.539844	8.511949
6.309087	424.726683	8.516966
6.631652	436.011615	8.521984
6.645845	451.024472	8.527002
7.095820	446.715836	8.532019
6.529819	435.172473	8.537037
6.225601	435.330626	8.542054
6.240309	418.770169	8.547072
6.503936	434.084750	8.552090
6.256223	449.391101	8.557107
6.554371	446.286504	8.562125
6.699402	449.100834	8.567143
6.782960	447.134371	8.572160
6.581553	446.506413	8.577178
6.406929	457.462167	8.582195
6.936900	439.258862	8.587213
6.651043	457.162065	8.592231
6.732907	447.688340	8.597248
6.539713	455.412362	8.602266
6.889443	449.535246	8.607283
6.761835	442.495869	8.612301
6.566029	437.288046	8.617319
6.587424	433.198039	8.622336
6.748671	443.738250	8.627354
6.828244	439.061625	8.632371
6.559889	427.512656	8.637389
6.652908	429.905951	8.642407
6.689654	439.541033	8.647424
6.837629	452.061980	8.652442
6.605336	441.438297	8.657459
6.614252	443.084237	8.662477
6.589190	450.740888	8.667495
6.806279	439.734377	8.672512
6.719601	439.691191	8.677530
6.563991	450.423060	8.682547
6.804063	441.934390	8.687565
6.444314	453.193697	8.692583
6.933261	448.048993	8.697600
6.987464	450.325298	8.702618
6.746389	454.276235	8.707635
6.924229	442.736239	8.712653
6.807498	436.370490	8.717671
6.895485	435.583583	8.722688
6.645429	428.875816	8.727706
6.765116	435.600927	8.732723
6.658510	430.559007	8.737741
6.607520	449.062862	8.742759
6.894211	441.106521	8.747776
7.267393	453.898292	8.752794
6.541222	438.242836	8.757811
6.666934	434.414191	8.762829
6.529983	450.760363	8.767847
6.481363	451.496996	8.772864
6.845449	438.905358	8.777882
6.637679	445.236819	8.782899
6.727078	447.394003	8.787917
6.622676	440.720213	8.792935
6.945525	446.526732	8.797952
6.951186	445.067926	8.802970
6.818740	447.278803	8.807987
6.960507	439.108489	8.813005
6.633968	449.305415	8.818023
7.026397	444.961616	8.823040
6.810881	444.357959	8.828058
6.824396	445.775964	8.833075
7.039317	445.726548	8.838093
6.674636	445.275648	8.843111
6.961531	437.549646	8.848128
6.778852	439.837819	8.853146
6.457666	450.008661	8.858163
6.662312	442.314479	8.863181
6.802616	457.361230	8.868199
7.081384	458.627224	8.873216
6.999664	455.503250	8.878234
7.068414	447.054043	8.883251
7.170555	441.240969	8.888269
6.936157	450.849114	8.893287
6.883152	443.264726	8.898304
7.117458	436.913403	8.903322
6.688616	449.013494	8.908339
6.787587	442.920054	8.913357
6.809643	465.915733	8.918375
6.929153	471.287068	8.923392
7.091718	459.755766	8.928410
7.248814	472.616120	8.933427
7.308669	469.356354	8.938445
6.959893	468.918740	8.943463
6.922313	459.962333	8.948480
7.478163	458.568797	8.953498
7.011291	449.543960	8.958515
7.299344	444.203519	8.963533
7.099957	453.632614	8.968551
7.289398	445.164498	8.973568
7.061974	438.046090	8.978586
6.627214	448.954236	8.983603
7.021164	450.325258	8.988621
6.913702	451.481357	8.993639
6.853613	445.037304	8.998656
7.241596	462.828622	9.003674
7.340107	458.723372	9.008691
7.228207	450.599109	9.013709
6.604200	456.598166	9.018727
6.794687	466.969709	9.023744
7.229857	473.048967	9.028762
7.456390	477.756607	9.033779
7.490388	472.597972	9.038797
7.267224	455.462535	9.043815
7.040184	457.615652	9.048832
7.122852	443.117852	9.053850
7.054371	457.301083	9.058867
7.538266	446.672480	9.063885
7.223923	445.718240	9.068903
6.842324	452.616572	9.073920
7.049208	453.688706	9.078938
7.196144	467.005076	9.083955
7.317484	461.457225	9.088973
7.213470	467.463174	9.093991
7.119783	471.397333	9.099008
7.442501	464.009684	9.104026
7.266739	473.608653	9.109043
7.163818	468.029667	9.114061
7.418701	467.727841	9.119079
7.026127	458.129635	9.124096
7.270859	457.409684	9.129114
7.097482	479.965796	9.134131
7.452895	469.130095	9.139149
7.150974	479.645068	9.144167
7.301248	469.412700	9.149184
7.345587	471.125674	9.154202
7.152044	474.419083	9.159219
7.230213	471.055463	9.164237
7.136692	470.814537	9.169255
6.989814	477.751840	9.174272
7.069399	473.264550	9.179290
7.009347	466.104128	9.184307
6.972694	461.275298	9.189325
6.880754	468.765713	9.194343
6.495691	486.649775	9.199360
7.170694	487.885247	9.204378
7.092960	488.108899	9.209395
7.615485	496.976788	9.214413
7.527628	493.737006	9.219431
7.434859	486.651128	9.224448
7.479658	494.066482	9.229466
7.519518	501.318514	9.234483
7.746246	489.404760	9.239501
7.745199	492.393461	9.244519
7.398290	488.433731	9.249536
7.280224	481.746288	9.254554
7.112188	490.845447	9.259571
7.191072	484.982354	9.264589
7.368819	482.174322	9.269607
7.651424	491.575253	9.274624
7.583798	488.669968	9.279642
7.586221	498.600788	9.284659
7.465929	492.308160	9.289677
7.570408	496.558409	9.294695
7.643156	498.910709	9.299712
7.651293	490.792866	9.304730
7.217193	480.727790	9.309747
7.312198	485.557024	9.314765
7.367719	489.041782	9.319783
7.274798	500.843126	9.324800
7.617476	494.332794	9.329818
7.422136	488.190779	9.334835
7.465473	485.072451	9.339853
7.646703	493.668771	9.344871
7.341859	498.065203	9.349888
7.534055	490.922052	9.354906
7.307641	495.454516	9.359923
7.438653	498.968472	9.364941
7.609426	500.923567	9.369959
7.669305	493.769589	9.374976
7.783655	478.919663	9.379994
7.702806	495.837745	9.385011
7.421826	499.712894	9.390029
7.834481	498.707860	9.395047
7.812439	496.054203	9.400064
7.655808	494.942709	9.405082
7.938686	495.040432	9.410099
7.838337	489.659850	9.415117
8.050310	491.876728	9.420135
7.722838	480.441126	9.425152
7.449756	476.422495	9.430170
7.506289	483.223790	9.435187
7.726652	488.737116	9.440205
7.854577	486.037874	9.445223
7.295216	478.510718	9.450240
7.713837	483.087278	9.455258
7.323511	479.456239	9.460275
7.399336	487.188616	9.465293
7.646068	489.305375	9.470311
7.566728	491.246009	9.475328
7.912929	483.671639	9.480346
7.466103	493.290999	9.485363
7.609086	495.291473	9.490381
7.606617	491.937327	9.495399
7.566761	503.124454	9.500416
7.702678	492.985839	9.505434
7.843393	493.541332	9.510451
7.770296	489.403003	9.515469
7.855297	490.958131	9.520487
7.751116	489.822641	9.525504
7.757496	488.849705	9.530522
7.708540	486.411702	9.535539
7.624506	488.555040	9.540557
7.671464	502.117470	9.545575
7.591372	500.650006	9.550592
7.748536	498.211264	9.555610
7.462406	503.841822	9.560627
7.895595	510.467349	9.565645
8.054725	506.447262	9.570663
8.059790	507.891843	9.575680
7.898807	499.462827	9.580698
7.652925	499.996843	9.585715
7.647984	500.732945	9.590733
7.758405	495.448723	9.595751
8.021686	520.003489	9.600768
8.083838	516.421467	9.605786
8.020010	503.997814	9.610803
7.767050	494.977307	9.615821
7.878760	488.184434	9.620839
7.640314	500.330466	9.625856
8.003590	502.820280	9.630874
7.958742	513.739956	9.635891
8.157105	518.827556	9.640909
7.802633	509.488435	9.645927
7.777120	515.270664	9.650944
7.606381	521.015690	9.655962
8.134240	523.918371	9.660979
7.702242	512.637980	9.665997
8.095259	518.872179	9.671015
8.030838	520.236130	9.676032
8.001926	519.360239	9.681050
8.172170	527.074684	9.686067
8.107902	524.714813	9.691085
8.359397	514.103647	9.696103
7.830973	521.167020	9.701120
8.304765	519.852608	9.706138
8.064046	510.486197	9.711155
7.896743	511.067860	9.716173
8.194549	509.291880	9.721191
8.016306	511.248013	9.726208
7.909125	509.917334	9.731226
7.959889	509.887326	9.736243
8.014995	514.842738	9.741261
8.319790	518.954310	9.746279
8.343287	518.351071	9.751296
8.026729	509.649785	9.756314
8.126418	503.616171	9.761331
7.775659	503.510222	9.766349
7.965532	508.277261	9.771367
7.949161	520.767203	9.776384
8.209855	519.098022	9.781402
8.450932	514.370826	9.786419
8.088191	526.053520	9.791437
8.157399	516.263010	9.796455
8.043901	516.672144	9.801472
8.110715	518.930704	9.806490
8.165748	523.819858	9.811507
8.244414	528.004732	9.816525
8.247812	528.512314	9.821543
8.058407	529.936874	9.826560
8.201000	531.435646	9.831578
8.578137	530.130066	9.836595
8.111843	537.884290	9.841613
7.739605	532.678836	9.846631
8.065366	527.322995	9.851648
7.861262	527.389725	9.856666
7.798414	529.665445	9.861683
7.845640	539.488285	9.866701
8.195279	524.825514	9.871719
8.005947	532.299658	9.876736
8.133112	530.692421	9.881754
8.462329	539.786278	9.886771
8.359868	545.889838	9.891789
8.370339	536.521925	9.896807
8.387828	533.836823	9.901824
8.246239	538.523262	9.906842
8.180576	538.741867	9.911859
8.200774	540.250350	9.916877
8.601681	538.821126	9.921895
8.112688	537.080059	9.926912
8.329066	542.022833	9.931930
8.526689	549.445823	9.936947
8.376258	552.808230	9.941965
8.370039	553.749659	9.946983
8.594646	552.060882	9.952000
8.375234	547.497346	9.957018
8.495780	537.130743	9.962035
8.280942	537.729323	9.967053
8.783310	533.093725	9.972071
8.793220	525.701414	9.977088
8.310445	524.552657	9.982106
8.559123	514.450010	9.987123
8.583877	523.506356	9.992141
8.307722	514.738778	9.997159
8.152151	529.020918	10.002176
8.381294	523.598167	10.007194
8.443131	531.752470	10.012211
8.152830	526.073439	10.017229
8.652997	534.594562	10.022247
8.464064	536.142122	10.027264
8.275717	544.635429	10.032282
8.855036	537.964929	10.037299
8.013651	530.371486	10.042317
8.388139	539.915835	10.047335
8.138307	549.415999	10.052352
8.295959	556.040534	10.057370
8.527859	547.666702	10.062387
8.454771	554.832312	10.067405
8.572801	548.641177	10.072423
8.696080	546.264541	10.077440
8.455603	551.149512	10.082458
8.481379	543.211916	10.087475
8.397652	558.410617	10.092493
8.767938	554.145999	10.097511
8.557834	551.685899	10.102528
8.622404	542.413648	10.107546
8.805331	550.179763	10.112563
8.190954	545.880080	10.117581
8.534119	548.224730	10.122599
8.541131	551.114350	10.127616
8.497214	559.742822	10.132634
8.240528	552.834078	10.137651
8.191323	562.214453	10.142669
8.669071	566.447259	10.147687
8.488468	570.985186	10.152704
8.678518	574.117527	10.157722
9.132495	574.204222	10.162739
8.914263	578.173698	10.167757
9.136710	573.114894	10.172775
8.621398	562.279866	10.177792
8.546099	558.274408	10.182810
9.009916	553.632223	10.187827
8.569585	555.594711	10.192845
8.530935	550.273870	10.197863
8.657529	562.839270	10.202880
8.905841	572.693737	10.207898
9.116791	565.424542	10.212915
8.840562	560.860437	10.217933
8.662002	556.186358	10.222951
8.721268	550.474638	10.227968
8.813522	555.465266	10.232986
8.553728	554.130093	10.238003
8.596755	568.507378	10.243021
9.031501	570.957602	10.248039
8.996923	575.646219	10.253056
8.695752	581.878754	10.258074
8.982876	573.915975	10.263091
8.751852	585.953606	10.268109
9.009858	571.507124	10.273127
9.010602	574.116866	10.278144
8.982857	568.131599	10.283162
9.218387	565.743684	10.288179
8.929712	561.721165	10.293197
8.881317	555.382536	10.298215
8.505185	543.010945	10.303232
8.772525	573.333887	10.308250
9.057875	565.074747	10.313267
8.656326	569.571554	10.318285
8.928788	573.631402	10.323303
9.036421	572.857189	10.328320
8.901379	583.674277	10.333338
9.261356	579.095691	10.338355
8.930596	584.057932	10.343373
9.035906	577.676278	10.348391
9.426150	577.072378	10.353408
9.138844	575.223967	10.358426
8.895673	554.740142	10.363443
8.802898	557.916793	10.368461
9.286904	566.298453	10.373479
9.058273	565.860947	10.378496
8.821330	574.144133	10.383514
9.481507	570.443155	10.388531
9.170314	565.960265	10.393549
8.983110	551.873885	10.398567
9.223678	545.392156	10.403584
8.760408	541.542163	10.408602
9.233256	551.945253	10.413619
8.787732	547.420300	10.418637
8.955249	562.724805	10.423655
9.308387	564.777565	10.428672
8.990436	578.296243	10.433690
9.673966	570.182994	10.438707
9.207121	566.645977	10.443725
8.926850	552.438481	10.448743
8.868355	547.076569	10.453760
8.941775	566.028106	10.458778
9.323408	560.644567	10.463795
9.393113	568.015024	10.468813
9.451615	564.256841	10.473831
9.468161	561.107984	10.478848
9.168599	549.169355	10.483866
9.193438	547.590772	10.488883
8.933833	550.575814	10.493901
8.694030	559.026697	10.498919
9.245396	567.467230	10.503936
9.000812	566.896525	10.508954
9.255234	564.530897	10.513971
9.499615	569.646014	10.518989
8.917424	567.184252	10.524007
9.023212	570.954637	10.529024
9.188434	576.110560	10.534042
9.470767	572.604481	10.539059
9.498024	563.839832	10.544077
9.311197	565.661617	10.549095
9.304460	565.930950	10.554112
9.157622	572.786234	10.559130
9.369244	567.164245	10.564147
9.218328	568.503883	10.569165
9.030076	568.902640	10.574183
9.457475	570.883806	10.579200
9.259851	573.578276	10.584218
9.219809	565.486882	10.589235
9.407458	568.509146	10.594253
9.269396	570.626245	10.599271
9.400668	567.857039	10.604288
9.241183	573.732861	10.609306
9.523718	570.037404	10.614323
9.278631	573.461982	10.619341
9.555739	573.570078	10.624359
9.517015	578.862097	10.629376
9.482336	573.928786	10.634394
9.474699	568.735623	10.639411
9.173914	575.050145	10.644429
9.532190	589.895600	10.649447
10.034883	595.721326	10.654464
9.884370	578.953080	10.659482
9.379280	574.582618	10.664499
9.477910	569.600020	10.669517
9.290866	575.271879	10.674535
9.370566	571.838574	10.679552
9.543082	581.417746	10.684570
9.772404	570.513378	10.689587
9.521767	573.077301	10.694605
9.465509	574.989081	10.699623
9.779178	568.618965	10.704640
9.688191	569.075065	10.709658
9.601583	570.811722	10.714675
9.639286	578.534332	10.719693
9.539857	565.756457	10.724711
9.737329	572.201192	10.729728
9.290507	574.969420	10.734746
9.641842	582.551375	10.739763
9.553566	584.846866	10.744781
9.757536	594.957598	10.749799
9.944932	595.070283	10.754816
9.614697	580.182634	10.759834
9.567276	588.556052	10.764851
9.651056	588.284189	10.769869
9.613347	599.874978	10.774887
10.062159	598.974726	10.779904
9.488826	588.192953	10.784922
10.010055	583.860497	10.789939
9.571274	582.720622	10.794957
9.332603	586.128419	10.799975
9.841227	589.491711	10.804992
9.944849	604.427570	10.810010
9.863727	603.951172	10.815027
9.801926	602.850058	10.820045
9.705789	598.226169	10.825063
9.793211	597.505615	10.830080
9.701856	607.454345	10.835098
9.846978	607.955502	10.840115
9.985284	601.158419	10.845133
9.591822	604.429527	10.850151
10.025420	599.782597	10.855168
9.927415	608.078744	10.860186
9.850755	595.900033	10.865203
9.694051	601.339931	10.870221
9.864315	610.938406	10.875239
9.901811	594.939099	10.880256
9.846978	603.613484	10.885274
9.863855	598.520612	10.890291
9.981332	597.710142	10.895309
9.493044	608.008240	10.900327
9.997562	610.397045	10.905344
9.880814	608.121125	10.910362
9.880156	615.243853	10.915379
9.861969	608.297718	10.920397
9.690795	618.325232	10.925415
9.507189	597.898295	10.930432
9.577707	608.342366	10.935450
9.456951	602.974414	10.940467
10.143858	607.976026	10.945485
9.996369	624.459707	10.950503
10.386427	629.359514	10.955520
10.169472	614.750731	10.960538
9.887464	599.741901	10.965555
9.719184	603.769827	10.970573
9.998959	620.760912	10.975591
10.308676	622.296622	10.980608
10.450797	624.316180	10.985626
10.081541	615.058215	10.990643
9.874877	601.871085	10.995661
10.021174	606.218949	11.000679
10.289374	615.388675	11.005696
10.328783	614.145472	11.010714
9.974602	609.770292	11.015731
9.922927	607.641965	11.020749
9.852752	617.095081	11.025767
10.494808	612.904632	11.030784
10.518954	619.120922	11.035802
10.224521	611.230311	11.040819
10.385840	604.117199	11.045837
10.228111	600.926214	11.050855
10.423256	602.842788	11.055872
10.068919	603.049820	11.060890
9.687707	600.405086	11.065907
10.603885	604.821670	11.070925
10.252524	611.677455	11.075943
10.059678	603.534247	11.080960
10.344968	609.709619	11.085978
10.094162	608.549757	11.090995
10.344436	619.183418	11.096013
10.391409	621.609200	11.101031
10.470746	607.581999	11.106048
10.188925	614.625705	11.111066
10.181251	604.594730	11.116083
10.661514	614.914646	11.121101
10.098864	610.957133	11.126119
10.482282	605.854165	11.131136
10.481436	599.896231	11.136154
10.641730	605.299086	11.141171
10.332002	601.727977	11.146189
10.232710	608.326518	11.151207
10.452731	596.801904	11.156224
10.160444	600.426385	11.161242
9.997426	606.318549	11.166259
10.305706	612.651264	11.171277
10.462027	616.388495	11.176295
10.360466	625.603538	11.181312
10.506470	628.613403	11.186330
10.404837	623.873604	11.191347
10.760400	622.577709	11.196365
10.478027	631.578090	11.201383
10.954082	634.081811	11.206400
10.270365	625.977633	11.211418
10.288202	629.859640	11.216435
10.645912	624.694423	11.221453
10.770603	624.195244	11.226471
10.790626	623.917591	11.231488
10.638574	616.206639	11.236506
10.434569	603.681805	11.241523
10.746359	608.975718	11.246541
10.259798	610.049215	11.251559
10.656867	607.333030	11.256576
10.433543	612.511973	11.261594
10.633542	624.586238	11.266611
10.655636	619.527256	11.271629
10.575072	624.125261	11.276647
10.942710	632.427356	11.281664
10.960907	619.141867	11.286682
10.551458	611.878341	11.291699
10.596624	599.336560	11.296717
10.663906	599.165110	11.301735
10.694492	598.481863	11.306752
10.692570	602.152367	11.311770
10.541551	606.685668	11.316787
10.899363	606.872637	11.321805
10.155977	611.520843	11.326823
10.594182	618.167715	11.331840
10.601791	622.212267	11.336858
10.717737	635.786081	11.341875
11.138124	629.796851	11.346893
10.876219	637.377083	11.351911
10.742378	635.110149	11.356928
10.772828	632.987885	11.361946
10.511941	629.349158	11.366963
10.816167	629.692845	11.371981
10.756163	630.980374	11.376999
10.486547	627.283055	11.382016
10.597349	627.006957	11.387034
10.649471	629.387753	11.392051
10.920272	624.387630	11.397069
10.769707	631.429711	11.402087
10.865779	633.273450	11.407104
10.707350	621.016016	11.412122
10.492804	628.289025	11.417139
10.545063	627.832753	11.422157
10.653585	636.390041	11.427175
10.994608	641.531062	11.432192
11.236449	646.390981	11.437210
10.851503	650.140442	11.442227
11.193288	636.886290	11.447245
10.850805	639.653959	11.452263
10.856718	635.986051	11.457280
10.839299	645.658133	11.462298
10.606297	655.240922	11.467315
10.889009	648.844070	11.472333
11.060849	659.351190	11.477351
11.081278	653.137442	11.482368
11.021533	650.060482	11.487386
10.824521	656.014794	11.492403
10.971171	647.054673	11.497421
11.124924	649.520533	11.502439
11.189767	645.256414	11.507456
11.241665	646.804120	11.512474
11.072990	647.348133	11.517491
11.199164	640.464574	11.522509
11.216152	635.150769	11.527527
11.316224	650.355464	11.532544
11.342442	647.299750	11.537562
11.057963	652.182175	11.542579
11.287564	648.627539	11.547597
11.144518	652.380124	11.552615
10.954293	649.885338	11.557632
11.002206	647.441603	11.562650
10.746371	649.289988	11.567667
10.921658	645.854315	11.572685
10.986365	647.630386	11.577703
11.001340	654.886379	11.582720
11.162886	650.736495	11.587738
10.817476	652.952362	11.592755
11.209501	661.610409	11.597773
11.577939	677.284317	11.602791
11.589077	671.494893	11.607808
11.595790	653.196632	11.612826
11.236645	659.170036	11.617843
11.560705	647.831059	11.622861
11.474457	642.438753	11.627879
11.055116	652.606154	11.632896
11.426090	650.821853	11.637914
11.134385	652.211958	11.642931
11.287139	645.781820	11.647949
11.449197	646.163561	11.652967
11.328054	652.462588	11.657984
11.452856	644.051843	11.663002
11.286968	649.272289	11.668019
11.723755	641.245006	11.673037
11.603943	642.958470	11.678055
11.329395	648.483117	11.683072
11.605687	652.151066	11.688090
11.215624	648.406343	11.693107
11.451712	641.489783	11.698125
11.334072	647.403253	11.703143
11.291847	645.598486	11.708160
11.331253	647.993899	11.713178
11.331309	657.959893	11.718195
11.634618	669.967509	11.723213
11.906731	671.742644	11.728231
11.954129	664.776745	11.733248
11.989425	651.255024	11.738266
11.506715	641.203785	11.743283
11.450789	643.730898	11.748301
11.405868	655.221869	11.753319
11.669346	643.936567	11.758336
12.115176	647.300242	11.763354
11.619502	646.301820	11.768371
11.886559	649.216982	11.773389
11.494254	642.906960	11.778407
11.260455	645.537682	11.783424
11.715430	638.299651	11.788442
11.447317	651.886315	11.793459
11.519313	642.928426	11.798477
11.511951	645.302765	11.803495
11.245495	647.458924	11.808512
11.815768	656.761223	11.813530
11.938273	671.315485	11.818547
11.747204	673.712299	11.823565
11.465112	673.175869	11.828583
11.678657	674.395295	11.833600
12.081140	677.305023	11.838618
11.731733	682.383820	11.843635
11.739877	676.175145	11.848653
11.597455	676.330039	11.853671
11.953864	676.334193	11.858688
11.526382	676.082473	11.863706
11.294249	675.168989	11.868723
11.500232	668.014140	11.873741
11.516292	667.118572	11.878759
11.343975	667.041467	11.883776
11.735689	671.410854	11.888794
11.849267	685.875009	11.893811
11.703523	696.946304	11.898829
11.940019	697.332163	11.903847
12.073750	697.551086	11.908864
12.500299	688.215732	11.913882
12.395557	690.545374	11.918899
12.170047	681.937035	11.923917
12.145725	676.579198	11.928935
11.991071	681.760024	11.933952
12.197233	676.385009	11.938970
11.745955	680.362618	11.943987
11.734928	672.339213	11.949005
12.046232	672.202113	11.954023
11.566570	676.559707	11.959040
11.969647	663.542083	11.964058
11.793896	681.226288	11.969075
11.948015	687.232890	11.974093
12.020912	689.291704	11.979111
11.863464	700.699349	11.984128
11.990855	700.568973	11.989146
11.998783	699.491643	11.994163
11.900788	690.677129	11.999181
12.215024	692.366771	12.004199
12.088262	686.832478	12.009216
12.670674	694.930538	12.014234
12.448623	687.946887	12.019251
12.334745	696.800981	12.024269
12.310925	694.712460	12.029287
12.078943	696.484529	12.034304
12.659369	681.854897	12.039322
12.302627	683.659136	12.044339
12.170859	667.844073	12.049357
12.338581	668.007178	12.054375
12.095188	667.609851	12.059392
12.122633	673.421704	12.064410
12.076811	679.664757	12.069427
11.937894	688.402850	12.074445
12.228357	692.781795	12.079463
12.109851	693.803941	12.084480
12.255862	689.968905	12.089498
12.216130	695.993260	12.094515
11.980911	690.356039	12.099533
12.552155	686.186135	12.104551
12.108724	696.256350	12.109568
12.440052	687.043213	12.114586
12.129789	692.866959	12.119603
12.172560	682.979515	12.124621
12.338110	693.039518	12.129639
12.437270	689.347522	12.134656
12.436963	688.719604	12.139674
12.407394	700.265003	12.144691
12.515600	696.426422	12.149709
12.725298	686.970411	12.154727
12.549963	696.345372	12.159744
12.542950	693.534697	12.164762
12.397346	695.993818	12.169779
12.468138	695.427343	12.174797
12.249821	686.956730	12.179815
12.249058	687.240907	12.184832
12.529955	704.130910	12.189850
12.616417	707.894885	12.194867
12.838461	714.118071	12.199885
12.851979	695.238035	12.204903
12.711375	694.531113	12.209920
12.807746	693.856490	12.214938
12.759903	695.170520	12.219955
12.590104	703.298080	12.224973
12.757181	692.362366	12.229991
13.037272	691.428584	12.235008
13.345108	690.114917	12.240026
13.062724	703.830088	12.245043
12.906632	700.777683	12.250061
13.223973	697.114616	12.255079
12.687036	683.155512	12.260096
12.543855	671.798210	12.265114
12.606668	681.634464	12.270131
12.664768	689.789426	12.275149
12.809620	691.262611	12.280167
12.637846	692.447737	12.285184
12.817750	687.045275	12.290202
12.813808	693.045087	12.295219
12.258717	692.541963	12.300237
12.714667	687.203546	12.305255
12.413288	685.723401	12.310272
12.359497	691.030437	12.315290
12.459708	683.743832	12.320307
12.320248	694.634262	12.325325
13.000339	700.684691	12.330343
12.753908	712.983597	12.335360
12.422464	717.592533	12.340378
12.346134	717.781253	12.345395
12.605313	723.424270	12.350413
12.778441	721.106072	12.355431
12.250290	720.122201	12.360448
13.225246	734.741767	12.365466
12.967731	736.953341	12.370483
12.961361	735.635252	12.375501
13.706214	738.406140	12.380519
13.245858	724.435005	12.385536
13.084283	721.667477	12.390554
13.215831	721.981417	12.395571
13.043410	715.062563	12.400589
13.345313	706.175917	12.405607
12.740379	716.284071	12.410624
12.806817	710.754213	12.415642
12.721953	708.785707	12.420659
12.720072	716.858561	12.425677
13.429061	732.188826	12.430695
13.203827	736.481325	12.435712
13.266370	730.197835	12.440730
13.172164	721.707759	12.445747
13.055483	721.214838	12.450765
13.317192	725.219601	12.455783
13.058365	723.006952	12.460800
13.196538	744.675142	12.465818
13.621997	741.156072	12.470835
13.501742	726.023962	12.475853
13.462995	718.970553	12.480871
13.188026	716.359648	12.485888
12.851153	708.541915	12.490906
13.232842	714.598078	12.495923
12.945114	725.757909	12.500941
13.267764	731.981118	12.505959
13.356151	736.808300	12.510976
13.434869	745.808967	12.515994
13.616905	739.986433	12.521011
13.091709	735.224607	12.526029
13.180256	742.080945	12.531047
12.939178	746.022478	12.536064
13.458585	739.799947	12.541082
13.615243	736.887882	12.546099
13.438059	748.036719	12.551117
13.758595	745.032704	12.556135
13.720856	748.566839	12.561152
13.542912	739.875280	12.566170
14.076082	741.587429	12.571187
13.472295	720.560312	12.576205
13.475079	714.604926	12.581223
12.930319	715.435084	12.586240
13.176165	726.388239	12.591258
13.619248	725.854951	12.596275
13.741449	732.901671	12.601293
13.763823	734.760123	12.606311
13.628689	737.637331	12.611328
13.278683	738.995552	12.616346
13.675574	736.648604	12.621363
13.383880	744.845774	12.626381
13.831151	735.724899	12.631399
13.727588	747.016834	12.636416
13.835376	747.432327	12.641434
13.870772	740.547173	12.646451
13.717459	737.061983	12.651469
13.695727	726.310465	12.656487
13.512961	724.912717	12.661504
13.876588	745.093916	12.666522
13.741263	742.798798	12.671539
13.482395	741.949459	12.676557
14.005219	739.787907	12.681575
13.562009	741.719308	12.686592
13.667989	738.916169	12.691610
13.845249	742.006362	12.696627
13.810394	737.208733	12.701645
13.680409	734.701341	12.706663
13.874655	737.993999	12.711680
13.675910	741.641721	12.716698
13.633406	730.994440	12.721715
13.231145	740.957244	12.726733
13.845005	737.216152	12.731751
13.660493	741.234029	12.736768
13.483491	733.435417	12.741786
14.019786	738.081969	12.746803
13.710511	740.427884	12.751821
13.787344	736.963438	12.756839
13.788812	746.455891	12.761856
13.729897	759.448126	12.766874
14.016308	759.333860	12.771891
14.176399	769.634603	12.776909
13.880817	767.449798	12.781927
14.099656	761.716165	12.786944
13.885422	765.795508	12.791962
14.015925	760.296623	12.796979
14.084122	757.871785	12.801997
14.264504	766.679809	12.807015
14.357544	766.046730	12.812032
14.139264	753.653415	12.817050
14.105764	753.194797	12.822067
14.103891	763.173775	12.827085
14.072626	754.828456	12.832103
14.174736	763.181683	12.837120
13.983977	763.886950	12.842138
14.311023	758.972652	12.847155
14.294264	766.044314	12.852173
14.254192	768.262848	12.857191
14.319101	763.014080	12.862208
14.326160	762.820507	12.867226
14.448968	756.265634	12.872243
14.267114	763.508329	12.877261
14.074841	747.803661	12.882279
13.904261	755.783044	12.887296
13.949427	764.388190	12.892314
14.213174	752.998636	12.897331
14.449511	770.795088	12.902349
14.663665	767.384860	12.907367
14.562810	767.492216	12.912384
14.387179	761.009348	12.917402
14.283100	764.361376	12.922419
14.373622	768.976794	12.927437
14.019945	764.005049	12.932455
14.326269	763.370111	12.937472
14.042906	772.418055	12.942490
14.630206	761.993970	12.947507
14.156471	763.668224	12.952525
14.258122	764.397104	12.957543
14.217739	763.179016	12.962560
14.390095	765.825013	12.967578
14.427697	755.168323	12.972595
14.585675	765.851247	12.977613
14.595647	772.006696	12.982631
14.715615	768.355604	12.987648
14.449288	765.333084	12.992666
14.632853	768.630577	12.997683
14.172615	767.661308	13.002701
14.646550	783.609114	13.007719
14.838284	790.648119	13.012736
14.823268	794.658385	13.017754
14.797772	778.618290	13.022771
14.566672	770.077056	13.027789
14.878960	767.339418	13.032807
14.470586	769.656683	13.037824
14.767043	773.378302	13.042842
14.769779	766.236324	13.047859
14.779967	766.405177	13.052877
14.771384	775.066087	13.057895
14.971986	781.885949	13.062912
14.715093	776.226849	13.067930
14.929643	762.411871	13.072947
14.708130	766.309318	13.077965
14.584234	764.438441	13.082983
15.065668	776.282520	13.088000
14.928820	778.954876	13.093018
14.908426	764.671778	13.098035
14.671687	770.184227	13.103053
14.561031	770.242627	13.108071
15.000909	791.506996	13.113088
14.778341	785.978215	13.118106
14.781909	785.289727	13.123123
15.002449	786.410235	13.128141
14.968853	782.937835	13.133159
14.997381	788.721153	13.138176
14.915016	788.374333	13.143194
15.005665	781.202795	13.148211
14.966354	786.599110	13.153229
14.758680	795.284911	13.158247
15.126151	795.820665	13.163264
15.176417	796.361936	13.168282
14.837606	782.589462	13.173299
14.857827	791.955924	13.178317
15.027756	789.631907	13.183335
15.147728	774.651466	13.188352
15.036217	786.244473	13.193370
15.031795	782.313067	13.198387
15.110669	786.942938	13.203405
15.333798	789.934434	13.208423
15.188832	781.714215	13.213440
14.729235	785.229247	13.218458
14.827935	787.801581	13.223475
14.776290	796.077928	13.228493
15.429753	804.136505	13.233511
15.471861	800.488138	13.238528
15.017804	804.242148	13.243546
15.284502	808.527015	13.248563
15.321430	813.103505	13.253581
15.203176	803.793490	13.258599
15.479625	801.818857	13.263616
15.223822	817.477085	13.268634
15.214950	807.490366	13.273651
15.298501	819.642968	13.278669
15.174886	812.082111	13.283687
15.433842	811.773330	13.288704
15.521793	805.725674	13.293722
15.678202	799.042445	13.298739
15.602363	806.363221	13.303757
15.531728	812.461885	13.308775
15.564851	800.938021	13.313792
15.699871	814.177622	13.318810
15.723504	803.690350	13.323827
15.299324	798.527670	13.328845
15.535614	804.887512	13.333863
16.120824	805.701575	13.338880
15.519771	794.999758	13.343898
15.146966	787.907144	13.348915
15.472760	796.395753	13.353933
15.195916	814.831233	13.358951
15.690858	801.158486	13.363968
15.229011	811.092794	13.368986
15.804632	807.158864	13.374003
15.593511	800.309156	13.379021
15.458164	809.804143	13.384039
16.073808	799.094728	13.389056
15.645033	805.041220	13.394074
15.816804	796.256970	13.399091
15.706324	804.293231	13.404109
15.560047	814.714586	13.409127
15.832367	794.512635	13.414144
15.544551	807.764833	13.419162
15.523462	806.193424	13.424179
15.748754	803.576708	13.429197
15.525606	807.752132	13.434215
15.926584	810.911427	13.439232
16.034737	815.726066	13.444250
15.634770	812.544595	13.449267
15.741048	805.515766	13.454285
15.454936	804.891599	13.459303
15.943868	812.852881	13.464320
15.915810	821.374854	13.469338
16.095552	829.116343	13.474355
16.054007	832.572196	13.479373
15.764276	820.388845	13.484391
16.369506	819.612398	13.489408
16.011379	817.339556	13.494426
16.158099	806.110316	13.499443
15.997812	806.103908	13.504461
15.563442	808.715586	13.509479
16.108504	821.900415	13.514496
16.293621	830.426861	13.519514
16.329440	827.824049	13.524531
15.943703	815.406435	13.529549
15.868034	826.659336	13.534567
16.283291	825.612852	13.539584
16.012370	832.626532	13.544602
16.264234	828.134251	13.549619
16.396834	826.775446	13.554637
16.089490	838.923035	13.559655
16.332048	826.555295	13.564672
16.334034	826.466658	13.569690
16.230403	819.950396	13.574707
16.162175	823.583997	13.579725
16.288573	827.366986	13.584743
16.529722	832.769865	13.589760
16.318602	823.351314	13.594778
16.126636	811.086380	13.599795
16.611308	817.530387	13.604813
16.356713	821.155317	13.609831
16.311872	810.483109	13.614848
16.617705	817.245471	13.619866
16.404371	817.168479	13.624883
16.077825	812.609037	13.629901
16.340990	822.041592	13.634919
16.625680	817.900777	13.639936
16.378953	827.791922	13.644954
16.336868	823.355166	13.649971
16.683299	820.050435	13.654989
16.509247	831.552284	13.660007
16.593293	825.199120	13.665024
16.331752	823.491814	13.670042
16.599009	829.439713	13.675059
16.516724	826.580850	13.680077
16.500429	825.674565	13.685095
16.422553	835.573973	13.690112
16.403162	828.470151	13.695130
16.133084	836.575613	13.700147
16.550806	822.056567	13.705165
16.314139	831.905113	13.710183
16.328088	826.263522	13.715200
16.602372	838.234774	13.720218
16.806299	848.661239	13.725235
16.889655	846.464389	13.730253
16.713833	843.134183	13.735271
16.794781	839.347179	13.740288
16.653562	842.427329	13.745306
16.403501	843.820391	13.750323
16.846755	851.504824	13.755341
16.632856	857.471316	13.760359
17.014739	859.308167	13.765376
16.789821	855.272436	13.770394
16.804877	849.337173	13.775411
17.084021	852.231541	13.780429
16.604497	858.637284	13.785447
16.924689	846.932712	13.790464
17.014286	847.849677	13.795482
17.163586	847.482336	13.800499
16.975999	845.681390	13.805517
16.877151	852.238926	13.810535
16.901227	853.043080	13.815552
16.978510	856.584461	13.820570
16.559237	861.039936	13.825587
17.107707	853.742988	13.830605
16.731746	864.919887	13.835623
16.607073	857.977716	13.840640
17.056120	850.873074	13.845658
16.684547	856.264663	13.850675
17.223450	858.916361	13.855693
17.058524	872.244026	13.860711
17.200473	871.413931	13.865728
17.437961	871.537705	13.870746
17.261569	858.452940	13.875763
17.320854	848.862620	13.880781
17.172703	850.214469	13.885799
17.133202	846.376907	13.890816
17.249023	838.633356	13.895834
17.346001	852.768886	13.900851
17.316888	850.157310	13.905869
17.175784	860.057171	13.910887
17.371078	867.670008	13.915904
17.334089	870.557106	13.920922
17.624041	875.119214	13.925939
17.586808	855.852481	13.930957
17.107327	852.983263	13.935975
17.290994	858.218431	13.940992
17.480244	865.317815	13.946010
17.710333	866.569376	13.951027
17.412423	855.359277	13.956045
17.301067	847.629224	13.961063
17.332465	863.053145	13.966080
17.683586	858.277060	13.971098
17.485770	874.582663	13.976115
17.756562	861.715011	13.981133
17.700516	871.955003	13.986151
17.503277	866.387515	13.991168
17.737003	861.860197	13.996186
17.583469	859.880343	14.001203
17.611760	855.457799	14.006221
17.532944	861.895435	14.011239
17.723841	863.137357	14.016256
17.756457	873.988312	14.021274
17.600510	867.862084	14.026291
17.820290	861.323537	14.031309
17.627543	867.917882	14.036327
17.863571	872.030844	14.041344
18.098001	867.165742	14.046362
17.774453	857.458673	14.051379
17.772912	849.686168	14.056397
17.452599	855.940732	14.061415
17.517800	862.071780	14.066432
17.726383	869.382732	14.071450
17.764340	873.397340	14.076467
18.120512	867.490676	14.081485
18.089226	867.729146	14.086503
17.829998	870.149288	14.091520
18.388428	862.806596	14.096538
17.748327	865.248543	14.101555
18.009449	866.381632	14.106573
17.823157	865.407306	14.111591
17.926654	871.418747	14.116608
18.295665	871.449330	14.121626
17.688440	868.805252	14.126643
17.917545	860.917709	14.131661
17.695038	866.582593	14.136679
17.768738	867.464180	14.141696
17.690187	858.633913	14.146714
17.905957	868.017113	14.151731
17.930346	879.730900	14.156749
18.155269	872.945389	14.161767
18.073753	870.897445	14.166784
18.112296	868.401499	14.171802
18.031909	889.943162	14.176819
18.216667	898.551748	14.181837
18.017373	902.003927	14.186855
18.051755	884.546856	14.191872
18.744650	890.020985	14.196890
18.488780	898.114781	14.201907
18.777820	889.125918	14.206925
18.424704	881.518938	14.211943
17.948035	877.295427	14.216960
18.489491	878.053233	14.221978
18.111627	878.718391	14.226995
18.670669	882.540903	14.232013
18.492803	871.760112	14.237031
17.848700	875.799534	14.242048
18.268953	889.975962	14.247066
18.135484	895.282920	14.252083
18.420654	892.325448	14.257101
18.554243	894.545190	14.262119
18.465036	897.841264	14.267136
18.558688	889.365856	14.272154
18.426766	902.473777	14.277171
18.328989	890.014149	14.282189
18.724692	893.694996	14.287207
18.554416	899.777744	14.292224
18.902311	898.038061	14.297242
18.769883	891.437921	14.302259
18.410941	886.940340	14.307277
18.709018	895.335509	14.312295
