Thu Aug 25 10:39:59 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.349712	113.491066	0.000000
1.469603	108.846906	0.005005
1.358445	110.269069	0.010010
1.608140	109.575086	0.015014
1.493206	114.266002	0.020019
1.250726	115.205703	0.025024
1.197274	112.119961	0.030029
1.183082	98.489598	0.035034
0.953087	96.725495	0.040038
0.992231	77.907725	0.045043
0.823846	78.813669	0.050048
0.758981	77.678592	0.055053
0.211349	62.578435	0.060058
0.049556	55.975771	0.065062
-0.241558	41.034756	0.070067
-0.809017	42.579028	0.075072
-0.847500	30.964664	0.080077
-1.455088	19.104120	0.085082
-2.063708	20.658002	0.090086
-1.458383	11.571847	0.095091
-2.424785	11.789741	0.100096
-2.349483	11.537537	0.105101
-2.609914	10.708351	0.110106
-3.120653	-3.761618	0.115110
-3.498808	-2.610840	0.120115
-4.006171	2.828064	0.125120
-3.783856	0.999430	0.130125
-4.125620	0.129205	0.135130
-4.884446	-2.434711	0.140134
-4.581825	-7.303623	0.145139
-5.211476	-2.633330	0.150144
-4.928189	-7.372663	0.155149
-5.174792	-4.701758	0.160154
-5.254761	-8.058570	0.165158
-5.990021	-10.218055	0.170163
-6.556618	-9.721119	0.175168
-6.615268	-13.751981	0.180173
-6.592534	-8.851715	0.185178
-7.114677	-4.558934	0.190182
-7.623465	-12.628961	0.195187
-7.873181	-7.043768	0.200192
-8.075157	-13.336391	0.205197
-8.061785	-7.694344	0.210202
-8.247697	-8.649098	0.215206
-8.653818	-11.170200	0.220211
-8.527827	-8.329886	0.225216
-8.674073	-11.008764	0.230221
-9.190571	-7.931741	0.235226
-9.746905	-12.207326	0.240230
-9.858347	-8.918525	0.245235
-10.286506	-10.388977	0.250240
-10.006681	-12.071597	0.255245
-10.283530	-5.415974	0.260250
-10.969800	-4.466855	0.265254
-11.206486	-5.986291	0.270259
-11.855945	-5.008138	0.275264
-11.624302	-11.700895	0.280269
-11.663034	-17.351545	0.285274
-11.685997	-1.446975	0.290278
-11.329522	-10.642824	0.295283
-12.476366	-7.815048	0.300288
-12.380526	-10.402143	0.305293
-13.240274	-4.908028	0.310298
-13.771794	0.835215	0.315302
-13.906693	-3.335561	0.320307
-14.491188	0.998629	0.325312
-14.160679	-5.728603	0.330317
-14.518214	-2.850492	0.335322
-14.657410	0.075666	0.340326
-14.361985	-4.241629	0.345331
-14.575217	-1.493695	0.350336
-14.519322	-13.144963	0.355341
-15.134373	-6.566062	0.360346
-15.719665	-8.657296	0.365350
-15.977444	-7.797460	0.370355
-16.867486	-4.301243	0.375360
-17.111757	-5.942875	0.380365
-17.228903	-4.617859	0.385370
-17.416736	0.106594	0.390374
-17.356792	-3.908051	0.395379
-17.354941	-0.273169	0.400384
-17.056155	-13.139404	0.405389
-17.353543	-7.344263	0.410394
-18.181551	-10.909732	0.415398
-18.195586	-4.190884	0.420403
-18.513057	0.566537	0.425408
-18.852737	-2.493320	0.430413
-19.629757	-0.343580	0.435418
-19.881193	-1.240611	0.440422
-19.578893	-7.548973	0.445427
-19.658809	-5.112992	0.450432
-20.432180	-1.046599	0.455437
-20.926238	-3.610870	0.460442
-21.425020	-7.534806	0.465446
-21.531326	-12.899625	0.470451
-21.590524	8.148536	0.475456
-21.575112	-7.096725	0.480461
-21.600043	1.506254	0.485466
-21.870704	4.275842	0.490470
-21.388707	-9.280322	0.495475
-22.407400	6.881510	0.500480
-22.568956	-4.972972	0.505485
-22.767878	7.491721	0.510490
-23.211359	-4.590668	0.515494
-23.865690	-10.913653	0.520499
-24.600052	-8.729468	0.525504
-24.619440	-8.644136	0.530509
-24.311156	1.001286	0.535514
-24.398218	-6.562183	0.540518
-24.533987	-0.950550	0.545523
-24.598209	-12.450119	0.550528
-25.272029	-10.503210	0.555533
-25.530752	-9.013643	0.560538
-26.238798	-3.043427	0.565542
-26.077602	-10.911546	0.570547
-26.209795	5.320189	0.575552
-26.001381	-5.042029	0.580557
-26.658956	-5.926044	0.585562
-27.524528	-0.323447	0.590566
-27.542760	-14.215678	0.595571
-27.619263	0.346366	0.600576
-27.733269	-14.442015	0.605581
-27.490352	-3.476568	0.610586
-28.592826	-3.996646	0.615590
-28.835981	-12.870751	0.620595
-29.237457	-3.829127	0.625600
-29.156271	-3.882938	0.630605
-28.818477	-7.890497	0.635610
-29.412357	-8.563031	0.640614
-29.556870	-11.036536	0.645619
-29.785885	-10.940504	0.650624
-30.085659	-2.367229	0.655629
-30.362726	0.181901	0.660634
-31.309056	-9.588096	0.665638
-31.482343	-14.126175	0.670643
-31.587556	-2.293101	0.675648
-31.425166	-9.025627	0.680653
-31.747064	-14.315536	0.685658
-32.229020	-5.169554	0.690662
-31.778192	-7.923002	0.695667
-32.457476	-12.014806	0.700672
-32.824607	-9.998892	0.705677
-33.070877	-13.595398	0.710682
-33.353610	-2.595045	0.715686
-33.211315	-3.604388	0.720691
-33.965318	-3.274238	0.725696
-34.814468	-12.252707	0.730701
-34.612640	-3.039858	0.735706
-34.872927	0.639260	0.740710
-34.957405	-3.628001	0.745715
-35.276001	-7.804794	0.750720
-35.369435	-12.247818	0.755725
-35.171370	-4.606757	0.760730
-35.576566	-10.038638	0.765734
-35.535595	-7.156530	0.770739
-36.680321	-6.028008	0.775744
-36.500901	-3.695936	0.780749
-36.338082	-13.329672	0.785754
-37.164139	-8.429291	0.790758
-37.602572	-8.385866	0.795763
-38.017828	-1.287779	0.800768
-37.970784	-7.021473	0.805773
-37.860382	-9.860786	0.810778
-38.185405	4.607324	0.815782
-38.396710	-5.224059	0.820787
-39.290172	4.786830	0.825792
-39.514930	1.209097	0.830797
-39.064729	-17.771049	0.835802
-39.337950	-10.258625	0.840806
-39.488013	-10.393261	0.845811
-40.510471	-13.690979	0.850816
-40.925547	-16.359370	0.855821
-40.805064	-9.503416	0.860826
-40.967176	-4.371708	0.865830
-40.622200	-18.077237	0.870835
-41.279645	-5.635623	0.875840
-41.409281	-4.023913	0.880845
-41.843440	-10.153605	0.885850
-42.613240	-8.555485	0.890854
-42.557542	-8.374350	0.895859
-42.211423	-5.106623	0.900864
-42.325287	-10.849905	0.905869
-42.777599	-4.536947	0.910874
-43.411713	5.458616	0.915878
-43.247179	-1.729826	0.920883
-43.700143	2.254728	0.925888
-44.088820	1.705066	0.930893
-44.461741	-3.168729	0.935898
-45.223893	-5.608733	0.940902
-45.096706	-6.065219	0.945907
-45.297858	-5.897623	0.950912
-45.367667	-4.497767	0.955917
-45.230767	-6.613572	0.960922
-45.752766	3.168271	0.965926
-46.063838	-14.844714	0.970931
-46.819852	2.560431	0.975936
-47.168498	1.374913	0.980941
-46.672482	-6.956955	0.985946
-46.766048	-6.413913	0.990950
-46.790028	-5.809008	0.995955
-47.476973	-6.457466	1.000960
-47.879764	-8.729152	1.005965
-48.124397	-13.632536	1.010970
-48.576688	-6.262894	1.015974
-48.065047	-14.815505	1.020979
-49.509155	-3.601542	1.025984
-49.382188	-5.336143	1.030989
-49.646352	-7.882649	1.035994
-49.977372	1.923053	1.040998
-49.885162	-4.785823	1.046003
-50.096490	2.473301	1.051008
-49.995602	2.381601	1.056013
-50.129475	0.064614	1.061018
-50.761156	2.995173	1.066022
-50.679685	-1.393001	1.071027
-51.178744	-7.708675	1.076032
-51.832127	-0.750446	1.081037
-52.417978	-12.949721	1.086042
-52.734794	-6.607374	1.091046
-52.396573	-18.188978	1.096051
-52.667120	-11.385650	1.101056
-52.708129	-11.072304	1.106061
-52.620889	-10.196926	1.111066
-53.411491	-1.689112	1.116070
-53.528392	-13.974521	1.121075
-54.024370	-1.289287	1.126080
-54.328644	-7.932872	1.131085
-54.350456	-0.209903	1.136090
-54.416823	-1.939520	1.141094
-54.448149	-9.220655	1.146099
-55.104006	-3.606626	1.151104
-55.479771	-10.239009	1.156109
-55.480162	-11.861905	1.161114
-55.583905	-10.969257	1.166118
-56.296334	-11.313167	1.171123
-56.945326	-7.323210	1.176128
-57.106491	-4.273389	1.181133
-56.586646	-12.049007	1.186138
-56.910747	-8.138430	1.191142
-56.747797	-15.177923	1.196147
-57.874127	-10.455116	1.201152
-58.543955	-11.011344	1.206157
-58.555899	-13.499293	1.211162
-58.603900	-6.262601	1.216166
-58.448658	-12.335947	1.221171
-59.092553	-4.078911	1.226176
-58.796502	-15.777293	1.231181
-58.787779	-6.410806	1.236186
-59.807186	-11.110534	1.241190
-59.894518	-7.613541	1.246195
-60.331435	-4.181992	1.251200
-60.389621	-7.289116	1.256205
-60.393251	-9.496796	1.261210
-61.107163	-13.364872	1.266214
-61.669030	-5.307350	1.271219
-61.966179	-4.558402	1.276224
-61.906086	-5.260638	1.281229
-61.696500	-15.259202	1.286234
-62.017104	0.400937	1.291238
-61.606501	-6.047780	1.296243
-62.208962	-6.155821	1.301248
-62.658937	-1.640229	1.306253
-62.659658	-6.882387	1.311258
-63.718160	5.119042	1.316262
-64.145750	-4.950530	1.321267
-64.554186	6.493463	1.326272
-64.603419	3.675999	1.331277
-64.208469	-8.613685	1.336282
-64.726759	-2.293551	1.341286
-64.913041	-4.643453	1.346291
-64.646501	-7.633780	1.351296
-64.930368	0.054321	1.356301
-65.761157	-8.556864	1.361306
-66.382689	-2.385068	1.366310
-66.197777	-7.668967	1.371315
-66.012284	-3.414297	1.376320
-66.132767	-4.024964	1.381325
-66.933887	-7.863558	1.386330
-67.029334	1.383214	1.391334
-67.092453	-8.974417	1.396339
-67.446313	-1.477829	1.401344
-67.888289	-4.160987	1.406349
-68.201518	-7.082616	1.411354
-68.524930	0.197232	1.416358
-68.710210	-7.467902	1.421363
-68.842600	-5.340072	1.426368
-69.067877	3.854279	1.431373
-69.544978	-16.426394	1.436378
-70.166653	-1.060765	1.441382
-70.021009	-3.687302	1.446387
-70.058564	4.598117	1.451392
-69.991034	-6.273530	1.456397
-70.476973	-2.559055	1.461402
-71.383884	-10.721715	1.466406
-71.555946	-0.944087	1.471411
-71.779813	7.149064	1.476416
-71.624274	-6.922255	1.481421
-71.284130	-6.042212	1.486426
-71.731106	0.114889	1.491430
-72.425232	-0.222397	1.496435
-72.658105	-3.542593	1.501440
-73.073890	-5.508523	1.506445
-73.073159	-4.559479	1.511450
-73.373612	-6.369475	1.516454
-73.727896	-5.598920	1.521459
-74.355629	-8.695893	1.526464
-74.460511	-6.683105	1.531469
-74.604884	-4.550234	1.536474
-74.989458	3.406746	1.541478
-75.018660	-8.648798	1.546483
-74.705306	-2.781676	1.551488
-75.055162	-11.718151	1.556493
-75.529353	-13.070655	1.561498
-76.393341	7.037420	1.566502
-76.287220	3.942514	1.571507
-76.201165	-3.107079	1.576512
-76.622565	-11.696988	1.581517
-76.636253	-1.918867	1.586522
-77.684541	0.080395	1.591526
-77.816898	-7.903076	1.596531
-77.965376	-9.006062	1.601536
-77.842078	-10.502807	1.606541
-77.615243	0.607524	1.611546
-78.328731	-13.289655	1.616550
-79.138343	-8.173551	1.621555
-79.157996	-8.616520	1.626560
-79.631485	0.313003	1.631565
-79.142758	-6.768047	1.636570
-79.477289	-9.101046	1.641574
-79.557503	1.684077	1.646579
-79.970322	-0.402540	1.651584
-80.541693	-2.116302	1.656589
-80.419528	-5.523765	1.661594
-80.705063	-6.330031	1.666598
-80.900215	-6.425964	1.671603
-81.591834	-6.788951	1.676608
-82.257278	-8.563901	1.681613
-82.247639	-12.162538	1.686618
-82.607877	-1.804936	1.691622
-82.680586	-12.553364	1.696627
-82.539637	-9.338913	1.701632
-82.627055	-1.691087	1.706637
-82.592860	-8.068167	1.711642
-83.540371	-3.291119	1.716646
-83.895806	0.355452	1.721651
-83.962701	-10.678624	1.726656
-84.036818	-5.234842	1.731661
-84.386465	2.887507	1.736666
-85.041112	4.148050	1.741670
-85.139979	-2.325241	1.746675
-84.910681	-1.294954	1.751680
-85.516967	4.792200	1.756685
-85.335469	-8.254970	1.761690
-86.002761	2.894225	1.766694
-86.478094	-8.850969	1.771699
-86.661470	7.426746	1.776704
-86.626766	3.023753	1.781709
-86.531687	-10.633130	1.786714
-87.392685	5.839345	1.791718
-87.889963	-8.873157	1.796723
-87.966928	0.984482	1.801728
-88.442984	10.490212	1.806733
-88.304738	-2.404653	1.811738
-88.412154	-2.583935	1.816742
-88.400689	-14.864143	1.821747
-88.590682	-5.466521	1.826752
-89.260315	-3.200726	1.831757
-89.504483	-4.111548	1.836762
-89.869668	2.792034	1.841766
-89.772887	-4.322514	1.846771
-90.078984	1.891606	1.851776
-90.529178	8.473154	1.856781
-90.805011	6.055027	1.861786
-91.315266	2.012671	1.866790
-90.935020	1.902507	1.871795
-91.146734	2.426098	1.876800
-91.448779	-1.920963	1.881805
-92.086826	-0.428905	1.886810
-92.779452	-6.935705	1.891814
-92.684607	-4.723260	1.896819
-92.952720	1.070459	1.901824
-93.120817	-1.215854	1.906829
-92.658734	-5.581409	1.911834
-93.100752	1.675896	1.916838
-93.730653	-5.837310	1.921843
-94.028183	-10.112311	1.926848
-94.449117	-5.322862	1.931853
-94.127794	-9.359477	1.936858
-94.544867	-1.058887	1.941862
-95.257360	-3.335826	1.946867
-95.595929	-2.241868	1.951872
-96.077726	-3.900062	1.956877
-95.728064	-12.835413	1.961882
-96.063688	-0.083558	1.966886
-96.255679	-2.081390	1.971891
-95.872652	-1.888271	1.976896
-96.510172	-5.164042	1.981901
-96.991530	1.077540	1.986906
-97.254208	-0.991473	1.991910
-97.282733	-1.660841	1.996915
-97.463488	2.187742	2.006912
-97.498188	1.208073	2.016909
-97.465317	-0.355552	2.026906
-96.734932	-6.064231	2.036902
-96.087553	-3.558508	2.046899
-95.686879	3.943457	2.056896
-94.848247	6.412878	2.066893
-94.622468	2.889843	2.076890
-93.718330	2.808434	2.086886
-93.636817	0.701831	2.096883
-93.364262	-0.487539	2.106880
-92.454065	-3.138970	2.116877
-92.088211	-4.510852	2.126874
-91.248696	-0.774456	2.136870
-90.783992	-1.426901	2.146867
-90.694467	5.300196	2.156864
-90.117962	-6.824480	2.166861
-89.326979	-2.107970	2.176858
-89.210804	-6.253721	2.186854
-88.258649	-3.323754	2.196851
-87.826874	-1.956327	2.206848
-87.771391	-3.852945	2.216845
-86.960751	1.636594	2.226842
-86.234643	-0.257402	2.236838
-86.494727	1.478193	2.246835
-85.131356	-8.140516	2.256832
-85.272131	-10.608260	2.266829
-84.563552	-3.572690	2.276826
-83.833113	-2.755739	2.286822
-83.772506	-1.504381	2.296819
-82.807830	-6.847462	2.306816
-82.409944	-7.426081	2.316813
-82.059905	-10.018248	2.326810
-81.518758	-9.767181	2.336806
-80.999140	-4.273223	2.346803
-80.421268	1.712118	2.356800
-79.584015	-3.531803	2.366797
-79.420498	-8.388221	2.376794
-79.048080	-3.229158	2.386790
-78.941856	-6.210773	2.396787
-77.964862	-5.391274	2.406784
-77.617371	-0.193458	2.416781
-76.699144	-2.041529	2.426778
-76.537852	4.094619	2.436774
-75.901760	1.558997	2.446771
-75.384328	0.635364	2.456768
-75.051905	0.513661	2.466765
-74.365972	-6.442495	2.476762
-73.706671	-9.200329	2.486758
-73.605659	-9.466336	2.496755
-73.205115	-8.249236	2.506752
-72.380388	-1.238199	2.516749
-72.267122	-5.009697	2.526746
-71.158485	-2.113750	2.536742
-70.984515	-3.325685	2.546739
-70.632598	-3.526470	2.556736
-69.302855	-9.842241	2.566733
-69.033178	-6.599428	2.576730
-69.020088	-9.309860	2.586726
-69.113614	-5.687022	2.596723
-68.254023	-0.328694	2.606720
-67.316768	-9.605035	2.616717
-66.656442	-4.399218	2.626714
-66.465346	-0.637245	2.636710
-66.448099	-2.233268	2.646707
-65.634699	-7.866255	2.656704
-64.736289	-13.360507	2.666701
-64.073238	-2.978955	2.676698
-63.591523	-14.803674	2.686694
-63.761882	-7.532181	2.696691
-63.151074	-6.237154	2.706688
-62.504366	-8.698411	2.716685
-62.055329	-1.663351	2.726682
-60.922043	-6.693897	2.736678
-60.650752	-8.906262	2.746675
-60.366757	-2.770336	2.756672
-60.577962	-9.284979	2.766669
-59.473502	-10.436806	2.776666
-58.758225	-7.175114	2.786662
-57.639690	-12.345898	2.796659
-58.317530	-5.292659	2.806656
-57.905655	-3.421602	2.816653
-56.926958	-12.865991	2.826650
-56.446922	-5.439816	2.836646
-55.921137	-10.321320	2.846643
-55.211973	-9.380657	2.856640
-54.736241	-17.016625	2.866637
-54.634301	-13.975610	2.876634
-53.882883	-12.987716	2.886630
-53.678326	-9.547799	2.896627
-52.585675	-6.075976	2.906624
-52.192517	-3.821852	2.916621
-51.965635	-10.094696	2.926618
-51.198668	-13.179841	2.936614
-50.777738	-9.029398	2.946611
-50.360053	-9.851869	2.956608
-50.092782	-6.564329	2.966605
-49.282540	-4.993275	2.976602
-48.903938	-12.620361	2.986598
-48.457845	-6.598531	2.996595
-47.568565	-7.171781	3.006592
-47.480900	-8.683804	3.016589
-47.284062	-10.688100	3.026586
-46.057419	-4.440116	3.036582
-45.930029	-3.531839	3.046579
-45.701755	-5.072229	3.056576
-44.729740	-5.956214	3.066573
-44.568904	0.823066	3.076570
-43.648422	-6.179344	3.086566
-43.211669	-5.028104	3.096563
-42.999211	-8.900674	3.106560
-42.481107	-3.384300	3.116557
-41.611287	-10.312247	3.126554
-41.700586	-15.385641	3.136550
-40.683366	-9.012978	3.146547
-40.052662	-4.711670	3.156544
-40.131478	-14.034709	3.166541
-39.482666	-6.723676	3.176538
-38.849397	-8.831201	3.186534
-38.586757	-10.072868	3.196531
-37.978899	0.713311	3.206528
-37.541408	-5.801608	3.216525
-36.738470	-14.271289	3.226522
-36.045185	-17.544458	3.236518
-35.864177	-8.120073	3.246515
-35.458832	-6.381039	3.256512
-34.694359	-5.845013	3.266509
-34.476189	-7.621404	3.276506
-33.903678	-9.491329	3.286502
-33.101189	-8.672991	3.296499
-32.872339	-9.405686	3.306496
-32.467791	-9.168057	3.316493
-31.705254	-7.630708	3.326490
-31.599211	-5.803596	3.336486
-30.900737	-9.023727	3.346483
-30.427841	-10.333184	3.356480
-30.023442	-1.856119	3.366477
-29.109787	-14.784384	3.376474
-28.838416	-9.777379	3.386470
-28.194187	-6.406351	3.396467
-27.465388	-6.590158	3.406464
-27.088782	-10.783052	3.416461
-27.232044	-9.756341	3.426458
-26.409079	-8.466043	3.436454
-25.787944	-10.223210	3.446451
-25.505743	-2.861066	3.456448
-24.877350	-9.054271	3.466445
-24.110932	-4.929448	3.476442
-23.812922	-8.495476	3.486438
-22.861321	-4.447185	3.496435
-22.897746	-13.149646	3.506432
-22.811112	-7.004968	3.516429
-22.047786	-3.110908	3.526426
-21.558619	-6.909626	3.536422
-20.335762	1.882691	3.546419
-20.322540	-6.444250	3.556416
-20.167576	-8.454656	3.566413
-18.960785	-4.487530	3.576410
-18.452988	-13.915155	3.586406
-18.507974	-8.112583	3.596403
-17.886293	1.306118	3.606400
-16.884238	-9.215812	3.616397
-16.609951	-8.612484	3.626394
-16.912608	-9.591349	3.636390
-15.820555	-3.106861	3.646387
-15.382862	-4.673728	3.656384
-14.935874	0.787269	3.666381
-14.221411	-4.383556	3.676378
-14.090234	-7.362747	3.686374
-12.539703	1.362392	3.696371
-12.681223	-5.511631	3.706368
-12.457793	-13.792311	3.716365
-12.142322	-1.655189	3.726362
-11.316094	-6.438049	3.736358
-10.862808	-9.803494	3.746355
-10.026879	-9.861535	3.756352
-9.504968	-7.599072	3.766349
-9.206972	-7.876935	3.776346
-9.157863	-4.590056	3.786342
-8.575760	-3.518607	3.796339
-7.880284	-3.896763	3.806336
-6.832537	-4.732422	3.816333
-6.548413	-5.768381	3.826330
-6.352068	-5.631176	3.836326
-6.151349	-5.022657	3.846323
-5.210845	-6.256493	3.856320
-5.072079	3.681366	3.866317
-4.164867	4.090493	3.876314
-4.075043	7.624419	3.886310
-3.685667	12.818850	3.896307
-3.052628	26.306399	3.906304
-2.181163	36.490604	3.916301
-2.000381	37.751647	3.926298
-1.530706	52.994428	3.936294
-1.230871	59.783634	3.946291
-1.126667	68.966673	3.956288
-0.434548	84.253824	3.966285
0.191294	110.873114	3.976282
0.000000	117.899457	3.981286
0.742477	123.446290	3.986291
0.560002	139.474057	3.991296
1.003535	140.116448	3.996301
1.323208	156.078207	4.001306
1.172586	163.849907	4.006310
1.372355	157.883420	4.011315
1.492047	164.448501	4.016320
1.598747	164.349564	4.021325
1.614875	171.759781	4.026330
1.469775	167.843663	4.031334
1.663596	154.183829	4.036339
1.511318	159.700023	4.041344
1.435582	165.748393	4.046349
1.787071	154.797350	4.051354
1.877247	164.622570	4.056358
1.891935	159.067897	4.061363
1.659050	174.644848	4.066368
1.619745	163.925873	4.071373
1.698928	158.911590	4.076378
1.541844	156.376754	4.081382
1.660464	158.664592	4.086387
1.502237	165.801567	4.091392
1.727934	157.328478	4.096397
1.714262	162.784991	4.101402
1.387812	161.561180	4.106406
1.477205	157.965829	4.111411
1.433998	161.259789	4.116416
1.253037	159.054562	4.121421
1.672224	178.205644	4.126426
1.665293	185.701738	4.131430
2.004734	185.037984	4.136435
1.979301	185.434315	4.141440
2.185835	184.351621	4.146445
2.097702	183.185381	4.151450
1.752700	171.321558	4.156454
1.982915	172.440301	4.161459
1.640265	165.505263	4.166464
1.823854	167.172315	4.171469
1.729386	170.325612	4.176474
2.161621	192.714364	4.181478
2.409187	179.365630	4.186483
1.631880	174.425428	4.191488
1.960061	163.737460	4.196493
1.872435	174.618769	4.201498
1.932956	177.383949	4.206502
2.257648	178.279081	4.211507
1.821300	178.575278	4.216512
1.972144	182.034992	4.221517
2.250353	190.043235	4.226522
2.255445	177.988511	4.231526
2.140007	173.197708	4.236531
1.644899	171.759876	4.241536
1.733124	178.102101	4.246541
1.964026	181.058887	4.251546
2.171718	189.220548	4.256550
2.327132	189.110814	4.261555
2.015261	197.799977	4.266560
2.165875	189.088700	4.271565
2.359403	196.034532	4.276570
2.198196	192.646118	4.281574
2.402896	189.023203	4.286579
2.168727	194.960365	4.291584
2.256959	195.829271	4.296589
2.226480	193.897856	4.301594
2.204740	192.689576	4.306598
2.305782	185.280049	4.311603
1.839179	192.345129	4.316608
2.381271	197.132440	4.321613
2.327120	189.234697	4.326618
1.962456	202.883437	4.331622
2.445250	196.521413	4.336627
2.211465	198.693628	4.341632
2.026853	193.299885	4.346637
2.244918	198.916254	4.351642
2.029628	193.002132	4.356646
2.404113	187.659997	4.361651
2.295647	202.537267	4.366656
2.352813	194.884673	4.371661
2.310818	200.143154	4.376666
2.037075	198.518774	4.381670
2.452454	189.107948	4.386675
2.223647	203.589620	4.391680
2.387493	221.942356	4.396685
2.847669	221.424201	4.401690
2.189832	210.586973	4.406694
2.655116	204.990160	4.411699
2.343055	213.201630	4.416704
2.455209	213.329629	4.421709
2.718961	212.997275	4.426714
2.332529	226.719047	4.431718
2.681982	219.843228	4.436723
2.649112	220.123665	4.441728
2.809748	225.840789	4.446733
2.852819	215.975751	4.451738
2.170373	206.613538	4.456742
2.669397	212.540232	4.461747
2.759794	217.214822	4.466752
3.063640	213.130275	4.471757
2.657192	205.648393	4.476762
2.433396	201.545280	4.481766
2.834190	200.109444	4.486771
2.383212	209.750558	4.491776
2.855066	214.137588	4.496781
2.699615	214.437230	4.501786
2.268775	222.126310	4.506790
2.851963	219.658977	4.511795
2.505425	211.826018	4.516800
2.801239	210.745153	4.521805
2.830461	215.517913	4.526810
2.755420	213.859235	4.531814
3.170051	223.073664	4.536819
2.922112	220.796665	4.541824
2.812563	213.859887	4.546829
3.098000	216.621472	4.551834
2.718414	214.934580	4.556838
3.105321	215.152409	4.561843
2.798481	217.418330	4.566848
2.929323	221.061520	4.571853
3.140601	216.488436	4.576858
3.085198	218.373274	4.581862
2.902889	211.368803	4.586867
2.704164	208.293151	4.591872
3.009096	217.451998	4.596877
3.192809	212.557364	4.601882
3.023768	224.406920	4.606886
3.113818	212.860884	4.611891
2.745020	216.576031	4.616896
2.664386	219.037465	4.621901
2.844539	215.481666	4.626906
2.886431	226.387006	4.631910
3.153874	221.672242	4.636915
2.543374	225.994741	4.641920
2.887353	227.070352	4.646925
3.099978	224.297244	4.651930
2.868738	220.951436	4.656934
3.117306	219.302165	4.661939
2.931836	234.248475	4.666944
2.861653	221.161469	4.671949
2.951718	229.284631	4.676954
3.209810	247.553024	4.681958
3.490302	252.925509	4.686963
2.899452	238.069257	4.691968
3.085205	252.432230	4.696973
3.302658	235.294799	4.701978
3.284793	250.312938	4.706982
3.596271	244.240334	4.711987
3.054023	242.442883	4.716992
3.049304	248.299819	4.721997
3.337947	244.432784	4.727002
3.101575	251.135945	4.732006
3.410219	251.587501	4.737011
3.240857	252.730890	4.742016
3.347804	257.491484	4.747021
3.551055	257.197082	4.752026
3.458184	256.942750	4.757030
3.110243	256.623977	4.762035
3.444546	265.705480	4.767040
3.318770	260.606222	4.772045
3.418420	259.622529	4.777050
3.268549	253.470345	4.782054
3.355279	251.776825	4.787059
3.618586	255.763103	4.792064
3.571122	254.830934	4.797069
3.316311	254.734854	4.802074
3.550487	257.463347	4.807078
3.711229	259.330142	4.812083
3.552037	264.967675	4.817088
3.567952	255.676351	4.822093
3.233876	246.253206	4.827098
3.340720	248.223358	4.832102
3.510771	248.171442	4.837107
3.324366	256.638493	4.842112
3.261379	254.636234	4.847117
3.312023	243.327309	4.852122
3.369013	249.943376	4.857126
3.369197	252.202325	4.862131
3.705661	271.521494	4.867136
3.715360	269.738802	4.872141
4.055469	273.633955	4.877146
3.476998	259.493925	4.882150
3.569321	253.680284	4.887155
3.449734	272.387532	4.892160
3.487636	280.139236	4.897165
3.853839	276.165128	4.902170
3.581384	286.733776	4.907174
3.798528	278.780831	4.912179
3.959859	281.182216	4.917184
4.014816	274.950474	4.922189
3.983614	278.748781	4.927194
3.707107	273.227043	4.932198
4.073580	274.922399	4.937203
4.168685	272.537860	4.942208
3.929749	258.031417	4.947213
3.995395	255.471161	4.952218
3.586364	264.713423	4.957222
3.797828	256.986006	4.962227
3.660384	261.949409	4.967232
3.669374	269.503156	4.972237
3.826697	273.284578	4.977242
3.931660	289.292753	4.982246
3.993654	280.762997	4.987251
4.068257	280.415985	4.992256
3.990412	282.010113	4.997261
3.888089	282.459622	5.002266
3.873283	289.862081	5.007270
3.853026	282.259546	5.012275
3.816113	284.847018	5.017280
4.038575	283.385332	5.022285
3.922043	275.212584	5.027290
3.762812	284.355605	5.032294
4.063636	285.890404	5.037299
4.216196	286.565735	5.042304
4.097513	285.049932	5.047309
4.283527	282.192398	5.052314
3.632627	291.513700	5.057318
3.996733	287.024221	5.062323
3.926517	283.637352	5.067328
4.116286	281.190523	5.072333
4.249766	279.132168	5.077338
3.946822	293.726771	5.082342
3.973042	285.019117	5.087347
3.888485	282.694365	5.092352
4.024372	305.582112	5.097357
4.380295	308.253572	5.102362
4.401150	313.489583	5.107366
4.313612	315.841380	5.112371
4.557403	311.332781	5.117376
4.134552	301.537533	5.122381
4.327333	293.496649	5.127386
4.010861	296.178545	5.132390
4.344600	288.836922	5.137395
4.321634	307.848611	5.142400
4.171218	306.638338	5.147405
4.340955	310.642452	5.152410
4.026770	310.679062	5.157414
4.425175	307.389609	5.162419
4.170085	316.626761	5.167424
4.053232	319.587436	5.172429
4.170275	313.149798	5.177434
4.323039	309.563470	5.182438
4.482254	312.771958	5.187443
4.440797	313.528311	5.192448
4.331512	317.196489	5.197453
4.689748	310.104123	5.202458
4.355592	316.895396	5.207462
4.668838	314.141311	5.212467
4.439226	316.955135	5.217472
4.329472	321.563035	5.222477
4.370928	318.566792	5.227482
3.922877	314.426022	5.232486
4.640224	323.482340	5.237491
4.649855	328.900451	5.242496
4.509446	337.436265	5.247501
4.862514	332.543538	5.252506
4.610896	344.042274	5.257510
5.038235	338.340632	5.262515
4.744636	323.108700	5.267520
4.022118	318.299079	5.272525
4.808716	331.875105	5.277530
4.708396	334.099191	5.282534
4.452515	338.280731	5.287539
4.948930	334.020450	5.292544
4.797290	339.754902	5.297549
4.687117	345.840367	5.302554
4.723733	338.823691	5.307558
4.752431	334.582908	5.312563
4.850557	332.150431	5.317568
4.799215	333.193075	5.322573
5.156658	337.537950	5.327578
4.566510	337.111590	5.332582
4.775536	339.185967	5.337587
5.051670	339.576180	5.342592
4.888744	340.262979	5.347597
4.644284	329.095152	5.352602
4.580868	337.156988	5.357606
4.720712	346.136120	5.362611
4.837597	340.014878	5.367616
5.052128	352.063850	5.372621
5.064062	349.448720	5.377626
4.792473	345.008208	5.382630
4.837092	344.678547	5.387635
4.852419	347.055361	5.392640
4.893231	345.134906	5.397645
5.283336	341.748669	5.402650
4.945471	349.745943	5.407654
4.721554	347.806854	5.412659
4.789046	353.760080	5.417664
4.680771	348.556813	5.422669
4.958179	348.111584	5.427674
5.040773	347.839249	5.432678
4.876127	343.400964	5.437683
4.730726	346.505324	5.442688
5.065660	357.757141	5.447693
5.150926	358.351269	5.452698
4.992246	355.683775	5.457702
4.906002	354.805134	5.462707
5.234117	366.421862	5.467712
5.021641	376.497103	5.472717
5.301028	373.166174	5.477722
5.536507	373.720948	5.482726
5.063265	358.080528	5.487731
5.399085	354.715450	5.492736
4.702147	364.040838	5.497741
4.858554	360.020489	5.502746
4.913753	368.506687	5.507750
5.540915	369.316471	5.512755
5.340423	364.415555	5.517760
4.666363	374.446055	5.522765
5.119973	362.877761	5.527770
5.096836	373.239715	5.532774
5.184366	371.017704	5.537779
5.461646	371.686153	5.542784
5.148745	377.287692	5.547789
5.276245	376.271155	5.552794
4.864001	366.455227	5.557798
5.187389	381.530741	5.562803
5.702608	388.483194	5.567808
5.378254	395.149573	5.572813
5.542006	388.644477	5.577818
5.497100	373.816469	5.582822
5.395984	373.136314	5.587827
5.461628	368.225335	5.592832
5.283547	382.522031	5.597837
5.709553	378.203168	5.602842
5.425011	391.744584	5.607846
5.465989	386.495774	5.612851
5.701296	387.180292	5.617856
5.804531	387.806407	5.622861
5.134655	367.201139	5.627866
5.389638	385.485980	5.632870
5.414084	389.319884	5.637875
5.543148	395.238166	5.642880
5.677300	387.984723	5.647885
5.858491	385.355723	5.652890
5.475147	393.742962	5.657894
5.599981	395.919124	5.662899
5.360302	391.888059	5.667904
5.708965	400.306145	5.672909
5.992413	384.784427	5.677914
5.599480	396.507823	5.682918
5.749601	402.062133	5.687923
5.388530	395.237462	5.692928
5.380031	395.378039	5.697933
5.686301	391.378495	5.702938
5.568884	398.891990	5.707942
5.516259	395.647879	5.712947
5.580758	390.673798	5.717952
5.399097	397.782899	5.722957
5.732603	402.688371	5.727962
5.398501	406.369646	5.732966
5.973256	410.509644	5.737971
5.816217	410.768409	5.742976
6.087168	421.527246	5.747981
6.089516	408.966586	5.752986
6.017086	398.442488	5.757990
5.443287	398.285653	5.762995
5.837293	401.017600	5.768000
5.876376	423.537846	5.773005
6.263220	424.964264	5.778010
5.647973	415.423729	5.783014
5.911065	423.915346	5.788019
6.068617	418.891875	5.793024
6.164010	422.142021	5.798029
5.866903	411.994810	5.803034
6.141287	421.240807	5.808038
6.063605	412.014687	5.813043
6.087125	407.638655	5.818048
5.521506	407.179976	5.823053
5.939500	408.395865	5.828058
6.006332	428.943880	5.833062
6.071595	418.588025	5.838067
6.247217	426.454258	5.843072
6.412836	423.068378	5.848077
6.827095	421.266576	5.853082
6.073667	405.894645	5.858086
5.864742	405.013076	5.863091
5.900793	396.556933	5.868096
5.937419	414.142013	5.873101
5.696940	416.634847	5.878106
6.067239	425.672826	5.883110
5.895903	417.913567	5.888115
6.193539	412.985210	5.893120
6.195877	415.645647	5.898125
6.486420	419.121484	5.903130
6.300895	425.607932	5.908134
6.409939	423.610338	5.913139
6.497659	414.158981	5.918144
6.314140	425.840093	5.923149
6.612981	415.289452	5.928154
6.428650	434.589155	5.933158
6.437628	412.409460	5.938163
6.109104	419.063846	5.943168
6.197075	424.953774	5.948173
6.560107	422.407011	5.953178
6.380113	417.189651	5.958182
6.558105	432.091833	5.963187
6.456882	431.838807	5.968192
6.394349	424.002386	5.973197
6.480986	425.921939	5.978202
6.544074	420.131807	5.983206
6.285865	422.111718	5.988211
6.343240	416.398414	5.993216
5.871563	431.237869	5.998221
6.095800	425.375028	6.003226
5.952004	430.621053	6.008230
5.969095	427.540022	6.013235
6.362124	416.598129	6.018240
6.119130	422.407033	6.023245
6.382990	424.653165	6.028250
6.430072	434.387208	6.033254
6.764120	432.857406	6.038259
6.394749	428.925748	6.043264
6.200903	438.352687	6.048269
6.338775	424.729887	6.053274
6.821936	439.065395	6.058278
6.552767	438.772243	6.063283
6.589490	423.406211	6.068288
6.363145	431.670791	6.073293
6.175322	417.488411	6.078298
6.102717	428.513056	6.083302
6.385818	436.169461	6.088307
6.643017	442.744738	6.093312
6.508773	445.157655	6.098317
6.364700	436.824629	6.103322
6.544362	439.609149	6.108326
6.263393	430.800857	6.113331
6.536980	433.077104	6.118336
6.139375	437.227088	6.123341
6.667894	436.641270	6.128346
6.478680	443.653496	6.133350
6.341560	433.190134	6.138355
6.566457	429.434290	6.143360
6.173217	427.423644	6.148365
6.517100	435.127473	6.153370
6.319077	441.774075	6.158374
6.574297	448.454071	6.163379
6.654753	442.825729	6.168384
6.209179	432.005729	6.173389
6.313376	438.203173	6.178394
6.765284	449.743611	6.183398
6.650328	440.985234	6.188403
6.779603	436.848893	6.193408
6.378774	442.306039	6.198413
6.478334	434.868167	6.203418
6.471083	433.154554	6.208422
6.156487	421.374385	6.213427
6.256655	427.278222	6.218432
6.370754	431.870060	6.223437
6.153362	423.513726	6.228442
6.437283	441.518839	6.233446
6.707909	443.295669	6.238451
6.465857	425.594124	6.243456
5.980563	434.266280	6.248461
6.428337	441.441297	6.253466
6.707011	445.747919	6.258470
6.596525	444.749683	6.263475
6.443500	436.978056	6.268480
6.416844	429.756118	6.273485
6.328445	429.975655	6.278490
6.302889	417.555405	6.283494
6.590337	432.361343	6.288499
6.695570	429.206389	6.293504
6.143347	429.356227	6.298509
6.315899	422.166356	6.303514
6.475825	438.729213	6.308518
6.374512	440.583301	6.313523
6.646153	438.829154	6.318528
6.229834	437.372627	6.323533
6.398152	436.295906	6.328538
6.484523	446.884357	6.333542
6.503363	436.238367	6.338547
6.729473	432.412729	6.343552
6.246501	429.160107	6.348557
6.766145	430.692271	6.353562
6.455196	424.248885	6.358566
6.465751	425.892452	6.363571
6.201192	421.732398	6.368576
6.179907	436.738575	6.373581
6.395871	430.937142	6.378586
6.474985	426.922560	6.383590
6.371310	436.923839	6.388595
6.807106	432.514842	6.393600
6.444138	440.399029	6.398605
6.405174	431.030789	6.403610
6.522451	428.408633	6.408614
6.175082	428.219484	6.413619
6.459535	427.605467	6.418624
6.071405	432.288649	6.423629
6.404260	444.062876	6.428634
6.614226	456.894098	6.433638
6.390367	456.119273	6.438643
6.412977	455.704472	6.443648
6.624807	459.882362	6.448653
6.623347	441.877344	6.453658
6.386462	432.470510	6.458662
6.301413	433.695615	6.463667
6.534638	420.991202	6.468672
6.260022	418.104578	6.473677
6.534480	425.705384	6.478682
6.369605	434.140672	6.483686
6.096598	437.454869	6.488691
6.870741	450.052154	6.493696
6.255106	441.925892	6.498701
6.469572	442.544073	6.503706
6.607831	442.493974	6.508710
6.148929	447.839995	6.513715
6.747190	442.440577	6.518720
6.504906	443.829526	6.523725
6.209935	428.983704	6.528730
6.710733	428.598386	6.533734
6.392873	441.543935	6.538739
6.482086	429.320835	6.543744
6.192882	431.843452	6.548749
6.348011	434.663453	6.553754
6.486247	438.941456	6.558758
6.372107	448.890597	6.563763
6.901888	442.141467	6.568768
6.343368	432.617345	6.573773
6.594762	424.469140	6.578778
6.291444	431.239806	6.583782
6.269072	424.014036	6.588787
6.523844	420.028882	6.593792
6.147874	430.794170	6.598797
6.602229	430.374999	6.603802
6.449678	431.718250	6.608806
6.169909	433.356685	6.613811
6.403888	436.271902	6.618816
6.492904	449.065119	6.623821
6.530301	436.204714	6.628826
6.658833	435.267107	6.633830
5.927679	434.011772	6.638835
6.591914	436.473590	6.643840
6.691302	450.790143	6.648845
6.511331	446.809823	6.653850
6.455511	435.397232	6.658854
6.231843	437.881108	6.663859
6.444023	429.368878	6.668864
6.473656	431.607417	6.673869
6.263573	437.110607	6.678874
6.425601	435.338832	6.683878
6.533988	447.072300	6.688883
6.870475	430.602579	6.693888
6.570565	438.049769	6.698893
6.103095	429.058723	6.703898
6.501824	434.979060	6.708902
6.573768	430.101880	6.713907
6.558338	425.905955	6.718912
6.353553	430.019398	6.723917
6.546683	421.924617	6.728922
6.828878	432.893674	6.733926
6.276054	439.168751	6.738931
6.403326	435.611703	6.743936
6.585898	432.362372	6.748941
6.467621	430.675646	6.753946
6.534203	445.728176	6.758950
6.247773	438.850663	6.763955
6.505130	430.122544	6.768960
6.376046	435.062538	6.773965
6.553067	432.636668	6.778970
6.331411	431.953250	6.783974
6.636068	430.326811	6.788979
6.871416	420.441025	6.793984
6.577745	432.326064	6.798989
6.335853	429.291939	6.803994
6.366093	424.108077	6.808998
6.178782	425.602308	6.814003
6.791127	419.014260	6.819008
6.272913	426.723445	6.824013
6.939598	429.213352	6.829018
6.535104	415.450907	6.834022
6.674200	426.572098	6.839027
6.191146	429.694574	6.844032
6.694187	423.753249	6.849037
6.320403	419.227488	6.854042
6.498142	424.144716	6.859046
6.369046	425.895586	6.864051
6.443869	420.828129	6.869056
6.338596	425.890942	6.874061
6.217210	418.430747	6.879066
6.299191	431.376917	6.884070
6.224173	426.244348	6.889075
6.072671	409.860597	6.894080
6.142935	423.545765	6.899085
6.612452	423.633593	6.904090
6.567914	438.257429	6.909094
6.193546	431.687932	6.914099
6.392627	426.680100	6.919104
6.215809	432.453327	6.924109
6.362556	433.838270	6.929114
6.770944	424.937790	6.934118
6.342488	428.270014	6.939123
6.457915	420.143115	6.944128
6.444567	427.839637	6.949133
6.610079	433.660470	6.954138
6.804425	430.842737	6.959142
6.325125	433.948807	6.964147
6.402171	432.142890	6.969152
6.238473	436.512494	6.974157
6.147727	426.437348	6.979162
6.569508	435.926018	6.984166
6.008164	436.548693	6.989171
6.226363	431.414475	6.994176
6.432084	433.252094	6.999181
6.450081	429.215450	7.004186
6.343061	421.499897	7.009190
6.349968	436.004938	7.014195
6.402265	431.026430	7.019200
6.476353	440.917600	7.024205
6.391187	434.669791	7.029210
6.371499	437.918988	7.034214
6.387731	436.344067	7.039219
6.551384	429.396038	7.044224
6.255392	438.000570	7.049229
6.475985	421.871725	7.054234
6.605504	433.519614	7.059238
6.588802	431.652454	7.064243
6.314132	427.373759	7.069248
6.583248	430.457479	7.074253
6.475809	430.002943	7.079258
6.329293	417.348540	7.084262
6.041686	434.234617	7.089267
6.730611	430.140307	7.094272
6.360073	436.250779	7.099277
6.208066	429.655934	7.104282
6.630353	438.132106	7.109286
6.497604	437.554982	7.114291
6.515648	429.142775	7.119296
6.503149	430.647583	7.124301
6.522103	426.838583	7.129306
6.445622	432.982076	7.134310
6.551703	431.342456	7.139315
6.289702	427.204147	7.144320
6.142125	420.741492	7.149325
6.309082	431.807699	7.154330
6.546587	435.380437	7.159334
6.313181	437.641207	7.164339
6.805294	434.501567	7.169344
6.853503	432.560961	7.174349
6.363553	429.989653	7.179354
6.294123	426.099588	7.184358
6.703866	428.405123	7.189363
6.799717	431.810225	7.194368
6.482938	422.681675	7.199373
6.371882	426.891165	7.204378
6.593848	421.076139	7.209382
6.622054	437.517261	7.214387
6.596762	422.641846	7.219392
6.571323	436.965290	7.224397
6.723617	432.395065	7.229402
6.518102	426.833681	7.234406
6.349513	425.996413	7.239411
6.182157	428.904907	7.244416
6.466323	432.289995	7.249421
6.409793	425.079068	7.254426
6.918381	432.453364	7.259430
6.744785	430.281751	7.264435
6.669872	421.298806	7.269440
6.441417	407.663812	7.274445
6.545434	400.089212	7.279450
6.218127	397.672763	7.284454
6.024772	401.619891	7.289459
6.180042	412.080466	7.294464
6.337595	419.902070	7.299469
6.091922	416.938143	7.304474
6.525478	419.575310	7.309478
6.355120	429.128280	7.314483
6.927355	426.324107	7.319488
6.746871	429.579514	7.324493
6.488800	428.072882	7.329498
6.583631	423.454714	7.334502
6.194447	424.464873	7.339507
6.557954	419.042131	7.344512
6.335976	430.561589	7.349517
6.533664	432.837074	7.354522
6.660080	430.564669	7.359526
6.171236	427.708445	7.364531
6.290769	429.138781	7.369536
6.457326	435.652326	7.374541
6.768588	434.091292	7.379546
6.381669	416.010650	7.384550
6.577516	417.258182	7.389555
5.949484	413.585358	7.394560
6.251620	426.205960	7.399565
6.482318	433.114423	7.404570
6.375025	444.571628	7.409574
6.208055	427.010181	7.414579
6.576285	423.488149	7.419584
6.513486	430.528019	7.424589
6.781908	438.854290	7.429594
6.755932	430.698920	7.434598
6.208383	427.709522	7.439603
6.397266	421.687705	7.444608
6.674207	427.532207	7.449613
6.351821	409.707221	7.454618
6.327941	412.776733	7.459622
6.281056	420.747430	7.464627
6.429484	424.979539	7.469632
6.528979	425.163309	7.474637
6.499427	426.946040	7.479642
6.575048	429.060312	7.484646
6.167383	420.142159	7.489651
6.260940	426.208386	7.494656
6.434196	422.748541	7.499661
6.472149	430.829339	7.504666
6.549116	427.681979	7.509670
6.412805	438.510964	7.514675
6.346308	424.686062	7.519680
6.467998	428.868577	7.524685
6.438417	436.488551	7.529690
6.528250	426.878666	7.534694
6.581922	431.783697	7.539699
6.478589	424.187790	7.544704
6.734530	422.360173	7.549709
6.329043	415.725954	7.554714
6.205606	406.158987	7.559718
6.097883	416.334898	7.564723
6.769322	425.800266	7.569728
6.695650	427.181778	7.574733
6.643386	426.000411	7.579738
6.621132	408.261282	7.584742
6.195875	404.338386	7.589747
6.212832	403.025950	7.594752
6.559920	406.461287	7.599757
6.401251	405.268119	7.604762
6.281156	405.074999	7.609766
6.233464	404.168168	7.614771
6.300960	417.395013	7.619776
6.041273	422.118181	7.624781
6.368422	431.387554	7.629786
6.464670	433.141084	7.634790
6.444443	430.189289	7.639795
6.336542	440.507613	7.644800
6.440226	431.243576	7.649805
6.157635	450.944677	7.654810
6.811516	432.365580	7.659814
6.164533	438.547840	7.664819
6.340874	430.417720	7.669824
6.281519	436.564857	7.674829
6.228500	434.108591	7.679834
6.252567	422.857501	7.684838
6.014889	419.746786	7.689843
6.303983	428.262805	7.694848
6.236011	436.015346	7.699853
6.276766	435.066182	7.704858
6.417203	434.297556	7.709862
6.493046	435.326606	7.714867
6.746765	429.164910	7.719872
6.458410	432.772583	7.724877
6.243003	434.150992	7.729882
6.540564	434.082261	7.734886
6.239949	439.302237	7.739891
6.397088	429.751409	7.744896
6.405310	438.200707	7.749901
6.103683	440.734764	7.754906
6.475214	438.531523	7.759910
6.645933	451.495442	7.764915
6.357421	451.135716	7.769920
6.645517	439.381330	7.774925
6.411001	447.501663	7.779930
6.571402	432.499066	7.784934
6.425118	436.938709	7.789939
6.581685	424.464609	7.794944
6.263651	433.262421	7.799949
6.777982	439.642383	7.804954
6.686407	431.652318	7.809958
6.274458	438.370403	7.814963
5.990431	438.032121	7.819968
6.201259	437.578339	7.824973
6.277894	442.802484	7.829978
6.614865	445.489590	7.834982
6.365311	444.718791	7.839987
6.945852	437.079005	7.844992
6.800337	441.265424	7.849997
6.221169	439.423116	7.855002
6.327952	425.460330	7.860006
6.362358	427.786707	7.865011
6.183103	426.872015	7.870016
6.220910	428.179112	7.875021
5.880738	438.432586	7.880026
6.245893	449.195662	7.885030
