Thu Aug 25 10:34:09 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.086318	107.733602	0.000000
1.152895	102.885824	0.005005
0.719254	92.105287	0.010010
0.966519	89.456485	0.015014
0.681486	84.015233	0.020019
0.627940	86.019988	0.025024
0.385950	89.133110	0.030029
0.344629	67.974119	0.035034
0.311139	70.766668	0.040038
-0.212667	62.816015	0.045043
-0.581548	54.420313	0.050048
-0.637984	50.430216	0.055053
-0.916293	40.536532	0.060058
-1.334632	20.575619	0.065062
-1.830007	19.792735	0.070067
-2.233626	21.567596	0.075072
-2.419848	14.858042	0.080077
-2.400511	20.125843	0.085082
-2.552177	11.107672	0.090086
-3.034118	7.016576	0.095091
-3.216158	8.218883	0.100096
-3.219055	0.142349	0.105101
-3.756662	0.327859	0.110106
-3.692138	-0.846469	0.115110
-4.636625	-4.814470	0.120115
-5.151449	-9.289549	0.125120
-5.440405	-7.510510	0.130125
-5.499869	-1.157862	0.135130
-5.697360	-8.662904	0.140134
-5.480444	-8.440591	0.145139
-5.301397	-7.203113	0.150144
-6.224248	-4.755280	0.155149
-7.021962	-4.842225	0.160154
-7.067994	-4.800174	0.165158
-7.167615	3.074197	0.170163
-7.437765	-3.204586	0.175168
-7.518709	-1.638471	0.180173
-7.326970	-8.448365	0.185178
-7.787048	-16.630428	0.190182
-8.542858	-0.095339	0.195187
-8.510118	5.341199	0.200192
-8.521426	1.669907	0.205197
-8.787550	-7.947249	0.210202
-9.586315	-8.695250	0.215206
-9.861671	-6.269775	0.220211
-9.823575	4.942908	0.225216
-10.117590	0.797059	0.230221
-10.061142	2.281536	0.235226
-9.819766	-5.744684	0.240230
-11.312006	-5.023622	0.245235
-11.187884	-7.210192	0.250240
-11.353021	-1.688869	0.255245
-11.678742	-3.653098	0.260250
-11.691569	-8.997766	0.265254
-11.710219	5.653299	0.270259
-12.392161	-3.905035	0.275264
-12.997155	1.574477	0.280269
-13.032013	-7.240524	0.285274
-12.805142	-4.248338	0.290278
-13.061061	1.277719	0.295283
-13.366854	1.857177	0.300288
-13.859597	-5.838884	0.305293
-13.980050	-6.395774	0.310298
-14.327609	-0.001150	0.315302
-14.380837	2.019365	0.320307
-14.689871	6.085771	0.325312
-15.121825	9.775970	0.330317
-15.724088	3.814975	0.335322
-15.681879	-1.766107	0.340326
-15.949411	-1.480544	0.345331
-16.202099	1.017310	0.350336
-16.151836	-6.327236	0.355341
-16.343572	0.160031	0.360346
-16.788761	3.564403	0.365350
-17.380003	5.118726	0.370355
-17.438107	-8.156667	0.375360
-17.587247	-9.354464	0.380365
-17.568998	13.712692	0.385370
-17.909868	2.139397	0.390374
-18.408126	9.778840	0.395379
-18.431707	-2.318728	0.400384
-18.577122	-1.008265	0.405389
-18.813487	2.464626	0.410394
-19.522831	-8.974998	0.415398
-20.205662	2.353804	0.420403
-19.903566	-3.710921	0.425408
-20.077714	3.469613	0.430413
-19.835423	1.615701	0.435418
-19.772114	-4.095236	0.440422
-20.843942	0.672815	0.445427
-21.084912	2.014068	0.450432
-21.068742	-1.588762	0.455437
-21.360235	1.566902	0.460442
-22.114421	-1.526085	0.465446
-23.004479	-5.410862	0.470451
-23.069838	5.998363	0.475456
-22.218628	-5.246019	0.480461
-22.932436	-1.951419	0.485466
-22.698853	-5.449109	0.490470
-22.958376	-1.358825	0.495475
-23.312029	-0.408038	0.500480
-23.790501	-8.761226	0.505485
-24.151413	-6.135686	0.510490
-24.542763	-11.354605	0.515494
-25.010650	-8.009954	0.520499
-24.658014	-6.625670	0.525504
-24.596973	-10.694270	0.530509
-25.346039	-1.414684	0.535514
-25.386917	-3.749407	0.540518
-25.959910	7.710883	0.545523
-25.807373	-0.693722	0.550528
-26.555254	-4.800092	0.555533
-27.058585	-0.244502	0.560538
-27.348353	-0.521763	0.565542
-27.405174	2.805938	0.570547
-27.331237	-4.899819	0.575552
-27.332577	5.642002	0.580557
-27.608864	-1.901314	0.585562
-27.750177	-5.998320	0.590566
-28.384868	-5.149031	0.595571
-28.998649	-4.473859	0.600576
-29.052727	-15.623844	0.605581
-29.153791	-0.238542	0.610586
-29.078661	-7.014346	0.615590
-29.338759	-7.321566	0.620595
-29.615013	-10.856429	0.625600
-29.941658	-7.163751	0.630605
-30.590005	-9.922144	0.635610
-30.359657	-7.610707	0.640614
-30.821275	-5.643263	0.645619
-31.189199	-6.949148	0.650624
-31.380939	-1.173722	0.655629
-31.940032	0.182576	0.660634
-31.712649	-4.317047	0.665638
-32.032922	-8.651766	0.670643
-32.113859	-5.472147	0.675648
-32.976966	-10.072986	0.680653
-33.390241	-2.019760	0.685658
-33.454145	-4.217998	0.690662
-33.063653	-5.146010	0.695667
-33.202190	-0.017994	0.700672
-33.193197	-9.178383	0.705677
-34.502349	-2.300900	0.710682
-34.682209	-3.686871	0.715686
-34.774454	2.734187	0.720691
-34.901512	-4.386422	0.725696
-34.700317	-9.824734	0.730701
-35.152254	-3.970575	0.735706
-36.056679	-7.685421	0.740710
-35.977243	-9.482177	0.745715
-36.181043	-10.513223	0.750720
-36.544717	-8.415593	0.755725
-36.504797	-3.647733	0.760730
-36.271513	-11.932107	0.765734
-37.012731	-6.804574	0.770739
-38.020324	-6.039223	0.775744
-38.068173	-10.160364	0.780749
-38.367003	-4.697188	0.785754
-38.109710	-13.159330	0.790758
-38.097279	-10.892842	0.795763
-38.077371	-6.561606	0.800768
-38.668708	-1.046270	0.805773
-39.038788	-4.110854	0.810778
-39.357901	-11.381701	0.815782
-39.506007	-3.911023	0.820787
-39.850147	1.410558	0.825792
-40.134218	-10.114678	0.830797
-40.917976	-11.070670	0.835802
-40.705018	-10.398487	0.840806
-41.096485	-0.330215	0.845811
-40.869058	-4.083203	0.850816
-40.748750	-5.424458	0.855821
-41.489871	6.929038	0.860826
-41.977342	-4.206829	0.865830
-42.319734	4.904636	0.870835
-42.342671	-7.079132	0.875840
-42.554567	1.138693	0.880845
-43.499274	-0.611488	0.885850
-43.001496	-6.684727	0.890854
-43.434196	-0.624774	0.895859
-43.422147	-1.022092	0.900864
-43.573194	-2.004456	0.905869
-43.712819	-1.533290	0.910874
-44.815824	-1.252859	0.915878
-45.160412	8.301875	0.920883
-45.268244	5.341730	0.925888
-44.872812	0.480419	0.930893
-45.499249	6.450508	0.935898
-45.244969	6.135457	0.940902
-45.722586	3.568610	0.945907
-46.285630	4.884399	0.950912
-46.387595	5.817897	0.955917
-46.388201	-1.271906	0.960922
-46.526366	2.919586	0.965926
-46.899372	2.740788	0.970931
-47.948884	-0.853249	0.975936
-48.326483	-3.935637	0.980941
-48.453156	1.677735	0.985946
-48.239646	-5.619621	0.990950
-48.583974	-0.854828	0.995955
-48.586377	5.283236	1.000960
-48.446837	-10.449706	1.005965
-48.676520	-9.350666	1.010970
-49.034798	-7.079876	1.015974
-49.862164	-4.874789	1.020979
-49.953535	0.454642	1.025984
-49.935548	-0.364383	1.030989
-50.352640	5.012922	1.035994
-50.850143	-2.068625	1.040998
-51.185929	0.714331	1.046003
-51.033246	-3.311682	1.051008
-51.124542	-8.941445	1.056013
-51.518225	-1.033657	1.061018
-51.965100	-13.359115	1.066022
-52.566479	-6.083170	1.071027
-53.066706	-2.996040	1.076032
-52.915654	-6.116969	1.081037
-53.173967	-5.649352	1.086042
-52.882720	-15.379143	1.091046
-53.040109	-10.941035	1.096051
-53.202459	-9.529843	1.101056
-53.517273	-11.438830	1.106061
-54.156622	-0.993199	1.111066
-53.977233	-10.806704	1.116070
-54.787653	0.896426	1.121075
-55.194618	-11.068293	1.126080
-55.500785	-16.993414	1.131085
-55.540462	-7.053033	1.136090
-55.619160	-8.011931	1.141094
-55.287068	-1.293534	1.146099
-56.138645	2.509870	1.151104
-56.503734	-0.299233	1.156109
-56.627176	-7.774744	1.161114
-56.941042	-7.070634	1.166118
-56.871425	-7.442171	1.171123
-57.363642	-4.834020	1.176128
-57.950834	-9.737515	1.181133
-58.507620	-7.808942	1.186138
-58.507737	-8.061985	1.191142
-58.665906	0.406847	1.196147
-58.643090	0.950636	1.201152
-58.517535	-7.054270	1.206157
-58.946900	-4.917873	1.211162
-59.008881	-8.271175	1.216166
-59.992136	-0.723421	1.221171
-59.978149	-0.716084	1.226176
-60.501066	-16.104776	1.231181
-60.513048	-5.042445	1.236186
-60.461521	-9.264577	1.241190
-60.407209	-4.179436	1.246195
-61.427609	-5.702620	1.251200
-61.251001	-17.031115	1.256205
-61.520945	-1.306147	1.261210
-61.753756	-10.292604	1.266214
-62.634490	-9.123188	1.271219
-63.187295	-6.780788	1.276224
-62.787759	-4.726815	1.281229
-63.302336	4.639417	1.286234
-63.234283	1.933288	1.291238
-63.060880	-8.233619	1.296243
-63.433991	-3.214382	1.301248
-63.409639	-11.738099	1.306253
-64.115045	-2.357788	1.311258
-64.524925	-12.303585	1.316262
-64.699522	-8.748626	1.321267
-64.768755	-8.509952	1.326272
-65.019852	-1.785597	1.331277
-65.671056	-0.516104	1.336282
-65.874434	-11.316829	1.341286
-66.261359	-1.989584	1.346291
-66.297861	-6.207415	1.351296
-65.991213	-2.898703	1.356301
-66.423798	-0.176509	1.361306
-66.604931	-9.765846	1.366310
-67.328137	5.270853	1.371315
-67.504919	-4.028105	1.376320
-67.382102	-6.568809	1.381325
-68.038968	-7.978113	1.386330
-68.469840	-12.311317	1.391334
-68.738718	8.472304	1.396339
-68.863595	-7.782352	1.401344
-68.493152	-5.571961	1.406349
-68.902853	-2.372466	1.411354
-69.385315	-13.967849	1.416358
-70.240750	-6.174372	1.421363
-70.293445	-4.868947	1.426368
-70.436608	-3.062130	1.431373
-70.669980	-6.837827	1.436378
-70.508721	-1.399286	1.441382
-70.495229	0.879691	1.446387
-70.890918	-9.808644	1.451392
-71.670006	-7.225146	1.456397
-72.055671	-1.036523	1.461402
-71.880693	-3.667658	1.466406
-72.008328	-7.121402	1.471411
-72.029088	-4.080926	1.476416
-72.491917	0.401880	1.481421
-73.271463	5.092500	1.486426
-73.257444	-1.385828	1.491430
-73.249310	-0.804938	1.496435
-73.766755	3.436492	1.501440
-74.075477	-0.419148	1.506445
-74.878196	2.579341	1.511450
-74.617066	9.356315	1.516454
-74.625980	0.904244	1.521459
-75.236554	9.804633	1.526464
-75.054392	-6.773378	1.531469
-75.345656	1.225929	1.536474
-75.284942	5.376767	1.541478
-75.885248	0.915086	1.546483
-76.072464	7.468083	1.551488
-76.273419	-8.796796	1.556493
-76.690333	2.869987	1.561498
-77.248160	-1.142772	1.566502
-78.222263	-5.719886	1.571507
-77.382041	3.025939	1.576512
-77.398795	-12.005469	1.581517
-78.041496	5.945070	1.586522
-78.141122	-3.435579	1.591526
-78.111063	-1.330040	1.596531
-78.904836	2.002403	1.601536
-79.121954	-11.251227	1.606541
-79.470977	6.118624	1.611546
-79.342188	9.062903	1.616550
-79.360889	-0.681602	1.621555
-79.620620	-2.229063	1.626560
-79.963394	-2.706823	1.631565
-80.468123	6.319347	1.636570
-80.709413	5.990199	1.641574
-80.657329	-2.139236	1.646579
-81.350310	2.316359	1.651584
-81.602101	-3.762816	1.656589
-82.358665	5.549586	1.661594
-82.449106	1.238967	1.666598
-82.181343	-6.984372	1.671603
-82.252188	-2.224467	1.676608
-82.337722	-6.289082	1.681613
-82.909320	2.826657	1.686618
-83.493143	-1.916014	1.691622
-83.690529	-5.077257	1.696627
-83.841265	2.906359	1.701632
-83.868959	-0.835128	1.706637
-83.635299	-5.063653	1.711642
-84.009462	-8.133921	1.716646
-84.895010	-5.688762	1.721651
-85.148418	-6.063467	1.726656
-85.345885	-9.806824	1.731661
-85.606714	4.126045	1.736666
-85.836000	-5.322870	1.741670
-86.543909	-7.572055	1.746675
-86.920930	-0.097146	1.751680
-86.187842	-4.562114	1.756685
-87.013666	3.014757	1.761690
-87.167033	-2.459747	1.766694
-86.866761	1.334015	1.771699
-87.303126	4.433286	1.776704
-87.234308	-0.354701	1.781709
-88.075732	3.010519	1.786714
-88.311393	1.288445	1.791718
-88.113902	-2.203590	1.796723
-88.429965	-4.172491	1.801728
-89.275831	0.382990	1.806733
-89.818871	-7.874652	1.811738
-89.944161	2.088637	1.816742
-89.813275	-0.994331	1.821747
-90.424895	-1.784303	1.826752
-90.022395	-2.885040	1.831757
-90.394195	-6.588425	1.836762
-90.125492	6.400936	1.841766
-90.837698	-4.130237	1.846771
-91.335160	7.966782	1.851776
-91.015227	3.243849	1.856781
-91.869807	4.491428	1.861786
-92.203619	3.790802	1.866790
-92.621161	5.330566	1.871795
-92.787295	4.746035	1.876800
-92.883098	-1.458821	1.881805
-92.893131	10.093590	1.886810
-92.853809	3.728354	1.891814
-92.785379	3.885347	1.896819
-93.831426	-1.851075	1.901824
-94.095989	4.486252	1.906829
-94.424754	4.506167	1.911834
-94.182953	-3.510625	1.916838
-94.732337	-5.044336	1.921843
-95.523940	4.574111	1.926848
-95.583204	-5.793618	1.931853
-95.667686	7.845867	1.936858
-95.599138	-6.145385	1.941862
-95.596283	4.671016	1.946867
-96.076383	7.856235	1.951872
-96.843895	0.978352	1.956877
-97.112658	-0.112115	1.961882
-97.033376	-5.398447	1.966886
-97.066866	-0.112888	1.971891
-97.273081	-2.921573	1.976896
-97.371390	-3.466112	1.981901
-98.155504	-2.169463	1.986906
-98.369786	-10.029367	1.991910
-98.857292	-0.256094	1.996915
-98.808476	-0.149106	2.006912
-98.839098	-1.918193	2.016909
-98.461457	-1.011118	2.026906
-97.465893	-2.640063	2.036902
-96.607422	6.893580	2.046899
-96.060184	-0.313280	2.056896
-96.248095	-0.255251	2.066893
-96.149131	-0.090119	2.076890
-95.155359	-1.753629	2.086886
-94.375825	3.031199	2.096883
-93.443956	4.332935	2.106880
-93.859599	2.345412	2.116877
-93.495647	5.899735	2.126874
-92.520372	0.650021	2.136870
-91.784414	5.390993	2.146867
-91.855369	9.070484	2.156864
-91.134479	9.559480	2.166861
-90.581563	9.992434	2.176858
-89.789199	0.083055	2.186854
-89.426348	-3.467795	2.196851
-89.230870	1.361034	2.206848
-88.979167	-5.970576	2.216845
-88.158638	-0.514265	2.226842
-86.831308	-4.786443	2.236838
-86.896943	0.248025	2.246835
-86.684073	-2.164264	2.256832
-86.257640	6.426554	2.266829
-85.637572	-1.409435	2.276826
-85.181405	-2.456517	2.286822
-84.350247	-0.011268	2.296819
-83.829331	-6.045087	2.306816
-83.730074	-0.988940	2.316813
-82.953908	-11.554674	2.326810
-82.611660	0.090406	2.336806
-81.997206	-4.209452	2.346803
-80.930110	-2.789522	2.356800
-81.127144	-10.874441	2.366797
-80.931825	-6.995924	2.376794
-79.965578	-1.027090	2.386790
-79.195915	-4.663858	2.396787
-79.370722	-3.201386	2.406784
-78.544367	-4.065721	2.416781
-78.057236	-4.214835	2.426778
-77.416056	-9.003550	2.436774
-76.918127	-10.278920	2.446771
-76.878917	-5.026465	2.456768
-75.812306	-3.223156	2.466765
-75.443740	-1.326309	2.476762
-75.037092	-2.299107	2.486758
-74.003813	-11.067812	2.496755
-73.782025	-9.749846	2.506752
-73.797489	-5.090703	2.516749
-73.499952	-14.146432	2.526746
-72.304481	-8.242026	2.536742
-71.873958	-12.373679	2.546739
-71.107825	-9.420899	2.556736
-70.837375	-7.907819	2.566733
-71.103688	-7.222955	2.576730
-69.762313	-7.629464	2.586726
-69.316963	-11.614554	2.596723
-69.281563	-3.881126	2.606720
-68.532493	-8.895821	2.616717
-68.404776	-5.985557	2.626714
-67.272096	-14.706479	2.636710
-66.982633	-12.309399	2.646707
-66.436341	-5.989660	2.656704
-65.813373	-5.032326	2.666701
-65.530112	-6.942462	2.676698
-65.080639	-10.902856	2.686694
-64.370285	-4.998461	2.696691
-64.201340	-6.418685	2.706688
-63.208430	-7.096874	2.716685
-62.504234	-4.723595	2.726682
-62.501772	-8.268659	2.736678
-62.549837	-11.599900	2.746675
-61.402662	-4.446151	2.756672
-61.229560	-8.496289	2.766669
-60.246987	-7.436911	2.776666
-59.948485	1.230973	2.786662
-59.398612	-4.715518	2.796659
-58.455241	-2.176976	2.806656
-58.179796	-1.722718	2.816653
-58.009401	-8.281319	2.826650
-57.809532	-4.989554	2.836646
-56.935156	-7.188713	2.846643
-56.718808	-3.310322	2.856640
-55.766623	-3.798397	2.866637
-55.335992	4.680893	2.876634
-55.093039	-8.531928	2.886630
-54.242364	-3.492149	2.896627
-53.810914	-9.182499	2.906624
-53.567655	-11.536192	2.916621
-53.157160	-9.392491	2.926618
-52.285197	-9.082385	2.936614
-52.124030	-10.571081	2.946611
-51.120168	-12.879226	2.956608
-50.701931	-3.168896	2.966605
-50.731045	-2.289950	2.976602
-49.733928	-14.562895	2.986598
-49.168750	-1.977064	2.996595
-48.970693	-11.653933	3.006592
-48.947679	-5.933275	3.016589
-47.813991	-4.650486	3.026586
-47.413267	-8.555725	3.036582
-46.681330	-4.853154	3.046579
-46.346893	-13.357135	3.056576
-46.264984	-8.716417	3.066573
-45.416969	-5.028866	3.076570
-45.079865	-4.286497	3.086566
-44.401715	-4.988224	3.096563
-43.822435	-6.856044	3.106560
-43.620063	-2.430602	3.116557
-42.419120	-5.916367	3.126554
-41.958983	-5.909195	3.136550
-41.971535	-10.614485	3.146547
-41.866026	-6.550833	3.156544
-40.921635	-5.985981	3.166541
-40.316217	-8.234862	3.176538
-40.195534	-10.832276	3.186534
-39.146799	-9.732577	3.196531
-38.728777	-7.685088	3.206528
-38.561820	-8.192677	3.216525
-37.788474	-5.358231	3.226522
-37.365899	-10.372451	3.236518
-36.891476	-2.153446	3.246515
-35.981882	-10.826743	3.256512
-36.199625	-9.097785	3.266509
-35.721872	-14.605321	3.276506
-34.880680	-11.325345	3.286502
-34.452629	-8.310084	3.296499
-33.583898	-4.793670	3.306496
-33.308627	-10.671790	3.316493
-33.017226	-7.115600	3.326490
-32.305953	-13.207753	3.336486
-31.933180	-6.372984	3.346483
-31.560969	-8.810238	3.356480
-30.594576	-7.453717	3.366477
-29.940667	-4.584716	3.376474
-29.788110	-3.072169	3.386470
-29.703875	-1.140271	3.396467
-29.073172	-7.802674	3.406464
-28.579645	-2.592891	3.416461
-27.653649	-0.048455	3.426458
-26.945560	-6.054581	3.436454
-26.848369	1.479104	3.446451
-26.479073	-6.041994	3.456448
-25.672608	-3.858963	3.466445
-25.290869	-0.674887	3.476442
-25.186216	1.795504	3.486438
-24.360947	-3.392687	3.496435
-23.863198	-1.886708	3.506432
-23.245461	-4.980152	3.516429
-22.814155	-2.098446	3.526426
-22.922962	-1.438262	3.536422
-21.773378	-2.378579	3.546419
-21.096111	-1.790877	3.556416
-21.385984	-10.288906	3.566413
-20.188163	-4.571757	3.576410
-19.450202	-4.240651	3.586406
-19.677306	-4.407732	3.596403
-18.828157	-6.504734	3.606400
-18.312039	0.846103	3.616397
-17.446694	2.063238	3.626394
-17.281444	-2.603390	3.636390
-16.859868	-4.243761	3.646387
-16.611061	-3.557247	3.656384
-15.635765	-0.025848	3.666381
-15.435942	4.732614	3.676378
-15.132672	-2.318811	3.686374
-14.338720	-2.240397	3.696371
-13.693157	-6.792214	3.706368
-13.464116	-3.653903	3.716365
-12.707309	-4.304597	3.726362
-12.429995	-3.812617	3.736358
-11.711824	-5.002116	3.746355
-11.120698	1.364459	3.756352
-11.013963	-4.493592	3.766349
-10.299237	3.146075	3.776346
-9.718393	-7.002587	3.786342
-9.471739	-10.139256	3.796339
-8.837596	-7.254485	3.806336
-7.870949	-6.069062	3.816333
-7.828216	-5.473803	3.826330
-7.757984	-1.135360	3.836326
-7.259280	-3.491064	3.846323
-6.057958	1.297380	3.856320
-5.538065	-0.333053	3.866317
-5.668073	1.008360	3.876314
-4.884437	10.436539	3.886310
-4.488796	18.056517	3.896307
-4.338370	18.083707	3.906304
-3.475303	21.518656	3.916301
-2.896205	34.412783	3.926298
-2.617810	43.920143	3.936294
-2.031799	52.213560	3.946291
-1.745471	63.436634	3.956288
-1.558230	78.381569	3.966285
-0.974511	91.050100	3.976282
-0.365376	109.489572	3.986278
0.000000	124.356585	3.991283
0.101051	130.212730	3.996288
-0.078794	150.783259	4.001293
0.513801	149.722335	4.006298
0.570585	154.395848	4.011302
0.908224	169.275963	4.016307
0.957786	160.770355	4.021312
0.976131	163.741459	4.026317
0.925352	172.418177	4.031322
0.753581	174.270622	4.036326
1.055000	167.377038	4.041331
1.039009	168.572321	4.046336
0.708814	176.372164	4.051341
1.025452	168.802311	4.056346
0.895574	185.578022	4.061350
1.279379	176.431575	4.066355
1.071721	176.185737	4.071360
0.752696	177.703749	4.076365
1.173148	171.702678	4.081370
1.232570	180.308349	4.086374
0.856856	171.011988	4.091379
1.088366	172.465887	4.096384
0.909869	183.060882	4.101389
0.971338	176.650981	4.106394
1.060456	177.253990	4.111398
0.914033	173.160906	4.116403
1.118225	184.714675	4.121408
1.177012	190.735650	4.126413
1.508836	198.618438	4.131418
1.376723	203.163372	4.136422
1.269806	182.580839	4.141427
1.270706	174.405554	4.146432
0.928474	174.800900	4.151437
1.589789	189.402526	4.156442
1.071925	196.969189	4.161446
1.268213	186.431584	4.166451
1.658791	195.858577	4.171456
1.189237	190.525298	4.176461
1.588548	188.909358	4.181466
1.368120	186.795732	4.186470
1.183708	186.093832	4.191475
1.297232	194.412621	4.196480
1.654020	193.265255	4.201485
1.910861	195.234045	4.206490
1.333403	182.166433	4.211494
0.991080	180.815392	4.216499
1.480853	195.693839	4.221504
1.478416	201.901582	4.226509
1.812442	200.669196	4.231514
1.652877	197.808872	4.236518
1.433865	180.872753	4.241523
1.407035	188.757948	4.246528
0.960055	195.019521	4.251533
1.678962	197.001336	4.256538
1.544892	198.822567	4.261542
1.367114	199.840719	4.266547
1.921931	200.044894	4.271552
1.666885	189.226824	4.276557
1.690603	199.650940	4.281562
1.726798	200.537491	4.286566
1.800523	201.307429	4.291571
1.762640	196.181761	4.296576
1.831813	199.632128	4.301581
1.761303	180.749167	4.306586
0.955917	186.089288	4.311590
1.354521	188.883756	4.316595
1.497282	201.681033	4.321600
1.688617	203.618959	4.326605
1.636394	199.125129	4.331610
1.699238	200.671896	4.336614
1.594532	208.857205	4.341619
1.881657	203.788180	4.346624
1.587886	205.542684	4.351629
1.826211	201.291233	4.356634
1.714415	215.947574	4.361638
1.984037	203.275575	4.366643
1.840661	204.437036	4.371648
1.662919	205.597553	4.376653
1.847836	195.748264	4.381658
1.503788	202.129754	4.386662
1.596381	212.055864	4.391667
1.807141	210.902903	4.396672
2.015499	222.263054	4.401677
2.224767	224.524041	4.406682
1.886086	222.523852	4.411686
1.803164	211.764222	4.416691
2.045647	223.394275	4.421696
2.046187	229.212416	4.426701
2.473423	210.934811	4.431706
1.923600	208.328623	4.436710
1.618041	201.966729	4.441715
1.961097	208.158306	4.446720
2.036049	226.385773	4.451725
2.307380	217.576470	4.456730
2.018515	215.084418	4.461734
2.136437	207.754493	4.466739
2.083218	203.539230	4.471744
1.929213	216.322903	4.476749
2.332522	221.701446	4.481754
2.006576	221.853794	4.486758
1.659819	229.583488	4.491763
1.794197	227.670531	4.496768
2.063961	231.630481	4.501773
2.120610	226.512140	4.506778
1.948788	228.892949	4.511782
1.956996	232.008023	4.516787
2.433281	226.760656	4.521792
2.219421	229.068959	4.526797
2.270925	221.819038	4.531802
2.120884	233.741555	4.536806
2.127991	239.273930	4.541811
2.008497	230.570149	4.546816
2.166353	227.736017	4.551821
2.389521	236.028155	4.556826
2.338686	234.324553	4.561830
2.059424	233.824175	4.566835
2.521439	229.923650	4.571840
1.880283	232.048964	4.576845
2.412303	236.309512	4.581850
2.716626	257.443388	4.586854
2.306151	241.865999	4.591859
2.408656	239.461321	4.596864
2.302891	246.552144	4.601869
2.514070	242.421997	4.606874
2.559138	258.752746	4.611878
2.461084	252.133693	4.616883
2.353561	238.331178	4.621888
2.652570	248.680552	4.626893
2.911307	239.367006	4.631898
2.599571	242.573340	4.636902
2.317562	238.786225	4.641907
2.321308	240.763038	4.646912
2.309751	236.731066	4.651917
2.765420	242.098247	4.656922
2.619718	238.273956	4.661926
2.487699	246.482543	4.666931
2.364016	250.652842	4.671936
2.421263	249.049363	4.676941
2.819284	251.302927	4.681946
3.013713	260.760688	4.686950
2.690560	250.399345	4.691955
2.436565	238.546524	4.696960
2.891007	251.506975	4.701965
2.848578	246.695220	4.706970
2.773446	246.479237	4.711974
2.448095	238.374023	4.716979
2.584244	243.196476	4.721984
2.955726	252.278476	4.726989
3.031628	240.772601	4.731994
2.693648	244.220330	4.736998
2.593232	239.541050	4.742003
2.399506	247.616937	4.747008
2.821791	250.376067	4.752013
2.974981	252.380087	4.757018
3.240916	259.931538	4.762022
2.651556	241.968209	4.767027
2.870339	246.182925	4.772032
2.573978	253.113788	4.777037
2.963049	254.853057	4.782042
2.708784	268.807258	4.787046
2.783033	263.176779	4.792051
2.746448	263.163566	4.797056
2.674271	268.170529	4.802061
3.073057	261.400859	4.807066
3.068146	262.062897	4.812070
3.154482	255.383314	4.817075
3.554112	255.491580	4.822080
3.301049	253.765877	4.827085
2.646890	245.060439	4.832090
2.503189	245.158922	4.837094
2.611324	255.690068	4.842099
2.952201	257.035088	4.847104
3.146447	266.644742	4.852109
3.178762	256.449166	4.857114
3.090137	268.871453	4.862118
2.798625	263.962677	4.867123
3.012386	255.095936	4.872128
2.829415	269.282579	4.877133
2.890979	258.402205	4.882138
2.796962	270.689295	4.887142
2.465288	261.740330	4.892147
2.634085	275.995249	4.897152
2.965938	284.896811	4.902157
3.123970	288.137118	4.907162
3.059317	295.439821	4.912166
3.163182	286.033456	4.917171
3.111328	288.509374	4.922176
3.050007	297.070744	4.927181
2.811435	292.701001	4.932186
2.852257	291.185514	4.937190
3.019887	287.220369	4.942195
3.282688	303.611958	4.947200
3.336968	306.441412	4.952205
3.659146	303.432824	4.957210
3.447835	300.425566	4.962214
3.097407	291.080887	4.967219
3.517668	298.535407	4.972224
3.227157	284.982993	4.977229
3.494144	286.364903	4.982234
3.303176	284.211848	4.987238
3.193271	294.441817	4.992243
3.588703	296.952059	4.997248
3.125757	300.447854	5.002253
3.812351	305.405545	5.007258
3.562908	306.501372	5.012262
3.567781	297.015599	5.017267
3.432864	286.608923	5.022272
2.921612	297.214994	5.027277
3.468845	302.960157	5.032282
3.462245	310.427779	5.037286
3.778142	319.338185	5.042291
3.854342	318.370817	5.047296
3.404328	307.991353	5.052301
3.695887	294.917214	5.057306
3.311126	303.279325	5.062310
3.337056	309.922427	5.067315
3.480001	313.788370	5.072320
3.677600	311.767421	5.077325
3.628181	310.228106	5.082330
3.595257	319.594969	5.087334
3.590484	321.693350	5.092339
3.760939	322.144413	5.097344
3.640855	317.401754	5.102349
3.640278	317.961873	5.107354
3.682548	320.831177	5.112358
3.384637	319.938244	5.117363
3.664251	321.118860	5.122368
3.634614	323.910844	5.127373
3.970372	313.012786	5.132378
3.613018	310.882633	5.137382
3.813785	311.733912	5.142387
3.475594	320.740476	5.147392
3.482831	317.661007	5.152397
3.971970	317.119327	5.157402
3.882416	325.403556	5.162406
3.913508	325.148782	5.167411
3.569033	317.815330	5.172416
3.729892	321.827166	5.177421
4.016090	313.265427	5.182426
3.838120	314.236159	5.187430
3.615730	312.616377	5.192435
3.999169	307.851776	5.197440
3.655894	319.744514	5.202445
4.144024	307.303964	5.207450
3.873539	326.072881	5.212454
3.560414	316.421783	5.217459
4.432598	327.918440	5.222464
4.030041	325.830169	5.227469
3.928741	315.209399	5.232474
4.021182	323.300595	5.237478
3.744948	319.094936	5.242483
3.941230	337.480679	5.247488
3.972558	344.676613	5.252493
4.418278	340.186987	5.257498
4.134242	332.739654	5.262502
3.785568	327.808179	5.267507
4.303244	324.367154	5.272512
4.284898	330.058572	5.277517
3.845782	325.932216	5.282522
4.056365	327.493812	5.287526
4.115993	342.325881	5.292531
4.163790	341.850187	5.297536
3.551341	346.932332	5.302541
4.083149	338.566219	5.307546
3.963222	346.570475	5.312550
4.423980	352.259600	5.317555
4.255931	344.949115	5.322560
4.224552	349.513105	5.327565
4.611098	346.032509	5.332570
4.540358	349.663017	5.337574
4.342634	349.241611	5.342579
4.366833	344.786390	5.347584
4.007493	349.838370	5.352589
4.487588	344.688450	5.357594
4.647678	347.241901	5.362598
4.209915	345.975404	5.367603
4.346596	349.095679	5.372608
4.242214	345.495848	5.377613
4.255566	342.820383	5.382618
4.303234	347.742151	5.387622
4.365584	345.353241	5.392627
4.567716	346.688370	5.397632
4.243840	347.403550	5.402637
4.514460	351.157747	5.407642
4.329789	352.252919	5.412646
4.217525	345.145668	5.417651
4.005403	345.258036	5.422656
4.398914	356.965755	5.427661
4.008634	348.952923	5.432666
4.015289	351.321604	5.437670
4.348623	362.617969	5.442675
4.692504	367.809712	5.447680
4.449122	379.050914	5.452685
5.092458	374.391110	5.457690
4.489773	358.226792	5.462694
4.176538	357.358405	5.467699
4.558515	368.368739	5.472704
4.744637	374.316040	5.477709
4.867264	373.211679	5.482714
4.853863	368.370032	5.487718
4.514381	360.896573	5.492723
4.719381	359.494564	5.497728
4.399831	365.903912	5.502733
4.728631	376.204399	5.507738
4.480619	382.574070	5.512742
4.454671	377.345238	5.517747
4.684971	367.953822	5.522752
4.684655	372.699615	5.527757
4.323408	368.931214	5.532762
4.490634	369.417586	5.537766
4.496354	374.940729	5.542771
4.821270	369.457606	5.547776
4.821253	377.031794	5.552781
4.953477	373.863128	5.557786
4.696819	377.823333	5.562790
4.677136	373.770457	5.567795
4.921722	372.849470	5.572800
4.795405	372.435858	5.577805
4.992785	377.922645	5.582810
4.972202	376.524342	5.587814
4.543967	380.182394	5.592819
5.017897	370.664218	5.597824
4.565681	378.388353	5.602829
4.955000	373.002707	5.607834
5.031466	382.210092	5.612838
4.837939	380.032115	5.617843
5.033618	375.644933	5.622848
4.895227	386.746302	5.627853
5.065163	396.587629	5.632858
5.075627	395.621065	5.637862
5.148032	386.184775	5.642867
5.085961	380.613584	5.647872
4.814280	385.711951	5.652877
5.136543	396.456407	5.657882
4.872591	391.236388	5.662886
4.980032	396.522133	5.667891
5.659179	397.330101	5.672896
5.113321	388.487398	5.677901
5.115596	377.132179	5.682906
5.149470	384.375188	5.687910
4.837317	382.627092	5.692915
5.530449	393.364059	5.697920
5.203444	390.912760	5.702925
5.058823	379.783038	5.707930
5.113125	380.859753	5.712934
5.123244	392.573781	5.717939
5.252814	392.357361	5.722944
5.036105	400.569797	5.727949
5.481964	392.166505	5.732954
5.125586	398.568980	5.737958
5.175341	400.817017	5.742963
5.277801	400.861113	5.747968
5.392719	414.532953	5.752973
5.228305	402.735590	5.757978
5.335694	404.699347	5.762982
5.108019	407.648926	5.767987
5.111748	398.954230	5.772992
5.158494	411.500941	5.777997
5.189486	404.165573	5.783002
5.067017	402.906620	5.788006
5.469082	411.430242	5.793011
5.233717	399.140953	5.798016
5.243051	404.287046	5.803021
5.526621	402.486738	5.808026
5.343833	394.460358	5.813030
5.258069	407.154380	5.818035
5.385073	405.005274	5.823040
5.104825	411.392661	5.828045
5.871646	421.643528	5.833050
5.903015	419.550534	5.838054
5.319285	409.365970	5.843059
5.743749	402.854820	5.848064
5.221171	401.626919	5.853069
5.345892	403.828409	5.858074
5.580207	411.460810	5.863078
5.568824	432.562100	5.868083
5.617828	427.745461	5.873088
5.635612	426.913793	5.878093
5.712948	421.105606	5.883098
5.466177	421.134817	5.888102
5.110863	428.195208	5.893107
5.575968	415.131756	5.898112
5.601853	431.500471	5.903117
5.949056	431.980793	5.908122
5.544090	423.783562	5.913126
5.509386	427.930469	5.918131
5.872534	419.217415	5.923136
5.349843	426.993742	5.928141
5.971704	417.325810	5.933146
6.226440	431.225697	5.938150
5.861369	429.745320	5.943155
5.786243	433.582180	5.948160
5.926057	429.368257	5.953165
5.426218	428.269671	5.958170
5.848032	426.416063	5.963174
5.902611	426.723930	5.968179
5.833954	421.049352	5.973184
5.593505	431.559287	5.978189
5.795404	420.302479	5.983194
5.637574	428.951801	5.988198
5.816182	437.083332	5.993203
5.702708	427.682472	5.998208
6.123009	433.567791	6.003213
5.913613	428.010176	6.008218
6.059786	430.562656	6.013222
5.659348	433.438066	6.018227
5.953037	425.745148	6.023232
5.951946	421.338164	6.028237
5.701842	424.819617	6.033242
5.719695	422.779361	6.038246
5.750362	437.935593	6.043251
5.946205	423.158405	6.048256
5.479719	433.722740	6.053261
5.985496	424.326098	6.058266
5.999402	427.180880	6.063270
5.675723	430.708664	6.068275
6.117593	431.784769	6.073280
5.923069	429.885358	6.078285
5.844812	425.424024	6.083290
5.850934	420.079421	6.088294
5.730727	422.218047	6.093299
5.663636	424.117393	6.098304
6.120309	437.770506	6.103309
5.984575	438.845361	6.108314
6.095187	442.501258	6.113318
6.071141	436.038223	6.118323
5.990152	432.757418	6.123328
5.558306	433.141499	6.128333
5.881025	439.548319	6.133338
6.069095	440.746450	6.138342
6.081098	437.985759	6.143347
6.207315	433.343686	6.148352
5.946958	433.349715	6.153357
6.023125	427.525891	6.158362
6.085780	433.736171	6.163366
6.030168	437.516189	6.168371
6.058993	433.015928	6.173376
5.702465	443.357392	6.178381
5.803666	436.071124	6.183386
5.948510	428.221189	6.188390
5.686805	433.707155	6.193395
6.401081	423.360340	6.198400
5.855348	428.182112	6.203405
6.230286	423.940842	6.208410
5.926811	432.454795	6.213414
5.668778	431.454366	6.218419
5.807795	429.262245	6.223424
5.831130	434.456774	6.228429
6.052185	436.706451	6.233434
6.182663	434.677022	6.238438
5.821579	434.645047	6.243443
6.024580	433.600857	6.248448
5.772616	433.096196	6.253453
6.069871	425.339444	6.258458
6.388946	437.109499	6.263462
5.702287	448.417035	6.268467
5.976994	428.584362	6.273472
5.597814	439.049597	6.278477
6.045434	435.477157	6.283482
6.010798	438.203502	6.288486
5.855687	437.348302	6.293491
5.919390	429.900229	6.298496
6.013011	433.704322	6.303501
6.105909	435.531144	6.308506
5.981686	435.851207	6.313510
5.809238	431.983607	6.318515
6.435106	421.799344	6.323520
5.867482	419.012412	6.328525
5.701571	407.424092	6.333530
5.546013	407.891436	6.338534
5.472513	422.393247	6.343539
5.773003	427.009664	6.348544
5.877305	427.224318	6.353549
5.794518	430.325209	6.358554
6.245605	434.807299	6.363558
5.729438	430.177290	6.368563
6.463024	428.746241	6.373568
6.112380	432.670563	6.378573
6.178223	420.729541	6.383578
6.073910	415.275691	6.388582
5.702056	403.381114	6.393587
5.586887	411.074600	6.398592
5.651155	419.840982	6.403597
5.906277	427.827640	6.408602
5.932743	428.475277	6.413606
5.942410	441.521374	6.418611
6.057085	430.841385	6.423616
6.112118	436.878850	6.428621
6.052223	422.031000	6.433626
6.066420	406.317324	6.438630
5.933809	412.922029	6.443635
5.977206	404.974102	6.448640
5.805025	416.631286	6.453645
5.981617	404.596992	6.458650
5.671339	417.297725	6.463654
5.464766	412.945085	6.468659
5.820421	416.648006	6.473664
5.959948	431.208198	6.478669
6.028312	432.425084	6.483674
6.188872	428.900785	6.488678
6.127457	426.085159	6.493683
5.802451	409.143283	6.498688
6.030983	419.133633	6.503693
5.744040	405.719775	6.508698
5.762761	405.584000	6.513702
5.769183	407.133298	6.518707
5.662718	401.701935	6.523712
5.708403	412.303071	6.528717
6.013498	424.410672	6.533722
6.187858	430.116221	6.538726
5.762497	433.802309	6.543731
5.805356	420.934727	6.548736
6.082628	426.592513	6.553741
6.063525	429.942859	6.558746
5.887589	407.355530	6.563750
5.395624	418.129496	6.568755
6.348475	426.762984	6.573760
6.055012	418.893141	6.578765
5.897856	404.139639	6.583770
5.976642	417.488107	6.588774
6.009818	409.639857	6.593779
5.775157	405.361224	6.598784
5.810287	401.527547	6.603789
6.038139	406.455902	6.608794
5.813404	399.885116	6.613798
5.728689	410.266232	6.618803
5.917350	403.643329	6.623808
5.933508	407.775934	6.628813
5.834003	400.843836	6.633818
5.876621	397.879034	6.638822
5.901976	401.605229	6.643827
5.927959	404.075295	6.648832
5.593188	411.800025	6.653837
5.831775	421.595808	6.658842
6.255437	424.614183	6.663846
5.881424	426.672352	6.668851
6.016239	407.187494	6.673856
5.485085	413.902101	6.678861
5.830272	427.835270	6.683866
6.257887	432.798773	6.688870
5.743398	425.238810	6.693875
6.090807	417.812730	6.698880
5.620379	419.344992	6.703885
5.827587	436.868568	6.708890
6.107060	433.626200	6.713894
6.160719	428.707590	6.718899
5.893266	411.000543	6.723904
5.866822	401.196912	6.728909
5.641430	407.502935	6.733914
6.117599	409.143150	6.738918
5.603545	419.129625	6.743923
6.165485	414.748323	6.748928
5.870878	419.872439	6.753933
5.777696	413.784082	6.758938
5.790598	409.868463	6.763942
5.671769	419.530417	6.768947
5.954068	427.123669	6.773952
6.263820	429.062049	6.778957
6.038954	429.603529	6.783962
5.533960	419.757806	6.788966
5.520923	423.395107	6.793971
5.920919	424.708731	6.798976
6.001141	432.830366	6.803981
6.067139	434.066605	6.808986
6.088665	433.031866	6.813990
6.012344	442.041754	6.818995
5.880712	416.710771	6.824000
5.751547	429.699516	6.829005
5.860076	434.096071	6.834010
6.112205	436.078282	6.839014
5.466391	435.717589	6.844019
6.216366	425.703707	6.849024
5.847800	439.565217	6.854029
6.076368	435.353205	6.859034
6.096818	430.686574	6.864038
5.800510	418.871901	6.869043
6.052420	405.876661	6.874048
5.599832	410.699654	6.879053
5.657331	417.372652	6.884058
5.826332	422.876555	6.889062
5.829704	437.590965	6.894067
6.159349	431.433189	6.899072
5.940362	438.418440	6.904077
5.772358	436.369337	6.909082
6.258814	426.858660	6.914086
5.828961	426.252155	6.919091
6.104099	413.265926	6.924096
5.847937	407.237910	6.929101
6.051256	410.698938	6.934106
5.903147	407.615319	6.939110
5.951114	406.801069	6.944115
5.804817	399.664327	6.949120
5.631488	406.338685	6.954125
5.560438	409.731968	6.959130
6.146176	415.996328	6.964134
5.760552	425.216024	6.969139
6.111321	423.917723	6.974144
6.123639	424.596050	6.979149
5.980942	412.402966	6.984154
6.122601	407.922998	6.989158
5.818521	406.300187	6.994163
5.826931	400.018745	6.999168
6.142595	406.619651	7.004173
5.888114	402.154296	7.009178
5.933261	407.193536	7.014182
5.871335	410.541096	7.019187
5.882885	392.625835	7.024192
5.718770	404.212144	7.029197
5.626329	406.491953	7.034202
5.833205	407.120813	7.039206
5.664474	415.945846	7.044211
6.017655	425.881867	7.049216
5.984322	416.794328	7.054221
5.573627	417.915427	7.059226
5.591772	415.077846	7.064230
6.034232	422.253689	7.069235
5.865711	428.304031	7.074240
5.931661	424.712298	7.079245
5.770063	424.838897	7.084250
5.897277	419.057698	7.089254
6.005582	424.757776	7.094259
5.960009	432.870646	7.099264
6.016288	430.634540	7.104269
6.221681	435.515800	7.109274
5.942377	425.236073	7.114278
5.786195	423.738786	7.119283
5.673355	419.494848	7.124288
5.651101	431.289905	7.129293
5.946807	428.342393	7.134298
6.200440	427.745859	7.139302
5.773273	431.403755	7.144307
6.154898	433.273926	7.149312
5.839930	433.940256	7.154317
6.255180	426.588967	7.159322
6.183915	408.999882	7.164326
5.672206	408.086658	7.169331
5.860815	403.494930	7.174336
5.601233	400.666063	7.179341
5.781628	422.139097	7.184346
6.025668	419.101603	7.189350
6.084187	426.517941	7.194355
5.790837	416.708663	7.199360
5.923017	411.916962	7.204365
5.878407	417.460660	7.209370
5.873513	401.816419	7.214374
5.750397	414.696636	7.219379
6.130530	419.550514	7.224384
6.056712	412.421394	7.229389
5.773428	414.386250	7.234394
5.999208	406.542626	7.239398
5.851715	406.508824	7.244403
5.641864	401.647327	7.249408
6.284194	419.349488	7.254413
6.124182	407.095843	7.259418
6.002844	393.510513	7.264422
5.849278	409.049932	7.269427
6.014677	408.910157	7.274432
5.683078	411.148343	7.279437
6.065407	409.253466	7.284442
5.931715	406.458659	7.289446
5.514519	404.094257	7.294451
5.957797	414.130052	7.299456
5.852229	389.987781	7.304461
5.685569	405.165411	7.309466
6.020182	406.843624	7.314470
5.771727	408.097493	7.319475
5.799439	411.605018	7.324480
5.918867	413.902253	7.329485
5.961107	424.757041	7.334490
6.302643	414.088975	7.339494
5.966452	412.661023	7.344499
5.851459	401.374783	7.349504
6.015630	399.836797	7.354509
5.707725	402.650247	7.359514
5.904183	399.490495	7.364518
5.428671	412.049431	7.369523
5.690221	412.748820	7.374528
6.036070	422.144976	7.379533
5.898941	429.006664	7.384538
6.063782	429.983803	7.389542
6.191135	422.639658	7.394547
6.124065	408.438361	7.399552
5.990778	417.678628	7.404557
5.613111	405.205983	7.409562
5.822874	401.129805	7.414566
5.805588	413.908017	7.419571
5.813869	407.243771	7.424576
5.818284	414.735021	7.429581
6.004048	416.689663	7.434586
6.091114	414.119698	7.439590
5.970699	417.530209	7.444595
5.875201	410.293753	7.449600
5.554232	410.758539	7.454605
5.693130	417.368163	7.459610
6.112428	427.828510	7.464614
5.936000	436.844588	7.469619
6.066484	431.591231	7.474624
5.913296	417.896975	7.479629
5.587983	418.482667	7.484634
5.898175	415.684750	7.489638
5.886023	432.970604	7.494643
6.246052	427.497781	7.499648
5.879907	423.027769	7.504653
5.481296	415.183894	7.509658
5.874041	418.580442	7.514662
5.786096	421.074687	7.519667
6.234189	420.839998	7.524672
6.233765	429.657651	7.529677
6.207323	418.566337	7.534682
5.905489	404.955493	7.539686
5.965466	406.885549	7.544691
5.894839	409.434028	7.549696
5.924181	401.545253	7.554701
5.931285	409.868162	7.559706
6.072077	400.484426	7.564710
5.938386	411.604056	7.569715
5.878968	404.153138	7.574720
6.000544	409.006394	7.579725
5.669178	406.925942	7.584730
5.968485	409.837246	7.589734
5.829637	409.431924	7.594739
5.873376	407.650210	7.599744
5.691439	406.916276	7.604749
5.554178	406.975785	7.609754
5.829522	402.569787	7.614758
5.830208	409.381400	7.619763
5.902519	413.410294	7.624768
6.193498	410.283188	7.629773
5.706208	413.849259	7.634778
5.980560	407.358463	7.639782
6.318620	408.352754	7.644787
5.821316	399.398032	7.649792
6.036337	402.151696	7.654797
5.852832	404.553342	7.659802
5.962069	395.541555	7.664806
6.030228	412.371872	7.669811
5.905539	401.846466	7.674816
6.004755	396.604345	7.679821
5.774038	401.996860	7.684826
5.969571	403.257096	7.689830
5.901943	403.875180	7.694835
5.678997	400.578658	7.699840
5.901681	401.280972	7.704845
5.533014	403.569258	7.709850
6.175607	395.049717	7.714854
5.954964	405.774837	7.719859
5.958638	401.471517	7.724864
5.796760	396.162736	7.729869
5.527516	392.531777	7.734874
5.711262	404.731146	7.739878
6.136371	398.431872	7.744883
6.120068	395.754718	7.749888
6.047477	396.019233	7.754893
5.571591	401.402705	7.759898
5.445108	399.606533	7.764902
5.803981	409.506851	7.769907
6.108321	419.270184	7.774912
6.133278	415.653237	7.779917
6.237790	412.666080	7.784922
6.030625	407.142925	7.789926
6.109568	405.830267	7.794931
6.016622	408.692297	7.799936
6.139471	410.356233	7.804941
5.786252	405.729174	7.809946
5.997460	405.617023	7.814950
5.788323	403.609171	7.819955
5.741162	405.261779	7.824960
5.817248	406.664118	7.829965
5.622538	414.344757	7.834970
6.190394	409.693606	7.839974
5.811232	407.918041	7.844979
5.894585	404.209688	7.849984
6.042288	408.840548	7.854989
5.641675	408.640758	7.859994
6.270216	402.315936	7.864998
6.125254	403.430200	7.870003
5.707500	414.600667	7.875008
6.276079	399.939108	7.880013
5.707583	412.174085	7.885018
5.809808	402.625545	7.890022
6.107257	401.759551	7.895027
