Thu Aug 25 10:37:08 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.729414	94.083861	0.000000
0.527757	98.826347	0.005005
0.464945	80.458002	0.010010
0.609760	79.770983	0.015014
0.252862	75.324943	0.020019
0.320842	72.220202	0.025024
-0.082786	70.239719	0.030029
-0.241690	56.065770	0.035034
-0.472597	41.159634	0.040038
-0.762561	54.227104	0.045043
-1.233084	38.947226	0.050048
-1.524796	42.023858	0.055053
-1.822835	30.564077	0.060058
-2.130374	19.906218	0.065062
-2.623296	20.739643	0.070067
-2.553737	12.762504	0.075072
-2.732644	9.266188	0.080077
-3.283977	5.739641	0.085082
-3.514494	5.048158	0.090086
-3.867549	1.069768	0.095091
-3.597314	-1.028944	0.100096
-4.447093	-2.018867	0.105101
-4.578843	-4.975242	0.110106
-4.752728	-6.735450	0.115110
-4.759907	1.089656	0.120115
-5.217563	-2.862853	0.125120
-6.019537	-3.528073	0.130125
-6.327486	-12.711546	0.135130
-6.460522	-12.665333	0.140134
-6.624626	2.413497	0.145139
-6.188938	-9.869898	0.150144
-6.294440	-6.869906	0.155149
-6.908194	-4.147781	0.160154
-7.600210	-11.682882	0.165158
-7.743120	1.690537	0.170163
-7.757999	-10.411530	0.175168
-7.758727	-5.852414	0.180173
-8.872254	-15.419026	0.185178
-8.893885	-2.026648	0.190182
-8.997946	-4.901940	0.195187
-9.238466	-8.268376	0.200192
-9.441644	-9.027417	0.205197
-9.120858	-1.339121	0.210202
-9.859579	-17.573503	0.215206
-10.427749	-5.797584	0.220211
-10.460654	-9.892571	0.225216
-10.541623	-0.929616	0.230221
-11.051112	-2.244937	0.235226
-10.723145	-7.747383	0.240230
-11.776005	-5.443673	0.245235
-12.024422	-6.711315	0.250240
-12.040915	2.187756	0.255245
-12.346869	8.303803	0.260250
-12.440862	-0.682246	0.265254
-12.302221	1.431612	0.270259
-12.783743	-0.141190	0.275264
-13.521322	-1.503030	0.280269
-13.843183	0.034416	0.285274
-13.562841	-7.425249	0.290278
-13.979859	-5.904532	0.295283
-13.798080	-1.218988	0.300288
-13.958565	-5.676799	0.305293
-15.138569	-1.252445	0.310298
-14.555345	-7.414979	0.315302
-15.464677	4.072718	0.320307
-15.311801	0.407361	0.325312
-15.366788	-0.308460	0.330317
-16.108084	5.568914	0.335322
-16.196287	-17.132834	0.340326
-16.609056	0.202733	0.345331
-16.625978	-10.165285	0.350336
-16.944384	0.530636	0.355341
-17.089623	-4.011822	0.360346
-17.448384	-9.159897	0.365350
-18.175996	-1.411737	0.370355
-17.958093	-7.216476	0.375360
-18.285417	-8.867221	0.380365
-18.410930	-10.147791	0.385370
-18.067736	-1.918845	0.390374
-18.770648	-5.136902	0.395379
-19.478339	-6.712230	0.400384
-19.295735	-7.860745	0.405389
-19.705677	-0.450259	0.410394
-19.308792	-11.294399	0.415398
-20.577021	0.942387	0.420403
-20.704209	-2.979642	0.425408
-20.926918	-13.786810	0.430413
-20.990826	-0.080926	0.435418
-20.768298	-7.113919	0.440422
-20.867285	2.247328	0.445427
-21.290452	-4.776244	0.450432
-21.708957	-9.237918	0.455437
-22.298127	-4.630895	0.460442
-22.298645	-13.122221	0.465446
-23.432810	-5.006644	0.470451
-23.438067	-4.983615	0.475456
-23.451400	-0.799008	0.480461
-23.695561	-0.593015	0.485466
-23.242487	-11.224497	0.490470
-23.740270	3.830685	0.495475
-23.878112	1.738964	0.500480
-23.851193	0.564222	0.505485
-24.906313	0.894117	0.510490
-24.887063	-1.854965	0.515494
-25.188138	6.639447	0.520499
-25.503838	-1.321612	0.525504
-25.974731	1.283218	0.530509
-26.233916	-5.921070	0.535514
-26.631777	-6.905869	0.540518
-26.632581	1.550983	0.545523
-26.719162	-3.082922	0.550528
-26.714912	-6.019476	0.555533
-26.819928	-4.718486	0.560538
-27.417697	-4.824081	0.565542
-28.047351	-2.918872	0.570547
-27.984525	-5.048360	0.575552
-28.116954	3.660069	0.580557
-28.021370	0.133403	0.585562
-28.414310	-8.546374	0.590566
-29.321079	3.728692	0.595571
-29.617499	2.927313	0.600576
-29.593775	0.326226	0.605581
-29.941834	6.898120	0.610586
-29.656060	-1.305877	0.615590
-30.059810	-2.273934	0.620595
-30.675775	-3.003098	0.625600
-30.969635	-3.567597	0.630605
-31.653160	8.055564	0.635610
-31.336564	5.101705	0.640614
-31.428880	9.374620	0.645619
-31.469902	-0.315750	0.650624
-31.221606	2.423165	0.655629
-31.847465	-2.594476	0.660634
-32.197543	0.209722	0.665638
-32.937624	0.575676	0.670643
-32.746879	-4.465511	0.675648
-33.275225	-11.510563	0.680653
-33.932680	-3.415895	0.685658
-33.938584	-14.408891	0.690662
-34.090113	-6.880711	0.695667
-33.836123	-3.225205	0.700672
-34.037349	-12.545619	0.705677
-34.223628	0.581492	0.710682
-35.217132	-10.136541	0.715686
-35.537866	1.423444	0.720691
-36.058210	-3.949249	0.725696
-35.759123	-7.757735	0.730701
-35.624441	-5.893193	0.735706
-35.937928	-6.793136	0.740710
-36.404434	-13.018978	0.745715
-36.585418	-14.116851	0.750720
-37.147307	-8.106241	0.755725
-37.093620	-7.162310	0.760730
-37.562851	-7.076074	0.765734
-38.488373	-4.197531	0.770739
-38.463065	-12.215179	0.775744
-38.657312	-10.223169	0.780749
-38.883661	-9.852289	0.785754
-38.437099	-9.672266	0.790758
-38.852215	-3.282857	0.795763
-38.755737	-11.071213	0.800768
-39.057233	-8.863083	0.805773
-39.565149	-7.710934	0.810778
-39.707418	-12.807507	0.815782
-40.158150	-10.639269	0.820787
-40.387209	-12.337046	0.825792
-40.785685	-6.681068	0.830797
-41.391589	1.756700	0.835802
-41.103265	-3.552876	0.840806
-41.468877	1.987225	0.845811
-41.419384	-4.094845	0.850816
-42.130298	-4.942008	0.855821
-42.660520	0.057576	0.860826
-42.283929	-3.794692	0.865830
-42.659805	-9.082452	0.870835
-42.941250	-7.146381	0.875840
-42.742128	-9.053617	0.880845
-43.912577	-1.549280	0.885850
-44.049718	10.184422	0.890854
-44.099643	6.746993	0.895859
-44.096083	-7.759238	0.900864
-44.183958	3.482689	0.905869
-44.708012	4.184953	0.910874
-44.974686	2.806278	0.915878
-45.705434	1.304166	0.920883
-45.530686	-5.268926	0.925888
-45.515357	-4.353786	0.930893
-45.739116	3.267972	0.935898
-46.021063	-5.128640	0.940902
-46.498054	-2.000838	0.945907
-47.135266	-5.510758	0.950912
-47.353656	1.224312	0.955917
-47.454980	3.619377	0.960922
-47.202351	-9.733149	0.965926
-47.473299	0.224511	0.970931
-48.502065	2.160621	0.975936
-48.185607	-5.602094	0.980941
-48.827720	7.229452	0.985946
-48.702737	-12.092026	0.990950
-48.868793	-1.815447	0.995955
-48.826802	-15.910079	1.000960
-49.691627	-10.804286	1.005965
-50.139400	-0.486728	1.010970
-50.390527	-7.470814	1.015974
-50.308665	-5.196202	1.020979
-50.406797	-5.437030	1.025984
-50.294206	-10.893073	1.030989
-50.931747	3.298159	1.035994
-51.233095	-10.483253	1.040998
-51.474711	-4.807561	1.046003
-52.094603	-7.497623	1.051008
-51.739657	-11.121873	1.056013
-52.422077	-0.169603	1.061018
-52.804653	-5.393038	1.066022
-53.185497	-6.374174	1.071027
-53.252293	-2.605132	1.076032
-53.161538	-9.022694	1.081037
-53.434789	-1.503913	1.086042
-53.458597	-5.476940	1.091046
-53.772319	-10.021468	1.096051
-54.555312	-7.462648	1.101056
-54.410089	-4.233024	1.106061
-54.871029	4.507896	1.111066
-54.372113	5.217550	1.116070
-55.171538	2.865664	1.121075
-55.646440	-7.342007	1.126080
-56.199158	-7.470478	1.131085
-56.580264	-1.383788	1.136090
-56.228645	-3.080803	1.141094
-56.188698	-0.245969	1.146099
-56.061093	-1.490271	1.151104
-56.851597	-2.192084	1.156109
-57.147314	1.359730	1.161114
-57.155381	-11.297053	1.166118
-58.088666	3.124015	1.171123
-58.499721	4.472959	1.176128
-58.558733	-6.467426	1.181133
-58.940421	-0.171839	1.186138
-58.852351	-7.110996	1.191142
-59.062315	1.742456	1.196147
-59.260438	0.612467	1.201152
-59.120221	-3.598231	1.206157
-59.583280	-9.647443	1.211162
-60.021531	-10.515181	1.216166
-60.237073	-11.158388	1.221171
-60.344007	-1.596586	1.226176
-60.661035	-6.248163	1.231181
-61.267359	6.473370	1.236186
-61.849643	-2.875923	1.241190
-62.248900	0.685787	1.246195
-62.331318	-5.071894	1.251200
-61.697127	-5.256627	1.256205
-62.035465	1.573167	1.261210
-61.889744	-5.729363	1.266214
-62.770659	8.664521	1.271219
-63.388330	1.070318	1.276224
-63.320497	-12.272231	1.281229
-63.672274	-4.244442	1.286234
-63.565659	3.948806	1.291238
-63.431035	-1.067769	1.296243
-64.634462	-2.695130	1.301248
-64.787723	-1.500475	1.306253
-65.192953	-2.034867	1.311258
-65.216138	-1.898299	1.316262
-64.853236	-1.471052	1.321267
-65.279919	-7.364613	1.326272
-65.627311	-7.348087	1.331277
-66.239292	-2.867200	1.336282
-66.353818	-4.013451	1.341286
-66.783179	-4.113794	1.346291
-66.809558	-11.822787	1.351296
-66.710540	-7.595676	1.356301
-67.935616	-8.156629	1.361306
-67.680714	-3.099734	1.366310
-67.971530	-1.719011	1.371315
-68.698739	-2.095385	1.376320
-68.279737	-13.499804	1.381325
-68.460253	0.686252	1.386330
-68.036945	-10.124062	1.391334
-68.239383	-10.310581	1.396339
-69.140677	3.055115	1.401344
-69.078252	1.381267	1.406349
-69.954775	-1.183162	1.411354
-70.297493	-5.470048	1.416358
-70.492890	-8.603107	1.421363
-70.727102	1.896122	1.426368
-70.548677	-12.716594	1.431373
-70.929511	-2.517093	1.436378
-71.053403	-6.971143	1.441382
-71.563847	-0.807241	1.446387
-71.799653	5.392725	1.451392
-71.758758	-0.846185	1.456397
-72.364452	4.801137	1.461402
-72.751291	-5.515243	1.466406
-73.271344	-3.026095	1.471411
-73.782740	-4.790363	1.476416
-73.483939	-11.781520	1.481421
-73.922852	-2.806776	1.486426
-73.943260	-9.827010	1.491430
-73.848531	-2.274142	1.496435
-73.791167	-5.494262	1.501440
-74.112455	-6.396145	1.506445
-74.751363	3.302798	1.511450
-75.033303	-6.090389	1.516454
-75.184821	-5.582537	1.521459
-75.433559	-0.797901	1.526464
-76.309016	9.437980	1.531469
-76.905413	6.364588	1.536474
-76.883316	-1.339349	1.541478
-76.817272	4.617166	1.546483
-76.541432	4.263957	1.551488
-76.375963	-9.166657	1.556493
-76.883574	1.524106	1.561498
-77.554091	-3.980074	1.566502
-77.636626	2.069324	1.571507
-78.086909	0.415702	1.576512
-78.133873	-3.145574	1.581517
-78.693833	1.282870	1.586522
-79.178513	0.368625	1.591526
-79.248523	4.055915	1.596531
-79.500485	-3.427910	1.601536
-79.641836	-7.838095	1.606541
-79.815251	-1.945299	1.611546
-79.983599	1.624522	1.616550
-79.843908	0.897179	1.621555
-80.843885	-5.599410	1.626560
-80.705834	-8.825845	1.631565
-81.111287	-1.248386	1.636570
-81.278371	-4.483958	1.641574
-80.928689	-1.007963	1.646579
-81.581194	4.149987	1.651584
-82.310421	-4.714371	1.656589
-82.443716	2.162388	1.661594
-82.513393	5.719912	1.666598
-83.322358	5.134888	1.671603
-83.792995	0.769970	1.676608
-83.190613	-4.747001	1.681613
-83.802604	-2.271920	1.686618
-83.871407	-7.095267	1.691622
-83.933420	-10.410576	1.696627
-84.123054	-5.995868	1.701632
-84.038875	-6.992921	1.706637
-84.897995	-3.776768	1.711642
-85.183818	-2.697382	1.716646
-85.452189	1.144375	1.721651
-85.582194	5.189076	1.726656
-85.781173	-11.936621	1.731661
-86.490300	6.018017	1.736666
-86.690065	4.271357	1.741670
-86.717677	3.313967	1.746675
-87.027712	-2.607363	1.751680
-86.910547	-5.697650	1.756685
-87.424765	-3.778887	1.761690
-87.139204	-1.238803	1.766694
-88.049131	1.751196	1.771699
-88.617511	4.886993	1.776704
-88.615002	3.611673	1.781709
-88.999200	3.491600	1.786714
-88.859182	-2.076309	1.791718
-88.635218	1.451021	1.796723
-89.045822	1.496436	1.801728
-89.767645	-2.322924	1.806733
-90.216067	5.628264	1.811738
-89.893295	-0.882601	1.816742
-90.259753	1.614119	1.821747
-90.343179	-1.672526	1.826752
-90.485732	-9.012140	1.831757
-91.622752	-1.010004	1.836762
-91.410419	-8.253367	1.841766
-91.784339	-12.548015	1.846771
-91.953051	-2.986027	1.851776
-91.798057	-1.377768	1.856781
-92.129497	-1.496616	1.861786
-93.040315	2.572356	1.866790
-93.230817	4.462542	1.871795
-93.135766	9.639398	1.876800
-93.203478	1.677451	1.881805
-93.187680	13.630795	1.886810
-93.903901	5.915995	1.891814
-94.096762	1.931493	1.896819
-94.685616	7.958990	1.901824
-94.532231	11.282247	1.906829
-94.721643	2.861646	1.911834
-94.856431	3.752852	1.916838
-95.126232	2.349359	1.921843
-95.850567	-3.674729	1.926848
-96.251505	1.358381	1.931853
-96.517000	1.941040	1.936858
-96.587896	-4.786548	1.941862
-96.380399	0.198680	1.946867
-97.047212	1.442169	1.951872
-97.315924	2.575822	1.956877
-97.488051	7.848325	1.961882
-97.790647	-0.396352	1.966886
-97.814541	11.009555	1.971891
-97.883240	17.009333	1.976896
-97.686606	4.984853	1.981901
-98.481052	10.908525	1.986906
-98.949500	5.236641	1.991910
-98.826652	0.076381	1.996915
-99.272314	0.992437	2.006912
-99.534733	0.745405	2.016909
-99.245548	9.693555	2.026906
-98.248951	2.387816	2.036902
-97.679451	4.398939	2.046899
-97.037931	7.222401	2.056896
-96.851347	9.353712	2.066893
-95.588887	3.042181	2.076890
-95.607992	5.570018	2.086886
-95.420409	0.776391	2.096883
-94.956915	3.428178	2.106880
-93.784588	-2.479590	2.116877
-93.880592	-3.329235	2.126874
-93.181821	-3.340409	2.136870
-92.772820	2.132910	2.146867
-92.181325	6.041258	2.156864
-91.513042	3.804740	2.166861
-91.013934	2.104743	2.176858
-90.824003	-0.196203	2.186854
-89.926769	-0.900542	2.196851
-89.828907	0.509744	2.206848
-89.277638	-1.359982	2.216845
-88.359164	-3.065501	2.226842
-88.277308	-5.105593	2.236838
-87.843687	-4.492347	2.246835
-86.777396	-8.137538	2.256832
-86.919396	2.104106	2.266829
-86.280300	1.490900	2.276826
-85.345699	-0.831697	2.286822
-85.339332	2.392229	2.296819
-84.653539	-0.851221	2.306816
-84.055792	0.354027	2.316813
-83.796873	4.308152	2.326810
-82.666739	-0.329057	2.336806
-82.316276	5.476551	2.346803
-82.421129	-2.974396	2.356800
-81.987813	10.059790	2.366797
-81.248732	3.446967	2.376794
-80.709926	-1.198954	2.386790
-79.806544	-1.353061	2.396787
-79.529336	-1.928568	2.406784
-79.381980	-3.167970	2.416781
-78.705359	3.939176	2.426778
-78.458864	-1.639790	2.436774
-77.249658	0.438991	2.446771
-77.036536	4.713903	2.456768
-76.948554	-5.281460	2.466765
-75.860274	0.256483	2.476762
-75.274171	1.983073	2.486758
-75.410080	0.024619	2.496755
-74.620483	4.937794	2.506752
-74.230052	0.270772	2.516749
-73.578280	2.573113	2.526746
-72.977111	6.647840	2.536742
-72.410837	4.652219	2.546739
-72.287282	-4.157631	2.556736
-71.317901	1.139185	2.566733
-71.021378	-5.036826	2.576730
-70.840886	-1.814842	2.586726
-70.279358	1.515330	2.596723
-69.544393	5.474060	2.606720
-69.112258	-3.285942	2.616717
-68.395564	0.042093	2.626714
-68.446063	-3.871597	2.636710
-67.649163	-1.075648	2.646707
-66.893618	-3.110428	2.656704
-67.031823	0.798219	2.666701
-65.778764	-0.674624	2.676698
-65.356176	0.887520	2.686694
-65.273037	-1.770492	2.696691
-64.614545	0.226689	2.706688
-64.230419	6.280447	2.716685
-63.674030	-0.753574	2.726682
-62.667658	3.945073	2.736678
-62.587980	7.033969	2.746675
-62.375233	0.091807	2.756672
-61.364277	-6.294350	2.766669
-61.196951	-5.975163	2.776666
-60.838681	-3.059800	2.786662
-60.181803	-0.913480	2.796659
-59.389547	-4.192616	2.806656
-58.912378	1.827556	2.816653
-58.739583	1.499658	2.826650
-58.125102	-8.419813	2.836646
-57.325368	-6.704522	2.846643
-57.075715	-4.076247	2.856640
-56.879705	-1.645473	2.866637
-55.801766	1.337692	2.876634
-55.311376	-2.993368	2.886630
-55.339400	0.216940	2.896627
-54.526468	-3.651476	2.906624
-54.106556	1.063036	2.916621
-53.716762	0.431875	2.926618
-52.740827	-5.153680	2.936614
-52.364675	-0.676231	2.946611
-52.392070	-0.332868	2.956608
-51.270122	1.164045	2.966605
-51.035452	-1.805979	2.976602
-50.777740	-1.884256	2.986598
-50.023834	3.886649	2.996595
-49.646056	2.443250	3.006592
-48.911919	-2.283961	3.016589
-48.033107	-5.830082	3.026586
-47.804072	2.370394	3.036582
-47.966283	-0.927081	3.046579
-47.275012	-8.321187	3.056576
-46.741974	-0.168345	3.066573
-45.930363	-7.644663	3.076570
-45.318069	-8.393048	3.086566
-45.281758	-5.576123	3.096563
-44.303760	-4.911957	3.106560
-43.701451	-6.469732	3.116557
-43.861011	-9.396990	3.126554
-42.981965	-7.361507	3.136550
-42.265317	-5.997492	3.146547
-41.986234	-7.425426	3.156544
-41.704181	-5.470630	3.166541
-40.990626	-10.020386	3.176538
-40.628571	-11.169884	3.186534
-39.801575	-9.281467	3.196531
-39.433460	-3.149174	3.206528
-39.500564	-6.125766	3.216525
-38.631867	-10.683991	3.226522
-37.947888	-8.678132	3.236518
-37.453665	-7.830459	3.246515
-36.489332	-9.121843	3.256512
-36.513817	-4.958586	3.266509
-36.396576	-7.419203	3.276506
-35.396903	-4.680364	3.286502
-35.064541	-5.369049	3.296499
-34.457025	-1.418857	3.306496
-33.728895	3.304384	3.316493
-33.371829	-9.273709	3.326490
-33.276070	3.366714	3.336486
-32.522393	-3.767909	3.346483
-31.705208	-5.875701	3.356480
-31.792037	1.119825	3.366477
-30.968172	-7.375272	3.376474
-30.450005	1.353272	3.386470
-30.100098	1.067315	3.396467
-29.093019	-4.510448	3.406464
-29.015624	0.172204	3.416461
-28.737126	-2.085599	3.426458
-27.852886	-8.908060	3.436454
-27.172599	-0.512194	3.446451
-27.064392	3.636610	3.456448
-26.590802	6.150606	3.466445
-26.212063	-1.194533	3.476442
-25.470599	-7.107643	3.486438
-24.493283	0.373710	3.496435
-23.992922	-7.018992	3.506432
-24.182267	-5.284939	3.516429
-24.154910	-2.023119	3.526426
-23.285473	0.010704	3.536422
-22.721482	-2.481898	3.546419
-21.896311	-2.471690	3.556416
-21.522179	-1.443643	3.566413
-20.342448	-4.751810	3.576410
-20.262337	-3.994473	3.586406
-20.384820	-2.980479	3.596403
-19.652340	-1.919882	3.606400
-18.730822	0.067769	3.616397
-18.666237	1.115808	3.626394
-17.666120	-7.245347	3.636390
-17.405744	-3.557542	3.646387
-17.391191	-8.982956	3.656384
-16.729193	-3.593621	3.666381
-15.799985	-6.453890	3.676378
-15.160357	-3.690313	3.686374
-14.372515	5.341270	3.696371
-14.488184	7.510440	3.706368
-14.388539	-2.391725	3.716365
-13.509713	0.033435	3.726362
-12.853132	-2.689084	3.736358
-12.529375	-4.415454	3.746355
-11.873313	-7.378643	3.756352
-11.538421	-1.253812	3.766349
-11.011276	-3.195782	3.776346
-10.319387	-3.414945	3.786342
-10.135276	6.404979	3.796339
-9.306541	5.077823	3.806336
-8.623015	-1.662506	3.816333
-8.682024	1.014134	3.826330
-8.026118	-2.468548	3.836326
-7.013382	0.059174	3.846323
-6.768797	-0.980052	3.856320
-7.042045	0.988894	3.866317
-6.182479	3.733851	3.876314
-5.318357	-2.838371	3.886310
-4.934049	11.451617	3.896307
-4.783424	18.473301	3.906304
-3.991825	29.617227	3.916301
-3.852493	31.141396	3.926298
-2.901140	40.926657	3.936294
-2.836659	44.661006	3.946291
-2.585860	54.999532	3.956288
-2.139092	76.014526	3.966285
-1.302465	80.090399	3.976282
-0.600105	97.802536	3.986278
-0.445919	111.000922	3.996275
0.000000	118.770419	4.001280
0.192093	123.944764	4.006285
0.269601	144.604696	4.011290
0.276992	141.063346	4.016294
0.716299	142.339172	4.021299
0.606705	143.023956	4.026304
0.913231	134.731223	4.031309
0.605258	137.136538	4.036314
0.422440	135.890245	4.041318
0.834798	152.096928	4.046323
0.769062	160.560868	4.051328
1.006103	149.922009	4.056333
0.994769	162.205580	4.061338
0.885232	166.414792	4.066342
0.770054	166.062737	4.071347
0.875063	167.479529	4.076352
0.919634	154.880814	4.081357
0.809932	163.275713	4.086362
0.724742	163.542221	4.091366
1.297088	159.532696	4.096371
0.983826	162.451374	4.101376
1.109944	165.114546	4.106381
1.192193	170.299787	4.111386
1.159092	167.663286	4.116390
1.090604	163.643436	4.121395
0.987988	165.788788	4.126400
1.376419	161.763787	4.131405
1.516797	165.883221	4.136410
1.151100	177.108680	4.141414
1.137862	164.079252	4.146419
1.020421	171.678099	4.151424
1.608307	164.638412	4.156429
1.292898	148.941829	4.161434
0.832011	150.137237	4.166438
1.247544	152.501960	4.171443
1.281632	164.082388	4.176448
1.585980	163.999959	4.181453
0.969717	148.995922	4.186458
1.023049	161.269361	4.191462
1.264236	164.822505	4.196467
1.236884	169.958480	4.201472
1.612704	166.533406	4.206477
1.505235	174.529325	4.211482
1.354799	168.041920	4.216486
1.244927	154.078510	4.221491
1.033586	158.705470	4.226496
1.111547	172.680328	4.231501
1.356733	160.739877	4.236506
1.389332	154.957792	4.241510
1.185557	162.222147	4.246515
1.552603	171.421879	4.251520
1.625883	168.208723	4.256525
1.291417	169.640589	4.261530
1.426616	175.981803	4.266534
1.286548	165.458969	4.271539
1.131657	172.804255	4.276544
1.135059	164.179350	4.281549
1.490519	171.713592	4.286554
1.718835	168.678626	4.291558
1.647350	164.871218	4.296563
1.357654	172.902016	4.301568
1.425103	169.787850	4.306573
1.533488	171.305354	4.311578
1.186934	169.720880	4.316582
1.587211	164.915735	4.321587
1.469727	186.305459	4.326592
1.101945	170.224756	4.331597
1.779538	174.117651	4.336602
1.422607	178.514325	4.341606
1.815139	178.282037	4.346611
1.539479	170.656312	4.351616
1.670715	170.578860	4.356621
1.736898	173.852540	4.361626
1.555806	174.931344	4.366630
1.852982	184.056608	4.371635
1.443115	187.268837	4.376640
1.648466	187.125989	4.381645
1.652998	189.944258	4.386650
1.719983	198.893624	4.391654
1.954893	195.946205	4.396659
1.783425	191.695710	4.401664
2.135488	188.467344	4.406669
1.719365	193.056795	4.411674
1.434717	183.281107	4.416678
1.903265	182.821773	4.421683
1.466298	196.554624	4.426688
1.595309	195.787819	4.431693
1.777155	196.407959	4.436698
1.714368	205.823753	4.441702
1.961433	198.907058	4.446707
1.772217	197.392842	4.451712
1.921884	193.854499	4.456717
1.694774	199.613406	4.461722
2.103648	200.954117	4.466726
2.003278	207.813145	4.471731
1.968934	205.091411	4.476736
1.966291	202.133755	4.481741
1.940282	194.946633	4.486746
1.433203	206.732103	4.491750
1.941430	190.292662	4.496755
1.669628	206.641392	4.501760
1.756438	204.631508	4.506765
2.596499	210.761054	4.511770
2.007938	205.436947	4.516774
2.011693	199.744789	4.521779
1.816914	201.863456	4.526784
2.049433	215.687580	4.531789
2.417820	214.285314	4.536794
2.102218	218.026949	4.541798
2.066845	210.085145	4.546803
2.024517	214.125649	4.551808
2.110335	217.310839	4.556813
2.298084	218.974101	4.561818
2.312204	225.097020	4.566822
2.170024	224.790323	4.571827
2.025512	234.073403	4.576832
2.436134	224.641177	4.581837
2.582981	223.317914	4.586842
1.987909	219.668462	4.591846
2.402897	208.141140	4.596851
2.531741	223.553911	4.601856
2.317834	210.397702	4.606861
1.865550	211.082397	4.611866
1.919050	223.235629	4.616870
2.234348	218.171700	4.621875
2.241750	224.668996	4.626880
2.203833	223.956819	4.631885
2.263228	235.666206	4.636890
2.379619	236.802808	4.641894
2.643165	224.761362	4.646899
2.254743	230.257649	4.651904
2.459513	221.857432	4.656909
2.547226	226.178123	4.661914
2.413952	227.758805	4.666918
2.627327	215.424667	4.671923
2.737600	234.149666	4.676928
2.523193	220.923925	4.681933
2.752251	225.614777	4.686938
2.569929	225.298550	4.691942
2.859441	219.349640	4.696947
2.310448	225.886657	4.701952
2.657061	221.143690	4.706957
2.678402	219.248466	4.711962
2.591832	218.847634	4.716966
2.588940	204.180884	4.721971
2.391693	202.455953	4.726976
2.604560	213.834394	4.731981
2.554741	215.512732	4.736986
2.598949	223.981622	4.741990
2.809479	216.267044	4.746995
2.544477	230.146985	4.752000
2.414944	228.313365	4.757005
2.671379	224.498858	4.762010
2.963638	219.479668	4.767014
3.016028	223.147827	4.772019
2.721621	229.246320	4.777024
2.750622	227.663110	4.782029
2.535041	213.785819	4.787034
2.897647	232.512409	4.792038
2.892512	227.900484	4.797043
2.581692	228.499739	4.802048
2.549440	232.086249	4.807053
2.791943	222.734149	4.812058
2.533277	225.868910	4.817062
2.716077	223.938897	4.822067
2.503354	224.902436	4.827072
2.458992	225.301753	4.832077
2.512726	220.715407	4.837082
2.590308	227.954688	4.842086
2.992308	227.632331	4.847091
2.374858	230.408853	4.852096
2.796968	239.324744	4.857101
2.828946	238.424442	4.862106
2.932303	243.574760	4.867110
3.114000	247.064475	4.872115
2.881530	249.837629	4.877120
2.955958	258.675126	4.882125
2.912674	256.489464	4.887130
2.853171	256.982905	4.892134
3.040068	249.215068	4.897139
3.030350	249.700708	4.902144
3.069844	252.396449	4.907149
3.279106	250.430649	4.912154
3.136509	249.029348	4.917158
3.097182	248.352191	4.922163
3.506019	260.266274	4.927168
3.099282	259.137314	4.932173
3.116355	245.008409	4.937178
3.449992	249.948641	4.942182
3.104045	237.509132	4.947187
2.664299	240.093296	4.952192
2.921199	247.981538	4.957197
3.221581	245.773669	4.962202
3.178764	247.150354	4.967206
3.198418	247.773762	4.972211
2.886954	249.018531	4.977216
3.101903	257.732770	4.982221
3.392687	253.738866	4.987226
2.833262	251.159508	4.992230
3.423601	244.578155	4.997235
3.100525	251.060802	5.002240
3.001936	259.495134	5.007245
2.999841	246.875192	5.012250
2.936032	252.339609	5.017254
3.034679	246.569292	5.022259
3.050835	258.468968	5.027264
3.184169	269.613131	5.032269
3.607422	277.105159	5.037274
3.293506	277.897893	5.042278
3.245611	267.379539	5.047283
3.267574	274.731959	5.052288
3.089694	277.306736	5.057293
3.465500	273.062223	5.062298
3.669141	277.842494	5.067302
3.616942	274.003567	5.072307
3.839998	274.000314	5.077312
3.013268	271.814015	5.082317
3.690639	264.602080	5.087322
3.173165	281.324733	5.092326
3.233373	271.710101	5.097331
3.228967	275.276437	5.102336
3.335375	281.391243	5.107341
3.328759	268.392340	5.112346
3.253409	287.943753	5.117350
3.326076	277.608986	5.122355
3.606911	286.018683	5.127360
3.745001	293.432010	5.132365
3.762465	293.938702	5.137370
3.629607	292.330226	5.142374
3.527105	284.822855	5.147379
3.631244	286.483404	5.152384
3.494861	297.919784	5.157389
3.914359	301.144457	5.162394
3.902082	294.543609	5.167398
3.993801	279.719602	5.172403
3.569849	285.398646	5.177408
3.486847	282.570628	5.182413
3.696568	288.039655	5.187418
3.568186	298.462369	5.192422
3.935436	285.850969	5.197427
3.954541	293.994791	5.202432
3.836569	293.231878	5.207437
3.864212	283.230033	5.212442
3.808906	282.394026	5.217446
3.782752	282.562699	5.222451
4.029983	295.875210	5.227456
3.883007	281.604299	5.232461
3.406566	281.349973	5.237466
3.563266	299.719750	5.242470
4.100011	293.273329	5.247475
4.021588	304.412727	5.252480
3.863928	300.590317	5.257485
4.453166	296.647720	5.262490
3.777398	299.572596	5.267494
3.981659	288.125697	5.272499
4.281529	283.304615	5.277504
3.922754	289.454344	5.282509
4.155698	267.961100	5.287514
3.636315	288.069308	5.292518
3.868708	295.727291	5.297523
4.055821	301.876915	5.302528
3.733907	307.318513	5.307533
4.297520	295.312263	5.312538
3.944956	306.595856	5.317542
4.029762	296.819167	5.322547
3.961307	305.365860	5.327552
4.322208	302.028520	5.332557
4.227535	299.417466	5.337562
3.839220	299.339159	5.342566
4.011934	300.457449	5.347571
4.166869	303.514765	5.352576
3.835177	309.454611	5.357581
4.195934	298.483064	5.362586
4.207776	306.593228	5.367590
4.168463	305.030206	5.372595
4.392598	297.088832	5.377600
4.273763	306.402729	5.382605
4.615955	298.088513	5.387610
4.496719	302.422665	5.392614
4.470386	298.453128	5.397619
4.711480	292.565563	5.402624
4.287048	303.483924	5.407629
4.305262	294.353593	5.412634
4.035595	301.928889	5.417638
4.271246	293.865488	5.422643
4.369631	303.822400	5.427648
4.251873	305.628452	5.432653
4.537567	299.613673	5.437658
4.383432	305.443439	5.442662
4.393144	302.183270	5.447667
4.276975	304.666124	5.452672
4.013428	303.641278	5.457677
4.108695	302.275471	5.462682
3.757012	305.374199	5.467686
3.883049	295.572068	5.472691
4.419089	301.670186	5.477696
4.166389	317.278862	5.482701
4.725764	323.385986	5.487706
4.632545	325.362203	5.492710
4.784967	323.383155	5.497715
4.264213	317.111907	5.502720
4.512054	323.422868	5.507725
4.815157	323.059057	5.512730
4.402878	322.089151	5.517734
4.762305	328.338338	5.522739
4.777446	312.934672	5.527744
4.382945	307.456741	5.532749
4.485319	305.368476	5.537754
4.440572	322.380935	5.542758
4.478465	322.498444	5.547763
4.864228	325.323442	5.552768
4.509954	326.964070	5.557773
4.751063	324.686384	5.562778
4.785833	330.834578	5.567782
4.678193	329.105086	5.572787
4.652763	330.396794	5.577792
4.660361	332.221173	5.582797
4.817342	333.971525	5.587802
4.373699	334.278379	5.592806
4.658126	330.797990	5.597811
5.045178	329.332679	5.602816
4.929783	341.828835	5.607821
4.797517	340.745451	5.612826
4.671409	340.195785	5.617830
4.923957	335.382103	5.622835
5.156836	322.586084	5.627840
4.750798	332.685322	5.632845
5.007455	321.581374	5.637850
4.938763	323.749903	5.642854
4.823560	327.937894	5.647859
5.196832	330.268134	5.652864
5.206035	335.518653	5.657869
4.885432	327.627815	5.662874
4.851967	328.715135	5.667878
5.025410	331.374082	5.672883
4.879907	331.713317	5.677888
4.310535	325.468667	5.682893
5.190107	330.750495	5.687898
4.742233	327.527215	5.692902
4.649906	323.650271	5.697907
5.021173	331.700968	5.702912
4.594166	335.134210	5.707917
4.661963	328.973226	5.712922
4.765297	333.313642	5.717926
4.803732	340.698309	5.722931
5.310369	346.298005	5.727936
5.139267	350.516907	5.732941
5.437639	346.768571	5.737946
5.199697	341.421125	5.742950
5.200708	341.003404	5.747955
4.850827	336.426482	5.752960
5.202102	353.199748	5.757965
5.192489	352.404036	5.762970
5.271546	357.767005	5.767974
5.294987	354.457219	5.772979
5.202401	343.388994	5.777984
5.133518	338.015061	5.782989
5.395185	335.091901	5.787994
5.162257	342.414682	5.792998
5.495453	359.589425	5.798003
5.463091	340.485204	5.803008
5.117657	338.574667	5.808013
5.422981	324.992165	5.813018
4.954254	322.148646	5.818022
5.397119	342.454166	5.823027
5.712440	346.346913	5.828032
5.211718	336.832789	5.833037
5.274426	332.713250	5.838042
5.166922	342.060191	5.843046
5.413599	354.556574	5.848051
5.640360	353.356824	5.853056
5.654118	359.989218	5.858061
5.410792	348.710487	5.863066
5.393461	336.586421	5.868070
5.417320	340.360316	5.873075
5.685305	352.638220	5.878080
5.270727	351.978725	5.883085
5.503083	349.224674	5.888090
5.621631	355.470482	5.893094
5.065328	351.988937	5.898099
5.527541	357.579778	5.903104
5.365861	371.858098	5.908109
5.944778	355.163818	5.913114
5.852533	362.682866	5.918118
5.637655	360.669612	5.923123
5.692359	349.217633	5.928128
5.208657	352.343382	5.933133
5.277131	357.888346	5.938138
5.481461	361.295442	5.943142
5.339733	362.864806	5.948147
5.810803	358.450320	5.953152
5.436291	363.735659	5.958157
5.569170	359.946809	5.963162
5.454294	361.556259	5.968166
5.582111	363.396607	5.973171
5.825244	363.497778	5.978176
5.254974	356.686936	5.983181
5.611436	359.877204	5.988186
5.638390	361.315733	5.993190
5.661689	364.713228	5.998195
6.021890	368.349008	6.003200
5.920167	366.988750	6.008205
5.649001	364.281951	6.013210
5.977539	366.366100	6.018214
5.725053	377.902981	6.023219
5.915604	365.616609	6.028224
5.527133	363.703321	6.033229
5.886736	359.113308	6.038234
5.976308	369.141241	6.043238
5.734754	359.668757	6.048243
5.624561	357.692886	6.053248
5.437019	359.674394	6.058253
5.794476	365.585377	6.063258
6.288831	377.982857	6.068262
6.063884	368.485619	6.073267
5.934689	361.260813	6.078272
5.640673	363.357082	6.083277
6.011344	358.471102	6.088282
5.761475	361.990492	6.093286
5.408782	365.174811	6.098291
5.919296	360.241609	6.103296
5.540115	361.588746	6.108301
5.608855	366.602152	6.113306
5.727086	362.777632	6.118310
5.467065	357.908211	6.123315
5.806281	373.107812	6.128320
5.716922	377.639784	6.133325
6.275289	379.349398	6.138330
6.148424	370.032948	6.143334
6.196968	361.910247	6.148339
5.876248	358.746134	6.153344
5.724532	377.506005	6.158349
5.690915	363.052750	6.163354
5.611270	365.713389	6.168358
5.316974	363.661958	6.173363
5.744132	360.782469	6.178368
5.818311	372.688950	6.183373
5.881875	364.715757	6.188378
5.731614	361.724255	6.193382
5.803025	361.181606	6.198387
5.857414	357.642341	6.203392
5.512957	364.482724	6.208397
5.782960	363.086371	6.213402
5.715287	362.359866	6.218406
5.567850	355.432154	6.223411
5.954796	368.956951	6.228416
5.813531	364.246094	6.233421
5.986848	364.374023	6.238426
5.522183	363.896385	6.243430
5.656052	366.694417	6.248435
5.821962	364.934716	6.253440
5.678328	371.386127	6.258445
6.045886	375.296007	6.263450
5.997670	370.769889	6.268454
5.462135	365.361494	6.273459
6.061377	365.185403	6.278464
5.555115	362.467983	6.283469
5.835500	355.726343	6.288474
5.593640	375.772184	6.293478
5.878112	376.702122	6.298483
6.099435	363.252978	6.303488
5.579524	378.198045	6.308493
5.881340	359.427428	6.313498
5.716713	373.177857	6.318502
5.503026	364.713421	6.323507
5.736275	370.020597	6.328512
5.800364	384.978573	6.333517
5.902527	381.172386	6.338522
5.635500	380.252486	6.343526
5.896444	387.981966	6.348531
6.205842	378.457950	6.353536
5.633290	374.710022	6.358541
5.735095	364.981253	6.363546
5.724801	364.264742	6.368550
5.655195	367.616682	6.373555
5.757086	366.708584	6.378560
5.771824	386.157403	6.383565
6.198478	380.648867	6.388570
5.916862	374.858994	6.393574
5.646904	364.384868	6.398579
5.503606	363.739816	6.403584
5.517790	361.171809	6.408589
5.558800	377.322985	6.413594
5.753735	382.177416	6.418598
5.775882	390.232218	6.423603
5.982107	388.352302	6.428608
5.632173	392.013929	6.433613
5.875578	389.001872	6.438618
6.011967	396.181386	6.443622
5.776866	388.362547	6.448627
5.709188	379.081112	6.453632
5.820661	386.416389	6.458637
5.991624	393.179191	6.463642
5.581988	378.996812	6.468646
5.726743	375.225082	6.473651
5.902552	383.429815	6.478656
5.872645	390.891651	6.483661
5.890070	385.694009	6.488666
5.604395	373.036151	6.493670
5.718567	379.257343	6.498675
5.971125	366.717642	6.503680
5.448103	377.822340	6.508685
5.580932	375.634381	6.513690
5.684729	389.114971	6.518694
5.894853	391.853601	6.523699
6.038424	391.521112	6.528704
5.549727	394.998833	6.533709
5.842538	381.604914	6.538714
5.924984	387.897520	6.543718
5.598987	395.288689	6.548723
5.620699	388.799541	6.553728
5.719544	398.693157	6.558733
5.589414	390.769284	6.563738
5.947766	389.966537	6.568742
5.712289	384.185250	6.573747
5.753198	386.194244	6.578752
5.755541	389.750054	6.583757
6.119222	389.209068	6.588762
5.799988	391.638327	6.593766
5.903705	387.506023	6.598771
6.083258	386.940102	6.603776
5.554458	374.269714	6.608781
5.823461	384.725130	6.613786
5.775799	392.151783	6.618790
5.568875	390.289142	6.623795
5.804087	391.242619	6.628800
6.049533	391.428851	6.633805
5.728544	388.160369	6.638810
6.075882	384.977002	6.643814
5.637059	376.494051	6.648819
5.656168	377.778784	6.653824
5.521873	382.039383	6.658829
5.819718	390.481266	6.663834
5.873996	392.086362	6.668838
5.970398	388.239946	6.673843
6.261836	382.945588	6.678848
5.974316	373.549902	6.683853
5.620855	373.773023	6.688858
5.938054	358.496000	6.693862
5.459484	361.418463	6.698867
5.855944	358.483672	6.703872
5.867315	360.683955	6.708877
5.726841	364.455128	6.713882
5.844022	367.227301	6.718886
5.318429	365.702498	6.723891
5.825870	378.904698	6.728896
5.724817	390.550740	6.733901
5.840578	388.454040	6.738906
5.954051	377.230120	6.743910
5.793821	381.757379	6.748915
5.749586	359.206450	6.753920
5.667435	372.232100	6.758925
5.832243	371.178100	6.763930
5.593570	360.227668	6.768934
5.564460	379.797247	6.773939
5.741764	377.516896	6.778944
5.689564	395.305725	6.783949
5.755441	389.344340	6.788954
5.797842	391.365755	6.793958
5.667976	388.693762	6.798963
6.118315	387.629825	6.803968
6.087928	388.128199	6.808973
5.786647	383.344331	6.813978
6.098468	372.184251	6.818982
5.851569	378.325972	6.823987
5.708693	359.922427	6.828992
6.008723	363.352495	6.833997
5.813464	363.639415	6.839002
5.419279	357.737469	6.844006
5.736928	358.045267	6.849011
5.856028	361.048095	6.854016
5.646650	363.235509	6.859021
5.780697	360.326013	6.864026
5.930017	370.119955	6.869030
5.687378	361.533505	6.874035
5.970625	362.343411	6.879040
5.411786	358.792657	6.884045
5.943479	364.815547	6.889050
5.924318	368.770197	6.894054
5.851161	363.593082	6.899059
5.667391	357.604383	6.904064
5.703268	366.890907	6.909069
5.708063	361.046671	6.914074
5.815653	360.090223	6.919078
5.846168	374.319449	6.924083
6.235631	367.823310	6.929088
5.842971	365.293737	6.934093
5.728250	368.946979	6.939098
5.965627	366.429424	6.944102
5.809836	368.500873	6.949107
5.794450	366.405741	6.954112
5.720635	367.682886	6.959117
5.625163	362.173904	6.964122
5.567700	362.224095	6.969126
5.352986	361.381423	6.974131
5.621939	371.934916	6.979136
5.919988	388.533055	6.984141
6.156081	384.085776	6.989146
5.854538	367.833161	6.994150
5.452637	373.511941	6.999155
5.618580	375.539308	7.004160
5.602900	367.822143	7.009165
5.641121	381.414243	7.014170
5.993784	378.714105	7.019174
5.792747	389.913897	7.024179
5.968211	383.179194	7.029184
5.952890	389.088479	7.034189
5.918347	378.628081	7.039194
6.081187	363.523938	7.044198
5.881924	371.176818	7.049203
5.807337	363.079737	7.054208
5.782061	363.846232	7.059213
5.727551	353.923659	7.064218
5.893618	364.053500	7.069222
5.932802	368.226802	7.074227
5.756967	366.922450	7.079232
5.827923	371.144560	7.084237
5.663708	359.018183	7.089242
6.138228	354.128588	7.094246
5.891021	367.097836	7.099251
6.091144	354.509410	7.104256
5.761057	363.014865	7.109261
5.741878	361.008914	7.114266
5.598272	351.131940	7.119270
5.948134	350.393801	7.124275
5.892307	353.594881	7.129280
5.913918	356.299767	7.134285
5.589636	360.688206	7.139290
5.609461	357.543504	7.144294
5.594386	355.682446	7.149299
5.830886	358.129033	7.154304
5.976279	355.436063	7.159309
5.742136	361.974419	7.164314
5.830411	355.326155	7.169318
5.688292	358.319290	7.174323
5.625681	353.248095	7.179328
5.308757	356.626128	7.184333
5.185807	357.252900	7.189338
5.567342	357.617129	7.194342
5.767147	379.068104	7.199347
6.077279	362.934794	7.204352
5.639869	367.043562	7.209357
5.771612	369.383176	7.214362
5.668120	365.352946	7.219366
5.827992	381.450700	7.224371
5.820600	376.854908	7.229376
5.986262	384.798636	7.234381
5.550340	366.874440	7.239386
5.462047	364.135825	7.244390
5.685790	384.387138	7.249395
6.256803	381.788832	7.254400
6.014927	382.380454	7.259405
5.646982	373.247310	7.264410
5.825234	361.149532	7.269414
5.840107	365.981550	7.274419
6.030699	351.259053	7.279424
5.514228	353.330064	7.284429
5.796394	356.728127	7.289434
5.645235	347.396512	7.294438
5.825847	359.270489	7.299443
6.168225	363.437415	7.304448
5.776928	361.179716	7.309453
5.553323	366.770446	7.314458
5.750608	364.569225	7.319462
5.726846	362.738002	7.324467
5.804459	358.356690	7.329472
5.828255	366.540939	7.334477
5.781561	359.613260	7.339482
5.636243	360.224554	7.344486
5.513898	362.853918	7.349491
5.990704	369.021453	7.354496
6.181318	378.236281	7.359501
5.842438	366.855449	7.364506
5.984719	356.898877	7.369510
5.660836	349.568535	7.374515
5.213759	356.741375	7.379520
5.773218	369.967056	7.384525
5.650472	376.608188	7.389530
6.070971	375.700790	7.394534
6.001347	377.160780	7.399539
5.938167	356.526924	7.404544
5.759974	358.867641	7.409549
5.390412	355.110059	7.414554
6.036456	355.113300	7.419558
5.691467	357.878789	7.424563
5.606247	361.198373	7.429568
5.838899	356.353001	7.434573
5.499768	370.526244	7.439578
5.945985	375.350793	7.444582
5.616282	374.522973	7.449587
6.009142	383.927582	7.454592
6.015744	376.396750	7.459597
5.746056	373.088595	7.464602
5.910222	353.406229	7.469606
5.648183	360.923406	7.474611
5.802807	355.827665	7.479616
5.653256	356.983796	7.484621
5.785406	364.290514	7.489626
6.158429	361.125273	7.494630
5.837047	360.141123	7.499635
5.703727	359.668517	7.504640
5.519726	352.642130	7.509645
6.087817	351.388900	7.514650
5.996226	354.174799	7.519654
5.243106	363.838046	7.524659
5.681250	359.754591	7.529664
5.812532	367.513869	7.534669
5.828064	363.961708	7.539674
5.854082	358.708943	7.544678
5.672714	358.193245	7.549683
5.760759	353.288272	7.554688
5.732618	365.138012	7.559693
5.945997	379.996663	7.564698
5.876023	374.021767	7.569702
5.616265	369.911614	7.574707
5.550494	367.735790	7.579712
6.059692	382.133634	7.584717
5.580703	377.545293	7.589722
5.747517	369.052876	7.594726
5.844527	383.474174	7.599731
6.007346	381.901621	7.604736
5.972109	372.399968	7.609741
5.799226	374.613303	7.614746
6.141850	368.437718	7.619750
5.660153	365.409560	7.624755
5.821758	353.418801	7.629760
5.758123	365.384835	7.634765
5.289798	366.018265	7.639770
5.781911	365.552070	7.644774
5.878299	372.867559	7.649779
5.610155	371.397332	7.654784
5.997300	370.178781	7.659789
5.509119	369.413756	7.664794
6.089230	370.670703	7.669798
5.593236	371.827331	7.674803
5.496880	365.087768	7.679808
5.774116	368.711236	7.684813
6.150637	380.817127	7.689818
5.881587	364.027905	7.694822
5.893358	369.284360	7.699827
5.785700	364.378409	7.704832
5.419307	355.137462	7.709837
5.611150	357.398054	7.714842
5.889131	373.875935	7.719846
5.744694	377.866035	7.724851
6.059216	375.649608	7.729856
6.078320	369.879059	7.734861
5.809050	370.231360	7.739866
5.939267	365.987339	7.744870
5.741686	356.359268	7.749875
5.474752	365.743856	7.754880
5.937615	355.904737	7.759885
5.700187	366.872932	7.764890
5.763146	363.107692	7.769894
5.898266	356.338191	7.774899
5.864790	363.655040	7.779904
5.945820	358.649924	7.784909
5.642345	362.535223	7.789914
5.579539	351.645827	7.794918
5.486635	368.406444	7.799923
5.550212	367.472711	7.804928
5.906357	382.217244	7.809933
5.784334	388.269799	7.814938
6.291176	381.046571	7.819942
5.646788	372.586338	7.824947
5.628782	369.093215	7.829952
5.546123	361.509935	7.834957
5.910690	373.326625	7.839962
5.923492	373.735972	7.844966
5.737208	375.559095	7.849971
5.299804	370.663679	7.854976
5.673390	375.790678	7.859981
5.380640	389.488426	7.864986
5.875714	385.029043	7.869990
5.696815	388.780932	7.874995
5.926998	391.870766	7.880000
5.972006	398.741891	7.885005
6.011417	389.399379	7.890010
5.982103	395.032443	7.895014
5.740213	393.725783	7.900019
5.840153	386.442919	7.905024
5.608697	385.897102	7.910029