18.537001	887.384569	14.317312
18.577350	883.411411	14.322330
18.468196	884.946502	14.327347
18.706786	891.413313	14.332365
18.670365	892.308999	14.337383
18.413058	887.041251	14.342400
18.640134	895.390740	14.347418
18.732961	907.576663	14.352435
18.801386	898.717036	14.357453
19.051208	917.966358	14.362471
18.914152	914.213496	14.367488
18.981937	907.490462	14.372506
19.261229	913.512244	14.377523
18.547301	894.212638	14.382541
18.577073	896.868372	14.387559
18.389589	909.382240	14.392576
18.832813	907.952670	14.397594
18.961232	913.250159	14.402611
18.872042	920.569918	14.407629
19.057326	917.448209	14.412647
19.099332	909.520531	14.417664
19.291658	911.753164	14.422682
18.946877	915.029323	14.427699
19.031307	917.736457	14.432717
19.266597	911.154436	14.437735
18.768918	919.895204	14.442752
19.075407	914.031024	14.447770
19.142748	916.952276	14.452787
19.336722	915.889964	14.457805
18.996677	917.811531	14.462823
18.962929	914.216052	14.467840
19.558845	915.640675	14.472858
19.165868	918.971724	14.477875
19.386485	917.384525	14.482893
19.421717	902.284709	14.487911
19.467680	907.588804	14.492928
19.615257	909.604384	14.497946
19.389914	921.578234	14.502963
19.368796	908.743661	14.507981
19.415395	909.358095	14.512999
19.149362	908.083833	14.518016
19.695622	905.006555	14.523034
19.221061	920.058515	14.528051
19.297038	910.620182	14.533069
19.071904	913.205403	14.538087
19.286841	924.898832	14.543104
19.769101	929.134175	14.548122
19.435915	938.272060	14.553139
19.792210	930.629648	14.558157
20.093502	936.872055	14.563175
19.697317	925.898217	14.568192
19.454509	906.581587	14.573210
19.529230	911.404647	14.578227
19.535647	902.882940	14.583245
19.895375	922.339111	14.588263
19.783799	925.941655	14.593280
19.847685	906.507544	14.598298
19.640268	907.193335	14.603315
19.674082	907.961252	14.608333
19.400379	914.975400	14.613351
19.982233	919.106773	14.618368
19.883567	927.649327	14.623386
19.558810	934.879767	14.628403
19.869685	933.275269	14.633421
19.970725	932.883931	14.638439
19.795327	935.748543	14.643456
20.070997	934.493548	14.648474
19.940144	940.974079	14.653491
20.145570	923.417587	14.658509
20.355148	935.364328	14.663527
20.062444	916.298506	14.668544
20.295872	910.663526	14.673562
19.504061	908.064143	14.678579
19.482145	914.126806	14.683597
19.808191	925.544049	14.688615
20.308630	932.086613	14.693632
20.095195	938.185604	14.698650
19.981814	931.083844	14.703667
19.843765	938.928822	14.708685
20.234181	928.838449	14.713703
19.794686	938.905027	14.718720
20.026930	927.949491	14.723738
20.266464	930.824831	14.728755
20.096416	943.282342	14.733773
20.158034	931.163788	14.738791
20.015592	931.773127	14.743808
20.077183	924.192671	14.748826
20.178542	932.987912	14.753843
20.359634	949.786487	14.758861
20.746201	955.087724	14.763879
20.298384	938.646590	14.768896
20.447965	940.286315	14.773914
20.075520	942.708427	14.778931
20.310647	946.067303	14.783949
20.565930	942.650598	14.788967
20.383659	957.338053	14.793984
20.623448	956.287496	14.799002
20.553823	955.875559	14.804019
20.729687	960.916317	14.809037
20.874221	946.376857	14.814055
20.649688	933.656189	14.819072
20.552888	939.105739	14.824090
20.629891	925.694042	14.829107
20.167211	927.871511	14.834125
20.939987	935.731572	14.839143
20.399534	939.442340	14.844160
20.348345	937.831454	14.849178
20.712183	943.303507	14.854195
20.840792	955.916207	14.859213
20.911991	947.491627	14.864231
21.007459	954.612052	14.869248
20.716817	947.011034	14.874266
20.802128	944.753905	14.879283
20.393659	954.285450	14.884301
20.790406	956.741683	14.889319
20.630647	959.515485	14.894336
20.640534	956.228745	14.899354
20.534602	960.717202	14.904371
20.543235	959.510355	14.909389
20.784260	952.141617	14.914407
20.831952	956.340913	14.919424
20.717787	953.370259	14.924442
20.915689	956.416229	14.929459
21.092571	966.042262	14.934477
21.063068	962.499758	14.939495
20.975167	961.472140	14.944512
21.049573	978.034991	14.949530
21.023711	982.804401	14.954547
21.341085	973.760563	14.959565
21.341240	973.918367	14.964583
20.902776	968.246629	14.969600
21.009549	974.759370	14.974618
21.477452	975.888471	14.979635
21.136188	970.201502	14.984653
21.578692	974.922773	14.989671
21.242757	973.744666	14.994688
21.264951	964.213745	14.999706
21.392336	966.245118	15.004723
21.381388	976.645364	15.009741
20.948395	958.109568	15.014759
21.137009	973.537353	15.019776
21.186318	974.072469	15.024794
21.320472	969.614374	15.029811
21.223787	971.201168	15.034829
21.537189	973.307540	15.039847
21.459129	976.949024	15.044864
21.371930	968.322031	15.049882
21.554602	973.633129	15.054899
21.358052	979.066761	15.059917
21.843720	977.993457	15.064935
21.442953	972.757629	15.069952
21.469132	978.967414	15.074970
21.120052	974.174773	15.079987
21.320390	977.261391	15.085005
21.485259	971.611888	15.090023
21.131324	970.973094	15.095040
21.339134	988.382909	15.100058
21.832751	985.720970	15.105075
21.822929	1004.550314	15.110093
22.151347	997.347748	15.115111
22.048318	1002.649968	15.120128
21.799590	998.586376	15.125146
21.990032	992.415301	15.130163
22.082542	993.278167	15.135181
21.947368	972.511849	15.140199
21.869485	967.468433	15.145216
21.992496	983.588167	15.150234
21.634018	965.760219	15.155251
21.629159	983.206506	15.160269
21.767321	987.820828	15.165287
21.849115	994.094490	15.170304
21.916561	988.049986	15.175322
22.011998	992.882445	15.180339
22.143238	990.195231	15.185357
22.455908	985.223163	15.190375
22.129097	989.077195	15.195392
22.292919	997.483980	15.200410
22.704275	981.839166	15.205427
22.033894	984.787652	15.210445
22.201094	986.225802	15.215463
22.213780	983.749671	15.220480
22.118588	981.495571	15.225498
22.563360	977.411690	15.230515
21.893774	980.694570	15.235533
22.678748	981.048149	15.240551
22.241998	976.427035	15.245568
22.021756	980.542082	15.250586
22.361444	986.472374	15.255603
22.099597	994.119020	15.260621
22.561712	987.179536	15.265639
22.323200	991.732955	15.270656
22.199094	986.639970	15.275674
22.339680	989.398277	15.280691
22.353332	996.099188	15.285709
22.499674	982.004390	15.290727
22.069797	988.418179	15.295744
22.542348	989.657007	15.300762
22.672268	983.413366	15.305779
22.371451	984.836481	15.310797
22.640049	997.304199	15.315815
22.637069	989.632845	15.320832
22.708835	1002.077756	15.325850
22.633129	986.484004	15.330867
22.556231	994.423568	15.335885
22.591727	987.980122	15.340903
22.447308	996.813903	15.345920
22.631800	992.076513	15.350938
23.147401	1001.207677	15.355955
22.678224	1002.269003	15.360973
22.952671	985.951350	15.365991
22.756232	992.656774	15.371008
22.211930	1003.841199	15.376026
22.772333	1007.101785	15.381043
22.704463	1011.937745	15.386061
23.080052	1016.559057	15.391079
23.195811	1018.986739	15.396096
23.181251	1021.018268	15.401114
23.083723	1006.346269	15.406131
23.255954	1025.705696	15.411149
23.202930	1010.461824	15.416167
23.472658	1012.767551	15.421184
22.980961	1007.173569	15.426202
23.194564	999.114822	15.431219
22.622701	993.003223	15.436237
23.123322	1004.752930	15.441255
23.243792	1001.388895	15.446272
22.895625	1006.726368	15.451290
23.159066	1000.244047	15.456307
22.849604	1012.546722	15.461325
23.115140	1011.059777	15.466343
23.210442	1012.534442	15.471360
23.453124	1011.256207	15.476378
23.365882	1013.822993	15.481395
23.553064	1010.757777	15.486413
23.335193	1011.621937	15.491431
23.352485	1003.565543	15.496448
23.389402	1018.420681	15.501466
23.799480	1011.104328	15.506483
23.394214	1011.653862	15.511501
23.254854	1011.861928	15.516519
23.416995	997.142941	15.521536
23.283818	1006.347354	15.526554
23.416971	999.620356	15.531571
23.241681	1009.099616	15.536589
23.492907	1010.814942	15.541607
23.160653	1024.055327	15.546624
23.464012	1032.156239	15.551642
23.824041	1029.452107	15.556659
23.947489	1032.736978	15.561677
23.832266	1034.869488	15.566695
23.827191	1031.815456	15.571712
24.026638	1033.059207	15.576730
24.151517	1025.579247	15.581747
23.876039	1018.401862	15.586765
23.894013	1005.775692	15.591783
23.651596	1010.446493	15.596800
23.390870	1012.431383	15.601818
23.702894	1019.435852	15.606835
23.548324	1026.137884	15.611853
23.737167	1030.220406	15.616871
23.967174	1031.863318	15.621888
23.875300	1040.060873	15.626906
24.000469	1027.515724	15.631923
23.798490	1031.413323	15.636941
23.975126	1030.644059	15.641959
23.945506	1032.889391	15.646976
23.756997	1036.977388	15.651994
24.144042	1031.936849	15.657011
24.047630	1025.283679	15.662029
24.111922	1028.965987	15.667047
24.148865	1037.361112	15.672064
24.263279	1046.324779	15.677082
24.386481	1051.171840	15.682099
24.337869	1039.064171	15.687117
24.377515	1046.325926	15.692135
24.511626	1038.538396	15.697152
24.389353	1033.410396	15.702170
24.346471	1021.377582	15.707187
23.999149	1031.641212	15.712205
24.144009	1043.156347	15.717223
24.276524	1047.320283	15.722240
24.177563	1061.786485	15.727258
24.579720	1057.071780	15.732275
24.724574	1047.237569	15.737293
24.663456	1055.016895	15.742311
24.685504	1053.255666	15.747328
24.211630	1057.293703	15.752346
24.620795	1044.543097	15.757363
24.698952	1049.548696	15.762381
24.540514	1045.827557	15.767399
24.671031	1050.569328	15.772416
24.739635	1050.328239	15.777434
24.947117	1049.816077	15.782451
24.533794	1042.764423	15.787469
24.664862	1039.354538	15.792487
24.870284	1042.535047	15.797504
24.777626	1050.805315	15.802522
24.815890	1046.090822	15.807539
24.670572	1046.463927	15.812557
24.459525	1046.923070	15.817575
24.591757	1046.097646	15.822592
24.901771	1059.051231	15.827610
25.106718	1057.842023	15.832627
24.592098	1067.750027	15.837645
25.016403	1084.106673	15.842663
25.377005	1069.580597	15.847680
25.162464	1077.453400	15.852698
25.211703	1068.732397	15.857715
25.275316	1056.471432	15.862733
24.875520	1051.629910	15.867751
25.078220	1054.059754	15.872768
25.175655	1070.922045	15.877786
25.287345	1074.227700	15.882803
25.463451	1071.315690	15.887821
25.306851	1069.686593	15.892839
25.309790	1052.953820	15.897856
25.140568	1052.216653	15.902874
24.831918	1050.286328	15.907891
25.246379	1061.550947	15.912909
25.361136	1065.345279	15.917927
25.801733	1072.616808	15.922944
25.413978	1073.595952	15.927962
25.418650	1068.990860	15.932979
25.667926	1068.844541	15.937997
25.486072	1074.998591	15.943015
25.676587	1064.844786	15.948032
25.302972	1066.383457	15.953050
25.337449	1074.157282	15.958067
25.427077	1069.037097	15.963085
25.331852	1066.416912	15.968103
25.383800	1054.416557	15.973120
25.409185	1058.584657	15.978138
25.475533	1060.720280	15.983155
25.828483	1061.712761	15.988173
25.278027	1072.371164	15.993191
26.039959	1061.158984	15.998208
25.824690	1062.155285	16.003226
25.669060	1063.498853	16.008243
25.815429	1069.008174	16.013261
25.928515	1064.395565	16.018279
26.006166	1054.818035	16.023296
26.028671	1063.679345	16.028314
26.174278	1062.381602	16.033331
25.979710	1060.853130	16.038349
25.618018	1061.613592	16.043367
26.523687	1062.421642	16.048384
26.004774	1063.607532	16.053402
25.800204	1062.216329	16.058419
26.028554	1061.413714	16.063437
26.148243	1068.801794	16.068455
26.144183	1068.843493	16.073472
26.287720	1074.463715	16.078490
26.330364	1080.427955	16.083507
26.363748	1064.113286	16.088525
25.824305	1064.917378	16.093543
26.291679	1073.538574	16.098560
26.278278	1073.891011	16.103578
26.415008	1074.327224	16.108595
26.544204	1082.569058	16.113613
26.415058	1083.491905	16.118631
26.816767	1073.914086	16.123648
26.503117	1070.229885	16.128666
26.360049	1058.837603	16.133683
26.717918	1052.772820	16.138701
26.121299	1053.216635	16.143719
26.439764	1061.018543	16.148736
26.168300	1080.412833	16.153754
26.434981	1079.635771	16.158771
26.827731	1086.908491	16.163789
26.922950	1082.355481	16.168807
26.700426	1072.439959	16.173824
26.790285	1085.229238	16.178842
26.541855	1082.266975	16.183859
26.810400	1080.325109	16.188877
26.507770	1084.506738	16.193895
26.881671	1085.044649	16.198912
26.748477	1086.801278	16.203930
26.834764	1083.452051	16.208947
26.986635	1080.307147	16.213965
26.540786	1079.767958	16.218983
26.628135	1088.391898	16.224000
26.599838	1086.067343	16.229018
26.471216	1079.962008	16.234035
26.718328	1076.240439	16.239053
26.564944	1079.499263	16.244071
26.827973	1093.290226	16.249088
27.020812	1097.075486	16.254106
27.169745	1102.158375	16.259123
27.171026	1099.422077	16.264141
27.076188	1102.009001	16.269159
27.055687	1101.182258	16.274176
26.915308	1108.977182	16.279194
27.300775	1106.464717	16.284211
27.489150	1090.340339	16.289229
26.825342	1104.462722	16.294247
26.927087	1097.753231	16.299264
26.850889	1104.073777	16.304282
27.332020	1106.974410	16.309299
27.469850	1100.726333	16.314317
27.293560	1104.509468	16.319335
27.136224	1100.289519	16.324352
27.473103	1117.410989	16.329370
27.778896	1125.142326	16.334387
27.563103	1110.946372	16.339405
27.662659	1103.063241	16.344423
27.424923	1103.488697	16.349440
27.669007	1111.166579	16.354458
27.457455	1118.609734	16.359475
27.757153	1120.159682	16.364493
27.589714	1121.192675	16.369511
27.775274	1117.108349	16.374528
28.032782	1121.864957	16.379546
27.954676	1119.611319	16.384563
28.112646	1098.931470	16.389581
27.913321	1103.494556	16.394599
28.210658	1093.106244	16.399616
28.161582	1097.093512	16.404634
28.003425	1089.386467	16.409651
27.729130	1086.668101	16.414669
27.804344	1090.938857	16.419687
27.892466	1087.766069	16.424704
27.925501	1087.101355	16.429722
27.974006	1102.068358	16.434739
28.099154	1086.149553	16.439757
27.851039	1099.856502	16.444775
27.866153	1097.225337	16.449792
27.780472	1113.753435	16.454810
27.789313	1114.055049	16.459827
27.890472	1119.199077	16.464845
28.244710	1125.101889	16.469863
28.005372	1117.836749	16.474880
27.831365	1123.459400	16.479898
27.951688	1123.386935	16.484915
28.276467	1122.199973	16.489933
28.465740	1125.430366	16.494951
28.374581	1128.988725	16.499968
28.267340	1135.232093	16.504986
28.504478	1148.260279	16.510003
28.785551	1143.485626	16.515021
28.744779	1146.243970	16.520039
28.457141	1122.358118	16.525056
28.508555	1122.962337	16.530074
28.477617	1113.742623	16.535091
28.548412	1121.084736	16.540109
28.540399	1128.177262	16.545127
28.855131	1137.901713	16.550144
28.736585	1131.507597	16.555162
28.794037	1138.192231	16.560179
28.923042	1118.621452	16.565197
28.765350	1116.178308	16.570215
28.427696	1110.509664	16.575232
28.723772	1122.083210	16.580250
28.416123	1133.520977	16.585267
28.962121	1137.001599	16.590285
28.914390	1143.424998	16.595303
29.275973	1133.361119	16.600320
29.341148	1138.270944	16.605338
29.302258	1124.874100	16.610355
29.125404	1122.519166	16.615373
28.814015	1111.314172	16.620391
28.923345	1123.829024	16.625408
29.077754	1133.556500	16.630426
28.746101	1144.508875	16.635443
29.048796	1133.447499	16.640461
29.229529	1147.563829	16.645479
28.971147	1138.436544	16.650496
29.436382	1141.096672	16.655514
28.940596	1137.668216	16.660531
29.334394	1128.328298	16.665549
29.480136	1140.010619	16.670567
29.537463	1136.905765	16.675584
29.309243	1134.101276	16.680602
29.342621	1142.153019	16.685619
29.559089	1128.163885	16.690637
29.734332	1133.608741	16.695655
29.572449	1124.166537	16.700672
29.695292	1133.583372	16.705690
29.199819	1138.498987	16.710707
29.706616	1133.016771	16.715725
29.812229	1131.605366	16.720743
29.878490	1133.277099	16.725760
29.965745	1130.344286	16.730778
29.790350	1129.980475	16.735795
29.586156	1122.277473	16.740813
29.666442	1129.864260	16.745831
29.857733	1132.264344	16.750848
29.900317	1125.961751	16.755866
29.498046	1132.030433	16.760883
29.843038	1132.506602	16.765901
29.654137	1128.395736	16.770919
29.501720	1134.201205	16.775936
29.539713	1133.876546	16.780954
29.557955	1145.496794	16.785971
30.235477	1155.098139	16.790989
29.864573	1157.819846	16.796007
30.200659	1160.942034	16.801024
30.208973	1155.462171	16.806042
29.856639	1162.697023	16.811059
30.087285	1159.448243	16.816077
30.171193	1154.663453	16.821095
30.216437	1162.694410	16.826112
30.520770	1153.273820	16.831130
30.250934	1155.515778	16.836147
30.579627	1145.867308	16.841165
30.129095	1151.473332	16.846183
29.914093	1156.411281	16.851200
30.402247	1152.330032	16.856218
30.311285	1152.502114	16.861235
30.369123	1154.358209	16.866253
30.199266	1154.454288	16.871271
30.258594	1154.183092	16.876288
30.348150	1161.815778	16.881306
30.349825	1164.914621	16.886323
30.702342	1162.091723	16.891341
30.785573	1162.507918	16.896359
30.453131	1173.750775	16.901376
30.784122	1165.701964	16.906394
30.482489	1174.500503	16.911411
30.750899	1169.636307	16.916429
30.737915	1167.659644	16.921447
30.783076	1172.225468	16.926464
30.878849	1167.637636	16.931482
30.737015	1160.391916	16.936499
30.815749	1171.084344	16.941517
30.698192	1175.527337	16.946535
30.557960	1161.019696	16.951552
30.787386	1161.065839	16.956570
30.875690	1165.646993	16.961587
30.934705	1157.457758	16.966605
30.747158	1168.154034	16.971623
30.857421	1184.572600	16.976640
31.136406	1189.963348	16.981658
31.171108	1192.589951	16.986675
31.104481	1190.233517	16.991693
31.472699	1185.492538	16.996711
31.205844	1187.964411	17.001728
31.159283	1182.003977	17.006746
31.092194	1188.689208	17.011763
31.107655	1182.586509	17.016781
31.565736	1181.621661	17.021799
31.430082	1180.386912	17.026816
31.653822	1182.835569	17.031834
31.690383	1179.607727	17.036851
31.644798	1186.649357	17.041869
32.148090	1182.209115	17.046887
31.931680	1186.541364	17.051904
31.747161	1180.924445	17.056922
32.180110	1188.784214	17.061939
32.089742	1178.579677	17.066957
31.708694	1154.796780	17.071975
31.922246	1157.114483	17.076992
31.728790	1149.504462	17.082010
31.967196	1153.598183	17.087027
31.879213	1150.800122	17.092045
32.198932	1151.630554	17.097063
31.732021	1152.173970	17.102080
31.853372	1139.155960	17.107098
31.613905	1144.100895	17.112115
31.717907	1146.341084	17.117133
31.818376	1158.636438	17.122151
31.514949	1168.883801	17.127168
31.981622	1169.107372	17.132186
32.138737	1169.155377	17.137203
32.118027	1176.862152	17.142221
32.122520	1176.675288	17.147239
32.059491	1180.579552	17.152256
32.033153	1167.714052	17.157274
32.493634	1175.837751	17.162291
32.232886	1168.869440	17.167309
32.044896	1174.039853	17.172327
31.833282	1171.557812	17.177344
32.074186	1177.276422	17.182362
32.365218	1199.164217	17.187379
32.234928	1198.307333	17.192397
32.681335	1195.274055	17.197415
32.557336	1203.839645	17.202432
32.757486	1203.697866	17.207450
32.766448	1212.087989	17.212467
32.613405	1202.051053	17.217485
32.648680	1190.927396	17.222503
32.452696	1199.908215	17.227520
32.890061	1192.316108	17.232538
32.842749	1197.685397	17.237555
32.799865	1193.343350	17.242573
32.642523	1196.176772	17.247591
32.870882	1182.125771	17.252608
32.874744	1196.017382	17.257626
32.952946	1190.898952	17.262643
32.816278	1189.339306	17.267661
32.802691	1195.618516	17.272679
32.618716	1193.397235	17.277696
32.956013	1189.835087	17.282714
32.707919	1193.661050	17.287731
32.871757	1194.364424	17.292749
32.614812	1191.324580	17.297767
32.639707	1188.142746	17.302784
32.726578	1209.693304	17.307802
33.087593	1211.886922	17.312819
33.168215	1218.164002	17.317837
33.408550	1213.701835	17.322855
33.197819	1222.268399	17.327872
33.343231	1206.204297	17.332890
33.354191	1212.735294	17.337907
33.390858	1215.490983	17.342925
33.434569	1212.063194	17.347943
33.429461	1219.114274	17.352960
33.516395	1216.184653	17.357978
33.192399	1218.002748	17.362995
33.675481	1219.596559	17.368013
33.789174	1207.797870	17.373031
33.531111	1216.605383	17.378048
33.776903	1212.978669	17.383066
33.749636	1212.437010	17.388083
33.236173	1219.987472	17.393101
33.408002	1221.371267	17.398119
33.862207	1237.142687	17.403136
33.925204	1229.962679	17.408154
34.144460	1235.189226	17.413171
34.254924	1227.070795	17.418189
34.091490	1216.877683	17.423207
33.791926	1214.478845	17.428224
33.898672	1213.155621	17.433242
34.451996	1223.379237	17.438259
33.998317	1217.100716	17.443277
34.012459	1208.296779	17.448295
34.121442	1218.735181	17.453312
34.485490	1216.364916	17.458330
34.233822	1217.720387	17.463347
34.133239	1221.535868	17.468365
34.219777	1213.632636	17.473383
34.236283	1223.170324	17.478400
34.733347	1223.083014	17.483418
34.376078	1220.945687	17.488435
34.149060	1224.913525	17.493453
34.400280	1226.026099	17.498471
34.318334	1235.080588	17.503488
34.537667	1237.589905	17.508506
34.145466	1233.968471	17.513523
34.413880	1231.455394	17.518541
34.547815	1231.724787	17.523559
34.326828	1236.234495	17.528576
34.409643	1235.135931	17.533594
34.672634	1230.865875	17.538611
34.297408	1222.132404	17.543629
34.725202	1229.844672	17.548647
34.860884	1250.548166	17.553664
34.898719	1249.687029	17.558682
34.978981	1256.043076	17.563699
34.790120	1252.910501	17.568717
34.674207	1245.086313	17.573735
34.968078	1244.428064	17.578752
35.133547	1249.350610	17.583770
34.926049	1252.728400	17.588787
34.820405	1254.060995	17.593805
35.346566	1243.633588	17.598823
34.965342	1251.166499	17.603840
35.322568	1244.925023	17.608858
35.269281	1250.920131	17.613875
35.239100	1249.583643	17.618893
35.411492	1242.156110	17.623911
35.324114	1244.555688	17.628928
35.326059	1243.053217	17.633946
35.308199	1239.505678	17.638963
35.528479	1246.319479	17.643981
35.788687	1243.776127	17.648999
35.369425	1244.280521	17.654016
35.270051	1244.823161	17.659034
35.422567	1250.230587	17.664051
35.279400	1250.344576	17.669069
35.576105	1238.252098	17.674087
35.301390	1242.546158	17.679104
35.633106	1247.590982	17.684122
35.401353	1247.567367	17.689139
35.375449	1257.114874	17.694157
35.701753	1265.934997	17.699175
35.917813	1277.559053	17.704192
35.816065	1270.458490	17.709210
35.968738	1268.714644	17.714227
35.615749	1275.959112	17.719245
35.740426	1262.915244	17.724263
35.662111	1271.969183	17.729280
35.846468	1277.996496	17.734298
36.063252	1268.946179	17.739315
35.734185	1276.410967	17.744333
36.015302	1279.686960	17.749351
36.403999	1293.180670	17.754368
36.285599	1297.380821	17.759386
36.244557	1286.789786	17.764403
36.580057	1295.592704	17.769421
36.515755	1291.146688	17.774439
36.183188	1276.770076	17.779456
36.236899	1280.473029	17.784474
36.682854	1276.653991	17.789491
36.664191	1287.102965	17.794509
36.693438	1283.977238	17.799527
36.521633	1273.217345	17.804544
36.470489	1275.781669	17.809562
36.466148	1286.638665	17.814579
36.414144	1284.728065	17.819597
36.679303	1292.150252	17.824615
36.767456	1287.427879	17.829632
36.447177	1294.616735	17.834650
36.581489	1280.463624	17.839667
36.291164	1293.331554	17.844685
36.916290	1286.647291	17.849703
36.919869	1290.209774	17.854720
36.656908	1297.481172	17.859738
36.863924	1283.187276	17.864755
37.130131	1301.333039	17.869773
36.842299	1302.590037	17.874791
37.190514	1303.056240	17.879808
37.022457	1314.494342	17.884826
37.037781	1317.212364	17.889843
37.106401	1317.160623	17.894861
37.390697	1313.228046	17.899879
37.417222	1314.265374	17.904896
37.652407	1316.911078	17.909914
37.509397	1307.093423	17.914931
36.985297	1291.462357	17.919949
37.380159	1298.185707	17.924967
37.431478	1310.946472	17.929984
37.087376	1310.236693	17.935002
37.361387	1304.443749	17.940019
37.300797	1311.585613	17.945037
37.539125	1307.944270	17.950055
37.867347	1303.108538	17.955072
37.597896	1309.472059	17.960090
37.872160	1310.439012	17.965107
37.542656	1313.643419	17.970125
37.792020	1300.961852	17.975143
37.865163	1298.914874	17.980160
37.599595	1307.127142	17.985178
37.623007	1306.271417	17.990195
37.687619	1315.732188	17.995213
38.104581	1299.622301	18.000231
38.432096	1300.047563	18.005248
37.932019	1300.880211	18.010266
37.782963	1310.633239	18.015283
37.943454	1312.697337	18.020301
37.860836	1318.820143	18.025319
38.058574	1321.588483	18.030336
38.036298	1324.735289	18.035354
38.265565	1326.185835	18.040371
37.972114	1328.210600	18.045389
38.348089	1324.430920	18.050407
38.671998	1323.095754	18.055424
38.345161	1328.657206	18.060442
38.094605	1326.496834	18.065459
38.354407	1336.305742	18.070477
38.381743	1322.690083	18.075495
38.305082	1321.597565	18.080512
38.159024	1324.924716	18.085530
38.589547	1335.315964	18.090547
38.563523	1339.763592	18.095565
38.702176	1344.062340	18.100583
38.888450	1346.901911	18.105600
38.834332	1344.303648	18.110618
38.777715	1341.576384	18.115635
39.175892	1343.811535	18.120653
39.174805	1344.316687	18.125671
39.250703	1341.461360	18.130688
39.045774	1344.819830	18.135706
39.084764	1339.726437	18.140723
39.178729	1343.249522	18.145741
39.309393	1346.435487	18.150759
39.366506	1328.810313	18.155776
39.389593	1326.471364	18.160794
39.228795	1314.201199	18.165811
38.956586	1313.685290	18.170829
39.088868	1322.182380	18.175847
39.532305	1341.143042	18.180864
39.372869	1341.316386	18.185882
39.125410	1334.882432	18.190899
39.250983	1355.941094	18.195917
39.246838	1348.247677	18.200935
39.381620	1339.566789	18.205952
39.020391	1346.402309	18.210970
39.443763	1343.539879	18.215987
39.268620	1342.440698	18.221005
39.408711	1344.504839	18.226023
39.710907	1347.506134	18.231040
39.472545	1368.167381	18.236058
39.893791	1368.278148	18.241075
39.473341	1368.362995	18.246093
40.025596	1370.504579	18.251111
40.083809	1370.119941	18.256128
39.566881	1371.747366	18.261146
39.917114	1369.041563	18.266163
39.902815	1372.897207	18.271181
39.590580	1368.048191	18.276199
39.943581	1367.497442	18.281216
40.024286	1378.101320	18.286234
40.251253	1367.919540	18.291251
39.963704	1359.841317	18.296269
40.005830	1363.432491	18.301287
40.389738	1382.247883	18.306304
40.470565	1387.054336	18.311322
40.603864	1379.203667	18.316339
40.300431	1372.342953	18.321357
40.479674	1384.976427	18.326375
40.534965	1388.941096	18.331392
40.657592	1393.248679	18.336410
40.586847	1379.253854	18.341427
40.609872	1390.283357	18.346445
40.486720	1392.230953	18.351463
40.654782	1381.723868	18.356480
40.795052	1386.634620	18.361498
41.075964	1375.169395	18.366515
40.869785	1387.004849	18.371533
40.976360	1386.031946	18.376551
40.741707	1382.395264	18.381568
40.969351	1380.475554	18.386586
41.111330	1378.979535	18.391603
41.070930	1384.193157	18.396621
41.119256	1393.968956	18.401639
41.447280	1377.150230	18.406656
40.970839	1386.882008	18.411674
41.441039	1380.954155	18.416691
41.458573	1380.105660	18.421709
41.286652	1380.893208	18.426727
41.506792	1376.891772	18.431744
41.131923	1380.661895	18.436762
41.138380	1371.205807	18.441779
41.265410	1364.571153	18.446797
40.930816	1371.323611	18.451815
41.308410	1374.786484	18.456832
41.228736	1379.930517	18.461850
41.475443	1374.066086	18.466867
41.229719	1377.187948	18.471885
41.419611	1377.925120	18.476903
41.593014	1388.994179	18.481920
41.938118	1403.602529	18.486938
41.456339	1393.459194	18.491955
41.432284	1394.608596	18.496973
41.226787	1390.124715	18.501991
41.406639	1394.278160	18.507008
41.822132	1405.047358	18.512026
41.612265	1425.540098	18.517043
42.273883	1421.106552	18.522061
41.805077	1429.877757	18.527079
41.767963	1427.235791	18.532096
41.770638	1424.489757	18.537114
42.000638	1422.345603	18.542131
42.106062	1429.016518	18.547149
42.214368	1422.447894	18.552167
42.359871	1417.110565	18.557184
42.484314	1423.983633	18.562202
42.356772	1427.232159	18.567219
42.494104	1417.941741	18.572237
42.086915	1421.189898	18.577255
42.249434	1425.188270	18.582272
42.409284	1438.796844	18.587290
42.715490	1440.838126	18.592307
42.796734	1439.682989	18.597325
43.033078	1441.091409	18.602343
43.095542	1434.129161	18.607360
42.634509	1419.444345	18.612378
42.798314	1422.580949	18.617395
43.173349	1428.177635	18.622413
42.623416	1425.300424	18.627431
43.136633	1426.703334	18.632448
43.109043	1431.504694	18.637466
43.228695	1422.753550	18.642483
43.131217	1412.871896	18.647501
42.817042	1412.532979	18.652519
43.064060	1419.724524	18.657536
43.327165	1431.060432	18.662554
43.178432	1438.235092	18.667571
43.223856	1420.917782	18.672589
43.114266	1435.688921	18.677607
42.911529	1429.099598	18.682624
43.227034	1429.207998	18.687642
43.259942	1434.785704	18.692659
43.361616	1433.576872	18.697677
43.411330	1432.887440	18.702695
43.765098	1427.397553	18.707712
43.659027	1423.806991	18.712730
43.601783	1427.243326	18.717747
43.681060	1428.742628	18.722765
43.573311	1428.081023	18.727783
43.776235	1436.939498	18.732800
43.719036	1452.036970	18.737818
44.003277	1459.342624	18.742835
43.785935	1449.063147	18.747853
43.735395	1452.763535	18.752871
43.660719	1444.064919	18.757888
43.749474	1452.029227	18.762906
43.839241	1452.845208	18.767923
44.175388	1441.794181	18.772941
43.825632	1442.969369	18.777959
44.279316	1447.439699	18.782976
44.111197	1453.648533	18.787994
43.983216	1465.036269	18.793011
44.281725	1465.172580	18.798029
44.232558	1470.185622	18.803047
44.379195	1473.694168	18.808064
44.803157	1476.297696	18.813082
44.370670	1472.663588	18.818099
44.095465	1467.871860	18.823117
44.085471	1477.429616	18.828135
44.235832	1471.993675	18.833152
44.918130	1484.968141	18.838170
44.656398	1489.973466	18.843187
45.175693	1491.410144	18.848205
44.785257	1487.630584	18.853223
45.173653	1483.391314	18.858240
45.089792	1480.242248	18.863258
45.046989	1467.615806	18.868275
44.870778	1469.284533	18.873293
44.836296	1472.060878	18.878311
45.205518	1483.096159	18.883328
45.316112	1491.180144	18.888346
45.220609	1490.806964	18.893363
45.033721	1490.328177	18.898381
45.369710	1500.320906	18.903399
45.602388	1496.677256	18.908416
45.496974	1491.129899	18.913434
45.027521	1488.145390	18.918451
45.329445	1497.477553	18.923469
45.392321	1492.257293	18.928487
45.478534	1487.576199	18.933504
45.469210	1492.163266	18.938522
45.347076	1496.768008	18.943539
45.710505	1496.105164	18.948557
45.420177	1491.647173	18.953575
45.305784	1490.598427	18.958592
45.344557	1493.205501	18.963610
45.698280	1510.245812	18.968627
45.789527	1507.034590	18.973645
45.447403	1517.079923	18.978663
45.915865	1515.930388	18.983680
46.121052	1515.140851	18.988698
45.826237	1515.168143	18.993715
46.323715	1517.943203	18.998733
46.000727	1513.641808	19.003751
46.169220	1512.750719	19.008768
46.428959	1512.454429	19.013786
46.185682	1513.660278	19.018803
46.451594	1509.348671	19.023821
46.069067	1514.316121	19.028839
46.675966	1515.095265	19.033856
46.621974	1514.803947	19.038874
46.321427	1518.814929	19.043891
46.091613	1525.140756	19.048909
46.227555	1535.085949	19.053927
46.505159	1535.380177	19.058944
46.718355	1530.322555	19.063962
46.773746	1532.595657	19.068979
47.257562	1522.323053	19.073997
47.095772	1527.833459	19.079015
46.802404	1527.525995	19.084032
47.033684	1527.322530	19.089050
47.213721	1531.971461	19.094067
47.582469	1529.221707	19.099085
47.033912	1530.188197	19.104103
47.104602	1530.063544	19.109120
46.719794	1522.499124	19.114138
46.947914	1525.196462	19.119155
47.097380	1518.349943	19.124173
46.868583	1519.862806	19.129191
47.240007	1534.833228	19.134208
47.324324	1544.628719	19.139226
47.221143	1548.498326	19.144243
47.314990	1554.189604	19.149261
47.541940	1547.050056	19.154279
47.645099	1544.370315	19.159296
47.799869	1541.231188	19.164314
47.593336	1550.128624	19.169331
47.559358	1542.922657	19.174349
47.679466	1541.808764	19.179367
47.557901	1546.770051	19.184384
47.462535	1546.333730	19.189402
48.320460	1562.935318	19.194419
48.277972	1559.502031	19.199437
47.974454	1552.574987	19.204455
47.887694	1541.119923	19.209472
48.401823	1546.710634	19.214490
48.430058	1558.859784	19.219507
48.211046	1545.711761	19.224525
48.280989	1546.868537	19.229543
48.154622	1549.040725	19.234560
48.083967	1553.874113	19.239578
48.064905	1567.469789	19.244595
48.341381	1555.067829	19.249613
48.380176	1564.684262	19.254631
48.421451	1566.347327	19.259648
48.744498	1556.731081	19.264666
48.460055	1560.360836	19.269683
48.288053	1557.023584	19.274701
48.731575	1566.030628	19.279719
48.387669	1565.103048	19.284736
48.808767	1561.915879	19.289754
48.614746	1578.047951	19.294771
49.024110	1575.683164	19.299789
49.000488	1587.502772	19.304807
49.029974	1591.809216	19.309824
49.541970	1589.065413	19.314842
49.246226	1582.181322	19.319859
49.272372	1585.689833	19.324877
49.529350	1573.404529	19.329895
48.878236	1559.850804	19.334912
49.075876	1569.461287	19.339930
49.369441	1580.142393	19.344947
49.558580	1584.322831	19.349965
49.198752	1584.470767	19.354983
49.546714	1580.146288	19.360000
49.292986	1580.454333	19.365018
49.136420	1575.940647	19.370035
49.586372	1575.295804	19.375053
49.771023	1575.421552	19.380071
49.430208	1587.107811	19.385088
49.596863	1579.002509	19.390106
49.413440	1589.105072	19.395123
49.997270	1595.022564	19.400141
50.024821	1602.772457	19.405159
50.358509	1605.633156	19.410176
50.499351	1601.085491	19.415194
50.118263	1601.448206	19.420211
50.009387	1595.983414	19.425229
50.072180	1593.707640	19.430247
50.270486	1591.735697	19.435264
50.403804	1596.464551	19.440282
50.267245	1599.364211	19.445299
50.548783	1592.014111	19.450317
50.583339	1594.511402	19.455335
50.734486	1599.691921	19.460352
50.735296	1597.255436	19.465370
50.269110	1591.130226	19.470387
50.961606	1589.308084	19.475405
50.827614	1586.858006	19.480423
50.626855	1596.164833	19.485440
50.928746	1582.079907	19.490458
50.936034	1595.744063	19.495475
50.769595	1584.695949	19.500493
50.847484	1593.889687	19.505511
50.744765	1599.397172	19.510528
51.207881	1585.678321	19.515546
50.592069	1593.374367	19.520563
50.839921	1587.168845	19.525581
50.923735	1594.553297	19.530599
51.053270	1607.065322	19.535616
51.284922	1613.391466	19.540634
51.433125	1612.494084	19.545651
51.297277	1625.293866	19.550669
51.394158	1617.227881	19.555687
51.088597	1616.512051	19.560704
51.257286	1616.517218	19.565722
50.961571	1623.241587	19.570739
51.070014	1621.536197	19.575757
51.575283	1629.694115	19.580775
51.905857	1642.635437	19.585792
51.991047	1640.861101	19.590810
51.735871	1647.478137	19.595827
51.853303	1647.876361	19.600845
52.336384	1638.029861	19.605863
52.025753	1643.178595	19.610880
52.330375	1634.530918	19.615898
52.272621	1635.991744	19.620915
52.188690	1643.658130	19.625933
52.175711	1632.696401	19.630951
52.429385	1630.873577	19.635968
52.663882	1628.735007	19.640986
52.269642	1641.720458	19.646003
52.313144	1637.222750	19.651021
52.716248	1627.524492	19.656039
52.559403	1630.613537	19.661056
52.457024	1632.447445	19.666074
52.241971	1633.592072	19.671091
52.366053	1633.083495	19.676109
52.608666	1633.941811	19.681127
52.284622	1631.729796	19.686144
52.488163	1623.991097	19.691162
52.764461	1638.238018	19.696179
52.698141	1646.147811	19.701197
53.217166	1655.644868	19.706215
53.122571	1664.985594	19.711232
53.494067	1653.345045	19.716250
53.582591	1659.646291	19.721267
52.970001	1638.878253	19.726285
53.091911	1649.977634	19.731303
53.019050	1659.646328	19.736320
52.924464	1650.379502	19.741338
52.967213	1654.011663	19.746355
52.991358	1649.558012	19.751373
53.171186	1651.858973	19.756391
53.050921	1676.645848	19.761408
53.322237	1683.552812	19.766426
53.616045	1687.136178	19.771443
53.550397	1684.729029	19.776461
53.803767	1675.398206	19.781479
53.467475	1685.502682	19.786496
54.125807	1676.398759	19.791514
53.620545	1680.470255	19.796531
53.736096	1688.907021	19.801549
54.080403	1693.618624	19.806567
53.971843	1701.187902	19.811584
54.339791	1711.390350	19.816602
54.444373	1708.650398	19.821619
54.408124	1707.478937	19.826637
54.380822	1698.027966	19.831655
54.476081	1707.310564	19.836672
54.724205	1704.841628	19.841690