6.148795	417.872696	7.900032
5.939153	411.948123	7.905037
6.024005	411.023688	7.910042
5.873528	403.897090	7.915046
5.871115	408.342659	7.920051
5.885988	412.902582	7.925056
5.965851	410.178720	7.930061
5.924785	409.492317	7.935066
6.134633	408.886825	7.940070
6.022401	408.781058	7.945075
6.122451	401.441199	7.950080
5.971114	406.954158	7.955085
5.997454	412.135554	7.960090
6.123945	406.303852	7.965094
6.038705	393.965734	7.970099
6.009114	390.243442	7.975104
5.648390	386.921052	7.980109
5.468555	381.554977	7.985114
6.117251	391.662980	7.990118
5.999188	405.584397	7.995136
5.954198	401.637343	8.000154
5.903287	398.000479	8.005171
6.042987	401.431006	8.010189
5.812550	406.147109	8.015206
5.928446	396.740666	8.020224
5.933153	400.618368	8.025242
5.912988	405.329927	8.030259
6.064560	402.529165	8.035277
6.221525	393.854732	8.040294
5.575247	387.682424	8.045312
5.565384	403.399579	8.050330
5.951276	400.338047	8.055347
5.981799	408.967404	8.060365
5.916129	418.403928	8.065382
6.129942	404.317954	8.070400
5.943205	414.754879	8.075418
6.084663	400.572950	8.080435
6.075257	406.406266	8.085453
5.778987	407.165920	8.090470
5.949241	410.143546	8.095488
5.912210	412.279510	8.100506
5.812652	409.398177	8.105523
6.038027	408.709664	8.110541
6.394525	402.926178	8.115558
6.214070	410.411502	8.120576
5.903660	409.336731	8.125594
6.245375	410.479254	8.130611
6.176655	409.568582	8.135629
5.991651	398.599856	8.140646
5.776456	396.112176	8.145664
6.101644	407.671224	8.150682
6.185952	406.550388	8.155699
5.989077	409.285740	8.160717
6.295914	400.518395	8.165734
6.276322	396.396953	8.170752
5.691800	403.188206	8.175770
5.841852	398.942355	8.180787
6.086089	400.254781	8.185805
5.875421	410.285207	8.190822
6.340232	403.806266	8.195840
5.813460	407.868226	8.200858
6.191994	413.116909	8.205875
5.711038	410.765539	8.210893
6.314072	406.133138	8.215910
6.177331	409.272471	8.220928
6.275191	408.386192	8.225946
6.143743	402.006985	8.230963
6.243661	413.238423	8.235981
6.125107	421.225283	8.240998
6.192433	410.497875	8.246016
6.344265	413.585683	8.251034
6.264973	407.974615	8.256051
6.323567	410.868752	8.261069
6.439227	412.614727	8.266086
6.375404	416.433743	8.271104
5.965008	404.099179	8.276122
5.878808	404.617641	8.281139
5.951122	414.029387	8.286157
6.460400	402.765688	8.291174
6.392433	403.767277	8.296192
5.879165	413.712576	8.301210
6.474003	406.465351	8.306227
6.160579	414.833027	8.311245
6.202248	406.725751	8.316262
6.094828	407.821882	8.321280
5.923878	414.450512	8.326298
6.083126	414.665435	8.331315
6.017000	401.945579	8.336333
6.069893	406.203888	8.341350
5.913939	411.886602	8.346368
5.704692	411.600694	8.351386
6.144407	408.966220	8.356403
6.242488	426.859722	8.361421
6.060994	426.171843	8.366438
6.787071	423.423072	8.371456
6.266629	423.151210	8.376474
6.474611	411.757991	8.381491
5.970499	406.806765	8.386509
6.487443	420.579508	8.391526
6.099862	414.941003	8.396544
6.408541	434.742297	8.401562
6.429017	433.994370	8.406579
6.436965	428.398029	8.411597
6.440823	425.645654	8.416614
6.125696	408.158612	8.421632
6.087207	423.249122	8.426650
6.505696	427.825687	8.431667
6.433277	430.468961	8.436685
6.429009	438.201241	8.441702
6.374153	429.638872	8.446720
6.543050	420.807924	8.451738
6.590866	405.744431	8.456755
6.268382	414.293404	8.461773
5.921443	414.941079	8.466790
6.255310	421.528486	8.471808
6.126610	428.021116	8.476826
6.329925	427.241386	8.481843
6.132125	434.388617	8.486861
5.958377	430.382837	8.491878
6.357290	432.677713	8.496896
6.444235	432.903964	8.501914
6.374225	436.496740	8.506931
6.358520	435.703991	8.511949
6.328007	434.414954	8.516966
6.427234	431.010175	8.521984
6.561965	432.630089	8.527002
6.394808	429.749877	8.532019
6.557653	436.869004	8.537037
6.399369	436.745522	8.542054
6.550806	430.583909	8.547072
6.641745	437.988853	8.552090
6.676066	435.178056	8.557107
6.687621	434.971159	8.562125
6.427306	441.563310	8.567143
6.408243	430.186719	8.572160
6.499040	440.652758	8.577178
6.189167	434.658095	8.582195
6.853834	438.968878	8.587213
6.700569	436.496735	8.592231
6.452530	437.971499	8.597248
6.462279	434.542870	8.602266
6.635130	429.122659	8.607283
6.340911	441.798084	8.612301
6.291744	430.400964	8.617319
6.739700	433.925208	8.622336
6.826140	441.570694	8.627354
7.002691	427.471605	8.632371
6.552111	429.934294	8.637389
6.290769	431.745651	8.642407
6.684705	426.694735	8.647424
6.831627	431.058236	8.652442
6.501817	431.618023	8.657459
6.498377	431.072656	8.662477
6.219624	435.881542	8.667495
6.570469	433.930006	8.672512
6.546776	427.757965	8.677530
6.602172	427.862930	8.682547
6.640857	430.848551	8.687565
6.649992	441.889107	8.692583
6.567655	431.904646	8.697600
6.307654	437.013546	8.702618
6.859246	440.224913	8.707635
6.835799	429.716839	8.712653
6.609988	434.577389	8.717671
6.663022	427.872629	8.722688
6.343752	433.195938	8.727706
6.995360	447.395718	8.732723
6.929720	440.965162	8.737741
6.698942	433.547489	8.742759
6.947237	432.299973	8.747776
6.572337	432.055799	8.752794
6.467937	435.653964	8.757811
6.619388	439.716961	8.762829
6.358400	449.575416	8.767847
6.720669	451.260665	8.772864
6.962464	466.218935	8.777882
6.946882	463.898782	8.782899
6.958506	453.943767	8.787917
6.566620	446.021166	8.792935
6.806834	445.772131	8.797952
6.711070	460.290989	8.802970
6.715462	453.265642	8.807987
7.057149	449.980658	8.813005
6.702024	455.464223	8.818023
6.952091	435.083139	8.823040
6.623690	433.250652	8.828058
6.455908	443.795075	8.833075
6.888880	456.356574	8.838093
6.675556	469.562133	8.843111
6.895406	462.200072	8.848128
6.893391	467.773479	8.853146
6.754200	470.900584	8.858163
6.986487	464.079363	8.863181
6.596673	464.187814	8.868199
6.439400	460.974694	8.873216
6.834260	457.280597	8.878234
6.905381	458.187814	8.883251
6.726451	456.641168	8.888269
6.965044	465.828077	8.893287
7.069756	454.656135	8.898304
6.930643	462.964965	8.903322
6.758942	470.240662	8.908339
7.117893	455.283011	8.913357
6.685548	466.979723	8.918375
6.893405	469.721098	8.923392
6.997196	467.439044	8.928410
7.026116	465.392780	8.933427
7.176079	469.228804	8.938445
7.250375	464.641363	8.943463
7.546167	455.115185	8.948480
7.208582	454.350777	8.953498
7.051619	446.672229	8.958515
6.777524	443.019834	8.963533
6.703825	449.929880	8.968551
6.935544	457.700931	8.973568
7.284577	466.637011	8.978586
6.786091	454.275189	8.983603
7.148373	451.665464	8.988621
6.773232	460.229020	8.993639
7.004833	451.577578	8.998656
7.310168	455.856305	9.003674
6.579705	458.075676	9.008691
6.969374	456.219039	9.013709
6.947192	461.120273	9.018727
7.174121	465.442845	9.023744
7.276656	464.606322	9.028762
6.856076	465.161398	9.033779
7.383260	455.254989	9.038797
6.985064	475.328025	9.043815
6.936790	466.843501	9.048832
6.973882	462.337628	9.053850
6.611502	467.806554	9.058867
7.265963	468.398315	9.063885
7.291480	468.460625	9.068903
7.178287	456.751633	9.073920
7.429180	459.281139	9.078938
7.236561	468.879589	9.083955
7.272761	458.895475	9.088973
6.810465	449.333447	9.093991
6.849225	459.217525	9.099008
7.129523	460.174017	9.104026
6.764388	461.970082	9.109043
7.073316	453.508491	9.114061
6.604166	460.433165	9.119079
6.831256	454.180797	9.124096
7.171442	465.434582	9.129114
7.114608	476.204634	9.134131
7.339579	467.358566	9.139149
6.840128	466.537469	9.144167
7.131642	469.836927	9.149184
6.899456	465.663573	9.154202
7.117833	475.342795	9.159219
7.502412	475.339380	9.164237
7.171880	473.923781	9.169255
7.350837	468.897070	9.174272
7.187726	468.815368	9.179290
6.944427	471.273986	9.184307
7.428599	478.831926	9.189325
7.323771	484.355176	9.194343
7.377040	472.695830	9.199360
7.166608	466.234304	9.204378
7.192136	463.282871	9.209395
7.237432	466.289553	9.214413
7.250473	484.893858	9.219431
7.033104	488.462397	9.224448
7.239803	490.528625	9.229466
7.340656	491.775162	9.234483
7.533255	486.373930	9.239501
7.528652	498.619016	9.244519
7.600062	487.414403	9.249536
7.284826	471.211708	9.254554
7.249507	462.447450	9.259571
7.482050	462.590929	9.264589
7.132815	458.000423	9.269607
7.392617	476.029579	9.274624
7.425561	470.849023	9.279642
7.221408	470.836867	9.284659
7.501056	464.765605	9.289677
7.274591	470.292131	9.294695
7.399378	479.629420	9.299712
7.293004	477.777918	9.304730
7.292057	485.913634	9.309747
7.257785	493.423425	9.314765
7.412221	490.877817	9.319783
7.469742	488.442067	9.324800
7.562383	489.879236	9.329818
7.320784	488.724252	9.334835
7.918945	479.538844	9.339853
7.512820	478.731526	9.344871
7.487462	482.083790	9.349888
7.369375	470.337687	9.354906
7.322386	466.760155	9.359923
7.494422	482.407854	9.364941
7.582076	480.791036	9.369959
7.587373	485.410265	9.374976
7.517401	477.178440	9.379994
7.438901	476.818398	9.385011
7.504867	477.783227	9.390029
7.608602	480.954321	9.395047
7.448798	479.171150	9.400064
7.316620	472.116703	9.405082
7.065359	481.954717	9.410099
7.598952	484.007595	9.415117
7.574434	492.298484	9.420135
7.085997	489.310813	9.425152
7.318154	479.759879	9.430170
7.286668	495.366896	9.435187
7.589453	483.602178	9.440205
7.079680	487.405876	9.445223
7.424760	493.997865	9.450240
7.304609	491.293311	9.455258
7.500322	503.371317	9.460275
7.263888	506.624116	9.465293
7.443054	502.458884	9.470311
7.708929	507.703156	9.475328
7.571964	510.220858	9.480346
7.488140	515.595662	9.485363
7.483364	506.189133	9.490381
7.680383	501.345773	9.495399
7.870311	515.169827	9.500416
7.821646	515.584582	9.505434
7.594340	518.946404	9.510451
7.701735	510.525829	9.515469
7.822736	508.853291	9.520487
7.578585	508.743262	9.525504
7.782178	505.063345	9.530522
7.747221	510.525163	9.535539
7.776946	501.529792	9.540557
7.710126	504.506710	9.545575
7.615720	505.203182	9.550592
7.559067	507.922891	9.555610
7.640643	513.123459	9.560627
7.693344	507.939796	9.565645
7.920544	509.586254	9.570663
7.713559	508.829783	9.575680
7.914473	509.653551	9.580698
7.476488	516.822669	9.585715
7.815338	507.684187	9.590733
7.382511	506.672771	9.595751
7.412978	504.736712	9.600768
7.494697	496.834555	9.605786
7.622039	501.062288	9.610803
7.754675	505.592144	9.615821
7.684490	505.902975	9.620839
7.943404	517.806989	9.625856
7.638681	508.128725	9.630874
7.755808	522.106199	9.635891
7.597730	523.705729	9.640909
8.271523	521.949733	9.645927
7.723283	533.696205	9.650944
8.210381	524.512397	9.655962
8.060189	509.271561	9.660979
7.989092	494.532734	9.665997
8.042860	498.535311	9.671015
8.023884	507.491203	9.676032
8.193606	500.430467	9.681050
8.118972	505.365178	9.686067
7.940440	493.836810	9.691085
7.867259	501.633562	9.696103
7.648601	506.922194	9.701120
7.921779	500.552137	9.706138
7.961051	506.207449	9.711155
7.876784	501.363980	9.716173
7.887078	505.385994	9.721191
7.584413	511.669230	9.726208
7.845056	498.330070	9.731226
7.695578	510.708315	9.736243
7.984428	519.341431	9.741261
8.058707	526.105247	9.746279
7.964607	538.790411	9.751296
8.443731	531.034253	9.756314
8.185649	527.388799	9.761331
8.010283	510.381524	9.766349
8.003254	513.169197	9.771367
7.837507	508.319558	9.776384
8.217190	508.288508	9.781402
8.184669	513.790971	9.786419
8.200507	509.503008	9.791437
8.005673	508.791969	9.796455
7.896676	517.525288	9.801472
7.942061	501.985576	9.806490
8.201011	509.547259	9.811507
7.794799	506.351045	9.816525
7.641174	509.508819	9.821543
7.737731	522.552257	9.826560
8.177544	525.282543	9.831578
8.269050	529.418069	9.836595
8.203006	528.279757	9.841613
8.402249	527.320783	9.846631
8.173036	539.408588	9.851648
8.219297	531.941155	9.856666
8.157360	533.270005	9.861683
8.035305	540.992382	9.866701
8.225148	535.339106	9.871719
8.227794	538.639656	9.876736
8.427097	533.287851	9.881754
8.345488	529.106668	9.886771
8.352508	532.845183	9.891789
8.273862	525.514087	9.896807
8.148825	526.385770	9.901824
8.118213	517.819560	9.906842
8.452035	531.766247	9.911859
8.256578	518.845668	9.916877
8.113952	516.450741	9.921895
8.273320	529.029913	9.926912
8.406472	519.074755	9.931930
8.315352	516.188927	9.936947
7.881146	519.002506	9.941965
8.378732	518.959295	9.946983
8.592485	521.870164	9.952000
8.467809	527.787852	9.957018
8.590994	506.369387	9.962035
8.380300	513.029528	9.967053
8.493203	509.613124	9.972071
8.272866	512.920205	9.977088
8.406857	506.840194	9.982106
8.740881	506.500722	9.987123
8.219846	511.249761	9.992141
8.356003	509.379191	9.997159
8.301534	504.101870	10.002176
8.050776	501.398844	10.007194
8.384460	510.495138	10.012211
8.215828	505.008489	10.017229
8.239195	498.264170	10.022247
8.146122	511.245795	10.027264
8.506119	511.287256	10.032282
8.742761	518.612600	10.037299
8.331061	513.788873	10.042317
8.377703	510.685804	10.047335
8.389397	512.978245	10.052352
8.442447	524.611566	10.057370
8.898606	526.263177	10.062387
8.237933	516.612276	10.067405
8.604430	506.431219	10.072423
8.214469	506.186248	10.077440
8.248303	514.174518	10.082458
8.631656	519.832726	10.087475
8.385324	527.928015	10.092493
8.640178	523.605754	10.097511
8.424803	525.744429	10.102528
8.169507	533.399318	10.107546
8.412946	520.510956	10.112563
8.441939	530.920460	10.117581
8.299922	525.600045	10.122599
8.404710	522.607783	10.127616
8.393840	532.862590	10.132634
8.498456	534.913260	10.137651
8.281489	536.607223	10.142669
8.478018	524.202728	10.147687
8.308037	523.762345	10.152704
8.067711	528.817697	10.157722
8.224283	530.970677	10.162739
8.514708	554.820651	10.167757
8.592195	549.617314	10.172775
8.476934	559.131109	10.177792
8.639249	554.924325	10.182810
9.096101	554.123800	10.187827
8.947777	555.223193	10.192845
8.775667	550.071586	10.197863
8.914444	558.340076	10.202880
8.713268	553.224580	10.207898
8.640728	536.885970	10.212915
8.428485	535.111010	10.217933
8.782228	551.292026	10.222951
8.615653	561.340875	10.227968
8.783080	547.337794	10.232986
8.913455	556.393384	10.238003
8.735260	555.080141	10.243021
8.800914	552.400114	10.248039
8.785895	549.808466	10.253056
8.666436	557.678765	10.258074
8.986285	542.547288	10.263091
8.678982	551.267514	10.268109
9.007085	543.336200	10.273127
8.855596	536.881192	10.278144
8.531318	532.779055	10.283162
8.850989	540.429066	10.288179
8.702977	548.591008	10.293197
8.685026	550.370554	10.298215
8.883348	546.341164	10.303232
8.911507	555.428548	10.308250
8.670044	553.358367	10.313267
8.956480	556.996304	10.318285
9.004896	562.091629	10.323303
8.861656	559.643144	10.328320
8.688297	557.417127	10.333338
9.004996	547.303808	10.338355
8.957570	553.354566	10.343373
8.942732	558.945789	10.348391
8.655675	555.579420	10.353408
9.012610	545.942630	10.358426
9.061056	554.824867	10.363443
8.531278	556.766656	10.368461
9.165783	546.237475	10.373479
9.202183	554.222206	10.378496
8.823122	553.745155	10.383514
9.239526	553.960812	10.388531
8.858287	555.705762	10.393549
9.217207	562.816308	10.398567
9.070381	559.210219	10.403584
9.304193	557.034013	10.408602
9.164663	542.252220	10.413619
8.746354	533.557401	10.418637
8.693411	526.935480	10.423655
8.483619	531.364363	10.428672
8.810227	546.924785	10.433690
8.954222	553.302152	10.438707
9.011621	547.054249	10.443725
9.172060	555.357212	10.448743
9.138432	553.888776	10.453760
8.875187	553.731246	10.458778
8.960145	551.527871	10.463795
8.699688	554.980099	10.468813
8.506765	556.427303	10.473831
8.950376	550.282986	10.478848
8.719021	554.267135	10.483866
8.884570	571.572706	10.488883
9.109522	578.571707	10.493901
9.238898	577.664702	10.498919
9.529201	584.034935	10.503936
8.933268	575.184892	10.508954
9.378421	569.377995	10.513971
9.264988	575.874598	10.518989
9.308058	579.702147	10.524007
9.466386	579.200856	10.529024
8.933285	570.060108	10.534042
9.213104	567.709436	10.539059
9.153964	578.606142	10.544077
9.229173	573.901767	10.549095
9.621446	578.596086	10.554112
9.187369	567.262343	10.559130
9.360247	567.989522	10.564147
9.084864	561.137355	10.569165
9.119326	560.396699	10.574183
9.289171	574.877190	10.579200
8.866989	574.997023	10.584218
9.585400	575.212699	10.589235
9.644047	583.342278	10.594253
9.370720	578.146562	10.599271
9.638729	579.553106	10.604288
8.900630	569.687092	10.609306
9.542835	569.390850	10.614323
9.307494	576.218976	10.619341
9.641356	579.836863	10.624359
9.450249	563.125491	10.629376
9.045553	562.658768	10.634394
9.511632	557.931024	10.639411
9.666482	568.655342	10.644429
9.381091	555.335422	10.649447
9.783880	553.094872	10.654464
8.976954	560.208205	10.659482
9.355450	549.526632	10.664499
9.152184	560.550049	10.669517
9.374624	574.283849	10.674535
9.642386	574.690052	10.679552
9.091296	583.158160	10.684570
9.571564	580.807638	10.689587
9.441728	581.238268	10.694605
9.468997	585.273419	10.699623
9.682120	565.525974	10.704640
9.502304	584.113263	10.709658
9.566944	576.412561	10.714675
9.609079	584.459522	10.719693
9.411293	585.165884	10.724711
9.576390	583.726268	10.729728
9.422867	591.163266	10.734746
9.411838	576.108850	10.739763
9.198737	577.969467	10.744781
9.616613	568.834351	10.749799
9.641446	567.274704	10.754816
9.405296	578.924971	10.759834
9.387903	573.607106	10.764851
9.505355	575.829337	10.769869
9.674404	571.185998	10.774887
9.426561	573.115173	10.779904
9.635885	573.353809	10.784922
9.568885	563.874950	10.789939
9.468016	575.147416	10.794957
9.502923	574.368821	10.799975
9.612712	585.084430	10.804992
9.192603	579.987450	10.810010
9.520574	592.612833	10.815027
9.734256	599.086594	10.820045
9.981907	605.542412	10.825063
9.824307	586.105491	10.830080
9.640208	586.348966	10.835098
9.697659	583.840631	10.840115
9.705140	588.364872	10.845133
9.716238	597.186710	10.850151
9.826232	595.531667	10.855168
9.834444	599.235296	10.860186
9.687910	589.061991	10.865203
10.039193	591.159225	10.870221
9.738758	586.996536	10.875239
9.722637	582.978647	10.880256
9.746249	596.888782	10.885274
9.974155	597.768285	10.890291
9.867045	588.415617	10.895309
9.735021	585.747623	10.900327
9.903496	584.600964	10.905344
9.585330	582.792103	10.910362
9.934113	595.442630	10.915379
9.917552	599.566701	10.920397
10.080794	608.033350	10.925415
10.150287	597.460124	10.930432
9.856500	587.047963	10.935450
9.821720	578.059504	10.940467
9.832819	582.393830	10.945485
10.001062	592.178800	10.950503
9.878757	588.224883	10.955520
9.980956	598.957469	10.960538
10.117765	595.572017	10.965555
10.135706	576.827119	10.970573
9.708481	588.308516	10.975591
10.041570	591.554146	10.980608
9.629885	601.859170	10.985626
9.837543	601.372240	10.990643
9.845802	606.903055	10.995661
9.682252	606.414326	11.000679
9.902420	602.053301	11.005696
9.817175	604.714389	11.010714
9.863232	602.356159	11.015731
10.152715	602.039443	11.020749
9.932141	604.106358	11.025767
10.136802	596.159649	11.030784
10.156477	611.323255	11.035802
10.230266	602.838475	11.040819
10.449314	600.503633	11.045837
10.158963	603.083249	11.050855
9.960250	606.708848	11.055872
9.906242	611.185925	11.060890
9.972074	599.391986	11.065907
10.129856	599.768085	11.070925
10.821203	603.288941	11.075943
10.176602	604.197854	11.080960
10.047104	605.445777	11.085978
10.261508	608.769966	11.090995
10.273046	604.110272	11.096013
10.174345	606.132846	11.101031
10.273909	603.125610	11.106048
9.998011	613.106410	11.111066
10.310081	615.673691	11.116083
10.454250	603.763334	11.121101
10.416752	604.908481	11.126119
10.484916	600.624920	11.131136
10.239701	607.975307	11.136154
10.147354	614.803133	11.141171
10.562155	609.474345	11.146189
10.116722	611.450262	11.151207
10.053319	610.368335	11.156224
10.489219	608.974649	11.161242
10.092247	609.929969	11.166259
10.053519	608.408679	11.171277
10.032825	609.693204	11.176295
10.192643	601.939709	11.181312
10.357233	618.601698	11.186330
10.026059	614.402793	11.191347
10.027311	611.306818	11.196365
10.325522	629.203880	11.201383
10.782603	632.010372	11.206400
10.395554	621.019517	11.211418
10.235782	618.314841	11.216435
10.441795	618.983182	11.221453
10.598275	632.430719	11.226471
10.399916	629.580609	11.231488
10.326502	627.802822	11.236506
10.222238	642.660828	11.241523
10.461206	633.806174	11.246541
10.060634	637.902060	11.251559
10.005091	636.478075	11.256576
10.271425	635.685308	11.261594
10.496725	640.923353	11.266611
10.532782	635.925297	11.271629
10.367196	643.992207	11.276647
10.296825	642.535832	11.281664
10.720869	642.002374	11.286682
10.417842	637.893727	11.291699
10.409217	635.544060	11.296717
10.479671	642.485243	11.301735
10.553573	641.678444	11.306752
10.799027	634.375417	11.311770
10.749755	636.428120	11.316787
10.472986	638.327121	11.321805
10.847742	636.624279	11.326823
10.500716	636.574548	11.331840
10.514230	635.013513	11.336858
10.521368	641.718465	11.341875
10.946559	649.143709	11.346893
10.332197	650.871544	11.351911
10.733102	658.597240	11.356928
10.943216	664.948509	11.361946
10.748997	660.226365	11.366963
11.103101	642.160870	11.371981
10.475600	645.604353	11.376999
10.832830	637.305519	11.382016
10.762225	631.191251	11.387034
10.674771	630.368709	11.392051
10.819085	637.819021	11.397069
10.549664	634.203723	11.402087
10.825089	642.782198	11.407104
10.664024	648.642512	11.412122
10.849471	661.182977	11.417139
10.836797	663.513970	11.422157
10.736467	660.462304	11.427175
10.883634	668.401329	11.432192
11.201435	657.372598	11.437210
10.854317	649.603836	11.442227
11.172749	658.671038	11.447245
10.512196	643.210252	11.452263
10.533806	649.591050	11.457280
10.856098	654.996939	11.462298
10.716142	663.062998	11.467315
10.909861	668.031447	11.472333
10.979304	649.442504	11.477351
11.018204	668.446889	11.482368
10.767679	667.621494	11.487386
11.025342	667.085702	11.492403
11.267366	664.936598	11.497421
11.190339	663.976723	11.502439
11.134614	660.353183	11.507456
11.086458	665.940193	11.512474
10.545712	660.120482	11.517491
10.835966	667.020924	11.522509
11.087552	668.600460	11.527527
11.029049	662.203420	11.532544
11.184422	663.555036	11.537562
11.529849	656.652900	11.542579
11.334368	656.159705	11.547597
10.937222	650.838202	11.552615
11.005101	648.407119	11.557632
11.092197	654.742944	11.562650
10.883795	660.872609	11.567667
11.269039	651.439609	11.572685
11.078767	661.889856	11.577703
10.807895	657.971824	11.582720
11.129757	664.024719	11.587738
10.794620	664.329728	11.592755
10.976323	652.107348	11.597773
11.031640	666.684752	11.602791
11.316557	664.396385	11.607808
11.128170	657.407475	11.612826
10.882467	658.257045	11.617843
11.138528	659.217346	11.622861
10.993977	665.153972	11.627879
10.892563	665.125718	11.632896
11.320954	667.220348	11.637914
11.032885	680.396748	11.642931
11.095593	687.238176	11.647949
11.487352	696.173989	11.652967
11.253990	680.456891	11.657984
11.478860	678.654454	11.663002
11.492712	688.163867	11.668019
11.493303	687.460071	11.673037
11.491936	675.932229	11.678055
11.232246	664.388064	11.683072
11.255229	661.828315	11.688090
11.346601	670.934256	11.693107
11.900090	672.946170	11.698125
11.469181	671.069758	11.703143
11.423602	667.659221	11.708160
11.436806	658.814680	11.713178
11.120310	657.507320	11.718195
11.164503	651.614897	11.723213
11.126970	672.265957	11.728231
11.566369	674.557677	11.733248
11.807025	684.116758	11.738266
11.859045	698.666303	11.743283
11.769951	676.346781	11.748301
11.541639	658.858514	11.753319
11.562392	659.265551	11.758336
11.655715	659.557078	11.763354
11.724450	660.966448	11.768371
11.607480	651.896156	11.773389
11.536029	658.578714	11.778407
11.353112	657.736415	11.783424
11.881836	659.297775	11.788442
11.016584	662.153667	11.793459
11.328535	661.972284	11.798477
11.265636	659.239800	11.803495
11.376653	680.315716	11.808512
11.884190	681.321823	11.813530
11.677333	687.776301	11.818547
11.391719	681.515823	11.823565
11.782399	684.708266	11.828583
11.684063	692.619495	11.833600
11.997185	683.475488	11.838618
11.583853	691.085778	11.843635
11.614800	690.967358	11.848653
12.041435	680.559030	11.853671
11.546750	691.539825	11.858688
11.776521	678.227460	11.863706
11.771973	688.228903	11.868723
11.814534	684.744592	11.873741
11.510108	686.635308	11.878759
11.724906	697.930976	11.883776
11.967908	695.961595	11.888794
12.143955	687.151487	11.893811
11.688639	685.392506	11.898829
11.745339	686.096868	11.903847
11.496614	679.104780	11.908864
12.005572	681.540236	11.913882
11.726123	687.513784	11.918899
11.792648	691.848920	11.923917
11.849215	685.771512	11.928935
11.915427	684.325291	11.933952
11.783923	689.369949	11.938970
11.681477	683.074460	11.943987
11.572476	677.288082	11.949005
11.957751	680.610758	11.954023
11.760953	690.014322	11.959040
12.028631	681.410765	11.964058
12.204438	680.556440	11.969075
11.634348	694.117863	11.974093
12.077935	683.123056	11.979111
11.861751	691.358861	11.984128
12.395258	682.716809	11.989146
11.935863	689.327619	11.994163
11.881961	693.164074	11.999181
12.021080	689.434261	12.004199
11.608457	685.374333	12.009216
11.720460	682.478742	12.014234
11.519962	693.302993	12.019251
11.982972	694.937767	12.024269
12.245111	696.985866	12.029287
11.924898	709.302637	12.034304
11.985337	709.151194	12.039322
11.935177	702.512992	12.044339
12.203455	710.439371	12.049357
12.375330	707.837352	12.054375
11.694051	709.897568	12.059392
12.044746	699.296002	12.064410
12.243100	705.248342	12.069427
12.361245	702.244489	12.074445
12.206235	710.729493	12.079463
12.014373	714.104732	12.084480
12.474528	702.656039	12.089498
12.665342	710.875421	12.094515
12.376845	703.330979	12.099533
12.732128	706.409052	12.104551
12.395834	704.965935	12.109568
12.660522	705.120160	12.114586
12.457152	697.978947	12.119603
12.488518	697.450209	12.124621
12.424913	682.246151	12.129639
12.020972	693.285313	12.134656
12.073422	695.442004	12.139674
12.249227	703.988781	12.144691
12.312211	712.843571	12.149709
12.584642	702.213240	12.154727
12.422366	714.123418	12.159744
12.466663	707.382052	12.164762
12.218870	705.360182	12.169779
12.516781	713.824716	12.174797
12.555144	706.563574	12.179815
12.078285	710.510484	12.184832
12.113257	706.613949	12.189850
12.401315	713.640986	12.194867
12.222595	719.778642	12.199885
12.177148	712.473826	12.204903
12.184985	718.421307	12.209920
12.743058	715.752465	12.214938
12.139540	712.867993	12.219955
12.286591	712.283259	12.224973
12.228658	708.805222	12.229991
12.452076	740.025252	12.235008
12.603935	735.592847	12.240026
12.735838	734.120551	12.245043
13.050817	733.014045	12.250061
12.984784	731.209845	12.255079
12.803234	718.659326	12.260096
12.607637	716.474642	12.265114
12.413102	707.255530	12.270131
12.499265	715.245158	12.275149
12.758697	710.322535	12.280167
12.575264	722.254968	12.285184
12.709603	725.951484	12.290202
12.633683	729.396923	12.295219
12.831930	734.282630	12.300237
12.776954	734.714158	12.305255
12.798335	737.923448	12.310272
12.624668	740.790914	12.315290
12.745297	739.225709	12.320307
13.072189	745.050626	12.325325
13.006143	737.506030	12.330343
12.985556	724.049820	12.335360
12.390089	712.965332	12.340378
12.664091	718.628114	12.345395
12.795839	722.378684	12.350413
12.959752	732.924956	12.355431
12.849387	737.126873	12.360448
13.008749	728.581289	12.365466
13.255435	732.705171	12.370483
13.074986	721.795492	12.375501
13.010779	715.058501	12.380519
12.538877	712.292262	12.385536
12.579524	725.240467	12.390554
12.900815	727.314015	12.395571
12.876240	736.999888	12.400589
13.293685	732.588987	12.405607
13.269996	739.434505	12.410624
13.271100	737.490398	12.415642
12.889072	729.048574	12.420659
12.893593	737.997744	12.425677
13.267530	724.915219	12.430695
13.169115	717.817514	12.435712
13.268053	722.258032	12.440730
13.115451	702.217445	12.445747
12.594609	709.973975	12.450765
12.905225	717.379329	12.455783
13.196782	724.670908	12.460800
13.327255	732.041378	12.465818
13.255167	724.191622	12.470835
13.020522	729.192490	12.475853
13.317661	722.329453	12.480871
13.030808	720.253740	12.485888
12.902376	738.375549	12.490906
13.479011	728.704238	12.495923
13.524674	735.251711	12.500941
13.541867	715.010937	12.505959
12.938108	710.681149	12.510976
13.038691	705.638250	12.515994
13.065526	720.579921	12.521011
13.046093	733.010527	12.526029
13.286957	727.418624	12.531047
13.263320	730.956857	12.536064
13.168578	730.823416	12.541082
13.381930	727.927718	12.546099
13.069992	732.022361	12.551117
13.632117	732.574951	12.556135
13.329013	733.525037	12.561152
13.423513	737.016359	12.566170
13.619294	730.816137	12.571187
13.324019	735.757080	12.576205
13.423188	728.416975	12.581223
13.609883	735.904869	12.586240
13.745264	733.886075	12.591258
13.853072	730.199029	12.596275
13.768135	722.417558	12.601293
13.706814	711.830046	12.606311
13.210914	715.407557	12.611328
13.234337	708.978729	12.616346
13.262789	713.850009	12.621363
13.454843	731.123180	12.626381
13.439116	733.366297	12.631399
13.425668	729.341645	12.636416
13.339823	737.045810	12.641434
13.500040	740.886597	12.646451
13.546666	740.809902	12.651469
13.563668	735.047944	12.656487
13.626286	733.529699	12.661504
13.425914	734.485780	12.666522
13.619407	732.861823	12.671539
13.368955	736.795355	12.676557
13.591822	738.152180	12.681575
13.449446	734.608474	12.686592
13.262158	736.951055	12.691610
13.343808	730.260633	12.696627
13.555755	752.387479	12.701645
13.997467	749.639035	12.706663
13.952530	755.408604	12.711680
13.660939	749.562449	12.716698
13.877629	735.933354	12.721715
13.376629	737.536139	12.726733
13.938000	750.491137	12.731751
13.777500	754.789276	12.736768
13.926368	760.399094	12.741786
14.159915	752.570866	12.746803
14.095567	741.415766	12.751821
13.891337	732.999732	12.756839
13.596994	730.095217	12.761856
13.740690	737.504642	12.766874
14.377289	745.247096	12.771891
14.002088	737.031417	12.776909
13.888543	728.582241	12.781927
13.628584	731.879791	12.786944
13.787423	732.069535	12.791962
14.118504	729.732902	12.796979
13.724301	733.890928	12.801997
13.830079	752.206427	12.807015
14.155184	748.791444	12.812032
14.063297	750.424803	12.817050
14.380688	744.284418	12.822067
14.218005	733.936836	12.827085
13.751062	733.423057	12.832103
13.618945	740.118306	12.837120
13.381274	749.247439	12.842138
14.033238	754.664821	12.847155
14.410500	752.664932	12.852173
14.210872	755.763685	12.857191
13.897464	754.250706	12.862208
13.722964	760.917890	12.867226
14.246410	748.058076	12.872243
14.083556	761.975465	12.877261
13.808521	757.619408	12.882279
14.154326	763.210994	12.887296
14.007775	749.862863	12.892314
14.341470	752.123818	12.897331
14.178019	759.546663	12.902349
14.318308	757.110532	12.907367
14.336119	758.275425	12.912384
14.164230	760.574571	12.917402
14.332310	753.390916	12.922419
14.183912	751.426050	12.927437
14.259446	759.316379	12.932455
14.411150	757.118300	12.937472
14.497711	764.101187	12.942490
14.508347	766.800926	12.947507
14.557265	760.645795	12.952525
14.395662	767.361454	12.957543
14.412369	745.104164	12.962560
14.361193	751.389105	12.967578
14.187502	756.437235	12.972595
14.146981	754.016811	12.977613
14.439240	771.656173	12.982631
14.765841	775.076423	12.987648
14.571390	777.003566	12.992666
14.639174	775.405613	12.997683
14.496576	757.995337	13.002701
14.338284	762.573997	13.007719
14.526978	770.124709	13.012736
14.567320	775.779938	13.017754
14.713363	775.719223	13.022771
14.226801	779.412048	13.027789
14.345354	787.983614	13.032807
14.720585	773.812098	13.037824
14.699761	782.616938	13.042842
14.754565	782.630480	13.047859
14.605252	792.320147	13.052877
14.389344	782.268055	13.057895
15.071091	778.535255	13.062912
14.951649	791.704252	13.067930
14.902150	779.685267	13.072947
14.761467	776.598878	13.077965
14.356724	753.350416	13.082983
14.995871	771.380396	13.088000
14.855910	779.664259	13.093018
14.825209	773.407990	13.098035
14.830676	775.338523	13.103053
14.524880	767.998735	13.108071
15.076242	766.378665	13.113088
14.729107	779.987270	13.118106
14.718893	784.018872	13.123123
14.815758	777.228218	13.128141
14.687316	781.486626	13.133159
15.157276	773.933772	13.138176
14.747392	778.693868	13.143194
14.833848	767.092246	13.148211
14.990903	773.843187	13.153229
14.442763	785.564561	13.158247
14.898741	777.568928	13.163264
14.798667	777.631982	13.168282
14.766571	779.505284	13.173299
14.778108	784.461285	13.178317
14.570599	780.467027	13.183335
15.155307	783.493388	13.188352
15.036398	776.373624	13.193370
15.271350	786.028328	13.198387
15.254423	782.127285	13.203405
14.797164	777.831332	13.208423
15.039919	772.519985	13.213440
15.107969	777.224132	13.218458
15.202105	784.865404	13.223475
15.230717	771.903223	13.228493
15.032070	771.969098	13.233511
15.342022	777.080312	13.238528
15.158432	783.767864	13.243546
14.808560	782.560397	13.248563
14.796119	787.842048	13.253581
15.050486	791.772236	13.258599
15.256593	796.962842	13.263616
15.168333	803.300949	13.268634
15.632788	797.364723	13.273651
15.617965	801.428608	13.278669
15.052447	796.641527	13.283687
15.305683	794.717870	13.288704
15.233579	802.277898	13.293722
15.141023	798.839983	13.298739
15.417421	802.495322	13.303757
15.437207	812.739175	13.308775
15.418194	804.893691	13.313792
15.305554	810.225761	13.318810
15.282331	807.808930	13.323827
15.459974	788.975671	13.328845
15.113963	806.743475	13.333863
15.271538	796.863231	13.338880
15.090041	796.377309	13.343898
15.780579	798.134235	13.348915
15.599352	793.902326	13.353933
15.212863	799.927396	13.358951
15.466646	799.900294	13.363968
15.509279	795.207276	13.368986
15.785409	788.293856	13.374003
15.794788	795.216266	13.379021
15.766319	792.399471	13.384039
15.936347	789.437968	13.389056
16.039442	788.771756	13.394074
15.716966	791.933945	13.399091
16.131587	783.357808	13.404109
15.895415	793.966802	13.409127
15.708762	771.965404	13.414144
15.498953	766.374672	13.419162
15.749143	785.068366	13.424179
15.464623	784.298784	13.429197
15.738562	795.436925	13.434215
15.882538	789.260579	13.439232
15.618695	797.115736	13.444250
15.555620	787.046007	13.449267
15.779129	788.402735	13.454285
15.468385	787.750871	13.459303
15.672040	790.158438	13.464320
15.640765	797.863547	13.469338
15.573484	793.642187	13.474355
15.751394	788.587148	13.479373
15.581860	800.697337	13.484391
15.828336	786.665905	13.489408
15.607285	794.801534	13.494426
15.741786	805.011630	13.499443
15.854795	816.982886	13.504461
15.954400	818.169682	13.509479
16.311288	813.780872	13.514496
16.055084	808.279448	13.519514
15.836623	804.185914	13.524531
16.133703	801.722055	13.529549
16.531361	816.179671	13.534567
16.029060	805.418199	13.539584
15.961476	792.616242	13.544602
15.969156	791.403246	13.549619
15.909987	791.889081	13.554637
15.748583	805.680045	13.559655
16.227762	814.725297	13.564672
15.785143	821.298813	13.569690
16.143448	819.200900	13.574707
16.569323	805.419056	13.579725
16.289806	817.281400	13.584743
16.304484	817.023517	13.589760
16.163814	818.822317	13.594778
16.150495	816.034703	13.599795
16.235665	815.762619	13.604813
16.065825	806.482781	13.609831
16.278067	814.998656	13.614848
16.336198	811.562374	13.619866
16.421433	821.625564	13.624883
16.309261	805.943015	13.629901
16.296323	810.508381	13.634919
16.214163	800.160768	13.639936
16.469347	806.946839	13.644954
15.918389	804.647408	13.649971
16.351225	808.767389	13.654989
16.200623	816.759445	13.660007
16.315445	808.444865	13.665024
16.410559	806.867874	13.670042
16.571131	810.219470	13.675059
16.606447	804.568229	13.680077
16.556446	812.774896	13.685095
16.209525	807.155142	13.690112
16.554842	813.946028	13.695130
16.638774	806.112816	13.700147
16.695388	799.943843	13.705165
16.591238	815.846548	13.710183
16.536086	807.230395	13.715200
16.771056	804.037807	13.720218
16.386191	813.644472	13.725235
16.599168	799.757134	13.730253
16.352217	813.769791	13.735271
16.611913	814.095213	13.740288
16.828399	822.878670	13.745306
16.885257	823.911218	13.750323
16.948973	811.442126	13.755341
16.404081	805.976467	13.760359
16.774931	813.820549	13.765376
17.233177	814.540897	13.770394
16.401553	812.891356	13.775411
16.920871	814.495229	13.780429
17.017815	819.084407	13.785447
16.753612	810.781874	13.790464
17.001328	805.592816	13.795482
16.916745	813.760721	13.800499
16.731569	807.812666	13.805517
16.745311	813.058664	13.810535
16.714090	810.832434	13.815552
16.699336	818.175201	13.820570
17.020003	823.433073	13.825587
17.004019	836.440725	13.830605
17.123440	831.319099	13.835623
16.887825	839.103578	13.840640
17.220632	832.897632	13.845658
17.064771	827.699217	13.850675
17.224968	820.052866	13.855693
16.814596	828.555845	13.860711
17.225905	825.326157	13.865728
17.439411	822.345213	13.870746
17.148120	821.229550	13.875763
17.059981	803.615036	13.880781
16.930229	806.857485	13.885799
17.130386	814.980777	13.890816
17.210653	827.291687	13.895834
17.436270	825.078863	13.900851
17.218424	815.907527	13.905869
17.034854	812.941461	13.910887
16.916032	824.014926	13.915904
17.488967	824.329139	13.920922
16.901309	837.539972	13.925939
16.911485	830.908048	13.930957
16.918914	834.040645	13.935975
16.701182	834.040082	13.940992
17.109881	828.768991	13.946010
16.997837	835.041408	13.951027
17.467364	837.978527	13.956045
17.488208	841.623422	13.961063
17.366203	840.904114	13.966080
17.574440	828.598560	13.971098
17.195579	837.727769	13.976115
17.466889	850.497913	13.981133
17.893929	844.857869	13.986151
17.488937	838.966335	13.991168
17.833507	824.401950	13.996186
17.612655	822.094977	14.001203
17.797792	823.309397	14.006221
17.808679	822.944810	14.011239
17.563894	832.621056	14.016256
17.811266	813.596964	14.021274
17.535361	824.852831	14.026291
17.772599	820.757323	14.031309
17.781012	824.060178	14.036327
17.250992	809.137374	14.041344
17.610250	817.952108	14.046362
17.589567	824.125000	14.051379
17.499524	825.483521	14.056397
17.352919	821.208311	14.061415
17.385064	833.435246	14.066432
17.864568	839.488748	14.071450
17.737353	850.472026	14.076467
17.909729	847.945648	14.081485
17.906991	855.179249	14.086503
18.285982	855.290320	14.091520
18.159199	832.941793	14.096538
17.458917	831.745043	14.101555
17.337937	826.840966	14.106573
17.567202	831.857540	14.111591
17.588284	847.627042	14.116608
17.822549	837.517009	14.121626
17.936818	846.329117	14.126643
17.633979	846.521771	14.131661
17.943899	846.577391	14.136679
18.135137	846.910385	14.141696
17.988173	842.925561	14.146714
18.079909	847.891104	14.151731
18.125941	845.586494	14.156749
17.985078	849.477634	14.161767
18.124382	853.716200	14.166784
17.934800	843.975529	14.171802
18.175245	851.196274	14.176819
17.997278	848.983564	14.181837
18.647810	847.900217	14.186855
17.998001	846.569326	14.191872
17.876712	847.834914	14.196890
17.995493	850.615551	14.201907
17.918924	850.870583	14.206925
18.020132	846.717487	14.211943
17.823271	854.312864	14.216960
18.128221	861.106937	14.221978
18.326934	870.410757	14.226995
18.519684	867.720237	14.232013
18.608436	872.247596	14.237031
18.299028	871.904789	14.242048
18.608196	871.758556	14.247066
18.487883	861.890257	14.252083
18.290618	854.912128	14.257101
18.377787	860.257088	14.262119
18.192965	869.403248	14.267136
18.663709	863.933076	14.272154
18.178866	866.303360	14.277171
18.414060	863.306388	14.282189
18.397934	859.938536	14.287207
18.470142	865.087026	14.292224
18.731933	867.636974	14.297242
18.574681	869.488870	14.302259
18.558288	869.216920	14.307277
18.802930	869.326950	14.312295
18.809344	852.275089	14.317312
19.141550	856.249900	14.322330
18.329917	843.435096	14.327347
18.721747	848.839616	14.332365
18.804635	853.774990	14.337383
18.634397	846.997757	14.342400
18.864722	849.041390	14.347418
18.690189	848.929917	14.352435
18.863313	860.715059	14.357453
19.061953	851.585747	14.362471
18.718106	836.390752	14.367488
18.777898	837.751045	14.372506
18.635141	835.602249	14.377523
18.684309	849.666368	14.382541
19.168862	849.899756	14.387559
18.674727	849.920410	14.392576
18.736235	845.710417	14.397594
18.873603	856.172559	14.402611
19.133367	858.079037	14.407629
19.368188	861.810331	14.412647
18.920740	843.213809	14.417664
18.792961	838.449650	14.422682
19.253551	852.222091	14.427699
18.927983	852.370969	14.432717
19.256220	846.768494	14.437735
18.866962	843.364434	14.442752
19.217030	847.926583	14.447770
19.321802	855.657738	14.452787
18.800552	845.827021	14.457805
19.103544	845.432445	14.462823
19.271156	857.136397	14.467840
19.284144	851.501263	14.472858
19.260969	844.287577	14.477875
18.609744	849.416865	14.482893
18.915110	844.487008	14.487911
18.974323	858.110902	14.492928
18.969685	855.047366	14.497946
19.318808	846.547734	14.502963
19.353260	859.285568	14.507981
19.163801	848.017459	14.512999
19.102159	848.746681	14.518016
19.159372	842.448211	14.523034
19.321372	849.356196	14.528051
19.066052	859.807283	14.533069
19.177645	849.624944	14.538087
19.360512	859.653924	14.543104
19.664338	860.796101	14.548122
19.411652	857.648352	14.553139
19.135058	858.957210	14.558157
19.792263	854.360390	14.563175
19.550575	872.575819	14.568192
19.431814	865.367634	14.573210
19.497080	869.021353	14.578227
19.333550	879.798898	14.583245
19.693886	878.136164	14.588263
19.403842	881.353248	14.593280
19.764172	872.441591	14.598298
20.049199	878.503486	14.603315
19.848690	877.585036	14.608333
19.604044	872.880204	14.613351
19.598336	885.412909	14.618368
19.949293	880.936649	14.623386
19.804251	879.940081	14.628403