5.680279	393.362020	7.915034
6.245508	394.409325	7.920038
5.887412	392.339412	7.925043
5.795396	371.352547	7.930048
5.833452	365.791005	7.935053
5.576084	373.816828	7.940058
5.745989	367.064020	7.945062
5.578035	380.615656	7.950067
5.928851	391.244921	7.955072
5.892410	383.723994	7.960077
5.482273	379.109045	7.965082
5.627213	386.742804	7.970086
5.874839	397.771062	7.975091
6.151030	389.995501	7.980096
5.847137	380.156280	7.985101
5.554774	374.665488	7.990106
5.609053	382.908246	7.995110
5.756767	393.344704	8.000115
6.025169	393.951855	8.005133
6.211075	391.300369	8.010150
5.906908	376.967401	8.015168
5.601031	369.473183	8.020186
5.441407	376.163160	8.025203
5.259007	386.116582	8.030221
5.740832	388.344834	8.035238
6.060797	390.945578	8.040256
6.123710	395.508442	8.045274
6.193138	396.864057	8.050291
5.883219	384.210837	8.055309
6.082986	375.835835	8.060326
5.893283	371.775786	8.065344
5.921018	366.817000	8.070362
5.740918	370.461746	8.075379
5.607443	368.848048	8.080397
5.929129	373.988885	8.085414
5.565830	378.397622	8.090432
5.615515	383.571612	8.095450
5.940838	383.574346	8.100467
6.002180	393.839869	8.105485
5.999154	387.614135	8.110502
5.717580	392.808472	8.115520
5.865365	382.251531	8.120538
6.014570	399.610006	8.125555
5.830844	406.660369	8.130573
5.739764	397.570394	8.135590
5.693320	403.857648	8.140608
6.244524	392.268680	8.145626
6.052202	391.951741	8.150643
5.971347	401.280204	8.155661
6.205341	395.784175	8.160678
6.165307	395.017351	8.165696
6.098328	371.681778	8.170714
6.033536	372.591372	8.175731
5.963250	370.819455	8.180749
6.172617	374.210679	8.185766
5.448891	371.622825	8.190784
5.812150	374.131579	8.195802
5.761610	383.272250	8.200819
5.947522	394.490222	8.205837
6.121528	396.204984	8.210854
5.989712	399.387745	8.215872
5.948026	395.945114	8.220890
6.279154	395.442021	8.225907
5.827751	397.724978	8.230925
6.108330	393.884723	8.235942
6.208729	397.797944	8.240960
6.124059	392.544344	8.245978
6.148884	392.553136	8.250995
5.816078	386.590507	8.256013
5.904176	387.555040	8.261030
6.221799	403.596436	8.266048
6.007189	398.735570	8.271066
5.922310	391.765283	8.276083
6.096376	403.395362	8.281101
6.163031	396.843133	8.286118
6.029358	402.244668	8.291136
5.851309	396.021108	8.296154
6.009429	399.606555	8.301171
6.105531	399.727253	8.306189
6.067112	398.079725	8.311206
5.791694	401.426994	8.316224
6.252246	388.110266	8.321242
6.092143	393.194055	8.326259
5.852160	398.713229	8.331277
6.371490	393.847821	8.336294
5.950162	396.848730	8.341312
6.119683	404.115137	8.346330
6.382115	389.797523	8.351347
5.980233	395.338908	8.356365
6.035177	398.325152	8.361382
6.159498	407.574135	8.366400
6.327480	404.890742	8.371418
6.365017	398.481927	8.376435
6.200449	395.623427	8.381453
5.866536	400.204287	8.386470
5.957860	399.628315	8.391488
5.855431	405.119628	8.396506
6.032825	395.145008	8.401523
5.704729	400.053152	8.406541
5.922140	394.831115	8.411558
5.612189	404.668835	8.416576
5.815590	414.012726	8.421594
6.024454	420.547156	8.426611
6.232400	422.723653	8.431629
6.511775	431.115238	8.436646
6.497951	430.467380	8.441664
6.305065	428.074050	8.446682
6.773526	426.495420	8.451699
6.410356	425.302707	8.456717
6.206529	410.193457	8.461734
6.298422	414.458301	8.466752
6.263414	411.756220	8.471770
6.266769	415.406944	8.476787
6.122627	418.039385	8.481805
6.555091	416.479019	8.486822
6.199049	417.263839	8.491840
6.172722	404.888056	8.496858
6.555307	416.160432	8.501875
6.236328	415.219566	8.506893
6.571921	400.448677	8.511910
6.250352	401.272275	8.516928
6.165285	402.579515	8.521946
6.115967	409.274311	8.526963
6.576997	416.147918	8.531981
6.348012	416.969634	8.536998
6.335260	414.604886	8.542016
6.404165	425.336291	8.547034
6.372234	417.972697	8.552051
6.149668	420.693163	8.557069
6.422943	417.579869	8.562087
6.527804	429.653145	8.567104
6.123005	432.698805	8.572122
6.111284	427.417987	8.577139
6.575543	443.423820	8.582157
6.516876	429.948576	8.587175
6.506022	431.474559	8.592192
6.660822	437.215907	8.597210
6.546131	423.875676	8.602227
6.185908	417.645938	8.607245
6.425256	430.701669	8.612263
6.675566	427.812872	8.617280
6.452767	419.251599	8.622298
6.488223	404.404658	8.627315
6.416296	408.692013	8.632333
6.376935	410.209838	8.637351
6.433988	411.753581	8.642368
6.559614	427.149752	8.647386
6.444408	412.916534	8.652403
6.494983	429.340614	8.657421
6.706578	421.017385	8.662439
6.359035	407.792543	8.667456
6.177213	413.384658	8.672474
6.819245	417.269823	8.677491
6.598204	421.851937	8.682509
6.373625	414.928775	8.687527
6.483930	414.832657	8.692544
6.251601	419.994041	8.697562
6.732739	423.386874	8.702579
6.570895	433.444396	8.707597
6.802185	422.893282	8.712615
6.631575	412.682849	8.717632
6.514738	403.420185	8.722650
6.347318	398.788606	8.727667
6.426875	417.047929	8.732685
6.539987	423.086133	8.737703
6.888484	422.233186	8.742720
6.568582	418.865699	8.747738
6.610308	404.506916	8.752755
6.352954	404.402133	8.757773
6.425655	419.715074	8.762791
6.958845	420.452084	8.767808
6.435475	435.744825	8.772826
6.698320	430.212707	8.777843
7.000710	425.040461	8.782861
6.646250	415.824489	8.787879
6.379750	403.470559	8.792896
6.075806	419.659849	8.797914
6.490553	418.291603	8.802931
6.654833	433.265165	8.807949
6.599051	433.453841	8.812967
6.771263	431.921628	8.817984
6.475241	432.479298	8.823002
6.560470	434.056498	8.828019
6.653346	426.960517	8.833037
6.714460	429.352521	8.838055
6.587081	437.331323	8.843072
6.557334	438.200716	8.848090
6.578443	420.440102	8.853107
6.842091	434.871088	8.858125
6.642762	440.024151	8.863143
6.901940	430.506902	8.868160
6.922499	429.437098	8.873178
7.292599	424.036497	8.878195
6.842477	430.585821	8.883213
6.588416	433.077699	8.888231
7.022910	424.896266	8.893248
6.630522	429.814492	8.898266
6.557086	430.283640	8.903283
6.443655	427.451835	8.908301
6.611012	429.009855	8.913319
6.886325	422.248202	8.918336
6.620047	432.299997	8.923354
6.491279	426.396902	8.928371
6.525457	434.394570	8.933389
6.191047	426.728077	8.938407
6.480562	423.811049	8.943424
6.436816	446.700261	8.948442
6.801718	459.168306	8.953459
6.798060	456.555979	8.958477
6.577938	450.540959	8.963495
7.067631	451.347901	8.968512
7.146408	455.150915	8.973530
7.113930	465.541630	8.978547
6.800254	453.138254	8.983565
6.956783	458.626879	8.988583
6.932357	452.057342	8.993600
6.741521	460.301713	8.998618
6.946228	461.481505	9.003635
6.755610	460.318557	9.008653
7.405929	463.224151	9.013671
7.122952	458.620130	9.018688
7.013025	448.778858	9.023706
7.167063	431.057365	9.028723
6.879723	439.878569	9.033741
6.490916	431.441128	9.038759
7.214030	426.509069	9.043776
6.794778	439.450250	9.048794
7.182180	423.364746	9.053811
7.034707	429.670994	9.058829
6.793979	433.899597	9.063847
6.939231	430.973614	9.068864
6.682426	443.438074	9.073882
6.975337	436.506404	9.078899
7.173766	445.118958	9.083917
6.934423	447.431810	9.088935
6.960711	438.960885	9.093952
6.844674	449.241609	9.098970
7.040838	456.832062	9.103987
7.188529	451.163348	9.109005
7.053403	455.839306	9.114023
6.893463	439.236798	9.119040
6.592195	444.519441	9.124058
7.167415	448.336187	9.129075
7.224289	448.103277	9.134093
6.907702	453.268404	9.139111
7.297101	450.916379	9.144128
7.137455	455.725564	9.149146
7.117703	457.107779	9.154163
7.195516	464.760959	9.159181
7.001429	456.438161	9.164199
7.282196	444.108908	9.169216
6.825914	448.671084	9.174234
6.822021	446.314410	9.179251
7.216381	457.960501	9.184269
7.239235	462.551748	9.189287
7.264641	456.271043	9.194304
6.985639	462.512706	9.199322
7.196772	459.598486	9.204339
7.408749	459.694717	9.209357
7.112960	467.046679	9.214375
7.083615	460.064508	9.219392
6.838544	463.583755	9.224410
7.038411	461.204621	9.229427
7.146401	459.332180	9.234445
7.143906	466.780197	9.239463
7.155242	452.760646	9.244480
6.690413	461.388767	9.249498
7.080420	461.450793	9.254515
7.306604	451.288619	9.259533
7.370214	452.320107	9.264551
7.163594	454.113446	9.269568
7.212954	459.726158	9.274586
7.061307	466.478034	9.279603
7.357585	456.869753	9.284621
7.221661	455.026061	9.289639
7.229951	448.808000	9.294656
7.093207	462.698994	9.299674
7.033394	460.057596	9.304691
7.196180	458.157635	9.309709
7.140007	464.465369	9.314727
7.349558	462.154144	9.319744
6.899358	463.307163	9.324762
7.376850	464.384256	9.329779
7.491434	462.352993	9.334797
7.014742	467.155053	9.339815
7.231470	455.615295	9.344832
7.421957	464.519432	9.349850
7.393638	462.321215	9.354867
7.814149	456.265777	9.359885
7.122422	448.399644	9.364903
7.352753	451.727640	9.369920
7.359308	456.880007	9.374938
7.235706	459.225218	9.379955
7.426084	450.195257	9.384973
6.949524	462.848794	9.389991
7.239834	467.527523	9.395008
7.535666	469.491443	9.400026
7.483104	471.781344	9.405043
7.494860	472.726286	9.410061
7.155510	464.255835	9.415079
7.260452	471.257838	9.420096
7.181260	477.900537	9.425114
7.319107	471.204585	9.430131
7.773862	480.594334	9.435149
7.435418	486.545522	9.440167
7.786752	481.302476	9.445184
7.761759	475.013882	9.450202
7.649349	469.496367	9.455219
7.912306	462.036059	9.460237
7.399838	452.958431	9.465255
7.242517	454.822940	9.470272
7.476191	457.017500	9.475290
7.172889	456.755817	9.480307
7.235656	460.116380	9.485325
7.222283	477.146960	9.490343
7.505070	475.941395	9.495360
7.292234	474.576804	9.500378
7.421547	473.628811	9.505395
7.689936	462.989810	9.510413
7.643673	474.894294	9.515431
7.626567	463.937114	9.520448
7.689705	478.301722	9.525466
7.446745	470.762891	9.530483
7.844996	463.524376	9.535501
7.477671	471.919479	9.540519
7.407948	478.844712	9.545536
7.451200	469.976646	9.550554
7.547386	467.153017	9.555571
7.853860	469.405598	9.560589
7.407849	476.702207	9.565607
7.491873	471.292767	9.570624
7.613707	472.914727	9.575642
7.487265	475.601206	9.580659
7.892307	466.524980	9.585677
7.621365	474.797686	9.590695
7.607217	474.370780	9.595712
7.599954	473.201193	9.600730
7.620160	483.514238	9.605747
7.777317	476.215665	9.610765
7.588950	482.935431	9.615783
7.852754	476.768842	9.620800
7.814145	471.230296	9.625818
7.856820	470.990143	9.630835
7.754075	471.558556	9.635853
7.515809	480.687666	9.640871
7.542041	479.162542	9.645888
8.098013	478.337044	9.650906
7.971626	479.843265	9.655923
7.992411	466.361856	9.660941
7.434805	482.846563	9.665959
7.703762	478.547372	9.670976
7.949056	471.386467	9.675994
7.663940	480.668082	9.681011
7.591233	468.574072	9.686029
7.494462	478.766589	9.691047
7.772882	483.305177	9.696064
7.838955	471.937334	9.701082
7.470167	473.008170	9.706099
7.607091	483.747888	9.711117
8.055466	480.698665	9.716135
7.902864	476.329828	9.721152
7.726823	483.599919	9.726170
7.758804	475.702432	9.731187
8.083707	475.910356	9.736205
7.710383	473.665209	9.741223
7.707484	487.046110	9.746240
7.922020	468.358909	9.751258
7.697401	476.889441	9.756275
8.135537	480.863370	9.761293
8.058098	476.738372	9.766311
7.888655	477.430842	9.771328
8.179630	491.033941	9.776346
7.907921	484.395842	9.781363
8.108012	477.084230	9.786381
7.900661	485.463741	9.791399
8.024079	487.337914	9.796416
7.847033	472.909214	9.801434
7.696931	486.821254	9.806451
7.610525	476.282016	9.811469
7.529815	478.058786	9.816487
7.665662	478.564570	9.821504
7.614940	484.650555	9.826522
7.684218	505.956881	9.831539
8.093469	502.134312	9.836557
7.851327	502.995962	9.841575
7.890606	504.422580	9.846592
8.344178	496.960793	9.851610
7.972619	504.640217	9.856627
7.645236	496.795871	9.861645
7.531209	500.493406	9.866663
7.667843	501.560792	9.871680
8.164341	500.296495	9.876698
7.838981	510.190335	9.881715
7.925984	505.657718	9.886733
7.856803	504.665086	9.891751
7.963942	504.496882	9.896768
8.334777	505.104702	9.901786
8.279372	510.519253	9.906803
8.047770	498.629997	9.911821
8.309204	506.601558	9.916839
8.256081	510.655620	9.921856
8.433732	504.227970	9.926874
8.428412	498.958750	9.931891
8.337614	505.533852	9.936909
8.559072	509.096775	9.941927
8.238151	499.645134	9.946944
8.096992	507.203255	9.951962
8.080313	509.487539	9.956979
8.051053	513.014007	9.961997
8.340443	508.216154	9.967015
8.422091	499.231606	9.972032
8.771666	508.189732	9.977050
8.313869	505.948349	9.982067
8.107677	502.613522	9.987085
8.087688	498.062958	9.992103
8.191380	512.263452	9.997120
8.565413	502.633497	10.002138
8.071571	511.616476	10.007155
7.984830	508.581664	10.012173
8.083660	508.799764	10.017191
8.147122	498.808223	10.022208
7.964332	503.131905	10.027226
7.938395	501.293066	10.032243
8.027269	501.134036	10.037261
8.379165	505.449681	10.042279
8.277618	502.978914	10.047296
8.117660	504.566135	10.052314
8.050556	498.350401	10.057331
8.314101	505.090886	10.062349
8.330702	510.655099	10.067367
8.192874	510.695687	10.072384
8.370172	500.276061	10.077402
8.210968	512.741056	10.082419
8.644272	514.636106	10.087437
8.466935	508.904693	10.092455
8.182662	509.665648	10.097472
8.266849	509.911289	10.102490
8.324469	517.157406	10.107507
8.578803	510.711427	10.112525
8.610315	513.363697	10.117543
8.495678	511.232646	10.122560
8.323641	497.251258	10.127578
8.454828	511.138180	10.132595
8.356364	506.773475	10.137613
8.321991	501.732865	10.142631
8.310021	512.540110	10.147648
8.751754	520.641216	10.152666
8.579799	514.612316	10.157683
8.282919	520.083639	10.162701
8.505184	503.452745	10.167719
8.193949	512.646952	10.172736
8.475590	518.434723	10.177754
8.521168	526.058267	10.182771
8.763361	537.488414	10.187789
8.922834	521.927677	10.192807
8.253691	524.200584	10.197824
8.794664	504.682725	10.202842
8.555478	506.250802	10.207859
8.574736	508.636751	10.212877
8.628984	499.561823	10.217895
8.756151	505.257031	10.222912
8.679584	499.386757	10.227930
8.417151	499.181785	10.232947
8.397722	500.560798	10.237965
8.556937	507.939314	10.242983
8.087268	518.338600	10.248000
8.640460	526.920855	10.253018
8.699244	529.063932	10.258035
8.698953	527.192671	10.263053
9.182271	527.517784	10.268071
8.582541	527.223651	10.273088
8.666251	509.841298	10.278106
8.654729	508.647130	10.283123
8.653472	510.203174	10.288141
8.833508	503.491132	10.293159
8.706163	501.788101	10.298176
8.512383	506.302850	10.303194
8.727220	512.003259	10.308211
8.843275	521.767985	10.313229
8.989238	521.694681	10.318247
8.749158	505.189874	10.323264
8.735816	498.236738	10.328282
8.647539	503.186230	10.333299
8.444039	505.998394	10.338317
8.882675	510.685452	10.343335
8.575732	515.350477	10.348352
8.779224	532.208277	10.353370
8.796941	524.006895	10.358387
8.640055	532.476349	10.363405
8.772556	522.805333	10.368423
8.731805	534.576451	10.373440
9.012100	531.525153	10.378458
8.790786	528.959540	10.383475
8.878448	538.059703	10.388493
8.939074	533.954083	10.393511
8.950253	529.433341	10.398528
9.066444	528.673591	10.403546
9.311039	524.195172	10.408563
8.695212	514.874935	10.413581
8.546352	503.875258	10.418599
8.914325	507.004976	10.423616
8.870242	518.820787	10.428634
8.769795	508.384714	10.433651
9.035918	517.658873	10.438669
8.789449	521.194130	10.443687
9.136004	528.290841	10.448704
9.026847	534.206120	10.453722
9.348184	531.725895	10.458739
8.897038	513.830901	10.463757
9.069200	506.637261	10.468775
8.897075	497.957558	10.473792
8.780457	501.068529	10.478810
8.710385	506.983987	10.483827
8.988004	519.109149	10.488845
9.159551	526.813940	10.493863
8.996360	530.806359	10.498880
8.834210	526.950238	10.503898
9.229177	530.769998	10.508915
9.084611	528.908719	10.513933
9.177224	525.542849	10.518951
9.123059	529.117404	10.523968
8.903009	519.750932	10.528986
9.136095	525.473731	10.534003
9.075311	531.820081	10.539021
9.197643	523.693824	10.544039
8.718596	523.800498	10.549056
8.936044	522.781890	10.554074
8.791125	519.705699	10.559091
9.084998	521.108207	10.564109
9.206006	523.317272	10.569127
9.034383	527.086952	10.574144
8.890490	525.588480	10.579162
8.887657	517.693273	10.584179
8.871896	535.229204	10.589197
8.974641	530.394317	10.594215
8.841872	522.453196	10.599232
8.982982	530.162757	10.604250
9.168339	534.807456	10.609267
9.523720	554.582650	10.614285
9.359510	531.139028	10.619303
9.358166	530.306177	10.624320
8.914250	520.589777	10.629338
9.478000	513.827078	10.634355
8.651200	518.737654	10.639373
9.032847	529.760944	10.644391
9.575149	544.325081	10.649408
9.370805	552.025663	10.654426
9.377927	537.037886	10.659443
8.812380	544.836083	10.664461
9.067092	547.245106	10.669479
9.321483	546.454235	10.674496
9.096836	547.777043	10.679514
9.376375	547.092683	10.684531
9.189813	552.975915	10.689549
9.319499	544.450871	10.694567
9.595023	546.459006	10.699584
9.427887	552.787313	10.704602
9.386860	544.607748	10.709619
9.145119	548.722930	10.714637
9.384730	549.512256	10.719655
9.515461	558.760313	10.724672
9.449396	561.784480	10.729690
9.447446	548.066733	10.734707
9.351164	551.086165	10.739725
9.906900	549.888321	10.744743
9.643099	543.018590	10.749760
9.244445	547.429753	10.754778
9.239558	541.936393	10.759795
9.268454	544.267189	10.764813
8.950940	546.368243	10.769831
8.985127	548.796039	10.774848
9.141978	555.565883	10.779866
9.472615	548.154894	10.784883
9.423378	551.482531	10.789901
9.549907	560.163210	10.794919
9.603407	563.477908	10.799936
9.672429	563.511333	10.804954
9.499756	549.946565	10.809971
9.567579	555.581660	10.814989
9.685459	546.749199	10.820007
9.624431	545.253521	10.825024
9.204095	560.138909	10.830042
9.662420	557.485741	10.835059
9.798416	565.600057	10.840077
9.865182	555.623745	10.845095
9.784174	556.286584	10.850112
9.667038	555.733802	10.855130
9.439883	542.635162	10.860147
9.496167	549.991954	10.865165
9.773602	544.975060	10.870183
9.501764	544.995620	10.875200
9.263006	546.349042	10.880218
9.583581	557.138923	10.885235
9.532344	562.117341	10.890253
9.629203	574.823122	10.895271
9.807811	570.115192	10.900288
9.272673	580.524772	10.905306
9.762556	571.141714	10.910323
9.855641	581.784219	10.915341
9.694849	570.511818	10.920359
9.590427	583.189183	10.925376
9.861222	579.277840	10.930394
9.838194	571.407864	10.935411
9.540365	579.201999	10.940429
9.602545	581.174138	10.945447
9.693780	583.769724	10.950464
9.665297	587.876747	10.955482
9.796901	579.146260	10.960499
9.637695	577.517641	10.965517
9.298459	579.918744	10.970535
9.816174	580.011253	10.975552
9.601375	582.781020	10.980570
9.785432	590.881505	10.985587
9.703581	601.986928	10.990605
9.762250	604.786433	10.995623
9.881683	597.758807	11.000640
9.997307	605.185219	11.005658
10.071658	602.251382	11.010675
9.849847	602.598615	11.015693
9.835242	599.880686	11.020711
10.044179	602.432586	11.025728
9.890813	614.110950	11.030746
10.025316	600.864084	11.035763
10.106379	603.300322	11.040781
9.982705	608.776092	11.045799
10.017919	607.442052	11.050816
10.043753	603.938310	11.055834
10.202869	596.995983	11.060851
10.279241	599.417177	11.065869
9.888330	580.010531	11.070887
10.123442	572.500892	11.075904
9.756746	569.377391	11.080922
9.869703	577.864547	11.085939
10.047163	590.832263	11.090957
9.637062	602.544533	11.095975
10.600374	604.621635	11.100992
10.053614	604.312889	11.106010
10.205128	602.323161	11.111027
10.180155	595.352875	11.116045
9.942547	605.936756	11.121063
10.248140	604.831750	11.126080
10.140616	606.839949	11.131098
9.953699	590.793787	11.136115
10.265342	599.802084	11.141133
10.257928	608.330205	11.146151
10.542887	595.956009	11.151168
9.907081	581.734797	11.156186
10.098379	578.558581	11.161203
10.247885	585.496843	11.166221
9.994625	582.532290	11.171239
10.186673	587.254849	11.176256
10.055321	600.182595	11.181274
10.176730	594.757793	11.186291
10.171294	590.574150	11.191309
10.202953	595.495408	11.196327
10.088449	591.174221	11.201344
10.171106	602.809285	11.206362
10.143871	600.150138	11.211379
10.268676	595.406451	11.216397
10.038815	590.923459	11.221415
10.380588	589.863278	11.226432
10.254945	604.188139	11.231450
10.189662	591.338653	11.236467
9.957644	595.654291	11.241485
9.704421	598.597336	11.246503
10.063422	603.019188	11.251520
10.614656	620.441119	11.256538
10.675700	621.908517	11.261555
10.474247	611.226280	11.266573
10.132762	597.618498	11.271591
10.423331	594.313117	11.276608
10.386965	607.992839	11.281626
10.431421	617.222887	11.286643
10.602922	616.905743	11.291661
10.123729	616.870430	11.296679
10.586118	620.616531	11.301696
10.457902	625.992032	11.306714
10.627401	622.844470	11.311731
10.284054	610.612889	11.316749
10.416557	619.734469	11.321767
10.516939	623.044989	11.326784
10.553670	630.209219	11.331802
10.685434	624.363067	11.336819
10.571392	628.300470	11.341837
10.315928	629.104253	11.346855
10.567206	623.649627	11.351872
10.425878	635.386078	11.356890
10.312132	623.140605	11.361907
10.682655	622.031736	11.366925
10.689150	631.577004	11.371943
10.621736	631.319384	11.376960
10.927682	629.510583	11.381978
10.780580	624.815802	11.386995
11.022481	621.672675	11.392013
10.214575	612.915807	11.397031
10.319178	620.811007	11.402048
10.531352	626.502402	11.407066
10.798670	622.285484	11.412083
11.061310	624.223064	11.417101
10.870890	631.198825	11.422119
11.049317	617.244482	11.427136
10.956227	607.469912	11.432154
10.689202	605.763509	11.437171
10.825143	601.601894	11.442189
10.291940	607.069245	11.447207
10.749777	606.893429	11.452224
10.524793	602.264505	11.457242
10.659795	608.097372	11.462259
10.892386	626.134117	11.467277
10.917115	623.772936	11.472295
10.902812	601.656407	11.477312
10.872912	610.519408	11.482330
10.595818	605.459995	11.487347
10.925647	607.358644	11.492365
10.656098	606.854987	11.497383
10.890422	606.903538	11.502400
10.766802	612.483440	11.507418
10.741657	624.652956	11.512435
10.898252	631.722669	11.517453
10.983105	635.764609	11.522471
10.935504	626.636147	11.527488
11.165918	622.544930	11.532506
10.694347	607.262870	11.537523
10.684402	622.349095	11.542541
10.491381	622.354150	11.547559
11.401721	621.031315	11.552576
11.020851	628.311468	11.557594
10.984604	627.017025	11.562611
11.103485	621.949214	11.567629
11.208174	629.673992	11.572647
11.018345	627.778769	11.577664
11.060310	620.419291	11.582682
10.957974	635.116063	11.587699
11.270662	622.387213	11.592717
10.705292	615.725649	11.597735
10.872800	613.998499	11.602752
11.409253	619.979908	11.607770
11.167947	628.986494	11.612787
11.271815	623.829516	11.617805
10.962640	614.798848	11.622823
11.106000	611.604891	11.627840
11.227494	618.610670	11.632858
11.060390	618.251906	11.637875
11.095818	613.500127	11.642893
10.870146	623.062833	11.647911
11.158856	619.205478	11.652928
11.114427	628.935448	11.657946
11.136095	631.841739	11.662963
11.376505	622.709179	11.667981
10.989993	629.740909	11.672999
11.195535	627.338774	11.678016
11.456310	618.269296	11.683034
11.197891	635.871748	11.688051
11.131328	613.409945	11.693069
11.208496	620.432138	11.698087
11.053162	621.308594	11.703104
11.046922	629.413667	11.708122
11.045472	637.975581	11.713139
10.966410	624.705356	11.718157
11.014846	626.187352	11.723175
10.972366	624.543595	11.728192
11.349681	619.037665	11.733210
10.728531	626.970841	11.738227
11.194007	634.800037	11.743245
11.100033	649.432395	11.748263
11.361512	652.623006	11.753280
11.556111	653.100656	11.758298
11.722526	660.181464	11.763315
11.748974	653.313550	11.768333
11.409687	634.451019	11.773351
11.237181	639.770348	11.778368
11.681395	627.973932	11.783386
11.659580	640.531098	11.788403
11.530270	616.696891	11.793421
11.479254	616.960561	11.798439
11.217583	631.029048	11.803456
11.417931	620.220736	11.808474
11.386018	621.791060	11.813491
11.609773	624.397446	11.818509
11.690893	617.965945	11.823527
11.450421	624.021747	11.828544
11.363903	623.741875	11.833562
11.332859	628.057589	11.838579
11.767220	634.686154	11.843597
11.569444	649.965932	11.848615
11.922832	648.105515	11.853632
11.613913	635.783316	11.858650
11.351916	637.689490	11.863667
11.334974	628.325851	11.868685
11.660887	643.611934	11.873703
11.549080	649.272047	11.878720
11.757097	641.921257	11.883738
11.613941	650.691572	11.888755
11.885751	646.249883	11.893773
12.280954	649.397451	11.898791
11.685971	631.045197	11.903808
11.520107	629.701636	11.908826
11.595598	628.547475	11.913843
11.638271	621.478217	11.918861
11.709264	627.396859	11.923879
11.652342	636.270418	11.928896
11.613793	635.948316	11.933914
11.698205	646.639556	11.938931
11.739733	643.568844	11.943949
12.017633	643.181381	11.948967
12.046787	647.560252	11.953984
12.013067	638.221328	11.959002
11.713140	627.137947	11.964019
11.605058	634.103965	11.969037
11.840873	635.872181	11.974055
11.784858	653.181007	11.979072
11.912583	650.289292	11.984090
11.547796	653.808399	11.989107
11.842726	648.192293	11.994125
11.862517	649.085493	11.999143
11.795154	649.793534	12.004160
12.079013	647.738884	12.009178
11.485123	656.251621	12.014195
11.523923	651.376228	12.019213
11.742680	650.524664	12.024231
11.367159	651.590255	12.029248
11.929695	646.415055	12.034266
11.215953	667.598107	12.039283
11.882245	669.343060	12.044301
11.924795	668.929356	12.049319
11.908925	670.023803	12.054336
11.951679	667.277941	12.059354
11.752904	674.516959	12.064371
11.735409	666.687099	12.069389
12.011605	675.899802	12.074407
11.904848	681.069988	12.079424
12.242545	668.091035	12.084442
12.174470	666.378702	12.089459
12.237606	664.945609	12.094477
12.372439	661.721421	12.099495
11.850766	673.593229	12.104512
12.274321	664.245760	12.109530
12.358097	667.237000	12.114547
12.261741	668.265163	12.119565
12.098549	665.848213	12.124583
11.842574	669.164083	12.129600
12.254411	662.535583	12.134618
12.092430	662.608358	12.139635
12.028815	668.847902	12.144653
12.314230	658.982441	12.149671
12.141105	663.402476	12.154688
12.244787	669.511668	12.159706
12.376836	665.663070	12.164723
12.299685	666.296907	12.169741
12.269919	664.853124	12.174759
12.008315	665.758856	12.179776
12.528494	658.800959	12.184794
12.285229	671.295014	12.189811
12.351875	673.522083	12.194829
12.475824	674.339005	12.199847
12.154742	670.321563	12.204864
12.797499	667.671040	12.209882
12.152163	667.582863	12.214899
12.413359	668.138441	12.219917
12.659130	664.306739	12.224935
12.437650	672.956793	12.229952
12.263367	667.518338	12.234970
12.315067	672.083029	12.239987
12.249031	679.320185	12.245005
12.236020	668.075061	12.250023
12.489481	693.714049	12.255040
13.105571	686.305615	12.260058
12.613478	677.884239	12.265075
12.656688	674.655470	12.270093
12.848636	672.107137	12.275111
12.471909	662.979731	12.280128
12.555210	669.912621	12.285146
12.380319	663.126742	12.290163
12.267655	663.879751	12.295181
12.466314	659.014023	12.300199
12.437896	670.893751	12.305216
12.896530	681.949254	12.310234
12.608314	670.718845	12.315251
12.652284	666.183463	12.320269
12.765839	672.625622	12.325287
12.496641	674.192104	12.330304
12.532021	675.303768	12.335322
12.918281	681.602218	12.340339
12.673354	684.818530	12.345357
12.998308	667.641221	12.350375
12.416806	677.852995	12.355392
12.641592	678.827686	12.360410
12.910093	686.776130	12.365427
12.511805	687.450816	12.370445
12.571187	686.264462	12.375463
12.766901	690.920202	12.380480
12.730329	694.119650	12.385498
12.892271	692.636361	12.390515
12.744139	700.249304	12.395533
13.025548	693.060562	12.400551
12.709294	695.404431	12.405568
12.739440	694.383602	12.410586
12.917011	691.755469	12.415603
12.895408	695.558483	12.420621
13.036329	691.904148	12.425639
12.700017	686.096601	12.430656
12.867976	688.168943	12.435674
13.200153	701.825707	12.440691
13.012989	693.100928	12.445709
13.146139	688.545256	12.450727
13.241391	694.428560	12.455744
13.164598	680.463664	12.460762
13.178738	672.796102	12.465779
12.527009	667.123186	12.470797
13.125350	679.835676	12.475815
13.188659	681.687730	12.480832
13.375273	678.486984	12.485850
13.338702	667.374939	12.490867
12.876067	673.935779	12.495885
12.823262	665.603370	12.500903
12.812708	667.810976	12.505920
13.081842	680.044875	12.510938
13.314758	682.488889	12.515955
13.212881	681.315178	12.520973
12.856398	665.443839	12.525991
12.857067	671.048467	12.531008
13.046159	688.950081	12.536026
13.334610	691.170802	12.541043
13.070101	688.485702	12.546061
13.235986	682.533200	12.551079
13.064351	688.455163	12.556096
13.163386	686.347417	12.561114
13.516276	685.061427	12.566131
13.001143	694.738951	12.571149
13.057129	694.578760	12.576167
13.240284	696.588762	12.581184
13.255952	694.194277	12.586202
13.086778	696.691826	12.591219
13.339111	685.502946	12.596237
12.911150	685.506942	12.601255
13.016324	687.352437	12.606272
13.215092	695.939813	12.611290
13.177159	692.035792	12.616307
13.206278	696.058076	12.621325
13.613574	688.051198	12.626343
13.411287	688.000900	12.631360
13.311219	694.315593	12.636378
13.650108	698.393483	12.641395
13.346687	701.341254	12.646413
13.027270	699.330628	12.651431
13.550354	711.985505	12.656448
13.420208	704.984317	12.661466
13.948983	707.968957	12.666483
13.394977	711.880638	12.671501
13.123616	699.618782	12.676519
13.287631	718.549987	12.681536
13.403530	725.430454	12.686554
14.025598	718.245132	12.691571
14.150592	715.265472	12.696589
13.570309	707.656315	12.701607
13.655275	704.853342	12.706624
13.828959	697.186018	12.711642
13.581823	693.712404	12.716659
13.330035	690.570877	12.721677
13.418665	694.536499	12.726695
13.560894	695.530438	12.731712
13.656925	718.224529	12.736730
13.777294	703.348257	12.741747
13.947879	714.695064	12.746765
13.982699	705.181264	12.751783
13.632317	697.394080	12.756800
13.516474	693.183531	12.761818
13.666999	692.109127	12.766835
13.680352	696.481019	12.771853
13.829677	709.125027	12.776871
13.652589	711.216720	12.781888
13.859365	714.040374	12.786906
13.844696	708.034102	12.791923
13.312537	713.958912	12.796941
13.655823	709.670110	12.801959
13.945861	715.980492	12.806976
13.930395	724.380543	12.811994
13.936180	714.628291	12.817011
13.543304	721.989257	12.822029
13.915364	725.509693	12.827047
14.172704	719.473422	12.832064
13.869248	717.577057	12.837082
14.061421	721.842042	12.842099
14.178531	723.950757	12.847117
14.217648	718.870170	12.852135
14.034724	721.953698	12.857152
13.868437	718.675694	12.862170
13.961606	712.494735	12.867187
14.114613	729.095545	12.872205
14.126917	713.567167	12.877223
14.030075	716.204863	12.882240
14.398340	723.897853	12.887258
14.281882	715.363956	12.892275
13.867933	696.737117	12.897293
13.596886	695.593067	12.902311
13.656290	716.146957	12.907328
13.962497	716.603966	12.912346
14.108016	725.329087	12.917363
14.072500	718.085850	12.922381
14.184840	723.325861	12.927399
14.069282	708.294046	12.932416
13.821599	709.756174	12.937434
14.194473	715.280409	12.942451
13.795606	719.672711	12.947469
14.086726	722.536800	12.952487
14.361096	723.020888	12.957504
14.147893	718.102910	12.962522
13.959432	721.796374	12.967539
14.028012	744.289673	12.972557
14.084388	741.213462	12.977575
14.301437	737.802810	12.982592
14.357707	748.820412	12.987610
14.609775	750.980569	12.992627
14.630845	743.977764	12.997645
14.681133	740.261881	13.002663
14.764120	725.397758	13.007680
14.412695	722.259214	13.012698
14.457226	717.670082	13.017715
14.318496	717.369986	13.022733
14.104228	728.038645	13.027751
14.459548	721.469471	13.032768
14.438853	738.832806	13.037786
14.700514	729.709485	13.042803
14.082925	722.809909	13.047821
14.287670	735.464188	13.052839
14.294687	738.199223	13.057856
14.579983	744.169533	13.062874
14.696214	741.203865	13.067891
14.341401	741.209023	13.072909
14.219330	740.694878	13.077927
14.511738	726.463816	13.082944
14.309040	744.104981	13.087962
14.504719	730.466582	13.092979
14.688786	743.897277	13.097997
14.537293	733.882479	13.103015
14.710293	734.205726	13.108032
14.851760	745.910564	13.113050
15.071829	734.966549	13.118067
14.436999	741.188320	13.123085
14.591810	744.143197	13.128103
14.676338	736.663394	13.133120
14.408609	740.628057	13.138138
14.510201	738.958560	13.143155
14.838189	740.709190	13.148173
14.578185	732.424993	13.153191
14.976677	732.422576	13.158208
14.622305	748.844126	13.163226
14.457375	746.695680	13.168243
14.678140	759.347466	13.173261
14.881488	758.990616	13.178279
15.214253	763.362971	13.183296
15.081250	763.566905	13.188314
15.202871	751.316024	13.193331
15.013752	742.225455	13.198349
15.013713	743.907560	13.203367
15.203189	733.280764	13.208384
14.546176	740.509554	13.213402
14.863784	734.400719	13.218419
15.134737	735.099937	13.223437
14.870648	743.314889	13.228455
15.114545	730.849204	13.233472
15.125970	737.796537	13.238490
14.927430	737.082935	13.243507
14.773138	734.159654	13.248525
14.757702	750.405025	13.253543
15.024415	748.905315	13.258560
15.257303	764.010417	13.263578
15.188895	766.163983	13.268595
15.609656	759.215313	13.273613
15.117247	745.220811	13.278631
15.364417	737.314738	13.283648
14.938764	738.034739	13.288666
15.035732	732.159289	13.293683
14.993563	747.831335	13.298701
15.076855	752.649873	13.303719
15.486723	754.457103	13.308736
15.027147	761.083767	13.313754
15.411219	757.672188	13.318771
15.552832	758.404295	13.323789
15.373394	757.504663	13.328807
15.611062	747.671880	13.333824
15.028262	738.040238	13.338842
14.968456	748.621592	13.343859
15.721273	747.566426	13.348877
15.691194	761.699716	13.353895
16.036739	744.998789	13.358912
15.579641	735.773485	13.363930
15.233015	727.944674	13.368947
15.622575	731.071051	13.373965
15.340552	740.125097	13.378983
15.619810	740.236036	13.384000
15.324477	726.999619	13.389018
15.416887	730.668013	13.394035
15.132458	735.992284	13.399053
15.071182	735.844153	13.404071
15.690337	740.263149	13.409088
15.158761	726.003400	13.414106
15.475774	742.868859	13.419123
16.179803	751.184594	13.424141
15.411426	745.555176	13.429159
15.913776	735.617814	13.434176
15.334993	726.919664	13.439194
15.516350	738.936983	13.444211
15.844183	738.863586	13.449229
15.618320	741.108092	13.454247
15.615524	741.042317	13.459264
15.624295	746.677257	13.464282
15.375068	750.156186	13.469299
16.188718	748.539224	13.474317
16.039248	745.583628	13.479335
15.931573	731.014461	13.484352
15.302647	732.470053	13.489370
15.398266	738.690985	13.494387
15.490847	743.725815	13.499405
15.700115	759.298515	13.504423
16.198454	747.556657	13.509440
15.773036	744.385520	13.514458
15.530931	755.405695	13.519475
15.897178	751.122753	13.524493
15.809177	752.951185	13.529511
16.012093	753.462248	13.534528
15.856537	749.649227	13.539546
15.871734	757.807804	13.544563
15.820927	750.604820	13.549581
15.762476	750.784450	13.554599
16.061236	740.512910	13.559616
15.786955	743.052180	13.564634
15.685754	757.398581	13.569651
15.710777	743.982570	13.574669
15.839263	741.283225	13.579687
15.903428	750.822678	13.584704
16.179235	750.574396	13.589722
15.855092	751.385789	13.594739
15.911406	754.416060	13.599757
16.227555	772.158996	13.604775
16.282267	769.420712	13.609792
15.831037	766.613378	13.614810
15.872422	773.442422	13.619827
16.298035	777.939088	13.624845
16.115514	781.492778	13.629863
16.270584	779.234231	13.634880
16.575166	768.425277	13.639898
16.241878	771.721721	13.644915
16.182421	777.332647	13.649933
16.309931	782.137953	13.654951
16.306554	772.554363	13.659968
16.179479	768.591708	13.664986
16.471698	769.480099	13.670003
16.534746	765.235193	13.675021
16.597007	773.670425	13.680039
16.318095	766.036115	13.685056
16.154777	759.377774	13.690074
16.243728	768.256946	13.695091
16.590515	771.285890	13.700109
16.390193	772.851055	13.705127
16.583740	774.373445	13.710144
16.319233	772.101742	13.715162
16.340792	777.362304	13.720179
16.490328	773.785498	13.725197
16.634113	771.885325	13.730215
16.140580	778.286942	13.735232
16.452596	772.898494	13.740250
16.348851	785.497001	13.745267
16.651535	779.766029	13.750285
16.427797	778.185372	13.755303
16.681784	778.221375	13.760320
16.540137	777.558817	13.765338
16.371675	783.537119	13.770355
16.600553	777.618896	13.775373
16.743263	769.110639	13.780391
16.757491	766.820511	13.785408
16.732046	769.762609	13.790426
16.424221	770.189595	13.795443
16.619503	762.048644	13.800461
16.461675	773.456412	13.805479
16.481087	770.196640	13.810496
16.530374	763.785853	13.815514
16.648792	778.018966	13.820531
16.903497	786.442987	13.825549
16.895663	788.978385	13.830567
17.108621	783.289873	13.835584
16.826765	766.803992	13.840602
16.468418	778.782823	13.845619
16.772970	793.236092	13.850637
17.159363	801.421737	13.855655
17.135786	782.900903	13.860672
17.024074	774.909032	13.865690
16.695934	776.024010	13.870707
16.865469	778.582110	13.875725
17.023945	780.406640	13.880743
16.847928	784.407436	13.885760
17.267288	787.529153	13.890778
17.021510	783.039139	13.895795
16.875753	776.071927	13.900813
16.925892	793.373725	13.905831
17.090244	788.784736	13.910848
17.182302	793.160098	13.915866
17.168161	801.045581	13.920883
17.090039	785.465036	13.925901
17.255136	787.929158	13.930919
17.094648	789.920430	13.935936
17.162869	791.348848	13.940954
17.063861	794.898923	13.945971
17.220479	785.274479	13.950989
17.555677	793.543881	13.956007
17.478624	793.549700	13.961024
17.770281	779.975122	13.966042
17.329418	777.570104	13.971059
17.412426	765.015994	13.976077
17.080219	770.846378	13.981095
17.066187	761.643160	13.986112
17.030689	760.342278	13.991130
16.870359	782.521197	13.996147
17.659992	781.109968	14.001165
17.391262	791.124478	14.006183
17.088207	795.037883	14.011200
17.248048	791.140723	14.016218
17.654577	789.170979	14.021235
17.561980	786.733484	14.026253
17.531965	792.194635	14.031271
17.440538	794.891455	14.036288
17.487930	792.271080	14.041306
17.358315	795.096960	14.046323
17.203172	791.735145	14.051341
17.300537	801.941610	14.056359
17.221691	798.700384	14.061376
17.263376	785.281732	14.066394
17.342144	785.266293	14.071411
17.438357	799.057933	14.076429
17.856137	813.884799	14.081447
17.606644	816.183509	14.086464
17.660766	812.063067	14.091482
17.822608	828.088228	14.096499
17.862070	819.968509	14.101517
17.888940	808.414090	14.106535
17.550144	800.082246	14.111552
17.739059	799.550932	14.116570
17.831672	807.299770	14.121587
17.670221	819.544425	14.126605
17.902186	816.213472	14.131623
17.840392	814.749449	14.136640
18.220194	809.848986	14.141658
17.969428	804.652847	14.146675
17.581463	795.981570	14.151693
17.664711	795.122829	14.156711
17.609170	805.501577	14.161728
17.784844	805.609810	14.166746
18.019224	808.126196	14.171763
17.765473	805.268980	14.176781
18.069789	807.812278	14.181799
17.916677	808.505358	14.186816
17.954452	806.110550	14.191834
18.305436	809.722668	14.196851
18.189481	805.729860	14.201869
18.003360	811.568926	14.206887
17.817168	812.851014	14.211904
18.179693	797.652699	14.216922
18.423536	800.038213	14.221939
18.138808	806.807912	14.226957
18.175600	806.164733	14.231975
18.197952	804.927368	14.236992
18.395113	818.662181	14.242010
18.442618	804.068641	14.247027
18.414826	805.082913	14.252045
18.964546	802.087186	14.257063
18.056336	790.751870	14.262080
18.027904	789.844355	14.267098
17.471763	786.895664	14.272115
17.784151	802.982422	14.277133
18.121988	800.849870	14.282151
18.060605	807.534083	14.287168
18.100875	801.004775	14.292186
18.313719	812.846797	14.297203
18.209895	810.436304	14.302221
18.424676	814.347474	14.307239
18.283990	809.837832	14.312256
18.412679	803.316760	14.317274
18.686127	819.968212	14.322291
18.323377	819.173037	14.327309
18.543119	824.696052	14.332327
18.700993	830.077283	14.337344
18.981464	821.790414	14.342362
18.728504	817.989484	14.347379
18.277341	818.240112	14.352397
18.406365	805.495727	14.357415
18.468665	811.292715	14.362432
18.835505	815.659744	14.367450
18.448286	814.035269	14.372467
18.429892	819.109599	14.377485
19.165283	819.186941	14.382503
18.674861	819.566797	14.387520
18.842348	816.185986	14.392538
18.952342	815.020095	14.397555
18.861141	814.059298	14.402573
18.591299	799.171500	14.407591
18.736665	802.869481	14.412608
18.845422	811.436302	14.417626
19.088838	812.758377	14.422643
18.632807	810.781766	14.427661
18.992349	808.387036	14.432679
18.984231	805.936303	14.437696
18.960441	805.567703	14.442714
18.824520	794.518482	14.447731
18.933289	806.266353	14.452749
19.117796	811.349915	14.457767
18.995521	813.802262	14.462784
18.847336	803.998346	14.467802
19.093565	812.508915	14.472819
18.983202	817.834339	14.477837
19.089248	817.088790	14.482855
19.278248	826.002809	14.487872
18.776257	815.345446	14.492890
19.015375	812.660315	14.497907
18.834200	816.081257	14.502925
19.172343	818.253182	14.507943
19.029449	821.576609	14.512960
19.338050	821.105437	14.517978
19.557851	818.183490	14.522995
19.296630	822.573185	14.528013
19.524171	821.470929	14.533031
19.359656	808.444329	14.538048
19.121479	809.251723	14.543066
19.123088	812.763946	14.548083
19.327681	815.480661	14.553101
19.421648	821.591427	14.558119
19.346334	823.673499	14.563136
19.263354	825.280245	14.568154
19.462491	828.657381	14.573171
19.529179	825.891966	14.578189
19.458257	817.480274	14.583207
19.297169	815.539501	14.588224
19.219689	824.302766	14.593242
19.642544	818.309957	14.598259
19.398498	818.038983	14.603277
19.603156	822.974224	14.608295
19.428960	830.805902	14.613312
19.406493	821.597662	14.618330
19.691899	820.956555	14.623347
19.254437	825.837770	14.628365
19.704922	828.875722	14.633383
19.389535	825.406464	14.638400