54.026478	1702.224224	19.846707
54.116366	1704.087980	19.851725
54.760513	1695.797354	19.856743
54.097062	1700.045124	19.861760
54.402832	1693.167738	19.866778
54.606934	1701.189829	19.871795
54.568083	1708.000224	19.876813
54.875548	1704.357438	19.881831
55.009735	1720.387720	19.886848
55.387114	1716.219555	19.891866
55.200806	1728.020561	19.896883
55.153987	1718.506361	19.901901
55.216221	1702.824095	19.906919
54.966592	1710.731077	19.911936
55.493664	1718.888776	19.916954
55.426183	1723.989969	19.921971
55.479090	1720.980386	19.926989
55.373352	1715.429854	19.932007
55.295415	1713.242390	19.937024
55.617074	1719.671240	19.942042
55.768804	1708.522705	19.947059
55.337424	1720.570397	19.952077
55.588333	1712.107832	19.957095
55.484412	1712.108371	19.962112
55.746951	1713.929297	19.967130
55.346381	1714.351874	19.972147
55.265232	1712.606749	19.977165
55.784511	1711.569168	19.982183
55.429548	1713.928677	19.987200
55.812789	1728.588127	19.992218
56.210989	1736.617695	19.997235
56.325040	1741.434817	20.002253
56.497926	1734.123775	20.007271
55.867666	1744.189130	20.012288
55.950475	1739.274961	20.017306
56.198473	1738.346157	20.022323
56.267426	1728.883245	20.027341
56.416561	1734.035714	20.032359
56.531427	1738.717002	20.037376
56.545733	1730.869042	20.042394
56.284215	1730.928988	20.047411
56.458846	1741.493118	20.052429
56.771314	1744.729571	20.057447
56.803085	1758.140693	20.062464
56.923054	1752.403299	20.067482
57.139220	1751.043957	20.072499
57.072433	1750.697832	20.077517
57.162254	1741.376819	20.082535
56.975250	1750.934050	20.087552
57.019184	1752.625119	20.092570
56.889125	1748.924635	20.097587
56.464622	1745.718432	20.102605
57.055710	1755.324180	20.107623
56.804337	1765.645783	20.112640
57.340481	1773.615883	20.117658
57.513904	1774.207321	20.122675
57.447278	1769.051454	20.127693
57.853465	1772.651945	20.132711
57.347856	1773.125697	20.137728
57.580823	1766.366992	20.142746
57.657083	1764.297381	20.147763
57.556790	1779.045254	20.152781
58.011108	1784.878956	20.157799
57.948042	1795.464579	20.162816
57.871227	1801.927487	20.167834
58.109215	1792.819932	20.172851
57.696167	1797.037961	20.177869
57.994754	1786.803695	20.182887
58.030059	1793.362649	20.187904
57.973782	1789.514889	20.192922
57.993542	1788.492447	20.197939
58.189030	1803.493816	20.202957
58.445383	1813.208848	20.207975
58.316240	1818.354445	20.212992
58.330698	1821.312535	20.218010
58.375952	1812.033184	20.223027
58.515255	1819.118684	20.228045
58.414893	1809.006875	20.233063
58.605248	1827.654236	20.238080
58.687378	1833.928142	20.243098
59.107813	1836.813160	20.248115
59.229947	1846.618670	20.253133
59.459920	1833.889269	20.258151
59.130280	1844.128499	20.263168
59.340168	1839.948675	20.268186
59.621362	1829.893846	20.273203
59.416217	1831.504020	20.278221
59.466681	1818.001132	20.283239
59.428799	1812.187459	20.288256
59.225955	1805.777904	20.293274
59.707379	1803.982500	20.298291
59.708267	1822.757377	20.303309
59.984065	1826.488768	20.308327
59.341523	1816.869024	20.313344
59.602713	1828.663104	20.318362
59.575458	1824.242711	20.323379
59.913724	1827.383612	20.328397
60.266119	1819.574168	20.333415
60.136453	1826.619755	20.338432
60.011879	1822.413438	20.343450
60.108905	1818.339669	20.348467
59.799292	1819.076220	20.353485
60.112599	1820.216977	20.358503
59.939640	1817.277482	20.363520
59.994701	1824.278347	20.368538
59.862351	1821.521847	20.373555
59.951743	1828.656198	20.378573
60.341739	1843.071672	20.383591
60.281990	1852.788911	20.388608
60.411772	1852.642374	20.393626
60.744961	1851.624474	20.398643
60.270090	1847.438317	20.403661
60.397076	1869.119093	20.408679
61.144492	1875.254063	20.413696
60.983173	1864.201818	20.418714
61.102100	1868.244991	20.423731
61.002523	1867.029790	20.428749
61.022277	1864.309417	20.433767
61.368999	1875.114923	20.438784
61.313604	1869.073588	20.443802
61.563878	1862.110152	20.448819
61.391400	1866.325221	20.453837
61.404550	1866.556741	20.458855
61.425658	1864.120196	20.463872
61.652341	1871.223586	20.468890
61.570155	1861.077340	20.473907
61.409358	1866.499326	20.478925
61.478216	1860.649979	20.483943
61.483786	1860.658610	20.488960
61.940793	1876.089312	20.493978
62.272825	1887.859707	20.498995
61.841281	1897.856142	20.504013
61.866320	1889.908595	20.509031
62.165620	1883.817995	20.514048
62.243002	1892.112506	20.519066
62.219463	1882.184292	20.524083
62.490976	1884.448826	20.529101
62.683327	1889.925950	20.534119
62.255326	1885.356876	20.539136
62.142890	1888.918719	20.544154
62.378869	1878.072478	20.549171
62.381009	1891.564087	20.554189
62.271873	1888.314760	20.559207
62.530679	1892.705275	20.564224
62.922886	1905.485644	20.569242
62.897242	1916.005511	20.574259
62.775386	1915.118866	20.579277
62.801954	1910.737359	20.584295
62.766986	1914.050369	20.589312
62.804622	1914.025572	20.594330
63.072915	1907.564258	20.599347
62.610879	1915.084859	20.604365
63.091232	1905.194457	20.609383
62.771558	1915.359578	20.614400
62.938599	1925.091820	20.619418
63.131676	1926.980460	20.624435
63.290122	1934.886724	20.629453
63.011859	1930.600312	20.634471
63.335733	1939.036118	20.639488
63.626876	1949.263359	20.644506
63.243282	1955.439849	20.649523
63.536516	1957.852478	20.654541
63.444011	1949.756053	20.659559
63.973195	1962.070003	20.664576
63.669886	1955.953864	20.669594
64.236486	1959.671282	20.674611
64.345267	1972.900074	20.679629
64.654340	1971.415699	20.684647
64.822449	1955.726092	20.689664
64.519867	1945.163019	20.694682
64.649666	1936.226987	20.699699
64.672273	1942.330363	20.704717
64.483034	1940.747327	20.709735
64.623719	1931.831683	20.714752
64.745750	1940.355922	20.719770
64.900576	1931.362318	20.724787
64.592216	1932.354314	20.729805
64.617545	1934.723702	20.734823
64.786067	1942.565272	20.739840
64.955973	1957.040569	20.744858
65.347309	1960.463533	20.749875
65.223006	1966.176497	20.754893
65.373483	1961.822904	20.759911
65.399693	1955.806626	20.764928
65.434250	1957.881062	20.769946
65.699124	1956.769710	20.774963
65.209046	1958.399289	20.779981
65.344019	1955.995388	20.784999
65.715994	1951.777519	20.790016
65.498582	1950.132619	20.795034
65.344405	1950.428229	20.800051
65.655905	1954.987241	20.805069
65.282882	1954.543914	20.810087
65.677443	1951.518636	20.815104
65.600494	1961.661535	20.820122
65.745457	1973.890515	20.825139
65.845236	1979.486318	20.830157
65.554320	1979.774948	20.835175
66.506344	1982.049648	20.840192
65.978147	1978.509331	20.845210
66.257180	1980.488658	20.850227
66.087442	1994.171385	20.855245
66.313331	1995.606737	20.860263
66.725374	1998.003913	20.865280
66.623580	2004.634921	20.870298
67.034132	2005.100846	20.875315
66.947697	2000.030073	20.880333
67.198562	2000.445272	20.885351
66.943478	2002.135874	20.890368
67.181114	1994.824049	20.895386
67.393316	1995.220057	20.900403
67.076918	2003.093444	20.905421
67.019544	2001.221480	20.910439
67.195435	1993.048267	20.915456
66.925938	1995.362863	20.920474
67.099779	1994.278395	20.925491
66.689007	1993.904103	20.930509
67.083763	2004.383404	20.935527
67.606386	2009.540557	20.940544
67.206304	2021.542518	20.945562
67.543633	2031.286010	20.950579
67.913508	2021.447570	20.955597
67.662768	2024.706038	20.960615
67.660676	2013.117478	20.965632
67.915014	2018.127305	20.970650
68.202432	2016.374901	20.975667
67.845446	2015.682891	20.980685
67.619436	2013.707950	20.985703
68.257789	2016.243253	20.990720
68.171571	2036.376468	20.995738
68.771182	2039.479617	21.000755
68.820514	2027.816714	21.005773
68.286960	2018.953011	21.010791
68.601351	2003.426648	21.015808
68.313853	2021.438974	21.020826
68.561835	2033.393060	21.025843
69.185046	2039.724286	21.030861
69.055012	2036.383525	21.035879
69.131135	2024.555468	21.040896
69.078421	2028.104826	21.045914
69.036199	2023.061835	21.050931
69.343384	2030.282073	21.055949
68.864801	2024.928725	21.060967
69.198048	2021.048291	21.065984
69.331035	2026.679935	21.071002
69.574622	2028.838402	21.076019
69.430907	2030.637798	21.081037
69.496456	2033.120827	21.086055
69.517292	2019.051188	21.091072
69.521822	2023.276434	21.096090
69.234518	2018.252906	21.101107
69.354891	2015.781852	21.106125
69.511989	2019.131066	21.111143
69.751693	2030.764533	21.116160
69.678108	2044.006170	21.121178
69.925459	2037.355572	21.126195
69.684684	2046.744647	21.131213
69.732747	2047.447260	21.136231
69.752452	2043.972577	21.141248
70.044542	2054.890901	21.146266
70.167296	2068.171228	21.151283
70.318482	2065.184061	21.156301
70.250500	2065.510352	21.161319
70.092671	2064.553590	21.166336
70.406664	2074.187145	21.171354
70.473048	2092.734277	21.176371
70.572798	2093.050069	21.181389
70.694078	2099.450488	21.186407
70.948623	2100.635187	21.191424
70.836620	2097.553541	21.196442
70.660196	2094.472520	21.201459
71.017177	2109.366788	21.206477
71.320750	2116.552911	21.211495
71.522641	2111.727288	21.216512
71.494855	2123.749889	21.221530
71.497062	2120.015980	21.226547
71.521684	2117.818709	21.231565
71.504274	2120.841807	21.236583
71.560227	2114.953369	21.241600
71.627953	2113.083886	21.246618
71.622112	2109.206063	21.251635
71.975846	2112.650728	21.256653
71.983802	2115.152260	21.261671
72.039400	2113.821204	21.266688
71.767695	2124.382901	21.271706
71.988648	2122.887071	21.276723
72.376346	2131.477083	21.281741
72.540718	2130.539270	21.286759
72.717119	2129.902553	21.291776
72.351779	2133.721834	21.296794
72.482961	2132.928087	21.301811
72.264846	2127.757978	21.306829
72.240984	2136.421942	21.311847
72.530298	2135.164729	21.316864
72.222849	2130.037020	21.321882
72.330451	2142.855837	21.326899
72.843686	2152.717015	21.331917
72.917026	2157.780488	21.336935
73.010944	2155.234658	21.341952
72.674762	2154.368955	21.346970
72.643860	2148.478335	21.351987
73.185855	2149.324489	21.357005
73.261625	2174.100275	21.362023
73.479314	2171.443526	21.367040
73.592865	2177.920928	21.372058
73.409055	2177.214402	21.377075
73.948346	2176.849058	21.382093
73.554534	2176.497351	21.387111
73.757226	2173.921853	21.392128
73.956885	2173.991602	21.397146
73.979925	2166.624959	21.402163
74.285344	2174.400997	21.407181
74.129338	2171.502971	21.412199
74.294711	2175.403228	21.417216
74.526031	2167.921895	21.422234
73.947876	2176.006794	21.427251
74.518291	2161.472213	21.432269
74.418961	2157.612182	21.437287
74.587749	2162.162047	21.442304
74.732680	2167.419450	21.447322
74.779059	2184.953563	21.452339
74.995093	2186.463063	21.457357
74.869500	2191.327322	21.462375
74.906744	2182.475101	21.467392
75.125927	2195.636265	21.472410
74.965188	2200.919476	21.477427
74.922913	2181.879340	21.482445
75.062066	2190.145374	21.487463
74.905980	2188.901131	21.492480
75.077451	2191.717909	21.497498
75.238179	2195.508435	21.502515
75.383952	2203.782907	21.507533
75.194738	2214.735708	21.512551
75.520845	2215.113877	21.517568
75.240985	2216.123514	21.522586
75.636400	2218.267686	21.527603
75.841379	2216.035834	21.532621
76.067683	2234.400254	21.537639
76.069828	2241.261237	21.542656
75.993416	2251.391591	21.547674
76.249434	2236.824149	21.552691
76.201193	2237.191535	21.557709
76.142577	2243.995762	21.562727
76.167439	2244.736734	21.567744
76.538458	2240.335897	21.572762
76.714540	2245.045599	21.577779
76.699895	2232.067039	21.582797
76.108889	2234.432036	21.587815
76.627046	2244.939486	21.592832
76.639327	2258.451875	21.597850
76.957026	2253.642787	21.602867
77.037090	2251.244294	21.607885
76.985791	2247.045332	21.612903
76.472447	2246.431461	21.617920
76.987858	2256.879384	21.622938
76.962486	2269.201530	21.627955
77.269268	2282.595206	21.632973
77.338693	2283.739488	21.637991
77.406340	2282.886255	21.643008
77.451087	2278.047336	21.648026
77.513504	2280.814936	21.653043
77.821145	2282.663572	21.658061
77.779680	2291.488172	21.663079
77.876931	2295.743139	21.668096
78.217787	2296.118999	21.673114
78.253249	2303.653342	21.678131
78.471957	2290.635023	21.683149
78.570843	2298.885324	21.688167
78.861036	2283.068998	21.693184
78.934095	2268.826865	21.698202
78.312460	2273.462724	21.703219
78.544830	2258.334033	21.708237
78.284778	2263.733816	21.713255
78.497031	2271.104737	21.718272
79.190159	2282.537929	21.723290
78.979858	2292.067537	21.728307
78.999406	2286.771776	21.733325
79.215509	2290.932376	21.738343
79.164500	2286.578712	21.743360
79.292848	2291.889247	21.748378
79.147252	2290.810625	21.753395
79.240660	2284.591188	21.758413
79.459011	2287.460602	21.763431
79.415704	2285.223456	21.768448
79.552174	2286.896922	21.773466
79.144960	2302.002606	21.778483
79.571184	2283.144603	21.783501
79.452937	2297.453865	21.788519
79.844758	2307.659226	21.793536
79.908035	2309.565087	21.798554
79.766210	2305.430792	21.803571
79.908919	2304.669948	21.808589
79.794320	2320.231618	21.813607
79.855841	2317.955952	21.818624
80.165072	2333.085126	21.823642
80.349849	2339.428340	21.828659
80.313017	2335.994019	21.833677
80.445506	2333.236976	21.838695
80.437356	2334.832110	21.843712
80.674953	2342.801900	21.848730
80.459564	2353.102421	21.853747
80.967036	2363.851479	21.858765
80.895836	2364.194059	21.863783
81.142234	2365.032884	21.868800
81.126682	2362.415806	21.873818
81.129137	2361.604344	21.878835
81.137302	2361.767217	21.883853
81.139600	2360.416089	21.888871
81.487991	2369.239613	21.893888
81.269288	2370.353296	21.898906
81.481164	2377.629637	21.903923
81.565146	2375.946945	21.908941
81.551167	2369.542314	21.913959
81.433617	2369.421899	21.918976
81.815029	2377.375486	21.923994
81.873160	2393.206829	21.929011
81.790405	2390.805422	21.934029
82.097446	2399.850053	21.939047
82.101978	2394.244160	21.944064
82.268659	2393.833039	21.949082
82.875527	2411.358462	21.954099
82.662765	2400.373911	21.959117
82.524472	2404.343886	21.964135
82.994453	2405.681063	21.969152
83.198744	2408.259182	21.974170
83.113962	2410.765816	21.979187
83.250054	2405.079342	21.984205
82.950058	2394.840675	21.989223
83.229953	2392.155212	21.994240
83.172955	2399.776671	21.999258
83.362239	2408.009704	22.004275
83.466985	2404.758334	22.009293
83.697493	2409.393275	22.014311
83.441811	2407.321943	22.019328
83.723839	2409.985722	22.024346
83.648394	2405.569579	22.029363
83.518621	2408.310500	22.034381
83.918364	2402.901486	22.039399
83.904353	2395.493213	22.044416
84.180046	2394.588443	22.049434
84.067979	2400.167071	22.054451
83.578805	2404.596000	22.059469
83.775058	2406.370574	22.064487
83.855459	2426.594897	22.069504
84.169788	2424.917141	22.074522
84.179485	2434.409200	22.079539
84.298511	2432.515866	22.084557
84.110768	2438.371475	22.089575
84.606412	2456.128982	22.094592
84.591473	2451.643382	22.099610
84.327067	2459.537226	22.104627
84.576882	2462.098752	22.109645
85.146479	2468.495342	22.114663
84.828287	2479.897742	22.119680
85.403517	2472.251939	22.124698
85.005514	2479.380852	22.129715
85.092078	2478.092259	22.134733
85.467634	2488.798937	22.139751
85.689965	2499.106709	22.144768
86.118724	2496.148575	22.149786
86.216389	2495.524181	22.154803
86.474118	2485.680966	22.159821
86.087385	2480.950623	22.164839
86.064132	2479.202663	22.169856
86.393980	2464.443573	22.174874
86.003582	2481.572991	22.179891
86.274484	2484.487857	22.184909
85.921233	2483.309200	22.189927
85.876660	2500.270835	22.194944
86.221319	2490.720140	22.199962
86.502586	2504.102200	22.204979
86.490062	2503.548723	22.209997
86.786853	2507.466336	22.215015
86.745293	2516.477271	22.220032
86.572076	2510.157505	22.225050
86.681069	2518.930238	22.230067
87.048868	2525.711949	22.235085
87.350513	2529.325820	22.240103
87.397566	2525.862539	22.245120
87.608014	2528.102006	22.250138
87.714205	2528.375768	22.255155
87.624760	2530.801090	22.260173
87.947816	2524.289946	22.265191
88.074167	2528.262672	22.270208
88.097499	2522.666418	22.275226
88.088223	2523.308599	22.280243
88.412569	2521.269468	22.285261
88.464286	2520.443969	22.290279
88.481194	2517.865968	22.295296
88.619283	2518.024268	22.300314
88.399679	2513.659089	22.305331
88.238621	2516.995121	22.310349
88.456240	2521.133445	22.315367
88.593241	2521.759021	22.320384
89.016643	2506.448699	22.325402
88.366058	2512.717706	22.330419
88.694448	2513.490038	22.335437
88.992856	2524.224606	22.340455
88.795395	2535.617593	22.345472
89.064585	2533.631288	22.350490
88.706609	2541.464080	22.355507
89.053989	2530.113952	22.360525
89.252559	2532.181695	22.365543
88.906345	2546.406939	22.370560
89.279259	2557.710579	22.375578
89.549265	2554.092429	22.380595
89.511384	2559.804665	22.385613
89.557197	2559.248359	22.390631
89.485781	2565.360367	22.395648
89.913725	2578.366016	22.400666
90.303974	2588.126771	22.405683
90.094766	2590.744451	22.410701
90.688512	2583.919449	22.415719
90.402655	2578.286404	22.420736
90.712506	2578.749188	22.425754
90.668703	2586.261351	22.430771
90.516608	2586.411462	22.435789
90.740324	2575.371043	22.440807
90.653747	2591.502972	22.445824
90.554860	2607.466414	22.450842
90.944037	2616.381510	22.455859
91.123918	2613.307698	22.460877
91.367076	2602.702919	22.465895
91.123904	2609.567760	22.470912
91.542450	2601.201604	22.475930
91.299539	2604.124399	22.480947
91.505161	2613.888845	22.485965
91.522977	2621.034726	22.490983
91.386552	2627.879694	22.496000
91.699555	2629.093145	22.501018
91.572360	2623.675093	22.506035
91.716330	2634.727443	22.511053
92.089183	2635.265574	22.516071
91.891668	2652.532210	22.521088
92.284934	2646.221483	22.526106
92.139932	2647.784431	22.531123
92.176533	2652.617090	22.536141
92.700563	2663.221708	22.541159
92.795107	2675.468535	22.546176
93.048964	2677.234112	22.551194
92.882867	2676.537415	22.556211
93.202630	2679.406784	22.561229
93.467983	2665.446669	22.566247
93.512232	2669.517505	22.571264
93.576113	2674.497391	22.576282
93.554444	2676.205139	22.581299
93.237194	2670.308711	22.586317
93.551611	2664.853020	22.591335
93.580938	2672.057085	22.596352
93.400001	2665.350267	22.601370
93.339575	2671.062915	22.606387
93.617621	2678.729841	22.611405
93.535636	2678.196710	22.616423
93.703031	2700.525483	22.621440
93.938372	2686.756266	22.626458
94.227828	2691.691347	22.631475
93.819789	2692.998832	22.636493
94.443251	2703.054507	22.641511
94.577526	2716.406101	22.646528
94.798868	2716.961659	22.651546
94.500300	2712.589866	22.656563
94.436425	2716.437785	22.661581
94.788714	2711.317012	22.666599
94.895514	2727.475576	22.671616
94.770045	2729.928662	22.676634
94.681704	2734.411648	22.681651
95.156294	2739.841658	22.686669
95.542830	2733.115344	22.691687
95.344662	2730.309048	22.696704
95.078299	2736.319098	22.701722
95.656255	2757.046572	22.706739
95.902356	2760.227330	22.711757
95.720019	2756.317051	22.716775
95.761750	2753.672005	22.721792
95.942503	2761.256369	22.726810
96.045255	2751.109050	22.731827
95.854531	2758.202441	22.736845
96.217985	2748.920096	22.741863
96.417361	2776.315891	22.746880
96.717689	2774.687640	22.751898
96.568535	2781.553597	22.756915
96.526154	2780.663924	22.761933
96.905100	2771.600071	22.766951
96.617248	2780.195238	22.771968
96.449768	2775.847078	22.776986
97.070423	2787.686471	22.782003
97.070948	2799.711400	22.787021
97.278307	2799.603202	22.792039
97.244097	2800.107272	22.797056
97.299758	2797.810370	22.802074
97.102803	2800.909054	22.807091
97.532980	2814.612037	22.812109
97.765756	2821.156210	22.817127
97.522126	2826.569368	22.822144
97.712306	2820.217807	22.827162
98.420282	2812.355382	22.832179
97.873419	2821.821220	22.837197
98.401830	2825.402780	22.842215
98.457206	2838.848885	22.847232
98.671102	2847.466473	22.852250
98.747201	2844.042767	22.857267
98.756220	2853.610901	22.862285
98.801685	2837.087574	22.867303
98.651774	2840.122083	22.872320
98.594501	2845.079967	22.877338
99.142390	2841.980023	22.882355
98.698953	2843.968485	22.887373
98.920033	2854.033632	22.892391
99.121137	2861.952561	22.897408
99.198845	2864.926163	22.902426
99.171104	2866.808469	22.907443
99.242013	2870.985640	22.912461
99.330826	2882.949450	22.917479
99.600919	2895.642350	22.922496
99.856419	2898.840597	22.927514
100.026288	2881.401385	22.932531
100.074149	2900.687642	22.937549
100.346070	2914.213500	22.942567
100.104421	2910.956341	22.947584
100.375336	2908.117557	22.952602
100.860037	2904.891786	22.957619
100.530698	2908.191131	22.962637
100.488264	2910.183054	22.967655
100.718131	2912.293281	22.972672
100.937511	2928.327078	22.977690
101.151465	2929.783313	22.982707
101.037963	2932.868945	22.987725
101.060565	2925.741930	22.992743
101.112669	2925.004725	22.997760
101.364820	2926.357134	23.002778
101.528463	2931.842232	23.007795
101.318332	2926.878949	23.012813
101.678599	2938.311058	23.017831
101.937938	2942.812217	23.022848
101.793615	2948.771655	23.027866
102.163419	2941.558676	23.032883
102.028950	2943.621833	23.037901
101.900981	2939.311630	23.042919
102.086337	2945.393005	23.047936
102.305668	2949.988808	23.052954
102.506560	2953.422866	23.057971
102.495078	2964.032657	23.062989
102.402350	2969.804115	23.068007
102.677839	2966.797326	23.073024
102.435671	2966.068349	23.078042
102.788527	2975.443807	23.083059
103.015247	2984.709627	23.088077
103.673237	2983.255724	23.093095
103.363634	2992.163707	23.098112
103.274930	2991.596901	23.103130
103.740187	2984.747694	23.108147
103.649444	2980.564208	23.113165
103.495603	2985.682445	23.118183
103.673438	2990.568817	23.123200
103.791556	3008.038838	23.128218
103.888074	3013.572352	23.133235
104.126779	3017.035216	23.138253
104.062685	3015.757565	23.143271
104.249100	3011.180311	23.148288
104.263567	3025.453578	23.153306
104.528172	3019.216535	23.158323
104.602024	3024.564231	23.163341
104.886462	3019.693872	23.168359
104.652503	3016.646955	23.173376
104.391871	3031.256853	23.178394
105.129989	3030.049202	23.183411
105.232454	3042.497034	23.188429
105.358155	3040.315377	23.193447
105.640891	3044.620368	23.198464
105.270605	3044.530076	23.203482
105.771032	3047.702602	23.208499
105.571874	3051.129919	23.213517
105.909764	3061.385191	23.218535
106.460551	3069.839638	23.223552
106.249568	3068.493465	23.228570
106.625244	3058.741928	23.233587
106.092427	3067.852198	23.238605
106.275143	3057.638523	23.243623
106.423213	3059.231340	23.248640
106.556265	3060.084801	23.253658
107.004138	3056.605965	23.258675
106.494733	3067.827226	23.263693
106.658816	3075.433271	23.268711
106.876561	3084.066151	23.273728
107.136991	3088.109525	23.278746
107.290172	3079.907816	23.283763
107.118527	3081.733785	23.288781
106.628313	3083.423448	23.293799
107.194228	3101.590363	23.298816
107.515846	3112.552051	23.303834
107.572038	3104.068842	23.308851
107.771872	3119.462004	23.313869
107.942362	3124.513686	23.318887
108.147292	3138.050209	23.323904
108.486444	3134.676765	23.328922
108.862900	3129.785649	23.333939
109.143964	3133.172463	23.338957
108.863332	3130.710427	23.343975
108.849206	3128.654821	23.348992
108.792752	3136.030321	23.354010
108.831005	3120.255889	23.359027
108.825233	3122.863867	23.364045
108.934902	3124.967701	23.369063
108.998185	3115.340825	23.374080
109.087616	3117.744513	23.379098
109.115370	3112.923813	23.384115
109.518941	3127.748506	23.389133
109.335922	3137.144880	23.394151
109.825639	3137.611062	23.399168
109.719872	3136.541929	23.404186
109.976184	3128.740662	23.409203
109.919071	3139.143083	23.414221
110.056366	3137.073221	23.419239
110.024790	3141.493760	23.424256
109.808603	3153.325629	23.429274
110.184959	3163.600184	23.434291
110.314631	3161.389484	23.439309
110.092933	3168.427921	23.444327
110.741473	3178.871308	23.449344
110.580742	3186.215823	23.454362
110.986998	3179.435755	23.459379
110.853263	3179.592461	23.464397
111.174831	3189.383243	23.469415
111.329114	3197.151843	23.474432
111.153145	3199.922215	23.479450
111.598490	3194.467947	23.484467
111.867337	3194.514238	23.489485
111.762522	3201.155628	23.494503
111.614502	3203.167281	23.499520
111.910787	3206.681130	23.504538
112.241692	3212.335796	23.509555
112.566663	3226.226014	23.514573
112.498711	3223.042585	23.519591
112.267441	3210.535974	23.524608
112.058859	3221.044234	23.529626
112.044150	3220.582608	23.534643
112.712551	3235.769898	23.539661
112.892190	3238.774936	23.544679
113.667569	3240.903894	23.549696
113.102050	3237.157699	23.554714
113.349520	3233.372509	23.559731
113.471369	3227.577540	23.564749
113.291033	3238.652664	23.569767
113.598392	3245.027495	23.574784
113.624238	3260.053506	23.579802
113.736159	3254.667239	23.584819
114.083379	3268.090036	23.589837
113.983610	3261.433404	23.594855
114.227962	3263.244717	23.599872
114.256338	3266.800551	23.604890
114.516174	3280.173922	23.609907
114.860972	3280.492377	23.614925
114.435696	3284.340225	23.619943
115.017544	3286.291196	23.624960
115.257437	3281.206809	23.629978
114.975870	3282.734395	23.634995
114.945672	3283.970099	23.640013
114.954933	3283.012342	23.645031
115.138526	3277.046715	23.650048
114.904604	3295.484324	23.655066
115.575460	3301.294070	23.660083
115.708713	3305.606763	23.665101
115.397610	3311.920699	23.670119
115.734098	3319.884901	23.675136
115.639703	3331.543149	23.680154
115.743137	3333.089327	23.685171
116.035233	3335.802169	23.690189
115.982528	3336.959341	23.695207
116.164773	3345.872502	23.700224
116.136033	3360.648335	23.705242
116.345342	3366.511475	23.710259
116.649547	3360.397518	23.715277
116.709542	3355.000420	23.720295
117.137462	3358.989209	23.725312
116.790829	3373.309854	23.730330
117.101296	3373.267563	23.735347
117.319681	3368.675742	23.740365
117.241659	3374.943715	23.745383
117.409766	3373.879004	23.750400
117.759981	3395.217336	23.755418
117.629379	3381.618548	23.760435
118.314092	3395.209504	23.765453
118.302318	3391.228177	23.770471
118.309155	3396.614890	23.775488
118.282243	3387.216625	23.780506
118.471484	3400.522240	23.785523
118.456988	3398.349879	23.790541
118.303096	3403.332522	23.795559
118.845502	3402.335419	23.800576
118.766551	3411.526255	23.805594
119.257772	3419.718761	23.810611
119.219843	3423.379702	23.815629
119.005406	3422.071918	23.820647
118.878817	3417.543601	23.825664
119.157540	3427.991417	23.830682
119.225972	3441.199206	23.835699
119.535213	3437.205452	23.840717
119.466112	3445.290065	23.845735
119.800758	3455.457696	23.850752
119.965224	3461.466769	23.855770
120.002068	3463.903993	23.860787
120.202947	3464.409125	23.865805
120.256825	3479.797056	23.870823
120.548903	3482.775051	23.875840
120.438797	3493.151258	23.880858
120.588311	3490.808002	23.885875
120.899075	3492.962438	23.890893
120.834483	3499.509259	23.895911
121.299117	3506.386642	23.900928
121.221412	3507.314176	23.905946
121.425704	3509.759891	23.910963
121.818430	3503.370046	23.915981
121.334816	3508.880975	23.920999
121.845885	3521.631252	23.926016
122.106835	3529.380129	23.931034
122.186411	3533.123684	23.936051
122.164438	3518.548262	23.941069
122.032693	3526.251346	23.946087
122.421142	3519.227751	23.951104
122.511147	3533.959872	23.956122
122.650759	3536.463069	23.961139
122.863608	3550.222758	23.966157
122.591463	3547.203826	23.971175
123.104441	3549.945222	23.976192
123.413185	3549.095189	23.981210
123.405702	3556.832475	23.986227
123.389219	3545.810159	23.991245
123.253210	3559.046908	23.996263
124.056847	3562.664407	24.001280
123.367823	3570.767291	24.006298
123.393637	3572.824346	24.011315
123.748199	3578.866802	24.016333
124.041453	3591.471345	24.021351
124.293017	3596.838714	24.026368
124.107776	3598.468017	24.031386
124.103044	3600.062728	24.036403
124.654450	3601.403026	24.041421
124.683797	3595.111110	24.046439
124.397855	3593.391572	24.051456
124.953156	3603.827723	24.056474
124.730528	3618.034445	24.061491
125.008242	3614.916731	24.066509
125.051836	3632.067621	24.071527
125.050860	3624.227542	24.076544
125.262671	3635.367724	24.081562
125.294272	3644.443512	24.086579
125.318348	3636.725756	24.091597
125.682541	3656.641869	24.096615
125.924526	3661.935007	24.101632
126.268488	3662.897489	24.106650
126.188445	3660.801648	24.111667
126.639086	3656.795162	24.116685
126.399615	3660.228908	24.121703
126.758114	3677.428351	24.126720
126.823347	3681.010055	24.131738
127.222264	3677.649244	24.136755
126.818204	3677.482173	24.141773
126.925347	3675.470632	24.146791
127.326015	3681.644778	24.151808
127.321345	3694.015155	24.156826
127.649146	3696.741397	24.161843
127.777761	3695.386161	24.166861
127.708960	3704.790184	24.171879
127.456816	3696.806358	24.176896
128.041168	3709.643134	24.181914
127.827145	3715.610587	24.186931
128.123670	3720.832071	24.191949
128.112806	3724.646649	24.196967
128.328183	3744.475702	24.201984
128.929433	3748.102853	24.207002
128.752100	3750.365353	24.212019
128.905127	3750.199380	24.217037
128.909719	3760.718744	24.222055
129.145408	3760.230500	24.227072
129.426329	3765.460755	24.232090
129.417044	3769.322440	24.237107
129.409590	3757.124425	24.242125
129.399044	3769.921880	24.247143
129.576823	3780.098489	24.252160
129.727702	3790.856927	24.257178
129.588497	3793.163960	24.262195
130.334974	3803.434553	24.267213
130.680462	3803.497248	24.272231
130.784064	3809.212964	24.277248
130.753577	3814.867624	24.282266
130.561540	3805.498169	24.287283
131.053413	3805.181263	24.292301
131.284392	3824.591324	24.297319
131.580232	3813.882893	24.302336
131.896632	3823.823178	24.307354
131.752671	3823.454382	24.312371
131.795849	3814.297423	24.317389
132.089046	3825.759544	24.322407
132.243074	3825.094712	24.327424
132.104239	3827.512163	24.332442
132.193101	3830.433676	24.337459
132.386682	3816.493388	24.342477
132.120521	3826.057804	24.347495
132.194086	3827.514015	24.352512
132.541558	3842.638470	24.357530
132.434381	3842.014560	24.362547
132.716553	3846.032605	24.367565
132.719035	3851.795741	24.372583
133.116172	3868.263353	24.377600
133.051383	3867.500234	24.382618
133.137485	3873.805793	24.387635
133.377562	3873.316860	24.392653
133.300940	3872.495624	24.397671
133.906869	3887.740599	24.402688
133.860945	3893.492393	24.407706
133.656962	3902.450558	24.412723
134.200890	3896.358836	24.417741
134.406584	3904.577359	24.422759
134.380114	3917.374256	24.427776
134.385643	3915.545895	24.432794
134.480405	3924.409922	24.437811
134.528782	3911.694882	24.442829
135.109534	3933.486969	24.447847
134.872368	3940.411342	24.452864
135.074579	3944.482970	24.457882
135.225088	3947.227557	24.462899
135.169744	3957.497603	24.467917
135.344055	3960.942333	24.472935
135.323939	3966.374470	24.477952
135.997958	3967.926003	24.482970
136.451000	3984.811073	24.487987
136.320658	3992.466789	24.493005
136.364544	3990.872296	24.498023
136.218111	3996.295824	24.503040
136.379823	3988.818334	24.508058
136.569204	3999.744466	24.513075
136.619345	4005.304488	24.518093
137.047189	4018.083939	24.523111
137.448452	4022.256968	24.528128
137.581711	4013.123671	24.533146
137.167533	4020.110527	24.538163
137.273836	4032.185989	24.543181
137.393256	4038.546357	24.548199
137.510326	4039.774822	24.553216
138.069563	4047.546631	24.558234
138.050085	4064.098630	24.563251
138.180737	4063.813061	24.568269
138.272247	4056.955723	24.573287
138.347349	4073.937963	24.578304
138.859015	4076.395573	24.583322
138.766498	4089.193470	24.588339
139.111912	4080.885439	24.593357
139.137329	4076.045911	24.598375
139.109920	4084.092713	24.603392
139.550330	4086.501516	24.608410
139.520607	4102.597479	24.613427
139.911864	4091.523577	24.618445
140.462598	4095.581671	24.623463
140.277924	4099.679225	24.628480
140.364913	4089.255863	24.633498
140.075020	4099.452263	24.638515
140.105131	4103.178435	24.643533
140.739188	4116.717903	24.648551
140.756504	4123.163738	24.653568
141.321708	4120.303913	24.658586
141.093469	4114.487755	24.663603
140.984565	4115.170852	24.668621
141.236585	4123.303307	24.673639
141.342472	4130.871570	24.678656
141.543374	4133.302121	24.683674
141.335667	4145.202749	24.688691
141.964626	4141.799501	24.693709
141.965657	4143.838408	24.698727
141.585179	4150.308697	24.703744
142.160663	4161.092371	24.708762
142.202995	4165.599428	24.713779
142.186316	4163.515697	24.718797
142.316375	4160.787166	24.723815
142.571086	4184.489756	24.728832
142.832578	4182.662301	24.733850
142.964650	4187.237371	24.738867
143.038224	4180.988826	24.743885
143.226116	4193.622923	24.748903
143.075550	4206.663571	24.753920
143.366680	4208.401368	24.758938
143.392609	4213.226649	24.763955
143.896968	4226.906463	24.768973
143.862726	4230.235566	24.773991
143.841049	4235.368169	24.779008
144.479853	4229.179407	24.784026
143.938910	4241.075489	24.789043
144.389804	4244.981968	24.794061
144.801078	4250.753785	24.799079
144.428001	4263.785143	24.804096
144.935444	4265.318611	24.809114
144.698951	4277.498444	24.814131
145.448459	4278.406895	24.819149
145.849635	4281.932931	24.824167
145.422619	4292.116200	24.829184
145.926497	4284.540793	24.834202
146.135527	4305.564584	24.839219
145.989074	4303.318095	24.844237
146.513905	4307.705407	24.849255
146.447555	4304.070167	24.854272
146.598242	4298.781679	24.859290
146.813479	4307.178807	24.864307
146.814664	4315.322238	24.869325
147.226155	4324.944886	24.874343
147.145829	4335.582049	24.879360
146.994835	4334.721941	24.884378
147.218043	4325.255596	24.889395
147.303078	4347.173192	24.894413
147.429866	4353.560925	24.899431
147.685561	4362.485177	24.904448
148.068724	4358.441764	24.909466
147.767186	4383.996207	24.914483
147.888419	4385.675415	24.919501
148.254941	4382.423714	24.924519
148.269090	4394.564358	24.929536
148.717057	4403.704711	24.934554
148.379626	4412.762944	24.939571
148.436856	4409.493408	24.944589
149.002722	4428.012037	24.949607
149.051247	4421.846245	24.954624
149.197388	4441.257632	24.959642
149.649409	4442.935526	24.964659
149.588291	4448.500489	24.969677
149.858670	4451.147463	24.974695
149.798395	4455.667511	24.979712
150.590562	4460.221304	24.984730
150.693633	4468.301495	24.989747
150.581363	4466.084351	24.994765
150.945415	4459.234667	24.999783
150.895310	4463.506921	25.004800
151.189735	4453.549572	25.009818
151.002462	4477.574306	25.014835
151.340301	4480.400102	25.019853
151.768277	4477.378647	25.024871
151.337529	4492.221541	25.029888
151.748661	4476.930421	25.034906
151.871381	4492.740861	25.039923
151.792688	4502.888616	25.044941
152.063715	4510.658431	25.049959
151.841870	4506.779212	25.054976
152.460057	4502.758920	25.059994
153.010669	4516.112906	25.065011
152.836581	4520.388815	25.070029
152.927322	4523.420622	25.075047
153.276641	4530.439568	25.080064
153.026240	4527.451785	25.085082
153.132754	4524.373364	25.090099
153.352916	4530.632899	25.095117
153.798572	4543.349959	25.100135
153.709107	4550.027314	25.105152
153.987273	4541.388712	25.110170
154.119231	4546.421579	25.115187
154.156627	4554.821431	25.120205
154.417164	4555.576081	25.125223
154.126811	4566.009548	25.130240
154.497664	4567.586537	25.135258
154.355787	4576.484799	25.140275
154.512623	4599.309984	25.145293
155.106324	4589.984317	25.150311
154.559324	4608.377613	25.155328
155.352750	4606.605667	25.160346
155.382450	4622.487610	25.165363
155.132628	4629.878229	25.170381
155.947724	4631.584485	25.175399
155.965336	4637.014069	25.180416
156.326339	4642.696036	25.185434
156.574205	4659.178286	25.190451
156.860142	4656.595711	25.195469
156.828908	4653.690361	25.200487
157.031467	4662.885074	25.205504
157.130453	4670.378889	25.210522
157.360373	4675.942517	25.215539
157.494885	4686.347370	25.220557
157.550327	4680.246692	25.225575
157.288606	4684.709975	25.230592
157.688179	4696.837787	25.235610
157.818449	4703.970030	25.240627
158.127280	4701.560626	25.245645
158.204323	4715.105741	25.250663
158.313017	4728.623811	25.255680
158.459896	4728.190492	25.260698
158.771685	4729.274866	25.265715
