Thu Aug 25 11:41:04 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.261512	104.610522	0.000000
1.453785	94.181127	0.005005
1.218101	87.488733	0.010010
0.719232	91.521538	0.015014
1.128739	89.657168	0.020019
0.774644	77.256955	0.025024
0.626199	72.426997	0.030029
0.425454	71.034729	0.035034
-0.102843	59.180677	0.040038
-0.125529	49.746764	0.045043
-0.412267	51.383013	0.050048
-0.388197	40.616174	0.055053
-0.605268	26.217193	0.060058
-0.979257	27.519100	0.065062
-1.452447	12.606606	0.070067
-1.971332	10.384673	0.075072
-2.321217	3.583655	0.080077
-2.282103	-1.449675	0.085082
-2.671817	-3.229941	0.090086
-2.670583	-4.897456	0.095091
-3.429574	-11.096535	0.100096
-3.490749	5.440323	0.105101
-3.908011	0.589229	0.110106
-4.247526	14.012306	0.115110
-4.569769	0.699167	0.120115
-5.206552	3.098932	0.125120
-5.566821	-0.457636	0.130125
-5.148569	-3.905231	0.135130
-5.703090	5.176094	0.140134
-5.576638	5.004384	0.145139
-5.601814	2.262175	0.150144
-5.620020	1.942289	0.155149
-6.339621	0.286476	0.160154
-6.638291	2.282091	0.165158
-6.518487	-2.346269	0.170163
-7.382250	8.017363	0.175168
-8.150048	3.964668	0.180173
-8.069701	2.221482	0.185178
-8.293584	-0.673090	0.190182
-8.115831	0.808120	0.195187
-8.163696	0.246111	0.200192
-8.417570	5.363634	0.205197
-8.627830	5.485125	0.210202
-9.279065	9.870814	0.215206
-9.738597	-3.765658	0.220211
-9.760901	5.501194	0.225216
-10.107863	0.689705	0.230221
-9.690545	-4.118146	0.235226
-10.817118	2.914128	0.240230
-10.792415	4.352880	0.245235
-11.103918	-6.788454	0.250240
-11.174707	0.540300	0.255245
-11.231166	-3.899092	0.260250
-11.553699	14.722492	0.265254
-11.878620	0.160100	0.270259
-12.351122	-6.128160	0.275264
-12.649205	-4.433191	0.280269
-12.587793	-1.563860	0.285274
-12.958074	-5.384610	0.290278
-12.585473	-3.212601	0.295283
-13.768817	-13.163807	0.300288
-14.498672	-6.867568	0.305293
-14.408197	-8.874929	0.310298
-14.470229	4.143998	0.315302
-14.231590	-9.124137	0.320307
-14.521907	6.771587	0.325312
-14.395826	12.035222	0.330317
-15.108086	10.732596	0.335322
-15.948740	10.883258	0.340326
-15.923335	-1.807311	0.345331
-16.040684	2.728841	0.350336
-16.028677	6.033017	0.355341
-16.056910	4.597907	0.360346
-17.211094	-0.115576	0.365350
-17.253475	-0.093155	0.370355
-17.498793	2.479391	0.375360
-17.658217	-6.028240	0.380365
-17.854622	-2.375037	0.385370
-18.015581	1.386507	0.390374
-17.524484	-3.243082	0.395379
-18.264304	0.770510	0.400384
-18.699796	3.790465	0.405389
-18.756116	-8.298840	0.410394
-19.045296	-3.432049	0.415398
-19.717688	0.355844	0.420403
-19.871129	-4.394216	0.425408
-20.244334	-6.082155	0.430413
-20.050545	-1.515662	0.435418
-20.455010	0.724318	0.440422
-20.097333	-4.282995	0.445427
-20.803865	-0.957984	0.450432
-21.147212	2.651805	0.455437
-21.077235	-9.795807	0.460442
-22.150713	-2.964840	0.465446
-22.716773	-0.968458	0.470451
-22.392130	1.492637	0.475456
-22.651826	-4.268986	0.480461
-22.745600	-10.091405	0.485466
-23.108736	-2.394146	0.490470
-23.171338	-6.301069	0.495475
-23.417241	-3.718941	0.500480
-23.533558	1.222005	0.505485
-23.729329	4.476480	0.510490
-24.233919	2.119434	0.515494
-24.325671	-4.538528	0.520499
-24.373680	-5.660494	0.525504
-24.872605	0.542617	0.530509
-25.389170	-5.656481	0.535514
-25.687818	5.229204	0.540518
-25.682683	-3.813571	0.545523
-25.485923	-8.409695	0.550528
-26.420144	-5.577351	0.555533
-27.002788	-4.065584	0.560538
-27.265960	-2.967702	0.565542
-27.244805	-2.993201	0.570547
-27.174185	5.613690	0.575552
-27.344669	11.866582	0.580557
-27.235830	15.032203	0.585562
-27.994922	12.117087	0.590566
-28.006595	-0.944155	0.595571
-28.629941	7.138725	0.600576
-28.579882	3.834239	0.605581
-28.706906	-1.024364	0.610586
-29.157414	7.053581	0.615590
-29.722665	0.953858	0.620595
-29.749100	0.736501	0.625600
-30.180314	6.157055	0.630605
-30.191496	0.881672	0.635610
-30.602745	11.066837	0.640614
-30.990626	0.177912	0.645619
-31.412404	6.511305	0.650624
-31.579103	4.025386	0.655629
-31.609279	-0.468744	0.660634
-31.880460	7.248912	0.665638
-31.882752	-3.618171	0.670643
-31.654938	-0.303517	0.675648
-32.429345	4.462136	0.680653
-32.927582	-2.964197	0.685658
-33.169528	4.986157	0.690662
-33.018880	-2.022995	0.695667
-33.248299	13.164007	0.700672
-33.988814	0.514354	0.705677
-33.903372	2.566843	0.710682
-34.327631	7.888232	0.715686
-34.369985	-1.545732	0.720691
-34.359270	1.666897	0.725696
-35.150191	1.313063	0.730701
-35.379027	-0.913184	0.735706
-36.021797	6.078089	0.740710
-35.731184	-1.601557	0.745715
-36.028107	2.978549	0.750720
-35.999916	3.420180	0.755725
-35.996541	-4.882006	0.760730
-36.810957	-1.638166	0.765734
-36.844367	-7.789580	0.770739
-37.421293	2.450013	0.775744
-37.608277	-2.649128	0.780749
-38.167817	3.079431	0.785754
-38.684462	5.881151	0.790758
-38.287845	0.652601	0.795763
-38.677475	1.846228	0.800768
-38.609988	-1.571718	0.805773
-38.943610	3.608919	0.810778
-39.066106	3.605929	0.815782
-39.154008	-5.498196	0.820787
-39.597847	3.619568	0.825792
-39.761454	3.411049	0.830797
-39.927130	-8.911053	0.835802
-40.958478	2.930984	0.840806
-41.595080	8.744386	0.845811
-41.693352	-1.107920	0.850816
-41.337101	2.218247	0.855821
-41.439263	-0.065813	0.860826
-41.897786	6.997831	0.865830
-41.821015	-2.802808	0.870835
-42.348985	0.642922	0.875840
-42.489998	3.360474	0.880845
-42.797931	5.927013	0.885850
-43.465106	4.367392	0.890854
-43.756403	-1.636050	0.895859
-43.664625	6.977016	0.900864
-43.513842	4.599539	0.905869
-43.445457	4.085754	0.910874
-43.959628	13.727066	0.915878
-44.394102	-7.088659	0.920883
-44.354274	-3.624330	0.925888
-44.984618	3.165681	0.930893
-45.410877	-4.888854	0.935898
-46.329534	0.794735	0.940902
-46.048269	0.766445	0.945907
-46.577848	5.316568	0.950912
-46.429847	-2.192037	0.955917
-45.996198	-3.471729	0.960922
-46.755493	1.013147	0.965926
-46.485077	-3.831798	0.970931
-47.434061	-0.772514	0.975936
-47.561574	5.850126	0.980941
-47.672770	-5.408010	0.985946
-47.908543	5.733575	0.990950
-47.636360	2.590437	0.995955
-48.638323	9.628501	1.000960
-48.892332	-0.484138	1.005965
-48.955087	2.028165	1.010970
-49.446809	-4.763276	1.015974
-49.537330	2.071864	1.020979
-50.236495	15.576601	1.025984
-50.441785	-2.060689	1.030989
-50.564280	2.226333	1.035994
-50.761410	-2.545353	1.040998
-50.434544	3.496730	1.046003
-50.764563	-0.305017	1.051008
-51.223516	9.267531	1.056013
-51.396123	10.186710	1.061018
-52.122358	14.663246	1.066022
-51.953482	4.952575	1.071027
-51.956036	12.144091	1.076032
-52.220999	8.553610	1.081037
-53.063218	5.642032	1.086042
-53.313516	5.437605	1.091046
-53.365686	-1.565076	1.096051
-53.531508	4.497259	1.101056
-54.147311	5.998405	1.106061
-53.866139	-0.708498	1.111066
-54.656316	2.531546	1.116070
-54.908881	1.305591	1.121075
-55.163463	1.551086	1.126080
-55.575329	12.862634	1.131085
-55.131439	4.848923	1.136090
-54.883345	8.169891	1.141094
-55.127673	5.332308	1.146099
-56.022977	9.730931	1.151104
-56.434205	9.722562	1.156109
-56.360187	11.295954	1.161114
-56.658102	14.183625	1.166118
-56.889910	10.470890	1.171123
-57.341914	5.425929	1.176128
-57.837734	-0.608740	1.181133
-58.033346	-3.162892	1.186138
-58.327082	0.353703	1.191142
-58.351697	9.760119	1.196147
-58.516376	6.062177	1.201152
-59.203986	11.061003	1.206157
-59.327592	13.412001	1.211162
-59.560363	6.927992	1.216166
-59.160900	-1.300216	1.221171
-59.304087	2.477525	1.226176
-59.613062	3.120681	1.231181
-60.619174	2.012799	1.236186
-60.735356	1.812668	1.241190
-60.443336	4.177634	1.246195
-60.889282	-0.672124	1.251200
-61.107723	10.368672	1.256205
-61.527076	-0.202108	1.261210
-61.886152	2.945078	1.266214
-62.321654	10.030426	1.271219
-62.109079	9.861039	1.276224
-62.770560	11.375671	1.281229
-63.470903	9.802266	1.286234
-64.012685	15.657760	1.291238
-63.250514	-0.280339	1.296243
-63.815409	6.581675	1.301248
-63.854775	2.731222	1.306253
-63.721346	8.945984	1.311258
-64.170853	15.938617	1.316262
-64.107931	13.293334	1.321267
-65.040010	11.367100	1.326272
-65.012499	13.694420	1.331277
-65.335077	10.242679	1.336282
-65.521225	9.408111	1.341286
-65.700767	2.842998	1.346291
-66.498017	6.859265	1.351296
-66.622168	7.957512	1.356301
-66.677096	3.271110	1.361306
-66.800882	7.061630	1.366310
-66.860428	7.548646	1.371315
-66.980022	9.582641	1.376320
-67.771015	19.479301	1.381325
-68.033417	3.970656	1.386330
-68.137489	8.849574	1.391334
-67.994897	11.484725	1.396339
-68.421480	14.443176	1.401344
-69.127375	10.652867	1.406349
-69.256113	-12.741733	1.411354
-69.626575	5.934800	1.416358
-70.034577	-6.238600	1.421363
-69.811616	-0.794001	1.426368
-69.984203	1.830423	1.431373
-69.737101	4.423887	1.436378
-70.626425	11.431650	1.441382
-70.690954	4.785241	1.446387
-71.173838	6.623062	1.451392
-71.179129	-1.449977	1.456397
-71.009048	-2.916160	1.461402
-72.002716	6.699042	1.466406
-72.288300	-5.620089	1.471411
-72.107872	0.653743	1.476416
-72.448066	3.380359	1.481421
-72.778590	2.055890	1.486426
-73.597000	3.126880	1.491430
-73.610215	0.534657	1.496435
-73.728155	-4.686030	1.501440
-73.840228	3.693220	1.506445
-73.510739	-4.998580	1.511450
-74.525063	9.077548	1.516454
-75.056762	1.457148	1.521459