19.646347	818.944207	14.643418
19.681797	817.569090	14.648435
19.378954	825.749126	14.653453
19.682640	825.925666	14.658471
19.601708	819.806661	14.663488
19.880596	828.570897	14.668506
20.153849	816.356174	14.673523
19.788306	830.324328	14.678541
20.000805	829.192869	14.683559
19.771025	832.640365	14.688576
19.621413	829.533297	14.693594
19.809640	827.818660	14.698611
19.477050	830.777334	14.703629
19.651168	823.747362	14.708647
19.663603	820.558102	14.713664
19.445545	823.416778	14.718682
19.883902	827.428621	14.723699
19.791912	838.725129	14.728717
19.785342	841.509646	14.733735
19.986054	849.639199	14.738752
19.861231	849.497868	14.743770
19.966015	837.820769	14.748787
20.104545	849.425149	14.753805
19.822102	843.716407	14.758823
19.520539	845.063911	14.763840
19.798661	848.952541	14.768858
19.852693	838.605680	14.773875
20.063239	862.310809	14.778893
20.203810	865.135393	14.783911
20.288956	868.811264	14.788928
20.693307	868.006352	14.793946
20.717579	850.541461	14.798963
19.819705	842.653801	14.803981
20.390262	840.282810	14.808999
20.369394	838.982787	14.814016
20.218533	847.984779	14.819034
20.361277	839.627962	14.824051
20.191850	835.356347	14.829069
20.410046	845.897357	14.834087
20.350654	857.356027	14.839104
20.584845	867.733597	14.844122
20.615378	847.358063	14.849139
20.224213	847.425721	14.854157
20.349168	848.375037	14.859175
20.540933	858.169112	14.864192
20.394183	865.570469	14.869210
20.925123	857.641973	14.874227
20.243420	855.476652	14.879245
20.136166	853.088781	14.884263
20.622356	852.854873	14.889280
20.341333	862.457937	14.894298
20.751130	856.101086	14.899315
20.635609	865.334237	14.904333
21.081099	866.192307	14.909351
20.975981	858.249859	14.914368
20.769175	869.785283	14.919386
20.859449	863.633127	14.924403
20.813176	856.116964	14.929421
20.980160	858.445100	14.934439
20.745512	850.267329	14.939456
20.679312	862.099456	14.944474
20.656947	859.947594	14.949491
20.770342	863.300301	14.954509
20.649794	861.656130	14.959527
21.188407	854.401779	14.964544
20.864822	864.333406	14.969562
20.798714	863.807333	14.974579
20.851064	865.156192	14.979597
20.571919	858.613792	14.984615
20.863085	857.350085	14.989632
20.790770	865.393034	14.994650
20.877396	859.061570	14.999667
20.922311	863.747295	15.004685
20.928588	858.135323	15.009703
21.278355	857.572494	15.014720
20.766551	853.928876	15.019738
20.907257	852.212215	15.024755
20.608555	864.708780	15.029773
20.931498	871.443254	15.034791
21.111130	872.611224	15.039808
21.290004	874.653476	15.044826
21.215687	871.108568	15.049843
21.160111	876.643177	15.054861
21.089255	887.961652	15.059879
20.999104	876.356095	15.064896
21.315862	877.092324	15.069914
21.284711	876.494501	15.074931
21.549160	881.890608	15.079949
20.934425	886.326241	15.084967
21.359761	870.893959	15.089984
21.330857	885.238603	15.095002
21.669408	877.419137	15.100019
21.869886	879.186604	15.105037
21.433487	884.922895	15.110055
21.859548	875.518120	15.115072
21.507263	877.703554	15.120090
21.811111	877.990524	15.125107
21.619338	879.106232	15.130125
21.805703	881.548100	15.135143
21.901897	877.439985	15.140160
21.594420	876.513071	15.145178
21.957216	870.397109	15.150195
22.075358	879.423243	15.155213
21.834290	872.975858	15.160231
22.247659	871.229097	15.165248
21.916092	876.829040	15.170266
21.811876	857.257251	15.175283
21.615190	853.463274	15.180301
21.664182	864.945994	15.185319
21.960720	870.027799	15.190336
22.000570	874.376647	15.195354
21.673002	864.291533	15.200371
21.570881	858.043291	15.205389
21.608630	860.186548	15.210407
21.658689	860.352333	15.215424
21.584272	864.267801	15.220442
22.030248	869.711202	15.225459
21.923370	867.638853	15.230477
21.835204	874.062198	15.235495
21.953781	867.479571	15.240512
21.809940	870.983036	15.245530
21.779520	866.572868	15.250547
22.057541	873.020890	15.255565
21.788192	876.572424	15.260583
22.435702	883.915617	15.265600
22.272819	893.250877	15.270618
22.627010	877.009223	15.275635
22.162472	876.864313	15.280653
21.931260	875.695074	15.285671
22.171633	871.362398	15.290688
22.290021	882.032677	15.295706
22.053756	884.559698	15.300723
21.906871	893.510598	15.305741
21.996854	897.340353	15.310759
22.398963	887.144056	15.315776
22.412384	890.954248	15.320794
22.402796	885.461519	15.325811
22.508581	894.426480	15.330829
22.363322	900.123472	15.335847
22.516287	887.776067	15.340864
22.477542	895.529746	15.345882
22.671490	896.048531	15.350899
22.392980	897.203077	15.355917
22.346211	894.095664	15.360935
22.594091	889.272655	15.365952
22.378484	890.426812	15.370970
22.226585	897.443979	15.375987
22.320768	892.446233	15.381005
22.528239	902.869036	15.386023
22.443081	913.956236	15.391040
22.873794	916.397695	15.396058
22.887986	921.441701	15.401075
23.055104	912.399372	15.406093
22.614371	913.768686	15.411111
22.825485	909.860311	15.416128
22.590976	916.776818	15.421146
22.929990	912.949389	15.426163
23.099695	901.722827	15.431181
22.681082	912.250042	15.436199
22.974519	909.439619	15.441216
23.422504	902.114241	15.446234
23.228375	897.048057	15.451251
23.054905	889.109993	15.456269
22.804102	888.246781	15.461287
23.306097	881.190662	15.466304
23.132661	880.447874	15.471322
23.361333	884.353727	15.476339
23.456119	879.220190	15.481357
23.048548	877.059252	15.486375
23.285628	874.188237	15.491392
23.129544	882.099151	15.496410
22.901660	876.407097	15.501427
23.420672	879.532152	15.506445
23.273035	883.149825	15.511463
23.203311	865.503986	15.516480
22.846839	871.786331	15.521498
22.960923	876.114081	15.526515
22.888696	867.746751	15.531533
23.224086	892.524274	15.536551
23.013735	892.989638	15.541568
23.354641	905.455446	15.546586
23.165248	892.199151	15.551603
23.466640	889.286499	15.556621
23.320501	901.014411	15.561639
23.365569	902.190844	15.566656
23.433988	904.509183	15.571674
23.742200	908.462540	15.576691
24.065716	904.448191	15.581709
23.755064	899.826299	15.586727
24.108392	891.509048	15.591744
23.929451	881.053496	15.596762
23.627337	873.025141	15.601779
23.776660	878.855854	15.606797
23.620959	873.824681	15.611815
23.597313	871.243827	15.616832
23.581569	872.511837	15.621850
23.564100	883.850346	15.626867
24.006070	886.207985	15.631885
24.091834	892.070752	15.636903
24.159455	876.334747	15.641920
23.522670	871.669287	15.646938
23.480101	872.120986	15.651955
23.728595	876.752727	15.656973
23.863777	891.002238	15.661991
24.293285	895.858089	15.667008
24.222995	895.790265	15.672026
23.692063	892.155948	15.677043
24.010880	893.696590	15.682061
23.623005	899.557829	15.687079
23.856749	896.526386	15.692096
24.034761	895.173107	15.697114
23.925371	905.809660	15.702131
24.486961	893.843200	15.707149
24.125431	895.925943	15.712167
23.992256	900.093622	15.717184
24.059874	900.171450	15.722202
24.078534	896.280607	15.727219
23.926215	891.958960	15.732237
24.393435	895.508702	15.737255
24.131669	896.064174	15.742272
24.061935	899.155244	15.747290
24.074467	895.988047	15.752307
24.066788	896.289112	15.757325
24.386340	921.990658	15.762343
24.541937	916.983283	15.767360
24.498958	916.545104	15.772378
24.506826	920.141575	15.777395
24.597263	905.124656	15.782413
24.568116	920.381400	15.787431
24.531635	915.703924	15.792448
24.475399	898.207419	15.797466
24.420707	916.068563	15.802483
24.616831	918.007130	15.807501
24.612025	907.650513	15.812519
24.902586	910.385331	15.817536
24.746610	922.562926	15.822554
24.821801	915.182342	15.827571
24.707849	895.428998	15.832589
24.562063	904.954091	15.837607
24.565163	920.436158	15.842624
24.816949	926.389689	15.847642
24.542837	928.354597	15.852659
24.464868	922.070989	15.857677
24.632925	922.473910	15.862695
24.819177	917.884613	15.867712
24.839057	917.960452	15.872730
24.616832	918.247795	15.877747
24.938651	916.777309	15.882765
25.028752	917.596389	15.887783
24.827195	919.265903	15.892800
24.549093	921.947809	15.897818
24.576013	922.896710	15.902835
24.979210	928.047029	15.907853
25.039514	945.315823	15.912871
25.272064	943.180816	15.917888
25.340016	940.667652	15.922906
25.302437	948.651547	15.927923
25.337102	948.207514	15.932941
25.020765	934.658649	15.937959
25.093514	940.706509	15.942976
25.222002	933.743604	15.947994
24.905015	947.552762	15.953011
25.053915	946.541715	15.958029
24.906375	945.905320	15.963047
25.092856	939.362521	15.968064
25.537858	943.569011	15.973082
25.344228	940.702352	15.978099
25.124955	940.209742	15.983117
25.049318	941.010610	15.988135
25.595933	960.494359	15.993152
25.713409	951.633359	15.998170
25.593373	962.202186	16.003187
25.476957	953.141143	16.008205
25.680169	950.089228	16.013223
25.633720	935.873222	16.018240
25.649850	937.041567	16.023258
25.588145	947.143650	16.028275
25.452422	961.744935	16.033293
25.912988	969.426726	16.038311
25.914095	968.388340	16.043328
26.236426	953.723216	16.048346
25.663683	946.980628	16.053363
25.739994	941.846812	16.058381
25.597347	942.957983	16.063399
25.492694	954.799352	16.068416
25.964300	959.623378	16.073434
25.749500	960.862621	16.078451
26.070786	963.665217	16.083469
25.780680	961.517423	16.088487
25.813410	965.583384	16.093504
25.778359	954.628713	16.098522
25.972120	963.005562	16.103539
25.957034	959.325123	16.108557
26.178682	959.344103	16.113575
25.954390	960.771028	16.118592
26.096228	954.875852	16.123610
26.112741	963.823276	16.128627
26.081053	954.259803	16.133645
26.556727	957.786143	16.138663
26.524555	964.140786	16.143680
26.485739	953.880990	16.148698
26.270006	961.899116	16.153715
26.384775	959.306029	16.158733
26.501474	962.251135	16.163751
26.051381	953.277086	16.168768
26.183665	952.820914	16.173786
26.365781	957.573530	16.178803
26.342547	955.664792	16.183821
26.507483	960.817737	16.188839
26.387090	961.846527	16.193856
26.101732	957.249059	16.198874
26.116937	976.074465	16.203891
26.602817	972.858336	16.208909
26.725941	981.751196	16.213927
26.646306	982.215017	16.218944
26.565650	972.974790	16.223962
26.595628	981.049102	16.228979
26.711252	978.670476	16.233997
26.670544	980.952274	16.239015
26.945348	985.731401	16.244032
26.939556	980.335879	16.249050
26.826098	985.008580	16.254067
27.007649	977.223137	16.259085
27.075027	972.014972	16.264103
26.786576	980.009785	16.269120
27.273450	972.886571	16.274138
26.683766	976.737625	16.279155
26.742248	982.058735	16.284173
27.129667	978.832785	16.289191
27.339617	981.532907	16.294208
27.262113	979.657917	16.299226
27.186662	974.743531	16.304243
27.342929	971.178254	16.309261
27.168692	957.076928	16.314279
26.548570	961.784824	16.319296
26.321897	966.263817	16.324314
27.118104	967.587656	16.329331
26.958559	970.452967	16.334349
27.315428	967.452714	16.339367
26.967965	981.547543	16.344384
27.177684	980.009407	16.349402
27.061002	971.052540	16.354419
26.863564	995.449780	16.359437
27.345667	991.890253	16.364455
27.292162	1001.394627	16.369472
27.424544	1000.957373	16.374490
27.310825	1002.947652	16.379507
27.316747	999.970822	16.384525
27.388180	997.971507	16.389543
27.411917	1004.645613	16.394560
27.731703	993.581673	16.399578
28.017124	992.934246	16.404595
27.737532	993.675553	16.409613
27.681867	989.771088	16.414631
27.711192	1002.143769	16.419648
28.018634	997.185165	16.424666
27.515189	997.507103	16.429683
27.377517	990.159839	16.434701
27.753335	993.906961	16.439719
27.764923	998.392813	16.444736
27.634818	991.075922	16.449754
27.728323	995.343809	16.454771
27.865667	990.749533	16.459789
28.232579	991.376922	16.464807
27.905839	991.576499	16.469824
28.203140	993.016378	16.474842
28.043900	992.277673	16.479859
27.774715	993.137270	16.484877
28.023218	989.645902	16.489895
28.007126	1006.131453	16.494912
28.742787	1000.190560	16.499930
28.507115	992.546221	16.504947
28.298776	987.693679	16.509965
28.458524	988.060033	16.514983
28.517814	989.843320	16.520000
28.431808	992.154307	16.525018
28.303068	987.021047	16.530035
28.314932	986.470130	16.535053
28.436679	979.748108	16.540071
28.435534	986.419794	16.545088
28.643667	978.232550	16.550106
28.374008	980.035817	16.555123
28.366127	984.158638	16.560141
28.582618	977.623746	16.565159
28.698583	983.964654	16.570176
28.720067	974.212957	16.575194
28.559221	984.374775	16.580211
28.627058	987.220242	16.585229
29.104269	976.365180	16.590247
28.636761	981.702429	16.595264
28.772921	977.767912	16.600282
28.757891	975.898913	16.605299
28.811734	981.741463	16.610317
28.921777	980.487191	16.615335
28.809219	977.377447	16.620352
28.364162	974.979370	16.625370
28.437084	974.062278	16.630387
28.646527	980.555798	16.635405
28.722232	968.305650	16.640423
28.666285	975.860086	16.645440
28.783920	975.014884	16.650458
28.909398	968.308060	16.655475
28.532787	978.323798	16.660493
28.760641	981.743802	16.665511
28.833513	996.306122	16.670528
28.915811	994.579663	16.675546
29.289182	993.826937	16.680563
29.027681	1004.944979	16.685581
29.377105	999.329693	16.690599
29.107220	999.662375	16.695616
29.164745	992.587488	16.700634
29.321359	996.659292	16.705651
29.081724	1000.143078	16.710669
29.200743	991.190297	16.715687
29.468866	999.085292	16.720704
29.212448	994.057242	16.725722
29.311698	986.622365	16.730739
29.015368	1001.182573	16.735757
29.389520	994.383129	16.740775
29.429579	999.599832	16.745792
29.560489	1002.536406	16.750810
29.598711	998.610918	16.755827
29.603740	1011.517594	16.760845
29.796280	1005.040093	16.765863
29.731439	992.575261	16.770880
29.676292	989.557507	16.775898
29.729014	992.730395	16.780915
29.281252	994.242828	16.785933
29.612003	1011.450379	16.790951
29.554236	1011.109189	16.795968
29.540939	1018.161493	16.800986
30.131940	1010.842065	16.806003
29.813026	1013.325249	16.811021
29.742365	1009.082298	16.816039
29.782236	1012.112034	16.821056
30.021192	1011.913705	16.826074
30.503703	1010.329670	16.831091
30.229980	1012.565928	16.836109
30.404948	1008.341298	16.841127
30.030730	1011.855640	16.846144
29.824574	1014.595715	16.851162
30.229216	1014.743817	16.856179
30.238679	1018.141240	16.861197
30.077263	1017.693212	16.866215
30.298455	1011.586766	16.871232
29.736141	1011.087940	16.876250
30.065997	1009.366875	16.881267
30.368565	1003.910409	16.886285
30.266844	1009.240848	16.891303
30.624521	1008.269672	16.896320
30.339772	1017.393714	16.901338
30.431159	1018.850079	16.906355
30.252057	1012.765324	16.911373
30.138895	1008.939293	16.916391
30.547601	1019.756674	16.921408
30.617868	1025.432562	16.926426
30.666239	1022.783597	16.931443
30.196498	1026.811532	16.936461
30.407630	1028.009292	16.941479
30.590070	1035.753623	16.946496
30.461048	1033.104048	16.951514
30.560411	1033.773358	16.956531
30.359478	1038.027427	16.961549
30.357719	1036.954772	16.966567
30.679511	1029.576529	16.971584
30.592075	1042.008558	16.976602
30.818871	1050.541221	16.981619
30.901707	1053.933467	16.986637
31.036018	1057.333427	16.991655
30.964118	1065.606779	16.996672
31.292858	1057.362732	17.001690
31.382685	1044.425499	17.006707
31.434236	1033.065886	17.011725
31.262456	1027.500694	17.016743
30.982940	1032.350905	17.021760
31.016336	1026.116085	17.026778
31.297511	1028.846081	17.031795
31.011182	1037.923043	17.036813
30.939667	1037.309449	17.041831
31.555422	1050.126777	17.046848
31.156963	1056.620895	17.051866
31.533251	1047.694050	17.056883
31.350447	1055.631318	17.061901
31.469493	1057.307418	17.066919
31.740288	1050.038144	17.071936
31.405784	1046.101615	17.076954
31.607909	1033.916823	17.081971
31.339925	1041.548690	17.086989
31.510286	1048.461775	17.092007
31.574609	1051.288867	17.097024
31.894002	1054.050749	17.102042
31.983878	1038.027089	17.107059
31.517908	1044.332961	17.112077
31.845713	1051.846238	17.117095
31.965384	1037.105498	17.122112
31.858915	1034.417675	17.127130
31.588999	1021.988109	17.132147
31.504085	1033.646554	17.137165
31.679697	1051.632698	17.142183
31.944933	1055.911563	17.147200
31.642748	1055.902163	17.152218
31.868912	1050.533394	17.157235
32.040003	1055.773766	17.162253
31.911330	1059.259113	17.167271
31.888250	1054.263915	17.172288
31.587461	1058.296944	17.177306
32.173923	1054.941964	17.182323
32.122865	1052.504236	17.187341
32.155454	1052.155201	17.192359
32.396058	1051.230767	17.197376
32.136557	1051.505017	17.202394
32.138379	1045.193085	17.207411
32.024674	1052.917551	17.212429
32.258660	1071.421597	17.217447
32.434422	1070.526257	17.222464
32.462510	1083.025423	17.227482
32.236783	1078.762569	17.232499
32.462298	1083.025573	17.237517
32.093898	1081.729489	17.242535
32.363348	1070.319933	17.247552
32.149178	1075.412386	17.252570
32.497342	1070.403199	17.257587
32.641825	1073.965674	17.262605
32.647605	1072.128118	17.267623
32.700905	1069.232217	17.272640
32.485550	1084.171133	17.277658
32.804621	1077.115195	17.282675
32.751258	1079.926016	17.287693
32.558783	1079.435515	17.292711
32.995343	1070.013213	17.297728
33.022169	1076.705797	17.302746
32.613386	1074.365140	17.307763
32.771457	1080.869902	17.312781
32.771764	1088.481845	17.317799
32.821181	1093.779161	17.322816
32.980469	1102.549648	17.327834
33.334259	1094.197517	17.332851
33.419068	1089.374757	17.337869
33.280863	1089.065104	17.342887
32.998012	1084.773328	17.347904
33.241794	1091.592875	17.352922
32.982947	1091.838620	17.357939
33.272440	1089.044567	17.362957
33.077573	1092.909527	17.367975
33.542747	1092.265493	17.372992
33.418181	1085.184384	17.378010
33.325504	1085.239989	17.383027
33.297645	1087.453515	17.388045
33.198186	1093.383238	17.393063
33.531802	1088.426820	17.398080
33.417202	1087.472829	17.403098
33.505405	1085.047992	17.408115
33.758060	1084.588736	17.413133
33.462738	1083.663061	17.418151
33.502025	1083.376092	17.423168
33.262959	1083.363114	17.428186
33.439076	1098.632032	17.433203
33.635209	1102.707137	17.438221
33.606553	1109.077061	17.443239
33.958732	1102.239992	17.448256
33.691203	1109.808699	17.453274
33.861288	1108.734363	17.458291
33.980056	1099.219823	17.463309
33.912977	1104.257680	17.468327
33.709860	1104.115990	17.473344
34.240653	1096.553493	17.478362
33.787658	1094.626866	17.483379
34.152328	1097.624662	17.488397
33.759373	1098.014498	17.493415
33.949676	1090.893522	17.498432
33.934471	1104.538751	17.503450
34.147215	1121.102165	17.508467
34.189507	1118.864401	17.513485
34.183898	1125.278057	17.518503
34.695131	1127.788983	17.523520
34.569645	1122.973916	17.528538
34.761937	1125.332837	17.533555
34.699299	1105.467076	17.538573
34.684947	1100.959657	17.543591
34.780788	1084.966578	17.548608
34.399441	1098.022218	17.553626
34.327338	1096.020134	17.558643
34.626867	1091.100614	17.563661
34.439001	1101.680151	17.568679
34.899511	1096.060053	17.573696
34.463923	1101.610091	17.578714
34.730155	1101.126616	17.583731
35.080763	1114.310587	17.588749
34.901424	1105.697990	17.593767
34.713445	1088.947787	17.598784
34.383333	1102.276274	17.603802
34.947201	1113.154611	17.608819
34.944567	1109.560554	17.613837
34.840941	1121.474457	17.618855
35.121437	1117.883376	17.623872
34.919232	1119.332099	17.628890
34.965460	1113.922075	17.633907
35.069957	1120.135438	17.638925
35.015361	1123.489268	17.643943
34.955220	1113.153824	17.648960
35.123910	1111.240247	17.653978
35.010982	1119.116101	17.658995
35.201741	1109.804875	17.664013
34.856393	1119.427623	17.669031
34.820805	1124.280667	17.674048
35.153758	1129.839689	17.679066
35.033670	1136.441703	17.684083
35.224996	1149.707462	17.689101
34.956805	1150.693146	17.694119
35.583819	1139.735618	17.699136
35.312648	1142.195558	17.704154
35.405791	1142.708054	17.709171
35.711063	1150.657257	17.714189
35.879189	1164.185444	17.719207
35.804345	1147.370122	17.724224
35.790079	1134.572212	17.729242
35.622663	1138.852611	17.734259
36.203547	1149.027701	17.739277
35.668803	1145.475980	17.744295
36.180735	1141.895971	17.749312
35.790750	1142.957543	17.754330
35.913777	1149.493067	17.759347
36.456949	1147.517657	17.764365
35.924848	1146.793181	17.769383
36.096731	1134.865528	17.774400
36.075332	1142.954275	17.779418
36.194052	1156.395520	17.784435
36.628954	1146.247588	17.789453
36.074497	1138.328078	17.794471
36.221569	1130.951922	17.799488
36.127514	1133.548217	17.804506
36.214071	1147.445783	17.809523
36.605416	1151.786966	17.814541
36.375924	1163.376628	17.819559
36.531233	1158.536492	17.824576
36.503740	1161.725133	17.829594
36.716407	1160.934462	17.834611
36.287261	1141.631025	17.839629
36.570220	1151.060671	17.844647
36.645699	1156.142480	17.849664
36.818180	1151.990791	17.854682
36.592968	1156.087742	17.859699
36.936025	1159.388743	17.864717
37.023966	1163.685945	17.869735
36.947249	1145.488646	17.874752
36.843094	1132.184102	17.879770
36.502219	1124.524631	17.884787
36.881878	1144.334548	17.889805
36.739678	1155.427680	17.894823
36.741143	1150.043594	17.899840
36.811268	1155.369243	17.904858
36.613693	1154.601822	17.909875
36.629686	1148.571662	17.914893
36.701776	1154.878479	17.919911
36.754334	1151.121128	17.924928
37.046582	1147.954242	17.929946
36.723066	1170.512669	17.934963
37.088404	1166.419125	17.939981
37.110196	1179.121320	17.944999
37.211253	1174.914543	17.950016
37.180702	1172.685029	17.955034
37.148912	1180.194739	17.960051
37.389522	1172.008630	17.965069
37.165812	1172.245716	17.970087
37.329910	1179.519603	17.975104
37.350151	1175.887233	17.980122
37.617695	1190.731643	17.985139
37.972542	1195.233193	17.990157
37.863731	1177.997120	17.995175
37.264964	1175.597851	18.000192
38.030895	1183.522233	18.005210
37.455441	1184.906362	18.010227
37.742394	1190.198049	18.015245
38.089812	1195.887373	18.020263
38.018698	1196.602335	18.025280
38.015587	1184.989251	18.030298
37.966221	1187.707943	18.035315
38.168080	1183.330733	18.040333
37.641978	1178.502677	18.045351
37.587200	1194.180247	18.050368
38.169855	1192.069254	18.055386
37.965810	1196.121871	18.060403
37.866738	1192.303060	18.065421
38.279249	1195.331248	18.070439
38.054142	1196.865619	18.075456
38.400261	1204.085750	18.080474
38.001810	1206.051233	18.085491
38.574396	1196.310901	18.090509
38.210117	1196.790922	18.095527
38.284427	1193.317339	18.100544
38.277941	1189.951092	18.105562
38.408734	1197.832978	18.110579
38.853185	1209.610574	18.115597
39.093198	1203.261267	18.120615
38.768012	1197.325572	18.125632
38.940236	1190.699706	18.130650
38.820284	1191.258214	18.135667
38.711904	1185.121293	18.140685
39.105509	1188.155597	18.145703
39.103134	1184.255364	18.150720
38.960131	1172.601089	18.155738
38.668326	1189.189969	18.160755
38.958755	1176.852386	18.165773
39.026005	1179.170944	18.170791
38.768185	1179.697402	18.175808
38.995932	1174.596598	18.180826
38.911535	1185.216778	18.185843
39.056437	1186.882528	18.190861
39.411515	1176.188496	18.195879
38.901756	1178.827838	18.200896
39.328754	1187.275549	18.205914
39.187613	1197.103035	18.210931
38.902892	1201.446010	18.215949
38.862253	1206.789029	18.220967
39.353047	1207.053027	18.225984
39.512711	1210.168171	18.231002
39.529042	1206.665799	18.236019
39.655754	1213.099782	18.241037
39.175799	1206.752821	18.246055
39.455273	1205.645561	18.251072
39.843399	1198.708147	18.256090
39.575338	1203.906912	18.261107
39.816893	1206.438011	18.266125
39.646593	1202.810242	18.271143
39.484290	1210.955811	18.276160
39.493530	1197.497749	18.281178
39.657717	1210.367010	18.286195
39.738159	1232.013290	18.291213
40.030186	1234.211429	18.296231
39.956341	1242.096994	18.301248
39.868800	1233.368964	18.306266
39.811784	1236.432853	18.311283
39.782746	1235.449669	18.316301
40.136870	1231.578779	18.321319
40.163883	1234.055131	18.326336
39.973313	1235.719797	18.331354
39.914484	1227.242898	18.336371
39.942704	1236.917635	18.341389
40.210636	1237.749895	18.346407
39.850695	1238.516423	18.351424
40.531123	1249.143045	18.356442
40.675917	1258.932077	18.361459
40.457291	1259.887909	18.366477
40.625877	1255.200305	18.371495
40.553424	1259.872964	18.376512
40.821879	1257.738607	18.381530
40.883169	1255.103364	18.386547
40.816728	1247.110499	18.391565
41.073476	1249.591886	18.396583
40.619474	1239.608420	18.401600
41.229075	1229.975882	18.406618
40.675590	1233.117556	18.411635
40.490601	1227.036805	18.416653
40.807781	1232.547838	18.421671
40.594908	1245.280535	18.426688
40.742069	1242.003817	18.431706
40.483456	1258.423455	18.436723
40.435435	1244.778664	18.441741
41.075182	1251.327944	18.446759
41.027508	1266.894009	18.451776
41.309648	1272.208566	18.456794
41.428884	1258.562807	18.461811
41.307999	1267.393052	18.466829
41.492043	1266.610017	18.471847
41.296053	1272.277205	18.476864
41.363625	1276.943709	18.481882
41.410159	1273.701688	18.486899
41.453406	1265.925165	18.491917
41.916013	1267.250803	18.496935
41.562244	1273.611762	18.501952
41.649990	1266.768723	18.506970
41.822482	1265.807612	18.511987
41.914135	1270.801711	18.517005
41.766029	1269.133416	18.522023
41.978252	1263.261826	18.527040
42.250894	1268.991293	18.532058
41.981572	1263.460244	18.537075
41.678581	1263.536178	18.542093
41.818495	1265.357356	18.547111
41.843135	1267.666822	18.552128
42.014587	1268.785607	18.557146
41.777222	1263.426281	18.562163
41.652492	1263.710977	18.567181
41.703006	1263.188711	18.572199
41.916872	1267.699745	18.577216
42.342445	1272.177610	18.582234
42.208911	1275.117791	18.587251
42.194277	1278.433830	18.592269
42.378891	1282.921048	18.597287
42.216665	1293.045387	18.602304
42.330924	1291.705224	18.607322
42.605574	1287.225063	18.612339
42.425378	1287.789856	18.617357
42.534328	1283.395619	18.622375
42.047977	1294.953024	18.627392
42.570276	1285.627633	18.632410
42.696920	1286.646139	18.637427
42.119926	1294.929304	18.642445
42.700445	1281.949734	18.647463
42.542222	1289.195269	18.652480
42.510132	1307.129004	18.657498
42.916028	1307.172769	18.662515
42.763060	1308.607481	18.667533
43.085156	1306.856045	18.672551
43.205654	1314.401914	18.677568
43.306218	1312.041383	18.682586
43.296274	1303.414774	18.687603
43.216878	1306.378037	18.692621
43.562057	1298.194422	18.697639
43.704877	1301.896063	18.702656
43.612925	1276.354090	18.707674
43.462869	1285.633895	18.712691
43.103669	1270.595595	18.717709
43.543743	1274.272748	18.722727
43.264164	1266.183878	18.727744
43.495726	1283.157917	18.732762
43.871691	1284.749603	18.737779
43.519213	1274.851199	18.742797
43.829779	1280.356971	18.747815
43.282714	1288.158904	18.752832
43.757989	1294.276364	18.757850
43.777838	1301.468758	18.762867
43.800460	1291.366404	18.767885
43.633795	1294.557938	18.772903
43.575988	1288.308913	18.777920
43.714503	1283.957383	18.782938
43.847998	1291.356035	18.787955
43.464084	1290.712479	18.792973
44.202494	1294.128293	18.797991
44.078454	1288.757516	18.803008
43.646759	1288.616923	18.808026
44.019667	1307.860020	18.813043
44.166811	1309.749499	18.818061
44.269600	1314.262168	18.823079
44.254524	1317.180640	18.828096
44.281074	1312.679382	18.833114
44.313991	1309.117586	18.838131
44.321538	1312.288140	18.843149
44.538316	1302.439391	18.848167
44.768264	1312.603286	18.853184
44.354023	1311.942390	18.858202
44.680027	1315.413355	18.863219
44.043712	1317.573912	18.868237
44.173360	1326.046187	18.873255
44.410592	1334.457428	18.878272
44.728660	1335.641610	18.883290
44.979287	1332.859922	18.888307
44.722214	1338.924878	18.893325
44.918872	1332.361405	18.898343
45.073840	1333.769963	18.903360
44.864364	1339.272023	18.908378
45.465084	1326.708990	18.913395
45.273737	1329.917022	18.918413
45.014646	1334.464304	18.923431
45.242393	1330.660532	18.928448
45.280722	1325.459971	18.933466
45.381774	1321.912743	18.938483
45.340947	1323.143688	18.943501
45.381374	1322.717678	18.948519
45.623836	1324.090436	18.953536
45.469121	1326.450103	18.958554
45.421706	1322.484310	18.963571
45.382376	1323.071217	18.968589
45.300244	1316.336828	18.973607
45.820356	1327.424131	18.978624
45.551588	1322.697732	18.983642
45.999841	1327.759056	18.988659
45.489702	1336.890171	18.993677
45.398436	1328.345721	18.998695
45.750279	1348.923953	19.003712
45.783989	1352.961446	19.008730
45.732497	1353.304098	19.013747
45.836015	1351.448044	19.018765
45.822296	1345.242586	19.023783
45.674967	1348.424789	19.028800
46.134621	1356.532940	19.033818
46.272269	1342.597044	19.038835
46.184353	1352.558291	19.043853
46.528544	1361.956365	19.048871
46.162695	1349.951867	19.053888
45.898618	1359.341096	19.058906
46.517287	1364.931170	19.063923
46.860103	1368.961263	19.068941
46.970482	1363.638946	19.073959
47.186738	1358.470460	19.078976
46.799369	1357.887406	19.083994
47.147649	1346.291748	19.089011
46.641697	1341.914940	19.094029
46.613103	1325.941141	19.099047
46.388518	1326.837949	19.104064
46.369136	1341.787401	19.109082
46.766470	1343.590346	19.114099
46.701821	1358.284965	19.119117
46.569749	1351.672000	19.124135
46.868048	1353.522022	19.129152
46.752847	1348.414939	19.134170
47.099467	1352.100439	19.139187
46.730285	1371.112723	19.144205
47.014529	1377.149686	19.149223
47.311037	1375.960849	19.154240
47.204557	1382.462988	19.159258
47.473906	1379.839310	19.164275
47.503623	1383.104237	19.169293
47.540806	1381.050284	19.174311
47.744988	1368.628248	19.179328
47.273096	1374.524895	19.184346
47.534754	1377.886029	19.189363
47.665208	1389.236399	19.194381
47.544655	1384.149079	19.199399
47.726593	1379.045927	19.204416
47.495250	1390.465606	19.209434
47.511050	1373.074117	19.214451
47.539692	1385.538693	19.219469
47.199471	1383.581741	19.224487
47.764082	1387.709637	19.229504
48.066189	1398.610226	19.234522
48.073285	1392.644496	19.239539
48.395259	1409.954796	19.244557
48.350507	1400.235335	19.249575
48.469270	1390.108394	19.254592
48.077017	1396.084092	19.259610
48.181865	1392.211197	19.264627
48.598689	1394.134174	19.269645
48.703470	1405.135114	19.274663
48.576789	1403.545504	19.279680
48.750890	1399.592327	19.284698
48.754163	1399.563470	19.289715
48.641175	1397.290037	19.294733
48.457388	1393.061563	19.299751
48.487756	1398.870058	19.304768
48.524214	1401.041985	19.309786
48.712246	1396.783658	19.314803
48.678615	1397.505379	19.319821
48.589936	1390.620504	19.324839
48.903892	1390.214755	19.329856
49.005968	1393.168535	19.334874
48.673700	1381.281836	19.339891
48.448311	1386.133129	19.344909
48.652904	1408.779533	19.349927
48.722008	1413.805608	19.354944
48.628072	1421.703867	19.359962
49.116753	1422.185958	19.364979
49.102983	1414.588724	19.369997
49.245108	1420.755270	19.375015
49.489516	1422.733667	19.380032
49.378695	1425.951191	19.385050
49.551046	1431.267218	19.390067
49.745590	1439.407476	19.395085
49.264673	1443.478280	19.400103
49.729373	1435.957556	19.405120
49.765597	1438.385155	19.410138
50.051514	1432.539834	19.415155
49.730188	1427.818486	19.420173
49.557151	1434.343695	19.425191
50.126547	1423.789513	19.430208
49.962160	1434.163588	19.435226
49.805235	1433.673818	19.440243
49.935286	1437.289122	19.445261
49.768075	1436.649480	19.450279
49.952934	1429.125264	19.455296
50.084629	1424.752676	19.460314
50.127249	1437.672707	19.465331
50.183470	1425.100238	19.470349
50.220512	1441.060296	19.475367
50.885362	1449.805395	19.480384
50.686925	1438.342675	19.485402
50.623370	1426.281295	19.490419
50.554456	1423.442356	19.495437
50.493179	1430.748502	19.500455
51.031839	1426.558313	19.505472
50.467757	1429.900504	19.510490
50.729968	1431.522650	19.515507
50.961070	1447.297668	19.520525
50.383344	1448.022583	19.525543
50.663356	1441.386049	19.530560
50.914370	1452.799624	19.535578
51.266321	1440.499559	19.540595
51.148639	1447.824017	19.545613
51.010048	1443.774649	19.550631
51.207047	1449.998882	19.555648
50.954747	1452.910361	19.560666
50.966772	1445.204926	19.565683
51.170121	1449.837580	19.570701
51.102593	1443.583711	19.575719
51.373948	1449.136706	19.580736
51.204489	1452.136195	19.585754
50.886493	1470.443106	19.590771
51.464148	1469.225993	19.595789
51.425535	1472.006162	19.600807
51.824967	1468.781400	19.605824
51.730329	1465.905458	19.610842
51.506450	1462.601623	19.615859
51.913168	1466.807927	19.620877
51.235872	1467.144484	19.625895
51.721887	1463.571630	19.630912
51.717243	1463.569260	19.635930
51.546084	1488.553215	19.640947
52.180524	1489.766739	19.645965
52.161783	1489.760266	19.650983
52.045318	1489.096891	19.656000
52.146809	1489.377706	19.661018
52.525028	1485.430401	19.666035
52.654034	1499.255317	19.671053
52.243017	1499.376579	19.676071
52.524343	1495.242473	19.681088
52.603982	1495.009139	19.686106
52.317094	1498.093309	19.691123
52.364431	1494.532372	19.696141
52.281717	1488.100979	19.701159
52.408910	1491.240196	19.706176
52.371977	1491.514295	19.711194
52.552765	1491.498653	19.716211
52.756897	1492.217840	19.721229
52.749278	1520.382643	19.726247
52.631262	1515.342227	19.731264
52.675656	1531.765136	19.736282
52.620013	1523.745208	19.741299
52.837163	1511.033852	19.746317
52.886892	1512.301117	19.751335
52.798420	1521.445158	19.756352
52.994259	1529.351715	19.761370
53.018944	1533.283360	19.766387
53.186489	1539.032537	19.771405
53.496166	1539.937170	19.776423
53.460424	1528.003914	19.781440
53.490103	1530.277909	19.786458
53.423866	1539.172313	19.791475
53.471816	1520.286040	19.796493
53.563783	1527.012770	19.801511
53.866016	1531.273331	19.806528
53.774384	1533.064539	19.811546
53.875816	1549.061944	19.816563
54.475858	1548.803881	19.821581
54.310508	1539.949031	19.826599
54.398634	1536.627858	19.831616
53.998847	1534.790679	19.836634
53.843808	1525.394554	19.841651
53.700323	1520.661098	19.846669
54.068607	1534.451707	19.851687
54.098847	1538.382484	19.856704
54.603487	1549.484973	19.861722
54.338130	1547.740345	19.866739
54.813962	1541.477053	19.871757
54.588357	1548.240923	19.876775
54.669650	1552.605536	19.881792
54.728790	1557.055675	19.886810
54.517217	1555.409921	19.891827
54.922042	1549.100945	19.896845
54.626862	1543.766373	19.901863
54.624879	1549.977633	19.906880
54.953017	1553.915391	19.911898
54.797844	1550.338832	19.916915
55.267489	1546.841113	19.921933
54.903510	1547.295847	19.926951
54.844339	1542.056847	19.931968
55.118693	1544.399812	19.936986
54.702651	1546.655277	19.942003
55.041300	1537.475300	19.947021
54.954548	1549.159617	19.952039
55.169221	1570.245611	19.957056
55.743437	1575.505031	19.962074
55.289261	1567.721101	19.967091
55.475927	1567.489933	19.972109
55.292519	1565.483144	19.977127
55.781714	1568.174321	19.982144
55.534386	1574.162086	19.987162
55.688494	1576.239859	19.992179
55.860331	1562.942248	19.997197
56.003786	1568.382770	20.002215
55.680238	1559.110863	20.007232
55.631462	1568.330763	20.012250
56.074287	1572.758663	20.017267
55.805836	1566.302692	20.022285
55.859118	1570.933641	20.027303
55.888568	1573.453842	20.032320
56.399734	1579.846658	20.037338
56.298311	1603.781542	20.042355
56.302633	1591.400133	20.047373
56.015739	1593.843662	20.052391
56.321690	1592.596525	20.057408
56.676363	1589.186242	20.062426
56.230579	1600.930000	20.067443
56.469803	1594.280864	20.072461
56.508920	1600.965407	20.077479
56.605075	1591.416278	20.082496
56.722871	1591.991199	20.087514
56.567663	1592.542618	20.092531
56.650572	1600.725688	20.097549
57.142296	1615.671034	20.102567
57.131878	1616.108247	20.107584
57.261877	1615.990103	20.112602
57.153218	1615.303409	20.117619
57.239203	1611.354523	20.122637
56.950110	1614.988193	20.127655
56.863221	1614.127667	20.132672
57.457135	1606.491949	20.137690
56.814151	1604.175289	20.142707
57.395408	1597.286362	20.147725
57.232693	1605.586816	20.152743
57.619958	1616.890783	20.157760
57.881505	1621.356565	20.162778
57.929723	1621.803526	20.167795
58.190419	1622.416023	20.172813
57.890735	1616.040670	20.177831
57.535565	1601.645273	20.182848
58.038482	1617.494625	20.187866
58.300300	1620.350828	20.192883
57.977151	1619.246437	20.197901
58.101016	1613.025642	20.202919
57.983401	1618.926824	20.207936
58.176530	1612.824571	20.212954
57.984591	1616.550323	20.217971
58.394699	1613.576339	20.222989
58.651980	1616.748848	20.228007
58.465745	1608.853489	20.233024
58.716358	1611.048697	20.238042
58.662636	1613.282119	20.243059
58.632442	1601.142807	20.248077
58.906820	1605.799088	20.253095
58.593879	1605.639884	20.258112
59.026061	1609.577133	20.263130
58.812475	1605.965532	20.268147
59.009891	1606.458548	20.273165
58.758564	1608.685058	20.278183
58.946343	1607.090344	20.283200
58.970454	1614.733497	20.288218
58.696598	1606.902362	20.293235
58.778875	1614.429099	20.298253
59.108584	1632.754622	20.303271
58.912159	1640.751090	20.308288
59.094453	1628.976119	20.313306
59.121575	1638.076861	20.318323
59.045257	1617.139648	20.323341
59.318068	1642.660202	20.328359
59.329615	1642.746818	20.333376
59.671303	1648.440343	20.338394
59.562228	1654.990326	20.343411
59.529833	1657.081550	20.348429
59.489649	1655.737154	20.353447
59.627678	1656.226852	20.358464
60.143989	1647.009516	20.363482
59.465560	1654.466096	20.368499
59.947869	1653.219728	20.373517
60.235480	1659.827489	20.378535
59.877107	1676.610295	20.383552
60.020170	1661.691797	20.388570
60.441434	1674.227611	20.393587
60.379893	1673.937495	20.398605
60.610711	1663.388880	20.403623
59.991510	1669.457032	20.408640
60.432543	1662.107188	20.413658
60.436626	1660.033141	20.418675
60.569479	1664.680051	20.423693
60.840865	1676.178945	20.428711
61.095818	1682.731868	20.433728
60.965492	1681.578327	20.438746
60.809955	1675.518056	20.443763
61.110037	1687.520571	20.448781
61.238641	1685.284993	20.453799
61.165717	1692.593070	20.458816
61.595685	1688.795412	20.463834
61.283968	1671.224561	20.468851
61.344939	1664.325602	20.473869
61.607328	1668.825980	20.478887
61.088477	1669.661605	20.483904
61.843008	1680.709245	20.488922
61.563606	1684.388751	20.493939
61.290139	1689.443328	20.498957
61.370339	1683.822671	20.503975
61.340082	1694.882818	20.508992
61.715962	1692.655837	20.514010
61.704546	1691.669867	20.519027
61.712570	1684.918058	20.524045
61.890551	1685.619259	20.529063
61.526844	1689.564451	20.534080
62.035093	1698.189036	20.539098
62.029066	1708.642606	20.544115
62.243920	1710.584639	20.549133
62.299583	1704.475489	20.554151
61.857355	1715.704341	20.559168
62.200168	1700.997525	20.564186
62.352908	1704.969109	20.569203
62.382645	1708.625433	20.574221
62.435336	1709.955367	20.579239
62.446095	1721.233178	20.584256
62.679135	1722.266600	20.589274
62.794664	1733.793106	20.594291
62.790405	1731.950743	20.599309
63.100728	1736.295297	20.604327
62.980548	1731.510794	20.609344
63.025459	1724.260859	20.614362
62.985832	1733.337392	20.619379
62.992125	1728.978066	20.624397
62.990413	1729.947276	20.629415
63.257007	1730.530449	20.634432
63.170313	1727.135640	20.639450
63.231827	1728.767167	20.644467
63.193627	1732.639277	20.649485
63.453297	1722.928752	20.654503
63.385158	1740.319431	20.659520
63.538432	1744.934760	20.664538
63.674757	1749.691607	20.669555
63.506465	1748.626065	20.674573
64.183784	1745.130487	20.679591
64.059531	1747.422315	20.684608
63.981387	1746.156447	20.689626
64.293157	1737.996803	20.694643
63.699133	1745.601151	20.699661
64.192146	1739.205705	20.704679
64.207022	1741.393680	20.709696
64.237559	1745.160344	20.714714
64.710941	1744.060544	20.719731
64.051822	1739.783377	20.724749
64.146668	1743.969178	20.729767
64.078770	1740.795496	20.734784
64.355019	1744.075515	20.739802
64.699777	1756.036362	20.744819
64.538655	1765.838885	20.749837
64.616495	1761.736600	20.754855
64.537769	1766.120024	20.759872
64.689312	1770.779813	20.764890
64.679543	1764.147534	20.769907
64.803529	1768.376115	20.774925
65.176844	1768.731118	20.779943
64.930570	1770.663350	20.784960
65.075178	1777.015833	20.789978
65.318427	1783.273964	20.794995
65.251612	1788.618102	20.800013
65.426171	1780.574616	20.805031
65.350271	1788.277696	20.810048
65.634470	1778.222452	20.815066
65.292656	1782.804898	20.820083
65.266898	1789.780559	20.825101
65.734318	1775.186710	20.830119
65.588181	1782.790333	20.835136
65.553377	1795.037904	20.840154
65.760229	1799.960450	20.845171
65.468811	1805.655382	20.850189
66.092693	1802.868794	20.855207
66.078693	1802.350308	20.860224
65.823718	1808.648636	20.865242
66.363261	1802.779239	20.870259
66.426545	1824.583569	20.875277
66.673939	1818.283386	20.880295
66.707404	1815.980642	20.885312
66.850545	1812.025913	20.890330
66.610005	1796.290040	20.895347
66.763770	1809.754691	20.900365
67.302857	1806.937204	20.905383
67.195051	1789.577300	20.910400
66.878515	1781.197322	20.915418
67.235337	1778.013898	20.920435
66.994831	1788.699922	20.925453
66.832671	1784.764629	20.930471
67.245565	1798.261260	20.935488
67.438251	1803.533185	20.940506
67.587256	1791.267833	20.945523
67.000445	1798.738522	20.950541
67.235422	1794.841997	20.955559
67.377717	1798.774210	20.960576
67.512924	1807.482542	20.965594
67.670978	1809.379834	20.970611
67.579062	1811.085903	20.975629
67.732389	1793.808165	20.980647
67.314312	1805.847534	20.985664
67.426576	1812.801579	20.990682
67.425189	1803.078260	20.995699
67.741032	1823.744737	21.000717
68.269182	1821.869446	21.005735
68.288785	1825.928192	21.010752
68.120859	1831.600627	21.015770
68.269188	1821.329947	21.020787
68.199364	1828.628126	21.025805
68.325624	1817.846479	21.030823
68.430238	1827.067728	21.035840
68.337994	1835.836958	21.040858
68.352229	1825.208565	21.045875
68.120798	1832.270118	21.050893
68.280259	1831.140597	21.055911