159.029621	4747.213921	25.270733
159.375198	4755.969617	25.275751
159.425916	4753.332341	25.280768
159.457156	4755.663296	25.285786
159.940592	4759.971980	25.290803
159.672915	4752.397308	25.295821
160.018513	4765.174391	25.300839
159.857796	4773.479122	25.305856
160.226410	4763.311121	25.310874
160.285343	4769.684380	25.315891
160.394279	4783.789564	25.320909
160.658646	4791.863569	25.325927
161.119863	4798.505247	25.330944
161.234298	4802.253074	25.335962
161.474147	4804.642893	25.340979
161.685738	4815.663889	25.345997
161.553002	4822.515419	25.351015
161.551094	4824.873671	25.356032
161.647875	4825.025841	25.361050
161.784912	4830.600912	25.366067
161.895318	4851.814395	25.371085
162.487387	4844.089212	25.376103
162.568378	4842.473048	25.381120
162.792985	4859.315811	25.386138
163.157793	4863.826182	25.391155
162.617954	4866.357097	25.396173
163.009884	4863.009793	25.401191
163.038870	4870.918691	25.406208
163.443753	4876.726432	25.411226
163.513322	4886.197772	25.416243
163.610218	4898.947626	25.421261
163.739306	4888.785516	25.426279
164.029519	4899.690081	25.431296
163.808490	4899.068187	25.436314
164.215946	4913.413948	25.441331
164.064313	4921.714167	25.446349
164.397683	4937.372045	25.451367
164.536685	4942.441797	25.456384
164.539630	4947.065698	25.461402
164.628040	4960.328283	25.466419
164.546689	4974.712793	25.471437
165.224773	4983.946807	25.476455
165.530760	4993.450609	25.481472
165.860574	5009.386883	25.486490
166.133069	5007.207247	25.491507
166.039571	5017.663792	25.496525
166.658164	5008.649669	25.501543
166.385225	5017.139388	25.506560
166.504270	5027.493198	25.511578
166.925772	5032.357734	25.516595
166.972508	5044.102294	25.521613
167.619964	5037.012290	25.526631
167.388127	5051.155285	25.531648
167.342847	5053.892835	25.536666
167.779576	5056.526464	25.541683
167.675986	5062.581222	25.546701
167.969675	5071.891285	25.551719
168.273830	5077.370806	25.556736
168.025989	5085.897661	25.561754
168.530454	5093.940499	25.566771
168.482143	5104.235344	25.571789
168.991524	5100.525531	25.576807
168.869684	5116.570535	25.581824
168.992831	5131.551288	25.586842
169.412319	5131.050000	25.591859
169.257298	5128.375456	25.596877
169.421062	5145.281677	25.601895
170.156283	5143.960722	25.606912
169.690628	5143.238253	25.611930
170.363755	5163.492729	25.616947
170.230696	5167.557183	25.621965
170.709597	5166.882445	25.626983
170.862244	5186.786035	25.632000
170.855312	5192.992992	25.637018
171.418469	5188.419304	25.642035
171.533637	5189.004205	25.647053
171.750970	5196.902678	25.652071
171.654668	5193.723342	25.657088
171.891648	5209.573325	25.662106
172.272135	5218.033371	25.667123
172.102457	5216.020837	25.672141
172.362212	5216.036998	25.677159
172.427251	5218.757290	25.682176
172.769036	5233.435565	25.687194
173.138760	5230.290538	25.692212
173.199287	5239.255269	25.697229
173.671067	5241.078504	25.702247
173.497906	5246.670734	25.707264
173.214935	5262.589593	25.712282
173.924220	5258.229740	25.717300
173.610387	5266.820679	25.722317
173.891559	5273.819025	25.727335
174.101431	5275.907413	25.732352
174.293567	5278.835078	25.737370
174.470520	5280.275209	25.742388
174.617740	5298.639355	25.747405
174.913284	5306.825499	25.752423
174.741653	5304.652275	25.757440
174.902728	5313.052041	25.762458
175.021742	5321.556255	25.767476
175.289163	5326.984789	25.772493
175.598856	5329.322700	25.777511
175.759652	5343.199231	25.782528
175.749746	5358.346219	25.787546
176.190048	5347.244935	25.792564
176.170557	5367.238823	25.797581
176.374270	5376.948245	25.802599
176.969762	5377.644143	25.807616
176.576476	5381.585269	25.812634
176.948239	5390.839072	25.817652
176.971463	5404.288963	25.822669
177.154278	5409.831788	25.827687
177.588929	5427.140916	25.832704
178.012327	5426.553780	25.837722
178.245223	5429.636071	25.842740
178.320842	5445.192719	25.847757
178.325188	5454.283152	25.852775
178.867995	5447.269362	25.857792
178.236144	5459.281486	25.862810
179.005943	5469.044322	25.867828
178.878264	5477.303160	25.872845
178.940196	5481.536003	25.877863
179.681731	5488.613829	25.882880
179.450690	5504.556330	25.887898
179.929202	5501.072238	25.892916
180.326612	5523.393712	25.897933
180.078296	5524.288099	25.902951
180.291643	5525.211173	25.907968
180.136303	5533.846853	25.912986
180.441800	5547.372581	25.918004
180.700122	5552.414340	25.923021
180.591632	5564.622327	25.928039
181.039116	5572.317605	25.933056
181.385666	5580.063422	25.938074
181.578690	5598.332308	25.943092
181.745048	5601.522909	25.948109
181.974467	5601.092423	25.953127
182.074790	5617.270365	25.958144
182.283129	5624.153990	25.963162
182.547493	5621.820880	25.968180
182.810979	5638.348921	25.973197
182.921052	5648.070002	25.978215
183.008231	5648.634049	25.983232
183.062497	5653.022810	25.988250
183.925617	5665.176506	25.993268
183.805937	5672.395638	25.998285
184.174893	5668.051126	26.003303
184.336014	5666.324481	26.008320
183.815118	5676.172834	26.013338
184.533919	5681.934814	26.018356
184.751812	5692.803835	26.023373
185.121119	5684.554470	26.028391
185.182265	5692.929030	26.033408
185.291983	5721.536547	26.038426
185.487096	5712.973538	26.043444
185.451010	5727.032725	26.048461
185.299647	5724.070263	26.053479
185.843913	5738.335267	26.058496
185.714251	5741.998419	26.063514
186.112009	5756.810398	26.068532
186.488100	5753.383342	26.073549
186.681700	5763.242919	26.078567
186.732292	5761.299986	26.083584
186.755869	5769.557356	26.088602
187.167210	5780.083614	26.093620
187.367631	5782.290339	26.098637
187.415291	5791.127932	26.103655
187.515475	5802.886705	26.108672
187.869869	5811.644688	26.113690
187.877020	5816.624856	26.118708
187.952719	5818.131401	26.123725
187.939333	5837.673440	26.128743
188.226511	5838.474481	26.133760
188.560956	5860.408489	26.138778
188.895248	5863.834833	26.143796
189.362553	5862.498983	26.148813
189.126889	5879.755720	26.153831
189.594102	5885.020540	26.158848
189.591951	5890.857651	26.163866
189.782676	5897.494760	26.168884
189.744945	5914.628977	26.173901
190.226960	5915.948764	26.178919
190.571368	5933.143086	26.183936
190.622833	5935.657270	26.188954
190.898919	5935.345734	26.193972
190.994073	5951.610013	26.198989
191.076987	5969.476678	26.204007
191.499032	5962.248015	26.209024
191.506390	5978.999579	26.214042
191.713932	5983.222355	26.219060
192.086272	5997.795445	26.224077
192.091064	5992.740825	26.229095
192.150938	6007.514396	26.234112
192.313627	6019.342434	26.239130
192.542745	6034.080043	26.244148
192.572014	6043.141610	26.249165
193.267591	6060.142142	26.254183
193.595447	6049.730434	26.259200
193.642084	6064.253587	26.264218
193.947608	6069.003990	26.269236
194.275005	6085.598186	26.274253
194.436008	6086.905142	26.279271
194.613459	6087.388770	26.284288
194.495367	6088.638433	26.289306
194.860064	6100.122360	26.294324
195.217198	6104.710007	26.299341
195.329420	6114.210027	26.304359
195.550193	6111.861588	26.309376
195.822772	6134.187583	26.314394
196.122790	6123.871740	26.319412
196.292116	6124.145141	26.324429
195.967090	6130.032909	26.329447
196.307337	6139.108941	26.334464
196.660372	6148.905869	26.339482
196.956453	6150.103279	26.344500
196.933415	6157.304304	26.349517
196.938727	6171.306839	26.354535
197.051547	6170.632598	26.359552
197.205098	6184.068959	26.364570
197.670114	6195.691911	26.369588
197.750131	6198.406847	26.374605
197.871243	6220.917671	26.379623
198.533082	6218.626391	26.384640
198.473307	6237.510050	26.389658
198.653509	6260.721937	26.394676
198.766124	6250.410127	26.399693
198.951712	6257.076583	26.404711
199.177358	6273.001872	26.409728
199.193216	6276.175131	26.414746
199.343742	6268.938376	26.419764
199.664504	6292.194575	26.424781
200.116021	6293.838003	26.429799
200.527966	6295.516041	26.434816
200.679897	6299.583451	26.439834
200.678339	6328.184095	26.444852
200.515312	6321.798261	26.449869
200.824654	6337.107550	26.454887
201.404205	6351.238081	26.459904
201.568734	6353.204270	26.464922
201.252765	6354.001963	26.469940
201.586845	6361.746911	26.474957
201.731789	6377.224043	26.479975
202.178566	6382.798419	26.484992
202.267811	6402.766933	26.490010
202.031375	6395.451851	26.495028
202.884219	6408.018041	26.500045
203.202258	6427.111033	26.505063
203.225262	6420.269855	26.510080
203.487599	6441.934904	26.515098
203.903749	6443.343970	26.520116
204.324468	6445.023805	26.525133
203.863932	6440.095625	26.530151
204.516224	6459.076309	26.535168
204.735669	6459.834324	26.540186
205.001802	6463.861781	26.545204
205.213184	6466.420435	26.550221
205.452022	6475.218939	26.555239
205.756739	6483.972402	26.560256
205.873364	6482.328415	26.565274
206.036383	6490.100216	26.570292
206.362242	6487.148102	26.575309
206.151399	6498.340470	26.580327
206.435088	6498.049834	26.585344
206.582536	6498.263532	26.590362
206.881785	6519.026357	26.595380
207.229497	6516.418064	26.600397
207.515054	6532.280527	26.605415
207.423665	6529.501104	26.610432
207.526896	6539.892974	26.615450
207.575690	6553.743776	26.620468
208.118188	6557.563806	26.625485
207.750024	6583.403244	26.630503
208.252185	6578.519935	26.635520
208.065606	6604.899184	26.640538
208.455483	6614.185499	26.645556
208.950526	6628.032742	26.650573
208.956657	6641.041107	26.655591
209.463036	6648.683421	26.660608
209.611217	6665.183103	26.665626
209.797587	6665.602213	26.670644
210.026018	6676.624855	26.675661
210.212263	6689.485079	26.680679
210.662397	6679.404269	26.685696
210.699480	6702.140356	26.690714
210.525338	6709.841953	26.695732
210.890678	6710.479261	26.700749
211.098112	6724.153811	26.705767
211.390211	6736.994328	26.710784
212.027428	6745.550613	26.715802
212.049715	6756.182579	26.720820
212.223877	6754.081282	26.725837
212.395678	6778.299019	26.730855
212.693199	6779.016405	26.735872
212.886456	6790.259292	26.740890
212.905691	6802.504917	26.745908
213.377173	6803.198208	26.750925
213.181401	6820.585323	26.755943
213.446874	6823.176593	26.760960
214.028094	6827.846123	26.765978
213.609940	6841.170489	26.770996
214.123706	6852.880930	26.776013
214.246805	6866.736112	26.781031
214.811365	6876.291941	26.786048
214.774558	6882.589386	26.791066
214.827953	6892.588341	26.796084
215.356242	6903.270555	26.801101
215.304288	6920.190115	26.806119
215.696821	6932.105854	26.811136
215.625155	6940.122966	26.816154
215.888917	6950.420469	26.821172
215.957344	6965.638593	26.826189
216.548215	6973.046826	26.831207
216.901367	6982.901007	26.836224
216.951195	7003.671887	26.841242
216.905159	6995.922654	26.846260
217.106573	7008.180915	26.851277
217.508207	7025.209456	26.856295
217.955500	7042.657041	26.861312
218.501636	7048.241312	26.866330
218.072346	7056.661757	26.871348
218.765437	7064.495980	26.876365
219.100660	7077.715122	26.881383
218.994070	7075.174764	26.886400
219.334180	7091.237522	26.891418
219.239026	7091.271406	26.896436
219.706163	7103.039823	26.901453
219.856961	7118.384074	26.906471
220.073143	7117.150618	26.911488
220.325033	7133.243016	26.916506
220.711458	7150.125681	26.921524
221.295186	7158.378005	26.926541
220.894213	7168.741884	26.931559
221.193880	7169.256907	26.936576
221.734011	7179.599638	26.941594
221.923761	7185.899578	26.946612
222.264045	7184.302572	26.951629
222.266498	7194.404379	26.956647
222.543963	7199.339419	26.961664
222.785752	7208.055734	26.966682
222.698154	7218.421058	26.971700
223.251488	7228.881712	26.976717
223.470458	7237.049152	26.981735
223.653101	7239.817618	26.986752
223.999788	7257.925184	26.991770
224.060324	7262.843713	26.996788
224.360412	7266.162033	27.001805
224.229936	7284.445397	27.006823
224.550824	7293.850202	27.011840
224.809542	7296.297378	27.016858
224.757227	7315.645046	27.021876
225.322504	7320.408753	27.026893
225.315544	7345.274003	27.031911
225.323818	7338.172764	27.036928
226.184040	7356.083170	27.041946
225.878109	7360.888660	27.046964
226.307744	7379.049646	27.051981
226.564192	7385.613862	27.056999
227.132806	7393.338292	27.062016
227.354278	7408.270779	27.067034
227.384629	7424.805387	27.072052
227.696721	7415.459276	27.077069
228.084871	7432.130414	27.082087
227.772373	7442.578451	27.087104
228.265966	7440.610140	27.092122
228.239195	7463.398212	27.097140
228.357770	7467.502677	27.102157
228.588848	7475.415769	27.107175
228.864283	7484.856204	27.112192
229.603440	7488.743491	27.117210
229.539310	7503.275664	27.122228
229.970053	7505.124507	27.127245
230.123772	7512.506734	27.132263
230.160548	7527.525077	27.137280
230.871242	7536.382766	27.142298
230.468672	7545.623219	27.147316
230.796079	7543.081105	27.152333
231.358265	7555.561030	27.157351
231.205483	7562.846070	27.162368
231.539513	7575.074464	27.167386
231.790219	7584.796640	27.172404
231.674356	7593.733330	27.177421
232.249701	7608.127524	27.182439
232.407725	7629.999736	27.187456
232.765485	7641.817205	27.192474
232.482405	7641.959454	27.197492
233.324530	7662.127095	27.202509
233.301539	7669.013004	27.207527
233.291585	7687.890346	27.212544
233.763666	7692.406720	27.217562
233.787303	7710.609537	27.222580
234.277771	7707.009513	27.227597
234.635847	7734.457365	27.232615
234.439858	7738.333351	27.237632
234.874212	7760.355008	27.242650
235.019690	7769.471833	27.247668
235.671663	7786.957517	27.252685
236.029458	7794.869838	27.257703
236.222535	7811.224606	27.262720
236.445589	7817.241727	27.267738
236.652119	7829.575504	27.272756
236.835580	7818.544544	27.277773
237.546433	7841.249100	27.282791
237.506526	7848.604967	27.287808
238.051960	7845.656127	27.292826
237.869762	7868.778437	27.297844
238.217027	7872.736671	27.302861
238.672241	7875.298368	27.307879
238.541610	7888.739454	27.312896
238.717205	7894.299950	27.317914
239.037383	7902.395005	27.322932
239.158241	7916.061906	27.327949
239.090364	7920.760792	27.332967
239.601439	7943.553598	27.337984
239.880318	7934.376596	27.343002
240.056486	7960.394724	27.348020
240.151205	7973.304912	27.353037
240.072470	7986.460118	27.358055
240.671843	7996.689848	27.363072
240.920299	8012.221598	27.368090
241.435694	8028.949113	27.373108
241.643893	8042.447729	27.378125
241.942544	8049.337063	27.383143
241.824337	8064.446421	27.388160
242.148632	8075.865306	27.393178
242.456909	8093.657689	27.398196
242.582080	8107.472439	27.403213
243.048933	8108.589560	27.408231
242.934866	8137.018057	27.413248
243.635993	8133.025044	27.418266
243.788967	8152.827620	27.423284
244.520251	8160.599506	27.428301
244.372531	8157.099372	27.433319
244.381406	8173.606444	27.438336
245.371384	8175.768702	27.443354
245.387098	8187.153912	27.448372
245.545764	8184.881242	27.453389
245.716477	8189.953243	27.458407
245.651251	8207.952631	27.463424
245.914536	8209.878295	27.468442
246.331421	8218.558188	27.473460
246.164506	8226.284540	27.478477
246.799352	8236.824558	27.483495
246.937033	8248.935776	27.488512
247.187144	8254.544692	27.493530
247.322198	8265.709201	27.498548
247.313892	8274.020048	27.503565
247.472131	8283.510824	27.508583
247.922731	8300.049839	27.513600
248.145389	8302.395459	27.518618
248.434045	8320.099578	27.523636
248.431413	8332.886355	27.528653
249.006094	8344.862878	27.533671
249.260045	8362.471447	27.538688
249.508776	8365.071875	27.543706
249.963253	8390.548185	27.548724
250.162399	8395.650517	27.553741
250.539318	8399.803119	27.558759
250.699346	8412.567626	27.563776
251.123313	8425.284481	27.568794
251.146046	8429.688317	27.573812
251.800881	8439.849622	27.578829
251.822843	8446.653007	27.583847
251.760335	8455.790125	27.588864
252.278535	8468.678520	27.593882
252.559393	8475.472930	27.598900
252.667875	8490.812324	27.603917
253.192564	8502.705225	27.608935
253.257007	8517.151752	27.613952
253.329652	8531.663306	27.618970
253.584191	8538.913336	27.623988
253.892162	8558.853081	27.629005
254.299997	8558.508242	27.634023
254.418996	8576.769588	27.639040
254.739932	8587.892543	27.644058
254.860404	8603.208052	27.649076
255.247259	8610.178494	27.654093
255.768697	8622.813916	27.659111
255.784018	8634.985598	27.664128
256.054715	8635.805137	27.669146
255.963861	8645.167790	27.674164
256.284401	8660.082616	27.679181
256.972268	8661.749228	27.684199
257.083435	8684.343552	27.689216
257.592636	8692.589303	27.694234
257.692128	8703.671246	27.699252
257.689643	8717.664308	27.704269
258.373633	8719.179989	27.709287
258.306471	8729.495601	27.714304
258.786279	8741.351486	27.719322
259.217214	8755.781831	27.724340
258.807358	8760.228255	27.729357
259.371434	8768.452815	27.734375
259.311220	8779.840812	27.739392
260.057862	8797.012694	27.744410
260.147360	8809.264429	27.749428
260.116370	8819.097687	27.754445
260.937901	8826.590515	27.759463
261.104271	8848.289217	27.764480
261.334853	8866.258691	27.769498
261.531832	8853.690595	27.774516
261.549793	8876.839636	27.779533
261.480865	8872.288300	27.784551
261.924867	8898.455224	27.789568
262.672063	8911.759538	27.794586
262.921007	8914.609431	27.799604
263.184247	8929.078810	27.804621
263.269077	8927.357502	27.809639
263.694723	8932.708651	27.814656
263.765278	8951.836719	27.819674
264.037533	8959.829244	27.824692
264.352198	8974.116956	27.829709
264.680325	8975.596846	27.834727
264.592549	8994.838164	27.839744
265.255352	9002.204383	27.844762
265.733571	9004.229066	27.849780
265.393942	9021.763915	27.854797
266.012311	9027.956299	27.859815
266.125442	9035.512828	27.864832
266.240119	9054.520430	27.869850
266.599476	9066.483796	27.874868
266.765437	9074.893992	27.879885
266.926590	9087.147315	27.884903
267.404224	9108.317659	27.889920
267.190407	9107.786042	27.894938
268.052971	9128.027866	27.899956
267.830378	9147.612501	27.904973
268.261820	9162.996577	27.909991
268.164151	9182.984753	27.915008
268.774467	9197.816731	27.920026
269.161445	9215.506306	27.925044
269.442928	9228.157632	27.930061
269.955039	9239.847757	27.935079
269.933221	9260.209321	27.940096
270.339033	9272.105554	27.945114
270.596285	9290.658516	27.950132
270.764534	9299.848305	27.955149
271.231355	9311.008831	27.960167
271.128154	9329.864566	27.965184
271.215186	9343.209462	27.970202
272.023510	9372.508847	27.975220
271.952653	9392.982429	27.980237
272.809312	9405.827931	27.985255
272.863211	9414.855724	27.990272
273.279812	9426.147321	27.995290
273.742790	9438.160999	28.000308
274.209829	9441.627215	28.005325
274.148515	9454.136642	28.010343
274.589080	9467.988247	28.015360
274.824045	9465.460357	28.020378
274.998271	9489.441314	28.025396
275.147912	9496.926007	28.030413
275.437573	9512.490450	28.035431
275.830227	9525.487655	28.040448
276.071712	9524.041698	28.045466
276.746334	9544.212384	28.050484
276.656437	9552.498696	28.055501
276.850136	9562.991762	28.060519
277.173081	9573.597194	28.065536
277.595901	9590.438505	28.070554
278.103386	9595.382361	28.075572
278.057211	9607.987397	28.080589
278.519014	9611.678637	28.085607
278.585008	9620.903546	28.090624
278.928007	9630.337655	28.095642
279.486988	9632.188734	28.100660
279.355907	9642.628529	28.105677
279.511117	9652.884559	28.110695
279.484870	9670.339352	28.115712
280.206430	9687.354968	28.120730
280.415140	9699.490738	28.125748
280.344905	9708.875956	28.130765
280.814858	9719.594209	28.135783
281.131555	9735.865009	28.140800
281.495849	9747.209200	28.145818
281.810038	9746.250699	28.150836
282.008429	9768.974760	28.155853
282.405331	9776.711310	28.160871
282.675802	9784.047739	28.165888
282.528806	9803.210763	28.170906
282.950050	9801.411417	28.175924
283.359269	9829.009075	28.180941
283.634846	9837.045663	28.185959
283.942434	9843.950056	28.190976
283.959799	9850.543132	28.195994
284.546223	9856.576617	28.201012
284.956480	9883.602709	28.206029
285.259395	9898.574969	28.211047
285.660779	9899.500390	28.216064
285.777696	9917.902306	28.221082
285.967885	9930.514737	28.226100
286.306384	9938.494151	28.231117
286.582238	9952.188792	28.236135
286.751202	9958.480307	28.241152
286.746647	9978.751545	28.246170
287.573803	9990.200192	28.251188
287.932550	10000.042484	28.256205
288.140971	10021.972775	28.261223
288.343747	10022.891426	28.266240
288.291393	10042.500850	28.271258
288.899909	10045.664010	28.276276
288.964578	10073.375996	28.281293
289.227891	10082.854392	28.286311
289.665626	10102.649174	28.291328
289.838664	10108.071811	28.296346
290.448824	10122.288859	28.301364
290.644569	10140.697591	28.306381
290.862441	10147.581420	28.311399
291.435773	10165.937343	28.316416
291.545614	10189.300959	28.321434
292.214460	10186.054575	28.326452
292.396166	10212.223393	28.331469
292.695174	10212.785976	28.336487
292.897035	10227.095481	28.341504
293.276917	10235.119059	28.346522
293.750249	10242.780683	28.351540
293.872351	10263.446015	28.356557
293.902428	10265.582089	28.361575
294.657555	10281.247921	28.366592
294.586988	10285.726803	28.371610
295.175398	10294.699709	28.376628
295.067046	10315.063351	28.381645
295.310303	10326.379495	28.386663
296.148978	10337.968640	28.391680
296.091415	10342.107651	28.396698
296.304755	10344.805471	28.401716
296.596155	10365.943275	28.406733
296.437570	10372.968253	28.411751
297.074184	10392.504851	28.416768
297.202222	10411.142322	28.421786
297.255002	10416.647037	28.426804
298.148433	10440.036620	28.431821
298.370428	10463.720860	28.436839
298.760874	10472.030217	28.441856
298.859070	10485.108954	28.446874
299.198928	10490.202452	28.451892
299.415272	10507.222183	28.456909
299.735052	10521.668160	28.461927
300.475921	10531.454033	28.466944
300.779015	10537.345834	28.471962
300.875981	10540.693412	28.476980
300.816457	10563.086258	28.481997
300.960987	10566.287459	28.487015
301.533595	10574.814611	28.492032
301.397495	10590.127743	28.497050
302.028482	10609.400221	28.502068
302.063207	10622.994198	28.507085
301.870270	10645.657485	28.512103
302.725835	10656.255883	28.517120
302.997288	10675.379511	28.522138
303.590381	10693.221342	28.527156
303.744030	10706.856743	28.532173
304.258042	10719.210585	28.537191
304.578354	10741.809377	28.542208
304.556309	10757.698394	28.547226
305.014810	10764.058498	28.552244
305.361749	10783.893487	28.557261
305.655182	10799.711019	28.562279
306.203970	10810.338616	28.567296
306.010382	10831.303473	28.572314
306.609386	10831.995905	28.577332
306.683262	10857.781511	28.582349
307.058692	10880.327630	28.587367
307.614971	10889.460578	28.592384
307.962758	10914.240300	28.597402
308.345517	10919.352457	28.602420
309.063518	10933.439562	28.607437
308.980278	10943.143191	28.612455
309.537099	10958.477540	28.617472
309.496703	10971.489915	28.622490
309.857936	10974.947737	28.627508
309.916685	10996.975242	28.632525
310.203471	11018.613403	28.637543
310.795050	11025.410599	28.642560
311.105045	11049.410184	28.647578
311.745158	11062.050786	28.652596
312.049102	11067.348997	28.657613
312.169628	11084.346373	28.662631
312.528821	11097.242562	28.667648
312.807538	11117.909565	28.672666
312.925449	11119.599388	28.677684
313.222105	11140.547789	28.682701
313.804865	11160.081000	28.687719
314.087540	11178.186638	28.692736
314.123506	11193.795384	28.697754
314.802185	11205.700636	28.702772
314.920997	11219.496590	28.707789
314.929368	11225.472668	28.712807
315.378788	11238.064321	28.717824
315.959564	11253.448839	28.722842
316.193439	11269.677115	28.727860
316.790211	11283.884520	28.732877
316.713915	11292.958876	28.737895
317.126155	11305.253266	28.742912
317.463602	11322.081100	28.747930
317.949100	11332.488404	28.752948
318.386488	11338.779387	28.757965
318.807179	11349.367364	28.762983
319.393024	11356.989721	28.768000
319.369686	11376.747564	28.773018
319.638066	11374.252078	28.778036
320.102896	11389.635926	28.783053
320.114990	11393.514804	28.788071
320.243029	11409.188247	28.793088
320.413536	11428.502128	28.798106
320.889798	11440.496076	28.803124
320.975764	11455.806704	28.808141
321.134112	11485.318596	28.813159
321.790637	11495.370804	28.818176
321.959493	11515.420767	28.823194
322.391689	11523.341978	28.828212
322.759462	11542.224053	28.833229
322.771300	11545.758817	28.838247
323.736804	11559.390815	28.843264
323.443510	11577.334448	28.848282
323.893795	11592.730215	28.853300
324.209303	11604.679981	28.858317
324.072946	11623.900036	28.863335
324.684396	11639.823189	28.868352
324.599032	11657.399614	28.873370
325.189545	11680.111939	28.878388
325.713826	11693.014256	28.883405
326.141826	11721.325407	28.888423
326.251361	11741.495423	28.893440
326.746748	11765.334261	28.898458
326.964082	11777.015322	28.903476
327.312683	11805.162206	28.908493
327.692762	11813.145385	28.913511
327.881067	11836.672438	28.918528
328.697570	11849.889067	28.923546
329.112712	11863.493822	28.928564
329.257894	11876.345129	28.933581
329.326519	11900.244674	28.938599
330.319889	11917.908139	28.943616
330.293344	11925.250889	28.948634
330.448445	11937.737546	28.953652
331.110878	11965.349219	28.958669
331.451584	11984.482282	28.963687
331.578666	11997.380716	28.968704
331.744726	12013.841300	28.973722
332.263787	12026.305739	28.978740
332.878413	12042.137162	28.983757
332.858352	12067.961248	28.988775
333.593129	12071.363920	28.993792
333.791899	12094.943339	28.998810
333.694708	12101.504627	29.003828
334.423482	12115.420420	29.008845
334.371971	12136.961291	29.013863
334.845457	12160.355660	29.018880
334.753940	12177.819854	29.023898
335.458266	12197.420365	29.028916
336.236656	12215.250414	29.033933
335.960900	12235.096063	29.038951
336.874849	12251.196553	29.043968
336.942315	12271.430567	29.048986
337.162555	12287.166086	29.054004
337.997031	12302.818033	29.059021
337.993076	12320.394954	29.064039
338.467566	12339.873727	29.069056
338.760058	12361.102029	29.074074
338.658232	12373.932370	29.079092
339.262036	12393.261472	29.084109
339.656476	12403.168914	29.089127
339.687702	12428.268637	29.094144
340.365720	12441.681059	29.099162
340.700378	12460.319777	29.104180
341.364860	12476.203756	29.109197
341.387654	12498.270229	29.114215
342.204806	12500.463264	29.119232
342.134669	12520.523313	29.124250
342.608510	12535.543541	29.129268
343.132561	12548.787529	29.134285
343.137763	12574.371513	29.139303
343.696247	12566.683160	29.144320
344.084327	12581.625281	29.149338
344.472922	12597.678892	29.154356
345.050875	12594.711605	29.159373
345.102867	12610.164281	29.164391
345.500897	12611.204055	29.169408
345.657787	12619.926739	29.174426
346.006676	12632.803494	29.179444
346.135078	12649.071588	29.184461
346.299055	12667.585671	29.189479
347.212433	12672.517300	29.194496
347.309046	12694.165077	29.199514
347.589519	12703.724219	29.204532
348.313498	12721.348539	29.209549
348.200356	12731.124087	29.214567
348.852227	12750.670236	29.219584
349.058681	12758.699963	29.224602
349.252990	12776.470461	29.229620
349.730741	12792.908165	29.234637
349.611953	12813.974034	29.239655
350.034153	12825.108923	29.244672
350.701189	12844.510689	29.249690
350.824566	12863.561848	29.254708
351.241534	12886.236501	29.259725
351.216223	12909.293092	29.264743
351.628692	12924.920086	29.269760
351.857180	12953.510658	29.274778
352.663303	12967.367601	29.279796
353.179224	12989.010034	29.284813
353.326602	13020.619738	29.289831
353.868336	13030.014964	29.294848
354.254972	13048.529279	29.299866
354.409799	13068.024141	29.304884
354.925658	13084.023495	29.309901
355.227214	13109.858626	29.314919
355.620450	13137.005761	29.319936
355.843165	13150.404746	29.324954
356.156707	13170.459069	29.329972
356.680910	13192.678340	29.334989
356.990415	13209.682770	29.340007
357.358198	13219.907455	29.345024
357.736397	13246.324460	29.350042
358.373590	13265.977656	29.355060
358.471380	13286.353271	29.360077
358.568772	13311.162743	29.365095
358.891380	13326.362031	29.370112
359.647075	13350.402107	29.375130
360.136559	13357.336153	29.380148
360.545213	13365.653420	29.385165
360.821213	13391.688733	29.390183
361.280916	13394.847366	29.395200
361.693069	13404.515714	29.400218
362.271361	13425.157274	29.405236
362.802272	13440.841934	29.410253
362.916336	13459.917257	29.415271
363.329910	13461.829408	29.420288
363.731635	13475.885866	29.425306
363.809374	13489.718338	29.430324
364.473553	13515.787757	29.435341
364.376902	13522.949471	29.440359
364.794545	13544.336347	29.445376
365.295123	13559.068983	29.450394
365.519797	13571.782674	29.455412
365.987472	13588.339496	29.460429
366.195164	13602.063270	29.465447
366.725804	13624.945223	29.470464
367.135807	13643.645943	29.475482
367.227290	13660.167014	29.480500
367.734249	13669.214309	29.485517
367.687970	13687.765482	29.490535
368.039703	13709.803948	29.495552
368.852708	13732.291261	29.500570
368.828291	13750.561165	29.505588
369.273246	13762.283595	29.510605
369.329127	13779.176678	29.515623
369.739423	13792.594106	29.520640
370.433569	13807.779795	29.525658
370.207389	13841.157882	29.530676
370.532893	13865.373373	29.535693
370.969119	13885.788203	29.540711
371.299577	13912.080977	29.545728
372.032088	13931.442026	29.550746
372.217355	13957.287054	29.555764
372.831083	13986.302025	29.560781
373.170891	14008.882736	29.565799
373.539995	14030.656734	29.570816
373.730675	14044.607716	29.575834
374.475506	14081.721722	29.580852
374.906455	14091.949618	29.585869
375.267501	14112.723858	29.590887
375.698706	14139.778057	29.595904
376.544136	14153.339174	29.600922
376.462825	14169.616157	29.605940
376.715811	14180.093044	29.610957
377.203785	14209.825996	29.615975
377.675103	14224.718481	29.620992
378.262589	14235.632510	29.626010
378.548705	14258.395625	29.631028
378.869114	14270.785293	29.636045
379.099172	14296.093202	29.641063
379.404111	14309.249584	29.646080
379.848469	14327.566622	29.651098
380.131016	14355.332885	29.656116
380.811211	14367.037791	29.661133
380.925959	14395.683093	29.666151
381.282495	14424.859030	29.671168
381.769172	14442.443177	29.676186
381.770069	14469.366284	29.681204
382.073847	14491.915315	29.686221
382.913016	14521.694805	29.691239
383.228348	14535.051837	29.696256
383.680299	14560.031631	29.701274
384.130822	14585.728586	29.706292
384.679965	14600.814458	29.711309
384.510077	14625.376959	29.716327
385.081868	14636.903206	29.721344
385.588657	14666.289682	29.726362
385.853308	14680.428511	29.731380
386.584111	14697.753582	29.736397
386.925061	14720.028615	29.741415
387.248323	14739.154565	29.746432
387.906504	14758.982884	29.751450
388.051792	14782.204515	29.756468
388.598089	14799.795445	29.761485
388.885375	14817.682777	29.766503
388.889570	14839.508543	29.771520
389.830470	14862.362467	29.776538
390.095024	14883.342156	29.781556
390.534530	14899.642404	29.786573
390.851434	14922.508869	29.791591
390.999807	14944.489032	29.796608
391.339413	14963.903206	29.801626
391.730071	14976.241273	29.806644
392.134640	15006.563333	29.811661
392.720125	15023.279816	29.816679
392.770854	15051.348696	29.821696
393.450263	15063.218386	29.826714
393.827139	15092.215296	29.831732
394.608703	15101.826650	29.836749
394.816491	15117.563311	29.841767
395.086790	15126.424138	29.846784
395.667257	15143.779482	29.851802
395.963604	15158.978035	29.856820
396.347693	15160.073834	29.861837
396.958805	15189.773237	29.866855
396.971187	15204.858392	29.871872
397.262936	15219.625030	29.876890
397.561346	15246.755293	29.881908
397.841505	15258.807658	29.886925
398.532850	15278.302862	29.891943
398.816939	15305.185947	29.896960
398.855721	15319.054274	29.901978
399.428048	15349.928569	29.906996
400.057163	15372.964593	29.912013
400.491294	15391.502180	29.917031
400.820159	15411.670168	29.922048
401.259247	15439.132399	29.927066
401.705382	15462.134026	29.932084
402.022066	15492.754871	29.937101
401.931090	15509.508257	29.942119
402.880354	15534.386163	29.947136
403.247183	15553.550323	29.952154
403.526225	15585.402645	29.957172
403.948340	15596.308620	29.962189
404.409786	15621.878926	29.967207
404.711180	15650.556882	29.972224
405.570848	15665.225433	29.977242
405.730654	15697.968322	29.982260
406.426073	15716.010494	29.987277
406.476320	15748.906441	29.992295
406.780179	15769.021872	29.997312
407.550516	15788.780003	30.002330
407.686518	15814.767914	30.007348
408.132665	15838.632228	30.012365
408.951739	15862.602393	30.017383
409.255967	15884.556064	30.022400
409.842773	15898.736927	30.027418
410.174142	15914.574906	30.032436
410.629058	15944.457868	30.037453
411.162247	15950.081606	30.042471
411.271297	15978.177451	30.047488
411.922239	15998.096629	30.052506
412.086681	16013.660788	30.057524
412.579959	16041.961849	30.062541
413.012566	16045.624206	30.067559
413.103272	16079.158697	30.072576
413.385091	16092.645248	30.077594
413.966292	16119.561898	30.082612
414.474479	16143.101031	30.087629
414.954694	16162.222773	30.092647
415.038274	16185.395761	30.097664
415.683383	16210.584341	30.102682
415.987806	16242.231638	30.107700
416.771667	16256.852510	30.112717
417.104833	16277.895625	30.117735
417.246640	16306.416368	30.122752
418.164241	16327.345886	30.127770
418.275929	16344.396735	30.132788
418.891449	16373.560348	30.137805
419.593955	16384.160702	30.142823
419.962502	16400.596526	30.147840
420.642184	16411.045706	30.152858
420.927505	16433.821011	30.157876
421.420277	16446.055598	30.162893
421.986535	16465.018875	30.167911
422.014756	16482.468254	30.172928
422.503189	16482.622355	30.177946
422.848874	16494.917913	30.182964
423.075791	16503.072358	30.187981
423.429706	16518.174536	30.192999
423.716315	16530.460419	30.198016
424.332476	16547.031302	30.203034
424.583900	16574.890941	30.208052
425.033937	16586.775401	30.213069
425.261273	16612.933279	30.218087
425.626808	16635.844710	30.223104
426.083578	16651.392024	30.228122
426.436798	16672.606150	30.233140
427.136428	16690.301147	30.238157
427.569823	16711.505916	30.243175
427.788399	16743.202228	30.248192
428.192860	16759.771710	30.253210
428.733618	16787.816910	30.258228
428.790599	16815.179878	30.263245
429.114361	16830.883989	30.268263
429.484941	16854.638220	30.273280
430.638083	16881.346330	30.278298
430.765409	16906.310547	30.283316
431.032550	16932.936407	30.288333
431.852515	16954.254615	30.293351
432.101915	16983.827101	30.298368
432.539284	17001.816150	30.303386
432.955964	17022.224762	30.308404
433.314976	17051.789660	30.313421
434.117999	17080.463825	30.318439
434.592195	17101.021441	30.323456
435.036536	17123.061974	30.328474
435.267258	17147.397542	30.333492
435.639514	17176.815262	30.338509
435.789028	17186.097104	30.343527
436.618156	17224.451656	30.348544
436.869969	17243.003799	30.353562
437.164762	17275.358672	30.358580
437.801215	17300.243653	30.363597
438.249929	17324.899065	30.368615
438.646479	17354.123733	30.373632
439.009178	17384.257114	30.378650
439.510947	17398.076532	30.383668
439.453801	17428.699001	30.388685
440.445763	17455.480536	30.393703
440.677439	17487.555055	30.398720
441.676847	17518.296454	30.403738
441.617044	17539.247727	30.408756
442.501852	17566.058834	30.413773
443.018818	17587.823195	30.418791
443.472948	17618.372199	30.423808
443.754531	17640.129267	30.428826
444.196757	17664.944063	30.433844
444.530675	17684.582988	30.438861
445.389857	17700.374513	30.443879
445.654303	17729.222445	30.448896
446.027758	17754.142889	30.453914
446.615984	17772.567038	30.458932
447.035506	17796.987566	30.463949
447.819711	17808.608809	30.468967
447.691154	17836.684562	30.473984
448.393826	17862.153733	30.479002
449.231424	17873.406560	30.484020
449.008037	17897.599408	30.489037
449.911460	17914.439189	30.494055
450.146712	17937.675810	30.499072
450.786180	17945.914707	30.504090
451.148447	17977.388379	30.509108
451.469923	17996.031412	30.514125
452.120697	18009.499422	30.519143
452.095765	18029.643445	30.524160
452.386318	18042.479295	30.529178