-75.083825	-0.484341	1.526464
-75.260873	3.482202	1.531469
-75.315130	3.765910	1.536474
-75.501674	6.949337	1.541478
-75.434969	4.749549	1.546483
-76.155102	7.788796	1.551488
-76.541804	8.839597	1.556493
-76.677485	-0.124164	1.561498
-76.586531	9.036354	1.566502
-77.037772	8.547042	1.571507
-77.784175	14.111897	1.576512
-77.892019	7.624134	1.581517
-78.039432	1.604476	1.586522
-78.166597	12.273469	1.591526
-78.102860	2.965250	1.596531
-78.244575	7.141391	1.601536
-78.916357	6.708782	1.606541
-79.429814	8.165419	1.611546
-79.562976	-0.915794	1.616550
-79.288989	-3.483416	1.621555
-79.431425	2.135495	1.626560
-80.060982	-3.852904	1.631565
-80.713819	-11.805490	1.636570
-81.160955	-1.032586	1.641574
-80.765503	-2.075342	1.646579
-80.992100	-6.424797	1.651584
-81.296404	-4.257458	1.656589
-81.191555	-4.612443	1.661594
-82.062464	-0.015164	1.666598
-82.287108	-1.960495	1.671603
-82.287379	-4.254191	1.676608
-82.682306	3.119023	1.681613
-82.336503	-0.497555	1.686618
-83.434711	0.905177	1.691622
-84.167466	1.244580	1.696627
-84.008795	-11.735773	1.701632
-84.250763	-0.833667	1.706637
-83.859202	-11.423934	1.711642
-84.204703	-2.957492	1.716646
-84.192739	-9.090702	1.721651
-84.792654	-7.740740	1.726656
-85.418486	-1.796152	1.731661
-85.724188	-11.568489	1.736666
-85.788345	-3.022746	1.741670
-85.476156	-6.548635	1.746675
-85.745674	-4.889778	1.751680
-86.741991	0.132108	1.756685
-86.919334	-2.665348	1.761690
-87.161272	4.335884	1.766694
-87.040605	-6.926941	1.771699
-86.954919	-3.808318	1.776704
-87.418078	4.407647	1.781709
-88.119796	-0.965174	1.786714
-88.571152	-3.735513	1.791718
-88.563756	-6.077866	1.796723
-88.327124	-10.382846	1.801728
-88.939767	1.485332	1.806733
-88.952761	-9.244024	1.811738
-89.731094	-12.725584	1.816742
-89.934362	-6.954777	1.821747
-90.033625	-2.693542	1.826752
-90.151893	8.154385	1.831757
-89.847497	-2.887296	1.836762
-90.781174	3.020110	1.841766
-91.583135	3.949319	1.846771
-91.561720	-4.627770	1.851776
-91.809277	1.545446	1.856781
-91.396021	-2.230396	1.861786
-91.925436	-2.672657	1.866790
-91.700373	1.294152	1.871795
-91.964459	-0.730418	1.876800
-92.642745	-7.723571	1.881805
-93.016861	1.250388	1.886810
-93.295384	7.687883	1.891814
-93.124454	-8.875729	1.896819
-93.501821	-0.986419	1.901824
-94.300870	7.180940	1.906829
-94.487086	-8.529452	1.911834
-94.595601	0.345942	1.916838
-94.528997	-1.024934	1.921843
-94.621830	3.633924	1.926848
-95.375769	-3.163881	1.931853
-95.548890	-3.165265	1.936858
-96.047324	4.461447	1.941862
-96.021199	-11.611242	1.946867
-96.009638	-1.549285	1.951872
-96.127836	1.471573	1.956877
-95.807227	0.415234	1.961882
-96.716832	5.692451	1.966886
-96.849571	-1.857582	1.971891
-97.125145	1.472671	1.976896
-98.359714	11.669784	1.981901
-98.592840	-1.489626	1.986906
-98.639145	3.744066	1.991910
-98.163011	-2.158160	1.996915
-98.620104	5.205216	2.006912
-98.631270	3.030627	2.016909
-98.025996	-0.263745	2.026906
-97.555498	-6.359485	2.036902
-96.761694	-3.046908	2.046899
-96.183307	-4.458575	2.056896
-96.054955	-1.431363	2.066893
-95.678108	-3.001516	2.076890
-94.807664	0.295885	2.086886
-94.834497	-1.581645	2.096883
-93.796277	2.427559	2.106880
-93.758711	5.953669	2.116877
-93.123681	-5.771650	2.126874
-92.444981	3.042384	2.136870
-92.169665	-6.817769	2.146867
-91.163102	-4.640915	2.156864
-90.837598	0.173710	2.166861
-90.518755	1.723401	2.176858
-89.566570	4.368105	2.186854
-89.608599	1.951265	2.196851
-89.292101	-8.178265	2.206848
-88.171080	-2.648832	2.216845
-87.885679	0.724402	2.226842
-87.859916	-2.963834	2.236838
-86.887504	-3.502747	2.246835
-86.634542	-4.705033	2.256832
-85.648590	3.649048	2.266829
-85.357890	0.926651	2.276826
-85.181981	-4.134585	2.286822
-84.555360	0.908454	2.296819
-83.874982	-5.128307	2.306816
-83.524868	0.258996	2.316813
-82.721848	-2.220563	2.326810
-82.738618	-5.927476	2.336806
-81.816143	-2.863139	2.346803
-81.243734	-2.072264	2.356800
-81.181594	-1.239448	2.366797
-80.391125	-0.536593	2.376794
-79.589814	-3.959882	2.386790
-79.521184	-4.439542	2.396787
-79.125826	3.161284	2.406784
-78.587558	-3.740188	2.416781
-78.059192	-7.637055	2.426778
-77.244839	-2.661446	2.436774
-76.733738	-1.132376	2.446771
-76.620771	-2.734040	2.456768
-75.775860	-4.599279	2.466765
-75.599166	-2.862589	2.476762
-75.042371	-2.595118	2.486758
-74.144881	2.779277	2.496755
-74.027923	4.008980	2.506752
-73.571858	-1.251375	2.516749
-72.985357	1.482307	2.526746
-72.478338	-0.361665	2.536742
-71.614740	-2.850716	2.546739
-71.512627	0.671615	2.556736
-71.034718	3.859466	2.566733
-70.099069	-1.754799	2.576730
-70.304685	2.002649	2.586726
-69.196567	-1.649276	2.596723
-68.673456	7.049761	2.606720
-68.458466	6.167034	2.616717
-68.212797	1.297604	2.626714
-67.524695	-3.587297	2.636710
-66.777756	-4.977856	2.646707
-65.863606	4.188927	2.656704
-66.111115	2.029196	2.666701
-65.359221	1.550180	2.676698
-64.981747	0.559631	2.686694
-64.582997	2.616319	2.696691
-63.785529	-3.689044	2.706688
-63.088054	-2.027619	2.716685
-62.787414	5.302952	2.726682
-62.789597	1.641267	2.736678
-61.698535	3.076298	2.746675
-61.614831	4.678673	2.756672
-60.939969	4.487324	2.766669
-60.146028	-2.226129	2.776666
-59.973505	-1.968138	2.786662
-59.531499	3.617012	2.796659
-58.950634	7.434960	2.806656
-58.579127	7.592082	2.816653
-57.503441	3.542931	2.826650
-57.514888	2.993456	2.836646
-56.914981	4.597311	2.846643
-55.859838	3.329520	2.856640
-55.886831	-0.378961	2.866637
-55.775815	1.196960	2.876634
-55.006603	-3.006906	2.886630
-54.440185	-7.305708	2.896627
-53.629360	0.863577	2.906624
-52.758244	2.244374	2.916621
-52.618304	1.424092	2.926618
-52.571807	0.700813	2.936614
-52.124213	-4.428335	2.946611
-51.350544	-1.673294	2.956608
-51.020961	-3.058645	2.966605
-49.975743	-5.924607	2.976602
-49.771941	-1.407688	2.986598
-49.811126	-1.502993	2.996595
-49.094821	-3.142173	3.006592
-48.655389	-9.806412	3.016589
-47.331892	-7.001308	3.026586
-46.801383	-6.016966	3.036582
-46.978888	-10.253056	3.046579
-46.734164	-2.153459	3.056576
-45.957907	-3.567617	3.066573
-45.329404	-8.984867	3.076570
-44.516405	-9.258047	3.086566
-44.219457	-7.008012	3.096563
-44.133401	-0.030288	3.106560
-43.609322	-0.834733	3.116557
-42.716671	-8.390441	3.126554
-42.419575	-11.246884	3.136550
-41.713908	-1.832025	3.146547
-41.166725	-1.407824	3.156544
-41.132440	-4.679250	3.166541
-40.130848	-8.605916	3.176538
-39.695449	-8.553837	3.186534
-39.538863	-6.250131	3.196531
-38.474697	-6.312411	3.206528
-38.458155	-4.927592	3.216525
-38.029279	-0.921105	3.226522
-37.054274	-1.954592	3.236518
-36.934947	2.182760	3.246515
-36.301961	-0.149779	3.256512
-35.583090	1.422766	3.266509
-35.258226	5.999913	3.276506
-35.139863	2.541085	3.286502
-34.047239	-1.932032	3.296499
-34.056159	-7.429971	3.306496
-33.067843	-6.035858	3.316493
-32.574502	-9.962082	3.326490
-32.314346	-5.175228	3.336486
-32.157994	2.105093	3.346483
-31.056871	0.475310	3.356480
-30.759900	-8.947917	3.366477
-30.270502	0.269584	3.376474
-29.315268	-1.505233	3.386470
-29.094671	0.512848	3.396467
-29.066961	0.654148	3.406464
-28.889589	-3.374622	3.416461
-28.207655	-3.345332	3.426458
-27.292486	-3.225875	3.436454
-26.805572	-0.799699	3.446451
-26.248882	-7.418956	3.456448
-25.757408	-3.187861	3.466445
-25.461877	-3.503503	3.476442
-24.351092	-0.722085	3.486438
-24.013273	-2.317799	3.496435
-23.789715	2.354416	3.506432
-23.737836	1.801354	3.516429
-22.847215	-4.290523	3.526426
-22.305358	0.151255	3.536422
-21.431247	5.465968	3.546419
-21.406284	0.612111	3.556416
-20.941862	2.658512	3.566413
-19.864075	4.577131	3.576410
-19.409261	4.971457	3.586406
-19.484182	4.606154	3.596403
-19.079323	-0.437104	3.606400
-18.099163	-1.737491	3.616397
-18.153428	6.903133	3.626394
-17.202743	2.252687	3.636390
-16.599387	6.529610	3.646387
-16.392700	5.990306	3.656384
-15.531698	4.388643	3.666381
-15.159086	-2.844833	3.676378
-15.020918	-2.312195	3.686374
-14.272037	-3.424291	3.696371
-13.915972	9.273322	3.706368
-13.332106	-1.303584	3.716365
-12.276559	0.428453	3.726362
-12.131326	0.966319	3.736358
-12.184166	-3.096073	3.746355
-11.193109	0.755809	3.756352
-11.018548	-3.826882	3.766349
-9.848837	-7.697524	3.776346
-9.773676	-6.841405	3.786342
-9.365907	-6.636110	3.796339
-9.189599	0.599905	3.806336
-8.189884	-2.125877	3.816333
-7.663306	-2.053237	3.826330
-6.599050	1.061756	3.836326
-6.388158	-1.334526	3.846323
-6.481017	2.151833	3.856320
-6.299219	6.551829	3.866317
-5.376181	4.956286	3.876314
-4.869390	5.538872	3.886310
-4.370586	6.784774	3.896307
-3.924428	8.719999	3.906304
-3.523509	19.544770	3.916301
-3.019387	30.293190	3.926298
-2.672431	39.194081	3.936294
-2.432562	53.481155	3.946291
-1.802729	63.360931	3.956288
-1.525119	83.436005	3.966285
-0.549393	104.786046	3.976282
0.000000	114.104830	3.981286
-0.270229	125.283529	3.986291
-0.217161	124.316560	3.991296
0.426847	143.429081	3.996301
0.386983	150.813164	4.001306
0.462037	147.580665	4.006310
0.545523	147.159422	4.011315
0.453532	147.050411	4.016320
0.595504	148.891580	4.021325
0.726981	160.387011	4.026330
0.886240	148.399862	4.031334
0.641770	150.405983	4.036339
0.748369	149.205999	4.041344