6.452903	455.307399	7.890035
6.758928	455.012711	7.895040
6.688119	453.451426	7.900045
6.734843	452.767086	7.905050
6.600489	439.341955	7.910054
6.389115	434.793907	7.915059
6.326106	439.685584	7.920064
6.147120	431.168202	7.925069
6.143770	440.707667	7.930074
6.195663	447.884601	7.935078
6.220661	455.540324	7.940083
6.359233	450.152816	7.945088
6.636769	456.734403	7.950093
6.576120	467.826804	7.955098
6.724034	460.669253	7.960102
6.929482	458.770447	7.965107
6.758735	446.619704	7.970112
6.373626	438.194727	7.975117
6.171201	442.513452	7.980122
6.607296	420.550536	7.985139
6.693243	433.658684	7.990157
6.571352	427.208547	7.995174
6.505443	434.155235	8.000192
6.624477	438.321139	8.005210
6.995184	424.990039	8.010227
6.504705	431.965379	8.015245
6.445691	433.448396	8.020262
6.760695	426.024108	8.025280
6.574037	426.526753	8.030298
6.529490	431.109598	8.035315
6.467993	434.357064	8.040333
6.501635	429.491986	8.045350
6.742376	437.545631	8.050368
6.368464	432.207933	8.055386
6.471922	428.871919	8.060403
6.538703	436.318515	8.065421
6.447802	434.732834	8.070438
6.468896	429.336402	8.075456
6.241158	425.935519	8.080474
6.556719	424.869966	8.085491
6.470181	430.576522	8.090509
6.635700	431.894973	8.095526
6.848398	427.696104	8.100544
6.692566	435.098686	8.105562
6.724324	429.088369	8.110579
6.548021	426.607215	8.115597
6.875131	432.343633	8.120614
6.831076	435.089759	8.125632
6.316542	430.806023	8.130650
6.668105	417.960756	8.135667
6.654674	425.233726	8.140685
6.200576	437.397720	8.145702
6.540187	431.799906	8.150720
6.456031	441.709543	8.155738
6.628447	432.224802	8.160755
6.546312	435.743740	8.165773
6.242425	437.498649	8.170790
6.381905	431.099076	8.175808
6.633709	440.732015	8.180826
6.692889	422.804472	8.185843
6.637415	440.485363	8.190861
6.334327	435.729847	8.195878
6.530981	432.013165	8.200896
6.435144	436.455727	8.205914
6.374425	429.390102	8.210931
6.695175	438.450516	8.215949
6.461456	435.691184	8.220966
6.453045	442.108168	8.225984
6.679625	460.972472	8.231002
7.015894	453.090413	8.236019
6.861424	465.242193	8.241037
6.398514	451.675619	8.246054
6.628596	454.138958	8.251072
6.633764	464.577401	8.256090
6.639869	468.016249	8.261107
7.045456	453.477322	8.266125
6.839732	459.650678	8.271142
6.699497	461.698679	8.276160
6.853576	457.922391	8.281178
6.628880	453.987705	8.286195
6.814753	455.388174	8.291213
6.732490	461.513784	8.296230
6.801998	461.370390	8.301248
6.999764	456.069343	8.306266
6.688816	443.327862	8.311283
6.693965	438.855403	8.316301
6.745166	450.766669	8.321318
7.012918	451.355905	8.326336
7.048174	453.300670	8.331354
6.893489	437.050765	8.336371
6.800114	435.288750	8.341389
6.471135	439.815178	8.346406
6.526132	429.613547	8.351424
6.699622	442.326141	8.356442
6.563550	452.704656	8.361459
6.693294	453.391253	8.366477
6.282836	459.000251	8.371494
6.454016	457.326168	8.376512
6.364504	458.088143	8.381530
6.557405	459.313945	8.386547
6.659079	464.457701	8.391565
6.628532	474.784983	8.396582
7.185783	478.323668	8.401600
6.915729	477.119497	8.406618
7.266302	462.197869	8.411635
6.881212	458.925774	8.416653
6.676602	470.132377	8.421670
7.224668	454.027965	8.426688
7.200044	463.612711	8.431706
6.985751	462.576526	8.436723
6.954925	461.716719	8.441741
7.000441	461.078476	8.446758
7.180572	465.209568	8.451776
7.004133	468.336197	8.456794
6.988609	468.477520	8.461811
7.032499	461.269262	8.466829
7.227425	458.445922	8.471846
7.146932	452.487898	8.476864
6.735498	464.531619	8.481882
7.029730	452.736707	8.486899
7.085140	449.395595	8.491917
7.040631	465.222370	8.496934
6.904649	457.269138	8.501952
7.162259	469.813939	8.506970
7.206929	458.695587	8.511987
7.053721	464.908052	8.517005
6.807330	468.484290	8.522022
7.123276	464.515385	8.527040
6.927721	470.210633	8.532058
7.041242	458.068498	8.537075
6.939143	457.522810	8.542093
7.135534	465.223660	8.547110
7.140195	452.757764	8.552128
6.949367	456.688205	8.557146
7.351357	457.032350	8.562163
7.305272	459.993389	8.567181
7.150520	459.468573	8.572199
7.141667	441.141424	8.577216
6.775736	442.691464	8.582234
6.961491	450.734795	8.587251
7.061969	457.204150	8.592269
7.014489	465.091531	8.597287
7.187674	456.206249	8.602304
7.179865	462.058267	8.607322
6.903534	460.807745	8.612339
7.396247	462.939608	8.617357
7.013710	469.509893	8.622375
7.390945	463.199286	8.627392
7.314846	453.150724	8.632410
6.861751	438.746348	8.637427
6.974271	451.455878	8.642445
7.166948	461.246413	8.647463
7.160532	456.198260	8.652480
7.173663	460.749985	8.657498
6.907470	464.635432	8.662515
7.023696	456.267150	8.667533
7.028581	460.649757	8.672551
7.085721	459.829815	8.677568
7.007327	460.564802	8.682586
6.855369	471.324508	8.687603
7.092944	466.490583	8.692621
7.024297	471.436969	8.697639
7.279776	461.121859	8.702656
7.304422	462.077383	8.707674
6.802053	469.124027	8.712691
7.302165	454.964757	8.717709
7.377944	463.848976	8.722727
7.066683	459.205185	8.727744
7.333421	470.366339	8.732762
7.204446	464.415907	8.737779
7.430648	460.546269	8.742797
7.010506	464.376944	8.747815
7.006119	461.250322	8.752832
7.252137	470.284592	8.757850
6.865804	465.867153	8.762867
7.231992	467.554946	8.767885
7.347283	490.741160	8.772903
7.467339	481.760050	8.777920
7.332753	476.353283	8.782938
7.468387	477.433427	8.787955
7.592086	462.234927	8.792973
6.723863	469.976355	8.797991
7.288081	477.095725	8.803008
7.568225	478.743352	8.808026
7.029187	484.167380	8.813043
7.581127	479.965839	8.818061
6.994017	474.756204	8.823079
7.423112	478.551650	8.828096
7.178475	492.500576	8.833114
7.228888	496.592040	8.838131
7.582556	486.160547	8.843149
7.475031	501.378699	8.848167
7.812947	496.611094	8.853184
7.682319	482.648456	8.858202
7.379906	479.527502	8.863219
7.239459	466.838183	8.868237
7.281604	475.932801	8.873255
7.073459	476.694430	8.878272
7.230312	485.310341	8.883290
7.257786	492.993489	8.888307
7.660829	490.806555	8.893325
7.146100	493.102581	8.898343
7.126303	490.896693	8.903360
7.337525	486.663330	8.908378
7.417838	496.089643	8.913395
7.410762	485.954510	8.918413
7.533299	499.561894	8.923431
7.372526	505.526254	8.928448
7.520119	497.209842	8.933466
7.423626	497.411188	8.938483
7.314431	493.117575	8.943501
7.103240	494.633907	8.948519
7.184186	494.037448	8.953536
7.227918	492.698906	8.958554
7.364260	501.971279	8.963571
7.485194	504.262382	8.968589
7.718445	515.981069	8.973607
7.677606	506.955729	8.978624
7.710709	503.381420	8.983642
7.228522	504.018732	8.988659
7.092815	500.000666	8.993677
7.572610	509.178206	8.998695
7.526060	519.902490	9.003712
8.120091	512.033667	9.008730
7.654800	519.667804	9.013747
7.891375	507.654675	9.018765
7.316081	504.863646	9.023783
7.520992	502.146030	9.028800
7.600372	503.402245	9.033818
7.422880	500.091303	9.038835
7.773402	505.350713	9.043853
7.588311	511.684954	9.048871
7.597403	512.141152	9.053888
7.538038	515.180019	9.058906
7.829637	517.624262	9.063923
7.791585	518.614859	9.068941
7.428667	509.008830	9.073959
7.461350	505.207372	9.078976
7.642130	512.951714	9.083994
7.436221	530.170277	9.089011
7.625364	522.043001	9.094029
7.698476	518.108975	9.099047
7.590895	524.042917	9.104064
8.097630	516.500190	9.109082
7.778009	515.120749	9.114099
7.881270	517.307327	9.119117
7.629425	519.189787	9.124135
7.907886	513.740382	9.129152
7.866973	501.445692	9.134170
7.641161	507.215119	9.139187
7.749473	501.861803	9.144205
7.675018	496.000647	9.149223
7.470772	494.729360	9.154240
8.014823	505.241182	9.159258
8.091131	508.369241	9.164275
8.063465	499.906721	9.169293
7.850543	501.038323	9.174311
7.802482	498.982028	9.179328
7.726802	500.694875	9.184346
8.107667	496.523290	9.189363
7.989861	493.221933	9.194381
7.838331	496.287860	9.199399
7.962673	505.644165	9.204416
7.753716	491.586497	9.209434
7.620639	494.479122	9.214451
8.134645	492.685051	9.219469
8.121392	485.507827	9.224487
7.843526	493.516523	9.229504
7.879491	498.740011	9.234522
7.722213	493.014907	9.239539
7.740076	490.878857	9.244557
8.027174	489.082469	9.249575
7.767344	494.336523	9.254592
8.154048	491.726122	9.259610
7.965954	490.398657	9.264627
8.053382	493.285135	9.269645
8.231360	485.705569	9.274663
7.899707	491.090794	9.279680
7.987776	488.423045	9.284698
8.018098	492.120031	9.289715
8.034707	491.637792	9.294733
8.098015	485.101814	9.299751
8.179959	486.995087	9.304768
7.808744	493.557296	9.309786
8.055834	490.410202	9.314803
8.197682	494.654594	9.319821
8.255555	489.164020	9.324839
7.822446	476.214441	9.329856
7.793570	470.598612	9.334874
7.901395	479.458883	9.339891
7.906200	483.791016	9.344909
7.976406	474.136077	9.349927
7.654153	496.387326	9.354944
7.915074	488.857878	9.359962
7.727461	489.985514	9.364979
7.709552	497.032001	9.369997
7.808526	488.145708	9.375015
7.693802	495.336749	9.380032
7.946963	487.095318	9.385050
7.616394	480.917695	9.390067
7.496334	490.880321	9.395085
8.019424	501.881410	9.400103
8.161088	503.288810	9.405120
8.188676	513.095773	9.410138
8.122387	503.929257	9.415155
8.163675	517.940698	9.420173
8.154340	515.742636	9.425191
7.820048	503.983054	9.430208
7.981564	503.272986	9.435226
8.110636	512.991466	9.440243
7.791398	513.196155	9.445261
8.157813	506.530627	9.450279
8.092237	516.440550	9.455296
7.882503	514.185525	9.460314
7.994501	518.545052	9.465331
7.968211	512.881468	9.470349
8.134479	506.086357	9.475367
8.067142	518.022552	9.480384
8.235382	511.552173	9.485402
7.797366	513.968723	9.490419
7.894284	513.035251	9.495437
8.032644	510.801424	9.500455
8.283059	533.467913	9.505472
8.163188	528.955061	9.510490
8.381271	534.705439	9.515507
8.335505	534.892526	9.520525
8.589180	517.297327	9.525543
8.131022	522.408896	9.530560
8.297102	508.727948	9.535578
8.022440	509.900782	9.540595
8.422041	514.174220	9.545613
8.276852	512.672776	9.550631
7.979690	517.203706	9.555648
8.134159	518.628034	9.560666
8.397238	536.467389	9.565683
8.208630	542.789568	9.570701
8.679202	531.547636	9.575719
8.576789	528.638330	9.580736
8.428254	512.687190	9.585754
8.483251	512.309387	9.590771
7.987073	526.190455	9.595789
8.132078	505.112557	9.600807
8.097529	526.431997	9.605824
8.311671	526.183892	9.610842
8.456774	529.042404	9.615859
8.297212	533.223579	9.620877
8.761254	530.130847	9.625895
8.689533	529.479413	9.630912
8.532666	515.243154	9.635930
8.713451	515.505196	9.640947
8.477713	513.576133	9.645965
8.563237	504.253289	9.650983
8.535679	508.173938	9.656000
8.797032	505.974490	9.661018
8.715871	504.769123	9.666035
8.414293	509.373325	9.671053
8.530502	503.816803	9.676071
8.209168	504.365797	9.681088
8.235080	508.767211	9.686106
8.440995	509.811099	9.691123
8.002958	510.772849	9.696141
7.999484	506.248076	9.701159
8.151165	511.967826	9.706176
8.226968	517.601638	9.711194
8.632239	527.191645	9.716211
8.477635	533.202384	9.721229
8.799567	525.597091	9.726247
8.218347	536.149542	9.731264
8.460830	528.550384	9.736282
8.479162	537.648765	9.741299
8.360413	536.872157	9.746317
8.241583	539.459604	9.751335
8.413006	538.157855	9.756352
8.394562	534.743093	9.761370
8.580006	531.451019	9.766387
8.385702	533.788362	9.771405
8.752684	534.747056	9.776423
8.330962	535.324403	9.781440
8.363067	533.747842	9.786458
8.588121	524.488331	9.791475
8.545906	533.804477	9.796493
8.844183	528.020608	9.801511
8.601606	531.012445	9.806528
8.373974	536.362450	9.811546
8.484129	535.654117	9.816563
8.130515	540.111848	9.821581
8.580474	541.480413	9.826599
8.555512	561.779082	9.831616
8.315511	558.979691	9.836634
8.868057	564.677674	9.841651
8.554133	573.471530	9.846669
8.895073	563.300759	9.851687
8.832015	570.095576	9.856704
8.553699	566.188201	9.861722
8.962901	554.678162	9.866739
8.688693	563.270132	9.871757
8.959844	558.774900	9.876775
8.921403	564.814786	9.881792
8.683389	561.030484	9.886810
8.908442	550.278282	9.891827
8.811703	546.273035	9.896845
8.810220	540.968468	9.901863
8.687064	545.588904	9.906880
8.535109	535.195580	9.911898
8.903649	553.968312	9.916915
8.519627	562.861507	9.921933
9.119907	557.664619	9.926951
8.801105	563.827326	9.931968
9.012976	566.413454	9.936986
8.765256	557.480463	9.942003
8.554834	553.824381	9.947021
8.946210	567.288710	9.952039
8.753033	556.690395	9.957056
8.778117	559.331034	9.962074
9.078957	551.198867	9.967091
8.762897	565.758635	9.972109
9.059530	556.642525	9.977127
9.232787	561.923415	9.982144
8.872036	557.590306	9.987162
9.277247	541.034833	9.992179
8.765180	530.735803	9.997197
8.916489	539.977449	10.002215
8.825650	537.839491	10.007232
8.623892	537.356751	10.012250
9.070392	544.150614	10.017267
9.170529	560.699570	10.022285
9.062639	545.253267	10.027303
8.797018	544.146225	10.032320
8.489352	545.548291	10.037338
9.227945	549.257391	10.042355
9.387637	564.156021	10.047373
9.045931	549.708857	10.052391
8.922277	541.655827	10.057408
8.640942	540.156778	10.062426
8.899160	550.849108	10.067443
8.847263	567.570212	10.072461
9.095954	571.902023	10.077479
9.266039	564.307882	10.082496
9.067044	571.751996	10.087514
9.079316	569.477959	10.092531
9.275352	574.262984	10.097549
9.157322	564.574374	10.102567
9.215659	558.370504	10.107584
8.914445	549.644711	10.112602
9.223919	548.163543	10.117619
8.841625	543.347825	10.122637
9.162495	550.467484	10.127655
9.517996	557.947788	10.132672
8.894486	552.914244	10.137690
9.105111	540.693723	10.142707
9.059590	550.215520	10.147725
8.858530	554.529432	10.152743
9.106961	559.596574	10.157760
8.987210	567.656267	10.162778
9.145462	559.808366	10.167795
8.809285	561.426336	10.172813
9.011695	559.015213	10.177831
9.380070	556.549685	10.182848
9.151219	558.355964	10.187866
9.342650	565.517999	10.192883
9.309877	568.549553	10.197901
9.324733	570.077810	10.202919
9.555596	565.219665	10.207936
9.078372	568.948853	10.212954
9.475204	563.174777	10.217971
9.202193	570.652578	10.222989
9.210120	568.098358	10.228007
9.425750	562.100212	10.233024
9.522077	564.060667	10.238042
9.429308	554.888807	10.243059
9.400044	561.795089	10.248077
9.094280	560.460809	10.253095
9.157387	560.520386	10.258112
9.193776	562.976221	10.263130
9.203808	561.551436	10.268147
9.229776	568.190294	10.273165
9.179778	571.716847	10.278183
9.500035	559.561186	10.283200
9.039594	558.128066	10.288218
9.186954	561.387012	10.293235
9.331861	567.413950	10.298253
9.084303	570.330836	10.303271
9.346740	564.685113	10.308288
9.182844	565.146326	10.313306
9.351891	561.976734	10.318323
9.154613	579.014114	10.323341
9.271693	571.289421	10.328359
9.324587	562.517607	10.333376
9.488087	590.303817	10.338394
9.615588	589.072062	10.343411
9.696303	571.642762	10.348429
9.409007	568.181757	10.353447
9.771191	557.597411	10.358464
9.395299	561.547404	10.363482
9.538188	563.923436	10.368499
9.625189	577.489111	10.373517
9.220693	572.654773	10.378535
9.710380	560.564082	10.383552
8.898997	568.220908	10.388570
9.879925	580.803933	10.393587
9.416563	565.564785	10.398605
9.690068	563.625354	10.403623
9.461312	567.590164	10.408640
9.485533	566.832179	10.413658
9.499418	563.254558	10.418675
9.444960	572.067718	10.423693
9.274283	582.461199	10.428711
9.786254	578.979101	10.433728
9.616077	592.001265	10.438746
9.986057	588.677111	10.443763
9.490721	576.519840	10.448781
9.394894	587.987180	10.453799
9.666437	594.455029	10.458816
9.785915	597.311255	10.463834
9.855143	591.323415	10.468851
9.889151	591.706284	10.473869
9.584110	584.013011	10.478887
9.414713	572.625175	10.483904
9.449287	587.679126	10.488922
9.568150	586.426635	10.493939
9.617502	589.650449	10.498957
9.647873	598.163157	10.503975
9.764158	600.142579	10.508992
9.459015	598.205447	10.514010
9.865540	596.964687	10.519027
9.526150	601.802052	10.524045
9.466094	596.825379	10.529063
10.035970	592.857685	10.534080
9.616922	596.625100	10.539098
9.589532	597.434152	10.544115
9.472306	591.260933	10.549133
9.625622	591.148588	10.554151
9.483962	592.414195	10.559168
9.344194	594.165495	10.564186
9.752584	611.190058	10.569203
9.658469	619.233135	10.574221
9.578011	621.959748	10.579239
9.978355	613.647861	10.584256
10.105930	614.618824	10.589274
10.407188	612.274256	10.594291
10.174781	601.969237	10.599309
9.851601	605.352408	10.604327
9.864893	592.922931	10.609344
9.853873	594.732953	10.614362
9.884419	589.227695	10.619379
9.822319	584.494340	10.624397
9.843434	585.463047	10.629415
10.113213	582.861487	10.634432
9.964489	581.168088	10.639450
9.963723	596.640991	10.644467
9.964333	589.287986	10.649485
9.971540	593.512472	10.654503
10.265083	582.465501	10.659520
10.025206	595.429161	10.664538
9.771426	593.061108	10.669555
9.767981	583.139943	10.674573
9.801642	592.119185	10.679591
10.284579	585.627874	10.684608
10.028094	596.571288	10.689626
10.059542	581.573332	10.694643
10.031659	589.347245	10.699661
9.792044	591.751655	10.704679
9.824362	588.467783	10.709696
10.383207	615.106503	10.714714
10.071061	607.950815	10.719731
10.345371	591.589373	10.724749
10.471903	604.044354	10.729767
10.407333	587.594002	10.734784
10.191807	599.480887	10.739802
9.871952	594.718488	10.744819
10.039493	591.145188	10.749837
9.887471	598.610356	10.754855
9.844095	592.094209	10.759872
10.038957	600.082533	10.764890
10.059478	599.678573	10.769907
10.109178	604.341368	10.774925
9.926091	615.847644	10.779943
10.596288	616.689408	10.784960
10.483465	612.812897	10.789978
9.927100	612.300509	10.794995
10.052055	610.182379	10.800013
9.956551	615.022561	10.805031
10.344223	613.690081	10.810048
10.245071	623.049907	10.815066
10.060325	621.643013	10.820083
10.341299	615.871294	10.825101
9.935691	619.453573	10.830119
10.001768	614.428731	10.835136
9.876736	615.751694	10.840154
10.254529	617.731171	10.845171
10.394271	613.802464	10.850189
10.240499	622.205180	10.855207
9.990062	625.750525	10.860224
10.069902	618.400873	10.865242
9.786025	618.350716	10.870259
10.454635	632.828843	10.875277
10.291300	641.349830	10.880295
10.677953	636.931155	10.885312
10.510987	634.132932	10.890330
10.284195	626.907058	10.895347
10.577287	619.751209	10.900365
10.595386	621.840691	10.905383
10.416968	626.785385	10.910400
10.599348	617.879647	10.915418
10.165704	623.927826	10.920435
10.409271	620.787573	10.925453
10.432289	620.086578	10.930471
10.368694	617.915939	10.935488
10.465825	615.707494	10.940506
10.383996	612.845442	10.945523
10.702166	621.739098	10.950541
10.501978	616.191089	10.955559
10.412599	616.470217	10.960576
10.560209	613.250327	10.965594
10.262265	609.084087	10.970611
10.580202	609.261527	10.975629
10.426511	617.074098	10.980647
10.590473	631.123212	10.985664
10.895785	639.252037	10.990682
10.568975	628.750356	10.995699
10.886677	617.223056	11.000717
10.655171	611.951352	11.005735
10.373370	623.551995	11.010752
10.630376	620.015164	11.015770
10.349821	617.376750	11.020787
10.621797	611.663247	11.025805
10.176370	618.426475	11.030823
10.494001	628.184901	11.035840
10.935180	639.221000	11.040858
10.663912	638.938495	11.045875
10.615069	641.862127	11.050893
10.894172	645.173029	11.055911
10.974008	639.540114	11.060928
10.702088	626.038155	11.065946
10.278621	623.049750	11.070963
10.636821	628.554145	11.075981
10.606193	636.906016	11.080999
10.941861	641.770166	11.086016
10.981718	638.999496	11.091034
10.712591	645.539453	11.096051
11.214206	639.070442	11.101069
10.718493	627.020492	11.106087
10.531180	620.280737	11.111104
10.796266	625.572504	11.116122
10.575242	639.697724	11.121139
10.719537	640.546149	11.126157
10.823217	637.626625	11.131175
10.654626	643.204095	11.136192
11.284356	636.995877	11.141210
10.686445	640.762923	11.146227
10.865761	633.716413	11.151245
10.946177	644.222065	11.156263
10.378984	643.364237	11.161280
10.789644	635.994303	11.166298
10.562022	647.939919	11.171315
10.576591	634.238433	11.176333
10.632996	640.228771	11.181351
10.419257	642.348268	11.186368
10.627267	645.824943	11.191386
10.449054	652.921854	11.196403
11.241878	656.032349	11.201421
11.209090	667.208998	11.206439
10.832038	668.988016	11.211456
11.262003	661.236352	11.216474
10.888251	655.346299	11.221491
11.012032	642.763777	11.226509
11.200165	641.576167	11.231527
11.190482	643.275532	11.236544
10.937360	636.811167	11.241562
11.016784	640.759265	11.246579
10.654599	640.566744	11.251597
10.987327	651.313732	11.256615
11.206340	667.168823	11.261632
11.240269	664.720968	11.266650
10.995515	660.316011	11.271667
11.109405	665.379017	11.276685
11.090643	656.406946	11.281703
11.218905	668.391490	11.286720
11.042967	666.879071	11.291738
11.270419	665.003650	11.296755
11.188970	657.322649	11.301773
11.282782	652.997189	11.306791
10.994461	663.753130	11.311808
11.331150	650.133705	11.316826
10.759558	650.810276	11.321843
11.245193	659.857591	11.326861
11.432161	660.573100	11.331879
11.204266	668.365763	11.336896
11.506361	668.406830	11.341914
11.031369	663.179573	11.346931
11.010610	656.704040	11.351949
11.299294	661.783839	11.356967
11.044888	670.489522	11.361984
11.475480	659.563041	11.367002
11.695810	657.411027	11.372019
11.414575	650.790117	11.377037
11.102540	644.265552	11.382055
10.989923	643.181868	11.387072
11.257160	649.296964	11.392090
11.424950	656.333353	11.397107
11.485187	659.359816	11.402125
11.453753	659.285885	11.407143
11.025369	665.273293	11.412160
11.367536	659.491973	11.417178
11.582172	665.309204	11.422195
11.319280	665.571338	11.427213
11.454929	661.501251	11.432231
11.052498	668.548093	11.437248
11.236255	659.452772	11.442266
11.170711	673.140250	11.447283
11.060988	672.034020	11.452301
11.168368	671.111523	11.457319
11.133799	675.172162	11.462336
11.231495	663.717173	11.467354
11.320423	667.237756	11.472371
11.281527	666.710561	11.477389
11.743131	676.837773	11.482407
11.391333	675.090977	11.487424
11.470308	668.404155	11.492442
11.996274	671.966716	11.497459
11.581661	678.387469	11.502477
11.076071	666.654618	11.507495
10.821843	675.218265	11.512512
11.422240	683.682727	11.517530
11.331284	692.665766	11.522547
11.535162	690.954981	11.527565
11.586963	683.944209	11.532583
11.779862	695.435807	11.537600
11.740976	698.518833	11.542618
11.780930	700.466046	11.547635
11.800098	694.438677	11.552653
12.101508	692.434901	11.557671
11.664672	697.385389	11.562688
11.733820	693.694943	11.567706
11.497991	698.560289	11.572723
11.621262	702.375298	11.577741
11.869387	691.616242	11.582759
11.758172	695.843528	11.587776
11.960846	699.743925	11.592794
11.812423	690.612273	11.597811
11.998429	690.261277	11.602829
11.605383	670.633943	11.607847
11.525526	686.677889	11.612864
11.698713	688.474838	11.617882
11.732688	692.127112	11.622899
11.465411	700.730685	11.627917
11.908503	697.483418	11.632935
11.758162	696.885322	11.637952
11.815601	694.828252	11.642970
11.587314	693.579653	11.647987
11.846534	700.567020	11.653005
11.882983	693.934188	11.658023
11.845108	699.052540	11.663040
11.892960	697.804855	11.668058
11.828801	696.975506	11.673075
11.756084	699.167588	11.678093
11.821460	697.895067	11.683111
11.438473	702.357440	11.688128
11.483870	694.912167	11.693146
11.841343	705.503833	11.698163
11.807824	704.688618	11.703181
12.219646	709.521920	11.708199
11.895846	710.506806	11.713216
12.007414	702.489431	11.718234
12.113859	703.438464	11.723251
12.078183	704.586488	11.728269
11.893448	691.834521	11.733287
11.706065	708.725307	11.738304
11.899423	712.251627	11.743322
12.097344	714.767380	11.748339
12.003302	728.642401	11.753357
12.046378	725.839655	11.758375
12.028194	729.591627	11.763392
12.432409	723.585970	11.768410
12.521877	726.027199	11.773427
12.134484	716.232389	11.778445
12.249553	699.933668	11.783463
11.862716	699.066513	11.788480
11.874942	689.411076	11.793498
12.141054	714.009834	11.798515
12.076331	716.443662	11.803533
12.135234	720.215112	11.808551
12.356240	725.895666	11.813568
12.687652	713.223759	11.818586
12.322495	703.166697	11.823603
12.228157	698.839148	11.828621
11.962166	695.687202	11.833639
11.935738	700.336704	11.838656
12.178522	713.928567	11.843674
12.190063	718.669954	11.848691
12.274439	725.100904	11.853709
12.568029	721.867590	11.858727
12.330622	729.459798	11.863744
12.146114	713.905433	11.868762
12.329724	722.832846	11.873779
12.293858	727.777322	11.878797
12.487249	719.280063	11.883815
12.602986	726.630747	11.888832
12.434917	720.269790	11.893850
12.202055	710.655898	11.898867
12.060869	721.433001	11.903885
12.692021	711.109379	11.908903
12.393027	721.210621	11.913920
12.375363	717.514837	11.918938
12.853455	721.368930	11.923955
12.393854	716.745158	11.928973
12.413088	705.245631	11.933991
12.308076	710.734265	11.939008
12.303227	718.782335	11.944026
12.583529	728.243709	11.949043
12.454003	726.165438	11.954061
12.870183	723.140133	11.959079
12.787111	715.500386	11.964096
12.168450	703.737890	11.969114
12.403243	708.112937	11.974131
12.267470	725.147130	11.979149
12.507511	722.016880	11.984167
12.384674	727.274783	11.989184
12.759962	729.576556	11.994202
12.491480	719.873566	11.999219
12.265338	729.281747	12.004237
12.694518	724.174736	12.009255
12.604618	721.222413	12.014272
12.291260	725.667570	12.019290
12.555420	720.002593	12.024307
12.580239	720.825561	12.029325
12.581725	717.912568	12.034343
12.610011	719.703821	12.039360
12.450939	723.111794	12.044378
12.459548	715.991013	12.049395
12.385946	726.785932	12.054413
12.618339	732.758193	12.059431
12.604930	753.014244	12.064448
12.370325	752.012782	12.069466
12.785340	741.492634	12.074483
12.636761	741.212995	12.079501
12.708892	747.787883	12.084519
12.979940	744.791625	12.089536
12.663303	747.892932	12.094554
13.014955	739.377178	12.099571
12.786555	750.739162	12.104589
12.585576	751.894155	12.109607
12.855307	741.065411	12.114624
12.705153	751.196998	12.119642
12.763893	747.394563	12.124659
12.453644	744.126467	12.129677
12.857982	747.913227	12.134695
12.828548	746.614532	12.139712
12.721811	746.795395	12.144730
12.563162	751.279435	12.149747
12.789503	769.569746	12.154765
13.224100	770.290642	12.159783
13.324957	764.474513	12.164800
13.058703	759.069355	12.169818
12.830964	750.742205	12.174835
12.751198	748.236413	12.179853
12.927906	753.030826	12.184871
13.242958	758.131768	12.189888
12.808433	760.588829	12.194906
13.133655	760.727259	12.199923
13.106241	768.630565	12.204941
13.217436	769.689309	12.209959
13.318939	754.468793	12.214976
12.825880	755.679016	12.219994
13.296343	747.027878	12.225011
13.190527	754.122954	12.230029
12.778351	746.481110	12.235047
13.110066	759.686690	12.240064
13.108361	758.885422	12.245082
13.533994	762.372203	12.250099
12.930330	760.974130	12.255117
13.071655	765.843518	12.260135
13.607913	765.276697	12.265152
13.497057	764.511465	12.270170
13.482108	743.852823	12.275187
13.044018	742.548729	12.280205
13.376559	743.213030	12.285223
13.146299	735.867736	12.290240
13.061629	740.393830	12.295258
13.186053	732.295533	12.300275
13.309167	752.656425	12.305293
13.323804	767.650536	12.310311
13.571199	759.211068	12.315328
13.338321	755.820395	12.320346
13.303480	744.834242	12.325363
13.285711	749.892654	12.330381
13.483346	749.139049	12.335399
13.786911	742.189793	12.340416
13.297948	748.448651	12.345434
13.566324	736.487191	12.350451
13.596303	739.805587	12.355469
13.269989	738.338813	12.360487
13.559930	736.854380	12.365504
13.275334	742.929738	12.370522
13.404829	738.570264	12.375539
13.403785	733.243481	12.380557
13.123974	743.206031	12.385575
13.573851	749.885835	12.390592
13.694644	758.873601	12.395610
13.563873	744.973896	12.400627
13.534174	750.185656	12.405645
13.477808	753.845786	12.410663
14.002390	753.994005	12.415680
13.558710	756.392540	12.420698
13.772981	745.219034	12.425715
13.741089	735.381136	12.430733
13.448802	740.823383	12.435751
13.736676	737.919165	12.440768
13.206917	746.964672	12.445786
13.651639	738.967666	12.450803
13.681192	742.282973	12.455821
13.583596	741.906983	12.460839
13.619762	744.811001	12.465856
13.531474	757.640574	12.470874
13.599036	767.586580	12.475891
13.839240	760.076044	12.480909
13.574838	765.059494	12.485927
13.742758	767.355893	12.490944
13.603249	771.145818	12.495962
13.711581	764.691046	12.500979
13.911173	767.285439	12.505997
13.812071	766.717181	12.511015
13.559613	757.425069	12.516032
13.904942	765.402515	12.521050
13.678070	766.444801	12.526067
13.648847	768.140928	12.531085
13.690993	767.200245	12.536103
13.696702	765.665669	12.541120
13.805404	771.710972	12.546138
13.910345	770.757294	12.551155
13.523500	770.754828	12.556173
13.612503	763.873895	12.561191
13.750881	757.767867	12.566208
13.515121	774.022511	12.571226
14.303569	776.726615	12.576243
14.302153	773.851938	12.581261
14.092213	774.986245	12.586279
14.497010	763.126469	12.591296
13.902840	769.430220	12.596314
13.761206	764.870225	12.601331
13.728947	758.330185	12.606349
13.597161	774.009962	12.611367
14.025672	786.477717	12.616384
13.783597	789.093977	12.621402
14.300784	783.105313	12.626419
14.220690	785.525780	12.631437
14.173369	794.587241	12.636455
14.361217	788.422959	12.641472
14.005479	791.341051	12.646490
14.416586	785.867625	12.651507
14.522347	797.584381	12.656525
14.045377	776.862391	12.661543
14.348487	768.048116	12.666560
13.940962	759.856428	12.671578
14.201356	772.833351	12.676595
14.125878	778.834931	12.681613
14.517762	785.754209	12.686631
14.501338	778.937126	12.691648
13.943496	775.161863	12.696666
14.205841	785.089984	12.701683
14.407363	789.378745	12.706701
14.326861	797.953101	12.711719
14.643110	782.938755	12.716736
14.233835	769.915799	12.721754
14.242375	762.078643	12.726771
14.103629	768.828590	12.731789
14.336442	784.214564	12.736807
14.791376	791.893983	12.741824
14.475769	785.666572	12.746842
14.124109	778.292943	12.751859
14.327081	778.614630	12.756877
14.295278	786.752161	12.761895
14.504838	784.361978	12.766912
14.819594	790.700051	12.771930
14.399719	794.606492	12.776947
14.683385	782.822487	12.781965
14.431979	781.675333	12.786983
14.478696	776.075966	12.792000
14.732346	784.601116	12.797018
14.455020	776.988623	12.802035
14.238196	774.592664	12.807053
14.185647	787.274648	12.812071
14.557188	778.070950	12.817088
14.629020	791.651787	12.822106
14.123097	787.189888	12.827123
14.169660	784.462327	12.832141
14.325619	785.479345	12.837159
14.530835	790.496519	12.842176
14.347156	792.926905	12.847194
14.400991	785.906307	12.852211
14.770915	794.245986	12.857229
14.441228	802.297652	12.862247
14.951429	816.049666	12.867264
14.480777	813.229567	12.872282
15.023015	815.019199	12.877299
14.855749	795.514142	12.882317
14.590538	802.328097	12.887335
14.544417	799.804404	12.892352
14.713941	806.370365	12.897370
14.878177	810.696532	12.902387
15.338817	799.490702	12.907405
14.807026	808.104213	12.912423
14.857462	793.358724	12.917440
14.702647	786.326636	12.922458
14.963308	793.219140	12.927475
14.981245	804.602523	12.932493
14.562750	801.903643	12.937511
14.794182	804.676089	12.942528
14.665735	806.842203	12.947546
14.694639	806.118188	12.952563
15.197592	799.342797	12.957581
14.979895	808.727606	12.962599
14.821353	806.373004	12.967616
14.728677	803.843981	12.972634
14.516603	807.108795	12.977651
14.375462	804.978685	12.982669
14.233878	811.422979	12.987687
14.921905	824.900985	12.992704
15.202889	834.501164	12.997722
14.959342	837.281764	13.002739
15.123273	828.763822	13.007757
14.964269	830.107903	13.012775
15.039873	832.942639	13.017792
15.134325	828.834788	13.022810
15.161156	832.254680	13.027827
15.165829	831.938405	13.032845
14.859048	833.472898	13.037863
14.682124	832.430835	13.042880
15.003165	835.170312	13.047898
15.141967	829.285101	13.052915
15.202174	826.605888	13.057933
15.149874	843.488259	13.062951
14.911297	830.135556	13.067968
15.379232	842.568771	13.072986
15.371129	859.901827	13.078003
15.598195	846.848541	13.083021
15.413325	846.748156	13.088039
15.513891	838.527317	13.093056
15.429547	837.060493	13.098074
15.266713	830.048578	13.103091
15.789238	828.767538	13.108109
15.387203	831.800188	13.113127
15.511809	830.388989	13.118144
15.747060	818.050811	13.123162
15.604395	824.946560	13.128179
15.509585	823.481377	13.133197
15.352500	833.803446	13.138215
15.822865	829.418945	13.143232
15.151631	835.646432	13.148250
15.188608	847.178337	13.153267
15.837356	840.765097	13.158285
15.410808	843.063129	13.163303
15.840905	840.834046	13.168320
15.705154	838.172910	13.173338
15.373068	840.768567	13.178355
15.574569	827.160721	13.183373
15.083863	839.245516	13.188391
15.041565	835.910173	13.193408
15.343240	838.299234	13.198426
15.218890	839.959779	13.203443
15.492414	845.900388	13.208461
15.612074	859.719937	13.213479
15.978287	851.993959	13.218496
16.014668	854.680209	13.223514
15.807310	850.859483	13.228531
15.717629	833.797454	13.233549
15.635909	828.792553	13.238567
15.417691	837.508426	13.243584
15.838137	849.456779	13.248602
15.632320	859.000699	13.253619
15.836619	855.601469	13.258637
15.649611	859.348362	13.263655
15.673815	860.546974	13.268672
16.110445	864.903060	13.273690
16.183180	863.866060	13.278707
15.932029	854.942924	13.283725
15.802299	869.710431	13.288743
16.190940	861.551743	13.293760
15.712969	851.578545	13.298778
15.838667	861.865791	13.303795
16.129931	851.762601	13.308813
16.059448	854.822203	13.313831
16.101256	855.197544	13.318848
15.939174	847.535407	13.323866
15.901349	849.135059	13.328883
15.921671	848.488126	13.333901
15.794966	851.013735	13.338919
15.742105	860.047695	13.343936
15.865456	855.379886	13.348954
15.732217	860.080878	13.353971
15.943461	861.587858	13.358989
15.869137	850.544711	13.364007
15.852502	861.876742	13.369024
16.236159	856.211935	13.374042
16.277481	860.762501	13.379059
16.036157	858.026385	13.384077
16.221122	862.330382	13.389095
16.106596	856.942447	13.394112
15.844148	859.079069	13.399130
15.963990	866.981436	13.404147
16.157791	867.282471	13.409165
16.054415	872.909754	13.414183
16.224436	891.938011	13.419200
16.209079	883.201980	13.424218
16.288886	879.980042	13.429235
16.425595	883.193379	13.434253
16.307638	888.299085	13.439271
16.142457	881.492647	13.444288
16.465962	881.659750	13.449306
16.461967	878.176386	13.454323
16.415786	876.839280	13.459341
16.458191	877.517488	13.464359
16.475108	885.388652	13.469376
16.889682	870.857447	13.474394
16.515665	869.319241	13.479411
16.515590	856.500353	13.484429
16.603008	848.521411	13.489447
16.771602	848.621267	13.494464
16.336795	849.064973	13.499482
16.283124	850.108528	13.504499
16.144869	854.163363	13.509517
16.282878	862.252231	13.514535
16.518784	876.157721	13.519552
17.084166	864.133862	13.524570
17.012350	874.556204	13.529587
16.233427	857.169796	13.534605
16.689465	859.872346	13.539623
16.921986	853.426486	13.544640
16.910657	848.164396	13.549658
16.500642	846.436172	13.554675
16.420774	848.831365	13.559693
16.907650	853.716064	13.564711
16.552631	848.567784	13.569728
16.644959	851.699706	13.574746
16.725638	860.829508	13.579763
16.842975	870.966590	13.584781
16.968421	871.079518	13.589799
16.278061	866.217305	13.594816
16.907986	870.120226	13.599834
16.944885	875.189043	13.604851
16.786339	871.130290	13.609869
17.161241	872.084606	13.614887
16.756758	876.376819	13.619904
16.554388	868.345443	13.624922
16.881053	867.959782	13.629939
16.802755	874.687674	13.634957
17.018907	871.507492	13.639975
16.827304	881.664582	13.644992
16.960230	871.302166	13.650010
16.841644	877.663985	13.655027
17.009096	871.076834	13.660045
16.899921	869.295160	13.665063
16.703142	875.069624	13.670080
16.828770	867.984096	13.675098
16.852895	876.816652	13.680115
16.828216	871.774399	13.685133
16.454945	874.083022	13.690151
16.644531	886.657710	13.695168
17.105747	886.481342	13.700186
17.193854	886.309785	13.705203
16.891021	890.620789	13.710221
17.702819	884.882579	13.715239
17.612107	906.400622	13.720256
17.433594	892.299998	13.725274
17.514002	882.324503	13.730291
17.277163	871.470908	13.735309
17.165217	869.677045	13.740327
16.913324	876.757187	13.745344
17.405227	877.358655	13.750362
17.197658	878.227508	13.755379
17.032803	890.204477	13.760397
17.453805	889.942892	13.765415
17.501774	902.344118	13.770432
17.288056	895.008789	13.775450
17.724929	903.584184	13.780467
17.064016	900.475143	13.785485
17.740832	883.643269	13.790503
16.926742	882.978747	13.795520
17.388830	883.196721	13.800538
17.448866	895.810648	13.805555
17.301070	898.443711	13.810573
17.733846	897.912035	13.815591
17.314959	906.236501	13.820608
17.797419	897.106882	13.825626
17.597900	904.513346	13.830643
17.447589	898.720748	13.835661
17.431379	898.309913	13.840679
17.425567	903.372806	13.845696
17.557623	901.799487	13.850714
17.547083	903.716763	13.855731
17.335602	894.897845	13.860749
17.660937	887.563267	13.865767
17.682166	890.229806	13.870784
17.604635	900.122880	13.875802
17.665781	892.362631	13.880819
17.777459	885.841019	13.885837
18.110906	885.350153	13.890855
17.967859	896.424300	13.895872
17.369656	891.765393	13.900890
17.543993	895.970076	13.905907
18.050543	886.287575	13.910925
18.008841	894.360433	13.915943
17.613615	885.472479	13.920960
18.107446	883.290209	13.925978
18.066350	882.460393	13.930995
17.836105	893.870095	13.936013
18.110966	883.475966	13.941031
17.766172	889.052717	13.946048
18.127636	882.930628	13.951066
18.392161	892.782728	13.956083
17.639632	895.851369	13.961101
17.978464	879.889811	13.966119
17.816235	886.826520	13.971136
17.885304	895.257566	13.976154
17.843766	895.314605	13.981171
17.801522	886.958328	13.986189
18.055458	891.289395	13.991207
17.955065	900.135162	13.996224
17.854708	890.752877	14.001242
18.216975	893.063023	14.006259
17.796076	904.341656	14.011277
17.988162	900.171154	14.016295
18.364167	894.867298	14.021312
18.092957	894.875115	14.026330
17.939494	887.483011	14.031347
18.079537	901.971590	14.036365
18.116067	898.595483	14.041383
18.177612	897.727493	14.046400
18.219561	911.278390	14.051418
18.564667	918.223984	14.056435
18.247018	906.032335	14.061453
18.179219	896.673348	14.066471
18.146277	909.437554	14.071488
18.329215	915.663780	14.076506
18.453116	912.034138	14.081523
18.093236	916.174204	14.086541
18.727497	916.541929	14.091559
18.396844	916.262412	14.096576
18.371848	918.472290	14.101594
18.382580	917.356639	14.106611
18.617155	924.960188	14.111629
18.770827	917.958609	14.116647
18.372305	915.019895	14.121664
18.406448	909.157367	14.126682
18.672734	915.272703	14.131699
18.365208	924.053104	14.136717
18.663909	909.334894	14.141735
18.894834	918.898780	14.146752
18.912829	919.703891	14.151770
18.581985	903.143488	14.156787
18.392067	902.027718	14.161805
18.472032	904.044424	14.166823
18.589376	918.867934	14.171840
18.512716	909.933210	14.176858
18.718072	917.667566	14.181875
18.471998	919.514450	14.186893
18.915758	917.097023	14.191911
18.840119	918.506944	14.196928
18.717806	927.621248	14.201946
18.847743	913.200878	14.206963
18.587360	913.550984	14.211981
18.695714	916.027150	14.216999
18.650290	914.670987	14.222016
18.687458	918.777246	14.227034
18.682927	911.879353	14.232051
18.622039	917.746149	14.237069
18.989742	908.546141	14.242087
18.529504	907.302309	14.247104
18.683250	910.617124	14.252122
18.928114	907.252555	14.257139
19.033728	922.257788	14.262157
18.988950	925.376491	14.267175
19.040233	932.645840	14.272192
18.938981	932.529197	14.277210
19.161573	931.635974	14.282227
19.215516	933.372735	14.287245
18.869787	924.584303	14.292263
19.192492	928.068310	14.297280
19.265916	939.963798	14.302298
19.499596	937.399401	14.307315
18.837061	919.795878	14.312333
18.973709	916.729131	14.317351
19.343677	931.191177	14.322368
18.989754	937.722435	14.327386
19.230117	923.073314	14.332403
18.902385	932.323948	14.337421
19.209259	936.501564	14.342439
19.340355	929.588726	14.347456
18.916639	934.322626	14.352474
19.310904	925.819043	14.357491
19.313329	929.570983	14.362509
19.104124	933.283499	14.367527
19.508633	925.863917	14.372544
19.489766	933.756489	14.377562
19.533290	931.556404	14.382579
19.617387	933.427298	14.387597
19.347849	934.570952	14.392615
19.223808	929.629458	14.397632
19.111120	932.948152	14.402650
19.700232	934.348596	14.407667
19.015739	937.592778	14.412685
19.456048	923.928508	14.417703
19.423025	928.096260	14.422720
19.226832	939.955095	14.427738
19.655926	947.225216	14.432755
19.724545	955.703699	14.437773
19.801141	959.548167	14.442791
20.147517	955.416595	14.447808
19.828145	930.220005	14.452826
19.779911	931.493089	14.457843
19.579982	926.689719	14.462861
19.553117	916.405962	14.467879
19.516348	923.796402	14.472896
19.357077	928.444686	14.477914
19.611257	939.554453	14.482931
19.953570	961.276117	14.487949
20.286295	952.198333	14.492967
20.099920	937.369907	14.497984
19.876438	937.597466	14.503002
20.160310	929.048061	14.508019
19.754679	927.723088	14.513037
19.571654	930.756153	14.518055
19.840427	932.970500	14.523072
19.814292	947.283179	14.528090
20.121572	944.672535	14.533107
19.921999	953.679036	14.538125
20.202436	952.426450	14.543143
20.055629	939.835622	14.548160
19.670678	939.864416	14.553178
19.884329	952.583704	14.558195
20.299278	959.527839	14.563213
20.209866	953.028241	14.568231
20.208383	943.879748	14.573248
19.937798	953.310788	14.578266
20.136492	946.393664	14.583283
20.220122	951.975894	14.588301
20.420327	944.600937	14.593319
20.471808	940.796442	14.598336
20.170625	938.593560	14.603354
20.206078	930.111479	14.608371