452.808757	18070.728101	30.534196
453.202402	18090.623417	30.539213
453.415071	18114.287059	30.544231
453.999699	18142.093610	30.549248
454.451534	18174.286403	30.554266
454.895279	18196.757846	30.559284
455.324903	18234.412559	30.564301
456.138346	18256.996739	30.569319
456.296356	18287.858519	30.574336
456.952871	18311.073827	30.579354
457.469529	18327.753435	30.584372
457.831543	18360.832430	30.589389
458.360146	18374.395642	30.594407
458.550893	18409.371550	30.599424
458.959594	18433.864069	30.604442
459.586769	18464.393622	30.609460
460.044317	18489.257617	30.614477
460.482749	18510.390921	30.619495
461.105573	18548.136017	30.624512
461.318365	18580.992372	30.629530
462.156729	18605.171421	30.634548
462.362709	18637.308726	30.639565
463.134105	18657.120187	30.644583
463.520079	18690.688770	30.649600
463.782656	18709.196407	30.654618
464.683276	18737.137531	30.659636
464.718660	18773.035541	30.664653
465.482545	18795.040565	30.669671
466.048242	18816.678640	30.674688
465.793998	18836.815191	30.679706
466.932258	18866.538787	30.684724
467.198705	18902.154451	30.689741
467.747035	18924.919926	30.694759
468.291493	18952.007388	30.699776
468.692297	18971.567646	30.704794
469.129354	19008.553010	30.709812
469.466430	19030.530386	30.714829
469.866688	19058.468213	30.719847
470.536828	19096.712387	30.724864
470.820909	19121.692810	30.729882
471.549969	19141.669344	30.734900
472.053581	19189.018506	30.739917
472.519707	19211.133819	30.744935
472.784158	19243.262965	30.749952
473.363852	19270.781284	30.754970
474.294939	19296.336604	30.759988
474.609795	19323.801711	30.765005
474.810977	19346.508331	30.770023
475.415317	19373.353238	30.775040
475.778047	19393.937067	30.780058
476.518849	19414.234255	30.785076
476.811477	19453.189004	30.790093
477.437852	19483.726602	30.795111
477.865949	19504.414032	30.800128
478.401475	19532.293443	30.805146
479.143310	19556.968963	30.810164
479.370702	19580.796348	30.815181
479.947076	19605.788473	30.820199
480.520254	19629.681800	30.825216
481.195003	19654.500629	30.830234
481.643858	19675.658839	30.835252
481.899713	19693.530346	30.840269
482.381298	19719.895835	30.845287
483.135699	19744.310586	30.850304
482.891487	19759.328915	30.855322
483.890367	19778.941623	30.860340
483.984383	19801.867735	30.865357
484.375152	19820.154172	30.870375
484.967136	19841.151147	30.875392
485.139016	19866.169052	30.880410
485.839919	19883.680396	30.885428
486.388783	19921.547145	30.890445
486.942071	19931.727408	30.895463
487.429422	19968.213904	30.900480
487.380136	19989.519975	30.905498
488.269694	20018.184939	30.910516
488.647379	20039.101965	30.915533
489.121644	20074.358676	30.920551
489.696680	20099.945547	30.925568
489.782668	20127.156996	30.930586
490.349218	20163.081772	30.935604
490.742069	20197.144686	30.940621
491.572895	20223.171836	30.945639
492.151203	20261.716996	30.950656
492.589502	20284.981478	30.955674
493.177171	20318.729771	30.960692
493.291012	20343.131872	30.965709
494.085277	20370.137950	30.970727
494.564708	20389.952681	30.975744
494.915561	20423.656110	30.980762
495.725599	20444.613263	30.985780
495.969544	20478.207165	30.990797
496.621156	20514.934319	30.995815
497.442764	20539.320584	31.000832
497.629111	20572.045426	31.005850
498.771059	20591.996690	31.010868
499.011748	20623.544223	31.015885
499.360397	20646.254527	31.020903
500.103076	20659.128701	31.025920
500.500212	20693.659363	31.030938
501.465145	20711.111142	31.035956
501.538376	20739.007817	31.040973
501.735396	20758.961930	31.045991
501.948021	20791.607202	31.051008
502.859510	20813.382885	31.056026
503.722804	20838.186325	31.061044
504.034280	20883.648894	31.066061
504.600466	20901.542401	31.071079
504.644852	20934.662868	31.076096
504.961276	20967.450135	31.081114
505.840959	21003.182082	31.086132
506.062800	21036.894133	31.091149
507.016057	21065.121001	31.096167
507.498871	21077.379034	31.101184
507.815792	21111.537568	31.106202
508.570891	21136.686892	31.111220
509.178182	21168.771817	31.116237
509.472070	21196.103826	31.121255
510.341281	21222.625456	31.126272
510.684877	21257.626744	31.131290
511.137369	21278.078444	31.136308
511.646845	21313.274998	31.141325
512.383860	21335.647257	31.146343
512.682570	21360.628245	31.151360
512.860007	21391.074851	31.156378
513.887310	21413.483874	31.161396
514.064948	21451.026286	31.166413
514.353057	21481.152406	31.171431
514.815013	21509.678014	31.176448
515.365976	21538.379280	31.181466
516.205306	21565.392585	31.186484
516.609798	21606.912080	31.191501
517.055997	21634.410401	31.196519
517.523787	21646.355212	31.201536
518.015832	21672.974434	31.206554
518.229299	21700.762045	31.211572
518.867536	21729.058164	31.216589
519.174315	21748.629605	31.221607
519.902582	21780.203723	31.226624
520.104288	21813.528497	31.231642
520.762776	21837.531211	31.236660
521.030820	21874.396805	31.241677
521.744286	21918.667751	31.246695
522.475471	21953.634844	31.251712
522.886676	21982.826233	31.256730
523.475317	22009.898368	31.261748
524.119499	22034.478569	31.266765
524.845156	22071.095932	31.271783
525.377833	22091.238935	31.276800
525.230143	22127.500323	31.281818
526.150758	22162.090583	31.286836
526.905123	22192.498614	31.291853
527.118221	22229.613590	31.296871
527.686308	22254.983199	31.301888
528.248456	22283.879682	31.306906
528.954733	22317.524364	31.311924
529.637442	22352.904163	31.316941
530.096689	22385.854664	31.321959
530.745555	22408.608444	31.326976
531.214966	22443.939667	31.331994
532.072922	22475.823168	31.337012
532.358324	22500.068370	31.342029
532.773642	22527.932949	31.347047
533.472679	22550.818051	31.352064
534.281673	22591.543264	31.357082
534.478850	22606.115486	31.362100
535.134475	22641.727525	31.367117
535.395359	22675.177178	31.372135
536.066844	22701.137786	31.377152
536.719601	22727.076085	31.382170
537.494052	22757.879936	31.387188
537.892536	22788.376218	31.392205
538.167956	22821.678504	31.397223
538.689987	22850.980196	31.402240
539.137448	22886.126075	31.407258
539.774302	22911.119251	31.412276
540.506355	22945.778330	31.417293
541.021191	22974.702189	31.422311
541.828768	23009.975138	31.427328
542.457351	23044.246174	31.432346
543.046863	23063.913655	31.437364
543.361186	23089.684267	31.442381
543.863975	23126.224744	31.447399
544.111090	23144.827450	31.452416
544.963263	23179.613464	31.457434
545.461398	23207.048964	31.462452
546.018893	23232.080251	31.467469
546.384640	23267.896794	31.472487
546.956195	23296.300387	31.477504
547.512604	23334.008212	31.482522
548.401968	23367.057276	31.487540
548.751131	23400.279471	31.492557
549.107541	23431.649059	31.497575
549.819809	23456.681665	31.502592
550.614828	23488.014244	31.507610
550.948285	23512.385859	31.512628
551.454286	23542.329324	31.517645
551.726891	23580.233727	31.522663
552.532007	23603.811188	31.527680
553.064515	23637.087212	31.532698
553.765816	23656.023695	31.537716
554.693498	23686.400556	31.542733
554.996749	23711.004639	31.547751
555.787794	23719.911053	31.552768
555.746792	23738.546800	31.557786
556.223218	23771.756002	31.562804
556.484035	23796.834466	31.567821
556.974934	23831.305363	31.572839
557.619833	23857.467548	31.577856
557.568433	23897.540277	31.582874
558.686648	23929.050428	31.587892
559.413840	23964.369259	31.592909
559.991004	23991.060416	31.597927
560.711697	24017.962947	31.602944
561.228505	24058.907554	31.607962
561.639654	24085.384701	31.612980
562.327570	24130.941105	31.617997
562.675251	24155.184890	31.623015
563.653026	24185.718974	31.628032
563.844401	24222.240721	31.633050
564.419836	24248.774507	31.638068
565.145265	24291.734424	31.643085
565.643583	24323.196939	31.648103
566.350315	24340.148906	31.653120
566.858443	24393.342734	31.658138
567.551214	24426.443307	31.663156
568.299922	24460.356713	31.668173
568.933452	24488.341530	31.673191
569.587050	24511.969077	31.678208
569.899846	24539.384883	31.683226
570.365801	24564.046689	31.688244
571.077785	24607.161058	31.693261
571.571092	24633.682941	31.698279
572.442839	24663.204270	31.703296
572.871529	24692.997261	31.708314
573.444734	24731.975338	31.713332
573.797008	24757.356664	31.718349
574.060165	24795.587150	31.723367
574.944378	24832.121572	31.728384
575.758983	24869.697066	31.733402
576.099872	24893.007499	31.738420
576.509455	24935.537970	31.743437
576.752444	24967.408028	31.748455
577.793372	25009.751302	31.753472
578.084238	25046.992055	31.758490
578.679141	25095.093106	31.763508
579.553655	25121.505373	31.768525
580.089800	25162.872632	31.773543
581.083157	25193.702846	31.778560
581.640798	25227.438924	31.783578
582.165923	25261.079035	31.788596
582.683013	25289.367599	31.793613
583.424004	25328.554389	31.798631
584.163484	25355.771769	31.803648
584.435788	25382.379813	31.808666
584.925340	25418.838079	31.813684
585.963528	25443.828456	31.818701
586.130769	25481.746638	31.823719
586.739269	25501.634747	31.828736
587.509607	25539.578661	31.833754
588.175974	25567.149051	31.838772
588.635613	25597.892840	31.843789
588.973461	25644.044700	31.848807
589.762807	25676.127349	31.853824
590.543714	25713.096669	31.858842
590.896544	25740.432006	31.863860
591.517031	25762.088076	31.868877
591.967284	25810.763328	31.873895
592.917288	25831.154435	31.878912
593.179250	25866.688522	31.883930
593.389602	25888.029763	31.888948
594.111884	25916.084834	31.893965
594.499531	25953.501705	31.898983
595.445382	25969.368486	31.904000
596.491057	25999.856786	31.909018
596.820247	26026.071251	31.914036
597.611111	26057.326348	31.919053
597.538635	26086.188690	31.924071
598.524965	26117.116225	31.929088
599.013611	26151.604104	31.934106
599.429098	26179.429508	31.939124
600.031488	26218.481738	31.944141
600.491433	26255.312719	31.949159
601.255139	26292.064593	31.954176
601.708234	26319.675737	31.959194
602.491737	26365.696251	31.964212
603.299382	26399.862829	31.969229
603.725778	26438.886166	31.974247
604.209148	26472.598042	31.979264
604.907525	26513.190567	31.984282
605.098971	26545.589447	31.989300
606.086556	26579.228854	31.994317
606.557787	26623.516566	31.999335
607.384738	26654.248681	32.004352
607.974444	26692.791876	32.009370
608.645209	26728.212891	32.014388
609.332925	26769.376422	32.019405
609.992200	26809.786060	32.024423
610.380574	26849.675699	32.029440
610.941924	26883.881670	32.034458
611.618568	26918.707991	32.039476
612.639829	26958.561931	32.044493
613.335406	26997.746438	32.049511
613.535465	27024.507007	32.054528
614.253984	27066.241467	32.059546
614.631469	27101.784912	32.064564
615.327491	27134.522853	32.069581
616.058378	27175.749973	32.074599
616.674563	27222.032492	32.079616
617.667056	27259.906927	32.084634
617.979400	27299.746155	32.089652
618.639822	27333.210520	32.094669
619.417290	27370.657447	32.099687
620.241229	27406.883638	32.104704
620.689196	27436.273154	32.109722
621.131984	27466.807529	32.114740
622.352153	27509.880123	32.119757
622.229875	27542.329726	32.124775
623.035273	27583.090929	32.129792
623.446189	27607.095105	32.134810
623.807193	27643.280450	32.139828
624.912547	27695.725796	32.144845
625.810944	27741.017219	32.149863
625.913283	27765.670362	32.154880
627.216084	27796.974386	32.159898
627.385562	27848.498518	32.164916
628.242164	27873.684686	32.169933
628.787675	27911.390157	32.174951
629.473114	27948.043524	32.179968
630.460844	27975.219239	32.184986
630.642090	28013.715140	32.190004
631.643570	28050.692114	32.195021
631.996271	28092.802007	32.200039
632.736875	28129.510267	32.205056
633.306542	28160.291280	32.210074
633.330954	28197.225598	32.215092
634.421735	28230.927435	32.220109
634.798803	28262.244422	32.225127
635.407363	28292.400113	32.230144
635.970806	28333.289202	32.235162
636.434406	28359.991291	32.240180
637.074016	28396.633679	32.245197
637.786477	28433.308970	32.250215
638.423922	28477.720067	32.255232
639.237643	28509.904525	32.260250
639.530288	28549.357391	32.265268
640.269109	28583.905034	32.270285
641.096688	28626.535813	32.275303
641.531383	28670.998046	32.280320
642.429991	28709.168002	32.285338
642.864095	28746.032828	32.290356
643.928254	28783.582835	32.295373
644.456381	28818.859169	32.300391
645.003646	28859.581181	32.305408
645.499674	28892.195249	32.310426
645.844325	28934.813809	32.315444
646.676196	28968.481564	32.320461
647.552093	29021.048428	32.325479
648.148371	29064.278908	32.330496
648.834381	29102.931683	32.335514
649.167408	29144.806625	32.340532
650.119744	29177.823760	32.345549
650.902734	29229.350102	32.350567
651.340947	29266.822038	32.355584
652.464804	29301.879487	32.360602
652.857134	29341.109672	32.365620
653.717242	29382.662354	32.370637
654.333243	29425.277364	32.375655
655.165820	29458.680330	32.380672
655.778862	29493.508372	32.385690
656.344991	29533.862145	32.390708
657.459571	29564.597862	32.395725
657.864235	29602.973264	32.400743
658.068249	29642.928840	32.405760
659.103746	29687.394003	32.410778
659.564820	29730.406856	32.415796
660.530037	29768.846489	32.420813
661.608462	29805.498532	32.425831
661.888891	29834.734421	32.430848
662.623809	29865.049636	32.435866
662.701828	29905.164519	32.440884
664.288355	29940.940758	32.445901
664.904617	29981.818543	32.450919
664.922562	30012.410610	32.455936
665.886803	30049.213716	32.460954
666.329282	30093.658847	32.465972
666.705071	30129.163571	32.470989
667.599055	30164.606167	32.476007
668.112311	30215.399704	32.481024
668.979710	30263.514553	32.486042
669.530101	30300.490383	32.491060
670.421009	30338.468619	32.496077
670.882386	30379.004809	32.501095
671.594190	30433.111790	32.506112
672.491913	30461.980077	32.511130
673.141632	30505.875287	32.516148
674.034856	30535.825343	32.521165
674.553163	30582.769253	32.526183
675.428776	30614.087608	32.531200
676.284859	30647.394005	32.536218
676.689117	30702.738288	32.541236
677.295386	30722.745644	32.546253
677.996029	30755.924843	32.551271
678.135057	30803.933768	32.556288
679.231419	30838.138424	32.561306
679.390159	30873.520381	32.566324
680.217407	30909.442503	32.571341
681.222675	30937.871073	32.576359
681.602370	30988.775929	32.581376
682.350274	31016.638043	32.586394
682.774575	31059.362312	32.591412
683.478914	31090.550175	32.596429
684.243556	31132.753499	32.601447
684.781939	31173.683770	32.606464
685.373344	31214.681677	32.611482
686.054270	31257.347201	32.616500
686.837944	31299.661674	32.621517
687.423643	31345.224962	32.626535
687.667838	31396.847422	32.631552
688.605780	31437.393235	32.636570
689.095128	31489.818318	32.641588
690.554861	31534.391714	32.646605
691.155591	31574.996927	32.651623
691.602593	31622.308376	32.656640
692.286950	31668.659785	32.661658
693.185703	31719.459859	32.666676
693.439620	31765.588091	32.671693
694.516018	31812.674972	32.676711
695.015133	31857.386856	32.681728
696.284469	31904.911545	32.686746
696.736595	31946.501674	32.691764
697.544117	31984.085071	32.696781
698.558667	32026.933839	32.701799
698.744450	32082.436129	32.706816
699.960095	32114.127073	32.711834
700.371545	32158.625744	32.716852
701.149195	32202.390717	32.721869
702.233368	32248.807246	32.726887
702.796018	32276.896047	32.731904
703.947447	32317.663025	32.736922
704.575683	32356.937847	32.741940
705.345046	32392.871604	32.746957
705.869935	32427.041942	32.751975
706.518741	32459.062417	32.756992
707.087500	32497.897957	32.762010
707.951966	32532.091153	32.767028
708.788175	32569.209608	32.772045
709.704182	32616.317105	32.777063
710.492437	32647.095876	32.782080
710.778186	32673.559553	32.787098
711.462093	32717.738580	32.792116
712.525496	32756.288511	32.797133
713.083747	32789.164512	32.802151
713.334767	32824.851438	32.807168
714.696840	32864.233570	32.812186
714.866885	32902.152373	32.817204
715.576251	32939.177552	32.822221
716.455836	32988.232490	32.827239
716.851373	33036.332832	32.832256
717.624354	33063.201186	32.837274
718.177668	33111.985078	32.842292
718.903597	33146.567664	32.847309
719.635373	33192.402937	32.852327
720.126592	33245.325272	32.857344
721.235467	33292.511569	32.862362
721.873832	33336.515690	32.867380
722.516365	33389.338825	32.872397
723.643032	33431.414250	32.877415
724.051479	33476.023675	32.882432
724.583465	33513.899548	32.887450
725.386180	33561.551669	32.892468
726.105424	33612.991409	32.897485
726.711064	33650.223760	32.902503
727.606994	33696.495961	32.907520
728.467741	33740.674743	32.912538
729.226099	33773.514631	32.917556
729.597575	33811.043155	32.922573
730.523215	33829.441857	32.927591
731.045691	33876.727623	32.932608
731.861722	33909.166701	32.937626
732.633857	33957.791844	32.942644
733.706794	33993.807262	32.947661
734.481436	34031.216142	32.952679
735.117380	34067.932369	32.957696
735.546220	34106.539904	32.962714
736.326031	34146.919752	32.967732
736.495195	34187.287822	32.972749
737.903763	34222.568243	32.977767
738.462313	34281.798851	32.982784
739.420930	34324.597865	32.987802
740.353837	34364.366158	32.992820
741.083928	34408.807064	32.997837
741.726298	34443.436486	33.002855
742.415264	34490.160138	33.007872
742.992825	34526.190819	33.012890
744.215210	34570.270455	33.017908
744.621901	34615.053280	33.022925
745.853236	34654.332803	33.027943
746.431583	34695.889655	33.032960
747.866366	34717.914493	33.037978
748.179126	34766.379502	33.042996
748.588221	34811.946382	33.048013
749.862180	34839.149537	33.053031
750.521224	34876.944740	33.058048
751.183023	34917.167510	33.063066
751.854174	34963.566217	33.068084
752.317097	35001.632620	33.073101
753.123381	35033.379456	33.078119
753.760850	35084.968376	33.083136
754.884033	35120.016794	33.088154
755.617370	35171.375937	33.093172
755.964804	35213.779288	33.098189
756.806505	35247.417747	33.103207
757.541516	35301.660156	33.108224
758.119404	35338.204323	33.113242
758.959990	35393.391510	33.118260
759.590115	35436.977677	33.123277
760.426885	35474.290869	33.128295
760.941984	35527.493401	33.133312
762.007147	35572.946535	33.138330
762.634937	35621.010081	33.143348
763.078390	35683.917302	33.148365
764.093620	35732.116440	33.153383
764.892573	35787.203681	33.158400
765.820993	35824.401969	33.163418
766.951011	35880.449290	33.168436
767.442599	35929.673007	33.173453
768.531082	35976.596623	33.178471
769.110143	36016.651068	33.183488
770.085803	36070.712329	33.188506
770.713536	36108.223771	33.193524
771.352200	36144.677610	33.198541
772.190919	36197.925989	33.203559
773.078182	36244.382181	33.208576
773.793276	36283.258694	33.213594
774.368893	36334.740198	33.218612
775.311423	36382.199740	33.223629
776.281551	36417.792776	33.228647
776.960684	36465.350659	33.233664
777.653470	36508.126165	33.238682
778.407109	36552.087317	33.243700
778.880076	36588.858731	33.248717
779.761798	36628.873257	33.253735
780.325469	36662.032669	33.258752
781.171116	36710.943495	33.263770
781.958725	36756.265574	33.268788
782.545802	36803.105126	33.273805
783.653936	36842.856960	33.278823
784.105320	36886.790253	33.283840
784.900370	36923.258875	33.288858
785.916393	36975.469700	33.293876
786.326404	37017.443180	33.298893
787.422996	37070.887323	33.303911
787.850991	37118.934950	33.308928
788.521632	37165.117223	33.313946
789.544731	37211.149553	33.318964
790.481105	37268.071864	33.323981
791.164028	37317.376320	33.328999
791.837728	37365.183672	33.334016
792.684548	37418.073391	33.339034
793.892834	37468.472093	33.344052
794.236848	37518.291696	33.349069
795.245936	37555.733319	33.354087
796.186539	37620.983980	33.359104
797.276904	37655.681283	33.364122
798.491643	37705.244824	33.369140
798.959610	37754.476445	33.374157
800.199848	37787.809895	33.379175
800.288651	37836.525632	33.384192
801.198014	37894.168403	33.389210
802.462621	37926.195588	33.394228
803.068190	37973.932760	33.399245
804.044127	38031.654007	33.404263
804.991510	38071.850662	33.409280
805.530431	38112.408568	33.414298
806.544487	38159.766003	33.419316
807.430966	38207.042340	33.424333
808.164374	38239.153175	33.429351
808.618611	38294.016292	33.434368
809.564717	38347.107760	33.439386
810.489573	38384.152977	33.444404
811.020865	38429.702123	33.449421
812.151959	38475.562164	33.454439
812.942490	38530.101298	33.459456
813.633811	38570.067059	33.464474
814.463534	38620.236852	33.469492
815.013032	38660.503237	33.474509
816.193290	38706.109442	33.479527
816.728013	38764.780761	33.484544
817.378673	38813.164091	33.489562
818.320384	38863.550898	33.494580
819.147960	38919.773698	33.499597
819.914194	38968.265756	33.504615
820.577507	39021.611858	33.509632
821.514980	39078.791751	33.514650
822.490219	39123.943998	33.519668
823.152966	39178.226525	33.524685
824.421559	39216.730783	33.529703
824.824521	39274.690533	33.534720
825.896578	39325.095950	33.539738
826.909977	39363.260988	33.544756
827.519439	39421.391165	33.549773
828.609685	39470.415426	33.554791
829.443039	39513.029453	33.559808
830.054040	39562.306042	33.564826
831.214594	39607.607357	33.569844
831.765879	39655.552796	33.574861
832.692565	39694.301169	33.579879
833.333413	39746.975893	33.584896
834.120669	39787.864860	33.589914
834.874763	39828.151975	33.594932
835.366543	39869.416220	33.599949
836.381584	39917.270646	33.604967
837.018261	39959.005662	33.609984
837.778924	40011.706536	33.615002
839.080288	40045.362776	33.620020
839.510632	40096.249928	33.625037
840.542530	40144.544914	33.630055
841.361790	40193.784001	33.635072
842.006045	40247.427022	33.640090
842.932366	40301.380168	33.645108
843.424047	40353.611720	33.650125
844.379969	40403.942967	33.655143
845.391488	40453.146212	33.660160
846.127217	40515.022539	33.665178
847.043007	40554.678541	33.670196
848.394396	40616.490374	33.675213
849.227537	40655.413221	33.680231
850.085337	40705.526527	33.685248
850.866748	40756.100945	33.690266
851.865134	40793.663705	33.695284
852.711177	40854.442238	33.700301
853.584629	40908.468412	33.705319
854.428518	40944.822349	33.710336
855.567666	40995.689154	33.715354
856.236680	41039.388102	33.720372
857.173414	41088.319889	33.725389
858.073156	41133.146613	33.730407
858.640647	41179.948125	33.735424
859.323687	41233.808858	33.740442
860.530661	41296.695115	33.745460
861.100575	41350.681367	33.750477
861.805725	41412.691518	33.755495
862.779628	41465.438412	33.760512
863.472741	41521.069177	33.765530
864.411753	41570.235698	33.770548
865.674754	41632.703043	33.775565
866.228696	41674.036864	33.780583
867.350385	41725.635444	33.785600
868.056589	41780.006196	33.790618
868.955727	41835.586525	33.795636
869.783425	41901.025863	33.800653
870.938095	41954.934688	33.805671
871.801835	42011.817589	33.810688
872.343042	42063.210592	33.815706
873.769697	42109.171175	33.820724
874.622292	42172.064836	33.825741
875.418797	42215.398300	33.830759
876.466948	42267.844553	33.835776
876.581222	42327.717125	33.840794
877.488128	42377.712720	33.845812
878.555580	42440.073835	33.850829
879.671547	42488.240664	33.855847
880.685781	42548.485237	33.860864
881.876583	42607.513230	33.865882
882.627708	42655.408655	33.870900
883.641115	42707.469247	33.875917
884.323252	42754.306762	33.880935
885.308317	42793.974950	33.885952
886.178958	42856.500887	33.890970
887.040698	42895.638290	33.895988
887.687587	42953.771993	33.901005
888.725887	43005.026104	33.906023
889.641097	43055.698724	33.911040
890.382783	43099.358766	33.916058
891.106838	43150.820549	33.921076
892.086243	43203.165942	33.926093
893.208295	43251.339813	33.931111
894.120764	43281.785504	33.936128
894.599149	43323.330332	33.941146
895.787456	43366.920970	33.946164
896.917719	43415.454450	33.951181
897.367507	43463.563267	33.956199
898.243329	43494.381853	33.961216
898.865301	43552.211093	33.966234
900.319215	43597.702451	33.971252
900.921409	43643.599253	33.976269
901.377487	43694.598239	33.981287
902.699096	43742.065126	33.986304
903.422250	43799.714711	33.991322
904.363364	43844.217891	33.996340
905.247167	43896.478688	34.001357
905.892578	43948.251931	34.006375
907.115408	44001.054474	34.011392
907.974645	44063.414820	34.016410
909.480165	44106.697907	34.021428
910.397765	44166.525566	34.026445
911.256319	44213.971089	34.031463
912.078446	44265.173411	34.036480
913.011391	44317.085929	34.041498
914.090142	44364.117766	34.046516
914.816738	44410.679826	34.051533
915.613890	44467.225245	34.056551
916.962718	44513.677441	34.061568
917.274687	44570.109325	34.066586
918.537481	44609.231239	34.071604
919.619425	44666.681405	34.076621
920.500846	44721.272324	34.081639
921.444694	44763.910871	34.086656
922.295228	44825.351179	34.091674
922.990332	44883.450756	34.096692
923.978031	44938.854224	34.101709
924.751771	44983.923574	34.106727
925.941430	45041.927150	34.111744
926.695153	45107.729132	34.116762
927.979163	45151.763743	34.121780
928.807806	45205.105294	34.126797
929.710940	45268.297134	34.131815
930.806300	45312.779101	34.136832
931.534476	45370.476243	34.141850
932.649299	45418.978563	34.146868
933.506427	45480.210886	34.151885
934.343991	45538.511262	34.156903
935.378749	45590.062881	34.161920
936.157386	45647.752836	34.166938
936.943346	45707.118147	34.171956
938.308641	45761.287920	34.176973
938.821887	45821.341473	34.181991
939.898736	45870.325159	34.187008
940.504466	45935.589738	34.192026
941.569088	45988.440738	34.197044
942.764494	46051.044991	34.202061
943.747835	46119.236831	34.207079
944.859763	46169.809825	34.212096
945.356702	46238.900566	34.217114
946.510066	46284.324283	34.222132
947.400543	46335.223320	34.227149
947.919040	46399.851322	34.232167
949.366173	46470.812009	34.237184
950.216121	46523.375250	34.242202
951.475196	46576.380643	34.247220
951.780183	46636.595501	34.252237
952.797183	46700.671852	34.257255
954.133026	46755.588794	34.262272
955.038013	46810.598636	34.267290
955.977604	46859.087222	34.272308
956.689120	46903.936101	34.277325
957.698369	46956.949876	34.282343
958.702744	47004.694790	34.287360
959.799497	47059.175441	34.292378
960.503993	47109.934539	34.297396
961.666520	47159.110057	34.302413
961.912287	47215.868934	34.307431
963.022105	47262.718531	34.312448
964.202894	47329.497656	34.317466
964.741491	47390.513017	34.322484
966.327439	47445.999808	34.327501
967.117113	47504.198895	34.332519
968.229780	47557.862155	34.337536
969.299721	47613.695860	34.342554
970.355620	47668.000909	34.347572
971.283922	47730.632666	34.352589
971.847891	47786.457448	34.357607
973.185111	47834.594851	34.362624
974.383994	47891.503529	34.367642
975.496512	47956.283373	34.372660
976.733101	48003.930773	34.377677
977.632851	48057.609575	34.382695
978.420218	48110.641812	34.387712
979.435033	48158.336914	34.392730
980.651190	48213.408996	34.397748
981.984469	48269.120837	34.402765
982.416340	48329.003991	34.407783
983.482792	48369.219744	34.412800
984.259001	48433.882787	34.417818
985.517886	48480.420538	34.422836
986.374585	48535.695195	34.427853
987.486526	48592.321888	34.432871
988.453975	48650.685877	34.437888
989.486865	48702.270201	34.442906
990.439273	48755.955058	34.447924
991.465751	48817.378688	34.452941
991.918640	48882.935082	34.457959
993.240178	48929.653745	34.462976
994.294158	48991.497430	34.467994
995.347392	49053.556511	34.473012
996.335214	49100.024087	34.478029
997.019708	49174.314011	34.483047
998.358504	49223.517018	34.488064
999.717542	49300.529838	34.493082
1000.331269	49346.328897	34.498100
1001.317081	49405.027263	34.503117
1002.538426	49462.885384	34.508135
1003.809165	49513.010746	34.513152
1004.651563	49576.439236	34.518170
1005.416173	49629.693682	34.523188
1006.855633	49691.542175	34.528205
1007.507567	49748.148852	34.533223
1008.360778	49808.880995	34.538240
1009.378061	49864.842346	34.543258
1010.544784	49919.964248	34.548276
1011.707696	49975.852452	34.553293
1012.550204	50043.856674	34.558311
1013.827379	50086.396129	34.563328
1014.766147	50144.844343	34.568346
1015.591128	50203.696476	34.573364
1016.692771	50259.360860	34.578381
1017.448986	50317.477449	34.583399
1018.832978	50377.925523	34.588416
1020.063556	50438.157344	34.593434
1020.688042	50484.045568	34.598452
1022.089405	50532.988504	34.603469
1022.697558	50596.095832	34.608487
1024.330851	50634.297019	34.613504
1024.967818	50685.315074	34.618522
1025.315081	50730.804286	34.623540
1026.941938	50779.345461	34.628557
1027.901723	50832.394969	34.633575
1028.537443	50878.630220	34.638592
1029.506454	50936.006394	34.643610
1030.375594	50991.278692	34.648628
1031.234597	51035.910121	34.653645
1032.002293	51105.112398	34.658663
1032.975900	51163.209735	34.663680
1034.066634	51225.003058	34.668698
1034.971821	51289.824787	34.673716
1036.441996	51357.690317	34.678733
1037.210571	51424.318147	34.683751
1038.359986	51481.325745	34.688768
1039.446210	51548.334466	34.693786
1040.303635	51618.966893	34.698804
1041.728851	51684.916861	34.703821
1042.945502	51759.125467	34.708839
1043.622356	51812.961842	34.713856
1044.604803	51874.546059	34.718874
1046.022492	51941.440742	34.723892
1047.227371	52003.167647	34.728909
1047.956782	52074.334037	34.733927
1049.390241	52127.350316	34.738944
1050.459663	52202.317394	34.743962
1051.534515	52262.141737	34.748980
1052.900798	52322.420493	34.753997
1054.007059	52383.455147	34.759015
1055.196853	52437.225313	34.764032
1056.454616	52493.813460	34.769050
1057.459025	52553.700203	34.774068
1058.748831	52614.529549	34.779085
1059.508669	52668.747232	34.784103
1060.898253	52714.754210	34.789120
1061.907813	52766.965080	34.794138
1063.125723	52824.737243	34.799156
1064.421403	52879.909287	34.804173
1064.997602	52938.902229	34.809191
1066.231644	52986.357863	34.814208
1067.013652	53039.250411	34.819226
1067.932106	53095.469174	34.824244
1069.082784	53153.328611	34.829261
1070.700636	53217.613833	34.834279
1071.397012	53282.435835	34.839296
1072.597819	53322.126635	34.844314
1073.463875	53385.682077	34.849332
1074.637292	53435.502123	34.854349
1075.816556	53488.251226	34.859367
1077.015232	53548.154398	34.864384
1077.935435	53604.836055	34.869402
1078.640397	53660.703589	34.874420
1080.067475	53719.204580	34.879437
1081.128729	53782.502725	34.884455
1082.543285	53837.304043	34.889472
1083.270086	53889.049110	34.894490
1083.893889	53951.758075	34.899508
1085.834222	54012.729679	34.904525
1086.646614	54068.170032	34.909543
1087.529220	54127.105333	34.914560
1088.469154	54185.671098	34.919578
1089.500634	54245.886995	34.924596
1090.555206	54303.321341	34.929613
1091.441171	54369.325347	34.934631
1092.965476	54429.040563	34.939648
1094.045477	54493.223641	34.944666
1094.961527	54536.897267	34.949684
1096.007186	54601.048046	34.954701
1097.187210	54654.685611	34.959719
1098.033931	54707.299663	34.964736
1098.831885	54762.073105	34.969754
1100.102651	54811.273307	34.974772
1100.833613	54871.588477	34.979789
1101.917957	54925.887132	34.984807
1102.852848	54989.524722	34.989824
1104.417421	55050.089542	34.994842
1104.955278	55113.833925	34.999860
1106.263444	55178.970381	35.004877
1107.260366	55239.751127	35.009895
1108.378773	55310.208256	35.014912
1109.867859	55375.753595	35.019930
1110.732525	55438.561694	35.024948
1111.906431	55504.188374	35.029965
1112.909051	55580.701865	35.034983
1113.862990	55645.882404	35.040000
1114.867873	55709.295796	35.045018
1116.056232	55783.021591	35.050036
1117.318594	55854.413419	35.055053
1118.554442	55930.726977	35.060071
1119.840536	56007.108858	35.065088
1121.287019	56068.663057	35.070106
1122.296048	56137.184196	35.075124
1123.715717	56204.280567	35.080141
1124.729880	56261.270318	35.085159
1126.060620	56331.804821	35.090176
1127.664085	56386.291353	35.095194
1128.615753	56455.733732	35.100212
1130.183258	56503.118926	35.105229
1131.295198	56555.410755	35.110247
1132.146991	56620.527678	35.115264
1133.724349	56667.171182	35.120282
1134.593174	56730.475687	35.125300
1135.574009	56792.357811	35.130317
1136.612873	56852.927257	35.135335
1137.810394	56917.193421	35.140352
1139.228587	56971.140694	35.145370
1140.591080	57037.242059	35.150388
1142.086051	57080.342401	35.155405
1143.318363	57144.711321	35.160423
1143.760728	57198.122020	35.165440
1145.209724	57255.868837	35.170458
1145.998087	57312.174938	35.175476
1147.207389	57369.326653	35.180493
1148.386623	57426.464223	35.185511
1149.422715	57486.700266	35.190528
1150.578987	57542.088556	35.195546
1151.766924	57614.952986	35.200564
1152.804020	57666.771621	35.205581
1154.023285	57722.992238	35.210599
1155.030286	57783.024717	35.215616
1156.728393	57841.670660	35.220634
1157.209908	57910.102241	35.225652
1158.508690	57976.671869	35.230669
1159.822604	58031.903695	35.235687
1161.049726	58087.541648	35.240704
1162.052661	58152.771979	35.245722
1162.926786	58216.478314	35.250740
1164.318156	58275.875884	35.255757
1165.795221	58339.253968	35.260775
1166.809283	58396.464006	35.265792
1168.055350	58462.005223	35.270810
1169.052056	58533.320037	35.275828
1170.580060	58587.728454	35.280845
1171.352587	58640.672923	35.285863
1172.303817	58705.412821	35.290880
1173.700375	58758.867476	35.295898
1174.548245	58804.274852	35.300916
1175.728938	58853.674712	35.305933
1176.667832	58916.910704	35.310951
1177.482783	58979.185199	35.315968
1178.936713	59030.150326	35.320986
1180.050685	59090.979483	35.326004
1180.730731	59150.591835	35.331021
1182.345839	59213.646785	35.336039
1183.361074	59281.150531	35.341056
1184.272037	59338.859982	35.346074
1185.257976	59415.116127	35.351092
1186.841609	59478.872947	35.356109
1188.042469	59551.272803	35.361127
1188.767260	59631.918950	35.366144
1190.421169	59694.019630	35.371162
1191.789977	59758.962812	35.376180
1192.695147	59828.339897	35.381197
1194.351056	59898.112357	35.386215
1195.450967	59970.048204	35.391232
1196.861268	60045.784150	35.396250
1198.430964	60105.797594	35.401268
1199.745437	60163.464820	35.406285
1200.805537	60233.413801	35.411303
1201.817185	60297.971248	35.416320
1203.243987	60357.134169	35.421338
1204.530899	60426.143031	35.426356
1205.677084	60491.623073	35.431373
1207.097955	60552.388847	35.436391
1208.267767	60618.789691	35.441408
1209.952344	60683.078232	35.446426
1211.089771	60746.363853	35.451444
1212.564403	60805.868518	35.456461
1213.579539	60865.723780	35.461479
1214.486639	60928.007816	35.466496
1215.757861	60982.550415	35.471514
1217.195797	61042.434869	35.476532
1218.213729	61099.327828	35.481549
1219.688374	61162.783283	35.486567
1220.598224	61235.531197	35.491584
1222.327985	61288.337894	35.496602
1223.305195	61358.372693	35.501620
1224.444443	61426.344037	35.506637
1226.001757	61475.456040	35.511655
1226.822562	61538.483095	35.516672
1228.442734	61602.929725	35.521690
1229.797892	61665.620248	35.526708
1230.898719	61721.944618	35.531725
1232.016306	61787.324981	35.536743
1233.050325	61844.445032	35.541760
1234.814118	61893.468576	35.546778
1235.873630	61961.112047	35.551796
1237.060051	62019.582305	35.556813
1238.340066	62069.302297	35.561831
1239.665297	62136.524837	35.566848
1240.889993	62195.451630	35.571866
1241.881028	62254.364499	35.576884
1243.092093	62312.635354	35.581901
1244.562817	62373.562420	35.586919
1245.461875	62445.347051	35.591936
1246.885262	62494.355447	35.596954
1248.138178	62557.988477	35.601972
1249.478449	62619.341715	35.606989
1250.729259	62684.209826	35.612007
1251.241066	62753.606102	35.617024
1252.810126	62804.592725	35.622042
1254.285372	62882.853093	35.627060
1255.357796	62945.097349	35.632077
1256.583441	62992.434789	35.637095
1257.356186	63046.072433	35.642112
1258.633358	63096.586249	35.647130
1259.718491	63148.940762	35.652148
1261.050074	63205.472947	35.657165
1262.113358	63274.031011	35.662183
1263.466577	63338.492306	35.667200