0.837064	147.458327	4.046349
0.549864	147.557072	4.051354
0.546520	153.654113	4.056358
1.224318	152.244410	4.061363
0.621366	140.623463	4.066368
0.531792	135.252753	4.071373
0.469419	139.214015	4.076378
0.789659	143.289335	4.081382
0.545723	148.610986	4.086387
0.803283	147.156396	4.091392
1.056914	142.117888	4.096397
0.989885	139.350577	4.101402
0.636300	141.221934	4.106406
0.807694	147.952819	4.111411
0.674936	145.860195	4.116416
0.729533	147.610650	4.121421
0.967832	150.139079	4.126426
0.647069	151.597170	4.131430
0.864718	162.810182	4.136435
0.881753	161.193960	4.141440
1.029514	155.093195	4.146445
0.908029	159.326315	4.151450
0.631384	163.552108	4.156454
0.825595	160.471780	4.161459
0.741063	161.484733	4.166464
1.273355	158.829161	4.171469
1.025393	166.748893	4.176474
1.060304	157.505216	4.181478
1.106320	155.457346	4.186483
0.881814	165.442498	4.191488
1.234610	155.095484	4.196493
1.094210	163.045817	4.201498
1.106043	154.081004	4.206502
1.235552	155.933618	4.211507
0.907028	164.251949	4.216512
1.405886	158.849147	4.221517
1.036376	165.193389	4.226522
1.181998	154.388454	4.231526
0.955577	160.074360	4.236531
1.029425	156.794591	4.241536
1.342248	163.623546	4.246541
0.964418	169.605261	4.251546
1.005453	169.393150	4.256550
1.178512	163.383332	4.261555
1.374195	166.880223	4.266560
1.279227	157.217133	4.271565
0.968853	166.127408	4.276570
1.166172	162.394858	4.281574
1.105975	164.460694	4.286579
1.074865	157.438827	4.291584
1.089852	170.290786	4.296589
1.191203	164.510502	4.301594
0.879318	165.644500	4.306598
0.875639	166.638458	4.311603
0.808206	172.055848	4.316608
0.956947	158.969351	4.321613
0.716842	174.914306	4.326618
1.015154	179.002562	4.331622
1.266289	185.588090	4.336627
1.252787	192.433383	4.341632
1.281845	187.088363	4.346637
0.966154	182.037806	4.351642
1.173147	190.288063	4.356646
1.410448	193.851205	4.361651
1.176925	187.863954	4.366656
1.514571	197.229533	4.371661
1.385010	197.939495	4.376666
1.898915	196.558631	4.381670
1.547636	191.782567	4.386675
1.340517	184.636407	4.391680
1.572148	187.884061	4.396685
1.313835	187.522698	4.401690
1.402594	181.583030	4.406694
1.532513	192.775005	4.411699
1.550891	201.412324	4.416704
1.500646	194.054919	4.421709
1.461828	207.367752	4.426714
1.344014	206.718620	4.431718
1.579302	211.740577	4.436723
1.468761	203.709241	4.441728
1.607412	209.306325	4.446733
1.812181	214.627295	4.451738
1.853137	212.757382	4.456742
2.068714	212.717240	4.461747
1.719276	215.059355	4.466752
1.604965	207.617069	4.471757
1.639866	208.873905	4.476762
2.209676	204.867848	4.481766
1.901901	207.614724	4.486771
1.659070	188.480329	4.491776
1.769485	181.683052	4.496781
1.569605	194.277628	4.501786
1.802198	210.037819	4.506790
2.099621	207.994845	4.511795
1.700973	203.529921	4.516800
1.588732	200.715901	4.521805
1.613838	213.971267	4.526810
2.288540	208.601011	4.531814
2.202691	204.972930	4.536819
1.730078	203.325855	4.541824
1.731079	190.683264	4.546829
1.662936	201.048898	4.551834
2.082967	212.363110	4.556838
2.016632	213.018874	4.561843
1.531389	211.823031	4.566848
1.897096	209.554222	4.571853
1.757087	207.845541	4.576858
1.522541	210.853028	4.581862
2.008470	212.172075	4.586867
1.912002	217.913568	4.591872
1.817925	212.350551	4.596877
2.116348	218.466772	4.601882
1.822554	208.009064	4.606886
1.755774	211.265513	4.611891
1.910521	216.537373	4.616896
2.193858	208.447485	4.621901
2.137136	214.685789	4.626906
2.063447	220.104174	4.631910
2.022209	214.086786	4.636915
1.949200	222.529625	4.641920
2.031304	213.325981	4.646925
1.724914	226.990802	4.651930
2.338132	228.350018	4.656934
2.335500	238.050509	4.661939
2.184249	240.646315	4.666944
2.486390	229.487778	4.671949
2.121564	237.688444	4.676954
2.128138	218.283985	4.681958
2.405444	226.640301	4.686963
1.991627	228.451501	4.691968
2.415428	238.430029	4.696973
2.420846	245.718470	4.701978
2.632753	227.996593	4.706982
2.308906	217.116479	4.711987
1.804228	214.474676	4.716992
2.194361	225.806237	4.721997
2.256622	236.505802	4.727002
2.547641	232.299809	4.732006
2.374936	237.167399	4.737011
2.794256	235.149615	4.742016
2.365946	214.936934	4.747021
2.047315	223.889660	4.752026
2.111641	229.280095	4.757030
2.209845	234.608277	4.762035
2.422508	234.087698	4.767040
2.607206	225.763320	4.772045
2.848626	233.710808	4.777050
2.654791	230.577372	4.782054
2.391466	235.854630	4.787059
2.583699	240.370811	4.792064
2.817466	233.253629	4.797069
2.478924	234.546832	4.802074
2.503192	232.473887	4.807078
2.385648	233.741955	4.812083
2.201326	240.563411	4.817088
2.633425	234.158640	4.822093
2.746550	240.977784	4.827098
2.787236	238.256857	4.832102
2.553128	242.203920	4.837107
2.750285	236.550971	4.842112
2.629516	241.062409	4.847117
2.435380	228.263704	4.852122
2.762427	236.162975	4.857126
2.356846	236.580827	4.862131
2.286033	241.913346	4.867136
2.391741	236.831549	4.872141
2.837376	244.421177	4.877146
2.962604	232.379192	4.882150
2.797807	233.192753	4.887155
2.770603	239.103736	4.892160
2.979509	240.538956	4.897165
2.239985	239.199453	4.902170
2.392499	237.818262	4.907174
2.270678	232.563307	4.912179
2.512599	238.973128	4.917184
2.956706	240.422116	4.922189
2.855377	255.991058	4.927194
3.099601	259.293699	4.932198
2.704810	247.646395	4.937203
2.407565	251.467310	4.942208
2.703963	251.155075	4.947213
2.711945	264.758013	4.952218
3.065314	258.191562	4.957222
2.869841	261.540950	4.962227
2.873091	262.900826	4.967232
3.305223	251.085990	4.972237
3.118475	264.789042	4.977242
3.016764	257.597863	4.982246
3.213114	259.228042	4.987251
2.609279	261.230369	4.992256
2.753848	254.032242	4.997261
2.612316	267.772504	5.002266
3.067376	261.860838	5.007270
2.969276	254.289442	5.012275
3.033991	265.213267	5.017280
2.935067	260.894358	5.022285
2.851495	260.413865	5.027290
3.145032	259.301644	5.032294
3.073146	262.074844	5.037299
3.261852	261.349209	5.042304
2.995216	258.701740	5.047309
3.131392	265.722928	5.052314
2.949778	265.950664	5.057318
2.500589	260.974785	5.062323
3.384619	273.687491	5.067328
3.712300	270.804532	5.072333
3.113402	280.683893	5.077338
3.547176	261.095393	5.082342
3.404018	273.168605	5.087347
3.048641	257.974853	5.092352
3.552700	256.620838	5.097357
3.334398	267.664939	5.102362
3.442658	266.461523	5.107366
3.582351	262.171666	5.112371
2.896636	262.927640	5.117376
3.601008	253.835287	5.122381
3.214724	257.144968	5.127386
3.781832	260.156573	5.132390
3.534959	256.373377	5.137395
3.613886	266.678041	5.142400
3.488455	255.273267	5.147405
3.239955	268.755042	5.152410
2.987430	263.121921	5.157414
3.104943	259.882749	5.162419
2.944102	277.166308	5.167424
3.390149	259.445679	5.172429
3.522933	260.418262	5.177434
3.418779	260.355448	5.182438
3.495990	253.560183	5.187443
3.044479	266.165761	5.192448
3.829537	273.645272	5.197453
3.534177	275.618252	5.202458
3.702733	279.904033	5.207462
3.475791	280.316042	5.212467
3.625707	278.678989	5.217472
3.641927	274.737507	5.222477
3.726485	264.261614	5.227482
3.483000	269.314310	5.232486
3.398351	267.457744	5.237491
3.324022	281.105229	5.242496
3.855330	282.037518	5.247501
3.340355	297.307471	5.252506
3.736742	282.343926	5.257510
3.812547	293.224902	5.262515
3.656460	294.688840	5.267520
4.052063	287.391255	5.272525
3.987703	284.949373	5.277530
3.882436	283.156147	5.282534
3.788242	274.723582	5.287539
3.493482	275.924506	5.292544
3.796055	276.740772	5.297549
3.823980	283.608084	5.302554
3.712174	289.760131	5.307558
3.836900	288.990735	5.312563
3.873726	284.046269	5.317568
3.883059	285.215367	5.322573
3.495106	292.824891	5.327578
3.826972	280.823263	5.332582
3.980090	287.968357	5.337587
3.669826	294.189465	5.342592
4.128126	283.512633	5.347597
4.088704	288.302405	5.352602
4.126420	289.489203	5.357606
3.800522	289.122608	5.362611
3.748988	293.218248	5.367616
4.271332	284.704897	5.372621
4.075902	299.301521	5.377626
4.062057	284.054235	5.382630
3.750997	285.558272	5.387635
3.967659	290.839436	5.392640
4.352456	281.949002	5.397645
3.742319	283.287926	5.402650
4.178365	282.257779	5.407654
4.336916	272.975687	5.412659
3.833711	277.641969	5.417664
4.376209	277.904947	5.422669
3.891665	282.144360	5.427674
4.042808	283.506375	5.432678
3.801617	281.724955	5.437683
4.072463	287.073559	5.442688
4.397643	286.199989	5.447693
4.037514	297.082831	5.452698
3.973281	288.506359	5.457702
3.740786	295.746675	5.462707
3.541877	294.205404	5.467712
3.813992	280.438258	5.472717
3.877494	285.983865	5.477722
3.951880	293.071693	5.482726
3.983714	298.644412	5.487731
3.872582	321.200576	5.492736
4.625538	307.769362	5.497741
4.656194	311.848965	5.502746
4.557409	306.609362	5.507750
4.433991	294.919506	5.512755
4.069508	293.764849	5.517760
4.326622	297.704562	5.522765
4.517936	305.773829	5.527770
4.712104	294.233533	5.532774
4.313237	291.372657	5.537779
3.890500	298.503576	5.542784
4.204135	293.237323	5.547789
4.271321	314.085572	5.552794
4.396125	301.825305	5.557798
4.616839	310.231657	5.562803
4.393790	314.192821	5.567808
4.627499	310.296350	5.572813
4.188157	307.220349	5.577818
4.384466	315.779225	5.582822
4.563315	316.697136	5.587827
4.303675	314.383924	5.592832
4.549659	309.893902	5.597837
4.320604	316.668611	5.602842