19.553617	873.115474	14.633421
20.032325	877.139920	14.638439
19.768037	874.341126	14.643456
19.889591	879.052696	14.648474
19.991646	870.004780	14.653491
19.668811	862.976894	14.658509
20.036291	866.251901	14.663527
20.003716	874.635748	14.668544
19.922276	865.619740	14.673562
19.908816	859.909852	14.678579
19.531231	872.245192	14.683597
19.755803	870.632132	14.688615
19.678280	871.086131	14.693632
19.857211	881.084181	14.698650
19.962912	875.636486	14.703667
19.909716	885.320612	14.708685
19.989342	872.429260	14.713703
19.726997	865.530751	14.718720
19.605839	869.096914	14.723738
19.950109	869.450112	14.728755
20.159598	886.471393	14.733773
20.381039	891.334575	14.738791
20.156217	881.583626	14.743808
19.985652	876.097165	14.748826
20.410563	883.699278	14.753843
20.364754	896.762140	14.758861
20.566601	882.930130	14.763879
20.201896	878.474482	14.768896
20.397603	876.067522	14.773914
20.494777	874.859433	14.778931
20.479020	876.307306	14.783949
20.467991	870.432931	14.788967
20.517177	876.345583	14.793984
19.967785	866.191059	14.799002
20.484382	866.848617	14.804019
20.269593	868.857852	14.809037
20.503957	874.788828	14.814055
20.276196	874.546838	14.819072
20.108424	886.543200	14.824090
20.686148	889.902036	14.829107
20.228216	897.604608	14.834125
20.525069	892.404671	14.839143
20.427027	894.379837	14.844160
20.448990	902.408011	14.849178
20.677324	886.223913	14.854195
20.275572	894.987507	14.859213
20.221614	896.154186	14.864231
20.544653	889.631012	14.869248
20.474119	889.348609	14.874266
20.734512	888.291672	14.879283
20.610755	898.337157	14.884301
20.522229	880.852016	14.889319
20.555226	895.433105	14.894336
20.893131	906.810604	14.899354
21.479918	909.350664	14.904371
21.496131	897.053059	14.909389
21.275129	893.114538	14.914407
21.122597	884.668240	14.919424
20.815650	889.434327	14.924442
21.394575	883.988225	14.929459
21.006473	889.158350	14.934477
21.106044	885.078084	14.939495
20.994822	884.363397	14.944512
20.707520	889.782818	14.949530
21.049911	877.023863	14.954547
20.928584	880.927728	14.959565
21.150773	880.880329	14.964583
21.064093	873.159026	14.969600
20.945597	881.224977	14.974618
20.911101	878.071441	14.979635
21.077342	889.529474	14.984653
21.042700	877.268252	14.989671
20.870161	876.796703	14.994688
21.052361	880.899166	14.999706
21.349637	875.711791	15.004723
21.361640	882.299306	15.009741
21.251460	882.490176	15.014759
21.177964	879.159712	15.019776
21.180401	876.685202	15.024794
21.305623	876.198558	15.029811
20.995251	879.270503	15.034829
21.092206	878.286512	15.039847
21.206529	886.783049	15.044864
21.019870	900.240369	15.049882
21.549261	896.461989	15.054899
21.712969	905.938572	15.059917
21.820839	908.118164	15.064935
21.834466	893.728652	15.069952
21.555962	888.385332	15.074970
21.481565	875.107853	15.079987
21.254752	874.676366	15.085005
21.417767	891.518739	15.090023
22.006642	884.972851	15.095040
21.524328	902.986170	15.100058
21.734963	895.931491	15.105075
21.704897	899.723230	15.110093
21.522552	890.666215	15.115111
21.625510	898.823709	15.120128
21.808592	900.739051	15.125146
21.904531	890.467622	15.130163
21.562963	898.685297	15.135181
21.943946	905.719942	15.140199
21.785285	901.200447	15.145216
21.621334	907.686150	15.150234
21.705990	902.039772	15.155251
21.904762	900.127793	15.160269
21.662956	908.108934	15.165287
21.799700	896.966411	15.170304
22.155629	908.186452	15.175322
22.177804	894.644518	15.180339
22.171986	903.339769	15.185357
21.916459	904.370772	15.190375
21.990143	901.872472	15.195392
22.001422	909.908636	15.200410
21.748108	897.542805	15.205427
21.927536	902.280028	15.210445
21.695768	906.844991	15.215463
21.936081	904.298493	15.220480
21.662842	899.317265	15.225498
22.258939	892.426257	15.230515
22.348309	899.566549	15.235533
21.675225	886.019944	15.240551
22.065514	895.590410	15.245568
22.312924	906.619168	15.250586
22.053208	899.581377	15.255603
22.106610	908.810154	15.260621
21.860619	913.412061	15.265639
22.629334	908.169747	15.270656
22.311519	919.927705	15.275674
22.327045	918.830237	15.280691
22.479795	926.727477	15.285709
22.076856	924.827719	15.290727
22.370517	918.328073	15.295744
22.710901	917.706729	15.300762
22.262588	927.948250	15.305779
22.579736	918.689883	15.310797
22.634730	910.425655	15.315815
22.633135	913.878419	15.320832
22.435384	913.631726	15.325850
22.685886	913.778709	15.330867
22.713167	929.326405	15.335885
22.799009	919.813941	15.340903
22.980135	911.331133	15.345920
22.657209	922.203106	15.350938
22.264708	917.581388	15.355955
22.283525	912.892070	15.360973
22.755501	916.510479	15.365991
23.068692	914.526922	15.371008
22.820555	916.797009	15.376026
23.083604	916.200406	15.381043
22.950952	922.886340	15.386061
22.874940	919.032395	15.391079
22.633320	915.532604	15.396096
22.611549	918.540403	15.401114
22.617192	916.273670	15.406131
22.699512	913.805574	15.411149
22.608047	915.012846	15.416167
22.714451	918.843168	15.421184
22.590176	926.928980	15.426202
23.236020	930.766305	15.431219
23.037928	940.599396	15.436237
23.052366	941.891063	15.441255
23.237485	929.907801	15.446272
22.948475	937.454534	15.451290
22.949480	940.193678	15.456307
23.191141	933.673770	15.461325
23.207951	940.686591	15.466343
23.457106	936.267294	15.471360
23.424229	936.496547	15.476378
23.279199	947.858219	15.481395
23.402588	932.457390	15.486413
23.455749	938.965894	15.491431
23.868921	924.775690	15.496448
23.319461	922.640111	15.501466
23.225807	917.119496	15.506483
22.982786	910.224254	15.511501
23.128982	926.103612	15.516519
23.258325	927.418300	15.521536
23.428442	935.186589	15.526554
22.978842	937.106388	15.531571
23.120077	933.218402	15.536589
23.456520	931.082876	15.541607
23.319754	938.305952	15.546624
23.000174	937.147377	15.551642
23.082930	941.495810	15.556659
23.420236	955.574829	15.561677
23.431935	958.713091	15.566695
24.115407	960.351220	15.571712
24.080103	960.520892	15.576730
24.225584	949.424306	15.581747
23.922212	936.138476	15.586765
23.802436	941.206613	15.591783
23.784437	933.679652	15.596800
23.940032	939.307408	15.601818
23.822065	935.419007	15.606835
23.886098	931.076053	15.611853
23.666986	921.431486	15.616871
23.810833	928.768384	15.621888
24.276465	936.752307	15.626906
23.953933	941.707044	15.631923
23.684192	932.714193	15.636941
23.607760	927.563265	15.641959
23.985899	926.623578	15.646976
23.757016	939.510027	15.651994
23.964558	947.831041	15.657011
24.140794	956.605092	15.662029
24.135284	960.626529	15.667047
24.055099	955.293142	15.672064
24.328739	958.936322	15.677082
24.258349	959.430232	15.682099
24.421675	956.005843	15.687117
24.185018	963.506514	15.692135
24.254758	954.586697	15.697152
24.582176	958.969385	15.702170
24.477383	956.713639	15.707187
24.514349	933.026501	15.712205
23.832484	927.203565	15.717223
24.435209	933.982569	15.722240
24.466797	943.479872	15.727258
24.515708	937.129020	15.732275
24.396824	929.520037	15.737293
24.370731	936.258709	15.742311
24.566574	941.491993	15.747328
24.384143	946.699337	15.752346
24.105280	948.901658	15.757363
24.684548	958.167990	15.762381
24.880480	951.901396	15.767399
24.667817	949.220735	15.772416
24.671298	957.046700	15.777434
24.582289	948.214875	15.782451
25.152796	950.867947	15.787469
24.443932	942.007010	15.792487
24.600451	934.894522	15.797504
24.366894	945.380119	15.802522
24.517008	963.894019	15.807539
24.466779	950.338140	15.812557
24.235467	953.770098	15.817575
24.476927	956.200168	15.822592
24.572704	951.382016	15.827610
24.526673	957.199160	15.832627
24.754341	968.843282	15.837645
24.720693	980.225394	15.842663
24.846576	968.169335	15.847680
24.789187	984.954811	15.852698
24.802844	977.340820	15.857715
25.118873	970.970195	15.862733
25.107282	975.832042	15.867751
25.153172	973.385425	15.872768
25.334466	971.192151	15.877786
25.065521	977.479734	15.882803
25.346707	968.810805	15.887821
25.078724	974.239848	15.892839
25.474705	968.380566	15.897856
25.409527	973.402288	15.902874
25.168569	973.055066	15.907891
25.472751	974.572741	15.912909
25.233681	970.236242	15.917927
25.520090	968.853329	15.922944
25.349782	969.463881	15.927962
25.419900	973.886886	15.932979
25.277073	966.101756	15.937997
25.459844	979.109930	15.943015
25.704301	973.198647	15.948032
25.477489	961.649138	15.953050
25.391390	975.617784	15.958067
25.592861	970.877743	15.963085
25.582797	975.676233	15.968103
25.399794	974.549906	15.973120
25.489652	979.862923	15.978138
25.399577	966.966533	15.983155
25.576820	973.089530	15.988173
25.384023	977.881938	15.993191
25.400601	971.046984	15.998208
25.737222	965.146511	16.003226
25.569280	969.998138	16.008243
25.781926	966.190475	16.013261
25.604146	971.706371	16.018279
25.644336	968.272870	16.023296
25.874116	965.229392	16.028314
25.836401	976.627918	16.033331
25.518380	967.857211	16.038349
25.622933	968.342646	16.043367
25.662862	978.460360	16.048384
25.990584	991.212300	16.053402
26.012993	997.709864	16.058419
25.742654	993.324609	16.063437
26.090787	994.090621	16.068455
25.816645	988.554080	16.073472
26.147391	989.064036	16.078490
25.844157	993.864284	16.083507
26.164310	989.288681	16.088525
26.053656	989.994029	16.093543
26.055950	993.146394	16.098560
26.220961	992.975409	16.103578
26.049505	987.337572	16.108595
26.013303	989.088463	16.113613
25.970503	989.511777	16.118631
26.149455	1000.974203	16.123648
26.607771	1013.563684	16.128666
26.302807	994.480770	16.133683
26.526909	1003.436695	16.138701
26.350985	1010.366131	16.143719
26.458865	1006.975666	16.148736
26.776744	1004.600040	16.153754
26.497976	1004.681625	16.158771
26.345765	990.671473	16.163789
26.484806	1004.633270	16.168807
26.451891	1013.481144	16.173824
26.797289	1013.739494	16.178842
26.701720	1012.899271	16.183859
26.629845	1003.544019	16.188877
26.806206	1005.024918	16.193895
26.494468	996.713966	16.198912
26.576322	995.180062	16.203930
26.829476	1009.685724	16.208947
26.534195	1016.305654	16.213965
26.847348	1011.633311	16.218983
26.926831	1011.425233	16.224000
26.790151	1010.354762	16.229018
26.689097	1010.657815	16.234035
26.963212	1003.959225	16.239053
26.634264	998.027321	16.244071
26.659800	1009.804127	16.249088
26.820358	999.102784	16.254106
26.609153	1012.513542	16.259123
26.940471	1009.959082	16.264141
26.882751	1000.917198	16.269159
27.065640	1009.421986	16.274176
27.108365	1002.627106	16.279194
26.969110	1009.910562	16.284211
26.905177	1010.091032	16.289229
27.353042	1027.352814	16.294247
27.382688	1038.813410	16.299264
27.439471	1019.282466	16.304282
27.138057	1007.621537	16.309299
27.318594	1017.199685	16.314317
27.282161	1019.411368	16.319335
27.212666	1035.416138	16.324352
27.571138	1031.743405	16.329370
27.614777	1026.753519	16.334387
27.349678	1018.719276	16.339405
27.659978	1034.920163	16.344423
27.591952	1022.995436	16.349440
27.316503	1013.874049	16.354458
27.498632	1027.103267	16.359475
27.149510	1025.845172	16.364493
27.402037	1030.498391	16.369511
27.517186	1032.437014	16.374528
27.816327	1032.721547	16.379546
27.826985	1029.611402	16.384563
27.891041	1031.207731	16.389581
27.801976	1040.853379	16.394599
27.516285	1030.001026	16.399616
27.883955	1026.090165	16.404634
28.177076	1036.707893	16.409651
27.602251	1024.827855	16.414669
27.791505	1019.534286	16.419687
27.562909	1023.082598	16.424704
27.925720	1023.549661	16.429722
27.831387	1031.129049	16.434739
27.997303	1027.227708	16.439757
28.097319	1018.208439	16.444775
28.010959	1026.502954	16.449792
28.189258	1023.896727	16.454810
27.747654	1030.094613	16.459827
27.993023	1017.451747	16.464845
27.883171	1018.475711	16.469863
27.641107	1029.947315	16.474880
28.115071	1025.770488	16.479898
27.846690	1049.292106	16.484915
28.067749	1059.851710	16.489933
28.397184	1052.951928	16.494951
28.443182	1057.340863	16.499968
28.366675	1043.151548	16.504986
28.418022	1046.668627	16.510003
28.099806	1056.861436	16.515021
28.764130	1051.117876	16.520039
28.561544	1057.751701	16.525056
28.747414	1049.403786	16.530074
28.285026	1045.689247	16.535091
28.511423	1054.329253	16.540109
28.622052	1040.959544	16.545127
28.294221	1062.051020	16.550144
28.703018	1040.612412	16.555162
28.649167	1051.600098	16.560179
28.585449	1050.496102	16.565197
28.523036	1043.149626	16.570215
28.681214	1049.600690	16.575232
28.704774	1048.880657	16.580250
28.715834	1046.676176	16.585267
28.898113	1045.082351	16.590285
29.093690	1036.546726	16.595303
28.624010	1049.975918	16.600320
28.923756	1038.375416	16.605338
28.848680	1041.189613	16.610355
28.516479	1039.193551	16.615373
28.721677	1041.316885	16.620391
28.573020	1053.518650	16.625408
28.790199	1040.012325	16.630426
28.736756	1050.397178	16.635443
29.204273	1070.657140	16.640461
29.233172	1060.115246	16.645479
29.431044	1073.689177	16.650496
29.189160	1058.736796	16.655514
29.312670	1053.996324	16.660531
28.957856	1057.065794	16.665549
29.254201	1058.461626	16.670567
29.618752	1071.050060	16.675584
29.536871	1050.518309	16.680602
29.479668	1053.471721	16.685619
29.117272	1047.781729	16.690637
29.454603	1042.610121	16.695655
29.516902	1056.691282	16.700672
29.434165	1050.474627	16.705690
29.752847	1050.989631	16.710707
29.486915	1043.119612	16.715725
29.374592	1036.907597	16.720743
29.290417	1043.393474	16.725760
29.624104	1047.645812	16.730778
29.299513	1056.700357	16.735795
29.415515	1070.605854	16.740813
29.590318	1063.032851	16.745831
29.550620	1070.493241	16.750848
29.698289	1069.980984	16.755866
30.010558	1068.795987	16.760883
29.725201	1061.541239	16.765901
29.972931	1067.678472	16.770919
29.731128	1062.815350	16.775936
29.461355	1066.259668	16.780954
29.510791	1064.626694	16.785971
29.590328	1061.748753	16.790989
29.883515	1062.627519	16.796007
29.758187	1078.366516	16.801024
30.071282	1074.461040	16.806042
30.230229	1074.249978	16.811059
29.954929	1085.543784	16.816077
30.142291	1085.533401	16.821095
30.138655	1078.758379	16.826112
30.293994	1073.586874	16.831130
30.435874	1087.857566	16.836147
30.127594	1086.290104	16.841165
30.385861	1075.197859	16.846183
30.736605	1088.063028	16.851200
30.661406	1076.808431	16.856218
30.411664	1063.258478	16.861235
30.304714	1062.319048	16.866253
30.093934	1047.103023	16.871271
30.257129	1072.359046	16.876288
30.078296	1072.282959	16.881306
30.339506	1086.705370	16.886323
30.376009	1085.948593	16.891341
30.392041	1073.799219	16.896359
30.428328	1074.970706	16.901376
30.798165	1078.485229	16.906394
30.765114	1075.000066	16.911411
30.602395	1079.222889	16.916429
30.817485	1076.093329	16.921447
30.357764	1082.840036	16.926464
30.563221	1076.335217	16.931482
30.731069	1076.479372	16.936499
30.759706	1084.617038	16.941517
31.028098	1069.726712	16.946535
31.065888	1076.221894	16.951552
30.616632	1076.349126	16.956570
30.844974	1074.271547	16.961587
30.622326	1080.652899	16.966605
31.274464	1082.851382	16.971623
30.768870	1084.577993	16.976640
30.882020	1096.287480	16.981658
31.523114	1094.514465	16.986675
30.956379	1093.561863	16.991693
31.279605	1090.118708	16.996711
31.454806	1098.842498	17.001728
31.086852	1083.326014	17.006746
31.262006	1089.578769	17.011763
31.236712	1101.126910	17.016781
31.478408	1090.498008	17.021799
31.376072	1096.137824	17.026816
31.434480	1097.069156	17.031834
31.563509	1098.380751	17.036851
31.247746	1096.394731	17.041869
31.647927	1092.412489	17.046887
31.701994	1081.734093	17.051904
31.052040	1073.128952	17.056922
31.373690	1094.838243	17.061939
31.269004	1088.303116	17.066957
31.163060	1079.584334	17.071975
31.083351	1089.739792	17.076992
31.272991	1091.158657	17.082010
31.826660	1097.623514	17.087027
31.758479	1093.266522	17.092045
31.875850	1099.310579	17.097063
31.715220	1095.507724	17.102080
31.622304	1110.503199	17.107098
31.670589	1106.475101	17.112115
31.775025	1111.047401	17.117133
32.094827	1103.347519	17.122151
32.074286	1117.990828	17.127168
31.911002	1111.805707	17.132186
32.334089	1110.290914	17.137203
32.498262	1109.457328	17.142221
32.342738	1113.170937	17.147239
32.367653	1091.372684	17.152256
31.949722	1089.509972	17.157274
32.272111	1081.976955	17.162291
32.153614	1082.768743	17.167309
31.985150	1081.176220	17.172327
32.400281	1102.410119	17.177344
31.948895	1111.276270	17.182362
32.340894	1108.497690	17.187379
32.304714	1102.084371	17.192397
32.407861	1109.875853	17.197415
32.609070	1107.811989	17.202432
32.303196	1105.268986	17.207450
32.835017	1112.927032	17.212467
32.401861	1113.102235	17.217485
32.608691	1105.991264	17.222503
32.801039	1108.618402	17.227520
32.502759	1109.043877	17.232538
32.615104	1092.672634	17.237555
32.713082	1098.413611	17.242573
32.856947	1102.096090	17.247591
32.666703	1095.785808	17.252608
32.563671	1101.747632	17.257626
32.634203	1097.870688	17.262643
32.690911	1110.106588	17.267661
32.839536	1106.618201	17.272679
32.862522	1107.690786	17.277696
32.923484	1108.000014	17.282714
32.994354	1104.088301	17.287731
32.715059	1113.536571	17.292749
32.578295	1104.936217	17.297767
32.426881	1104.275155	17.302784
32.433480	1122.527679	17.307802
32.847510	1117.766918	17.312819
32.779272	1124.632188	17.317837
33.128324	1122.090714	17.322855
32.693069	1119.627942	17.327872
32.974055	1130.392797	17.332890
33.072928	1136.266193	17.337907
33.139460	1138.894113	17.342925
33.129424	1141.713914	17.347943
33.473345	1132.132498	17.352960
33.374335	1143.935219	17.357978
33.884679	1150.122855	17.362995
33.511759	1148.161563	17.368013
33.579157	1143.502444	17.373031
33.847663	1135.867391	17.378048
33.753329	1144.510355	17.383066
33.852981	1151.390356	17.388083
33.509766	1140.004139	17.393101
33.975066	1141.865821	17.398119
34.066043	1132.131529	17.403136
33.868021	1120.441703	17.408154
33.606578	1112.340571	17.413171
33.858141	1124.066260	17.418189
33.891672	1135.447413	17.423207
33.912852	1139.704555	17.428224
33.726012	1137.051377	17.433242
34.175610	1135.712313	17.438259
34.037502	1139.195977	17.443277
33.883038	1148.050340	17.448295
33.935510	1139.922102	17.453312
33.986327	1137.878642	17.458330
34.152074	1130.269160	17.463347
33.885219	1133.845579	17.468365
33.866815	1138.020558	17.473383
33.989022	1142.940384	17.478400
33.516410	1143.200666	17.483418
33.975903	1139.158627	17.488435
34.239148	1154.862057	17.493453
34.245016	1161.759912	17.498471
34.326928	1159.689486	17.503488
34.185113	1156.915640	17.508506
34.400078	1161.735729	17.513523
34.489937	1160.645534	17.518541
34.649821	1162.413057	17.523559
34.840549	1160.593832	17.528576
34.598611	1151.290394	17.533594
34.621646	1160.167446	17.538611
34.669903	1158.547272	17.543629
34.666397	1153.432190	17.548647
34.967792	1156.067496	17.553664
34.668148	1159.002105	17.558682
34.766655	1159.201307	17.563699
34.590128	1153.864020	17.568717
34.890776	1155.855646	17.573735
35.094738	1150.427186	17.578752
34.702966	1156.472138	17.583770
34.961491	1149.577117	17.588787
35.100961	1137.701856	17.593805
34.982055	1149.135304	17.598823
34.913832	1147.422925	17.603840
34.760523	1149.693963	17.608858
34.848145	1149.020695	17.613875
35.075379	1148.527528	17.618893
34.717623	1157.246485	17.623911
35.230917	1159.463575	17.628928
35.502111	1180.208868	17.633946
35.480768	1175.308018	17.638963
35.340681	1166.086447	17.643981
35.324741	1159.565792	17.648999
35.682227	1161.741021	17.654016
35.254920	1157.254084	17.659034
35.275271	1152.488722	17.664051
35.300407	1167.418411	17.669069
35.732212	1167.492808	17.674087
35.447752	1174.874823	17.679104
35.584364	1177.902032	17.684122
35.664644	1173.969894	17.689139
35.589921	1170.731087	17.694157
35.689410	1173.240237	17.699175
36.026614	1167.491088	17.704192
35.569270	1178.217015	17.709210
35.314067	1175.574543	17.714227
35.610494	1171.914660	17.719245
35.493592	1174.211555	17.724263
35.936478	1169.641924	17.729280
35.809621	1173.691889	17.734298
35.844327	1180.162346	17.739315
36.017741	1187.554680	17.744333
36.123358	1196.178964	17.749351
36.273897	1191.005021	17.754368
36.069250	1201.530420	17.759386
36.259206	1196.132545	17.764403
36.275737	1196.230980	17.769421
36.140788	1196.810752	17.774439
36.250309	1182.674231	17.779456
36.106566	1199.347203	17.784474
36.451370	1203.392706	17.789491
36.335837	1193.551877	17.794509
36.281220	1193.465795	17.799527
36.218639	1195.208215	17.804544
36.646773	1187.036878	17.809562
36.446961	1184.474090	17.814579
36.674347	1186.672862	17.819597
36.471638	1185.846261	17.824615
36.853439	1186.177807	17.829632
36.689956	1196.829301	17.834650
36.651171	1189.857768	17.839667
36.953504	1187.847480	17.844685
36.688622	1197.296692	17.849703
36.870595	1198.038253	17.854720
36.852493	1189.646489	17.859738
37.044228	1193.081640	17.864755
37.146609	1192.371343	17.869773
36.873003	1195.983548	17.874791
37.037074	1190.021671	17.879808
36.836195	1196.216613	17.884826
36.687595	1192.695880	17.889843
36.826864	1178.021359	17.894861
36.569746	1195.441099	17.899879
37.063625	1201.038027	17.904896
37.508767	1212.256907	17.909914
37.123134	1215.842485	17.914931
37.350925	1205.909988	17.919949
37.272159	1222.932572	17.924967
37.263135	1211.765353	17.929984
37.583617	1216.180752	17.935002
37.198684	1209.818879	17.940019
37.276531	1214.385905	17.945037
37.120755	1217.954405	17.950055
37.347729	1204.743074	17.955072
37.581924	1200.802594	17.960090
37.548263	1212.206947	17.965107
37.590431	1211.016922	17.970125
37.518435	1215.780998	17.975143
37.866790	1215.290944	17.980160
37.621815	1208.850338	17.985178
37.581752	1215.114766	17.990195
37.930499	1223.240212	17.995213
37.780978	1222.203299	18.000231
37.807323	1225.528666	18.005248
37.919981	1227.975798	18.010266
38.126637	1227.419580	18.015283
38.117303	1220.503382	18.020301
38.435017	1224.903437	18.025319
38.272923	1214.618600	18.030336
38.285741	1210.394059	18.035354
37.961553	1200.882571	18.040371
38.195399	1212.806759	18.045389
38.206953	1228.199385	18.050407
38.412987	1228.031438	18.055424
38.649356	1227.861895	18.060442
38.459113	1235.210237	18.065459
38.267976	1219.568098	18.070477
38.249737	1234.520419	18.075495
38.484085	1229.633143	18.080512
38.863785	1223.706900	18.085530
38.395885	1229.044262	18.090547
38.405251	1218.480089	18.095565
38.579707	1231.483439	18.100583
38.783869	1221.816573	18.105600
38.693752	1220.953394	18.110618
38.715448	1221.401323	18.115635
38.438646	1219.011543	18.120653
38.338353	1222.694431	18.125671
38.461174	1215.495590	18.130688
38.826032	1214.261319	18.135706
38.658350	1227.327739	18.140723
39.272166	1233.593869	18.145741
39.025759	1234.071181	18.150759
39.089371	1244.892255	18.155776
39.056607	1241.899333	18.160794
38.667626	1244.911070	18.165811
38.990416	1247.918588	18.170829
38.990158	1245.494944	18.175847
39.045185	1244.220849	18.180864
39.187560	1240.212694	18.185882
39.218235	1242.357084	18.190899
39.332293	1233.032542	18.195917
39.075684	1239.602313	18.200935
39.297361	1234.852724	18.205952
39.199228	1231.008489	18.210970
39.156116	1257.256486	18.215987
39.588446	1263.775130	18.221005
39.565931	1262.926605	18.226023
39.913979	1266.905340	18.231040
39.905698	1268.563518	18.236058
39.570749	1263.907444	18.241075
39.886405	1264.738519	18.246093
40.205992	1269.457036	18.251111
39.970357	1244.328926	18.256128
39.829184	1234.069203	18.261146
39.845009	1235.152386	18.266163
39.834350	1231.739425	18.271181
39.562948	1237.131212	18.276199
40.174656	1252.319372	18.281216
40.140070	1243.570394	18.286234
40.006863	1252.197410	18.291251
40.082870	1254.678691	18.296269
40.052713	1253.733530	18.301287
40.153029	1255.232677	18.306304
40.712710	1255.066128	18.311322
40.472681	1259.660878	18.316339
40.460763	1255.774726	18.321357
40.325949	1249.670304	18.326375
40.236155	1252.218589	18.331392
40.368910	1247.372473	18.336410
40.574232	1251.196837	18.341427
40.596848	1253.011123	18.346445
40.378573	1252.546729	18.351463
40.287201	1248.638312	18.356480
40.575556	1254.087573	18.361498
40.225320	1256.717691	18.366515
40.744830	1249.737559	18.371533
40.451172	1252.002195	18.376551
40.358722	1251.104666	18.381568
40.746711	1255.951322	18.386586
40.511886	1277.905818	18.391603
40.839861	1275.465458	18.396621
40.974759	1277.227440	18.401639
40.780684	1282.408303	18.406656
41.226197	1271.968273	18.411674
41.121239	1280.919089	18.416691
41.073495	1280.326986	18.421709
41.142046	1272.514915	18.426727
41.144943	1284.500583	18.431744
41.355012	1270.928924	18.436762
41.343041	1287.231028	18.441779
41.580996	1282.614580	18.446797
41.253281	1278.437065	18.451815
41.342435	1274.490891	18.456832
41.641052	1264.547264	18.461850
41.129760	1269.926151	18.466867
41.073391	1272.484981	18.471885
41.723857	1292.410411	18.476903
41.631129	1299.544680	18.481920
42.003229	1304.557945	18.486938
41.928304	1303.427287	18.491955
41.739482	1276.098448	18.496973
41.796575	1283.938249	18.501991
41.508261	1275.083838	18.507008
41.666662	1281.112061	18.512026
41.551543	1305.897610	18.517043
41.799461	1290.540079	18.522061
41.989170	1291.201534	18.527079
42.152683	1289.355001	18.532096
42.162508	1295.602173	18.537114
41.731290	1303.180809	18.542131
42.003311	1296.656013	18.547149
42.154934	1293.381721	18.552167
42.360113	1298.351708	18.557184
42.326333	1294.610988	18.562202
41.963120	1294.137742	18.567219
42.248393	1304.687431	18.572237
41.997753	1297.815322	18.577255
41.550976	1311.304239	18.582272
42.399510	1310.429694	18.587290
42.039687	1333.508408	18.592307
42.025528	1326.416194	18.597325
42.308763	1317.330198	18.602343
42.368377	1335.722960	18.607360
42.907652	1334.297246	18.612378
42.639178	1341.515873	18.617395
43.105304	1344.759736	18.622413
43.072598	1341.861465	18.627431
42.840849	1322.198664	18.632448
43.037550	1321.909099	18.637466
42.812995	1325.027635	18.642483
42.809434	1330.061895	18.647501
43.197038	1332.484899	18.652519
42.982667	1341.083647	18.657536
43.209710	1329.241876	18.662554
43.391476	1330.198076	18.667571
43.399724	1328.492634	18.672589
43.774525	1317.429319	18.677607
43.460441	1312.258708	18.682624
43.571356	1301.321958	18.687642
43.117141	1306.609860	18.692659
42.983892	1301.218409	18.697677
43.618427	1307.089989	18.702695
43.735672	1324.937208	18.707712
43.673201	1313.424839	18.712730
43.581445	1306.221711	18.717747
43.164951	1303.998977	18.722765
43.432581	1314.803908	18.727783
43.460678	1318.046965	18.732800
43.532894	1327.471833	18.737818
43.859280	1322.024141	18.742835
43.616548	1320.477947	18.747853
43.633295	1320.573193	18.752871
43.326945	1323.859183	18.757888
43.896762	1332.278256	18.762906
44.404549	1337.014644	18.767923
44.192894	1332.061515	18.772941
43.975400	1326.822115	18.777959
44.232054	1340.784685	18.782976
44.201866	1342.250636	18.787994
44.253744	1339.373828	18.793011
44.533835	1342.990831	18.798029
44.735608	1328.928106	18.803047
44.228635	1326.934147	18.808064
44.403475	1320.809588	18.813082
44.276311	1330.587599	18.818099
44.581363	1340.253713	18.823117
44.550243	1334.824159	18.828135
44.692562	1342.044699	18.833152
44.750248	1339.728732	18.838170
44.441329	1344.731941	18.843187
44.333757	1352.711183	18.848205
44.296335	1343.650166	18.853223
44.342986	1346.956595	18.858240
44.699211	1347.841279	18.863258
44.300025	1339.622765	18.868275
44.849224	1351.046343	18.873293
45.284882	1360.335388	18.878311
44.904999	1366.274402	18.883328
45.106745	1378.115365	18.888346
45.269720	1367.949927	18.893363
45.305361	1370.204012	18.898381
45.287208	1358.921363	18.903399
45.045552	1371.456662	18.908416
45.131248	1373.362066	18.913434
44.858097	1372.410789	18.918451
45.198421	1370.280916	18.923469
45.495096	1361.240130	18.928487
45.678898	1364.963745	18.933504
45.471673	1360.546419	18.938522
45.474306	1365.371428	18.943539
45.493551	1370.724029	18.948557
45.695810	1363.594736	18.953575
45.545335	1365.306761	18.958592
45.587085	1360.042513	18.963610
45.435983	1361.300185	18.968627
45.376533	1374.718996	18.973645
46.157011	1376.259916	18.978663
45.759763	1386.591530	18.983680
46.077514	1378.554170	18.988698
45.737199	1387.169516	18.993715
45.911246	1381.991835	18.998733
46.230026	1377.665667	19.003751
46.240781	1384.831095	19.008768
46.087249	1386.246945	19.013786
46.382698	1384.789999	19.018803
46.022208	1386.329796	19.023821
46.356521	1373.795823	19.028839
46.610632	1391.568015	19.033856
46.279963	1384.096164	19.038874
46.498830	1383.487534	19.043891
46.534610	1376.277019	19.048909
46.397435	1380.442261	19.053927
46.018866	1381.823938	19.058944
46.121447	1379.440969	19.063962
46.757395	1378.236799	19.068979
46.810529	1384.171094	19.073997
46.838340	1386.704128	19.079015
47.107198	1401.687348	19.084032
46.530352	1389.889435	19.089050
46.664405	1395.485996	19.094067
46.535524	1401.433034	19.099085
46.944093	1393.558169	19.104103
46.587762	1403.441554	19.109120
46.792908	1405.495510	19.114138
47.031000	1394.210562	19.119155
46.662354	1406.292395	19.124173
47.086570	1403.868498	19.129191
47.371468	1426.079431	19.134208
47.310323	1417.678524	19.139226
47.201080	1420.879999	19.144243
47.019588	1430.575054	19.149261
47.477704	1415.894565	19.154279
47.220756	1421.410379	19.159296
47.145073	1420.295611	19.164314
47.404056	1417.859730	19.169331
47.392777	1439.612136	19.174349
47.852491	1438.826909	19.179367
47.909058	1444.091630	19.184384
47.857425	1441.234179	19.189402
48.486964	1448.586717	19.194419
48.086738	1434.741309	19.199437
47.808696	1413.656029	19.204455
47.746975	1421.789070	19.209472
47.623116	1434.353296	19.214490
47.935562	1437.359312	19.219507
48.005434	1442.931229	19.224525
48.062360	1433.804888	19.229543
48.155114	1445.524112	19.234560
48.037584	1448.635369	19.239578
48.141338	1441.130145	19.244595
48.088179	1446.879134	19.249613
48.343380	1439.192387	19.254631
48.520538	1449.374079	19.259648
48.614720	1454.819109	19.264666
48.529416	1455.855031	19.269683
48.474602	1466.836811	19.274701
48.475333	1458.161093	19.279719
48.459715	1453.129877	19.284736
48.643483	1460.347126	19.289754
48.945862	1466.826244	19.294771
48.948838	1466.478663	19.299789
48.924459	1459.315411	19.304807
48.999661	1463.412682	19.309824
49.118692	1459.963578	19.314842
49.480369	1455.731660	19.319859
49.098471	1465.256153	19.324877
49.340340	1454.327196	19.329895
49.468925	1458.046858	19.334912
49.202201	1457.473279	19.339930
49.411508	1440.101878	19.344947
49.297367	1458.010731	19.349965
49.684465	1445.234900	19.354983
49.456997	1458.863142	19.360000
49.664178	1455.999854	19.365018
49.606420	1442.107096	19.370035
49.365969	1438.761658	19.375053
49.587613	1437.306804	19.380071
49.358478	1438.889143	19.385088
49.606866	1439.702363	19.390106
49.630855	1441.121963	19.395123
49.703629	1437.260373	19.400141
49.407136	1442.817104	19.405159
49.504080	1444.449345	19.410176
49.575265	1445.899421	19.415194
49.770929	1453.039062	19.420211
49.927754	1464.366393	19.425229
49.790899	1464.040720	19.430247
50.117508	1469.490366	19.435264
50.059428	1469.057673	19.440282
50.199016	1468.931695	19.445299
50.055374	1475.341836	19.450317
50.109997	1468.260881	19.455335
50.362904	1474.564708	19.460352
50.000430	1489.031511	19.465370
50.262858	1496.375312	19.470387
50.303009	1501.147141	19.475405
50.323753	1492.181081	19.480423
50.787266	1485.307465	19.485440
50.765803	1495.169994	19.490458
50.962976	1489.038724	19.495475
50.676458	1494.723301	19.500493
50.916219	1475.409352	19.505511
50.921394	1480.489624	19.510528
50.752960	1480.298292	19.515546
51.376923	1486.218927	19.520563
50.737911	1483.150529	19.525581
50.909766	1485.143436	19.530599
51.160012	1491.646510	19.535616
51.169353	1505.698452	19.540634
51.293020	1507.506399	19.545651
51.159140	1510.415092	19.550669
51.370816	1504.546643	19.555687
51.551672	1506.269887	19.560704
51.632105	1504.180718	19.565722
51.437065	1497.811082	19.570739
51.655822	1504.057152	19.575757
51.509092	1504.465202	19.580775
51.611164	1500.116151	19.585792
51.665502	1498.091034	19.590810
51.486786	1492.400523	19.595827
51.567052	1500.684930	19.600845
51.593722	1494.179568	19.605863
51.611267	1501.438657	19.610880
51.553358	1514.977258	19.615898
52.051938	1522.359813	19.620915
52.048994	1533.210425	19.625933
52.027251	1528.464182	19.630951
52.200663	1522.645905	19.635968
52.284435	1524.561094	19.640986
52.336315	1522.965567	19.646003
52.157741	1523.612146	19.651021
52.133391	1520.235991	19.656039
52.513697	1519.775639	19.661056
52.172465	1527.640084	19.666074
52.688559	1515.165898	19.671091
52.552348	1515.256707	19.676109
52.660002	1515.552315	19.681127
52.565573	1521.162622	19.686144
52.522321	1521.194683	19.691162
52.773967	1522.124166	19.696179
52.557290	1527.409631	19.701197
52.682523	1538.050808	19.706215
53.005008	1539.366842	19.711232
52.777882	1552.303951	19.716250
53.065187	1548.569678	19.721267
52.998541	1543.050949	19.726285
52.924773	1546.007037	19.731303
53.242915	1547.251165	19.736320
52.899791	1541.166657	19.741338
53.252164	1540.174172	19.746355
53.234909	1541.193125	19.751373
53.415565	1544.175625	19.756391
53.844678	1556.766913	19.761408
53.537882	1550.017118	19.766426
53.084069	1551.035040	19.771443
53.616856	1556.878462	19.776461
53.584712	1564.176921	19.781479
54.070223	1558.398100	19.786496
53.531620	1571.548133	19.791514
53.867751	1565.657009	19.796531
53.850709	1558.984895	19.801549
53.882761	1557.098968	19.806567
54.160700	1557.999086	19.811584
54.108416	1551.098957	19.816602
54.197658	1559.808038	19.821619
54.168672	1564.420294	19.826637
53.703584	1557.436510	19.831655
54.008807	1551.622819	19.836672
54.172903	1562.516709	19.841690
54.437465	1563.680867	19.846707
54.602508	1580.586694	19.851725
54.367620	1578.493268	19.856743
54.510706	1573.512896	19.861760
54.893329	1570.136087	19.866778
54.804974	1571.715316	19.871795
54.717696	1571.782679	19.876813
54.835783	1580.269490	19.881831
54.770260	1570.578415	19.886848
55.035805	1575.333885	19.891866
54.765102	1564.330527	19.896883
54.743108	1571.195034	19.901901
54.766910	1575.126807	19.906919
54.860566	1568.812903	19.911936
55.357838	1566.437502	19.916954
55.004408	1561.942042	19.921971
55.560282	1565.632652	19.926989
55.159686	1572.578570	19.932007
55.446439	1565.041466	19.937024
55.211662	1565.715788	19.942042
55.345683	1559.212519	19.947059
55.409610	1571.125698	19.952077
55.207126	1589.035900	19.957095
55.499180	1594.822373	19.962112
55.418650	1599.123963	19.967130
55.831731	1586.107265	19.972147
55.542066	1592.944288	19.977165
55.431872	1592.911095	19.982183
55.531989	1595.678994	19.987200
55.483520	1590.122686	19.992218
55.878163	1604.581419	19.997235
56.199263	1606.115435	20.002253
56.218847	1616.773212	20.007271
56.438906	1618.932159	20.012288
56.665745	1614.793917	20.017306
56.277857	1595.038508	20.022323
56.530005	1598.817739	20.027341
56.470872	1601.556938	20.032359
56.337434	1593.318761	20.037376
56.654351	1600.657224	20.042394
56.733817	1604.564502	20.047411
56.702215	1608.640668	20.052429
56.702456	1610.344882	20.057447
56.895608	1601.159242	20.062464
56.782032	1611.519127	20.067482
56.587212	1602.135484	20.072499
56.766192	1608.261585	20.077517
56.393861	1605.031456	20.082535
56.741865	1600.186236	20.087552
56.999595	1598.145021	20.092570
56.827762	1609.656487	20.097587
57.220640	1611.627403	20.102605
56.802641	1624.105296	20.107623
57.388886	1626.882246	20.112640
57.338695	1624.766189	20.117658
57.249833	1626.717906	20.122675
57.321442	1633.094378	20.127693
57.207293	1629.858509	20.132711
57.180541	1629.575546	20.137728
57.406745	1628.419778	20.142746
57.230914	1635.106432	20.147763
57.887046	1636.761537	20.152781
57.626076	1659.266578	20.157799
57.793026	1652.281566	20.162816
58.050361	1651.887818	20.167834
58.132490	1659.657585	20.172851
58.209666	1656.183442	20.177869
58.149768	1662.586841	20.182887
58.058121	1646.392226	20.187904
58.291615	1655.227083	20.192922
58.242569	1653.811466	20.197939
58.274806	1641.728598	20.202957
58.076340	1650.956194	20.207975
58.425005	1646.290748	20.212992
58.181060	1650.554834	20.218010
58.301688	1658.662570	20.223027
58.947810	1664.324161	20.228045
58.613293	1675.826442	20.233063
58.785654	1671.052906	20.238080
58.715663	1671.578331	20.243098
58.770255	1673.750586	20.248115
59.110253	1663.775007	20.253133
58.743270	1675.904099	20.258151
58.806554	1667.742369	20.263168
59.060379	1663.473649	20.268186
59.243767	1662.498165	20.273203
59.302653	1671.890589	20.278221
59.168001	1672.700713	20.283239
59.126714	1663.886304	20.288256
59.391941	1662.238402	20.293274
59.097783	1667.794837	20.298291
59.336877	1663.509489	20.303309
59.574813	1680.552320	20.308327
59.904718	1686.067792	20.313344
59.798154	1679.409660	20.318362
59.278483	1675.170602	20.323379
59.698425	1678.358643	20.328397
59.730918	1683.068601	20.333415
59.887839	1683.539539	20.338432
59.660318	1683.578380	20.343450
59.830313	1691.015642	20.348467
60.076310	1672.284358	20.353485
59.840753	1678.566953	20.358503
59.962635	1685.238541	20.363520
59.889441	1683.195512	20.368538
59.948074	1684.335134	20.373555
60.222971	1700.952451	20.378573
60.303996	1700.248637	20.383591
60.297594	1697.292535	20.388608
60.858955	1704.567495	20.393626
60.294686	1706.199209	20.398643
60.755749	1700.641935	20.403661
60.925706	1695.979228	20.408679
60.583120	1696.695693	20.413696
61.054938	1689.498791	20.418714
60.642789	1696.667483	20.423731
60.651460	1691.338889	20.428749
60.620281	1709.736795	20.433767
61.415983	1715.564325	20.438784
61.414509	1711.938383	20.443802
60.946255	1717.020310	20.448819
61.423617	1708.563299	20.453837
61.317389	1709.135430	20.458855
61.109952	1707.457433	20.463872
61.538014	1713.642380	20.468890
61.390220	1710.181382	20.473907
61.728260	1705.413438	20.478925
61.572275	1708.079461	20.483943
61.447967	1712.337442	20.488960
61.661643	1706.550668	20.493978
61.700319	1709.362927	20.498995
61.788699	1725.785416	20.504013
62.018263	1739.070852	20.509031
62.076819	1739.939076	20.514048
62.347201	1734.184437	20.519066
61.886668	1735.569514	20.524083
62.119511	1726.699500	20.529101
62.271484	1732.798315	20.534119
62.232856	1728.493345	20.539136
62.563443	1737.565508	20.544154
62.439064	1732.778484	20.549171
62.402737	1731.562851	20.554189
62.503383	1733.494355	20.559207
62.219107	1732.522708	20.564224
62.701214	1731.247941	20.569242
62.755011	1730.737750	20.574259
62.837648	1741.982201	20.579277
62.703842	1752.417925	20.584295
62.821387	1760.289491	20.589312
62.697122	1761.470398	20.594330
62.648653	1766.590716	20.599347
63.377550	1749.872951	20.604365
63.039213	1756.181145	20.609383
63.077285	1749.307810	20.614400
63.343376	1751.071377	20.619418
63.182792	1758.017633	20.624435
63.287591	1758.054902	20.629453
63.057126	1766.536448	20.634471
63.531385	1783.738023	20.639488
63.581590	1782.508829	20.644506
63.401813	1786.608251	20.649523
63.698638	1780.956758	20.654541
63.971123	1782.324828	20.659559
63.980111	1785.334264	20.664576
63.982292	1781.448945	20.669594
63.734661	1786.660436	20.674611
64.199667	1768.532247	20.679629
64.162134	1780.837024	20.684647
64.157956	1778.773703	20.689664
64.402900	1776.046468	20.694682
63.921787	1778.627733	20.699699
64.346229	1770.699721	20.704717
64.015475	1780.639269	20.709735
64.207072	1800.428869	20.714752
64.503792	1801.187194	20.719770
64.698464	1810.981318	20.724787
64.826783	1799.445056	20.729805
65.039953	1793.181780	20.734823
64.714245	1794.949703	20.739840
64.848922	1805.520128	20.744858
64.747487	1810.389966	20.749875
64.697582	1801.078194	20.754893
64.723810	1804.646698	20.759911
64.838140	1809.549007	20.764928
65.191722	1816.439976	20.769946
65.434110	1819.040444	20.774963
65.432920	1809.717878	20.779981
65.340734	1806.986650	20.784999
65.482331	1825.938307	20.790016
65.584736	1822.217168	20.795034
65.612246	1817.027605	20.800051
65.910172	1811.315965	20.805069
65.603881	1816.978494	20.810087
65.545682	1817.842923	20.815104
65.753997	1819.795439	20.820122
65.593849	1822.875566	20.825139
65.799841	1828.192733	20.830157
65.981636	1841.738209	20.835175
66.023775	1835.492247	20.840192
66.439967	1840.227342	20.845210
66.127493	1842.441347	20.850227
66.292341	1840.102214	20.855245
66.399489	1846.126035	20.860263
66.183591	1843.414184	20.865280
66.435689	1830.656075	20.870298
66.292982	1847.351580	20.875315
66.261129	1837.610901	20.880333
66.908568	1847.955839	20.885351
66.724131	1855.600188	20.890368
66.905523	1857.777847	20.895386
66.886421	1853.087912	20.900403
66.879054	1856.333467	20.905421
67.061140	1849.216611	20.910439
67.292859	1852.222723	20.915456
67.249566	1845.920710	20.920474
66.985213	1848.673164	20.925491
67.298635	1844.663323	20.930509
67.146788	1843.532058	20.935527
67.208879	1856.988996	20.940544
67.660966	1848.479072	20.945562
67.508753	1857.049392	20.950579
67.703912	1863.526518	20.955597
67.968164	1865.991015	20.960615
67.745381	1873.410992	20.965632
67.795278	1875.577696	20.970650
67.995785	1872.428192	20.975667
68.238671	1869.978992	20.980685
68.261943	1863.010097	20.985703
67.890430	1873.909193	20.990720
68.440214	1861.653566	20.995738
68.283152	1860.052873	21.000755
68.345013	1862.432308	21.005773
68.540954	1867.347094	21.010791
68.521137	1875.410656	21.015808
68.411400	1858.423371	21.020826
68.354024	1857.854851	21.025843
68.460619	1860.072633	21.030861