1264.780605	63405.245248	35.672218
1266.054721	63461.970600	35.677236
1267.185703	63537.950928	35.682253
1268.643943	63596.692557	35.687271
1269.763313	63661.526820	35.692288
1271.103196	63726.966130	35.697306
1272.066801	63799.339648	35.702324
1273.212067	63874.343838	35.707341
1274.985774	63935.657797	35.712359
1276.023993	64009.780187	35.717376
1277.353776	64085.617108	35.722394
1278.430509	64140.361718	35.727412
1279.841097	64221.472603	35.732429
1281.158516	64290.265900	35.737447
1282.656361	64377.947684	35.742464
1283.931920	64432.022393	35.747482
1285.463616	64520.421094	35.752500
1286.878949	64588.275574	35.757517
1288.283773	64652.656213	35.762535
1289.610024	64728.843834	35.767552
1290.797156	64798.165394	35.772570
1292.514163	64865.258002	35.777588
1293.659751	64922.228371	35.782605
1295.254629	64995.373867	35.787623
1296.745131	65060.976686	35.792640
1297.927825	65111.306777	35.797658
1299.754872	65170.469197	35.802676
1300.933124	65235.741489	35.807693
1302.383151	65296.792900	35.812711
1303.620496	65349.280139	35.817728
1304.711466	65411.970807	35.822746
1306.392217	65467.953293	35.827764
1307.750073	65542.682275	35.832781
1308.908734	65599.924372	35.837799
1310.178021	65656.997334	35.842816
1311.657609	65704.654705	35.847834
1313.019770	65765.689352	35.852852
1313.832690	65821.580549	35.857869
1315.648696	65878.606418	35.862887
1316.797399	65942.954477	35.867904
1317.943687	66006.986516	35.872922
1319.152892	66073.370430	35.877940
1320.628022	66129.221959	35.882957
1321.986385	66184.211841	35.887975
1323.215710	66256.861067	35.892992
1324.337233	66310.280144	35.898010
1325.460634	66374.582610	35.903028
1326.990888	66448.888410	35.908045
1328.232215	66503.618726	35.913063
1329.043036	66571.579504	35.918080
1330.722236	66641.835790	35.923098
1332.511921	66710.523777	35.928116
1333.505160	66783.610346	35.933133
1334.824263	66834.283410	35.938151
1336.295213	66906.903003	35.943168
1337.412650	66978.970318	35.948186
1338.893823	67033.765536	35.953204
1340.204284	67109.108050	35.958221
1341.566158	67174.128660	35.963239
1342.824245	67249.296172	35.968256
1344.348436	67306.750829	35.973274
1345.363433	67364.836171	35.978292
1346.121396	67422.942885	35.983309
1347.393101	67468.780958	35.988327
1348.952150	67541.768467	35.993344
1350.043373	67596.720911	35.998362
1351.654294	67667.959459	36.003380
1352.659790	67729.206615	36.008397
1354.031920	67794.106898	36.013415
1355.252567	67859.999809	36.018432
1356.457360	67924.920285	36.023450
1357.918140	67993.688544	36.028468
1359.771725	68071.019355	36.033485
1360.938534	68141.841196	36.038503
1362.040229	68220.296906	36.043520
1363.707612	68279.478912	36.048538
1365.578238	68355.104657	36.053556
1366.319444	68427.526209	36.058573
1367.626303	68502.271861	36.063591
1369.165167	68567.337958	36.068608
1370.770763	68645.241196	36.073626
1372.016507	68712.348091	36.078644
1373.754616	68792.447204	36.083661
1375.108627	68858.176166	36.088679
1376.448436	68929.093401	36.093696
1377.937415	68991.243009	36.098714
1379.928159	69055.796369	36.103732
1380.990245	69126.346039	36.108749
1383.277018	69192.221120	36.113767
1384.677988	69244.621120	36.118784
1385.923445	69310.330235	36.123802
1387.452986	69356.466924	36.128820
1388.388241	69430.779534	36.133837
1390.114300	69480.627952	36.138855
1391.428282	69534.561862	36.143872
1392.614512	69604.789465	36.148890
1394.362688	69673.295601	36.153908
1395.354263	69745.187748	36.158925
1396.395678	69795.720169	36.163943
1398.293966	69877.747889	36.168960
1399.447515	69943.283030	36.173978
1401.145640	70007.023393	36.178996
1402.449122	70078.665009	36.184013
1403.834419	70136.869614	36.189031
1405.006188	70203.035785	36.194048
1406.612057	70276.251679	36.199066
1408.093839	70344.649313	36.204084
1409.089857	70411.666726	36.209101
1410.744969	70492.752942	36.214119
1411.893783	70553.275141	36.219136
1413.594354	70626.540520	36.224154
1415.251164	70698.711118	36.229172
1416.282198	70768.066955	36.234189
1417.536702	70837.172694	36.239207
1419.071571	70903.701750	36.244224
1420.306654	70980.701143	36.249242
1421.769771	71057.373774	36.254260
1423.518896	71125.364326	36.259277
1425.018317	71197.041672	36.264295
1426.455543	71258.862858	36.269312
1427.753675	71329.064929	36.274330
1428.942891	71397.637769	36.279348
1430.459669	71472.986045	36.284365
1431.801648	71533.442283	36.289383
1433.305672	71617.126674	36.294400
1434.701147	71680.804517	36.299418
1436.202747	71755.180753	36.304436
1437.378202	71827.708448	36.309453
1439.095883	71893.882108	36.314471
1440.733220	71952.494598	36.319488
1441.590977	72021.792216	36.324506
1442.845201	72066.393629	36.329524
1444.305671	72134.925936	36.334541
1445.868126	72197.489662	36.339559
1447.306814	72262.289382	36.344576
1448.520506	72327.339793	36.349594
1449.867537	72396.017192	36.354612
1451.526193	72459.947036	36.359629
1452.780301	72534.174228	36.364647
1454.507077	72608.682285	36.369664
1455.774579	72681.121927	36.374682
1456.955482	72752.030097	36.379700
1458.236749	72828.825020	36.384717
1460.043357	72906.893185	36.389735
1461.468006	72974.154028	36.394752
1462.845806	73052.923037	36.399770
1464.613708	73135.317018	36.404788
1466.271168	73210.926895	36.409805
1467.755178	73282.232351	36.414823
1469.134992	73356.201517	36.419840
1470.671197	73434.642880	36.424858
1472.197281	73505.803024	36.429876
1474.053863	73587.918542	36.434893
1475.334792	73663.892634	36.439911
1476.884676	73743.485394	36.444928
1478.483415	73816.648934	36.449946
1480.209302	73888.652803	36.454964
1481.747141	73956.683732	36.459981
1483.172883	74028.962955	36.464999
1484.536990	74106.584588	36.470016
1485.934903	74176.879938	36.475034
1487.574577	74244.085007	36.480052
1488.965881	74324.628978	36.485069
1490.898516	74389.267919	36.490087
1492.419184	74466.410097	36.495104
1493.608410	74545.225704	36.500122
1495.353684	74614.885173	36.505140
1496.883745	74685.794512	36.510157
1498.637602	74751.690983	36.515175
1499.889625	74822.948206	36.520192
1501.240231	74919.194468	36.525210
1503.071804	74973.957861	36.530228
1504.305644	75054.085333	36.535245
1505.792991	75127.903243	36.540263
1507.384455	75201.451721	36.545280
1508.416631	75285.006187	36.550298
1510.336746	75364.305151	36.555316
1511.905357	75441.873310	36.560333
1513.205396	75511.554128	36.565351
1515.007930	75587.591377	36.570368
1516.394059	75665.100071	36.575386
1518.202038	75729.445078	36.580404
1519.431769	75807.650022	36.585421
1520.910112	75882.915476	36.590439
1522.945879	75958.917269	36.595456
1523.892439	76034.329715	36.600474
1525.774794	76104.630293	36.605492
1527.134512	76175.696896	36.610509
1528.596733	76257.920324	36.615527
1530.163874	76331.830381	36.620544
1531.102191	76414.756990	36.625562
1533.297314	76480.550629	36.630580
1534.618086	76571.917783	36.635597
1536.111286	76641.381267	36.640615
1538.183040	76713.325910	36.645632
1539.525820	76793.466826	36.650650
1540.915644	76860.489519	36.655668
1542.472391	76924.813356	36.660685
1543.804677	76988.969793	36.665703
1545.305099	77038.101380	36.670720
1546.636358	77107.794089	36.675738
1547.884508	77162.868599	36.680756
1549.269070	77238.811226	36.685773
1550.619793	77305.372423	36.690791
1552.040385	77377.762778	36.695808
1553.523443	77460.455297	36.700826
1555.199617	77539.760812	36.705844
1556.715823	77614.771783	36.710861
1558.143431	77690.442899	36.715879
1559.893864	77772.030393	36.720896
1561.290670	77860.260934	36.725914
1562.899732	77936.981128	36.730932
1564.800761	78019.343887	36.735949
1566.505334	78113.101107	36.740967
1568.138070	78185.194362	36.745984
1569.849697	78268.347614	36.751002
1571.392649	78338.327038	36.756020
1573.250132	78420.089734	36.761037
1574.694378	78501.486623	36.766055
1576.350034	78576.111014	36.771072
1577.784344	78667.087346	36.776090
1579.494973	78739.917312	36.781108
1581.271743	78820.464979	36.786125
1582.836604	78893.318165	36.791143
1584.681691	78980.709355	36.796160
1586.165717	79066.269689	36.801178
1587.954480	79143.193164	36.806196
1589.401374	79223.388238	36.811213
1591.019722	79299.223964	36.816231
1592.722914	79375.097296	36.821248
1594.280302	79459.633856	36.826266
1596.031563	79533.321045	36.831284
1597.921622	79611.560211	36.836301
1599.236069	79699.226759	36.841319
1600.908381	79772.825589	36.846336
1602.218002	79854.678285	36.851354
1603.980615	79934.661308	36.856372
1605.512911	80007.965948	36.861389
1606.909248	80090.033810	36.866407
1608.881733	80174.634277	36.871424
1610.214853	80264.732181	36.876442
1612.354652	80342.566914	36.881460
1614.064717	80416.693654	36.886477
1615.208915	80507.797452	36.891495
1617.131226	80586.946517	36.896512
1618.844569	80667.091390	36.901530
1620.218904	80749.848791	36.906548
1621.817162	80833.204869	36.911565
1623.179803	80909.667812	36.916583
1625.359408	80985.280936	36.921600
1626.849675	81060.267312	36.926618
1628.747701	81152.028079	36.931636
1630.340319	81222.247739	36.936653
1631.915959	81310.942731	36.941671
1633.440837	81388.319153	36.946688
1635.184935	81467.980057	36.951706
1636.882235	81548.649432	36.956724
1638.388207	81619.542481	36.961741
1639.744290	81699.872925	36.966759
1641.636470	81771.263390	36.971776
1643.311940	81854.344352	36.976794
1644.749539	81939.730725	36.981812
1646.612050	82021.870666	36.986829
1648.207271	82099.238036	36.991847
1649.979043	82172.928987	36.996864
1650.689059	82249.193633	37.001882
1652.538205	82308.631552	37.006900
1653.970154	82375.293572	37.011917
1655.232928	82450.737379	37.016935
1657.390889	82515.195512	37.021952
1658.985664	82597.074943	37.026970
1660.614479	82668.635606	37.031988
1662.042907	82739.873039	37.037005
1663.735943	82826.083702	37.042023
1665.194772	82896.024386	37.047040
1666.902504	82978.318038	37.052058
1668.495094	83063.860937	37.057076
1670.569788	83136.582044	37.062093
1672.208489	83231.646505	37.067111
1673.894085	83318.696090	37.072128
1675.710628	83397.666889	37.077146
1677.287059	83475.598473	37.082164
1679.247042	83561.186738	37.087181
1680.709229	83634.980628	37.092199
1682.554694	83715.265545	37.097216
1684.108741	83811.789667	37.102234
1685.742895	83886.013446	37.107252
1687.729826	83973.030543	37.112269
1689.117942	84058.494392	37.117287
1691.072286	84137.065545	37.122304
1692.834232	84232.038028	37.127322
1694.342430	84314.417453	37.132340
1696.712786	84409.992221	37.137357
1697.835144	84497.057521	37.142375
1699.679039	84583.820095	37.147392
1701.406957	84677.190135	37.152410
1703.149555	84759.762238	37.157428
1705.382825	84849.176335	37.162445
1706.870406	84936.350536	37.167463
1708.880015	85018.944954	37.172480
1710.458289	85107.081177	37.177498
1712.177199	85191.508259	37.182516
1713.803224	85272.541486	37.187533
1715.694722	85363.087747	37.192551
1717.608851	85440.300235	37.197568
1719.218163	85532.006287	37.202586
1720.913252	85613.371798	37.207604
1722.735341	85699.355505	37.212621
1724.512665	85786.981129	37.217639
1726.233166	85862.438333	37.222656
1728.037168	85945.473080	37.227674
1729.772788	86039.885414	37.232692
1731.817502	86113.505804	37.237709
1733.226597	86195.994820	37.242727
1734.653978	86279.431605	37.247744
1736.692836	86363.571271	37.252762
1738.098017	86448.355246	37.257780
1739.850604	86532.286761	37.262797
1741.629154	86631.991225	37.267815
1743.778150	86715.823216	37.272832
1745.603159	86792.939208	37.277850
1747.183894	86885.363651	37.282868
1748.886104	86958.570912	37.287885
1750.495304	87056.187063	37.292903
1752.317938	87124.383012	37.297920
1754.490537	87208.225399	37.302938
1756.442080	87289.378057	37.307956
1758.070032	87366.855887	37.312973
1759.480073	87446.535015	37.317991
1761.413223	87527.931990	37.323008
1763.099618	87608.873578	37.328026
1764.329304	87689.392632	37.333044
1766.554786	87769.033733	37.338061
1767.971336	87850.474431	37.343079
1769.721465	87910.535057	37.348096
1771.227467	87982.102793	37.353114
1772.460694	88051.330919	37.358132
1774.115290	88125.790477	37.363149
1776.057237	88213.587718	37.368167
1777.284695	88292.689420	37.373184
1779.373634	88383.163475	37.378202
1780.758906	88471.732935	37.383220
1782.782535	88550.203817	37.388237
1784.034159	88650.897383	37.393255
1785.925291	88743.950768	37.398272
1787.699808	88840.482440	37.403290
1789.522410	88941.328428	37.408308
1791.255205	89032.988113	37.413325
1792.752159	89135.051650	37.418343
1795.072318	89233.780388	37.423360
1796.764712	89342.099972	37.428378
1798.432569	89449.942205	37.433396
1800.504612	89550.941329	37.438413
1802.490899	89662.675916	37.443431
1803.972711	89756.823077	37.448448
1806.353526	89854.796652	37.453466
1808.410016	89962.060308	37.458484
1810.350972	90051.219216	37.463501
1811.856015	90152.055634	37.468519
1814.015785	90257.251062	37.473536
1815.993562	90361.702245	37.478554
1817.647526	90463.162765	37.483572
1819.680326	90549.913450	37.488589
1821.413559	90652.439478	37.493607
1823.399665	90755.902172	37.498624
1825.300963	90851.799496	37.503642
1827.423522	90946.331736	37.508660
1829.419848	91030.770188	37.513677
1830.894439	91138.040394	37.518695
1832.821293	91226.089689	37.523712
1834.865229	91321.928169	37.528730
1836.414831	91434.929063	37.533748
1838.340191	91524.348272	37.538765
1840.140661	91627.272671	37.543783
1841.669369	91724.790009	37.548800
1843.583275	91829.028142	37.553818
1845.288228	91935.922924	37.558836
1847.581788	92036.033889	37.563853
1849.242525	92146.041561	37.568871
1851.388287	92225.301468	37.573888
1853.426812	92338.812250	37.578906
1854.877083	92437.294741	37.583924
1857.062391	92541.949137	37.588941
1859.054223	92640.715104	37.593959
1860.699090	92748.585421	37.598976
1862.931531	92850.964733	37.603994
1864.664873	92951.445222	37.609012
1866.570785	93039.338289	37.614029
1868.471395	93147.360117	37.619047
1870.565986	93234.920024	37.624064
1872.222152	93331.167747	37.629082
1873.972201	93433.332973	37.634100
1875.882464	93505.370298	37.639117
1877.513219	93618.024369	37.644135
1879.627987	93718.903993	37.649152
1881.155591	93817.518253	37.654170
1883.007823	93921.646435	37.659188
1884.953941	94017.039724	37.664205
1886.822193	94116.805784	37.669223
1889.091747	94227.929822	37.674240
1890.664704	94308.019934	37.679258
1892.528282	94393.084226	37.684276
1894.150174	94481.038540	37.689293
1895.576720	94555.967963	37.694311
1897.152062	94650.369168	37.699328
1898.886961	94746.178028	37.704346
1900.448863	94845.081740	37.709364
1902.354545	94946.631877	37.714381
1904.129305	95055.985678	37.719399
1906.090527	95171.192209	37.724416
1908.050065	95266.080224	37.729434
1909.461611	95382.856613	37.734452
1911.751145	95503.717102	37.739469
1913.242034	95616.298926	37.744487
1915.091365	95731.575741	37.749504
1917.087459	95838.514584	37.754522
1918.658109	95966.803389	37.759540
1921.109304	96091.126760	37.764557
1923.252106	96215.815786	37.769575
1925.089858	96334.164254	37.774592
1927.381102	96445.495643	37.779610
1929.113970	96584.295522	37.784628
1931.057561	96693.413139	37.789645
1933.499589	96819.553544	37.794663
1935.623906	96942.651126	37.799680
1937.543953	97045.917149	37.804698
1939.282221	97171.940912	37.809716
1941.624478	97292.888782	37.814733
1943.327661	97409.766516	37.819751
1945.382683	97532.737799	37.824768
1947.968862	97653.534791	37.829786
1949.370549	97775.506375	37.834804
1951.740115	97896.439602	37.839821
1954.266501	98011.428669	37.844839
1955.716585	98129.464219	37.849856
1957.639577	98239.743990	37.854874
1959.400532	98359.582580	37.859892
1961.796279	98469.383509	37.864909
1963.925171	98585.666520	37.869927
1965.572257	98705.524227	37.874944
1967.838552	98812.025189	37.879962
1970.165919	98934.515573	37.884980
1972.009471	99050.768860	37.889997
1974.273533	99164.903050	37.895015
1975.789317	99274.819082	37.900032
1977.950280	99390.263294	37.905050
1979.526381	99507.333404	37.910068
1981.594731	99622.526715	37.915085
1983.504937	99746.365895	37.920103
1985.226314	99877.638799	37.925120
1987.915890	99981.262988	37.930138
1989.324854	100103.495847	37.935156
1991.583262	100220.702659	37.940173
1993.434473	100344.046253	37.945191
1995.268970	100465.034862	37.950208
1997.620630	100589.644932	37.955226
1999.159918	100722.826075	37.960244
2001.327991	100831.035242	37.965261
2003.389941	100959.482768	37.970279
2005.099380	101091.244215	37.975296
2007.204399	101210.025321	37.980314
2009.333497	101338.958281	37.985332
2011.360005	101470.265946	37.990349
2013.180460	101589.460625	37.995367
2014.966495	101718.398047	38.000384
2016.868369	101853.073816	38.005402
2018.688417	101980.954645	38.010420
2020.577157	102108.736476	38.015437
2022.533006	102228.368715	38.020455
2024.416651	102351.740174	38.025472
2026.636407	102477.557185	38.030490
2028.488528	102590.677503	38.035508
2030.388635	102717.496341	38.040525
2032.312651	102830.200513	38.045543
2033.809128	102961.064556	38.050560
2035.974857	103086.372511	38.055578
2037.481644	103214.370529	38.060596
2039.263260	103356.906787	38.065613
2041.697321	103494.308021	38.070631
2043.185576	103649.963453	38.075648
2045.596261	103781.118769	38.080666
2047.683474	103930.760667	38.085684
2049.660869	104076.908283	38.090701
2051.925492	104220.615220	38.095719
2053.998974	104367.636620	38.100736
2056.425882	104515.389485	38.105754
2058.353018	104663.373351	38.110772
2060.056066	104803.696496	38.115789
2062.268546	104953.931977	38.120807
2064.145375	105116.735388	38.125824
2066.439925	105257.043950	38.130842
2068.630354	105423.895296	38.135860
2070.646815	105578.678200	38.140877
2072.750709	105734.779511	38.145895
2074.911826	105897.795796	38.150912
2077.074825	106049.755670	38.155930
2079.255998	106214.634287	38.160948
2081.111611	106371.842490	38.165965
2083.643745	106535.615303	38.170983
2085.570027	106701.385721	38.176000
2087.698816	106854.216786	38.181018
2089.730933	107019.959507	38.186036
2091.757652	107189.634783	38.191053
2094.102647	107338.934404	38.196071
2096.140595	107511.716211	38.201088
2098.153715	107666.838795	38.206106
2100.186758	107830.949493	38.211124
2102.540462	108003.189817	38.216141
2104.854822	108160.473919	38.221159
2106.542865	108337.232941	38.226176
2108.859041	108489.686880	38.231194
2110.678247	108669.749449	38.236212
2113.073272	108842.076241	38.241229
2115.345714	109008.741970	38.246247
2117.428423	109179.673661	38.251264
2119.394800	109350.560983	38.256282
2121.665987	109517.723901	38.261300
2123.818444	109686.187001	38.266317
2125.772187	109863.470156	38.271335
2128.118054	110039.044273	38.276352
2130.338737	110209.819901	38.281370
2132.159106	110388.825883	38.286388
2134.276956	110552.454205	38.291405
2136.244026	110729.638177	38.296423
2138.553543	110892.223553	38.301440
2140.804885	111061.083561	38.306458
2142.885622	111242.551424	38.311476
2144.828784	111400.783175	38.316493
2147.435155	111581.409614	38.321511
2149.223810	111770.611119	38.326528
2151.749240	111937.454006	38.331546
2154.252754	112110.185605	38.336564
2155.818790	112292.119792	38.341581
2158.662556	112452.612225	38.346599
2160.601758	112619.943156	38.351616
2162.649434	112784.163397	38.356634
2164.399487	112954.099992	38.361652
2166.752210	113112.135707	38.366669
2168.900430	113259.398595	38.371687
2170.543164	113415.593609	38.376704
2172.801231	113573.899801	38.381722
2174.640272	113721.973898	38.386740
2176.526704	113887.175569	38.391757
2178.502509	114050.334757	38.396775
2180.366635	114222.643808	38.401792
2182.430503	114400.249247	38.406810
2184.334537	114580.505933	38.411828
2186.698334	114761.794998	38.416845
2188.752244	114940.444621	38.421863
2190.808933	115134.314486	38.426880
2192.811953	115315.041246	38.431898
2195.374244	115511.662354	38.436916
2197.505673	115714.300419	38.441933
2199.712833	115911.106043	38.446951
2201.519657	116108.571469	38.451968
2203.744696	116305.997878	38.456986
2205.787170	116508.311733	38.462004
2207.549580	116726.892973	38.467021
2210.277169	116923.800094	38.472039
2212.167663	117145.940568	38.477056
2214.704513	117361.119223	38.482074
2217.191232	117571.207982	38.487092
2219.118708	117791.672191	38.492109
2221.452849	118011.515960	38.497127
2223.513446	118224.186478	38.502144
2225.948292	118440.604925	38.507162
2228.678952	118655.646466	38.512180
2230.903307	118875.804154	38.517197
2233.472843	119085.723447	38.522215
2235.530133	119316.932653	38.527232
2237.767749	119534.922995	38.532250
2240.264503	119749.296939	38.537268
2242.390031	119967.319953	38.542285
2244.930885	120177.439974	38.547303
2246.836697	120386.480788	38.552320
2249.456705	120607.791562	38.557338
2251.668726	120830.626212	38.562356
2254.393258	121040.062548	38.567373
2257.054263	121256.930802	38.572391
2259.223511	121467.826312	38.577408
2261.781679	121675.300494	38.582426
2263.988200	121877.870788	38.587444
2265.902160	122100.810050	38.592461
2268.513536	122290.202334	38.597479
2270.895969	122503.670590	38.602496
2273.498740	122698.305342	38.607514
2275.550046	122909.493425	38.612532
2277.634299	123129.595609	38.617549
2280.159470	123326.186511	38.622567
2282.123572	123536.896819	38.627584
2284.218628	123743.312563	38.632602
2286.677253	123952.590292	38.637620
2288.661669	124175.530168	38.642637
2291.162153	124384.613308	38.647655
2293.292058	124606.238815	38.652672
2295.502089	124809.851066	38.657690
2297.635553	125035.258901	38.662708
2299.731758	125258.732784	38.667725
2301.933159	125475.429502	38.672743
2304.479437	125695.270450	38.677760
2306.655525	125915.157810	38.682778
2308.917125	126136.961361	38.687796
2311.346748	126363.370521	38.692813
2313.592862	126581.677333	38.697831
2315.654896	126799.493933	38.702848
2317.913350	127002.728929	38.707866
2320.281590	127191.763581	38.712884
2322.112740	127401.195245	38.717901
2324.609175	127609.293227	38.722919
2326.690124	127816.746761	38.727936
2328.340836	128027.960650	38.732954
2330.609812	128245.029277	38.737972
2332.876527	128463.647255	38.742989
2334.913262	128688.379682	38.748007
2336.874843	128929.022642	38.753024
2338.740438	129171.902335	38.758042
2341.172487	129410.203338	38.763060
2343.595149	129660.421023	38.768077
2345.804984	129904.481776	38.773095
2348.282217	130167.153425	38.778112
2350.175535	130423.117235	38.783130
2352.548858	130681.887687	38.788148
2354.957276	130948.774662	38.793165
2357.291114	131207.947787	38.798183
2359.636845	131478.844656	38.803200
2362.081601	131752.785642	38.808218
2364.531560	132028.922655	38.813236
2367.349943	132288.572035	38.818253
2369.344324	132555.076861	38.823271
2372.028906	132821.323068	38.828288
2374.517883	133095.773097	38.833306
2377.110505	133370.969953	38.838324
2379.905541	133643.954349	38.843341
2382.174475	133915.500036	38.848359
2384.927194	134184.192775	38.853376
2387.143033	134447.895428	38.858394
2389.680031	134700.636599	38.863412
2392.116512	134986.704512	38.868429
2394.713844	135257.712077	38.873447
2396.951694	135530.807827	38.878464
2399.483010	135804.252691	38.883482
2402.355469	136062.710083	38.888500
2404.503877	136334.111543	38.893517
2407.280429	136606.368086	38.898535
2409.998851	136872.582257	38.903552
2412.579094	137160.950900	38.908570
2414.961327	137419.441864	38.913588
2417.196379	137680.876023	38.918605
2419.347605	137949.570865	38.923623
2421.968983	138222.521090	38.928640
2424.099707	138488.646118	38.933658
2427.046754	138755.647500	38.938676
2429.042135	139031.352655	38.943693
2431.734489	139301.442690	38.948711
2434.131536	139573.598272	38.953728
2436.477249	139841.651655	38.958746
2439.005507	140113.599441	38.963764
2441.512902	140391.009102	38.968781
2444.006595	140656.962611	38.973799
2445.752654	140937.730709	38.978816
2447.871237	141218.289873	38.983834
2450.526759	141496.824924	38.988852
2452.407772	141791.549803	38.993869
2454.967171	142080.357733	38.998887
2457.097826	142371.582337	39.003904
2459.091885	142678.681645	39.008922
2461.966568	142977.281399	39.013940
2464.285600	143285.107826	39.018957
2466.486564	143570.452290	39.023975
2468.699793	143882.360297	39.028992
2471.193448	144199.709252	39.034010
2473.906229	144497.175790	39.039028
2475.850510	144808.154339	39.044045
2478.506647	145087.534449	39.049063
2480.952231	145367.609023	39.054080
2483.297613	145646.126979	39.059098
2486.009628	145930.326003	39.064116
2488.554665	146213.283489	39.069133
2490.665640	146495.739269	39.074151
2493.306973	146795.185008	39.079168
2495.736247	147083.597746	39.084186
2498.392026	147372.027420	39.089204
2500.448379	147679.147239	39.094221
2502.685170	147983.232444	39.099239
2504.858624	148292.469909	39.104256
2507.004336	148617.440041	39.109274
2509.654933	148934.285827	39.114292
2511.657583	149264.257935	39.119309
2514.347598	149599.316052	39.124327
2516.637701	149933.397965	39.129344
2518.777876	150275.768735	39.134362
2521.433244	150614.989275	39.139380
2523.980775	150961.400600	39.144397
2526.557982	151318.192792	39.149415
2529.249193	151676.378455	39.154432
2531.455601	152023.306785	39.159450
2534.506156	152369.559403	39.164468
2536.823342	152734.779276	39.169485
2539.635726	153088.474119	39.174503
2542.226051	153438.930854	39.179520
2544.808082	153805.182522	39.184538
2547.917895	154157.974310	39.189556
2550.546220	154510.551618	39.194573
2553.250780	154876.042003	39.199591
2555.670607	155225.558869	39.204608
2557.977886	155589.478308	39.209626
2560.789070	155945.767915	39.214644
2563.599631	156315.071804	39.219661
2565.900900	156678.656167	39.224679
2568.323053	157041.157482	39.229696
2570.803583	157421.132732	39.234714
2573.741658	157783.697484	39.239732
2576.396508	158157.086810	39.244749
2578.760422	158523.808218	39.249767
2581.571337	158892.505835	39.254784
2583.837112	159276.017459	39.259802
2586.767935	159642.669568	39.264820
2589.493351	160022.889300	39.269837
2591.963847	160394.492882	39.274855
2594.642766	160767.437184	39.279872
2597.418459	161145.586465	39.284890
2600.211194	161509.643068	39.289908
2602.623979	161890.900509	39.294925
2605.334461	162267.251123	39.299943
2608.050004	162639.616605	39.304960
2610.516241	163028.451870	39.309978
2612.950955	163397.285318	39.314996
2615.284186	163792.532046	39.320013
2617.500744	164176.169614	39.325031
2620.050458	164555.008851	39.330048
2622.289553	164957.755334	39.335066
2624.652809	165344.271403	39.340084
2627.289429	165749.499700	39.345101
2629.645994	166165.109246	39.350119
2632.353872	166570.826406	39.355136
2634.899554	166975.453989	39.360154
2637.104553	167393.938665	39.365172
2639.498862	167813.107243	39.370189
2642.198050	168225.234566	39.375207
2644.694325	168643.223954	39.380224
2647.476676	169056.295321	39.385242
2650.150599	169457.704566	39.390260
2652.745335	169856.500066	39.395277
2655.152704	170258.615644	39.400295
2657.735444	170642.574067	39.405312
2659.880541	171054.981781	39.410330
2662.594337	171458.401822	39.415348
2665.092876	171867.216073	39.420365
2667.919558	172284.894961	39.425383
2670.083136	172702.146525	39.430400
2672.521251	173137.616862	39.435418
2675.248449	173560.498886	39.440436
2678.017824	173994.373015	39.445453
2680.016109	174433.271555	39.450471
2683.172349	174875.610339	39.455488
2685.448003	175342.749123	39.460506
2688.045624	175774.869252	39.465524
2690.914267	176235.774420	39.470541
2693.360042	176696.316535	39.475559
2696.030290	177163.556244	39.480576
2698.946814	177636.347357	39.485594
2701.799321	178101.277965	39.490612
2704.511888	178575.071225	39.495629
2707.008784	179054.132662	39.500647
2709.774349	179532.087977	39.505664
2712.223125	180012.254205	39.510682
2714.838403	180496.435208	39.515700
2717.546532	180986.420402	39.520717
2720.438033	181475.287400	39.525735
2723.032131	181972.610304	39.530752
2726.025316	182477.442137	39.535770
2728.397259	183044.143072	39.540788
2731.564965	183562.211356	39.545805
2734.271582	184072.176078	39.550823
2737.105117	184563.150557	39.555840
2739.543884	185078.800885	39.560858
2742.777228	185582.061740	39.565876
2745.552761	186086.209438	39.570893
2748.112839	186605.505945	39.575911
2750.903341	187114.532938	39.580928
2753.378547	187627.853413	39.585946
2756.543863	188143.760762	39.590964
2759.254207	188663.475480	39.595981
2762.110869	189181.747331	39.600999
2765.329305	189692.217924	39.606016
2767.819154	190221.702545	39.611034
2770.720175	190732.100370	39.616052
2773.626860	191249.459250	39.621069
2776.009102	191771.703096	39.626087
2779.280525	192292.794082	39.631104
2782.282452	192820.965438	39.636122
2785.211333	193328.956698	39.641140
2788.045365	193842.172020	39.646157
2790.867581	194359.175984	39.651175
2793.831662	194886.294873	39.656192
2796.529986	195394.762018	39.661210
2798.743609	195910.825678	39.666228
2802.016756	196442.271269	39.671245
2804.987944	196952.936764	39.676263
2807.759474	197470.442945	39.681280
2810.298819	197999.164046	39.686298
2812.832026	198517.701822	39.691316
2815.949376	199044.050008	39.696333
2818.398101	199567.913535	39.701351
2821.085904	200095.551716	39.706368
2823.784017	200629.515148	39.711386
2826.303060	201157.691180	39.716404
2829.064023	201696.982662	39.721421
2831.568712	202234.080486	39.726439
2834.203834	202747.865427	39.731456
2836.963872	203274.511398	39.736474
2839.293876	203779.837078	39.741492
2842.209243	204301.076269	39.746509
2844.050523	204834.881399	39.751527
2847.010403	205369.529124	39.756544
2849.702102	205911.028168	39.761562
2852.403239	206454.533960	39.766580
2854.721287	207000.641329	39.771597
2857.393065	207566.610754	39.776615
2860.264166	208139.688686	39.781632
2862.984805	208728.592341	39.786650
2865.396586	209292.955306	39.791668
2868.304244	209883.331210	39.796685
2871.230637	210473.603881	39.801703
2874.081457	211061.679530	39.806720
2876.958980	211656.255504	39.811738
2880.047320	212267.083370	39.816756
2882.874605	212857.427128	39.821773
2885.781580	213473.137734	39.826791
2888.737697	214078.223000	39.831808
2891.606442	214709.895247	39.836826
2894.525346	215328.909595	39.841844
2897.658209	215950.126947	39.846861
2900.351060	216584.471573	39.851879
2902.738676	217192.978224	39.856896
2905.990168	217833.867519	39.861914
2908.914618	218470.871094	39.866932
2912.139807	219109.962243	39.871949
2914.986331	219755.616646	39.876967
2918.701244	220384.877235	39.881984
2921.438833	221028.364969	39.887002
2924.595390	221659.492051	39.892020
2927.676745	222302.393323	39.897037
2930.623502	222943.181999	39.902055
2933.449581	223575.682645	39.907072
2936.577801	224211.006865	39.912090
2939.865098	224851.742785	39.917108
2943.209703	225484.645322	39.922125
2946.062195	226126.287588	39.927143
2949.220812	226756.754905	39.932160
2952.256029	227397.377597	39.937178
2954.983608	228045.440765	39.942196
2957.877067	228680.978910	39.947213
2960.562865	229332.121864	39.952231
2963.525348	229976.362039	39.957248
2966.290108	230638.008988	39.962266
2969.274861	231284.734227	39.967284
2972.194235	231928.750848	39.972301
2975.243519	232600.131901	39.977319
2977.959448	233253.121050	39.982336
2981.056665	233911.232122	39.987354
2983.545273	234587.093103	39.992372
2986.631871	235244.949861	39.997389
2989.763049	235923.045365	40.002407
2992.810616	236586.316987	40.007424
2995.691666	237250.502555	40.012442
2998.305154	237927.709900	40.017460
3002.157731	238595.576781	40.022477
3005.024453	239271.369834	40.027495
3007.961089	239936.684178	40.032512
3011.740346	240599.782085	40.037530
3014.716953	241278.195024	40.042548
3018.055004	241935.642782	40.047565
3020.490971	242595.516123	40.052583
3023.968748	243245.266691	40.057600
3027.047505	243916.721156	40.062618
3029.920327	244553.352947	40.067636
3033.199211	245191.748328	40.072653
3036.072316	245813.261523	40.077671
3038.991060	246429.481876	40.082688
3042.407667	247052.176278	40.087706
3044.952882	247670.356211	40.092724
3047.744660	248290.045038	40.097741
3051.042844	248927.789783	40.102759
3053.994378	249550.929277	40.107776
3057.171948	250195.851563	40.112794
3059.890416	250827.176796	40.117812
3063.035789	251470.752720	40.122829
3065.413465	252115.690722	40.127847
3068.487133	252772.709983	40.132864
3071.567844	253427.896316	40.137882
3074.300665	254085.623434	40.142900
3077.504014	254747.388942	40.147917
3080.062052	255430.309836	40.152935
3083.114175	256101.414700	40.157952
3086.121095	256777.984444	40.162970
3089.256674	257472.438140	40.167988
3091.695437	258170.349886	40.173005
3094.738151	258886.705681	40.178023
3097.735721	259586.706436	40.183040
3100.630131	260300.460746	40.188058
3103.548279	261029.320035	40.193076
3106.916324	261749.823935	40.198093
3109.413706	262492.430146	40.203111
3112.322084	263244.593507	40.208128
3115.371015	263985.680877	40.213146
3118.683484	264736.195742	40.218164
3121.636159	265495.549491	40.223181
3124.378172	266276.189338	40.228199
3127.586168	267032.875461	40.233216
3130.943571	267808.555804	40.238234
3133.961638	268592.918339	40.243252
3137.031401	269372.948593	40.248269
3140.240547	270164.252502	40.253287
3142.946434	270948.288311	40.258304
3146.429259	271747.154799	40.263322
3149.782136	272546.491485	40.268340
3153.088889	273336.634303	40.273357
3156.160586	274142.984189	40.278375
3159.675735	274938.488869	40.283392
3162.838680	275735.336121	40.288410
3165.934572	276544.858561	40.293428
3169.554970	277335.142432	40.298445
3172.607814	278147.651856	40.303463
3176.096440	278937.813062	40.308480
3179.963346	279737.328397	40.313498
3182.911462	280546.933535	40.318516
3186.246416	281336.610961	40.323533
3189.275289	282128.181440	40.328551
3192.665307	282926.923932	40.333568
3195.901497	283710.445386	40.338586
3199.638831	284506.855593	40.343604
3203.583151	285284.535066	40.348621
3206.879668	286060.681805	40.353639
3210.046514	286847.072932	40.358656
3213.149705	287624.552090	40.363674
3216.200551	288413.913498	40.368692
3219.664277	289179.155071	40.373709
3222.722740	289967.404359	40.378727
3226.436525	290741.677977	40.383744
3229.567753	291509.685449	40.388762
3232.464378	292291.938485	40.393780
3235.711591	293053.992548	40.398797
3238.662026	293840.863476	40.403815
3241.960324	294610.404998	40.408832
3245.267757	295354.850890	40.413850
3248.202001	296103.204654	40.418868
3251.356092	296834.072659	40.423885
3254.268230	297589.493751	40.428903
3257.019248	298335.460386	40.433920
3260.251640	299095.913997	40.438938
3262.869217	299873.563952	40.443956
3265.924484	300651.464430	40.448973
3268.792896	301423.594918	40.453991
3271.940468	302207.322645	40.459008
3275.203828	302994.117682	40.464026
3278.230612	303803.352773	40.469044
3281.317575	304612.210456	40.474061
3284.460135	305424.651255	40.479079
3287.208080	306255.899316	40.484096
3290.872926	307069.907354	40.489114
3293.516989	307917.135538	40.494132
3297.267996	308751.941780	40.499149
3300.137155	309601.796218	40.504167
3303.542234	310454.572320	40.509184
3306.828501	311313.138678	40.514202
3310.042063	312177.360710	40.519220
3313.495512	313044.118080	40.524237
3317.204420	313919.651438	40.529255
3319.866721	314802.463297	40.534272
3323.249098	315684.028790	40.539290
3326.536081	316580.133630	40.544308
3330.242388	317460.547668	40.549325
3333.227302	318364.987584	40.554343
3336.750491	319264.350838	40.559360
3340.271471	320163.061374	40.564378
3343.222706	321066.562023	40.569396
3347.112188	321954.976287	40.574413
3351.133036	322863.244847	40.579431
3354.447639	323771.198075	40.584448
3358.060038	324665.053352	40.589466
3361.375868	325576.899425	40.594484
3364.899573	326477.224282	40.599501
3368.664628	327373.837743	40.604519
3371.921289	328277.538316	40.609536
3375.935461	329174.199025	40.614554