68.450210	1834.882282	21.060928
68.225245	1852.083032	21.065946
68.700741	1851.475230	21.070963
68.561346	1858.623365	21.075981
68.953481	1867.499768	21.080999
69.175126	1868.478176	21.086016
69.414106	1877.517443	21.091034
69.310255	1875.958929	21.096051
69.320560	1875.540782	21.101069
69.000415	1878.431398	21.106087
69.273354	1875.740811	21.111104
69.280339	1871.491802	21.116122
69.480543	1877.112887	21.121139
69.718489	1888.434109	21.126157
70.058476	1890.302905	21.131175
70.326353	1892.612216	21.136192
69.862647	1886.726395	21.141210
70.221603	1875.226560	21.146227
70.249574	1875.582021	21.151245
69.817390	1871.386038	21.156263
70.601288	1876.751561	21.161280
70.468640	1887.707941	21.166298
70.449133	1883.889140	21.171315
70.338571	1887.204541	21.176333
70.813386	1892.883599	21.181351
70.806322	1890.669251	21.186368
70.672831	1887.714116	21.191386
70.768568	1885.638307	21.196403
70.525639	1894.323869	21.201421
70.811773	1889.601904	21.206439
70.556617	1884.500814	21.211456
70.608804	1888.125253	21.216474
70.664471	1883.294221	21.221491
70.685588	1883.044804	21.226509
71.138578	1906.523978	21.231527
71.287840	1909.773427	21.236544
70.914015	1913.196356	21.241562
71.078735	1904.545247	21.246579
71.065007	1913.523133	21.251597
71.062734	1910.058255	21.256615
71.538431	1914.190739	21.261632
71.482810	1932.605345	21.266650
71.723248	1930.402712	21.271667
71.907066	1934.618803	21.276685
71.768254	1935.467484	21.281703
72.042041	1929.592343	21.286720
71.601478	1932.744847	21.291738
71.988847	1924.674267	21.296755
72.142672	1931.404082	21.301773
72.024686	1932.476733	21.306791
72.326122	1934.114873	21.311808
72.266400	1942.358318	21.316826
72.728557	1937.469897	21.321843
72.609589	1948.837609	21.326861
72.736516	1946.766374	21.331879
73.233435	1938.587100	21.336896
72.573087	1934.572026	21.341914
73.040815	1930.295000	21.346931
73.009976	1921.576686	21.351949
72.828492	1919.746290	21.356967
73.140530	1920.694759	21.361984
73.241609	1933.359820	21.367002
73.063099	1940.321600	21.372019
73.071404	1936.425841	21.377037
72.990731	1936.792012	21.382055
73.499588	1923.539168	21.387072
73.257776	1938.315672	21.392090
73.644116	1927.395375	21.397107
73.715457	1936.511433	21.402125
73.507871	1927.489426	21.407143
73.689075	1918.990372	21.412160
73.625727	1924.229859	21.417178
73.754860	1925.866590	21.422195
73.685416	1943.724760	21.427213
73.580815	1954.345406	21.432231
73.967383	1953.865150	21.437248
74.106564	1961.686096	21.442266
74.060054	1962.091099	21.447283
74.190563	1958.627500	21.452301
74.029157	1962.358006	21.457319
74.398694	1969.237088	21.462336
74.348344	1974.758595	21.467354
74.572913	1971.611638	21.472371
74.459093	1974.817105	21.477389
74.591018	1978.350169	21.482407
75.075105	1969.137718	21.487424
74.670124	1982.087241	21.492442
74.922592	1981.255584	21.497459
75.026048	1994.295882	21.502477
75.206682	2000.825850	21.507495
75.469836	1997.852737	21.512512
75.288291	1997.635069	21.517530
75.564952	1995.208988	21.522547
75.415749	1991.195874	21.527565
75.477204	1991.883784	21.532583
75.613820	1993.086974	21.537600
75.691029	1999.440629	21.542618
75.797098	1992.941604	21.547635
75.660693	1994.739873	21.552653
75.252245	1996.246226	21.557671
75.781734	1999.426652	21.562688
75.616705	2020.443271	21.567706
75.956230	2019.197158	21.572723
75.984232	2018.637370	21.577741
75.965522	2022.408652	21.582759
76.345561	2023.034027	21.587776
76.006116	2039.075695	21.592794
76.485135	2037.870846	21.597811
76.971314	2034.954310	21.602829
76.180764	2044.123401	21.607847
76.765390	2028.690418	21.612864
76.879198	2036.199768	21.617882
76.848467	2032.821381	21.622899
77.006388	2032.648365	21.627917
76.908956	2038.114147	21.632935
77.262881	2032.002339	21.637952
77.248965	2039.859929	21.642970
77.317022	2050.418865	21.647987
77.571927	2059.035978	21.653005
77.525660	2061.943678	21.658023
77.559501	2060.603433	21.663040
77.748474	2054.091398	21.668058
77.441661	2058.491692	21.673075
77.821839	2060.553040	21.678093
77.664702	2064.926729	21.683111
78.111444	2051.797140	21.688128
77.994769	2054.299274	21.693146
78.039353	2051.982134	21.698163
77.805736	2050.573333	21.703181
77.714387	2055.406961	21.708199
77.771484	2046.438106	21.713216
77.808451	2057.860357	21.718234
78.031039	2074.921769	21.723251
78.272788	2079.513854	21.728269
78.174184	2086.466326	21.733287
78.662892	2077.218380	21.738304
78.325224	2081.793940	21.743322
78.433616	2100.135681	21.748339
78.341797	2105.269220	21.753357
78.609819	2099.833617	21.758375
78.707962	2102.137987	21.763392
78.657509	2113.419324	21.768410
78.654198	2123.355120	21.773427
79.179926	2122.966675	21.778445
78.986916	2120.674126	21.783463
79.329285	2121.229661	21.788480
79.305665	2132.042867	21.793498
79.777215	2150.280422	21.798515
79.608176	2145.980024	21.803533
79.473451	2150.820474	21.808551
79.777591	2144.299831	21.813568
80.090954	2146.037116	21.818586
79.834306	2152.869197	21.823603
80.005259	2154.199573	21.828621
79.965812	2151.586292	21.833639
80.644037	2154.086987	21.838656
80.649925	2151.394015	21.843674
80.401340	2147.011398	21.848691
80.497764	2138.654921	21.853709
80.471092	2156.427700	21.858727
80.894570	2159.927746	21.863744
80.802356	2166.702510	21.868762
81.169035	2163.514319	21.873779
81.130700	2160.171816	21.878797
80.931238	2167.361045	21.883815
80.825420	2166.304625	21.888832
81.325063	2163.401739	21.893850
81.277629	2164.583280	21.898867
81.267971	2163.925237	21.903885
81.405500	2162.240511	21.908903
81.451841	2158.976267	21.913920
81.298148	2166.284567	21.918938
81.285944	2160.675082	21.923955
81.621678	2157.845217	21.928973
81.755108	2179.743140	21.933991
82.057945	2180.320651	21.939008
82.377274	2179.535319	21.944026
82.036748	2178.490423	21.949043
82.229000	2184.873460	21.954061
81.897321	2181.090880	21.959079
82.315852	2183.594393	21.964096
82.640640	2180.438010	21.969114
82.112190	2184.759441	21.974131
82.484262	2179.335917	21.979149
82.531680	2182.891730	21.984167
82.551979	2180.859267	21.989184
82.566809	2172.247293	21.994202
82.521661	2187.444505	21.999219
82.686314	2191.123974	22.004237
82.484491	2194.699902	22.009255
82.583587	2198.522198	22.014272
82.553151	2196.260978	22.019290
82.920559	2215.335490	22.024307
83.326044	2216.373484	22.029325
83.314989	2228.122129	22.034343
83.430220	2221.255484	22.039360
83.260764	2223.551299	22.044378
83.133744	2235.198186	22.049395
83.587271	2225.188753	22.054413
83.601229	2244.599562	22.059431
83.792537	2240.908614	22.064448
83.969221	2242.749381	22.069466
84.120575	2245.042277	22.074483
84.280460	2246.295492	22.079501
84.109763	2237.396948	22.084519
84.135308	2243.891338	22.089536
84.319336	2233.393905	22.094554
84.199456	2235.887098	22.099571
84.356992	2243.976713	22.104589
84.172095	2260.060642	22.109607
84.480075	2261.470551	22.114624
84.781655	2251.323951	22.119642
84.648288	2252.799850	22.124659
85.058408	2253.975988	22.129677
85.207818	2265.926754	22.134695
84.865942	2275.691597	22.139712
85.437172	2267.232266	22.144730
85.546128	2279.968928	22.149747
85.415328	2271.824729	22.154765
85.479339	2272.748955	22.159783
85.612550	2274.151530	22.164800
85.815663	2265.869805	22.169818
85.549439	2276.882067	22.174835
85.731161	2269.717784	22.179853
85.871426	2280.944097	22.184871
85.797207	2271.594882	22.189888
85.923956	2287.203940	22.194906
85.958808	2290.894298	22.199923
86.032150	2291.318404	22.204941
86.228688	2300.888444	22.209959
86.326253	2298.588220	22.214976
86.815666	2293.098936	22.219994
86.356411	2304.084649	22.225011
86.757331	2306.360545	22.230029
86.887827	2325.159840	22.235047
86.913191	2319.197252	22.240064
86.924799	2322.155892	22.245082
86.648979	2316.887487	22.250099
86.783591	2314.209039	22.255117
87.056809	2315.924227	22.260135
87.349594	2323.803323	22.265152
87.639776	2319.582428	22.270170
87.300998	2328.911276	22.275187
87.500756	2333.538411	22.280205
87.732772	2339.672255	22.285223
87.753016	2341.171436	22.290240
87.920533	2329.732866	22.295258
87.910214	2342.573474	22.300275
88.238480	2336.541330	22.305293
88.086308	2335.668903	22.310311
87.908871	2338.534077	22.315328
88.186282	2328.233416	22.320346
87.858672	2346.419637	22.325363
88.229779	2352.989326	22.330381
88.540940	2361.724014	22.335399
88.296522	2365.653819	22.340416
88.898305	2356.362766	22.345434
88.646965	2362.168368	22.350451
88.964124	2355.490961	22.355469
88.963877	2350.539165	22.360487
89.037477	2358.140164	22.365504
89.022810	2349.977735	22.370522
88.803204	2363.892654	22.375539
89.139524	2374.018396	22.380557
89.131865	2374.275298	22.385575
89.643083	2376.041574	22.390592
89.561258	2371.004714	22.395610
89.401277	2372.715187	22.400627
89.972946	2369.176080	22.405645
89.905526	2376.780245	22.410663
89.520699	2379.911468	22.415680
89.773966	2378.590475	22.420698
90.007573	2385.607790	22.425715
90.101041	2394.285075	22.430733
90.072386	2386.749726	22.435751
90.039105	2397.652976	22.440768
90.391338	2391.127865	22.445786
90.528034	2408.215676	22.450803
91.095626	2412.195012	22.455821
91.025636	2411.906208	22.460839
90.865604	2405.167833	22.465856
91.212318	2412.460955	22.470874
91.310972	2415.039866	22.475891
91.322287	2413.030876	22.480909
91.286181	2403.517817	22.485927
91.174599	2406.713542	22.490944
91.572045	2401.857229	22.495962
91.870093	2405.847233	22.500979
91.193480	2401.541082	22.505997
91.830803	2397.253158	22.511015
91.840062	2394.228231	22.516032
91.811242	2403.903068	22.521050
91.792421	2395.501405	22.526067
91.750951	2404.834210	22.531085
91.787011	2417.434054	22.536103
91.861858	2427.458768	22.541120
91.899604	2421.945527	22.546138
92.058283	2427.974116	22.551155
91.884435	2427.288134	22.556173
92.109613	2447.322537	22.561191
92.123183	2451.271906	22.566208
92.428775	2456.201258	22.571226
92.664786	2481.495223	22.576243
93.155909	2471.763813	22.581261
93.170778	2483.372851	22.586279
92.940688	2482.777737	22.591296
93.417521	2476.842203	22.596314
93.155037	2470.949910	22.601331
93.280311	2471.571031	22.606349
93.598108	2473.462304	22.611367
93.698447	2484.852805	22.616384
93.775184	2490.029480	22.621402
94.073669	2490.588747	22.626419
93.913657	2488.079521	22.631437
94.271383	2492.164347	22.636455
94.051524	2495.462266	22.641472
94.096705	2493.454274	22.646490
94.030380	2486.259333	22.651507
94.120313	2488.549259	22.656525
94.473321	2488.607631	22.661543
94.264186	2493.961652	22.666560
94.423737	2501.243103	22.671578
94.507263	2512.500544	22.676595
94.461479	2522.342219	22.681613
94.796529	2514.301666	22.686631
94.698952	2514.910361	22.691648
95.022213	2508.440246	22.696666
95.087870	2504.797336	22.701683
95.137524	2528.031219	22.706701
95.767595	2524.385092	22.711719
95.482569	2533.017591	22.716736
95.773605	2531.173068	22.721754
95.842117	2543.187191	22.726771
95.675979	2538.397046	22.731789
95.835729	2523.487844	22.736807
95.625431	2536.719718	22.741824
96.020870	2522.221759	22.746842
96.266328	2528.842760	22.751859
95.759403	2530.209933	22.756877
96.053126	2521.282672	22.761895
96.173090	2539.578865	22.766912
96.239156	2552.852667	22.771930
96.604013	2551.230129	22.776947
96.529953	2559.075276	22.781965
96.524265	2544.491807	22.786983
96.520669	2553.929219	22.792000
96.729496	2564.797795	22.797018
97.038494	2571.689752	22.802035
96.685817	2567.544268	22.807053
97.218680	2557.045649	22.812071
97.268534	2570.479810	22.817088
97.303489	2586.573772	22.822106
97.662094	2577.159744	22.827123
97.669459	2579.418432	22.832141
97.834501	2586.834772	22.837159
97.920147	2580.180929	22.842176
97.977211	2580.048959	22.847194
97.744572	2577.917209	22.852211
97.601245	2590.535811	22.857229
98.068888	2599.798422	22.862247
98.189240	2608.989203	22.867264
98.116124	2615.372940	22.872282
98.003542	2611.798963	22.877299
98.136087	2626.517379	22.882317
98.900055	2621.338470	22.887335
98.921711	2637.324096	22.892352
98.854664	2632.423718	22.897370
98.945523	2628.164545	22.902387
99.069897	2629.098269	22.907405
99.364683	2647.970004	22.912423
99.067567	2650.642516	22.917440
98.987064	2648.509015	22.922458
99.499961	2653.380694	22.927475
99.635113	2652.204433	22.932493
99.705260	2648.557634	22.937511
100.046748	2664.625734	22.942528
99.873067	2673.632216	22.947546
100.214406	2673.332618	22.952563
99.911938	2679.654470	22.957581
100.432639	2674.267480	22.962599
100.711340	2678.730841	22.967616
100.722584	2675.156389	22.972634
100.980215	2673.468579	22.977651
100.733759	2675.886980	22.982669
100.857436	2670.309701	22.987687
101.033935	2681.312815	22.992704
100.730739	2682.038946	22.997722
100.905520	2673.827751	23.002739
100.859534	2678.300952	23.007757
101.150216	2686.581367	23.012775
101.174577	2704.422441	23.017792
101.241402	2699.087615	23.022810
101.545692	2696.180535	23.027827
101.265214	2704.673533	23.032845
101.369999	2699.702029	23.037863
101.407088	2706.188465	23.042880
101.701232	2726.991944	23.047898
101.688542	2722.139835	23.052915
101.637811	2729.476418	23.057933
101.846850	2721.771130	23.062951
101.914627	2747.439004	23.067968
101.989818	2749.945892	23.072986
102.181395	2743.830875	23.078003
102.390423	2756.233426	23.083021
102.677269	2758.729248	23.088039
102.724793	2768.919397	23.093056
103.073137	2772.570207	23.098074
103.181653	2770.394454	23.103091
102.989352	2771.977469	23.108109
103.307858	2769.491075	23.113127
103.444612	2760.200082	23.118144
103.344535	2768.791092	23.123162
103.329404	2769.674089	23.128179
103.405493	2791.966793	23.133197
103.880327	2786.236622	23.138215
104.027257	2789.287760	23.143232
103.663072	2798.942759	23.148250
104.002257	2792.280678	23.153267
103.976581	2792.884429	23.158285
104.317313	2811.550299	23.163303
104.272954	2820.246227	23.168320
104.233024	2822.433451	23.173338
104.485536	2811.337906	23.178355
104.541424	2817.407980	23.183373
104.618524	2816.739477	23.188391
104.629529	2828.172597	23.193408
104.854768	2839.142922	23.198426
105.086042	2840.394464	23.203443
105.393484	2847.220491	23.208461
105.233097	2842.236837	23.213479
105.056395	2837.618701	23.218496
105.391480	2854.331832	23.223514
105.708932	2863.150997	23.228531
105.952928	2867.806057	23.233549
106.063447	2851.585016	23.238567
106.253767	2855.042826	23.243584
106.218092	2866.243415	23.248602
106.257336	2853.678919	23.253619
106.284417	2859.242220	23.258637
106.244417	2849.177205	23.263655
106.462517	2851.563877	23.268672
106.769318	2881.474261	23.273690
107.171257	2873.893339	23.278707
107.165026	2877.274637	23.283725
107.353479	2876.348817	23.288743
107.138939	2867.270615	23.293760
107.294246	2876.222499	23.298778
107.155328	2865.907854	23.303795
107.351384	2870.289526	23.308813
107.644077	2867.516795	23.313831
107.602950	2862.908973	23.318848
107.322662	2863.738831	23.323866
107.815544	2864.453870	23.328883
107.993843	2886.828520	23.333901
107.984148	2888.591244	23.338919
108.306928	2892.959381	23.343936
108.609182	2887.521335	23.348954
108.528825	2882.951216	23.353971
108.389549	2888.521652	23.358989
108.646241	2887.237962	23.364007
108.714710	2888.022650	23.369024
108.538445	2882.735323	23.374042
108.761245	2879.361243	23.379059
108.851825	2874.388760	23.384077
108.939864	2881.549011	23.389095
109.281128	2889.764785	23.394112
109.344433	2895.322423	23.399130
109.401021	2895.080059	23.404147
109.207697	2896.133007	23.409165
109.316332	2890.949384	23.414183
109.542112	2890.162899	23.419200
109.484696	2892.917828	23.424218
109.830610	2910.213208	23.429235
109.184613	2912.927792	23.434253
109.610680	2915.651163	23.439271
109.963523	2927.422158	23.444288
110.128659	2950.913083	23.449306
110.211769	2937.161241	23.454323
110.673434	2941.772751	23.459341
110.376405	2934.194001	23.464359
111.132776	2943.664051	23.469376
110.842926	2963.180044	23.474394
110.764653	2970.252763	23.479411
111.196987	2967.928412	23.484429
111.196941	2966.205198	23.489447
111.363253	2959.566984	23.494464
111.105407	2962.940375	23.499482
111.933850	2974.864134	23.504499
111.783884	2983.646122	23.509517
111.666884	2991.671776	23.514535
111.791999	2977.461987	23.519552
111.839938	2988.324464	23.524570
112.148781	2976.771813	23.529587
111.823249	2991.148834	23.534605
111.836880	2998.399694	23.539623
112.486384	3005.146941	23.544640
112.417546	3020.272819	23.549658
112.786426	3009.812254	23.554675
112.827792	3019.290209	23.559693
112.609479	3030.352236	23.564711
112.789928	3028.562863	23.569728
112.788484	3028.140217	23.574746
113.051081	3037.924392	23.579763
113.608736	3045.670780	23.584781
113.611641	3047.021239	23.589799
113.573111	3040.209934	23.594816
113.540768	3052.435883	23.599834
113.873938	3047.153912	23.604851
113.764975	3051.283577	23.609869
113.601226	3054.717992	23.614887
113.946527	3064.707002	23.619904
114.160420	3071.254244	23.624922
114.233254	3076.561104	23.629939
114.527535	3074.693926	23.634957
114.564964	3087.985235	23.639975
115.168906	3086.937499	23.644992
115.320361	3098.052102	23.650010
115.500333	3093.589486	23.655027
115.577368	3083.016791	23.660045
115.077854	3091.468537	23.665063
115.281513	3083.224227	23.670080
115.516604	3081.142230	23.675098
115.511578	3086.814787	23.680115
115.583340	3089.565288	23.685133
115.667718	3087.172344	23.690151
116.093842	3101.564252	23.695168
115.983926	3106.741942	23.700186
116.157876	3108.340199	23.705203
116.413431	3107.214482	23.710221
116.111065	3110.717968	23.715239
116.077344	3113.305094	23.720256
116.095688	3110.275468	23.725274
116.535892	3114.461139	23.730291
116.898826	3123.172308	23.735309
116.344422	3141.173925	23.740327
116.717250	3137.362827	23.745344
116.818900	3130.984022	23.750362
116.939150	3137.624865	23.755379
117.125229	3151.723018	23.760397
117.201437	3160.116160	23.765415
117.587594	3147.172018	23.770432
117.458238	3151.907739	23.775450
117.673972	3165.679322	23.780467
117.921404	3159.861569	23.785485
117.934325	3177.079970	23.790503
118.076047	3177.534416	23.795520
118.255476	3173.308582	23.800538
118.065642	3180.824952	23.805555
118.569155	3189.823440	23.810573
118.689556	3191.250189	23.815591
118.943649	3192.201495	23.820608
118.698519	3194.269414	23.825626
118.731277	3191.903480	23.830643
119.231954	3203.159123	23.835661
119.464532	3219.787655	23.840679
119.397859	3209.208996	23.845696
119.425277	3220.087453	23.850714
119.483597	3217.029452	23.855731
119.909610	3219.692911	23.860749
119.767892	3220.087608	23.865767
120.380691	3227.642375	23.870784
120.759747	3237.247445	23.875802
120.347240	3235.352107	23.880819
120.940712	3228.567965	23.885837
120.509831	3232.432482	23.890855
120.959617	3230.509362	23.895872
120.765080	3225.628796	23.900890
120.681677	3228.207941	23.905907
120.862668	3221.504206	23.910925
120.752436	3230.299026	23.915943
121.060031	3237.513396	23.920960
120.892742	3254.214075	23.925978
120.939912	3255.292490	23.930995
121.517728	3257.812235	23.936013
121.193587	3271.510669	23.941031
121.760821	3272.330858	23.946048
121.803752	3274.407312	23.951066
122.023067	3283.803871	23.956083
121.931036	3287.823624	23.961101
122.030652	3296.632944	23.966119
122.004053	3301.428355	23.971136
122.431656	3304.344077	23.976154
122.193927	3306.133099	23.981171
122.689204	3314.744721	23.986189
122.637579	3331.338976	23.991207
122.907878	3321.900521	23.996224
123.038346	3326.917519	24.001242
123.219524	3343.778313	24.006259
123.536003	3342.207474	24.011277
123.272178	3347.677627	24.016295
123.360633	3336.708463	24.021312
124.028571	3342.998451	24.026330
123.880811	3358.888165	24.031347
124.116250	3372.584226	24.036365
124.129023	3366.380231	24.041383
124.156010	3355.897281	24.046400
124.385962	3370.310670	24.051418
124.369285	3371.503252	24.056435
124.244810	3358.133958	24.061453
124.390034	3369.972489	24.066471
124.464782	3380.647939	24.071488
124.801292	3381.333843	24.076506
124.811228	3382.727414	24.081523
125.245622	3396.007258	24.086541
125.272806	3404.149381	24.091559
125.482843	3409.456938	24.096576
125.546723	3407.464853	24.101594
125.499090	3419.279974	24.106611
125.435310	3406.971109	24.111629
125.859559	3426.868104	24.116647
125.954835	3427.048925	24.121664
126.081529	3428.935522	24.126682
126.255869	3436.398101	24.131699
126.463305	3434.727555	24.136717
126.488852	3443.580114	24.141735
126.806520	3447.336871	24.146752
127.067581	3445.698955	24.151770
127.217582	3446.278362	24.156787
127.087309	3444.285127	24.161805
126.995311	3449.516920	24.166823
127.158070	3454.926586	24.171840
128.023204	3464.348311	24.176858
127.849113	3473.055409	24.181875
128.272828	3463.684378	24.186893
127.758515	3467.047542	24.191911
128.086173	3463.862083	24.196928
128.519937	3472.862172	24.201946
128.103878	3473.975298	24.206963
128.486873	3465.263995	24.211981
128.500452	3461.935211	24.216999
128.628256	3489.813600	24.222016
129.192900	3477.478828	24.227034
128.958559	3491.494769	24.232051
129.530649	3481.794323	24.237069
129.130278	3481.020693	24.242087
128.980841	3485.724927	24.247104
129.279517	3486.012759	24.252122
129.198237	3499.938444	24.257139
129.545347	3503.804227	24.262157
129.627969	3507.926074	24.267175
129.429202	3511.274529	24.272192
129.880594	3517.506973	24.277210
130.050188	3537.674395	24.282227
130.268719	3530.065122	24.287245
130.500261	3535.116844	24.292263
130.844998	3544.800051	24.297280
130.642717	3556.456425	24.302298
130.662762	3560.925812	24.307315
131.481284	3555.892754	24.312333
131.211226	3558.204497	24.317351
131.291132	3557.074710	24.322368
131.644003	3549.210816	24.327386
131.584195	3560.582901	24.332403
131.647511	3565.919803	24.337421
131.562965	3562.442245	24.342439
131.823968	3576.320677	24.347456
132.148161	3568.325548	24.352474
131.570079	3569.483001	24.357491
132.213383	3579.577113	24.362509
132.132186	3589.488045	24.367527
132.156974	3585.756631	24.372544
132.605764	3596.992244	24.377562
132.548038	3612.107407	24.382579
132.667469	3607.584711	24.387597
133.030128	3608.572689	24.392615
132.761801	3609.340735	24.397632
133.161664	3623.333170	24.402650
133.271573	3628.022061	24.407667
133.022106	3632.745162	24.412685
133.836401	3640.887173	24.417703
134.120358	3655.667931	24.422720
134.357723	3656.561914	24.427738
134.232861	3662.546963	24.432755
134.236781	3654.387343	24.437773
134.117350	3659.339427	24.442791
134.282950	3655.017802	24.447808
134.686618	3650.292749	24.452826
134.439269	3667.445080	24.457843
134.761533	3670.156424	24.462861
135.071664	3677.045474	24.467879
134.949415	3680.366190	24.472896
135.320001	3693.293275	24.477914
135.349772	3705.882380	24.482931
135.971951	3701.830096	24.487949
136.062932	3697.576966	24.492967
135.755086	3697.871446	24.497984
136.117806	3690.842374	24.503002
135.871144	3699.993365	24.508019
136.444018	3715.050853	24.513037
136.490129	3719.538289	24.518055
136.601023	3714.568706	24.523072
136.575833	3721.885909	24.528090
136.743573	3735.302470	24.533107
136.626308	3732.713776	24.538125
136.864535	3744.500107	24.543143
137.054647	3740.528131	24.548160
137.462584	3732.191552	24.553178
137.704277	3753.077030	24.558195
137.565255	3759.806067	24.563213
138.160406	3758.106314	24.568231
137.930822	3760.664248	24.573248
138.275088	3755.929536	24.578266
138.020736	3763.995988	24.583283
138.306607	3780.092737	24.588301
138.560888	3769.605501	24.593319
138.720576	3785.450580	24.598336
138.860849	3784.986776	24.603354
138.838763	3785.454275	24.608371
139.279044	3782.323714	24.613389
139.357487	3793.317619	24.618407
139.256059	3811.627694	24.623424
139.279265	3802.511772	24.628442
139.268580	3810.098183	24.633459
139.615271	3814.409142	24.638477
139.879876	3817.688215	24.643495
139.836252	3820.624191	24.648512
140.168913	3823.078266	24.653530
140.026625	3827.999257	24.658547
140.187679	3837.054879	24.663565
140.461387	3856.325727	24.668583
140.346166	3848.361440	24.673600
140.663630	3858.768735	24.678618
140.989114	3872.160685	24.683635
141.039252	3883.127515	24.688653
141.184942	3872.688796	24.693671
141.276722	3883.939488	24.698688
141.744328	3896.270751	24.703706
141.979672	3903.364141	24.708723
141.802959	3899.124495	24.713741
141.661660	3903.777061	24.718759
141.592690	3902.904146	24.723776
142.353253	3909.372362	24.728794
142.287301	3926.827936	24.733811
142.357324	3917.262731	24.738829
142.625303	3915.510061	24.743847
142.643764	3923.578032	24.748864
142.807936	3929.609422	24.753882
143.177326	3943.676320	24.758899
143.303357	3941.781755	24.763917
143.250786	3944.444550	24.768935
143.479371	3942.189875	24.773952
143.488726	3949.021991	24.778970
144.185197	3956.093661	24.783987
144.249039	3952.693784	24.789005
144.506393	3951.892841	24.794023
144.415633	3955.271801	24.799040
144.463870	3953.373642	24.804058
144.715869	3950.673407	24.809075
144.513203	3953.880518	24.814093
145.079028	3956.373836	24.819111
145.186721	3976.197933	24.824128
145.081571	3976.725797	24.829146
145.601468	3971.909856	24.834163
145.510713	3974.850084	24.839181
145.465804	3964.753652	24.844199
145.591831	3971.204516	24.849216
145.784109	3991.558273	24.854234
145.869005	3994.139568	24.859251
145.625380	3989.923008	24.864269
146.053974	4005.281103	24.869287
146.344883	4015.386481	24.874304
146.074002	4009.043635	24.879322
146.196167	4024.074144	24.884339
146.573530	4045.506853	24.889357
146.762215	4045.477352	24.894375
147.086754	4060.564565	24.899392
147.105249	4074.550814	24.904410
146.978494	4072.121377	24.909427
147.020014	4079.384084	24.914445
147.348844	4089.095326	24.919463
147.567322	4100.439933	24.924480
147.875442	4110.324877	24.929498
148.070113	4120.341230	24.934515
148.235302	4119.002350	24.939533
148.759678	4125.122568	24.944551
148.895793	4132.348381	24.949568
149.189170	4135.174796	24.954586
149.370959	4139.966190	24.959603
149.004408	4150.761734	24.964621
149.604209	4140.046552	24.969639
149.747431	4150.585474	24.974656
149.415259	4137.292331	24.979674
149.737234	4137.854288	24.984691
149.741400	4139.248821	24.989709
150.118029	4149.766958	24.994727
149.931958	4160.594204	24.999744
150.404011	4166.855202	25.004762
150.427864	4159.011028	25.009779
150.614664	4189.690449	25.014797
150.902227	4187.691643	25.019815
150.738153	4186.584258	25.024832
151.262101	4190.368827	25.029850
151.450327	4186.349703	25.034867
151.260645	4197.344826	25.039885
151.808979	4199.809356	25.044903
151.729727	4208.378848	25.049920
151.936926	4206.597797	25.054938
151.959249	4212.503153	25.059955
151.577492	4208.816364	25.064973
151.939572	4219.371541	25.069991
152.128456	4227.289848	25.075008
152.279654	4229.147440	25.080026
152.674595	4233.188960	25.085043
152.729202	4246.554184	25.090061
152.459951	4255.740558	25.095079
152.811769	4255.404578	25.100096
152.861325	4269.038905	25.105114
153.157830	4269.683767	25.110131
153.186651	4277.339938	25.115149
153.328236	4283.037248	25.120167
153.673576	4289.460179	25.125184
153.688896	4298.043306	25.130202
154.216192	4300.918324	25.135219
154.140603	4317.337320	25.140237
154.550443	4322.364487	25.145255
154.712750	4316.543920	25.150272
154.814100	4321.063885	25.155290
155.093731	4318.270888	25.160307
155.213639	4346.164460	25.165325
155.333377	4335.284484	25.170343
155.408523	4339.634956	25.175360
155.261402	4341.375161	25.180378
155.647546	4353.833131	25.185395
155.640302	4368.429674	25.190413
156.046090	4359.338759	25.195431
156.107428	4374.205484	25.200448
156.322547	4384.168277	25.205466
156.438120	4379.907978	25.210483
156.547500	4388.675267	25.215501
156.723141	4393.808586	25.220519
157.192475	4415.372522	25.225536
157.137588	4410.902187	25.230554
157.228707	4413.018570	25.235571
156.817175	4417.562093	25.240589
157.561854	4429.629363	25.245607
157.601564	4433.464596	25.250624
157.779747	4442.277948	25.255642
158.080114	4455.945720	25.260659
157.991905	4467.250224	25.265677
158.734374	4466.433232	25.270695
158.509968	4468.204496	25.275712
158.879540	4475.772646	25.280730
158.933983	4478.781745	25.285747
159.098769	4487.887612	25.290765
159.405748	4481.709742	25.295783
159.450875	4492.450463	25.300800
159.245157	4513.059701	25.305818
159.842288	4511.167029	25.310835
159.780024	4515.251832	25.315853
159.863135	4519.279140	25.320871
159.998586	4530.412916	25.325888
160.158815	4528.115219	25.330906
160.722334	4546.003059	25.335923
160.605937	4556.611299	25.340941
160.662942	4553.856300	25.345959
161.157242	4549.233608	25.350976
161.002641	4550.536256	25.355994
161.785655	4561.420247	25.361011
161.894159	4577.289820	25.366029
161.750828	4575.929799	25.371047
161.898218	4575.587963	25.376064
162.076471	4581.917230	25.381082
162.338183	4556.845482	25.386099
162.191016	4573.417964	25.391117
162.658723	4590.781102	25.396135
162.748111	4588.456618	25.401152
162.946641	4594.205078	25.406170
163.280544	4590.406092	25.411187
163.016214	4596.561651	25.416205
163.337322	4592.278572	25.421223
163.166958	4590.048442	25.426240
163.343064	4617.561163	25.431258
163.547094	4615.303941	25.436275
163.537310	4627.284370	25.441293
163.952785	4635.192609	25.446311
164.011210	4642.424484	25.451328
164.050783	4644.612099	25.456346
164.158823	4651.580530	25.461363
164.234894	4660.713008	25.466381
164.487272	4663.934178	25.471399
164.698357	4670.867534	25.476416
164.776201	4687.142880	25.481434
165.238484	4690.359579	25.486451
165.291360	4694.154926	25.491469
165.501909	4712.849474	25.496487
165.753391	4711.452842	25.501504
165.464168	4719.080112	25.506522
166.383107	4727.263045	25.511539
166.347912	4738.979226	25.516557
166.363029	4730.656386	25.521575
166.770615	4743.881452	25.526592
166.961506	4759.144855	25.531610
167.088973	4752.912948	25.536627
166.924846	4755.943709	25.541645
167.355106	4770.206888	25.546663
167.960141	4775.857000	25.551680
168.059892	4784.446068	25.556698
168.166908	4784.274692	25.561715
167.889381	4781.755145	25.566733
167.932103	4785.555259	25.571751
168.046241	4805.982146	25.576768
168.204948	4810.376457	25.581786
168.716175	4812.124046	25.586803
168.661187	4827.729052	25.591821
169.077850	4834.778620	25.596839
169.583986	4831.751201	25.601856
169.215793	4838.488130	25.606874
169.331125	4841.137377	25.611891
169.544773	4854.285585	25.616909
169.490014	4857.248724	25.621927
170.421352	4870.811648	25.626944
170.068747	4881.210873	25.631962
169.964504	4877.332112	25.636979
170.265369	4896.669256	25.641997
170.566382	4896.262314	25.647015
171.182718	4901.989608	25.652032
171.661808	4912.451104	25.657050
171.854305	4923.443609	25.662067
171.720154	4925.513273	25.667085
171.763286	4927.211102	25.672103
171.955545	4924.573746	25.677120
171.760101	4918.834284	25.682138
171.947924	4925.282120	25.687156
172.214712	4946.944708	25.692173
172.354843	4954.081837	25.697191
172.508440	4948.395007	25.702208
172.846076	4969.014334	25.707226
173.155863	4974.366700	25.712244
173.060432	4977.228909	25.717261
173.030770	4983.006928	25.722279
173.100141	4996.143120	25.727296
173.393756	4995.576350	25.732314
173.481732	5004.419891	25.737332
173.525344	5018.841692	25.742349
173.934083	5021.880603	25.747367
174.034909	5019.560586	25.752384
173.782671	5036.986435	25.757402
174.394753	5041.196140	25.762420
175.005371	5048.338512	25.767437
174.880669	5075.753851	25.772455
175.187118	5066.624486	25.777472
175.714505	5071.361985	25.782490
175.633872	5063.009802	25.787508
175.955579	5080.869766	25.792525
175.480093	5085.625493	25.797543
175.883423	5083.460096	25.802560
175.618269	5096.573010	25.807578
176.047166	5106.546901	25.812596
176.325463	5118.457270	25.817613
176.314448	5134.396558	25.822631
176.640069	5137.375910	25.827648
176.901889	5149.749739	25.832666
177.030552	5157.384326	25.837684
177.563521	5162.297743	25.842701
177.475385	5164.887372	25.847719
177.639292	5181.768367	25.852736
177.883609	5185.328647	25.857754
178.313034	5192.761459	25.862772
178.574505	5197.714263	25.867789
178.529812	5214.956251	25.872807
178.824150	5207.615339	25.877824
179.166079	5214.755679	25.882842
179.098412	5215.953214	25.887860
179.117242	5229.277416	25.892877
179.032546	5242.087541	25.897895
179.466800	5227.897006	25.902912
179.439786	5250.183638	25.907930
180.006199	5256.625942	25.912948
180.158249	5258.963310	25.917965
180.115988	5287.799143	25.922983
180.047908	5286.402026	25.928000
180.781342	5297.628830	25.933018
181.128508	5298.792947	25.938036
181.299672	5308.008708	25.943053
181.201140	5313.216807	25.948071
181.275595	5320.680029	25.953088
181.483399	5328.226531	25.958106
181.240340	5334.543149	25.963124
181.656437	5346.842437	25.968141
181.826371	5358.946710	25.973159
182.189705	5375.449414	25.978176
182.475124	5383.820282	25.983194
182.780206	5385.360321	25.988212
183.453219	5378.499798	25.993229
183.715787	5379.348887	25.998247
184.160572	5380.885980	26.003264
184.498707	5381.524364	26.008282
184.323844	5366.450597	26.013300
184.556061	5373.706043	26.018317
184.631450	5365.193544	26.023335
185.097862	5361.746121	26.028352
185.044108	5349.222874	26.033370
185.061013	5352.717803	26.038388
185.119120	5359.744834	26.043405
185.135040	5374.827830	26.048423
185.336485	5360.686291	26.053440
185.034251	5374.180849	26.058458
185.467145	5384.542530	26.063476
186.014891	5387.310355	26.068493
186.026009	5398.318937	26.073511
186.034919	5401.341636	26.078528
186.077977	5413.671002	26.083546
186.253038	5426.431092	26.088564
186.098353	5430.426410	26.093581
186.491452	5433.161650	26.098599
186.662243	5433.728397	26.103616
186.920252	5454.818461	26.108634
186.593495	5458.780766	26.113652
187.406343	5466.431407	26.118669
187.190740	5476.395988	26.123687
187.127903	5490.800116	26.128704
187.279492	5502.834755	26.133722
187.485638	5519.911471	26.138740
188.206858	5522.917298	26.143757
187.852290	5536.322318	26.148775
188.475611	5551.067242	26.153792
188.644396	5563.342289	26.158810
188.848323	5574.172409	26.163828
189.460354	5579.651221	26.168845
189.327118	5595.256515	26.173863
189.629517	5593.419380	26.178880
190.068463	5599.392497	26.183898
190.069621	5606.163387	26.188916
190.607937	5612.000988	26.193933
190.788981	5626.057664	26.198951
191.308897	5621.667442	26.203968
191.075180	5618.894695	26.208986
191.377460	5623.285651	26.214004
191.346629	5635.459439	26.219021
191.392430	5647.008839	26.224039
191.621028	5642.705286	26.229056
192.032453	5651.997221	26.234074
192.349838	5657.392793	26.239092
192.791496	5666.080234	26.244109
192.503383	5668.199354	26.249127
192.521025	5656.324454	26.254144
192.936987	5667.235052	26.259162
192.804562	5694.040136	26.264180
193.022813	5689.271007	26.269197
193.856887	5699.847807	26.274215
193.695467	5710.245960	26.279232
193.736162	5716.827610	26.284250
193.703316	5719.348679	26.289268
194.576325	5718.975222	26.294285
194.460054	5736.560368	26.299303
194.287955	5736.461120	26.304320
194.512033	5749.756706	26.309338
194.758885	5765.820296	26.314356
195.504446	5771.508685	26.319373
195.448295	5774.033413	26.324391
195.555236	5784.518991	26.329408
195.827644	5786.244115	26.334426
195.655942	5796.252499	26.339444
195.912337	5803.494859	26.344461
196.278649	5816.020076	26.349479
195.861246	5827.007661	26.354496
196.395894	5841.069085	26.359514
196.868613	5863.972649	26.364532
197.323255	5866.594144	26.369549
197.336181	5857.526153	26.374567
197.495933	5878.051268	26.379584
197.874074	5878.683404	26.384602
197.497413	5888.562956	26.389620
198.143148	5899.163064	26.394637
198.347277	5914.311721	26.399655
198.496950	5916.943119	26.404672
198.776353	5916.230186	26.409690
198.823476	5940.103336	26.414708
198.870915	5937.049741	26.419725
198.882019	5952.149751	26.424743
199.213216	5959.661401	26.429760
199.245209	5959.921612	26.434778
199.567500	5981.826116	26.439796
199.990540	5989.727450	26.444813
200.310886	6003.768908	26.449831
200.395901	6014.071806	26.454848
200.751244	6014.344496	26.459866
200.951920	6016.952135	26.464884
201.467480	6006.148050	26.469901
201.050931	6007.494993	26.474919
201.428832	6025.511231	26.479936
201.310657	6030.432193	26.484954
201.671442	6054.246884	26.489972
201.800586	6054.327726	26.494989
202.453895	6056.223647	26.500007
202.377671	6069.386577	26.505024
202.834056	6073.251580	26.510042
202.892833	6083.867988	26.515060
203.101577	6084.239407	26.520077
203.672345	6100.287271	26.525095
203.647619	6103.668910	26.530112
203.617621	6093.221720	26.535130
203.991152	6105.234615	26.540148
204.248117	6112.855817	26.545165
204.306288	6127.465617	26.550183
204.426050	6128.567557	26.555200
205.193852	6133.463393	26.560218
204.884859	6139.462315	26.565236
205.093823	6141.964501	26.570253
205.826232	6155.862605	26.575271
205.490181	6174.713731	26.580288
205.598184	6170.473142	26.585306
205.578585	6179.633996	26.590324
205.747739	6186.928057	26.595341
206.353191	6201.398515	26.600359
206.435530	6225.825267	26.605376
206.608580	6210.576343	26.610394
206.386768	6235.053911	26.615412
206.925522	6242.886720	26.620429
207.123740	6255.981537	26.625447
207.174885	6269.250927	26.630464
207.807943	6285.816376	26.635482
208.196080	6298.565794	26.640500
207.894053	6296.608619	26.645517
208.353628	6310.584308	26.650535
208.342890	6326.395164	26.655552
208.796128	6339.791021	26.660570
209.092314	6349.587510	26.665588
208.780416	6362.452953	26.670605
209.330946	6371.761346	26.675623
209.288020	6376.692709	26.680640
209.684207	6387.032303	26.685658
209.711050	6404.649334	26.690676
210.323255	6416.542967	26.695693
210.703379	6426.515755	26.700711
210.548474	6443.312119	26.705728
211.063634	6446.404052	26.710746
211.393359	6457.117129	26.715764
211.604220	6452.633072	26.720781
212.026596	6464.910037	26.725799
211.663514	6468.527843	26.730816
212.204282	6475.356576	26.735834
212.360672	6486.384093	26.740852
212.501482	6490.298624	26.745869
212.823528	6502.907012	26.750887
212.639063	6512.753632	26.755904
213.345973	6513.571049	26.760922
213.711182	6535.425298	26.765940
213.626283	6530.438270	26.770957
213.730723	6531.195386	26.775975
213.825014	6528.945653	26.780992
214.278344	6543.253963	26.786010
214.140548	6546.138836	26.791028
214.441619	6551.953930	26.796045
214.625360	6552.752289	26.801063
214.586361	6570.566046	26.806080
214.882336	6574.601501	26.811098
215.589105	6598.378485	26.816116
215.863167	6591.295901	26.821133
215.951856	6594.479925	26.826151
215.756241	6610.585162	26.831168
215.933601	6622.225056	26.836186
216.198745	6634.902428	26.841204
216.443984	6638.857455	26.846221
216.715872	6640.184984	26.851239
217.008316	6667.325849	26.856256
217.038903	6675.320532	26.861274
217.500337	6684.339987	26.866292
217.282639	6703.558248	26.871309
217.555344	6713.945783	26.876327
217.980097	6729.193140	26.881344
218.456075	6719.818576	26.886362
218.672000	6744.348208	26.891380
218.497640	6763.480821	26.896397
218.789408	6756.272284	26.901415
219.314881	6779.193987	26.906432
219.792495	6775.106866	26.911450
219.912108	6778.024058	26.916468
220.058092	6796.191034	26.921485
220.277948	6803.240634	26.926503
220.250146	6807.424725	26.931520
221.039441	6821.418603	26.936538
220.977316	6826.255232	26.941556
221.300353	6831.779700	26.946573
221.753203	6842.379008	26.951591
221.588075	6843.898132	26.956608
221.574599	6854.494736	26.961626
222.170439	6862.205223	26.966644
222.304277	6880.506774	26.971661
222.354746	6872.900344	26.976679
222.622005	6890.132923	26.981696
222.812441	6894.235493	26.986714
223.276407	6909.978801	26.991732
223.107037	6925.111041	26.996749
223.473508	6917.325657	27.001767
223.656388	6939.107931	27.006784
223.799104	6944.360778	27.011802
223.942958	6961.877935	27.016820
224.273518	6965.835451	27.021837
224.719611	6978.203752	27.026855
224.951929	7002.462826	27.031872
225.006206	7007.767428	27.036890
225.150507	7012.417081	27.041908
225.424192	7026.214083	27.046925
226.150280	7031.959592	27.051943
225.858727	7048.127594	27.056960
226.168318	7050.197432	27.061978
226.258587	7057.071702	27.066996
226.422220	7075.018364	27.072013
226.891214	7085.429027	27.077031
226.996949	7095.369400	27.082048
227.658737	7110.845123	27.087066
227.562511	7112.034626	27.092084
227.729164	7125.011889	27.097101
228.110996	7114.319659	27.102119
227.960639	7148.722045	27.107136
228.116202	7162.070430	27.112154
228.388569	7171.028195	27.117172
228.862595	7170.313140	27.122189
229.349097	7176.724454	27.127207
229.401569	7185.000052	27.132224
229.539968	7197.827104	27.137242
229.926632	7201.425464	27.142260
229.746910	7211.375893	27.147277
230.494887	7218.709123	27.152295
230.318524	7233.915321	27.157312
230.626492	7233.472519	27.162330
230.651718	7254.332785	27.167348
230.873676	7261.480097	27.172365
231.782897	7270.919020	27.177383
231.372096	7285.653720	27.182400
232.120396	7294.063446	27.187418
232.254667	7303.390172	27.192436
232.301276	7314.198614	27.197453
232.335436	7329.592898	27.202471
232.890714	7336.388113	27.207488
232.953255	7343.131086	27.212506
233.364834	7344.597789	27.217524
233.068408	7355.093787	27.222541
233.540107	7367.609874	27.227559
233.911433	7372.606044	27.232576
233.879063	7394.261573	27.237594
234.706578	7402.709452	27.242612
234.871678	7405.547008	27.247629
234.856472	7415.967417	27.252647
235.263276	7428.916745	27.257664
235.616009	7443.737162	27.262682
236.181683	7448.361955	27.267700
235.950606	7454.096539	27.272717
236.340385	7466.032017	27.277735