68.973747	1863.444936	21.035879
68.434219	1871.309038	21.040896
68.475048	1866.401414	21.045914
68.552409	1869.188701	21.050931
68.659287	1888.786531	21.055949
68.928732	1882.362920	21.060967
68.796612	1892.836333	21.065984
69.048521	1891.786982	21.071002
68.629868	1896.760195	21.076019
68.630612	1894.039642	21.081037
68.959415	1899.867798	21.086055
68.903533	1917.247241	21.091072
69.165389	1915.745021	21.096090
69.163138	1914.741802	21.101107
69.218541	1922.348603	21.106125
69.725758	1923.446363	21.111143
69.673668	1932.600674	21.116160
69.844573	1928.837220	21.121178
69.669483	1932.096443	21.126195
69.790990	1924.575611	21.131213
70.220939	1928.519573	21.136231
70.222487	1933.591074	21.141248
70.584304	1934.500163	21.146266
70.615682	1931.402395	21.151283
70.628779	1925.981513	21.156301
70.950592	1915.885560	21.161319
70.765133	1923.429107	21.166336
70.635576	1916.383143	21.171354
70.985249	1920.001987	21.176371
70.675887	1922.389095	21.181389
71.040340	1908.199436	21.186407
70.688953	1915.156711	21.191424
70.774531	1906.852514	21.196442
70.818754	1914.599928	21.201459
70.982319	1933.422017	21.206477
71.363167	1937.720835	21.211495
71.043278	1942.145221	21.216512
71.210445	1929.406660	21.221530
71.346445	1933.923731	21.226547
71.110346	1936.775919	21.231565
71.207549	1928.936981	21.236583
71.548474	1939.159571	21.241600
71.527534	1938.143497	21.246618
71.848264	1941.325039	21.251635
71.569024	1961.661987	21.256653
71.755820	1960.304076	21.261671
71.662916	1961.565295	21.266688
71.869413	1952.639333	21.271706
72.085307	1960.599728	21.276723
71.913108	1961.706101	21.281741
72.110776	1951.635890	21.286759
72.073612	1956.363146	21.291776
72.437012	1965.436597	21.296794
72.644355	1972.767133	21.301811
72.469202	1972.087665	21.306829
72.590605	1962.856273	21.311847
72.786967	1978.047009	21.316864
72.719816	1977.795618	21.321882
73.190673	1975.998699	21.326899
73.010877	1962.171997	21.331917
73.064317	1946.358349	21.336935
73.029440	1959.969422	21.341952
72.953325	1961.196450	21.346970
73.479924	1964.358366	21.351987
73.274534	1964.968133	21.357005
73.354875	1966.713483	21.362023
73.159441	1970.916393	21.367040
73.305451	1964.174398	21.372058
73.446527	1968.583377	21.377075
72.911016	1968.815648	21.382093
72.801402	1967.387404	21.387111
73.029685	1973.433318	21.392128
73.538409	1995.253262	21.397146
73.854672	1993.701484	21.402163
73.485615	1998.171459	21.407181
73.901800	1996.758670	21.412199
73.796218	2000.511978	21.417216
74.047090	2008.173404	21.422234
74.058202	2015.695659	21.427251
73.959912	2020.249459	21.432269
74.151692	2009.141807	21.437287
74.309049	2012.396298	21.442304
74.212682	2016.735186	21.447322
74.914403	2017.707798	21.452339
74.425943	2025.103186	21.457357
74.504103	2027.792536	21.462375
74.777862	2042.027549	21.467392
74.722840	2040.164682	21.472410
75.016803	2039.203415	21.477427
74.851591	2037.439869	21.482445
74.917129	2033.752867	21.487463
75.001480	2031.966001	21.492480
75.303386	2037.981466	21.497498
75.405053	2039.168022	21.502515
75.596991	2055.094872	21.507533
75.423187	2053.635649	21.512551
75.533263	2052.318156	21.517568
75.609323	2059.634580	21.522586
76.132445	2065.492311	21.527603
76.046151	2059.938627	21.532621
76.125967	2056.754348	21.537639
75.876828	2053.839374	21.542656
75.983514	2054.816846	21.547674
76.230177	2052.313378	21.552691
76.025357	2050.710682	21.557709
76.077779	2050.607825	21.562727
76.179050	2059.422570	21.567744
75.859356	2052.971271	21.572762
76.315084	2066.063716	21.577779
76.221626	2071.633014	21.582797
76.490017	2085.285036	21.587815
76.480070	2086.640572	21.592832
76.572696	2083.261763	21.597850
76.684401	2073.987649	21.602867
76.578212	2087.925595	21.607885
77.105123	2093.047384	21.612903
77.414990	2089.344182	21.617920
77.428520	2100.577594	21.622938
77.455722	2096.647258	21.627955
77.160770	2101.386536	21.632973
77.346394	2087.641351	21.637991
77.461540	2097.978307	21.643008
77.239838	2099.584786	21.648026
77.905401	2085.294159	21.653043
77.382985	2086.445942	21.658061
77.545715	2093.275396	21.663079
77.509054	2093.789299	21.668096
77.563485	2099.070328	21.673114
77.859507	2100.198033	21.678131
78.150062	2104.993912	21.683149
78.722660	2108.060278	21.688167
78.379154	2106.491929	21.693184
78.288094	2110.040998	21.698202
78.460284	2105.431488	21.703219
78.610517	2114.396391	21.708237
78.771035	2116.037669	21.713255
78.540308	2108.341555	21.718272
78.544293	2110.461827	21.723290
78.844289	2090.396110	21.728307
78.615966	2105.240051	21.733325
79.001763	2105.226985	21.738343
78.830655	2099.011185	21.743360
78.757943	2095.134375	21.748378
79.088903	2102.237299	21.753395
79.100755	2128.152891	21.758413
79.199558	2122.036817	21.763431
79.346197	2121.098628	21.768448
79.103777	2119.265113	21.773466
79.611379	2137.165603	21.778483
79.576054	2130.306778	21.783501
79.470045	2122.515373	21.788519
79.604508	2138.877368	21.793536
79.500033	2150.025150	21.798554
79.683757	2140.083260	21.803571
79.773097	2150.118153	21.808589
79.919101	2151.304082	21.813607
80.275321	2150.623411	21.818624
79.902668	2155.636829	21.823642
80.287381	2159.935096	21.828659
80.265299	2171.243564	21.833677
80.586156	2173.560371	21.838695
80.754170	2169.399657	21.843712
80.605064	2181.138320	21.848730
80.556033	2172.845622	21.853747
80.588878	2176.217489	21.858765
80.547593	2182.132125	21.863783
80.816117	2190.617749	21.868800
80.618265	2204.125143	21.873818
81.083201	2204.809791	21.878835
80.856661	2205.397631	21.883853
81.011060	2201.333725	21.888871
81.629156	2207.220808	21.893888
81.238632	2223.400023	21.898906
81.724817	2234.363790	21.903923
81.626247	2220.666186	21.908941
81.649575	2217.433919	21.913959
82.259857	2215.877087	21.918976
81.791978	2219.463122	21.923994
82.041808	2219.187313	21.929011
82.232963	2220.669154	21.934029
82.244044	2222.273890	21.939047
82.105592	2203.513915	21.944064
81.974223	2220.160650	21.949082
81.904093	2212.612913	21.954099
82.532049	2222.503494	21.959117
82.373103	2233.833445	21.964135
82.769093	2236.312072	21.969152
82.393028	2243.440610	21.974170
82.717138	2240.539943	21.979187
83.149525	2238.597535	21.984205
82.938961	2239.921392	21.989223
83.316795	2225.297007	21.994240
82.953801	2241.749659	21.999258
83.288495	2238.194028	22.004275
83.333887	2221.387238	22.009293
82.849319	2228.220320	22.014311
83.260822	2236.424769	22.019328
83.225583	2245.844864	22.024346
83.458056	2250.372149	22.029363
83.315313	2255.150741	22.034381
83.404301	2256.276176	22.039399
83.949509	2250.910697	22.044416
83.603570	2259.530496	22.049434
83.550809	2261.258856	22.054451
84.108510	2273.000460	22.059469
83.862928	2276.198199	22.064487
84.208776	2275.765323	22.069504
84.004261	2287.850436	22.074522
84.500740	2274.820175	22.079539
84.104959	2273.512486	22.084557
84.132421	2288.079798	22.089575
84.500344	2291.572773	22.094592
84.551933	2294.850199	22.099610
84.799965	2292.835675	22.104627
84.670783	2288.437451	22.109645
84.857388	2299.451351	22.114663
84.973105	2315.494525	22.119680
84.654433	2317.226678	22.124698
85.000427	2313.085389	22.129715
85.549672	2322.729560	22.134733
85.218731	2312.887145	22.139751
85.469053	2304.370746	22.144768
85.526393	2335.035714	22.149786
85.529522	2332.030674	22.154803
85.688709	2340.407256	22.159821
85.856453	2332.096302	22.164839
86.273551	2333.397574	22.169856
86.184036	2336.198455	22.174874
86.124641	2329.400134	22.179891
86.074323	2329.875154	22.184909
86.078308	2335.202030	22.189927
86.559080	2324.964169	22.194944
86.625868	2322.630869	22.199962
86.509541	2336.965106	22.204979
86.413916	2349.636012	22.209997
86.656729	2353.363214	22.215015
87.186342	2351.642268	22.220032
87.149018	2357.537405	22.225050
87.423829	2348.764661	22.230067
87.290321	2353.870065	22.235085
87.576167	2346.320153	22.240103
87.546262	2353.830041	22.245120
87.374138	2350.483192	22.250138
87.207592	2356.067185	22.255155
87.300350	2350.939835	22.260173
87.366497	2349.247317	22.265191
87.145785	2353.548958	22.270208
87.766266	2363.039966	22.275226
87.838896	2370.817844	22.280243
88.041040	2366.787450	22.285261
87.767313	2378.189128	22.290279
88.141832	2367.649125	22.295296
88.123807	2376.397502	22.300314
88.383918	2364.338411	22.305331
88.729740	2364.827114	22.310349
88.603544	2373.469350	22.315367
88.461134	2366.674553	22.320384
88.409412	2364.615458	22.325402
88.481407	2368.748156	22.330419
88.975712	2377.397329	22.335437
88.489350	2387.790819	22.340455
88.665690	2388.145115	22.345472
88.900788	2388.505986	22.350490
89.068986	2385.276242	22.355507
89.215448	2390.902732	22.360525
89.067698	2388.164339	22.365543
89.521003	2398.902966	22.370560
89.721274	2404.603089	22.375578
89.397219	2407.895203	22.380595
89.690746	2410.415157	22.385613
89.746620	2413.246925	22.390631
89.614255	2413.498095	22.395648
89.760178	2417.638158	22.400666
89.666005	2410.949406	22.405683
90.168444	2414.875808	22.410701
89.935957	2426.482514	22.415719
90.109570	2427.594702	22.420736
90.356405	2426.066390	22.425754
90.575154	2437.334139	22.430771
90.469903	2428.441004	22.435789
90.188550	2430.088418	22.440807
90.636727	2430.147639	22.445824
90.728538	2452.557373	22.450842
90.684449	2461.297250	22.455859
91.081696	2447.834245	22.460877
90.946219	2453.239815	22.465895
90.714782	2454.197694	22.470912
91.285424	2454.203010	22.475930
91.217806	2471.326029	22.480947
91.685974	2458.757706	22.485965
91.319625	2472.487378	22.490983
91.389713	2469.326643	22.496000
91.861340	2464.584913	22.501018
91.495260	2474.142177	22.506035
92.049276	2468.942527	22.511053
91.851501	2484.624674	22.516071
92.263648	2483.887889	22.521088
92.331008	2483.407113	22.526106
92.369180	2483.394858	22.531123
92.518164	2480.777235	22.536141
92.125940	2485.355110	22.541159
92.360336	2488.837483	22.546176
92.603671	2484.699614	22.551194
92.559651	2489.027258	22.556211
93.233423	2500.091201	22.561229
93.104360	2511.470299	22.566247
93.361916	2504.104652	22.571264
93.289335	2498.460313	22.576282
93.441998	2504.297327	22.581299
93.673597	2504.617720	22.586317
93.207142	2510.428646	22.591335
93.527455	2501.910657	22.596352
93.567587	2491.568151	22.601370
93.563780	2499.017200	22.606387
94.010913	2494.771653	22.611405
93.385078	2504.379097	22.616423
94.000099	2508.164794	22.621440
94.176901	2521.923027	22.626458
94.342782	2529.105638	22.631475
94.324084	2520.609192	22.636493
94.614598	2522.545753	22.641511
94.504215	2522.417903	22.646528
94.186658	2529.578416	22.651546
94.049699	2526.831999	22.656563
94.348464	2531.071231	22.661581
94.480665	2538.517925	22.666599
94.577757	2540.541602	22.671616
94.630494	2546.656243	22.676634
94.566978	2548.307412	22.681651
95.112230	2554.455357	22.686669
95.165628	2576.344192	22.691687
95.042874	2568.690930	22.696704
95.498546	2568.528049	22.701722
95.066232	2572.288479	22.706739
95.586307	2574.731933	22.711757
95.894673	2583.492397	22.716775
96.123323	2597.195223	22.721792
96.035684	2592.389587	22.726810
96.002939	2593.609863	22.731827
96.000146	2589.415848	22.736845
96.091427	2598.361824	22.741863
96.429143	2597.355801	22.746880
96.594011	2585.841713	22.751898
96.350877	2589.237959	22.756915
96.699484	2584.187235	22.761933
96.919135	2583.837247	22.766951
96.719550	2583.044805	22.771968
96.640010	2582.766941	22.776986
96.604374	2604.515109	22.782003
96.987653	2604.268886	22.787021
97.219483	2610.330241	22.792039
96.936777	2605.902337	22.797056
97.583800	2607.246511	22.802074
97.202911	2611.355535	22.807091
97.708566	2619.573815	22.812109
97.806941	2629.932642	22.817127
97.726789	2628.528134	22.822144
97.669167	2625.441034	22.827162
97.680669	2630.905689	22.832179
97.743310	2618.284014	22.837197
98.173547	2638.232831	22.842215
98.242171	2641.851671	22.847232
98.559492	2641.685216	22.852250
98.313252	2653.212163	22.857267
98.408120	2650.498841	22.862285
98.484674	2646.377597	22.867303
98.387270	2637.167515	22.872320
98.936340	2649.163211	22.877338
99.206867	2664.377628	22.882355
99.209685	2664.774897	22.887373
99.206754	2663.206793	22.892391
99.408217	2669.108807	22.897408
99.566675	2659.306304	22.902426
99.385382	2662.951678	22.907443
99.159844	2665.552990	22.912461
99.335462	2672.289119	22.917479
99.752562	2681.124123	22.922496
100.218887	2687.884147	22.927514
100.100014	2701.950802	22.932531
100.093708	2687.686060	22.937549
100.236169	2681.673421	22.942567
100.084698	2683.796024	22.947584
100.590634	2675.441395	22.952602
100.313844	2674.982971	22.957619
99.977230	2678.356005	22.962637
100.405359	2691.847751	22.967655
100.516711	2702.750600	22.972672
101.096021	2700.008715	22.977690
100.988390	2709.967471	22.982707
101.027679	2699.391424	22.987725
101.083796	2693.622708	22.992743
100.998650	2703.912489	22.997760
101.423207	2715.792023	23.002778
101.441674	2725.917245	23.007795
101.552399	2726.752095	23.012813
101.618216	2719.959259	23.017831
101.209337	2732.808914	23.022848
101.731919	2718.732715	23.027866
101.949200	2726.339745	23.032883
101.609219	2725.329425	23.037901
101.921506	2747.635550	23.042919
102.083519	2746.969506	23.047936
102.406883	2748.405430	23.052954
102.186357	2751.018594	23.057971
102.285236	2745.628212	23.062989
102.672740	2740.161051	23.068007
102.415633	2762.300753	23.073024
102.899753	2755.707484	23.078042
102.726512	2772.089860	23.083059
102.619277	2767.792232	23.088077
102.992909	2771.691552	23.093095
103.165580	2778.772204	23.098112
103.649768	2791.065370	23.103130
103.321328	2794.531830	23.108147
103.276343	2785.187213	23.113165
103.651042	2785.459943	23.118183
103.415260	2789.521024	23.123200
103.892052	2792.031257	23.128218
103.803447	2802.185922	23.133235
103.880209	2810.474640	23.138253
104.306051	2814.239544	23.143271
104.281184	2809.960563	23.148288
104.341574	2809.749144	23.153306
104.249908	2824.316618	23.158323
104.284018	2832.006045	23.163341
104.821584	2832.212229	23.168359
104.445698	2841.673382	23.173376
104.836534	2838.310834	23.178394
104.994403	2841.448619	23.183411
105.158200	2827.602136	23.188429
105.263569	2827.399451	23.193447
105.525637	2855.918603	23.198464
105.547427	2853.630159	23.203482
105.639534	2857.513637	23.208499
106.059446	2857.548884	23.213517
105.948304	2863.626185	23.218535
105.682240	2853.880617	23.223552
106.305355	2857.156978	23.228570
105.676125	2852.104726	23.233587
105.893757	2853.677158	23.238605
106.191902	2859.620898	23.243623
106.305089	2873.698673	23.248640
106.326553	2877.192389	23.253658
106.423207	2880.743762	23.258675
106.497468	2872.453517	23.263693
106.793001	2876.570248	23.268711
106.976145	2897.116709	23.273728
107.366435	2906.823975	23.278746
107.144016	2905.091398	23.283763
107.331474	2901.195746	23.288781
107.713324	2898.510018	23.293799
107.411804	2898.768758	23.298816
107.530900	2899.962110	23.303834
107.536449	2903.231079	23.308851
107.448788	2892.902053	23.313869
108.211077	2912.527722	23.318887
107.864314	2922.921740	23.323904
107.757035	2921.698204	23.328922
107.846363	2916.183021	23.333939
108.072523	2914.380164	23.338957
108.455876	2923.861281	23.343975
108.451482	2931.203291	23.348992
108.808751	2938.577015	23.354010
108.679496	2925.742162	23.359027
108.194502	2936.931109	23.364045
108.455929	2927.421634	23.369063
108.660736	2945.032661	23.374080
109.114631	2951.053029	23.379098
109.080165	2950.370417	23.384115
109.403658	2956.486965	23.389133
109.260517	2957.105948	23.394151
109.286418	2963.051345	23.399168
109.251282	2970.546528	23.404186
109.637547	2974.851063	23.409203
109.592044	2982.991738	23.414221
109.805505	2982.229252	23.419239
110.187593	2998.095587	23.424256
110.247898	2997.631684	23.429274
110.591450	3007.655635	23.434291
110.234271	3007.033049	23.439309
110.526920	3001.331331	23.444327
110.907931	3003.967068	23.449344
111.113500	3001.040666	23.454362
111.173340	2991.464898	23.459379
111.018077	2999.657496	23.464397
111.180415	2991.517520	23.469415
111.066330	2990.225610	23.474432
111.553811	3001.956603	23.479450
111.591224	3013.726554	23.484467
111.507354	3014.617154	23.489485
111.869541	3012.379515	23.494503
112.331240	3014.775366	23.499520
112.488467	3021.987937	23.504538
112.150239	3019.143572	23.509555
111.673186	3019.562375	23.514573
112.222869	3011.175489	23.519591
112.009877	3021.138300	23.524608
111.873188	3039.623533	23.529626
112.083078	3044.725831	23.534643
112.542184	3044.612910	23.539661
112.483404	3054.090772	23.544679
112.700168	3068.098816	23.549696
112.665537	3067.529849	23.554714
112.921975	3070.361860	23.559731
112.846144	3088.723986	23.564749
113.200057	3078.035300	23.569767
113.068128	3086.571464	23.574784
113.282689	3083.189146	23.579802
113.470926	3102.109594	23.584819
113.447916	3107.576645	23.589837
113.579481	3108.629183	23.594855
113.754564	3118.812151	23.599872
114.091955	3121.726174	23.604890
114.264152	3125.499320	23.609907
114.450659	3125.444888	23.614925
114.661788	3134.485979	23.619943
114.717028	3126.631000	23.624960
114.470401	3128.206755	23.629978
115.061405	3134.429795	23.634995
115.022208	3146.199210	23.640013
115.069069	3143.562773	23.645031
115.315495	3145.054971	23.650048
115.448133	3140.972170	23.655066
115.734009	3127.889074	23.660083
115.583060	3133.429832	23.665101
116.024896	3133.041870	23.670119
116.034746	3130.486982	23.675136
115.886821	3126.132518	23.680154
115.986497	3132.839687	23.685171
116.096115	3141.035037	23.690189
116.571302	3153.017396	23.695207
116.557222	3151.520434	23.700224
116.432853	3154.121746	23.705242
116.869274	3152.813014	23.710259
116.383583	3152.106401	23.715277
117.009672	3155.915755	23.720295
116.819664	3150.245421	23.725312
116.842857	3148.357559	23.730330
116.928182	3153.422592	23.735347
117.024404	3159.559035	23.740365
117.485778	3168.185346	23.745383
117.652671	3172.956701	23.750400
117.486388	3178.604031	23.755418
117.745363	3164.193195	23.760435
117.719514	3174.054177	23.765453
117.848567	3182.486374	23.770471
117.896265	3192.070719	23.775488
117.782309	3203.760353	23.780506
118.173927	3202.951009	23.785523
118.534807	3199.078624	23.790541
118.610872	3196.163011	23.795559
118.850880	3211.994983	23.800576
118.975631	3224.761384	23.805594
119.123539	3222.626727	23.810611
118.967931	3227.650621	23.815629
119.329505	3221.111102	23.820647
119.265974	3220.212097	23.825664
119.218965	3214.263685	23.830682
119.164209	3217.400129	23.835699
119.535173	3244.652967	23.840717
119.388230	3242.602377	23.845735
119.590780	3242.741118	23.850752
119.675764	3251.268626	23.855770
119.838330	3259.354735	23.860787
120.082284	3268.794749	23.865805
120.405842	3261.569955	23.870823
120.356693	3264.815997	23.875840
120.601949	3269.515132	23.880858
121.179031	3286.310671	23.885875
121.078636	3288.188623	23.890893
121.070940	3288.669616	23.895911
120.818699	3288.633421	23.900928
121.070601	3287.094776	23.905946
120.982733	3285.502050	23.910963
120.928208	3301.424432	23.915981
121.488514	3307.750187	23.920999
121.301665	3312.633812	23.926016
121.452491	3308.942656	23.931034
122.067022	3317.522951	23.936051
121.949405	3330.974429	23.941069
122.207719	3334.781472	23.946087
122.526634	3325.736220	23.951104
122.580505	3321.264875	23.956122
122.368792	3318.602642	23.961139
122.528337	3331.666667	23.966157
122.879740	3333.514872	23.971175
123.248970	3338.819541	23.976192
123.206915	3338.990293	23.981210
123.456852	3334.762822	23.986227
123.184198	3338.788770	23.991245
123.134588	3335.476198	23.996263
123.602781	3342.674898	24.001280
123.320149	3344.644532	24.006298
123.651754	3356.599023	24.011315
123.705946	3370.295052	24.016333
123.962318	3365.593126	24.021351
123.854779	3370.000371	24.026368
123.983660	3381.137604	24.031386
124.289449	3385.742067	24.036403
124.770456	3392.537934	24.041421
124.448270	3380.004422	24.046439
124.695942	3384.797897	24.051456
124.539178	3391.056116	24.056474
124.780802	3394.909974	24.061491
124.957686	3408.990813	24.066509
125.439781	3401.005715	24.071527
125.529934	3406.038500	24.076544
125.340764	3424.106253	24.081562
125.522869	3405.948149	24.086579
125.509066	3407.102387	24.091597
125.401710	3412.851027	24.096615
125.950621	3429.171361	24.101632
125.470514	3439.046842	24.106650
126.178946	3429.968920	24.111667
126.130155	3437.412779	24.116685
126.009920	3450.539661	24.121703
126.341961	3448.593913	24.126720
126.474287	3460.112565	24.131738
126.717365	3471.105711	24.136755
127.200731	3477.471987	24.141773
126.907478	3491.695984	24.146791
127.438170	3480.774208	24.151808
127.249989	3481.258231	24.156826
127.238909	3481.241067	24.161843
127.559127	3485.849608	24.166861
127.818118	3498.361606	24.171879
128.268743	3498.619298	24.176896
127.881702	3496.956641	24.181914
128.233145	3491.479125	24.186931
128.046706	3499.376985	24.191949
128.037161	3495.007065	24.196967
128.141427	3512.637556	24.201984
128.664088	3519.281756	24.207002
128.732190	3520.120166	24.212019
128.716716	3526.324733	24.217037
129.259274	3538.486174	24.222055
129.533376	3547.495513	24.227072
129.093386	3548.501901	24.232090
129.906172	3542.750089	24.237107
129.769841	3547.673206	24.242125
129.341142	3543.406818	24.247143
129.639662	3542.261697	24.252160
129.658672	3558.362163	24.257178
130.126726	3562.240552	24.262195
130.370154	3564.209856	24.267213
130.360785	3569.958976	24.272231
130.336336	3561.630223	24.277248
130.505758	3573.335670	24.282266
130.786190	3587.640304	24.287283
130.895224	3585.906232	24.292301
130.704448	3591.573309	24.297319
131.133864	3581.686824	24.302336
130.869247	3589.707442	24.307354
131.263015	3606.449937	24.312371
131.318271	3605.197734	24.317389
131.490371	3601.077085	24.322407
131.408876	3601.260330	24.327424
131.762872	3610.351873	24.332442
132.125475	3610.992645	24.337459
131.895302	3620.434530	24.342477
132.086836	3627.029646	24.347495
132.336664	3639.713619	24.352512
132.302864	3643.033076	24.357530
132.724373	3643.197487	24.362547
133.107390	3642.765074	24.367565
133.158877	3648.198522	24.372583
133.188591	3642.035945	24.377600
133.232376	3640.432030	24.382618
133.362382	3639.928785	24.387635
133.361708	3658.210276	24.392653
133.364647	3666.059602	24.397671
133.917110	3666.345531	24.402688
133.743598	3669.109276	24.407706
133.844534	3663.484731	24.412723
134.017685	3664.533945	24.417741
134.160023	3685.318108	24.422759
134.503394	3675.915344	24.427776
134.355128	3677.772429	24.432794
134.696452	3673.959821	24.437811
134.538246	3673.896267	24.442829
135.074420	3690.951099	24.447847
135.023945	3693.209499	24.452864
135.316875	3693.217301	24.457882
135.454649	3694.707630	24.462899
135.488993	3696.810708	24.467917
135.391453	3701.083901	24.472935
135.745931	3697.897335	24.477952
135.926133	3721.181725	24.482970
135.781864	3715.895431	24.487987
136.097360	3715.656661	24.493005
136.238695	3721.994545	24.498023
136.264376	3723.685505	24.503040
136.663024	3740.522049	24.508058
136.827823	3753.576088	24.513075
137.175216	3745.545661	24.518093
136.704689	3750.524347	24.523111
136.850764	3742.039386	24.528128
137.006640	3746.651647	24.533146
137.016025	3765.547154	24.538163
137.238675	3766.130951	24.543181
137.333396	3769.733304	24.548199
137.862397	3783.197443	24.553216
137.523733	3794.386086	24.558234
137.868521	3792.848629	24.563251
138.188437	3791.043624	24.568269
138.030090	3817.758456	24.573287
138.190248	3816.373020	24.578304
138.291980	3826.258558	24.583322
138.443426	3836.101594	24.588339
138.806879	3840.624544	24.593357
138.820676	3845.994518	24.598375
138.925611	3847.979238	24.603392
139.379619	3856.269307	24.608410
139.254022	3863.861097	24.613427
139.614576	3861.361635	24.618445
139.734724	3863.056746	24.623463
139.524584	3865.330712	24.628480
139.775091	3875.821083	24.633498
139.892554	3894.002239	24.638515
140.283548	3894.957366	24.643533
140.089382	3901.616165	24.648551
140.714171	3908.396016	24.653568
140.880119	3916.169411	24.658586
141.089536	3916.938355	24.663603
141.272565	3914.700268	24.668621
140.987840	3923.368080	24.673639
141.213323	3911.670053	24.678656
141.577247	3923.597763	24.683674
141.665423	3926.187982	24.688691
141.889721	3928.403363	24.693709
141.965933	3935.259699	24.698727
141.922739	3937.700057	24.703744
141.826323	3931.168909	24.708762
142.049121	3937.664550	24.713779
142.473003	3938.683967	24.718797
142.372189	3946.290848	24.723815
142.787403	3937.930918	24.728832
143.035751	3941.846968	24.733850
142.846137	3942.602674	24.738867
143.054985	3954.346380	24.743885
143.372968	3950.654157	24.748903
143.841081	3970.298666	24.753920
143.589985	3969.195437	24.758938
143.829600	3973.908266	24.763955
144.045630	3968.941059	24.768973
143.715546	3968.288939	24.773991
143.562130	3971.027486	24.779008
143.905626	3981.285561	24.784026
143.918671	3995.427246	24.789043
144.416276	3995.630242	24.794061
144.451691	4007.779919	24.799079
144.890826	4011.217889	24.804096
144.802572	4015.290849	24.809114
144.841788	4024.965344	24.814131
144.985512	4023.333114	24.819149
145.250929	4036.718795	24.824167
145.319863	4041.890806	24.829184
145.731883	4036.937064	24.834202
145.562173	4050.031098	24.839219
145.723442	4058.619633	24.844237
145.927545	4065.326570	24.849255
146.066519	4064.645151	24.854272
146.352433	4072.308284	24.859290
146.081419	4084.957381	24.864307
146.711974	4076.184885	24.869325
146.831587	4094.350124	24.874343
147.179783	4111.251734	24.879360
147.280064	4119.988735	24.884378
147.076873	4110.055877	24.889395
147.570403	4104.959935	24.894413
147.498012	4113.212649	24.899431
147.589713	4128.210122	24.904448
148.350792	4128.138271	24.909466
147.704163	4131.743210	24.914483
147.963625	4130.329567	24.919501
148.058710	4133.430069	24.924519
148.606170	4144.233903	24.929536
148.567896	4144.953282	24.934554
148.368782	4152.086407	24.939571
148.754696	4157.252981	24.944589
148.905296	4173.292344	24.949607
149.190055	4171.091948	24.954624
148.921041	4173.962266	24.959642
149.427893	4195.453759	24.964659
149.712723	4196.103582	24.969677
149.792311	4198.780409	24.974695
149.582458	4197.250902	24.979712
150.262145	4208.649558	24.984730
150.372818	4222.255317	24.989747
150.120298	4220.135931	24.994765
150.486681	4223.118192	24.999783
150.693021	4232.842370	25.004800
150.947741	4244.983099	25.009818
150.878730	4246.900422	25.014835
151.148486	4239.229146	25.019853
151.244853	4255.157135	25.024871
151.468001	4261.618117	25.029888
151.534204	4256.011457	25.034906
151.025151	4263.376254	25.039923
151.943814	4282.887390	25.044941
152.056200	4286.442888	25.049959
152.100486	4294.746847	25.054976
152.469642	4295.610726	25.059994
152.290461	4294.931796	25.065011
152.609948	4299.376527	25.070029
152.587114	4302.558660	25.075047
152.811042	4302.760348	25.080064
153.062438	4305.312425	25.085082
152.640157	4315.889515	25.090099
152.977333	4322.578857	25.095117
153.299739	4331.233813	25.100135
153.501919	4343.941528	25.105152
153.592325	4350.205544	25.110170
153.480627	4361.614648	25.115187
153.755156	4363.001542	25.120205
153.907327	4379.113439	25.125223
154.268972	4384.533239	25.130240
154.616299	4380.116666	25.135258
154.652559	4403.831665	25.140275
155.123345	4403.224509	25.145293
154.880367	4412.359478	25.150311
154.994214	4407.865844	25.155328
155.448695	4414.861956	25.160346
155.157620	4430.629847	25.165363
155.728612	4423.267979	25.170381
155.928613	4428.154425	25.175399
155.641961	4442.984169	25.180416
155.916864	4445.125401	25.185434
155.855453	4451.716256	25.190451
156.623302	4460.828617	25.195469
156.653012	4466.224690	25.200487
157.003711	4473.454878	25.205504
157.372579	4477.693061	25.210522
157.574597	4470.426858	25.215539
157.875879	4468.978230	25.220557
157.764350	4462.089422	25.225575
157.845178	4477.467662	25.230592
158.130054	4482.539682	25.235610
158.006219	4490.216682	25.240627
158.270766	4487.640640	25.245645
158.589531	4489.702408	25.250663
158.674101	4491.399996	25.255680
158.609894	4488.834423	25.260698
158.378029	4496.039099	25.265715
158.655500	4510.367024	25.270733
158.938875	4513.955753	25.275751
159.307600	4525.327572	25.280768
159.270576	4527.176784	25.285786
158.968513	4537.548937	25.290803
159.331937	4539.215469	25.295821
159.892846	4564.657140	25.300839
159.903265	4566.953455	25.305856
160.300072	4568.977754	25.310874
160.405161	4575.807713	25.315891
160.455269	4574.395270	25.320909
160.657886	4587.311414	25.325927
160.819799	4598.273773	25.330944
160.983019	4594.864499	25.335962
160.952614	4592.880720	25.340979
161.189842	4611.176405	25.345997
161.199727	4615.183621	25.351015
161.277632	4621.661174	25.356032
161.545388	4629.775608	25.361050
161.821709	4642.778096	25.366067
162.178162	4647.498050	25.371085
162.144756	4637.620372	25.376103
162.382734	4657.412159	25.381120
162.879958	4658.047665	25.386138
163.024001	4664.353891	25.391155
162.771200	4658.058465	25.396173
163.184713	4658.318838	25.401191
163.099461	4660.431295	25.406208
163.372784	4667.891482	25.411226
163.511493	4679.094261	25.416243
163.944474	4678.470924	25.421261
164.201630	4675.728720	25.426279
163.811561	4681.260063	25.431296
164.006317	4675.491091	25.436314
163.982997	4692.467230	25.441331
164.237963	4708.427587	25.446349
164.482563	4703.866049	25.451367
164.729821	4717.715927	25.456384
164.895767	4727.244683	25.461402
164.842384	4730.602128	25.466419
165.081278	4728.475138	25.471437
165.740376	4731.787250	25.476455
165.536192	4748.596073	25.481472
165.669749	4753.647686	25.486490
165.796878	4751.673932	25.491507
165.986455	4767.597237	25.496525
166.213645	4770.711874	25.501543
165.961979	4781.590781	25.506560
166.383732	4790.609175	25.511578
166.655093	4804.780465	25.516595
166.829279	4807.025902	25.521613
167.357929	4808.745487	25.526631
167.223273	4816.250712	25.531648
167.259522	4822.892688	25.536666
167.702579	4814.531153	25.541683
167.534138	4829.538396	25.546701
167.777659	4846.166692	25.551719
168.103983	4853.451357	25.556736
168.375670	4847.310436	25.561754
168.515699	4857.591415	25.566771
168.507479	4868.949904	25.571789
168.675598	4861.101743	25.576807
168.750353	4872.816548	25.581824
169.073970	4882.525858	25.586842
169.306821	4897.413472	25.591859
169.476227	4888.059434	25.596877
169.708189	4904.083541	25.601895
169.832775	4908.271713	25.606912
169.927628	4912.284622	25.611930
170.156788	4916.172326	25.616947
170.221619	4927.431024	25.621965
170.882497	4931.064861	25.626983
170.747749	4934.687613	25.632000
170.822291	4932.081302	25.637018
171.293657	4942.364083	25.642035
171.475733	4949.999664	25.647053
171.445943	4947.851611	25.652071
171.348168	4956.405398	25.657088
171.932579	4957.573339	25.662106
172.186848	4969.392658	25.667123
172.450764	4971.109542	25.672141
172.721952	4965.978752	25.677159
172.534930	4966.835102	25.682176
172.646048	4969.958489	25.687194
172.546204	4976.236744	25.692212
172.626992	4989.143852	25.697229
172.976474	4995.875708	25.702247
173.326121	5008.690204	25.707264
173.531946	5017.572086	25.712282
173.848011	5018.886237	25.717300
173.568392	5026.436354	25.722317
174.078120	5018.796601	25.727335
174.248039	5035.360844	25.732352
174.004522	5036.974151	25.737370
174.926497	5031.274219	25.742388
174.359613	5038.099146	25.747405
174.750696	5038.378823	25.752423
174.391320	5057.084078	25.757440
174.793318	5062.254707	25.762458
175.060344	5059.684510	25.767476
175.041891	5087.020072	25.772493
175.300572	5086.389308	25.777511
175.491350	5099.929514	25.782528
175.596063	5109.452281	25.787546
175.926203	5105.925221	25.792564
176.114986	5124.525730	25.797581
176.587439	5134.372844	25.802599
176.864433	5130.254357	25.807616
176.626100	5130.471657	25.812634
176.892167	5142.863736	25.817652
177.103693	5152.537090	25.822669
177.343403	5163.345557	25.827687
177.594131	5175.206600	25.832704
177.880831	5179.896586	25.837722
177.901761	5193.239354	25.842740
177.851385	5189.932876	25.847757
178.441463	5202.040649	25.852775
178.382181	5205.430671	25.857792
178.343302	5199.224650	25.862810
178.983663	5221.075234	25.867828
178.739138	5235.595990	25.872845
179.347465	5225.320739	25.877863
179.503651	5236.224405	25.882880
179.635221	5240.780881	25.887898
179.896998	5245.727316	25.892916
179.790663	5247.877865	25.897933
180.007104	5250.078859	25.902951
180.296246	5269.560265	25.907968
180.578848	5275.614566	25.912986
180.722192	5280.352290	25.918004
180.467829	5287.182010	25.923021
181.192133	5293.798438	25.928039
181.079837	5296.325562	25.933056
181.172476	5306.061815	25.938074
181.527526	5317.935018	25.943092
181.406212	5336.145556	25.948109
181.835495	5328.035318	25.953127
182.148758	5349.091332	25.958144
182.201420	5350.064823	25.963162
182.522597	5352.299927	25.968180
182.659368	5378.311087	25.973197
183.169717	5374.392734	25.978215
183.125086	5373.490660	25.983232
183.460011	5374.956557	25.988250
183.682887	5377.121836	25.993268
183.817094	5391.801189	25.998285
183.815143	5401.523902	26.003303
184.284121	5393.558934	26.008320
184.300899	5391.479291	26.013338
184.580058	5407.423847	26.018356
184.713841	5409.271642	26.023373
185.076143	5407.295698	26.028391
184.795318	5412.308244	26.033408
184.916074	5417.122144	26.038426
185.212149	5422.539903	26.043444
185.239624	5435.834474	26.048461
185.491790	5442.490200	26.053479
185.906256	5448.852190	26.058496
185.774037	5458.083968	26.063514
185.903308	5463.183799	26.068532
186.135446	5477.188144	26.073549
186.379555	5482.001677	26.078567
186.666379	5481.126587	26.083584
186.756949	5492.441578	26.088602
187.137686	5498.711014	26.093620
186.927542	5510.508742	26.098637
186.946198	5502.106057	26.103655
187.349806	5522.709346	26.108672
187.499592	5535.523959	26.113690
188.053293	5530.228802	26.118708
188.166365	5546.139522	26.123725
187.978312	5559.073367	26.128743
188.212909	5558.544216	26.133760
188.391304	5576.354497	26.138778
189.133422	5586.528939	26.143796
188.763368	5590.621144	26.148813
188.928118	5595.958516	26.153831
189.246166	5607.468377	26.158848
189.425903	5617.251128	26.163866
189.864949	5630.484521	26.168884
190.065799	5643.366970	26.173901
190.240877	5637.670225	26.178919
190.448053	5655.217229	26.183936
190.372260	5657.842853	26.188954
191.002326	5656.541497	26.193972
190.674119	5669.929840	26.198989
191.110260	5673.371758	26.204007
191.269298	5680.944967	26.209024
191.516929	5706.519391	26.214042
192.008794	5712.894602	26.219060
191.724793	5722.529092	26.224077
191.980304	5718.663217	26.229095
192.257642	5736.350827	26.234112
192.173275	5750.777454	26.239130
193.173122	5753.701770	26.244148
193.140140	5758.571412	26.249165
193.035132	5755.058736	26.254183
193.541914	5767.738669	26.259200
193.412617	5777.743537	26.264218
194.030871	5778.278054	26.269236
193.935064	5786.295285	26.274253
193.939098	5796.020428	26.279271
194.182035	5800.206049	26.284288
194.283413	5807.870417	26.289306
194.558648	5811.811073	26.294324
194.648327	5816.576283	26.299341
194.764531	5827.726476	26.304359
195.259701	5841.191137	26.309376
195.387323	5843.617617	26.314394
195.682916	5858.369920	26.319412
195.883010	5867.003737	26.324429
195.855837	5870.515119	26.329447
196.292610	5885.545213	26.334464
196.251632	5894.005310	26.339482
196.405122	5893.441506	26.344500
196.810257	5909.534071	26.349517
197.518572	5905.710862	26.354535
197.895622	5914.266472	26.359552
197.340290	5915.597249	26.364570
197.907187	5919.242857	26.369588
198.183157	5936.261654	26.374605
198.177937	5939.697007	26.379623
198.467723	5935.071264	26.384640
198.219880	5939.289609	26.389658
198.954100	5953.790185	26.394676
198.952930	5958.957941	26.399693
199.115480	5954.816163	26.404711
199.409981	5950.600050	26.409728
199.581617	5970.618315	26.414746
200.271767	5977.915884	26.419764
200.167374	5973.380294	26.424781
200.115573	5985.526014	26.429799
200.267255	5971.694820	26.434816
200.101395	5985.758750	26.439834
200.491963	5991.663795	26.444852
200.831239	6003.517820	26.449869
200.842130	6002.095628	26.454887
201.506408	6022.020989	26.459904
201.260338	6020.332849	26.464922
201.443067	6025.651747	26.469940
201.610455	6037.494842	26.474957
201.676679	6049.195956	26.479975
201.767495	6052.979309	26.484992
201.575616	6064.345216	26.490010
202.318884	6075.315250	26.495028
202.505749	6100.372571	26.500045
202.707842	6097.755583	26.505063
203.289940	6109.088657	26.510080
203.037252	6134.742060	26.515098
203.454790	6144.017486	26.520116
203.847603	6141.171739	26.525133
203.862116	6158.588415	26.530151
204.150460	6157.078551	26.535168
204.421563	6171.238319	26.540186
204.813417	6167.104765	26.545204
204.924683	6171.039619	26.550221
205.397770	6178.907922	26.555239
205.526584	6190.081615	26.560256
205.675529	6202.896828	26.565274
205.840426	6203.054125	26.570292
205.809895	6194.036947	26.575309
205.743369	6215.958431	26.580327
206.058820	6218.181914	26.585344
206.336237	6229.338664	26.590362
206.632286	6247.491039	26.595380
206.747884	6257.729286	26.600397
207.177659	6272.268341	26.605415
207.729121	6279.262612	26.610432
207.427948	6272.308125	26.615450
207.592656	6286.528845	26.620468
208.427003	6293.702936	26.625485
208.394271	6301.060217	26.630503
208.580248	6297.760706	26.635520
208.631490	6315.913619	26.640538
208.975030	6323.543423	26.645556
209.217267	6321.684054	26.650573
208.772066	6331.672420	26.655591
208.965683	6344.310269	26.660608
209.253210	6351.503755	26.665626
209.608542	6369.549104	26.670644
209.978888	6375.100726	26.675661
210.290057	6394.453612	26.680679
210.620729	6388.486031	26.685696
210.639409	6402.489802	26.690714
211.053719	6410.986144	26.695732
210.972923	6417.826974	26.700749
211.061681	6424.237175	26.705767
211.812445	6433.975104	26.710784
211.993380	6447.820906	26.715802
212.024730	6452.734320	26.720820
212.289844	6451.954135	26.725837
212.238425	6465.467005	26.730855
212.903855	6458.152672	26.735872
212.985520	6469.984222	26.740890
213.233973	6483.926805	26.745908
213.405681	6490.144097	26.750925
213.400786	6496.348019	26.755943
213.740675	6500.395499	26.760960
214.106108	6514.291368	26.765978
214.154639	6515.205590	26.770996
214.635398	6515.685911	26.776013
214.574955	6506.408094	26.781031
214.809051	6502.457020	26.786048
214.955593	6521.378095	26.791066
215.225614	6532.813988	26.796084
215.397531	6535.836572	26.801101
215.287848	6540.582694	26.806119
215.714538	6545.292143	26.811136
215.774657	6551.255452	26.816154
216.196279	6555.198592	26.821172
216.568283	6575.419734	26.826189
216.416555	6574.663807	26.831207
216.981117	6571.121844	26.836224
216.818518	6597.879295	26.841242
217.362375	6596.193625	26.846260
217.446620	6598.592276	26.851277
217.765124	6615.273577	26.856295
218.013846	6619.496363	26.861312
217.920391	6623.854832	26.866330
217.732784	6650.808844	26.871348
218.370663	6650.740521	26.876365
218.404872	6667.258056	26.881383
218.510128	6677.027789	26.886400
218.629098	6699.782608	26.891418
218.798263	6723.069411	26.896436
219.776621	6730.337920	26.901453
219.664658	6735.573761	26.906471
219.763264	6753.729158	26.911488
220.190988	6767.296620	26.916506
220.252922	6776.473391	26.921524
220.504419	6783.492751	26.926541
220.726812	6809.590396	26.931559
220.822239	6819.134450	26.936576
221.361173	6832.877108	26.941594
221.584890	6839.436783	26.946612
221.642888	6849.217168	26.951629
221.779094	6858.458109	26.956647
222.061673	6864.683415	26.961664
222.474630	6881.710045	26.966682
222.679220	6900.868653	26.971700
223.148790	6904.526553	26.976717
223.659385	6915.943940	26.981735
223.531836	6927.117204	26.986752
223.678333	6926.898565	26.991770
224.306544	6931.238759	26.996788
224.375325	6938.911865	27.001805
224.430025	6945.027681	27.006823
224.754799	6943.635166	27.011840
224.636987	6961.632102	27.016858
224.600555	6968.901837	27.021876
225.465624	6971.661219	27.026893
225.572836	6983.729022	27.031911
225.643257	6985.343824	27.036928
226.260886	6993.754920	27.041946
226.204658	7007.685652	27.046964
226.667153	7007.335430	27.051981
226.606171	7026.283221	27.056999
227.054227	7021.029448	27.062016
227.119029	7028.539056	27.067034
227.124019	7039.776861	27.072052
227.593631	7051.285989	27.077069
227.850852	7062.484295	27.082087
227.934884	7064.036991	27.087104
228.351838	7076.943421	27.092122
228.439495	7073.384524	27.097140
228.473256	7092.513270	27.102157
228.541427	7091.359828	27.107175
228.978012	7099.221621	27.112192
229.510143	7117.419955	27.117210
229.473376	7119.155739	27.122228
229.666981	7121.382638	27.127245
229.768200	7141.378488	27.132263
229.938520	7148.691671	27.137280
230.059522	7165.473865	27.142298
229.971357	7171.429035	27.147316
230.322258	7172.968346	27.152333
230.673935	7199.046292	27.157351
230.920390	7210.189550	27.162368
231.215027	7232.955393	27.167386
231.412995	7252.759419	27.172404
231.945552	7251.091248	27.177421
232.373490	7261.079081	27.182439
232.611047	7267.141103	27.187456
232.786015	7280.773798	27.192474
232.809447	7289.770597	27.197492
233.252092	7305.631217	27.202509
233.680916	7313.854210	27.207527
233.242654	7316.480028	27.212544
233.923670	7331.173141	27.217562
234.325390	7335.015391	27.222580
234.543732	7340.808950	27.227597
234.495253	7363.612921	27.232615
234.532549	7363.913340	27.237632
234.939721	7366.049988	27.242650
235.527597	7383.775782	27.247668
235.858161	7395.218515	27.252685