3379.080708	330078.509927	40.619572
3382.450165	330971.678337	40.624589
3386.019246	331879.432577	40.629607
3388.967747	332791.701681	40.634624
3392.479520	333684.835119	40.639642
3395.844450	334602.347852	40.644660
3399.474164	335504.982680	40.649677
3402.944752	336415.711959	40.654695
3406.436131	337326.719718	40.659712
3409.815454	338232.497084	40.664730
3413.179630	339151.316365	40.669748
3416.554735	340057.099057	40.674765
3419.860774	340977.706419	40.679783
3423.312662	341898.824837	40.684800
3426.742748	342808.915635	40.689818
3430.317688	343733.694255	40.694836
3433.820446	344654.325621	40.699853
3437.441632	345553.840234	40.704871
3440.998162	346473.272704	40.709888
3444.091025	347386.463772	40.714906
3447.337065	348301.177989	40.719924
3450.910468	349220.303775	40.724941
3454.569159	350137.666301	40.729959
3457.689926	351054.656050	40.734976
3461.348093	351975.085349	40.739994
3464.391684	352895.381502	40.745012
3467.853138	353800.764558	40.750016
3471.140576	354682.149240	40.755021
3474.394672	355521.374530	40.760026
3477.212320	356298.225148	40.765031
3479.858036	357038.943277	40.770036
3482.850924	357725.279039	40.775040
3485.807768	358360.879239	40.780045
3488.370643	358952.816995	40.785050
3491.057820	359477.557736	40.790055
3492.805836	359967.926154	40.795060
3495.755541	360399.295281	40.800064
3498.031544	360786.699627	40.805069
3499.856308	361114.986291	40.810074
3501.935177	361417.233980	40.815079
3504.034992	361668.043545	40.820084
3505.413106	361879.246764	40.825088
3507.006484	362056.644092	40.830093
3508.513991	362181.733519	40.835098
3510.095481	362283.560293	40.840103
3511.217760	362353.466834	40.845108
3512.301915	362396.749125	40.850112
3513.147644	362392.881620	40.855117
3514.352306	362380.013550	40.860122
3515.300803	362338.903752	40.865127
3516.042700	362282.020895	40.870132
3516.508605	362192.071169	40.875136
3517.284008	362095.211920	40.880141
3518.170267	361969.341403	40.885146
3518.749888	361830.711231	40.890151
3519.297311	361678.007772	40.895156
3519.908242	361509.894472	40.900160
3520.474177	361333.249076	40.905165
3520.678834	361124.945654	40.910170
3520.908422	360931.299386	40.915175
3521.103869	360708.281184	40.920180
3521.558092	360487.380888	40.925184
3521.673961	360250.877969	40.930189
3521.881469	360006.353966	40.935194
3522.247933	359755.195857	40.940199
3522.144876	359511.859973	40.945204
3522.191062	359246.440303	40.950208
3522.418103	358982.031983	40.955213
3522.169362	358727.505345	40.960218
3522.667860	358447.700215	40.965223
3522.634856	358180.225126	40.970228
3522.779414	357888.957713	40.975232
3522.715752	357601.710148	40.980237
3522.594182	357329.133190	40.985242
3522.534118	357037.305163	40.990247
3522.635816	356755.030579	40.995252
3522.323675	356466.870932	41.000256
3522.393364	356177.988109	41.005261
3522.517168	355888.992477	41.010266
3522.201976	355591.243430	41.015271
3521.960484	355310.890171	41.020276
3521.886683	355018.638677	41.025280
3521.909790	354720.904708	41.030285
3521.470066	354428.959099	41.035290
3521.723345	354146.078057	41.040295
3521.430246	353862.568212	41.045300
3521.136501	353571.633967	41.050304
3521.494233	353292.592454	41.055309
3520.782776	353013.995245	41.060314
3521.099636	352719.043346	41.065319
3520.844905	352445.122995	41.070324
3520.846710	352161.221444	41.075328
3520.952459	351882.181583	41.080333
3520.115443	351596.626846	41.085338
3520.036918	351312.959135	41.090343
3519.932393	351050.772629	41.095348
3519.666128	350770.281545	41.100352
3519.893037	350497.413228	41.105357
3519.619948	350233.187436	41.110362
3519.752390	349960.049758	41.115367
3519.492506	349694.699034	41.120372
3519.386345	349428.813706	41.125376
3519.097230	349160.895710	41.130381
3518.766757	348894.608963	41.135386
3518.607088	348637.216324	41.140391
3518.685715	348383.648529	41.145396
3518.786378	348122.626714	41.150400
3518.735345	347864.194196	41.155405
3518.276169	347611.187589	41.160410
3518.406862	347343.290922	41.165415
3518.152297	347103.061426	41.170420
3518.041829	346849.282684	41.175424
3517.892818	346595.863968	41.180429
3517.383851	346343.923317	41.185434
3517.731972	346096.295895	41.190439
3517.332987	345861.546136	41.195444
3517.246572	345614.593280	41.200448
3516.988187	345372.419800	41.205453
3516.548947	345141.459518	41.210458
3516.876534	344900.894486	41.215463
3516.491399	344670.710702	41.220468
3516.543147	344436.897601	41.225472
3516.516981	344201.976385	41.230477
3515.984276	343984.447224	41.235482
3515.972493	343745.172940	41.240487
3516.028012	343525.616592	41.245492
3515.783393	343291.664040	41.250496
3516.127138	343077.195742	41.255501
3515.596153	342861.464443	41.260506
3515.517856	342629.668034	41.265511
3515.382355	342418.118298	41.270516
3515.102375	342201.707998	41.275520
3515.068989	341991.690714	41.280525
3514.576612	341779.836922	41.285530
3514.955220	341564.514762	41.290535
3514.681608	341370.245087	41.295540
3514.360638	341156.479128	41.300544
3514.473585	340945.873297	41.305549
3514.091175	340751.235799	41.310554
3514.142147	340548.621496	41.315559
3513.975569	340339.072845	41.320564
3513.869096	340148.813313	41.325568
3513.968796	339952.494089	41.330573
3513.651269	339765.850848	41.335578
3513.730033	339566.939098	41.340583
3513.549870	339373.228687	41.345588
3513.356204	339182.113049	41.350592
3513.092516	338981.954721	41.355597
3512.742572	338806.093293	41.360602
3513.082520	338616.645803	41.365607
3512.730732	338434.883326	41.370612
3512.869993	338265.808626	41.375616
3512.955566	338075.075735	41.380621
3512.549692	337892.505240	41.385626
3512.381472	337716.762660	41.390631
3512.166974	337552.495261	41.395636
3512.384780	337372.799917	41.400640
3512.514391	337195.126440	41.405645
3512.117649	337027.426685	41.410650
3511.857070	336860.289765	41.415655
3511.735923	336681.076312	41.420660
3511.484208	336520.624624	41.425664
3511.566225	336355.313686	41.430669
3511.324210	336199.004251	41.435674
3511.463183	336030.504114	41.440679
3511.242596	335871.443412	41.445684
3511.021516	335710.754518	41.450688
3511.245499	335550.961725	41.455693
3510.643383	335402.563414	41.460698
3510.900589	335252.173678	41.465703
3510.798379	335102.220994	41.470708
3510.761973	334946.204716	41.475712
3510.605050	334789.723422	41.480717
3510.441969	334638.583096	41.485722
3510.530630	334491.370164	41.490727
3510.143897	334353.361033	41.495732
3510.251561	334212.603738	41.500736
3510.137876	334062.063722	41.505741
3509.863727	333928.180855	41.510746
3509.881438	333776.398404	41.515751
3509.840068	333646.877930	41.520756
3509.543443	333500.408012	41.525760
3509.633464	333359.192488	41.530765
3509.748939	333234.198508	41.535770
3509.445290	333097.417969	41.540775
3509.253488	332969.724413	41.545780
3509.240599	332840.781673	41.550784
3509.363416	332714.182550	41.555789
3509.388281	332586.453828	41.560794
3509.299341	332443.965778	41.565799
3508.857548	332321.929861	41.570804
3508.869482	332195.651545	41.575808
3508.988176	332070.322591	41.580813
3508.876822	331955.228039	41.585818
3508.752525	331813.709634	41.590823
3508.569980	331694.530612	41.595828
3508.659348	331584.261401	41.600832
3508.726433	331458.404401	41.605837
3508.362313	331347.544125	41.610842
3508.261529	331233.107033	41.615847
3508.168388	331119.075350	41.620852
3507.905466	331000.237381	41.625856
3508.129346	330892.081624	41.630861
3507.505758	330779.683354	41.635866
3507.661989	330668.205651	41.640871
3507.523912	330567.328937	41.645876
3507.356395	330459.945326	41.650880
3507.486430	330354.651403	41.655885
3507.083798	330272.001008	41.660890
3507.231268	330165.839070	41.665895
3507.214359	330068.477540	41.670900
3507.340534	329959.571411	41.675904
3507.248535	329860.695009	41.680909
3506.959769	329773.498337	41.685914
3506.982547	329676.968977	41.690919
3506.903475	329587.984090	41.695924
3507.046009	329494.309722	41.700928
3506.663087	329389.678394	41.705933
3506.860195	329294.087372	41.710938
3506.744338	329195.848899	41.715943
3506.897570	329109.548188	41.720948
3506.666613	329020.941853	41.725952
3506.573070	328933.000594	41.730957
3506.352776	328849.224952	41.735962
3506.619587	328754.588272	41.740967
3506.234600	328668.040073	41.745972
3506.215519	328584.613946	41.750976
3506.410856	328501.281300	41.755981
3506.114402	328420.746999	41.760986
3506.187219	328338.348855	41.765991
3506.177475	328255.429291	41.770996
3506.129570	328165.139077	41.776000
3506.153873	328080.382430	41.781005
3506.049791	328004.802677	41.786010
3506.090912	327922.154260	41.791015
3505.933640	327838.748166	41.796020
3505.837790	327763.268410	41.801024
3505.882118	327687.283306	41.806029
3505.865309	327607.161487	41.811034
3505.918587	327537.686408	41.816039
3505.638111	327463.557642	41.821044
3505.801763	327382.567755	41.826048
3505.987856	327295.927278	41.831053
3505.541794	327235.636029	41.836058
3505.554174	327147.699685	41.841063
3505.438719	327074.816231	41.846068
3505.513087	327005.006251	41.851072
3505.892104	326939.650834	41.856077
3505.423035	326865.219764	41.861082
3505.400041	326787.005031	41.866087
3505.444543	326735.081381	41.871092
3505.383389	326649.495637	41.876096
3505.584875	326577.401149	41.881101
3505.160354	326510.644437	41.886106
3505.254527	326436.099078	41.891111
3505.089664	326377.466863	41.896116
3504.761700	326312.882322	41.901120
3505.084950	326243.108421	41.906125
3504.922186	326189.868299	41.911130
3504.864065	326115.651404	41.916135
3505.135228	326054.152447	41.921140
3504.821047	325982.926073	41.926144
3504.904960	325923.669246	41.931149
3504.863129	325873.538605	41.936154
3504.929302	325793.094944	41.941159
3504.704771	325731.749306	41.946164
3504.578334	325679.087896	41.951168
3504.535466	325619.697819	41.956173
3504.622086	325567.231893	41.961178
3504.534659	325500.191872	41.966183
3503.983471	325454.006875	41.971188
3504.235261	325398.996575	41.976192
3504.287885	325338.675399	41.981197
3504.079300	325289.027987	41.986202
3504.449908	325234.380456	41.991207
3504.451731	325179.765070	41.996212
3503.950029	325132.249199	42.001216
3504.159805	325071.470615	42.006221
3504.147059	325032.043773	42.011226
3503.954868	324980.994333	42.016231
3504.370635	324930.180477	42.021236
3503.906611	324887.517100	42.026240
3504.247652	324823.130855	42.031245
3503.860764	324777.886053	42.036250
3503.998053	324712.132390	42.041255
3504.309932	324672.069371	42.046260
3504.138589	324630.759071	42.051264
3503.896243	324573.662662	42.056269
3504.122596	324532.035705	42.061274
3504.027475	324480.385384	42.066279
3504.007755	324431.368800	42.071284
3503.851390	324381.025286	42.076288
3503.993297	324338.292045	42.081293
3503.913961	324293.431080	42.086298
3503.688811	324240.299918	42.091303
3503.791072	324200.142019	42.096308
3503.693031	324162.177671	42.101312
3503.836001	324112.957203	42.106317
3503.501432	324075.538525	42.111322
3503.514657	324021.657533	42.116327
3503.689244	323985.049524	42.121332
3503.475057	323931.789056	42.126336
3503.761355	323897.554740	42.131341
3503.386448	323859.735153	42.136346
3503.488042	323816.549778	42.141351
3503.719058	323767.340573	42.146356
3503.656454	323725.630783	42.151360
3503.711561	323686.497308	42.156365
3503.455090	323646.318638	42.161370
3503.702915	323607.078643	42.166375
3503.340803	323565.466394	42.171380
3503.488068	323522.477083	42.176384
3503.153704	323475.060329	42.181389
3503.123248	323457.105221	42.186394
3503.435797	323414.827688	42.191399
3503.229164	323381.331423	42.196404
3502.863808	323339.236113	42.201408
3503.536638	323303.465413	42.206413
3503.295447	323275.443864	42.211418
3503.390589	323221.625342	42.216423
3503.455756	323200.729675	42.221428
3503.446428	323169.288402	42.226432
3503.433697	323110.653164	42.231437
3503.337654	323081.769298	42.236442
3503.013991	323039.107504	42.241447
3502.457120	323009.532457	42.246452
3503.082241	322983.741123	42.251456
3503.370878	322941.339652	42.256461
3503.101094	322909.480994	42.261466
3503.293082	322870.325352	42.266471
3502.854434	322833.583247	42.271476
3502.724885	322809.817740	42.276480
3502.948996	322775.286951	42.281485
3502.910773	322744.969207	42.286490
3502.898799	322718.819403	42.291495
3502.748712	322679.462668	42.296500
3502.664790	322648.134421	42.301504
3502.664415	322614.478097	42.306509
3502.722028	322592.998199	42.311514
3502.859146	322561.584452	42.316519
3503.050944	322539.371242	42.321524
3502.731607	322501.134699	42.326528
3503.085499	322473.808202	42.331533
3502.498165	322453.726481	42.336538
3502.880429	322422.833975	42.341543
3502.632399	322392.803173	42.346548
3502.789932	322352.812927	42.351552
3502.837457	322325.356154	42.356557
3502.797895	322306.435267	42.361562
3502.300500	322266.013095	42.366567
3502.434127	322246.810709	42.371572
3502.320524	322228.639113	42.376576
3502.643491	322195.160859	42.381581
3502.532644	322176.708974	42.386586
3502.514491	322150.712420	42.391591
3502.437900	322131.746364	42.396596
3502.219220	322108.401431	42.401600
3502.515858	322079.633562	42.406605
3502.224404	322059.734352	42.411610
3502.564563	322038.947753	42.416615
3502.222911	322008.727795	42.421620
3502.379292	321988.478699	42.426624
3502.449142	321965.190337	42.431629
3502.144300	321938.068239	42.436634
3502.418922	321918.462061	42.441639
3502.740375	321897.601997	42.446644
3501.946241	321882.258716	42.451648
3502.390221	321853.467658	42.456653
3502.495538	321834.218629	42.461658
3502.481643	321808.424718	42.466663
3502.751449	321783.629477	42.471668
3502.578122	321768.087339	42.476672
3502.603842	321731.933109	42.481677
3502.107126	321717.179271	42.486682
3502.361420	321679.819021	42.491687
3502.577392	321658.949890	42.496692
3502.458844	321638.463768	42.501696
3502.267639	321615.088826	42.506701
3501.985024	321602.794603	42.511706
3502.162040	321583.992173	42.516711
3502.359765	321556.028055	42.521716
3502.368600	321539.694150	42.526720
3502.861512	321508.936317	42.531725
3502.388300	321488.149408	42.536730
3502.286004	321463.055991	42.541735
3502.570668	321444.287550	42.546740
3502.245756	321422.434376	42.551744
3502.536185	321389.520255	42.556749
3502.283680	321375.415003	42.561754
3502.318738	321346.738412	42.566759
3502.451489	321326.670776	42.571764
3502.095418	321297.393852	42.576768
3501.817133	321280.799452	42.581773
3502.394608	321268.345227	42.586778
3502.442500	321242.770274	42.591783
3502.549716	321233.671357	42.596788
3502.003236	321204.246056	42.601792
3502.615108	321181.406771	42.606797
3501.958038	321156.959593	42.611802
3502.123354	321139.761538	42.616807
3502.115184	321115.594494	42.621812
3502.131930	321099.131980	42.626816
3502.438237	321080.665280	42.631821
3501.944182	321064.079088	42.636826
3502.159158	321044.329189	42.641831
3502.276890	321022.915415	42.646836
3502.412578	320999.590789	42.651840
3502.306848	320981.366546	42.656845
3501.973638	320958.674895	42.661850
3502.191697	320937.118191	42.666855
3502.389391	320914.445277	42.671860
3502.141451	320906.902805	42.676864
3502.023302	320889.977931	42.681869
3501.956392	320874.317065	42.686874
3502.228980	320856.160826	42.691879
3502.316711	320838.084360	42.696884
3502.212603	320827.949892	42.701888
3501.947040	320798.989202	42.706893
3501.537247	320782.135321	42.711898
3501.809174	320759.196313	42.716903
3501.646481	320747.671752	42.721908
3501.755288	320742.363132	42.726912
3502.005813	320724.744539	42.731917
3502.041476	320722.754631	42.736922
3502.073978	320702.676934	42.741927
3502.098461	320681.201245	42.746932
3501.594548	320667.771079	42.751936
3501.895081	320645.158266	42.756941
3501.600309	320635.384289	42.761946
3501.522619	320629.952168	42.766951
3501.667534	320609.093631	42.771956
3501.588216	320593.841654	42.776960
3502.012905	320576.602822	42.781965
3501.639625	320575.643588	42.786970
3501.948292	320554.199729	42.791975
3502.220216	320543.472150	42.796980
3502.218103	320527.241331	42.801985
3502.269893	320501.716206	42.806989
3501.739248	320501.646558	42.811994
3501.803420	320468.792541	42.816999
3502.115697	320468.896401	42.822004
3502.021584	320450.975404	42.827009
3501.993881	320431.873741	42.832013
3501.678092	320414.445321	42.837018
3502.095216	320400.133293	42.842023
3501.999140	320381.780081	42.847028
3502.274677	320373.417891	42.852033
3502.226918	320340.377748	42.857037
3501.833769	320333.824628	42.862042
3501.850355	320315.937150	42.867047
3501.991169	320291.949875	42.872052
3501.656857	320285.412990	42.877057
3501.822938	320273.658815	42.882061
3501.954925	320251.631845	42.887066
3501.758414	320241.486243	42.892071
3501.910386	320228.309571	42.897076
3501.760938	320213.831649	42.902081
3501.889222	320205.314361	42.907085
3501.900163	320199.588478	42.912090
3501.944797	320173.555458	42.917095
3501.819214	320163.653158	42.922100
3501.856595	320158.228428	42.927105
3501.984409	320131.470031	42.932109
3502.009282	320127.522829	42.937114
3502.077869	320105.887311	42.942119
3501.843527	320086.843241	42.947124
3501.620913	320067.008658	42.952129
3502.032142	320060.126213	42.957133
3501.754130	320037.756176	42.962138
3501.341658	320040.212154	42.967143
3501.549311	320033.361531	42.972148
3501.274446	320022.134163	42.977153
3501.681003	320001.056339	42.982157
3501.431199	320001.604250	42.987162
3501.666901	319983.987671	42.992167
3501.444296	319985.930588	42.997172
3501.473597	319980.100041	43.002177
3501.797311	319947.739311	43.007181
3501.847440	319949.944884	43.012186
3501.507081	319947.657553	43.017191
3501.726059	319932.104294	43.022196
3501.681452	319914.556950	43.027201
3501.638296	319901.079950	43.032205
3501.249937	319909.358178	43.037210
3501.636774	319894.592778	43.042215
3502.012918	319866.345250	43.047220
3501.628969	319861.444292	43.052225
3501.827069	319851.033376	43.057229
3501.736755	319840.336812	43.062234
3501.630427	319819.822466	43.067239
3501.786803	319821.375406	43.072244
3501.499112	319812.261603	43.077249
3501.611687	319793.315814	43.082253
3501.378162	319783.099567	43.087258
3501.828626	319773.590501	43.092263
3501.951771	319765.760842	43.097268
3501.666781	319742.526742	43.102273
3501.487808	319734.795192	43.107277
3501.869136	319727.561192	43.112282
3501.723310	319718.043573	43.117287
3501.509245	319694.187769	43.122292
3501.253437	319693.668091	43.127297
3501.578303	319677.309508	43.132301
3501.640260	319684.626934	43.137306
3501.663638	319685.411994	43.142311
3501.469343	319651.656435	43.147316
3501.350747	319647.833384	43.152321
3501.666817	319641.220162	43.157325
3501.521646	319638.240825	43.162330
3501.874804	319630.680477	43.167335
3501.747554	319604.063394	43.172340
3501.963888	319610.364488	43.177345
3501.848448	319581.048769	43.182349
3501.693777	319571.786913	43.187354
3501.680368	319555.481170	43.192359
3501.470279	319548.085188	43.197364
3501.004850	319532.664226	43.202369
3501.818915	319521.266485	43.207373
3501.638449	319515.646760	43.212378
3501.533626	319506.071800	43.217383
3501.539872	319506.248949	43.222388
3501.568197	319499.757016	43.227393
3501.828460	319480.966090	43.232397
3501.528731	319481.979757	43.237402
3501.564391	319479.124786	43.242407
3501.429024	319465.255004	43.247412
3501.479138	319460.515112	43.252417
3501.942496	319443.524196	43.257421
3501.692631	319441.578869	43.262426
3501.787336	319423.500718	43.267431
3501.727303	319405.421310	43.272436
3501.682825	319398.075735	43.277441
3502.059043	319392.343521	43.282445
3501.750273	319369.596325	43.287450
3501.747384	319358.402587	43.292455
3501.914071	319354.153287	43.297460
3501.643422	319338.854453	43.302465
3501.998006	319318.852963	43.307469
3501.511481	319318.598323	43.312474
3501.418778	319310.064525	43.317479
3501.739199	319285.158160	43.322484
3501.626644	319275.355385	43.327489
3501.788524	319261.540832	43.332493
3501.738907	319267.959878	43.337498
3501.361101	319236.827717	43.342503
3501.379888	319224.129507	43.347508
3501.380195	319230.082807	43.352513
3501.668924	319215.383397	43.357517
3501.184141	319221.234446	43.362522
3501.529524	319218.763543	43.367527
3501.357572	319196.987084	43.372532
3501.478259	319196.688396	43.377537
3501.535306	319174.596269	43.382541
3501.783420	319180.103769	43.387546
3501.573143	319173.954388	43.392551
3501.577864	319154.516350	43.397556
3501.842960	319148.725152	43.402561
3501.755917	319138.460410	43.407565
3501.714538	319130.147526	43.412570
3501.645388	319108.507601	43.417575
3502.021761	319099.849544	43.422580
3501.793479	319086.121374	43.427585
3501.773838	319059.614342	43.432589
3501.559502	319058.095949	43.437594
3501.640716	319052.180837	43.442599
3501.509650	319046.273470	43.447604
3501.381599	319021.258975	43.452609
3501.647895	319004.349580	43.457613
3501.552818	319008.409700	43.462618
3501.780804	319004.481524	43.467623
3501.857635	318992.511980	43.472628
3501.377114	318989.839443	43.477633
3501.790328	318972.881625	43.482637
3501.630557	318964.231036	43.487642
3501.693179	318944.936502	43.492647
3501.757643	318937.650142	43.497652
3501.924574	318930.296879	43.502657
3501.636672	318925.965957	43.507661
3501.733905	318911.550800	43.512666
3501.581300	318889.440421	43.517671
3501.885921	318883.057849	43.522676
3501.790573	318870.224730	43.527681
3501.696275	318840.472696	43.532685
3501.757524	318840.488599	43.537690
3501.990307	318833.939159	43.542695
3501.906832	318824.386154	43.547700
3501.751175	318818.838784	43.552705
3501.659620	318805.394451	43.557709
3501.642871	318790.539122	43.562714
3501.804958	318764.105265	43.567719
3502.039768	318767.452348	43.572724
3501.709810	318746.107434	43.577729
3501.913666	318735.517258	43.582733
3501.788446	318736.223800	43.587738
3501.711806	318717.358006	43.592743
3501.617577	318698.800256	43.597748
3501.508854	318695.280878	43.602753
3502.071928	318682.853603	43.607757
3501.616968	318672.646270	43.612762
3501.655636	318648.953915	43.617767
3501.488382	318644.807637	43.622772
3501.618852	318651.096853	43.627777
3501.760885	318617.694978	43.632781
3501.955410	318614.433487	43.637786
3501.397771	318605.590609	43.642791
3501.083767	318608.133040	43.647796
3501.281760	318603.166400	43.652801
3501.873028	318581.422964	43.657805
3501.447415	318567.445621	43.662810
3501.740898	318555.442085	43.667815
3501.670995	318554.486258	43.672820
3501.576111	318535.496029	43.677825
3501.737609	318525.930101	43.682829
3501.511655	318530.214262	43.687834
3501.644251	318513.071160	43.692839
3501.690282	318490.344360	43.697844
3501.319860	318481.930143	43.702849
3501.685943	318478.158423	43.707853
3501.707682	318476.119706	43.712858
3501.359835	318463.529478	43.717863
3501.513335	318444.678470	43.722868
3501.670880	318440.405069	43.727873
3501.704673	318429.078148	43.732877
3501.954390	318418.302632	43.737882
3501.853659	318409.261072	43.742887
3501.971887	318396.445307	43.747892
3501.588405	318395.843805	43.752897
3501.713213	318357.661331	43.757901
3501.619814	318351.391792	43.762906
3501.544869	318343.084006	43.767911
3501.777765	318338.926025	43.772916
3501.415163	318327.075883	43.777921
3501.903424	318317.815012	43.782925
3501.683754	318309.529846	43.787930
3501.833565	318298.057543	43.792935
3501.632343	318272.926849	43.797940
3501.596790	318275.629302	43.802945
3501.745171	318259.170568	43.807949
3501.624961	318248.987128	43.812954
3501.151025	318234.890022	43.817959
3501.729156	318221.111832	43.822964
3501.474787	318224.688086	43.827969
3501.558897	318218.212683	43.832973
3501.777820	318214.972789	43.837978
3501.554843	318196.740260	43.842983
3501.634219	318183.167243	43.847988
3501.418454	318176.662389	43.852993
3501.643339	318170.215854	43.857997
3501.780885	318159.737674	43.863002
3501.662211	318149.096013	43.868007
3501.957682	318147.065369	43.873012
3501.612979	318135.161492	43.878017
3501.476580	318116.381108	43.883021
3501.453602	318108.752091	43.888026
3501.689027	318102.151246	43.893031
3501.552778	318098.763334	43.898036
3501.599242	318078.656795	43.903041
3501.565087	318071.589247	43.908045
3501.721002	318063.601506	43.913050
3502.195628	318056.327202	43.918055
3501.550240	318033.810030	43.923060
3501.262039	318028.334166	43.928065
3501.991795	318018.170443	43.933069
3501.877783	318006.052370	43.938074
3501.344219	317996.137032	43.943079
3501.519195	317984.024656	43.948084
3501.410667	317980.988593	43.953089
3501.684450	317977.002281	43.958093
3501.613940	317951.978179	43.963098
3501.558494	317939.545624	43.968103
3501.819720	317934.518139	43.973108
3501.545874	317934.332008	43.978113
3501.347733	317906.529185	43.983117
3501.423912	317898.477553	43.988122
3501.314824	317893.075439	43.993127
3501.691415	317897.926960	43.998132
3501.896711	317898.403746	44.003137
3501.467665	317881.704396	44.008141
3501.662689	317865.238223	44.013146
3501.944130	317872.089120	44.018151
3502.042576	317846.529698	44.023156
3501.749885	317836.958301	44.028161
3501.815128	317812.421742	44.033165
3501.925875	317814.567062	44.038170
3501.909922	317790.272166	44.043175
3501.998800	317776.875636	44.048180
3501.712854	317764.275529	44.053185
3501.844576	317753.238431	44.058189
3501.709817	317737.281731	44.063194
3501.625534	317731.087006	44.068199
3501.629740	317714.421627	44.073204
3501.771287	317710.761274	44.078209
3501.910581	317698.527187	44.083213
3501.630816	317679.667260	44.088218
3501.860318	317670.090515	44.093223
3501.750322	317662.144274	44.098228
3501.351275	317657.805159	44.103233
3501.504015	317641.345513	44.108237
3501.684052	317634.804142	44.113242
3501.655523	317617.355129	44.118247
3501.534540	317606.103078	44.123252
3501.187925	317606.742480	44.128257
3501.571605	317581.723488	44.133261
3501.409349	317573.683631	44.138266
3501.638147	317574.233074	44.143271
3501.379702	317574.629710	44.148276
3501.456200	317569.427524	44.153281
3501.333151	317557.946801	44.158285
3501.471136	317548.333453	44.163290
3501.525153	317538.402476	44.168295
3501.796837	317529.022646	44.173300
3501.330170	317530.902057	44.178305
3501.697014	317522.117967	44.183309
3501.693044	317506.115293	44.188314
3501.548722	317500.565984	44.193319
3501.635309	317504.826824	44.198324
3501.469775	317491.139229	44.203329
3501.642242	317466.611158	44.208333
3501.663347	317463.224038	44.213338
3501.376645	317453.880604	44.218343
3501.675653	317451.747606	44.223348
3501.683742	317437.778425	44.228353
3501.532727	317418.592948	44.233357
3501.339926	317412.364258	44.238362
3501.328334	317408.117200	44.243367
3501.455122	317417.409390	44.248372
3501.361669	317410.376449	44.253377
3501.540919	317386.228910	44.258381
3501.819115	317383.005133	44.263386
3501.668052	317371.757725	44.268391
3501.570498	317365.081614	44.273396
3501.362200	317349.746892	44.278401
3501.486227	317334.919947	44.283405
3501.172299	317333.824145	44.288410
3501.136847	317332.837463	44.293415
3501.706968	317329.847911	44.298420
3501.616740	317331.185069	44.303425
3501.776350	317314.062719	44.308429
3501.485931	317288.614654	44.313434
3501.415461	317283.562625	44.318439
3501.549479	317282.752987	44.323444
3501.605996	317279.156777	44.328449
3501.757323	317258.550061	44.333453
3501.389964	317252.730278	44.338458
3501.698284	317245.049317	44.343463
3501.985044	317235.158214	44.348468
3501.654043	317225.490903	44.353473
3501.714604	317206.831995	44.358477
3501.395515	317203.854239	44.363482
3501.188629	317202.258288	44.368487
3501.672417	317190.606270	44.373492
3501.639580	317176.541634	44.378497
3501.811910	317166.235880	44.383501
3501.525411	317173.048464	44.388506
3501.867543	317149.180645	44.393511
3501.920126	317129.912327	44.398516
3501.789908	317131.026758	44.403521
3501.495765	317113.898943	44.408525
3501.744025	317094.701789	44.413530
3501.567840	317084.883029	44.418535
3501.831052	317082.857381	44.423540
3501.934309	317071.213938	44.428545
3502.129994	317049.938679	44.433549
3501.683908	317042.909924	44.438554
3501.587707	317024.809746	44.443559
3501.674940	316997.267049	44.448564
3501.537625	317006.473401	44.453569
3501.583154	316999.571323	44.458573
3501.522920	316992.355023	44.463578
3501.575712	316967.438300	44.468583
3501.813671	316956.638824	44.473588
3501.708236	316970.954205	44.478593
3501.669857	316942.693272	44.483597
3501.737993	316933.294252	44.488602
3501.473831	316924.201610	44.493607
3501.726787	316915.664192	44.498612
3501.703878	316902.666516	44.503617
3501.549526	316889.282300	44.508621
3501.686655	316880.508555	44.513626
3501.525936	316872.010359	44.518631
3501.484479	316866.470331	44.523636
3501.248000	316857.805876	44.528641
3501.537632	316841.299090	44.533645
3501.706988	316841.298092	44.538650
3501.516909	316839.216086	44.543655
3501.603738	316833.401569	44.548660
3501.208880	316818.070387	44.553665
3501.809642	316814.821582	44.558669
3501.527077	316807.665454	44.563674
3501.380607	316800.309946	44.568679
3501.121430	316796.941153	44.573684
3501.156711	316792.228735	44.578689
3501.177084	316771.998467	44.583693
3501.418886	316777.049285	44.588698
3501.135259	316770.274960	44.593703
3501.543769	316760.975348	44.598708
3501.500000	316760.931341	44.603713
3501.311685	316764.039413	44.608717
3501.231109	316758.276501	44.613722
3501.212021	316755.073713	44.618727
3501.397671	316734.690374	44.623732
3501.541414	316725.762906	44.628737
3501.375038	316716.375061	44.633741
3501.289282	316723.588860	44.638746
3501.161270	316711.574393	44.643751
3501.634472	316704.529078	44.648756
3501.267904	316700.617322	44.653761
3501.419464	316687.388763	44.658765
3501.427392	316678.100875	44.663770
3501.447428	316673.365385	44.668775
3501.572682	316667.417624	44.673780
3501.256467	316681.358964	44.678785
3501.176855	316672.797163	44.683789
3500.814598	316669.851563	44.688794
3500.931821	316666.016825	44.693799
3501.002482	316666.387459	44.698804
3501.119984	316671.584937	44.703809
3500.937679	316670.519427	44.708813
3500.733337	316673.426466	44.713818
3501.309499	316674.913891	44.718823
3501.586064	316671.461330	44.723828
3501.436085	316648.458911	44.728833
3501.423905	316631.439486	44.733837
3501.306645	316634.536458	44.738842
3501.334006	316630.842981	44.743847
3501.587803	316618.005507	44.748852
3501.262348	316619.913764	44.753857
3501.401066	316600.987953	44.758861
3501.114595	316598.157715	44.763866
3501.130566	316586.731336	44.768871
3501.126379	316584.238610	44.773876
3501.101544	316580.324302	44.778881
3501.272922	316589.355264	44.783885
3500.997222	316586.777771	44.788890
3501.286751	316587.037859	44.793895
3501.399166	316579.743614	44.798900
3501.007207	316581.280625	44.803905
3501.198466	316575.831394	44.808909
3500.697568	316584.280498	44.813914
3501.107783	316575.056910	44.818919
3501.301568	316582.863104	44.823924
3501.072242	316586.918992	44.828929
3501.444870	316575.284193	44.833933
3501.431941	316550.173967	44.838938
3501.174263	316549.908972	44.843943
3501.731816	316539.797279	44.848948
3501.285571	316544.421387	44.853953
3501.708226	316535.602935	44.858957
3501.655930	316525.586582	44.863962
3501.497879	316503.908389	44.868967
3501.625822	316496.942463	44.873972
3501.427204	316504.962677	44.878977
3501.674298	316492.456975	44.883981
3501.527366	316478.180968	44.888986
3501.448407	316476.157901	44.893991
3501.626604	316464.578913	44.898996
3501.365266	316459.429415	44.904001
3501.746905	316447.207982	44.909005
3501.637895	316435.546673	44.914010
3501.320033	316424.884851	44.919015
3501.497368	316415.901183	44.924020
3501.183983	316418.952503	44.929025
3501.295429	316419.698410	44.934029
3501.474395	316411.808541	44.939034
3501.390033	316404.901235	44.944039
3501.505345	316387.454694	44.949044
3501.007702	316378.932749	44.954049
3501.316804	316371.429618	44.959053
3501.644013	316371.302169	44.964058
3501.465669	316370.159703	44.969063
3501.519363	316349.542387	44.974068
3501.533172	316345.927335	44.979073
3501.466800	316339.653286	44.984077
3501.503192	316340.563587	44.989082
3501.341730	316331.810972	44.994087
3501.367113	316337.302765	44.999092
3501.145263	316315.074705	45.004097
3501.316482	316293.039615	45.009101
3501.361206	316290.361123	45.014106
3501.068927	316293.918015	45.019111
3501.678824	316282.856683	45.024116
3501.452462	316294.061672	45.029121
3501.595614	316288.060177	45.034125
3501.640962	316267.571345	45.039130
3501.422826	316254.476786	45.044135
3501.571611	316252.901525	45.049140
3501.551478	316261.377300	45.054145
3501.633583	316240.602833	45.059149
3501.639988	316238.719069	45.064154
3501.630046	316226.813228	45.069159
3501.638095	316219.026376	45.074164
3501.348333	316227.137219	45.079169
3501.559727	316203.213004	45.084173
3501.305951	316190.785523	45.089178
3501.321783	316183.124664	45.094183
3501.701828	316169.733016	45.099188
3501.616131	316185.546715	45.104193
3501.672441	316171.900360	45.109197
3501.730395	316165.428746	45.114202
3501.195134	316150.195615	45.119207
3501.562423	316140.520670	45.124212
3501.602310	316146.646301	45.129217
3501.762639	316113.265121	45.134221
3501.819311	316106.742813	45.139226
3501.631354	316106.517801	45.144231
3501.695912	316090.325802	45.149236
3501.024919	316072.823966	45.154241
3501.399980	316060.679787	45.159245
3501.510063	316057.176877	45.164250
3501.292386	316059.729834	45.169255
3501.533809	316046.359821	45.174260
3501.469623	316058.379145	45.179265
3501.434291	316035.358487	45.184269
3501.451452	316023.295694	45.189274
3501.231516	316025.136593	45.194279
3501.298383	316006.069104	45.199284
3501.316187	316014.513551	45.204289
3501.397449	316011.116917	45.209293
3501.284972	316017.724367	45.214298
3501.393302	315998.548619	45.219303
3501.665227	315972.121368	45.224308
3501.413364	315976.791475	45.229313
3501.608096	315967.881328	45.234317
3501.476686	315968.766984	45.239322
3501.521456	315958.150130	45.244327
3501.950341	315949.076156	45.249332
3501.486727	315941.362995	45.254337
3501.244413	315928.679215	45.259341
3501.440021	315937.197653	45.264346
3501.695504	315906.167679	45.269351
3501.456019	315899.157329	45.274356
3501.434125	315899.822317	45.279361
3501.455115	315889.692590	45.284365
3501.538697	315889.501456	45.289370
3501.426322	315882.827440	45.294375
3501.541540	315857.722236	45.299380
3501.391993	315863.495870	45.304385
3501.298835	315862.848941	45.309389
3501.360603	315854.850080	45.314394
3501.434268	315856.187102	45.319399
3501.515412	315852.154388	45.324404
3501.605109	315831.887414	45.329409
3501.563448	315813.676445	45.334413
3501.680614	315808.213262	45.339418
3501.591196	315800.085366	45.344423
3502.017115	315776.890690	45.349428
3501.872289	315773.224063	45.354433
3501.657020	315758.754962	45.359437
3501.882609	315742.181454	45.364442
3501.725016	315732.664811	45.369447
3501.634283	315719.321187	45.374452
3501.539344	315729.208151	45.379457
3501.395486	315697.451716	45.384461
3501.549304	315691.041378	45.389466
3501.601242	315690.498980	45.394471
3501.465333	315678.587244	45.399476
3501.265580	315688.007176	45.404481
3501.371715	315671.477760	45.409485
3501.578303	315661.522514	45.414490
3501.466039	315650.268606	45.419495
3501.462371	315652.839015	45.424500
3501.471284	315649.428221	45.429505
3501.604937	315640.629334	45.434509
3501.737002	315625.418912	45.439514
3501.577550	315612.645758	45.444519
3501.782239	315605.616808	45.449524
3501.487293	315592.712170	45.454529
3501.960527	315570.782170	45.459533
3501.703843	315575.503959	45.464538
3501.662374	315576.960764	45.469543
3501.534418	315552.631273	45.474548
3501.527013	315546.983984	45.479553
3501.488317	315539.407871	45.484557
3501.423043	315528.324692	45.489562