236.569061	7477.932757	27.282752
236.624526	7478.729155	27.287770
236.945691	7486.767064	27.292788
236.882900	7497.415962	27.297805
237.354862	7506.860367	27.302823
237.305027	7521.961743	27.307840
237.536169	7538.982757	27.312858
237.939562	7548.501065	27.317876
238.188069	7553.459700	27.322893
238.594803	7577.897414	27.327911
238.689261	7587.312602	27.332928
238.856337	7600.533223	27.337946
239.518582	7602.775184	27.342964
239.447173	7615.048193	27.347981
239.649761	7626.530080	27.352999
240.020253	7638.778077	27.358016
239.985326	7653.785673	27.363034
240.372545	7652.253909	27.368052
240.371379	7673.939605	27.373069
240.862246	7687.930387	27.378087
240.832810	7697.942773	27.383104
241.329962	7711.553747	27.388122
241.505506	7720.675327	27.393140
241.487606	7731.563574	27.398157
241.676090	7749.873214	27.403175
242.352230	7755.992993	27.408192
242.407738	7779.374725	27.413210
242.890075	7789.695303	27.418228
243.150093	7802.437427	27.423245
243.182168	7808.961194	27.428263
243.465843	7826.567766	27.433280
243.957172	7834.519188	27.438298
244.329002	7835.982688	27.443316
244.348086	7851.597604	27.448333
244.771995	7859.887930	27.453351
245.138518	7863.843166	27.458368
245.271998	7872.845130	27.463386
245.455985	7858.458158	27.468404
245.701948	7874.511108	27.473421
245.964635	7881.923787	27.478439
246.373128	7883.204753	27.483456
245.989127	7891.107058	27.488474
246.865053	7894.149041	27.493492
246.746801	7909.435090	27.498509
246.790165	7913.696681	27.503527
247.138620	7931.129039	27.508544
247.500271	7926.232688	27.513562
247.887949	7945.199555	27.518580
247.859570	7951.811769	27.523597
248.277849	7957.479511	27.528615
248.248562	7982.159704	27.533632
248.634783	7986.506513	27.538650
248.897278	7999.229442	27.543668
249.253198	8006.444457	27.548685
249.074332	8012.508839	27.553703
249.518168	8028.013167	27.558720
249.683784	8043.532679	27.563738
249.732141	8052.567008	27.568756
249.838598	8078.839328	27.573773
250.653032	8083.864148	27.578791
251.405430	8106.044776	27.583808
251.193094	8112.752164	27.588826
251.678345	8111.729082	27.593844
251.604946	8130.541059	27.598861
251.685944	8136.309049	27.603879
252.136161	8149.542537	27.608896
251.827219	8160.419802	27.613914
252.692410	8162.532172	27.618932
252.822405	8191.986468	27.623949
253.165862	8199.121427	27.628967
253.697841	8209.011414	27.633984
253.394364	8228.200499	27.639002
253.501417	8239.599864	27.644020
254.055823	8264.087969	27.649037
254.048223	8276.616618	27.654055
254.656480	8288.354236	27.659072
254.715504	8310.915241	27.664090
255.457254	8306.521214	27.669108
255.718062	8332.046735	27.674125
255.497366	8341.780034	27.679143
256.338212	8341.932512	27.684160
256.072731	8368.096181	27.689178
256.357082	8370.274311	27.694196
256.614742	8386.701572	27.699213
257.068363	8407.050876	27.704231
257.616646	8410.444203	27.709248
257.807430	8428.893070	27.714266
258.036436	8440.614425	27.719284
258.742045	8449.504945	27.724301
258.558492	8445.464208	27.729319
258.997715	8449.496583	27.734336
259.546555	8460.340677	27.739354
259.880445	8466.959468	27.744372
259.508931	8478.490777	27.749389
259.759575	8486.076072	27.754407
260.289142	8487.353902	27.759424
260.355874	8500.063644	27.764442
260.576315	8505.396319	27.769460
260.811777	8512.125260	27.774477
261.074271	8523.386792	27.779495
261.116164	8533.593671	27.784512
261.534415	8554.131794	27.789530
261.810968	8548.184650	27.794548
262.027808	8571.630512	27.799565
261.968233	8576.473513	27.804583
262.168535	8590.008512	27.809600
262.596477	8605.711560	27.814618
262.992831	8611.667085	27.819636
262.974082	8620.614331	27.824653
263.397886	8640.747563	27.829671
263.728492	8645.608389	27.834688
263.623138	8655.822616	27.839706
263.916213	8675.862707	27.844724
264.372630	8690.655258	27.849741
264.478414	8706.317301	27.854759
264.872777	8714.764187	27.859776
265.140060	8734.426362	27.864794
265.918054	8745.736721	27.869812
265.926004	8756.463662	27.874829
266.109812	8768.991074	27.879847
266.458795	8770.041482	27.884864
266.708548	8792.686855	27.889882
266.907663	8803.475435	27.894900
267.143157	8816.572551	27.899917
267.064690	8828.399147	27.904935
267.746810	8843.914193	27.909952
268.146933	8862.242298	27.914970
268.412093	8870.760011	27.919988
268.897710	8872.085798	27.925005
269.079707	8894.445132	27.930023
269.339160	8891.922977	27.935040
269.784039	8909.072792	27.940058
269.746303	8922.844227	27.945076
270.239703	8923.370023	27.950093
270.528831	8941.702965	27.955111
270.985649	8940.112840	27.960128
271.307542	8951.946257	27.965146
271.166964	8951.756803	27.970164
271.755863	8968.530503	27.975181
271.581152	8973.944159	27.980199
272.092364	8978.420014	27.985216
272.223326	8998.271158	27.990234
272.489700	9008.222128	27.995252
272.882279	9013.426953	28.000269
272.774388	9037.688325	28.005287
273.204152	9047.872614	28.010304
273.658629	9064.238073	28.015322
273.984078	9061.266701	28.020340
274.014323	9071.463073	28.025357
274.116829	9086.421885	28.030375
274.575402	9112.564738	28.035392
275.028317	9118.372649	28.040410
275.023479	9140.347947	28.045428
275.126549	9149.045886	28.050445
275.649178	9169.631487	28.055463
275.699342	9178.915506	28.060480
275.922126	9197.991579	28.065498
276.177602	9213.709533	28.070516
276.659128	9221.760968	28.075533
277.049946	9242.695655	28.080551
277.597769	9254.825388	28.085568
277.607579	9266.111169	28.090586
277.771262	9282.127715	28.095604
278.447307	9293.400708	28.100621
278.320527	9313.728270	28.105639
278.910205	9320.862981	28.110656
279.057006	9343.480952	28.115674
278.960947	9344.926311	28.120692
279.633892	9348.934902	28.125709
279.947540	9378.570695	28.130727
280.462783	9386.793730	28.135744
280.344221	9385.764139	28.140762
280.778760	9394.343965	28.145780
281.592396	9405.295530	28.150797
281.762357	9423.732864	28.155815
281.566292	9409.596822	28.160832
281.836231	9429.982342	28.165850
282.378193	9439.530440	28.170868
282.311030	9447.345881	28.175885
282.698618	9457.442285	28.180903
282.637010	9470.188582	28.185920
283.164342	9482.479541	28.190938
283.340834	9494.276093	28.195956
283.749097	9501.095146	28.200973
284.358431	9513.654280	28.205991
284.852113	9520.961973	28.211008
285.067326	9527.612366	28.216026
284.976032	9536.419866	28.221044
285.407351	9549.537341	28.226061
285.552480	9561.607222	28.231079
285.824838	9565.830165	28.236096
285.776855	9594.531552	28.241114
286.041280	9604.783095	28.246132
286.508849	9617.699185	28.251149
286.724524	9640.325673	28.256167
287.052023	9648.701371	28.261184
287.333901	9671.746925	28.266202
287.406716	9682.363204	28.271220
288.023299	9692.638563	28.276237
288.275320	9717.223322	28.281255
288.321993	9734.565731	28.286272
288.704976	9753.468885	28.291290
289.036477	9776.090023	28.296308
289.804557	9782.401312	28.301325
289.785250	9802.943059	28.306343
290.134264	9801.451843	28.311360
290.577610	9819.414184	28.316378
290.540894	9825.580025	28.321396
290.920294	9840.533957	28.326413
291.321579	9854.284670	28.331431
291.476713	9872.235378	28.336448
292.110707	9888.140884	28.341466
292.326495	9903.925630	28.346484
292.616660	9903.782355	28.351501
292.823963	9923.275216	28.356519
293.309472	9939.061944	28.361536
293.542733	9949.419595	28.366554
293.561868	9960.881150	28.371572
294.106400	9964.928938	28.376589
294.239022	9988.124561	28.381607
294.556569	10011.082855	28.386624
294.784964	10021.763363	28.391642
295.074127	10036.466367	28.396660
295.351754	10047.505438	28.401677
296.007311	10073.786131	28.406695
296.186248	10067.882214	28.411712
296.534069	10085.913454	28.416730
296.835423	10093.137835	28.421748
297.149674	10097.884783	28.426765
297.488816	10108.036491	28.431783
297.829614	10122.576761	28.436800
298.157203	10132.736607	28.441818
297.996165	10141.129066	28.446836
298.520477	10152.489503	28.451853
299.098756	10168.002984	28.456871
299.609427	10191.676402	28.461888
299.973826	10193.248614	28.466906
299.756787	10188.934886	28.471924
300.353904	10200.148177	28.476941
300.574352	10205.774984	28.481959
301.087886	10217.102418	28.486976
300.691404	10219.801045	28.491994
301.046261	10235.968439	28.497012
301.451406	10236.909099	28.502029
301.576624	10251.394832	28.507047
301.792829	10262.301567	28.512064
302.196193	10281.779877	28.517082
302.161087	10287.715125	28.522100
302.493608	10297.223854	28.527117
302.705607	10324.673178	28.532135
303.165244	10335.140825	28.537152
303.686695	10354.818579	28.542170
303.798767	10371.213570	28.547188
304.444921	10387.054451	28.552205
304.515837	10397.204130	28.557223
304.626566	10422.061392	28.562240
305.027435	10425.152971	28.567258
305.199187	10445.400268	28.572276
305.582015	10463.183263	28.577293
305.629035	10486.045591	28.582311
306.005154	10500.779545	28.587328
306.519263	10518.043145	28.592346
306.901830	10541.917053	28.597364
307.348515	10551.357509	28.602381
307.741388	10569.382159	28.607399
307.954077	10589.260087	28.612416
308.323249	10602.710108	28.617434
308.603811	10616.688691	28.622452
308.836969	10629.856917	28.627469
309.046929	10644.073921	28.632487
309.347965	10667.161911	28.637504
310.048591	10689.183243	28.642522
309.942513	10701.864724	28.647540
310.627718	10722.218184	28.652557
310.685009	10737.374856	28.657575
311.104156	10758.698346	28.662592
311.629855	10763.507068	28.667610
311.944974	10784.108020	28.672628
312.402831	10798.608379	28.677645
312.223576	10815.816676	28.682663
312.271314	10828.262593	28.687680
312.869554	10853.353500	28.692698
313.158325	10871.464215	28.697716
313.557717	10883.747727	28.702733
313.807421	10904.482203	28.707751
314.241649	10915.980364	28.712768
314.793293	10935.016174	28.717786
314.457725	10950.386121	28.722804
315.529425	10963.612682	28.727821
315.611837	10985.434394	28.732839
316.419579	11005.266916	28.737856
316.360453	11010.675682	28.742874
316.579673	11031.203517	28.747892
316.630938	11034.031048	28.752909
317.296444	11056.822450	28.757927
316.826740	11072.838709	28.762944
317.622134	11078.015753	28.767962
318.105099	11102.654573	28.772980
318.886491	11111.029298	28.777997
318.868930	11133.637295	28.783015
319.160507	11142.732911	28.788032
319.647188	11152.246347	28.793050
320.197209	11167.929284	28.798068
320.132636	11174.605148	28.803085
320.271541	11190.620900	28.808103
320.721136	11197.513044	28.813120
321.098456	11222.313821	28.818138
321.607994	11236.181218	28.823156
321.769501	11251.066214	28.828173
322.521842	11257.674136	28.833191
322.372191	11259.939543	28.838208
322.528553	11270.139462	28.843226
322.888026	11287.213280	28.848244
323.198343	11297.133332	28.853261
323.612469	11300.958707	28.858279
323.556341	11328.606228	28.863296
323.921966	11331.668747	28.868314
324.003469	11351.466990	28.873332
324.725352	11374.297314	28.878349
325.258166	11390.194694	28.883367
324.981282	11411.811102	28.888384
325.613288	11422.508130	28.893402
325.827856	11445.515895	28.898420
326.228544	11463.391775	28.903437
326.407781	11479.193050	28.908455
326.880279	11498.712324	28.913472
327.548603	11507.597535	28.918490
327.734559	11525.794457	28.923508
328.189722	11545.332283	28.928525
328.626559	11550.395114	28.933543
328.575455	11579.330542	28.938560
328.751041	11583.398591	28.943578
329.470214	11610.615628	28.948596
329.717682	11615.755505	28.953613
329.465292	11629.875169	28.958631
329.571461	11664.953034	28.963648
330.087073	11667.790023	28.968666
330.492856	11701.595843	28.973684
330.912130	11721.471032	28.978701
332.020193	11753.938596	28.983719
331.926194	11771.535440	28.988736
332.586240	11776.260229	28.993754
332.938698	11790.714714	28.998772
333.142008	11803.310582	29.003789
333.489299	11820.614149	29.008807
334.045577	11836.059839	29.013824
334.446425	11844.879748	29.018842
334.864034	11856.122159	29.023860
335.115083	11867.592761	29.028877
335.611334	11885.646695	29.033895
335.563336	11903.448024	29.038912
336.298718	11905.574872	29.043930
336.934742	11915.371604	29.048948
336.935692	11924.917314	29.053965
337.231722	11946.128818	29.058983
337.545044	11948.375465	29.064000
338.053414	11963.171958	29.069018
337.892368	11975.152418	29.074036
338.144730	11989.565897	29.079053
338.663098	11997.420148	29.084071
338.755803	12024.780128	29.089088
339.073371	12036.511979	29.094106
339.564808	12060.579181	29.099124
339.770794	12082.171242	29.104141
340.397205	12095.812558	29.109159
340.183767	12117.151426	29.114176
340.412175	12132.197160	29.119194
340.660591	12145.739835	29.124212
341.064134	12175.084941	29.129229
341.712742	12192.480594	29.134247
341.706433	12216.973319	29.139264
342.218270	12232.988382	29.144282
342.758876	12257.152339	29.149300
343.188304	12281.377953	29.154317
343.476720	12300.936370	29.159335
343.756100	12311.821773	29.164352
343.947698	12325.187168	29.169370
344.394137	12349.416519	29.174388
344.797836	12359.638286	29.179405
345.404761	12372.704980	29.184423
345.742253	12386.331767	29.189440
345.862860	12402.825088	29.194458
346.337610	12412.805234	29.199476
346.630877	12433.367212	29.204493
347.082679	12446.669829	29.209511
347.046161	12461.618382	29.214528
347.489065	12483.088529	29.219546
347.760312	12495.705797	29.224564
348.011506	12510.985102	29.229581
348.624980	12529.801276	29.234599
348.857156	12551.026621	29.239616
349.130570	12569.154012	29.244634
349.512549	12589.032803	29.249652
349.612010	12617.440986	29.254669
350.241054	12642.144207	29.259687
350.509473	12666.199750	29.264704
350.948618	12678.730841	29.269722
351.478041	12686.798385	29.274740
352.013456	12708.131143	29.279757
352.217500	12718.018068	29.284775
352.652912	12748.293800	29.289792
352.913398	12759.766627	29.294810
353.523053	12773.843689	29.299828
353.659607	12799.107415	29.304845
354.004791	12814.069087	29.309863
354.355266	12837.493051	29.314880
354.764570	12851.525766	29.319898
355.478883	12859.993896	29.324916
355.455674	12888.759594	29.329933
356.183832	12897.143466	29.334951
356.462103	12909.431491	29.339968
356.681812	12924.371852	29.344986
357.304904	12933.422725	29.350004
357.630549	12959.446519	29.355021
357.976965	12970.034433	29.360039
358.388820	12985.399482	29.365056
358.195149	12994.126743	29.370074
358.694680	13012.591774	29.375092
358.923584	13030.328684	29.380109
359.130879	13046.780568	29.385127
359.458822	13075.917864	29.390144
359.950003	13093.970595	29.395162
360.533766	13116.227828	29.400180
360.670705	13133.458183	29.405197
361.532650	13151.828686	29.410215
361.793735	13166.194331	29.415232
362.119412	13193.667933	29.420250
362.723347	13205.336710	29.425268
362.847803	13220.361700	29.430285
363.289255	13233.900184	29.435303
363.380992	13238.401733	29.440320
363.969135	13263.690080	29.445338
364.385738	13284.135769	29.450356
364.586306	13297.790980	29.455373
364.923338	13303.207823	29.460391
365.267993	13331.679725	29.465408
365.387946	13345.442337	29.470426
365.829257	13362.271531	29.475444
366.111261	13384.238446	29.480461
366.330541	13405.409928	29.485479
367.208058	13418.794973	29.490496
367.458680	13442.333226	29.495514
368.280035	13453.788096	29.500532
368.163235	13476.512342	29.505549
368.773116	13482.960212	29.510567
368.932093	13501.062212	29.515584
369.379184	13515.121082	29.520602
369.795652	13530.511117	29.525620
369.991578	13537.200696	29.530637
370.332445	13549.943558	29.535655
371.016684	13558.975681	29.540672
370.904856	13582.024548	29.545690
371.271219	13591.283327	29.550708
371.761144	13612.340012	29.555725
371.981444	13624.422839	29.560743
372.729276	13641.946401	29.565760
373.051363	13666.152711	29.570778
373.491089	13674.417896	29.575796
373.702122	13697.978458	29.580813
374.103371	13702.955867	29.585831
374.352987	13730.877970	29.590848
374.693473	13738.836610	29.595866
375.009163	13763.647229	29.600884
375.314642	13777.210560	29.605901
375.678446	13805.301210	29.610919
376.099291	13824.590977	29.615936
376.239920	13851.156581	29.620954
376.140099	13875.220813	29.625972
376.812510	13901.317907	29.630989
377.252373	13916.603534	29.636007
377.833321	13956.152568	29.641024
378.343855	13982.676204	29.646042
378.879934	13999.412170	29.651060
379.562971	14022.037047	29.656077
380.067267	14024.238243	29.661095
380.828403	14056.091457	29.666112
380.947998	14065.029100	29.671130
381.859397	14077.123970	29.676148
381.931609	14083.030967	29.681165
382.329251	14096.327443	29.686183
382.482643	14102.512275	29.691200
382.979296	14109.101264	29.696218
383.128863	14122.724002	29.701236
383.506292	14144.566318	29.706253
383.629888	14157.915237	29.711271
383.974790	14168.630386	29.716288
384.623266	14196.430693	29.721306
384.683554	14202.219588	29.726324
384.956992	14229.608131	29.731341
385.887865	14252.014450	29.736359
386.088541	14275.773154	29.741376
386.121083	14291.473437	29.746394
387.046641	14321.738073	29.751412
386.998078	14335.512008	29.756429
387.433681	14356.795941	29.761447
387.571127	14372.625132	29.766464
387.695931	14397.261201	29.771482
388.494230	14411.988939	29.776500
389.038002	14443.570511	29.781517
389.619790	14465.251701	29.786535
390.010703	14487.543914	29.791552
390.036621	14502.585354	29.796570
390.633540	14512.629591	29.801588
390.982379	14533.472538	29.806605
391.344460	14549.661460	29.811623
391.600389	14576.563731	29.816640
392.045873	14598.010611	29.821658
392.547690	14615.507291	29.826676
392.940968	14640.145834	29.831693
393.446048	14659.896983	29.836711
393.564131	14677.223280	29.841728
393.944205	14697.669899	29.846746
394.509382	14707.662364	29.851764
394.467521	14721.511324	29.856781
395.041866	14749.336686	29.861799
395.415905	14766.237671	29.866816
395.555420	14798.056855	29.871834
396.123810	14812.975670	29.876852
396.428826	14830.102282	29.881869
397.042608	14858.679596	29.886887
397.634433	14867.398370	29.891904
397.556110	14893.175429	29.896922
397.971379	14917.940375	29.901940
398.125236	14943.336887	29.906957
398.776315	14968.598702	29.911975
399.641812	14990.273951	29.916992
399.553995	15011.710084	29.922010
400.059325	15023.935491	29.927028
400.494018	15053.949725	29.932045
400.751857	15079.197485	29.937063
401.369581	15103.343525	29.942080
401.537564	15130.670925	29.947098
402.422303	15155.621620	29.952116
402.604310	15170.099074	29.957133
403.014271	15195.228411	29.962151
403.569797	15217.514643	29.967168
403.944118	15245.441542	29.972186
404.280300	15269.177100	29.977204
404.703934	15297.573251	29.982221
404.983883	15321.845116	29.987239
405.727148	15338.066592	29.992256
405.263052	15362.767724	29.997274
405.943909	15384.595516	30.002292
406.648984	15414.065795	30.007309
406.938537	15443.534881	30.012327
407.426063	15450.530032	30.017344
407.709579	15494.642076	30.022362
408.440007	15508.948610	30.027380
408.691733	15539.810271	30.032397
409.018707	15562.931763	30.037415
409.562301	15581.935627	30.042432
410.008553	15617.984511	30.047450
410.848980	15636.183934	30.052468
411.538753	15656.058786	30.057485
411.637067	15672.924805	30.062503
412.180094	15693.504885	30.067520
412.506564	15715.079047	30.072538
412.595305	15732.470905	30.077556
413.294701	15753.017081	30.082573
413.207251	15773.708636	30.087591
414.117266	15792.522664	30.092608
414.355116	15815.623679	30.097626
414.984564	15836.101942	30.102644
415.442987	15858.966323	30.107661
415.549442	15877.318843	30.112679
416.399670	15894.800026	30.117696
416.680404	15910.045854	30.122714
417.366519	15924.438602	30.127732
417.872482	15939.131199	30.132749
417.840605	15963.395869	30.137767
418.572621	15963.688702	30.142784
418.664501	15991.076626	30.147802
418.998729	16007.002685	30.152820
419.479916	16031.446066	30.157837
419.604883	16058.582548	30.162855
420.441121	16059.774998	30.167872
420.607321	16098.411173	30.172890
421.337736	16118.194864	30.177908
421.858853	16119.938865	30.182925
421.998174	16141.274356	30.187943
422.391766	16160.915026	30.192960
422.905419	16171.813327	30.197978
423.231436	16192.617442	30.202996
423.797185	16199.714322	30.208013
423.652740	16224.584422	30.213031
424.491877	16240.775859	30.218048
424.671123	16267.882026	30.223066
424.784870	16278.084999	30.228084
425.408418	16297.803496	30.233101
425.863865	16329.667332	30.238119
426.752832	16349.173751	30.243136
426.674115	16375.720369	30.248154
427.150743	16388.345955	30.253172
427.736782	16402.404149	30.258189
427.981238	16439.939082	30.263207
428.522248	16451.806068	30.268224
428.664219	16477.269644	30.273242
429.490317	16499.679232	30.278260
429.791859	16515.301301	30.283277
429.962662	16548.602978	30.288295
430.481595	16575.953271	30.293312
430.884872	16606.227539	30.298330
431.287104	16619.114452	30.303348
431.918886	16641.245109	30.308365
432.121605	16678.787044	30.313383
433.031328	16703.505279	30.318400
432.981783	16732.707290	30.323418
433.514107	16750.630708	30.328436
434.309204	16775.790233	30.333453
434.846055	16797.724318	30.338471
435.440804	16824.807249	30.343488
435.689660	16838.795395	30.348506
436.037707	16871.024390	30.353524
436.162602	16887.413529	30.358541
436.157459	16911.507803	30.363559
437.047959	16942.814937	30.368576
437.553420	16965.682746	30.373594
438.133697	16989.404310	30.378612
438.672486	17011.979524	30.383629
438.976375	17034.711584	30.388647
439.283823	17070.235344	30.393664
440.026525	17097.914566	30.398682
440.271761	17114.016569	30.403700
440.662424	17128.674444	30.408717
441.454206	17169.302606	30.413735
441.942032	17176.731074	30.418752
442.357675	17207.582373	30.423770
442.642002	17240.981174	30.428788
443.014456	17256.747509	30.433805
443.256294	17283.722116	30.438823
443.755741	17304.737164	30.443840
444.295070	17332.044275	30.448858
444.666139	17366.427830	30.453876
445.187511	17389.625305	30.458893
445.374168	17418.434430	30.463911
445.817377	17439.123619	30.468928
446.324353	17465.216752	30.473946
446.575648	17493.194617	30.478964
447.470881	17527.123637	30.483981
447.755363	17557.231645	30.488999
448.416377	17581.380345	30.494016
448.942402	17604.924804	30.499034
449.228091	17627.913106	30.504052
449.789726	17650.030641	30.509069
450.414044	17684.646741	30.514087
450.668422	17703.685374	30.519104
451.212614	17723.234561	30.524122
451.033782	17730.142243	30.529140
452.129917	17746.357875	30.534157
452.541039	17785.227554	30.539175
452.962027	17798.800915	30.544192
453.397848	17814.178738	30.549210
453.720722	17842.234341	30.554228
454.343621	17848.675350	30.559245
454.835946	17879.926344	30.564263
454.941323	17899.411775	30.569280
455.354843	17914.445712	30.574298
455.555824	17950.379446	30.579316
456.237219	17972.996624	30.584333
456.320003	18004.059267	30.589351
457.058758	18035.271913	30.594368
457.643414	18054.638208	30.599386
457.901364	18080.897527	30.604404
458.675760	18102.281016	30.609421
459.167290	18143.280449	30.614439
459.776883	18156.672901	30.619456
460.351199	18177.468696	30.624474
460.742727	18210.605995	30.629492
461.128549	18229.037027	30.634509
461.580151	18248.215878	30.639527
462.153740	18262.770153	30.644544
462.318716	18290.446813	30.649562
462.880598	18324.138839	30.654580
463.403334	18342.782284	30.659597
463.449976	18373.560571	30.664615
463.829889	18408.961721	30.669632
464.752334	18436.589441	30.674650
464.935983	18472.526856	30.679668
465.836648	18490.201513	30.684685
466.329960	18527.676250	30.689703
466.560823	18541.336771	30.694720
467.070857	18574.487719	30.699738
467.651946	18593.343383	30.704756
468.449759	18623.637987	30.709773
468.712421	18649.922609	30.714791
469.198208	18670.777023	30.719808
469.822846	18683.902143	30.724826
469.711144	18712.589345	30.729844
470.480288	18736.867860	30.734861
470.820505	18761.554744	30.739879
471.279426	18791.618393	30.744896
471.624763	18819.343369	30.749914
472.182745	18855.109140	30.754932
472.676884	18870.623977	30.759949
473.480436	18895.908141	30.764967
474.006031	18928.804546	30.769984
474.387368	18947.483356	30.775002
474.753445	18985.124212	30.780020
475.465055	18999.903817	30.785037
475.878856	19030.524550	30.790055
476.326381	19057.286190	30.795072
476.891308	19075.550982	30.800090
477.258379	19099.008434	30.805108
477.592078	19123.911605	30.810125
478.002639	19153.098892	30.815143
478.390852	19175.599133	30.820160
479.051557	19203.578517	30.825178
479.868100	19239.974190	30.830196
480.210601	19261.199164	30.835213
480.776617	19281.163485	30.840231
480.838971	19306.008302	30.845248
481.945393	19340.324403	30.850266
482.202737	19362.295700	30.855284
482.350457	19376.348904	30.860301
483.166058	19402.453168	30.865319
483.321615	19415.822839	30.870336
483.953644	19443.592251	30.875354
484.087093	19470.561601	30.880372
484.329258	19489.496493	30.885389
484.844617	19511.238008	30.890407
485.418227	19537.241360	30.895424
486.392300	19562.885080	30.900442
486.430217	19601.709440	30.905460
486.741098	19611.472625	30.910477
487.441633	19635.219664	30.915495
487.912101	19667.538378	30.920512
488.766799	19679.516173	30.925530
488.908154	19712.947934	30.930548
489.336401	19735.720544	30.935565
489.947416	19768.731349	30.940583
490.476705	19797.117569	30.945600
491.218207	19818.609193	30.950618
491.191486	19848.605223	30.955636
492.083520	19875.443681	30.960653
492.647403	19910.881927	30.965671
493.152595	19924.525725	30.970688
493.898851	19955.373834	30.975706
493.877136	19985.419834	30.980724
494.214416	20020.780046	30.985741
494.780667	20034.148995	30.990759
495.596818	20060.759505	30.995776
496.400768	20094.865269	31.000794
496.418407	20121.360840	31.005812
496.977404	20152.036410	31.010829
497.590157	20183.120606	31.015847
498.254495	20200.758023	31.020864
498.764039	20228.212873	31.025882
499.217217	20258.981002	31.030900
499.928402	20276.939696	31.035917
500.439280	20297.235923	31.040935
501.003630	20326.223968	31.045952
501.401862	20346.127205	31.050970
502.046205	20380.226874	31.055988
502.208824	20395.775897	31.061005
502.870523	20429.645478	31.066023
503.395384	20447.690377	31.071040
503.658668	20479.897564	31.076058
504.270608	20503.444716	31.081076
504.709817	20528.560609	31.086093
505.231379	20554.497649	31.091111
505.263514	20582.413186	31.096128
505.847596	20620.572737	31.101146
506.358964	20650.201390	31.106164
506.974179	20681.349175	31.111181
507.773111	20712.525101	31.116199
508.124338	20748.307768	31.121216
508.936253	20767.874952	31.126234
509.421410	20802.404663	31.131252
509.924717	20837.039004	31.136269
510.084620	20858.250083	31.141287
510.702723	20884.930645	31.146304
511.478580	20926.314725	31.151322
512.075461	20945.125966	31.156340
512.650082	20972.912861	31.161357
512.957485	20989.077837	31.166375
513.219635	21020.369917	31.171392
514.119026	21041.269500	31.176410
514.512867	21071.296303	31.181428
514.989395	21098.700678	31.186445
515.793177	21133.092608	31.191463
516.020931	21160.163242	31.196480
516.506775	21187.572600	31.201498
516.672480	21208.113387	31.206516
517.449730	21227.699098	31.211533
517.982247	21249.572547	31.216551
518.440091	21275.387831	31.221568
519.010514	21297.261715	31.226586
519.605035	21317.842869	31.231604
519.846264	21344.741047	31.236621
520.589528	21372.792747	31.241639
520.560835	21396.877290	31.246656
521.407353	21415.018027	31.251674
521.854974	21455.942829	31.256692
522.018504	21481.911896	31.261709
523.113978	21503.059279	31.266727
523.129001	21543.363290	31.271744
524.066089	21560.061974	31.276762
524.314428	21591.597231	31.281780
524.673064	21636.397018	31.286797
525.366975	21667.679370	31.291815
525.865077	21705.102575	31.296832
526.176853	21737.405324	31.301850
526.801429	21773.519842	31.306868
527.611777	21809.447364	31.311885
528.214620	21834.425561	31.316903
528.367519	21881.242196	31.321920
529.184259	21905.896321	31.326938
529.875571	21943.908952	31.331956
530.132617	21977.749797	31.336973
530.944695	21993.539575	31.341991
531.256475	22035.061858	31.347008
532.370233	22064.080155	31.352026
532.695405	22085.462551	31.357044
532.953346	22117.306763	31.362061
533.825737	22148.277579	31.367079
534.408928	22188.613974	31.372096
535.057334	22211.178047	31.377114
535.616334	22240.365635	31.382132
535.764104	22277.750012	31.387149
536.442501	22297.522881	31.392167
536.974279	22330.619910	31.397184
537.528510	22367.428968	31.402202
537.526378	22393.216656	31.407220
538.109543	22434.059065	31.412237
539.018676	22449.631805	31.417255
539.547572	22491.291650	31.422272
540.130381	22525.575284	31.427290
540.783853	22553.895486	31.432308
541.290813	22594.889179	31.437325
541.902450	22626.356548	31.442343
542.585791	22655.133499	31.447360
542.854928	22687.103253	31.452378
543.265616	22720.396829	31.457396
543.823221	22748.997722	31.462413
544.712962	22775.139100	31.467431
544.766682	22825.227778	31.472448
545.621164	22849.289505	31.477466
546.173875	22877.625951	31.482484
546.999623	22912.478833	31.487501
547.493874	22934.802476	31.492519
547.769115	22967.643753	31.497536
548.428734	23003.426438	31.502554
549.131419	23039.398335	31.507572
549.462466	23065.153668	31.512589
550.210860	23086.180181	31.517607
550.499056	23122.033891	31.522624
551.359091	23152.818643	31.527642
551.970786	23180.381671	31.532660
552.337369	23207.471277	31.537677
553.473539	23233.467241	31.542695
553.525786	23253.522389	31.547712
554.629224	23270.032176	31.552730
555.153974	23303.365738	31.557748
555.782328	23313.700320	31.562765
555.988837	23335.595544	31.567783
556.560150	23356.346758	31.572800
557.276286	23365.049910	31.577818
557.987458	23381.330544	31.582836
558.428596	23400.699334	31.587853
558.671202	23421.306203	31.592871
559.613639	23437.297895	31.597888
559.712440	23460.638265	31.602906
560.275463	23478.073321	31.607924
560.857177	23503.966903	31.612941
561.626518	23521.742517	31.617959
562.014340	23552.873576	31.622976
561.855512	23578.042778	31.627994
562.794273	23606.345079	31.633012
563.137635	23647.575103	31.638029
563.622692	23675.733706	31.643047
564.222981	23716.121084	31.648064
564.960567	23743.456641	31.653082
565.962672	23768.482176	31.658100
566.600015	23803.321895	31.663117
567.170674	23829.729498	31.668135
567.995021	23857.500295	31.673152
568.136121	23886.218613	31.678170
569.026025	23915.047193	31.683188
569.210006	23934.690595	31.688205
569.724731	23964.380565	31.693223
570.319867	23989.621782	31.698240
570.738208	24029.368437	31.703258
571.901770	24061.206634	31.708276
572.015461	24094.195139	31.713293
572.603882	24129.453853	31.718311
573.181123	24157.301686	31.723328
573.442683	24206.444965	31.728346
574.092700	24236.550192	31.733364
574.137082	24272.993950	31.738381
574.883302	24306.060684	31.743399
575.694528	24334.864277	31.748416
576.161578	24382.181070	31.753434
576.790083	24400.061682	31.758452
577.591521	24444.387681	31.763469
578.407969	24481.835775	31.768487
579.014922	24523.557164	31.773504
579.189044	24556.941417	31.778522
579.816461	24586.444034	31.783540
580.624325	24621.157362	31.788557
581.448321	24655.318420	31.793575
581.985058	24693.322603	31.798592
582.369528	24730.813540	31.803610
582.997708	24759.027092	31.808628
583.848627	24786.706548	31.813645
584.192893	24825.992414	31.818663
584.910322	24842.601888	31.823680
584.984737	24881.538308	31.828698
586.229280	24921.043583	31.833716
586.872260	24952.244294	31.838733
587.124063	24986.451294	31.843751
587.553673	25017.660244	31.848768
588.132980	25059.892656	31.853786
588.895294	25089.589759	31.858804
589.281519	25130.455900	31.863821
589.655899	25166.306099	31.868839
590.531678	25198.526131	31.873856
591.065203	25233.365643	31.878874
591.642572	25264.286405	31.883892
592.307883	25302.492799	31.888909
592.865792	25323.494632	31.893927
593.383042	25349.122632	31.898944
593.778229	25383.010820	31.903962
594.725688	25403.875890	31.908980
595.323554	25447.382815	31.913997
595.821619	25479.687734	31.919015
596.490876	25508.319337	31.924032
596.799668	25546.190199	31.929050
597.320844	25568.917046	31.934068
597.816056	25618.722374	31.939085
598.562562	25643.050866	31.944103
599.252965	25681.254051	31.949120
599.638771	25717.646955	31.954138
600.898406	25743.658464	31.959156
601.085745	25784.715081	31.964173
601.830455	25815.661044	31.969191
602.583105	25854.941841	31.974208
603.199790	25884.429089	31.979226
603.630227	25907.417009	31.984244
604.181804	25944.365799	31.989261
604.582061	25986.583958	31.994279
605.274762	26024.521994	31.999296
605.568816	26062.547815	32.004314
606.229373	26095.150595	32.009332
607.168762	26145.993667	32.014349
607.733087	26185.961890	32.019367
608.336453	26220.267607	32.024384
609.109822	26250.514541	32.029402
609.792928	26280.465973	32.034420
610.159417	26321.470342	32.039437
610.998095	26365.308101	32.044455
611.690770	26402.488437	32.049472
612.335102	26439.303524	32.054490
612.497923	26466.859219	32.059508
613.410624	26510.078963	32.064525
614.002681	26547.325885	32.069543
614.929524	26582.415821	32.074560
615.185938	26616.694386	32.079578
615.895100	26657.784815	32.084596
616.050330	26698.172052	32.089613
616.742167	26738.993589	32.094631
617.631976	26782.615677	32.099648
618.465936	26829.741713	32.104666
619.056208	26868.664377	32.109684
620.144695	26904.481671	32.114701
620.412175	26941.925519	32.119719
621.021812	26966.770030	32.124736
621.482963	27008.121222	32.129754
622.169488	27045.253141	32.134772
622.587261	27088.943495	32.139789
623.111621	27119.799561	32.144807
624.109659	27153.792237	32.149824
624.829807	27215.404324	32.154842
625.395793	27245.729470	32.159860
626.410587	27274.518039	32.164877
626.434083	27313.770497	32.169895
627.396282	27341.910075	32.174912
627.612328	27380.462541	32.179930
628.462217	27406.748949	32.184948
629.330093	27451.494632	32.189965
629.655230	27496.856332	32.194983
630.448980	27525.945337	32.200000
631.254458	27555.582430	32.205018
631.954715	27586.108274	32.210036
632.873243	27619.791840	32.215053
633.731482	27658.351707	32.220071
634.143831	27683.373367	32.225088
634.551174	27712.409385	32.230106
634.943884	27733.426959	32.235124
635.906567	27759.828892	32.240141
636.263290	27792.614722	32.245159
637.105895	27813.403907	32.250176
637.500742	27850.943253	32.255194
637.736389	27873.034786	32.260212
638.714937	27899.876859	32.265229
639.258492	27931.862540	32.270247
639.844425	27951.952553	32.275264
640.286103	27996.342702	32.280282
640.754869	28036.917358	32.285300
641.950334	28074.173714	32.290317
642.212289	28109.231369	32.295335
642.824426	28140.574571	32.300352
643.390954	28176.140862	32.305370
644.292267	28213.936555	32.310388
645.077730	28247.079459	32.315405
645.508492	28286.111989	32.320423
646.294557	28313.130129	32.325440
647.042838	28351.651645	32.330458
647.646983	28389.367789	32.335476
648.228234	28420.804750	32.340493
648.642883	28467.861198	32.345511
649.649304	28499.288582	32.350528
650.180752	28534.336365	32.355546
650.971641	28571.890864	32.360564
651.936542	28609.449784	32.365581
652.497755	28650.769680	32.370599
653.100573	28679.390892	32.375616
653.593633	28719.229881	32.380634
653.921075	28749.999163	32.385652
654.697871	28788.769873	32.390669
655.197787	28830.978334	32.395687
656.153405	28868.931081	32.400704
656.795254	28916.376479	32.405722
657.612903	28954.900912	32.410740
658.016410	28988.496735	32.415757
658.663919	29032.566136	32.420775
659.480145	29070.737037	32.425792
659.958273	29104.043241	32.430810
660.599145	29147.899017	32.435828
661.759564	29181.774841	32.440845
662.256826	29215.400601	32.445863
663.233364	29250.588500	32.450880
664.009715	29292.470175	32.455898
664.307999	29320.084364	32.460916
665.322622	29351.347430	32.465933
665.833649	29395.394739	32.470951
666.869191	29421.054176	32.475968
667.264180	29460.796187	32.480986
667.560357	29493.708006	32.486004
668.482792	29523.140013	32.491021
668.654975	29565.508771	32.496039
669.650910	29608.045704	32.501056
670.473844	29648.327886	32.506074
671.172534	29679.065706	32.511092
671.814811	29718.687314	32.516109
672.212015	29743.947753	32.521127
673.064157	29793.991854	32.526144
673.646345	29826.069267	32.531162
674.159967	29874.617887	32.536180
674.831547	29909.450119	32.541197
675.452319	29952.027554	32.546215
676.264256	29991.850683	32.551232
677.010155	30035.590768	32.556250
677.540158	30082.259898	32.561268
678.250454	30108.698079	32.566285
678.567049	30159.105075	32.571303
679.130478	30187.797775	32.576320
679.932252	30216.902002	32.581338
680.324221	30261.241626	32.586356
681.021145	30297.726735	32.591373
681.783796	30342.292942	32.596391
682.513893	30373.741195	32.601408
682.920219	30423.243472	32.606426
683.471308	30460.352237	32.611444
684.543954	30508.448163	32.616461
684.924252	30557.929552	32.621479
685.846575	30606.833105	32.626496
686.551427	30644.006620	32.631514
687.131873	30689.297470	32.636532
687.667017	30736.675279	32.641549
688.601942	30778.832256	32.646567
689.197211	30819.354671	32.651584
690.281667	30857.828246	32.656602
690.414598	30907.368174	32.661620
691.390135	30952.566120	32.666637
692.211113	31001.025005	32.671655
692.782188	31042.158514	32.676672
693.736365	31098.163681	32.681690
694.354230	31143.468630	32.686708
695.356688	31185.451500	32.691725
695.825963	31226.361096	32.696743
696.369321	31268.934404	32.701760
697.278141	31306.159350	32.706778
697.894647	31355.491864	32.711796
698.619436	31392.537170	32.716813
699.075953	31443.974779	32.721831
700.003252	31488.637785	32.726848
700.676286	31535.110787	32.731866
701.426943	31581.318868	32.736884
702.332013	31627.806313	32.741901
703.054760	31679.904528	32.746919
704.143104	31719.978504	32.751936
704.835907	31754.595584	32.756954
705.398300	31805.024987	32.761972
706.152737	31835.137752	32.766989
707.010529	31878.478583	32.772007
707.428299	31922.349906	32.777024
708.346315	31961.224586	32.782042
709.230794	31998.587346	32.787060
710.269242	32036.058821	32.792077
710.731418	32082.452274	32.797095
711.367811	32110.750581	32.802112
712.009845	32141.918184	32.807130
712.480727	32192.988726	32.812148
713.510967	32219.259387	32.817165
713.741819	32269.786090	32.822183
714.617876	32307.536362	32.827200
715.284502	32348.923018	32.832218
715.607571	32401.306898	32.837236
716.449489	32432.108569	32.842253
717.107789	32487.588517	32.847271
718.125892	32538.397193	32.852288
718.695691	32581.386300	32.857306
719.228928	32626.543361	32.862324
720.682945	32667.978040	32.867341
721.269498	32709.415884	32.872359
721.549983	32758.880210	32.877376
722.747333	32797.036245	32.882394
723.260685	32838.681793	32.887412
724.174342	32879.569303	32.892429
724.630507	32922.191258	32.897447
725.300139	32968.358206	32.902464
725.964230	33012.319689	32.907482
726.515073	33056.393832	32.912500
727.510883	33101.296137	32.917517
728.148479	33140.166354	32.922535
729.046003	33174.134159	32.927552
729.646822	33200.169842	32.932570
730.501513	33230.205704	32.937588
731.261664	33263.455466	32.942605
731.882828	33310.130216	32.947623
732.388728	33343.363020	32.952640
733.718018	33381.904090	32.957658
734.184442	33416.489836	32.962676
735.136161	33450.392703	32.967693
735.702167	33486.278008	32.972711
736.611344	33526.383519	32.977728
737.551656	33569.190189	32.982746
738.155886	33606.466949	32.987764
739.027479	33635.362725	32.992781
739.268543	33667.676520	32.997799
739.889974	33704.438649	33.002816
740.960798	33744.601456	33.007834
741.676948	33785.110712	33.012852
742.616163	33817.511402	33.017869
743.205950	33856.263987	33.022887
743.860338	33900.462784	33.027904
744.668217	33942.133949	33.032922
745.038627	33991.062336	33.037940
745.900606	34025.100314	33.042957
746.483507	34068.210548	33.047975
746.965072	34118.677154	33.052992
747.913137	34164.303657	33.058010
748.578956	34220.621587	33.063028
748.924592	34272.374353	33.068045
749.794061	34321.269612	33.073063
750.770732	34374.681481	33.078080
751.522378	34419.530007	33.083098
752.624756	34484.625576	33.088116
753.349993	34537.925490	33.093133
754.225551	34583.045800	33.098151
754.864028	34626.338152	33.103168
755.596672	34671.057413	33.108186
756.391376	34734.678174	33.113204
757.639318	34779.727946	33.118221
758.252591	34813.629111	33.123239
758.899026	34859.260095	33.128256
759.739078	34898.038633	33.133274
760.498481	34943.740627	33.138292
760.879032	35003.114942	33.143309
762.030819	35044.766049	33.148327
762.753290	35091.877802	33.153344
763.244002	35135.712806	33.158362
763.943200	35188.854047	33.163380
764.625052	35231.875289	33.168397
765.757072	35289.305433	33.173415
766.481246	35339.901359	33.178432
767.443321	35374.431671	33.183450
768.237011	35433.963798	33.188468
769.074618	35468.924744	33.193485
769.680911	35516.005051	33.198503
770.111292	35563.675749	33.203520
771.019958	35601.705052	33.208538
771.588268	35653.571753	33.213556
772.650269	35707.454173	33.218573
773.794906	35747.893776	33.223591
774.377425	35792.803314	33.228608
775.610353	35827.804116	33.233626
775.962115	35878.130848	33.238644
777.274502	35913.776943	33.243661
778.169950	35956.652394	33.248679
778.482477	35993.036915	33.253696
779.087882	36029.944710	33.258714
779.808038	36065.519401	33.263732
780.415307	36093.562066	33.268749
781.027425	36133.782287	33.273767
781.588858	36178.234356	33.278784
782.254090	36221.816643	33.283802
782.938078	36266.919957	33.288820