20.346887	926.838949	14.613389
20.354691	929.659078	14.618407
20.137062	925.653750	14.623424
19.726136	929.577753	14.628442
20.383950	943.720152	14.633459
20.038092	938.390528	14.638477
20.230267	946.221637	14.643495
20.437381	951.513117	14.648512
20.312910	951.485320	14.653530
20.569252	939.692869	14.658547
20.363816	948.037561	14.663565
19.999098	954.797736	14.668583
20.380100	938.226755	14.673600
19.955222	942.503244	14.678618
20.278190	945.037307	14.683635
20.667432	960.468354	14.688653
20.883374	958.995497	14.693671
20.694180	955.998731	14.698688
20.331817	950.788455	14.703706
20.530646	951.290677	14.708723
20.810876	963.485140	14.713741
20.753370	963.866577	14.718759
20.953028	952.461700	14.723776
21.199091	957.384158	14.728794
21.187419	945.974526	14.733811
20.877328	939.799845	14.738829
20.524904	938.630638	14.743847
20.550386	940.264561	14.748864
20.613208	947.951835	14.753882
20.491297	940.242337	14.758899
20.398595	942.245075	14.763917
20.581902	955.852753	14.768935
20.750641	957.590465	14.773952
20.848443	971.561850	14.778970
21.194563	958.549790	14.783987
21.090028	968.200978	14.789005
21.215239	973.915556	14.794023
21.292355	965.613125	14.799040
20.738318	963.585558	14.804058
20.920022	957.333818	14.809075
21.112535	973.032386	14.814093
20.763422	976.132508	14.819111
20.953235	964.981632	14.824128
21.125598	975.918046	14.829146
21.342045	965.321581	14.834163
21.291020	964.701602	14.839181
20.758454	960.950741	14.844199
21.292350	966.430869	14.849216
21.159382	970.797329	14.854234
21.177468	964.372404	14.859251
21.542154	972.321664	14.864269
21.120288	966.723070	14.869287
21.313683	966.778015	14.874304
21.207229	969.373052	14.879322
21.420094	961.241859	14.884339
21.547869	970.159209	14.889357
20.913317	974.957713	14.894375
21.519430	969.702989	14.899392
21.539480	966.398879	14.904410
21.361288	967.878522	14.909427
21.704864	958.461360	14.914445
21.427072	966.069464	14.919463
21.505587	974.407548	14.924480
21.367238	974.157861	14.929498
21.080233	970.718821	14.934515
20.941277	965.063278	14.939533
20.937033	966.563004	14.944551
21.339096	965.752113	14.949568
21.167581	974.381839	14.954586
21.533999	981.431418	14.959603
21.808305	988.388133	14.964621
21.409506	988.769395	14.969639
21.350308	982.495429	14.974656
21.597875	991.460293	14.979674
21.752336	985.660940	14.984691
21.830316	984.815618	14.989709
21.588037	990.597248	14.994727
21.990916	985.166077	14.999744
21.851180	992.389639	15.004762
21.822802	994.742070	15.009779
21.976356	992.038739	15.014797
21.832270	995.147767	15.019815
22.082073	988.105852	15.024832
22.168394	984.463149	15.029850
22.014520	995.826235	15.034867
21.992979	982.369984	15.039885
21.800002	991.422808	15.044903
22.152998	985.592348	15.049920
21.801950	1000.246315	15.054938
21.987804	1003.423571	15.059955
21.965714	994.909449	15.064973
21.974368	999.231636	15.069991
22.160614	993.509352	15.075008
21.664322	991.529540	15.080026
21.700640	995.841081	15.085043
22.176015	981.252922	15.090061
22.162895	996.873276	15.095079
22.092930	986.933906	15.100096
22.485029	978.077183	15.105114
22.596785	988.704361	15.110131
22.282773	988.444326	15.115149
22.200847	993.241457	15.120167
22.403018	983.862216	15.125184
22.355233	983.809781	15.130202
22.006444	993.944225	15.135219
22.265815	983.574555	15.140237
21.976051	988.000301	15.145255
22.311471	971.830911	15.150272
22.264048	987.926851	15.155290
22.078507	988.940582	15.160307
22.573318	994.644596	15.165325
22.595700	1004.828190	15.170343
22.470438	1002.963815	15.175360
22.466342	1000.537652	15.180378
22.548726	1020.144672	15.185395
22.740376	1002.334649	15.190413
22.201318	1006.433381	15.195431
22.317208	1013.490666	15.200448
22.859787	1010.798965	15.205466
22.732129	1015.436007	15.210483
22.469301	1005.072403	15.215501
22.197683	1012.505987	15.220519
22.717881	1009.082480	15.225536
22.828179	1007.462068	15.230554
22.623219	1010.577479	15.235571
22.740715	1010.366602	15.240589
22.823782	1011.309846	15.245607
22.819582	1014.002479	15.250624
22.688205	1012.407308	15.255642
22.884333	1008.065732	15.260659
22.850770	1003.062704	15.265677
22.829944	1009.320889	15.270695
23.163471	1007.618163	15.275712
22.812375	1001.434106	15.280730
23.058082	1000.026011	15.285747
23.070648	1006.348392	15.290765
22.784001	1008.170082	15.295783
22.793532	1004.545718	15.300800
23.484462	994.979438	15.305818
23.135248	998.272086	15.310835
23.121775	1007.549261	15.315853
23.196991	1006.467682	15.320871
23.483369	996.548216	15.325888
23.109755	1003.363453	15.330906
23.226614	1000.795259	15.335923
23.329808	1000.567688	15.340941
23.211781	1006.658062	15.345959
23.410301	1000.738191	15.350976
23.471345	996.603978	15.355994
23.022716	992.839958	15.361011
23.528105	995.758862	15.366029
23.440192	995.229870	15.371047
23.154089	1000.447161	15.376064
23.159761	998.133078	15.381082
23.003387	1004.882719	15.386099
23.149617	1007.005821	15.391117
23.171152	1005.216277	15.396135
23.401979	1016.055192	15.401152
23.575670	1014.087171	15.406170
23.165779	1030.662824	15.411187
23.674012	1024.479822	15.416205
23.859833	1033.492252	15.421223
23.522398	1023.904042	15.426240
23.535503	1029.790840	15.431258
23.747820	1028.741429	15.436275
23.774723	1017.496123	15.441293
23.801137	1019.189868	15.446311
23.795160	1017.534023	15.451328
23.844060	1004.584277	15.456346
23.701777	1004.937972	15.461363
23.797030	1002.654034	15.466381
23.550796	991.776590	15.471399
23.740391	1011.609804	15.476416
23.760490	1017.391359	15.481434
23.697354	1026.468039	15.486451
24.018275	1023.284038	15.491469
23.851382	1028.432166	15.496487
23.844175	1029.023477	15.501504
24.008524	1019.684858	15.506522
23.955147	1019.068402	15.511539
23.988072	1022.263310	15.516557
23.905420	1024.879873	15.521575
24.053529	1029.012957	15.526592
23.846725	1022.998792	15.531610
23.431482	1021.870980	15.536627
24.050448	1022.537754	15.541645
23.836345	1024.288119	15.546663
23.638748	1030.829632	15.551680
23.910170	1031.601353	15.556698
23.700917	1046.930583	15.561715
23.903846	1043.727196	15.566733
24.333534	1034.025100	15.571751
24.283172	1050.232011	15.576768
24.774199	1040.447716	15.581786
24.314035	1044.796031	15.586803
24.317531	1044.057052	15.591821
24.371078	1046.800603	15.596839
24.373303	1038.992717	15.601856
24.837313	1036.897154	15.606874
24.606266	1042.632859	15.611891
24.513706	1024.270888	15.616909
24.357399	1027.896239	15.621927
24.001565	1032.464893	15.626944
24.227178	1031.309255	15.631962
24.285895	1038.236651	15.636979
24.273328	1038.440633	15.641997
24.788946	1040.985552	15.647015
24.297586	1042.157656	15.652032
24.692674	1035.875611	15.657050
24.376173	1047.848043	15.662067
24.548899	1042.901046	15.667085
24.626691	1039.657304	15.672103
24.358002	1041.226872	15.677120
24.877419	1037.456339	15.682138
24.240655	1044.091912	15.687155
24.672578	1049.998304	15.692173
25.074255	1054.034861	15.697191
24.936425	1061.283399	15.702208
25.045994	1061.979493	15.707226
25.154854	1065.799994	15.712243
25.241556	1054.775673	15.717261
24.796714	1035.099246	15.722279
24.767157	1035.965462	15.727296
25.089870	1045.859023	15.732314
25.000472	1051.714550	15.737331
25.012383	1054.436223	15.742349
25.243079	1050.805600	15.747367
25.088180	1058.233539	15.752384
25.480265	1052.194959	15.757402
24.831199	1046.909653	15.762419
24.824379	1039.036911	15.767437
25.251649	1050.406810	15.772455
25.045464	1058.104721	15.777472
25.244024	1054.457040	15.782490
25.516800	1061.281478	15.787507
25.372426	1054.067764	15.792525
25.668928	1054.447386	15.797543
25.241161	1046.965648	15.802560
25.162593	1040.558994	15.807578
24.965314	1055.217316	15.812595
25.535993	1054.862849	15.817613
25.827166	1058.212964	15.822631
25.430144	1066.341572	15.827648
25.677921	1049.478932	15.832666
25.509501	1047.640249	15.837683
25.475179	1033.261298	15.842701
25.585421	1030.047188	15.847719
25.086531	1039.867500	15.852736
25.394980	1044.972715	15.857754
25.477253	1058.612082	15.862771
25.621404	1050.586291	15.867789
25.631834	1063.744604	15.872807
25.662757	1062.827755	15.877824
25.841767	1057.488444	15.882842
25.823040	1067.236695	15.887859
25.440707	1063.714741	15.892877
25.971557	1059.510060	15.897895
25.677643	1055.137953	15.902912
25.870720	1050.926235	15.907930
25.587812	1052.094083	15.912947
25.458331	1058.236763	15.917965
25.574229	1053.749954	15.922983
25.625975	1058.175859	15.928000
25.712001	1052.134738	15.933018
25.749782	1065.907315	15.938035
25.937285	1079.037897	15.943053
26.424401	1065.763823	15.948071
26.308833	1072.914202	15.953088
26.092350	1059.769307	15.958106
26.006164	1058.772975	15.963123
25.798204	1059.124338	15.968141
26.290081	1067.085271	15.973159
26.000427	1086.015340	15.978176
26.208118	1081.195400	15.983194
26.107435	1079.933091	15.988211
26.218378	1084.075168	15.993229
26.214879	1075.968356	15.998247
26.287276	1086.292485	16.003264
26.210592	1075.476790	16.008282
26.204341	1077.358698	16.013299
26.217336	1083.251842	16.018317
26.866519	1087.148640	16.023335
26.513482	1081.416147	16.028352
26.416238	1079.042437	16.033370
26.581624	1077.457569	16.038387
26.229850	1087.567287	16.043405
26.247479	1077.999157	16.048423
26.438241	1090.804183	16.053440
26.197067	1073.219697	16.058458
26.175561	1074.643240	16.063475
25.970205	1084.950925	16.068493
26.342741	1095.158606	16.073511
26.246358	1101.315050	16.078528
26.710332	1106.774619	16.083546
26.969294	1101.719419	16.088563
26.849173	1102.382073	16.093581
27.044856	1106.416202	16.098599
26.669433	1118.969124	16.103616
26.700778	1112.725108	16.108634
27.205301	1100.524431	16.113651
27.264319	1101.938515	16.118669
26.953533	1100.339888	16.123687
26.717067	1092.985950	16.128704
26.844784	1097.753417	16.133722
26.867880	1101.170790	16.138739
26.536975	1104.356445	16.143757
26.916143	1090.196689	16.148775
27.079881	1100.026825	16.153792
26.883380	1103.942517	16.158810
26.745303	1097.800791	16.163827
27.221127	1089.814536	16.168845
27.246332	1091.577907	16.173863
26.889342	1096.099420	16.178880
26.668792	1087.669997	16.183898
27.386628	1106.334937	16.188915
27.424591	1112.697558	16.193933
27.378707	1109.053452	16.198951
27.032498	1092.012433	16.203968
27.275354	1106.141081	16.208986
27.738377	1109.451658	16.214003
27.505286	1108.159598	16.219021
27.399890	1087.489482	16.224039
27.075110	1088.673359	16.229056
27.453019	1110.566357	16.234074
27.660638	1105.465550	16.239091
27.644323	1113.379893	16.244109
27.904951	1105.850233	16.249127
27.213531	1087.007660	16.254144
26.920182	1101.580084	16.259162
27.805109	1101.312082	16.264179
27.845372	1113.755690	16.269197
27.413731	1109.951113	16.274215
27.780289	1119.948301	16.279232
27.734668	1115.351081	16.284250
27.655906	1107.407528	16.289267
27.940399	1117.717380	16.294285
27.829907	1116.207292	16.299303
27.685117	1112.812215	16.304320
27.956350	1112.690860	16.309338
27.928330	1118.170712	16.314355
27.703374	1112.143582	16.319373
27.926800	1108.321578	16.324391
27.738022	1110.244711	16.329408
27.843946	1105.418619	16.334426
28.031622	1107.525771	16.339443
27.897224	1116.452713	16.344461
28.222828	1109.468303	16.349479
28.195898	1103.798320	16.354496
28.165109	1106.914862	16.359514
28.133927	1099.068002	16.364531
28.009408	1107.245452	16.369549
28.292653	1099.548147	16.374567
28.170637	1102.076212	16.379584
28.345198	1092.824319	16.384602
28.104312	1090.889687	16.389619
28.182562	1100.831049	16.394637
28.601903	1097.104586	16.399655
28.588464	1096.276739	16.404672
28.000627	1103.709412	16.409690
28.115497	1096.369854	16.414707
27.993665	1122.879294	16.419725
28.221327	1110.371687	16.424743
28.465702	1120.397487	16.429760
28.507523	1123.531058	16.434778
28.825124	1125.292802	16.439795
28.616357	1130.456988	16.444813
28.853226	1126.875876	16.449831
28.761964	1122.146947	16.454848
28.539075	1127.575281	16.459866
28.900910	1122.459775	16.464883
28.746641	1123.923058	16.469901
28.643802	1117.999871	16.474919
28.873627	1118.254240	16.479936
28.714956	1117.843629	16.484954
28.721387	1117.429242	16.489971
28.646650	1127.918462	16.494989
28.635028	1123.883969	16.500007
28.899235	1118.594407	16.505024
28.767622	1126.435301	16.510042
28.827217	1123.920244	16.515059
29.163616	1124.397761	16.520077
28.875577	1119.800651	16.525095
29.226708	1119.436400	16.530112
28.828458	1127.016106	16.535130
29.265364	1118.919169	16.540147
28.896900	1132.496667	16.545165
28.929664	1118.075577	16.550183
28.838556	1112.396711	16.555200
28.809071	1140.457017	16.560218
29.210309	1138.339719	16.565235
28.996969	1139.619751	16.570253
29.440563	1149.330326	16.575271
29.242457	1142.781415	16.580288
29.432862	1151.180948	16.585306
29.590770	1141.704417	16.590323
29.506146	1143.775340	16.595341
29.340571	1138.376383	16.600359
29.377411	1144.423604	16.605376
29.512516	1143.815483	16.610394
29.449930	1135.342353	16.615411
29.255550	1143.341414	16.620429
29.527921	1146.931182	16.625447
29.786264	1142.052796	16.630464
29.412116	1139.444747	16.635482
29.706124	1139.272485	16.640499
29.668350	1141.194054	16.645517
29.796769	1136.017283	16.650535
29.930688	1134.579354	16.655552
29.907923	1134.033838	16.660570
30.187991	1137.180578	16.665587
29.866370	1133.320887	16.670605
29.659409	1137.004690	16.675623
29.896984	1131.801351	16.680640
29.831799	1131.944148	16.685658
29.950469	1131.742553	16.690675
29.722014	1138.475136	16.695693
29.683230	1141.561378	16.700711
29.865728	1132.671146	16.705728
29.716080	1146.463684	16.710746
30.085741	1157.523935	16.715763
30.380005	1159.832149	16.720781
30.085226	1163.797966	16.725799
30.402487	1156.208918	16.730816
30.238992	1161.599554	16.735834
30.388373	1154.866805	16.740851
30.364754	1156.457946	16.745869
30.435035	1159.912120	16.750887
30.480356	1163.947729	16.755904
30.472092	1157.681501	16.760922
30.367824	1140.943362	16.765939
30.084795	1140.205089	16.770957
30.202321	1139.943712	16.775975
30.442242	1154.183313	16.780992
30.344903	1146.656072	16.786010
30.711914	1138.456466	16.791027
30.249832	1152.806056	16.796045
29.988993	1153.822126	16.801063
30.246589	1154.498187	16.806080
30.237697	1152.905903	16.811098
30.257814	1160.360113	16.816115
30.277907	1173.416006	16.821133
30.574116	1166.922184	16.826151
30.518476	1169.547159	16.831168
30.449841	1172.104741	16.836186
30.610709	1169.952516	16.841203
30.799664	1171.002257	16.846221
30.639595	1177.014068	16.851239
30.923852	1178.194049	16.856256
30.580017	1181.807786	16.861274
30.842266	1191.761396	16.866291
30.768063	1194.774300	16.871309
30.999898	1199.557041	16.876327
31.199546	1203.786235	16.881344
30.975098	1209.763962	16.886362
31.297954	1208.286957	16.891379
30.895119	1205.806472	16.896397
30.923482	1205.098305	16.901415
31.353669	1196.992918	16.906432
31.508608	1195.807317	16.911450
31.665581	1191.834758	16.916467
31.770550	1197.252771	16.921485
31.449730	1191.142801	16.926503
31.544243	1171.763578	16.931520
31.464626	1174.070411	16.936538
31.169518	1162.888089	16.941555
31.367366	1174.773707	16.946573
31.448620	1188.747855	16.951591
31.673258	1188.917829	16.956608
31.401802	1190.232217	16.961626
31.550954	1186.737422	16.966643
31.471959	1195.917661	16.971661
32.034286	1181.975294	16.976679
31.809365	1183.342352	16.981696
31.775782	1196.103707	16.986714
31.665110	1196.872184	16.991731
31.821349	1187.105549	16.996749
31.761193	1189.576597	17.001767
32.236767	1183.184058	17.006784
31.351631	1179.463142	17.011802
31.665486	1182.320567	17.016819
31.700423	1186.834346	17.021837
31.579294	1184.808354	17.026855
31.972842	1186.974781	17.031872
31.549952	1182.525018	17.036890
31.873163	1191.446573	17.041907
32.058385	1182.451745	17.046925
31.933602	1188.587423	17.051943
31.804412	1192.858669	17.056960
31.739752	1203.911257	17.061978
32.152784	1214.100037	17.066995
32.129972	1207.028165	17.072013
32.246463	1210.333094	17.077031
32.064074	1211.642996	17.082048
32.096073	1210.072703	17.087066
32.169433	1206.302594	17.092083
32.251050	1208.871355	17.097101
32.124877	1209.030020	17.102119
32.240169	1203.413463	17.107136
32.483831	1209.535603	17.112154
32.321219	1215.292199	17.117171
32.410741	1219.352454	17.122189
32.390970	1235.245465	17.127207
32.901618	1231.968584	17.132224
32.551090	1229.738682	17.137242
33.007634	1232.362315	17.142259
32.698363	1215.965502	17.147277
32.352810	1212.971099	17.152295
32.524093	1218.186220	17.157312
32.695956	1224.802464	17.162330
32.785780	1230.607878	17.167347
32.875586	1227.908189	17.172365
32.950684	1237.534532	17.177383
33.142843	1221.715575	17.182400
32.862482	1228.450012	17.187418
33.062746	1226.749211	17.192435
33.463916	1224.571952	17.197453
33.018607	1228.858021	17.202471
33.100609	1226.812822	17.207488
33.083867	1237.075264	17.212506
33.288370	1228.607581	17.217523
33.320140	1214.464287	17.222541
32.777474	1212.690535	17.227559
33.388477	1214.393695	17.232576
33.469273	1219.032844	17.237594
33.305830	1213.848129	17.242611
33.490194	1201.871118	17.247629
33.506993	1206.779073	17.252647
33.422836	1197.447738	17.257664
33.272699	1194.271239	17.262682
33.301500	1189.911653	17.267699
33.375389	1197.685665	17.272717
33.272618	1209.135557	17.277735
33.807955	1208.600429	17.282752
33.819294	1219.088840	17.287770
33.443764	1217.733880	17.292787
33.463210	1213.716590	17.297805
33.186810	1221.924201	17.302823
33.490464	1215.501781	17.307840
33.321411	1225.166371	17.312858
33.736894	1225.760892	17.317875
33.721364	1210.959120	17.322893
33.524060	1225.011655	17.327911
33.947992	1215.758498	17.332928
33.794664	1226.225375	17.337946
34.005833	1233.046908	17.342963
33.681267	1222.888515	17.347981
33.844802	1228.436221	17.352999
34.126091	1242.394849	17.358016
34.339626	1244.699943	17.363034
33.991078	1240.213270	17.368051
34.332998	1236.076021	17.373069
34.255988	1229.107308	17.378087
34.225505	1226.697871	17.383104
34.219138	1223.685038	17.388122
34.049713	1220.637792	17.393139
34.282090	1230.324698	17.398157
34.374760	1244.751549	17.403175
34.094391	1236.546029	17.408192
34.177206	1240.137113	17.413210
34.094480	1243.747823	17.418227
34.460145	1238.896778	17.423245
34.227276	1246.330700	17.428263
34.108113	1242.505538	17.433280
34.287699	1251.193999	17.438298
34.008812	1248.782452	17.443315
34.927546	1257.430849	17.448333
34.992968	1268.043363	17.453351
34.793397	1255.441643	17.458368
34.550935	1254.722256	17.463386
34.899371	1249.514136	17.468403
34.877161	1238.459427	17.473421
34.890277	1244.753404	17.478439
34.884748	1236.646837	17.483456
34.915311	1244.784272	17.488474
34.695194	1248.498562	17.493491
34.960493	1255.567250	17.498509
34.995778	1262.589925	17.503527
35.108395	1268.521172	17.508544
35.085486	1262.282448	17.513562
35.354351	1264.995453	17.518579
35.632655	1259.940334	17.523597
35.251975	1239.401537	17.528615
35.170247	1236.744501	17.533632
35.173612	1235.626829	17.538650
35.021508	1234.031729	17.543667
35.307855	1227.627796	17.548685
35.246775	1235.789054	17.553703
35.429500	1242.473032	17.558720
35.510049	1243.978431	17.563738
35.014777	1249.073928	17.568755
35.438808	1254.366228	17.573773
35.162199	1264.054003	17.578791
35.212380	1263.285609	17.583808
35.409782	1258.344154	17.588826
35.347791	1258.502232	17.593843
35.581968	1253.274142	17.598861
35.345987	1257.956622	17.603879
35.074256	1251.696925	17.608896
35.578585	1271.963967	17.613914
35.998803	1281.255388	17.618931
35.995455	1270.068312	17.623949
35.473172	1275.572003	17.628967
35.745583	1283.157153	17.633984
35.741727	1271.490460	17.639002
36.090375	1283.377771	17.644019
36.519360	1281.757897	17.649037
36.092614	1289.058106	17.654055
36.037675	1282.587701	17.659072
36.178363	1281.290715	17.664090
36.018450	1276.515695	17.669107
36.095689	1275.029830	17.674125
36.075847	1272.909062	17.679143
35.800115	1284.900511	17.684160
36.512375	1274.844735	17.689178
35.942364	1285.664118	17.694195
36.199580	1275.155758	17.699213
36.142950	1277.619953	17.704231
35.873146	1267.288848	17.709248
36.423709	1274.338095	17.714266
36.361951	1278.087542	17.719283
36.247979	1271.781029	17.724301
36.636760	1293.325401	17.729319
36.731766	1299.451927	17.734336
36.902080	1295.505658	17.739354
36.704163	1285.999590	17.744371
36.484230	1270.974167	17.749389
36.983195	1290.443631	17.754407
36.716090	1300.770583	17.759424
36.888414	1291.736694	17.764442
36.780594	1285.299821	17.769459
36.682125	1289.635707	17.774477
36.815418	1286.042388	17.779495
36.624008	1306.027146	17.784512
36.928628	1305.584969	17.789530
36.699844	1303.774653	17.794547
36.813847	1303.305536	17.799565
36.903546	1303.597642	17.804583
36.885565	1305.658143	17.809600
37.002888	1301.537132	17.814618
37.017520	1301.809441	17.819635
37.066848	1308.940391	17.824653
36.903596	1301.871549	17.829671
37.187276	1324.514898	17.834688
37.704230	1324.029986	17.839706
37.247124	1328.608269	17.844723
37.614665	1321.939109	17.849741
37.575664	1325.669221	17.854759
37.415142	1332.577431	17.859776
37.698970	1332.498284	17.864794
37.422230	1326.422388	17.869811
37.497220	1311.492738	17.874829
37.751245	1315.700816	17.879847
37.346528	1325.285615	17.884864
37.466176	1315.448902	17.889882
37.623293	1328.284617	17.894899
37.742098	1319.066591	17.899917
37.843878	1310.577093	17.904935
37.594199	1318.300864	17.909952
37.764377	1312.278031	17.914970
37.873743	1320.229580	17.919987
37.957463	1315.394286	17.925005
37.873372	1315.536891	17.930023
37.726664	1316.815963	17.935040
38.001886	1320.493686	17.940058
38.100803	1317.729437	17.945075
37.978940	1314.387536	17.950093
38.065976	1309.327655	17.955111
37.641580	1318.328537	17.960128
37.821740	1324.167167	17.965146
38.075278	1340.882166	17.970163
38.302599	1344.460099	17.975181
38.418585	1340.878948	17.980199
37.962552	1332.628321	17.985216
38.239536	1326.374147	17.990234
38.413344	1336.802457	17.995251
38.389946	1333.890107	18.000269
38.851850	1337.781589	18.005287
38.475974	1337.098881	18.010304
38.882822	1331.704855	18.015322
38.789456	1335.446643	18.020339
38.449734	1334.010322	18.025357
38.930760	1318.881344	18.030375
38.730118	1337.037162	18.035392
38.850678	1323.454244	18.040410
38.665750	1322.141998	18.045427
38.827311	1332.928842	18.050445
38.917028	1332.119536	18.055463
39.035026	1332.631278	18.060480
38.957347	1327.212180	18.065498
38.519534	1328.227584	18.070515
38.714698	1335.244174	18.075533
38.760557	1343.761122	18.080551
38.708252	1352.526992	18.085568
39.022870	1349.182971	18.090586
39.389477	1355.708790	18.095603
39.374620	1357.929758	18.100621
39.563637	1346.270668	18.105639
39.507256	1360.411687	18.110656
39.601157	1354.438661	18.115674
39.752107	1348.428296	18.120691
39.445265	1356.413512	18.125709
39.573560	1358.974981	18.130727
39.558807	1348.171509	18.135744
39.598885	1357.143820	18.140762
39.346419	1348.009195	18.145779
39.149030	1356.879852	18.150797
39.459622	1354.754641	18.155815
39.295948	1360.060155	18.160832
39.716699	1348.437342	18.165850
39.698020	1359.154608	18.170867
39.636556	1358.043930	18.175885
39.839749	1365.239160	18.180903
39.804862	1383.381677	18.185920
39.840036	1371.191235	18.190938
39.909637	1380.925818	18.195955
39.654974	1386.438107	18.200973
39.880434	1380.283508	18.205991
39.952930	1385.081797	18.211008
39.984848	1376.839906	18.216026
40.130761	1373.001588	18.221043
39.956306	1379.148269	18.226061
39.799848	1374.934433	18.231079
40.147144	1380.996212	18.236096
40.075919	1376.551264	18.241114
40.390005	1390.296580	18.246131
40.163366	1402.343535	18.251149
40.450189	1402.263919	18.256167
40.674058	1398.653231	18.261184
40.470693	1388.715602	18.266202
40.563321	1392.765943	18.271219
40.709308	1393.263834	18.276237
41.269851	1392.768935	18.281255
40.604622	1381.041685	18.286272
40.666894	1374.675963	18.291290
40.477971	1370.457748	18.296307
40.713329	1388.295988	18.301325
41.026053	1388.960265	18.306343
40.850924	1389.192877	18.311360
41.095839	1384.073524	18.316378
41.162658	1388.266768	18.321395
40.736676	1388.036892	18.326413
40.866566	1391.254545	18.331431
40.650493	1393.273506	18.336448
41.008938	1397.121249	18.341466
41.052263	1395.328252	18.346483
41.317352	1392.582139	18.351501
40.844122	1386.884158	18.356519
40.939150	1399.590793	18.361536
41.180233	1386.329783	18.366554
41.002651	1389.119067	18.371571
41.207913	1403.285401	18.376589
40.990344	1406.374453	18.381607
41.042773	1417.560312	18.386624
41.471834	1409.401355	18.391642
41.195760	1410.741730	18.396659
40.949795	1413.592227	18.401677
41.438720	1414.932668	18.406695
41.692766	1429.148185	18.411712
41.850781	1429.514799	18.416730
41.937720	1432.770749	18.421747
41.730971	1429.811368	18.426765
42.003540	1431.116279	18.431783
42.098176	1423.034960	18.436800
41.831962	1422.808455	18.441818
42.299809	1420.813238	18.446835
41.972183	1413.328277	18.451853
41.998948	1408.558688	18.456871
42.148312	1410.207960	18.461888
42.101305	1419.910340	18.466906
42.256148	1411.245217	18.471923
41.929534	1417.968036	18.476941
42.141347	1420.958257	18.481959
42.331076	1428.600607	18.486976
42.446915	1428.522533	18.491994
42.529286	1439.419682	18.497011
42.385403	1434.828307	18.502029
42.498220	1431.181361	18.507047
42.312065	1436.802857	18.512064
42.480806	1438.575332	18.517082
42.676805	1440.725403	18.522099
42.323057	1439.559524	18.527117
42.643153	1425.058452	18.532135
42.569728	1427.575794	18.537152
42.701944	1432.550938	18.542170
43.140407	1433.151334	18.547187
42.879557	1442.912478	18.552205
42.832883	1429.519790	18.557223
42.883490	1431.960892	18.562240
42.804863	1429.716767	18.567258
43.365950	1429.852966	18.572275
42.731620	1430.646691	18.577293
43.161858	1425.482511	18.582311
43.173092	1431.054143	18.587328
42.994482	1425.641360	18.592346
42.969579	1420.826213	18.597363
42.855490	1428.841224	18.602381
42.944903	1429.925513	18.607399
43.253209	1433.026855	18.612416
43.044614	1439.522900	18.617434
43.482985	1438.813604	18.622451
43.277310	1451.431684	18.627469
43.440867	1446.271410	18.632487
43.344720	1455.571239	18.637504
43.429077	1453.737092	18.642522
43.560829	1450.885624	18.647539
43.628299	1458.689159	18.652557
43.744708	1447.006664	18.657575
43.724392	1457.367627	18.662592
43.517547	1443.488763	18.667610
43.872288	1435.956844	18.672627
43.579262	1453.890560	18.677645
43.700520	1444.258658	18.682663
43.562043	1456.834655	18.687680
43.684325	1457.970603	18.692698
44.095631	1460.557175	18.697715
43.933055	1470.921498	18.702733
44.002268	1472.889459	18.707751
44.272426	1476.034656	18.712768
44.080345	1467.442796	18.717786
44.192717	1466.399552	18.722803
43.917681	1468.430916	18.727821
44.487334	1468.105008	18.732839
44.460279	1465.669754	18.737856
44.340482	1468.011323	18.742874
44.539579	1468.671315	18.747891
44.431287	1469.149085	18.752909
44.329103	1471.509987	18.757927
44.779257	1468.173112	18.762944
44.090136	1474.728679	18.767962
44.558948	1481.494161	18.772979
44.498234	1491.053554	18.777997
45.066068	1486.893476	18.783015
45.066047	1495.537610	18.788032
44.928591	1490.904187	18.793050
45.168944	1485.094371	18.798067
45.195462	1499.617003	18.803085
45.023489	1471.313208	18.808103
44.988281	1465.533949	18.813120
44.869339	1472.145353	18.818138
45.312875	1486.533207	18.823155
45.247212	1492.962695	18.828173
44.714151	1491.348361	18.833191
45.044532	1490.034263	18.838208
45.576585	1490.367524	18.843226
45.130801	1488.281906	18.848243
45.663616	1490.082554	18.853261
45.280017	1498.196629	18.858279
45.389836	1483.248755	18.863296
45.414491	1486.331429	18.868314
45.644339	1492.348529	18.873331
45.586045	1491.300464	18.878349
45.310090	1485.981813	18.883367
45.487747	1487.655062	18.888384
45.105150	1488.854335	18.893402
45.632571	1496.529016	18.898419
45.644114	1508.747016	18.903437
45.552235	1515.486745	18.908455
45.875110	1509.323151	18.913472
45.423253	1514.683331	18.918490
45.999803	1508.476837	18.923507
46.205541	1515.081570	18.928525
45.858342	1511.055383	18.933543
45.966371	1506.951561	18.938560
45.905985	1507.311369	18.943578
45.713470	1499.158237	18.948595
46.136364	1520.230461	18.953613
46.044994	1534.497025	18.958631
46.440901	1534.141531	18.963648
46.493213	1532.747917	18.968666
46.514674	1529.613902	18.973683
46.366486	1529.567727	18.978701
46.549247	1530.435417	18.983719
46.676811	1534.682297	18.988736
46.586543	1530.723152	18.993754
46.578558	1529.023391	18.998771
46.630636	1524.252962	19.003789
46.629632	1525.894244	19.008807
46.868915	1522.227465	19.013824
46.717652	1524.485605	19.018842
46.426829	1520.917662	19.023859
46.876154	1526.297603	19.028877
46.766796	1525.061868	19.033895
46.944996	1537.402106	19.038912
47.140070	1546.110376	19.043930
47.484239	1527.269189	19.048947
47.391178	1542.353412	19.053965
47.126440	1538.945487	19.058983
47.288711	1542.558899	19.064000
46.896137	1545.975208	19.069018
47.082111	1541.272162	19.074035
47.535693	1533.655285	19.079053
47.310115	1538.651802	19.084071
47.508378	1536.926037	19.089088
47.334910	1540.017670	19.094106
47.621112	1541.415131	19.099123
47.603938	1552.539394	19.104141
47.389848	1537.121493	19.109159
47.998735	1535.031580	19.114176
47.589682	1543.635678	19.119194
47.731901	1535.234416	19.124211
47.930031	1533.988375	19.129229
47.649116	1547.126418	19.134247
48.014969	1548.359915	19.139264
47.913612	1568.286672	19.144282
48.049514	1565.257804	19.149299
47.882920	1567.417361	19.154317
47.671674	1571.089300	19.159335
47.871184	1562.170942	19.164352
48.318611	1566.440301	19.169370
48.366074	1561.288715	19.174387
48.420980	1558.338812	19.179405
48.164740	1555.447127	19.184423
48.655515	1556.115075	19.189440
47.930588	1559.491936	19.194458
48.553532	1573.722358	19.199475
48.673450	1574.893399	19.204493
48.750798	1587.296811	19.209511
48.874007	1574.196148	19.214528
48.730311	1569.434288	19.219546
48.982116	1565.295303	19.224563
48.607210	1563.700366	19.229581
48.599620	1574.453895	19.234599
48.699277	1574.706574	19.239616
48.968559	1580.897415	19.244634
49.091103	1568.273409	19.249651
49.103369	1583.530520	19.254669
48.879639	1582.476810	19.259687
49.572338	1571.909515	19.264704
49.575422	1577.337296	19.269722
49.309389	1572.881793	19.274739
49.593338	1579.859322	19.279757
49.424342	1566.526723	19.284775
49.477603	1557.255724	19.289792
49.345776	1552.037553	19.294810
49.384405	1563.058401	19.299827
49.598403	1576.860570	19.304845
49.587270	1576.758206	19.309863
49.929565	1573.419276	19.314880
49.427397	1570.016985	19.319898
49.754789	1573.415176	19.324915
50.148489	1570.440593	19.329933
49.458627	1572.458063	19.334951
49.893597	1563.840499	19.339968
49.589078	1571.421487	19.344986
49.656970	1570.268436	19.350003
50.061027	1564.309865	19.355021
49.908866	1574.552690	19.360039
49.668122	1570.143721	19.365056
49.900668	1571.843094	19.370074
49.715599	1569.082273	19.375091
50.331826	1585.223103	19.380109
50.038538	1594.263544	19.385127
50.396249	1591.496577	19.390144
50.036676	1588.494839	19.395162
50.346228	1593.398060	19.400179
50.345421	1591.867589	19.405197
50.193479	1599.109088	19.410215
50.392259	1588.451904	19.415232
50.208517	1588.161979	19.420250
50.310223	1606.535798	19.425267
50.485930	1604.643140	19.430285
50.365418	1614.603306	19.435303
50.869182	1607.461397	19.440320
50.846014	1620.959916	19.445338
50.883285	1605.647748	19.450355
50.835880	1608.451385	19.455373
50.673275	1615.871295	19.460391
51.034758	1623.505755	19.465408
51.118137	1629.829885	19.470426
51.051122	1636.821397	19.475443
51.391158	1642.707669	19.480461
51.535474	1633.321374	19.485479
51.437699	1634.334013	19.490496
51.742487	1630.398161	19.495514
51.783565	1635.668521	19.500531
51.910735	1630.883142	19.505549
51.362047	1617.764635	19.510567
51.726009	1620.443861	19.515584
51.891679	1632.006606	19.520602
51.563315	1630.663159	19.525619
51.535537	1621.767758	19.530637
51.676468	1630.045875	19.535655
52.000622	1623.266631	19.540672
51.983788	1630.935120	19.545690
51.903173	1629.025812	19.550707
51.735951	1624.958777	19.555725
51.918875	1630.636121	19.560743
52.013772	1629.519863	19.565760
52.229423	1623.786460	19.570778
52.136440	1624.826752	19.575795
52.419241	1627.913188	19.580813
52.228193	1625.784486	19.585831
52.028012	1622.697806	19.590848
52.121206	1623.917220	19.595866
51.929525	1634.589170	19.600883
52.342208	1637.020911	19.605901
52.297323	1656.146774	19.610919
52.682145	1647.013139	19.615936
52.597436	1654.360896	19.620954
52.496233	1652.186555	19.625971
53.005830	1645.138396	19.630989
52.580877	1646.003471	19.636007
52.762246	1641.335836	19.641024
52.685674	1636.039552	19.646042
52.849545	1650.774328	19.651059
52.899191	1641.472292	19.656077
52.605251	1647.536795	19.661095
52.689868	1661.640181	19.666112
52.906377	1663.806002	19.671130
53.021644	1673.214838	19.676147
53.234956	1672.376684	19.681165
53.348510	1675.814710	19.686183
53.381753	1676.248219	19.691200
53.376602	1675.715706	19.696218
53.392985	1669.069877	19.701235
53.824848	1653.654817	19.706253
53.719697	1664.717190	19.711271
53.730665	1661.423842	19.716288
53.527861	1657.384467	19.721306
53.427454	1664.725220	19.726323
53.764431	1660.929493	19.731341
53.635777	1673.071736	19.736359
54.316497	1686.497893	19.741376
54.516536	1679.312019	19.746394
54.069150	1680.603510	19.751411
54.087847	1658.007088	19.756429
53.886425	1660.601324	19.761447
54.185943	1668.497988	19.766464
54.576362	1675.092782	19.771482
54.241172	1673.721997	19.776499
54.112612	1670.721921	19.781517
53.983910	1686.376767	19.786535
54.233429	1679.347251	19.791552
54.512711	1685.419790	19.796570
54.189190	1683.993525	19.801587
54.643964	1681.290237	19.806605
54.337497	1677.797300	19.811623
54.587699	1679.654871	19.816640
54.746255	1684.944711	19.821658
54.704622	1690.941294	19.826675
54.954889	1690.962085	19.831693
54.988349	1701.428377	19.836711
55.056906	1707.922124	19.841728
55.209586	1705.739559	19.846746
55.044439	1703.070275	19.851763
55.198727	1707.496055	19.856781
55.155988	1702.674158	19.861799
55.332934	1693.188040	19.866816
55.083686	1700.217596	19.871834
54.796522	1711.093908	19.876851
55.151057	1701.239118	19.881869
55.536101	1697.442164	19.886887
55.188582	1690.177964	19.891904
55.868201	1689.582348	19.896922
55.617061	1704.669383	19.901939
55.781263	1694.822324	19.906957
55.652694	1698.673850	19.911975
55.579088	1698.338264	19.916992
56.027259	1713.546127	19.922010
55.891484	1724.973116	19.927027
56.284254	1715.124951	19.932045
56.026496	1708.840811	19.937063
55.973620	1701.224314	19.942080
56.115844	1698.592084	19.947098
55.577966	1710.609110	19.952115
56.262521	1714.030269	19.957133
55.952793	1721.113492	19.962151
56.353036	1717.039583	19.967168
56.661065	1720.096835	19.972186
56.478943	1711.642160	19.977203
56.578161	1708.297106	19.982221
56.648198	1718.025493	19.987239
56.472737	1715.474594	19.992256
56.282215	1716.984632	19.997274
56.489936	1709.178972	20.002291
56.356526	1714.167408	20.007309
56.514947	1720.154749	20.012327
56.507345	1736.273528	20.017344
56.901963	1731.064347	20.022362
56.821593	1744.041718	20.027379
56.811852	1740.085690	20.032397
56.849372	1740.083006	20.037415
56.981078	1739.904610	20.042432
57.298781	1744.121749	20.047450
57.008980	1738.476970	20.052467
57.053094	1738.104004	20.057485
57.007424	1748.330244	20.062503
56.906207	1747.888524	20.067520
57.316141	1748.790064	20.072538
57.204590	1758.764686	20.077555
57.363897	1760.633351	20.082573
57.554479	1756.986779	20.087591
57.190738	1759.729544	20.092608
57.625974	1770.483242	20.097626
57.493959	1782.506158	20.102643
57.614703	1783.743359	20.107661
58.102905	1780.848617	20.112679
57.847997	1778.045054	20.117696
58.305918	1773.122604	20.122714
57.717770	1774.802249	20.127731
57.918008	1774.701483	20.132749
58.315431	1789.308258	20.137767
58.291674	1796.081603	20.142784
58.720534	1794.597412	20.147802
58.524193	1796.206204	20.152819
58.627925	1797.076822	20.157837
58.500160	1792.908887	20.162855
58.384727	1796.117710	20.167872
58.512612	1789.271319	20.172890
58.420512	1798.365553	20.177907
58.343583	1792.709496	20.182925
58.619102	1786.240786	20.187943
58.562665	1801.338425	20.192960
58.964174	1794.316610	20.197978
58.758229	1799.966567	20.202995
58.805019	1801.505707	20.208013
59.429558	1808.344752	20.213031
59.340535	1811.925003	20.218048
59.617271	1817.764444	20.223066
59.615799	1814.785460	20.228083
59.599156	1801.775974	20.233101
59.211947	1792.703259	20.238119
58.839871	1804.205193	20.243136
58.998566	1807.301637	20.248154
59.299179	1815.371775	20.253171
59.695906	1804.673981	20.258189
59.629733	1806.559042	20.263207
59.721453	1809.025315	20.268224
59.932351	1803.418839	20.273242
59.615972	1813.324592	20.278259
59.740129	1802.827303	20.283277
59.994338	1805.230246	20.288295
59.910043	1798.499150	20.293312
60.312928	1801.547867	20.298330
59.906612	1813.383394	20.303347
60.319664	1819.810584	20.308365
60.491555	1829.201163	20.313383
60.629321	1829.296388	20.318400
60.702562	1802.500083	20.323418
60.280478	1801.010351	20.328435
60.365462	1804.986240	20.333453
60.177604	1801.588310	20.338471
60.240518	1814.672679	20.343488
60.432184	1823.176479	20.348506
60.618805	1825.110304	20.353523
60.862699	1821.442743	20.358541
61.220401	1816.384496	20.363559
60.479390	1822.995657	20.368576
60.930051	1824.061243	20.373594
60.746965	1831.837921	20.378611
60.881309	1820.193402	20.383629
61.032802	1835.987526	20.388647
61.111148	1847.687176	20.393664
61.412949	1846.980327	20.398682
61.133326	1839.980000	20.403699
60.799881	1849.834794	20.408717
61.712874	1846.728311	20.413735
61.208291	1847.451228	20.418752
61.613744	1838.109124	20.423770
61.705890	1842.929704	20.428787
61.444245	1846.540164	20.433805
61.451319	1841.423229	20.438823
61.509617	1853.915023	20.443840
61.831375	1857.086920	20.448858
61.945583	1869.907657	20.453875
61.601369	1860.496792	20.458893
62.180866	1863.019202	20.463911
62.203246	1871.508520	20.468928
62.442214	1862.104120	20.473946
62.492972	1867.458243	20.478963
62.284449	1861.166335	20.483981
62.579311	1864.942087	20.488999
62.406901	1863.113412	20.494016
62.300585	1864.745977	20.499034
62.300388	1860.927291	20.504051
62.391872	1861.092888	20.509069
62.527742	1867.333135	20.514087
62.486433	1874.816203	20.519104
62.635208	1888.998084	20.524122
62.740164	1894.050216	20.529139
62.816714	1898.661804	20.534157
63.132979	1895.948625	20.539175
62.901058	1903.553093	20.544192
63.087291	1886.614097	20.549210
63.022149	1894.337607	20.554227
62.901587	1898.613981	20.559245
62.708228	1893.610491	20.564263
63.104701	1905.222464	20.569280
63.231931	1918.277895	20.574298
63.114976	1919.397703	20.579315
63.436144	1921.193686	20.584333
63.694408	1913.146475	20.589351
63.267479	1914.068679	20.594368
63.601576	1912.009154	20.599386
63.396908	1916.803670	20.604403
63.646053	1940.879727	20.609421
63.951637	1932.828249	20.614439
63.962748	1929.680006	20.619456
63.945033	1932.696807	20.624474
64.338272	1927.500410	20.629491
64.147920	1920.962621	20.634509
64.304205	1920.130236	20.639527
64.489350	1929.294715	20.644544
64.658718	1930.492748	20.649562
64.721320	1921.987007	20.654579
64.795411	1920.410058	20.659597
64.948434	1914.351838	20.664615
64.507276	1920.228045	20.669632
64.540695	1929.072290	20.674650
64.652235	1922.026425	20.679667
64.674363	1927.176756	20.684685
64.889276	1917.179610	20.689703
64.493139	1927.435614	20.694720
64.863443	1918.550284	20.699738
64.940496	1910.408381	20.704755
64.611104	1919.621909	20.709773
64.659370	1921.201857	20.714791
64.925537	1925.764807	20.719808
64.650952	1942.001345	20.724826
65.041134	1935.015967	20.729843
64.949521	1937.788710	20.734861
65.467513	1948.624231	20.739879
65.420909	1955.802030	20.744896
65.800600	1959.119513	20.749914
65.506625	1963.719737	20.754931
65.478611	1966.400464	20.759949
65.795345	1956.990142	20.764967
66.053739	1973.256821	20.769984
65.936818	1964.479365	20.775002
66.286312	1958.551305	20.780019
66.016357	1970.012096	20.785037
66.303333	1959.662787	20.790055
66.107634	1967.021750	20.795072
65.860059	1963.629990	20.800090
66.394260	1957.218525	20.805107
66.409076	1970.159055	20.810125
66.691270	1975.997693	20.815143
66.248799	1973.810504	20.820160
66.482945	1987.944372	20.825178
66.924072	1991.230144	20.830195
66.877185	1982.949826	20.835213
67.176938	1977.386183	20.840231
66.863902	1981.437095	20.845248
66.869300	1984.585992	20.850266
66.781395	1978.445570	20.855283
66.831287	1982.543769	20.860301
66.943277	1977.375642	20.865319
66.729662	1983.822174	20.870336
67.079135	1976.656953	20.875354
67.210041	1979.587357	20.880371
67.357745	1992.929989	20.885389
67.475515	2009.742632	20.890407
67.080712	2016.252279	20.895424
67.356704	2006.725230	20.900442
67.624414	2003.937586	20.905459
67.587991	2007.200345	20.910477
67.601125	2007.053148	20.915495
67.808637	2006.099116	20.920512
67.920078	2012.071824	20.925530
67.826534	2026.821992	20.930547
67.726180	2040.238239	20.935565
67.961844	2034.249088	20.940583
67.873337	2026.748497	20.945600
68.178792	2023.241675	20.950618
68.143201	2030.607139	20.955635
67.945729	2033.604780	20.960653
68.114298	2027.222173	20.965671
68.289146	2034.343214	20.970688
68.104627	2043.477300	20.975706
68.958982	2050.902170	20.980723
68.371674	2055.535751	20.985741
68.946738	2044.320689	20.990759