235.531542	7398.650821	27.257703
235.935024	7405.817087	27.262720
236.412191	7425.782764	27.267738
236.465777	7426.434212	27.272756
236.813638	7453.753804	27.277773
236.855268	7456.932700	27.282791
236.969136	7462.332258	27.287808
237.480441	7473.045879	27.292826
237.425679	7495.371137	27.297844
238.159226	7499.123556	27.302861
238.063606	7497.099166	27.307879
238.188953	7513.328526	27.312896
238.829597	7530.749440	27.317914
239.108139	7549.590913	27.322932
239.361488	7563.647202	27.327949
239.285193	7560.824218	27.332967
239.422100	7571.896461	27.337984
239.665478	7580.448538	27.343002
240.134251	7594.126992	27.348020
240.446162	7606.538818	27.353037
240.115340	7610.448528	27.358055
240.672309	7629.716858	27.363072
240.799037	7630.997726	27.368090
241.294663	7652.990709	27.373108
241.592089	7658.235289	27.378125
241.587630	7672.976077	27.383143
241.895877	7689.085387	27.388160
242.295449	7695.119013	27.393178
242.459806	7711.386635	27.398196
242.828895	7717.014632	27.403213
242.869059	7740.452370	27.408231
242.995598	7745.963679	27.413248
243.570679	7755.114221	27.418266
243.456395	7759.832964	27.423284
244.005051	7775.645813	27.428301
244.340337	7778.744036	27.433319
244.617296	7786.012354	27.438336
244.937359	7797.747429	27.443354
245.191332	7819.554319	27.448372
245.341724	7806.018711	27.453389
245.699577	7810.606678	27.458407
245.361228	7824.847413	27.463424
246.201987	7826.376340	27.468442
246.199262	7828.880331	27.473460
246.643444	7841.303165	27.478477
246.609405	7846.558684	27.483495
246.967795	7853.072369	27.488512
247.301616	7863.173143	27.493530
247.395422	7875.133134	27.498548
247.292408	7879.120866	27.503565
247.650880	7889.748176	27.508583
247.966763	7908.356860	27.513600
248.159768	7913.317952	27.518618
248.684698	7934.694215	27.523636
248.660310	7934.546534	27.528653
248.986198	7957.526215	27.533671
248.685138	7956.844135	27.538688
249.184813	7971.206266	27.543706
249.382194	7990.515521	27.548724
249.870621	8001.716065	27.553741
250.359016	8013.197600	27.558759
250.854241	8033.262135	27.563776
251.148275	8023.293452	27.568794
251.349706	8038.996754	27.573812
251.332385	8041.610401	27.578829
251.550244	8049.263773	27.583847
252.006643	8065.722738	27.588864
252.147796	8074.310002	27.593882
252.568221	8084.233164	27.598900
252.524187	8089.158824	27.603917
253.286841	8090.845237	27.608935
253.587821	8117.036609	27.613952
253.987352	8120.421592	27.618970
253.848825	8134.476564	27.623988
253.976842	8140.682318	27.629005
254.083003	8140.558384	27.634023
254.452052	8155.080035	27.639040
254.950572	8157.884399	27.644058
254.670106	8171.383887	27.649076
254.613169	8178.376330	27.654093
255.042889	8198.804901	27.659111
255.373025	8222.507222	27.664128
255.715581	8236.341682	27.669146
255.914224	8250.359709	27.674164
256.072702	8254.672782	27.679181
256.282556	8269.364687	27.684199
256.414770	8297.549631	27.689216
256.975270	8304.293856	27.694234
257.175301	8330.507659	27.699252
257.456589	8343.272063	27.704269
257.972507	8359.201042	27.709287
258.174850	8370.528713	27.714304
258.306868	8375.796253	27.719322
258.827395	8402.187264	27.724340
259.236830	8410.808429	27.729357
259.539120	8416.434478	27.734375
259.485814	8424.503026	27.739392
260.527332	8436.760076	27.744410
260.029207	8446.922040	27.749428
260.397210	8455.432902	27.754445
260.705988	8455.785526	27.759463
260.683937	8470.637048	27.764480
261.056809	8486.307560	27.769498
261.497972	8501.203359	27.774516
261.854688	8521.173309	27.779533
262.395401	8522.825075	27.784551
262.191859	8519.971362	27.789568
262.538033	8529.161308	27.794586
262.772532	8536.285032	27.799604
263.018925	8548.919287	27.804621
263.661472	8543.669349	27.809639
263.595475	8566.638563	27.814656
263.861952	8557.715773	27.819674
264.019557	8571.914117	27.824692
263.980417	8583.301847	27.829709
264.303728	8577.486262	27.834727
264.495421	8595.370004	27.839744
264.732994	8610.679800	27.844762
264.965925	8630.353543	27.849780
265.087100	8645.766846	27.854797
265.590267	8652.807484	27.859815
265.779369	8667.749217	27.864832
266.164760	8687.276008	27.869850
266.515154	8699.161608	27.874868
266.768556	8714.257479	27.879885
266.638063	8723.348548	27.884903
266.995386	8739.984653	27.889920
267.369438	8758.667168	27.894938
267.607734	8770.185198	27.899956
267.644987	8787.480823	27.904973
268.410812	8805.404274	27.909991
268.771616	8821.714716	27.915008
269.098900	8824.650196	27.920026
269.184109	8836.931034	27.925044
269.538410	8847.430105	27.930061
270.355796	8856.780032	27.935079
270.225724	8866.095266	27.940096
270.573424	8877.608853	27.945114
270.928450	8892.865755	27.950132
270.642244	8896.197286	27.955149
271.592199	8904.130981	27.960167
271.849775	8916.669020	27.965184
272.124203	8923.306741	27.970202
272.418790	8940.101243	27.975220
272.147671	8947.904204	27.980237
272.649823	8963.640115	27.985255
272.897252	8969.739040	27.990272
273.098308	8975.759986	27.995290
273.341380	8990.788242	28.000308
273.019606	9002.580428	28.005325
273.836787	9014.724619	28.010343
274.213829	9037.719731	28.015360
274.525071	9042.387926	28.020378
274.761239	9071.012405	28.025396
274.724733	9079.053348	28.030413
275.297334	9088.867968	28.035431
275.510560	9110.335466	28.040448
275.399538	9121.968423	28.045466
276.007456	9136.652334	28.050484
275.897234	9155.881544	28.055501
276.483411	9168.279874	28.060519
276.787367	9189.022867	28.065536
277.207138	9198.653107	28.070554
277.448510	9213.883875	28.075572
277.272568	9236.006049	28.080589
278.045619	9225.652273	28.085607
278.475681	9256.841940	28.090624
278.835364	9258.537921	28.095642
279.320206	9274.709355	28.100660
279.169825	9297.465368	28.105677
279.731380	9282.771856	28.110695
280.090109	9309.265283	28.115712
280.191418	9314.383195	28.120730
280.757736	9319.043076	28.125748
280.694682	9342.533741	28.130765
281.373317	9346.077297	28.135783
281.392354	9345.910173	28.140800
280.983265	9355.420910	28.145818
281.535802	9365.403000	28.150836
281.848865	9378.216815	28.155853
282.293755	9385.541549	28.160871
282.742775	9404.503445	28.165888
282.607776	9418.950341	28.170906
282.934773	9419.085435	28.175924
283.232254	9440.180184	28.180941
283.698868	9447.271056	28.185959
283.872016	9463.358876	28.190976
283.827753	9463.596330	28.195994
284.669285	9476.968364	28.201012
284.521204	9503.244672	28.206029
284.763849	9510.601137	28.211047
285.402853	9523.493444	28.216064
285.520920	9545.150005	28.221082
285.607968	9543.074674	28.226100
285.633368	9573.175840	28.231117
286.029983	9592.796547	28.236135
286.169437	9616.170587	28.241152
286.516454	9632.105022	28.246170
286.669024	9640.798574	28.251188
287.084897	9663.617883	28.256205
287.631926	9687.218641	28.261223
288.103093	9702.123336	28.266240
288.228842	9713.340690	28.271258
288.539441	9736.451269	28.276276
288.825313	9751.694452	28.281293
289.581831	9757.173981	28.286311
289.620112	9776.702619	28.291328
290.039522	9801.655921	28.296346
290.191957	9798.648367	28.301364
290.277496	9822.482615	28.306381
290.700929	9829.340438	28.311399
291.292036	9837.747528	28.316416
291.580434	9866.554492	28.321434
292.078686	9861.320480	28.326452
292.111593	9883.896942	28.331469
292.426477	9890.108742	28.336487
292.478889	9910.895103	28.341504
292.607692	9934.192276	28.346522
293.019029	9940.868907	28.351540
292.991767	9956.297077	28.356557
293.778576	9979.945896	28.361575
294.063820	9983.838525	28.366592
294.006245	10013.691337	28.371610
294.802904	10020.642321	28.376628
294.712546	10035.417386	28.381645
295.109858	10045.553613	28.386663
295.956815	10059.512498	28.391680
295.788627	10086.629491	28.396698
296.194598	10096.350768	28.401716
296.424693	10121.564646	28.406733
297.118646	10120.897114	28.411751
297.252989	10136.543239	28.416768
297.051165	10155.206863	28.421786
297.660904	10161.255740	28.426804
298.114282	10175.639470	28.431821
298.382107	10198.340542	28.436839
298.701020	10202.720504	28.441856
298.775191	10218.281401	28.446874
299.199442	10224.397246	28.451892
299.544597	10234.693304	28.456909
299.891105	10243.779855	28.461927
300.465814	10250.816215	28.466944
300.585946	10265.154336	28.471962
301.059186	10266.567398	28.476980
301.140098	10268.221893	28.481997
301.292352	10282.706553	28.487015
301.739627	10290.059690	28.492032
301.798540	10297.849402	28.497050
302.442108	10304.082475	28.502068
302.557381	10310.388834	28.507085
303.059233	10325.393421	28.512103
303.265652	10340.005411	28.517120
303.137676	10345.083745	28.522138
303.341012	10360.728724	28.527156
303.669330	10376.903537	28.532173
303.766576	10392.738822	28.537191
304.393888	10410.319262	28.542208
304.261756	10419.645066	28.547226
305.074946	10435.548213	28.552244
305.331458	10453.300448	28.557261
305.598591	10477.407046	28.562279
305.982216	10483.946128	28.567296
305.870214	10507.344887	28.572314
306.176789	10510.754349	28.577332
306.619519	10536.421733	28.582349
307.022105	10556.168821	28.587367
307.461461	10562.487648	28.592384
307.301863	10587.166434	28.597402
308.160000	10612.888836	28.602420
308.573140	10626.082523	28.607437
308.538397	10648.127415	28.612455
309.203171	10659.485085	28.617472
308.999939	10675.162440	28.622490
309.324841	10688.136338	28.627508
309.933936	10701.757223	28.632525
309.972666	10722.537158	28.637543
310.543372	10730.152155	28.642560
310.474675	10753.787567	28.647578
310.979968	10773.503009	28.652596
311.545901	10796.233892	28.657613
311.912066	10822.740937	28.662631
312.481140	10830.422539	28.667648
312.753947	10847.695808	28.672666
313.248351	10857.327850	28.677684
313.573980	10866.294832	28.682701
313.621541	10876.473671	28.687719
313.929382	10885.718155	28.692736
314.034771	10908.811812	28.697754
314.620058	10920.662042	28.702772
314.929580	10928.261198	28.707789
314.555679	10953.037186	28.712807
315.212737	10967.247532	28.717824
315.735632	10977.029894	28.722842
316.062650	11001.197254	28.727860
316.509960	11019.889513	28.732877
316.906081	11033.142992	28.737895
317.227645	11035.277700	28.742912
317.278077	11066.242525	28.747930
317.411689	11080.386548	28.752948
317.941816	11086.198752	28.757965
318.244801	11097.256556	28.762983
318.797331	11103.835708	28.768000
319.081215	11117.798340	28.773018
319.253985	11129.574388	28.778036
319.915842	11139.783447	28.783053
320.074345	11153.781534	28.788071
320.646351	11163.777333	28.793088
320.866381	11177.948941	28.798106
321.374938	11189.268254	28.803124
321.664689	11192.361560	28.808141
321.625140	11202.405813	28.813159
321.952069	11214.151452	28.818176
321.959522	11225.179843	28.823194
322.232622	11236.760259	28.828212
322.915861	11253.429659	28.833229
322.944159	11267.909239	28.838247
323.379552	11284.156478	28.843264
323.370818	11299.532331	28.848282
323.085924	11307.357375	28.853300
323.925846	11333.285713	28.858317
324.140061	11357.597507	28.863335
324.508782	11377.761261	28.868352
324.752645	11382.784786	28.873370
325.420372	11401.828132	28.878388
325.200017	11420.912724	28.883405
325.886727	11438.364841	28.888423
326.478996	11459.002045	28.893440
326.541481	11482.343111	28.898458
327.140701	11495.287229	28.903476
327.459784	11502.417789	28.908493
327.444479	11523.450215	28.913511
328.077306	11539.145736	28.918528
328.613428	11559.128737	28.923546
328.869364	11567.402814	28.928564
329.322101	11583.218155	28.933581
329.892800	11611.288900	28.938599
329.989246	11610.995955	28.943616
330.091256	11634.662574	28.948634
330.024704	11655.280046	28.953652
331.107246	11673.987130	28.958669
331.206216	11696.245976	28.963687
331.406049	11697.351478	28.968704
331.618840	11725.598451	28.973722
332.257992	11737.229199	28.978740
332.194763	11758.259921	28.983757
332.400306	11777.044490	28.988775
332.954203	11791.669495	28.993792
333.348447	11821.154427	28.998810
333.587979	11840.426338	29.003828
334.687864	11852.730206	29.008845
334.525044	11876.748069	29.013863
335.261352	11891.565620	29.018880
335.294334	11901.387317	29.023898
335.421459	11916.979223	29.028916
335.984364	11928.154690	29.033933
336.203170	11948.020452	29.038951
336.695199	11961.884796	29.043968
337.290680	11980.873737	29.048986
337.596789	11993.447294	29.054004
337.923999	12001.050432	29.059021
338.448956	12019.456805	29.064039
338.583603	12033.487704	29.069056
338.751627	12042.811503	29.074074
338.998811	12054.494374	29.079092
339.435799	12075.971281	29.084109
339.516322	12085.709842	29.089127
339.888210	12110.512627	29.094144
340.406363	12124.780350	29.099162
340.559659	12140.027302	29.104180
341.192884	12144.532166	29.109197
340.997731	12170.516438	29.114215
341.456759	12193.496282	29.119232
341.705645	12213.550237	29.124250
342.044540	12225.610413	29.129268
342.593081	12250.148877	29.134285
342.892622	12269.459194	29.139303
343.441684	12279.266561	29.144320
343.919372	12292.110274	29.149338
343.876887	12311.657362	29.154356
344.450292	12324.776621	29.159373
344.836095	12336.532687	29.164391
344.861642	12359.732210	29.169408
345.231240	12371.162426	29.174426
345.637305	12391.394049	29.179444
346.184439	12404.005914	29.184461
346.156008	12418.122643	29.189479
346.211131	12430.527393	29.194496
346.899815	12445.040219	29.199514
347.016834	12469.734983	29.204532
347.952565	12492.548944	29.209549
347.735955	12513.936106	29.214567
348.030315	12531.213864	29.219584
348.571028	12549.618288	29.224602
348.619169	12561.010554	29.229620
349.283603	12581.675585	29.234637
349.403799	12614.567782	29.239655
349.593490	12627.008424	29.244672
349.888682	12663.170082	29.249690
349.923232	12680.346571	29.254708
350.845705	12702.319717	29.259725
351.604379	12726.238525	29.264743
351.964092	12749.976702	29.269760
352.541887	12766.562917	29.274778
352.619859	12787.834770	29.279796
353.209810	12801.084401	29.284813
353.482271	12812.106946	29.289831
353.871294	12823.022819	29.294848
354.093180	12838.483801	29.299866
354.209797	12862.279146	29.304884
355.079646	12877.420769	29.309901
355.233732	12900.528189	29.314919
355.910031	12916.767528	29.319936
356.369706	12931.465024	29.324954
356.338951	12953.009884	29.329972
357.149109	12961.308289	29.334989
357.403980	12990.191620	29.340007
357.749369	12998.307053	29.345024
357.883483	13013.646138	29.350042
358.184434	13029.543315	29.355060
358.245747	13043.055924	29.360077
358.332664	13071.905687	29.365095
358.829252	13087.680688	29.370112
359.444517	13104.049751	29.375130
359.470725	13135.561775	29.380148
360.155399	13152.201062	29.385165
360.420515	13173.655617	29.390183
361.122265	13198.518690	29.395200
361.461792	13216.661593	29.400218
361.567362	13236.025388	29.405236
361.796070	13255.622551	29.410253
362.325982	13272.598824	29.415271
362.786176	13292.709249	29.420288
363.091547	13300.423705	29.425306
363.449705	13323.679679	29.430324
364.114746	13346.233914	29.435341
364.015319	13362.181455	29.440359
364.520723	13385.818661	29.445376
365.252148	13399.081290	29.450394
365.582544	13417.525823	29.455412
366.045795	13427.899879	29.460429
366.271137	13449.102022	29.465447
366.756538	13464.610664	29.470464
367.365603	13469.678599	29.475482
367.586703	13488.882447	29.480500
367.723023	13493.405475	29.485517
368.189199	13511.636194	29.490535
368.560196	13527.851249	29.495552
368.911125	13542.689418	29.500570
369.006208	13551.153781	29.505588
369.597810	13565.695313	29.510605
369.942555	13569.153046	29.515623
370.393281	13588.336817	29.520640
370.424890	13598.137505	29.525658
370.806645	13621.734372	29.530676
371.096850	13622.358450	29.535693
371.569507	13649.042277	29.540711
371.777718	13671.993735	29.545728
371.795143	13678.493401	29.550746
371.999155	13710.272224	29.555764
372.372173	13721.604826	29.560781
372.910831	13747.043665	29.565799
372.941165	13779.083503	29.570816
373.591070	13807.366177	29.575834
374.097473	13830.770088	29.580852
374.443078	13859.274198	29.585869
374.914832	13886.069032	29.590887
374.849962	13904.579111	29.595904
375.487115	13930.561744	29.600922
375.624345	13953.392021	29.605940
376.267206	13991.074473	29.610957
376.870968	14022.216433	29.615975
377.151837	14042.387325	29.620992
377.971388	14059.255774	29.626010
377.978512	14090.851325	29.631028
378.369391	14105.004688	29.636045
378.724345	14130.662302	29.641063
379.197978	14148.586131	29.646080
379.933370	14168.581744	29.651098
380.059858	14186.793685	29.656116
380.573127	14206.344099	29.661133
381.376008	14222.555262	29.666151
381.194800	14241.544975	29.671168
381.784448	14256.008393	29.676186
382.422050	14280.068143	29.681204
382.632184	14297.487033	29.686221
383.498767	14317.070647	29.691239
383.557036	14327.486527	29.696256
384.281313	14341.281506	29.701274
384.090019	14361.605648	29.706292
384.445823	14382.804189	29.711309
385.315488	14396.453268	29.716327
385.032479	14408.239593	29.721344
385.718955	14428.953724	29.726362
385.929809	14465.912093	29.731380
386.506717	14481.700943	29.736397
386.794482	14500.307956	29.741415
387.076471	14515.700888	29.746432
387.509558	14536.217965	29.751450
387.980417	14564.870896	29.756468
388.226021	14579.631629	29.761485
389.037968	14598.320856	29.766503
389.243058	14611.076205	29.771520
389.301027	14626.804344	29.776538
390.096419	14652.289453	29.781556
390.247714	14675.904780	29.786573
390.807865	14695.486253	29.791591
391.004763	14722.060032	29.796608
391.267098	14742.319841	29.801626
391.456630	14765.436611	29.806644
391.562390	14787.240086	29.811661
392.521670	14816.480113	29.816679
392.330019	14844.564540	29.821696
392.889675	14866.003294	29.826714
393.744771	14887.253676	29.831732
393.951344	14908.182463	29.836749
394.438187	14923.947889	29.841767
394.718939	14949.757193	29.846784
395.201152	14964.512745	29.851802
395.610003	14986.240548	29.856820
395.856440	15013.909197	29.861837
396.543958	15024.485870	29.866855
396.886512	15047.620070	29.871872
397.254472	15052.473543	29.876890
397.640625	15078.727615	29.881908
397.963895	15095.917911	29.886925
398.398871	15117.629138	29.891943
398.850343	15146.800776	29.896960
398.974015	15155.905661	29.901978
399.347844	15174.926217	29.906996
399.648963	15195.117267	29.912013
400.445558	15224.490785	29.917031
400.382538	15255.338105	29.922048
400.906529	15272.178133	29.927066
401.245180	15303.562689	29.932084
401.759302	15322.166631	29.937101
402.544201	15351.406370	29.942119
402.341897	15377.023460	29.947136
402.919261	15401.845741	29.952154
404.032747	15422.001374	29.957172
403.753811	15451.057329	29.962189
404.379819	15466.138161	29.967207
404.626489	15507.062935	29.972224
405.460785	15515.655575	29.977242
405.657844	15543.869640	29.982260
405.753152	15565.618789	29.987277
406.224139	15582.337902	29.992295
406.788851	15606.376006	29.997312
407.428302	15629.265431	30.002330
408.178860	15648.900176	30.007348
408.450337	15670.615534	30.012365
408.953163	15690.876580	30.017383
408.960121	15715.747556	30.022400
409.509057	15731.544984	30.027418
409.948151	15749.355714	30.032436
410.252129	15775.636248	30.037453
410.671794	15792.711004	30.042471
410.934890	15820.280301	30.047488
411.462644	15837.142347	30.052506
412.326756	15858.294492	30.057524
412.827704	15871.844471	30.062541
413.437823	15884.733050	30.067559
413.985254	15915.552140	30.072576
414.231624	15919.433147	30.077594
414.597907	15939.052581	30.082612
414.521858	15961.918666	30.087629
415.013988	15971.926378	30.092647
415.149275	15997.204002	30.097664
415.612487	16011.540116	30.102682
415.764244	16031.278524	30.107700
416.256495	16058.600656	30.112717
417.003921	16086.069205	30.117735
417.109245	16109.848264	30.122752
417.480357	16129.666118	30.127770
417.945678	16159.487766	30.132788
418.476306	16188.838101	30.137805
419.134449	16208.026766	30.142823
419.186463	16240.822199	30.147840
419.763872	16268.229203	30.152858
420.244814	16278.807348	30.157876
420.641772	16314.157754	30.162893
420.976665	16336.435613	30.167911
421.055357	16360.825577	30.172928
421.353888	16385.408548	30.177946
422.026171	16411.227980	30.182964
422.259087	16427.482926	30.187981
423.174574	16443.804687	30.192999
423.134683	16472.050914	30.198016
423.476163	16495.717657	30.203034
424.084674	16515.315532	30.208052
424.360426	16553.572219	30.213069
425.284065	16557.464137	30.218087
425.363221	16592.062575	30.223104
425.573799	16622.818699	30.228122
425.995988	16644.549454	30.233140
426.377918	16664.814674	30.238157
427.028269	16697.289751	30.243175
427.666257	16726.883090	30.248192
427.676167	16749.067039	30.253210
428.358856	16778.523956	30.258228
428.619848	16807.140470	30.263245
429.059171	16825.438579	30.268263
429.601616	16855.407154	30.273280
430.168442	16876.430113	30.278298
430.819868	16898.220006	30.283316
431.190290	16927.609196	30.288333
432.282640	16942.848725	30.293351
432.365129	16964.794137	30.298368
432.409016	16991.805640	30.303386
433.316361	17009.098839	30.308404
433.849425	17025.957942	30.313421
434.437451	17047.634751	30.318439
434.807289	17067.930717	30.323456
435.111728	17090.586931	30.328474
435.448476	17109.207759	30.333492
435.542914	17131.233612	30.338509
435.930528	17143.169254	30.343527
436.432006	17180.614816	30.348544
436.906526	17200.483908	30.353562
437.420393	17226.215539	30.358580
437.888327	17254.765560	30.363597
438.470161	17275.792923	30.368615
438.840902	17299.437119	30.373632
438.980164	17321.727809	30.378650
439.754413	17339.402236	30.383668
439.893634	17373.335673	30.388685
440.568102	17393.420018	30.393703
441.013727	17415.656513	30.398720
441.528234	17440.345981	30.403738
442.047142	17469.507429	30.408756
442.252294	17498.098970	30.413773
442.506149	17510.845452	30.418791
443.119061	17538.248705	30.423808
443.590273	17565.408865	30.428826
443.902801	17589.473160	30.433844
444.003270	17614.429856	30.438861
444.914736	17649.923230	30.443879
445.236778	17677.441731	30.448896
445.443483	17705.502678	30.453914
446.252142	17731.049827	30.458932
446.161114	17759.233294	30.463949
446.587220	17788.207602	30.468967
447.093552	17811.938583	30.473984
447.603660	17839.465762	30.479002
448.432405	17865.749080	30.484020
448.858704	17902.696107	30.489037
449.104624	17921.698356	30.494055
450.208052	17953.952966	30.499072
450.179434	17988.330720	30.504090
451.168130	18001.941633	30.509108
451.088142	18020.887629	30.514125
451.533713	18038.999546	30.519143
452.069884	18057.027798	30.524160
452.093747	18084.492501	30.529178
452.917926	18107.529677	30.534196
453.536780	18126.758002	30.539213
453.758854	18148.291207	30.544231
454.575397	18178.695877	30.549248
454.371802	18185.165353	30.554266
455.248686	18211.997544	30.559284
455.669026	18235.205524	30.564301
456.615111	18263.018801	30.569319
456.678711	18276.951698	30.574336
456.942065	18305.636396	30.579354
457.485749	18317.017644	30.584372
457.848057	18352.465655	30.589389
458.247046	18364.223379	30.594407
458.518407	18386.317711	30.599424
458.975483	18409.501193	30.604442
459.736266	18448.064713	30.609460
460.089458	18475.421529	30.614477
460.654257	18504.109845	30.619495
461.045285	18527.089013	30.624512
461.212305	18552.346056	30.629530
462.280251	18579.489984	30.634548
462.449303	18608.177263	30.639565
462.934131	18633.681564	30.644583
463.386806	18657.339856	30.649600
464.195181	18693.457789	30.654618
464.203548	18709.958310	30.659636
464.753981	18741.498505	30.664653
465.172405	18757.018772	30.669671
465.481294	18794.642928	30.674688
466.278802	18827.035360	30.679706
466.694683	18857.497534	30.684724
466.903167	18887.404689	30.689741
467.328421	18907.687587	30.694759
468.164947	18938.709460	30.699776
468.604164	18973.893847	30.704794
468.841931	19003.259583	30.709812
469.523711	19025.201909	30.714829
470.424851	19054.192153	30.719847
470.759182	19089.121511	30.724864
471.073605	19108.417447	30.729882
471.730419	19130.850274	30.734900
472.196064	19159.441368	30.739917
472.355362	19189.242969	30.744935
472.931608	19201.535726	30.749952
473.247258	19237.226418	30.754970
473.971065	19256.079307	30.759988
474.412569	19289.071606	30.765005
475.133647	19314.034366	30.770023
475.174565	19335.875248	30.775040
475.587002	19366.414571	30.780058
476.470849	19383.802037	30.785076
476.910893	19419.511485	30.790093
477.471884	19441.574288	30.795111
478.020124	19458.521587	30.800128
478.284125	19488.117708	30.805146
479.006918	19514.603080	30.810164
479.390777	19539.795850	30.815181
480.096889	19566.037505	30.820199
480.611077	19586.869481	30.825216
480.565195	19608.882212	30.830234
481.158958	19631.154907	30.835252
481.262097	19671.371766	30.840269
482.106369	19686.383816	30.845287
482.144587	19709.988262	30.850304
482.506401	19743.954150	30.855322
483.043983	19777.109130	30.860340
483.597160	19789.355329	30.865357
484.446492	19816.750045	30.870375
485.045632	19840.285746	30.875392
485.415631	19869.669983	30.880410
486.064651	19885.736295	30.885428
486.393945	19913.667500	30.890445
486.491184	19934.002844	30.895463
487.526857	19962.600604	30.900480
487.637296	19987.369238	30.905498
487.916642	20017.349160	30.910516
488.420172	20041.127531	30.915533
489.254192	20066.857013	30.920551
489.613728	20096.413818	30.925568
489.822072	20127.510704	30.930586
490.431560	20153.079604	30.935604
490.935001	20189.684027	30.940621
491.320320	20209.007856	30.945639
492.171737	20242.152380	30.950656
492.273661	20266.827927	30.955674
492.818998	20290.739054	30.960692
493.301099	20329.564768	30.965709
493.953104	20369.267453	30.970727
494.706555	20391.730825	30.975744
495.015977	20428.176535	30.980762
495.487317	20458.986342	30.985780
495.941709	20489.647214	30.990797
496.111327	20520.908745	30.995815
496.798229	20554.003746	31.000832
497.031100	20593.450300	31.005850
497.749114	20613.366885	31.010868
498.522853	20647.750014	31.015885
498.829383	20678.642845	31.020903
499.460298	20709.598647	31.025920
499.945289	20753.814287	31.030938
500.741203	20779.626496	31.035956
501.361750	20805.207154	31.040973
501.696362	20841.188444	31.045991
502.561019	20860.797987	31.051008
502.610932	20892.502189	31.056026
503.366975	20919.274905	31.061044
503.965762	20944.707511	31.066061
504.426926	20970.003745	31.071079
504.913750	20994.948479	31.076096
505.503376	21022.650936	31.081114
505.826703	21054.451581	31.086132
506.618354	21079.203355	31.091149
506.919563	21115.411524	31.096167
507.417050	21132.962163	31.101184
507.952442	21162.290839	31.106202
508.228906	21185.891335	31.111220
508.605555	21219.415160	31.116237
508.962836	21250.774828	31.121255
509.683525	21278.495029	31.126272
510.016175	21316.290909	31.131290
510.638716	21346.294929	31.136308
511.268576	21382.439477	31.141325
511.824381	21408.656598	31.146343
512.474183	21437.689749	31.151360
512.910100	21470.478083	31.156378
513.529287	21490.505819	31.161396
514.468984	21517.332728	31.166413
514.806757	21541.044100	31.171431
515.567750	21567.652642	31.176448
516.021586	21600.166686	31.181466
516.461765	21617.808876	31.186484
517.031229	21627.658920	31.191501
517.387582	21654.697436	31.196519
517.922066	21672.407047	31.201536
518.118641	21701.195641	31.206554
518.604824	21721.282355	31.211572
518.977944	21740.919217	31.216589
519.288106	21778.751098	31.221607
519.960054	21792.028852	31.226624
520.558898	21828.589792	31.231642
520.519343	21856.777407	31.236660
521.400787	21883.032619	31.241677
521.519886	21914.083118	31.246695
522.283541	21945.917335	31.251712
522.771430	21981.459664	31.256730
523.307489	22019.180800	31.261748
523.655818	22038.733379	31.266765
523.937315	22081.227254	31.271783
524.552124	22110.513310	31.276800
525.110005	22159.213340	31.281818
525.538336	22187.530347	31.286836
526.163122	22227.500116	31.291853
526.687747	22263.479515	31.296871
527.332612	22296.065887	31.301888
527.848859	22335.958092	31.306906
528.213150	22369.435255	31.311924
528.952616	22413.292497	31.316941
529.658513	22451.904095	31.321959
530.873847	22495.598523	31.326976
531.031604	22522.593504	31.331994
531.573823	22543.544288	31.337012
532.520337	22574.908556	31.342029
532.737444	22604.428243	31.347047
533.416620	22636.112511	31.352064
533.982316	22663.239678	31.357082
534.389535	22689.488092	31.362100
535.061482	22721.078844	31.367117
535.190025	22755.320264	31.372135
536.100087	22782.734885	31.377152
536.484298	22806.175104	31.382170
537.256188	22857.857497	31.387188
537.583570	22877.376271	31.392205
538.561041	22911.996842	31.397223
538.980983	22943.873862	31.402240
539.531960	22956.994416	31.407258
540.064576	22999.558352	31.412276
540.791093	23021.858334	31.417293
541.286077	23051.448908	31.422311
541.884661	23070.249255	31.427328
542.220249	23099.289827	31.432346
542.507690	23131.883001	31.437364
543.285029	23156.867116	31.442381
543.829540	23195.581269	31.447399
544.219967	23214.761906	31.452416
544.644834	23245.810832	31.457434
545.049982	23283.529602	31.462452
545.924895	23307.013622	31.467469
546.284903	23340.562605	31.472487
546.775682	23375.165423	31.477504
547.473913	23415.321979	31.482522
547.981427	23446.661596	31.487540
548.439724	23472.770341	31.492557
548.633278	23508.310952	31.497575
549.487309	23540.177814	31.502592
550.096685	23569.574304	31.507610
550.160583	23609.969625	31.512628
550.914487	23633.694159	31.517645
551.747197	23670.525192	31.522663
552.259060	23706.471290	31.527680
552.936547	23741.677432	31.532698
553.353263	23776.431572	31.537716
553.918737	23790.201297	31.542733
554.331616	23832.419248	31.547751
554.816018	23860.755136	31.552768
555.511414	23887.794151	31.557786
555.722020	23917.519022	31.562804
557.199549	23940.106853	31.567821
557.656713	23974.311538	31.572839
558.308652	23994.248210	31.577856
559.063349	24013.025000	31.582874
559.294660	24032.623149	31.587892
559.891369	24053.573314	31.592909
560.232972	24084.358534	31.597927
560.782037	24115.136588	31.602944
561.554116	24138.795684	31.607962
561.851441	24159.179865	31.612980
562.532835	24187.927727	31.617997
562.643740	24230.282285	31.623015
562.752491	24251.669291	31.628032
563.777032	24284.521754	31.633050
564.193568	24329.754570	31.638068
564.474243	24360.954206	31.643085
565.363525	24408.148037	31.648103
565.904890	24442.144430	31.653120
566.841399	24475.870451	31.658138
567.394247	24513.258756	31.663156
567.692324	24544.797208	31.668173
568.487864	24583.285153	31.673191
569.124158	24611.882700	31.678208
569.786755	24651.497523	31.683226
570.178187	24689.556035	31.688244
570.990499	24719.585995	31.693261
571.279710	24754.728343	31.698279
571.975789	24788.448310	31.703296
572.465699	24817.429295	31.708314
573.116887	24857.823629	31.713332
573.731605	24895.114481	31.718349
574.123664	24932.149570	31.723367
575.063190	24966.135053	31.728384
576.026727	24994.523902	31.733402
576.162325	25030.998969	31.738420
576.966996	25051.083410	31.743437
577.640069	25078.159132	31.748455
578.322772	25116.185475	31.753472
578.526851	25131.169240	31.758490
579.114036	25175.789504	31.763508
579.438085	25204.266166	31.768525
580.061946	25244.520204	31.773543
580.344258	25280.208052	31.778560
581.643305	25317.165001	31.783578
582.095560	25350.810344	31.788596
582.575709	25380.729003	31.793613
583.443674	25414.814933	31.798631
583.843404	25451.546426	31.803648
584.567940	25478.361835	31.808666
584.915525	25502.417662	31.813684
585.842193	25525.807717	31.818701
586.224049	25556.949126	31.823719
586.702795	25596.335495	31.828736
587.600726	25616.589175	31.833754
588.363295	25648.777082	31.838772
588.783543	25673.630681	31.843789
589.319256	25712.856678	31.848807
589.869189	25748.497123	31.853824
590.601172	25772.461471	31.858842
590.691075	25807.586314	31.863860
591.224796	25833.452490	31.868877
592.209863	25870.364834	31.873895
592.450040	25904.878554	31.878912
593.098481	25927.984014	31.883930
593.738945	25962.334022	31.888948
594.126281	25984.690440	31.893965
594.671917	26019.099637	31.898983
595.077656	26050.288629	31.904000
595.863587	26072.664880	31.909018
596.463312	26115.882217	31.914036
597.074260	26147.797626	31.919053
597.682554	26180.313908	31.924071
597.779872	26212.398343	31.929088
598.437810	26239.041915	31.934106
598.902241	26291.267978	31.939124
599.852943	26327.573492	31.944141
600.322137	26355.498161	31.949159
600.654840	26402.948172	31.954176
601.481000	26434.684967	31.959194
601.993545	26478.112657	31.964212
602.699213	26522.022129	31.969229
603.309374	26565.624324	31.974247
603.731086	26604.971032	31.979264
604.597251	26635.140788	31.984282
605.237122	26685.539133	31.989300
605.799367	26728.359155	31.994317
606.773653	26766.848569	31.999335
606.959128	26804.962294	32.004352
607.859034	26845.884166	32.009370
608.465522	26880.582353	32.014388
609.009784	26914.822642	32.019405
609.583649	26959.922960	32.024423
610.344411	26996.120378	32.029440
611.050536	27029.109368	32.034458
611.478194	27078.669721	32.039476
612.193803	27110.696667	32.044493
612.872680	27148.487269	32.049511
613.483865	27182.395191	32.054528
614.193372	27218.499907	32.059546
614.676366	27259.178210	32.064564
615.551857	27303.366159	32.069581
616.219837	27336.190972	32.074599
616.659015	27377.306163	32.079616
617.690790	27411.704797	32.084634
617.960243	27444.946146	32.089652
618.518392	27483.394647	32.094669
619.222209	27523.204592	32.099687
619.749548	27560.071622	32.104704
620.646552	27594.491673	32.109722
621.046196	27632.200498	32.114740
621.670944	27671.391066	32.119757
622.196710	27704.561095	32.124775
622.923169	27747.325946	32.129792
623.696367	27782.758033	32.134810
624.328085	27815.955894	32.139828
624.644854	27856.579258	32.144845
625.604635	27886.989042	32.149863
626.060120	27937.318242	32.154880
626.786118	27963.251838	32.159898
627.304049	28004.191625	32.164916
627.952634	28046.962982	32.169933
628.618026	28085.054509	32.174951
629.149143	28118.060036	32.179968
629.837628	28155.402240	32.184986
630.799642	28191.684043	32.190004
630.939892	28230.085629	32.195021
631.812885	28262.279365	32.200039
632.239596	28303.973563	32.205056
633.455258	28339.773456	32.210074
634.087530	28375.569965	32.215092
634.318821	28409.754334	32.220109
634.991313	28434.761439	32.225127
635.628277	28470.829174	32.230144
635.993249	28494.588753	32.235162
636.642010	28525.282071	32.240180
637.270228	28563.424559	32.245197
637.706813	28591.610242	32.250215
638.058536	28631.376363	32.255232
638.917129	28666.935673	32.260250
639.286951	28721.293952	32.265268
639.706909	28752.529112	32.270285
641.006657	28795.117888	32.275303
641.217288	28847.067894	32.280320
642.043439	28877.891983	32.285338
642.749480	28929.290544	32.290356
643.210863	28970.911142	32.295373
643.632537	29005.161503	32.300391
644.050487	29054.146649	32.305408
644.624194	29097.854792	32.310426
645.508712	29149.984472	32.315444
646.351464	29200.793415	32.320461
647.381285	29238.141030	32.325479
647.468115	29293.619717	32.330496
648.192209	29332.526110	32.335514
649.005090	29386.311081	32.340532
649.334382	29437.763597	32.345549
650.537143	29473.655995	32.350567
651.063596	29520.830074	32.355584
652.284838	29560.714666	32.360602
652.817756	29600.542784	32.365620
653.411882	29650.829199	32.370637
654.201273	29683.701987	32.375655
654.975613	29737.683548	32.380672
655.710979	29772.322223	32.385690
656.473987	29808.688633	32.390708
657.152334	29845.934371	32.395725
658.126205	29884.499276	32.400743
658.603768	29920.626132	32.405760
659.289301	29961.303377	32.410778
659.802326	29993.379218	32.415796
660.455020	30024.946499	32.420813
661.266048	30057.253905	32.425831
661.630997	30099.163705	32.430848
662.319898	30130.339880	32.435866
663.340709	30177.526542	32.440884
663.698309	30216.352936	32.445901
664.415585	30243.946977	32.450919
664.834884	30292.903254	32.455936
665.306253	30332.236720	32.460954
666.615398	30373.316504	32.465972
666.780999	30418.943527	32.470989
667.759614	30448.121507	32.476007
668.345256	30490.610714	32.481024
668.659876	30521.542668	32.486042
669.453573	30563.721301	32.491060
669.990933	30612.767312	32.496077
671.080526	30653.426896	32.501095
671.788930	30693.248608	32.506112
672.725363	30736.543104	32.511130
673.603846	30772.077662	32.516148
673.798731	30811.019157	32.521165
674.459652	30835.872966	32.526183
675.035327	30874.976200	32.531200
675.870753	30916.700192	32.536218
676.376308	30962.091848	32.541236
677.044087	30995.542073	32.546253
677.669151	31035.978045	32.551271
678.553048	31081.519325	32.556288
678.830968	31110.441324	32.561306
679.529201	31133.152952	32.566324
680.128142	31184.270478	32.571341
680.718083	31220.811880	32.576359
681.425037	31255.248883	32.581376
681.801800	31291.830117	32.586394
682.577178	31335.606247	32.591412
682.986525	31379.686338	32.596429
684.306060	31431.311148	32.601447
684.694994	31463.497208	32.606464
685.162098	31502.890463	32.611482
685.659957	31537.790557	32.616500
686.664841	31594.149441	32.621517
687.256388	31628.377555	32.626535
687.798941	31681.717747	32.631552
688.332942	31720.013595	32.636570
690.120566	31770.529175	32.641588
690.663780	31810.347297	32.646605
691.079649	31842.276854	32.651623
691.884868	31893.755775	32.656640
692.365833	31941.473534	32.661658
693.625947	31971.026825	32.666676
694.156977	32015.297829	32.671693
694.755912	32042.729470	32.676711
695.493111	32094.377587	32.681728
696.047137	32132.108410	32.686746
696.929992	32173.479799	32.691764
697.338891	32220.020964	32.696781
698.253086	32253.598998	32.701799
698.818755	32310.717698	32.706816
699.742064	32354.807874	32.711834
700.827375	32389.370844	32.716852
701.103427	32433.884970	32.721869
701.898297	32467.134327	32.726887
702.686602	32519.521489	32.731904
703.427671	32551.704664	32.736922
704.242035	32588.858173	32.741940
704.786954	32637.566391	32.746957
705.406908	32678.120156	32.751975
706.142357	32710.203302	32.756992
706.834127	32765.337335	32.762010
707.632208	32789.640951	32.767028
707.699896	32841.029082	32.772045
708.727272	32880.937804	32.777063
709.932929	32938.590210	32.782080
710.589287	32971.324680	32.787098
711.629383	33003.404825	32.792116
712.084705	33052.134362	32.797133
712.659436	33090.786714	32.802151
713.513276	33139.536235	32.807168
713.968223	33177.233885	32.812186
714.869859	33215.297885	32.817204
715.712241	33266.401363	32.822221
716.312644	33303.469528	32.827239
717.029832	33349.648816	32.832256
717.375626	33388.931862	32.837274
718.615338	33430.464818	32.842292
718.991305	33474.794809	32.847309
719.618089	33516.790615	32.852327
720.265090	33554.585315	32.857344
720.864058	33607.200844	32.862362
721.735959	33640.914182	32.867380
722.245293	33689.933894	32.872397
722.668365	33742.330735	32.877415
723.685629	33794.267957	32.882432
724.209140	33853.964362	32.887450
725.417293	33898.892005	32.892468
725.858356	33947.050512	32.897485
726.444245	33987.485697	32.902503
727.406870	34024.820857	32.907520
727.748148	34069.960488	32.912538
728.615986	34104.358035	32.917556
729.270595	34150.156890	32.922573
729.976083	34200.967955	32.927591
730.855650	34236.799095	32.932608
731.222756	34283.680157	32.937626
732.031758	34324.296017	32.942644
732.807248	34381.988144	32.947661
733.779016	34428.117290	32.952679
734.486782	34465.404628	32.957696
735.378770	34511.382063	32.962714
736.169365	34555.187848	32.967732
736.949742	34607.214755	32.972749
737.628024	34648.819075	32.977767
738.646775	34682.934708	32.982784
739.254788	34736.234490	32.987802
740.115407	34766.309539	32.992820
740.608764	34822.087018	32.997837
741.317206	34860.430840	33.002855
742.208248	34904.721116	33.007872
742.855772	34949.776735	33.012890
743.657389	34991.969401	33.017908
744.388409	35041.140899	33.022925
745.474412	35088.771067	33.027943
745.983301	35127.450117	33.032960
746.706535	35181.491714	33.037978
747.523436	35222.310397	33.042996
748.374853	35271.937789	33.048013
749.174847	35314.637181	33.053031
749.755624	35356.435204	33.058048
750.573192	35396.805196	33.063066
751.379049	35443.449405	33.068084
752.229167	35483.915632	33.073101
753.117013	35534.916329	33.078119
754.030597	35576.902941	33.083136
754.912935	35614.278783	33.088154
755.570891	35656.356167	33.093172
756.327460	35693.119547	33.098189
757.171827	35737.412553	33.103207
757.906246	35781.824037	33.108224
758.360392	35824.774629	33.113242
759.529817	35858.394342	33.118260
760.133806	35904.438876	33.123277
760.193116	35947.116424	33.128295
761.611950	35993.141040	33.133312
762.200726	36037.032083	33.138330
763.175589	36076.847601	33.143348
763.784578	36130.928477	33.148365
764.186193	36177.757742	33.153383
765.086809	36217.913953	33.158400
766.066790	36268.965217	33.163418
766.729037	36316.904784	33.168436
767.264982	36363.991642	33.173453
768.208742	36409.237928	33.178471
769.198192	36467.117217	33.183488
769.606380	36507.901206	33.188506
770.469398	36554.899328	33.193524
771.291368	36598.438849	33.198541
772.064601	36652.824138	33.203559
772.889839	36688.984102	33.208576
773.492950	36735.157035	33.213594
774.570942	36774.483465	33.218612
775.354015	36829.588518	33.223629
775.958296	36879.656734	33.228647
777.105942	36916.519072	33.233664
777.734619	36957.908049	33.238682
778.352288	36997.085657	33.243700
779.045629	37034.822407	33.248717
779.830468	37081.928783	33.253735
780.933937	37117.982673	33.258752
781.405010	37147.780641	33.263770
782.098919	37194.054168	33.268788