783.686686	36303.306275	33.293837
784.881259	36359.167704	33.298855
785.347964	36410.818206	33.303872
786.273565	36450.724363	33.308890
787.025201	36497.164411	33.313908
787.653420	36542.327627	33.318925
788.542803	36594.430889	33.323943
789.548131	36649.905382	33.328960
790.246855	36698.187896	33.333978
790.998913	36747.891228	33.338996
791.682898	36795.853783	33.344013
792.904774	36839.242671	33.349031
793.356530	36893.381739	33.354048
794.421562	36948.955158	33.359066
795.388305	36997.594749	33.364084
796.180438	37048.898637	33.369101
797.094981	37090.009163	33.374119
798.010707	37136.911808	33.379136
798.617226	37180.941563	33.384154
799.399416	37223.419956	33.389172
800.207142	37279.173641	33.394189
800.949053	37314.936715	33.399207
801.692235	37366.179472	33.404224
802.611194	37415.668518	33.409242
803.418876	37471.966531	33.414260
803.911720	37517.760062	33.419277
804.693582	37566.088428	33.424295
805.612852	37614.983475	33.429312
806.728065	37661.697945	33.434330
807.498152	37724.376644	33.439348
808.382912	37773.688489	33.444365
809.535146	37816.097465	33.449383
810.269321	37865.262364	33.454400
810.552438	37918.108794	33.459418
811.580589	37962.706494	33.464436
812.723000	38010.859255	33.469453
812.871783	38059.351103	33.474471
814.237748	38127.761764	33.479488
814.874039	38171.763596	33.484506
815.792266	38224.776923	33.489524
816.410070	38267.156651	33.494541
817.202210	38304.469146	33.499559
817.839121	38370.414658	33.504576
818.968880	38420.353618	33.509594
819.877375	38463.915026	33.514612
820.627531	38527.743791	33.519629
821.474246	38567.046517	33.524647
822.081556	38626.161407	33.529664
822.726633	38675.810073	33.534682
823.639218	38734.820543	33.539700
824.482656	38784.994899	33.544717
825.634523	38830.049316	33.549735
826.216533	38893.032795	33.554752
827.303524	38941.310148	33.559770
828.399142	38991.862876	33.564788
829.198816	39039.306412	33.569805
830.189842	39070.625608	33.574823
831.135087	39133.673065	33.579840
831.895728	39180.269286	33.584858
832.773320	39219.694847	33.589876
833.754273	39267.123146	33.594893
834.445236	39290.717433	33.599911
834.780824	39339.088042	33.604928
835.262853	39372.574312	33.609946
836.348388	39411.853829	33.614964
837.260535	39443.774056	33.619981
838.044694	39484.568081	33.624999
838.515634	39532.955872	33.630016
838.969528	39582.617586	33.635034
840.091008	39621.695809	33.640052
840.520071	39687.564051	33.645069
841.997147	39722.280036	33.650087
842.896278	39778.999798	33.655104
843.358550	39832.518513	33.660122
844.823864	39878.360827	33.665140
845.210960	39933.156401	33.670157
846.013324	39982.011881	33.675175
846.795768	40033.817686	33.680192
847.480101	40092.646252	33.685210
848.721761	40142.881561	33.690228
849.457158	40201.708751	33.695245
850.662538	40252.449613	33.700263
851.598544	40312.086821	33.705280
852.326022	40358.671795	33.710298
852.960286	40410.419484	33.715316
853.943715	40464.047876	33.720333
854.996104	40512.340476	33.725351
856.026226	40559.055571	33.730368
856.835549	40618.327667	33.735386
857.904087	40657.523563	33.740404
858.596175	40706.075392	33.745421
859.862403	40759.021461	33.750439
860.496077	40810.283209	33.755456
861.098074	40863.763606	33.760474
862.353038	40895.075736	33.765492
862.894905	40947.402046	33.770509
864.118193	40990.818054	33.775527
864.832077	41041.517552	33.780544
865.455853	41091.801209	33.785562
866.479646	41129.834920	33.790580
867.127598	41195.066285	33.795597
868.065829	41250.632686	33.800615
868.959293	41310.355180	33.805632
870.075582	41357.381050	33.810650
870.847255	41405.827103	33.815668
871.670664	41456.364947	33.820685
872.540769	41502.765589	33.825703
873.287713	41555.636787	33.830720
874.004078	41617.323201	33.835738
875.200913	41665.513515	33.840756
876.369690	41715.770189	33.845773
876.847048	41756.452068	33.850791
877.875846	41816.780902	33.855808
878.683234	41869.814161	33.860826
879.472379	41918.144766	33.865844
880.642494	41971.355490	33.870861
881.654759	42029.176552	33.875879
882.430052	42074.340937	33.880896
883.029290	42129.621107	33.885914
884.007407	42175.089157	33.890932
884.914335	42232.067066	33.895949
885.853142	42279.793143	33.900967
886.534266	42338.678852	33.905984
887.666070	42387.064357	33.911002
888.694138	42436.528801	33.916020
889.292738	42497.843981	33.921037
889.781311	42544.913764	33.926055
890.765195	42600.805333	33.931072
891.685427	42644.113950	33.936090
892.533406	42689.894392	33.941108
893.413600	42739.913972	33.946125
894.728006	42783.654495	33.951143
895.260334	42828.213318	33.956160
896.125257	42884.769390	33.961178
897.060018	42911.087151	33.966196
897.833927	42985.753760	33.971213
898.802041	43019.624911	33.976231
899.601671	43062.605354	33.981248
900.141445	43118.049116	33.986266
900.907044	43165.159070	33.991284
901.937144	43235.592840	33.996301
902.754918	43283.080711	34.001319
903.992245	43343.349450	34.006336
904.863444	43401.594688	34.011354
906.058233	43451.693126	34.016372
906.740169	43518.115193	34.021389
907.726299	43568.404698	34.026407
908.567628	43616.041401	34.031424
909.348472	43663.630751	34.036442
910.508874	43726.765281	34.041460
911.569729	43792.875829	34.046477
912.559328	43850.439549	34.051495
913.486498	43902.402608	34.056512
914.064246	43960.518153	34.061530
915.366383	44011.916727	34.066548
916.584792	44071.557872	34.071565
917.173484	44122.828049	34.076583
918.339492	44174.419100	34.081600
919.321397	44228.556625	34.086618
920.146717	44267.113899	34.091636
920.902357	44334.304897	34.096653
921.718972	44398.867797	34.101671
923.194116	44442.137326	34.106688
923.840766	44504.576474	34.111706
924.824239	44551.345308	34.116724
925.632226	44619.035012	34.121741
926.564309	44674.604672	34.126759
927.897025	44720.813133	34.131776
928.678856	44774.742941	34.136794
930.084380	44823.015010	34.141812
930.629529	44873.465077	34.146829
931.388518	44924.172755	34.151847
932.643017	44974.935800	34.156864
933.683370	45022.639240	34.161882
934.839230	45073.266139	34.166900
935.545912	45121.313016	34.171917
936.308816	45168.092378	34.176935
937.604363	45220.095720	34.181952
938.297273	45278.538258	34.186970
939.540082	45326.590193	34.191988
940.611220	45373.321722	34.197005
941.360533	45419.850708	34.202023
942.445960	45467.212775	34.207040
943.324344	45529.903165	34.212058
944.248682	45558.642165	34.217076
944.891954	45609.097505	34.222093
945.585948	45655.553407	34.227111
946.879765	45695.690843	34.232128
947.691648	45750.200278	34.237146
949.017816	45801.213342	34.242164
949.678929	45849.072814	34.247181
950.505254	45898.329852	34.252199
951.607990	45939.939953	34.257216
952.479848	45999.026900	34.262234
953.517885	46042.133918	34.267252
954.351304	46091.402920	34.272269
955.236980	46152.069598	34.277287
956.075386	46192.241275	34.282304
956.512403	46226.871028	34.287322
957.437349	46272.121734	34.292340
958.633391	46321.233246	34.297357
959.378624	46376.494783	34.302375
960.564375	46415.302982	34.307392
960.767874	46476.545474	34.312410
961.665168	46525.198123	34.317428
962.866930	46577.946802	34.322445
963.760405	46638.980486	34.327463
964.975672	46697.800410	34.332480
965.977092	46749.884986	34.337498
966.782042	46812.843499	34.342516
968.014903	46865.708182	34.347533
968.810312	46925.872330	34.352551
970.068028	46984.863491	34.357568
971.113532	47051.435234	34.362586
972.157831	47095.960369	34.367604
973.208914	47155.692870	34.372621
973.880562	47204.546797	34.377639
975.016112	47258.933292	34.382656
975.899771	47326.404214	34.387674
976.884012	47383.338899	34.392692
977.920931	47441.397895	34.397709
979.023848	47505.716132	34.402727
979.874708	47561.115863	34.407744
980.834120	47624.387748	34.412762
981.630380	47685.964570	34.417780
982.810395	47744.678865	34.422797
983.503721	47813.357753	34.427815
985.004474	47869.902793	34.432832
985.756427	47929.538662	34.437850
986.607088	47989.260457	34.442868
987.655533	48057.435299	34.447885
988.544055	48116.158236	34.452903
990.185568	48179.786709	34.457920
991.089912	48243.385269	34.462938
991.591536	48298.379638	34.467956
993.101924	48355.531733	34.472973
994.058521	48424.139611	34.477991
995.001827	48475.971538	34.483008
995.956532	48545.377234	34.488026
997.095874	48606.611806	34.493044
998.156598	48666.232894	34.498061
999.053215	48727.328647	34.503079
1000.315133	48785.615245	34.508096
1001.363993	48850.964355	34.513114
1002.291565	48895.694776	34.518132
1003.446912	48951.189407	34.523149
1004.318657	49009.695836	34.528167
1005.462468	49069.393544	34.533184
1006.128376	49118.366364	34.538202
1007.303634	49180.457299	34.543220
1008.561415	49239.827594	34.548237
1009.744424	49306.200932	34.553255
1010.671612	49355.645827	34.558272
1011.875045	49397.942481	34.563290
1012.841356	49454.182870	34.568308
1013.957647	49499.460673	34.573325
1014.765277	49551.031573	34.578343
1016.026273	49608.365050	34.583360
1016.874116	49649.091818	34.588378
1017.790701	49716.805087	34.593396
1018.834017	49752.642317	34.598413
1019.802630	49812.508588	34.603431
1020.490486	49868.787265	34.608448
1021.685379	49917.982668	34.613466
1022.777486	49968.358447	34.618484
1023.467068	50014.336783	34.623501
1024.702230	50061.185177	34.628519
1025.648979	50101.713779	34.633536
1026.326364	50156.647132	34.638554
1027.447103	50208.645019	34.643572
1028.509004	50249.073599	34.648589
1029.247504	50305.902203	34.653607
1030.681751	50360.046865	34.658624
1031.307254	50410.990188	34.663642
1032.098922	50465.431847	34.668660
1033.523810	50522.874819	34.673677
1034.397516	50582.460576	34.678695
1035.269376	50637.586080	34.683712
1036.356232	50699.479842	34.688730
1037.210667	50763.276702	34.693748
1038.462843	50811.490652	34.698765
1039.290167	50875.418612	34.703783
1040.761637	50935.576057	34.708800
1041.669855	50995.347296	34.713818
1042.955430	51054.983680	34.718836
1044.045376	51111.215092	34.723853
1044.708863	51177.757429	34.728871
1046.259242	51224.052650	34.733888
1047.635590	51288.167871	34.738906
1048.862485	51337.690324	34.743924
1049.925479	51395.065582	34.748941
1050.493053	51451.620049	34.753959
1051.829585	51507.813818	34.758976
1052.666124	51562.016919	34.763994
1053.632773	51621.432616	34.769012
1055.119073	51678.780266	34.774029
1056.163709	51734.286294	34.779047
1057.321858	51786.977910	34.784064
1058.662364	51844.766415	34.789082
1059.294558	51905.709525	34.794100
1060.853942	51951.410002	34.799117
1061.724588	51994.174826	34.804135
1062.950359	52068.458924	34.809152
1063.949964	52110.172370	34.814170
1064.800297	52166.102165	34.819188
1065.987215	52217.625967	34.824205
1066.942244	52278.513181	34.829223
1067.700571	52330.781397	34.834240
1069.078940	52382.572993	34.839258
1069.709716	52449.427823	34.844276
1070.998191	52495.051560	34.849293
1072.248530	52560.696027	34.854311
1073.315160	52617.504238	34.859328
1074.539572	52683.488482	34.864346
1075.126539	52740.922608	34.869364
1076.106087	52800.541786	34.874381
1077.228375	52868.497838	34.879399
1078.680823	52919.601952	34.884416
1079.519854	52981.945584	34.889434
1080.898852	53061.429347	34.894452
1081.927090	53101.906148	34.899469
1082.536093	53169.867502	34.904487
1084.209448	53216.527123	34.909504
1085.452642	53266.993999	34.914522
1086.006708	53326.295128	34.919540
1087.463789	53378.576522	34.924557
1088.474425	53445.735422	34.929575
1089.601288	53507.263375	34.934592
1091.219779	53559.817320	34.939610
1091.868178	53620.357372	34.944628
1093.090723	53665.398884	34.949645
1094.033500	53718.413346	34.954663
1095.001274	53777.290144	34.959680
1096.096465	53828.781239	34.964698
1096.625551	53877.962724	34.969716
1097.695658	53931.096950	34.974733
1098.548150	53986.878886	34.979751
1099.645149	54039.091567	34.984768
1100.755455	54096.061060	34.989786
1101.808547	54154.919118	34.994804
1103.039767	54203.358539	34.999821
1103.924718	54268.590385	35.004839
1105.139966	54335.681825	35.009856
1106.422493	54394.105883	35.014874
1107.002954	54454.443555	35.019892
1108.627803	54510.466523	35.024909
1109.716587	54583.090396	35.029927
1110.445954	54649.372837	35.034944
1112.109850	54696.530497	35.039962
1112.860944	54767.923157	35.044980
1114.503087	54825.975567	35.049997
1115.254048	54898.944405	35.055015
1116.239340	54963.814401	35.060032
1117.528809	55021.821253	35.065050
1118.672494	55099.886883	35.070068
1119.928507	55145.786657	35.075085
1121.129225	55221.521220	35.080103
1122.402842	55282.511900	35.085120
1123.328577	55350.138840	35.090138
1124.708034	55413.011837	35.095156
1125.783472	55470.838128	35.100173
1126.932724	55546.461543	35.105191
1128.238012	55614.650014	35.110208
1129.321906	55663.336996	35.115226
1130.613350	55735.616247	35.120244
1131.659625	55794.688299	35.125261
1132.964644	55857.036194	35.130279
1134.090366	55908.913092	35.135296
1135.524178	55976.234441	35.140314
1136.214004	56037.153912	35.145332
1137.200799	56095.799345	35.150349
1139.059297	56155.529893	35.155367
1139.832342	56224.486940	35.160384
1141.027606	56281.302833	35.165402
1142.137393	56341.942159	35.170420
1143.757933	56405.887574	35.175437
1144.947300	56466.812211	35.180455
1145.751977	56521.107676	35.185472
1146.933324	56578.331499	35.190490
1147.878571	56638.541663	35.195508
1149.260258	56708.480725	35.200525
1150.713142	56763.238528	35.205543
1151.826115	56820.195166	35.210560
1153.062137	56871.272110	35.215578
1154.124587	56936.913863	35.220596
1155.414263	56989.001615	35.225613
1156.458164	57050.944158	35.230631
1157.467275	57112.006253	35.235648
1158.637242	57159.473986	35.240666
1159.843871	57225.593948	35.245684
1161.063413	57278.364184	35.250701
1161.907961	57342.009548	35.255719
1163.178302	57397.202440	35.260736
1164.584794	57458.146244	35.265754
1165.677465	57509.886228	35.270772
1166.832384	57564.774793	35.275789
1167.862405	57627.100743	35.280807
1168.766088	57683.408655	35.285824
1170.199174	57737.228749	35.290842
1171.530922	57799.501581	35.295860
1172.408182	57855.402638	35.300877
1173.461279	57891.833074	35.305895
1174.456528	57946.848775	35.310912
1175.325078	57994.409653	35.315930
1176.660287	58055.416766	35.320948
1178.030777	58104.760071	35.325965
1179.403199	58168.305995	35.330983
1179.967127	58214.889660	35.336000
1181.059269	58264.852831	35.341018
1182.228894	58336.070375	35.346036
1183.136193	58388.290649	35.351053
1184.599552	58448.822987	35.356071
1185.265327	58510.929757	35.361088
1186.694881	58573.777908	35.366106
1187.933767	58643.213296	35.371124
1189.071002	58709.240599	35.376141
1190.368079	58780.945852	35.381159
1191.830556	58848.080898	35.386176
1193.388123	58912.017537	35.391194
1194.291689	58981.696274	35.396212
1195.624429	59030.711923	35.401229
1197.141921	59093.199537	35.406247
1198.461604	59162.782004	35.411264
1199.429232	59226.020640	35.416282
1200.819968	59278.603891	35.421300
1201.852478	59344.484753	35.426317
1203.708365	59400.793181	35.431335
1204.538432	59466.699737	35.436352
1205.699968	59524.294454	35.441370
1207.122095	59584.677850	35.446388
1208.405582	59642.544919	35.451405
1209.599029	59696.970237	35.456423
1210.752626	59755.459225	35.461440
1212.162047	59818.117537	35.466458
1213.526790	59876.447168	35.471476
1214.665623	59941.300252	35.476493
1215.863503	60000.263954	35.481511
1217.022211	60057.632507	35.486528
1218.282688	60115.225795	35.491546
1219.208270	60179.365985	35.496564
1220.113065	60240.813111	35.501581
1221.458263	60308.685821	35.506599
1222.593172	60383.630399	35.511616
1224.089499	60442.016743	35.516634
1225.350941	60509.808176	35.521652
1226.464893	60565.672096	35.526669
1228.071416	60628.548501	35.531687
1228.747131	60700.742808	35.536704
1230.462459	60753.677218	35.541722
1231.649139	60819.759477	35.546740
1233.094907	60882.250255	35.551757
1234.237748	60938.889088	35.556775
1235.449036	61009.538240	35.561792
1236.809326	61069.795734	35.566810
1238.139280	61122.392482	35.571828
1239.564452	61190.919772	35.576845
1240.701985	61242.774637	35.581863
1241.664836	61309.975695	35.586880
1242.755514	61370.447045	35.591898
1244.482582	61437.978253	35.596916
1245.533243	61494.252993	35.601933
1246.990405	61548.349966	35.606951
1247.842850	61617.170666	35.611968
1249.308710	61666.803792	35.616986
1250.544617	61719.790022	35.622004
1251.657167	61780.898304	35.627021
1252.911334	61837.806641	35.632039
1254.151819	61907.478954	35.637056
1255.165266	61960.899331	35.642074
1256.428649	62008.881004	35.647092
1257.767738	62059.383020	35.652109
1259.162247	62113.427742	35.657127
1260.004324	62172.566312	35.662144
1261.522840	62215.956979	35.667162
1262.461591	62280.834909	35.672180
1263.253237	62333.379250	35.677197
1264.628387	62388.813945	35.682215
1266.052351	62454.559594	35.687232
1267.381916	62506.184488	35.692250
1268.303506	62558.145562	35.697268
1269.220120	62627.376835	35.702285
1270.538219	62686.929557	35.707303
1271.858991	62757.060147	35.712320
1273.138412	62825.640119	35.717338
1275.237271	62900.004658	35.722356
1276.266714	62960.780691	35.727373
1277.641980	63030.789577	35.732391
1279.186228	63096.518100	35.737408
1280.375847	63165.923376	35.742426
1281.713527	63225.164130	35.747444
1282.878439	63293.706346	35.752461
1284.401359	63355.735515	35.757479
1285.548257	63415.620654	35.762496
1286.544257	63486.633452	35.767514
1288.004934	63547.647284	35.772532
1289.208534	63621.020945	35.777549
1291.155642	63685.757358	35.782567
1292.521796	63760.441754	35.787584
1293.718202	63809.557932	35.792602
1295.348835	63872.628755	35.797620
1296.408228	63930.914499	35.802637
1297.630582	63991.396960	35.807655
1299.008337	64052.431340	35.812672
1300.160144	64127.612533	35.817690
1301.482512	64186.357839	35.822708
1303.097978	64253.660967	35.827725
1304.570308	64314.408957	35.832743
1305.400801	64384.215705	35.837760
1306.890384	64441.884516	35.842778
1308.318048	64499.132654	35.847796
1309.366582	64564.227259	35.852813
1310.794431	64639.202174	35.857831
1312.588376	64699.337303	35.862848
1313.650343	64760.834354	35.867866
1314.761406	64818.765876	35.872884
1316.006423	64885.761498	35.877901
1317.811004	64945.363752	35.882919
1319.093921	65005.408675	35.887936
1320.299899	65078.286087	35.892954
1321.964535	65138.309560	35.897972
1322.297669	65206.930242	35.902989
1323.960417	65266.891008	35.908007
1325.615563	65331.335510	35.913024
1326.560584	65391.611518	35.918042
1328.489379	65448.561789	35.923060
1329.764238	65516.263502	35.928077
1330.717950	65579.843447	35.933095
1332.564587	65649.368018	35.938112
1333.412836	65711.863183	35.943130
1334.840919	65763.928908	35.948148
1336.279001	65843.761830	35.953165
1337.641898	65895.489814	35.958183
1338.874481	65952.809788	35.963200
1340.187605	66014.656790	35.968218
1341.767472	66077.240933	35.973236
1342.635360	66150.433946	35.978253
1344.234397	66202.676417	35.983271
1344.960473	66262.298662	35.988288
1346.380790	66302.539829	35.993306
1348.174364	66361.919233	35.998324
1349.080387	66417.828840	36.003341
1350.148192	66474.935199	36.008359
1351.604177	66530.372753	36.013376
1352.829755	66582.953050	36.018394
1354.413278	66641.872143	36.023412
1355.520030	66707.602635	36.028429
1356.786800	66768.179785	36.033447
1357.894007	66836.037900	36.038464
1359.134738	66900.975482	36.043482
1360.535015	66952.680781	36.048500
1362.225479	67024.107696	36.053517
1363.940766	67097.538017	36.058535
1365.364137	67165.930022	36.063552
1366.374605	67236.799164	36.068570
1368.222250	67307.562783	36.073588
1369.350344	67373.785517	36.078605
1370.584023	67433.185422	36.083623
1372.110926	67499.377713	36.088640
1373.641891	67577.257738	36.093658
1375.232376	67637.216435	36.098676
1376.246678	67717.298864	36.103693
1377.684883	67778.573391	36.108711
1379.493615	67852.092565	36.113728
1380.623258	67917.499674	36.118746
1382.494368	67979.890952	36.123764
1383.785382	68053.852654	36.128781
1385.303677	68114.235335	36.133799
1386.467559	68177.054386	36.138816
1387.894262	68240.832875	36.143834
1389.697680	68310.111891	36.148852
1390.602378	68378.955574	36.153869
1392.207403	68450.551815	36.158887
1393.556270	68522.087043	36.163904
1394.789910	68578.861887	36.168922
1396.235132	68647.457051	36.173940
1397.463343	68707.379984	36.178957
1398.820736	68782.587111	36.183975
1400.788030	68866.791675	36.188992
1401.948378	68939.016093	36.194010
1403.517654	69007.865075	36.199028
1404.617472	69079.421838	36.204045
1406.320804	69140.506149	36.209063
1408.011624	69202.979279	36.214080
1409.208536	69278.320617	36.219098
1410.368092	69343.194776	36.224116
1411.924020	69411.768314	36.229133
1413.459047	69486.025202	36.234151
1415.261290	69541.345430	36.239168
1416.249569	69618.392094	36.244186
1417.795645	69679.654268	36.249204
1419.070952	69752.800124	36.254221
1420.334359	69826.954867	36.259239
1421.812029	69890.843441	36.264256
1423.304804	69973.169236	36.269274
1424.894265	70029.530638	36.274292
1426.411082	70102.544694	36.279309
1427.626407	70164.955267	36.284327
1429.266354	70219.814765	36.289344
1430.450903	70295.186322	36.294362
1432.108360	70368.001806	36.299380
1433.780841	70426.719364	36.304397
1435.264616	70497.536050	36.309415
1436.681276	70558.877549	36.314432
1437.844722	70626.629202	36.319450
1439.163907	70680.273404	36.324468
1440.706022	70738.201525	36.329485
1441.790200	70792.402001	36.334503
1443.403124	70834.412214	36.339520
1444.810202	70900.834629	36.344538
1445.816278	70951.628139	36.349556
1447.435152	71014.940118	36.354573
1448.402394	71066.829116	36.359591
1449.911644	71122.204910	36.364608
1450.832960	71194.530008	36.369626
1452.660363	71255.302253	36.374644
1453.754849	71329.044434	36.379661
1455.542589	71405.072024	36.384679
1456.963948	71477.534941	36.389696
1458.290503	71549.835586	36.394714
1459.831193	71623.394767	36.399732
1461.788007	71699.662718	36.404749
1463.012564	71781.922214	36.409767
1464.732679	71838.431729	36.414784
1465.960421	71917.803453	36.419802
1468.005116	71986.712560	36.424820
1469.178031	72062.584982	36.429837
1470.763834	72127.437348	36.434855
1472.358654	72198.380577	36.439872
1473.735042	72265.913156	36.444890
1475.571622	72345.342859	36.449908
1476.830193	72407.093401	36.454925
1478.311562	72490.264835	36.459943
1480.316430	72553.862088	36.464960
1481.573444	72614.055478	36.469978
1482.900211	72676.796570	36.474996
1484.737742	72758.798517	36.480013
1485.896510	72828.304464	36.485031
1487.833693	72898.727356	36.490048
1489.189704	72964.618352	36.495066
1490.739619	73040.447242	36.500084
1492.298005	73111.411295	36.505101
1493.676609	73175.652706	36.510119
1495.253295	73242.345808	36.515136
1496.619802	73314.467714	36.520154
1498.432558	73386.443972	36.525172
1499.744430	73446.060696	36.530189
1501.225034	73526.803613	36.535207
1502.872592	73591.776571	36.540224
1504.519865	73659.928953	36.545242
1505.942218	73732.841226	36.550260
1507.662860	73808.417596	36.555277
1509.114951	73862.364144	36.560295
1511.059695	73925.872778	36.565312
1512.271381	73998.768087	36.570330
1513.681242	74063.627406	36.575348
1515.194041	74132.714030	36.580365
1516.713706	74208.753652	36.585383
1518.109388	74265.876466	36.590400
1519.565109	74344.143122	36.595418
1521.047936	74408.257199	36.600436
1522.705915	74478.981317	36.605453
1523.569331	74552.426645	36.610471
1525.374579	74618.390759	36.615488
1526.576379	74702.626208	36.620506
1527.574240	74773.277089	36.625524
1530.181459	74862.321768	36.630541
1531.317730	74941.197506	36.635559
1532.790084	75003.617295	36.640576
1534.272374	75090.533435	36.645594
1535.748155	75162.073221	36.650612
1537.436239	75236.556705	36.655629
1538.696887	75319.923526	36.660647
1540.638057	75394.177830	36.665664
1541.871388	75447.832475	36.670682
1543.195944	75522.272312	36.675700
1544.728562	75579.731174	36.680717
1546.079760	75642.690764	36.685735
1547.460057	75711.194172	36.690752
1548.805346	75783.858081	36.695770
1550.170920	75850.844082	36.700788
1551.860450	75926.127285	36.705805
1553.226557	76006.300234	36.710823
1555.062219	76071.832471	36.715840
1556.585907	76158.960922	36.720858
1557.985540	76242.764868	36.725876
1559.854946	76323.138667	36.730893
1561.057819	76403.933714	36.735911
1562.805640	76482.097534	36.740928
1564.549904	76569.560142	36.745946
1566.136071	76652.449428	36.750964
1568.024414	76726.969021	36.755981
1569.575822	76809.674213	36.760999
1571.146273	76885.751452	36.766016
1572.422388	76970.058350	36.771034
1574.250042	77059.713677	36.776052
1576.184740	77130.819482	36.781069
1577.783306	77215.798741	36.786087
1579.347205	77284.011364	36.791104
1581.025280	77368.497274	36.796122
1582.654171	77452.763120	36.801140
1584.680437	77531.671795	36.806157
1586.107548	77604.416448	36.811175
1587.723815	77682.578973	36.816192
1589.161379	77765.900286	36.821210
1591.119941	77842.970910	36.826228
1592.721149	77916.449237	36.831245
1594.327678	77996.970471	36.836263
1596.127426	78070.494148	36.841280
1597.639292	78135.397954	36.846298
1599.080375	78212.689961	36.851316
1601.089491	78284.889275	36.856333
1602.622949	78369.565601	36.861351
1604.057955	78441.424453	36.866368
1605.933707	78517.737163	36.871386
1607.356778	78588.103386	36.876404
1609.308287	78657.246915	36.881421
1610.761585	78730.953271	36.886439
1612.617072	78803.988784	36.891456
1614.079719	78869.814171	36.896474
1615.886614	78940.602633	36.901492
1617.471616	79015.454657	36.906509
1618.839996	79089.846705	36.911527
1620.862153	79153.165471	36.916544
1622.165005	79238.057923	36.921562
1623.666611	79304.499022	36.926580
1625.408796	79379.973546	36.931597
1626.865018	79451.945734	36.936615
1628.860156	79526.823638	36.941632
1630.345962	79590.936813	36.946650
1631.705087	79677.557456	36.951668
1633.871793	79744.085555	36.956685
1635.446562	79812.556142	36.961703
1636.822700	79882.882336	36.966720
1638.891641	79961.119848	36.971738
1640.253314	80034.147218	36.976756
1642.216675	80087.557365	36.981773
1643.825347	80160.723780	36.986791
1645.186591	80222.184702	36.991808
1647.049711	80287.925450	36.996826
1648.812330	80362.145193	37.001844
1650.154215	80416.730131	37.006861
1651.443372	80470.385896	37.011879
1653.031509	80528.340576	37.016896
1654.815467	80584.110929	37.021914
1655.882640	80647.987998	37.026932
1657.400783	80711.161161	37.031949
1658.951941	80781.132830	37.036967
1660.226817	80849.678246	37.041984
1661.788306	80919.281227	37.047002
1663.089642	81009.475212	37.052020
1664.780109	81072.761590	37.057037
1666.195975	81165.282037	37.062055
1668.342122	81243.092972	37.067072
1669.901660	81319.741624	37.072090
1671.349283	81415.602744	37.077108
1673.153442	81493.771973	37.082125
1675.149438	81589.839273	37.087143
1677.169601	81677.680340	37.092160
1678.559214	81750.505106	37.097178
1680.166319	81843.339947	37.102196
1682.048569	81945.153101	37.107213
1683.605104	82022.855755	37.112231
1685.353061	82105.508019	37.117248
1687.189735	82190.427268	37.122266
1689.185713	82279.059547	37.127284
1690.917662	82361.081556	37.132301
1692.674270	82451.551011	37.137319
1694.303427	82528.090697	37.142336
1696.598422	82613.877096	37.147354
1697.915405	82700.386981	37.152372
1699.809736	82786.996832	37.157389
1701.550644	82873.694311	37.162407
1702.949599	82949.726335	37.167424
1705.041021	83032.644321	37.172442
1706.689939	83131.482680	37.177460
1708.757013	83208.019024	37.182477
1710.144410	83289.603492	37.187495
1712.053001	83368.610505	37.192512
1713.658253	83448.894269	37.197530
1715.447752	83538.627145	37.202548
1717.325429	83619.236207	37.207565
1719.259733	83707.717888	37.212583
1720.727641	83787.441243	37.217600
1722.792238	83870.948734	37.222618
1724.281105	83947.590229	37.227636
1726.365380	84030.600942	37.232653
1727.971666	84110.341556	37.237671
1729.600238	84190.788482	37.242688
1731.552272	84269.043603	37.247706
1733.112511	84356.926941	37.252724
1734.950200	84427.344301	37.257741
1736.902534	84502.520926	37.262759
1738.043309	84589.026106	37.267776
1739.739725	84665.396289	37.272794
1741.568042	84759.422478	37.277812
1743.547797	84835.913500	37.282829
1745.420398	84929.363105	37.287847
1747.037981	85007.938683	37.292864
1748.923544	85096.647700	37.297882
1750.516954	85171.476762	37.302900
1752.337926	85258.840540	37.307917
1754.137408	85343.965082	37.312935
1755.775022	85419.687551	37.317952
1757.743152	85490.834730	37.322970
1759.390281	85575.172814	37.327988
1761.002471	85661.746828	37.333005
1762.615089	85734.128709	37.338023
1764.128952	85814.395382	37.343040
1766.104572	85898.315522	37.348058
1767.378585	85972.132213	37.353076
1769.178180	86043.079034	37.358093
1770.526660	86110.675218	37.363111
1772.285124	86189.371355	37.368128
1773.589136	86258.875630	37.373146
1775.363071	86344.184521	37.378164
1777.063173	86432.787270	37.383181
1779.060362	86520.811572	37.388199
1780.404972	86616.110670	37.393216
1781.844448	86691.968848	37.398234
1783.700503	86795.526760	37.403252
1785.420166	86889.120675	37.408269
1787.141489	86991.927363	37.413287
1789.305514	87091.775849	37.418304
1791.690869	87182.681380	37.423322
1793.488781	87278.557992	37.428340
1795.247413	87370.259164	37.433357
1797.192809	87466.962366	37.438375
1798.795664	87560.754124	37.443392
1801.083488	87659.419304	37.448410
1802.624474	87753.284722	37.453428
1804.763885	87841.049967	37.458445
1806.840533	87937.556764	37.463463
1808.529752	88029.498968	37.468480
1810.463065	88122.176298	37.473498
1812.360034	88216.443706	37.478516
1814.163325	88309.268701	37.483533
1816.257689	88397.270767	37.488551
1818.225324	88491.299885	37.493568
1820.205971	88567.965333	37.498586
1821.965328	88663.865170	37.503604
1823.618062	88753.154014	37.508621
1825.855044	88836.800901	37.513639
1827.143764	88928.542445	37.518656
1829.140153	89013.139943	37.523674
1830.842720	89106.794285	37.528692
1832.839543	89205.687605	37.533709
1834.929083	89285.620236	37.538727
1836.527257	89378.176525	37.543744
1838.668217	89467.454486	37.548762
1840.286190	89568.334643	37.553780
1842.081050	89655.677611	37.558797
1843.565457	89749.938422	37.563815
1845.600585	89853.111524	37.568832
1847.873190	89947.072188	37.573850
1849.504390	90044.935588	37.578868
1851.030295	90136.086101	37.583885
1853.147783	90232.087039	37.588903
1854.718576	90334.852868	37.593920
1857.039667	90425.626355	37.598938
1858.944994	90523.042863	37.603956
1860.587136	90619.905203	37.608973
1862.673223	90715.519717	37.613991
1864.393132	90813.878702	37.619008
1866.297903	90914.274932	37.624026
1867.981570	91006.265230	37.629044
1869.737784	91103.694282	37.634061
1871.749618	91193.618631	37.639079
1873.436723	91298.663559	37.644096
1875.540877	91385.152029	37.649114
1877.427427	91491.585922	37.654132
1879.071368	91583.863031	37.659149
1881.427102	91683.113946	37.664167
1883.078557	91781.131920	37.669184
1885.269099	91877.481561	37.674202
1887.088295	91966.994758	37.679220
1888.900518	92071.781980	37.684237
1890.818249	92163.118127	37.689255
1892.337356	92244.782917	37.694272
1894.215023	92315.821269	37.699290
1896.077446	92388.053579	37.704308
1897.796418	92468.166750	37.709325
1899.411989	92548.080843	37.714343
1900.914316	92637.556879	37.719360
1902.761486	92733.519357	37.724378
1904.961289	92830.757804	37.729396
1906.300613	92925.849750	37.734413
1908.501508	93023.570282	37.739431
1910.156746	93124.393127	37.744448
1911.793321	93222.456097	37.749466
1913.505584	93332.219179	37.754484
1915.062615	93441.474596	37.759501
1917.547844	93552.613163	37.764519
1919.184166	93670.716836	37.769536
1920.968328	93774.411562	37.774554
1922.926406	93896.965424	37.779572
1924.934902	94008.015460	37.784589
1927.276269	94125.009210	37.789607
1929.121835	94244.514647	37.794624
1931.307356	94359.252115	37.799642
1933.250003	94478.363005	37.804660
1935.391432	94605.885105	37.809677
1937.515643	94715.259093	37.814695
1939.473072	94827.359459	37.819712
1941.807214	94937.575996	37.824730
1943.502534	95047.664725	37.829748
1945.272548	95160.251942	37.834765
1947.308261	95275.561302	37.839783
1949.237719	95403.677581	37.844800
1951.509904	95516.808625	37.849818
1952.957541	95640.526702	37.854836
1954.711684	95757.846667	37.859853
1957.504164	95877.172191	37.864871
1959.245385	95997.549989	37.869888
1961.352824	96117.249818	37.874906
1963.142450	96239.687172	37.879924
1965.000602	96360.149475	37.884941
1967.288359	96471.405464	37.889959
1969.194032	96590.961205	37.894976
1971.376850	96715.443151	37.899994
1973.574978	96827.475004	37.905012
1975.288457	96949.686188	37.910029
1977.617410	97066.376017	37.915047
1979.622143	97181.316946	37.920064
1981.260661	97294.338054	37.925082
1983.569976	97416.356400	37.930100
1985.171348	97533.833662	37.935117
1987.521986	97650.534932	37.940135
1989.342584	97766.305430	37.945152
1991.557372	97880.797699	37.950170
1993.739258	97990.807933	37.955188
1995.580390	98113.523385	37.960205
1997.487954	98236.748669	37.965223
1999.633999	98352.115423	37.970240
2001.662510	98465.257154	37.975258
2003.594960	98568.171255	37.980276
2005.486887	98692.186723	37.985293
2007.368691	98818.359372	37.990311
2009.235810	98928.193905	37.995328
2011.383828	99042.890954	38.000346
2013.515602	99168.544135	38.005364
2015.318027	99287.910670	38.010381
2017.331729	99410.705517	38.015399
2019.184197	99530.610251	38.020416
2021.157341	99649.583771	38.025434
2022.813033	99772.537435	38.030452
2024.655459	99882.417126	38.035469
2026.779336	99983.150626	38.040487
2028.339373	100091.642644	38.045504
2030.411926	100213.100185	38.050522
2032.377099	100320.616786	38.055540
2034.042474	100440.795050	38.060557
2035.781772	100558.604116	38.065575
2037.629788	100694.665432	38.070592
2039.530592	100825.318254	38.075610
2041.381306	100957.779713	38.080628
2043.129926	101098.080037	38.085645
2045.220258	101235.221364	38.090663
2047.261169	101384.491315	38.095680
2049.218882	101546.110870	38.100698
2051.381392	101683.623130	38.105716
2053.490522	101825.645126	38.110733
2055.610417	101970.353870	38.115751
2057.586125	102138.452180	38.120768
2059.742887	102287.644722	38.125786
2062.114513	102433.634681	38.130804
2063.906090	102591.557873	38.135821
2065.915119	102738.506096	38.140839
2068.255729	102892.718722	38.145856
2070.188837	103053.893090	38.150874
2072.547704	103206.227856	38.155892
2074.470174	103383.152630	38.160909
2076.731540	103535.035040	38.165927
2078.915096	103697.973761	38.170944
2081.296913	103854.263767	38.175962
2083.326121	104007.401848	38.180980
2085.415544	104174.846048	38.185997
2087.413853	104333.746825	38.191015
2089.376466	104489.826447	38.196032
2091.735318	104659.056736	38.201050
2093.968641	104823.387884	38.206068
2095.541580	104985.718358	38.211085
2097.321547	105141.575990	38.216103
2100.118755	105320.212668	38.221120
2102.034436	105476.722634	38.226138
2104.176990	105639.334837	38.231156
2106.136246	105824.052096	38.236173
2108.066794	105989.374594	38.241191
2110.603094	106159.928705	38.246208
2112.544679	106336.942096	38.251226
2115.424538	106499.240174	38.256244
2117.331167	106666.814078	38.261261
2119.684107	106833.862486	38.266279
2121.877609	106989.093277	38.271296
2124.285514	107156.857437	38.276314
2126.339880	107312.390428	38.281332
2128.421853	107477.087771	38.286349
2130.504071	107634.431165	38.291367
2132.795887	107799.249383	38.296384
2134.912630	107973.999354	38.301402
2137.241615	108128.491292	38.306420
2138.983997	108283.849223	38.311437
2141.026628	108435.090337	38.316455
2143.545807	108597.987346	38.321472
2145.574810	108771.829364	38.326490
2147.771267	108922.160865	38.331508
2150.043238	109095.979168	38.336525
2151.950396	109254.536639	38.341543
2153.760447	109419.057486	38.346560
2155.976932	109584.796321	38.351578
2158.654493	109755.206600	38.356596
2160.495125	109912.674186	38.361613
2162.226260	110076.690529	38.366631
2164.481433	110236.935342	38.371648
2166.334377	110394.504609	38.376666
2168.722581	110530.203906	38.381684
2170.330118	110685.454095	38.386701
2172.336503	110829.076880	38.391719
2174.296373	110994.938585	38.396736
2175.632569	111151.793119	38.401754
2178.038372	111319.032292	38.406772
2179.949942	111494.795723	38.411789
2182.231825	111680.203788	38.416807
2184.277188	111849.340727	38.421824
2186.361994	112038.979239	38.426842
2188.366958	112227.236207	38.431860
2190.573645	112409.032713	38.436877
2192.632478	112598.919208	38.441895
2195.424511	112785.863827	38.446912
2197.207667	112992.891352	38.451930
2199.137987	113178.615801	38.456948
2201.589975	113371.120853	38.461965
2203.543050	113572.760383	38.466983
2205.871341	113775.623281	38.472000
2208.151675	113985.039126	38.477018
2210.327528	114180.572117	38.482036
2212.351063	114396.549481	38.487053
2214.667946	114599.545571	38.492071
2216.860024	114799.493010	38.497088
2219.092214	115024.674695	38.502106
2221.644926	115230.072535	38.507124
2223.844363	115444.405084	38.512141
2226.241848	115668.347242	38.517159
2228.987156	115868.480272	38.522176
2230.742795	116070.684423	38.527194
2233.161368	116288.044287	38.532212
2235.419729	116499.278919	38.537229
2237.786422	116708.620608	38.542247
2240.366773	116913.668291	38.547264
2242.781727	117137.641915	38.552282
2245.266847	117345.776354	38.557300
2247.371133	117548.314463	38.562317
2249.657407	117762.380371	38.567335
2251.868999	117954.769306	38.572352
2253.676919	118180.721347	38.577370
2256.340472	118386.563133	38.582388
2258.685368	118606.307194	38.587405
2261.120683	118809.459843	38.592423
2263.618866	119008.354437	38.597440
2265.624840	119222.117255	38.602458
2268.096386	119424.278110	38.607476
2270.816447	119628.113583	38.612493
2272.635681	119832.661883	38.617511
2275.318549	120034.095223	38.622528
2277.407458	120250.755609	38.627546
2279.630226	120449.941765	38.632564
2282.116647	120660.732547	38.637581
2284.270463	120881.255236	38.642599
2286.344731	121087.634974	38.647616
2288.923965	121300.089143	38.652634
2291.028191	121505.857514	38.657652
2293.175219	121712.064259	38.662669
2295.311697	121926.887147	38.667687
2297.741443	122131.288589	38.672704
2299.824520	122360.964239	38.677722
2302.379860	122568.836833	38.682740
2304.391530	122790.597626	38.687757
2306.419949	123012.179437	38.692775
2308.816940	123224.888157	38.697792
2310.812850	123448.050527	38.702810
2312.963465	123670.428782	38.707828
2315.239035	123883.680134	38.712845
2317.326956	124095.401584	38.717863
2319.596154	124288.218741	38.722880
2321.547475	124505.697878	38.727898
2323.685081	124716.298431	38.732916
2325.843690	124923.408039	38.737933
2327.791028	125145.521772	38.742951
2330.052513	125374.324119	38.747968
2332.061819	125600.959735	38.752986
2334.289623	125835.846824	38.758004
2336.607600	126071.114444	38.763021
2338.579156	126317.196029	38.768039
2341.182021	126557.686901	38.773056
2343.199909	126814.941368	38.778074
2345.150475	127065.965941	38.783092
2348.010567	127322.571643	38.788109
2350.100536	127574.998447	38.793127
2352.522519	127835.634262	38.798144
2354.785548	128079.219387	38.803162
2357.138373	128345.578512	38.808180
2359.894408	128613.957004	38.813197
2362.025729	128885.099334	38.818215
2364.684997	129147.863072	38.823232
2366.845382	129420.641001	38.828250
2369.300413	129689.961561	38.833268
2372.110203	129963.148895	38.838285
2374.292297	130238.072926	38.843303
2376.864250	130504.170270	38.848320
2379.333272	130766.948380	38.853338
2381.769613	131043.271557	38.858356
2384.767283	131310.284283	38.863373
2387.290839	131572.284779	38.868391
2389.879179	131836.218058	38.873408
2392.496329	132096.214981	38.878426
2394.791838	132355.768913	38.883444
2397.588302	132620.029656	38.888461
2400.507058	132873.703113	38.893479
2402.842255	133124.119465	38.898496
2405.359717	133389.265938	38.903514
2407.551580	133641.953585	38.908532
2410.549767	133886.674694	38.913549
2412.599705	134143.562096	38.918567
2415.486249	134386.438112	38.923584
2417.966930	134641.154584	38.928602
2420.050854	134885.580061	38.933620
2422.672229	135138.373941	38.938637
2424.914872	135398.867555	38.943655
2427.185969	135660.018073	38.948672
2429.763031	135905.196742	38.953690
2432.238574	136170.556548	38.958708
2434.700464	136427.823955	38.963725
2436.739632	136705.906837	38.968743
2439.368906	136954.598056	38.973760
2441.641092	137221.264745	38.978778
2443.399221	137485.957595	38.983796
2445.505301	137758.846116	38.988813
2448.214467	138035.690076	38.993831
2450.418030	138313.959942	38.998848
2452.596208	138587.260809	39.003866
2454.569745	138868.108019	39.008884
2457.470208	139155.753618	39.013901
2459.415469	139452.167303	39.018919
2461.924143	139738.964009	39.023936
2464.357704	140033.756676	39.028954
2466.422526	140325.182320	39.033972
2468.761974	140616.706376	39.038989
2470.983600	140921.614237	39.044007
2473.359116	141225.890779	39.049024
2476.204548	141516.896936	39.054042
2478.333638	141808.511849	39.059060
2480.870116	142088.211111	39.064077
2482.973305	142372.040987	39.069095
2485.223428	142651.432899	39.074112
2487.946700	142947.467100	39.079130
2490.111027	143226.837614	39.084148
2492.316770	143534.162944	39.089165
2494.606327	143842.187797	39.094183
2496.624946	144140.598456	39.099200
2499.149482	144461.104488	39.104218