68.900629	2036.191713	20.995776
69.129384	2043.383214	21.000794
69.360687	2048.898466	21.005811
69.289646	2051.327153	21.010829
69.030813	2048.865012	21.015847
69.085370	2049.187886	21.020864
69.420845	2047.598378	21.025882
69.226044	2042.471986	21.030899
69.588835	2050.551425	21.035917
69.598512	2034.889738	21.040935
69.113482	2034.063144	21.045952
69.167467	2038.309048	21.050970
69.848472	2042.731290	21.055987
69.655037	2042.562804	21.061005
69.449142	2055.566379	21.066023
69.971750	2052.921842	21.071040
70.191838	2049.892326	21.076058
70.052729	2051.732032	21.081075
70.085869	2058.786916	21.086093
70.057600	2055.569077	21.091111
69.904793	2056.606142	21.096128
70.632970	2056.842412	21.101146
70.396564	2048.402394	21.106163
70.241699	2051.847831	21.111181
70.134028	2054.471619	21.116199
70.175271	2055.576118	21.121216
70.115282	2073.925254	21.126234
70.630193	2077.919058	21.131251
70.294956	2078.934209	21.136269
70.403733	2075.925285	21.141287
70.600655	2086.328320	21.146304
70.795072	2101.958152	21.151322
71.060487	2095.222651	21.156339
70.917786	2106.808769	21.161357
71.230137	2106.611537	21.166375
71.557428	2101.314961	21.171392
71.185977	2098.914642	21.176410
71.602357	2095.317839	21.181427
71.312412	2101.880521	21.186445
70.991584	2099.497519	21.191463
71.677112	2091.897721	21.196480
71.602401	2097.817566	21.201498
71.787317	2118.564838	21.206515
71.970198	2119.454632	21.211533
71.610084	2121.297410	21.216551
72.207799	2117.994107	21.221568
72.207063	2119.951006	21.226586
72.290933	2113.136636	21.231603
72.289976	2124.722651	21.236621
72.226186	2123.968921	21.241639
72.506834	2115.185911	21.246656
72.425388	2124.108214	21.251674
72.149009	2109.731604	21.256691
72.499357	2116.004612	21.261709
72.478002	2113.912385	21.266727
72.407679	2106.569868	21.271744
72.603405	2114.028523	21.276762
72.699900	2125.971683	21.281779
73.021760	2142.225416	21.286797
72.823511	2135.442615	21.291815
73.462585	2139.795705	21.296832
72.742602	2140.571315	21.301850
73.295626	2134.368295	21.306867
73.150476	2141.877212	21.311885
73.288715	2137.200426	21.316903
73.409575	2135.663471	21.321920
73.629438	2133.732280	21.326938
73.397252	2133.509900	21.331955
73.484144	2130.905213	21.336973
73.403612	2126.890757	21.341991
73.493036	2122.426766	21.347008
73.357713	2128.652784	21.352026
73.611131	2144.424900	21.357043
73.852983	2149.360975	21.362061
73.659302	2156.514556	21.367079
73.627071	2145.195748	21.372096
73.763411	2156.280553	21.377114
74.344535	2160.750034	21.382131
74.497404	2164.415543	21.387149
74.317293	2184.588872	21.392167
74.639135	2168.411064	21.397184
74.452620	2163.365397	21.402202
74.643605	2162.366606	21.407219
74.951459	2168.396962	21.412237
75.093671	2172.225100	21.417255
75.194242	2167.475307	21.422272
75.420668	2160.540747	21.427290
75.026183	2173.643387	21.432307
74.547688	2173.607931	21.437325
74.705355	2174.299690	21.442343
75.150614	2164.231602	21.447360
74.916515	2168.046108	21.452378
74.933621	2164.657025	21.457395
75.154592	2176.962599	21.462413
74.904356	2197.026999	21.467431
75.520957	2193.572390	21.472448
75.389823	2189.496416	21.477466
75.357908	2200.617078	21.482483
75.651476	2210.440110	21.487501
75.650835	2217.336235	21.492519
75.897517	2217.316560	21.497536
75.691999	2219.939922	21.502554
76.011386	2223.203783	21.507571
76.235720	2224.513155	21.512589
75.980605	2225.064444	21.517607
76.257023	2219.198246	21.522624
76.266435	2234.402707	21.527642
76.217785	2233.488797	21.532659
76.564679	2240.062216	21.537677
76.578752	2239.321530	21.542695
76.689104	2231.032242	21.547712
76.807213	2242.479748	21.552730
76.822957	2237.755850	21.557747
77.067766	2231.017215	21.562765
76.697269	2241.215726	21.567783
77.175417	2238.871642	21.572800
77.398192	2255.267245	21.577818
77.593738	2249.852400	21.582835
77.406392	2242.190464	21.587853
77.346614	2248.363659	21.592871
77.523282	2247.376574	21.597888
77.576066	2262.359651	21.602906
77.624575	2261.111755	21.607923
77.977041	2251.632561	21.612941
77.896486	2267.315086	21.617959
77.828143	2246.820875	21.622976
77.764916	2251.773216	21.627994
77.902539	2255.813547	21.633011
77.890564	2254.186932	21.638029
77.922675	2256.037705	21.643047
78.159992	2257.878421	21.648064
78.068185	2251.839510	21.653082
77.974676	2256.042297	21.658099
78.439909	2255.606498	21.663117
78.175018	2276.345524	21.668135
78.410382	2275.469173	21.673152
78.549047	2274.649001	21.678170
78.510912	2273.212690	21.683187
78.558924	2267.404354	21.688205
78.461162	2285.879555	21.693223
78.778383	2284.084586	21.698240
78.876970	2295.481531	21.703258
78.741177	2299.649924	21.708275
79.295284	2289.391128	21.713293
78.834330	2301.465928	21.718311
79.128114	2303.389328	21.723328
79.289007	2319.002509	21.728346
79.795737	2321.889868	21.733363
80.260804	2316.454869	21.738381
79.802689	2324.341127	21.743399
79.867151	2314.900709	21.748416
80.274777	2314.963126	21.753434
80.271439	2307.812022	21.758451
79.886592	2303.330765	21.763469
79.916919	2314.946718	21.768487
80.003337	2309.877184	21.773504
80.011431	2314.045129	21.778522
80.161375	2312.885488	21.783539
80.355717	2305.397274	21.788557
80.454342	2309.885578	21.793575
80.544691	2320.027712	21.798592
80.634399	2325.259095	21.803610
80.736460	2336.974287	21.808627
80.968296	2336.537180	21.813645
81.081822	2334.723623	21.818663
81.446469	2332.728698	21.823680
81.218305	2331.492584	21.828698
81.099623	2333.909836	21.833715
81.568397	2323.203603	21.838733
81.352401	2332.241772	21.843751
81.322990	2328.310788	21.848768
81.230615	2324.474885	21.853786
81.098841	2331.710362	21.858803
81.176261	2323.274699	21.863821
81.175231	2334.153899	21.868839
81.391955	2341.082294	21.873856
81.784715	2348.450212	21.878874
81.463099	2351.880802	21.883891
81.822340	2350.445349	21.888909
81.739492	2360.453681	21.893927
81.453910	2365.737561	21.898944
81.486706	2370.706451	21.903962
81.648982	2383.769355	21.908979
81.969384	2383.526674	21.913997
82.439735	2396.162590	21.919015
82.689874	2397.366937	21.924032
82.659577	2396.917245	21.929050
82.584834	2389.221824	21.934067
82.694500	2381.241870	21.939085
83.192341	2400.857905	21.944103
83.504777	2405.016062	21.949120
83.351850	2388.540022	21.954138
83.381085	2387.812735	21.959155
83.664298	2385.896841	21.964173
83.498390	2382.561639	21.969191
83.444153	2375.087093	21.974208
83.441080	2386.847193	21.979226
83.623808	2389.987316	21.984243
83.677205	2374.479443	21.989261
83.266575	2382.452969	21.994279
83.527414	2393.878210	21.999296
83.818098	2401.161147	22.004314
83.887345	2400.313972	22.009331
84.158816	2404.364928	22.014349
84.070666	2406.389207	22.019367
83.968658	2404.082344	22.024384
84.047471	2397.991403	22.029402
84.256791	2409.907608	22.034419
84.370110	2405.947933	22.039437
84.532766	2427.655347	22.044455
84.813878	2424.177511	22.049472
84.626070	2429.174668	22.054490
84.624739	2431.469396	22.059507
84.679775	2426.998092	22.064525
84.515112	2420.957914	22.069543
84.924269	2423.106271	22.074560
85.181898	2433.692519	22.079578
85.311132	2447.256154	22.084595
85.256646	2448.183153	22.089613
85.352524	2448.982444	22.094631
85.570204	2445.249430	22.099648
85.384382	2443.710000	22.104666
85.301529	2449.239879	22.109683
85.580983	2446.301992	22.114701
85.483987	2446.787485	22.119719
85.574559	2458.627644	22.124736
86.207682	2465.140522	22.129754
86.075155	2474.089938	22.134771
86.057912	2467.827813	22.139789
86.217245	2470.974771	22.144807
86.285456	2466.005885	22.149824
86.132020	2466.992574	22.154842
86.429380	2467.343693	22.159859
86.517151	2472.392368	22.164877
86.817068	2489.423100	22.169895
86.535147	2500.614678	22.174912
86.981638	2494.974234	22.179930
86.930334	2490.390174	22.184947
87.307565	2487.392776	22.189965
87.037817	2496.884460	22.194983
86.906464	2494.724207	22.200000
87.251252	2490.807152	22.205018
87.236846	2492.759921	22.210035
87.457576	2480.580682	22.215053
87.436056	2489.923007	22.220071
87.450068	2503.406898	22.225088
87.645483	2502.331648	22.230106
87.549355	2524.796160	22.235123
87.942464	2512.690888	22.240141
87.789706	2513.387110	22.245159
87.368652	2510.997662	22.250176
87.673958	2526.651521	22.255194
87.929572	2531.235218	22.260211
88.181944	2535.251322	22.265229
88.217457	2537.780156	22.270247
88.450629	2533.621778	22.275264
89.052573	2536.279639	22.280282
88.315862	2530.442669	22.285299
88.252039	2546.836098	22.290317
88.414420	2549.446053	22.295335
88.741568	2560.090919	22.300352
88.923383	2563.357460	22.305370
89.029732	2563.943655	22.310387
88.901176	2562.597235	22.315405
89.213584	2576.444724	22.320423
89.273527	2571.988396	22.325440
89.780614	2566.524647	22.330458
89.860046	2578.429753	22.335475
89.928290	2566.558397	22.340493
90.103818	2563.816672	22.345511
89.698819	2572.676269	22.350528
89.796445	2568.703236	22.355546
89.673721	2569.577810	22.360563
89.694378	2568.277447	22.365581
90.027496	2569.550865	22.370599
89.973599	2563.739463	22.375616
89.956506	2562.946837	22.380634
90.255032	2577.427726	22.385651
90.126484	2586.105148	22.390669
90.291492	2589.872994	22.395687
90.342558	2597.831090	22.400704
90.696720	2588.853277	22.405722
90.616861	2611.037609	22.410739
90.549102	2616.287436	22.415757
90.858612	2621.834799	22.420775
90.798186	2620.323050	22.425792
91.114088	2613.942401	22.430810
91.113562	2619.112260	22.435827
91.432029	2625.977483	22.440845
91.784510	2632.329243	22.445863
91.361243	2645.884905	22.450880
91.589808	2635.137219	22.455898
91.485044	2642.393839	22.460915
91.539985	2629.356757	22.465933
91.983356	2634.895776	22.470951
91.970850	2643.087937	22.475968
92.058315	2651.958789	22.480986
92.033831	2664.025414	22.486003
92.261642	2649.231671	22.491021
92.140071	2650.576332	22.496039
92.742813	2654.439731	22.501056
92.372426	2660.939471	22.506074
92.539183	2653.521713	22.511091
92.406199	2652.052891	22.516109
92.956181	2675.549416	22.521127
92.549279	2685.640260	22.526144
93.443288	2678.717688	22.531162
93.207344	2683.611991	22.536179
93.151863	2682.462418	22.541197
93.546933	2674.150412	22.546215
93.461770	2683.865765	22.551232
93.604039	2670.518294	22.556250
93.373827	2678.690926	22.561267
93.608959	2685.152617	22.566285
93.384167	2692.740520	22.571303
93.701492	2702.752625	22.576320
93.978073	2687.209516	22.581338
93.859958	2689.544667	22.586355
93.656649	2689.633369	22.591373
94.433533	2693.485274	22.596391
94.166567	2713.843235	22.601408
94.649224	2709.405862	22.606426
94.573181	2713.486085	22.611443
94.912218	2711.271046	22.616461
94.913393	2703.424725	22.621479
94.484216	2718.531034	22.626496
94.482601	2708.147607	22.631514
94.662996	2708.498120	22.636531
94.893546	2723.914528	22.641549
95.150181	2733.096623	22.646567
94.978291	2741.279082	22.651584
95.279637	2740.095694	22.656602
95.217642	2732.530686	22.661619
95.171824	2728.507501	22.666637
95.579666	2735.254611	22.671655
95.506327	2751.659186	22.676672
95.972615	2749.200120	22.681690
95.608867	2749.673759	22.686707
95.927582	2751.571209	22.691725
96.584106	2753.870221	22.696743
96.013308	2753.514669	22.701760
96.260285	2750.180990	22.706778
96.443523	2743.353970	22.711795
96.228410	2748.456489	22.716813
96.323997	2760.532772	22.721831
96.517566	2772.997701	22.726848
96.993267	2775.432354	22.731866
96.976177	2771.641371	22.736883
96.552141	2774.532602	22.741901
97.103717	2773.499378	22.746919
96.805334	2773.997494	22.751936
96.932948	2776.291001	22.756954
97.454815	2793.227282	22.761971
97.101806	2798.711222	22.766989
97.581861	2784.108248	22.772007
97.632096	2793.092312	22.777024
97.558079	2791.409089	22.782042
97.425904	2791.732826	22.787059
97.390755	2803.760186	22.792077
98.103594	2820.783351	22.797095
97.904154	2825.943403	22.802112
97.852542	2816.413598	22.807130
98.240876	2816.037180	22.812147
98.155944	2833.406275	22.817165
98.663821	2842.006204	22.822183
98.892193	2847.474821	22.827200
98.687291	2835.781797	22.832218
98.970217	2835.765914	22.837235
99.609427	2833.828918	22.842253
99.239938	2838.078234	22.847271
98.984751	2837.215588	22.852288
99.237495	2827.698061	22.857306
99.408940	2831.430233	22.862323
99.312836	2829.905118	22.867341
99.717281	2833.635504	22.872359
99.383336	2836.023425	22.877376
99.553297	2834.601809	22.882394
99.791723	2848.167577	22.887411
99.479238	2857.419964	22.892429
99.735257	2848.403744	22.897447
99.783952	2851.280891	22.902464
99.919307	2854.759916	22.907482
100.207167	2870.735582	22.912499
100.331878	2880.547564	22.917517
100.736396	2874.092973	22.922535
100.393385	2878.158248	22.927552
100.694347	2870.280667	22.932570
100.875924	2869.987139	22.937587
100.583228	2879.612021	22.942605
100.802709	2882.140487	22.947623
101.047341	2896.544862	22.952640
101.126858	2895.254190	22.957658
101.517345	2896.995227	22.962675
101.641923	2890.622363	22.967693
101.308636	2892.328454	22.972711
101.523180	2890.416954	22.977728
101.445970	2886.783706	22.982746
101.843323	2891.247447	22.987763
101.717667	2905.662499	22.992781
101.811282	2909.937119	22.997799
102.033456	2913.705546	23.002816
102.005483	2920.139108	23.007834
102.291810	2916.537270	23.012851
102.362131	2921.462559	23.017869
102.379210	2908.516424	23.022887
102.244570	2916.327009	23.027904
102.373392	2926.681235	23.032922
102.852861	2924.601979	23.037939
102.748485	2931.924933	23.042957
102.746971	2934.371251	23.047975
102.901420	2934.921517	23.052992
103.132965	2936.188783	23.058010
103.577184	2947.137469	23.063027
103.064916	2960.445347	23.068045
103.566143	2955.664137	23.073063
103.371059	2959.580007	23.078080
103.416086	2952.487348	23.083098
103.696360	2950.098429	23.088115
103.349370	2971.299295	23.093133
103.912280	2971.567791	23.098151
104.062684	2975.508442	23.103168
103.970749	2973.761729	23.108186
103.785310	2978.897537	23.113203
104.426365	2993.173602	23.118221
104.455544	3002.180006	23.123239
104.511135	3010.926625	23.128256
104.551157	3010.639491	23.133274
104.834344	2997.727349	23.138291
105.008834	3000.720529	23.143309
105.480868	2991.089655	23.148327
105.246145	2994.153258	23.153344
104.967510	2997.223741	23.158362
105.631889	3008.661900	23.163379
105.336662	3018.205191	23.168397
105.790781	3013.851121	23.173415
105.817142	3010.760268	23.178432
105.633891	3013.654844	23.183450
105.669084	3007.002416	23.188467
105.743981	3008.972812	23.193485
105.812176	3024.774721	23.198503
105.773508	3038.068424	23.203520
105.631793	3039.940200	23.208538
106.570404	3040.515956	23.213555
106.426090	3045.875744	23.218573
106.722203	3052.201766	23.223591
106.994854	3055.239544	23.228608
106.700053	3063.501374	23.233626
107.212792	3060.286968	23.238643
107.124369	3061.339251	23.243661
107.099752	3053.582036	23.248679
107.463369	3052.038533	23.253696
107.280725	3052.647928	23.258714
107.944443	3053.670747	23.263731
107.767635	3059.060879	23.268749
107.575679	3044.531418	23.273767
107.572518	3053.905878	23.278784
107.596611	3068.597439	23.283802
108.173996	3071.350761	23.288819
108.386570	3074.890324	23.293837
107.690158	3080.611209	23.298855
108.615836	3071.815052	23.303872
108.107738	3078.892009	23.308890
108.431338	3092.428836	23.313907
108.678930	3101.786129	23.318925
108.523005	3096.176756	23.323943
108.586204	3102.955907	23.328960
108.669510	3100.077052	23.333978
109.176520	3105.555749	23.338995
109.260325	3121.336360	23.344013
109.230630	3113.478916	23.349031
109.371321	3114.419558	23.354048
109.143439	3112.552100	23.359066
109.755055	3111.597826	23.364083
109.346330	3113.937530	23.369101
109.386370	3117.677724	23.374119
109.651957	3128.654507	23.379136
109.964626	3141.195719	23.384154
110.195426	3136.065458	23.389171
110.128684	3134.138034	23.394189
110.437174	3153.115441	23.399207
110.557331	3143.416522	23.404224
110.119787	3143.349392	23.409242
110.739917	3156.568375	23.414259
110.625567	3162.677840	23.419277
110.579019	3154.336960	23.424295
110.549975	3162.484605	23.429312
110.945567	3174.138574	23.434330
111.132501	3188.580628	23.439347
111.065087	3190.775338	23.444365
111.243833	3191.249213	23.449383
111.502397	3182.516489	23.454400
111.816649	3191.683480	23.459418
111.873153	3200.745671	23.464435
111.986974	3211.626346	23.469453
111.470631	3209.321167	23.474471
111.845744	3218.134608	23.479488
111.932623	3222.855386	23.484506
112.064276	3226.278251	23.489523
112.644364	3230.918604	23.494541
112.476705	3232.103248	23.499559
112.689103	3223.611298	23.504576
112.367828	3232.237162	23.509594
112.598325	3229.641381	23.514611
113.068584	3246.033834	23.519629
113.058602	3248.109086	23.524647
113.309830	3253.839370	23.529664
113.203839	3257.971751	23.534682
113.175505	3253.800522	23.539699
113.471485	3261.909916	23.544717
114.109597	3273.589079	23.549735
114.180633	3277.520136	23.554752
113.493036	3279.029272	23.559770
113.963812	3282.638892	23.564787
113.753557	3280.336249	23.569805
113.609854	3288.309384	23.574823
114.508114	3295.945684	23.579840
114.548876	3307.005143	23.584858
114.484182	3302.473475	23.589875
114.635867	3302.162530	23.594893
114.851462	3297.751075	23.599911
115.039946	3306.107735	23.604928
115.456011	3326.839128	23.609946
115.089439	3315.789745	23.614963
115.615046	3321.287690	23.619981
115.428393	3319.429532	23.624999
115.781461	3314.441035	23.630016
115.711741	3314.193183	23.635034
116.051604	3310.188350	23.640051
116.107380	3308.955025	23.645069
116.223242	3308.065786	23.650087
115.981291	3311.670293	23.655104
116.299255	3310.651547	23.660122
116.385164	3311.332501	23.665139
116.552796	3318.874966	23.670157
116.164519	3339.479888	23.675175
116.671961	3333.236261	23.680192
116.495192	3343.231446	23.685210
116.756476	3342.322579	23.690227
116.814560	3338.396604	23.695245
116.867851	3340.638703	23.700263
117.436441	3352.278309	23.705280
117.147222	3362.164872	23.710298
117.224403	3352.311605	23.715315
117.579460	3355.532213	23.720333
117.240953	3360.783642	23.725351
117.712453	3360.400497	23.730368
117.685300	3376.517498	23.735386
117.530860	3379.887369	23.740403
118.054161	3385.524570	23.745421
117.860545	3394.809108	23.750439
118.387517	3401.651432	23.755456
118.296498	3401.690981	23.760474
118.578577	3400.649446	23.765491
118.795534	3398.652296	23.770509
118.834673	3409.327008	23.775527
118.825922	3403.382010	23.780544
118.846948	3418.443620	23.785562
119.026404	3419.864270	23.790579
119.166781	3424.652471	23.795597
119.440815	3424.959922	23.800615
119.664213	3412.647074	23.805632
119.428121	3438.713861	23.810650
119.536073	3445.315691	23.815667
120.201824	3449.412428	23.820685
119.984119	3455.800155	23.825703
120.179768	3445.991402	23.830720
120.076912	3458.588466	23.835738
119.903472	3462.561022	23.840755
120.411658	3468.951812	23.845773
120.417396	3470.144024	23.850791
120.626092	3467.362248	23.855808
121.173851	3483.506056	23.860826
121.386810	3489.510695	23.865843
121.306896	3492.764754	23.870861
121.560771	3496.001239	23.875879
121.803100	3481.302386	23.880896
121.604687	3488.633986	23.885914
121.694307	3485.533141	23.890931
121.676103	3482.253499	23.895949
121.808356	3488.122437	23.900967
122.083970	3486.987222	23.905984
121.908584	3490.575023	23.911002
121.852462	3493.042597	23.916019
122.616083	3500.999927	23.921037
121.865813	3516.674836	23.926055
122.525215	3505.278379	23.931072
122.185755	3515.624245	23.936090
122.498948	3533.998466	23.941107
122.832525	3527.415882	23.946125
122.592073	3532.920283	23.951143
123.081603	3541.807490	23.956160
123.168253	3558.108826	23.961178
123.372781	3547.430647	23.966195
123.377097	3553.389088	23.971213
123.592640	3561.921537	23.976231
123.905959	3566.799464	23.981248
124.075319	3579.445497	23.986266
123.831181	3580.351765	23.991283
124.236930	3574.742622	23.996301
124.104079	3580.441652	24.001319
124.304596	3583.983204	24.006336
124.618758	3588.886255	24.011354
124.414577	3603.901238	24.016371
125.052781	3590.683706	24.021389
124.789279	3589.715011	24.026407
125.039891	3591.152934	24.031424
124.955837	3595.417676	24.036442
124.801510	3603.253736	24.041459
124.997728	3600.436019	24.046477
125.250442	3623.955109	24.051495
125.517075	3622.202657	24.056512
125.574792	3620.085242	24.061530
125.664050	3639.507827	24.066547
125.566145	3643.907316	24.071565
125.682041	3653.219246	24.076583
126.180145	3650.101721	24.081600
126.265788	3653.677066	24.086618
126.449063	3662.858506	24.091635
127.150930	3658.238215	24.096653
126.592464	3667.226546	24.101671
126.842325	3663.118953	24.106688
126.917908	3661.172330	24.111706
126.939500	3657.365631	24.116723
127.125201	3673.664178	24.121741
127.535823	3687.812770	24.126759
127.583941	3682.669945	24.131776
127.700487	3683.633338	24.136794
127.470773	3671.921563	24.141811
128.168627	3671.916428	24.146829
128.164638	3682.304521	24.151847
128.258836	3690.780291	24.156864
128.038773	3691.180938	24.161882
128.349770	3699.862627	24.166899
128.714196	3693.575001	24.171917
128.455513	3691.718620	24.176935
128.576165	3705.840060	24.181952
129.280388	3701.651805	24.186970
128.851223	3715.726826	24.191987
129.094601	3701.939806	24.197005
129.222898	3706.329122	24.202023
129.359365	3712.756141	24.207040
129.505978	3730.945187	24.212058
129.656082	3729.971656	24.217075
129.811015	3732.377790	24.222093
129.838674	3729.261360	24.227111
130.005428	3738.795779	24.232128
130.428038	3745.222169	24.237146
130.505459	3747.293253	24.242163
130.491190	3755.161094	24.247181
130.415924	3757.019375	24.252199
130.511164	3754.653028	24.257216
130.817149	3760.116078	24.262234
130.984246	3780.078977	24.267251
131.344576	3771.737193	24.272269
131.049562	3778.853633	24.277287
131.237918	3775.746738	24.282304
131.631170	3768.662331	24.287322
131.671992	3781.959910	24.292339
131.813668	3793.571997	24.297357
131.925360	3802.325992	24.302375
132.060203	3791.917406	24.307392
132.285914	3792.103026	24.312410
132.426953	3794.091553	24.317427
132.370788	3795.356612	24.322445
132.392270	3804.380404	24.327463
132.681764	3812.699381	24.332480
133.229478	3815.113430	24.337498
132.803845	3828.730316	24.342515
132.987109	3820.851825	24.347533
132.870761	3829.862504	24.352551
133.185867	3836.750813	24.357568
133.551456	3841.620626	24.362586
133.281314	3844.077589	24.367603
133.902677	3847.932022	24.372621
133.815558	3845.711018	24.377639
133.462846	3854.739801	24.382656
133.727390	3861.462443	24.387674
133.924561	3871.929601	24.392691
134.204324	3862.533553	24.397709
134.341732	3877.984481	24.402727
134.160032	3886.910736	24.407744
134.602482	3887.226531	24.412762
134.473013	3902.602506	24.417779
134.621802	3904.908623	24.422797
134.787701	3914.452737	24.427815
134.968428	3922.122814	24.432832
135.384278	3929.696088	24.437850
135.455093	3942.632417	24.442867
135.636661	3938.150385	24.447885
136.118527	3939.779365	24.452903
136.095926	3941.017081	24.457920
136.366287	3935.043963	24.462938
136.213633	3942.292824	24.467955
136.408778	3948.057368	24.472973
136.862267	3953.658342	24.477991
136.969597	3948.275750	24.483008
136.950978	3948.174545	24.488026
136.863867	3950.422935	24.493043
136.869516	3954.143439	24.498061
136.944160	3965.835578	24.503079
137.254864	3979.192024	24.508096
137.250165	3970.484385	24.513114
137.618469	3984.043287	24.518131
138.022370	3990.734675	24.523149
138.211032	3997.715453	24.528167
138.361942	3998.563007	24.533184
138.485660	3997.805072	24.538202
138.259179	3992.850371	24.543219
138.461260	3997.783720	24.548237
138.730846	3994.862913	24.553255
138.441670	4001.606073	24.558272
139.061293	4012.180730	24.563290
138.964071	4016.270877	24.568307
139.191121	4013.580834	24.573325
139.482925	4015.804588	24.578343
139.214204	4021.600795	24.583360
139.706760	4025.162966	24.588378
139.800977	4038.528121	24.593395
139.600506	4031.347246	24.598413
139.792769	4042.882128	24.603431
139.837875	4035.646996	24.608448
140.657200	4050.738728	24.613466
140.390192	4057.592065	24.618483
140.458034	4059.169134	24.623501
140.915295	4052.330256	24.628519
140.640080	4060.210703	24.633536
141.006518	4063.196084	24.638554
140.913396	4061.862936	24.643571
141.197755	4077.701342	24.648589
141.386931	4069.553525	24.653607
141.501680	4075.624249	24.658624
141.776338	4085.220856	24.663642
141.767236	4094.934520	24.668659
141.966489	4104.034772	24.673677
142.265173	4104.477256	24.678695
141.937152	4105.980623	24.683712
142.432841	4095.597397	24.688730
142.646441	4110.411622	24.693747
142.302678	4119.461229	24.698765
142.569032	4118.740914	24.703783
143.022604	4116.084809	24.708800
143.210196	4120.300804	24.713818
143.158466	4125.939949	24.718835
142.968937	4136.830830	24.723853
143.541648	4146.156670	24.728871
143.530264	4152.954213	24.733888
143.856336	4144.358802	24.738906
143.790091	4150.817736	24.743923
143.803031	4154.489793	24.748941
144.020662	4164.452049	24.753959
143.783294	4166.512526	24.758976
143.996343	4160.207422	24.763994
144.222936	4185.584142	24.769011
144.524359	4194.873599	24.774029
144.521080	4190.164796	24.779047
144.869156	4210.440709	24.784064
145.146239	4219.472011	24.789082
145.499350	4211.516239	24.794099
145.243780	4215.141996	24.799117
145.643909	4217.228861	24.804135
145.733282	4235.373723	24.809152
145.811115	4241.977407	24.814170
146.258642	4233.688037	24.819187
146.110478	4237.498981	24.824205
146.112915	4236.103503	24.829223
146.134274	4257.772130	24.834240
146.641042	4260.943883	24.839258
146.727443	4261.953064	24.844275
147.147157	4268.260152	24.849293
147.256514	4275.076702	24.854311
147.036738	4280.843228	24.859328
147.363722	4284.541866	24.864346
147.789383	4279.172433	24.869363
147.422227	4289.680898	24.874381
147.824062	4292.853314	24.879399
148.003915	4298.664556	24.884416
148.144189	4300.924712	24.889434
148.285956	4295.710225	24.894451
148.263050	4306.960187	24.899469
148.564192	4321.953412	24.904487
148.516482	4332.159342	24.909504
149.020062	4328.040259	24.914522
149.033377	4334.167994	24.919539
149.161859	4354.671014	24.924557
149.333488	4350.644965	24.929575
149.389697	4349.206333	24.934592
149.385327	4352.234074	24.939610
149.549320	4360.061624	24.944627
149.763487	4371.621692	24.949645
149.847796	4379.808942	24.954663
149.797614	4386.836758	24.959680
150.036004	4398.680284	24.964698
150.318922	4406.956376	24.969715
150.147817	4413.684347	24.974733
150.643720	4416.592689	24.979751
150.892449	4424.217605	24.984768
150.878585	4428.922918	24.989786
151.063901	4440.910514	24.994803
151.500446	4442.641335	24.999821
151.632575	4447.304842	25.004839
151.746009	4449.392460	25.009856
151.638275	4444.144421	25.014874
152.112864	4455.493295	25.019891
151.901519	4466.185778	25.024909
152.293562	4466.307471	25.029927
152.589567	4468.505372	25.034944
152.591117	4466.106264	25.039962
153.154754	4475.686214	25.044979
152.935271	4489.615350	25.049997
153.309303	4483.872014	25.055015
153.649625	4489.983293	25.060032
153.510941	4479.310989	25.065050
153.627617	4475.129386	25.070067
153.558299	4480.888186	25.075085
154.001514	4474.420657	25.080103
153.913594	4469.721885	25.085120
154.269233	4491.152190	25.090138
154.405393	4495.237446	25.095155
154.365185	4504.542707	25.100173
154.514360	4500.337068	25.105191
154.531956	4494.270796	25.110208
154.718068	4493.989160	25.115226
154.815869	4523.284754	25.120243
154.770680	4522.887845	25.125261
154.965974	4521.768308	25.130279
155.002223	4538.024763	25.135296
155.043002	4537.955283	25.140314
155.577930	4567.993678	25.145331
155.584737	4577.948156	25.150349
156.173782	4576.482847	25.155367
156.320291	4580.178256	25.160384
156.325143	4585.707672	25.165402
156.436997	4587.113756	25.170419
156.497489	4602.975068	25.175437
156.558249	4592.438745	25.180455
156.786510	4623.702641	25.185472
156.902920	4618.561477	25.190490
157.424555	4623.047218	25.195507
157.143314	4634.596686	25.200525
157.747101	4636.784268	25.205543
157.717584	4647.574629	25.210560
157.464498	4649.833325	25.215578
158.200261	4665.064924	25.220595
158.379308	4670.371374	25.225613
158.880284	4672.366739	25.230631
158.370412	4673.961770	25.235648
158.051374	4686.937612	25.240666
158.496729	4688.180978	25.245683
158.947909	4704.918650	25.250701
159.268950	4707.507221	25.255719
159.351947	4716.831167	25.260736
159.636586	4728.746576	25.265754
159.757550	4721.126820	25.270771
159.873001	4735.006827	25.275789
160.159943	4734.409525	25.280807
160.036800	4745.435567	25.285824
160.121075	4748.143306	25.290842
160.576795	4750.253091	25.295859
160.705837	4769.225589	25.300877
160.699931	4762.929327	25.305895
160.816635	4768.318173	25.310912
161.008264	4777.959720	25.315930
161.270071	4785.102951	25.320947
161.407009	4778.238230	25.325965
161.721445	4792.762600	25.330983
162.240719	4807.554760	25.336000
162.261277	4810.313525	25.341018
162.536977	4804.206714	25.346035
162.315078	4811.832924	25.351053
162.726682	4815.407937	25.356071
162.566231	4809.142184	25.361088
162.317158	4823.666478	25.366106
162.770319	4828.980535	25.371123
162.702543	4828.015829	25.376141
163.351927	4837.364738	25.381159
163.242291	4851.081237	25.386176
162.765104	4863.586407	25.391194
163.494514	4863.566868	25.396211
163.730504	4873.618178	25.401229
163.771733	4876.499975	25.406247
164.111633	4887.339927	25.411264
164.303145	4902.780096	25.416282
164.358073	4897.926260	25.421299
164.825010	4906.050647	25.426317
165.016874	4903.687953	25.431335
165.011404	4905.068251	25.436352
165.071295	4907.817712	25.441370
165.403624	4923.115889	25.446387
165.491894	4930.450504	25.451405
165.778823	4930.538165	25.456423
166.012606	4924.917674	25.461440
165.711269	4943.932526	25.466458
166.005663	4945.976069	25.471475
166.129907	4949.116335	25.476493
165.620107	4962.497885	25.481511
166.122572	4978.867930	25.486528
166.288299	4984.110272	25.491546
166.754368	5004.665304	25.496563
166.832841	5010.647328	25.501581
167.173469	5014.912158	25.506599
167.576906	5026.294634	25.511616
167.520891	5046.047671	25.516634
168.017668	5025.925787	25.521651
167.947968	5050.819835	25.526669
168.222635	5044.659444	25.531687
168.462797	5057.068147	25.536704
168.618525	5061.579757	25.541722
169.010150	5053.630213	25.546739
169.378078	5070.204498	25.551757
169.312497	5072.538036	25.556775
169.254852	5069.261130	25.561792
169.257545	5070.772736	25.566810
169.802428	5068.159010	25.571827
169.767336	5065.516195	25.576845
169.855827	5091.648139	25.581863
170.077509	5091.004231	25.586880
169.668153	5097.981268	25.591898
170.506581	5103.983155	25.596915
170.910397	5120.390879	25.601933
170.907254	5116.262623	25.606951
171.290728	5116.287813	25.611968
171.104518	5122.194547	25.616986
171.250257	5123.819480	25.622003
171.331835	5131.076310	25.627021
171.487123	5130.916288	25.632039
171.759107	5126.498715	25.637056
171.413890	5143.055371	25.642074
171.843269	5150.235626	25.647091
172.182903	5161.637653	25.652109
172.391771	5169.313320	25.657127
172.523458	5179.592630	25.662144
172.339094	5184.798335	25.667162
172.494968	5197.788522	25.672180
173.091604	5200.911644	25.677197
173.037484	5218.795876	25.682215
173.598190	5226.665818	25.687232
173.525565	5241.162801	25.692250
173.769920	5237.503954	25.697268
173.966143	5241.617848	25.702285
174.007176	5259.215747	25.707303
174.253661	5259.634875	25.712320
174.319520	5263.491418	25.717338
174.617008	5277.756835	25.722356
174.845265	5281.714203	25.727373
174.770320	5282.253134	25.732391
174.583594	5291.537558	25.737408
174.934485	5313.566174	25.742426
175.275556	5303.080224	25.747444
175.256318	5309.554301	25.752461
175.434722	5319.169798	25.757479
175.631259	5326.721200	25.762496
175.777054	5339.997162	25.767514
176.231311	5348.313131	25.772532
176.437540	5359.354233	25.777549
176.566293	5364.605634	25.782567
176.840183	5365.367699	25.787584
177.155320	5375.122792	25.792602
177.456845	5373.841359	25.797620
177.752702	5376.200383	25.802637
177.254913	5382.168640	25.807655
177.756869	5382.733989	25.812672
177.662050	5400.574270	25.817690
177.897301	5395.041790	25.822708
178.113100	5422.641028	25.827725
178.415854	5424.462354	25.832743
178.499118	5430.276465	25.837760
178.741807	5447.704062	25.842778
178.951441	5445.098612	25.847796
179.182142	5454.655483	25.852813
178.860694	5471.953675	25.857831
179.299557	5478.583321	25.862848
179.780095	5487.794877	25.867866
180.126213	5498.867811	25.872884
180.543820	5495.645796	25.877901
180.273151	5499.450941	25.882919
180.561502	5494.386763	25.887936
181.003022	5510.886789	25.892954
181.122420	5512.837861	25.897972
181.409471	5514.011390	25.902989
181.399857	5510.212348	25.908007
181.489842	5511.138966	25.913024
181.130612	5515.715580	25.918042
181.506510	5534.353479	25.923060
181.896266	5532.758332	25.928077
182.121193	5547.669812	25.933095
182.121927	5555.880155	25.938112
182.208828	5562.975335	25.943130
182.470645	5569.515955	25.948148
182.852422	5584.952149	25.953165
182.636631	5592.284159	25.958183
183.239630	5598.992306	25.963200
183.323988	5609.891663	25.968218
183.521286	5615.081892	25.973236
183.856401	5617.393762	25.978253
183.704203	5626.862346	25.983271
184.627899	5630.253128	25.988288
184.433796	5630.330924	25.993306
184.753040	5636.815223	25.998324
184.594187	5638.001796	26.003341
184.954604	5656.620149	26.008359
185.132066	5646.551060	26.013376
185.363542	5659.274043	26.018394
185.247088	5663.089785	26.023412
185.990013	5686.020217	26.028429
185.558577	5686.854914	26.033447
185.879970	5684.339248	26.038464
186.198980	5697.708288	26.043482
186.350846	5699.714270	26.048500
186.329585	5707.451471	26.053517
185.956510	5723.024978	26.058535
186.803327	5733.770238	26.063552
186.848763	5736.370569	26.068570
187.157146	5754.110149	26.073588
187.583163	5764.880314	26.078605
186.881027	5768.639468	26.083623
187.224613	5768.986577	26.088640
187.528772	5791.111480	26.093658
187.666190	5804.701603	26.098676
188.272672	5813.025506	26.103693
188.305999	5822.957570	26.108711
188.589160	5817.395360	26.113728
188.982794	5831.374674	26.118746
188.856591	5836.299977	26.123764
189.340944	5835.150862	26.128781
189.468194	5848.771022	26.133799
189.673987	5858.575072	26.138816
189.622979	5858.898771	26.143834
189.712916	5862.707474	26.148852
190.593481	5872.683611	26.153869
190.199008	5877.382633	26.158887
190.652823	5883.233539	26.163904
190.861876	5895.710821	26.168922
190.729151	5906.410768	26.173940
190.878127	5905.651956	26.178957
190.845425	5916.819215	26.183975
191.152528	5926.443282	26.188992
191.497420	5935.306981	26.194010
191.816530	5944.007418	26.199028
192.265386	5948.880543	26.204045
192.025041	5955.919814	26.209063
192.427470	5967.287256	26.214080
192.791665	5973.464746	26.219098
192.654920	5983.650823	26.224116
193.029456	5985.180014	26.229133
193.001867	5995.951930	26.234151
193.525123	6012.572189	26.239168
193.766522	6025.780008	26.244186
193.789990	6027.001178	26.249204
194.187499	6036.671118	26.254221
194.293118	6053.157967	26.259239
194.528310	6049.920240	26.264256
194.949786	6056.338165	26.269274
194.926078	6057.639332	26.274292
195.216083	6067.910125	26.279309
195.313991	6078.229958	26.284327
195.778934	6075.530759	26.289344
195.772742	6075.787462	26.294362
195.799683	6094.647909	26.299380
196.110035	6096.079835	26.304397
196.120433	6095.437427	26.309415
196.303314	6113.882029	26.314432
196.379868	6113.680670	26.319450
196.599778	6129.470985	26.324468
197.009120	6125.748235	26.329485
197.541233	6144.343346	26.334503
197.630090	6140.487709	26.339520
197.807802	6148.752668	26.344538
197.946232	6165.035603	26.349556
198.236655	6162.508942	26.354573
198.073107	6167.506476	26.359591
198.691802	6179.689336	26.364608
199.170418	6187.926114	26.369626
199.033769	6192.565884	26.374644
199.164947	6190.862824	26.379661
198.865075	6194.445400	26.384679
199.356918	6199.744334	26.389696
199.381789	6213.765928	26.394714
199.209562	6223.080120	26.399732
199.786348	6227.592349	26.404749
200.174317	6240.120757	26.409767
200.233832	6239.154973	26.414784
200.327661	6253.787677	26.419802
200.495175	6260.008703	26.424820
200.926045	6250.231044	26.429837
200.784921	6270.873160	26.434855
201.068168	6274.796878	26.439872
201.865830	6274.318397	26.444890
201.459956	6292.151454	26.449908
202.208427	6300.484906	26.454925
202.463507	6302.812561	26.459943
202.247575	6305.895866	26.464960
202.760486	6303.921490	26.469978
202.678079	6324.494489	26.474996
203.270063	6326.636783	26.480013
203.177735	6328.782107	26.485031
203.338530	6324.716286	26.490048
203.515166	6345.618070	26.495066
203.399370	6349.165525	26.500084
203.635700	6350.943687	26.505101
203.808198	6364.945427	26.510119
203.880581	6386.772742	26.515136
204.502115	6387.117361	26.520154
204.195648	6403.444951	26.525172
204.547482	6414.508078	26.530189
204.905109	6421.469633	26.535207
205.139343	6434.925100	26.540224
205.660757	6443.540418	26.545242
205.842598	6456.603197	26.550260
206.249652	6463.269756	26.555277
206.274231	6478.304931	26.560295
206.515362	6491.011197	26.565312
206.376163	6481.287998	26.570330
206.725272	6491.609750	26.575348
206.954113	6498.967169	26.580365
207.147025	6514.263271	26.585383
207.379081	6526.522718	26.590400
207.653512	6534.201318	26.595418
207.782302	6540.491642	26.600436
208.073085	6550.317475	26.605453
207.988970	6558.052254	26.610471
208.544521	6564.468297	26.615488
208.968061	6574.731083	26.620506
209.130529	6583.790989	26.625524
209.254604	6585.189000	26.630541
209.418384	6597.822225	26.635559
209.745044	6598.538197	26.640576
209.675230	6600.758946	26.645594
210.170516	6616.332917	26.650612
210.119594	6612.836858	26.655629
210.167494	6630.832761	26.660647
210.791100	6635.410366	26.665664
210.841276	6647.357450	26.670682
210.491938	6660.472019	26.675700
210.953765	6661.514069	26.680717
211.372564	6668.870210	26.685735
211.447098	6684.478585	26.690752
211.703701	6692.336827	26.695770
211.885682	6697.435059	26.700788
212.242373	6716.130841	26.705805
212.504194	6724.458649	26.710823
212.542657	6730.542210	26.715840
212.881307	6738.715931	26.720858
213.067625	6750.963752	26.725876
213.181608	6758.440289	26.730893
213.470189	6764.989775	26.735911
213.645902	6781.557847	26.740928
213.956276	6786.639148	26.745946
213.922865	6807.126090	26.750964
214.182779	6799.818330	26.755981
214.574297	6813.221024	26.760999
214.964955	6821.074105	26.766016
214.881184	6831.536471	26.771034
215.156002	6826.278325	26.776052
215.535665	6843.512169	26.781069
215.800845	6844.490331	26.786087
216.285974	6841.926763	26.791104
216.096697	6845.757315	26.796122
216.033641	6864.174907	26.801140
216.402384	6869.471224	26.806157
216.335977	6871.287393	26.811175
216.556195	6893.991860	26.816192
217.201273	6886.241745	26.821210
217.062730	6907.686017	26.826228
217.442651	6914.363307	26.831245
217.900167	6921.280993	26.836263
218.052401	6937.139431	26.841280
218.197836	6931.105990	26.846298
218.217127	6942.398317	26.851316
218.782157	6958.993953	26.856333
219.124821	6957.024083	26.861351
219.172983	6958.677096	26.866368
219.426967	6971.795235	26.871386
219.549478	6986.812328	26.876404
219.663527	6989.247400	26.881421
220.102632	7015.895407	26.886439
220.262781	7011.438080	26.891456
220.257737	7012.818470	26.896474
220.508607	7034.091394	26.901492
220.913124	7032.853697	26.906509
221.207982	7043.976641	26.911527
221.265026	7060.364671	26.916544
221.716937	7062.690001	26.921562
221.658686	7067.005177	26.926580
221.773823	7079.668452	26.931597
221.983865	7085.535838	26.936615
222.137168	7098.622487	26.941632
222.790888	7114.462498	26.946650
222.729564	7118.936013	26.951668
223.110780	7133.950580	26.956685
223.635041	7138.468111	26.961703
223.515459	7150.416860	26.966720
223.778865	7157.317691	26.971738
223.758092	7160.436860	26.976756
223.965838	7174.108534	26.981773
224.227991	7188.860833	26.986791
224.473708	7197.147182	26.991808
225.011012	7210.221108	26.996826
225.246869	7224.545056	27.001844
225.248973	7236.645272	27.006861
225.396324	7237.054726	27.011879
225.379032	7248.820198	27.016896
225.636464	7254.418188	27.021914
225.916415	7271.421815	27.026932
226.124948	7280.317002	27.031949
226.949726	7295.947271	27.036967
226.790060	7313.442836	27.041984
227.222222	7312.958456	27.047002
227.346402	7316.307499	27.052020
227.651664	7335.507610	27.057037
228.100915	7328.858195	27.062055
228.285221	7342.808321	27.067072
228.154975	7354.058030	27.072090
228.872570	7356.578549	27.077108
228.633357	7362.759487	27.082125
228.968569	7379.363096	27.087143
229.028083	7377.560661	27.092160
229.499764	7379.510415	27.097178
229.961258	7395.210307	27.102196
229.929527	7408.484011	27.107213
230.279942	7406.446584	27.112231
230.279008	7408.587187	27.117248
230.491067	7415.357253	27.122266
230.859151	7428.015870	27.127284
231.051935	7432.285491	27.132301
231.405227	7439.036598	27.137319
231.191137	7452.480965	27.142336
231.530715	7440.049343	27.147354
231.721090	7458.333119	27.152372
231.835996	7477.244345	27.157389
232.127793	7480.623985	27.162407
232.454184	7503.337829	27.167424
232.421810	7504.214264	27.172442
232.601708	7516.725631	27.177460
232.569983	7530.630818	27.182477
233.204834	7547.506493	27.187495
233.296184	7566.705629	27.192512
233.588265	7581.068402	27.197530
233.825734	7597.321309	27.202548
234.016719	7614.604378	27.207565
234.442442	7619.333199	27.212583
234.629302	7640.162245	27.217600
234.554457	7647.510875	27.222618