3501.302518	315532.719875	45.494567
3501.508769	315525.181796	45.499572
3501.773263	315506.642959	45.504577
3501.418718	315495.248785	45.509581
3501.517764	315498.998996	45.514586
3501.462583	315492.137875	45.519591
3501.863753	315480.956317	45.524596
3501.686313	315464.929145	45.529601
3501.758878	315457.132075	45.534605
3501.834937	315451.064627	45.539610
3501.689391	315427.043142	45.544615
3502.198231	315412.358949	45.549620
3501.588325	315406.933055	45.554625
3501.539517	315380.352052	45.559629
3501.656122	315369.036849	45.564634
3501.638468	315378.657370	45.569639
3501.709059	315364.347001	45.574644
3501.450221	315348.968607	45.579649
3501.268166	315339.557481	45.584653
3501.385220	315331.702546	45.589658
3501.437206	315333.679067	45.594663
3501.584440	315329.101656	45.599668
3501.565507	315322.972710	45.604673
3501.921368	315302.155012	45.609677
3501.557428	315298.217277	45.614682
3501.387783	315291.882895	45.619687
3501.819891	315287.693487	45.624692
3501.536821	315262.370339	45.629697
3501.699691	315259.647872	45.634701
3501.509330	315257.260510	45.639706
3501.919804	315255.364421	45.644711
3501.781832	315220.553477	45.649716
3501.598877	315213.814065	45.654721
3501.766915	315211.218006	45.659725
3501.631479	315195.743936	45.664730
3501.427874	315186.717804	45.669735
3501.919261	315171.196616	45.674740
3501.752824	315175.878894	45.679745
3501.728645	315155.832971	45.684749
3501.797114	315139.665463	45.689754
3501.630686	315136.485594	45.694759
3501.759829	315118.400304	45.699764
3501.416768	315109.319628	45.704769
3501.435622	315093.872289	45.709773
3501.354722	315087.015127	45.714778
3501.435962	315088.020218	45.719783
3501.383429	315082.837916	45.724788
3501.205346	315062.866901	45.729793
3501.552169	315052.278944	45.734797
3501.398614	315046.018344	45.739802
3501.275946	315039.880134	45.744807
3501.594181	315040.262964	45.749812
3501.196610	315035.592591	45.754817
3501.572365	315007.240251	45.759821
3501.823527	314956.084155	45.764826
3501.252844	314854.779160	45.769831
3501.225781	314698.404297	45.774836
3501.079864	314507.748711	45.779841
3501.086083	314270.861662	45.784845
3500.823455	313972.770556	45.789850
3500.176547	313635.120240	45.794855
3500.283651	313262.719091	45.799860
3499.807933	312824.172446	45.804865
3499.445606	312338.428208	45.809869
3499.231102	311817.693476	45.814874
3498.563726	311241.169886	45.819879
3498.176329	310628.614443	45.824884
3497.907068	309965.470179	45.829889
3497.220490	309255.635839	45.834893
3496.955453	308488.163144	45.839898
3495.980715	307672.972880	45.844903
3495.440323	306809.400427	45.849908
3494.436865	305913.947282	45.854913
3493.709081	304961.428936	45.859917
3493.189518	303958.597121	45.864922
3492.036362	302922.377916	45.869927
3491.715797	301828.413063	45.874932
3490.438808	300685.988767	45.879937
3489.469462	299494.904667	45.884941
3488.738222	298276.548900	45.889946
3487.314385	297004.263627	45.894951
3486.495755	295670.461260	45.899956
3485.381651	294313.103827	45.904961
3484.206300	292905.680723	45.909965
3483.525840	291438.556379	45.914970
3482.463124	289939.280515	45.919975
3481.224980	288388.192255	45.924980
3479.469790	286803.493155	45.929985
3478.215241	285171.988222	45.934989
3477.065800	283487.194132	45.939994
3475.298805	281783.310860	45.944999
3473.940485	280015.190533	45.950004
3472.227164	278224.118572	45.955009
3470.780297	276376.949360	45.960013
3469.045396	274505.390338	45.965018
3467.218106	272599.913492	45.970023
3465.835812	270635.964629	45.975028
3464.242858	268654.130657	45.980033
3462.333012	266628.099463	45.985037
3460.955710	264575.893481	45.990042
3458.764620	262466.707695	45.995047
3456.773338	260326.637181	46.000052
3454.581630	258156.992978	46.005057
3452.592952	255955.242688	46.010061
3450.537608	253720.461711	46.015066
3448.648106	251450.373732	46.020071
3446.866999	249149.191082	46.025076
3444.321230	246818.452641	46.030081
3442.269660	244444.032590	46.035085
3439.979860	242053.832938	46.040090
3437.401737	239625.197473	46.045095
3434.963985	237162.544074	46.050100
3432.202312	234686.501476	46.055105
3429.863814	232184.170932	46.060109
3427.484354	229642.766596	46.065114
3424.805687	227090.857773	46.070119
3422.523192	224491.689764	46.075124
3419.502958	221891.313811	46.080129
3416.966611	219251.212443	46.085133
3414.002838	216587.018043	46.090138
3410.814862	213919.231549	46.095143
3408.234217	211221.800773	46.100148
3404.785623	208510.191892	46.105153
3401.729231	205771.428310	46.110157
3398.809396	203024.554784	46.115162
3395.370214	200254.628194	46.120167
3392.512131	197464.742525	46.125172
3389.249504	194681.823207	46.130177
3385.633679	191855.496089	46.135181
3382.606588	189038.309373	46.140186
3378.757576	186215.388073	46.145191
3375.317935	183363.984863	46.150196
3372.201063	180520.507781	46.155201
3368.360265	177655.716733	46.160205
3364.329926	174786.162142	46.165210
3360.981819	171912.821508	46.170215
3357.113483	169037.645747	46.175220
3352.433735	166184.833568	46.180225
3348.444635	163316.591094	46.185229
3344.222167	160451.182499	46.190234
3339.603333	157596.784225	46.195239
3334.713830	154751.115442	46.200244
3330.074655	151918.909596	46.205249
3325.430746	149095.628948	46.210253
3320.499305	146296.566235	46.215258
3315.434163	143477.927886	46.220263
3310.066256	140667.906015	46.225268
3304.093950	137955.267007	46.230273
3297.954141	135261.207368	46.235277
3291.822279	132620.531852	46.240282
3284.838156	130018.614351	46.245287
3278.173069	127470.443701	46.250292
3271.275688	125001.792661	46.255297
3263.815762	122575.094769	46.260301
3256.756593	120212.768695	46.265306
3248.179371	117919.963867	46.270311
3240.437352	115709.641851	46.275316
3231.863869	113571.993709	46.280321
3223.525142	111540.929868	46.285325
3214.854565	109599.117973	46.290330
3206.076201	107744.056577	46.295335
3197.510088	105984.836352	46.300340
3188.386315	104338.471015	46.305345
3179.162519	102776.451482	46.310349
3170.360138	101327.830828	46.315354
3161.166041	99969.182937	46.320359
3152.549911	98709.127930	46.325364
3144.055302	97550.433200	46.330369
3136.236510	96470.989955	46.335373
3128.740260	95482.143349	46.340378
3121.187337	94570.689996	46.345383
3114.628784	93740.385607	46.350388
3107.767023	92974.182915	46.355393
3101.425873	92274.451713	46.360397
3095.689765	91633.130965	46.365402
3089.499471	91059.493246	46.370407
3084.124722	90512.790497	46.375412
3079.070985	90028.789926	46.380417
3074.551408	89557.711721	46.385421
3069.993519	89133.022621	46.390426
3065.859913	88728.729083	46.395431
3062.149000	88332.303073	46.400436
3057.755850	87973.494733	46.405441
3054.087592	87619.888096	46.410445
3050.554756	87280.786204	46.415450
3046.559689	86958.467245	46.420455
3043.368989	86640.548882	46.425460
3039.784383	86340.151522	46.430465
3036.639416	86024.887937	46.435469
3033.403067	85729.892564	46.440474
3029.842915	85433.108730	46.445479
3026.658304	85133.105920	46.450484
3023.358335	84845.688341	46.455489
3020.216798	84551.033145	46.460493
3017.098785	84254.636893	46.465498
3013.683873	83967.893925	46.470503
3010.420863	83672.186936	46.475508
3007.504277	83380.112746	46.480513
3003.643551	83072.488222	46.485517
3000.773649	82783.741029	46.490522
2996.907340	82488.407408	46.495527
2993.759340	82184.034565	46.500532
2989.782411	81888.533952	46.505537
2986.582096	81604.690088	46.510541
2983.191044	81313.854559	46.515546
2979.502404	81029.813403	46.520551
2975.987156	80729.438637	46.525556
2971.726060	80455.349569	46.530561
2968.079112	80164.832704	46.535565
2964.993007	79887.072478	46.540570
2961.298066	79624.118559	46.545575
2957.827532	79340.987662	46.550580
2954.206236	79073.543855	46.555585
2950.466411	78809.486963	46.560589
2946.903717	78532.005341	46.565594
2943.056894	78275.362267	46.570599
2939.867281	78015.049891	46.575604
2936.008906	77760.915471	46.580609
2932.359832	77501.137042	46.585613
2929.040390	77254.873552	46.590618
2925.252297	77001.370207	46.595623
2922.043124	76747.715176	46.600628
2917.885070	76496.598511	46.605633
2914.501317	76245.604370	46.610637
2910.935745	76007.290005	46.615642
2907.031788	75768.941757	46.620647
2903.457353	75518.200065	46.625652
2899.748199	75299.801957	46.630657
2896.609922	75062.432350	46.635661
2892.846227	74819.549569	46.640666
2889.027996	74592.907033	46.645671
2886.069929	74360.379215	46.650676
2882.546081	74130.837255	46.655681
2878.975962	73889.697770	46.660685
2875.600408	73666.168550	46.665690
2872.124171	73426.910670	46.670695
2868.933549	73198.645262	46.675700
2865.155252	72966.003890	46.680705
2861.532815	72735.410000	46.685709
2858.077189	72507.534830	46.690714
2854.634688	72280.459547	46.695719
2851.410020	72046.990472	46.700724
2847.719379	71824.719646	46.705729
2844.113528	71593.714091	46.710733
2841.072879	71353.048163	46.715738
2837.207149	71117.351227	46.720743
2833.823271	70886.660003	46.725748
2830.391783	70649.667710	46.730753
2826.875252	70423.915157	46.735757
2823.359552	70187.067200	46.740762
2819.737698	69956.789617	46.745767
2816.415679	69723.692920	46.750772
2812.816227	69493.155652	46.755777
2809.364977	69256.439401	46.760781
2806.162536	69032.065471	46.765786
2802.342673	68797.150489	46.770791
2799.251312	68555.807315	46.775796
2795.695810	68327.431921	46.780801
2792.270292	68084.126737	46.785805
2788.744286	67844.768952	46.790810
2785.140874	67607.494918	46.795815
2782.224450	67369.398327	46.800820
2778.840777	67140.124264	46.805825
2775.327940	66884.446906	46.810829
2771.799908	66645.386294	46.815834
2767.792549	66403.787685	46.820839
2764.481780	66161.181070	46.825844
2760.975031	65919.007313	46.830849
2757.459525	65671.892602	46.835853
2754.065739	65432.409823	46.840858
2750.390430	65202.963986	46.845863
2746.952646	64952.727621	46.850868
2743.718909	64718.240895	46.855873
2740.057548	64466.482922	46.860877
2736.617877	64227.317078	46.865882
2732.929730	63979.896860	46.870887
2729.408657	63724.919152	46.875892
2725.531665	63487.326645	46.880897
2722.080897	63248.273435	46.885901
2719.125622	63000.278619	46.890906
2715.433900	62757.174158	46.895911
2712.195027	62512.262271	46.900916
2708.487246	62269.406265	46.905921
2705.132215	62026.110328	46.910925
2701.822422	61779.262052	46.915930
2698.180828	61532.023891	46.920935
2694.670146	61280.915526	46.925940
2691.354263	61035.306823	46.930945
2687.853944	60787.146525	46.935949
2684.302047	60528.551105	46.940954
2680.945667	60293.097236	46.945959
2677.534512	60031.895853	46.950964
2673.985491	59781.798787	46.955969
2670.330164	59534.386168	46.960973
2667.058456	59275.874391	46.965978
2663.401327	59027.109207	46.970983
2659.842495	58765.018016	46.975988
2656.324001	58523.057886	46.980993
2652.587880	58268.195692	46.985997
2649.595934	58009.234838	46.991002
2645.576386	57772.969963	46.996007
2642.092533	57503.881739	47.001012
2638.659222	57265.747107	47.006017
2635.355285	57009.809022	47.011021
2632.080060	56750.360320	47.016026
2627.951517	56506.713839	47.021031
2624.889179	56249.559552	47.026036
2621.350578	56001.739767	47.031041
2618.028201	55742.899442	47.036045
2614.690111	55488.696080	47.041050
2610.712412	55233.466120	47.046055
2607.488231	54968.185317	47.051060
2604.038401	54713.075068	47.056065
2600.647972	54458.154954	47.061069
2597.123874	54196.501665	47.066074
2593.287736	53943.871028	47.071079
2589.764314	53681.557184	47.076084
2586.369040	53423.362658	47.081089
2582.700872	53158.393678	47.086093
2579.605645	52908.976261	47.091098
2575.801692	52657.280659	47.096103
2572.680141	52401.294010	47.101108
2569.152935	52142.068452	47.106113
2565.498664	51879.433644	47.111117
2562.182106	51617.751284	47.116122
2558.486259	51366.953509	47.121127
2555.092623	51104.375496	47.126132
2551.977931	50838.356688	47.131137
2547.853666	50578.157225	47.136141
2544.695697	50318.678585	47.141146
2540.761064	50058.588525	47.146151
2537.524727	49792.994067	47.151156
2534.103816	49535.804536	47.156161
2530.765208	49274.596167	47.161165
2527.204664	49004.158320	47.166170
2523.758735	48747.051318	47.171175
2520.540564	48482.541144	47.176180
2516.858680	48219.229247	47.181185
2513.203394	47953.163482	47.186189
2509.559478	47680.972036	47.191194
2506.258695	47414.755631	47.196199
2502.516395	47152.683307	47.201204
2499.087668	46881.539670	47.206209
2495.583241	46622.284031	47.211213
2492.002974	46347.453875	47.216218
2488.652762	46094.389276	47.221223
2485.302878	45826.474163	47.226228
2481.952231	45560.629873	47.231233
2477.880085	45287.525856	47.236237
2474.718967	45008.822266	47.241242
2471.103315	44755.218139	47.246247
2468.068103	44483.762801	47.251252
2464.326192	44209.339250	47.256257
2461.148580	43946.714983	47.261261
2457.561236	43656.064915	47.266266
2454.094250	43411.400722	47.271271
2450.528794	43126.220503	47.276276
2447.219020	42847.871583	47.281281
2443.567901	42574.728632	47.286285
2440.247545	42286.997082	47.291290
2436.257081	42027.369891	47.296295
2432.863885	41739.041806	47.301300
2429.860272	41478.391660	47.306305
2425.782089	41196.949932	47.311309
2422.518844	40913.501134	47.316314
2418.634361	40647.653419	47.321319
2415.309145	40369.179770	47.326324
2411.878871	40098.512250	47.331329
2408.543012	39827.250002	47.336333
2405.204206	39548.991853	47.341338
2401.780070	39272.468828	47.346343
2398.194075	38987.776790	47.351348
2394.509318	38708.302828	47.356353
2391.675278	38433.004267	47.361357
2387.879318	38148.641424	47.366362
2384.399422	37866.356739	47.371367
2380.928503	37579.674551	47.376372
2377.696317	37298.436328	47.381377
2374.291799	37013.970193	47.386381
2370.575796	36723.774921	47.391386
2366.751149	36444.295207	47.396391
2363.408807	36152.426342	47.401396
2359.931733	35873.597056	47.406401
2356.289723	35584.591142	47.411405
2352.849127	35287.221739	47.416410
2349.079037	35018.046901	47.421415
2345.768165	34724.937580	47.426420
2342.513690	34447.404359	47.431425
2339.059843	34160.556307	47.436429
2335.884207	33859.457339	47.441434
2332.066103	33571.704467	47.446439
2328.631209	33278.514204	47.451444
2325.233285	32986.025812	47.456449
2321.501263	32690.728849	47.461453
2318.093226	32400.519327	47.466458
2314.882470	32105.789232	47.471463
2311.284418	31802.022454	47.476468
2307.884402	31515.189487	47.481473
2304.615095	31220.493744	47.486477
2301.169608	30921.729201	47.491482
2297.662460	30612.977743	47.496487
2294.585067	30309.518915	47.501492
2290.845156	30012.974659	47.506497
2286.897668	29710.231131	47.511501
2283.869161	29392.081699	47.516506
2280.154476	29102.238798	47.521511
2277.191917	28791.452186	47.526516
2273.812693	28472.452971	47.531521
2269.839487	28163.792127	47.536525
2266.607560	27847.593203	47.541530
2262.928181	27533.275147	47.546535
2259.347300	27221.772668	47.551540
2256.154715	26912.565065	47.556545
2252.774464	26591.155855	47.561549
2249.118041	26275.193506	47.566554
2245.511853	25971.070671	47.571559
2242.137745	25644.245362	47.576564
2238.759792	25338.651697	47.581569
2235.079592	25021.831959	47.586573
2231.867349	24703.372706	47.591578
2228.158235	24387.479850	47.596583
2224.693723	24061.049195	47.601588
2221.508660	23743.139461	47.606593
2217.889081	23420.057013	47.611597
2214.388022	23092.608873	47.616602
2210.446278	22786.667176	47.621607
2207.275360	22454.793884	47.626612
2203.588686	22146.921587	47.631617
2199.794652	21824.418154	47.636621
2196.470596	21509.498925	47.641626
2192.901697	21197.270938	47.646631
2189.300354	20872.123979	47.651636
2185.236141	20574.432651	47.656641
2181.211284	20264.875270	47.661645
2177.776366	19967.531756	47.666650
2172.799759	19700.977714	47.671655
2168.270426	19441.926661	47.676660
2163.603857	19191.305854	47.681665
2159.067687	18960.632674	47.686669
2154.910778	18722.739205	47.691674
2150.789275	18513.339165	47.696679
2146.840812	18301.311119	47.701684
2142.984505	18109.880946	47.706689
2139.380053	17908.798740	47.711693
2136.225649	17717.205623	47.716698
2132.263400	17527.697866	47.721703
2129.130603	17332.938400	47.726708
2125.177265	17147.100073	47.731713
2122.045677	16969.191004	47.736717
2118.986711	16771.657969	47.741722
2115.526929	16589.408445	47.746727
2112.456794	16384.550401	47.751732
2109.100429	16196.518898	47.756737
2105.294823	16014.208609	47.761741
2101.807162	15810.289644	47.766746
2098.621272	15620.973678	47.771751
2095.294759	15435.158326	47.776756
2091.872434	15244.166873	47.781761
2088.477761	15058.144201	47.786765
2085.526260	14863.530219	47.791770
2081.907087	14656.753263	47.796775
2078.348148	14469.416354	47.801780
2075.166245	14269.851271	47.806785
2071.189862	14070.789368	47.811789
2068.215244	13870.132199	47.816794
2064.535832	13683.641921	47.821799
2060.959269	13467.702083	47.826804
2057.757644	13271.791592	47.831809
2054.178182	13065.355012	47.836813
2050.728809	12857.184356	47.841818
2047.190208	12657.980149	47.846823
2043.745245	12462.002146	47.851828
2040.151897	12264.374633	47.856833
2036.605410	12066.608895	47.861837
2033.430869	11853.660669	47.866842
2029.991364	11659.358558	47.871847
2026.401798	11452.070627	47.876852
2022.717566	11240.858460	47.881857
2019.340331	11039.629566	47.886861
2016.048701	10838.186835	47.891866
2012.549828	10646.421213	47.896871
2009.082241	10424.652297	47.901876
2005.569049	10221.971972	47.906881
2001.904748	10015.797428	47.911885
1998.651175	9810.630832	47.916890
1995.011903	9613.484806	47.921895
1991.318790	9406.498497	47.926900
1987.528410	9196.073110	47.931905
1984.117012	9000.357175	47.936909
1980.560290	8796.952161	47.941914
1976.803545	8601.851567	47.946919
1973.208353	8399.526804	47.951924
1970.492081	8205.888183	47.956929
1966.914153	7995.648928	47.961933
1963.531231	7792.132810	47.966938
1960.015884	7595.814970	47.971943
1956.979871	7393.723907	47.976948
1953.221892	7187.282157	47.981953
1949.431892	6976.261638	47.986957
1946.200969	6768.178606	47.991962
1942.658691	6567.093689	47.996967
1938.999854	6351.461174	48.001972
1935.595212	6149.963683	48.006977
1931.768452	5947.410947	48.011981
1928.692267	5732.267386	48.016986
1925.300096	5531.698874	48.021991
1921.729685	5330.119262	48.026996
1918.110830	5124.375236	48.032001
1914.216580	4913.492929	48.037005
1910.921897	4704.804095	48.042010
1907.135984	4502.368621	48.047015
1903.520475	4297.820139	48.052020
1900.259843	4095.756367	48.057025
1896.734262	3900.112723	48.062029
1893.184108	3694.940579	48.067034
1889.184706	3488.252531	48.072039
1886.159456	3299.685476	48.077044
1882.669447	3095.656223	48.082049
1878.950738	2896.079265	48.087053
1875.424024	2693.088708	48.092058
1872.046214	2511.457847	48.097063
1868.164056	2305.445322	48.102068
1864.500310	2114.070035	48.107073
1860.862236	1912.988388	48.112077
1857.564092	1716.905691	48.117082
1853.661039	1531.206159	48.122087
1850.016806	1340.247406	48.127092
1846.293719	1153.251696	48.132097
1842.862872	972.793251	48.137101
1839.051188	791.662195	48.142106
1835.412295	625.142138	48.147111
1831.787157	445.507243	48.152116
1828.297558	271.114412	48.157121
1823.658403	120.827913	48.162125
1817.975313	17.381435	48.167130
1808.051795	48.936705	48.172135
1801.487655	51.561704	48.177140
1796.426299	57.194425	48.182145
1792.755498	57.151980	48.187149
1790.646673	58.475470	48.192154
1788.413780	64.257187	48.197159
1785.424424	62.364848	48.202164
1783.054431	54.234649	48.207169
1779.430822	65.286596	48.212173
1776.121074	56.711835	48.217178
1772.622446	62.179101	48.222183
1769.544378	61.009342	48.227188
1766.325781	57.112234	48.232193
1762.347626	56.273166	48.237197
1759.244538	48.415894	48.242202
1755.598696	63.720305	48.247207
1752.475232	61.820490	48.252212
1749.123768	53.293399	48.257217
1745.597358	61.663060	48.262221
1742.209163	55.103274	48.267226
1738.383428	63.136962	48.272231
1735.057858	60.737264	48.277236
1732.150026	61.935869	48.282241
1728.194802	55.430027	48.287245
1725.134299	51.989091	48.292250
1721.663950	59.644457	48.297255
1718.488043	56.525307	48.302260
1714.730470	52.658785	48.307265
1710.933421	51.854669	48.312269
1707.630458	51.343394	48.317274
1704.081366	63.728311	48.322279
1700.954308	52.866038	48.327284
1697.489819	47.020575	48.332289
1693.923872	51.565078	48.337293
1690.589953	54.769786	48.342298
1686.958736	60.950699	48.347303
1683.058190	52.639284	48.352308
1680.312970	47.095716	48.357313
1676.432413	49.158427	48.362317
1673.421696	53.926092	48.367322
1669.485765	56.434075	48.372327
1666.176981	60.688401	48.377332
1662.242788	56.109212	48.382337
1659.002529	56.989700	48.387341
1655.550025	49.313704	48.392346
1652.317028	51.860377	48.397351
1648.564508	50.233058	48.402356
1645.660132	40.911532	48.407361
1642.019003	51.656197	48.412365
1638.566435	58.065431	48.417370
1634.567732	60.497829	48.422375
1630.969876	49.857969	48.427380
1628.312326	44.376628	48.432385
1624.704343	52.483835	48.437389
1621.152690	46.503346	48.442394
1617.160679	41.841480	48.447399
1613.599114	49.036579	48.452404
1610.319107	46.753183	48.457409
1606.892278	51.535369	48.462413
1603.578862	50.658764	48.467418
1599.716810	51.845399	48.472423
1596.551337	54.501745	48.477428
1593.129819	52.575864	48.482433
1589.125515	56.318966	48.487437
1585.902958	50.002240	48.492442
1582.587714	48.278032	48.497447
1579.097391	54.054105	48.502452
1575.511391	55.751206	48.507457
1572.195321	52.562294	48.512461
1568.630961	45.321463	48.517466
1565.190335	55.778501	48.522471
1561.824005	58.478949	48.527476
1558.182436	52.351204	48.532481
1554.381059	50.007059	48.537485
1551.329163	50.924538	48.542490
1547.689403	57.091010	48.547495
1543.931652	58.093660	48.552500
1540.861865	59.713140	48.557505
1537.404195	56.846963	48.562509
1533.631809	54.264167	48.567514
1529.911555	59.769357	48.572519
1526.487192	53.240627	48.577524
1522.902245	47.334992	48.582529
1519.311440	54.996610	48.587533
1516.355442	44.692944	48.592538
1512.843614	58.619163	48.597543
1509.397841	47.148787	48.602548
1505.542768	45.262325	48.607553
1501.895552	43.802080	48.612557
1498.429399	44.980570	48.617562
1495.170796	60.101036	48.622567
1491.357976	49.327205	48.627572
1488.300892	43.082696	48.632577
1484.489442	48.810981	48.637581
1481.041575	55.861773	48.642586
1477.654820	57.303092	48.647591
1473.900170	56.834119	48.652596
1470.665628	48.776065	48.657601
1467.252776	58.314446	48.662605
1464.196680	52.110917	48.667610
1460.630185	52.042774	48.672615
1456.731532	53.731906	48.677620
1453.451507	56.507465	48.682625
1449.695202	59.806835	48.687629
1446.303558	50.064934	48.692634
1442.681167	57.582821	48.697639
1438.979622	58.744392	48.702644
1435.613554	55.148898	48.707649
1431.926693	51.787119	48.712653
1428.788613	41.942264	48.717658
1424.862249	51.959670	48.722663
1421.498899	45.120875	48.727668
1418.626027	51.705188	48.732673
1414.870218	45.804196	48.737677
1411.176411	61.831207	48.742682
1407.723721	53.829469	48.747687
1404.568766	52.602256	48.752692
1401.120971	52.718036	48.757697
1396.967934	50.470129	48.762701
1393.411900	55.123907	48.767706
1389.926440	55.039941	48.772711
1386.735452	49.661158	48.777716
1383.363641	51.948063	48.782721
1380.145122	53.967362	48.787725
1376.588907	47.924410	48.792730
1372.463076	49.623825	48.797735
1368.976748	50.701112	48.802740
1365.686002	41.519265	48.807745
1362.171121	48.188268	48.812749
1358.804535	44.289162	48.817754
1355.480686	52.484848	48.822759
1351.556540	57.009599	48.827764
1348.438287	48.370236	48.832769
1344.450912	57.163343	48.837773
1341.355929	42.303503	48.842778
1337.608776	49.973828	48.847783
1333.956145	48.106365	48.852788
1330.557483	48.072108	48.857793
1327.233245	45.033262	48.862797
1323.927941	43.472104	48.867802
1320.243664	48.908451	48.872807
1316.391248	49.729849	48.877812
1312.954208	46.847872	48.882817
1309.574080	45.801474	48.887821
1306.299607	46.095801	48.892826
1303.075184	51.586719	48.897831
1299.453754	50.207936	48.902836
1295.974061	53.024290	48.907841
1292.242379	52.121517	48.912845
1288.665600	43.300856	48.917850
1285.107529	53.232178	48.922855
1281.348712	47.081776	48.927860
1278.370140	39.271636	48.932865
1274.616807	37.489565	48.937869
1271.620032	42.147579	48.942874
1267.869594	48.619366	48.947879
1264.128387	48.834911	48.952884
1260.409218	44.336134	48.957889
1257.056151	43.503819	48.962893
1254.026551	36.752054	48.967898
1250.222353	47.525513	48.972903
1246.752496	41.842425	48.977908
1243.320678	32.176513	48.982913
1239.577458	41.206675	48.987917
1236.218817	43.162531	48.992922
1232.414418	43.802436	48.997927
1229.025132	44.367865	49.002932
1225.777937	36.239128	49.007937
1222.291396	42.356401	49.012941
1218.861636	39.318296	49.017946
1215.418474	45.963459	49.022951
1211.691475	33.062931	49.027956
1207.929135	46.171045	49.032961
1204.345970	42.337542	49.037965
1201.117940	39.761412	49.042970
1197.563945	41.172057	49.047975
1194.173194	39.374383	49.052980
1190.825199	35.336390	49.057985
1187.580824	49.081601	49.062989
1183.637796	40.571428	49.067994
1180.008457	43.351136	49.072999
1176.508620	48.344200	49.078004
1173.466314	35.387117	49.083009
1169.553386	58.133551	49.088013
1166.055825	35.674141	49.093018
1162.477532	42.542957	49.098023
1158.681870	41.412969	49.103028
1155.805379	40.278287	49.108033
1152.112356	41.761334	49.113037
1148.506278	38.785662	49.118042
1144.945111	46.487040	49.123047
1141.621448	50.130074	49.128052
1138.454535	40.188611	49.133057
1134.573058	53.081283	49.138061
1131.210878	43.214685	49.143066
1127.783151	49.547409	49.148071
1123.972910	43.996754	49.153076
1120.503234	41.439503	49.158081
1117.018916	53.213298	49.163085
1113.480656	44.639786	49.168090
1110.252333	46.426584	49.173095
1106.876246	44.515914	49.178100
1102.792167	40.469809	49.183105
1099.182093	48.118747	49.188109
1096.249587	45.297068	49.193114
1092.528113	50.745642	49.198119
1089.271713	50.790437	49.203124
1085.984929	40.222352	49.208129
1082.251652	47.694430	49.213133
1078.640335	42.201238	49.218138
1075.106681	45.149501	49.223143
1071.373454	50.343656	49.228148
1067.955404	42.377773	49.233153
1063.737952	36.248657	49.238157
1061.104832	36.796995	49.243162
1058.217139	39.330913	49.248167
1053.984981	44.078002	49.253172
1050.594436	36.379907	49.258177
1047.037503	41.233253	49.263181
1043.687650	41.080722	49.268186
1040.124114	47.760604	49.273191
1036.075105	37.432107	49.278196
1033.010250	34.656483	49.283201
1029.662176	33.136929	49.288205
1025.957645	50.652674	49.293210
1022.450540	44.118125	49.298215
1019.190257	39.569751	49.303220
1016.074653	31.616652	49.308225
1011.660387	42.045934	49.313229
1008.562518	29.423496	49.318234
1004.944285	46.878274	49.323239
1001.607355	42.088804	49.328244
998.149984	37.669374	49.333249
994.299082	41.752511	49.338253
991.164525	35.463370	49.343258
987.605604	42.101415	49.348263
983.833232	40.610345	49.353268
980.310713	39.697093	49.358273
977.049701	44.437689	49.363277
973.545581	34.084022	49.368282
969.836963	54.099804	49.373287
966.584632	44.833014	49.378292
963.407522	34.573683	49.383297
959.422644	48.861998	49.388301
955.943078	41.231664	49.393306
952.100069	47.939514	49.398311
949.012190	39.564479	49.403316
945.608504	34.171715	49.408321
941.922940	38.377680	49.413325
938.858469	37.294645	49.418330
934.851630	45.277843	49.423335
931.309268	45.762940	49.428340
928.062221	32.350803	49.433345
924.586282	37.495228	49.438349
921.002532	40.657033	49.443354
917.477597	33.457768	49.448359
913.620151	39.971736	49.453364
910.635081	40.584715	49.458369
906.773902	41.062794	49.463373
903.140956	50.752845	49.468378
899.805003	45.697504	49.473383
896.236132	46.237385	49.478388
893.109568	37.805156	49.483393
889.473541	40.820133	49.488397
885.941084	39.025780	49.493402
882.657366	41.501536	49.498407
879.037978	41.302684	49.503412
875.358427	41.110090	49.508417
871.746127	41.628306	49.513421
868.589818	39.686475	49.518426
864.812662	38.503090	49.523431
861.311726	36.488675	49.528436
857.980243	37.662118	49.533441
854.300369	38.893279	49.538445
850.943433	39.808117	49.543450
847.329163	44.509156	49.548455
843.418418	34.529272	49.553460
840.431948	21.557273	49.558465
836.942850	35.435784	49.563469
833.538828	25.734068	49.568474
829.675437	32.771016	49.573479
826.166246	31.947485	49.578484
823.283450	28.691007	49.583489
819.831858	34.176503	49.588493
816.134070	35.881886	49.593498
812.478346	37.027024	49.598503
808.591698	40.220481	49.603508
805.287501	42.133155	49.608513
801.622243	39.739532	49.613517
798.088979	36.882315	49.618522
794.931468	34.959681	49.623527
791.049978	40.781429	49.628532
787.713827	32.581382	49.633537
784.189574	32.839071	49.638541
780.933612	38.205361	49.643546
777.316353	31.226262	49.648551
773.807606	26.210692	49.653556
770.604969	31.255420	49.658561
766.652555	30.684818	49.663565
763.298012	35.370521	49.668570
759.744514	38.451715	49.673575
756.251910	36.812525	49.678580
752.914875	31.985209	49.683585
749.287554	31.540876	49.688589
745.914139	41.671220	49.693594
742.259568	34.935261	49.698599
738.857127	29.630973	49.703604
735.325393	26.602700	49.708609
731.649023	35.271372	49.713613
728.343659	32.413295	49.718618
724.842886	31.243635	49.723623
721.364636	32.221809	49.728628
718.196419	34.388464	49.733633
713.889853	36.486617	49.738637
710.302143	35.191370	49.743642
707.238105	37.604307	49.748647
703.520117	34.276182	49.753652
700.409667	29.793055	49.758657
696.966753	41.762952	49.763661
693.499645	27.455244	49.768666
689.613465	28.804199	49.773671
686.122921	27.892380	49.778676
682.620931	27.646746	49.783681
679.192929	37.918533	49.788685
675.662715	35.276024	49.793690
671.960171	36.200757	49.798695
668.434584	35.307088	49.803700
665.349801	27.868164	49.808705
661.797103	34.593922	49.813709
658.308984	29.388507	49.818714
655.283440	30.124965	49.823719
651.194894	37.013740	49.828724
647.733816	31.813586	49.833729
644.338792	39.647285	49.838733
640.598312	34.693371	49.843738
637.107512	38.609515	49.848743
633.754819	40.131208	49.853748
630.253287	29.448267	49.858753
626.246210	34.482983	49.863757
622.952709	36.144107	49.868762
619.873441	32.852028	49.873767
616.015266	39.954676	49.878772
613.141788	39.025339	49.883777
609.338791	49.884230	49.888781
605.634216	33.522503	49.893786
602.114469	35.358272	49.898791
598.296961	36.357987	49.903796
595.066755	28.565378	49.908801
591.396481	38.220236	49.913805
588.132820	35.064615	49.918810
584.750573	33.145617	49.923815
581.393663	31.788966	49.928820
577.699855	35.328799	49.933825
573.784415	36.631765	49.938829
570.364545	38.508851	49.943834
567.363695	29.506577	49.948839
563.731934	35.327260	49.953844
560.108626	27.814533	49.958849
556.720393	42.056975	49.963853
553.450137	33.919476	49.968858
549.614613	33.333825	49.973863
545.871433	44.692731	49.978868
542.471173	36.455374	49.983873
538.848018	45.527067	49.988877
535.191401	43.284063	49.993882
531.650024	40.662343	49.998887
528.609604	31.897235	50.003892
524.963255	33.762354	50.008897
521.283911	42.064567	50.013901
518.221616	28.633180	50.018906
514.907689	41.278950	50.023911
510.941418	35.110774	50.028916
507.883785	40.591618	50.033921
503.827456	40.496152	50.038925
500.672698	36.067495	50.043930
496.922983	45.836069	50.048935
493.287254	43.314564	50.053940
490.439277	42.855836	50.058945
486.291747	52.218490	50.063949
483.229963	35.000011	50.068954
479.467029	37.101707	50.073959
475.799955	38.030454	50.078964
472.778692	38.842230	50.083969
468.884761	38.889023	50.088973
465.283484	36.979067	50.093978
461.954456	38.478132	50.098983
458.605412	41.486283	50.103988
455.141083	32.208635	50.108993
451.506114	32.300295	50.113997
448.166420	37.357099	50.119002
444.711552	39.793371	50.124007
440.879168	34.834960	50.129012
437.528584	29.842216	50.134017
433.542979	30.292525	50.139021
430.544004	24.536031	50.144026
427.367388	39.798888	50.149031
423.407031	38.239424	50.154036
420.146844	35.462976	50.159041
416.415647	40.258411	50.164045
412.600720	30.684522	50.169050
409.617206	36.710606	50.174055
406.228793	35.494998	50.179060
402.398854	28.878416	50.184065
398.766815	36.021651	50.189069
395.377938	35.897616	50.194074
391.799985	37.049718	50.199079
388.257114	39.831990	50.204084
385.209926	31.485618	50.209089
381.601237	41.273267	50.214093
377.625541	42.003623	50.219098
374.378318	44.442196	50.224103
370.892593	47.705906	50.229108
367.617653	39.509108	50.234113
363.545335	45.050861	50.239117
360.187103	39.784097	50.244122
357.103159	41.472600	50.249127
353.565922	40.258178	50.254132
350.341405	30.911377	50.259137
346.331700	37.012803	50.264141
342.850842	39.057713	50.269146
339.278420	35.801859	50.274151
335.648098	39.078740	50.279156
332.573983	42.480467	50.284161
328.598329	42.131997	50.289165
325.278729	43.392353	50.294170
321.943513	33.101122	50.299175
318.159441	37.170886	50.304180
315.041979	31.088145	50.309185
311.384264	50.381091	50.314189
308.225634	34.845170	50.319194
304.398217	39.064098	50.324199
300.763270	36.169231	50.329204
297.227368	28.124081	50.334209
293.377242	35.089543	50.339213
290.232829	38.888273	50.344218
287.070408	31.195908	50.349223
283.116005	39.965232	50.354228
280.115473	22.458861	50.359233
276.556425	37.012866	50.364237
272.845015	33.054314	50.369242
269.612280	37.686298	50.374247
265.858762	33.939989	50.379252
262.598632	34.843039	50.384257
258.574672	35.777161	50.389261
255.478969	39.128510	50.394266
252.053131	34.527282	50.399271
248.250588	34.531381	50.404276
244.653562	29.732348	50.409281
240.993449	34.820433	50.414285
237.255702	37.949665	50.419290
234.273445	43.849053	50.424295
230.810651	38.662001	50.429300
227.283860	36.822735	50.434305
223.276015	41.082616	50.439309
220.223226	31.984217	50.444314
217.081200	26.955731	50.449319
213.284267	45.197995	50.454324
209.672096	41.552954	50.459329
206.126407	45.484178	50.464333
202.817661	33.954992	50.469338
199.472298	39.613881	50.474343
195.735149	45.084213	50.479348
192.578292	39.007691	50.484353
189.099199	41.767391	50.489357
185.214425	38.101793	50.494362
181.497663	42.572354	50.499367
177.786069	40.923411	50.504372
175.069466	34.736798	50.509377
171.263287	33.903106	50.514381
167.654061	42.874662	50.519386
164.181744	37.910593	50.524391
160.222734	41.207398	50.529396
157.094975	36.176698	50.534401
153.769899	39.279277	50.539405
150.113757	34.087751	50.544410
146.606132	39.515815	50.549415
143.171900	34.143994	50.554420
139.865787	34.946724	50.559425
136.198973	34.486683	50.564429
132.718945	41.153782	50.569434
128.966655	37.711063	50.574439
125.349543	38.113270	50.579444
122.254380	39.091766	50.584449
118.560885	36.528855	50.589453
115.241304	49.257879	50.594458
111.837971	41.701404	50.599463
108.398746	44.347322	50.604468
105.325606	36.963747	50.609473
101.093348	47.140250	50.614477
97.523841	37.363555	50.619482
94.015604	28.795312	50.624487
90.306632	31.708122	50.629492
86.688545	39.371300	50.634497
83.428558	43.909541	50.639501
80.414098	31.790144	50.644506
76.814360	37.618640	50.649511
73.020700	35.131554	50.654516
69.618214	35.737440	50.659521
65.847829	38.609263	50.664525
62.663406	34.742248	50.669530
59.094293	34.608616	50.674535
55.628006	43.788769	50.679540
52.176212	41.029830	50.684545
48.983789	41.624958	50.689549
45.206738	32.725530	50.694554
41.654362	38.103695	50.699559
38.177939	35.633359	50.704564
34.688155	40.951101	50.709569
31.036611	39.884435	50.714573
27.555850	36.411876	50.719578
24.286112	35.051276	50.724583
19.877539	43.154707	50.729588
16.953228	42.050035	50.734593
13.288087	47.869823	50.739597
10.119529	43.788370	50.744602
6.703942	38.568711	50.749607
2.711728	36.824610	50.754612