782.586989	37235.541582	33.273805
783.254604	37272.435442	33.278823
784.080495	37303.954949	33.283840
784.609789	37359.082137	33.288858
785.365419	37391.953349	33.293876
786.368063	37455.581284	33.298893
786.861365	37496.062949	33.303911
787.979945	37551.945703	33.308928
788.613076	37608.948004	33.313946
789.272258	37651.598251	33.318964
790.236845	37703.237123	33.323981
790.729790	37760.540015	33.328999
791.682881	37810.309166	33.334016
792.573806	37867.322373	33.339034
793.531479	37917.381941	33.344052
794.209883	37986.178035	33.349069
795.093340	38021.047437	33.354087
795.879676	38072.588638	33.359104
796.532821	38135.299473	33.364122
797.838215	38181.194810	33.369140
798.415704	38230.947869	33.374157
799.167335	38279.864336	33.379175
800.280027	38334.156470	33.384192
800.852707	38383.461649	33.389210
801.617655	38437.934974	33.394228
802.532388	38494.825964	33.399245
803.325771	38548.207424	33.404263
804.123008	38601.607383	33.409280
804.985590	38653.226568	33.414298
805.787300	38702.629412	33.419316
806.716394	38742.849143	33.424333
807.285149	38798.757999	33.429351
808.319913	38852.431255	33.434368
808.859421	38906.144254	33.439386
810.017618	38961.556500	33.444404
810.825277	39007.683318	33.449421
811.538927	39066.384331	33.454439
812.785781	39121.466907	33.459456
813.632146	39174.285109	33.464474
814.439909	39207.365951	33.469492
815.236105	39257.795417	33.474509
816.187229	39316.251230	33.479527
817.170456	39351.265267	33.484544
817.778722	39399.428865	33.489562
818.719960	39442.076435	33.494580
819.559797	39489.128879	33.499597
820.266037	39530.972320	33.504615
820.957929	39583.929544	33.509632
821.733719	39632.326716	33.514650
822.846275	39681.581937	33.519668
823.751763	39723.280715	33.524685
824.187150	39763.105344	33.529703
824.979847	39806.244880	33.534720
825.783572	39850.072110	33.539738
826.738022	39909.705303	33.544756
827.584520	39942.863420	33.549773
828.088527	40006.988039	33.554791
829.266398	40052.888358	33.559808
829.831313	40105.461987	33.564826
830.471643	40159.080087	33.569844
831.653556	40217.091112	33.574861
832.762370	40256.570872	33.579879
833.489565	40294.358626	33.584896
834.400594	40329.796631	33.589914
834.993898	40370.242726	33.594932
836.063333	40410.222230	33.599949
836.423863	40451.590335	33.604967
837.280717	40484.931065	33.609984
837.942734	40527.618168	33.615002
838.510731	40577.725946	33.620020
839.551742	40619.892204	33.625037
840.180388	40678.712078	33.630055
841.124575	40719.761619	33.635072
842.063087	40771.955809	33.640090
842.792017	40820.502102	33.645108
843.629747	40869.195903	33.650125
844.206942	40922.825769	33.655143
845.414986	40976.584666	33.660160
846.528644	41021.769768	33.665178
847.467638	41072.623803	33.670196
848.388294	41115.328478	33.675213
849.058079	41171.733585	33.680231
849.957682	41223.523851	33.685248
850.941103	41267.724247	33.690266
851.368297	41324.490288	33.695284
852.418933	41368.787883	33.700301
853.151173	41429.674358	33.705319
853.793822	41477.527261	33.710336
854.927986	41523.633591	33.715354
855.653521	41584.863081	33.720372
856.605668	41648.549190	33.725389
857.227263	41695.627927	33.730407
858.243673	41757.596617	33.735424
859.455375	41805.291558	33.740442
860.008715	41858.029335	33.745460
861.070439	41904.489348	33.750477
861.980356	41977.815668	33.755495
862.673690	42026.053968	33.760512
863.879429	42081.441420	33.765530
864.411928	42140.273950	33.770548
865.644186	42179.978207	33.775565
866.591096	42244.583970	33.780583
867.300141	42290.613010	33.785600
868.717482	42345.088833	33.790618
869.096429	42395.236694	33.795636
870.324865	42436.206998	33.800653
871.189098	42487.708517	33.805671
872.048971	42550.083450	33.810688
872.668048	42596.721764	33.815706
873.645010	42652.361527	33.820724
874.872971	42681.896777	33.825741
875.534656	42743.322915	33.830759
876.280625	42781.225874	33.835776
877.172602	42833.508161	33.840794
877.802374	42888.829707	33.845812
879.088299	42925.649007	33.850829
880.117387	42984.810837	33.855847
880.853585	43034.138875	33.860864
881.618256	43082.741501	33.865882
882.280241	43144.902422	33.870900
883.328647	43184.776437	33.875917
884.256382	43242.424142	33.880935
884.948426	43294.694551	33.885952
886.068653	43351.882289	33.890970
886.588758	43403.016040	33.895988
887.927776	43459.935766	33.901005
888.704032	43503.021907	33.906023
889.597917	43554.179708	33.911040
890.329553	43604.123281	33.916058
890.899428	43666.034426	33.921076
891.646139	43700.858434	33.926093
893.055633	43753.795597	33.931111
893.844677	43794.951085	33.936128
894.733623	43837.583784	33.941146
895.304127	43881.955295	33.946164
896.355230	43926.877851	33.951181
897.060363	43971.943227	33.956199
898.057430	44012.946364	33.961216
899.042337	44060.681702	33.966234
899.682142	44121.836772	33.971252
900.572468	44170.776333	33.976269
901.286210	44229.984542	33.981287
902.095347	44276.944535	33.986304
903.133328	44329.302375	33.991322
903.801995	44393.704965	33.996340
905.029747	44435.204103	34.001357
905.866171	44504.875193	34.006375
906.517390	44561.703027	34.011392
907.572915	44627.949707	34.016410
908.534182	44684.438331	34.021428
909.651584	44735.108412	34.026445
910.639936	44799.253373	34.031463
911.400075	44862.314617	34.036480
912.434699	44919.342679	34.041498
913.219601	44974.094799	34.046516
914.475530	45022.884102	34.051533
915.233307	45078.254315	34.056551
916.195149	45137.533623	34.061568
917.330756	45186.652084	34.066586
917.993522	45251.798181	34.071604
919.111840	45314.912156	34.076621
920.483190	45369.004101	34.081639
921.213019	45422.374273	34.086656
922.371720	45469.573029	34.091674
923.278400	45518.639504	34.096692
923.886175	45567.189891	34.101709
924.776733	45617.182676	34.106727
925.679394	45684.183894	34.111744
926.719042	45737.329182	34.116762
927.478198	45803.347412	34.121780
928.393786	45853.102746	34.126797
929.170574	45915.632974	34.131815
930.315591	45970.122388	34.136832
931.725141	46021.375910	34.141850
932.498092	46083.881904	34.146868
933.453346	46136.339169	34.151885
934.572007	46185.215762	34.156903
935.099920	46244.616550	34.161920
936.132876	46296.226989	34.166938
937.098030	46350.384905	34.171956
938.205251	46408.019017	34.176973
939.252389	46461.348302	34.181991
940.174371	46524.186444	34.187008
940.810714	46580.958465	34.192026
942.412181	46637.016489	34.197044
942.916767	46686.452129	34.202061
943.771382	46735.535741	34.207079
944.673523	46793.886175	34.212096
945.656379	46850.503401	34.217114
946.631069	46906.723497	34.222132
947.511503	46961.294698	34.227149
948.707631	47016.809818	34.232167
949.372632	47069.985285	34.237184
950.567312	47111.678029	34.242202
951.253980	47171.758614	34.247220
952.188835	47223.993861	34.252237
953.512907	47273.954082	34.257255
954.439671	47328.227905	34.262272
955.786701	47369.650546	34.267290
956.322639	47413.123466	34.272308
957.100705	47457.874440	34.277325
957.743086	47503.545091	34.282343
958.373902	47553.032450	34.287360
959.226080	47620.009368	34.292378
960.233369	47667.837453	34.297396
961.333992	47720.478087	34.302413
962.491088	47770.085963	34.307431
963.004667	47830.410494	34.312448
964.175564	47876.049755	34.317466
964.725671	47941.891870	34.322484
965.731345	48000.735324	34.327501
966.937305	48058.712471	34.332519
967.634746	48122.267145	34.337536
968.772569	48181.735684	34.342554
969.936947	48245.635146	34.347572
970.552290	48300.820470	34.352589
971.940526	48363.957656	34.357607
973.026386	48426.509700	34.362624
973.900207	48488.544699	34.367642
974.959547	48553.929252	34.372660
975.838043	48609.637194	34.377677
977.325219	48662.162546	34.382695
978.360847	48715.758338	34.387712
979.410840	48769.402622	34.392730
980.730181	48818.468594	34.397748
981.709106	48878.172614	34.402765
982.902769	48934.325489	34.407783
983.506983	48983.516439	34.412800
984.562343	49031.207005	34.417818
985.747315	49082.452019	34.422836
986.632942	49128.290302	34.427853
987.732195	49183.977736	34.432871
989.012583	49233.778287	34.437888
989.772156	49275.853152	34.442906
990.539700	49329.043153	34.447924
991.487245	49379.902109	34.452941
992.387232	49437.006945	34.457959
993.226653	49486.440534	34.462976
994.224050	49544.966598	34.467994
995.281849	49608.937181	34.473012
996.468178	49673.058646	34.478029
997.048849	49725.627149	34.483047
998.138134	49788.916317	34.488064
999.410785	49843.597522	34.493082
1000.232421	49900.753743	34.498100
1001.178643	49968.096122	34.503117
1002.251028	50024.871731	34.508135
1003.076103	50087.197087	34.513152
1004.557275	50146.142451	34.518170
1005.750296	50206.012551	34.523188
1006.277903	50268.150868	34.528205
1007.447665	50307.575607	34.533223
1008.260201	50373.124214	34.538240
1009.130209	50439.676356	34.543258
1010.376711	50500.424653	34.548276
1011.522493	50558.657997	34.553293
1012.837190	50613.163616	34.558311
1013.619941	50677.781324	34.563328
1014.714535	50723.343314	34.568346
1015.648333	50784.761391	34.573364
1016.475044	50845.221997	34.578381
1017.708216	50887.636936	34.583399
1018.548866	50946.001287	34.588416
1019.662544	51003.696633	34.593434
1020.792614	51069.418958	34.598452
1021.449167	51134.848620	34.603469
1022.613362	51183.444085	34.608487
1023.590960	51239.364349	34.613504
1024.715249	51284.486209	34.618522
1025.392850	51323.736649	34.623540
1026.296671	51382.085882	34.628557
1027.421254	51426.651159	34.633575
1028.261635	51487.788340	34.638592
1029.192064	51535.465698	34.643610
1030.174381	51595.328100	34.648628
1030.659994	51654.414211	34.653645
1032.342234	51705.897265	34.658663
1033.247217	51762.418621	34.663680
1034.607414	51830.581142	34.668698
1035.567378	51893.548315	34.673716
1036.898049	51939.195964	34.678733
1038.095254	52001.841546	34.683751
1038.887997	52059.570787	34.688768
1040.053624	52111.958218	34.693786
1040.908520	52163.932500	34.698804
1041.741623	52222.997288	34.703821
1042.947213	52284.395769	34.708839
1043.966626	52356.106065	34.713856
1045.066398	52412.275791	34.718874
1046.274959	52463.910624	34.723892
1047.034786	52533.852379	34.728909
1048.271332	52591.817187	34.733927
1049.590671	52651.718132	34.738944
1050.418597	52713.480606	34.743962
1051.721926	52771.498683	34.748980
1052.590603	52835.102818	34.753997
1053.896505	52893.158762	34.759015
1054.995574	52951.709166	34.764032
1055.589604	53014.863218	34.769050
1057.046720	53080.210976	34.774068
1058.207889	53143.884060	34.779085
1059.372338	53198.001637	34.784103
1060.186113	53255.939366	34.789120
1061.286069	53326.962942	34.794138
1062.725283	53384.391750	34.799156
1063.445524	53447.736032	34.804173
1063.979410	53502.370683	34.809191
1065.397265	53561.752296	34.814208
1066.635618	53624.503368	34.819226
1067.868810	53684.274901	34.824244
1069.005770	53750.965579	34.829261
1070.433766	53811.187871	34.834279
1071.266217	53869.238096	34.839296
1072.518384	53923.337287	34.844314
1073.808680	53979.373370	34.849332
1074.697532	54031.181954	34.854349
1075.771630	54085.360023	34.859367
1076.932567	54135.120210	34.864384
1077.904210	54192.339434	34.869402
1079.174173	54237.994759	34.874420
1080.248003	54303.070539	34.879437
1081.028358	54356.719354	34.884455
1082.050970	54412.564234	34.889472
1083.129011	54472.684805	34.894490
1084.461865	54525.367874	34.899508
1085.446770	54585.351435	34.904525
1086.702921	54635.104101	34.909543
1087.805171	54691.108038	34.914560
1088.620901	54749.675644	34.919578
1089.993242	54797.777752	34.924596
1090.828388	54860.063664	34.929613
1091.916919	54916.057625	34.934631
1093.214350	54969.253503	34.939648
1094.236975	55037.661736	34.944666
1095.297806	55073.485423	34.949684
1095.999513	55129.040504	34.954701
1097.110184	55181.196593	34.959719
1098.186772	55229.788876	34.964736
1098.886873	55283.851053	34.969754
1099.951938	55330.160764	34.974772
1100.572367	55400.949242	34.979789
1102.024705	55455.058581	34.984807
1103.091555	55511.582614	34.989824
1104.188488	55569.386769	34.994842
1105.433687	55634.844413	34.999860
1105.785767	55692.879397	35.004877
1106.819400	55767.762161	35.009895
1108.207761	55827.907206	35.014912
1109.088449	55895.935102	35.019930
1110.352464	55966.358700	35.024948
1111.774965	56036.466576	35.029965
1112.852619	56097.698851	35.034983
1114.183526	56165.429198	35.040000
1115.027610	56242.703743	35.045018
1116.710627	56297.544665	35.050036
1117.858000	56368.911714	35.055053
1118.899647	56428.327790	35.060071
1120.025773	56497.534105	35.065088
1121.124312	56563.491924	35.070106
1122.447141	56621.712616	35.075124
1123.466085	56694.790544	35.080141
1124.601502	56755.350935	35.085159
1125.965906	56824.995559	35.090176
1127.036380	56884.851281	35.095194
1128.425342	56944.087688	35.100212
1129.633557	57015.940799	35.105229
1130.423291	57073.581512	35.110247
1131.951507	57137.087629	35.115264
1132.847085	57196.610760	35.120282
1134.409183	57263.289059	35.125300
1135.681026	57321.399186	35.130317
1136.752500	57379.793985	35.135335
1138.131456	57437.267378	35.140352
1139.304902	57500.146461	35.145370
1140.357416	57561.266169	35.150388
1141.481632	57618.216589	35.155405
1142.550296	57678.429005	35.160423
1143.633918	57731.082250	35.165440
1144.535033	57799.409828	35.170458
1146.097243	57850.152955	35.175476
1147.220923	57915.547265	35.180493
1148.217649	57967.581713	35.185511
1149.290457	58029.034880	35.190528
1150.382782	58097.016908	35.195546
1151.514768	58151.866072	35.200564
1152.294621	58223.435420	35.205581
1153.717030	58288.764987	35.210599
1155.088107	58344.191098	35.215616
1156.181790	58415.110600	35.220634
1157.284205	58471.585424	35.225652
1158.605228	58544.659661	35.230669
1159.451685	58598.250696	35.235687
1160.960866	58648.718989	35.240704
1161.718079	58722.673202	35.245722
1163.071143	58785.875638	35.250740
1164.622896	58841.932865	35.255757
1165.474563	58907.074963	35.260775
1167.038903	58959.484737	35.265792
1167.986567	59011.003771	35.270810
1169.304157	59081.206591	35.275828
1170.322683	59141.012760	35.280845
1171.437641	59200.500163	35.285863
1172.926969	59242.295044	35.290880
1173.326629	59308.148263	35.295898
1174.591091	59346.294735	35.300916
1176.179026	59396.359829	35.305933
1176.806281	59449.278152	35.310951
1177.880185	59498.544118	35.315968
1179.010211	59558.498430	35.320986
1180.169582	59609.200721	35.326004
1181.089190	59680.429680	35.331021
1181.897343	59733.896300	35.336039
1182.971584	59793.290255	35.341056
1184.698708	59857.373715	35.346074
1186.062564	59921.235708	35.351092
1187.362092	59978.816201	35.356109
1188.647603	60042.095783	35.361127
1189.825795	60103.411119	35.366144
1190.753915	60163.727677	35.371162
1191.933348	60239.348428	35.376180
1193.307712	60308.944574	35.381197
1194.195658	60372.274592	35.386215
1195.425997	60433.380039	35.391232
1196.521409	60500.874589	35.396250
1197.998759	60575.177440	35.401268
1199.353270	60635.567668	35.406285
1200.396151	60710.597255	35.411303
1201.935055	60773.180752	35.416320
1203.109806	60834.232604	35.421338
1204.408665	60894.670163	35.426356
1206.089213	60961.162868	35.431373
1207.169147	61018.470021	35.436391
1208.333435	61070.421586	35.441408
1209.516261	61131.308334	35.446426
1211.249384	61197.622540	35.451444
1212.190030	61261.035224	35.456461
1213.317264	61328.267540	35.461479
1214.794874	61380.816379	35.466496
1215.890892	61442.160593	35.471514
1217.137296	61499.354187	35.476532
1218.514682	61548.652741	35.481549
1219.601188	61623.475723	35.486567
1221.001143	61671.087173	35.491584
1222.363508	61736.296128	35.496602
1223.278212	61798.828036	35.501620
1224.492719	61857.147898	35.506637
1225.729229	61929.080746	35.511655
1226.919732	61979.985645	35.516672
1228.359190	62039.403834	35.521690
1229.189250	62104.481865	35.526708
1230.512751	62151.238967	35.531725
1231.873288	62226.255099	35.536743
1233.092213	62283.157292	35.541760
1234.208492	62348.469693	35.546778
1235.494904	62412.723786	35.551796
1236.903670	62470.027154	35.556813
1237.909615	62533.787388	35.561831
1239.816579	62595.570924	35.566848
1240.623847	62652.595383	35.571866
1242.355049	62709.981770	35.576884
1243.333733	62763.402966	35.581901
1244.431551	62824.053985	35.586919
1245.918075	62885.904064	35.591936
1247.002552	62938.872275	35.596954
1248.255659	62999.828599	35.601972
1249.282638	63056.465085	35.606989
1250.352750	63127.452567	35.612007
1252.074987	63178.434956	35.617024
1253.129402	63243.012395	35.622042
1254.322120	63299.281639	35.627060
1255.567680	63356.080838	35.632077
1256.539112	63407.801629	35.637095
1257.856929	63460.278621	35.642112
1258.557900	63522.810354	35.647130
1259.782420	63569.718574	35.652148
1261.118732	63623.085634	35.657165
1262.294162	63680.922118	35.662183
1263.795209	63742.379556	35.667200
1264.932125	63806.761951	35.672218
1265.824659	63867.175430	35.677236
1267.619485	63923.313845	35.682253
1268.458637	63998.929740	35.687271
1269.788259	64062.358340	35.692288
1271.072383	64117.045094	35.697306
1272.232526	64189.667508	35.702324
1273.625649	64242.672476	35.707341
1274.710897	64321.068028	35.712359
1276.373510	64369.181668	35.717376
1277.784036	64439.898015	35.722394
1278.987981	64520.029255	35.727412
1280.453249	64579.772357	35.732429
1281.541930	64655.680378	35.737447
1282.487464	64715.169624	35.742464
1284.138008	64787.552398	35.747482
1285.497708	64855.112403	35.752500
1286.826748	64917.359371	35.757517
1288.029425	64994.978927	35.762535
1289.250013	65062.592921	35.767552
1290.729723	65124.139397	35.772570
1292.095734	65201.961941	35.777588
1293.382691	65268.907671	35.782605
1294.437106	65333.940010	35.787623
1296.051650	65401.980739	35.792640
1297.791595	65472.110282	35.797658
1298.839062	65547.217061	35.802676
1300.308640	65602.080618	35.807693
1301.328822	65682.326628	35.812711
1302.594992	65748.827374	35.817728
1304.775574	65813.823947	35.822746
1305.705693	65878.997439	35.827764
1307.005415	65925.759012	35.832781
1308.256266	66006.197866	35.837799
1309.638954	66063.386933	35.842816
1310.678361	66136.249125	35.847834
1312.072019	66197.336845	35.852852
1313.772612	66261.732260	35.857869
1314.886174	66332.126859	35.862887
1316.374787	66389.160792	35.867904
1317.718226	66454.429349	35.872922
1319.028330	66519.291752	35.877940
1320.658677	66578.500911	35.882957
1321.798114	66649.696427	35.887975
1323.002983	66710.897247	35.892992
1324.314391	66776.665497	35.898010
1325.368676	66840.574729	35.903028
1327.015440	66907.056927	35.908045
1328.138986	66971.829391	35.913063
1329.446765	67038.903173	35.918080
1330.986983	67100.907190	35.923098
1332.163707	67173.351974	35.928116
1333.485752	67227.431711	35.933133
1334.499490	67307.158345	35.938151
1336.139413	67374.143028	35.943168
1337.255952	67445.293699	35.948186
1338.771505	67511.589072	35.953204
1340.296408	67568.240073	35.958221
1341.536420	67639.390952	35.963239
1342.885669	67711.025130	35.968256
1344.126363	67765.359345	35.973274
1345.043945	67834.053891	35.978292
1346.413357	67872.292005	35.983309
1347.737422	67933.280817	35.988327
1349.017667	67989.014959	35.993344
1350.368944	68040.780759	35.998362
1351.797454	68110.592769	36.003380
1352.991242	68162.066879	36.008397
1354.447233	68236.319839	36.013415
1355.710008	68295.248609	36.018432
1356.956707	68359.676057	36.023450
1358.436606	68427.897929	36.028468
1359.757805	68486.609042	36.033485
1360.449126	68560.159493	36.038503
1362.266576	68631.298718	36.043520
1363.626965	68698.577568	36.048538
1364.687365	68764.884111	36.053556
1366.632764	68841.329042	36.058573
1367.695298	68911.574100	36.063591
1368.659235	68985.868254	36.068608
1370.410593	69058.133434	36.073626
1371.825355	69137.239428	36.078644
1373.550350	69202.486931	36.083661
1374.631322	69285.406857	36.088679
1376.303340	69366.315912	36.093696
1377.868907	69426.548606	36.098714
1379.576867	69503.602554	36.103732
1381.067890	69570.571953	36.108749
1382.658446	69633.391057	36.113767
1383.894524	69693.593632	36.118784
1385.376000	69768.106633	36.123802
1386.973701	69828.322570	36.128820
1388.469078	69890.998894	36.133837
1389.452881	69967.072104	36.138855
1390.746645	70031.167081	36.143872
1392.521701	70103.330158	36.148890
1393.756820	70169.017719	36.153908
1395.484253	70231.500235	36.158925
1396.857966	70288.947101	36.163943
1397.872965	70360.799268	36.168960
1399.638979	70418.045702	36.173978
1401.194951	70495.259367	36.178996
1402.753704	70551.018773	36.184013
1403.785360	70616.296046	36.189031
1405.009001	70683.569798	36.194048
1406.565718	70746.042279	36.199066
1407.686534	70824.515528	36.204084
1409.137154	70887.954821	36.209101
1410.753595	70957.979401	36.214119
1411.684019	71032.607610	36.219136
1413.325829	71094.966288	36.224154
1414.757492	71177.470067	36.229172
1416.642093	71237.093430	36.234189
1417.901991	71311.189589	36.239207
1419.164761	71380.422100	36.244224
1420.967651	71440.464002	36.249242
1422.146161	71512.154424	36.254260
1423.443329	71579.773598	36.259277
1425.039224	71649.815913	36.264295
1426.465907	71723.519839	36.269312
1428.271892	71776.216159	36.274330
1429.121398	71849.326854	36.279348
1430.818646	71898.354823	36.284365
1432.335707	71963.090857	36.289383
1433.920396	72034.174515	36.294400
1435.304724	72094.600068	36.299418
1436.931307	72157.254966	36.304436
1438.371522	72221.712359	36.309453
1439.803090	72287.133846	36.314471
1440.627351	72334.665418	36.319488
1441.979998	72375.059627	36.324506
1443.435716	72430.965825	36.329524
1444.433764	72493.745237	36.334541
1445.821884	72546.736493	36.339559
1446.855780	72613.588930	36.344576
1448.337901	72673.569871	36.349594
1449.880464	72740.938302	36.354612
1450.948826	72808.621778	36.359629
1452.918532	72886.803657	36.364647
1454.225937	72947.699177	36.369664
1456.000692	73019.465032	36.374682
1457.080853	73092.885048	36.379700
1458.493105	73158.476374	36.384717
1459.968739	73234.190752	36.389735
1461.443205	73311.400123	36.394752
1462.866940	73376.470884	36.399770
1464.605974	73456.134483	36.404788
1466.660601	73532.177069	36.409805
1467.943986	73593.521148	36.414823
1469.177806	73666.209391	36.419840
1471.159458	73733.777611	36.424858
1472.637992	73805.173972	36.429876
1473.950034	73872.986684	36.434893
1475.730416	73944.614832	36.439911
1476.862095	74015.939385	36.444928
1478.783130	74076.627453	36.449946
1479.800654	74161.080003	36.454964
1481.472464	74236.462534	36.459981
1483.167864	74308.168294	36.464999
1484.197733	74381.751734	36.470016
1486.292683	74446.428722	36.475034
1487.371371	74522.272228	36.480052
1488.760067	74593.228761	36.485069
1490.495225	74661.306583	36.490087
1491.981567	74749.234283	36.495104
1494.128682	74819.515373	36.500122
1495.456150	74888.189588	36.505140
1496.907175	74957.287978	36.510157
1498.626696	75027.940547	36.515175
1499.863790	75108.244985	36.520192
1501.533634	75168.531511	36.525210
1502.949235	75243.994983	36.530228
1504.308013	75313.450737	36.535245
1505.942825	75377.150637	36.540263
1507.045241	75460.859304	36.545280
1508.885880	75532.684948	36.550298
1510.334342	75615.719245	36.555316
1511.459669	75684.224459	36.560333
1513.545991	75754.251504	36.565351
1514.705473	75834.126902	36.570368
1516.210433	75904.562013	36.575386
1517.894492	75984.482423	36.580404
1519.177733	76064.440471	36.585421
1521.151154	76138.286390	36.590439
1522.572746	76217.982556	36.595456
1524.143980	76274.385428	36.600474
1525.694923	76352.883675	36.605492
1526.771771	76422.513085	36.610509
1528.715291	76499.480880	36.615527
1530.295859	76582.522806	36.620544
1531.738503	76655.553814	36.625562
1533.054212	76723.284470	36.630580
1534.631237	76804.870851	36.635597
1536.502865	76864.318853	36.640615
1537.784556	76943.747692	36.645632
1539.438591	77007.448429	36.650650
1540.752432	77081.172133	36.655668
1541.982999	77156.555893	36.660685
1543.530234	77219.070395	36.665703
1544.600534	77273.577560	36.670720
1546.229091	77349.165587	36.675738
1547.698449	77420.674315	36.680756
1548.838758	77482.036984	36.685773
1550.655481	77555.543916	36.690791
1551.913231	77638.259548	36.695808
1553.770557	77706.832651	36.700826
1555.201738	77787.203325	36.705844
1556.647174	77861.478608	36.710861
1558.341414	77932.928144	36.715879
1559.545035	78016.350143	36.720896
1561.558178	78101.989328	36.725914
1563.416567	78189.287218	36.730932
1564.750042	78267.558982	36.735949
1566.536562	78344.493222	36.740967
1567.928203	78431.358197	36.745984
1569.481346	78506.581172	36.751002
1571.283097	78572.517430	36.756020
1572.827829	78665.478075	36.761037
1574.719233	78748.110548	36.766055
1576.096795	78833.534777	36.771072
1578.099867	78902.189410	36.776090
1579.759823	78980.564129	36.781108
1581.028672	79066.867568	36.786125
1582.727011	79133.556143	36.791143
1584.567756	79225.965598	36.796160
1585.751790	79306.252706	36.801178
1587.703331	79383.848142	36.806196
1589.439760	79467.064456	36.811213
1591.089513	79548.381573	36.816231
1592.176898	79625.226108	36.821248
1594.272050	79703.420745	36.826266
1595.747966	79786.222706	36.831284
1597.464463	79866.808176	36.836301
1599.213001	79942.777299	36.841319
1600.952750	80013.959061	36.846336
1601.885639	80094.110389	36.851354
1604.201956	80175.958484	36.856372
1605.624775	80256.565709	36.861389
1607.513434	80329.384650	36.866407
1609.044603	80410.418789	36.871424
1610.493923	80483.750321	36.876442
1612.444630	80564.364505	36.881460
1613.715838	80654.131260	36.886477
1615.437262	80714.840045	36.891495
1616.981738	80804.703881	36.896512
1618.449867	80882.746581	36.901530
1620.459928	80960.679345	36.906548
1622.165800	81044.855384	36.911565
1623.792025	81111.319276	36.916583
1625.406170	81186.894729	36.921600
1627.043305	81264.760009	36.926618
1628.989791	81338.636793	36.931636
1630.722097	81416.183525	36.936653
1632.469091	81478.600393	36.941671
1634.105753	81550.638421	36.946688
1635.217285	81619.730716	36.951706
1637.156826	81696.891034	36.956724
1638.677809	81764.728631	36.961741
1640.378864	81829.991542	36.966759
1641.817681	81906.267883	36.971776
1643.436167	81988.103807	36.976794
1645.413560	82059.937775	36.981812
1646.603187	82138.394989	36.986829
1648.367857	82203.218026	36.991847
1649.760278	82272.888801	36.996864
1651.442003	82341.247449	37.001882
1652.780597	82395.405941	37.006900
1654.350663	82455.787422	37.011917
1655.800143	82528.604795	37.016935
1657.273591	82597.452791	37.021952
1658.639925	82669.016506	37.026970
1660.327067	82747.803001	37.031988
1661.837304	82829.734329	37.037005
1663.608028	82903.401992	37.042023
1665.276754	82979.467864	37.047040
1666.579052	83060.304727	37.052058
1668.341810	83146.543444	37.057076
1669.755827	83232.760979	37.062093
1671.585989	83317.380498	37.067111
1673.706856	83412.180021	37.072128
1674.984656	83494.301692	37.077146
1677.035786	83583.018078	37.082164
1678.254974	83669.520842	37.087181
1680.082705	83762.606166	37.092199
1681.815794	83851.119744	37.097216
1683.491221	83946.839708	37.102234
1685.049536	84035.520590	37.107252
1686.845614	84132.578088	37.112269
1688.754499	84217.770826	37.117287
1690.491714	84315.421025	37.122304
1692.403436	84409.230234	37.127322
1694.369537	84500.750429	37.132340
1696.032388	84589.087215	37.137357
1697.921608	84676.299118	37.142375
1699.781492	84761.463130	37.147392
1701.516775	84854.553802	37.152410
1703.308647	84940.071113	37.157428
1705.254975	85033.002621	37.162445
1706.982249	85106.872845	37.167463
1708.702282	85195.684061	37.172480
1710.000139	85279.087526	37.177498
1711.821653	85359.773598	37.182516
1713.235469	85455.640906	37.187533
1715.262556	85548.422050	37.192551
1717.384668	85636.069265	37.197568
1718.934896	85725.086088	37.202586
1720.792276	85807.465808	37.207604
1722.324842	85893.938893	37.212621
1724.146050	85979.771489	37.217639
1726.069753	86076.562132	37.222656
1727.797043	86155.072937	37.227674
1729.582839	86240.721770	37.232692
1731.400083	86328.583529	37.237709
1733.350931	86408.720063	37.242727
1734.728847	86500.414682	37.247744
1736.461392	86585.806752	37.252762
1738.505010	86665.397249	37.257780
1740.021219	86756.412081	37.262797
1741.722801	86836.588804	37.267815
1743.544896	86918.419621	37.272832
1745.024608	87011.392483	37.277850
1746.682413	87096.886454	37.282868
1748.469937	87180.282109	37.287885
1750.282246	87272.329360	37.292903
1751.940945	87363.881371	37.297920
1753.503107	87451.989193	37.302938
1755.500588	87541.017610	37.307956
1757.262134	87640.753498	37.312973
1758.973492	87717.192706	37.317991
1760.476438	87808.757807	37.323008
1762.441407	87912.087149	37.328026
1764.616922	87990.925602	37.333044
1766.122367	88065.940583	37.338061
1767.581211	88146.247588	37.343079
1769.178328	88214.696787	37.348096
1770.943453	88295.881383	37.353114
1772.693199	88365.181472	37.358132
1774.206233	88453.160582	37.363149
1775.943804	88525.314353	37.368167
1777.665700	88602.983488	37.373184
1779.021069	88690.392349	37.378202
1780.765132	88774.648422	37.383220
1782.380473	88866.351295	37.388237
1783.975269	88966.409244	37.393255
1786.090193	89053.953777	37.398272
1787.695091	89145.937958	37.403290
1789.647864	89247.474290	37.408308
1791.774695	89348.400761	37.413325
1793.185597	89451.251895	37.418343
1795.252338	89543.963453	37.423360
1796.913033	89647.371822	37.428378
1798.865373	89735.298662	37.433396
1800.624737	89838.882356	37.438413
1802.262598	89936.744318	37.443431
1804.591107	90035.537754	37.448448
1806.208758	90144.999872	37.453466
1808.379058	90237.811446	37.458484
1810.288206	90339.054157	37.463501
1811.871242	90438.079645	37.468519
1813.854009	90538.741192	37.473536
1815.467116	90635.886909	37.478554
1817.989035	90731.471251	37.483572
1819.705132	90838.284333	37.488589
1821.239321	90937.712004	37.493607
1823.141833	91021.430000	37.498624
1825.026287	91131.386272	37.503642
1827.111897	91234.885714	37.508660
1829.123757	91331.565708	37.513677
1830.719012	91435.776279	37.518695
1832.907708	91522.948951	37.523712
1834.559128	91623.982836	37.528730
1836.379065	91724.344299	37.533748
1838.044623	91821.739116	37.538765
1839.870178	91919.983740	37.543783
1841.962913	92022.483491	37.548800
1843.940894	92122.973637	37.553818
1845.774774	92223.651434	37.558836
1847.570835	92324.538275	37.563853
1849.343356	92420.359309	37.568871
1851.400282	92524.818243	37.573888
1852.802851	92630.102388	37.578906
1854.764701	92723.828783	37.583924
1856.644707	92825.173110	37.588941
1858.469390	92934.131294	37.593959
1861.044363	93023.022301	37.598976
1862.943094	93126.709539	37.603994
1864.752198	93228.129673	37.609012
1866.647307	93318.864389	37.614029
1868.356228	93412.417004	37.619047
1870.349999	93501.691876	37.624064
1872.450399	93605.894205	37.629082
1873.878066	93684.573130	37.634100
1876.069647	93797.545676	37.639117
1877.977341	93906.887259	37.644135
1879.622134	93980.526272	37.649152
1881.365254	94076.635950	37.654170
1883.241899	94170.975844	37.659188
1885.360743	94265.303478	37.664205
1886.968635	94369.737568	37.669223
1889.032603	94460.030944	37.674240
1890.380365	94549.524026	37.679258
1892.036856	94637.929667	37.684276
1893.798007	94721.920782	37.689293
1895.692924	94818.338579	37.694311
1897.540435	94902.202590	37.699328
1898.741232	94995.028282	37.704346
1900.618779	95082.285147	37.709364
1903.040949	95182.398917	37.714381
1904.423105	95280.939175	37.719399
1905.990710	95386.460431	37.724416
1907.495265	95498.621366	37.729434
1909.752120	95597.824331	37.734452
1911.658292	95713.016103	37.739469
1913.543416	95834.105915	37.744487
1915.395473	95952.780252	37.749504
1917.164499	96064.572258	37.754522
1918.918235	96184.543140	37.759540
1920.937761	96302.698230	37.764557
1922.638570	96426.354402	37.769575
1925.020398	96543.414258	37.774592
1927.162911	96678.436281	37.779610
1928.914888	96808.145219	37.784628
1931.130366	96925.448026	37.789645
1932.678692	97047.951595	37.794663
1934.662252	97171.452360	37.799680
1936.805609	97302.407768	37.804698
1938.935538	97432.655929	37.809716
1941.283658	97546.771139	37.814733
1943.351501	97668.409866	37.819751
1945.348680	97787.752951	37.824768
1947.446953	97912.468301	37.829786
1949.068362	98032.733127	37.834804
1951.509117	98152.084232	37.839821
1953.379182	98275.150689	37.844839
1955.322295	98388.926638	37.849856
1957.552520	98517.883180	37.854874
1959.359411	98645.740193	37.859892
1961.536570	98764.424922	37.864909
1962.964181	98875.570361	37.869927
1965.200102	99005.390027	37.874944
1967.020017	99125.463103	37.879962
1969.047318	99262.707305	37.884980
1970.784750	99387.738425	37.889997
1972.987873	99516.880713	37.895015
1974.875985	99641.369467	37.900032
1976.587978	99770.348749	37.905050
1978.229471	99906.160114	37.910068
1980.741041	100043.826295	37.915085
1982.956972	100182.528181	37.920103
1985.005770	100303.431914	37.925120
1986.837187	100434.525018	37.930138
1988.681744	100573.033130	37.935156
1990.704008	100703.539633	37.940173
1993.215225	100838.775092	37.945191
1994.925382	100965.705592	37.950208
1996.672426	101101.315273	37.955226
1998.462723	101232.874437	37.960244
2000.711366	101370.853626	37.965261
2002.463192	101511.243923	37.970279
2004.540834	101643.482436	37.975296
2006.665513	101782.243452	37.980314
2008.542540	101919.192764	37.985332
2010.507399	102048.826138	37.990349
2012.655420	102182.463115	37.995367
2014.254094	102315.616059	38.000384
2016.710711	102463.545293	38.005402
2018.674199	102595.222284	38.010420
2020.422015	102727.554800	38.015437
2022.423063	102876.977181	38.020455
2024.180461	102982.443003	38.025472
2025.984567	103117.532243	38.030490
2027.847774	103244.079906	38.035508
2029.474203	103358.227084	38.040525
2031.267533	103501.155139	38.045543
2033.418538	103633.593011	38.050560
2035.220234	103769.788353	38.055578
2036.919534	103914.419209	38.060596
2039.142121	104064.813915	38.065613
2041.134437	104210.503294	38.070631
2043.113221	104359.986532	38.075648
2045.246278	104517.358212	38.080666
2047.141252	104671.382480	38.085684
2049.508383	104819.539061	38.090701
2051.164852	104982.743967	38.095719
2053.599647	105139.412011	38.100736
2055.329984	105294.377818	38.105754
2057.390063	105453.362925	38.110772
2059.507360	105615.370291	38.115789
2061.307601	105776.109337	38.120807
2063.419079	105945.524207	38.125824
2065.636946	106114.162479	38.130842
2067.759956	106284.781830	38.135860
2069.984151	106443.023133	38.140877
2072.059215	106622.426285	38.145895
2074.085980	106786.659736	38.150912
2076.547918	106961.705549	38.155930
2078.481470	107132.434857	38.160948
2080.953150	107295.447224	38.165965
2082.935269	107469.721117	38.170983
2085.194483	107643.318511	38.176000
2087.537913	107800.938761	38.181018
2089.264725	107975.648255	38.186036
2091.925877	108145.964408	38.191053
2093.949144	108310.269080	38.196071
2095.609591	108480.096729	38.201088
2098.022310	108644.887326	38.206106
2099.962957	108826.897198	38.211124
2102.265171	108993.038233	38.216141
2104.579615	109165.429912	38.221159
2106.538660	109331.930598	38.226176
2109.069283	109506.002086	38.231194
2111.115799	109675.546888	38.236212
2113.534752	109832.568509	38.241229
2115.573629	110009.712225	38.246247
2117.710781	110170.406318	38.251264
2119.880209	110327.913042	38.256282
2121.631616	110505.395900	38.261300
2124.123408	110665.542182	38.266317
2125.964223	110837.014315	38.271335
2128.150764	111008.839001	38.276352
2130.446665	111180.064046	38.281370
2132.126744	111356.598507	38.286388
2134.463367	111525.498064	38.291405
2136.118611	111704.270149	38.296423
2138.383401	111882.630709	38.301440
2140.672058	112060.379683	38.306458
2142.571756	112231.861994	38.311476
2145.024623	112409.498231	38.316493
2146.853736	112589.655255	38.321511
2149.184375	112763.533042	38.326528
2151.096681	112944.947060	38.331546
2152.950557	113123.631715	38.336564
2155.410076	113286.064945	38.341581
2157.735196	113477.233326	38.346599
2160.104767	113653.836062	38.351616
2162.063065	113835.906842	38.356634
2164.399925	114011.958394	38.361652
2166.274486	114157.733084	38.366669
2168.464431	114312.857034	38.371687
2170.240063	114480.780142	38.376704
2172.448590	114631.653749	38.381722
2174.252252	114791.964097	38.386740
2176.496508	114963.468816	38.391757
2178.797884	115126.607188	38.396775
2180.655186	115293.785609	38.401792
2183.156408	115464.212432	38.406810
2185.146393	115632.614592	38.411828
2187.206574	115807.957039	38.416845
2189.207350	115986.391692	38.421863
2191.161537	116157.833185	38.426880
2193.528271	116346.967943	38.431898
2195.188542	116536.138087	38.436916
2197.487411	116732.806825	38.441933
2199.555316	116927.521378	38.446951
2201.412141	117127.584499	38.451968
2203.914626	117326.685165	38.456986
2205.777333	117536.668369	38.462004
2207.987919	117733.039058	38.467021
2210.202796	117941.612223	38.472039
2212.541734	118169.523215	38.477056
2214.608353	118371.018788	38.482074
2216.773343	118589.661949	38.487092
2219.043260	118799.816762	38.492109
2221.420818	119019.393147	38.497127
2223.223655	119244.908290	38.502144
2225.552484	119463.974782	38.507162
2227.937156	119694.107535	38.512180
2230.397987	119920.170620	38.517197
2232.797634	120132.570331	38.522215
2235.013539	120369.037888	38.527232
2237.446711	120583.198034	38.532250
2239.465343	120805.162108	38.537268
2241.689824	121034.135499	38.542285
2244.385094	121267.374926	38.547303
2246.406805	121498.881755	38.552320
2248.938474	121714.225125	38.557338
2251.090003	121943.709984	38.562356
2253.681296	122160.479928	38.567373
2256.101661	122378.254597	38.572391
2258.076484	122622.118442	38.577408
2260.418003	122836.520900	38.582426
2262.123710	123072.526412	38.587444
2264.839328	123299.342986	38.592461
2267.285098	123531.404305	38.597479
2269.605754	123766.150610	38.602496
2271.940941	123988.742742	38.607514
2274.048958	124217.613241	38.612532
2276.295571	124445.473832	38.617549
2278.707027	124661.752700	38.622567
2281.197736	124899.790145	38.627584
2283.499672	125120.021375	38.632602
2285.701238	125357.814956	38.637620
2287.919400	125585.369250	38.642637
2290.257205	125813.540430	38.647655
2292.129379	126055.969498	38.652672
2295.327666	126279.010084	38.657690
2297.569044	126503.571768	38.662708
2299.316200	126720.447586	38.667725
2302.165662	126948.139046	38.672743
2304.028695	127177.965265	38.677760
2306.302604	127397.743693	38.682778
2308.682041	127641.206500	38.687796
2310.824600	127872.248864	38.692813
2313.026870	128102.775672	38.697831
2315.215517	128332.937946	38.702848
2317.405977	128540.073390	38.707866
2319.286950	128752.904235	38.712884
2321.557837	128978.654597	38.717901
2323.770580	129188.048140	38.722919
2325.864143	129404.173185	38.727936
2327.968326	129621.579139	38.732954
2329.712237	129858.036332	38.737972
2332.039520	130086.651231	38.742989
2334.644658	130331.489937	38.748007
2336.756051	130569.682591	38.753024
2339.234399	130811.460665	38.758042
2341.658631	131059.516554	38.763060
2343.847510	131305.428298	38.768077
2346.746977	131544.213597	38.773095
2348.806448	131787.521826	38.778112
2351.108922	132038.114680	38.783130
2353.561490	132291.185148	38.788148
2355.777263	132551.450538	38.793165
2358.167098	132805.168224	38.798183
2360.570116	133064.138484	38.803200
2363.173316	133309.730229	38.808218
2365.135886	133575.560950	38.813236
2367.362882	133845.209367	38.818253
2369.682755	134096.471039	38.823271
2371.961616	134377.065274	38.828288
2374.365879	134638.645802	38.833306
2376.414213	134923.847660	38.838324
2378.957557	135203.542808	38.843341
2381.168529	135480.918745	38.848359
2383.735362	135774.724487	38.853376
2386.130274	136046.656650	38.858394
2388.338401	136329.456697	38.863412
2391.215771	136619.386999	38.868429
2393.701931	136907.908304	38.873447
2396.416591	137210.798806	38.878464
2398.646531	137492.587395	38.883482
2401.378207	137771.532757	38.888500
2403.882809	138053.269092	38.893517
2406.137165	138340.020872	38.898535
2408.309968	138628.639959	38.903552
2410.816873	138912.005470	38.908570
2413.482574	139211.249078	38.913588
2415.701954	139498.990561	38.918605
2418.104686	139790.245809	38.923623
2420.425739	140079.294731	38.928640
2422.884616	140373.844358	38.933658
2425.604051	140667.580889	38.938676
2427.641553	140966.476905	38.943693
2430.392756	141262.547237	38.948711
2432.697840	141553.130440	38.953728
2435.098785	141846.225938	38.958746
2438.076499	142129.321067	38.963764
2440.188839	142425.422258	38.968781
2442.739092	142724.566136	38.973799
2444.911996	143024.633881	38.978816
2447.481859	143326.202417	38.983834
2450.084690	143613.806775	38.988852
2452.467440	143913.022101	38.993869
2455.142117	144203.258501	38.998887
2457.428951	144506.287228	39.003904
2460.074668	144790.134824	39.008922
2462.525985	145092.608277	39.013940
2464.665888	145395.982618	39.018957
2466.950187	145688.306653	39.023975
2469.112787	145997.430582	39.028992
2471.427527	146300.782937	39.034010
2474.136963	146598.160664	39.039028
2476.174272	146906.713099	39.044045
2478.782894	147198.220717	39.049063
2481.400650	147474.560832	39.054080
2483.939860	147752.767828	39.059098
2486.424651	148031.733684	39.064116
2488.262707	148324.637379	39.069133
2490.980918	148604.940577	39.074151
2493.087718	148907.248977	39.079168
2495.347918	149194.811155	39.084186