235.092559	7659.688409	27.227636
235.513475	7677.885775	27.232653
235.777962	7685.010783	27.237671
235.692768	7700.225160	27.242688
236.330427	7718.347572	27.247706
236.624161	7714.661560	27.252724
237.004955	7738.273233	27.257741
237.374159	7723.273284	27.262759
237.620483	7743.850042	27.267776
238.019020	7745.236718	27.272794
238.387748	7750.435427	27.277812
238.344459	7758.599982	27.282829
238.561903	7752.267704	27.287847
238.960381	7768.530267	27.292864
239.082636	7777.669673	27.297882
239.317528	7778.564235	27.302900
239.138207	7785.316824	27.307917
239.367700	7800.002119	27.312935
239.704825	7806.190787	27.317952
239.614128	7824.070659	27.322970
240.089708	7829.180040	27.327988
239.971346	7850.644345	27.333005
240.427334	7852.817603	27.338023
240.718987	7877.680977	27.343040
240.989986	7875.857992	27.348058
241.249074	7895.078549	27.353076
241.275164	7911.595310	27.358093
241.125800	7911.243059	27.363111
241.853957	7923.315226	27.368128
242.478967	7948.388509	27.373146
242.912514	7958.249560	27.378164
242.735327	7963.079234	27.383181
243.125356	7971.024463	27.388199
243.412671	7991.102575	27.393216
243.653417	7988.640278	27.398234
243.969443	7998.980692	27.403252
244.492172	8008.388967	27.408269
244.445247	8015.483962	27.413287
244.616226	8011.431960	27.418304
244.967250	8042.227848	27.423322
245.412795	8032.380654	27.428340
245.148634	8040.519950	27.433357
245.615240	8052.699475	27.438375
246.188184	8054.273535	27.443392
246.136214	8058.843680	27.448410
246.427358	8057.800475	27.453428
246.667198	8071.057370	27.458445
246.868156	8074.833357	27.463463
247.025748	8076.605082	27.468480
247.269018	8088.775419	27.473498
247.467184	8091.080649	27.478516
247.740437	8098.027649	27.483533
248.045749	8103.722583	27.488551
248.074905	8122.234326	27.493568
247.872020	8130.338806	27.498586
248.580410	8140.084287	27.503604
248.753248	8152.635078	27.508621
249.014673	8163.141992	27.513639
249.500429	8170.185170	27.518656
249.337491	8189.910982	27.523674
249.723512	8197.348645	27.528692
249.420462	8209.693043	27.533709
250.031062	8220.015849	27.538727
250.328052	8240.866206	27.543744
250.195727	8260.950365	27.548762
250.780399	8269.032558	27.553780
251.003585	8291.229990	27.558797
251.339386	8299.894207	27.563815
251.649941	8318.210523	27.568832
251.801049	8338.089351	27.573850
252.319183	8349.459093	27.578868
252.272640	8366.480150	27.583885
252.806218	8365.569435	27.588903
253.073337	8385.013400	27.593920
253.282455	8399.427694	27.598938
253.653538	8410.454283	27.603956
253.758654	8421.175258	27.608973
254.272374	8433.259255	27.613991
254.767654	8440.528359	27.619008
254.400333	8455.235054	27.624026
255.010899	8461.381108	27.629044
255.152231	8477.722466	27.634061
255.554637	8484.488365	27.639079
256.006805	8494.804573	27.644096
256.102407	8511.513039	27.649114
256.513436	8516.433825	27.654132
256.663121	8533.607411	27.659149
257.105808	8541.718282	27.664167
257.448033	8551.243514	27.669184
257.404661	8548.446793	27.674202
257.740212	8561.054458	27.679220
257.973106	8569.842266	27.684237
257.995767	8575.044908	27.689255
258.142628	8577.768668	27.694272
258.129527	8603.814181	27.699290
258.673077	8616.780789	27.704308
259.071378	8629.634402	27.709325
259.128362	8629.489755	27.714343
259.713575	8636.760635	27.719360
259.526049	8662.022161	27.724378
260.338470	8666.305503	27.729396
260.302256	8693.030398	27.734413
260.694886	8703.119261	27.739431
260.793452	8707.915402	27.744448
260.692745	8728.475006	27.749466
261.332888	8732.605392	27.754484
261.717198	8754.632909	27.759501
261.800821	8768.359939	27.764519
262.231227	8774.755325	27.769536
261.949205	8775.585683	27.774554
262.416751	8793.240125	27.779572
262.779413	8804.893393	27.784589
262.930073	8823.121599	27.789607
263.186238	8824.085498	27.794624
263.544955	8843.417723	27.799642
263.575115	8855.865054	27.804660
264.212666	8869.047590	27.809677
264.385114	8873.213388	27.814695
264.452390	8884.136306	27.819712
264.664918	8908.224160	27.824730
265.204382	8911.009599	27.829748
265.422308	8929.006366	27.834765
265.409577	8942.979096	27.839783
265.857162	8955.237972	27.844800
266.467934	8970.028645	27.849818
266.565380	8983.059079	27.854836
266.725838	8985.758669	27.859853
267.063634	9011.661384	27.864871
267.673770	9009.769378	27.869888
267.558050	9023.565712	27.874906
268.014637	9031.942987	27.879924
267.886497	9041.709489	27.884941
268.558401	9063.843870	27.889959
268.914776	9061.578012	27.894976
269.055198	9078.049489	27.899994
269.391738	9082.521139	27.905012
269.685855	9102.978263	27.910029
269.755462	9109.458700	27.915047
270.463959	9119.583557	27.920064
270.487772	9129.758845	27.925082
270.571111	9137.004354	27.930100
271.092644	9149.166529	27.935117
270.981879	9162.030798	27.940135
271.300221	9178.525009	27.945152
271.067612	9191.067401	27.950170
271.847554	9201.168482	27.955188
272.064178	9220.075028	27.960205
272.465866	9238.188543	27.965223
272.880717	9255.425449	27.970240
272.854380	9269.877306	27.975258
272.911398	9274.165466	27.980276
273.188775	9292.184845	27.985293
273.570452	9306.484411	27.990311
274.401326	9321.458739	27.995328
274.257194	9338.821175	28.000346
274.835341	9348.982364	28.005364
275.070775	9363.639555	28.010381
275.258345	9376.716136	28.015399
275.800821	9385.086433	28.020416
276.139609	9395.136750	28.025434
276.368748	9408.058449	28.030452
276.789854	9410.452058	28.035469
277.105565	9426.024969	28.040487
277.546571	9434.389082	28.045504
277.435440	9441.990376	28.050522
277.485280	9441.600573	28.055540
277.927864	9459.856292	28.060557
278.366269	9460.592767	28.065575
279.270374	9470.513524	28.070592
278.832405	9483.347182	28.075610
279.145293	9485.113661	28.080628
279.700964	9492.566319	28.085645
280.009451	9505.488285	28.090663
280.079986	9504.132257	28.095680
280.329258	9518.929482	28.100698
280.122730	9526.978308	28.105716
280.949622	9533.081364	28.110733
280.792032	9556.176651	28.115751
281.227652	9555.439096	28.120768
281.285433	9564.621058	28.125786
281.277034	9575.489934	28.130804
281.621094	9575.871786	28.135821
281.974986	9605.353220	28.140839
282.168515	9615.723202	28.145856
282.219897	9638.773225	28.150874
282.465646	9644.367461	28.155892
283.247810	9657.177443	28.160909
283.564479	9683.049674	28.165927
283.919445	9694.136387	28.170944
283.980349	9716.323059	28.175962
284.173588	9732.196417	28.180980
284.368112	9739.083750	28.185997
284.846180	9761.685045	28.191015
285.339849	9771.910219	28.196032
285.184861	9788.295992	28.201050
285.353452	9805.774058	28.206068
285.547580	9808.323255	28.211085
285.851901	9834.090280	28.216103
286.406720	9848.205272	28.221120
286.619241	9857.814644	28.226138
286.744714	9878.333771	28.231156
287.246902	9896.981571	28.236173
287.381547	9918.834879	28.241191
288.188631	9934.031292	28.246208
288.281664	9940.940913	28.251226
288.702671	9965.186922	28.256244
289.281314	9980.649649	28.261261
289.071479	9989.946363	28.266279
289.369437	10006.848650	28.271296
289.925012	10022.466580	28.276314
290.163422	10043.186058	28.281332
290.648909	10049.270148	28.286349
290.609977	10071.798095	28.291367
290.743786	10076.721681	28.296384
291.324501	10098.104332	28.301402
291.296871	10111.717170	28.306420
291.837450	10121.619447	28.311437
292.133110	10142.484781	28.316455
292.776132	10151.550096	28.321472
292.908963	10176.185683	28.326490
293.346463	10181.582700	28.331508
293.647990	10190.932021	28.336525
293.960995	10217.964348	28.341543
294.498437	10215.335302	28.346560
294.258423	10229.584567	28.351578
294.646718	10238.219368	28.356596
295.479149	10256.471636	28.361613
295.322535	10261.977531	28.366631
295.669564	10277.006327	28.371648
295.881291	10293.786613	28.376666
296.221556	10313.574776	28.381684
296.434464	10312.594226	28.386701
296.739137	10328.494841	28.391719
297.227482	10335.099559	28.396736
297.589104	10350.037719	28.401754
297.538342	10367.348595	28.406772
297.894729	10383.133802	28.411789
298.078592	10395.330748	28.416807
298.556831	10406.966920	28.421824
298.728870	10419.500426	28.426842
299.244643	10434.783931	28.431860
299.481253	10439.022124	28.436877
299.592636	10455.016275	28.441895
299.894230	10467.460054	28.446912
300.088216	10486.579827	28.451930
300.251986	10504.315059	28.456948
300.817235	10513.484302	28.461965
301.121049	10523.417568	28.466983
301.259073	10537.892022	28.472000
301.390066	10556.162896	28.477018
301.636110	10565.281128	28.482036
302.103232	10574.573128	28.487053
302.199871	10595.886935	28.492071
302.629595	10609.393760	28.497088
302.752747	10629.873030	28.502106
302.770488	10649.847845	28.507124
303.720839	10655.849844	28.512141
303.932380	10683.501823	28.517159
303.756786	10693.800770	28.522176
304.401118	10703.106122	28.527194
304.545332	10738.574118	28.532212
305.322262	10743.214001	28.537229
305.700551	10768.699183	28.542247
305.705816	10766.570221	28.547264
306.054357	10787.169076	28.552282
306.274639	10809.322607	28.557300
306.872705	10821.982256	28.562317
307.042836	10848.185340	28.567335
307.381909	10845.587284	28.572352
307.996669	10861.869205	28.577370
308.199242	10873.031014	28.582388
308.710552	10885.742188	28.587405
308.621143	10896.706618	28.592423
308.988845	10911.934771	28.597440
309.792239	10925.073851	28.602458
310.113026	10941.518721	28.607476
310.362785	10946.010734	28.612493
310.833131	10953.388937	28.617511
310.942159	10967.262014	28.622528
311.004064	10970.782511	28.627546
311.068133	10989.225328	28.632564
311.466487	10998.989317	28.637581
311.910666	11011.006955	28.642599
312.110190	11034.048124	28.647616
312.490717	11055.940027	28.652634
312.359678	11067.810989	28.657652
313.001010	11080.179854	28.662669
313.512260	11102.234474	28.667687
313.457902	11115.179663	28.672704
314.007544	11126.337779	28.677722
314.172896	11157.193175	28.682740
314.611315	11164.058618	28.687757
315.023804	11178.509519	28.692775
315.236954	11197.194426	28.697792
315.589273	11204.070213	28.702810
316.110719	11223.502568	28.707828
316.226508	11238.618884	28.712845
316.267558	11254.760513	28.717863
316.516043	11277.004908	28.722880
317.586416	11278.188736	28.727898
318.010351	11296.070265	28.732916
317.965153	11304.170362	28.737933
318.517602	11315.299732	28.742951
318.783335	11327.654974	28.747968
319.129442	11337.127351	28.752986
319.387227	11360.886049	28.758004
319.595161	11367.980288	28.763021
320.165096	11390.354449	28.768039
320.102407	11401.135003	28.773056
320.604586	11408.855741	28.778074
320.664344	11441.919547	28.783092
320.983474	11442.033793	28.788109
321.410030	11455.759605	28.793127
321.182040	11471.349926	28.798144
322.001789	11474.985472	28.803162
322.151228	11492.758620	28.808180
322.349696	11508.095868	28.813197
322.893722	11527.755511	28.818215
322.799249	11541.136719	28.823232
323.367956	11554.432998	28.828250
323.412592	11586.296358	28.833268
324.132561	11586.290977	28.838285
324.804673	11601.355174	28.843303
324.775357	11613.412636	28.848320
325.089914	11626.966658	28.853338
325.433098	11646.158974	28.858356
325.645484	11652.065336	28.863373
325.861550	11683.339940	28.868391
326.560292	11698.636871	28.873408
326.899685	11709.588286	28.878426
327.207023	11726.676964	28.883444
327.566131	11728.790084	28.888461
327.992351	11745.569650	28.893479
328.048770	11757.506412	28.898496
328.405458	11765.960571	28.903514
328.351380	11788.606630	28.908532
328.607849	11807.323251	28.913549
329.241762	11827.155434	28.918567
329.394936	11848.382867	28.923584
329.832085	11865.132408	28.928602
329.905746	11890.505792	28.933620
330.251584	11912.110462	28.938637
330.815028	11928.278202	28.943655
331.036966	11951.885377	28.948672
331.576488	11956.859585	28.953690
331.955437	11982.630511	28.958708
332.841307	12000.869805	28.963725
333.140690	12021.695602	28.968743
333.504949	12021.231233	28.973760
334.133935	12034.262634	28.978778
334.136029	12044.038719	28.983796
334.367349	12048.464416	28.988813
334.922835	12053.189845	28.993831
334.796998	12075.803281	28.998848
335.591946	12085.729916	29.003866
335.942324	12092.928427	29.008884
336.095916	12108.623705	29.013901
336.424280	12114.710985	29.018919
336.738800	12137.577607	29.023936
337.184862	12139.531897	29.028954
337.009372	12158.550206	29.033972
337.538863	12173.990876	29.038989
337.715159	12186.212278	29.044007
338.113997	12216.085508	29.049024
338.540288	12225.713138	29.054042
338.487292	12248.757460	29.059060
338.725511	12265.709040	29.064077
339.462083	12279.036380	29.069095
339.498208	12303.756224	29.074112
339.703648	12324.653912	29.079130
340.461659	12351.591190	29.084148
340.488154	12366.476091	29.089165
340.652125	12384.740422	29.094183
341.268321	12416.341976	29.099200
341.487332	12434.705099	29.104218
341.899369	12451.032793	29.109236
342.365943	12472.104471	29.114253
342.837812	12489.007021	29.119271
343.110338	12513.516429	29.124288
343.227572	12537.330209	29.129306
343.487237	12545.847285	29.134324
343.621564	12563.715389	29.139341
344.258481	12586.412058	29.144359
344.351444	12608.922386	29.149376
345.041350	12622.134125	29.154394
345.411055	12643.985367	29.159412
345.841562	12662.969257	29.164429
346.224840	12670.728090	29.169447
346.100003	12697.317846	29.174464
346.468409	12702.944314	29.179482
347.073315	12727.853508	29.184500
347.430713	12753.145713	29.189517
347.707894	12758.303334	29.194535
348.222007	12773.326909	29.199552
348.381021	12791.677673	29.204570
349.081860	12812.791983	29.209588
349.188858	12823.925714	29.214605
349.737232	12846.598672	29.219623
350.232970	12868.645168	29.224640
350.520872	12888.741093	29.229658
350.723938	12900.077714	29.234676
351.132233	12917.300081	29.239693
351.534381	12925.848695	29.244711
351.974980	12944.790236	29.249728
351.902883	12959.817364	29.254746
352.276754	12981.494660	29.259764
352.978475	12998.945876	29.264781
353.464763	13018.729811	29.269799
353.455653	13039.361896	29.274816
353.861507	13047.783669	29.279834
354.287909	13073.520233	29.284852
354.458256	13090.183184	29.289869
355.427884	13111.211515	29.294887
355.511807	13134.055466	29.299904
355.827027	13140.612512	29.304922
356.316395	13162.379293	29.309940
356.573636	13178.346597	29.314957
357.269969	13189.277701	29.319975
357.090722	13210.211364	29.324992
357.546677	13220.074860	29.330010
358.299515	13230.971874	29.335028
358.281575	13263.700512	29.340045
358.586988	13270.410720	29.345063
359.077189	13295.875484	29.350080
359.194591	13309.319493	29.355098
359.426735	13333.552074	29.360116
359.885585	13346.197346	29.365133
360.640171	13366.454367	29.370151
360.591732	13385.296107	29.375168
360.786890	13400.060663	29.380186
361.812640	13422.738487	29.385204
361.917698	13447.395341	29.390221
362.395276	13457.470317	29.395239
362.429115	13480.998340	29.400256
362.584506	13508.331676	29.405274
362.913881	13522.118433	29.410292
363.359607	13547.334705	29.415309
364.077885	13566.419695	29.420327
363.993664	13580.438655	29.425344
364.460977	13605.920053	29.430362
365.480908	13638.350970	29.435380
365.315001	13657.836667	29.440397
366.031264	13667.271187	29.445415
366.178636	13687.756304	29.450432
366.802759	13703.887645	29.455450
367.089179	13717.157041	29.460468
367.421267	13745.217808	29.465485
367.986321	13750.687467	29.470503
368.297428	13777.279926	29.475520
368.485322	13786.263563	29.480538
369.024565	13796.288007	29.485556
369.075822	13807.449996	29.490573
369.398254	13816.529420	29.495591
369.539885	13846.574997	29.500608
369.822482	13859.797722	29.505626
370.419592	13875.415520	29.510644
370.393105	13896.139684	29.515661
370.949171	13909.546987	29.520679
371.682827	13932.596458	29.525696
371.858733	13962.137875	29.530714
372.254964	13976.407149	29.535732
372.221959	14003.960193	29.540749
373.053648	14010.904037	29.545767
373.296848	14048.368127	29.550784
373.233222	14068.905654	29.555802
374.248751	14095.043987	29.560820
374.468310	14115.600368	29.565837
374.748797	14131.558518	29.570855
375.448500	14154.285135	29.575872
375.746148	14183.214105	29.580890
376.356468	14189.355793	29.585908
376.775340	14200.299367	29.590925
377.443476	14229.044049	29.595943
377.178590	14225.857992	29.600960
377.680928	14248.331407	29.605978
378.243177	14262.682268	29.610996
378.317441	14292.028525	29.616013
378.954878	14298.301801	29.621031
379.106572	14320.220709	29.626048
379.358687	14345.007283	29.631066
380.002476	14358.698028	29.636084
380.282015	14381.275978	29.641101
381.102846	14401.662691	29.646119
381.331292	14422.221170	29.651136
381.655793	14442.613033	29.656154
381.889518	14457.966103	29.661172
382.104888	14483.494461	29.666189
382.481431	14499.308390	29.671207
382.537982	14520.645541	29.676224
383.478518	14539.377726	29.681242
384.122618	14562.318823	29.686260
384.185528	14582.066490	29.691277
384.546320	14611.415730	29.696295
384.860318	14630.997791	29.701312
385.110238	14653.555438	29.706330
385.658137	14667.975176	29.711348
385.834754	14692.701390	29.716365
386.632526	14705.970335	29.721383
387.335312	14727.970774	29.726400
387.769363	14752.047210	29.731418
387.734014	14761.388413	29.736436
388.288981	14788.436767	29.741453
388.438132	14805.827772	29.746471
389.046560	14820.114974	29.751488
389.191817	14840.589030	29.756506
389.967661	14856.441774	29.761524
389.789535	14885.345271	29.766541
390.391884	14902.384295	29.771559
390.945670	14920.255237	29.776576
391.059266	14940.712252	29.781594
391.942682	14961.636137	29.786612
391.916179	14990.733962	29.791629
392.160762	15003.227568	29.796647
392.641218	15032.097610	29.801664
393.134595	15051.389871	29.806682
393.591548	15065.426217	29.811700
393.771101	15090.499894	29.816717
394.122737	15111.235631	29.821735
394.752687	15130.879254	29.826752
395.009197	15148.414826	29.831770
395.257119	15160.017383	29.836788
395.493913	15191.307162	29.841805
396.061452	15201.605848	29.846823
396.395723	15213.637069	29.851840
396.517591	15237.671428	29.856858
396.848755	15258.486330	29.861876
397.814994	15280.313495	29.866893
398.191734	15295.152145	29.871911
398.610496	15320.539224	29.876928
398.805362	15349.024952	29.881946
399.439272	15372.976118	29.886964
399.549747	15387.487027	29.891981
400.276883	15401.118096	29.896999
400.652928	15420.782840	29.902016
400.960287	15448.988956	29.907034
401.422555	15463.776442	29.912052
401.796149	15481.069739	29.917069
402.095033	15500.550836	29.922087
402.781529	15515.656971	29.927104
403.300880	15542.550900	29.932122
403.603135	15555.721191	29.937140
404.112720	15574.758778	29.942157
404.475841	15590.752583	29.947175
404.901768	15608.900023	29.952192
405.103053	15637.400967	29.957210
405.679897	15643.485209	29.962228
405.826709	15672.004211	29.967245
406.414803	15692.615108	29.972263
406.629195	15713.524597	29.977280
406.868778	15734.774424	29.982298
407.303220	15758.371998	29.987316
408.075038	15782.428412	29.992333
408.225847	15813.015727	29.997351
408.660201	15828.022636	30.002368
408.937248	15854.174839	30.007386
409.466593	15875.666848	30.012404
409.477068	15897.792871	30.017421
410.117989	15920.638192	30.022439
410.446881	15955.461664	30.027456
410.669239	15981.208857	30.032474
411.577797	16010.247041	30.037492
412.166758	16041.789413	30.042509
412.221912	16060.162754	30.047527
413.139351	16077.232435	30.052544
413.343276	16099.830578	30.057562
413.681382	16118.165971	30.062580
414.072906	16139.885161	30.067597
414.237843	16160.632329	30.072615
415.069482	16177.036477	30.077632
415.698943	16212.779816	30.082650
416.039491	16232.874185	30.087668
416.628857	16250.150173	30.092685
416.322303	16271.975697	30.097703
417.226913	16287.348333	30.102720
417.771349	16314.662650	30.107738
418.045492	16321.609404	30.112756
418.082730	16349.281159	30.117773
418.620522	16384.751757	30.122791
419.277134	16392.115558	30.127808
419.964370	16418.065307	30.132826
420.345173	16435.143561	30.137844
420.878640	16452.523241	30.142861
421.085520	16465.162681	30.147879
421.823724	16479.509764	30.152896
421.688165	16500.487559	30.157914
421.994669	16512.283903	30.162932
422.389927	16537.486768	30.167949
422.710491	16554.126058	30.172967
423.407258	16569.815742	30.177984
423.762038	16602.782296	30.183002
424.194738	16607.041704	30.188020
424.483372	16630.615813	30.193037
424.990740	16646.066753	30.198055
425.374985	16662.702480	30.203072
425.842178	16694.726141	30.208090
426.469074	16710.632187	30.213108
426.779841	16725.690744	30.218125
426.946636	16743.172340	30.223143
427.481578	16769.626515	30.228160
427.645548	16793.829947	30.233178
428.059754	16802.991178	30.238196
428.396317	16833.241484	30.243213
428.685326	16868.278162	30.248231
429.511132	16891.553671	30.253248
429.942156	16919.739420	30.258266
430.444816	16936.931694	30.263284
430.963413	16961.850477	30.268301
430.424124	16985.068283	30.273319
431.615840	17004.910113	30.278336
431.819355	17038.858152	30.283354
432.338316	17063.483263	30.288372
432.947108	17090.810714	30.293389
433.059692	17122.764287	30.298407
433.858136	17144.294532	30.303424
433.782840	17176.366063	30.308442
434.563001	17203.433095	30.313460
434.834918	17236.928565	30.318477
435.398765	17270.258340	30.323495
436.148879	17284.657858	30.328512
436.479993	17306.356242	30.333530
436.953453	17338.746391	30.338548
437.326475	17362.466109	30.343565
437.787055	17387.871483	30.348583
438.458665	17401.973840	30.353600
438.836207	17438.491718	30.358618
439.478296	17461.341850	30.363636
440.046932	17482.769490	30.368653
440.071491	17506.272322	30.373671
440.756914	17528.938862	30.378688
441.066707	17555.410430	30.383706
441.522774	17569.098142	30.388724
442.205306	17593.489838	30.393741
442.551829	17613.290957	30.398759
442.657704	17635.770436	30.403776
442.984607	17660.350584	30.408794
443.755822	17685.480271	30.413812
444.480386	17715.298463	30.418829
444.512591	17737.852773	30.423847
445.349151	17755.385155	30.428864
446.011348	17772.313126	30.433882
446.384347	17792.047108	30.438900
446.794972	17805.243031	30.443917
447.146539	17838.948178	30.448935
447.847199	17848.958953	30.453952
448.679172	17865.847780	30.458970
448.917681	17874.585347	30.463988
449.326334	17885.741110	30.469005
448.786133	17902.762767	30.474023
450.029891	17919.574508	30.479040
450.201053	17940.565837	30.484058
450.935276	17959.251573	30.489076
451.969757	17967.807653	30.494093
451.903601	17991.862265	30.499111
452.478075	18008.538851	30.504128
452.750813	18022.464076	30.509146
452.463596	18033.760507	30.514164
453.305979	18049.776054	30.519181
453.688700	18078.138474	30.524199
454.001631	18090.244335	30.529216
453.955380	18112.805053	30.534234
454.357377	18139.010278	30.539252
454.969150	18162.447200	30.544269
455.495114	18190.534648	30.549287
455.737304	18216.973487	30.554304
456.264717	18257.152554	30.559322
456.425266	18278.190134	30.564340
457.309549	18294.142464	30.569357
457.493195	18326.573344	30.574375
458.335067	18356.715301	30.579392
458.571616	18388.449383	30.584410
459.079276	18419.130238	30.589428
459.485196	18432.586349	30.594445
459.933375	18476.909990	30.599463
460.194997	18504.527570	30.604480
460.789344	18526.464069	30.609498
461.235444	18556.327174	30.614516
461.926667	18581.249438	30.619533
462.072961	18620.105387	30.624551
463.205542	18644.301567	30.629568
463.851954	18673.444852	30.634586
463.884047	18705.009309	30.639604
464.607556	18721.467319	30.644621
464.856088	18750.230800	30.649639
465.385230	18779.083045	30.654656
465.949056	18803.008397	30.659674
466.325020	18828.239385	30.664692
467.082919	18852.791445	30.669709
467.326796	18877.171337	30.674727
467.565778	18906.631497	30.679744
468.511616	18924.387902	30.684762
468.874099	18946.835025	30.689780
469.664904	18970.889296	30.694797
469.960476	18997.428237	30.699815
470.204735	19023.406651	30.704832
470.926688	19045.165805	30.709850
471.393408	19063.597573	30.714868
472.210138	19082.492596	30.719885
472.198693	19113.148451	30.724903
472.625261	19132.249943	30.729920
473.137518	19153.599816	30.734938
473.624281	19186.332133	30.739956
474.062261	19210.233474	30.744973
474.733002	19234.041526	30.749991
474.979424	19260.203135	30.755008
475.852833	19282.020965	30.760026
476.136870	19311.954840	30.765044
476.668882	19319.503552	30.770061
477.046765	19348.860493	30.775079
477.160827	19373.634095	30.780096
477.904638	19400.116014	30.785114
478.292547	19425.484899	30.790132
478.778520	19449.119982	30.795149
479.009461	19480.136478	30.800167
479.663747	19504.345469	30.805184
480.203038	19541.031505	30.810202
480.694437	19571.381874	30.815220
481.159470	19590.452519	30.820237
481.758578	19619.269779	30.825255
481.888365	19647.926825	30.830272
482.239087	19683.884506	30.835290
482.562763	19711.847886	30.840308
483.284991	19731.655501	30.845325
483.949542	19753.348623	30.850343
484.207568	19786.300997	30.855360
484.599428	19808.074799	30.860378
484.994424	19834.713032	30.865396
485.654449	19857.335732	30.870413
486.292673	19889.735922	30.875431
486.682788	19909.444102	30.880448
486.827870	19931.496780	30.885466
487.734757	19963.545427	30.890484
487.991323	19991.292267	30.895501
488.500773	20010.419547	30.900519
489.115366	20047.922414	30.905536
489.924948	20067.779870	30.910554
490.107431	20099.822157	30.915572
490.508101	20115.990737	30.920589
490.907607	20146.053121	30.925607
491.467105	20180.715385	30.930624
492.000751	20200.710968	30.935642
492.317185	20242.980580	30.940660
493.151492	20261.589680	30.945677
493.934744	20296.672014	30.950695
494.127355	20309.537333	30.955712
494.858123	20345.752616	30.960730
495.464334	20369.660618	30.965748
496.285684	20392.372399	30.970765
496.716995	20419.656519	30.975783
497.056965	20448.698820	30.980800
497.560378	20466.886074	30.985818
497.872120	20503.571647	30.990836
498.526753	20521.438308	30.995853
498.996522	20540.117407	31.000871
499.314581	20564.601515	31.005888
499.728923	20589.866678	31.010906
500.161068	20619.994178	31.015924
500.821376	20640.659068	31.020941
500.793350	20667.863838	31.025959
501.646447	20705.494884	31.030976
502.406407	20730.920920	31.035994
502.624800	20761.398033	31.041012
503.193066	20784.592194	31.046029
503.841847	20817.838927	31.051047
504.149562	20848.681288	31.056064
504.767501	20878.527350	31.061082
505.167925	20914.523733	31.066100
505.897476	20937.414804	31.071117
506.415763	20963.801482	31.076135
506.758099	20987.934803	31.081152
507.464002	21025.159864	31.086170
507.424478	21056.303355	31.091188
508.089240	21084.171042	31.096205
508.551096	21115.084455	31.101223
509.430713	21139.146447	31.106240
509.604589	21173.453845	31.111258
510.279093	21206.905718	31.116276
511.163291	21228.888319	31.121293
511.715958	21264.059048	31.126311
511.990956	21300.619175	31.131328
512.496461	21314.491339	31.136346
512.805510	21348.904241	31.141364
513.282323	21378.621522	31.146381
514.152405	21396.316230	31.151399
514.217733	21429.529010	31.156416
515.114372	21451.933257	31.161434
515.557422	21491.159126	31.166452
516.248390	21518.492564	31.171469
516.798531	21545.683813	31.176487
516.991277	21577.170863	31.181504
517.621021	21593.127862	31.186522
518.108465	21611.672522	31.191540
518.914805	21638.905915	31.196557
519.431596	21655.297686	31.201575
519.891314	21674.270095	31.206592
520.973358	21694.023345	31.211610
520.995218	21705.608361	31.216628
521.217258	21722.842503	31.221645
521.802529	21746.401619	31.226663
522.620579	21777.228691	31.231680
522.912211	21797.472324	31.236698
523.113727	21819.783666	31.241716
523.715118	21847.302195	31.246733
524.437887	21872.767130	31.251751
524.633452	21912.980406	31.256768
525.181769	21932.090837	31.261786
525.712331	21957.807140	31.266804
525.951087	21992.800861	31.271821
526.527204	22016.494428	31.276839
527.107059	22053.273588	31.281856
527.752771	22088.330115	31.286874
528.152034	22120.322781	31.291892
529.013984	22159.345357	31.296909
529.197727	22191.302386	31.301927
529.848094	22222.845166	31.306944
530.094223	22259.165155	31.311962
530.910924	22285.696430	31.316980
531.276546	22324.594865	31.321997
532.133006	22355.138795	31.327015
532.577198	22398.372444	31.332032
533.206148	22423.732725	31.337050
533.580647	22458.592269	31.342068
534.174264	22492.090586	31.347085
534.860830	22516.374068	31.352103
535.553096	22546.394265	31.357120
536.191171	22573.225617	31.362138
536.429352	22602.331266	31.367156
536.906227	22633.118325	31.372173
537.617000	22661.903604	31.377191
538.340146	22697.429324	31.382208
538.693236	22723.515644	31.387226
539.578427	22754.915072	31.392244
539.771689	22781.778461	31.397261
540.567958	22807.068795	31.402279
540.888771	22839.251841	31.407296
541.231711	22877.295527	31.412314
542.093339	22906.373486	31.417332
542.829301	22937.076207	31.422349
543.475537	22973.549685	31.427367
543.796436	23002.358607	31.432384
543.967474	23019.924139	31.437402
544.544942	23051.094194	31.442420
545.457305	23084.101254	31.447437
546.183349	23108.752107	31.452455
546.411012	23148.640587	31.457472
546.864154	23167.192080	31.462490
547.231821	23205.276755	31.467508
547.807393	23238.760203	31.472525
548.558400	23268.759656	31.477543
548.834315	23309.595092	31.482560
549.046822	23336.753216	31.487578
549.969496	23378.953547	31.492596
550.710093	23404.518770	31.497613
551.370705	23440.137763	31.502631
551.803097	23477.081684	31.507648
552.523127	23508.242767	31.512666
553.127172	23536.641601	31.517684
553.429077	23568.133672	31.522701
553.814609	23590.007433	31.527719
554.382099	23625.129483	31.532736
555.167612	23646.782681	31.537754
555.754870	23673.433903	31.542772
555.888606	23703.726587	31.547789
556.640715	23728.803839	31.552807
557.262726	23754.710370	31.557824
557.766656	23776.471003	31.562842
558.629469	23805.474264	31.567860
558.817149	23828.548348	31.572877
559.500106	23858.944829	31.577895
559.886376	23893.716575	31.582912
560.263180	23917.222454	31.587930
561.364184	23947.496723	31.592948
561.693532	23977.677035	31.597965
562.445688	24011.273152	31.602983
562.948772	24039.467339	31.608000
563.412658	24073.449957	31.613018
564.168311	24098.994757	31.618036
564.295155	24139.659338	31.623053
565.237114	24172.783641	31.628071
565.666036	24207.309115	31.633088
565.888890	24227.306901	31.638106
566.698307	24264.648232	31.643124
566.872230	24306.045154	31.648141
567.567338	24337.685399	31.653159
568.235721	24377.374601	31.658176
569.102542	24415.806817	31.663194
569.686475	24440.841791	31.668212
569.896702	24478.605981	31.673229
570.563853	24503.425775	31.678247
571.323382	24550.836163	31.683264
572.049553	24572.221602	31.688282
572.622462	24601.758032	31.693300
573.076219	24647.908387	31.698317
573.765611	24677.748985	31.703335
574.203522	24712.115932	31.708352
575.109202	24748.924884	31.713370
575.782634	24781.997461	31.718388
576.044952	24821.839616	31.723405
576.683706	24846.304065	31.728423
577.437847	24873.480563	31.733440
577.914999	24908.423109	31.738458
578.978682	24930.862014	31.743476
579.117306	24971.551715	31.748493
579.763519	24995.471686	31.753511
580.171707	25028.478776	31.758528
581.008110	25064.022578	31.763546
581.645913	25079.285959	31.768564
582.149830	25123.268208	31.773581
582.850523	25155.635643	31.778599
583.579229	25185.748910	31.783616
583.866931	25213.618257	31.788634
584.796880	25244.610141	31.793652
585.204959	25279.570471	31.798669
585.756415	25297.685124	31.803687
586.208740	25328.985774	31.808704
586.377760	25364.590393	31.813722
587.451252	25390.858085	31.818740
587.982513	25421.527174	31.823757
588.434828	25460.784694	31.828775
588.954245	25484.516552	31.833792
589.407393	25526.396806	31.838810
589.756048	25559.192897	31.843828
590.583583	25585.354008	31.848845
591.392409	25619.165146	31.853863
591.978960	25650.028161	31.858880
592.437461	25688.286613	31.863898
592.937045	25723.214423	31.868916
593.399398	25751.847154	31.873933
594.477498	25779.903175	31.878951
594.877712	25812.855923	31.883968
595.499054	25839.068617	31.888986
595.685473	25858.959976	31.894004
596.220873	25901.321085	31.899021
596.678848	25913.661837	31.904039
597.188632	25948.778040	31.909056
597.800750	25989.597882	31.914074
598.755824	26021.250631	31.919092
599.208559	26062.936145	31.924109
599.549504	26101.548753	31.929127
600.275724	26151.761594	31.934144
600.893883	26179.662685	31.939162
601.404485	26208.452829	31.944180
602.295859	26260.213774	31.949197
603.059863	26285.222849	31.954215
603.584972	26335.998534	31.959232
604.100439	26363.644197	31.964250
604.817301	26395.973175	31.969268
605.425420	26435.631641	31.974285
605.835725	26467.730659	31.979303
606.826407	26502.589227	31.984320
607.194360	26538.632453	31.989338
608.009436	26571.869077	31.994356
608.608404	26612.281425	31.999373
608.948564	26644.789882	32.004391
609.745815	26677.485934	32.009408
610.068093	26715.123003	32.014426
610.970862	26755.747188	32.019444
611.693350	26793.802064	32.024461
612.543415	26830.585618	32.029479
613.060058	26867.282411	32.034496
613.590234	26898.769233	32.039514
614.675801	26925.618509	32.044532
615.213496	26968.000456	32.049549
615.443916	26995.483055	32.054567
616.380174	27025.098865	32.059584
616.792179	27067.772479	32.064602
617.438067	27097.958460	32.069620
617.848881	27136.378809	32.074637
618.598720	27172.919548	32.079655
619.217829	27196.258585	32.084672
619.781789	27235.413583	32.089690
620.648936	27273.029559	32.094708
620.990225	27306.322630	32.099725
622.049604	27344.496431	32.104743
622.718359	27376.120302	32.109760
623.195862	27405.239677	32.114778
623.916835	27431.849665	32.119796
624.343068	27468.599628	32.124813
625.010693	27498.428855	32.129831
626.009956	27528.541174	32.134848
626.534128	27572.538224	32.139866
627.483557	27596.489644	32.144884
627.797861	27628.927881	32.149901
628.345595	27654.522407	32.154919
629.107697	27686.119502	32.159936
629.271036	27733.169344	32.164954
629.984416	27748.871675	32.169972
630.382895	27785.664481	32.174989
631.281493	27826.898242	32.180007
632.022883	27857.089358	32.185024
632.518631	27891.332567	32.190042
633.199696	27923.479973	32.195060
633.543949	27957.961921	32.200077
634.118024	28001.187288	32.205095
635.124558	28018.354549	32.210112
635.198063	28072.814388	32.215130
636.158551	28092.946988	32.220148
636.794165	28126.245872	32.225165
636.996768	28150.921691	32.230183
637.774942	28179.584242	32.235200
638.082366	28224.103338	32.240218
638.799925	28266.440862	32.245236
639.845365	28296.268977	32.250253
640.252849	28330.520426	32.255271
640.690577	28357.213911	32.260288
641.209630	28399.747138	32.265306
641.596562	28439.753875	32.270324
642.630786	28486.688027	32.275341
643.039994	28523.075953	32.280359
643.341945	28570.845548	32.285376
644.262696	28620.610538	32.290394
644.902212	28671.443667	32.295412
645.711409	28702.624110	32.300429
646.558675	28745.315243	32.305447
647.102667	28782.788674	32.310464
647.885759	28832.771685	32.315482
648.788354	28863.179240	32.320500
649.383728	28909.544680	32.325517
650.122480	28949.010606	32.330535
650.708577	28989.296953	32.335552
651.235145	29029.927711	32.340570
652.205117	29066.829274	32.345588
652.808880	29100.937498	32.350605
653.086250	29144.116935	32.355623
654.009071	29176.765738	32.360640
654.365903	29220.242619	32.365658
655.194062	29268.652027	32.370676
656.126320	29312.449854	32.375693
656.752105	29343.040537	32.380711
657.708370	29386.626168	32.385728
658.346737	29418.207399	32.390746
659.203847	29457.611522	32.395764
659.481085	29485.216562	32.400781
660.357146	29523.372589	32.405799
660.997010	29550.693369	32.410816
661.410313	29598.688121	32.415834
662.487611	29634.910183	32.420852
663.124968	29675.189850	32.425869
663.856670	29710.220901	32.430887
664.567525	29744.522022	32.435904
664.936795	29782.878001	32.440922
665.942676	29817.107756	32.445940
666.386635	29845.388823	32.450957
667.000798	29889.648576	32.455975
667.852950	29921.045391	32.460992
668.279243	29965.808822	32.466010
669.042080	29998.616736	32.471028
669.252387	30038.388760	32.476045
670.249371	30081.672392	32.481063
671.111333	30121.766048	32.486080
671.558989	30156.393533	32.491098
672.230534	30191.150367	32.496116
672.911128	30236.317051	32.501133
673.465598	30280.422639	32.506151
673.969894	30307.222021	32.511168
674.457355	30352.905949	32.516186
675.311445	30397.211397	32.521204
676.361173	30434.083966	32.526221
677.006686	30480.647383	32.531239
677.358234	30519.993646	32.536256
678.173299	30562.864281	32.541274
678.909556	30594.906095	32.546292
679.723369	30638.364976	32.551309
680.316076	30667.546807	32.556327
681.131007	30693.994616	32.561344
681.424982	30724.841604	32.566362
681.838241	30766.587151	32.571380
682.529279	30799.723660	32.576397
683.023490	30844.813399	32.581415
683.940171	30884.893650	32.586432
684.910367	30930.256717	32.591450
685.720410	30958.374514	32.596468
686.126402	30991.100819	32.601485
686.573518	31031.166387	32.606503
687.172596	31070.582400	32.611520
688.074476	31112.011904	32.616538
688.862918	31161.285395	32.621556
689.315205	31194.238670	32.626573
689.984503	31241.546026	32.631591
690.517113	31282.964163	32.636608
691.561384	31326.205072	32.641626
692.296193	31366.605535	32.646644
692.982609	31411.634799	32.651661
693.398699	31460.632265	32.656679
694.113125	31493.804154	32.661696
694.989429	31546.800929	32.666714
695.355469	31596.242751	32.671732
696.484819	31631.417088	32.676749
697.235957	31676.278748	32.681767
698.090353	31717.179549	32.686784
699.226636	31765.097719	32.691802
699.859796	31795.159855	32.696820
700.556335	31829.858634	32.701837
701.494878	31884.686170	32.706855
702.068513	31904.137131	32.711872
703.011207	31948.748118	32.716890
703.618688	31983.682366	32.721908
704.701942	32009.976045	32.726925
705.048347	32053.713393	32.731943
705.545141	32093.115757	32.736960
706.332837	32123.236352	32.741978
707.001608	32155.860122	32.746996
707.909235	32194.774774	32.752013
708.434940	32241.961491	32.757031
709.046617	32277.755358	32.762048
709.903170	32312.948285	32.767066
710.433713	32358.187348	32.772084
711.061571	32384.995357	32.777101
711.749131	32432.378428	32.782119
712.241464	32459.517534	32.787136
713.598538	32502.237759	32.792154
714.058568	32541.261085	32.797172
714.950504	32588.903319	32.802189
715.145860	32627.178000	32.807207
715.802421	32666.063307	32.812224
716.709150	32706.003228	32.817242
717.126191	32760.067580	32.822260
717.975041	32808.810784	32.827277
718.456385	32847.028436	32.832295
719.262876	32889.184500	32.837312
720.218668	32926.423935	32.842330
720.601148	32980.601746	32.847348
721.806855	33018.990774	32.852365
722.018022	33073.246228	32.857383
722.964698	33121.456423	32.862400
724.048222	33164.366255	32.867418
724.591776	33209.175212	32.872436
725.746508	33251.599906	32.877453
726.158695	33284.543802	32.882471
727.038096	33309.783625	32.887488
728.256023	33350.611739	32.892506
728.749863	33381.469298	32.897524
729.783255	33404.232079	32.902541
730.406414	33437.351812	32.907559
730.725406	33458.197073	32.912576
731.750182	33493.068500	32.917594
731.852936	33528.147597	32.922612
732.891212	33553.824365	32.927629
733.106801	33590.687758	32.932647
733.798378	33624.625299	32.937664
734.828550	33659.028305	32.942682
735.313961	33700.774754	32.947700
735.980562	33742.233694	32.952717
736.693529	33778.431547	32.957735
737.622614	33825.312093	32.962752
738.300803	33866.763142	32.967770
738.580406	33913.461085	32.972788
739.882271	33947.992724	32.977805
740.661708	33991.489280	32.982823
740.974998	34039.851356	32.987840
741.909904	34082.849570	32.992858
742.827992	34129.694584	32.997876
743.787525	34163.761743	33.002893
744.099580	34208.817729	33.007911
744.971010	34264.743169	33.012928
745.867056	34293.743484	33.017946
746.420142	34346.842236	33.022964
747.533507	34381.366173	33.027981
748.311198	34428.202225	33.032999
748.677555	34460.503915	33.038016
749.783521	34503.634267	33.043034
750.066677	34551.622879	33.048052
751.172275	34602.150961	33.053069
751.805866	34656.356993	33.058087
752.704781	34707.126340	33.063104
753.433426	34743.399271	33.068122
754.042724	34799.253370	33.073140
755.039778	34832.790954	33.078157
755.525743	34881.684317	33.083175
756.208269	34925.311787	33.088192
757.121438	34971.843307	33.093210
757.968161	35023.702779	33.098228
759.144203	35064.009675	33.103245
759.354396	35115.589684	33.108263
760.231521	35152.978170	33.113280
761.178391	35203.545194	33.118298
762.026035	35259.818429	33.123316
762.852958	35305.441056	33.128333
763.627689	35336.668479	33.133351
763.863011	35380.670416	33.138368
765.029636	35425.304320	33.143386
765.893824	35474.683593	33.148404
766.720483	35522.153015	33.153421
767.570233	35559.900590	33.158439
767.826831	35604.241097	33.163456
768.921284	35645.750592	33.168474
769.698831	35696.269433	33.173492
770.622338	35721.827721	33.178509
771.601625	35773.276247	33.183527
771.936922	35824.262995	33.188544
772.949171	35858.476390	33.193562
773.378705	35913.115943	33.198580
774.326825	35949.735956	33.203597
775.332814	35988.560038	33.208615
776.007484	36027.461366	33.213632
776.696848	36071.501125	33.218650
776.753727	36124.195160	33.223668
777.832992	36175.382404	33.228685
778.882638	36220.422012	33.233703
779.654380	36260.762884	33.238720