4.461041	321.907943	5.607846
4.702538	320.294503	5.612851
4.163108	314.532310	5.617856
4.530796	318.793228	5.622861
4.393391	313.904526	5.627866
4.533771	314.122941	5.632870
4.574984	319.010820	5.637875
4.167503	316.803029	5.642880
4.291265	311.439970	5.647885
4.614579	322.320149	5.652890
5.196310	344.002147	5.657894
5.270402	330.933548	5.662899
4.691716	330.533793	5.667904
4.638731	324.163864	5.672909
4.438023	322.474174	5.677914
4.659491	326.058807	5.682918
5.156724	330.236155	5.687923
4.673864	325.540782	5.692928
4.782282	313.438100	5.697933
4.641688	314.712949	5.702938
4.652753	313.809500	5.707942
4.496659	320.098211	5.712947
4.395612	339.058758	5.717952
4.897067	340.460805	5.722957
4.730604	340.110358	5.727962
5.163402	349.325066	5.732966
5.097293	342.039688	5.737971
5.048813	339.706043	5.742976
4.861769	326.621414	5.747981
4.676316	334.202392	5.752986
4.964420	336.691407	5.757990
5.276914	334.886505	5.762995
4.884740	334.463854	5.768000
4.962201	323.852996	5.773005
4.945392	323.732204	5.778010
4.983606	325.099262	5.783014
5.295763	328.353307	5.788019
4.893468	330.956822	5.793024
4.846315	315.917209	5.798029
4.690770	330.305128	5.803034
4.997940	336.258666	5.808038
4.820655	338.839582	5.813043
5.126488	339.449694	5.818048
5.375565	333.693666	5.823053
5.531001	342.727199	5.828058
5.168737	333.387471	5.833062
4.960075	331.028304	5.838067
5.177459	344.813632	5.843072
5.650759	332.055811	5.848077
5.012332	315.001758	5.853082
4.902450	314.417818	5.858086
5.207312	323.813911	5.863091
5.231510	342.947830	5.868096
5.364052	324.516948	5.873101
5.350259	328.628829	5.878106
5.115585	322.366463	5.883110
5.072495	313.742373	5.888115
4.830194	328.188175	5.893120
5.308757	330.460685	5.898125
5.526507	334.317988	5.903130
5.307969	330.001984	5.908134
5.733439	336.658331	5.913139
5.378633	332.183341	5.918144
5.358521	313.751078	5.923149
4.997418	312.032735	5.928154
5.294090	320.806845	5.933158
5.457266	325.802167	5.938163
4.859852	328.743140	5.943168
5.353141	338.138192	5.948173
5.018211	337.864761	5.953178
5.175634	331.803552	5.958182
5.318868	331.983555	5.963187
4.601139	342.644040	5.968192
5.042277	338.705571	5.973197
5.381585	355.777962	5.978202
5.601976	354.781601	5.983206
5.787471	351.500123	5.988211
5.474889	351.871768	5.993216
5.317081	344.477368	5.998221
5.371519	361.198925	6.003226
5.658973	350.017305	6.008230
5.623131	360.906324	6.013235
5.222178	355.369197	6.018240
5.623283	352.152014	6.023245
5.484335	359.972492	6.028250
5.711175	358.054456	6.033254
5.427315	352.847001	6.038259
5.495601	348.397467	6.043264
5.359759	334.713181	6.048269
5.038320	348.522823	6.053274
5.543047	365.199142	6.058278
5.627522	364.942256	6.063283
5.402174	368.365949	6.068288
5.766824	353.897705	6.073293
5.503906	365.730313	6.078298
5.242812	364.505667	6.083302
5.660835	360.387315	6.088307
5.300375	363.158288	6.093312
5.920384	361.653219	6.098317
5.697019	347.207508	6.103322
5.378395	342.979949	6.108326
5.392846	335.732572	6.113331
5.102617	343.263531	6.118336
4.991406	345.552518	6.123341
5.410131	363.877990	6.128346
5.300635	365.087858	6.133350
5.660232	348.747445	6.138355
5.824558	362.458841	6.143360
5.614004	358.752191	6.148365
5.914143	352.358562	6.153370
5.310276	353.766112	6.158374
5.805341	348.702373	6.163379
5.370969	336.320885	6.168384
5.437272	331.023770	6.173389
5.160062	351.229990	6.178394
5.776844	351.686977	6.183398
5.526074	347.350709	6.188403
5.671740	342.987129	6.193408
5.427704	337.909482	6.198413
5.204775	339.061190	6.203418
5.488670	352.000862	6.208422
5.533907	347.877645	6.213427
5.376100	355.773843	6.218432
5.818273	352.657795	6.223437
5.276442	345.272944	6.228442
5.483964	349.267895	6.233446
5.854838	349.301499	6.238451
5.319507	343.782266	6.243456
5.717246	333.181332	6.248461
5.340267	337.868981	6.253466
5.516684	340.660237	6.258470
5.303068	344.464905	6.263475
5.423384	330.917659	6.268480
5.657210	327.432458	6.273485
5.204960	327.066677	6.278490
5.370907	337.965195	6.283494
5.677222	345.418506	6.288499
5.642327	333.559730	6.293504
5.533586	328.767774	6.298509
5.171550	332.551401	6.303514
5.336495	333.047544	6.308518
5.457695	340.722848	6.313523
5.461487	348.267853	6.318528
5.593250	351.714684	6.323533
5.558202	362.404261	6.328538
5.408267	353.059729	6.333542
5.631588	338.930020	6.338547
5.429779	343.397233	6.343552
5.805511	334.248762	6.348557
5.511757	343.055279	6.353562
5.372386	327.232831	6.358566
5.553969	320.225032	6.363571
5.148706	333.895934	6.368576
5.690760	339.974025	6.373581
5.277363	344.354167	6.378586
5.291370	341.950619	6.383590
5.463186	352.231287	6.388595
5.611020	358.396461	6.393600
5.910839	349.541454	6.398605
5.858466	339.058498	6.403610
5.399193	328.357724	6.408614
5.122397	331.375014	6.413619
5.362534	330.559060	6.418624
5.506088	333.627550	6.423629
5.175318	337.653054	6.428634
5.961950	336.871698	6.433638
6.044406	332.100405	6.438643
5.529087	337.031194	6.443648
5.400884	324.323330	6.448653
5.411793	331.965290	6.453658
5.783905	331.875311	6.458662
5.752792	330.310910	6.463667
5.314713	328.123731	6.468672
5.658457	325.203445	6.473677
5.267941	333.120276	6.478682
5.443839	332.883868	6.483686
5.478495	321.798822	6.488691
5.017304	327.018523	6.493696
5.626764	330.890382	6.498701
5.772900	337.884728	6.503706
5.400087	340.765201	6.508710
5.403666	332.269833	6.513715
5.527764	335.860233	6.518720
5.602352	328.536997	6.523725
5.749250	334.863663	6.528730
5.507774	332.044560	6.533734
5.497418	329.923244	6.538739
5.409631	331.025304	6.543744
5.439108	333.292246	6.548749
5.192178	343.733432	6.553754
5.098499	338.227262	6.558758
5.602757	334.560481	6.563763
5.213646	340.841416	6.568768
5.374040	342.954969	6.573773
5.554412	334.305348	6.578778
5.416112	339.974340	6.583782
5.799588	332.982360	6.588787
5.436569	342.046505	6.593792
5.609301	333.812537	6.598797
5.499948	335.164751	6.603802
5.397446	337.037917	6.608806
5.588597	334.847062	6.613811
5.376532	342.182274	6.618816
5.737271	340.455235	6.623821
5.818032	338.753080	6.628826
5.466122	340.997522	6.633830
6.021978	334.339204	6.638835
5.616230	339.781179	6.643840
5.962529	343.729075	6.648845
5.740318	347.614185	6.653850
5.606688	340.200180	6.658854
5.466357	327.579636	6.663859
4.977759	325.590200	6.668864
5.540607	338.416553	6.673869
5.439771	338.881572	6.678874
5.242085	338.630931	6.683878
5.666335	331.578778	6.688883
5.822452	337.005485	6.693888
5.540836	334.689386	6.698893
5.484508	330.620052	6.703898
5.361275	334.173273	6.708902
5.475649	333.791479	6.713907
5.595113	341.517676	6.718912
5.743439	331.300675	6.723917
5.344599	324.317376	6.728922
5.559006	330.582843	6.733926
5.293631	327.330883	6.738931
5.378528	334.894812	6.743936
5.609588	324.642705	6.748941
5.596046	332.101833	6.753946
5.362803	323.618264	6.758950
5.751441	330.362638	6.763955
5.464997	319.524058	6.768960
5.220486	310.583512	6.773965
5.200032	323.311419	6.778970
5.399597	332.205153	6.783974
5.352427	335.487026	6.788979
5.500189	336.128232	6.793984
5.437474	331.892218	6.798989
5.452861	341.915813	6.803994
5.174667	329.013144	6.808998
5.530897	323.898398	6.814003
5.005912	337.363433	6.819008
5.175401	341.924332	6.824013
5.389078	346.440344	6.829018
5.448050	342.545933	6.834022
5.302049	331.856186	6.839027
5.360057	332.134964	6.844032
5.335700	329.142637	6.849037
5.349645	339.375266	6.854042
5.241745	335.146330	6.859046
5.586495	335.348544	6.864051
5.441696	344.818265	6.869056
5.601700	335.947205	6.874061
5.425892	333.968872	6.879066
5.330964	335.128999	6.884070
5.421441	337.199721	6.889075
5.487374	349.325647	6.894080
5.432670	353.557840	6.899085
5.641351	358.656775	6.904090
5.652567	356.487782	6.909094
5.515985	339.899249	6.914099
5.056693	339.502933	6.919104
5.655845	334.688648	6.924109
5.190798	350.615219	6.929114
5.473968	349.071178	6.934118
5.570818	347.806268	6.939123
5.526584	353.020760	6.944128
5.734560	350.653258	6.949133
5.470540	348.970322	6.954138
5.259307	341.166675	6.959142
5.466269	345.212334	6.964147
5.788120	354.102738	6.969152
6.009890	342.542267	6.974157
5.445293	335.774762	6.979162
5.075883	330.140952	6.984166
5.525390	328.074135	6.989171
5.214735	336.889625	6.994176
5.702264	331.605607	6.999181
5.460365	347.063773	7.004186
5.255822	339.246423	7.009190
5.476835	355.293299	7.014195
5.713457	361.080727	7.019200
5.761556	349.202610	7.024205
5.340853	350.869366	7.029210
5.323182	340.706842	7.034214
5.371641	338.588965	7.039219
5.376656	345.934458	7.044224
5.493529	352.212051	7.049229
5.524130	354.798363	7.054234
5.515717	352.319231	7.059238
5.634852	341.989737	7.064243
5.432773	344.429005	7.069248
5.309001	335.479020	7.074253
5.429405	348.061487	7.079258
5.778508	351.319239	7.084262
5.859875	348.512826	7.089267
5.421615	349.147774	7.094272
5.437792	338.018156	7.099277
5.370645	332.915958	7.104282
5.384041	341.253566	7.109286
5.520761	335.961236	7.114291
5.213356	343.624601	7.119296
5.426668	338.177899	7.124301
5.612450	351.537908	7.129306
5.448283	349.912094	7.134310
5.659885	340.612164	7.139315
5.645929	341.949431	7.144320
5.616064	336.819245	7.149325
5.500402	339.453781	7.154330
5.560989	339.279734	7.159334