2497.719056	149499.785178	39.089204
2499.651751	149813.016625	39.094221
2502.063066	150130.757292	39.099239
2504.132459	150454.049524	39.104256
2506.692512	150771.643739	39.109274
2508.929691	151101.247576	39.114292
2511.022785	151441.754320	39.119309
2513.534675	151782.743483	39.124327
2515.826422	152140.093318	39.129344
2518.008211	152482.483945	39.134362
2520.670374	152849.770409	39.139380
2523.090452	153209.798102	39.144397
2525.399622	153574.072556	39.149415
2527.913247	153953.080647	39.154432
2530.606793	154321.920424	39.159450
2533.318468	154691.356365	39.164468
2535.719267	155069.932479	39.169485
2538.386526	155444.838763	39.174503
2540.769439	155825.136339	39.179520
2543.865231	156209.831465	39.184538
2546.500606	156586.857341	39.189556
2549.129644	156966.679459	39.194573
2551.767579	157343.493917	39.199591
2554.410604	157730.973709	39.204608
2557.441198	158098.514939	39.209626
2560.281749	158486.628815	39.214644
2562.776724	158867.956504	39.219661
2565.633562	159234.909693	39.224679
2568.745500	159613.657225	39.229696
2571.314167	159975.492875	39.234714
2573.931971	160351.643455	39.239732
2576.392090	160723.415590	39.244749
2579.108288	161098.539596	39.249767
2581.449372	161475.679632	39.254784
2584.145241	161851.788823	39.259802
2586.618380	162233.280015	39.264820
2588.971452	162610.869191	39.269837
2591.651744	162997.575900	39.274855
2594.272285	163381.805806	39.279872
2597.021856	163772.505512	39.284890
2599.393667	164153.998351	39.289908
2601.803560	164544.222480	39.294925
2604.551336	164936.567108	39.299943
2606.913980	165320.137517	39.304960
2609.122828	165722.220299	39.309978
2611.938930	166112.313735	39.314996
2614.151199	166530.182594	39.320013
2616.660192	166932.961895	39.325031
2618.923958	167338.854507	39.330048
2621.412257	167752.853055	39.335066
2624.166263	168157.556362	39.340084
2626.571287	168590.199275	39.345101
2628.995348	169002.145490	39.350119
2631.452908	169426.811401	39.355136
2634.377510	169850.797260	39.360154
2637.188610	170265.508858	39.365172
2639.437151	170691.966995	39.370189
2641.945496	171117.510801	39.375207
2644.408044	171552.460370	39.380224
2647.301567	171980.996203	39.385242
2649.963621	172381.610299	39.390260
2652.478782	172783.417645	39.395277
2654.716158	173187.556127	39.400295
2657.261817	173597.768861	39.405312
2659.658388	174011.816435	39.410330
2662.227576	174426.194708	39.415348
2664.657986	174850.628324	39.420365
2666.558089	175279.286711	39.425383
2669.699755	175711.016602	39.430400
2671.427363	176160.899926	39.435418
2674.021714	176607.551716	39.440436
2676.455178	177071.221556	39.445453
2678.976414	177535.210368	39.450471
2681.451124	178010.917062	39.455488
2683.407581	178489.170971	39.460506
2686.498561	178970.018374	39.465524
2689.005836	179463.074337	39.470541
2691.369324	179959.711197	39.475559
2694.444016	180458.677751	39.480576
2696.733021	180956.322240	39.485594
2699.942799	181450.320461	39.490612
2702.593065	181965.235389	39.495629
2705.812927	182475.644720	39.500647
2708.553123	182985.827022	39.505664
2711.230632	183510.600663	39.510682
2714.868222	184053.742693	39.515700
2717.957533	184558.900434	39.520717
2721.006119	185048.599057	39.525735
2724.121200	185537.934054	39.530752
2727.086211	186034.736852	39.535770
2729.582292	186517.518681	39.540788
2732.544683	187019.736641	39.545805
2734.708116	187506.156334	39.550823
2738.100242	188006.660718	39.555840
2740.518378	188517.428883	39.560858
2743.478609	189003.527401	39.565876
2745.921252	189507.006450	39.570893
2748.620756	190019.210625	39.575911
2751.686584	190530.013553	39.580928
2754.518580	191044.233533	39.585946
2756.943406	191549.857820	39.590964
2759.434554	192069.317208	39.595981
2762.398557	192577.071281	39.600999
2765.612714	193083.645254	39.606016
2767.646220	193608.923216	39.611034
2770.545468	194123.424861	39.616052
2773.416173	194649.185712	39.621069
2776.054530	195178.795167	39.626087
2778.818658	195701.274631	39.631104
2781.053236	196239.740215	39.636122
2783.837070	196766.284824	39.641140
2786.551388	197297.643154	39.646157
2788.649845	197850.335604	39.651175
2791.945697	198375.535847	39.656192
2794.730520	198923.831983	39.661210
2797.532383	199471.060507	39.666228
2800.256304	200015.686695	39.671245
2802.926688	200567.816737	39.676263
2805.883291	201122.977535	39.681280
2808.160178	201682.361642	39.686298
2810.976815	202238.589444	39.691316
2813.650039	202794.892224	39.696333
2816.362659	203366.940157	39.701351
2819.025303	203928.963603	39.706368
2822.054632	204512.523689	39.711386
2824.896438	205076.046600	39.716404
2827.276649	205648.534284	39.721421
2830.357074	206202.979540	39.726439
2833.537604	206747.986052	39.731456
2836.002471	207288.330056	39.736474
2838.931480	207818.289078	39.741492
2841.702047	208365.345031	39.746509
2844.497689	208911.737815	39.751527
2848.059272	209437.917985	39.756544
2850.548125	209980.093292	39.761562
2853.706535	210516.296795	39.766580
2856.765450	211058.308886	39.771597
2859.828847	211598.390631	39.776615
2862.357877	212141.148085	39.781632
2864.605251	212701.199577	39.786650
2867.502944	213246.162179	39.791668
2869.960399	213818.732095	39.796685
2872.374157	214382.545479	39.801703
2875.245187	214955.077896	39.806720
2877.940107	215540.111945	39.811738
2880.770963	216119.485899	39.816756
2883.820811	216700.477606	39.821773
2886.958029	217294.082091	39.826791
2889.863542	217883.938315	39.831808
2892.342154	218493.702412	39.836826
2895.616916	219088.201847	39.841844
2898.063776	219700.944338	39.846861
2900.812220	220313.995830	39.851879
2903.690606	220917.805792	39.856896
2906.046578	221552.157292	39.861914
2909.122927	222180.705988	39.866932
2911.890277	222809.176284	39.871949
2914.750338	223446.523745	39.876967
2917.475025	224084.197406	39.881984
2920.031411	224738.613392	39.887002
2923.300475	225385.398368	39.892020
2926.037291	226048.499778	39.897037
2928.779048	226712.210028	39.902055
2932.473172	227365.025259	39.907072
2935.164944	228032.655169	39.912090
2938.035218	228704.956610	39.917108
2940.912854	229361.760055	39.922125
2943.678761	230034.864513	39.927143
2947.043080	230707.925667	39.932160
2949.610207	231389.417982	39.937178
2953.087212	232054.127726	39.942196
2955.992424	232742.119926	39.947213
2958.894208	233419.721607	39.952231
2962.016294	234108.643437	39.957248
2964.792754	234789.057205	39.962266
2967.830959	235462.087272	39.967284
2971.533872	236136.206233	39.972301
2974.100316	236823.254349	39.977319
2977.648176	237504.177801	39.982336
2980.630959	238181.809555	39.987354
2983.542699	238868.926475	39.992372
2986.631613	239535.716755	39.997389
2989.576172	240228.515724	40.002407
2992.867311	240897.862272	40.007424
2996.014433	241577.797380	40.012442
2998.721614	242262.524432	40.017460
3001.918313	242930.254505	40.022477
3004.791659	243620.260873	40.027495
3008.104738	244299.196854	40.032512
3010.823530	244985.361827	40.037530
3013.610302	245660.565291	40.042548
3016.567766	246339.728009	40.047565
3019.447514	247045.166801	40.052583
3022.236049	247732.733829	40.057600
3024.525708	248425.710776	40.062618
3028.266655	249110.227699	40.067636
3031.372112	249774.976727	40.072653
3034.242840	250438.210277	40.077671
3037.439557	251081.144734	40.082688
3040.105493	251749.866307	40.087706
3043.058231	252412.469101	40.092724
3046.222292	253078.515960	40.097741
3048.676371	253753.027933	40.102759
3052.017781	254422.038270	40.107776
3054.345885	255107.460709	40.112794
3057.203096	255785.456031	40.117812
3060.656878	256460.839923	40.122829
3063.656546	257162.149480	40.127847
3066.832316	257850.625662	40.132864
3069.677842	258550.656192	40.137882
3072.496619	259256.554422	40.142900
3076.139930	259956.960096	40.147917
3078.829663	260668.635995	40.152935
3082.470366	261376.247192	40.157952
3085.366472	262090.167960	40.162970
3088.474291	262807.708581	40.167988
3091.134474	263525.060468	40.173005
3094.108746	264263.439886	40.178023
3097.124941	264999.648609	40.183040
3099.998544	265749.513610	40.188058
3102.853824	266491.857855	40.193076
3106.098600	267238.986763	40.198093
3108.815016	268003.234881	40.203111
3111.805698	268765.808512	40.208128
3114.593882	269545.525855	40.213146
3117.495396	270323.466435	40.218164
3120.846685	271100.263307	40.223181
3123.945549	271891.645541	40.228199
3127.107183	272681.715553	40.233216
3130.324620	273480.074360	40.238234
3132.911524	274281.038496	40.243252
3136.691007	275068.297579	40.248269
3139.464752	275882.905609	40.253287
3142.503182	276700.333753	40.258304
3145.888905	277504.696624	40.263322
3149.417713	278311.212838	40.268340
3152.879909	279115.674011	40.273357
3156.561863	279926.948875	40.278375
3159.842885	280731.167148	40.283392
3163.080147	281532.742471	40.288410
3166.358290	282342.961880	40.293428
3169.855369	283140.821943	40.298445
3172.857080	283952.005777	40.303463
3176.137484	284765.879021	40.308480
3179.550191	285559.229948	40.313498
3182.622033	286371.135987	40.318516
3185.915746	287170.910790	40.323533
3189.115763	287980.212483	40.328551
3192.443059	288787.732190	40.333568
3195.347947	289591.905368	40.338586
3198.462549	290398.726993	40.343604
3202.190555	291202.268491	40.348621
3205.277744	292018.137841	40.353639
3208.519429	292809.064657	40.358656
3211.805789	293614.090723	40.363674
3214.998864	294419.983749	40.368692
3218.606783	295227.324230	40.373709
3221.691081	296029.581535	40.378727
3224.727682	296834.424723	40.383744
3227.597606	297634.052720	40.388762
3230.457143	298457.154368	40.393780
3233.709907	299272.007744	40.398797
3236.759759	300094.192159	40.403815
3239.734712	300904.748962	40.408832
3242.968578	301696.949853	40.413850
3246.185980	302484.851397	40.418868
3249.526721	303265.030197	40.423885
3252.532347	304057.231365	40.428903
3255.882467	304845.812727	40.433920
3259.215054	305638.319210	40.438938
3262.055016	306428.656580	40.443956
3264.890801	307222.231218	40.448973
3268.101867	308039.238975	40.453991
3271.265302	308853.473949	40.459008
3274.275686	309668.176133	40.464026
3277.357369	310496.737105	40.469044
3280.696324	311317.273846	40.474061
3283.590874	312160.708402	40.479079
3286.751604	313007.842436	40.484096
3290.124687	313861.247358	40.489114
3293.377211	314706.584711	40.494132
3297.147447	315558.195496	40.499149
3300.000148	316427.673059	40.504167
3303.044217	317292.408910	40.509184
3306.912721	318166.819964	40.514202
3310.280042	319038.602011	40.519220
3313.905105	319897.181384	40.524237
3317.475948	320767.044305	40.529255
3320.683617	321637.073146	40.534272
3324.072517	322520.961064	40.539290
3327.314777	323395.033471	40.544308
3330.950611	324290.111389	40.549325
3334.190886	325168.409356	40.554343
3337.790322	326053.152978	40.559360
3341.386621	326934.756972	40.564378
3344.592244	327830.610608	40.569396
3347.936645	328723.606179	40.574413
3351.126561	329618.965075	40.579431
3354.020901	330518.180455	40.584448
3357.973974	331415.966324	40.589466
3360.941401	332325.656233	40.594484
3364.369647	333227.997141	40.599501
3367.315952	334144.521342	40.604519
3370.224983	335073.128766	40.609536
3374.027398	335996.601533	40.614554
3377.384124	336927.781101	40.619572
3380.421072	337859.012245	40.624589
3383.889124	338800.703419	40.629607
3386.936479	339739.163763	40.634624
3390.643161	340687.083333	40.639642
3393.495646	341633.107372	40.644660
3397.406101	342576.176038	40.649677
3401.049088	343523.293209	40.654695
3404.537825	344471.372098	40.659712
3408.173568	345417.626528	40.664730
3411.735850	346362.319132	40.669748
3415.109062	347311.528407	40.674765
3418.523312	348257.027468	40.679783
3422.010956	349207.990338	40.684800
3425.506823	350154.816767	40.689818
3428.621956	351106.974346	40.694836
3432.976717	352039.235318	40.699853
3437.148211	352967.035655	40.704871
3440.849705	353899.623366	40.709888
3444.821234	354814.775330	40.714906
3448.505094	355733.393328	40.719924
3452.323692	356642.634244	40.724941
3455.648267	357556.792801	40.729959
3459.302677	358452.165133	40.734976
3462.645520	359361.349280	40.739994
3466.418304	360265.445509	40.745012
3469.533925	361145.764225	40.750016
3472.928909	362005.347457	40.755021
3475.859635	362808.542811	40.760026
3479.460772	363562.037883	40.765031
3482.250899	364270.057146	40.770036
3485.094266	364917.884404	40.775040
3488.099785	365507.386737	40.780045
3490.926419	366051.121304	40.785050
3493.707661	366530.548245	40.790055
3495.818764	366959.818154	40.795060
3498.178291	367350.857533	40.800064
3500.339680	367684.886685	40.805069
3501.837611	367977.122025	40.810074
3503.528274	368231.775281	40.815079
3505.279285	368457.302635	40.820084
3506.802612	368635.178831	40.825088
3508.237665	368765.560806	40.830093
3509.736038	368883.534801	40.835098
3510.695609	368949.208263	40.840103
3511.447476	369007.445102	40.845108
3512.525492	369020.207528	40.850112
3513.624058	369014.548436	40.855117
3514.227142	368993.724062	40.860122
3515.261672	368942.651547	40.865127
3516.122853	368874.711931	40.870132
3516.811346	368778.117179	40.875136
3517.265730	368666.722258	40.880141
3517.402790	368550.016060	40.885146
3518.593162	368401.769422	40.890151
3518.929117	368265.672264	40.895156
3519.215365	368098.206601	40.900160
3519.679710	367908.482265	40.905165
3519.799969	367725.111078	40.910170
3520.631286	367522.496919	40.915175
3520.918419	367313.157574	40.920180
3520.995431	367083.753187	40.925184
3521.275784	366860.946267	40.930189
3521.104446	366632.136038	40.935194
3521.478240	366389.849336	40.940199
3521.547160	366137.394601	40.945204
3521.297715	365882.573733	40.950208
3521.875953	365638.571881	40.955213
3521.789310	365378.131458	40.960218
3521.838174	365113.475191	40.965223
3521.577640	364841.598127	40.970228
3521.606919	364572.518967	40.975232
3521.718231	364301.544258	40.980237
3521.450728	364038.375992	40.985242
3521.827969	363763.035203	40.990247
3521.787691	363494.439785	40.995252
3521.495192	363221.104332	41.000256
3521.715623	362936.785309	41.005261
3521.554036	362660.578288	41.010266
3521.699958	362382.287786	41.015271
3521.421658	362094.506601	41.020276
3521.717562	361831.001874	41.025280
3521.471449	361537.264129	41.030285
3521.287236	361249.637949	41.035290
3520.726217	360962.322028	41.040295
3520.982314	360691.240820	41.045300
3521.098861	360402.822553	41.050304
3521.081144	360131.829934	41.055309
3520.642061	359855.233765	41.060314
3520.440593	359568.991893	41.065319
3520.333053	359299.784750	41.070324
3520.187487	359020.314225	41.075328
3520.276922	358746.014150	41.080333
3519.870255	358478.701685	41.085338
3519.804201	358189.299775	41.090343
3519.772922	357927.997733	41.095348
3519.554969	357657.293924	41.100352
3519.754281	357375.975445	41.105357
3519.314774	357117.678426	41.110362
3519.550824	356847.455646	41.115367
3518.896870	356582.122296	41.120372
3519.055206	356320.853232	41.125376
3518.937608	356055.202782	41.130381
3518.609578	355805.874542	41.135386
3518.625903	355534.810550	41.140391
3518.477830	355277.799710	41.145396
3518.206357	355018.238983	41.150400
3518.345853	354763.263119	41.155405
3517.694369	354521.778146	41.160410
3517.504175	354263.570991	41.165415
3517.405936	354026.342056	41.170420
3517.361199	353778.885137	41.175424
3517.482023	353528.121516	41.180429
3517.242708	353294.925155	41.185434
3517.017295	353059.208520	41.190439
3516.945584	352817.746996	41.195444
3516.635381	352585.090304	41.200448
3516.898084	352347.868668	41.205453
3516.609329	352116.781173	41.210458
3516.495710	351878.928592	41.215463
3515.918610	351653.475026	41.220468
3515.951614	351424.035334	41.225472
3516.163426	351191.820743	41.230477
3515.546476	350977.197415	41.235482
3515.451222	350741.850132	41.240487
3515.550574	350530.543550	41.245492
3515.429686	350311.593109	41.250496
3515.077732	350090.084435	41.255501
3514.710578	349890.260400	41.260506
3515.079475	349677.787643	41.265511
3514.954214	349466.712648	41.270516
3514.560938	349262.465623	41.275520
3514.764659	349046.430225	41.280525
3514.552883	348842.736904	41.285530
3514.449693	348625.882399	41.290535
3514.047620	348426.156597	41.295540
3514.000016	348227.162249	41.300544
3514.013166	348034.817776	41.305549
3513.648878	347837.116274	41.310554
3513.910810	347640.663076	41.315559
3513.520147	347457.352469	41.320564
3513.615566	347259.143480	41.325568
3513.671876	347063.303745	41.330573
3513.443693	346873.252918	41.335578
3513.336356	346683.004157	41.340583
3513.206396	346494.410361	41.345588
3512.898643	346307.444972	41.350592
3513.125074	346128.810201	41.355597
3512.734373	345943.838790	41.360602
3513.050839	345756.010044	41.365607
3512.473595	345577.091216	41.370612
3512.485190	345393.960692	41.375616
3512.491393	345226.847240	41.380621
3512.170111	345065.199532	41.385626
3511.826444	344879.452225	41.390631
3511.881081	344710.498104	41.395636
3511.893512	344536.159717	41.400640
3511.709175	344372.631312	41.405645
3511.267299	344211.557754	41.410650
3511.364718	344044.220844	41.415655
3511.338446	343888.877701	41.420660
3511.176272	343726.359751	41.425664
3510.896108	343562.689912	41.430669
3511.032769	343411.895710	41.435674
3511.036351	343248.281718	41.440679
3510.922667	343102.991812	41.445684
3510.487894	342949.513522	41.450688
3510.626487	342791.368241	41.455693
3510.344192	342650.272650	41.460698
3510.289756	342504.182760	41.465703
3510.114367	342350.661266	41.470708
3510.059948	342217.613847	41.475712
3509.920247	342071.179499	41.480717
3509.444486	341922.966360	41.485722
3509.890774	341783.228090	41.490727
3509.862077	341650.174486	41.495732
3509.777484	341515.578074	41.500736
3509.747521	341383.311886	41.505741
3509.659039	341247.774256	41.510746
3509.703602	341107.689264	41.515751
3509.473624	340978.783784	41.520756
3509.103490	340848.602946	41.525760
3509.655308	340710.522116	41.530765
3509.287150	340580.746820	41.535770
3509.127534	340444.505247	41.540775
3509.006330	340316.877152	41.545780
3509.400861	340196.084341	41.550784
3509.052118	340051.021933	41.555789
3508.914939	339932.676150	41.560794
3508.635003	339804.308185	41.565799
3508.495372	339688.250501	41.570804
3508.542375	339572.926110	41.575808
3508.831595	339443.933871	41.580813
3508.494217	339330.194490	41.585818
3508.366976	339208.539047	41.590823
3508.044407	339085.235438	41.595828
3507.829227	338970.331519	41.600832
3507.816930	338857.658675	41.605837
3507.974488	338756.605345	41.610842
3508.287143	338639.151245	41.615847
3508.497290	338524.459122	41.620852
3507.543712	338418.263885	41.625856
3507.592349	338310.131608	41.630861
3507.192848	338209.926706	41.635866
3507.478012	338101.248239	41.640871
3507.411593	337996.565969	41.645876
3507.423707	337898.711645	41.650880
3507.391517	337796.184948	41.655885
3506.766063	337704.151420	41.660890
3506.948374	337607.642900	41.665895
3506.656112	337503.935410	41.670900
3506.786358	337411.299829	41.675904
3507.160823	337314.938499	41.680909
3507.069547	337223.354266	41.685914
3506.928655	337122.902486	41.690919
3506.695960	337034.315198	41.695924
3506.658203	336952.512495	41.700928
3506.782935	336849.984025	41.705933
3506.269333	336756.557379	41.710938
3506.870896	336671.526173	41.715943
3506.596750	336579.536598	41.720948
3506.014189	336496.749970	41.725952
3506.452950	336409.531159	41.730957
3506.087839	336326.862735	41.735962
3505.950659	336233.808225	41.740967
3506.535701	336156.534750	41.745972
3506.312416	336063.951023	41.750976
3506.151870	335972.298195	41.755981
3506.198797	335890.251003	41.760986
3505.983576	335812.923902	41.765991
3505.847061	335737.720536	41.770996
3505.611505	335666.194568	41.776000
3505.586483	335581.589403	41.781005
3505.593316	335514.348530	41.786010
3505.580530	335434.038976	41.791015
3505.608421	335358.681979	41.796020
3505.656336	335282.507897	41.801024
3505.246178	335207.117349	41.806029
3505.228916	335132.275577	41.811034
3505.278611	335068.231548	41.816039
3505.278727	334991.759164	41.821044
3505.017244	334922.397487	41.826048
3505.188977	334856.630101	41.831053
3505.281097	334795.783348	41.836058
3505.312351	334724.162985	41.841063
3505.291128	334658.984912	41.846068
3505.216028	334583.871329	41.851072
3505.241747	334516.345946	41.856077
3505.006262	334449.039299	41.861082
3505.066564	334389.061540	41.866087
3505.073341	334320.190872	41.871092
3504.829898	334260.082369	41.876096
3505.121445	334188.318555	41.881101
3505.326139	334122.010648	41.886106
3505.110454	334052.589329	41.891111
3505.054257	333987.619010	41.896116
3504.687642	333921.044013	41.901120
3504.639885	333860.115876	41.906125
3504.596167	333802.442342	41.911130
3504.655545	333745.184951	41.916135
3504.658122	333683.841741	41.921140
3504.069636	333632.102559	41.926144
3504.314931	333574.383492	41.931149
3504.262517	333525.383357	41.936154
3504.275192	333459.536652	41.941159
3504.391647	333411.044051	41.946164
3504.035520	333356.623177	41.951168
3504.274536	333290.537330	41.956173
3504.350869	333243.831072	41.961178
3504.204509	333180.475712	41.966183
3504.090874	333131.001414	41.971188
3503.857069	333088.234660	41.976192
3504.034776	333034.925204	41.981197
3504.054278	332989.422858	41.986202
3503.818448	332934.143284	41.991207
3504.125397	332885.620227	41.996212
3503.807036	332845.460575	42.001216
3504.027531	332786.777729	42.006221
3503.688395	332745.451302	42.011226
3504.002657	332691.891117	42.016231
3503.876288	332647.835417	42.021236
3503.607993	332598.206570	42.026240
3503.800762	332550.514795	42.031245
3503.572252	332504.135047	42.036250
3503.422770	332460.972904	42.041255
3503.444076	332430.169992	42.046260
3503.576269	332383.326774	42.051264
3503.703735	332346.810149	42.056269
3503.589604	332298.326739	42.061274
3503.497259	332253.349663	42.066279
3503.293470	332210.704393	42.071284
3503.230128	332169.613988	42.076288
3503.715361	332126.301369	42.081293
3503.356240	332088.334562	42.086298
3503.121173	332043.735620	42.091303
3503.144705	332002.377119	42.096308
3503.100506	331970.948239	42.101312
3503.384181	331934.101594	42.106317
3503.209441	331903.100004	42.111322
3503.433684	331861.328468	42.116327
3503.214463	331816.421579	42.121332
3503.324805	331774.922092	42.126336
3503.379922	331738.390762	42.131341
3503.108345	331713.635409	42.136346
3503.046494	331666.948816	42.141351
3503.021820	331638.314321	42.146356
3502.988224	331606.603712	42.151360
3503.340050	331562.471997	42.156365
3503.179809	331537.343051	42.161370
3503.045217	331494.915068	42.166375
3503.310492	331451.279999	42.171380
3503.004837	331423.197948	42.176384
3503.504437	331385.147061	42.181389
3503.374791	331348.517075	42.186394
3503.265331	331303.770463	42.191399
3503.259803	331276.073761	42.196404
3503.088594	331233.651214	42.201408
3503.356266	331193.067559	42.206413
3503.195676	331170.380095	42.211418
3503.379026	331120.602417	42.216423
3503.242609	331083.566292	42.221428
3503.010661	331051.911670	42.226432
3503.300037	330998.429307	42.231437
3503.316299	330972.483938	42.236442
3503.227151	330941.162978	42.241447
3503.517833	330899.888694	42.246452
3503.012836	330867.742490	42.251456
3503.147544	330824.584941	42.256461
3502.893269	330785.277869	42.261466
3503.204174	330748.018882	42.266471
3503.210033	330711.494278	42.271476
3503.004262	330672.815368	42.276480
3503.312300	330636.930179	42.281485
3503.191127	330612.125168	42.286490
3503.324873	330575.249794	42.291495
3502.947954	330532.782332	42.296500
3502.981446	330500.271856	42.301504
3502.909747	330459.333535	42.306509
3502.884222	330432.402390	42.311514
3502.987574	330399.651996	42.316519
3503.029636	330371.794597	42.321524
3502.536742	330342.469302	42.326528
3502.751461	330311.024022	42.331533
3502.787825	330281.488764	42.336538
3502.675791	330243.634113	42.341543
3502.744504	330224.369359	42.346548
3502.649346	330190.250916	42.351552
3502.822310	330159.498778	42.356557
3502.681089	330135.561376	42.361562
3502.468030	330107.972586	42.366567
3502.659387	330082.279028	42.371572
3502.456744	330049.550743	42.376576
3502.651860	330018.082856	42.381581
3502.959107	330005.571797	42.386586
3502.966121	329965.866957	42.391591
3503.049199	329931.822161	42.396596
3502.477229	329906.349564	42.401600
3502.936452	329867.972845	42.406605
3502.760268	329840.734189	42.411610
3502.692595	329809.180043	42.416615
3502.483987	329778.792478	42.421620
3502.519630	329755.056106	42.426624
3502.780007	329721.212323	42.431629
3502.433262	329711.677570	42.436634
3502.838893	329669.773567	42.441639
3502.935294	329649.181578	42.446644
3502.546185	329619.763206	42.451648
3502.239278	329579.369432	42.456653
3502.704140	329549.766629	42.461658
3502.446146	329535.334413	42.466663
3502.759515	329505.348298	42.471668
3502.458129	329476.577417	42.476672
3502.819337	329457.266556	42.481677
3502.429289	329433.215013	42.486682
3502.597332	329406.202025	42.491687
3502.520113	329372.817683	42.496692
3502.358126	329343.338159	42.501696
3502.369443	329324.666945	42.506701
3502.492547	329300.357047	42.511706
3502.277531	329276.685008	42.516711
3502.704202	329241.517612	42.521716
3502.515934	329225.370215	42.526720
3502.492360	329198.895747	42.531725
3502.258927	329173.700404	42.536730
3502.288330	329147.624586	42.541735
3502.586050	329125.398418	42.546740
3502.423512	329105.736863	42.551744
3502.550333	329080.968412	42.556749
3502.454622	329049.697826	42.561754
3502.594328	329021.824198	42.566759
3502.334477	328998.031823	42.571764
3502.424039	328991.989649	42.576768
3502.593261	328958.261200	42.581773
3502.591591	328933.309259	42.586778
3502.358529	328904.756196	42.591783
3502.673183	328875.685079	42.596788
3502.149412	328863.659674	42.601792
3502.161093	328830.311843	42.606797
3502.341751	328819.041104	42.611802
3502.017880	328796.886494	42.616807
3502.335549	328774.860494	42.621812
3502.179279	328760.971673	42.626816
3502.409004	328730.896302	42.631821
3502.337829	328711.576366	42.636826
3502.320061	328681.336164	42.641831
3502.200770	328658.869699	42.646836
3502.358135	328632.290255	42.651840
3502.483887	328606.173579	42.656845
3502.335111	328587.755965	42.661850
3502.263356	328573.955609	42.666855
3502.550765	328547.940800	42.671860
3502.104880	328519.624216	42.676864
3502.259438	328489.941949	42.681869
3502.173576	328481.688771	42.686874
3501.622783	328457.458273	42.691879
3502.169219	328433.819297	42.696884
3501.994121	328424.460881	42.701888
3502.020300	328396.986098	42.706893
3501.654422	328398.696667	42.711898
3501.960161	328371.763186	42.716903
3501.934396	328348.798641	42.721908
3501.744234	328336.441123	42.726912
3501.978523	328322.516524	42.731917
3501.837576	328315.467412	42.736922
3501.515722	328297.127592	42.741927
3502.025686	328267.974622	42.746932
3501.771485	328268.624863	42.751936
3501.856712	328249.458301	42.756941
3501.483284	328222.681769	42.761946
3501.809342	328217.874303	42.766951
3501.991932	328208.841455	42.771956
3501.923809	328179.931413	42.776960
3501.785236	328173.365188	42.781965
3501.633459	328147.876626	42.786970
3501.415820	328138.168688	42.791975
3501.907999	328121.049633	42.796980
3501.816569	328121.318324	42.801985
3501.628209	328100.998968	42.806989
3501.926442	328085.588998	42.811994
3501.460548	328077.242533	42.816999
3501.550598	328055.404335	42.822004
3501.514074	328047.855564	42.827009
3502.006553	328035.365793	42.832013
3501.774258	328012.255289	42.837018
3501.584338	327999.414341	42.842023
3501.955561	328003.655047	42.847028
3501.670406	327996.475806	42.852033
3501.822502	327960.383623	42.857037
3501.929737	327949.505658	42.862042
3501.763038	327937.296964	42.867047
3501.787772	327917.071380	42.872052
3501.705113	327911.132274	42.877057
3501.687981	327889.208997	42.882061
3501.617665	327866.429191	42.887066
3501.764046	327869.662178	42.892071
3501.407732	327858.347935	42.897076
3501.671676	327834.803639	42.902081
3501.595924	327828.125791	42.907085
3501.499696	327817.940941	42.912090
3501.352296	327819.439324	42.917095
3502.023598	327797.128569	42.922100
3501.636371	327791.847531	42.927105
3501.741946	327772.957356	42.932109
3501.994958	327753.840633	42.937114
3501.883801	327742.131921	42.942119
3501.798758	327727.010659	42.947124
3501.620278	327714.829175	42.952129
3501.690911	327701.311489	42.957133
3502.022682	327692.051711	42.962138
3501.585837	327670.066748	42.967143
3501.963014	327656.297632	42.972148
3501.353554	327654.383480	42.977153
3501.699802	327636.218704	42.982157
3501.814418	327624.525534	42.987162
3501.576799	327626.012593	42.992167
3501.597855	327606.168970	42.997172
3501.392522	327589.285916	43.002177
3501.509549	327574.514551	43.007181
3501.908806	327568.016761	43.012186
3501.601324	327559.289311	43.017191
3501.744134	327538.281982	43.022196
3501.289894	327532.782458	43.027201
3501.311944	327527.513708	43.032205
3501.468603	327523.266807	43.037210
3501.677547	327512.957860	43.042215
3501.724265	327485.377489	43.047220
3501.695461	327481.566561	43.052225
3501.449804	327479.951635	43.057229
3501.524863	327454.096490	43.062234
3501.372946	327448.066397	43.067239
3501.523486	327452.570592	43.072244
3501.413940	327442.871021	43.077249
3501.314047	327423.453201	43.082253
3501.183899	327413.985773	43.087258
3501.493586	327400.074500	43.092263
3501.574926	327396.526146	43.097268
3501.192961	327401.647764	43.102273
3501.213396	327390.020122	43.107277
3501.291462	327365.995879	43.112282
3501.245326	327359.364195	43.117287
3501.485974	327361.488715	43.122292
3501.213619	327361.836570	43.127297
3501.269932	327361.268199	43.132301
3501.314977	327354.469640	43.137306
3501.285992	327350.149997	43.142311
3501.639839	327328.117540	43.147316
3501.705821	327324.775073	43.152321
3501.524374	327308.066221	43.157325
3501.615251	327307.238081	43.162330
3501.529626	327290.666860	43.167335
3501.791013	327281.824976	43.172340
3501.500522	327273.985087	43.177345
3501.434901	327254.892503	43.182349
3501.749560	327227.549867	43.187354
3501.324414	327232.729130	43.192359
3501.377700	327215.551119	43.197364
3501.527440	327228.627605	43.202369
3501.706078	327190.012350	43.207373
3501.504589	327182.005909	43.212378
3501.551993	327181.820478	43.217383
3501.804831	327176.998898	43.222388
3501.886928	327160.604895	43.227393
3501.620257	327155.686475	43.232397
3501.465396	327147.698173	43.237402
3501.129970	327130.351966	43.242407
3501.629102	327111.527134	43.247412
3501.419343	327103.496533	43.252417
3501.546493	327106.834335	43.257421
3501.595313	327104.690058	43.262426
3501.534322	327089.412174	43.267431
3501.601076	327060.988967	43.272436
3501.476063	327059.558655	43.277441
3501.485712	327059.913298	43.282445
3501.955838	327036.336298	43.287450
3501.407224	327024.314215	43.292455
3501.889350	327016.836784	43.297460
3501.816191	326997.999623	43.302465
3501.942722	326993.859123	43.307469
3501.822131	326973.121607	43.312474
3501.432424	326965.831341	43.317479
3501.648469	326955.266773	43.322484
3501.614594	326952.881048	43.327489
3501.353541	326941.958639	43.332493
3501.540652	326925.624433	43.337498
3501.337100	326914.769338	43.342503
3501.769412	326899.694065	43.347508
3501.592000	326904.554835	43.352513
3501.455455	326888.703640	43.357517
3501.525636	326874.346329	43.362522
3501.291379	326869.982416	43.367527
3501.455891	326857.874231	43.372532
3501.248145	326865.868481	43.377537
3501.573005	326850.377561	43.382541
3501.315860	326832.510250	43.387546
3501.378154	326826.955311	43.392551
3501.482223	326819.791317	43.397556
3501.282686	326815.727212	43.402561
3501.263292	326814.890864	43.407565
3501.784311	326796.749259	43.412570
3500.965739	326798.988532	43.417575
3501.070738	326774.272927	43.422580
3501.165029	326784.051430	43.427585
3501.165205	326768.484055	43.432589
3501.532209	326760.236031	43.437594
3501.176929	326782.599778	43.442599
3501.492382	326761.514177	43.447604
3501.118826	326743.715899	43.452609
3501.544061	326738.434886	43.457613
3501.359305	326730.959914	43.462618
3500.580853	326734.032337	43.467623
3501.309240	326727.432082	43.472628
3501.104776	326732.347975	43.477633
3500.943706	326726.319204	43.482637
3501.239838	326721.210994	43.487642
3501.045071	326711.092142	43.492647
3501.432710	326694.701055	43.497652
3501.267382	326688.469448	43.502657
3501.514476	326680.316464	43.507661
3501.727453	326688.092352	43.512666
3501.291284	326677.833172	43.517671
3501.214941	326661.005870	43.522676
3501.169579	326642.367692	43.527681
3501.118143	326647.208798	43.532685
3501.058430	326637.221435	43.537690
3500.979842	326645.806023	43.542695
3501.489384	326640.155699	43.547700
3501.376141	326642.208399	43.552705
3501.759964	326629.964112	43.557709
3501.491465	326606.909327	43.562714
3501.467886	326604.852653	43.567719
3501.445948	326596.029476	43.572724
3501.556357	326593.621172	43.577729
3501.435469	326578.708576	43.582733
3501.679354	326566.511584	43.587738
3501.552524	326562.614146	43.592743
3501.805743	326557.029321	43.597748
3501.461361	326541.032422	43.602753
3501.835811	326522.252244	43.607757
3501.589200	326522.545206	43.612762
3501.676326	326513.526901	43.617767
3501.832468	326492.008198	43.622772
3501.847675	326487.350872	43.627777
3501.424914	326476.428180	43.632781
3501.782444	326448.773067	43.637786
3501.346729	326452.427856	43.642791
3501.815548	326435.820475	43.647796
3501.521290	326434.645534	43.652801
3501.115427	326416.953911	43.657805
3501.948677	326401.128967	43.662810
3501.634699	326402.780631	43.667815
3501.382923	326377.662692	43.672820
3501.284154	326369.945275	43.677825
3501.174551	326358.617472	43.682829
3501.265816	326358.755864	43.687834
3501.423313	326358.934776	43.692839
3501.544476	326355.939722	43.697844
3501.780305	326345.906082	43.702849
3501.816410	326331.706529	43.707853
3501.757484	326326.246783	43.712858
3501.385155	326313.840806	43.717863
3501.381866	326297.358052	43.722868
3501.647866	326291.491383	43.727873
3501.408781	326285.449305	43.732877
3501.425072	326289.084316	43.737882
3501.451254	326268.577863	43.742887
3501.473345	326247.537858	43.747892
3501.648015	326243.008196	43.752897
3501.157108	326240.236010	43.757901
3501.917575	326237.471684	43.762906
3501.608074	326217.093996	43.767911
3501.352127	326203.804924	43.772916
3501.446943	326203.815575	43.777921
3501.464707	326197.529830	43.782925
3501.903091	326165.079675	43.787930
3501.493620	326158.962467	43.792935
3501.560511	326165.133308	43.797940
3501.484400	326167.892472	43.802945
3501.164494	326145.659453	43.807949
3501.557289	326123.315000	43.812954
3501.175629	326124.341323	43.817959
3501.269265	326117.992829	43.822964
3501.287192	326123.586273	43.827969
3501.180382	326121.491712	43.832973
3501.601053	326113.133416	43.837978
3501.330205	326095.649479	43.842983
3501.508930	326082.139786	43.847988
3501.696550	326077.862455	43.852993
3501.226670	326072.263424	43.857997
3501.754528	326049.160132	43.863002
3501.262613	326041.427803	43.868007
3501.180969	326032.588400	43.873012
3500.997469	326031.319819	43.878017
3501.093568	326025.276175	43.883021
3501.418830	326023.800868	43.888026
3501.746772	326029.167796	43.893031
3501.709167	326001.116279	43.898036
3501.318645	325998.074008	43.903041
3501.446489	326005.252840	43.908045
3501.604085	325994.773471	43.913050
3501.572275	325969.951575	43.918055
3501.808891	325951.370743	43.923060
3501.752327	325959.494160	43.928065
3501.806231	325927.129362	43.933069
3501.861152	325918.014209	43.938074
3501.389647	325916.536276	43.943079
3501.492877	325901.461204	43.948084
3501.536116	325888.684878	43.953089
3501.241008	325873.519446	43.958093
3501.544291	325864.568952	43.963098
3501.764289	325871.377276	43.968103
3501.773783	325861.582401	43.973108
3501.588536	325849.859282	43.978113
3501.504461	325832.803906	43.983117
3501.854391	325818.605985	43.988122
3501.483241	325802.969102	43.993127
3501.237766	325788.787943	43.998132
3501.681203	325782.842585	44.003137
3501.653898	325788.239647	44.008141
3501.548269	325757.629406	44.013146
3501.649693	325755.756646	44.018151
3501.454300	325746.019211	44.023156
3501.454581	325750.292713	44.028161
3501.511603	325728.254912	44.033165
3501.780886	325719.309702	44.038170
3501.274383	325721.576556	44.043175
3501.527393	325698.973909	44.048180
3501.559418	325693.805110	44.053185
3501.910613	325675.333427	44.058189
3501.765604	325668.564296	44.063194
3501.771299	325661.135663	44.068199
3501.869037	325641.355396	44.073204
3501.563761	325642.166288	44.078209
3501.694802	325621.159799	44.083213
3501.822024	325597.330318	44.088218
3501.691207	325597.045555	44.093223
3501.858154	325587.912814	44.098228
3501.474389	325559.151979	44.103233
3501.655027	325549.660962	44.108237
3501.518411	325541.796677	44.113242
3501.952507	325533.614228	44.118247
3501.639700	325523.335468	44.123252
3501.468355	325516.061674	44.128257
3501.563627	325508.186568	44.133261
3501.805532	325472.052673	44.138266
3501.553996	325481.325927	44.143271
3501.578121	325475.395204	44.148276
3501.703927	325463.114590	44.153281
3501.518236	325433.101688	44.158285
3501.482940	325434.430007	44.163290
3501.329996	325427.840140	44.168295
3501.670876	325414.304874	44.173300
3501.604458	325401.163971	44.178305
3501.364514	325388.126506	44.183309
3501.458524	325388.874979	44.188314
3501.404627	325396.896341	44.193319
3501.831497	325370.908546	44.198324
3501.383358	325351.467857	44.203329
3501.452770	325349.981650	44.208333
3501.515917	325349.691999	44.213338
3501.618810	325333.548382	44.218343
3501.583910	325314.907957	44.223348
3501.691127	325309.294911	44.228353
3501.427813	325300.280247	44.233357
3501.501558	325276.179122	44.238362
3501.744843	325280.872564	44.243367
3501.661092	325271.015810	44.248372
3501.510008	325258.091600	44.253377
3501.724358	325240.455125	44.258381
3501.362306	325226.673563	44.263386
3501.630115	325227.649246	44.268391
3502.085770	325208.601387	44.273396
3501.744117	325198.479681	44.278401
3501.851778	325188.491231	44.283405
3501.764042	325172.657170	44.288410
3501.476339	325162.730524	44.293415
3501.455193	325153.194647	44.298420
3501.185224	325147.030037	44.303425
3501.521916	325154.074617	44.308429
3501.583463	325128.220096	44.313434
3501.638066	325113.635655	44.318439
3501.822574	325106.865790	44.323444
3501.765634	325100.922248	44.328449
3501.391572	325078.035724	44.333453
3501.351780	325067.434347	44.338458
3501.352282	325069.520220	44.343463
3501.420069	325059.080088	44.348468
3501.336033	325041.948061	44.353473
3501.583954	325035.626154	44.358477
3501.937965	325022.851846	44.363482
3501.716528	325031.204728	44.368487
3501.689439	325013.504150	44.373492
3501.549520	325000.043914	44.378497
3501.082069	324995.690817	44.383501
3501.728429	324989.255735	44.388506
3501.862124	324981.247331	44.393511
3501.623714	324964.266595	44.398516
3501.649592	324957.445191	44.403521
3501.298223	324947.579322	44.408525
3501.350250	324923.328756	44.413530
3501.436370	324912.834845	44.418535
3501.006928	324903.947818	44.423540
3501.544766	324905.339179	44.428545
3501.398056	324902.843783	44.433549
3501.571078	324896.380936	44.438554
3501.550610	324876.771407	44.443559
3501.247484	324869.797920	44.448564
3501.488989	324862.357713	44.453569
3501.430716	324879.130567	44.458573
3501.606677	324847.610723	44.463578
3501.177835	324838.392893	44.468583
3501.435949	324829.118539	44.473588
3501.232914	324818.975067	44.478593
3501.145702	324831.733240	44.483597
3501.262134	324819.021450	44.488602
3501.454110	324817.363433	44.493607
3501.714502	324793.945112	44.498612
3501.508887	324786.345850	44.503617
3501.307113	324780.653848	44.508621
3501.430481	324777.607457	44.513626
3501.446855	324760.154356	44.518631
3501.441397	324749.751035	44.523636
3501.399819	324744.466432	44.528641
3501.567806	324745.457733	44.533645
3501.184988	324732.238889	44.538650
3501.378557	324715.190515	44.543655
3501.280117	324696.356236	44.548660
3501.317979	324708.280871	44.553665
3501.419459	324704.551065	44.558669
3501.833261	324696.854948	44.563674
3501.623826	324682.947589	44.568679
3501.588444	324659.168420	44.573684
3501.432942	324663.797087	44.578689
3501.592905	324655.555568	44.583693
3501.772067	324635.940152	44.588698
3501.885058	324628.367365	44.593703
3501.298157	324620.573300	44.598708
3501.924204	324612.920300	44.603713
3501.914013	324595.420405	44.608717
3501.775115	324580.789711	44.613722
3501.639215	324572.365486	44.618727
3502.014081	324551.879970	44.623732
3502.137669	324539.675740	44.628737
3501.508518	324523.976948	44.633741
3501.316721	324502.689658	44.638746
3501.605064	324502.695493	44.643751
3501.281478	324489.569064	44.648756
3501.179457	324489.228914	44.653761
3501.145674	324470.969505	44.658765
3501.694774	324457.681192	44.663770
3501.366882	324454.908834	44.668775
3501.586426	324453.907891	44.673780
3501.530604	324455.315765	44.678785
3501.393551	324436.996170	44.683789
3501.674118	324415.940247	44.688794
3501.775208	324417.349029	44.693799
3501.585266	324404.557816	44.698804
3501.225368	324387.341451	44.703809
3501.317086	324382.214030	44.708813
3501.392980	324359.918157	44.713818
3501.649081	324379.949060	44.718823
3501.479926	324368.299314	44.723828