2501.404330	144774.255322	39.109236
2504.140613	145094.046883	39.114253
2505.864809	145420.420993	39.119271
2508.315744	145755.999598	39.124288
2510.902184	146090.581897	39.129306
2513.093639	146450.765240	39.134324
2515.883135	146783.873344	39.139341
2518.398589	147132.143286	39.144359
2521.306534	147465.592620	39.149376
2524.090587	147815.881312	39.154394
2526.369241	148174.171706	39.159412
2529.044163	148528.708911	39.164429
2531.596361	148885.615881	39.169447
2534.411766	149231.047621	39.174464
2537.412467	149576.769933	39.179482
2539.901467	149930.495079	39.184500
2543.035342	150279.171277	39.189517
2544.659040	150627.705135	39.194535
2547.204510	150983.345004	39.199552
2549.754648	151344.431982	39.204570
2552.472481	151717.224016	39.209588
2555.257514	152077.720524	39.214605
2557.788874	152443.260405	39.219623
2560.422817	152798.860009	39.224640
2562.851834	153159.787300	39.229658
2565.156048	153540.171006	39.234676
2567.705200	153917.129610	39.239693
2570.242491	154288.887929	39.244711
2572.996061	154661.338399	39.249728
2575.674866	155043.184116	39.254746
2578.189972	155428.802818	39.259764
2581.033278	155798.580714	39.264781
2583.329996	156180.125494	39.269799
2585.749995	156565.741154	39.274816
2588.229315	156942.273265	39.279834
2590.976304	157334.037816	39.284852
2593.149055	157721.832360	39.289869
2595.756552	158114.436287	39.294887
2598.503018	158506.602079	39.299904
2601.410331	158899.164171	39.304922
2603.819607	159301.937510	39.309940
2606.482441	159688.042886	39.314957
2609.464933	160078.087029	39.319975
2611.987192	160471.519124	39.324992
2614.905568	160851.459776	39.330010
2618.054372	161242.868949	39.335028
2620.848012	161625.309402	39.340045
2623.653123	162009.997506	39.345063
2625.978892	162395.092975	39.350080
2628.592128	162768.909827	39.355098
2630.575458	163167.191069	39.360116
2633.341321	163543.222975	39.365133
2636.203895	163944.088361	39.370151
2638.453280	164334.222149	39.375168
2641.284763	164724.698839	39.380186
2643.711069	165116.955185	39.385204
2646.079792	165517.081940	39.390221
2648.294098	165908.347592	39.395239
2650.342846	166299.171591	39.400256
2653.035440	166669.937860	39.405274
2655.192909	167064.215365	39.410292
2657.680332	167448.032060	39.415309
2660.152232	167840.449087	39.420327
2662.257662	168245.457533	39.425344
2664.892302	168651.947238	39.430362
2666.914095	169072.806676	39.435380
2669.514867	169502.135916	39.440397
2671.991469	169927.030350	39.445415
2674.646470	170358.019458	39.450432
2677.230700	170794.672494	39.455450
2679.447398	171245.987698	39.460468
2681.971124	171684.280643	39.465485
2684.328833	172153.317719	39.470503
2686.682018	172617.609411	39.475520
2689.483028	173082.621105	39.480538
2691.844952	173565.074957	39.485556
2694.881286	174044.569231	39.490573
2697.753601	174530.034732	39.495591
2699.964528	175020.241424	39.500608
2702.771569	175511.703847	39.505626
2705.001027	176016.072113	39.510644
2707.822773	176517.252413	39.515661
2710.976896	177020.656746	39.520679
2713.807891	177535.568667	39.525696
2716.368507	178037.878190	39.530714
2718.991743	178551.000093	39.535732
2721.827336	179069.958608	39.540749
2724.578387	179580.526786	39.545767
2727.028485	180105.824853	39.550784
2729.932045	180632.020170	39.555802
2732.742801	181162.880872	39.560820
2735.426197	181687.821361	39.565837
2738.472970	182211.107864	39.570855
2741.415617	182756.510214	39.575872
2744.460675	183294.686436	39.580890
2746.826378	183894.030523	39.585908
2749.872126	184425.812361	39.590925
2753.836705	184923.621799	39.595943
2756.550028	185450.838426	39.600960
2759.883477	185965.438922	39.605978
2762.663976	186481.500019	39.610996
2765.775443	186997.588081	39.616013
2768.643417	187510.414766	39.621031
2771.138390	188016.469680	39.626048
2773.999701	188518.532650	39.631066
2776.891661	189052.089113	39.636084
2779.507191	189563.313816	39.641101
2782.112981	190072.434107	39.646119
2784.848708	190600.738980	39.651136
2787.113388	191123.353986	39.656154
2789.533665	191650.214237	39.661172
2792.397258	192176.016812	39.666189
2795.135110	192718.580420	39.671207
2797.915178	193250.445989	39.676224
2800.807668	193788.036821	39.681242
2803.180632	194331.909007	39.686260
2805.344070	194884.173204	39.691277
2808.104680	195424.941077	39.696295
2810.764319	195986.632253	39.701312
2813.737956	196536.515674	39.706330
2816.125932	197108.770044	39.711348
2818.663538	197675.592701	39.716365
2821.715526	198238.018770	39.721383
2824.401964	198809.775803	39.726400
2827.121763	199369.489183	39.731418
2829.844499	199939.009299	39.736436
2832.409491	200488.716988	39.741453
2835.214223	201029.599832	39.746471
2837.849194	201582.500869	39.751488
2841.014875	202131.383303	39.756506
2843.715351	202689.510502	39.761524
2845.868744	203241.196519	39.766541
2848.904494	203796.277151	39.771559
2851.452498	204370.106691	39.776576
2854.140680	204938.403582	39.781594
2856.880525	205513.527375	39.786612
2859.646884	206100.715021	39.791629
2862.640460	206675.599091	39.796647
2865.690609	207273.516414	39.801664
2868.446491	207865.460785	39.806682
2870.823364	208463.130839	39.811700
2873.751589	209069.404054	39.816717
2876.838952	209671.284464	39.821735
2879.331278	210286.189641	39.826752
2882.222633	210893.666799	39.831770
2885.356475	211519.905924	39.836788
2887.839993	212140.532271	39.841805
2891.498727	212752.237224	39.846823
2894.761202	213370.330802	39.851840
2897.815963	213980.049352	39.856858
2901.230176	214600.915763	39.861876
2903.964860	215228.545239	39.866893
2907.269939	215833.832737	39.871911
2910.257919	216457.893307	39.876928
2913.370867	217075.736625	39.881946
2916.410328	217689.807016	39.886964
2919.416606	218308.786256	39.891981
2922.172491	218930.117065	39.896999
2924.555003	219555.241249	39.902016
2927.458035	220185.035125	39.907034
2930.529185	220815.971786	39.912052
2933.216018	221466.504692	39.917069
2936.380367	222095.928752	39.922087
2938.865915	222739.075854	39.927104
2942.083834	223388.154849	39.932122
2944.746845	224020.782756	39.937140
2947.502362	224683.525565	39.942157
2950.329164	225347.730724	39.947175
2953.083249	226009.178199	39.952192
2956.206410	226664.445490	39.957210
2959.018993	227329.617984	39.962228
2961.694321	228004.897130	39.967245
2965.265448	228670.763402	39.972263
2967.974444	229354.343718	39.977280
2970.833357	230024.359779	39.982298
2973.744343	230700.464131	39.987316
2976.837517	231384.338401	39.992333
2979.881379	232059.404511	39.997351
2983.142407	232726.078013	40.002368
2986.461986	233409.330280	40.007386
2989.585268	234087.201292	40.012404
2992.179722	234769.040791	40.017421
2995.655828	235444.009336	40.022439
2998.856545	236107.842171	40.027456
3002.079930	236780.231328	40.032474
3005.079145	237450.037691	40.037492
3007.823291	238133.067056	40.042509
3010.951132	238803.434803	40.047527
3014.009322	239473.557915	40.052544
3017.116469	240151.699282	40.057562
3019.811830	240811.231914	40.062580
3022.974166	241494.568938	40.067597
3026.105578	242164.394438	40.072615
3029.247888	242827.281322	40.077632
3032.176806	243466.828873	40.082650
3035.122431	244115.567867	40.087668
3037.712301	244734.181896	40.092685
3040.993219	245370.976073	40.097703
3043.640435	246016.478880	40.102720
3046.762921	246661.498805	40.107738
3049.771668	247315.476041	40.112756
3052.296499	247976.969565	40.117773
3055.506611	248629.234037	40.122791
3057.999975	249303.504929	40.127808
3060.743683	249979.512149	40.132826
3063.610480	250659.307666	40.137844
3066.614135	251336.183081	40.142861
3069.481423	252031.671056	40.147879
3072.134869	252735.851291	40.152896
3074.882721	253454.339938	40.157914
3077.663410	254160.169943	40.162932
3080.283913	254893.175523	40.167949
3083.453861	255611.155368	40.172967
3086.502592	256361.689121	40.177984
3089.363298	257098.760088	40.183002
3092.893433	257836.890575	40.188020
3095.754858	258604.840020	40.193037
3099.084762	259358.385527	40.198055
3102.272362	260122.438871	40.203072
3104.999218	260883.866860	40.208090
3108.347316	261654.311236	40.213108
3111.205985	262433.488180	40.218125
3114.829709	263198.798776	40.223143
3118.054504	263982.758688	40.228160
3121.136477	264754.797462	40.233178
3124.601894	265531.621729	40.238196
3127.683653	266312.995629	40.243213
3131.037941	267097.952780	40.248231
3133.921432	267886.380623	40.253248
3136.851771	268674.083500	40.258266
3140.470818	269449.785816	40.263284
3143.501757	270250.031655	40.268301
3146.907595	271036.649513	40.273319
3150.361525	271832.243570	40.278336
3153.034714	272624.396890	40.283354
3156.893435	273418.795652	40.288372
3159.686871	274212.845608	40.293389
3163.139715	275005.032543	40.298407
3166.721762	275795.032952	40.303424
3170.312375	276585.405232	40.308442
3173.795355	277365.475854	40.313460
3176.911141	278153.443296	40.318477
3180.230933	278929.384292	40.323495
3183.454526	279707.719529	40.328512
3186.741769	280496.042202	40.333530
3190.307663	281275.881976	40.338548
3193.556051	282061.425920	40.343565
3197.013356	282830.371866	40.348583
3199.886726	283614.306757	40.353600
3202.827621	284384.840079	40.358618
3205.992974	285165.867767	40.363636
3209.149432	285954.378716	40.368653
3212.203343	286742.312426	40.373671
3215.443375	287526.271915	40.378688
3218.171180	288324.953140	40.383706
3221.033174	289114.107138	40.388724
3224.270442	289918.681275	40.393741
3227.756265	290716.883990	40.398759
3230.628748	291514.029812	40.403776
3233.745306	292332.861078	40.408794
3236.571127	293128.875998	40.413812
3239.869057	293938.618403	40.418829
3242.903221	294713.277916	40.423847
3246.636942	295494.926678	40.428864
3249.475245	296270.738649	40.433882
3252.460853	297046.440945	40.438900
3255.079696	297846.232155	40.443917
3258.011420	298630.019812	40.448935
3260.930245	299437.966839	40.453952
3263.989243	300252.277500	40.458970
3267.091699	301060.552640	40.463988
3270.015428	301886.791363	40.469005
3273.226709	302711.271476	40.474023
3277.059146	303552.116438	40.479040
3280.022257	304391.129132	40.484058
3283.075982	305237.500799	40.489076
3285.995136	306088.194697	40.494093
3289.601703	306939.198287	40.499111
3293.192501	307803.642769	40.504128
3296.166403	308671.138321	40.509146
3299.511084	309530.336738	40.514164
3302.605707	310411.133301	40.519181
3305.668808	311298.619191	40.524199
3309.160902	312188.254874	40.529216
3312.047018	313091.140695	40.534234
3315.323142	313981.207415	40.539252
3318.312640	314898.203553	40.544269
3321.681784	315812.710877	40.549287
3324.981253	316738.985933	40.554304
3328.012473	317673.658255	40.559322
3331.726706	318596.023026	40.564340
3334.983515	319529.808476	40.569357
3338.486623	320468.965687	40.574375
3341.289024	321411.688264	40.579392
3344.956200	322353.138176	40.584410
3348.202165	323306.507940	40.589428
3351.773782	324269.928981	40.594445
3355.316291	325217.854484	40.599463
3359.738044	326158.338586	40.604480
3363.192146	327109.608228	40.609498
3367.006748	328036.924562	40.614516
3370.645128	328984.898435	40.619533
3374.257328	329921.944409	40.624551
3377.717514	330852.928299	40.629568
3380.873622	331794.313087	40.634586
3384.227749	332737.800025	40.639604
3388.017136	333669.526358	40.644621
3391.128619	334614.500977	40.649639
3394.901348	335557.242832	40.654656
3397.681406	336496.108044	40.659674
3401.517464	337443.712531	40.664692
3404.681858	338383.306078	40.669709
3408.135979	339326.761154	40.674727
3411.671839	340273.754678	40.679744
3414.768056	341236.211838	40.684762
3418.277447	342172.962844	40.689780
3421.795577	343132.359884	40.694797
3424.999531	344089.192646	40.699815
3428.736438	345038.104643	40.704832
3432.169025	345988.204210	40.709850
3435.719908	346934.809805	40.714868
3439.036894	347893.850241	40.719885
3442.421052	348862.107589	40.724903
3446.058385	349803.140800	40.729920
3449.633479	350762.741896	40.734938
3453.301410	351701.991248	40.739956
3456.802133	352654.144286	40.744973
3460.019797	353606.592057	40.749991
3463.308186	354542.901580	40.755008
3466.624472	355479.135622	40.760013
3470.237916	356390.590526	40.765018
3473.493178	357240.164467	40.770023
3476.649444	358052.498911	40.775028
3479.738759	358793.131095	40.780032
3482.671705	359504.900750	40.785037
3485.401998	360140.016573	40.790042
3488.400144	360743.363249	40.795047
3490.695937	361288.742787	40.800052
3493.446473	361770.285380	40.805056
3495.771525	362214.558657	40.810061
3497.691180	362596.176354	40.815066
3499.700851	362941.642195	40.820071
3501.980466	363243.306416	40.825076
3503.863800	363491.949251	40.830080
3504.840091	363714.357010	40.835085
3506.955762	363882.844783	40.840090
3508.137432	364023.197437	40.845095
3508.976751	364145.588063	40.850100
3510.383290	364218.952196	40.855104
3511.832844	364269.949727	40.860109
3512.524769	364284.375415	40.865114
3513.907968	364276.307928	40.870119
3514.066130	364245.818157	40.875124
3515.464761	364198.186750	40.880128
3515.919524	364128.114346	40.885133
3516.568759	364032.653243	40.890138
3517.137635	363916.572244	40.895143
3517.455120	363794.990891	40.900148
3518.060308	363655.984112	40.905152
3518.920164	363503.723970	40.910157
3519.180400	363334.481563	40.915162
3519.512657	363156.333526	40.920167
3519.864281	362970.837933	40.925172
3520.108126	362763.759489	40.930176
3520.078773	362558.170690	40.935181
3520.419013	362338.775652	40.940186
3520.867419	362115.779186	40.945191
3520.899736	361900.189818	40.950196
3520.974680	361651.659583	40.955200
3521.075313	361401.446120	40.960205
3521.312731	361164.499352	40.965210
3521.176431	360907.762654	40.970215
3521.036416	360665.432856	40.975220
3521.200751	360397.666879	40.980224
3521.496736	360138.619766	40.985229
3521.271702	359874.518556	40.990234
3521.490670	359599.494388	40.995239
3521.571311	359332.596084	41.000244
3521.731809	359065.530470	41.005248
3521.799045	358802.771956	41.010253
3521.660229	358523.168739	41.015258
3521.448008	358246.522446	41.020263
3521.397624	357965.299226	41.025268
3521.481349	357678.283406	41.030272
3521.027160	357403.446337	41.035277
3520.915804	357115.134203	41.040282
3521.015646	356838.604349	41.045287
3520.868866	356561.856427	41.050292
3521.116955	356278.283781	41.055296
3520.741809	356014.503159	41.060301
3520.764756	355725.242133	41.065306
3520.570815	355438.198123	41.070311
3520.085947	355181.137474	41.075316
3520.022440	354894.779746	41.080320
3520.450677	354617.950095	41.085325
3520.160881	354338.663141	41.090330
3519.905184	354074.872925	41.095335
3519.951360	353796.697845	41.100340
3519.989663	353521.190413	41.105344
3519.522169	353255.545570	41.110349
3519.694289	352989.646004	41.115354
3519.363305	352716.019435	41.120359
3518.992120	352455.665303	41.125364
3519.110405	352184.099104	41.130368
3518.989144	351922.583141	41.135373
3518.913413	351669.395428	41.140378
3518.856806	351405.857040	41.145383
3518.200636	351139.207362	41.150388
3518.441836	350885.099681	41.155392
3518.631105	350630.235526	41.160397
3517.733131	350372.056778	41.165402
3517.774859	350116.728679	41.170407
3517.855703	349872.094541	41.175412
3517.830806	349609.655121	41.180416
3517.451800	349368.444654	41.185421
3517.178457	349123.402716	41.190426
3517.192201	348883.067865	41.195431
3516.880187	348655.213327	41.200436
3516.863865	348402.651907	41.205440
3516.978500	348178.489797	41.210445
3516.615936	347930.554848	41.215450
3516.789013	347700.228219	41.220455
3516.169559	347473.506771	41.225460
3516.243303	347236.099594	41.230464
3516.016036	346999.169976	41.235469
3515.729408	346774.603532	41.240474
3515.930420	346545.942487	41.245479
3515.521792	346335.222368	41.250484
3515.737839	346107.878006	41.255488
3515.175831	345885.713056	41.260493
3515.117214	345661.078105	41.265498
3514.854812	345454.321160	41.270503
3515.027743	345245.206722	41.275508
3515.110254	345032.113518	41.280512
3514.686852	344818.691280	41.285517
3514.631343	344612.252807	41.290522
3514.719544	344404.341406	41.295527
3514.406489	344200.381484	41.300532
3514.644452	343987.613403	41.305536
3514.070005	343785.980135	41.310541
3513.677989	343579.537193	41.315546
3514.025758	343388.639478	41.320551
3513.954331	343185.271391	41.325556
3513.726629	342983.223255	41.330560
3513.355883	342790.909018	41.335565
3513.320344	342587.252119	41.340570
3513.376366	342402.725676	41.345575
3512.987669	342224.522668	41.350580
3513.294494	342031.818608	41.355584
3513.097046	341836.395389	41.360589
3512.772266	341658.510042	41.365594
3512.393076	341465.655842	41.370599
3512.687121	341291.536777	41.375604
3512.552118	341108.965821	41.380608
3512.281001	340934.475653	41.385613
3512.285712	340761.034878	41.390618
3512.240662	340580.761016	41.395623
3512.142902	340421.345177	41.400628
3511.936543	340236.772073	41.405632
3511.916478	340061.450081	41.410637
3511.709943	339895.539328	41.415642
3511.547284	339723.823317	41.420647
3511.456042	339567.937140	41.425652
3511.482197	339401.301141	41.430656
3511.194954	339238.146211	41.435661
3511.234652	339072.320272	41.440666
3511.235056	338916.213493	41.445671
3510.860248	338768.657934	41.450676
3510.892426	338597.821490	41.455680
3510.372405	338443.421471	41.460685
3510.531985	338296.746734	41.465690
3510.625017	338145.428243	41.470695
3510.190111	337992.538742	41.475700
3510.458013	337848.032176	41.480704
3510.111781	337711.326215	41.485709
3509.700203	337565.831278	41.490714
3509.831713	337429.965036	41.495719
3509.577534	337286.122736	41.500724
3509.648592	337143.881971	41.505728
3509.849438	337014.055676	41.510733
3509.759782	336858.488121	41.515738
3509.916663	336718.953312	41.520743
3509.495614	336582.814274	41.525748
3509.812081	336450.145126	41.530752
3509.414674	336319.901285	41.535757
3509.267097	336183.412841	41.540762
3509.340328	336051.644922	41.545767
3509.087057	335921.682304	41.550772
3508.921981	335785.322272	41.555776
3508.953705	335664.215020	41.560781
3508.918243	335538.870877	41.565786
3508.961923	335406.927256	41.570791
3508.460957	335280.688628	41.575796
3508.420715	335158.802600	41.580800
3508.336899	335047.349880	41.585805
3508.202096	334929.775798	41.590810
3508.705842	334804.370304	41.595815
3508.087775	334678.707430	41.600820
3508.232016	334573.168653	41.605824
3508.186537	334449.551758	41.610829
3508.110323	334334.230071	41.615834
3508.328550	334218.455084	41.620839
3507.944692	334107.326212	41.625844
3508.126267	333982.909313	41.630848
3508.194475	333872.522899	41.635853
3507.963915	333764.268319	41.640858
3507.632937	333654.604912	41.645863
3507.582318	333552.603393	41.650868
3507.543085	333447.878536	41.655872
3507.601985	333340.416756	41.660877
3507.204869	333231.398270	41.665882
3507.094672	333129.125160	41.670887
3506.802265	333032.984135	41.675892
3507.133172	332922.859061	41.680896
3507.068848	332833.447020	41.685901
3506.735396	332732.225058	41.690906
3507.223473	332632.044310	41.695911
3507.163342	332545.581173	41.700916
3507.119181	332445.483143	41.705920
3506.707740	332350.300025	41.710925
3506.619339	332263.713500	41.715930
3507.074478	332153.566774	41.720935
3506.843346	332067.383618	41.725940
3506.645107	331964.230961	41.730944
3506.439413	331865.530072	41.735949
3506.193943	331784.486105	41.740954
3506.610574	331694.690994	41.745959
3506.137561	331612.817492	41.750964
3505.846431	331514.129052	41.755968
3505.976677	331431.346967	41.760973
3505.894769	331355.312431	41.765978
3506.208432	331277.054013	41.770983
3505.767089	331195.479875	41.775988
3505.669821	331106.577620	41.780992
3505.854746	331023.404597	41.785997
3505.645316	330954.841413	41.791002
3505.861258	330866.296584	41.796007
3505.520440	330803.349209	41.801012
3505.660122	330717.384826	41.806016
3505.478086	330641.110190	41.811021
3505.567714	330567.209207	41.816026
3505.614744	330481.742039	41.821031
3505.103379	330426.018679	41.826036
3505.284465	330347.906277	41.831040
3505.282938	330276.740493	41.836045
3505.248223	330210.056273	41.841050
3505.641901	330141.753445	41.846055
3505.348538	330064.096168	41.851060
3505.404254	329983.052197	41.856064
3505.285407	329915.515840	41.861069
3505.070862	329849.342378	41.866074
3505.257786	329778.731224	41.871079
3504.954392	329718.523214	41.876084
3505.175357	329645.210385	41.881088
3505.001232	329578.394267	41.886093
3504.771475	329504.286844	41.891098
3505.064605	329440.068132	41.896103
3504.940190	329377.567883	41.901108
3504.642538	329310.236479	41.906112
3504.712138	329245.009546	41.911117
3504.529880	329183.128477	41.916122
3504.626926	329120.542324	41.921127
3504.584857	329064.209503	41.926132
3504.710022	328999.431313	41.931136
3504.286712	328940.207401	41.936141
3504.213226	328882.200486	41.941146
3504.368948	328815.585856	41.946151
3504.138466	328774.314512	41.951156
3504.481224	328713.698712	41.956160
3504.192806	328649.696804	41.961165
3503.827822	328604.580082	41.966170
3504.228351	328534.772674	41.971175
3504.024723	328485.993273	41.976180
3504.162626	328432.353044	41.981184
3503.891115	328377.250595	41.986189
3504.022566	328326.053075	41.991194
3504.022705	328276.834585	41.996199
3503.907052	328237.783091	42.001204
3504.207965	328180.657743	42.006208
3503.976986	328123.818956	42.011213
3503.994519	328073.808977	42.016218
3503.817944	328015.384493	42.021223
3503.915051	327974.468076	42.026228
3503.981020	327914.759154	42.031232
3503.654410	327873.094918	42.036237
3503.839924	327831.452319	42.041242
3503.900179	327772.710653	42.046247
3503.604761	327734.042875	42.051252
3503.620076	327690.213779	42.056256
3503.683662	327643.986071	42.061261
3503.490430	327600.571025	42.066266
3503.820777	327546.467093	42.071271
3503.703539	327501.869984	42.076276
3503.350856	327460.921613	42.081280
3503.468691	327402.958930	42.086285
3503.383050	327366.649030	42.091290
3503.562822	327319.054645	42.096295
3503.268212	327286.618263	42.101300
3503.593426	327231.446370	42.106304
3503.579141	327194.514679	42.111309
3503.452091	327152.106264	42.116314
3503.678962	327103.588540	42.121319
3503.477422	327056.740247	42.126324
3503.585536	327030.421819	42.131328
3503.760238	326974.662622	42.136333
3503.471154	326942.504901	42.141338
3503.367095	326897.701563	42.146343
3503.289496	326855.768402	42.151348
3503.250919	326809.886381	42.156352
3503.404028	326759.828122	42.161357
3503.056479	326729.536265	42.166362
3503.176426	326680.424259	42.171367
3503.224972	326643.355052	42.176372
3503.114815	326612.491816	42.181376
3503.383512	326575.337255	42.186381
3502.807219	326530.938018	42.191386
3503.286128	326486.551822	42.196391
3503.238134	326464.734357	42.201396
3503.244053	326408.313959	42.206400
3503.500221	326373.552262	42.211405
3503.108625	326340.697845	42.216410
3503.229704	326302.396000	42.221415
3502.936593	326266.092102	42.226420
3503.039390	326227.742171	42.231424
3502.856556	326190.556098	42.236429
3502.809353	326164.541196	42.241434
3502.672075	326119.055377	42.246439
3502.724278	326095.594059	42.251444
3502.604220	326063.612708	42.256448
3503.207285	326023.709006	42.261453
3503.112047	326004.849413	42.266458
3503.168640	325953.431624	42.271463
3502.943921	325912.843229	42.276468
3502.858285	325880.881789	42.281472
3503.055405	325846.535870	42.286477
3502.552770	325816.089510	42.291482
3502.798361	325778.072953	42.296487
3502.542827	325758.144492	42.301492
3502.596417	325718.835145	42.306496
3502.765085	325693.447568	42.311501
3502.407437	325666.794066	42.316506
3502.664512	325634.575352	42.321511
3502.563845	325607.398320	42.326516
3502.804710	325567.499920	42.331520
3502.469614	325541.071748	42.336525
3502.384821	325514.400926	42.341530
3502.198539	325480.623391	42.346535
3502.010305	325471.673362	42.351540
3502.107849	325443.829289	42.356544
3502.499318	325414.794547	42.361549
3502.262720	325397.966355	42.366554
3502.401875	325362.738767	42.371559
3502.445409	325341.796710	42.376564
3502.499975	325312.738252	42.381568
3502.439085	325284.460959	42.386573
3502.406376	325263.454468	42.391578
3502.199486	325234.284203	42.396583
3502.131789	325203.057124	42.401588
3502.378060	325188.086635	42.406592
3502.360962	325155.910407	42.411597
3502.134539	325124.835273	42.416602
3502.296480	325110.284946	42.421607
3502.308904	325080.953094	42.426612
3502.291325	325060.198512	42.431616
3502.465211	325038.320153	42.436621
3501.983785	325021.250264	42.441626
3502.205522	324994.327675	42.446631
3502.309234	324973.325144	42.451636
3502.436644	324957.228442	42.456640
3502.296154	324935.602681	42.461645
3501.820880	324911.460003	42.466650
3502.314598	324874.930097	42.471655
3502.166075	324854.552016	42.476660
3501.826990	324836.976472	42.481664
3502.073514	324818.012023	42.486669
3501.699228	324801.103358	42.491674
3502.503849	324777.371020	42.496679
3502.146064	324757.966818	42.501684
3501.982228	324739.448060	42.506688
3501.898546	324701.838113	42.511693
3502.100310	324694.811121	42.516698
3501.985357	324663.082254	42.521703
3501.932066	324640.526928	42.526708
3501.757709	324623.001854	42.531712
3501.927107	324603.998487	42.536717
3501.757694	324588.787507	42.541722
3501.951267	324575.478521	42.546727
3501.760480	324546.356124	42.551732
3502.133029	324537.725230	42.556736
3501.899011	324514.867392	42.561741
3502.110792	324512.214194	42.566746
3502.178305	324476.437400	42.571751
3501.887834	324471.471516	42.576756
3502.187818	324436.243426	42.581760
3502.130415	324417.555252	42.586765
3501.692123	324398.773988	42.591770
3502.193899	324370.535289	42.596775
3502.014198	324369.800289	42.601780
3501.768218	324336.870610	42.606784
3502.103985	324325.091057	42.611789
3502.088626	324301.639270	42.616794
3502.065968	324290.170127	42.621799
3502.008680	324258.177547	42.626804
3502.005621	324245.865857	42.631808
3502.125564	324218.551658	42.636813
3501.706034	324197.986673	42.641818
3502.125983	324177.366751	42.646823
3501.866080	324170.539038	42.651828
3502.073724	324149.138260	42.656832
3502.089977	324125.223537	42.661837
3502.023982	324112.387437	42.666842
3501.842101	324098.577346	42.671847
3501.835185	324080.033758	42.676852
3501.748952	324045.781504	42.681856
3501.647219	324040.786060	42.686861
3501.572873	324029.833698	42.691866
3501.870005	324015.999569	42.696871
3501.699265	324008.674556	42.701876
3501.787569	323981.873919	42.706880
3502.003931	323963.956777	42.711885
3501.759318	323949.215213	42.716890
3502.075984	323918.105136	42.721895
3502.055423	323918.133848	42.726900
3501.956842	323896.373794	42.731904
3502.206383	323881.834777	42.736909
3501.700924	323845.714555	42.741914
3501.979963	323824.480519	42.746919
3501.806001	323819.241953	42.751924
3501.832694	323796.241202	42.756928
3502.178454	323782.780974	42.761933
3501.918364	323760.639078	42.766938
3501.904561	323751.508770	42.771943
3502.309260	323729.135732	42.776948
3501.946230	323708.892374	42.781952
3502.217503	323671.811086	42.786957
3501.856155	323658.664877	42.791962
3502.036769	323642.508465	42.796967
3501.759637	323632.656132	42.801972
3501.963528	323618.760131	42.806977
3502.201683	323597.354298	42.811981
3501.685809	323582.934839	42.816986
3501.893380	323549.475725	42.821991
3502.078031	323536.574821	42.826996
3501.881030	323514.651882	42.832001
3502.249255	323498.974862	42.837005
3502.087758	323478.394617	42.842010
3502.137290	323460.274388	42.847015
3502.042014	323434.519657	42.852020
3502.009875	323434.168594	42.857025
3502.075103	323394.244666	42.862029
3502.174668	323378.049944	42.867034
3501.852694	323355.892069	42.872039
3501.867320	323335.233339	42.877044
3501.793221	323322.042115	42.882049
3501.955096	323297.162902	42.887053
3501.874135	323286.364011	42.892058
3502.096403	323260.991992	42.897063
3502.020638	323251.133526	42.902068
3501.825871	323220.382714	42.907073
3502.134834	323199.448949	42.912077
3501.655558	323193.774693	42.917082
3501.958836	323161.546821	42.922087
3501.959208	323154.576492	42.927092
3502.128780	323134.351344	42.932097
3502.335582	323120.734553	42.937101
3501.566027	323090.658607	42.942106
3502.017398	323076.927248	42.947111
3501.862247	323053.242216	42.952116
3502.030125	323039.020942	42.957121
3501.905913	323016.221426	42.962125
3501.882068	322999.282674	42.967130
3501.578207	322986.229020	42.972135
3502.154229	322962.912973	42.977140
3501.973246	322958.642089	42.982145
3502.126788	322924.275104	42.987149
3501.807584	322918.372271	42.992154
3501.695521	322900.913045	42.997159
3501.726371	322881.803352	43.002164
3501.530995	322872.319647	43.007169
3502.009189	322852.885611	43.012173
3501.501520	322841.237500	43.017178
3501.974346	322819.463867	43.022183
3501.403704	322801.262234	43.027188
3501.440575	322791.029899	43.032193
3501.765970	322782.558650	43.037197
3501.602210	322783.067659	43.042202
3501.472077	322744.216665	43.047207
3501.724564	322758.652271	43.052212
3501.676791	322737.265258	43.057217
3501.568057	322721.866029	43.062221
3501.565568	322711.029282	43.067226
3501.162084	322691.504056	43.072231
3501.569323	322670.147631	43.077236
3501.297368	322656.045869	43.082241
3501.640543	322640.779475	43.087245
3501.542442	322652.929496	43.092250
3501.580883	322634.327293	43.097255
3501.503182	322617.880156	43.102260
3501.251093	322611.992225	43.107265
3501.694708	322608.539478	43.112269
3501.474643	322583.058124	43.117274
3501.627978	322570.899565	43.122279
3501.739653	322563.606463	43.127284
3501.551386	322542.521150	43.132289
3501.792052	322540.499299	43.137293
3501.740660	322534.198388	43.142298
3502.054210	322512.805651	43.147303
3501.895916	322488.433923	43.152308
3501.944997	322472.959051	43.157313
3501.656992	322449.116371	43.162317
3501.537178	322439.315479	43.167322
3501.583311	322417.532028	43.172327
3501.443605	322409.158857	43.177332
3501.369156	322404.515105	43.182337
3501.369274	322398.053483	43.187341
3501.419484	322379.449327	43.192346
3501.598423	322364.895380	43.197351
3501.853850	322354.272614	43.202356
3501.648029	322342.144699	43.207361
3501.199975	322327.205408	43.212365
3501.083717	322315.521396	43.217370
3501.517709	322303.420641	43.222375
3501.564763	322300.716737	43.227380
3501.478234	322285.364756	43.232385
3501.696180	322282.583255	43.237389
3501.594829	322276.824349	43.242394
3501.417689	322271.840481	43.247399
3501.654278	322250.078047	43.252404
3501.408441	322233.428088	43.257409
3501.556619	322227.223129	43.262413
3501.359890	322209.115418	43.267418
3501.162869	322191.592860	43.272423
3501.252605	322202.899573	43.277428
3501.211009	322200.540239	43.282433
3501.621969	322186.560510	43.287437
3501.344534	322164.242400	43.292442
3501.604133	322158.350728	43.297447
3501.868004	322146.530921	43.302452
3501.800259	322135.449830	43.307457
3501.921212	322110.474550	43.312461
3501.231767	322108.470893	43.317466
3501.309863	322087.267389	43.322471
3501.447942	322065.520260	43.327476
3501.623494	322066.459586	43.332481
3501.511196	322064.289377	43.337485
3501.390161	322047.339994	43.342490
3501.382302	322023.707673	43.347495
3501.548999	322022.307918	43.352500
3501.365800	322028.569379	43.357505
3501.273445	322011.793578	43.362509
3501.008088	322002.803973	43.367514
3501.400977	321980.508167	43.372519
3501.495498	321979.628493	43.377524
3501.196846	321973.595113	43.382529
3501.380100	321960.872022	43.387533
3501.388556	321949.066652	43.392538
3501.488227	321943.988589	43.397543
3501.487967	321939.155109	43.402548
3501.544547	321923.500783	43.407553
3501.799444	321892.144457	43.412557
3501.896607	321907.774875	43.417562
3501.589457	321879.508319	43.422567
3501.595067	321861.190746	43.427572
3501.317952	321858.283095	43.432577
3501.477154	321838.745822	43.437581
3501.332068	321824.573065	43.442586
3501.553395	321808.053422	43.447591
3501.878475	321814.159131	43.452596
3501.848254	321799.510488	43.457601
3501.691276	321780.353340	43.462605
3501.052166	321778.799716	43.467610
3501.558924	321766.738311	43.472615
3501.202407	321745.678902	43.477620
3501.286764	321735.489766	43.482625
3501.298539	321726.634857	43.487629
3501.509108	321729.018797	43.492634
3501.126331	321713.407642	43.497639
3501.413499	321695.961820	43.502644
3501.199506	321688.846681	43.507649
3501.629087	321673.362909	43.512653
3501.414653	321671.488488	43.517658
3501.374123	321649.565548	43.522663
3501.365307	321643.537688	43.527668
3501.308496	321651.560250	43.532673
3500.980591	321639.527539	43.537677
3501.095310	321643.580074	43.542682
3501.287555	321632.051163	43.547687
3501.420763	321606.971909	43.552692
3501.382416	321605.960359	43.557697
3501.118612	321597.352026	43.562701
3501.264712	321607.505283	43.567706
3501.355349	321593.473677	43.572711
3501.347495	321577.676656	43.577716
3501.129790	321571.884964	43.582721
3501.413139	321568.177347	43.587725
3501.307410	321570.305465	43.592730
3501.458607	321562.420888	43.597735
3501.394514	321547.523053	43.602740
3501.239258	321542.357597	43.607745
3501.399814	321527.958876	43.612749
3501.406872	321525.922619	43.617754
3501.441979	321507.015158	43.622759
3501.220171	321494.609656	43.627764
3500.700463	321498.328908	43.632769
3501.000920	321479.583471	43.637773
3500.865159	321483.369899	43.642778
3500.775712	321479.084553	43.647783
3501.113583	321481.397725	43.652788
3501.076984	321488.221470	43.657793
3500.846518	321484.416094	43.662797
3501.107147	321479.948817	43.667802
3500.935232	321473.234106	43.672807
3501.046587	321472.682512	43.677812
3500.817916	321468.775093	43.682817
3501.073845	321445.813533	43.687821
3501.350902	321449.459104	43.692826
3501.497205	321435.673145	43.697831
3501.332360	321433.994482	43.702836
3501.335531	321437.988155	43.707841
3501.226893	321420.654980	43.712845
3501.565398	321411.240120	43.717850
3501.157122	321398.685661	43.722855
3500.919337	321388.597685	43.727860
3501.205455	321391.554959	43.732865
3501.206953	321397.151632	43.737869
3501.355309	321390.590359	43.742874
3501.289046	321367.831770	43.747879
3501.411190	321352.675787	43.752884
3500.956728	321361.014976	43.757889
3501.505664	321349.150380	43.762893
3501.310072	321346.204508	43.767898
3501.271859	321330.106858	43.772903
3501.414064	321321.027950	43.777908
3501.190512	321318.213648	43.782913
3501.384606	321310.831124	43.787917
3501.099714	321315.633053	43.792922
3501.217041	321297.908337	43.797927
3501.298281	321280.876143	43.802932
3501.027892	321276.720825	43.807937
3501.264232	321266.787660	43.812941
3501.401033	321278.977673	43.817946
3501.359239	321268.299341	43.822951
3501.697784	321239.626126	43.827956
3501.814631	321240.294806	43.832961
3501.404687	321227.587914	43.837965
3501.409517	321202.986418	43.842970
3501.638831	321189.670767	43.847975
3501.693825	321194.623095	43.852980
3501.099218	321184.260132	43.857985
3501.394015	321154.169039	43.862989
3501.520040	321151.300074	43.867994
3501.588445	321143.377483	43.872999
3501.398245	321135.749724	43.878004
3501.292693	321120.959981	43.883009
3501.563619	321103.745419	43.888013
3501.390237	321115.653248	43.893018
3501.508154	321108.079075	43.898023
3501.429503	321077.842790	43.903028
3501.208118	321075.053573	43.908033
3501.660753	321077.094422	43.913037
3501.079534	321064.363377	43.918042
3501.195050	321062.462785	43.923047
3501.335033	321032.548452	43.928052
3501.318955	321034.942426	43.933057
3501.275596	321027.393452	43.938061
3501.351241	321025.041164	43.943066
3501.066235	321020.481059	43.948071
3501.353175	320993.901863	43.953076
3501.415533	320993.714089	43.958081
3501.544392	320987.791814	43.963085
3501.428971	320986.639656	43.968090
3501.556602	320964.868156	43.973095
3501.692813	320953.831190	43.978100
3501.268899	320942.042254	43.983105
3501.253072	320943.062407	43.988109
3501.422953	320926.575904	43.993114
3501.306018	320915.374981	43.998119
3501.333809	320904.125988	44.003124
3501.094193	320914.263391	44.008129
3501.410509	320905.640545	44.013133
3501.306253	320894.361312	44.018138
3501.438125	320875.438441	44.023143
3501.428561	320864.805851	44.028148
3501.276753	320869.307178	44.033153
3501.416561	320857.175681	44.038157
3501.207119	320836.601638	44.043162
3501.061879	320828.839592	44.048167
3501.294348	320829.261236	44.053172
3501.084233	320830.082801	44.058177
3501.129235	320827.124719	44.063181
3501.105787	320819.852442	44.068186
3501.041060	320813.197191	44.073191
3501.622973	320799.012195	44.078196
3501.287028	320786.497127	44.083201
3501.524822	320778.013734	44.088205
3501.437231	320779.604803	44.093210
3501.182442	320761.683634	44.098215
3501.448338	320746.683046	44.103220
3501.399218	320744.553773	44.108225
3501.452015	320741.696229	44.113229
3501.272681	320726.281869	44.118234
3501.265975	320705.574304	44.123239
3501.433567	320700.638119	44.128244
3501.445537	320708.828190	44.133249
3501.268284	320694.482000	44.138253
3501.025218	320681.011077	44.143258
3501.162272	320672.645175	44.148263
3501.231638	320668.029630	44.153268
3501.073872	320663.525916	44.158273
3501.142933	320659.520994	44.163277
3501.040430	320660.427501	44.168282
3501.132310	320659.599093	44.173287
3501.333381	320649.594976	44.178292
3501.009846	320640.156245	44.183297
3501.562819	320631.547226	44.188301
3501.122319	320623.297049	44.193306
3501.196541	320608.097413	44.198311
3501.363152	320611.226069	44.203316
3501.441696	320603.072827	44.208321
3501.412458	320583.844286	44.213325
3500.837197	320573.147419	44.218330
3500.994897	320582.764852	44.223335
3501.207443	320582.935207	44.228340
3501.426669	320576.718899	44.233345
3501.583810	320561.302757	44.238349
3501.486238	320544.501751	44.243354
3501.392571	320549.528277	44.248359
3501.264978	320540.465942	44.253364
3501.152977	320538.575455	44.258369
3501.360875	320507.072812	44.263373
3501.560559	320496.356535	44.268378
3501.601886	320491.160217	44.273383
3501.320775	320485.785341	44.278388
3501.222631	320473.614615	44.283393
3501.121871	320457.958907	44.288397
3501.367079	320457.310052	44.293402
3501.254626	320454.580086	44.298407
3501.422272	320450.407087	44.303412
3501.341486	320447.977460	44.308417
3501.357323	320422.279839	44.313421
3501.223746	320410.369042	44.318426
3500.979809	320420.430916	44.323431
3500.961660	320407.789730	44.328436
3501.009071	320407.858699	44.333441
3501.168320	320400.430583	44.338445
3501.098615	320379.325657	44.343450
3500.966493	320372.350143	44.348455
3501.374018	320379.180954	44.353460
3501.063824	320371.826226	44.358465
3500.962294	320369.043666	44.363469
3501.346077	320369.314455	44.368474
3501.188954	320365.268545	44.373479
3501.364489	320352.291772	44.378484
3501.271035	320342.944209	44.383489
3501.326008	320339.221309	44.388493
3501.342501	320330.518017	44.393498
3500.980292	320328.692079	44.398503
3501.212605	320325.068657	44.403508
3501.165772	320320.980058	44.408513
3500.899468	320295.580879	44.413517
3501.119428	320300.100466	44.418522
3501.252896	320289.318167	44.423527
3501.378574	320286.271112	44.428532
3501.491686	320292.664589	44.433537
3501.490737	320278.748632	44.438541
3501.588853	320262.832793	44.443546
3501.735935	320264.921452	44.448551
3501.349757	320237.810999	44.453556
3501.349539	320224.174760	44.458561
3501.280852	320221.081764	44.463565
3501.301040	320212.835807	44.468570
3500.999278	320211.280264	44.473575
3501.095248	320220.576697	44.478580
3500.857352	320204.611605	44.483585
3501.043945	320186.951922	44.488589
3501.161700	320180.573335	44.493594
3500.900839	320183.514444	44.498599
3501.080869	320172.877481	44.503604
3501.158373	320180.752117	44.508609
3501.220945	320166.190169	44.513613
3501.195498	320172.503562	44.518618
3501.272856	320169.336848	44.523623
3501.316599	320152.335508	44.528628
3500.966214	320138.194286	44.533633
3501.544634	320132.735869	44.538637
3501.378641	320132.482028	44.543642
3500.984827	320136.334360	44.548647
3501.266279	320129.446795	44.553652
3501.113512	320111.458521	44.558657
3500.997973	320109.670333	44.563661
3500.981247	320100.285280	44.568666
3500.757512	320099.582528	44.573671
3501.006481	320100.128806	44.578676
3501.305254	320096.952913	44.583681
3500.989715	320093.313357	44.588685
3501.433866	320093.142214	44.593690
3500.940269	320089.097999	44.598695
3501.329494	320081.099613	44.603700
3501.276795	320061.721860	44.608705
3501.104883	320048.901080	44.613709
3501.080099	320047.785608	44.618714
3500.824033	320050.725976	44.623719
3500.931781	320055.644748	44.628724
3501.239557	320050.152310	44.633729
3501.162904	320049.044947	44.638733
3501.304802	320033.605558	44.643738
3501.262878	320025.801773	44.648743
3501.285652	320016.741260	44.653748
3501.295030	320017.910141	44.658753
3501.261677	320008.654873	44.663757
3501.723818	320009.116943	44.668762
3501.320968	319983.967897	44.673767
3501.254122	319972.835219	44.678772
3501.047612	319974.292263	44.683777
3501.493133	319967.022846	44.688781
3501.725507	319949.330468	44.693786
3501.269614	319942.227414	44.698791
3501.652198	319927.462708	44.703796
3501.800038	319933.265664	44.708801
3501.750002	319899.843937	44.713805
3501.444220	319889.766237	44.718810
3501.732008	319890.255566	44.723815
3501.439759	319868.803565	44.728820
3501.312255	319859.562984	44.733825
3501.567792	319847.845609	44.738829