5.630479	329.106724	7.164339
5.434161	344.405884	7.169344
5.465560	340.262691	7.174349
5.375382	339.302336	7.179354
5.166175	337.392511	7.184358
5.828096	325.421399	7.189363
5.264439	337.949685	7.194368
5.389631	333.041980	7.199373
5.308510	338.243264	7.204378
5.280171	340.756551	7.209382
5.746270	340.474674	7.214387
5.626072	339.455746	7.219392
5.492347	335.224530	7.224397
5.256430	342.996918	7.229402
5.146119	338.458308	7.234406
6.006290	346.837253	7.239411
5.703846	345.967104	7.244416
5.543076	330.059420	7.249421
5.502984	336.080023	7.254426
5.495979	336.773952	7.259430
5.681109	327.592072	7.264435
5.355268	332.132501	7.269440
5.333834	327.570477	7.274445
5.771757	329.532976	7.279450
5.303643	336.512830	7.284454
5.491451	338.872026	7.289459
5.294553	328.810357	7.294464
5.456166	323.460346	7.299469
5.210664	332.221332	7.304474
5.476051	335.659879	7.309478
5.764279	331.485939	7.314483
5.508928	341.336816	7.319488
5.581897	334.365012	7.324493
5.275217	333.947948	7.329498
5.352144	337.453989	7.334502
5.680346	329.793620	7.339507
5.144890	341.207001	7.344512
5.398041	335.750894	7.349517
5.405475	343.285835	7.354522
5.816024	352.193979	7.359526
5.600190	339.474524	7.364531
5.340187	344.836716	7.369536
5.663529	340.907212	7.374541
5.599682	337.867286	7.379546
5.675175	333.546341	7.384550
5.794787	331.993126	7.389555
5.445142	339.653616	7.394560
5.614694	324.947041	7.399565
5.601031	331.899983	7.404570
5.629230	336.081217	7.409574
5.829804	325.526999	7.414579
5.664871	332.168280	7.419584
5.678311	333.251315	7.424589
5.658264	333.403116	7.429594
5.533416	338.367640	7.434598
5.880814	333.700369	7.439603
5.497371	341.157345	7.444608
5.319224	329.526663	7.449613
5.252071	333.634251	7.454618
5.621260	332.117862	7.459622
5.788013	328.143292	7.464627
5.230207	328.967814	7.469632
5.628014	331.812967	7.474637
5.571937	336.330112	7.479642
5.561758	328.830331	7.484646
5.535486	312.237194	7.489651
5.270200	309.342731	7.494656
5.304605	310.416152	7.499661
5.502874	323.612831	7.504666
5.598405	327.337420	7.509670
5.753830	328.268494	7.514675
5.107142	319.394120	7.519680
5.375979	326.198392	7.524685
5.920679	336.502886	7.529690
5.213200	318.959770	7.534694
5.789352	314.054181	7.539699
5.147982	319.355895	7.544704
5.539303	324.584393	7.549709
5.378722	333.107445	7.554714
5.475305	332.484827	7.559718
5.570468	333.523420	7.564723
5.679061	344.918152	7.569728
5.299841	323.720044	7.574733
5.547625	324.506931	7.579738
5.459245	332.142302	7.584742
5.402285	318.856961	7.589747
5.334631	335.192659	7.594752
5.569100	334.700299	7.599757
5.678423	344.740815	7.604762
4.821156	331.410013	7.609766
5.418129	330.952606	7.614771
5.511023	342.947751	7.619776
5.473508	329.697321	7.624781
5.534584	332.930595	7.629786
5.335161	330.699696	7.634790
5.464238	333.957117	7.639795
5.606823	330.729823	7.644800
5.659059	332.287675	7.649805
5.516122	332.686524	7.654810
5.612886	342.501214	7.659814
5.685906	335.640134	7.664819
5.493525	333.442932	7.669824
5.194663	326.801476	7.674829
5.336908	333.663550	7.679834
5.153663	337.042674	7.684838
5.423418	339.442815	7.689843
5.322230	331.201147	7.694848
5.377038	324.940880	7.699853
5.494914	325.147002	7.704858
5.477621	331.768314	7.709862
5.289225	340.849391	7.714867
5.257786	337.370948	7.719872
5.801765	332.328025	7.724877
5.559543	328.540920	7.729882
5.552036	335.372675	7.734886
5.678824	328.129846	7.739891
5.480874	340.062991	7.744896
5.741215	335.200550	7.749901
5.243672	335.057003	7.754906
5.428696	340.096363	7.759910
5.501072	332.064784	7.764915
5.138292	333.165637	7.769920
5.518282	335.924996	7.774925
5.855956	336.378257	7.779930
5.321143	334.206234	7.784934
5.507881	337.634958	7.789939
5.418962	339.183289	7.794944
5.592809	340.162097	7.799949
5.310165	342.041342	7.804954
5.557009	331.448232	7.809958
5.364702	325.251994	7.814963
5.168451	334.217238	7.819968
5.637623	323.405799	7.824973
5.488674	328.557596	7.829978
5.236252	332.124730	7.834982
5.611170	326.956434	7.839987
5.551488	331.091325	7.844992
5.509116	325.523335	7.849997
5.600958	330.317862	7.855002
5.268840	330.622964	7.860006
5.393821	332.767374	7.865011
5.340376	336.192600	7.870016
5.607062	332.221354	7.875021
5.243397	342.791562	7.880026
5.108450	342.075505	7.885030
5.145163	332.866257	7.890035
5.195403	342.583831	7.895040
5.362925	357.816505	7.900045
5.452189	358.356145	7.905050
5.672557	365.319888	7.910054
5.619966	357.304713	7.915059
5.579810	365.805749	7.920064
5.222563	354.022776	7.925069
5.639583	355.548786	7.930074
5.406213	358.011941	7.935078
5.799011	353.229983	7.940083
5.339353	351.533406	7.945088
5.644312	332.825561	7.950093
5.470660	336.586000	7.955098
5.144494	341.563085	7.960102
5.772935	352.708690	7.965107
5.518098	361.638834	7.970112
5.627882	335.896820	7.975117
5.423090	332.641695	7.980122
5.341423	342.788856	7.985139
5.458104	336.780985	7.990157
5.323055	340.156633	7.995174
5.589777	347.985166	8.000192
5.632793	356.404160	8.005210
5.296639	348.018397	8.010227
5.899458	355.330382	8.015245
5.662341	340.548240	8.020262
5.373040	329.337090	8.025280
5.199788	331.891926	8.030298
5.647722	344.015395	8.035315
5.554642	336.519334	8.040333
5.336789	347.850899	8.045350
5.953150	355.066091	8.050368
5.694837	342.142832	8.055386
5.231434	345.696158	8.060403
5.393461	342.543417	8.065421
5.498985	352.451581	8.070438
5.538784	354.288247	8.075456
6.012339	365.091782	8.080474
5.489472	351.465217	8.085491
5.486523	337.359581	8.090509
5.454062	344.304052	8.095526
5.527486	352.812951	8.100544
5.869595	365.707233	8.105562
5.777480	352.227767	8.110579
5.787090	339.669619	8.115597
5.507318	349.505610	8.120614
5.261639	341.503295	8.125632
5.543478	343.844821	8.130650
5.394863	361.660015	8.135667
5.747298	356.249499	8.140685
5.611147	361.720723	8.145702
5.581042	359.794101	8.150720
5.519938	358.639176	8.155738
5.588810	362.598244	8.160755
6.101546	364.584868	8.165773
5.988145	371.810268	8.170790
5.900482	362.546142	8.175808
5.553921	344.253049	8.180826
5.601145	341.055181	8.185843
5.665769	344.655159	8.190861
5.801840	353.416167	8.195878
5.727984	354.084091	8.200896
5.535969	347.231515	8.205914
5.371489	364.029900	8.210931
6.030535	358.303107	8.215949
6.018005	357.812740	8.220966
6.025766	360.579053	8.225984
5.641982	341.960444	8.231002
5.612883	337.913024	8.236019
5.659539	331.370188	8.241037
5.437008	351.844599	8.246054
5.752022	358.769346	8.251072
5.905533	357.716491	8.256090
5.787926	364.608040	8.261107
5.949611	352.859167	8.266125
5.704437	358.991239	8.271142
5.627218	358.280640	8.276160
6.119563	366.275796	8.281178
5.654150	354.221244	8.286195
5.773471	353.173746	8.291213
5.734613	359.579597	8.296230
5.683473	359.615973	8.301248
6.175311	359.668258	8.306266
5.727567	354.301067	8.311283
6.221495	352.519552	8.316301
5.846134	345.531605	8.321318
5.400798	340.896167	8.326336
5.717847	345.778841	8.331354
5.772932	361.204798	8.336371
6.134211	362.107493	8.341389
5.965383	358.268150	8.346406
5.695096	356.492766	8.351424
5.664633	356.241887	8.356442
5.590852	368.279863	8.361459
5.866098	365.355525	8.366477
5.958218	364.631016	8.371494
6.139005	368.225422	8.376512
6.091673	362.139101	8.381530
5.971017	362.861693	8.386547
5.722086	343.868513	8.391565
5.601916	359.618564	8.396582
5.873240	356.751645	8.401600
6.147886	364.414846	8.406618
5.973718	361.226417	8.411635
6.165844	352.596939	8.416653
5.928350	355.742496	8.421670
5.531009	352.611125	8.426688
5.819090	348.656014	8.431706
5.857973	359.685436	8.436723
6.107727	350.573572	8.441741
6.104247	356.409005	8.446758
5.758314	359.259136	8.451776
6.313328	359.465620	8.456794
6.284471	361.549724	8.461811
5.828185	360.251595	8.466829
6.130398	356.407874	8.471846
5.970057	352.125400	8.476864
5.961863	356.724530	8.481882
5.985718	366.449843	8.486899
6.126329	357.276183	8.491917
6.125226	352.918268	8.496934
5.761653	350.302301	8.501952
5.689841	364.589994	8.506970
6.018016	366.207914	8.511987
5.928392	366.092534	8.517005
5.708667	358.553192	8.522022
5.691139	360.698635	8.527040
5.932272	356.880262	8.532058
5.998387	358.567643	8.537075
5.942487	355.430110	8.542093
5.776290	352.833709	8.547110
5.741772	354.934478	8.552128
6.161004	355.449406	8.557146
6.174608	366.265049	8.562163
5.935227	351.637883	8.567181
6.192992	354.342935	8.572199
6.059420	366.390277	8.577216
6.294711	367.110747	8.582234
5.991295	364.179247	8.587251
5.993403	357.132154	8.592269
6.115567	367.681486	8.597287
6.167465	376.894340	8.602304
6.103178	376.023927	8.607322
5.917562	384.746993	8.612339
5.834618	377.350309	8.617357
5.828597	379.629648	8.622375
5.935019	375.901804	8.627392
6.136088	380.212539	8.632410
6.011357	383.217360	8.637427
6.272068	372.671068	8.642445
6.237558	378.700713	8.647463
6.268313	387.213158	8.652480
6.420438	377.731578	8.657498
5.978192	381.953765	8.662515
6.019623	368.582746	8.667533
6.354725	373.626697	8.672551
6.181425	377.235558	8.677568
6.230434	381.775240	8.682586
5.802627	376.427008	8.687603
6.048945	385.385348	8.692621
6.263164	379.822916	8.697639
6.266368	374.744816	8.702656
6.623879	377.639365	8.707674
6.366067	379.819302	8.712691
6.066924	376.874508	8.717709
6.204559	375.041520	8.722727