3501.614555	324347.088103	44.728833
3501.161407	324341.155516	44.733837
3501.426120	324334.372985	44.738842
3501.262039	324335.238143	44.743847
3501.270447	324332.845653	44.748852
3501.659408	324326.883164	44.753857
3501.554288	324314.434800	44.758861
3501.545889	324295.967837	44.763866
3501.344639	324299.687913	44.768871
3501.481872	324291.577066	44.773876
3501.753996	324275.203067	44.778881
3501.402264	324260.834480	44.783885
3501.360493	324248.961278	44.788890
3501.461627	324248.538488	44.793895
3501.484358	324240.165710	44.798900
3501.253937	324226.388669	44.803905
3501.278273	324225.265607	44.808909
3501.348142	324209.788111	44.813914
3501.216032	324222.553493	44.818919
3501.425008	324207.817404	44.823924
3501.326495	324203.075841	44.828929
3501.412299	324187.112513	44.833933
3501.710858	324173.659771	44.838938
3501.260412	324183.244239	44.843943
3501.098131	324169.176702	44.848948
3501.322175	324174.865382	44.853953
3501.391794	324160.761588	44.858957
3501.426587	324142.211487	44.863962
3501.054962	324138.860858	44.868967
3501.082925	324124.381985	44.873972
3501.356010	324133.980542	44.878977
3501.153044	324128.059688	44.883981
3501.195816	324130.164439	44.888986
3501.288880	324124.960460	44.893991
3500.947831	324104.917349	44.898996
3501.260931	324095.507041	44.904001
3501.239463	324095.332365	44.909005
3501.503456	324084.759557	44.914010
3501.464956	324086.393682	44.919015
3501.315791	324085.323181	44.924020
3501.282704	324077.874885	44.929025
3501.409170	324070.376204	44.934029
3501.374743	324048.173726	44.939034
3501.092047	324049.159188	44.944039
3501.085398	324045.497105	44.949044
3501.296155	324053.350160	44.954049
3501.301060	324050.118728	44.959053
3501.325016	324043.653613	44.964058
3500.830033	324030.731903	44.969063
3501.215172	324014.976098	44.974068
3501.478021	324010.178018	44.979073
3501.113701	324002.679739	44.984077
3501.487802	323993.310748	44.989082
3501.581005	323993.932180	44.994087
3501.512937	323994.553386	44.999092
3501.484229	323966.142940	45.004097
3501.422041	323955.875481	45.009101
3501.403911	323960.355557	45.014106
3501.408864	323959.642537	45.019111
3501.302834	323943.785423	45.024116
3501.317167	323932.157745	45.029121
3501.263302	323932.267958	45.034125
3501.276399	323916.137822	45.039130
3501.142875	323924.757010	45.044135
3501.134802	323910.868786	45.049140
3501.261638	323909.602497	45.054145
3501.040019	323923.552145	45.059149
3501.274134	323908.226929	45.064154
3501.396074	323897.574527	45.069159
3501.309593	323884.461713	45.074164
3501.457272	323882.479881	45.079169
3501.011397	323883.796123	45.084173
3501.081611	323871.116704	45.089178
3501.034322	323880.739968	45.094183
3501.557533	323873.026593	45.099188
3501.400485	323852.852838	45.104193
3501.011320	323848.843520	45.109197
3501.211982	323835.914748	45.114202
3501.225546	323840.644270	45.119207
3501.250959	323833.008712	45.124212
3501.644819	323824.221685	45.129217
3500.953676	323829.646472	45.134221
3501.220434	323821.388090	45.139226
3501.121785	323804.715729	45.144231
3501.297259	323799.447948	45.149236
3501.519084	323788.652709	45.154241
3501.011399	323795.905848	45.159245
3501.404732	323796.887381	45.164250
3501.097187	323797.011816	45.169255
3501.157342	323782.654984	45.174260
3501.311147	323779.756395	45.179265
3501.029468	323765.631070	45.184269
3501.123732	323749.310108	45.189274
3501.356432	323752.504492	45.194279
3501.165108	323759.911689	45.199284
3501.068719	323747.436350	45.204289
3501.071086	323747.537772	45.209293
3501.008791	323752.304602	45.214298
3501.323694	323751.492245	45.219303
3501.256613	323755.369465	45.224308
3500.885278	323750.568747	45.229313
3501.289712	323734.580870	45.234317
3501.658838	323718.598506	45.239322
3501.248988	323713.244152	45.244327
3501.385558	323716.046546	45.249332
3501.321418	323711.426747	45.254337
3501.240609	323706.148144	45.259341
3501.331506	323700.919012	45.264346
3501.155014	323678.662229	45.269351
3501.221465	323670.893032	45.274356
3501.493667	323674.411951	45.279361
3500.929176	323675.848498	45.284365
3501.424890	323669.080621	45.289370
3501.051197	323674.226849	45.294375
3501.264726	323673.048755	45.299380
3501.307880	323661.314740	45.304385
3501.083316	323643.669884	45.309389
3501.381125	323648.278672	45.314394
3501.566715	323633.240768	45.319399
3501.187286	323643.755496	45.324404
3501.064982	323629.935914	45.329409
3501.346336	323639.558732	45.334413
3501.196330	323620.121490	45.339418
3501.467308	323615.627360	45.344423
3501.232085	323609.711475	45.349428
3501.251703	323598.846043	45.354433
3501.084341	323606.274960	45.359437
3500.936234	323596.987521	45.364442
3501.539049	323606.153068	45.369447
3501.240609	323603.757630	45.374452
3501.281194	323587.572191	45.379457
3501.083537	323578.877589	45.384461
3501.316239	323562.891055	45.389466
3501.252196	323563.308127	45.394471
3501.363599	323556.295048	45.399476
3501.555775	323553.365005	45.404481
3501.018215	323556.730703	45.409485
3501.358323	323552.581904	45.414490
3501.139657	323531.857969	45.419495
3501.122895	323518.785018	45.424500
3501.214905	323509.587214	45.429505
3500.945793	323515.658352	45.434509
3501.121101	323507.236132	45.439514
3501.228971	323521.236159	45.444519
3501.469032	323514.940688	45.449524
3501.470619	323502.653469	45.454529
3500.879739	323493.231718	45.459533
3501.262802	323484.242796	45.464538
3501.259081	323478.214382	45.469543
3501.331058	323480.314600	45.474548
3501.082718	323480.582413	45.479553
3500.821381	323478.079411	45.484557
3501.135121	323471.746976	45.489562
3501.257775	323466.640045	45.494567
3500.995720	323470.802163	45.499572
3501.335579	323474.997374	45.504577
3500.840680	323467.137827	45.509581
3500.902415	323466.186971	45.514586
3500.987647	323467.928971	45.519591
3500.978454	323469.355028	45.524596
3501.331576	323455.740889	45.529601
3501.104801	323449.492953	45.534605
3501.016982	323432.081018	45.539610
3501.274520	323426.571410	45.544615
3501.110817	323431.913788	45.549620
3501.481721	323418.474930	45.554625
3501.181170	323433.378325	45.559629
3501.143362	323428.398232	45.564634
3501.194610	323427.499892	45.569639
3500.998627	323407.611836	45.574644
3501.192509	323395.167328	45.579649
3500.945802	323396.528763	45.584653
3501.084802	323394.471948	45.589658
3501.190456	323389.367666	45.594663
3500.964942	323387.571350	45.599668
3500.975372	323381.133686	45.604673
3500.963801	323387.317213	45.609677
3501.117966	323378.465810	45.614682
3501.078205	323385.238842	45.619687
3501.030687	323395.320156	45.624692
3501.238579	323385.366477	45.629697
3501.052650	323388.957044	45.634701
3500.919406	323383.940988	45.639706
3501.414693	323389.358419	45.644711
3500.792681	323382.052948	45.649716
3501.160869	323372.303157	45.654721
3501.317751	323372.838326	45.659725
3501.456777	323348.064452	45.664730
3501.412931	323346.443245	45.669735
3501.446256	323345.649462	45.674740
3501.468154	323344.170612	45.679745
3501.264486	323329.193454	45.684749
3501.168813	323306.567688	45.689754
3501.272376	323310.876175	45.694759
3501.258199	323303.094076	45.699764
3501.589156	323299.811610	45.704769
3501.356831	323303.791024	45.709773
3501.525355	323291.503083	45.714778
3501.534384	323277.408461	45.719783
3501.017822	323273.647955	45.724788
3501.223839	323263.084002	45.729793
3501.248250	323267.913650	45.734797
3501.741529	323267.760251	45.739802
3501.866142	323258.735369	45.744807
3501.568816	323246.265854	45.749812
3501.511659	323237.269385	45.754817
3501.260384	323205.051908	45.759821
3501.425596	323146.210818	45.764826
3501.430180	323054.705377	45.769831
3500.901154	322903.271872	45.774836
3501.302961	322705.112722	45.779841
3500.640109	322473.513423	45.784845
3500.841623	322180.798679	45.789850
3500.580814	321834.653984	45.794855
3500.262137	321459.539139	45.799860
3499.872108	321016.175463	45.804865
3499.408704	320547.835855	45.809869
3498.952440	320015.531270	45.814874
3498.491176	319441.802333	45.819879
3498.031628	318822.804686	45.824884
3497.828456	318158.293103	45.829889
3497.234877	317453.455209	45.834893
3496.663406	316687.844842	45.839898
3495.813305	315876.288626	45.844903
3495.455306	315025.457226	45.849908
3494.846422	314118.518758	45.854913
3493.825328	313173.917425	45.859917
3493.072477	312167.040735	45.864922
3492.279477	311114.956541	45.869927
3491.424925	310032.577185	45.874932
3490.838171	308892.290086	45.879937
3489.585902	307711.058466	45.884941
3488.514443	306478.542619	45.889946
3487.478551	305205.425092	45.894951
3486.096605	303889.650664	45.899956
3485.145267	302518.955342	45.904961
3484.083697	301118.591150	45.909965
3483.148957	299659.835209	45.914970
3481.819595	298171.908187	45.919975
3480.291007	296623.139716	45.924980
3479.219855	295045.953089	45.929985
3477.631768	293423.648371	45.934989
3476.500122	291757.470754	45.939994
3474.742811	290047.510572	45.944999
3473.284029	288295.733847	45.950004
3472.172169	286513.408501	45.955009
3470.652163	284695.916296	45.960013
3468.983117	282812.257565	45.965018
3467.671652	280908.099919	45.970023
3465.690288	278963.312412	45.975028
3464.132141	276971.332128	45.980033
3462.367515	274952.268438	45.985037
3460.699585	272882.801679	45.990042
3458.152843	270781.033932	45.995047
3456.287991	268655.022130	46.000052
3454.246944	266495.428594	46.005057
3452.526226	264304.391297	46.010061
3450.410195	262070.105137	46.015066
3448.311789	259807.631990	46.020071
3446.000279	257521.822130	46.025076
3444.192429	255185.570876	46.030081
3441.478601	252832.358535	46.035085
3439.398519	250437.778466	46.040090
3437.428328	248019.562946	46.045095
3434.992045	245569.934939	46.050100
3432.472103	243094.312660	46.055105
3429.845219	240595.707816	46.060109
3427.370930	238061.272265	46.065114
3424.788679	235505.032115	46.070119
3422.162943	232926.114953	46.075124
3419.779116	230320.914305	46.080129
3416.493765	227691.064679	46.085133
3413.900130	225030.947268	46.090138
3411.046714	222367.814423	46.095143
3408.008398	219677.387135	46.100148
3405.108656	216955.646674	46.105153
3402.028161	214225.340924	46.110157
3398.892471	211476.675500	46.115162
3395.835756	208712.232716	46.120167
3392.883128	205922.718505	46.125172
3389.798707	203117.344287	46.130177
3385.984421	200298.068748	46.135181
3382.852198	197474.583828	46.140186
3379.340973	194631.475866	46.145191
3375.786505	191788.842466	46.150196
3372.422693	188929.183674	46.155201
3369.020311	186064.128552	46.160205
3365.135297	183191.715630	46.165210
3361.672764	180305.444131	46.170215
3357.552514	177432.836255	46.175220
3354.102467	174533.371231	46.180225
3349.918383	171647.873583	46.185229
3345.573062	168755.088824	46.190234
3341.558775	165865.830119	46.195239
3336.641798	162994.500867	46.200244
3332.469446	160131.988383	46.205249
3327.824250	157271.563911	46.210253
3323.302889	154416.308584	46.215258
3318.212853	151576.401990	46.220263
3313.394065	148757.697095	46.225268
3308.053094	145958.093335	46.230273
3302.868998	143205.581633	46.235277
3297.175940	140413.617501	46.240282
3291.718493	137674.958879	46.245287
3285.426562	135008.266510	46.250292
3279.039329	132385.583163	46.255297
3272.202100	129816.463112	46.260301
3264.980947	127299.415239	46.265306
3257.997540	124841.077971	46.270311
3250.436821	122436.955239	46.275316
3243.076642	120111.997720	46.280321
3235.202953	117870.439004	46.285325
3227.266350	115691.037643	46.290330
3218.891166	113610.679890	46.295335
3209.673500	111617.551818	46.300340
3201.410615	109697.997819	46.305345
3192.509887	107895.036313	46.310349
3183.509496	106181.768716	46.315354
3174.168392	104571.364675	46.320359
3165.200060	103070.677554	46.325364
3156.293444	101664.031611	46.330369
3147.316970	100365.747888	46.335373
3138.584405	99172.002898	46.340378
3130.531070	98050.613639	46.345383
3122.611002	97021.725653	46.350388
3115.455200	96086.222849	46.355393
3108.337060	95232.481080	46.360397
3101.714609	94434.154995	46.365402
3095.635430	93702.085297	46.370407
3088.991139	93040.481642	46.375412
3083.563262	92421.512068	46.380417
3077.638888	91866.204853	46.385421
3072.462068	91350.117808	46.390426
3067.448449	90879.210708	46.395431
3062.528815	90446.669049	46.400436
3058.202761	90022.833370	46.405441
3054.024133	89639.969799	46.410445
3050.263312	89284.223355	46.415450
3046.539097	88929.313997	46.420455
3042.711040	88599.632708	46.425460
3039.358272	88276.805149	46.430465
3035.985726	87962.344204	46.435469
3032.758393	87658.396378	46.440474
3029.633869	87357.599131	46.445479
3025.882873	87061.362309	46.450484
3022.734133	86742.267554	46.455489
3019.102022	86457.160227	46.460493
3015.914698	86163.283611	46.465498
3012.851247	85861.704503	46.470503
3009.566395	85571.825541	46.475508
3006.236864	85279.263210	46.480513
3002.565717	84988.497690	46.485517
2999.210674	84702.856092	46.490522
2996.477145	84406.080669	46.495527
2992.616307	84116.916147	46.500532
2989.488641	83831.476298	46.505537
2985.978882	83554.940509	46.510541
2982.393362	83256.201473	46.515546
2978.930059	82957.408342	46.520551
2975.350482	82682.670341	46.525556
2972.056840	82394.209428	46.530561
2968.230562	82113.341987	46.535565
2964.831233	81827.888480	46.540570
2961.774443	81550.183534	46.545575
2957.916169	81279.808833	46.550580
2954.522669	80993.473703	46.555585
2950.871176	80729.588139	46.560589
2947.200070	80449.437037	46.565594
2943.907577	80172.633595	46.570599
2939.996838	79905.316076	46.575604
2936.634818	79635.705247	46.580609
2932.769298	79373.822001	46.585613
2929.013714	79110.336376	46.590618
2925.325653	78849.243211	46.595623
2921.875162	78598.034851	46.600628
2918.063117	78343.595788	46.605633
2914.373580	78090.194080	46.610637
2911.255378	77844.732178	46.615642
2907.501966	77589.859094	46.620647
2903.479038	77357.154700	46.625652
2899.848198	77110.268193	46.630657
2896.018898	76877.258197	46.635661
2892.643629	76640.813654	46.640666
2889.149562	76401.405242	46.645671
2885.305334	76169.978435	46.650676
2882.173358	75930.365147	46.655681
2878.815879	75713.534364	46.660685
2874.926630	75484.787385	46.665690
2871.856147	75251.088496	46.670695
2867.888275	75032.161639	46.675700
2864.710671	74806.153776	46.680705
2861.130335	74579.525044	46.685709
2857.418019	74349.413932	46.690714
2854.068134	74126.892870	46.695719
2850.123011	73908.327196	46.700724
2847.254525	73680.528037	46.705729
2843.765048	73456.078789	46.710733
2839.852821	73236.395999	46.715738
2836.787716	73012.976187	46.720743
2833.457136	72790.742621	46.725748
2830.124722	72550.568661	46.730753
2826.598339	72325.817281	46.735757
2822.910746	72109.181632	46.740762
2819.275138	71872.959523	46.745767
2815.502834	71654.905997	46.750772
2812.494577	71423.618110	46.755777
2809.272809	71191.260965	46.760781
2805.562106	70971.095687	46.765786
2802.079484	70722.200662	46.770791
2798.748737	70505.776366	46.775796
2795.256064	70270.270066	46.780801
2791.550121	70043.699826	46.785805
2788.250287	69817.899686	46.790810
2784.494594	69575.584497	46.795815
2780.842450	69350.357740	46.800820
2777.619931	69115.295767	46.805825
2774.135323	68895.645927	46.810829
2770.607025	68664.501933	46.815834
2767.514323	68428.898997	46.820839
2763.976973	68204.800574	46.825844
2760.515619	67965.158705	46.830849
2756.987370	67730.049253	46.835853
2753.446838	67493.579085	46.840858
2750.290240	67254.315145	46.845863
2746.226224	67023.999692	46.850868
2742.902957	66792.707173	46.855873
2739.678413	66553.352513	46.860877
2736.401657	66324.754707	46.865882
2732.635120	66071.315222	46.870887
2729.213244	65838.002902	46.875892
2725.813597	65599.414568	46.880897
2722.389114	65363.733097	46.885901
2718.470017	65121.631578	46.890906
2715.385661	64874.406564	46.895911
2711.803539	64637.493436	46.900916
2708.217082	64395.486502	46.905921
2704.397142	64151.804720	46.910925
2701.247947	63918.365954	46.915930
2698.138875	63669.017732	46.920935
2694.296602	63428.716686	46.925940
2691.074407	63180.139961	46.930945
2687.134020	62947.976429	46.935949
2683.835149	62698.477185	46.940954
2680.679872	62446.597051	46.945959
2677.036794	62217.383088	46.950964
2673.643501	61965.240434	46.955969
2670.037382	61720.514513	46.960973
2666.232341	61468.872879	46.965978
2663.068303	61221.182479	46.970983
2659.361020	60978.244010	46.975988
2655.955402	60727.480369	46.980993
2652.521026	60490.520191	46.985997
2649.063073	60234.439053	46.991002
2645.797188	59981.833522	46.996007
2642.277726	59739.658500	47.001012
2638.656977	59481.922697	47.006017
2634.862296	59241.984979	47.011021
2631.264779	58990.120586	47.016026
2627.874484	58735.694480	47.021031
2624.386472	58498.495527	47.026036
2621.022174	58248.277587	47.031041
2617.463339	58004.146221	47.036045
2614.218108	57756.383127	47.041050
2610.772622	57500.550931	47.046055
2606.765922	57260.101292	47.051060
2603.723024	57011.051511	47.056065
2600.088484	56755.390063	47.061069
2596.367872	56497.175059	47.066074
2593.172687	56245.441368	47.071079
2589.546286	56002.514731	47.076084
2585.993894	55749.649294	47.081089
2582.481489	55497.186352	47.086093
2579.074532	55245.635923	47.091098
2575.844637	54981.891420	47.096103
2572.529245	54734.392661	47.101108
2568.702464	54474.826732	47.106113
2565.439936	54216.393525	47.111117
2561.827367	53956.780746	47.116122
2558.197075	53696.310773	47.121127
2554.532102	53440.708791	47.126132
2551.157035	53193.990486	47.131137
2547.790496	52939.007076	47.136141
2544.308549	52683.784387	47.141146
2540.876518	52417.759251	47.146151
2536.947912	52169.190735	47.151156
2533.724029	51911.703062	47.156161
2530.098407	51647.683573	47.161165
2526.573549	51398.235443	47.166170
2523.522439	51134.664783	47.171175
2519.839268	50889.408295	47.176180
2516.408682	50619.603713	47.181185
2513.145055	50368.983974	47.186189
2509.393374	50106.321195	47.191194
2506.272913	49837.149635	47.196199
2502.436139	49574.950254	47.201204
2498.342106	49312.717991	47.206209
2495.182076	49048.452397	47.211213
2491.864640	48793.411774	47.216218
2488.646898	48526.839700	47.221223
2484.962774	48264.828065	47.226228
2481.440950	47997.466145	47.231233
2478.006344	47732.256571	47.236237
2474.347502	47463.431830	47.241242
2471.025755	47200.367293	47.246247
2467.423122	46936.005147	47.251252
2463.935781	46677.469384	47.256257
2460.445872	46409.886511	47.261261
2456.722088	46143.700633	47.266266
2453.327705	45884.303215	47.271271
2449.489034	45621.433064	47.276276
2446.608565	45349.721203	47.281281
2443.399277	45080.283744	47.286285
2439.722578	44809.432308	47.291290
2436.319995	44549.246194	47.296295
2432.738195	44286.522756	47.301300
2429.180217	44009.663196	47.306305
2425.758220	43735.785359	47.311309
2422.026473	43464.286672	47.316314
2418.857790	43187.255966	47.321319
2415.041863	42927.908101	47.326324
2411.668861	42651.448730	47.331329
2407.904263	42373.367328	47.336333
2404.825765	42108.859814	47.341338
2401.155638	41834.530693	47.346343
2397.854220	41560.134632	47.351348
2394.338181	41288.197777	47.356353
2391.134928	41008.390855	47.361357
2387.206176	40751.267516	47.366362
2384.313107	40464.114550	47.371367
2380.481911	40191.562182	47.376372
2377.323460	39898.441012	47.381377
2373.687470	39623.595335	47.386381
2369.875462	39341.679552	47.391386
2366.724050	39062.555221	47.396391
2362.602417	38786.566124	47.401396
2359.507657	38497.936370	47.406401
2356.218682	38216.086564	47.411405
2352.189668	37947.682627	47.416410
2349.490639	37652.193253	47.421415
2345.565793	37372.875760	47.426420
2342.111633	37091.700493	47.431425
2338.861392	36811.821977	47.436429
2335.020224	36539.310926	47.441434
2331.884577	36244.511502	47.446439
2328.361143	35966.322356	47.451444
2324.807726	35675.875170	47.456449
2321.224204	35381.214809	47.461453
2318.160469	35096.397798	47.466458
2314.849490	34797.126127	47.471463
2311.147876	34503.776897	47.476468
2307.583245	34210.822329	47.481473
2304.300036	33919.184276	47.486477
2300.986810	33617.945652	47.491482
2297.787885	33322.575584	47.496487
2293.947356	33019.634231	47.501492
2290.404738	32720.536035	47.506497
2286.883943	32425.133885	47.511501
2283.533787	32131.642345	47.516506
2280.074858	31819.309916	47.521511
2276.727812	31522.866586	47.526516
2273.130620	31204.898870	47.531521
2269.843147	30888.300885	47.536525
2266.400631	30593.007541	47.541530
2263.203382	30272.469151	47.546535
2259.419343	29966.185458	47.551540
2255.919054	29650.381190	47.556545
2252.569156	29338.816888	47.561549
2248.732095	29025.090156	47.566554
2245.337102	28711.286380	47.571559
2241.709680	28405.571757	47.576564
2238.502960	28078.808059	47.581569
2235.329587	27764.274388	47.586573
2231.903302	27453.333687	47.591578
2228.780086	27125.311180	47.596583
2225.420567	26792.793995	47.601588
2221.696791	26471.814461	47.606593
2218.318092	26133.735044	47.611597
2214.754471	25806.651815	47.616602
2211.293945	25484.816706	47.621607
2207.736863	25147.947530	47.626612
2204.667699	24817.825059	47.631617
2201.185695	24473.928927	47.636621
2197.370091	24143.997670	47.641626
2193.923371	23803.402065	47.646631
2190.407108	23471.261966	47.651636
2186.946538	23133.936360	47.656641
2183.361942	22799.309340	47.661645
2180.173234	22459.253811	47.666650
2176.610190	22110.349287	47.671655
2173.022405	21772.528203	47.676660
2169.816164	21423.725645	47.681665
2166.318981	21086.776299	47.686669
2162.755756	20740.480520	47.691674
2158.909499	20388.097006	47.696679
2155.645735	20053.953983	47.701684
2152.447066	19701.848849	47.706689
2148.686332	19361.936189	47.711693
2145.335372	19012.508615	47.716698
2141.951930	18660.204109	47.721703
2138.127718	18310.014416	47.726708
2134.718168	17955.642917	47.731713
2131.364562	17613.296582	47.736717
2127.302282	17268.318449	47.741722
2123.963206	16927.470322	47.746727
2120.893233	16576.126759	47.751732
2117.099254	16227.334789	47.756737
2113.632602	15886.214692	47.761741
2109.871701	15542.097396	47.766746
2106.300722	15184.413903	47.771751
2102.607325	14854.018361	47.776756
2098.746579	14516.578076	47.781761
2095.267052	14178.504689	47.786765
2091.264637	13841.247328	47.791770
2087.395687	13515.911303	47.796775
2083.801500	13204.617326	47.801780
2079.114992	12890.694286	47.806785
2075.065899	12596.400637	47.811789
2070.876585	12316.174327	47.816794
2066.213343	12052.393867	47.821799
2061.548462	11800.330912	47.826804
2056.976559	11553.771586	47.831809
2053.177963	11313.207550	47.836813
2049.081858	11097.999801	47.841818
2045.574248	10871.524460	47.846823
2041.848524	10671.693138	47.851828
2037.912201	10452.776676	47.856833
2034.568363	10253.475709	47.861837
2030.939315	10048.460229	47.866842
2027.581103	9855.645603	47.871847
2024.228190	9647.156766	47.876852
2020.715140	9461.863098	47.881857
2017.363756	9259.633257	47.886861
2013.838073	9064.808187	47.891866
2010.833092	8864.722041	47.896871
2007.120893	8675.479069	47.901876
2003.566927	8486.976103	47.906881
2000.071864	8282.877072	47.911885
1996.409797	8097.151911	47.916890
1993.345322	7897.636271	47.921895
1989.742066	7717.808759	47.926900
1986.289546	7520.374109	47.931905
1982.806536	7325.649313	47.936909
1979.415575	7139.850232	47.941914
1976.248378	6941.734640	47.946919
1972.661481	6754.029973	47.951924
1969.056989	6556.233835	47.956929
1965.951797	6362.887510	47.961933
1962.097984	6162.741967	47.966938
1959.118022	5970.418265	47.971943
1955.627260	5781.778058	47.976948
1952.166092	5592.021169	47.981953
1948.614326	5382.928081	47.986957
1945.022626	5185.505548	47.991962
1941.641590	4982.881130	47.996967
1938.281300	4787.312842	48.001972
1934.925891	4594.204784	48.006977
1931.305171	4387.001035	48.011981
1927.480690	4203.916743	48.016986
1924.537601	3997.700001	48.021991
1920.614796	3797.062790	48.026996
1916.862535	3614.795913	48.032001
1913.695062	3407.570412	48.037005
1910.221032	3211.283800	48.042010
1906.794326	3014.726114	48.047015
1903.176879	2825.788378	48.052020
1899.705567	2630.058252	48.057025
1895.952832	2425.321464	48.062029
1892.345589	2246.203622	48.067034
1888.899204	2035.585412	48.072039
1885.315125	1841.523711	48.077044
1881.565899	1650.635051	48.082049
1878.019474	1461.937851	48.087053
1874.552761	1279.941043	48.092058
1870.961395	1090.599841	48.097063
1867.226300	913.492822	48.102068
1863.414049	733.061699	48.107073
1859.726244	560.212589	48.112077
1855.511524	393.999963	48.117082
1851.643500	240.848720	48.122087
1847.369559	100.490311	48.127092
1840.153431	40.475960	48.132097
1831.526645	53.956008	48.137101
1825.133918	65.729189	48.142106
1820.901269	62.579221	48.147111
1817.739001	66.263239	48.152116
1815.324812	64.404271	48.157121
1812.887623	64.953392	48.162125
1809.918686	67.695982	48.167130
1807.212171	66.411118	48.172135
1804.143317	70.801868	48.177140
1800.828567	71.418720	48.182145
1797.061600	71.714032	48.187149
1793.778510	71.462214	48.192154
1790.380782	68.118322	48.197159
1787.122508	65.546721	48.202164
1783.827632	66.714134	48.207169
1780.354898	62.910578	48.212173
1777.037866	68.852469	48.217178
1773.514861	60.393343	48.222183
1770.203018	60.930655	48.227188
1766.160818	64.524600	48.232193
1763.100741	58.622149	48.237197
1759.383217	64.661522	48.242202
1756.103652	64.605320	48.247207
1752.740033	60.813173	48.252212
1749.334297	57.983086	48.257217
1745.903937	68.656780	48.262221
1742.437055	79.478567	48.267226
1739.185378	64.791761	48.272231
1735.813209	68.714298	48.277236
1731.959936	63.850329	48.282241
1728.352410	58.362602	48.287245
1724.675019	70.913128	48.292250
1721.533406	58.689529	48.297255
1718.433562	69.283029	48.302260
1715.018537	68.453927	48.307265
1711.943652	66.040315	48.312269
1708.394550	67.506969	48.317274
1704.459586	62.915228	48.322279
1700.699080	59.843284	48.327284
1696.904483	69.808355	48.332289
1694.024507	54.307258	48.337293
1690.194480	62.385923	48.342298
1687.112164	63.915573	48.347303
1683.764035	60.760113	48.352308
1680.134802	62.365869	48.357313
1676.642142	54.395590	48.362317
1673.158970	61.685975	48.367322
1669.949794	51.852150	48.372327
1666.262288	57.779281	48.377332
1662.510724	60.676034	48.382337
1658.970123	59.363562	48.387341
1655.773441	61.259137	48.392346
1652.400303	69.845285	48.397351
1648.912217	53.237139	48.402356
1645.326070	63.603037	48.407361
1641.913768	58.021514	48.412365
1638.288349	64.271138	48.417370
1634.852392	67.374773	48.422375
1630.950689	63.837729	48.427380
1627.570852	65.046961	48.432385
1625.025276	54.511335	48.437389
1621.194480	59.783856	48.442394
1617.648953	53.773936	48.447399
1613.813973	55.168304	48.452404
1610.356972	60.594299	48.457409
1606.849320	55.192232	48.462413
1602.856188	56.415201	48.467418
1600.218580	57.441833	48.472423
1596.823511	55.157468	48.477428
1592.899451	58.495698	48.482433
1589.906123	55.047458	48.487437
1585.776348	56.098828	48.492442
1582.276305	55.744992	48.497447
1579.154783	46.109462	48.502452
1575.686063	61.895555	48.507457
1572.126216	52.860145	48.512461
1568.506281	54.920069	48.517466
1565.136719	60.079289	48.522471
1561.589486	55.964770	48.527476
1557.690786	53.525125	48.532481
1554.768862	52.024107	48.537485
1550.749998	57.534896	48.542490
1547.492644	52.935245	48.547495
1544.268738	52.756504	48.552500
1540.247286	54.360420	48.557505
1537.086576	53.605471	48.562509
1533.252176	58.578025	48.567514
1530.059354	54.509287	48.572519
1526.604783	57.897445	48.577524
1523.012250	55.523789	48.582529
1519.839249	44.497945	48.587533
1516.237219	59.200751	48.592538
1512.691331	54.522886	48.597543
1509.095393	54.702947	48.602548
1505.212581	53.124551	48.607553
1502.334695	44.874622	48.612557
1498.450100	54.885467	48.617562
1495.160641	47.123908	48.622567
1492.021305	55.066048	48.627572
1488.127269	54.147483	48.632577
1484.559286	50.194433	48.637581
1480.957959	51.356121	48.642586
1477.582661	50.590487	48.647591
1474.228103	61.524463	48.652596
1470.523652	55.305357	48.657601
1467.534301	53.523851	48.662605
1463.739759	56.025597	48.667610
1460.051065	53.186121	48.672615
1456.586943	50.001444	48.677620
1452.622932	52.336729	48.682625
1449.057836	51.186357	48.687629
1446.003401	61.570320	48.692634
1442.522915	57.511838	48.697639
1439.593810	54.256077	48.702644
1435.541951	64.283635	48.707649
1432.378904	57.641274	48.712653
1428.612462	60.461341	48.717658
1425.308497	52.047174	48.722663
1421.738899	57.835702	48.727668
1418.308987	50.507450	48.732673
1414.512016	48.915654	48.737677
1410.685017	52.744963	48.742682
1407.644387	52.626163	48.747687
1404.339215	50.758070	48.752692
1400.750634	52.550549	48.757697
1397.650574	44.360746	48.762701
1393.594249	48.169008	48.767706
1390.180967	48.206624	48.772711
1386.510803	45.905285	48.777716
1383.121799	51.099236	48.782721
1379.842919	45.743709	48.787725
1376.110443	57.179793	48.792730
1372.760183	53.366713	48.797735
1369.373888	48.426640	48.802740
1365.450542	59.500297	48.807745
1362.119362	47.202125	48.812749
1358.416158	51.195572	48.817754
1354.922602	44.797973	48.822759
1351.509177	45.987241	48.827764
1347.900181	52.531775	48.832769
1344.755866	43.491534	48.837773
1341.442503	57.032376	48.842778
1337.424182	50.024059	48.847783
1334.405625	49.775275	48.852788
1330.565463	56.213631	48.857793
1326.927571	51.452165	48.862797
1323.397030	44.231457	48.867802
1319.964744	50.577492	48.872807
1316.817606	48.048770	48.877812
1313.108347	58.478319	48.882817
1309.684180	54.537625	48.887821
1306.046336	56.464400	48.892826
1302.607005	46.881893	48.897831
1299.321897	40.635186	48.902836
1295.528105	49.205009	48.907841
1292.202452	50.136946	48.912845
1288.601373	52.871064	48.917850
1285.345550	49.286845	48.922855
1281.809069	56.259814	48.927860
1278.082068	58.194229	48.932865
1274.660603	48.741815	48.937869
1270.821157	58.600129	48.942874
1267.410022	63.215446	48.947879
1264.428491	48.322061	48.952884
1260.568992	52.988585	48.957889
1257.247839	41.327978	48.962893
1253.571238	38.613245	48.967898
1250.351112	51.819965	48.972903
1246.481222	47.208749	48.977908
1242.637893	43.922165	48.982913
1239.337610	38.516260	48.987917
1236.042356	35.226139	48.992922
1232.375258	47.028511	48.997927
1229.171719	45.834275	49.002932
1225.732979	46.736481	49.007937
1222.354361	45.152036	49.012941
1218.682671	46.381780	49.017946
1215.191420	44.077810	49.022951
1211.919484	42.770899	49.027956
1207.769382	53.702928	49.032961
1204.538420	42.641998	49.037965
1200.819458	49.013964	49.042970
1197.455845	48.414278	49.047975
1194.374895	44.426226	49.052980
1190.212819	49.867813	49.057985
1187.073708	49.976472	49.062989
1183.972499	48.911764	49.067994
1180.040716	51.295892	49.072999
1176.495433	46.814223	49.078004
1172.785828	57.047711	49.083009
1169.404137	42.273969	49.088013
1165.772468	45.085684	49.093018
1162.627526	49.865002	49.098023
1159.154834	45.985749	49.103028
1155.665105	44.855325	49.108033
1151.987214	38.518308	49.113037
1148.229570	52.258460	49.118042
1144.875743	42.456992	49.123047
1141.659305	54.767811	49.128052
1138.003043	44.450542	49.133057
1134.406979	40.502029	49.138061
1131.138456	52.653323	49.143066
1127.493541	49.313577	49.148071
1124.140131	47.554377	49.153076
1120.209915	43.544288	49.158081
1117.043366	38.263027	49.163085
1113.381767	42.101346	49.168090
1109.861910	45.107548	49.173095
1106.877968	46.169547	49.178100
1103.113199	50.865588	49.183105
1099.668486	45.194444	49.188109
1095.739374	46.394933	49.193114
1091.908796	52.214931	49.198119
1088.944311	46.332562	49.203124
1085.577270	51.592768	49.208129
1082.298454	50.176247	49.213133
1078.909127	44.683102	49.218138
1075.511054	48.185945	49.223143
1071.691520	46.037831	49.228148
1067.809694	55.807928	49.233153
1064.261266	41.775356	49.238157
1061.210502	44.793553	49.243162
1057.234658	50.547721	49.248167
1053.981754	38.275403	49.253172
1050.045205	54.846698	49.258177
1046.909595	41.138645	49.263181
1043.732148	46.625444	49.268186
1039.765757	40.624713	49.273191
1036.343948	40.834631	49.278196
1032.873896	40.783183	49.283201
1029.624094	39.029943	49.288205
1026.078683	34.523048	49.293210
1022.198193	34.349204	49.298215
1019.098384	42.465603	49.303220
1015.415968	35.123276	49.308225
1012.164308	39.375174	49.313229
1008.447865	50.410213	49.318234
1004.805498	40.843811	49.323239
1001.676508	37.698587	49.328244
997.501957	46.378741	49.333249
994.052657	44.909850	49.338253
990.996323	46.574845	49.343258
987.568961	43.204258	49.348263
984.241828	35.755696	49.353268
980.337471	47.066938	49.358273
976.831194	33.613114	49.363277
973.623744	30.749107	49.368282
969.790888	28.150705	49.373287
966.460714	29.099278	49.378292
962.655608	48.741014	49.383297
959.230377	42.513217	49.388301
955.651981	47.521815	49.393306
952.581151	35.461484	49.398311
948.956037	31.729570	49.403316
945.259659	41.562412	49.408321
942.123973	47.223035	49.413325
938.776975	48.319786	49.418330
934.834145	45.839856	49.423335
931.216709	45.900108	49.428340
927.919561	51.358227	49.433345
924.179681	40.978224	49.438349
921.056728	42.058881	49.443354
917.819674	51.149095	49.448359
914.003674	39.360482	49.453364
910.300140	51.462883	49.458369
906.691275	52.910699	49.463373
903.237976	45.374353	49.468378
899.315404	44.659816	49.473383
896.278193	46.688843	49.478388
892.861656	43.857603	49.483393
889.349947	46.935372	49.488397
885.992460	40.241416	49.493402
882.473518	48.132415	49.498407
878.854538	41.567993	49.503412
875.106880	43.860133	49.508417
871.403254	53.507476	49.513421
867.969367	45.151853	49.518426
864.685539	43.486258	49.523431
861.511486	40.028599	49.528436
857.927676	46.044156	49.533441
854.344843	42.492322	49.538445
851.041824	45.467823	49.543450
847.347056	44.961246	49.548455
844.176241	37.731875	49.553460
840.230805	44.003381	49.558465
836.717708	38.384185	49.563469
833.185876	37.459793	49.568474
829.629452	44.129134	49.573479
826.329471	43.355101	49.578484
822.652946	40.400085	49.583489
819.391757	49.142925	49.588493
816.038687	35.769592	49.593498
812.068542	37.748580	49.598503
808.684867	37.671034	49.603508
804.860844	45.913551	49.608513
801.738986	38.882175	49.613517
798.121730	39.989657	49.618522
794.349975	45.582247	49.623527
791.112486	38.385484	49.628532
788.076863	43.131971	49.633537
784.394209	48.264522	49.638541
781.045571	43.122633	49.643546
777.021963	39.279185	49.648551
773.562547	33.449130	49.653556
770.174909	36.596096	49.658561
766.564964	37.778376	49.663565
763.500073	34.531452	49.668570
759.764676	41.380702	49.673575
756.217091	39.240757	49.678580
752.877597	45.569267	49.683585
749.259664	37.995498	49.688589
745.750647	37.336488	49.693594
742.209588	43.066976	49.698599
738.712713	41.156379	49.703604
735.436735	43.985314	49.708609
731.163035	38.830124	49.713613
727.689236	43.170682	49.718618
724.938762	42.222047	49.723623
721.424065	33.584920	49.728628
717.484689	46.812643	49.733633
714.449975	42.330304	49.738637
710.652134	38.600228	49.743642
706.644857	43.647600	49.748647
703.714210	31.862820	49.753652
699.536004	41.027709	49.758657
696.318495	39.098689	49.763661
693.440688	37.765043	49.768666
689.950246	47.280977	49.773671
686.567568	40.796694	49.778676
682.628853	40.986451	49.783681
679.099163	43.004084	49.788685
675.714246	38.364633	49.793690
671.628454	43.940008	49.798695
668.420501	44.224136	49.803700
665.021917	45.370190	49.808705
661.656429	38.664927	49.813709
658.033269	38.450934	49.818714
654.657445	42.345902	49.823719
651.125906	38.324211	49.828724
647.624365	42.748235	49.833729
644.423601	36.526549	49.838733
640.965188	43.658330	49.843738
637.105958	44.167853	49.848743
633.727324	41.726249	49.853748
630.506789	38.981477	49.858753
626.521016	32.851103	49.863757
622.508233	32.356458	49.868762
619.066559	45.015881	49.873767
616.001988	26.817022	49.878772
612.490328	38.769229	49.883777
609.160622	34.902609	49.888781
605.999544	33.686122	49.893786
602.440570	38.172940	49.898791
598.733847	35.659348	49.903796
594.912217	36.511014	49.908801
591.364210	33.210102	49.913805
588.096582	28.751637	49.918810
584.116083	39.356753	49.923815
581.044092	34.301335	49.928820
577.498115	42.259936	49.933825
574.153297	44.678926	49.938829
570.608993	32.790995	49.943834
566.716638	52.712249	49.948839
563.506191	29.198993	49.953844
559.992934	35.700307	49.958849
556.431790	44.907813	49.963853
552.930097	42.491842	49.968858
549.243942	39.152472	49.973863
546.289453	41.535647	49.978868
542.531516	42.874070	49.983873
538.969268	38.388999	49.988877
535.877962	44.609101	49.993882
531.596222	43.390991	49.998887
528.100239	39.892130	50.003892
524.721590	52.402506	50.008897
521.630383	40.627126	50.013901
518.100579	43.723679	50.018906
514.446246	48.041968	50.023911
510.856009	40.878423	50.028916
507.523632	43.877619	50.033921
504.014274	34.284300	50.038925
500.453160	48.044469	50.043930
496.836877	50.553461	50.048935
493.414470	36.814656	50.053940
490.000759	36.928593	50.058945
486.767685	47.245837	50.063949
482.875834	37.933898	50.068954
479.214128	45.005823	50.073959
476.084186	27.573411	50.078964
472.399981	36.540786	50.083969
468.567005	35.401114	50.088973
465.600993	33.220817	50.093978
461.345998	47.485148	50.098983
458.337998	34.206638	50.103988
454.760807	38.000334	50.108993
451.263623	35.577373	50.113997
447.920431	38.204959	50.119002
444.682424	41.325436	50.124007
441.364143	32.771569	50.129012
437.672938	36.877360	50.134017
434.017501	40.620045	50.139021
430.704822	38.823090	50.144026
426.869254	34.422009	50.149031
423.354056	22.248025	50.154036
419.314316	37.870699	50.159041
416.076212	26.899833	50.164045
413.050278	33.511525	50.169050
409.417798	31.530553	50.174055
406.043622	33.191733	50.179060
402.520753	39.476308	50.184065
398.670104	37.811087	50.189069
395.245578	32.624300	50.194074
391.273243	38.612286	50.199079
388.239975	40.280186	50.204084
384.806431	40.194790	50.209089
381.662534	39.124389	50.214093
377.953833	29.214345	50.219098
374.087556	38.539304	50.224103
371.158309	38.007924	50.229108
367.645261	38.140632	50.234113
363.640892	36.173639	50.239117
360.050753	32.876261	50.244122
356.390505	35.857264	50.249127
352.995838	31.434611	50.254132
349.982254	30.967070	50.259137
346.013982	36.685517	50.264141
342.898927	33.886367	50.269146
339.349627	35.692064	50.274151
335.926229	30.128640	50.279156
332.476951	35.477893	50.284161
328.858470	36.183953	50.289165
325.460680	26.316983	50.294170
321.625272	33.688251	50.299175
318.286634	32.524993	50.304180
314.714380	32.455026	50.309185
310.936723	32.626043	50.314189
307.815402	28.904073	50.319194
304.283801	35.626645	50.324199
300.997582	28.013783	50.329204
297.268705	26.158691	50.334209
293.433336	34.782810	50.339213
290.562892	37.668590	50.344218
286.797011	38.603401	50.349223
283.521579	25.233992	50.354228
279.477925	36.912126	50.359233
276.073863	36.607019	50.364237
272.935649	27.914291	50.369242
269.092774	44.581855	50.374247
265.678572	32.762281	50.379252
262.262287	37.663465	50.384257
258.434585	35.985222	50.389261
255.349611	39.951821	50.394266
251.454020	45.257126	50.399271
248.226966	34.955317	50.404276
244.484288	39.584937	50.409281
241.173627	40.657262	50.414285
237.967063	38.812120	50.419290
233.904455	38.635504	50.424295
230.895411	34.082890	50.429300
227.290017	39.855270	50.434305
223.346721	42.238425	50.439309
219.879846	40.063911	50.444314
216.420674	44.471958	50.449319
213.048876	38.239278	50.454324
209.428779	43.216703	50.459329
206.449166	39.940806	50.464333
203.284630	41.360412	50.469338
199.132777	42.162737	50.474343
195.408728	29.657750	50.479348
192.267737	34.076069	50.484353
189.036927	27.482795	50.489357
185.487288	30.041575	50.494362
181.579263	37.746976	50.499367
178.527711	35.191040	50.504372
174.533923	33.826755	50.509377
170.818804	33.560929	50.514381
167.291168	30.288645	50.519386
163.702721	36.260872	50.524391
160.588999	37.106221	50.529396
157.441748	35.463789	50.534401
153.776442	40.590686	50.539405
150.010775	36.795716	50.544410
146.391617	33.907937	50.549415
142.796616	30.196966	50.554420
139.516890	33.317754	50.559425
136.433478	34.107743	50.564429
132.953318	29.923204	50.569434
128.709417	40.019256	50.574439
125.607440	34.576410	50.579444
122.192795	37.949296	50.584449
118.739781	27.553238	50.589453
115.367303	31.033414	50.594458
111.750762	27.645370	50.599463
108.311688	32.164200	50.604468
104.607119	28.998757	50.609473
100.540903	35.026876	50.614477
97.434406	32.682059	50.619482
94.087086	36.294343	50.624487
90.721600	29.870906	50.629492
86.894150	33.226222	50.634497
83.666259	25.841600	50.639501
79.999686	24.106557	50.644506
76.392123	30.872745	50.649511
73.002187	29.417065	50.654516
69.050282	37.565980	50.659521
65.964493	31.453072	50.664525
62.547010	30.843268	50.669530
58.988470	30.391607	50.674535
55.571265	25.618275	50.679540
52.278929	29.740812	50.684545
48.640767	36.211250	50.689549
45.023438	23.639008	50.694554
40.934362	28.873469	50.699559
37.858429	35.221020	50.704564
34.698784	36.696866	50.709569
31.421447	39.807828	50.714573
27.641625	30.367849	50.719578
23.886903	32.550702	50.724583
20.430674	27.422832	50.729588
16.848521	26.297847	50.734593
13.200041	27.983169	50.739597
10.155283	35.398353	50.744602
6.229402	38.417950	50.749607
3.144957	25.863475	50.754612