780.558218	36289.088146	33.243738
780.919014	36329.208958	33.248756
781.368604	36364.788556	33.253773
782.414113	36397.125956	33.258791
782.789490	36460.627838	33.263808
784.303970	36492.114192	33.268826
785.160610	36529.963586	33.273844
785.577912	36566.022817	33.278861
786.255869	36610.432225	33.283879
787.192906	36658.196739	33.288896
787.586252	36702.935454	33.293914
788.335368	36750.002426	33.298932
789.288867	36796.171206	33.303949
790.275761	36836.675500	33.308967
790.676587	36890.272385	33.313984
791.958386	36937.129889	33.319002
792.872114	36984.177924	33.324020
793.482177	37022.250182	33.329037
794.763510	37076.942708	33.334055
795.130522	37120.769531	33.339072
796.140073	37168.776770	33.344090
796.699558	37211.953947	33.349108
797.668052	37263.173797	33.354125
798.653101	37308.314350	33.359143
799.640023	37361.940782	33.364160
799.875336	37396.834780	33.369178
800.864766	37448.032824	33.374196
801.654227	37491.933372	33.379213
802.828004	37535.596771	33.384231
803.530822	37585.309735	33.389248
804.393894	37635.775516	33.394266
805.111781	37683.241493	33.399284
805.599131	37734.563108	33.404301
806.476466	37772.392494	33.409319
807.014129	37823.889828	33.414336
808.073636	37879.985040	33.419354
809.079215	37925.566333	33.424372
809.766460	37966.366312	33.429389
810.765955	38023.919410	33.434407
811.610942	38069.228943	33.439424
812.168805	38122.178272	33.444442
813.043113	38171.056309	33.449460
813.665763	38223.976772	33.454477
815.398360	38265.815133	33.459495
815.863176	38320.651343	33.464512
816.330542	38363.744083	33.469530
817.496973	38416.276328	33.474548
818.255286	38456.983901	33.479565
818.897940	38506.822247	33.484583
819.546938	38555.774382	33.489600
820.538028	38607.076112	33.494618
820.948047	38661.295710	33.499636
822.081407	38704.746483	33.504653
823.212833	38756.798105	33.509671
824.202438	38790.305151	33.514688
825.314383	38826.866500	33.519706
826.166603	38874.143325	33.524724
827.469823	38900.303653	33.529741
828.281276	38936.260880	33.534759
829.135214	38974.336355	33.539776
830.155024	39005.834321	33.544794
830.833404	39046.289920	33.549812
831.612428	39081.929946	33.554829
832.341560	39111.620664	33.559847
832.641229	39152.584765	33.564864
833.603769	39187.127476	33.569882
834.183849	39230.950529	33.574900
834.755171	39275.350528	33.579917
835.550631	39297.884976	33.584935
836.047692	39342.815312	33.589952
836.970008	39384.055470	33.594970
836.973624	39430.075102	33.599988
837.914116	39472.507831	33.605005
838.750575	39524.822513	33.610023
839.803720	39574.908926	33.615040
840.224573	39628.566406	33.620058
841.087129	39692.197586	33.625076
841.788534	39734.086444	33.630093
842.960460	39793.748504	33.635111
843.847352	39853.992917	33.640128
844.785122	39903.010395	33.645146
845.643290	39958.731469	33.650164
846.507471	40021.952286	33.655181
847.452556	40069.881227	33.660199
847.884830	40136.338457	33.665216
849.260427	40187.716539	33.670234
850.071584	40242.471762	33.675252
850.778261	40303.915637	33.680269
851.903055	40356.490741	33.685287
852.494035	40408.017502	33.690304
853.726213	40457.995703	33.695322
854.677885	40514.487781	33.700340
855.067645	40571.409510	33.705357
856.440845	40620.177016	33.710375
857.007138	40670.266297	33.715392
858.145844	40727.912309	33.720410
858.872630	40777.515022	33.725428
859.883677	40835.655642	33.730445
861.075214	40889.998760	33.735463
862.241107	40938.799442	33.740480
862.895935	40993.125666	33.745498
863.686461	41036.919407	33.750516
864.542954	41089.082926	33.755533
865.613293	41126.736173	33.760551
866.197903	41174.572201	33.765568
867.012941	41226.862707	33.770586
868.338627	41282.874463	33.775604
868.917292	41336.182556	33.780621
869.726186	41377.615022	33.785639
870.681964	41428.846735	33.790656
871.502252	41470.676046	33.795674
872.855089	41515.141655	33.800692
873.364970	41570.459684	33.805709
874.471623	41611.529735	33.810727
875.343670	41671.515857	33.815744
876.168977	41717.721555	33.820762
877.006300	41763.071630	33.825780
877.835506	41816.297387	33.830797
879.059015	41850.904667	33.835815
879.792350	41905.378981	33.840832
880.316587	41947.255559	33.845850
881.875858	41991.114257	33.850868
882.352946	42040.626111	33.855885
883.208798	42086.947977	33.860903
883.730872	42135.744620	33.865920
884.667965	42184.798954	33.870938
885.835275	42242.425505	33.875956
886.576176	42284.395297	33.880973
887.490020	42339.639359	33.885991
888.853683	42380.057093	33.891008
889.322703	42417.420898	33.896026
890.813850	42456.926998	33.901044
891.495125	42513.485550	33.906061
892.228722	42548.651341	33.911079
892.843545	42602.526093	33.916096
893.524741	42636.087359	33.921114
894.746895	42668.242048	33.926132
895.003336	42708.972909	33.931149
895.991691	42755.167909	33.936167
896.866481	42801.500965	33.941184
897.421877	42851.103580	33.946202
898.582824	42892.003077	33.951220
899.155542	42945.164201	33.956237
899.905751	42994.799886	33.961255
901.016157	43058.711976	33.966272
901.610863	43109.966196	33.971290
902.678481	43160.773302	33.976308
903.574931	43220.494169	33.981325
904.320830	43275.779524	33.986343
905.424227	43329.731352	33.991360
906.237421	43391.628932	33.996378
907.200789	43441.997594	34.001396
907.844110	43508.925349	34.006413
908.875557	43574.641336	34.011431
909.910212	43632.665482	34.016448
910.720214	43687.682492	34.021466
911.887829	43731.289724	34.026484
913.053487	43808.864310	34.031501
914.065972	43858.916289	34.036519
914.793837	43919.025980	34.041536
915.678010	43974.234499	34.046554
917.325468	44028.982069	34.051572
918.398968	44088.373934	34.056589
918.927615	44123.365584	34.061607
920.155994	44180.734616	34.066624
921.079329	44237.063582	34.071642
922.068473	44268.219717	34.076660
923.092119	44323.084666	34.081677
924.055956	44368.825117	34.086695
925.205917	44410.994241	34.091712
925.765242	44458.487122	34.096730
927.089713	44511.312898	34.101748
928.136488	44568.470997	34.106765
928.992669	44605.967640	34.111783
930.005457	44643.996474	34.116800
930.601219	44683.880807	34.121818
931.835181	44728.517007	34.126836
932.598394	44779.014927	34.131853
933.437148	44822.220354	34.136871
934.399999	44870.036790	34.141888
935.234493	44928.215848	34.146906
936.531658	44967.541745	34.151924
936.950795	45019.068233	34.156941
938.110367	45062.344080	34.161959
939.255124	45118.950566	34.166976
939.848037	45168.027448	34.171994
940.638993	45219.761860	34.177012
941.612064	45272.106776	34.182029
942.279552	45322.272998	34.187047
943.517738	45373.634104	34.192064
943.909726	45433.996570	34.197082
945.497582	45490.825606	34.202100
946.330608	45541.738147	34.207117
947.382391	45595.102603	34.212135
948.583239	45646.520789	34.217152
949.231443	45698.392525	34.222170
950.206573	45745.848339	34.227188
951.122286	45793.680459	34.232205
952.184483	45847.303247	34.237223
952.900846	45894.230561	34.242240
954.028874	45959.577882	34.247258
954.700961	46001.495890	34.252276
955.960679	46043.435835	34.257293
956.750134	46090.579850	34.262311
957.834112	46129.036560	34.267328
958.334106	46170.045584	34.272346
959.042375	46208.308217	34.277364
960.069561	46263.360831	34.282381
960.729474	46315.074007	34.287399
962.047499	46365.823915	34.292416
963.112136	46423.705127	34.297434
963.889943	46466.733489	34.302452
964.762545	46528.801270	34.307469
965.485325	46578.442901	34.312487
966.886415	46636.126479	34.317504
967.673863	46686.947535	34.322522
968.664130	46733.511082	34.327540
969.862815	46803.259117	34.332557
970.535001	46857.970221	34.337575
971.586233	46913.134531	34.342592
972.210624	46969.004755	34.347610
973.588859	47028.280796	34.352628
974.663707	47094.202772	34.357645
975.679076	47143.009053	34.362663
976.635525	47200.624517	34.367680
977.582932	47257.874618	34.372698
978.914408	47311.148744	34.377716
979.832292	47376.381246	34.382733
980.496956	47426.457705	34.387751
981.442734	47477.989606	34.392768
982.640831	47544.355421	34.397786
983.653657	47589.746823	34.402804
984.795651	47654.147911	34.407821
985.458606	47713.689576	34.412839
986.655349	47767.359131	34.417856
987.489066	47826.267018	34.422874
988.461289	47891.524127	34.427892
989.520565	47947.973974	34.432909
990.605073	48005.919393	34.437927
991.404907	48068.230544	34.442944
992.790627	48136.428713	34.447962
993.918372	48184.359234	34.452980
994.623727	48246.318726	34.457997
995.745341	48307.820964	34.463015
996.975794	48364.611988	34.468032
998.032918	48428.465493	34.473050
999.127876	48469.474101	34.478068
999.967186	48534.051608	34.483085
1000.967245	48590.993150	34.488103
1002.324234	48643.374353	34.493120
1003.081538	48698.962303	34.498138
1003.815605	48755.522014	34.503156
1004.929077	48812.806976	34.508173
1005.664367	48875.092479	34.513191
1007.039777	48927.193074	34.518208
1007.775740	48990.725159	34.523226
1009.157292	49040.876406	34.528244
1010.042547	49100.386890	34.533261
1010.681538	49156.083053	34.538279
1012.262009	49205.178571	34.543296
1013.082597	49260.087334	34.548314
1014.489449	49314.676670	34.553332
1015.511552	49375.773469	34.558349
1016.367716	49428.260197	34.563367
1017.571953	49476.776190	34.568384
1018.430600	49534.191435	34.573402
1019.412798	49575.523381	34.578420
1020.487869	49634.220995	34.583437
1021.390194	49688.896545	34.588455
1022.645016	49736.785127	34.593472
1023.491637	49790.387727	34.598490
1024.143890	49836.396837	34.603508
1025.419764	49873.134222	34.608525
1025.997842	49928.379925	34.613543
1027.609182	49970.525174	34.618560
1028.483542	50021.510901	34.623578
1029.341755	50059.282017	34.628596
1030.286146	50115.362934	34.633613
1030.821083	50170.179404	34.638631
1032.113758	50214.197199	34.643648
1032.808172	50269.558377	34.648666
1033.694601	50328.660603	34.653684
1035.015222	50386.391605	34.658701
1035.995444	50446.447503	34.663719
1037.053376	50500.961425	34.668736
1037.982678	50561.531771	34.673754
1038.966040	50626.073637	34.678772
1040.351837	50681.928645	34.683789
1040.873926	50758.634461	34.688807
1041.923374	50810.417066	34.693824
1043.193721	50881.634282	34.698842
1044.492491	50940.255915	34.703860
1045.576596	50991.046440	34.708877
1046.531612	51059.966138	34.713895
1047.746031	51113.836929	34.718912
1048.588706	51172.549543	34.723930
1049.660639	51232.270431	34.728948
1051.272010	51300.088355	34.733965
1052.334250	51366.771259	34.738983
1053.537745	51422.378195	34.744000
1054.563761	51480.366866	34.749018
1055.426324	51535.869265	34.754036
1056.698426	51588.726064	34.759053
1057.544946	51643.263127	34.764071
1058.334437	51701.922133	34.769088
1059.730106	51771.382400	34.774106
1060.887316	51837.621517	34.779124
1062.352294	51898.206408	34.784141
1063.001231	51964.860827	34.789159
1064.048397	52012.432305	34.794176
1065.242791	52067.921991	34.799194
1066.409698	52128.149182	34.804212
1067.429161	52184.349917	34.809229
1068.348985	52246.134734	34.814247
1069.531288	52307.821671	34.819264
1070.863348	52361.208695	34.824282
1071.770523	52414.396600	34.829300
1073.128200	52475.854039	34.834317
1074.055357	52531.620796	34.839335
1075.170583	52576.341616	34.844352
1076.444437	52640.989148	34.849370
1077.251503	52693.864319	34.854388
1078.497328	52749.739901	34.859405
1079.279786	52815.338087	34.864423
1080.879713	52870.892752	34.869440
1081.729195	52926.596681	34.874458
1082.511977	52976.109877	34.879476
1083.777989	53027.762279	34.884493
1084.895351	53099.681004	34.889511
1086.050582	53153.432907	34.894528
1087.107255	53208.016667	34.899546
1087.733929	53267.394847	34.904564
1089.416016	53322.855462	34.909581
1090.362763	53377.830178	34.914599
1091.263077	53434.615768	34.919616
1091.992428	53494.851712	34.924634
1093.159501	53551.209812	34.929652
1094.576840	53618.216918	34.934669
1095.393166	53675.921151	34.939687
1096.523417	53719.192684	34.944704
1097.931158	53770.223372	34.949722
1098.701984	53820.157876	34.954740
1099.673493	53868.656229	34.959757
1100.408478	53932.296933	34.964775
1101.746625	53983.389605	34.969792
1102.450815	54036.037115	34.974810
1103.388838	54102.576425	34.979828
1104.600474	54152.853954	34.984845
1105.614317	54213.401577	34.989863
1106.591103	54278.910148	34.994880
1107.849701	54337.546621	34.999898
1108.636445	54411.571471	35.004916
1110.297733	54480.213501	35.009933
1111.341884	54541.636852	35.014951
1112.344620	54602.130257	35.019968
1113.548844	54660.041962	35.024986
1114.446890	54740.916643	35.030004
1115.931218	54802.714743	35.035021
1116.817787	54865.752025	35.040039
1118.253472	54929.500883	35.045056
1119.490294	54998.761445	35.050074
1120.513672	55061.018420	35.055092
1121.907479	55126.521010	35.060109
1123.422424	55190.353089	35.065127
1124.105315	55254.397876	35.070144
1125.573193	55301.555771	35.075162
1126.509266	55367.497742	35.080180
1127.543141	55423.444508	35.085197
1129.030792	55485.243873	35.090215
1130.147064	55553.860436	35.095232
1131.531417	55605.759445	35.100250
1132.472645	55673.479787	35.105268
1133.560712	55729.804835	35.110285
1134.829324	55788.101594	35.115303
1136.088124	55839.400566	35.120320
1137.310200	55902.723496	35.125338
1138.223474	55970.126299	35.130356
1139.776314	56023.733899	35.135373
1140.610223	56080.175512	35.140391
1141.768988	56137.414447	35.145408
1143.335649	56193.083426	35.150426
1144.107480	56256.844853	35.155444
1145.047746	56308.568102	35.160461
1146.319530	56374.422336	35.165479
1147.575891	56444.070111	35.170496
1148.717734	56492.268709	35.175514
1149.858683	56557.738889	35.180532
1151.153150	56623.837084	35.185549
1152.082771	56678.872785	35.190567
1153.309753	56744.621136	35.195584
1155.146937	56784.509252	35.200602
1156.226345	56848.527893	35.205620
1157.403992	56891.823127	35.210637
1159.038610	56951.052744	35.215655
1159.841829	57000.723061	35.220672
1161.061977	57050.157328	35.225690
1162.045492	57106.647565	35.230708
1163.589525	57149.461867	35.235725
1164.803686	57191.150698	35.240743
1166.143555	57237.117311	35.245760
1167.569089	57272.058125	35.250778
1168.281320	57318.566184	35.255796
1169.318908	57364.099360	35.260813
1170.165620	57411.953618	35.265831
1171.096589	57461.041606	35.270848
1172.657781	57514.372774	35.275866
1173.143778	57573.347046	35.280884
1174.247352	57613.300768	35.285901
1175.170729	57665.580228	35.290919
1175.936324	57712.422469	35.295936
1177.230448	57758.498511	35.300954
1178.408456	57828.833472	35.305972
1179.330493	57864.493219	35.310989
1180.485500	57920.262317	35.316007
1182.012660	57992.815272	35.321024
1183.043691	58031.413940	35.326042
1183.978346	58107.205614	35.331060
1185.134771	58165.778906	35.336077
1186.302271	58232.300157	35.341095
1187.349572	58295.561842	35.346112
1188.878612	58353.292427	35.351130
1189.863994	58421.374398	35.356148
1191.541738	58481.715004	35.361165
1192.617256	58541.890537	35.366183
1193.433100	58605.701947	35.371200
1194.620433	58673.056782	35.376218
1195.505339	58741.016137	35.381236
1197.180312	58810.003951	35.386253
1198.439446	58879.930522	35.391271
1199.684012	58941.188234	35.396288
1201.669870	59009.950725	35.401306
1202.210235	59078.534616	35.406324
1203.546086	59141.652071	35.411341
1204.961663	59210.808226	35.416359
1206.268192	59275.443374	35.421376
1207.443049	59336.966181	35.426394
1208.466484	59401.772574	35.431412
1210.024691	59459.096142	35.436429
1211.285628	59525.156919	35.441447
1212.162005	59600.012948	35.446464
1213.692290	59656.936259	35.451482
1214.783835	59728.290360	35.456500
1216.161151	59788.598971	35.461517
1217.668651	59853.330789	35.466535
1218.679073	59914.184534	35.471552
1220.006608	59971.811271	35.476570
1221.047763	60030.970463	35.481588
1222.619696	60105.320383	35.486605
1223.838440	60162.654445	35.491623
1225.195960	60224.859836	35.496640
1226.481835	60273.480205	35.501658
1227.653597	60328.112861	35.506676
1228.755923	60395.257906	35.511693
1229.916020	60448.746960	35.516711
1230.866945	60509.225383	35.521728
1232.578546	60567.470698	35.526746
1233.825746	60633.359394	35.531764
1234.966134	60694.947995	35.536781
1236.356883	60757.909130	35.541799
1237.182454	60823.275659	35.546816
1238.586371	60878.417576	35.551834
1239.888401	60938.323040	35.556852
1241.066397	61000.856018	35.561869
1242.603630	61066.263706	35.566887
1243.657539	61119.074550	35.571904
1245.197638	61178.360971	35.576922
1246.347765	61241.240746	35.581940
1247.477799	61291.875171	35.586957
1248.823756	61347.014557	35.591975
1250.040432	61416.556255	35.596992
1251.707498	61463.612759	35.602010
1252.872406	61518.932796	35.607028
1253.838714	61573.378839	35.612045
1255.355176	61624.212991	35.617063
1256.099676	61676.054317	35.622080
1257.813286	61716.539653	35.627098
1258.514163	61766.223081	35.632116
1259.623460	61815.051401	35.637133
1260.819330	61852.395945	35.642151
1261.937539	61917.390402	35.647168
1263.164242	61971.771242	35.652186
1264.471567	62012.390301	35.657204
1265.394897	62072.940196	35.662221
1266.932775	62126.266155	35.667239
1267.916318	62193.244803	35.672256
1269.639280	62256.505940	35.677274
1270.648261	62319.068727	35.682292
1271.585509	62370.761063	35.687309
1273.073223	62429.495302	35.692327
1274.012892	62506.464621	35.697344
1275.350642	62565.488535	35.702362
1276.576841	62625.777139	35.707380
1277.821513	62696.001744	35.712397
1279.365477	62754.550699	35.717415
1280.522309	62834.095176	35.722432
1282.016551	62902.698687	35.727450
1283.320132	62974.706382	35.732468
1284.750968	63035.584337	35.737485
1286.618514	63086.448842	35.742503
1287.886040	63157.532126	35.747520
1289.217369	63211.962621	35.752538
1290.604311	63270.847573	35.757556
1291.708160	63334.809786	35.762573
1293.261899	63389.079242	35.767591
1294.389970	63453.215225	35.772608
1295.937209	63515.367578	35.777626
1297.099858	63575.738075	35.782644
1298.286157	63636.984977	35.787661
1299.853386	63692.329194	35.792679
1301.123229	63759.381201	35.797696
1302.331034	63823.246097	35.802714
1303.721346	63887.620698	35.807732
1304.884316	63948.732741	35.812749
1306.533531	64005.767788	35.817767
1307.755202	64078.950025	35.822784
1309.257199	64132.463180	35.827802
1310.721127	64188.172862	35.832820
1311.367880	64253.177595	35.837837
1312.828685	64306.134128	35.842855
1314.052974	64383.191308	35.847872
1315.321533	64440.097008	35.852890
1316.855567	64509.211516	35.857908
1318.232022	64576.996070	35.862925
1319.422337	64629.178945	35.867943
1320.686741	64698.336181	35.872960
1322.209220	64761.831338	35.877978
1323.449846	64829.986040	35.882996
1324.947464	64887.338053	35.888013
1326.466816	64946.832998	35.893031
1327.757181	65013.188744	35.898048
1329.288847	65054.550045	35.903066
1330.640075	65118.775655	35.908084
1331.792044	65182.000660	35.913101
1333.301037	65237.806920	35.918119
1334.781797	65302.360931	35.923136
1336.008555	65353.254399	35.928154
1337.355257	65416.303896	35.933172
1338.154939	65472.823164	35.938189
1339.399498	65531.165927	35.943207
1341.354069	65594.392955	35.948224
1342.614306	65654.537926	35.953242
1343.480593	65706.488857	35.958260
1344.731248	65766.901505	35.963277
1345.992664	65816.131712	35.968295
1347.153471	65875.197475	35.973312
1348.287975	65931.399448	35.978330
1349.622415	65973.983406	35.983348
1350.831388	66034.396887	35.988365
1352.252582	66091.466039	35.993383
1353.218898	66160.654957	35.998400
1354.359035	66212.545067	36.003418
1355.633249	66275.443443	36.008436
1357.141157	66348.840728	36.013453
1358.343776	66420.335957	36.018471
1359.807495	66483.224178	36.023488
1361.146374	66553.216914	36.028506
1362.620812	66620.947307	36.033524
1363.565391	66708.337568	36.038541
1365.865922	66756.317945	36.043559
1366.953207	66828.889728	36.048576
1368.449793	66904.031540	36.053594
1369.878422	66975.309340	36.058612
1371.346150	67057.882960	36.063629
1372.606611	67120.981859	36.068647
1374.118784	67194.285945	36.073664
1375.654735	67267.377580	36.078682
1376.771287	67327.985888	36.083700
1378.127010	67404.962058	36.088717
1379.391410	67472.316041	36.093735
1381.136666	67558.349219	36.098752
1382.400388	67622.366934	36.103770
1383.916246	67689.745446	36.108788
1385.257999	67764.648100	36.113805
1386.909375	67823.882205	36.118823
1388.386692	67901.303050	36.123840
1389.668995	67972.992775	36.128858
1391.438212	68036.672801	36.133876
1392.866368	68104.072465	36.138893
1394.334585	68172.251176	36.143911
1396.216555	68242.822042	36.148928
1397.106452	68304.392585	36.153946
1398.695810	68363.960571	36.158964
1400.121371	68432.355601	36.163981
1401.465696	68492.443461	36.168999
1402.933089	68566.701937	36.174016
1404.100084	68634.726407	36.179034
1405.903489	68709.882485	36.184052
1407.124692	68765.469269	36.189069
1408.493697	68845.132421	36.194087
1409.903419	68903.615355	36.199104
1411.155539	68964.966148	36.204122
1412.907761	69032.906397	36.209140
1414.019475	69105.341498	36.214157
1415.630313	69165.680486	36.219175
1416.518158	69238.847526	36.224192
1418.211195	69311.667116	36.229210
1419.820151	69376.698951	36.234228
1421.374910	69446.887426	36.239245
1423.001011	69516.406385	36.244263
1424.569471	69583.768966	36.249280
1425.472084	69656.314325	36.254298
1427.182487	69708.755478	36.259316
1428.485375	69775.932170	36.264333
1429.642939	69839.889701	36.269351
1431.160431	69908.179272	36.274368
1432.815737	69983.564871	36.279386
1434.432059	70027.650196	36.284404
1435.423076	70103.773347	36.289421
1436.954446	70172.365389	36.294439
1438.398150	70230.852339	36.299456
1439.485999	70294.511621	36.304474
1441.262014	70354.960508	36.309492
1442.538498	70414.031289	36.314509
1443.883001	70461.440046	36.319527
1445.141976	70525.009783	36.324544
1446.153581	70588.897018	36.329562
1447.350009	70640.318674	36.334580
1449.013339	70707.245052	36.339597
1450.275865	70771.524064	36.344615
1451.576539	70850.323866	36.349632
1453.058105	70924.105619	36.354650
1454.587923	70989.191877	36.359668
1456.207122	71066.182048	36.364685
1457.524623	71135.937287	36.369703
1459.160958	71201.083391	36.374720
1460.657341	71270.735000	36.379738
1461.839677	71329.429974	36.384756
1463.339539	71430.896222	36.389773
1464.657647	71494.370406	36.394791
1466.735678	71582.157006	36.399808
1468.144909	71664.843158	36.404826
1469.658484	71727.793368	36.409844
1471.071984	71805.425842	36.414861
1472.812650	71881.626813	36.419879
1474.228967	71950.659492	36.424896
1475.578833	72039.422842	36.429914
1477.300434	72104.342534	36.434932
1478.660800	72181.617137	36.439949
1479.877699	72256.621958	36.444967
1481.970719	72330.679264	36.449984
1483.133218	72414.242318	36.455002
1484.838552	72484.713039	36.460020
1486.284231	72555.883205	36.465037
1487.840512	72630.114023	36.470055
1489.763032	72707.466833	36.475072
1491.394809	72778.823790	36.480090
1492.645004	72843.350454	36.485108
1493.990083	72916.120566	36.490125
1495.619708	73000.460971	36.495143
1497.462240	73068.783905	36.500160
1498.686271	73140.091664	36.505178
1500.527659	73213.772858	36.510196
1502.030099	73284.429461	36.515213
1503.443396	73356.911453	36.520231
1505.393649	73413.970947	36.525248
1506.908490	73483.574854	36.530266
1508.826786	73546.504057	36.535284
1509.786421	73619.437757	36.540301
1511.470633	73681.821275	36.545319
1513.415284	73745.076146	36.550336
1514.754298	73803.144120	36.555354
1516.453475	73859.787887	36.560372
1517.776174	73923.837178	36.565389
1519.163964	73987.293782	36.570407
1520.887048	74040.539605	36.575424
1522.634874	74105.460107	36.580442
1523.893100	74168.962756	36.585460
1525.717808	74230.844248	36.590477
1527.259612	74292.466166	36.595495
1528.582170	74344.457969	36.600512
1529.988714	74411.028617	36.605530
1531.396656	74467.503930	36.610548
1532.888510	74536.556858	36.615565
1534.012864	74602.310818	36.620583
1535.797080	74665.719657	36.625600
1536.916745	74734.856684	36.630618
1538.956405	74803.191225	36.635636
1540.262108	74865.370755	36.640653
1541.324138	74925.409876	36.645671
1542.837693	74977.474352	36.650688
1544.119943	75044.851375	36.655706
1545.665381	75097.772441	36.660724
1547.139969	75164.118975	36.665741
1548.414568	75224.036826	36.670759
1549.575141	75290.293483	36.675776
1551.380371	75364.049617	36.680794
1552.533686	75430.649765	36.685812
1554.257773	75497.971437	36.690829
1555.514912	75579.984218	36.695847
1557.089230	75649.381784	36.700864
1558.680110	75730.456087	36.705882
1560.091799	75816.017544	36.710900
1561.939951	75892.821213	36.715917
1563.414645	75976.853247	36.720935
1565.018268	76050.630148	36.725952
1566.703218	76143.053576	36.730970
1568.398038	76220.072185	36.735988
1570.211628	76301.569372	36.741005
1571.929186	76383.119837	36.746023
1573.584179	76460.221368	36.751040
1575.067523	76538.756084	36.756058
1576.681310	76615.218460	36.761076
1578.343316	76689.139976	36.766093
1579.868367	76767.440809	36.771111
1582.091980	76836.068413	36.776128
1583.234739	76921.130741	36.781146
1584.816084	77004.047173	36.786164
1586.830307	77078.167979	36.791181
1588.014252	77166.606935	36.796199
1589.806066	77238.191411	36.801216
1591.508537	77319.253001	36.806234
1593.296785	77386.835359	36.811252
1595.209202	77472.247663	36.816269
1596.411161	77542.417764	36.821287
1598.169450	77612.298285	36.826304
1599.787713	77697.415293	36.831322
1601.544683	77773.440466	36.836340
1603.039955	77841.893235	36.841357
1604.725415	77924.479467	36.846375
1606.514066	77997.953995	36.851392
1608.011516	78075.908195	36.856410
1609.887852	78147.203125	36.861428
1611.542308	78224.727790	36.866445
1613.071200	78308.353152	36.871463
1614.485585	78365.190310	36.876480
1615.798324	78448.761250	36.881498
1617.418530	78524.683229	36.886516
1619.140565	78611.459076	36.891533
1620.804233	78683.637477	36.896551
1622.490243	78750.783139	36.901568
1623.898601	78832.300635	36.906586
1625.519481	78919.498681	36.911604
1627.316352	78998.878204	36.916621
1629.090201	79076.525941	36.921639
1630.723666	79144.238211	36.926656
1632.432685	79231.436117	36.931674
1634.131907	79308.538760	36.936692
1635.796986	79369.532147	36.941709
1637.218172	79458.321420	36.946727
1638.934165	79526.946544	36.951744
1640.956489	79593.294156	36.956762
1642.691291	79670.024838	36.961780
1643.991984	79746.190221	36.966797
1645.236039	79816.764943	36.971815
1647.502511	79890.309103	36.976832
1649.045301	79963.497959	36.981850
1650.229451	80028.166105	36.986868
1651.919759	80088.511002	36.991885
1653.433422	80156.269838	36.996903
1654.682826	80212.389138	37.001920
1656.627087	80278.813957	37.006938
1658.018361	80344.159903	37.011956
1659.979639	80408.922690	37.016973
1661.059660	80478.219822	37.021991
1662.880047	80543.093657	37.027008
1664.772315	80610.274901	37.032026
1666.033943	80691.200027	37.037044
1667.949195	80758.137312	37.042061
1668.999204	80847.052459	37.047079
1670.968498	80917.541811	37.052096
1672.778952	80993.415445	37.057114
1674.219215	81068.713740	37.062132
1675.997475	81158.630833	37.067149
1677.309007	81246.733469	37.072167
1679.068641	81325.707372	37.077184
1680.755121	81414.017919	37.082202
1682.589736	81501.203284	37.087220
1684.285871	81585.775258	37.092237
1685.608592	81678.324626	37.097255
1687.881569	81772.524716	37.102272
1689.811886	81861.888128	37.107290
1691.462675	81949.382393	37.112308
1693.411523	82030.621945	37.117325
1695.037154	82118.944229	37.122343
1696.665745	82194.051356	37.127360
1698.724199	82287.551876	37.132378
1700.307133	82374.323208	37.137396
1702.433484	82450.594802	37.142413
1703.686191	82542.093659	37.147431
1705.415959	82629.995795	37.152448
1707.303024	82707.534555	37.157466
1709.216471	82803.872302	37.162484
1711.008889	82871.708110	37.167501
1712.506200	82972.216782	37.172519
1714.129831	83039.864010	37.177536
1716.286147	83115.967993	37.182554
1717.795658	83208.961951	37.187572
1719.750486	83286.517032	37.192589
1721.571519	83373.583600	37.197607
1723.312234	83449.386070	37.202624
1725.020011	83538.954328	37.207642
1726.620570	83621.925495	37.212660
1728.782178	83694.178282	37.217677
1730.267924	83787.925429	37.222695
1731.922077	83858.598166	37.227712
1733.816460	83933.212153	37.232730
1735.378943	84021.803663	37.237748
1737.198557	84091.310696	37.242765
1739.219739	84182.200396	37.247783
1740.863471	84257.057192	37.252800
1742.875206	84335.886004	37.257818
1744.610345	84406.838860	37.262836
1746.039424	84493.488682	37.267853
1747.572354	84584.494082	37.272871
1749.638498	84647.298830	37.277888
1751.124659	84736.221275	37.282906
1752.438781	84812.829058	37.287924
1754.589756	84898.290067	37.292941
1756.327731	84982.738896	37.297959
1758.171226	85067.792359	37.302976
1760.092075	85145.142392	37.307994
1761.696068	85235.606530	37.313012
1763.977083	85305.133002	37.318029
1765.578773	85386.905309	37.323047
1767.022967	85457.855607	37.328064
1768.237468	85524.875805	37.333082
1769.495931	85592.776295	37.338100
1771.489995	85668.304228	37.343117
1773.130557	85736.246634	37.348135
1774.458560	85812.968946	37.353152
1776.353499	85891.592212	37.358170
1778.092609	85977.171563	37.363188
1779.841984	86060.354579	37.368205
1781.523075	86146.082899	37.373223
1783.266142	86234.184097	37.378240
1785.159508	86306.206657	37.383258
1786.754209	86407.041582	37.388276
1788.523133	86481.453717	37.393293
1790.472438	86579.635979	37.398311
1791.980480	86671.538891	37.403328
1794.023195	86765.740789	37.408346
1795.556960	86864.014382	37.413364
1797.341988	86960.259442	37.418381
1800.062236	87057.397595	37.423399
1801.417582	87143.598014	37.428416
1803.226735	87237.394453	37.433434
1804.824549	87341.349521	37.438452
1806.919688	87430.552430	37.443469
1809.164161	87525.916417	37.448487
1811.029225	87630.895180	37.453504
1812.945325	87704.970591	37.458522
1814.942621	87810.258790	37.463540
1816.821397	87895.251646	37.468557
1818.497129	87993.189994	37.473575
1819.965151	88079.337512	37.478592
1822.334367	88166.510151	37.483610
1823.897295	88264.669818	37.488628
1825.727677	88355.222268	37.493645
1827.745022	88455.161695	37.498663
1829.606669	88552.236397	37.503680
1831.989968	88643.805753	37.508698
1833.460507	88734.605772	37.513716
1835.566667	88817.892870	37.518733
1837.079260	88906.126878	37.523751
1838.779674	89012.390963	37.528768
1841.109861	89103.475803	37.533786
1843.136067	89200.235396	37.538804
1844.660115	89294.995473	37.543821
1846.575201	89377.781770	37.548839
1848.402012	89469.858983	37.553856
1850.025888	89562.094972	37.558874
1851.995873	89662.818959	37.563892
1854.186664	89742.813001	37.568909
1855.838539	89845.551769	37.573927
1857.708449	89936.977335	37.578944
1859.379246	90025.646156	37.583962
1861.450201	90123.833863	37.588980
1863.178457	90217.094779	37.593997
1865.137878	90313.767053	37.599015
1866.980373	90414.057273	37.604032
1868.915384	90494.511589	37.609050
1871.155748	90580.951064	37.614068
1873.338758	90661.835953	37.619085
1875.646649	90740.103377	37.624103
1877.468097	90824.467227	37.629120
1879.660207	90906.694786	37.634138
1881.674806	90979.584290	37.639156
1883.349295	91059.117669	37.644173
1884.655808	91132.866112	37.649191
1886.134968	91220.148965	37.654208
1888.039488	91295.971496	37.659226
1889.816697	91388.822822	37.664244
1891.464044	91471.023103	37.669261
1893.274588	91542.982666	37.674279
1894.992065	91628.163513	37.679296
1897.153121	91693.528684	37.684314
1898.239210	91776.590753	37.689332
1900.114395	91853.521941	37.694349
1901.776438	91944.453823	37.699367
1903.450371	92038.806208	37.704384
1905.094407	92125.267386	37.709402
1906.859321	92228.351488	37.714420
1908.439873	92321.933547	37.719437
1910.862085	92423.825449	37.724455
1912.354862	92529.551442	37.729472
1914.283939	92633.967414	37.734490
1916.348059	92745.675912	37.739508
1917.463848	92860.562477	37.744525
1919.706222	92968.226003	37.749543
1921.229804	93094.000654	37.754560
1923.482109	93211.220314	37.759578
1925.584500	93322.063038	37.764596
1927.872802	93447.187130	37.769613
1929.587570	93559.954591	37.774631
1931.600126	93672.016766	37.779648
1934.073809	93790.585585	37.784666
1935.605584	93914.004739	37.789684
1937.551406	94020.324095	37.794701
1939.827425	94136.643637	37.799719
1941.564596	94262.186842	37.804736
1943.970797	94379.653060	37.809754
1945.941195	94494.361300	37.814772
1947.847608	94619.740045	37.819789
1950.185496	94723.858321	37.824807
1952.177448	94847.779596	37.829824
1953.997625	94957.227348	37.834842
1956.000583	95074.315655	37.839860
1958.091962	95188.893455	37.844877
1960.153136	95304.820033	37.849895
1961.974406	95424.308452	37.854912
1964.164925	95540.050882	37.859930
1966.046986	95648.477316	37.864948
1967.944177	95764.646754	37.869965
1969.878440	95878.326331	37.874983
1972.008263	96004.322172	37.880000
1973.904899	96115.245124	37.885018
1976.041635	96236.563347	37.890036
1977.939424	96356.043356	37.895053
1980.295490	96465.932271	37.900071
1982.103903	96594.680812	37.905088
1984.174558	96699.050321	37.910106
1986.341230	96813.356091	37.915124
1987.892566	96936.872893	37.920141
1989.918587	97051.670563	37.925159
1991.793079	97182.198544	37.930176
1993.790080	97295.138194	37.935194
1996.161812	97406.435039	37.940212
1998.116266	97537.674542	37.945229
2000.444920	97648.497266	37.950247
2001.890686	97766.760325	37.955264
2004.130780	97881.324682	37.960282
2005.966788	98010.125377	37.965300
2007.823448	98135.196357	37.970317
2009.915573	98250.672580	37.975335
2011.629966	98369.504339	37.980352
2013.627583	98501.463655	37.985370
2015.212115	98625.045216	37.990388
2017.349630	98737.929977	37.995405
2019.582159	98871.426027	38.000423
2021.440932	99005.044501	38.005440
2023.419906	99117.955410	38.010458
2025.160024	99233.908613	38.015476
2027.047147	99353.224090	38.020493
2029.458102	99461.530119	38.025511
2031.111396	99572.997652	38.030528
2032.872619	99685.716433	38.035546
2034.706310	99805.878663	38.040564
2036.319136	99921.981038	38.045581
2038.261254	100046.754519	38.050599
2040.375760	100182.416997	38.055616
2042.596539	100309.290419	38.060634
2044.474562	100441.098918	38.065652
2046.134629	100585.455086	38.070669
2048.204968	100718.122068	38.075687
2050.309948	100860.964565	38.080704
2052.170493	101003.706477	38.085722
2054.364417	101156.070217	38.090740
2056.391405	101303.097939	38.095757
2058.565751	101442.052623	38.100775
2060.658150	101601.217149	38.105792
2062.567289	101751.422208	38.110810
2064.904599	101894.790719	38.115828
2067.275298	102052.151598	38.120845
2069.436399	102189.349222	38.125863
2071.678683	102350.699983	38.130880
2073.135963	102494.475050	38.135898
2075.497394	102648.125403	38.140916
2077.295852	102800.698114	38.145933
2080.223159	102946.768205	38.150951
2082.209792	103093.455239	38.155968
2084.858130	103239.443482	38.160986
2086.964027	103384.693110	38.166004
2088.722266	103536.755664	38.171021
2090.981794	103677.443458	38.176039
2093.132038	103838.600321	38.181056
2095.159367	103990.064960	38.186074
2097.182543	104136.497290	38.191092
2099.417017	104294.676238	38.196109
2101.572082	104438.604117	38.201127
2103.846779	104597.171260	38.206144
2106.028472	104743.201057	38.211162
2108.114119	104885.366592	38.216180
2110.041221	105044.611525	38.221197
2112.277217	105194.425969	38.226215
2114.238701	105349.317856	38.231232
2116.505215	105504.251485	38.236250
2118.926951	105652.745570	38.241268
2120.605915	105811.956862	38.246285
2123.112909	105965.333394	38.251303
2125.209334	106109.619933	38.256320
2127.177367	106266.353577	38.261338
2129.468633	106419.575711	38.266356
2131.385436	106584.294592	38.271373
2133.665068	106732.384502	38.276391
2135.268318	106886.971717	38.281408
2137.552841	107053.004788	38.286426
2139.356753	107216.539745	38.291444
2141.669414	107378.639078	38.296461
2143.682777	107546.086443	38.301479
2145.671843	107711.217884	38.306496
2147.648434	107865.928615	38.311514
2149.886428	108041.103763	38.316532
2151.888331	108211.777037	38.321549
2154.107343	108367.149522	38.326567
2156.414347	108547.819894	38.331584
2158.105003	108713.662208	38.336602
2160.640383	108878.586930	38.341620
2162.203466	109058.247737	38.346637
2164.767211	109221.825456	38.351655
2167.124159	109386.209846	38.356672
2168.803053	109527.393039	38.361690
2170.920322	109678.906842	38.366708
2173.028150	109831.640183	38.371725
2175.424079	109972.674941	38.376743
2178.155110	110117.728571	38.381760
2180.219613	110270.457916	38.386778
2182.611919	110412.002262	38.391796
2184.279590	110572.441956	38.396813
2186.768176	110728.404144	38.401831
2188.794962	110874.687052	38.406848
2190.658051	111037.862889	38.411866
2192.553560	111193.247778	38.416884
2194.746785	111358.782979	38.421901
2196.865015	111526.207606	38.426919
2199.003458	111705.081683	38.431936
2200.688679	111887.718037	38.436954
2203.271697	112068.173041	38.441972
2205.481345	112246.024112	38.446989
2207.504571	112420.113244	38.452007
2209.383917	112615.493939	38.457024
2211.448363	112804.847975	38.462042
2214.101193	112994.123633	38.467060
2216.084796	113190.619867	38.472077
2218.112080	113383.597261	38.477095
2220.482671	113573.376677	38.482112
2222.598863	113776.539090	38.487130
2224.856729	113974.594678	38.492148
2227.265031	114178.969228	38.497165
2229.301316	114384.417757	38.502183
2231.619490	114592.474081	38.507200
2233.689376	114795.180130	38.512218
2236.351531	115006.152819	38.517236
2238.472627	115210.654150	38.522253
2240.419321	115416.236610	38.527271
2243.005831	115613.653511	38.532288
2244.990124	115831.395721	38.537306
2247.261058	116040.127138	38.542324
2249.984174	116262.182822	38.547341
2251.752509	116473.468594	38.552359
2254.568966	116689.994844	38.557376
2257.332262	116889.788081	38.562394
2260.011549	117081.401768	38.567412
2262.666895	117279.057717	38.572429
2265.027118	117473.805512	38.577447
2267.860163	117656.671509	38.582464
2270.078649	117847.688938	38.587482
2272.277331	118043.365518	38.592500
2274.348810	118238.137060	38.597517
2276.508450	118426.008241	38.602535
2278.825682	118613.741536	38.607552
2281.128232	118811.879276	38.612570
2283.415788	118998.578988	38.617588
2285.265164	119190.992785	38.622605
2287.809156	119389.070377	38.627623
2290.159871	119590.045965	38.632640
2291.953984	119797.616953	38.637658
2293.788795	119987.779136	38.642676
2296.401979	120198.940795	38.647693
2298.265913	120400.948130	38.652711
2300.692739	120615.464671	38.657728
2302.889032	120828.280607	38.662746
2305.279301	121037.807279	38.667764
2307.507657	121243.212341	38.672781
2309.446178	121457.023428	38.677799
2311.729273	121668.434986	38.682816
2313.541964	121895.435546	38.687834
2316.023497	122096.429004	38.692852
2318.508027	122307.051356	38.697869
2320.266226	122503.136567	38.702887
2322.541715	122707.108434	38.707904
2324.365404	122912.750437	38.712922
2326.800319	123117.359133	38.717940
2328.702203	123333.088988	38.722957
2330.729799	123550.271914	38.727975
2333.473359	123762.726303	38.732992
2335.624747	123992.185019	38.738010
2338.057684	124215.727308	38.743028
2340.395966	124438.461041	38.748045
2342.060598	124665.614735	38.753063
2344.332259	124902.823844	38.758080
2346.495422	125154.361638	38.763098
2348.879592	125388.397058	38.768116
2351.241401	125627.879876	38.773133
2353.443104	125876.409377	38.778151
2356.162313	126126.534083	38.783168
2358.385467	126384.578383	38.788186
2360.549756	126628.995075	38.793204
2363.529338	126885.947291	38.798221
2365.847104	127147.736918	38.803239
2368.435771	127387.384804	38.808256
2370.981143	127643.229741	38.813274
2373.875715	127885.065593	38.818292
2376.420067	128133.580442	38.823309
2378.471594	128384.749415	38.828327
2381.311921	128633.703053	38.833344
2384.258272	128876.475406	38.838362
2386.675373	129126.424359	38.843380
2388.973575	129355.699679	38.848397
2391.400579	129602.820530	38.853415
2393.759339	129840.792839	38.858432
2395.959387	130107.440719	38.863450
2398.478038	130351.734848	38.868468
2401.185837	130599.997535	38.873485
2403.029255	130853.281827	38.878503
2405.744753	131095.354337	38.883520
2408.064550	131344.151477	38.888538
2410.110681	131599.438565	38.893556
2412.827719	131863.707153	38.898573
2415.211500	132126.963639	38.903591
2417.612974	132389.051590	38.908608
2419.815377	132646.350542	38.913626
2422.186393	132912.392573	38.918644
2424.441699	133179.875464	38.923661
2426.543800	133453.728409	38.928679
2428.872977	133715.404137	38.933696
2431.110877	133994.073687	38.938714
2433.988758	134267.188524	38.943732
2436.364078	134532.757408	38.948749
2438.777429	134810.973170	38.953767
2441.735597	135086.770578	38.958784
2444.275374	135359.627715	38.963802
2446.827791	135639.273432	38.968820
2449.456991	135904.671094	38.973837
2451.776612	136188.176184	38.978855
2454.389176	136442.438016	38.983872
2456.604837	136715.150943	38.988890
2459.021620	136986.577724	38.993908
2461.549068	137252.113321	38.998925
2463.480577	137523.276538	39.003943
2466.330914	137795.350892	39.008960
2469.428174	138062.388265	39.013978
2472.201048	138316.990661	39.018996
2474.545477	138573.488875	39.024013
2477.056927	138838.553787	39.029031
2479.029701	139089.351497	39.034048
2482.331156	139325.564287	39.039066
2484.397181	139559.522220	39.044084
2486.494587	139782.232448	39.049101
2488.765133	140018.584570	39.054119
2490.969060	140253.273095	39.059136
2493.192207	140500.612567	39.064154