6.055612	382.957285	8.727744
6.383604	372.463567	8.732762
6.094917	387.646770	8.737779
6.252130	375.775510	8.742797
6.450279	372.061696	8.747815
6.137617	372.688144	8.752832
6.165918	367.656606	8.757850
6.370039	381.970505	8.762867
6.628075	383.280688	8.767885
6.553103	377.646806	8.772903
6.137955	384.313589	8.777920
6.562418	379.384074	8.782938
6.280101	380.652691	8.787955
6.712080	374.131515	8.792973
6.301735	380.791233	8.797991
6.574836	378.318498	8.803008
6.410774	379.985142	8.808026
6.335657	380.508101	8.813043
6.488335	379.736235	8.818061
6.340839	379.629922	8.823079
6.385228	373.355662	8.828096
6.500911	365.504995	8.833114
6.721670	367.663595	8.838131
6.774970	369.381386	8.843149
6.597210	370.176041	8.848167
6.124296	371.414561	8.853184
6.335850	364.568172	8.858202
6.245333	368.691067	8.863219
6.450404	367.453412	8.868237
6.557645	373.179987	8.873255
6.215173	381.694104	8.878272
6.462287	374.021651	8.883290
6.144785	384.968076	8.888307
6.062224	383.100162	8.893325
6.577659	376.600622	8.898343
6.317780	386.114787	8.903360
6.287275	373.360935	8.908378
5.954657	392.886991	8.913395
6.645326	402.211208	8.918413
6.652015	393.361462	8.923431
6.500124	402.899741	8.928448
6.632466	402.585485	8.933466
6.535564	404.225830	8.938483
6.693178	404.033844	8.943501
6.492240	413.425183	8.948519
6.784306	411.637420	8.953536
6.425432	401.434336	8.958554
6.660420	406.708571	8.963571
6.511140	406.116555	8.968589
6.610999	407.729228	8.973607
6.476966	415.150377	8.978624
6.128653	409.319477	8.983642
6.522867	402.807363	8.988659
6.316940	404.685691	8.993677
6.786461	398.067108	8.998695
6.557299	406.093279	9.003712
6.405765	405.103995	9.008730
6.475382	398.185160	9.013747
6.125726	403.680382	9.018765
6.619258	404.079532	9.023783
6.267093	407.659621	9.028800
6.672423	406.434767	9.033818
6.166421	411.768300	9.038835
6.430816	425.214432	9.043853
6.898509	424.172305	9.048871
6.999030	425.740695	9.053888
6.843907	411.343270	9.058906
6.840836	409.854209	9.063923
6.798293	408.589078	9.068941
6.915046	403.720392	9.073959
6.587369	400.029001	9.078976
6.685256	394.491103	9.083994
6.974775	393.956565	9.089011
7.223577	402.857721	9.094029
7.090269	393.790074	9.099047
6.743908	400.266210	9.104064
6.912405	388.229075	9.109082
6.762412	381.489819	9.114099
6.957773	395.085596	9.119117
7.051695	387.664352	9.124135
6.697617	398.695409	9.129152
6.770159	398.728186	9.134170
6.467845	402.549765	9.139187
6.749779	398.412574	9.144205
6.664414	395.538421	9.149223
6.604846	390.350234	9.154240
6.362624	389.403561	9.159258
6.453382	393.750518	9.164275
6.450784	397.610341	9.169293
6.789648	395.026316	9.174311
6.699611	394.349281	9.179328
7.321807	390.010461	9.184346
6.543724	396.140837	9.189363
6.540848	405.781999	9.194381
7.012359	404.145999	9.199399
6.592411	410.703094	9.204416
7.186353	416.151459	9.209434
6.894779	405.533894	9.214451
6.566861	403.710732	9.219469
7.289920	411.619268	9.224487
6.752525	409.869951	9.229504
6.657936	399.309886	9.234522
7.180359	408.808787	9.239539
7.261946	411.232189	9.244557
6.963150	401.297396	9.249575
6.500786	403.193812	9.254592
6.759192	407.606021	9.259610
6.854961	417.291692	9.264627
7.033757	422.842974	9.269645
7.182453	420.007881	9.274663
6.945573	410.830224	9.279680
7.123767	411.505994	9.284698
7.023707	408.580494	9.289715
6.933085	403.100530	9.294733
7.154084	391.872500	9.299751
6.746394	399.194512	9.304768
6.742878	403.395300	9.309786
6.942144	425.501490	9.314803
6.957966	419.080215	9.319821
7.231940	418.169424	9.324839
7.290501	431.657278	9.329856
7.022149	423.342905	9.334874
7.261916	417.246296	9.339891
7.119609	420.096090	9.344909
7.113694	406.801887	9.349927
7.109667	410.425257	9.354944
6.851488	408.111497	9.359962
6.771762	399.291066	9.364979
7.112040	414.467262	9.369997
7.525048	411.865307	9.375015
7.144411	412.224702	9.380032
6.941957	400.968341	9.385050
7.182393	405.481192	9.390067
7.249543	408.616895	9.395085
7.170960	410.844492	9.400103
7.084018	409.311769	9.405120
6.740189	410.829861	9.410138
6.992789	405.734767	9.415155
7.198850	417.662660	9.420173
7.073569	407.688054	9.425191
6.872482	426.442474	9.430208
7.329797	427.598364	9.435226
7.467375	423.426982	9.440243
7.089838	420.787946	9.445261
7.227777	421.653056	9.450279
7.289106	434.619783	9.455296
7.034025	418.000599	9.460314
7.149655	428.285909	9.465331
7.159338	435.955943	9.470349
7.175049	432.636767	9.475367
7.445898	433.711422	9.480384
7.205865	423.369787	9.485402
7.260660	430.417382	9.490419
7.223767	424.465101	9.495437
7.529563	418.686341	9.500455
7.136156	419.839826	9.505472
7.267303	420.421985	9.510490
7.302349	417.686748	9.515507
7.127321	425.925348	9.520525
7.434839	423.740697	9.525543
7.141310	432.392333	9.530560
7.375347	433.810419	9.535578
7.612221	420.487633	9.540595
6.863153	422.025039	9.545613
7.164806	430.611822	9.550631
7.136191	424.743449	9.555648
7.137631	430.874774	9.560666
7.148830	426.338193	9.565683
6.935908	432.496794	9.570701
7.247664	434.423400	9.575719
7.238096	432.916420	9.580736
7.239444	430.057076	9.585754
7.265255	429.257750	9.590771
7.379590	427.838652	9.595789
7.417742	422.729817	9.600807
7.262794	427.500278	9.605824
7.307132	427.515384	9.610842
7.528761	416.735354	9.615859
7.466999	427.029523	9.620877
7.238786	419.182223	9.625895
7.184826	431.043570	9.630912
7.065190	428.550313	9.635930
7.378339	436.011857	9.640947
7.541258	454.759766	9.645965
7.862359	454.318107	9.650983
7.547297	442.886863	9.656000
7.763087	434.506097	9.661018
7.738025	428.252166	9.666035
7.485530	436.862662	9.671053
7.859147	429.949831	9.676071
7.382184	426.692070	9.681088
7.591000	432.257586	9.686106
7.809021	425.176636	9.691123
7.654809	438.606317	9.696141
7.468817	427.918548	9.701159
7.825503	428.840902	9.706176
7.815016	418.823057	9.711194
7.578730	425.736380	9.716211
7.460196	431.918061	9.721229
7.635379	437.870692	9.726247
7.352347	432.247301	9.731264
7.420424	432.356514	9.736282
7.729032	427.886941	9.741299
7.519827	431.731808	9.746317
7.661139	420.838130	9.751335
7.644973	422.819269	9.756352
7.797697	421.422558	9.761370
7.929024	425.807346	9.766387
7.495727	427.591916	9.771405
7.590031	422.180800	9.776423
7.642957	428.165206	9.781440
7.544060	430.061480	9.786458
7.743917	423.358910	9.791475
7.767436	424.478627	9.796493
7.625747	424.384027	9.801511
7.405324	424.743566	9.806528
7.667016	427.066170	9.811546
7.910589	427.119485	9.816563
7.729936	429.217912	9.821581
7.603252	422.474989	9.826599
7.551376	423.556028	9.831616
7.712984	425.405174	9.836634
7.725517	426.094278	9.841651
7.770728	427.456744	9.846669
7.658306	430.267144	9.851687
7.890889	427.554604	9.856704
7.890112	425.957887	9.861722
7.689362	419.611568	9.866739
7.673963	428.484706	9.871757
7.401713	434.365432	9.876775
7.481481	424.424959	9.881792
7.343916	424.831474	9.886810
7.435344	420.051956	9.891827
7.632147	429.911148	9.896845
7.647094	443.159697	9.901863
8.054366	453.099532	9.906880
7.935809	454.954709	9.911898
7.972805	450.344654	9.916915
7.850599	449.685280	9.921933
7.920348	447.730380	9.926951
7.986465	448.240680	9.931968
7.746367	438.243021	9.936986
7.762834	435.864135	9.942003
7.783975	452.191717	9.947021
7.790975	445.601405	9.952039
8.215596	450.391515	9.957056
8.091002	445.544853	9.962074
8.295319	444.644975	9.967091
7.534699	437.815183	9.972109
7.816070	450.059494	9.977127
7.941425	449.001578	9.982144
7.957209	445.322635	9.987162
8.199552	440.904465	9.992179
7.999461	436.438856	9.997197
7.737170	436.479914	10.002215
7.805756	444.850762	10.007232
7.722281	451.209989	10.012250
8.206875	445.706158	10.017267
7.821497	446.265108	10.022285
8.175604	452.454791	10.027303
8.346483	441.629050	10.032320
8.143855	453.649403	10.037338
8.236678	437.976059	10.042355
8.204370	426.693023	10.047373
7.738661	425.992799	10.052391
7.860297	428.425707	10.057408
7.780891	442.219202	10.062426
8.136035	441.639668	10.067443
8.060071	453.457142	10.072461
7.969735	446.976751	10.077479
8.137365	443.715820	10.082496
8.067077	454.206996	10.087514
8.246860	445.734038	10.092531
7.847636	449.343598	10.097549
7.651604	448.067800	10.102567
7.921767	441.234289	10.107584
7.766415	452.145882	10.112602
8.063299	441.899988	10.117619
7.823212	447.131908	10.122637
7.995340	441.487692	10.127655
8.336325	450.667912	10.132672
7.775574	444.848194	10.137690
8.222568	445.532342	10.142707
8.039772	445.516764	10.147725
8.170508	455.670339	10.152743
8.532281	450.687512	10.157760
8.346487	460.827568	10.162778
8.028671	442.529870	10.167795
7.662651	458.346931	10.172813
8.056464	463.097692	10.177831
8.464075	458.385386	10.182848
8.611170	470.915832	10.187866
8.790988	462.588025	10.192883
8.387544	458.422509	10.197901
8.324403	451.098429	10.202919
8.481640	441.104785	10.207936
8.108854	436.530537	10.212954
8.363917	433.767137	10.217971
8.155227	444.365197	10.222989
8.235113	445.283585	10.228007
8.344625	441.672005	10.233024
8.037118	441.262566	10.238042
8.170899	434.232681	10.243059
8.426704	448.330257	10.248077
8.348472	447.402067	10.253095
8.160858	446.888638	10.258112
8.458759	458.183645	10.263130
8.501314	461.765014	10.268147
8.706963	463.001362	10.273165