3501.793481	319845.266269	44.743834
3501.417347	319832.935293	44.748839
3501.237373	319807.471447	44.753844
3501.396639	319820.930422	44.758849
3501.449830	319804.207320	44.763853
3501.472864	319789.397014	44.768858
3501.366615	319782.977065	44.773863
3501.485612	319766.269102	44.778868
3501.398161	319767.580333	44.783873
3501.329437	319754.972303	44.788877
3501.506598	319741.359063	44.793882
3501.197368	319734.690987	44.798887
3501.431031	319725.750091	44.803892
3501.514310	319715.102700	44.808897
3501.203794	319704.033489	44.813901
3501.652076	319694.728297	44.818906
3501.141852	319690.813849	44.823911
3501.590655	319676.980032	44.828916
3501.352294	319663.686142	44.833921
3501.451570	319659.396549	44.838925
3501.478095	319648.936104	44.843930
3501.138028	319650.770216	44.848935
3501.332326	319629.903502	44.853940
3501.085859	319631.951953	44.858945
3501.196358	319619.163216	44.863949
3501.370504	319615.065444	44.868954
3500.949435	319622.000477	44.873959
3501.355471	319615.246001	44.878964
3501.206106	319598.300073	44.883969
3501.205618	319584.332938	44.888973
3501.427220	319572.493587	44.893978
3501.174975	319579.122379	44.898983
3501.277932	319571.830128	44.903988
3501.103180	319563.818054	44.908993
3501.094470	319545.374520	44.913997
3501.012549	319534.752912	44.919002
3500.532623	319534.751678	44.924007
3500.976486	319533.410277	44.929012
3500.969206	319540.000777	44.934017
3500.866884	319537.930644	44.939021
3501.096927	319531.000138	44.944026
3500.962626	319530.995751	44.949031
3501.278125	319530.106921	44.954036
3501.370585	319533.349015	44.959041
3501.511312	319516.764764	44.964045
3501.409663	319489.812887	44.969050
3501.501216	319493.996456	44.974055
3501.133051	319490.136104	44.979060
3501.397779	319478.340868	44.984065
3501.098723	319467.015391	44.989069
3501.156622	319457.440443	44.994074
3501.236052	319452.746870	44.999079
3501.270150	319451.545853	45.004084
3501.216930	319449.773336	45.009089
3501.322814	319443.600026	45.014093
3501.474107	319424.190095	45.019098
3501.356255	319424.412110	45.024103
3501.718777	319413.161278	45.029108
3501.744318	319400.309435	45.034113
3501.554576	319391.765402	45.039117
3501.332705	319372.515554	45.044122
3501.255152	319370.594189	45.049127
3501.297944	319359.851275	45.054132
3501.140126	319344.992767	45.059137
3501.066236	319335.743692	45.064141
3501.218813	319330.326310	45.069146
3500.936471	319334.390258	45.074151
3501.127173	319328.559853	45.079156
3501.186056	319321.376217	45.084161
3501.169330	319315.476472	45.089165
3501.151975	319305.607958	45.094170
3501.379434	319296.871475	45.099175
3501.561228	319291.424079	45.104180
3501.485413	319281.666465	45.109185
3501.382852	319277.459272	45.114189
3501.261172	319252.214958	45.119194
3500.897439	319243.850747	45.124199
3501.009435	319240.271486	45.129204
3501.238000	319242.398339	45.134209
3501.121821	319250.608722	45.139213
3501.097005	319244.328611	45.144218
3501.018288	319229.915644	45.149223
3501.334995	319210.047251	45.154228
3501.092002	319212.120620	45.159233
3500.787760	319212.041035	45.164237
3501.131813	319208.959765	45.169242
3500.815366	319205.396600	45.174247
3501.027648	319193.889343	45.179252
3500.672756	319197.481257	45.184257
3501.015431	319199.768362	45.189261
3501.122053	319192.119294	45.194266
3501.335711	319204.883036	45.199271
3501.029348	319193.355097	45.204276
3501.378852	319174.143040	45.209281
3501.100869	319168.614861	45.214285
3501.063720	319155.620097	45.219290
3500.973938	319160.722501	45.224295
3501.224837	319160.021854	45.229300
3500.975275	319163.902602	45.234305
3500.799376	319167.771834	45.239309
3501.032868	319164.402546	45.244314
3500.994212	319156.165587	45.249319
3501.128298	319136.300269	45.254324
3501.208300	319130.461702	45.259329
3501.336756	319133.189367	45.264333
3501.421727	319119.157838	45.269338
3501.238511	319127.200634	45.274343
3501.035912	319112.120073	45.279348
3501.413333	319088.502221	45.284353
3501.060156	319081.688265	45.289357
3501.402849	319084.814946	45.294362
3501.083526	319083.516523	45.299367
3501.176379	319082.484401	45.304372
3501.164592	319077.169009	45.309377
3501.011789	319066.227627	45.314381
3501.297027	319047.407185	45.319386
3500.913751	319047.619814	45.324391
3500.985337	319043.792439	45.329396
3501.101564	319033.495913	45.334401
3501.020328	319040.683208	45.339405
3501.142488	319042.928472	45.344410
3501.070564	319048.053540	45.349415
3501.090275	319029.427252	45.354420
3501.001623	319021.808682	45.359425
3500.715664	319008.700123	45.364429
3500.811922	318993.013082	45.369434
3500.848026	319000.003948	45.374439
3500.890713	319001.676481	45.379444
3501.030999	318993.818581	45.384449
3500.799871	318997.442046	45.389453
3500.965255	318995.177384	45.394458
3501.189010	319003.436436	45.399463
3500.764537	318995.386972	45.404468
3500.874213	319001.679411	45.409473
3500.743581	318998.697779	45.414477
3501.241634	318987.476532	45.419482
3501.139768	318994.081902	45.424487
3501.034472	318995.345063	45.429492
3501.118980	318994.441452	45.434497
3501.042614	318977.941819	45.439501
3500.997212	318965.762422	45.444506
3500.926055	318970.225895	45.449511
3501.041411	318966.900503	45.454516
3501.194157	318965.502832	45.459521
3500.864744	318970.439189	45.464525
3501.147449	318966.273501	45.469530
3500.921666	318969.667157	45.474535
3500.995826	318965.050681	45.479540
3500.982316	318968.411151	45.484545
3500.905241	318970.763892	45.489549
3501.066749	318964.047544	45.494554
3500.946347	318954.551243	45.499559
3501.201940	318937.490863	45.504564
3500.849327	318930.422378	45.509569
3500.970452	318933.863569	45.514573
3501.101399	318917.662244	45.519578
3501.226671	318925.885824	45.524583
3500.989352	318929.688354	45.529588
3500.973175	318929.665500	45.534593
3501.221418	318931.662083	45.539597
3501.421899	318914.991936	45.544602
3501.059574	318899.452880	45.549607
3501.025013	318892.614524	45.554612
3501.110714	318878.862662	45.559617
3500.622994	318878.760878	45.564621
3501.167446	318865.395241	45.569626
3500.808327	318876.569474	45.574631
3501.048807	318876.659145	45.579636
3501.024785	318883.608546	45.584641
3501.043647	318884.114490	45.589645
3501.102195	318873.241784	45.594650
3501.159899	318879.745900	45.599655
3500.952612	318855.735941	45.604660
3501.424023	318843.755571	45.609665
3501.000937	318852.980797	45.614669
3501.135134	318848.583897	45.619674
3500.734739	318850.783658	45.624679
3500.844178	318852.318553	45.629684
3501.094955	318843.145824	45.634689
3500.951086	318851.818563	45.639693
3500.955349	318839.682249	45.644698
3501.266566	318845.612460	45.649703
3500.966387	318828.689809	45.654708
3501.137299	318820.598115	45.659713
3500.703036	318806.851195	45.664717
3500.903946	318791.936415	45.669722
3500.944217	318805.414310	45.674727
3501.284271	318805.971807	45.679732
3500.896939	318808.194969	45.684737
3500.552284	318803.516744	45.689741
3500.816121	318793.502385	45.694746
3500.775804	318806.891111	45.699751
3501.214278	318791.048729	45.704756
3501.088135	318805.239569	45.709761
3500.893139	318800.232645	45.714765
3501.201000	318797.182445	45.719770
3501.516650	318789.017233	45.724775
3501.267975	318773.689341	45.729780
3501.227894	318764.816486	45.734785
3501.322849	318760.451154	45.739789
3501.505110	318749.711727	45.744794
3501.061217	318745.634172	45.749799
3501.107973	318732.193653	45.754804
3501.401337	318712.812077	45.759809
3501.224309	318716.325340	45.764813
3501.518957	318687.402873	45.769818
3501.252949	318638.748841	45.774823
3501.591371	318531.865524	45.779828
3501.241198	318396.136622	45.784833
3500.722337	318192.452401	45.789837
3500.758271	317945.250592	45.794842
3500.593235	317659.787989	45.799847
3500.006477	317330.399222	45.804852
3500.019285	316942.039595	45.809857
3499.414203	316526.396445	45.814861
3499.210262	316041.557201	45.819866
3498.529922	315524.524684	45.824871
3498.311721	314948.791155	45.829876
3498.031617	314328.634279	45.834881
3497.334352	313666.779536	45.839885
3496.941098	312946.929385	45.844890
3496.341308	312200.840662	45.849895
3495.192539	311387.317941	45.854900
3495.214446	310544.945623	45.859905
3494.179882	309644.246836	45.864909
3493.569379	308697.354417	45.869914
3492.694374	307718.140812	45.874919
3491.524534	306675.765643	45.879924
3490.872301	305585.749294	45.884929
3490.193640	304460.567955	45.889933
3489.534396	303286.978460	45.894938
3488.264397	302060.622582	45.899943
3487.019600	300794.352349	45.904948
3486.199486	299477.998586	45.909953
3484.856150	298126.468870	45.914957
3484.108361	296720.420128	45.919962
3482.847111	295274.505557	45.924967
3481.340330	293771.473832	45.929972
3480.363379	292230.291491	45.934977
3478.998436	290663.293292	45.939981
3477.504272	289027.951089	45.944986
3476.465746	287374.701408	45.949991
3475.079177	285671.542077	45.954996
3473.616920	283917.613230	45.960001
3471.973899	282134.823432	45.965005
3470.356255	280298.723905	45.970010
3468.927099	278440.399047	45.975015
3467.321141	276531.364295	45.980020
3465.591619	274584.543737	45.985025
3463.867382	272602.818992	45.990029
3462.137014	270587.235264	45.995034
3459.860849	268537.418270	46.000039
3457.977271	266432.773722	46.005044
3456.417991	264302.671339	46.010049
3454.020240	262155.569746	46.015053
3451.990911	259966.223804	46.020058
3450.072996	257739.741520	46.025063
3448.023539	255488.003322	46.030068
3445.917986	253194.318264	46.035073
3443.928160	250874.908326	46.040077
3441.515363	248524.103986	46.045082
3439.220810	246139.071964	46.050087
3436.668047	243718.166756	46.055092
3434.333878	241285.383525	46.060097
3431.833312	238823.059556	46.065101
3429.234122	236321.126983	46.070106
3426.998958	233803.075069	46.075111
3424.409777	231259.596176	46.080116
3421.704012	228684.569761	46.085121
3418.993365	226093.314620	46.090125
3416.349050	223470.593311	46.095130
3413.518121	220836.188292	46.100135
3410.441199	218172.106866	46.105140
3407.625729	215478.351053	46.110145
3404.708285	212784.857589	46.115149
3401.583378	210055.227996	46.120154
3398.538396	207325.333287	46.125159
3395.068233	204552.267870	46.130164
3391.639812	201790.873269	46.135169
3388.302711	199005.569058	46.140173
3385.569170	196206.621021	46.145178
3381.975441	193397.549249	46.150183
3378.439691	190579.871501	46.155188
3375.120357	187760.699186	46.160193
3371.349441	184926.060736	46.165197
3368.074741	182065.069289	46.170202
3364.377313	179213.676808	46.175207
3360.512055	176359.410216	46.180212
3356.898920	173494.049669	46.185217
3352.578375	170623.416932	46.190221
3348.701065	167749.604335	46.195226
3344.303087	164895.082491	46.200231
3339.352695	162050.275275	46.205236
3335.069732	159198.844844	46.210241
3330.219700	156369.945080	46.215245
3326.043368	153533.986086	46.220250
3321.156835	150727.383322	46.225255
3316.080425	147926.514767	46.230260
3311.539538	145153.692188	46.235265
3305.969317	142423.564427	46.240269
3300.347238	139610.411967	46.245274
3294.687981	136911.232956	46.250279
3288.770458	134265.046770	46.255284
3282.210052	131656.834614	46.260289
3275.623436	129103.339236	46.265293
3268.685542	126595.791301	46.270298
3261.377931	124151.995443	46.275303
3253.864209	121764.236671	46.280308
3246.556560	119448.035037	46.285313
3239.075158	117201.494652	46.290317
3231.032934	115030.363159	46.295322
3222.365498	112938.238361	46.300327
3214.115090	110944.856484	46.305332
3205.722037	109030.444799	46.310337
3196.769476	107219.567786	46.315341
3187.991613	105499.549015	46.320346
3179.091214	103874.058072	46.325351
3170.011268	102354.480384	46.330356
3161.055143	100930.891591	46.335361
3151.968625	99621.050117	46.340365
3143.582909	98405.761314	46.345370
3135.361902	97259.299428	46.350375
3127.008479	96228.763850	46.355380
3119.907897	95266.893747	46.360385
3112.387598	94391.786409	46.365389
3105.610902	93583.340077	46.370394
3099.426947	92850.048976	46.375399
3093.205052	92173.022260	46.380404
3087.665498	91551.813270	46.385409
3081.986188	90983.459537	46.390413
3076.738887	90456.649119	46.395418
3071.404618	89976.225796	46.400423
3066.526977	89532.369690	46.405428
3062.016012	89112.756059	46.410433
3057.489238	88727.569994	46.415437
3053.920963	88357.599791	46.420442
3049.896561	88000.969751	46.425447
3046.148263	87676.571653	46.430452
3042.650279	87349.876505	46.435457
3039.117517	87031.130908	46.440461
3036.029178	86721.771523	46.445466
3032.642828	86422.549389	46.450471
3029.356776	86122.806460	46.455476
3026.156708	85822.468771	46.460481
3022.724280	85533.146881	46.465485
3019.191193	85230.529830	46.470490
3016.273646	84947.929897	46.475495
3012.982943	84658.022911	46.480500
3009.656992	84365.697962	46.485505
3005.852146	84083.740697	46.490509
3003.076558	83789.696786	46.495514
2999.760861	83499.792685	46.500519
2996.046295	83206.282703	46.505524
2992.849974	82909.074350	46.510529
2989.661847	82624.265784	46.515533
2986.101562	82337.219082	46.520538
2982.723189	82050.667643	46.525543
2979.101020	81770.292518	46.530548
2975.756454	81468.511449	46.535553
2971.933100	81186.598500	46.540557
2968.453325	80893.863295	46.545562
2965.083181	80616.648462	46.550567
2961.541687	80344.162841	46.555572
2957.753963	80068.873205	46.560577
2953.994422	79791.244791	46.565581
2950.711353	79508.959411	46.570586
2946.968771	79245.470492	46.575591
2943.305475	78974.757400	46.580596
2939.808040	78715.718701	46.585601
2936.107079	78451.075037	46.590605
2932.255703	78184.984141	46.595610
2928.537096	77935.919405	46.600615
2924.887459	77687.214458	46.605620
2921.489470	77429.772580	46.610625
2917.812101	77182.041792	46.615629
2914.072496	76933.789571	46.620634
2910.850201	76685.915911	46.625639
2906.503903	76452.241117	46.630644
2903.331141	76215.019322	46.635649
2899.327642	75980.723478	46.640653
2896.102080	75749.406722	46.645658
2892.225297	75513.050457	46.650663
2888.620613	75299.106389	46.655668
2885.398168	75067.109214	46.660673
2881.376531	74848.065290	46.665677
2878.215757	74618.056126	46.670682
2874.529569	74391.255073	46.675687
2871.028501	74172.249542	46.680692
2867.666350	73955.255893	46.685697
2864.332996	73740.723060	46.690701
2860.508884	73514.890716	46.695706
2857.381746	73297.306921	46.700711
2854.175443	73073.972195	46.705716
2850.799431	72847.034165	46.710721
2846.732414	72634.110701	46.715725
2843.880655	72414.294277	46.720730
2839.991511	72185.524751	46.725735
2836.188674	71971.905006	46.730740
2833.214087	71740.939237	46.735745
2829.639434	71524.595497	46.740749
2826.194653	71306.595237	46.745754
2822.734401	71079.698272	46.750759
2819.011609	70861.224596	46.755764
2815.727172	70627.739506	46.760769
2811.911348	70414.070983	46.765773
2808.886003	70195.011301	46.770778
2805.494898	69968.494074	46.775783
2801.405883	69746.646135	46.780788
2798.617857	69508.325767	46.785793
2794.469404	69297.073680	46.790797
2791.411980	69066.271463	46.795802
2787.573874	68843.363594	46.800807
2784.065518	68621.935976	46.805812
2781.044955	68397.615416	46.810817
2777.186423	68171.663116	46.815821
2774.403411	67942.218246	46.820826
2770.905997	67721.069626	46.825831
2766.828251	67487.616302	46.830836
2763.995817	67256.579280	46.835841
2760.384039	67026.605704	46.840845
2756.297829	66800.948660	46.845850
2753.307250	66572.189643	46.850855
2749.609222	66340.579009	46.855860
2746.209576	66105.337469	46.860865
2742.359051	65885.523138	46.865869
2738.983010	65659.746106	46.870874
2735.673596	65427.581579	46.875879
2732.164163	65204.888891	46.880884
2728.783892	64965.338750	46.885889
2725.016266	64730.573766	46.890893
2721.515563	64495.997720	46.895898
2718.294162	64275.889553	46.900903
2714.574050	64042.843615	46.905908
2711.179965	63807.203726	46.910913
2707.786321	63580.343727	46.915917
2704.321352	63333.923335	46.920922
2700.948148	63111.551600	46.925927
2697.395625	62884.227731	46.930932
2693.721590	62625.762912	46.935937
2690.037458	62406.720977	46.940941
2687.000688	62175.959227	46.945946
2683.466047	61939.400669	46.950951
2680.055408	61707.534012	46.955956
2676.565750	61467.177786	46.960961
2673.007262	61222.696890	46.965965
2669.769899	60990.492555	46.970970
2666.743233	60745.343016	46.975975
2662.997861	60502.656394	46.980980
2659.620724	60262.624334	46.985985
2655.912570	60023.439649	46.990989
2652.261709	59784.356224	46.995994
2648.825843	59528.932683	47.000999
2644.991334	59281.208145	47.006004
2641.550220	59047.810341	47.011009
2638.165218	58808.174564	47.016013
2635.001844	58563.182532	47.021018
2631.510393	58313.218633	47.026023
2627.767983	58075.460826	47.031028
2624.399840	57830.336914	47.036033
2620.975971	57583.542693	47.041037
2617.289334	57329.640981	47.046042
2613.642720	57088.667217	47.051047
2609.978536	56854.335642	47.056052
2607.032186	56592.654645	47.061057
2603.362377	56358.531840	47.066061
2599.387956	56105.614474	47.071066
2596.324636	55863.889233	47.076071
2592.387891	55619.619205	47.081076
2588.890831	55369.775663	47.086081
2585.685294	55131.284204	47.091085
2582.323234	54884.083077	47.096090
2579.456213	54639.370294	47.101095
2575.094161	54384.933044	47.106100
2571.483581	54140.652609	47.111105
2568.100586	53898.496186	47.116109
2564.965781	53654.964782	47.121114
2561.420999	53406.101091	47.126119
2557.406387	53156.285774	47.131124
2554.271189	52899.997810	47.136129
2550.669731	52651.233464	47.141133
2547.413962	52406.439758	47.146138
2544.097424	52159.253789	47.151143
2540.343692	51906.188321	47.156148
2536.839385	51655.306901	47.161153
2533.250715	51414.553219	47.166157
2530.031053	51150.152395	47.171162
2526.567466	50898.854099	47.176167
2522.768196	50650.357765	47.181172
2519.564780	50395.433830	47.186177
2515.940891	50142.912831	47.191181
2512.378775	49890.993889	47.196186
2508.850744	49637.810076	47.201191
2505.355017	49392.121580	47.206196
2502.199812	49134.127648	47.211201
2498.591158	48878.649603	47.216205
2495.319855	48633.238599	47.221210
2491.662213	48371.925704	47.226215
2487.950383	48112.463684	47.231220
2484.662923	47856.356955	47.236225
2480.975752	47592.495165	47.241229
2477.473342	47336.002964	47.246234
2474.127259	47078.265109	47.251239
2470.384068	46829.287764	47.256244
2467.057646	46570.182655	47.261249
2463.577765	46302.504399	47.266253
2459.954230	46045.240316	47.271258
2456.577967	45790.363184	47.276263
2452.899908	45523.188169	47.281268
2450.014332	45267.739182	47.286273
2446.248942	45009.443697	47.291277
2442.726160	44746.369547	47.296282
2439.784072	44485.471662	47.301287
2435.870481	44215.774341	47.306292
2432.246971	43955.566344	47.311297
2428.905181	43689.901647	47.316301
2425.264064	43426.588901	47.321306
2421.739290	43162.607917	47.326311
2418.428596	42907.055898	47.331316
2414.752044	42633.079359	47.336321
2411.269413	42368.403724	47.341325
2407.714631	42103.393791	47.346330
2404.296348	41839.855830	47.351335
2401.060291	41583.831887	47.356340
2397.601055	41313.585255	47.361345
2394.179588	41043.329704	47.366349
2390.400180	40777.483202	47.371354
2387.064642	40497.697218	47.376359
2383.692646	40234.602482	47.381364
2379.993366	39961.005248	47.386369
2376.684634	39690.793184	47.391373
2373.304789	39408.219331	47.396378
2369.943939	39133.704604	47.401383
2365.956084	38865.358959	47.406388
2362.819895	38594.581966	47.411393
2359.287762	38316.782205	47.416397
2355.879163	38049.852308	47.421402
2352.319743	37763.181744	47.426407
2348.392114	37490.779957	47.431412
2344.856003	37222.751800	47.436417
2341.567415	36952.862470	47.441421
2338.092258	36674.086051	47.446426
2334.645207	36398.142588	47.451431
2331.113221	36127.991115	47.456436
2327.555424	35839.837282	47.461441
2324.302990	35571.867865	47.466445
2320.715739	35293.482027	47.471450
2317.522216	35011.887759	47.476455
2314.066660	34733.748565	47.481460
2310.592121	34441.714927	47.486465
2307.422504	34158.125204	47.491469
2303.669150	33872.513502	47.496474
2300.060607	33588.949394	47.501479
2296.772434	33307.601831	47.506484
2293.206593	33020.324357	47.511489
2289.684864	32725.951338	47.516493
2286.120711	32445.083189	47.521498
2283.047758	32153.912197	47.526503
2279.460503	31864.048971	47.531508
2275.966489	31570.182269	47.536513
2272.811052	31275.385780	47.541517
2269.033632	30975.994479	47.546522
2265.606633	30677.104055	47.551527
2262.220764	30390.487454	47.556532
2258.729294	30086.520206	47.561537
2255.368323	29791.922741	47.566541
2252.471276	29492.478552	47.571546
2248.825989	29181.222755	47.576551
2244.901861	28881.263728	47.581556
2241.865717	28575.378094	47.586561
2238.337527	28261.139517	47.591565
2234.611891	27951.752669	47.596570
2231.220490	27639.606081	47.601575
2227.656237	27332.928174	47.606580
2224.532238	27010.604383	47.611585
2221.016897	26702.908132	47.616589
2217.216851	26398.384923	47.621594
2214.099649	26073.629103	47.626599
2210.106632	25765.198112	47.631604
2207.040798	25442.288223	47.636609
2203.841899	25135.345642	47.641613
2200.075555	24816.046511	47.646618
2196.949859	24486.755733	47.651623
2193.297885	24170.179696	47.656628
2189.691920	23830.128165	47.661633
2186.108456	23525.734905	47.666637
2182.836910	23204.166632	47.671642
2179.012627	22868.657409	47.676647
2176.086920	22563.897171	47.681652
2172.380397	22218.244229	47.686657
2168.866794	21905.071766	47.691661
2165.539523	21576.931178	47.696666
2161.890178	21236.804073	47.701671
2158.377790	20913.359504	47.706676
2155.108813	20584.136736	47.711681
2151.557942	20245.708980	47.716685
2147.785512	19918.109065	47.721690
2144.087557	19591.472105	47.726695
2140.156961	19264.528619	47.731700
2136.755358	18944.943957	47.736705
2133.112334	18623.565469	47.741709
2129.289365	18309.903336	47.746714
2126.065129	17994.765502	47.751719
2121.857356	17682.345440	47.756724
2118.191296	17368.648626	47.761729
2114.544574	17072.674705	47.766733
2110.634989	16771.122476	47.771738
2106.978965	16480.187730	47.776743
2103.003456	16192.211095	47.781748
2099.596455	15908.535432	47.786753
2095.432665	15618.342302	47.791757
2091.557511	15352.980582	47.796762
2087.767515	15073.237057	47.801767
2083.564041	14824.836122	47.806772
2079.488780	14574.616741	47.811777
2075.170110	14338.879983	47.816781
2070.888891	14109.773495	47.821786
2067.256303	13891.577063	47.826791
2063.591754	13670.804569	47.831796
2060.300324	13454.601935	47.836801
2056.377675	13230.233937	47.841805
2052.431190	13026.869428	47.846810
2048.997802	12818.931108	47.851815
2045.372093	12619.794881	47.856820
2041.814157	12420.656484	47.861825
2038.897362	12216.455746	47.866829
2034.983946	12032.006681	47.871834
2031.828313	11827.654411	47.876839
2028.085889	11635.897906	47.881844
2024.937222	11430.380684	47.886849
2021.626426	11238.193474	47.891853
2018.044032	11034.755525	47.896858
2014.702200	10843.014090	47.901863
2010.919326	10645.427067	47.906868
2007.781454	10452.173043	47.911873
2004.343379	10252.997737	47.916877
2000.607419	10058.866376	47.921882
1997.366755	9868.236549	47.926887
1993.724861	9670.489013	47.931892
1990.115129	9475.590601	47.936897
1986.723275	9283.632450	47.941901
1983.081159	9090.180240	47.946906
1980.047081	8892.200271	47.951911
1976.360974	8692.694313	47.956916
1972.844537	8500.833394	47.961921
1969.487203	8310.487873	47.966925
1965.944582	8116.318090	47.971930
1962.437696	7921.293326	47.976935
1958.823934	7726.948860	47.981940
1955.377297	7528.870793	47.986945
1951.906211	7328.352086	47.991949
1948.242930	7143.054632	47.996954
1945.197100	6932.896299	48.001959
1941.483860	6747.446073	48.006964
1938.087167	6556.890624	48.011969
1934.712686	6365.700699	48.016973
1931.027679	6166.117496	48.021978
1928.005352	5961.375371	48.026983
1924.000664	5770.571950	48.031988
1920.671489	5574.427132	48.036993
1917.310007	5374.697508	48.041997
1913.885653	5176.309082	48.047002
1910.675657	4973.022025	48.052007
1906.971969	4774.520289	48.057012
1903.450070	4579.194841	48.062017
1900.073821	4376.298067	48.067021
1896.788893	4172.449407	48.072026
1893.166072	3967.500876	48.077031
1889.214145	3765.963645	48.082036
1885.788532	3569.342912	48.087041
1882.570728	3365.733324	48.092045
1878.857936	3164.880523	48.097050
1875.377473	2962.905080	48.102055
1871.756580	2772.611066	48.107060
1868.156748	2576.639116	48.112065
1864.662422	2369.052806	48.117069
1861.113541	2179.497385	48.122074
1857.555857	1968.343773	48.127079
1853.699393	1780.884726	48.132084
1850.298923	1584.920875	48.137089
1847.091950	1389.340211	48.142093
1843.431666	1201.938790	48.147098
1840.141053	1006.603205	48.152103
1836.061700	813.968627	48.157108
1832.574695	618.813559	48.162113
1828.953516	432.394905	48.167117
1824.692387	254.155615	48.172122
1821.064545	82.216216	48.177127
1816.303828	-65.379323	48.182132
1801.918516	57.535623	48.187137
1795.246704	65.337654	48.192141
1791.161532	75.424126	48.197146
1789.056112	52.961665	48.202151
1786.824067	62.568300	48.207156
1784.850738	74.146628	48.212161
1781.869709	66.529696	48.217165
1778.830914	74.288380	48.222170
1775.631540	69.746031	48.227175
1772.623189	71.672233	48.232180
1769.306027	68.727056	48.237185
1766.060553	71.566741	48.242189
1761.894045	65.752042	48.247194
1759.173860	71.091182	48.252199
1755.265973	68.459923	48.257204
1751.971752	63.824858	48.262209
1748.900709	66.542336	48.267213
1745.197661	69.770017	48.272218
1741.763536	71.813481	48.277223
1738.501604	76.035167	48.282228
1735.037867	64.523228	48.287233
1731.689356	58.096468	48.292237
1728.263388	70.193207	48.297242
1724.857458	72.564463	48.302247
1721.007249	69.478095	48.307252
1717.789422	67.782909	48.312257
1714.530176	68.685357	48.317261
1710.522681	61.795415	48.322266
1707.666900	62.387946	48.327271
1703.971002	55.385968	48.332276
1700.400966	71.482152	48.337281
1697.065176	66.220853	48.342285
1693.486308	73.010534	48.347290
1690.340909	63.793168	48.352295
1687.101732	68.612427	48.357300
1683.228079	70.205835	48.362305
1679.629021	65.169245	48.367309
1676.190936	68.678188	48.372314
1673.031787	67.192135	48.377319
1669.299784	67.140352	48.382324
1665.534779	63.271870	48.387329
1662.865627	61.924271	48.392333
1658.811134	79.361810	48.397338
1655.383045	66.597788	48.402343
1652.155550	69.447348	48.407348
1648.415838	67.435225	48.412353
1644.858999	70.285711	48.417357
1641.436614	69.030695	48.422362
1638.319602	73.283512	48.427367
1634.641433	67.424078	48.432372
1630.781937	75.921856	48.437377
1627.630530	67.686229	48.442381
1624.334603	66.227927	48.447386
1620.750427	65.868284	48.452391
1617.311240	61.891879	48.457396
1613.581972	65.300879	48.462401
1610.203026	64.985050	48.467405
1606.973150	66.243606	48.472410
1603.289403	67.051174	48.477415
1599.812101	63.912819	48.482420
1596.204825	69.169370	48.487425
1592.947951	64.430439	48.492429
1588.980307	66.323334	48.497434
1585.495631	59.424389	48.502439
1582.017889	59.063920	48.507444
1578.695810	64.756735	48.512449
1575.525479	59.713198	48.517453
1571.551663	57.358092	48.522458
1568.173783	64.496004	48.527463
1565.033117	59.147268	48.532468
1561.483195	65.726808	48.537473
1558.363521	57.875392	48.542477
1554.354306	72.603985	48.547482
1551.089399	64.977784	48.552487
1546.919349	68.047667	48.557492
1544.104753	67.203762	48.562497
1540.643906	62.079156	48.567501
1536.866880	55.469602	48.572506
1533.082099	61.921392	48.577511
1529.631475	64.774273	48.582516
1526.095057	64.989326	48.587521
1523.004329	61.603829	48.592525
1519.569526	61.635299	48.597530
1516.088076	59.712521	48.602535
1512.614472	62.926512	48.607540
1508.859731	67.152629	48.612545
1505.234806	64.736612	48.617549
1501.443864	76.482405	48.622554
1498.461039	67.733217	48.627559
1494.899568	67.357409	48.632564
1491.107263	66.679208	48.637569
1488.026029	63.485228	48.642573
1484.573554	71.128393	48.647578
1480.980856	65.094292	48.652583
1477.469374	70.620628	48.657588
1474.282926	74.200978	48.662593
1470.959468	68.890375	48.667597
1467.323377	65.131510	48.672602
1463.362038	66.618500	48.677607
1460.086829	71.721876	48.682612
1456.253920	66.835874	48.687617
1453.015230	65.128223	48.692621
1449.513913	71.130708	48.697626
1446.000934	59.164694	48.702631
1442.462546	60.610799	48.707636
1438.792731	70.104010	48.712641
1435.350387	63.033981	48.717645
1431.705128	65.078955	48.722650
1428.481690	61.255514	48.727655
1425.166693	57.338838	48.732660
1421.546628	62.413944	48.737665
1417.944430	54.742518	48.742669
1414.486491	67.059470	48.747674
1411.283871	65.273419	48.752679
1407.631421	58.843739	48.757684
1403.822771	62.186141	48.762689
1400.546482	51.524550	48.767693
1396.928125	60.525654	48.772698
1393.105970	64.974336	48.777703
1390.101690	63.068660	48.782708
1386.898385	63.851721	48.787713
1383.360733	57.255384	48.792717
1379.689115	63.860354	48.797722
1375.818031	65.478784	48.802727
1372.599473	64.878498	48.807732
1368.993870	60.577057	48.812737
1365.727886	53.713574	48.817741
1361.935886	61.979399	48.822746
1358.302336	57.897475	48.827751
1355.072399	52.584937	48.832756
1351.452131	68.752331	48.837761
1347.885747	63.511441	48.842765
1344.315014	67.095035	48.847770
1340.846755	68.061956	48.852775
1337.299415	61.755058	48.857780
1333.821939	71.047346	48.862785
1330.606905	68.181251	48.867789
1327.307999	65.888277	48.872794
1323.998595	61.847373	48.877799
1319.979520	57.215205	48.882804
1316.123193	64.791918	48.887809
1312.789714	59.261482	48.892813
1309.009676	60.236091	48.897818
1305.833815	61.714078	48.902823
1302.998305	69.273367	48.907828
1299.236537	71.143635	48.912833
1295.838239	60.460053	48.917837
1292.186961	59.291613	48.922842
1288.787012	54.303109	48.927847
1284.965880	54.743153	48.932852
1281.003526	53.730983	48.937857
1277.782381	57.006768	48.942861
1274.281198	62.743524	48.947866
1271.148536	62.525299	48.952871
1267.872028	59.611902	48.957876
1263.866603	69.989777	48.962881
1260.945799	54.511098	48.967885
1256.993718	67.079451	48.972890
1253.574469	71.708721	48.977895
1249.920971	62.716605	48.982900
1245.630380	67.539230	48.987905
1242.851909	61.820694	48.992909
1239.381782	58.364974	48.997914
1235.983416	62.760021	49.002919
1232.452786	57.307937	49.007924
1228.516117	62.141601	49.012929
1225.309419	59.309041	49.017933
1222.059672	68.562545	49.022938
1218.856299	62.303088	49.027943
1215.265017	62.846382	49.032948
1211.642148	59.047586	49.037953
1208.377314	52.813578	49.042957
1204.518658	54.221317	49.047962
1200.912691	54.918777	49.052967
1197.631812	52.256030	49.057972
1193.506124	49.171881	49.062977
1190.351330	40.149187	49.067981
1186.783529	53.771042	49.072986
1183.377385	53.522892	49.077991
1180.078769	54.165915	49.082996
1176.162304	54.668383	49.088001
1173.203194	56.314959	49.093005
1169.408555	62.853833	49.098010
1165.658460	57.556359	49.103015
1162.543121	51.052190	49.108020
1159.142336	58.136852	49.113025
1155.703216	55.856400	49.118029
1151.674551	63.324105	49.123034
1148.478896	52.912591	49.128039
1145.380741	59.522768	49.133044
1141.328464	60.356562	49.138049
1137.849253	59.186553	49.143053
1134.526590	61.608236	49.148058
1131.171638	67.989702	49.153063
1127.889678	54.690520	49.158068
1123.937563	57.033582	49.163073
1120.184505	55.482507	49.168077
1116.764955	58.893808	49.173082
1112.872844	50.192221	49.178087
1109.514370	56.159786	49.183092
1106.419965	62.497302	49.188097
1103.230754	48.822944	49.193101
1099.444552	60.507986	49.198106
1095.815459	56.105930	49.203111
1092.290250	63.678332	49.208116
1088.935674	64.690818	49.213121
1085.734395	56.763775	49.218125
1082.006053	50.270190	49.223130
1078.381981	54.972707	49.228135
1074.587182	57.661320	49.233140
1070.896324	55.407659	49.238145
1068.160154	57.323084	49.243149
1064.335321	61.050959	49.248154
1060.988178	60.186169	49.253159
1057.425893	54.444883	49.258164
1053.296834	63.864573	49.263169
1050.499737	57.234687	49.268173
1047.009105	62.685123	49.273178
1043.544325	50.993331	49.278183
1039.895668	51.153365	49.283188
1036.186920	54.534041	49.288193
1032.873072	50.013052	49.293197
1029.303253	60.772051	49.298202
1025.213884	58.261262	49.303207
1022.352489	52.736121	49.308212
1018.975343	54.742426	49.313217
1015.719345	53.464747	49.318221
1011.920268	58.906538	49.323226
1008.192830	63.688541	49.328231
1004.867010	60.365343	49.333236
1001.423281	60.977362	49.338241
997.851115	50.004765	49.343245
994.061567	58.159589	49.348250
990.577185	68.573029	49.353255
987.234941	64.686092	49.358260
983.624247	59.404835	49.363265
980.271310	57.769021	49.368269
977.088625	63.047875	49.373274
973.168094	52.930268	49.378279
969.969403	53.867766	49.383284
966.250333	60.692271	49.388289
963.128319	50.506589	49.393293
959.251987	64.857030	49.398298
955.496403	47.857707	49.403303
952.290896	54.386665	49.408308
948.672736	57.560199	49.413313
945.167473	56.242480	49.418317
941.559939	63.808836	49.423322
938.283877	61.727562	49.428327
934.914651	57.623408	49.433332
931.215855	57.047847	49.438337
927.696201	52.426245	49.443341
924.321050	47.193558	49.448346
920.777864	54.601144	49.453351
917.243071	48.358903	49.458356
913.605412	60.397229	49.463361
910.286501	55.880243	49.468365
906.590608	54.285502	49.473370
903.242639	54.341558	49.478375
900.128796	50.444204	49.483380
896.350813	53.807298	49.488385
892.886043	58.738036	49.493389
889.230497	60.120423	49.498394
885.642865	59.590748	49.503399
882.272545	43.973824	49.508404
878.351793	52.664922	49.513409
875.134057	59.895012	49.518413
871.641907	53.655603	49.523418
868.349718	54.734325	49.528423
865.068166	54.647116	49.533428
861.140218	64.430853	49.538433
857.468145	59.390218	49.543437
853.769980	62.370668	49.548442
850.505198	62.344113	49.553447
847.447220	57.397148	49.558452
843.630769	58.630740	49.563457
840.121546	56.250654	49.568461
836.419808	59.067154	49.573466
832.893429	52.336410	49.578471
829.995064	48.446470	49.583476
826.263677	61.913703	49.588481
822.842603	47.263376	49.593485
819.309252	56.466475	49.598490
815.783867	60.397488	49.603495
812.114969	52.192606	49.608500
808.662699	53.340710	49.613505
805.035072	56.598035	49.618509
801.780240	52.251393	49.623514
798.109182	52.971851	49.628519
794.789101	53.801865	49.633524
790.910023	54.833313	49.638529
787.153963	52.045811	49.643533
784.051280	60.001395	49.648538
780.540030	56.694666	49.653543
777.107845	56.393793	49.658548
773.362349	53.639444	49.663553
770.295810	59.169089	49.668557
766.716484	55.363660	49.673562
763.217371	56.987353	49.678567
759.543340	51.545270	49.683572
755.911146	58.213871	49.688577
752.479112	54.812490	49.693581
749.320218	58.278008	49.698586
745.641096	54.722334	49.703591
742.887557	53.676117	49.708596
738.606577	59.743968	49.713601
735.080805	54.000266	49.718605
731.510003	47.963062	49.723610
727.618175	58.712461	49.728615
724.527173	53.340443	49.733620
720.891649	66.239038	49.738625
717.550529	60.381003	49.743629
713.851983	61.184893	49.748634
710.240599	58.216578	49.753639
707.008247	56.732825	49.758644
703.531711	54.860206	49.763649
700.076699	53.895381	49.768653
697.147948	58.163272	49.773658
692.947348	54.363419	49.778663
689.660063	52.227049	49.783668
685.867883	63.438588	49.788673
682.374421	55.339170	49.793677
678.945971	47.757924	49.798682
675.177312	47.791359	49.803687
671.990482	45.364017	49.808692
668.877636	52.985862	49.813697
665.319542	52.078324	49.818701
661.626410	48.531209	49.823706
658.068763	49.569320	49.828711
654.438631	41.459687	49.833716
650.542765	47.644428	49.838721
647.204409	55.833109	49.843725
644.085427	49.228472	49.848730
640.217014	36.793335	49.853735
637.161935	46.959295	49.858740
633.210136	59.793548	49.863745
630.224008	48.700873	49.868749
626.763494	41.554947	49.873754
622.984208	48.518709	49.878759
619.641398	46.574560	49.883764
615.955060	48.768632	49.888769
612.519004	46.263285	49.893773
609.047429	43.823614	49.898778
604.853471	61.004847	49.903783
601.482969	47.409734	49.908788
598.455577	47.004403	49.913793
595.458471	47.113187	49.918797
591.786685	50.535693	49.923802
588.053686	46.805029	49.928807
584.962104	48.703484	49.933812
581.019743	53.781890	49.938817
577.367540	47.352542	49.943821
573.970878	46.653876	49.948826
570.139444	43.770706	49.953831
566.616151	36.754864	49.958836
563.500531	47.249864	49.963841
559.979431	47.681174	49.968845
556.193479	44.996531	49.973850
552.579440	52.706396	49.978855
549.452437	51.199875	49.983860
545.616893	53.417343	49.988865
541.955403	46.704727	49.993869
538.919113	59.063426	49.998874
535.714666	58.511839	50.003879
532.518311	52.185120	50.008884
528.393228	56.618285	50.013889
524.819115	55.276713	50.018893
521.242085	55.821201	50.023898
517.326718	52.413360	50.028903
514.361892	51.631261	50.033908
510.747240	57.389198	50.038913
507.503756	54.474078	50.043917
503.742459	52.598683	50.048922
500.339778	56.618155	50.053927
496.909119	51.457612	50.058932
493.104729	55.252103	50.063937
489.571922	46.001003	50.068941
486.409405	46.490071	50.073946
482.655541	55.031784	50.078951
479.299916	46.594496	50.083956
475.909498	51.839594	50.088961
472.770238	48.756304	50.093965
469.245859	48.928734	50.098970
465.186701	54.462078	50.103975
462.088100	43.804712	50.108980
458.055365	47.869099	50.113985
454.654164	47.519203	50.118989
451.370002	46.704886	50.123994
447.671809	55.987702	50.128999
444.213633	43.978791	50.134004
440.357211	52.172748	50.139009
437.114043	47.536522	50.144013
433.933542	45.139915	50.149018
430.256823	57.842560	50.154023
427.146380	49.667448	50.159028
423.290140	56.241540	50.164033
419.693684	55.590046	50.169037
416.328264	50.890719	50.174042
412.639027	49.813999	50.179047
409.285109	47.245248	50.184052
405.994284	39.617260	50.189057
402.194161	50.440984	50.194061
398.731065	42.384401	50.199066
394.741711	53.921142	50.204071
391.630190	53.117770	50.209076
388.390468	52.869156	50.214081
384.714088	52.024552	50.219085
381.678432	48.912412	50.224090
377.724231	58.203715	50.229095
374.460364	52.219831	50.234100
370.645482	51.532969	50.239105
366.996504	47.827208	50.244109
363.326071	56.064827	50.249114
359.456674	58.664162	50.254119
356.762283	52.932767	50.259124
353.201721	50.738093	50.264129
349.508610	51.228065	50.269133
346.475564	58.154130	50.274138
342.789716	58.744208	50.279143
339.078230	49.837542	50.284148
335.971983	43.917572	50.289153
332.426164	48.604929	50.294157
329.006642	54.762633	50.299162
325.062095	55.687472	50.304167
321.742155	51.885894	50.309172
317.900961	51.854911	50.314177
314.314757	54.549108	50.319181
311.295111	50.143674	50.324186
308.071182	67.100288	50.329191
304.028730	52.598175	50.334196
300.533564	45.283815	50.339201
297.291597	47.424221	50.344205
293.821711	42.545160	50.349210
289.710634	54.816013	50.354215
286.462090	49.029084	50.359220
283.216358	48.449256	50.364225
279.654760	46.314886	50.369229
276.312356	40.757802	50.374234
272.765592	45.660463	50.379239
269.136211	44.400421	50.384244
265.831871	48.198924	50.389249
262.019975	52.466080	50.394253
258.864834	43.042034	50.399258
254.957341	50.971976	50.404263
251.528233	41.309278	50.409268
248.050998	49.984904	50.414273
244.027645	50.824047	50.419277
241.106739	42.359898	50.424282
237.422128	46.850732	50.429287
234.134267	51.146538	50.434292
230.723338	45.736248	50.439297
227.034143	52.717678	50.444301
223.342045	54.713491	50.449306
219.832493	53.586557	50.454311
216.669311	43.407653	50.459316
213.142187	49.373443	50.464321
209.813853	48.847711	50.469325
205.954496	46.082977	50.474330
202.018702	52.957516	50.479335
199.118716	43.794080	50.484340
195.899455	51.078388	50.489345
192.244437	51.261902	50.494349
188.831060	43.659534	50.499354
185.011786	54.796382	50.504359
181.783572	46.168426	50.509364
177.747201	40.020914	50.514369
174.276537	46.787793	50.519373
170.929535	48.511264	50.524378
167.305908	63.578488	50.529383
163.636679	50.413205	50.534388
160.553509	47.273791	50.539393
157.051580	55.260456	50.544397
153.765900	50.865123	50.549402
149.631617	45.656779	50.554407
146.351773	48.271406	50.559412
143.137833	46.035173	50.564417
139.649859	46.031187	50.569421
136.487249	38.633168	50.574426
132.265185	41.540947	50.579431
128.814465	37.269561	50.584436
125.354575	34.964301	50.589441
121.842792	38.877609	50.594445
118.963925	47.956238	50.599450
114.774110	56.977667	50.604455
111.405974	48.627928	50.609460
108.076198	47.653209	50.614465
104.445389	53.530880	50.619469
100.830425	50.990496	50.624474
97.317789	60.076681	50.629479
94.019206	52.472188	50.634484
90.412537	48.516313	50.639489
86.433217	50.136402	50.644493
83.482978	42.800044	50.649498
79.883885	54.076436	50.654503
76.567916	44.576428	50.659508
72.700700	57.315355	50.664513
69.380685	47.373058	50.669517
65.786797	48.983389	50.674522
62.189768	47.158383	50.679527
58.838235	45.361355	50.684532
55.697267	45.110047	50.689537
51.829332	43.637538	50.694541
48.384834	40.956576	50.699546
44.885013	50.104041	50.704551
41.605567	43.297005	50.709556
38.203532	45.573312	50.714561
34.269188	53.637259	50.719565
30.652719	44.551349	50.724570
26.889392	52.012701	50.729575
23.968624	45.174785	50.734580
20.503025	45.015482	50.739585
16.766472	49.217147	50.744589
13.569378	42.476315	50.749594
9.681036	38.558284	50.754599
6.281689	43.447435	50.759604
2.780787	40.882897	50.764609