2495.287680	140751.602893	39.069172
2498.240945	141006.051904	39.074189
2500.301632	141259.677355	39.079207
2502.711876	141511.536150	39.084224
2505.343775	141774.783667	39.089242
2507.423328	142032.357166	39.094260
2510.110208	142311.653445	39.099277
2512.209177	142593.657710	39.104295
2514.804477	142865.039322	39.109312
2516.807617	143142.835450	39.114330
2518.887505	143438.490952	39.119348
2521.786514	143724.298230	39.124365
2524.230112	144022.032508	39.129383
2526.606643	144315.958796	39.134400
2528.819232	144630.232236	39.139418
2531.309780	144928.129528	39.144436
2533.812482	145246.778238	39.149453
2536.308285	145554.197452	39.154471
2539.049755	145871.353118	39.159488
2541.260895	146191.411397	39.164506
2544.406975	146502.072657	39.169524
2547.160049	146832.597532	39.174541
2548.998507	147158.774408	39.179559
2551.514638	147481.750316	39.184576
2554.104287	147804.869029	39.189594
2556.153172	148132.631029	39.194612
2559.135427	148479.796099	39.199629
2561.740153	148819.267095	39.204647
2564.470907	149152.526335	39.209664
2566.887326	149505.282684	39.214682
2569.207550	149846.683279	39.219700
2572.012357	150188.264100	39.224717
2574.768318	150541.507222	39.229735
2577.055683	150878.717945	39.234752
2579.757017	151239.234774	39.239770
2581.943584	151608.529609	39.244788
2584.656426	151942.278407	39.249805
2587.605679	152307.003111	39.254823
2589.805570	152655.459645	39.259840
2592.638859	153013.822086	39.264858
2595.293786	153378.015869	39.269876
2598.014574	153723.515983	39.274893
2600.385231	154084.699484	39.279911
2603.108596	154452.024889	39.284928
2605.878604	154819.193011	39.289946
2608.538795	155171.934400	39.294964
2611.410609	155534.305334	39.299981
2614.138414	155898.694087	39.304999
2616.409530	156265.898578	39.310016
2619.208223	156627.157867	39.315034
2621.307278	156988.452619	39.320052
2624.326056	157353.337994	39.325069
2626.950261	157726.196263	39.330087
2629.348948	158086.587500	39.335104
2632.014123	158456.422442	39.340122
2634.284517	158830.701215	39.345140
2637.217232	159202.339622	39.350157
2639.605099	159568.619188	39.355175
2642.281588	159942.955447	39.360192
2644.988683	160316.755954	39.365210
2647.613075	160688.083292	39.370228
2650.678721	161051.409022	39.375245
2653.331610	161391.872941	39.380263
2655.912470	161727.550941	39.385280
2658.909615	162071.430578	39.390298
2661.146132	162404.157054	39.395316
2664.262558	162739.083669	39.400333
2666.568228	163074.760922	39.405351
2669.040486	163408.941089	39.410368
2671.508286	163760.758625	39.415386
2673.859979	164111.935984	39.420404
2676.677637	164460.337999	39.425421
2678.753404	164837.031109	39.430439
2680.987646	165208.546778	39.435456
2683.699060	165576.549091	39.440474
2686.116260	165958.946540	39.445492
2688.769247	166345.232503	39.450509
2691.504121	166727.152837	39.455527
2693.682252	167120.272038	39.460544
2696.561530	167514.020196	39.465562
2698.693931	167919.047973	39.470580
2701.452375	168331.192039	39.475597
2704.135181	168752.669967	39.480615
2706.655555	169164.805260	39.485632
2709.021043	169579.341494	39.490650
2711.791274	170019.312954	39.495668
2713.931502	170437.622265	39.500685
2716.984116	170889.769602	39.505703
2719.542745	171327.940762	39.510720
2722.301489	171778.209371	39.515738
2724.417566	172231.209572	39.520756
2727.685900	172677.518276	39.525773
2730.569847	173146.987011	39.530791
2732.805417	173603.709694	39.535808
2735.679752	174060.512884	39.540826
2738.389805	174538.486636	39.545844
2741.539633	175001.423358	39.550861
2744.217966	175475.445799	39.555879
2746.977302	175930.461705	39.560896
2750.606210	176389.217103	39.565914
2753.830547	176860.330357	39.570932
2756.908638	177317.399206	39.575949
2759.991226	177768.171329	39.580967
2762.813258	178222.135825	39.585984
2765.764937	178659.447157	39.591002
2768.427890	179122.482677	39.596020
2770.593455	179573.737729	39.601037
2773.917937	180028.902841	39.606055
2776.715082	180487.149674	39.611072
2779.277213	180941.625868	39.616090
2781.750409	181413.769906	39.621108
2784.646274	181863.677565	39.626125
2787.356144	182338.252881	39.631143
2789.694506	182877.553258	39.636160
2792.550797	183341.011498	39.641178
2795.095785	183825.017427	39.646196
2797.507703	184294.518387	39.651213
2800.137292	184786.211639	39.656231
2802.982751	185277.721133	39.661248
2805.909776	185765.613543	39.666266
2807.873423	186259.424582	39.671284
2810.704648	186749.317739	39.676301
2813.383321	187258.464519	39.681319
2815.981025	187761.530440	39.686336
2819.264695	188267.005988	39.691354
2822.342362	188777.342062	39.696372
2824.979548	189276.217720	39.701389
2827.843682	189790.071586	39.706407
2830.660365	190291.463621	39.711424
2833.471644	190775.154577	39.716442
2836.115877	191271.523084	39.721460
2838.757417	191743.890491	39.726477
2841.746968	192205.791017	39.731495
2844.404352	192685.627378	39.736512
2847.572797	193154.768076	39.741530
2850.371299	193644.593963	39.746548
2852.560499	194125.067795	39.751565
2855.205572	194612.508216	39.756583
2858.108463	195109.587983	39.761600
2861.309774	195604.463788	39.766618
2863.597716	196117.392239	39.771636
2866.237741	196617.846149	39.776653
2869.161101	197125.471567	39.781671
2871.575267	197649.638711	39.786688
2874.537706	198165.085350	39.791706
2877.238370	198707.526106	39.796724
2879.904538	199234.961594	39.801741
2882.526582	199780.517433	39.806759
2885.543238	200320.501146	39.811776
2888.495553	200867.914157	39.816794
2891.138170	201422.845674	39.821812
2894.261290	201978.161086	39.826829
2897.429520	202522.243302	39.831847
2900.177834	203074.953499	39.836864
2903.773701	203638.633760	39.841882
2906.327599	204193.740123	39.846900
2909.986286	204737.777503	39.851917
2913.586154	205289.497231	39.856935
2916.820469	205838.176459	39.861952
2920.049345	206380.507223	39.866970
2922.727300	206923.763804	39.871988
2925.276510	207477.507924	39.877005
2928.334183	208030.487974	39.882023
2931.294607	208583.865572	39.887040
2934.233272	209136.638143	39.892058
2936.910712	209696.083042	39.897076
2939.559224	210264.043793	39.902093
2942.295843	210835.345203	39.907111
2945.142650	211412.651161	39.912128
2948.275011	211993.800334	39.917146
2950.809338	212573.697736	39.922164
2953.311661	213156.979869	39.927181
2956.404259	213744.235288	39.932199
2959.307031	214342.724404	39.937216
2962.242816	214935.112411	39.942234
2964.955340	215544.887011	39.947252
2968.237480	216145.402632	39.952269
2971.691975	216732.580479	39.957287
2974.958660	217332.160111	39.962304
2977.954453	217921.240174	39.967322
2981.085577	218517.260379	39.972340
2984.292986	219100.440233	39.977357
2987.872291	219683.155977	39.982375
2991.059575	220259.988949	39.987392
2994.391661	220845.665690	39.992410
2997.315375	221430.365096	39.997428
3000.363621	221999.396448	40.002445
3003.045320	222583.499181	40.007463
3004.962606	223178.721640	40.012480
3008.130712	223769.353768	40.017498
3011.294003	224367.989062	40.022516
3013.915972	224968.665199	40.027533
3016.902876	225558.589171	40.032551
3019.704421	226158.500504	40.037568
3022.859317	226763.919994	40.042586
3025.920695	227375.196908	40.047604
3028.986656	227975.676182	40.052621
3031.924601	228559.052902	40.057639
3034.696437	229140.778653	40.062656
3037.761352	229708.079572	40.067674
3040.875865	230279.513237	40.072692
3043.672759	230851.301015	40.077709
3046.486468	231426.845501	40.082727
3049.113745	232002.317024	40.087744
3051.936068	232598.106038	40.092762
3054.785886	233191.044878	40.097780
3057.512573	233800.438586	40.102797
3060.778745	234394.555664	40.107815
3063.494777	235014.161772	40.112832
3066.357588	235635.268233	40.117850
3068.998069	236267.332075	40.122868
3071.546099	236895.243094	40.127885
3074.962020	237528.733087	40.132903
3077.495812	238187.026678	40.137920
3080.699279	238835.255999	40.142938
3083.561970	239505.739831	40.147956
3086.303032	240169.687036	40.152973
3089.661299	240836.609919	40.157991
3092.216282	241515.418426	40.163008
3095.634751	242208.798522	40.168026
3098.522149	242895.426225	40.173044
3101.338668	243593.748372	40.178061
3104.197029	244292.646054	40.183079
3107.160892	245002.778433	40.188096
3110.452248	245719.258663	40.193114
3113.634910	246443.247109	40.198132
3117.099764	247173.971200	40.203149
3120.027590	247895.860123	40.208167
3123.080787	248623.111857	40.213184
3126.386923	249353.140665	40.218202
3129.742515	250087.654776	40.223220
3132.941050	250817.033546	40.228237
3136.203677	251555.467454	40.233255
3139.609036	252291.487758	40.238272
3142.509884	253025.551228	40.243290
3145.607695	253768.496180	40.248308
3148.975672	254509.337515	40.253325
3153.042193	255248.008183	40.258343
3156.161461	255976.179877	40.263360
3159.497095	256714.397949	40.268378
3162.672000	257448.699818	40.273396
3165.332918	258200.731300	40.278413
3168.420431	258933.818899	40.283431
3171.929377	259678.291747	40.288448
3175.032299	260419.851580	40.293466
3178.275010	261171.875048	40.298484
3181.780614	261914.733866	40.303501
3185.049596	262650.919196	40.308519
3188.019976	263396.721885	40.313536
3191.188036	264137.916578	40.318554
3194.478547	264889.551361	40.323572
3197.891263	265633.033864	40.328589
3201.094731	266382.766329	40.333607
3204.121257	267139.226036	40.338624
3207.359456	267878.756814	40.343642
3210.550826	268635.661595	40.348660
3213.866947	269398.433123	40.353677
3217.466843	270135.552985	40.358695
3220.345339	270888.221417	40.363712
3223.213088	271647.717095	40.368730
3226.887378	272396.184717	40.373748
3229.825245	273165.002384	40.378765
3232.749262	273912.126478	40.383783
3235.644263	274676.568863	40.388800
3239.009458	275444.587712	40.393818
3242.160346	276188.074868	40.398836
3244.994297	276928.176250	40.403853
3249.013376	277653.990864	40.408871
3251.684620	278384.529821	40.413888
3254.911011	279106.848607	40.418906
3258.435542	279846.966448	40.423924
3261.121616	280573.317231	40.428941
3264.268126	281315.917413	40.433959
3267.357107	282063.394670	40.438976
3270.158144	282821.498377	40.443994
3273.704516	283570.640498	40.449012
3276.733855	284343.064850	40.454029
3279.713911	285103.858299	40.459047
3283.044131	285883.556823	40.464064
3286.208220	286658.650877	40.469082
3289.550955	287444.829679	40.474100
3292.430903	288229.954180	40.479117
3295.758943	289031.859021	40.484135
3298.797721	289840.883155	40.489152
3301.789091	290655.363359	40.494170
3305.127717	291459.901747	40.499188
3308.079073	292296.430944	40.504205
3312.581331	293094.088319	40.509223
3316.553342	293903.979551	40.514240
3320.249749	294727.536767	40.519258
3323.845419	295525.988732	40.524276
3327.154716	296333.538136	40.529293
3330.491520	297147.875861	40.534311
3334.137511	297966.850266	40.539328
3337.121758	298778.528481	40.544346
3341.061764	299592.685621	40.549364
3344.114365	300410.371215	40.554381
3347.441487	301240.364611	40.559399
3350.632038	302071.686580	40.564416
3353.742291	302894.300915	40.569434
3357.225781	303726.439515	40.574452
3360.019586	304573.116411	40.579469
3363.737072	305404.962936	40.584487
3366.914356	306259.065654	40.589504
3369.635865	307111.625992	40.594522
3373.126107	307974.331585	40.599540
3376.194851	308848.611564	40.604557
3379.386915	309715.318166	40.609575
3382.563072	310589.626122	40.614592
3385.689805	311462.098374	40.619610
3389.449822	312346.384348	40.624628
3393.380416	313223.368259	40.629645
3397.215661	314087.000838	40.634663
3400.753697	314953.404562	40.639680
3404.293712	315843.799577	40.644698
3407.748704	316718.405107	40.649716
3411.538131	317591.723058	40.654733
3414.758601	318461.128478	40.659751
3418.379123	319347.507104	40.664768
3421.314852	320228.671059	40.669786
3424.448438	321103.594360	40.674804
3427.725215	321995.580000	40.679821
3431.228640	322884.618626	40.684839
3434.569497	323778.205652	40.689856
3437.631665	324675.622937	40.694874
3441.475916	325563.992449	40.699892
3444.480054	326469.929954	40.704909
3447.945451	327367.021736	40.709927
3451.355024	328271.586532	40.714944
3454.892547	329170.732084	40.719962
3458.731656	330068.389140	40.724980
3462.635447	330962.894914	40.729997
3466.709911	331841.345559	40.735015
3470.466097	332701.077130	40.740020
3473.994592	333539.196352	40.745024
3477.570799	334319.508079	40.750029
3480.851306	335055.090395	40.755034
3483.508434	335739.715635	40.760039
3486.387057	336348.383389	40.765044
3488.935683	336924.186013	40.770048
3491.843002	337451.225449	40.775053
3494.249242	337924.933745	40.780058
3496.703237	338340.675346	40.785063
3498.831047	338708.021110	40.790068
3500.791823	339037.271669	40.795072
3502.476724	339308.127735	40.800077
3504.818890	339563.316875	40.805082
3506.084190	339755.534481	40.810087
3507.808011	339918.131992	40.815092
3508.919966	340046.598413	40.820096
3510.729948	340137.169426	40.825101
3512.209084	340199.923030	40.830106
3512.953280	340224.471717	40.835111
3514.271796	340227.545811	40.840116
3515.120257	340205.723268	40.845120
3515.939091	340146.399247	40.850125
3516.945426	340076.467798	40.855130
3517.621906	339974.955364	40.860135
3518.095245	339862.158906	40.865140
3518.861979	339743.162606	40.870144
3519.627611	339589.761645	40.875149
3519.777829	339422.318052	40.880154
3520.134256	339260.028851	40.885159
3520.902544	339075.170186	40.890164
3520.865094	338868.974645	40.895168
3521.625986	338656.194159	40.900173
3521.472650	338435.062025	40.905178
3521.637761	338216.040233	40.910183
3521.807297	337982.063929	40.915188
3521.946473	337753.888800	40.920192
3522.422752	337503.586517	40.925197
3522.722760	337260.608454	40.930202
3522.446993	336997.527288	40.935207
3522.958525	336735.999539	40.940212
3522.876546	336475.020456	40.945216
3522.596787	336206.848129	40.950221
3522.676989	335928.368939	40.955226
3523.207813	335652.665471	40.960231
3523.168550	335370.767557	40.965236
3522.779993	335092.660522	40.970240
3523.146523	334799.454133	40.975245
3522.957510	334519.785715	40.980250
3522.992151	334225.202511	40.985255
3522.904232	333932.518131	40.990260
3522.308920	333654.712449	40.995264
3522.341308	333356.791131	41.000269
3522.322975	333083.596061	41.005274
3522.142552	332795.469769	41.010279
3522.239818	332513.376401	41.015284
3522.192314	332222.681663	41.020288
3522.202827	331935.383734	41.025293
3521.812545	331653.767159	41.030298
3521.550372	331366.126079	41.035303
3521.474716	331081.175135	41.040308
3521.357294	330793.456273	41.045312
3521.117547	330511.528022	41.050317
3520.878791	330239.822302	41.055322
3520.823067	329968.187805	41.060327
3520.873762	329685.089011	41.065332
3520.504830	329410.472824	41.070336
3520.789274	329136.719107	41.075341
3520.561211	328869.784030	41.080346
3520.077341	328594.035496	41.085351
3520.215719	328322.995142	41.090356
3520.076526	328064.002158	41.095360
3519.874399	327782.684289	41.100365
3519.506264	327518.687159	41.105370
3519.381942	327264.824802	41.110375
3519.105021	326998.851354	41.115380
3518.758756	326746.037874	41.120384
3518.860381	326483.995428	41.125389
3518.716602	326233.309221	41.130394
3518.576039	325988.395243	41.135399
3518.413569	325734.122188	41.140404
3518.232836	325487.608898	41.145408
3518.209384	325247.327239	41.150413
3517.998606	324992.039582	41.155418
3517.735282	324747.696961	41.160423
3517.920529	324521.522032	41.165428
3517.283299	324277.056995	41.170432
3517.247689	324027.968375	41.175437
3516.948728	323806.088026	41.180442
3516.721244	323565.039821	41.185447
3516.899998	323343.133185	41.190452
3516.817618	323122.207439	41.195456
3516.513557	322896.583467	41.200461
3516.530807	322676.021372	41.205466
3516.759982	322433.470617	41.210471
3516.511169	322215.033738	41.215476
3516.017490	322003.401008	41.220480
3516.028754	321779.120919	41.225485
3515.771008	321567.220155	41.230490
3515.384605	321350.250395	41.235495
3515.469568	321137.225412	41.240500
3514.843477	320935.885954	41.245504
3514.795319	320730.206609	41.250509
3514.827373	320520.137925	41.255514
3514.630818	320320.102211	41.260519
3514.798380	320129.294596	41.265524
3514.522817	319929.498383	41.270528
3514.659384	319719.612972	41.275533
3514.163465	319531.654088	41.280538
3513.899947	319346.125874	41.285543
3514.045012	319148.880758	41.290548
3513.758271	318971.444984	41.295552
3513.842725	318777.744051	41.300557
3513.468671	318594.494226	41.305562
3513.649357	318401.845138	41.310567
3513.626860	318232.888116	41.315572
3513.312905	318045.377768	41.320576
3513.014954	317855.497983	41.325581
3512.919162	317695.404274	41.330586
3512.796756	317515.316343	41.335591
3513.014486	317334.004143	41.340596
3513.009650	317169.823494	41.345600
3512.740422	316997.465549	41.350605
3512.400541	316820.843574	41.355610
3512.124423	316659.654829	41.360615
3512.273979	316482.191704	41.365620
3511.615864	316333.604945	41.370624
3511.614501	316161.608983	41.375629
3511.674431	316016.954397	41.380634
3511.128924	315860.206589	41.385639
3510.989608	315701.740902	41.390644
3511.079437	315560.922150	41.395648
3510.943431	315409.782681	41.400653
3511.105691	315261.827436	41.405658
3510.807926	315110.814033	41.410663
3511.160040	314971.046528	41.415668
3510.659075	314831.564626	41.420672
3510.798494	314670.889015	41.425677
3510.781616	314541.253746	41.430682
3510.568396	314405.949291	41.435687
3510.280132	314261.216318	41.440692
3510.565440	314124.306432	41.445696
3510.226848	313976.501654	41.450701
3510.453051	313844.485517	41.455706
3510.288809	313714.082167	41.460711
3509.845957	313573.442339	41.465716
3509.649014	313446.554717	41.470720
3509.958543	313303.913528	41.475725
3509.784182	313171.958093	41.480730
3509.496291	313053.505888	41.485735
3509.797573	312929.974036	41.490740
3509.473889	312808.142606	41.495744
3509.402189	312682.683688	41.500749
3509.252811	312549.577547	41.505754
3508.974002	312435.626166	41.510759
3509.375600	312309.328890	41.515764
3509.342073	312199.918762	41.520768
3509.422014	312070.159655	41.525773
3509.075764	311956.853792	41.530778
3508.727790	311834.794615	41.535783
3508.753647	311719.063557	41.540788
3508.592288	311607.305582	41.545792
3508.414429	311505.015780	41.550797
3508.487786	311390.167095	41.555802
3508.407732	311289.261060	41.560807
3508.440589	311173.476681	41.565812
3507.852710	311074.481695	41.570816
3507.539330	310963.433013	41.575821
3507.779751	310865.733081	41.580826
3507.776916	310755.958566	41.585831
3507.744481	310653.084376	41.590836
3507.458760	310560.809800	41.595840
3507.109051	310480.581197	41.600845
3507.087059	310386.458359	41.605850
3507.341810	310294.963953	41.610855
3507.465227	310200.283641	41.615860
3507.584708	310112.601571	41.620864
3507.566241	310011.428741	41.625869
3507.292101	309916.911810	41.630874
3507.059990	309820.276044	41.635879
3507.194415	309738.443707	41.640884
3507.261636	309662.016467	41.645888
3507.012351	309563.118103	41.650893
3507.009286	309473.850877	41.655898
3506.954743	309385.558519	41.660903
3506.974683	309294.735101	41.665908
3506.569382	309208.024079	41.670912
3507.003730	309129.528284	41.675917
3506.930031	309047.294718	41.680922
3506.414592	308969.048942	41.685927
3506.643252	308876.563491	41.690932
3506.498611	308801.109566	41.695936
3506.195693	308719.700148	41.700941
3506.445978	308640.621608	41.705946
3506.199238	308560.170142	41.710951
3506.335001	308489.608694	41.715956
3506.308196	308424.289294	41.720960
3506.303326	308338.633813	41.725965
3506.450122	308259.952550	41.730970
3505.906879	308195.477012	41.735975
3506.113966	308110.398738	41.740980
3506.114506	308041.817256	41.745984
3505.772359	307963.033826	41.750989
3505.802375	307888.670892	41.755994
3505.948827	307824.621444	41.760999
3505.999217	307761.808427	41.766004
3505.596650	307699.269728	41.771008
3505.851430	307626.016412	41.776013
3505.922172	307561.723982	41.781018
3505.750672	307495.535295	41.786023
3506.084359	307416.136376	41.791028
3505.815673	307356.044768	41.796032
3505.855577	307282.824539	41.801037
3505.741111	307202.808245	41.806042
3505.743267	307148.425314	41.811047
3505.718120	307070.201660	41.816052
3505.355635	307012.923602	41.821056
3505.488595	306950.580166	41.826061
3505.233200	306878.728818	41.831066
3504.930488	306816.962293	41.836071
3505.275687	306755.501572	41.841076
3505.259112	306703.716816	41.846080
3505.103788	306640.043851	41.851085
3504.844983	306575.012769	41.856090
3504.812167	306526.945839	41.861095
3504.852164	306464.870817	41.866100
3504.843370	306416.698232	41.871104
3504.879429	306364.243236	41.876109
3504.890029	306308.661992	41.881114
3504.631585	306254.242486	41.886119
3504.571444	306200.682621	41.891124
3504.476800	306149.011293	41.896128
3504.971251	306104.577028	41.901133
3504.735074	306050.077475	41.906138
3504.583073	305997.193421	41.911143
3504.602267	305946.216652	41.916148
3504.815125	305903.633096	41.921152
3504.449783	305838.999450	41.926157
3504.642159	305797.284266	41.931162
3504.525749	305752.538013	41.936167
3504.535724	305693.851432	41.941172
3504.552961	305647.659055	41.946176
3504.328291	305591.935662	41.951181
3504.269652	305545.831402	41.956186
3504.127855	305503.048467	41.961191
3504.389153	305452.491432	41.966196
3504.422142	305408.790377	41.971200
3504.250519	305363.772474	41.976205
3504.138643	305314.317054	41.981210
3504.153851	305273.927041	41.986215
3504.258981	305232.377728	41.991220
3504.142228	305191.804687	41.996224
3503.769867	305149.057500	42.001229
3503.792844	305108.818836	42.006234
3503.862469	305079.007011	42.011239
3504.063556	305032.072757	42.016244
3504.100035	304996.209155	42.021248
3504.191373	304951.735110	42.026253
3503.973977	304904.128135	42.031258
3504.046400	304857.391980	42.036263
3504.420573	304821.653607	42.041268
3504.164348	304781.102046	42.046272
3504.199440	304734.066223	42.051277
3504.026361	304690.218624	42.056282
3503.529717	304650.238983	42.061287
3503.889783	304606.104366	42.066292
3503.816374	304572.980736	42.071296
3504.015978	304537.727547	42.076301
3504.012346	304494.922167	42.081306
3503.757710	304446.837051	42.086311
3503.997135	304409.516140	42.091316
3503.999392	304381.953999	42.096320
3503.840999	304347.087493	42.101325
3503.864005	304300.689402	42.106330
3503.447160	304271.080411	42.111335
3503.826057	304226.764378	42.116340
3503.355023	304189.605280	42.121344
3503.343295	304155.148358	42.126349
3503.625010	304131.741584	42.131354
3503.481697	304098.094134	42.136359
3503.634901	304050.173934	42.141364
3503.475439	304024.418363	42.146368
3503.397111	303992.414916	42.151373
3503.607653	303957.948563	42.156378
3503.294289	303933.184098	42.161383
3503.445196	303891.601096	42.166388
3503.387162	303859.976140	42.171392
3503.477521	303827.920769	42.176397
3503.423869	303798.865521	42.181402
3503.393221	303771.740847	42.186407
3503.667132	303728.204297	42.191412
3503.442439	303707.396036	42.196416
3503.418953	303672.049887	42.201421
3503.483294	303641.474561	42.206426
3503.345304	303611.999746	42.211431
3503.341081	303565.147156	42.216436
3503.083741	303555.592804	42.221440
3503.105736	303516.447398	42.226445
3503.110379	303492.829154	42.231450
3502.887567	303470.875257	42.236455
3503.260898	303433.329110	42.241460
3503.230209	303415.875251	42.246464
3502.935743	303384.694170	42.251469
3503.210083	303367.319857	42.256474
3502.700071	303330.547988	42.261479
3503.109514	303310.556630	42.266484
3502.774034	303284.700961	42.271488
3502.865541	303254.706513	42.276493
3502.738053	303226.018790	42.281498
3502.696000	303213.860259	42.286503
3502.661427	303185.870590	42.291508
3502.614424	303169.666255	42.296512
3502.915595	303142.209425	42.301517
3502.908365	303124.904503	42.306522
3502.729634	303101.951003	42.311527
3502.844095	303080.962220	42.316532
3502.829350	303062.996747	42.321536
3502.660746	303043.324710	42.326541
3502.693834	303012.499401	42.331546
3502.528898	303007.282485	42.336551
3502.947575	302978.407439	42.341556
3502.661983	302972.191374	42.346560
3502.924656	302937.181742	42.351565
3503.200256	302906.827462	42.356570
3503.067134	302883.306831	42.361575
3502.771135	302863.909146	42.366580
3502.658160	302846.289810	42.371584
3502.965427	302817.101240	42.376589
3502.978303	302801.421885	42.381594
3502.532537	302773.878037	42.386599
3502.521031	302754.664887	42.391604
3503.003997	302740.159087	42.396608
3502.751482	302717.471458	42.401613
3502.846033	302682.258888	42.406618
3502.515852	302664.113541	42.411623
3502.591172	302645.573937	42.416628
3502.476400	302623.704596	42.421632
3502.221142	302615.218662	42.426637
3502.562980	302596.204717	42.431642
3502.649807	302576.441672	42.436647
3502.701976	302558.007458	42.441652
3502.795671	302541.068321	42.446656
3502.827197	302517.725389	42.451661
3502.714009	302487.457100	42.456666
3502.827429	302483.367335	42.461671
3503.259271	302450.825077	42.466676
3502.653845	302423.585961	42.471680
3502.589612	302406.976877	42.476685
3502.897721	302387.433670	42.481690
3502.568396	302364.961502	42.486695
3503.024778	302344.351628	42.491700
3502.753426	302327.087735	42.496704
3502.257354	302312.124067	42.501709
3502.288078	302286.897819	42.506714
3502.383061	302289.173557	42.511719
3503.205833	302260.973008	42.516724
3502.902311	302241.805326	42.521728
3502.546946	302218.242792	42.526733
3502.990931	302197.151238	42.531738
3502.922540	302168.810008	42.536743
3503.057469	302140.004315	42.541748
3502.421898	302124.247983	42.546752
3502.610718	302109.686194	42.551757
3502.799664	302076.570866	42.556762
3502.386230	302070.654638	42.561767
3502.810779	302049.209755	42.566772
3502.944862	302030.813453	42.571776
3502.989695	302007.875427	42.576781
3502.866225	301991.199122	42.581786
3502.772527	301962.047316	42.586791
3502.815407	301941.272876	42.591796
3502.504718	301918.135886	42.596800
3502.521308	301897.645497	42.601805
3503.017905	301877.665423	42.606810
3502.492033	301867.389224	42.611815
3502.737733	301839.304122	42.616820
3502.625786	301822.244201	42.621824
3502.799931	301808.269991	42.626829
3503.015975	301788.944565	42.631834
3502.374105	301775.326979	42.636839
3502.542931	301754.558227	42.641844
3502.500526	301733.517080	42.646848
3502.707630	301712.895032	42.651853
3502.756204	301689.447268	42.656858
3502.670275	301670.907083	42.661863
3502.666497	301654.542820	42.666868
3502.739924	301626.713597	42.671872
3502.558395	301609.359076	42.676877
3502.505548	301590.024713	42.681882
3502.477153	301586.287912	42.686887
3502.801636	301564.502166	42.691892
3502.655773	301541.186538	42.696896
3502.284703	301509.812719	42.701901
3502.529814	301502.953591	42.706906
3502.436895	301494.034883	42.711911
3502.732205	301462.607757	42.716916
3502.393839	301449.502558	42.721920
3502.301190	301440.914662	42.726925
3502.405190	301416.440074	42.731930
3502.181005	301414.668143	42.736935
3502.094402	301393.990086	42.741940
3502.416514	301379.559966	42.746944
3502.268188	301376.859939	42.751949
3502.694053	301358.010572	42.756954
3502.558291	301341.514142	42.761959
3502.368650	301321.208480	42.766964
3502.676163	301303.726501	42.771968
3502.764816	301285.540654	42.776973
3502.731163	301260.069475	42.781978
3502.374762	301247.297910	42.786983
3502.723050	301229.325963	42.791988
3502.864386	301210.368322	42.796993
3502.461653	301185.667439	42.801997
3502.432571	301169.357886	42.807002
3502.328539	301164.360326	42.812007
3502.729943	301144.751177	42.817012
3502.713621	301126.454432	42.822017
3502.358134	301110.984876	42.827021
3502.458781	301081.013221	42.832026
3502.124767	301080.123787	42.837031
3502.327153	301062.836324	42.842036
3502.486730	301047.489833	42.847041
3502.027481	301033.843507	42.852045
3502.307741	301023.797430	42.857050
3502.109333	301003.594823	42.862055
3502.198921	300992.255090	42.867060
3502.364239	301001.162639	42.872065
3502.272205	300981.757830	42.877069
3502.349930	300968.867426	42.882074
3502.172556	300958.892883	42.887079
3502.459139	300931.844413	42.892084
3502.660806	300917.738414	42.897089
3502.394062	300901.720448	42.902093
3502.595433	300883.847708	42.907098
3502.322466	300876.789533	42.912103
3502.543227	300850.642105	42.917108
3502.259037	300834.652298	42.922113
3502.295302	300834.952081	42.927117
3502.535686	300811.397592	42.932122
3502.306173	300796.748142	42.937127
3502.714862	300785.231221	42.942132
3502.695108	300757.237957	42.947137
3502.452650	300743.201346	42.952141
3502.394984	300723.918328	42.957146
3502.251947	300708.899016	42.962151
3502.600797	300694.159117	42.967156
3502.447287	300679.166885	42.972161
3502.503172	300663.760143	42.977165
3502.423370	300641.680912	42.982170
3502.419545	300622.796661	42.987175
3502.454251	300617.497396	42.992180
3502.128036	300596.652883	42.997185
3502.208341	300584.703683	43.002189
3502.401500	300568.435558	43.007194
3502.353938	300556.837211	43.012199
3502.256874	300536.160460	43.017204
3502.153043	300529.890241	43.022209
3501.785900	300527.275283	43.027213
3502.192533	300504.178246	43.032218
3502.224354	300495.061711	43.037223
3502.097159	300490.194966	43.042228
3502.430630	300490.524641	43.047233
3502.183684	300475.877828	43.052237
3502.468927	300461.096908	43.057242
3501.969104	300446.667782	43.062247
3502.279823	300422.771260	43.067252
3502.110552	300416.638516	43.072257
3502.093667	300423.004051	43.077261
3502.359698	300398.707282	43.082266
3502.302111	300383.623617	43.087271
3501.939292	300368.002285	43.092276
3502.270116	300373.626276	43.097281
3502.003955	300348.598241	43.102285
3502.200232	300329.580799	43.107290
3502.196250	300334.544496	43.112295
3502.110200	300314.502225	43.117300
3501.985345	300297.112969	43.122305
3501.935656	300296.739003	43.127309
3502.186171	300288.657205	43.132314
3501.978814	300281.995919	43.137319
3501.835482	300249.262283	43.142324
3502.024539	300247.298449	43.147329
3501.787647	300243.925020	43.152333
3502.071154	300242.200935	43.157338
3502.120609	300238.782739	43.162343
3501.874333	300210.595543	43.167348
3502.165676	300209.761035	43.172353
3501.751672	300208.476867	43.177357
3502.121032	300193.682723	43.182362
3501.991610	300196.757179	43.187367
3502.216189	300169.947087	43.192372
3502.241367	300167.143518	43.197377
3502.391520	300165.414827	43.202381
3502.400065	300132.250152	43.207386
3502.461033	300125.852316	43.212391
3502.031104	300112.837462	43.217396
3501.914001	300087.786002	43.222401
3502.028686	300082.906858	43.227405
3502.140976	300074.973896	43.232410
3502.549812	300079.720368	43.237415
3502.549639	300050.043873	43.242420
3502.297880	300044.153047	43.247425
3502.221005	300030.166719	43.252429
3502.303215	300010.047128	43.257434
3502.332297	300002.050810	43.262439
3502.173662	299987.720930	43.267444
3502.319592	299966.547844	43.272449
3501.773767	299967.422217	43.277453
3502.173823	299947.889202	43.282458
3502.440168	299946.498662	43.287463
3502.223248	299922.353540	43.292468
3502.192512	299905.865704	43.297473
3502.150338	299909.639183	43.302477
3502.449773	299888.263906	43.307482
3502.136748	299874.161747	43.312487
3502.102712	299877.348567	43.317492
3502.279284	299850.673082	43.322497
3502.195903	299838.367534	43.327501
3502.063285	299833.017996	43.332506
3502.309704	299837.484460	43.337511
3502.061376	299816.016630	43.342516
3502.193352	299793.114942	43.347521
3502.152453	299798.695301	43.352525
3502.175997	299783.471528	43.357530
3501.896688	299769.924009	43.362535
3501.726045	299749.105753	43.367540
3502.312178	299750.515808	43.372545
3501.788362	299743.980285	43.377549
3501.948891	299722.372143	43.382554
3502.005329	299714.575120	43.387559
3502.161972	299703.351894	43.392564
3502.432156	299707.356521	43.397569
3502.103108	299689.566315	43.402573
3502.248400	299676.639589	43.407578
3501.964843	299679.432750	43.412583
3502.309449	299674.924852	43.417588
3502.470757	299645.655572	43.422593
3501.968268	299645.276036	43.427597
3502.460475	299631.455155	43.432602
3502.251562	299613.086202	43.437607
3502.113174	299589.641306	43.442612
3502.545575	299581.250998	43.447617
3502.619545	299572.382238	43.452621
3502.155764	299552.984134	43.457626
3502.177366	299550.359256	43.462631
3502.025263	299530.810609	43.467636
3502.260667	299512.855744	43.472641
3502.067709	299503.545118	43.477645
3502.541669	299502.682050	43.482650
3501.920191	299479.668959	43.487655
3501.845543	299471.688780	43.492660
3502.145393	299462.555621	43.497665
3501.997074	299465.073131	43.502669
3502.131256	299438.633140	43.507674
3502.329288	299426.563474	43.512679
3502.195861	299421.086763	43.517684
3502.287491	299410.891717	43.522689
3502.371111	299394.054974	43.527693
3502.066575	299380.409496	43.532698
3502.296554	299375.919494	43.537703
3502.241515	299363.583957	43.542708
3502.319365	299339.112522	43.547713
3502.229687	299343.758832	43.552717
3502.367129	299311.667941	43.557722
3501.846501	299310.960363	43.562727
3502.060087	299296.546659	43.567732
3502.280837	299285.236969	43.572737
3502.194375	299264.278108	43.577741
3502.254315	299257.320388	43.582746
3502.211483	299252.822123	43.587751
3502.220699	299227.903234	43.592756
3502.172373	299217.831841	43.597761
3502.078989	299229.019900	43.602765
3502.158330	299205.922581	43.607770
3502.003614	299204.674207	43.612775
3502.066940	299187.458794	43.617780
3502.154673	299173.726485	43.622785
3501.973918	299171.387745	43.627789
3501.942496	299145.813420	43.632794
3501.680271	299141.680323	43.637799
3501.864193	299141.269826	43.642804
3501.921865	299131.003681	43.647809
3501.948764	299129.116064	43.652813
3502.075461	299128.103665	43.657818
3501.966284	299103.763174	43.662823
3501.619122	299089.080753	43.667828
3501.937712	299093.892324	43.672833
3501.946131	299089.742362	43.677837
3501.738927	299086.262412	43.682842
3501.786434	299090.225542	43.687847
3501.766839	299070.630564	43.692852
3501.858138	299057.610326	43.697857
3502.016776	299051.986109	43.702861
3502.163308	299048.781730	43.707866
3502.123167	299047.617248	43.712871
3502.037984	299029.330565	43.717876
3502.155020	299008.416148	43.722881
3501.858184	299025.566391	43.727885
3502.378064	299014.795278	43.732890
3502.412383	298998.067931	43.737895
3502.159622	298988.079361	43.742900
3502.693596	298971.782932	43.747905
3502.075118	298955.844836	43.752909
3502.438156	298937.131718	43.757914
3501.954283	298919.569084	43.762919
3502.036932	298903.801333	43.767924
3502.199750	298895.045834	43.772929
3502.047404	298893.415301	43.777933
3501.862778	298887.488403	43.782938
3501.793455	298888.033774	43.787943
3501.801666	298861.638653	43.792948
3501.943491	298843.443678	43.797953
3501.800943	298853.595961	43.802957
3502.157649	298849.289722	43.807962
3501.856764	298849.260443	43.812967
3501.962048	298839.648557	43.817972
3501.941184	298816.490384	43.822977
3501.943418	298817.737229	43.827981
3502.031899	298808.611556	43.832986
3501.811024	298810.682299	43.837991
3502.051317	298790.792070	43.842996
3502.153007	298772.679704	43.848001
3501.567971	298770.047821	43.853005
3502.109619	298763.676486	43.858010
3501.845174	298765.728590	43.863015
3501.728113	298751.926385	43.868020
3501.811653	298730.889840	43.873025
3501.707266	298723.117820	43.878029
3502.280266	298719.414061	43.883034
3502.012648	298723.451936	43.888039
3501.924928	298719.826021	43.893044
3502.095112	298698.954083	43.898049
3501.589049	298691.779353	43.903053
3501.632984	298689.812701	43.908058
3501.434507	298685.440532	43.913063
3501.914523	298686.409067	43.918068
3502.258643	298682.868349	43.923073
3502.252731	298675.131832	43.928077
3502.052717	298653.783256	43.933082
3502.082519	298642.605097	43.938087
3501.795919	298636.668662	43.943092
3502.466060	298636.538479	43.948097
3502.080274	298621.531093	43.953101
3501.757162	298607.557448	43.958106
3502.199207	298604.281391	43.963111
3502.199040	298597.256628	43.968116
3502.265535	298573.702913	43.973121
3502.047403	298572.031750	43.978125
3502.202710	298553.020100	43.983130
3502.103085	298550.541389	43.988135
3501.934125	298530.715048	43.993140
3502.433921	298513.914783	43.998145
3502.134353	298516.481434	44.003149
3502.143673	298506.171828	44.008154
3501.932270	298497.143892	44.013159
3501.861685	298488.882961	44.018164
3502.231536	298479.204198	44.023169
3501.804758	298472.093401	44.028173
3501.592950	298442.958175	44.033178
3502.050257	298445.762832	44.038183
3502.064737	298433.848909	44.043188
3502.142279	298437.883747	44.048193
3501.981245	298437.069034	44.053197
3501.802255	298408.539515	44.058202
3502.050714	298402.824833	44.063207
3502.244330	298389.126681	44.068212
3502.147959	298396.701138	44.073217
3501.615868	298387.545154	44.078221
3502.055368	298364.951130	44.083226
3501.835245	298362.033105	44.088231
3501.839919	298361.014317	44.093236
3502.009041	298362.311439	44.098241
3501.695721	298365.363842	44.103245
3502.115503	298352.572060	44.108250
3502.015447	298330.036923	44.113255
3502.112653	298326.992929	44.118260
3501.946747	298315.005372	44.123265
3501.660401	298319.020752	44.128269
3502.031413	298307.890991	44.133274
3501.588285	298288.158332	44.138279
3501.413202	298294.523393	44.143284
3501.916012	298285.638287	44.148289
3501.547243	298279.307422	44.153293
3501.536666	298279.156399	44.158298
3501.641272	298273.515098	44.163303
3501.545763	298278.493290	44.168308
3502.163117	298264.525241	44.173313
3501.793579	298279.778148	44.178317
3501.734234	298267.341230	44.183322
3501.750324	298250.463793	44.188327
3501.821758	298245.794868	44.193332
3502.056008	298249.321624	44.198337
3501.866747	298244.820718	44.203341
3501.922921	298238.423412	44.208346
3501.928439	298229.616044	44.213351
3501.732390	298202.081732	44.218356
3502.156517	298196.288660	44.223361
3502.040944	298203.917050	44.228365
3501.703339	298191.040021	44.233370
3502.265054	298189.857786	44.238375
3501.718511	298172.126546	44.243380
3501.622386	298159.160852	44.248385
3501.761316	298148.500035	44.253389
3501.890891	298149.574272	44.258394
3501.799588	298151.370257	44.263399
3501.823026	298152.919232	44.268404
3501.994014	298134.795825	44.273409
3501.812330	298137.802208	44.278413
3501.863552	298112.545369	44.283418
3501.647765	298114.029935	44.288423
3501.813006	298105.655721	44.293428
3502.081691	298103.068503	44.298433
3501.753056	298110.602954	44.303437
3501.946498	298091.152492	44.308442
3501.681430	298077.016924	44.313447
3502.044756	298074.287646	44.318452
3501.853318	298070.652452	44.323457
3501.725202	298072.861435	44.328461
3501.772105	298072.803236	44.333466
3502.193484	298058.560344	44.338471
3501.929991	298040.403023	44.343476
3501.967554	298034.619464	44.348481
3501.962436	298037.496438	44.353485
3501.842728	298022.014599	44.358490
3501.654131	298031.003414	44.363495
3501.894812	298015.567041	44.368500
3502.086138	298002.963612	44.373505
3501.591666	297996.143315	44.378509
3502.018348	297980.881474	44.383514
3502.207964	297984.771560	44.388519
3501.789067	297976.717724	44.393524
3501.913010	297955.063708	44.398529
3501.781253	297961.065697	44.403533
3501.648579	297947.113018	44.408538
3501.554153	297942.953597	44.413543
3501.655599	297946.246610	44.418548
3501.937136	297935.385289	44.423553
3501.945644	297938.031065	44.428557
3501.716723	297916.101317	44.433562
3501.665556	297914.327673	44.438567
3501.609021	297920.674243	44.443572
3501.831635	297903.891677	44.448577
3501.830875	297913.741984	44.453581
3502.060872	297914.444190	44.458586
3501.955088	297913.824451	44.463591
3501.972406	297892.747038	44.468596
3502.212821	297863.897146	44.473601
3501.922495	297873.258227	44.478605
3502.005598	297866.169448	44.483610
3501.890847	297856.464530	44.488615
3501.865879	297843.258565	44.493620
3502.030982	297824.703284	44.498625
3501.739852	297827.828604	44.503629
3501.902971	297821.083647	44.508634
3502.220192	297826.888195	44.513639
3501.739547	297811.589990	44.518644
3502.094058	297792.496033	44.523649
3501.876617	297786.828674	44.528653
3501.898659	297781.582021	44.533658
3501.932401	297779.082425	44.538663
3501.605188	297782.900610	44.543668
3502.184014	297749.238108	44.548673
3502.082687	297754.522688	44.553677
3502.002644	297743.386975	44.558682
3502.021889	297741.118717	44.563687
3501.861689	297733.406191	44.568692
3502.072062	297709.727808	44.573697
3501.440788	297713.288103	44.578701
3501.847693	297709.686603	44.583706
3501.895522	297706.904822	44.588711
3501.870384	297714.086445	44.593716
3502.167577	297697.190347	44.598721
3501.969839	297680.880674	44.603725
3502.035178	297674.456419	44.608730
3501.860041	297680.057977	44.613735
3501.850362	297669.394850	44.618740
3502.184828	297654.656391	44.623745
3501.775478	297642.324960	44.628749
3501.842523	297629.002748	44.633754
3502.343325	297628.491795	44.638759
3501.881646	297622.328097	44.643764
3502.246139	297616.391572	44.648769
3502.013104	297601.818180	44.653773
3502.147351	297590.063523	44.658778
3501.753989	297599.797095	44.663783
3501.766582	297594.271923	44.668788
3501.952194	297579.149472	44.673793
3501.983055	297563.236723	44.678797
3502.095092	297560.164916	44.683802
3501.925012	297546.065270	44.688807
3501.756826	297552.582053	44.693812
3502.089882	297545.021460	44.698817
3501.978892	297522.564066	44.703821
3501.876046	297501.250765	44.708826