8.335175	448.644166	10.278183
8.817784	441.354500	10.283200
8.557297	447.810886	10.288218
8.390844	441.989350	10.293235
8.272522	445.507562	10.298253
8.408542	451.491578	10.303271
8.570071	450.620495	10.308288
8.306224	449.399502	10.313306
8.167155	440.329578	10.318323
8.217779	444.411441	10.323341
8.851125	449.465488	10.328359
8.763556	447.263843	10.333376
8.605547	454.846552	10.338394
8.398965	445.869253	10.343411
8.580648	440.422351	10.348429
8.515127	438.393974	10.353447
8.523958	436.779972	10.358464
8.367193	437.397775	10.363482
8.658260	427.692431	10.368499
8.509399	434.901322	10.373517
8.525479	440.550685	10.378535
8.603673	440.693027	10.383552
8.331886	437.857543	10.388570
8.289780	440.518075	10.393587
8.437469	451.647269	10.398605
8.622433	456.386570	10.403623
8.927445	453.779439	10.408640
8.673874	453.550893	10.413658
8.770254	443.989651	10.418675
8.663152	437.120580	10.423693
8.570430	437.330725	10.428711
8.541883	440.074338	10.433728
9.016560	438.409437	10.438746
8.729864	434.774732	10.443763
8.656259	436.007496	10.448781
8.555155	431.434862	10.453799
8.675472	435.013509	10.458816
8.496997	446.941713	10.463834
8.541670	434.340136	10.468851
8.610082	430.154344	10.473869
8.824833	449.133962	10.478887
9.102199	440.484774	10.483904
8.629445	440.644013	10.488922
8.649132	438.760072	10.493939
8.549973	442.884338	10.498957
8.721064	443.049993	10.503975
8.740498	455.111292	10.508992
8.801284	465.004438	10.514010
8.708964	457.157919	10.519027
8.932469	460.657289	10.524045
8.819187	462.839837	10.529063
8.634188	456.989644	10.534080
8.481732	468.295261	10.539098
8.926766	456.154793	10.544115
8.960569	464.758314	10.549133
9.144856	459.973703	10.554151
9.101559	447.947621	10.559168
8.784815	448.729342	10.564186
8.996641	446.146280	10.569203
9.093712	446.190992	10.574221
8.588221	448.034211	10.579239
8.678632	444.864272	10.584256
8.302760	463.422059	10.589274
8.981935	462.365730	10.594291
9.304148	458.105452	10.599309
8.931021	471.705154	10.604327
9.221814	466.711354	10.609344
8.897604	473.250316	10.614362
8.512224	466.024055	10.619379
8.658066	465.912806	10.624397
8.634285	467.977192	10.629415
9.018369	458.695906	10.634432
8.623641	462.162756	10.639450
8.845290	460.947744	10.644467
8.695064	471.205307	10.649485
8.354087	467.440248	10.654503
8.523361	470.812421	10.659520
9.109507	487.919339	10.664538
9.468190	496.481440	10.669555
9.298372	480.214905	10.674573
8.959175	480.460513	10.679591
8.920923	473.066254	10.684608
9.068878	487.291211	10.689626
9.443995	485.597724	10.694643
9.477506	469.185735	10.699661
8.993093	471.432744	10.704679
9.130266	464.553791	10.709696
8.992572	467.667952	10.714714
9.019865	461.664577	10.719731
9.086077	463.800068	10.724749
9.015730	471.741426	10.729767
9.116877	474.619355	10.734784
9.338218	480.634194	10.739802
9.298957	478.137804	10.744819
9.226726	470.326001	10.749837
8.870694	469.043713	10.754855
9.030973	472.698156	10.759872
9.148228	483.043202	10.764890
9.123816	492.447949	10.769907
9.422380	499.113402	10.774925
9.306167	491.157005	10.779943
9.296426	482.316100	10.784960
9.261105	482.072293	10.789978
9.243273	477.038485	10.794995
9.563811	470.796661	10.800013
9.036557	471.683947	10.805031
9.320212	468.805611	10.810048
9.244122	473.298647	10.815066
9.196262	475.947463	10.820083
9.327798	479.275058	10.825101
8.955119	493.152411	10.830119
9.554634	489.710196	10.835136
9.744197	491.974683	10.840154
9.624602	481.396398	10.845171
9.665092	470.865618	10.850189
9.191595	474.641452	10.855207
9.058513	465.330741	10.860224
8.929545	462.299310	10.865242
8.884954	479.422995	10.870259
9.163393	478.016051	10.875277
9.483307	487.527789	10.880295
9.607669	485.043630	10.885312
9.425483	486.365992	10.890330
9.506259	490.733470	10.895347
9.085067	490.913032	10.900365
9.440424	496.313599	10.905383
9.345314	479.965932	10.910400
9.319341	494.521097	10.915418
9.571405	490.931353	10.920435
9.654401	483.284568	10.925453
9.622828	484.293003	10.930471
9.366184	484.980103	10.935488
9.669118	489.947078	10.940506
9.717502	490.936674	10.945523
9.610801	494.251107	10.950541
9.434993	492.950047	10.955559
9.900446	486.376249	10.960576
9.792946	497.583324	10.965594
9.739528	487.559544	10.970611
9.828468	483.171711	10.975629
9.711174	487.724853	10.980647
9.776960	481.538719	10.985664
9.409519	470.109353	10.990682
9.314191	466.892774	10.995699
9.553575	470.421215	11.000717
9.334316	490.955233	11.005735
9.498452	483.377784	11.010752
9.680374	493.138359	11.015770
9.588071	483.442560	11.020787
9.845228	485.775349	11.025805
9.161422	489.252785	11.030823
9.274845	485.713166	11.035840
9.633075	490.488444	11.040858
9.373171	488.203345	11.045875
9.707580	482.486352	11.050893
9.315485	489.859605	11.055911
9.599372	490.357876	11.060928
9.845389	497.687955	11.065946
10.014123	498.409392	11.070963
9.915480	499.901698	11.075981
9.960275	495.908935	11.080999
9.814207	485.262213	11.086016
9.745946	488.498040	11.091034
9.746308	490.811106	11.096051
9.898076	485.248959	11.101069
9.871427	495.395657	11.106087
9.989160	484.303668	11.111104
9.723437	490.883964	11.116122
9.828875	491.047283	11.121139
10.066911	488.848265	11.126157
9.643212	487.958422	11.131175
9.808321	479.396231	11.136192
9.689065	473.472617	11.141210
9.798820	471.722881	11.146227
9.981597	476.999006	11.151245
9.711091	487.597310	11.156263
10.098295	489.893945	11.161280
9.892622	481.654930	11.166298
9.712893	490.541223	11.171315
9.981959	477.696179	11.176333
9.990296	494.139412	11.181351
9.977981	491.297978	11.186368
10.062582	481.615488	11.191386
9.680190	485.367582	11.196403
10.036864	504.776294	11.201421
10.094045	501.507412	11.206439
10.110732	498.049218	11.211456
10.002546	496.226331	11.216474
10.308530	498.081266	11.221491
10.591949	488.317128	11.226509
10.471037	487.625993	11.231527
10.215401	482.670467	11.236544
9.979330	480.078683	11.241562
9.989477	483.194929	11.246579
10.200636	488.668578	11.251597
9.940765	485.354702	11.256615
10.086128	493.031903	11.261632
10.022183	483.580965	11.266650
10.233992	491.487591	11.271667
10.190612	482.935974	11.276685
10.345742	490.172996	11.281703
10.112544	494.100528	11.286720
9.812653	492.960917	11.291738
9.974237	494.223106	11.296755
9.973664	478.564360	11.301773
9.826653	489.856514	11.306791
10.454900	500.957780	11.311808
10.356476	496.785489	11.316826
10.269909	497.057786	11.321843
10.196269	485.771722	11.326861
10.415916	488.561660	11.331879
10.465086	485.420264	11.336896
10.302976	487.017186	11.341914
10.040392	488.169112	11.346931
10.273551	488.684798	11.351949
10.486314	497.777837	11.356967
10.130370	487.886662	11.361984
10.145560	478.783082	11.367002
10.031841	492.506254	11.372019
10.638460	495.131423	11.377037
10.397161	498.406986	11.382055
10.419850	487.639149	11.387072
10.565226	494.543192	11.392090
10.423240	488.212888	11.397107
10.605652	482.058972	11.402125
10.288545	479.934312	11.407143
10.377385	475.215144	11.412160
10.505861	472.077104	11.417178
10.469013	482.354779	11.422195
10.035438	470.282536	11.427213
10.393890	485.604265	11.432231
10.424208	486.779725	11.437248
10.417977	479.875898	11.442266
10.291253	499.982026	11.447283
10.773094	501.279242	11.452301
10.644799	504.152100	11.457319
10.257877	486.455309	11.462336
10.515616	489.438091	11.467354
10.610010	492.916672	11.472371
10.539681	489.194408	11.477389
10.257117	491.586516	11.482407
10.531096	503.049398	11.487424
10.766116	500.270194	11.492442
10.696152	501.152104	11.497459
10.947924	483.001801	11.502477
10.404756	485.415805	11.507495
10.386574	477.453522	11.512512
10.773788	486.134222	11.517530
10.594908	498.655803	11.522547
11.067808	490.846941	11.527565
10.799193	487.206237	11.532583
10.283904	481.117457	11.537600
10.509287	472.757260	11.542618
10.313766	489.866734	11.547635
10.944195	497.354330	11.552653
10.882777	503.224135	11.557671
10.695466	511.594085	11.562688
11.137259	498.904995	11.567706
10.657779	489.676947	11.572723
10.766922	480.833195	11.577741
10.719228	483.895389	11.582759
10.570329	483.921836	11.587776
10.665902	487.709495	11.592794
10.513628	505.793644	11.597811
10.774517	509.091511	11.602829
11.018185	505.976441	11.607847
11.061366	512.041296	11.612864
11.132951	504.497273	11.617882
10.652600	499.144614	11.622899
10.603220	489.577783	11.627917
10.598367	502.106813	11.632935
10.332102	515.421567	11.637952
10.684198	506.441908	11.642970
11.023707	511.649307	11.647987
10.902094	511.292789	11.653005
11.164451	511.440990	11.658023
10.942398	511.425251	11.663040
11.061150	511.204640	11.668058
10.984455	514.773146	11.673075
10.952101	508.062746	11.678093
10.849628	508.145035	11.683111
10.869073	512.932375	11.688128
10.757347	509.229216	11.693146
10.730929	513.900668	11.698163
10.723511	509.051408	11.703181
11.146251	513.882856	11.708199
10.999937	506.499203	11.713216
11.053069	511.221305	11.718234
11.008794	507.977785	11.723251
10.936961	513.555740	11.728269
10.911699	512.928511	11.733287
10.761284	512.573350	11.738304
11.156387	518.917577	11.743322
10.943358	515.574265	11.748339
10.842684	511.632693	11.753357
11.198156	511.797862	11.758375
11.140363	526.203406	11.763392
11.715104	517.602261	11.768410