3502.057285	297510.563635	44.713831
3501.693396	297517.136471	44.718836
3501.928936	297494.548531	44.723841
3501.824209	297488.329012	44.728845
3501.658147	297475.781339	44.733850
3501.839775	297468.626202	44.738855
3501.847261	297472.442987	44.743860
3502.010928	297461.116401	44.748865
3501.810284	297470.667150	44.753869
3501.968813	297456.541559	44.758874
3502.218033	297434.485966	44.763879
3501.673605	297434.316591	44.768884
3501.873307	297416.290275	44.773889
3501.986575	297420.345054	44.778893
3502.064362	297417.787650	44.783898
3501.958424	297399.172791	44.788903
3501.932746	297384.770547	44.793908
3502.289216	297382.678629	44.798913
3501.965506	297380.362163	44.803917
3501.764613	297359.904081	44.808922
3501.746691	297349.165823	44.813927
3501.694251	297353.424684	44.818932
3501.765578	297343.741492	44.823937
3501.422848	297345.474999	44.828941
3501.456113	297342.186420	44.833946
3501.739777	297348.861660	44.838951
3501.700158	297339.679416	44.843956
3501.901430	297348.149237	44.848961
3501.760006	297342.979005	44.853965
3501.944248	297317.522844	44.858970
3502.224282	297301.825595	44.863975
3501.706087	297299.743154	44.868980
3502.112922	297294.538109	44.873985
3502.039762	297304.501654	44.878989
3501.876459	297282.077796	44.883994
3502.138247	297272.364815	44.888999
3501.779531	297270.333799	44.894004
3501.848745	297254.414967	44.899009
3501.418046	297257.765762	44.904013
3501.381125	297253.648205	44.909018
3501.819929	297255.106814	44.914023
3501.708594	297250.771815	44.919028
3501.948076	297226.401451	44.924033
3501.945977	297227.598103	44.929037
3501.788046	297219.706981	44.934042
3501.930894	297211.667023	44.939047
3501.928499	297216.070787	44.944052
3501.877091	297207.806669	44.949057
3501.781161	297195.324328	44.954061
3501.849204	297188.721425	44.959066
3502.068483	297182.094877	44.964071
3501.485585	297177.808143	44.969076
3501.417019	297175.095438	44.974081
3501.799297	297174.552106	44.979085
3501.703146	297179.072342	44.984090
3501.582272	297170.284568	44.989095
3502.037319	297175.864012	44.994100
3501.980243	297149.300122	44.999105
3501.726707	297151.325126	45.004109
3501.677897	297149.194749	45.009114
3502.103528	297141.263288	45.014119
3501.679430	297144.485793	45.019124
3502.042914	297132.720655	45.024129
3502.135224	297122.906879	45.029133
3501.961311	297115.603660	45.034138
3501.914045	297104.284526	45.039143
3502.105757	297103.109209	45.044148
3502.060929	297078.197812	45.049153
3501.799217	297080.885874	45.054157
3501.986075	297080.703981	45.059162
3502.087846	297074.630303	45.064167
3501.826500	297072.227715	45.069172
3501.963108	297057.494582	45.074177
3502.044529	297042.439183	45.079181
3501.955645	297032.424643	45.084186
3501.899652	297032.458888	45.089191
3502.237960	297023.981098	45.094196
3501.881367	297006.372511	45.099201
3501.952308	296996.587508	45.104205
3501.643443	296997.704859	45.109210
3502.393014	296981.654132	45.114215
3501.849683	296983.648089	45.119220
3501.640017	296958.075179	45.124225
3501.532733	296946.510867	45.129229
3501.801000	296945.629015	45.134234
3501.801166	296949.268808	45.139239
3501.743967	296945.612554	45.144244
3502.093215	296938.787487	45.149249
3501.962276	296944.025865	45.154253
3501.336060	296924.397711	45.159258
3501.906758	296905.244204	45.164263
3501.656064	296902.458148	45.169268
3501.583283	296903.818576	45.174273
3501.632827	296896.734923	45.179277
3501.644201	296891.031701	45.184282
3501.943641	296896.660953	45.189287
3501.556627	296910.262513	45.194292
3501.759096	296898.904295	45.199297
3501.974671	296899.685128	45.204301
3502.075915	296882.463079	45.209306
3502.053397	296869.587394	45.214311
3501.842627	296865.395176	45.219316
3502.238500	296855.966598	45.224321
3501.783407	296855.808708	45.229325
3501.916104	296841.050676	45.234330
3502.037108	296814.815131	45.239335
3501.504912	296825.919554	45.244340
3501.385400	296814.408033	45.249345
3501.648667	296824.395424	45.254349
3501.385980	296819.447728	45.259354
3501.524730	296812.630102	45.264359
3501.619288	296818.367752	45.269364
3501.741527	296821.912110	45.274369
3501.857759	296823.522973	45.279373
3501.802359	296810.168807	45.284378
3501.741256	296786.430669	45.289383
3501.842034	296789.316603	45.294388
3502.199410	296779.308610	45.299393
3501.889135	296780.629811	45.304397
3501.740927	296770.726312	45.309402
3501.953674	296772.805697	45.314407
3501.885348	296761.769771	45.319412
3501.673164	296749.076430	45.324417
3502.134851	296743.990025	45.329421
3501.809886	296738.084840	45.334426
3502.178561	296736.856396	45.339431
3501.846575	296728.432449	45.344436
3501.835090	296714.409614	45.349441
3501.728218	296714.222735	45.354445
3501.852424	296701.629510	45.359450
3501.883940	296693.123275	45.364455
3502.009458	296699.696051	45.369460
3501.756226	296689.783504	45.374465
3501.704838	296665.789266	45.379469
3501.872935	296667.392025	45.384474
3501.986354	296656.327665	45.389479
3501.984715	296664.447513	45.394484
3501.892488	296661.993015	45.399489
3502.252740	296642.745055	45.404493
3501.822137	296637.187266	45.409498
3501.963332	296625.482229	45.414503
3501.827682	296628.812386	45.419508
3501.783072	296618.281788	45.424513
3501.956638	296622.021759	45.429517
3501.859886	296591.136773	45.434522
3502.368705	296574.589054	45.439527
3501.786731	296585.014070	45.444532
3501.940185	296585.397368	45.449537
3502.005035	296567.748210	45.454541
3502.010814	296556.675207	45.459546
3502.223674	296536.737566	45.464551
3501.857071	296544.379972	45.469556
3502.078853	296549.308710	45.474561
3501.988005	296524.047921	45.479565
3501.652794	296506.384930	45.484570
3502.091986	296505.323630	45.489575
3502.262068	296502.955381	45.494580
3502.182313	296486.016043	45.499585
3501.910062	296474.044721	45.504589
3502.024846	296461.122025	45.509594
3501.947039	296458.588903	45.514599
3502.111686	296445.302062	45.519604
3501.787951	296446.523562	45.524609
3501.593324	296446.655841	45.529613
3501.844406	296440.049688	45.534618
3501.677569	296425.567457	45.539623
3501.548406	296425.511329	45.544628
3501.691425	296425.845353	45.549633
3501.681371	296439.464450	45.554637
3501.892258	296426.959427	45.559642
3502.072537	296429.476605	45.564647
3501.818987	296409.739104	45.569652
3501.837212	296394.693415	45.574657
3501.732803	296391.324492	45.579661
3501.792317	296379.988520	45.584666
3501.780391	296382.535750	45.589671
3501.674038	296383.926892	45.594676
3501.863576	296369.668918	45.599681
3501.521020	296355.366861	45.604685
3501.557446	296354.470339	45.609690
3501.921706	296344.639367	45.614695
3501.703981	296356.101969	45.619700
3501.853202	296344.904686	45.624705
3502.015452	296349.486403	45.629709
3501.660625	296341.422315	45.634714
3502.319847	296336.101366	45.639719
3501.976721	296327.297302	45.644724
3501.757688	296316.972092	45.649729
3502.275522	296301.568283	45.654733
3501.941806	296289.631985	45.659738
3501.828316	296277.406722	45.664743
3501.996232	296275.013350	45.669748
3501.987443	296269.542298	45.674753
3502.274467	296266.010357	45.679757
3502.093975	296257.919003	45.684762
3502.227081	296231.884926	45.689767
3501.745448	296219.437219	45.694772
3501.493423	296221.054766	45.699777
3501.792812	296219.811690	45.704781
3501.593292	296221.013775	45.709786
3501.490586	296213.368413	45.714791
3501.968970	296214.108168	45.719796
3502.055990	296205.287743	45.724801
3501.853799	296183.938574	45.729805
3502.154369	296186.436957	45.734810
3502.218104	296179.732797	45.739815
3501.931417	296177.461400	45.744820
3501.921422	296143.024591	45.749825
3502.039337	296088.103235	45.754829
3501.611212	295990.429062	45.759834
3501.707376	295843.038436	45.764839
3501.573216	295656.866729	45.769844
3500.981614	295414.615112	45.774849
3501.143589	295130.373150	45.779853
3500.789959	294799.171505	45.784858
3500.590701	294416.348356	45.789863
3500.294222	293991.767408	45.794868
3500.095496	293512.008225	45.799873
3499.495046	292990.256783	45.804877
3499.230411	292422.680286	45.809882
3498.817762	291803.371153	45.814887
3497.782631	291146.937143	45.819892
3497.054377	290431.085298	45.824897
3496.342918	289687.755515	45.829901
3496.210439	288889.009714	45.834906
3495.468248	288043.305225	45.839911
3494.809194	287153.357768	45.844916
3493.862444	286220.878423	45.849921
3493.081125	285225.122998	45.854925
3492.072868	284192.575914	45.859930
3491.574007	283122.611487	45.864935
3490.713070	282007.243130	45.869940
3489.286658	280834.076655	45.874945
3488.409796	279622.488482	45.879949
3487.273866	278366.925957	45.884954
3486.563625	277054.830055	45.889959
3485.245471	275728.014447	45.894964
3483.644049	274324.607616	45.899969
3482.856793	272900.807551	45.904973
3481.492047	271428.491862	45.909978
3480.539237	269905.339835	45.914983
3479.001017	268348.667920	45.919988
3477.425586	266740.106725	45.924993
3475.830153	265101.882147	45.929997
3474.577055	263431.747212	45.935002
3473.105632	261699.842465	45.940007
3471.330124	259944.377603	45.945012
3469.819911	258161.189340	45.950017
3467.969679	256324.371650	45.955021
3466.007356	254454.745074	45.960026
3464.516984	252549.264400	45.965031
3462.489820	250598.588405	45.970036
3460.739502	248632.794267	45.975041
3458.497658	246624.549340	45.980045
3456.654013	244584.156933	45.985050
3454.950206	242502.031582	45.990055
3452.720836	240387.192278	45.995060
3450.867386	238242.912347	46.000065
3448.498938	236083.162336	46.005069
3445.836309	233874.112760	46.010074
3443.830240	231631.942412	46.015079
3441.532206	229387.441150	46.020084
3439.153711	227093.129810	46.025089
3436.980661	224772.245109	46.030093
3433.907612	222434.131755	46.035098
3431.459219	220068.265077	46.040103
3428.876676	217682.458742	46.045108
3426.554589	215263.716464	46.050113
3424.048548	212828.819087	46.055117
3421.096127	210352.954353	46.060122
3418.714075	207863.728277	46.065127
3415.368312	205360.366159	46.070132
3412.872856	202827.308196	46.075137
3409.634368	200276.981927	46.080141
3406.184971	197720.972736	46.085146
3403.418926	195131.132292	46.090151
3399.747576	192526.406926	46.095156
3396.823569	189906.161495	46.100161
3393.590467	187293.713897	46.105165
3390.248196	184658.530874	46.110170
3386.904823	182010.939820	46.115175
3383.163089	179352.052364	46.120180
3379.705278	176681.181801	46.125185
3376.414527	174010.815292	46.130189
3372.830849	171338.661588	46.135194
3369.120176	168649.882406	46.140199
3364.959257	165958.778699	46.145204
3361.029704	163272.835177	46.150209
3356.848344	160583.960120	46.155213
3352.305985	157910.299688	46.160218
3348.008372	155234.198756	46.165223
3343.364196	152563.645132	46.170228
3338.636983	149907.115029	46.175233
3334.278299	147263.496975	46.180237
3329.162270	144644.319820	46.185242
3324.402057	142026.914607	46.190247
3319.021030	139407.392230	46.195252
3313.712750	136793.384234	46.200257
3307.816460	134278.934098	46.205261
3301.825229	131788.555042	46.210266
3295.604302	129333.245446	46.215271
3288.905699	126925.036245	46.220276
3282.484509	124577.948014	46.225281
3275.396486	122273.387427	46.230285
3267.909981	120039.655121	46.235290
3260.532655	117862.381647	46.240295
3252.645562	115756.674189	46.245300
3244.670893	113733.722697	46.250305
3236.958445	111780.542994	46.255309
3228.812325	109912.224069	46.260314
3220.730806	108106.008694	46.265319
3212.248183	106426.655714	46.270324
3203.537560	104797.759977	46.275329
3194.871230	103280.338151	46.280333
3186.346010	101850.375528	46.285338
3178.050675	100522.540779	46.290343
3169.521838	99270.966497	46.295348
3161.159284	98113.832500	46.300353
3153.136173	97044.010314	46.305357
3145.411928	96062.539900	46.310362
3138.328771	95142.469239	46.315367
3131.668867	94291.401049	46.320372
3124.586945	93509.017244	46.325377
3118.807273	92794.395044	46.330381
3112.398543	92136.319330	46.335386
3106.810310	91517.850570	46.340391
3101.117644	90965.941640	46.345396
3095.582235	90453.775981	46.350401
3090.851119	89964.694462	46.355405
3085.934884	89535.634108	46.360410
3081.754412	89111.801236	46.365415
3077.255266	88717.678843	46.370420
3073.133026	88347.299833	46.375425
3069.226786	87992.887503	46.380429
3065.375794	87662.902579	46.385434
3062.134672	87329.725981	46.390439
3058.494068	87018.315366	46.395444
3054.898047	86707.421974	46.400449
3051.697501	86402.110838	46.405453
3048.325423	86105.240011	46.410458
3044.959207	85785.452843	46.415463
3041.515036	85505.191144	46.420468
3038.255627	85204.144947	46.425473
3034.774439	84908.599218	46.430477
3031.154192	84641.788683	46.435482
3028.318564	84338.512893	46.440487
3025.369002	84053.678147	46.445492
3021.921533	83767.641052	46.450497
3018.623825	83471.674881	46.455501
3015.062798	83179.144676	46.460506
3011.425711	82887.607494	46.465511
3008.184645	82596.049473	46.470516
3004.781867	82302.055410	46.475521
3001.550910	82008.748868	46.480525
2997.616248	81723.519842	46.485530
2994.285710	81425.344488	46.490535
2990.658870	81150.565223	46.495540
2987.082209	80873.773872	46.500545
2983.491313	80581.249791	46.505549
2979.806859	80308.227949	46.510554
2976.253738	80037.753974	46.515559
2972.453344	79766.559200	46.520564
2968.649541	79491.023712	46.525569
2965.338926	79220.875389	46.530573
2961.721758	78959.071510	46.535578
2957.706426	78695.935258	46.540583
2954.065322	78445.774160	46.545588
2950.450077	78192.690096	46.550593
2946.748988	77936.751421	46.555597
2942.882242	77696.818394	46.560602
2939.367313	77446.837159	46.565607
2935.851466	77213.584745	46.570612
2931.970351	76974.993832	46.575617
2928.873346	76737.615893	46.580621
2924.816504	76508.391165	46.585626
2921.479808	76287.488510	46.590631
2918.317610	76054.825705	46.595636
2914.335891	75820.870693	46.600641
2910.974708	75577.168945	46.605645
2907.290515	75364.455919	46.610650
2903.767449	75133.711601	46.615655
2899.921809	74922.690934	46.620660
2896.471743	74698.237791	46.625665
2893.137655	74475.647852	46.630669
2889.495960	74254.161884	46.635674
2886.046054	74029.739708	46.640679
2882.577738	73826.618161	46.645684
2878.799273	73608.003466	46.650689
2875.967750	73395.515568	46.655693
2872.138661	73177.623443	46.660698
2868.754822	72971.066617	46.665703
2865.171209	72747.209486	46.670708
2861.493295	72524.448337	46.675713
2858.131709	72311.086954	46.680717
2854.452588	72102.284734	46.685722
2851.294384	71881.085764	46.690727
2847.830780	71669.713689	46.695732
2844.363859	71451.195048	46.700737
2840.939260	71233.268389	46.705741
2837.267749	71013.337868	46.710746
2834.100011	70799.577494	46.715751
2830.458017	70574.706774	46.720756
2827.006868	70369.526784	46.725761
2823.922638	70151.479715	46.730765
2819.914639	69925.979840	46.735770
2816.867503	69707.778320	46.740775
2813.262757	69480.238539	46.745780
2810.052928	69261.088570	46.750785
2806.376843	69033.176623	46.755789
2802.865382	68816.566103	46.760794
2799.468610	68577.378197	46.765799
2796.024119	68363.401827	46.770804
2792.206661	68134.783545	46.775809
2788.697493	67915.812423	46.780813
2785.131684	67699.962505	46.785818
2781.749025	67467.873326	46.790823
2778.361041	67243.074357	46.795828
2774.794320	67031.146812	46.800833
2771.541036	66796.796382	46.805837
2767.760692	66573.010483	46.810842
2764.423878	66348.789021	46.815847
2760.900844	66125.512705	46.820852
2757.178926	65899.006861	46.825857
2753.995080	65668.731036	46.830861
2750.343535	65450.190545	46.835866
2746.961283	65214.973555	46.840871
2743.428812	64991.207280	46.845876
2740.025514	64762.719525	46.850881
2736.744219	64535.154135	46.855885
2732.404244	64312.910211	46.860890
2729.404406	64082.607393	46.865895
2726.062308	63863.270638	46.870900
2722.691566	63638.831029	46.875905
2719.382251	63398.421523	46.880909
2715.777692	63173.089684	46.885914
2712.125007	62939.973633	46.890919
2708.922232	62706.440329	46.895924
2705.202527	62471.333608	46.900929
2701.779998	62247.003491	46.905933
2698.203664	62012.716437	46.910938
2694.768773	61769.080234	46.915943
2691.382113	61534.120711	46.920948
2687.671307	61308.765313	46.925953
2684.215454	61066.618012	46.930957
2680.621752	60838.614910	46.935962
2677.568556	60604.176912	46.940967
2673.959467	60370.297710	46.945972
2670.579956	60142.565840	46.950977
2666.886409	59891.265610	46.955981
2662.977380	59669.256169	46.960986
2659.617213	59434.445871	46.965991
2655.979807	59201.432631	46.970996
2652.778578	58963.987557	46.976001
2649.583920	58719.576267	46.981005
2645.548023	58493.377561	46.986010
2642.170578	58241.638813	46.991015
2638.884677	58003.467620	46.996020
2634.894018	57781.799147	47.001025
2631.901860	57541.644876	47.006029
2628.452438	57304.166080	47.011034
2624.875771	57065.332624	47.016039
2621.467840	56826.671849	47.021044
2618.000106	56586.696683	47.026049
2614.711435	56343.142707	47.031053
2610.743714	56106.917977	47.036058
2607.413166	55861.897084	47.041063
2604.056381	55626.514248	47.046068
2600.619019	55383.221742	47.051073
2597.059168	55136.036210	47.056077
2593.616725	54909.651609	47.061082
2590.188330	54655.287439	47.066087
2586.580021	54409.094131	47.071092
2583.136289	54175.236596	47.076097
2579.651050	53921.713987	47.081101
2576.190891	53685.814646	47.086106
2572.492573	53432.336979	47.091111
2569.010759	53184.912237	47.096116
2565.252519	52950.919397	47.101121
2562.180201	52702.725148	47.106125
2558.484255	52454.561296	47.111130
2555.279982	52215.039694	47.116135
2551.736067	51969.248872	47.121140
2548.221521	51719.922569	47.126145
2544.507250	51476.396605	47.131149
2540.884516	51229.471375	47.136154
2537.453869	50983.153083	47.141159
2533.902940	50736.843539	47.146164
2530.325407	50493.997951	47.151169
2527.099798	50257.290997	47.156173
2523.622816	50006.550000	47.161178
2520.135952	49758.350573	47.166183
2516.598163	49500.685103	47.171188
2513.054881	49262.801151	47.176193
2509.929597	49017.217272	47.181197
2505.980405	48759.332707	47.186202
2502.865202	48512.021044	47.191207
2499.334529	48261.979865	47.196212
2495.754741	48018.811969	47.201217
2492.636801	47769.923093	47.206221
2488.915328	47508.611032	47.211226
2485.667309	47251.731119	47.216231
2482.187579	46990.590170	47.221236
2478.388896	46750.127599	47.226241
2475.171923	46483.522306	47.231245
2471.118750	46229.919396	47.236250
2467.439970	45976.362250	47.241255
2464.340549	45720.802014	47.246260
2460.696479	45476.105008	47.251265
2457.429171	45211.907254	47.256269
2453.593110	44964.347588	47.261274
2450.189421	44707.863495	47.266279
2446.983853	44458.809254	47.271284
2443.017008	44193.204602	47.276289
2439.772713	43941.213319	47.281293
2436.249807	43686.110389	47.286298
2432.758692	43426.496636	47.291303
2429.409845	43169.400220	47.296308
2425.659421	42913.308121	47.301313
2422.416825	42656.321526	47.306317
2418.817671	42403.071575	47.311322
2415.555864	42134.458020	47.316327
2412.008901	41883.254048	47.321332
2408.438780	41620.420936	47.326337
2405.118922	41356.873346	47.331341
2401.705439	41104.306798	47.336346
2397.868286	40845.475061	47.341351
2394.625356	40583.566986	47.346356
2391.105136	40330.328604	47.351361
2387.820740	40048.872782	47.356365
2384.562634	39796.848669	47.361370
2381.098058	39519.346257	47.366375
2377.410654	39264.700833	47.371380
2373.706985	38992.460598	47.376385
2370.504330	38714.058911	47.381389
2366.664901	38453.620262	47.386394
2363.225083	38180.524771	47.391399
2360.233749	37918.305184	47.396404
2356.292640	37643.253490	47.401409
2353.264294	37361.684782	47.406413
2349.714131	37101.350379	47.411418
2346.253025	36820.300252	47.416423
2342.815257	36553.349126	47.421428
2339.237029	36271.538440	47.426433
2335.667045	35996.329395	47.431437
2332.155650	35725.374693	47.436442
2328.755416	35447.965490	47.441447
2325.283092	35163.230566	47.446452
2321.830469	34889.900183	47.451457
2318.264955	34612.882741	47.456461
2314.446482	34331.186094	47.461466
2311.144855	34049.507428	47.466471
2307.458115	33776.652767	47.471476
2304.148009	33497.004838	47.476481
2300.965196	33213.683420	47.481485
2297.410060	32935.291949	47.486490
2293.684798	32652.069318	47.491495
2290.745654	32375.522097	47.496500
2287.082985	32093.406427	47.501505
2283.784692	31802.085435	47.506509
2280.374809	31511.869762	47.511514
2277.378087	31214.888042	47.516519
2273.582231	30915.101200	47.521524
2269.841303	30622.972353	47.526529
2266.870192	30323.166446	47.531533
2263.223408	30030.530565	47.536538
2259.709015	29731.787870	47.541543
2256.305644	29428.526305	47.546548
2252.791529	29134.241028	47.551553
2249.593798	28831.336328	47.556557
2245.915439	28534.075212	47.561562
2242.547298	28222.758892	47.566567
2238.986334	27925.241111	47.571572
2235.262685	27617.633317	47.576577
2232.191386	27304.928479	47.581581
2228.192364	27005.344530	47.586586
2225.019468	26685.625183	47.591591
2221.884199	26388.177320	47.596596
2218.266177	26072.605228	47.601601
2214.914817	25757.268794	47.606605
2211.418718	25449.664598	47.611610
2208.029423	25135.965842	47.616615
2204.716199	24813.985411	47.621620
2200.871251	24498.752232	47.626625
2197.613675	24175.252745	47.631629
2194.305478	23862.625580	47.636634
2190.762894	23542.671809	47.641639
2187.331407	23217.111645	47.646644
2183.369852	22896.384848	47.651649
2180.132220	22566.059873	47.656653
2176.561964	22253.486267	47.661658
2173.169776	21922.125556	47.666663
2169.454044	21591.688883	47.671668
2165.954946	21277.877906	47.676673
2162.832870	20937.787469	47.681677
2159.044388	20619.065885	47.686682
2155.743198	20295.915127	47.691687
2152.421013	19967.686494	47.696692
2148.565849	19642.935555	47.701697
2145.085799	19318.188320	47.706701
2141.520956	18983.103622	47.711706
2137.538522	18672.684599	47.716711
2133.698858	18353.881216	47.721716
2130.314222	18045.715836	47.726721
2126.559949	17736.454127	47.731725
2122.712088	17428.852372	47.736730
2118.662396	17132.547895	47.741735
2114.947176	16840.404120	47.746740
2110.784447	16545.896494	47.751745
2107.362490	16259.516866	47.756749
2103.055074	15983.384403	47.761754
2099.027566	15710.163269	47.766759
2095.877515	15436.859398	47.771764
2091.769219	15183.150966	47.776769
2088.333949	14916.276255	47.781773
2084.754782	14669.049354	47.786778
2080.725446	14405.862147	47.791783
2077.236879	14161.166993	47.796788
2073.305881	13924.003727	47.801793
2069.962574	13668.552502	47.806797
2065.816538	13436.890552	47.811802
2062.054844	13208.122064	47.816807
2057.881951	12997.625315	47.821812
2054.310576	12781.781250	47.826817
2050.596925	12563.790068	47.831821
2046.876109	12367.191467	47.836826
2043.045624	12157.328021	47.841831
2039.537624	11952.402667	47.846836
2035.753332	11756.852439	47.851841
2032.553436	11557.166933	47.856845
2029.052901	11369.262865	47.861850
2025.427609	11151.555970	47.866855
2022.041218	10960.978933	47.871860
2018.528474	10782.291637	47.876865
2015.453592	10580.985649	47.881869
2011.595533	10385.527752	47.886874
2008.124817	10201.875793	47.891879
2005.005716	9994.175964	47.896884
2001.347029	9801.757214	47.901889
1997.733320	9604.721348	47.906893
1994.604150	9415.759546	47.911898
1991.190461	9224.175761	47.916903
1987.554062	9034.831891	47.921908
1983.847100	8843.164985	47.926913
1980.896287	8645.636738	47.931917
1977.048685	8457.857482	47.936922
1973.546608	8255.969299	47.941927
1970.343821	8066.678263	47.946932
1966.647824	7878.374744	47.951937
1963.128382	7673.966677	47.956941
1959.809841	7487.766700	47.961946
1956.513807	7295.583118	47.966951
1953.233270	7088.083556	47.971956
1949.494094	6896.403931	47.976961
1945.853939	6703.998697	47.981965
1942.441290	6508.129102	47.986970
1939.004156	6305.138097	47.991975
1935.386521	6108.722508	47.996980
1931.838494	5924.118752	48.001985
1928.494161	5721.379217	48.006989
1924.859095	5532.105989	48.011994
1921.082683	5337.286931	48.016999
1918.226470	5145.269122	48.022004
1914.369914	4950.162934	48.027009
1911.002904	4745.383937	48.032013
1907.346883	4558.893148	48.037018
1903.849858	4363.211679	48.042023
1900.916932	4168.630743	48.047028
1896.511943	3979.525803	48.052033
1893.549104	3784.035974	48.057037
1889.581640	3586.493535	48.062042
1886.132851	3397.852616	48.067047
1882.762818	3207.435634	48.072052
1879.051892	3013.795771	48.077057
1875.634909	2831.503419	48.082061
1872.108956	2643.369766	48.087066
1868.492850	2456.723550	48.092071
1865.318335	2254.935980	48.097076
1861.278754	2073.096804	48.102081
1858.121391	1883.486390	48.107085
1854.692371	1696.173322	48.112090
1851.239207	1504.971038	48.117095
1847.268202	1318.803526	48.122100
1843.465830	1141.704869	48.127105
1839.929432	954.005054	48.132109
1836.403369	782.925695	48.137114
1832.091153	607.775677	48.142119
1828.468402	432.427736	48.147124
1824.812079	275.959054	48.152129
1820.956962	108.414729	48.157133
1815.351944	11.074943	48.162138
1804.503850	53.073033	48.167143
1797.992451	54.883013	48.172148
1793.052078	60.965044	48.177153
1790.240910	55.640576	48.182157
1788.120403	58.149155	48.187162
1785.614787	63.584403	48.192167
1783.470736	60.566349	48.197172
1779.861623	65.348540	48.202177
1776.292464	55.586829	48.207181
1773.239728	61.642383	48.212186
1769.828604	72.154871	48.217191
1766.734506	58.737396	48.222196
1763.244925	65.237811	48.227201
1759.675666	65.755300	48.232205
1756.451407	62.836698	48.237210
1752.943225	68.871786	48.242215
1749.603627	65.300511	48.247220
1745.644276	67.622306	48.252225
1742.496538	63.290171	48.257229
1739.021322	63.476569	48.262234
1736.016383	63.155930	48.267239
1732.847786	64.983812	48.272244
1728.934759	66.007534	48.277249
1725.451562	62.743484	48.282253
1722.214969	67.423100	48.287258
1718.369227	76.380593	48.292263
1715.202745	59.402539	48.297268
1711.640559	77.667839	48.302273
1708.388945	63.155052	48.307277
1704.869193	65.025244	48.312282
1701.154174	70.153070	48.317287
1698.134866	58.214068	48.322292
1694.123821	62.682697	48.327297
1690.867526	76.224037	48.332301
1687.760170	70.964934	48.337306
1683.640420	69.119824	48.342311
1680.768099	62.985535	48.347316
1677.139882	65.087850	48.352321
1673.650999	57.243534	48.357325
1670.113657	60.502231	48.362330
1666.434118	72.784185	48.367335
1663.192536	58.636852	48.372340
1659.634795	71.532502	48.377345
1656.195281	62.696524	48.382349
1652.974830	59.286973	48.387354
1648.785734	64.973072	48.392359
1645.697713	58.154374	48.397364
1642.245404	58.536539	48.402369
1639.099823	67.299047	48.407373
1635.577042	60.757206	48.412378
1631.749680	59.932556	48.417383
1628.667892	59.291778	48.422388
1624.493230	65.595730	48.427393
1621.326318	54.100647	48.432397
1618.196247	54.932266	48.437402
1614.235618	57.089790	48.442407
1611.103691	54.511133	48.447412
1607.342980	60.731319	48.452417
1603.824626	55.492282	48.457421
1600.533113	65.916483	48.462426
1596.973491	57.978865	48.467431
1593.866829	53.741596	48.472436
1590.094837	56.825070	48.477441
1586.531188	51.691209	48.482445
1582.743377	56.036350	48.487450
1579.243718	57.416214	48.492455
1576.087626	50.282328	48.497460
1572.777024	65.246398	48.502465
1568.843530	49.416703	48.507469
1565.578084	54.145168	48.512474
1561.719026	55.451574	48.517479
1558.528044	45.270100	48.522484
1555.166292	53.047715	48.527489
1552.120923	50.490332	48.532493
1548.671422	55.310886	48.537498
1544.663375	60.481460	48.542503
1541.110461	52.289714	48.547508
1537.142104	58.210223	48.552513
1533.944147	55.410970	48.557517
1530.555074	64.265397	48.562522
1526.924163	65.412719	48.567527
1523.567299	61.432935	48.572532
1520.412071	59.468566	48.577537
1516.689566	65.958051	48.582541
1513.358211	58.756704	48.587546
1509.784975	62.097002	48.592551
1506.559291	49.592428	48.597556
1502.743701	55.931967	48.602561
1498.884708	58.614635	48.607565
1495.726913	58.666010	48.612570
1491.817916	54.623963	48.617575
1488.672577	55.002424	48.622580
1485.568989	56.105187	48.627585
1481.481605	59.779074	48.632589
1478.149588	55.485368	48.637594
1474.704191	60.631173	48.642599
1470.997222	51.951037	48.647604
1467.713985	53.110399	48.652609
1464.460821	55.916551	48.657613
1460.779789	45.773857	48.662618
1457.324549	51.781756	48.667623
1453.857810	52.004889	48.672628
1450.097577	54.849287	48.677633
1446.406700	53.269347	48.682637
1443.279651	50.389423	48.687642
1439.636284	51.950017	48.692647
1436.305931	51.303914	48.697652
1432.619280	56.867148	48.702657
1429.205692	53.848580	48.707661
1425.875262	43.777575	48.712666
1422.276364	59.669493	48.717671
1418.803406	51.958835	48.722676
1415.395459	54.510818	48.727681
1411.501047	63.197601	48.732685
1408.368260	59.496001	48.737690
1404.449432	65.101917	48.742695
1401.674722	51.419470	48.747700
1397.633169	54.336396	48.752705
1393.937712	54.332758	48.757709
1390.950411	43.948626	48.762714
1386.975372	59.586216	48.767719
1383.999118	47.150222	48.772724
1380.041731	56.213869	48.777729
1376.620157	45.923030	48.782733
1373.312060	49.829314	48.787738
1369.571442	51.778482	48.792743
1366.132770	53.617111	48.797748
1362.641375	60.124250	48.802753
1359.352026	55.877693	48.807757
1355.882198	51.390469	48.812762
1352.200270	58.183702	48.817767
1349.085686	45.345430	48.822772
1345.276640	47.080690	48.827777
1341.596969	60.093573	48.832781
1338.193418	49.113386	48.837786
1334.442027	65.282303	48.842791
1331.181680	60.420605	48.847796
1328.197235	60.400603	48.852801
1323.831634	63.833362	48.857805
1320.946121	60.583470	48.862810
1316.954153	62.812452	48.867815
1313.908929	52.864523	48.872820
1310.244307	52.865580	48.877825
1306.678847	57.698033	48.882829
1303.303703	47.545491	48.887834
1299.430634	56.637094	48.892839
1296.446988	55.955747	48.897844
1292.828809	57.664311	48.902849
1289.247706	50.432550	48.907853
1286.070323	50.483894	48.912858
1282.496683	52.270911	48.917863
1278.742335	47.537191	48.922868
1275.262646	57.345510	48.927873
1271.593282	60.042868	48.932877
1268.073995	62.239002	48.937882
1264.248378	55.776361	48.942887
1261.359966	48.818991	48.947892
1257.647985	47.618919	48.952897
1253.865136	50.821269	48.957901
1250.891396	49.341113	48.962906
1247.006773	58.121327	48.967911
1243.778242	42.434554	48.972916
1240.621325	49.091846	48.977921
1236.447965	53.168429	48.982925
1233.561719	52.155475	48.987930
1229.319409	49.646372	48.992935
1225.871781	46.585754	48.997940
1222.820688	48.540926	49.002945
1219.410426	58.003031	49.007949
1215.574634	49.178662	49.012954
1211.798980	57.233142	49.017959
1208.879424	43.842376	49.022964
1205.465901	49.097166	49.027969
1201.500473	55.368512	49.032973
1198.110075	56.411858	49.037978
1194.589005	52.242769	49.042983
1190.951786	50.448882	49.047988
1187.864371	51.577677	49.052993
1184.319695	53.192515	49.057997
1181.181657	49.798705	49.063002
1177.088121	54.780311	49.068007
1173.656031	48.708525	49.073012
1169.940332	51.280292	49.078017
1166.560730	55.055464	49.083021
1163.012735	47.692024	49.088026
1159.797101	45.522098	49.093031
1156.312090	52.414277	49.098036
1152.900002	58.304781	49.103041
1148.868159	51.741600	49.108045
1145.988640	53.138419	49.113050
1141.787977	57.595805	49.118055
1138.833071	49.323266	49.123060
1135.215015	51.702588	49.128065
1131.261014	52.100197	49.133069
1128.082324	46.396886	49.138074
1124.305560	55.214036	49.143079
1121.274828	46.225708	49.148084
1117.876620	47.937861	49.153089
1114.188881	54.358753	49.158093
1110.829441	46.813953	49.163098
1106.752921	58.522277	49.168103
1103.493327	58.659318	49.173108
1100.030875	48.653412	49.178113
1096.546254	52.103360	49.183117
1093.276165	46.436518	49.188122
1089.739682	60.407820	49.193127
1086.064263	52.694198	49.198132
1082.649272	49.982867	49.203137
1079.114511	51.842964	49.208141
1075.824185	48.039598	49.213146
1071.613116	50.843984	49.218151
1068.385251	55.829303	49.223156
1065.031300	41.427762	49.228161
1061.605036	52.939375	49.233165
1058.268962	47.785918	49.238170
1055.074879	54.518683	49.243175
1051.171773	51.428203	49.248180
1047.542044	52.335064	49.253185
1043.670793	68.481691	49.258189
1040.317308	52.254580	49.263194
1036.898157	53.830834	49.268199
1033.703085	47.298050	49.273204
1030.396270	53.428372	49.278209
1026.222902	57.210809	49.283213
1022.758196	41.475697	49.288218
1019.343063	52.833717	49.293223
1016.195942	58.995990	49.298228
1012.754782	55.485182	49.303233
1008.980265	53.393322	49.308237
1005.480007	49.967703	49.313242
1001.953862	54.537833	49.318247
998.509529	52.701166	49.323252
994.797282	45.391991	49.328257
991.368952	50.959215	49.333261
988.303587	50.284433	49.338266
984.737733	52.250672	49.343271
981.118127	53.399583	49.348276
977.266429	57.970075	49.353281
973.466169	48.029774	49.358285
970.504355	49.082023	49.363290
967.067770	55.210536	49.368295
963.598959	53.187889	49.373300
960.413255	54.363782	49.378305
956.405632	51.011296	49.383309
952.968780	49.986565	49.388314
949.426578	65.290750	49.393319
945.984843	47.593697	49.398324
942.532104	48.153344	49.403329
938.826857	60.341430	49.408333
935.340531	47.004720	49.413338
931.728414	51.319413	49.418343
928.465680	64.738527	49.423348
925.018806	55.033979	49.428353
921.508066	58.314069	49.433357
918.168685	46.820985	49.438362
914.437794	58.718862	49.443367
910.677792	55.843318	49.448372
907.554793	52.035960	49.453377
904.120990	51.975720	49.458381
900.439118	53.472935	49.463386
896.764606	43.826197	49.468391
893.364129	42.441451	49.473396
889.947325	44.362238	49.478401
886.399650	52.207116	49.483405
883.102206	38.888317	49.488410
878.993439	52.544315	49.493415
875.694191	41.791619	49.498420
872.450209	52.230694	49.503425
869.093290	48.434670	49.508429
865.532665	47.869117	49.513434
861.984474	53.315945	49.518439
858.517063	54.526493	49.523444
854.810190	54.815916	49.528449
851.327430	52.567704	49.533453
847.946505	51.698771	49.538458
843.997486	48.564951	49.543463
840.794485	48.819772	49.548468
837.315604	46.188143	49.553473
833.861014	56.805743	49.558477
830.661627	44.139166	49.563482
826.639778	58.781325	49.568487
823.374795	54.129358	49.573492
820.396165	56.089124	49.578497
816.402662	51.864454	49.583501
813.356274	46.580311	49.588506
809.382334	47.800591	49.593511
805.439136	51.977347	49.598516
801.889940	50.407114	49.603521
798.367392	57.150259	49.608525
795.808317	52.489002	49.613530
792.075065	58.654537	49.618535
788.301538	54.582095	49.623540
784.713293	57.561155	49.628545
780.944543	52.598949	49.633549
777.970324	58.408344	49.638554
774.526692	58.422458	49.643559
770.857504	51.831143	49.648564
767.343529	47.262484	49.653569
763.311308	47.172620	49.658573
760.091421	45.123726	49.663578
756.897676	52.581024	49.668583
753.456055	45.868661	49.673588
750.096308	49.833847	49.678593
746.048884	64.951442	49.683597
742.767484	49.159285	49.688602
739.242562	61.898161	49.693607
735.935497	48.878325	49.698612
732.353746	48.939394	49.703617
729.100787	44.418462	49.708621
725.009018	47.868702	49.713626
721.343245	57.994221	49.718631
717.971305	51.122262	49.723636
715.115668	44.071376	49.728641
711.259023	50.594783	49.733645
707.376644	49.215971	49.738650
704.141377	54.398711	49.743655
700.761753	53.384095	49.748660
697.428665	44.930508	49.753665
693.845879	47.816996	49.758669
690.257165	48.723897	49.763674
686.814189	56.935258	49.768679
683.485840	50.863248	49.773684
679.709090	54.599533	49.778689
676.052874	56.320607	49.783693
672.878549	51.075533	49.788698
669.254945	62.801659	49.793703
665.574521	58.328710	49.798708
662.491920	57.950966	49.803713
658.700093	52.903843	49.808717
655.324847	51.569019	49.813722
651.826467	53.660854	49.818727
648.247589	53.398802	49.823732
644.610330	50.380763	49.828737
640.734623	52.038149	49.833741
637.841527	57.708327	49.838746
633.954882	51.651006	49.843751
630.922821	56.434948	49.848756
627.283500	50.879901	49.853761
623.641611	49.523573	49.858765
620.019632	50.362944	49.863770
616.603017	54.058670	49.868775
612.879264	50.373982	49.873780
609.553904	45.772686	49.878785
605.989672	48.042531	49.883789
602.835822	53.940217	49.888794
599.371035	46.554503	49.893799
595.836341	43.378054	49.898804
592.476030	45.903869	49.903809
588.714969	48.606344	49.908813
584.932536	56.614636	49.913818
581.332751	48.212358	49.918823
578.074795	46.875013	49.923828
574.901991	42.189728	49.928833
570.974984	54.077291	49.933837
567.304669	49.393996	49.938842
564.094035	49.001537	49.943847
560.458484	51.703349	49.948852
557.434250	54.913696	49.953857
553.506721	52.225897	49.958861
550.202139	54.891696	49.963866
546.370844	49.392062	49.968871
543.304965	48.303057	49.973876
539.821181	49.459338	49.978881
536.107451	53.125696	49.983885
532.498178	42.741251	49.988890
529.016384	56.188436	49.993895
525.587892	50.530810	49.998900
522.250537	50.344875	50.003905
518.450506	49.320244	50.008909
515.220206	46.501114	50.013914
511.468099	54.871677	50.018919
507.869570	45.162605	50.023924
504.775294	38.965427	50.028929
501.169070	39.311995	50.033933
497.422406	45.922656	50.038938
493.715038	47.705596	50.043943
490.381485	48.949097	50.048948
487.367756	43.191726	50.053953
483.178205	58.043755	50.058957
479.538053	48.274776	50.063962
476.201681	50.059726	50.068967
473.074556	54.336583	50.073972
469.794711	46.305028	50.078977
465.832999	49.194003	50.083981
462.527230	43.036294	50.088986
458.578410	51.985015	50.093991
455.353987	50.126770	50.098996
452.259254	42.436389	50.104001
448.457475	48.707689	50.109005
445.044357	48.397607	50.114010
441.762190	51.319360	50.119015
438.183030	51.797754	50.124020
434.723344	49.925747	50.129025
430.848816	43.809681	50.134029
427.513034	39.001287	50.139034
423.869912	43.909474	50.144039
420.568479	51.532431	50.149044
416.674585	42.660609	50.154049
413.517117	55.250265	50.159053
410.046273	36.665887	50.164058
406.342053	40.416225	50.169063
402.921124	43.046513	50.174068
399.401166	40.687252	50.179073
395.765351	45.119741	50.184077
392.335846	41.676965	50.189082
388.811008	51.606503	50.194087
385.304911	45.204958	50.199092
382.228476	47.983773	50.204097
378.447688	51.907468	50.209101
375.069460	49.488050	50.214106
371.422449	45.047967	50.219111
367.969259	47.148647	50.224116
364.813895	41.669774	50.229121
360.994528	44.280232	50.234125
357.361897	48.073159	50.239130
354.115265	54.526455	50.244135
350.106032	54.218038	50.249140
346.677254	41.283899	50.254145
343.270471	58.047655	50.259149
339.859451	40.510636	50.264154
336.392711	49.817320	50.269159
332.699252	49.652436	50.274164
329.437689	46.904714	50.279169
325.901903	53.776636	50.284173
322.679372	50.396378	50.289178
318.585274	48.057483	50.294183
315.215846	38.920063	50.299188
311.902483	40.644519	50.304193
308.292927	49.663535	50.309197
304.881985	43.712193	50.314202
301.388349	52.096123	50.319207
297.702637	45.922070	50.324212
294.326375	52.680428	50.329217
290.542133	49.786808	50.334221
287.420816	59.789211	50.339226
283.691224	50.569013	50.344231
280.191182	50.016348	50.349236
276.808646	39.273811	50.354241
273.530105	50.711876	50.359245
270.024674	43.940120	50.364250
266.105967	40.795494	50.369255
262.570758	48.613307	50.374260
259.334861	49.208843	50.379265
255.846711	48.480318	50.384269
252.373990	51.533227	50.389274
249.081562	43.554361	50.394279
245.652449	47.742555	50.399284
242.077874	45.005937	50.404289
238.038587	53.934111	50.409293
234.629788	47.893877	50.414298
231.268161	43.235145	50.419303
227.636723	50.799127	50.424308
224.508627	37.378187	50.429313
220.408412	46.293762	50.434317
217.198207	47.717355	50.439322
213.850050	47.805311	50.444327
210.137070	45.501677	50.449332
207.088990	40.221197	50.454337
203.362459	49.207953	50.459341
199.535278	46.390704	50.464346
196.209953	47.506472	50.469351
193.132882	47.286213	50.474356
189.413628	36.685055	50.479361
185.270738	42.222116	50.484365
182.204079	39.314205	50.489370
178.713738	35.260956	50.494375
174.807449	43.136931	50.499380
171.774505	36.348150	50.504385
168.108738	44.743267	50.509389
164.669149	44.478570	50.514394
161.318086	38.277468	50.519399
157.550075	41.145718	50.524404
154.290049	46.816563	50.529409
150.606075	45.796058	50.534413
146.965245	40.475587	50.539418
143.460335	43.270987	50.544423
140.148391	49.345439	50.549428
137.223656	37.196146	50.554433
133.465334	42.840659	50.559437
129.926701	41.376615	50.564442
125.774745	44.257574	50.569447
122.623286	41.464211	50.574452
119.352135	30.081047	50.579457
115.365606	39.753967	50.584461
112.167489	46.215554	50.589466
108.554213	42.086681	50.594471
105.063284	44.028857	50.599476
101.779701	40.974629	50.604481
98.351043	50.357678	50.609485
94.763829	36.394964	50.614490
90.917847	36.953267	50.619495
87.545304	39.022434	50.624500
84.313417	41.126513	50.629505
80.387752	42.760324	50.634509
77.055443	27.058758	50.639514
73.713487	39.547678	50.644519
69.962409	42.400656	50.649524
66.526309	34.608901	50.654529
62.915028	47.488038	50.659533
59.495864	46.125527	50.664538
56.219231	42.513409	50.669543
52.817816	38.873387	50.674548
49.316551	42.747088	50.679553
45.461198	42.458996	50.684557
42.043240	47.661077	50.689562
38.623838	35.744356	50.694567
34.526862	41.400838	50.699572
31.909040	37.498848	50.704577
27.925638	46.481618	50.709581
24.558290	35.240118	50.714586
21.114955	48.263797	50.719591
17.345349	45.057963	50.724596
13.974813	41.637744	50.729601
10.558840	43.780184	50.734605
7.461673	42.395717	50.739610
3.598711	45.848382	50.744615