11.421936	515.278190	11.773427
11.636595	511.940450	11.778445
11.221778	506.400799	11.783463
10.996995	510.778288	11.788480
11.141631	501.562898	11.793498
11.052412	508.633089	11.798515
10.959299	508.663419	11.803533
11.309408	507.926884	11.808551
11.128128	510.634479	11.813568
10.923207	513.049138	11.818586
10.805438	526.230182	11.823603
11.187135	528.451947	11.828621
11.527641	521.427506	11.833639
11.270851	521.657047	11.838656
11.470457	526.132146	11.843674
11.176824	523.991180	11.848691
11.279219	529.283071	11.853709
11.437100	539.233627	11.858727
11.348969	532.393104	11.863744
11.300836	530.784863	11.868762
10.788264	535.579828	11.873779
11.242465	529.436960	11.878797
11.384373	538.159276	11.883815
11.518593	539.854938	11.888832
11.539454	527.730389	11.893850
11.677944	536.248116	11.898867
11.503541	534.587076	11.903885
11.927331	524.734655	11.908903
11.400142	524.732012	11.913920
11.193885	529.497916	11.918938
11.429653	528.529992	11.923955
11.382595	526.372482	11.928973
11.306468	523.686205	11.933991
11.243324	535.994022	11.939008
11.205977	541.828511	11.944026
11.457042	543.868778	11.949043
11.285092	534.848138	11.954061
11.511124	541.086321	11.959079
11.252276	533.483608	11.964096
11.908818	532.273034	11.969114
11.501299	529.417776	11.974131
11.217464	529.654710	11.979149
11.618211	530.046311	11.984167
11.316820	526.672662	11.989184
11.529914	530.946836	11.994202
11.606097	539.916132	11.999219
11.633528	550.704474	12.004237
11.850425	551.320538	12.009255
11.343112	553.378644	12.014272
11.582491	559.163470	12.019290
11.453489	546.702632	12.024307
11.538286	554.657589	12.029325
11.568001	552.131447	12.034343
11.834184	564.898917	12.039360
12.056836	551.123833	12.044378
11.936429	551.019586	12.049395
11.952503	548.255744	12.054413
11.995936	557.334320	12.059431
11.757775	550.918078	12.064448
11.946318	548.079877	12.069466
12.030130	555.230271	12.074483
11.794756	547.081084	12.079501
11.888682	522.909049	12.084519
11.160518	536.472911	12.089536
12.130351	541.445861	12.094554
11.692514	553.143378	12.099571
11.864132	554.287236	12.104589
12.104248	558.812799	12.109607
11.663828	557.436430	12.114624
11.967685	557.256242	12.119642
12.044997	564.713766	12.124659
12.331635	559.506000	12.129677
12.077161	550.832792	12.134695
11.554095	544.716808	12.139712
11.767123	545.816308	12.144730
11.839136	556.190576	12.149747
11.919812	553.186241	12.154765
12.176075	546.111875	12.159783
12.091631	553.550559	12.164800
12.050671	554.131286	12.169818
12.136069	550.750677	12.174835
11.892972	551.432502	12.179853
11.986761	550.682478	12.184871
11.929061	557.435330	12.189888
12.144948	560.497263	12.194906
11.984455	564.189361	12.199923
11.864246	562.090644	12.204941
12.216348	555.663967	12.209959
12.080294	556.026068	12.214976
12.106080	564.558311	12.219994
12.157859	558.333320	12.225011
12.147498	559.051262	12.230029
12.151691	551.994298	12.235047
11.882880	561.863401	12.240064
12.157630	559.630220	12.245082
12.116268	559.627195	12.250099
11.832070	563.468061	12.255117
12.371934	554.544164	12.260135
12.009735	570.808842	12.265152
12.259345	552.933359	12.270170
12.309333	553.916396	12.275187
12.361817	563.135566	12.280205
12.714275	554.506115	12.285223
12.575938	559.220361	12.290240
12.272499	560.154633	12.295258
11.901497	561.490805	12.300275
12.228954	556.566974	12.305293
12.632813	551.271417	12.310311
12.239057	558.433523	12.315328
12.236790	547.338205	12.320346
12.252230	563.868751	12.325363
12.229912	570.792787	12.330381
12.623471	572.656098	12.335399
12.435824	587.028390	12.340416
12.431732	580.114722	12.345434
12.099983	580.387566	12.350451
12.188775	576.618262	12.355469
12.151767	583.588784	12.360487
12.201182	584.650807	12.365504
12.556513	582.647991	12.370522
12.413200	587.394582	12.375539
12.311048	596.328732	12.380557
12.455396	585.238821	12.385575
12.280378	587.579378	12.390592
12.364640	585.082554	12.395610
12.631214	573.175093	12.400627
12.186166	585.852045	12.405645
12.495320	592.787269	12.410663
12.597110	602.383737	12.415680
12.639500	595.096712	12.420698
12.660106	594.894632	12.425715
12.167220	598.070779	12.430733
12.682059	602.717410	12.435751
12.783627	606.785017	12.440768
12.782395	605.030567	12.445786
13.340078	598.555885	12.450803
13.362731	591.593842	12.455821
13.041404	583.606426	12.460839
12.573793	577.617438	12.465856
12.690060	573.193744	12.470874
12.836301	582.638071	12.475891
12.506375	580.758401	12.480909
12.662828	570.098942	12.485927
12.588931	576.923766	12.490944
12.520234	580.601484	12.495962
12.695441	585.023617	12.500979
12.728094	595.823791	12.505997
12.882607	592.883619	12.511015
13.238250	598.154786	12.516032
12.904355	600.261465	12.521050
13.011034	588.988108	12.526067
12.618877	600.416570	12.531085
12.833198	591.786654	12.536103
13.192074	596.350424	12.541120
12.772326	596.504513	12.546138
13.263100	593.603174	12.551155
12.511296	591.284680	12.556173
12.859888	592.201999	12.561191
13.031796	596.608873	12.566208
13.236983	604.753270	12.571226
13.298285	604.762562	12.576243
12.469602	599.505473	12.581261
13.003045	597.985983	12.586279
12.997852	601.167768	12.591296
12.982284	601.952799	12.596314
13.263398	604.916159	12.601331
12.992365	608.770750	12.606349
13.051330	609.720826	12.611367
13.024206	614.950986	12.616384
12.737304	606.702549	12.621402
13.318329	606.557828	12.626419
12.998823	607.409414	12.631437
13.001152	608.453570	12.636455
12.962997	602.996882	12.641472
12.967661	604.491945	12.646490
12.981298	594.656412	12.651507
13.259221	600.586689	12.656525
13.129964	601.007685	12.661543
13.035661	601.069759	12.666560
12.883285	600.260474	12.671578
13.114475	602.373288	12.676595
12.821522	623.827864	12.681613
13.465977	623.976159	12.686631
13.425898	625.566596	12.691648
13.356314	621.525455	12.696666
13.632294	620.888892	12.701683
13.385724	627.766035	12.706701
13.721791	618.747807	12.711719
13.492719	610.790105	12.716736
13.330590	603.137494	12.721754
13.266708	606.252737	12.726771
13.143009	616.572499	12.731789
13.834423	610.487109	12.736807
13.292439	607.741268	12.741824
13.220148	612.741822	12.746842
13.664656	617.143859	12.751859
13.701285	625.431438	12.756877
13.810453	611.525767	12.761895
13.377271	614.866129	12.766912
13.577017	592.930636	12.771930
13.381880	605.000409	12.776947
12.694688	606.689078	12.781965
13.395464	617.293067	12.786983
13.816119	618.199097	12.792000
13.731276	628.995610	12.797018
13.888141	621.460267	12.802035
13.686185	618.579098	12.807053
13.484222	615.391822	12.812071
13.472668	609.855226	12.817088
13.624325	622.123136	12.822106
13.862493	618.068490	12.827123
13.307351	628.411677	12.832141
13.817819	615.670720	12.837159
13.804665	626.774732	12.842176
13.640422	624.736556	12.847194
13.752975	623.690103	12.852211
13.865033	630.353269	12.857229
13.853934	615.052654	12.862247
13.643424	611.358639	12.867264
13.714009	615.203888	12.872282
13.785609	616.805228	12.877299
13.902678	623.259326	12.882317
13.694638	615.478205	12.887335
13.874952	620.035244	12.892352
13.586031	629.156462	12.897370
14.005997	621.201205	12.902387
13.971379	624.671623	12.907405
14.015888	616.346010	12.912423
14.078859	622.085913	12.917440
13.593300	616.787681	12.922458
13.968090	623.766282	12.927475
14.037227	624.534886	12.932493
13.842492	621.611561	12.937511
13.798209	624.890992	12.942528
13.418381	625.524815	12.947546
13.723954	622.560971	12.952563
13.543648	627.793045	12.957581
13.661744	622.700029	12.962599
14.031159	629.124058	12.967616
13.780336	622.851783	12.972634
13.921658	625.388931	12.977651
14.258012	644.387574	12.982669
14.149169	628.086104	12.987687
14.093202	634.359036	12.992704
14.004326	631.778881	12.997722
14.082817	631.545641	13.002739
14.067037	644.060704	13.007757
14.421017	649.676126	13.012775
14.118477	638.031358	13.017792
14.106307	638.740120	13.022810
14.385068	647.371620	13.027827
14.262850	629.232430	13.032845
14.040193	632.337841	13.037863
14.116484	634.052055	13.042880
14.179239	648.757544	13.047898
14.393960	644.129060	13.052915
14.462091	648.937211	13.057933
14.531049	639.929264	13.062951
14.185420	626.139020	13.067968
14.060084	630.557761	13.072986
14.501369	636.822212	13.078003
14.289303	645.410694	13.083021
14.525747	649.394064	13.088039
14.660499	640.751345	13.093056
14.182041	628.607133	13.098074
14.531096	628.176868	13.103091
14.299723	623.646686	13.108109
14.324878	622.774871	13.113127
14.550264	625.084254	13.118144
14.089607	634.727839	13.123162
14.942013	630.308711	13.128179
14.495493	634.077196	13.133197
14.261707	616.024926	13.138215
14.509108	631.162212	13.143232
14.371484	642.553976	13.148250
14.512514	640.875062	13.153267
14.822314	641.299850	13.158285
14.620132	639.081425	13.163303
14.419529	645.758871	13.168320
14.311627	636.857532	13.173338
14.447825	637.694524	13.178355
14.256500	646.832017	13.183373
14.236357	638.525991	13.188391
14.416052	641.120243	13.193408
14.730939	640.010530	13.198426
14.591433	633.727122	13.203443
14.653030	640.508650	13.208461
14.329301	640.732901	13.213479
14.657752	635.856229	13.218496
14.801234	642.394557	13.223514
14.791050	633.692500	13.228531
14.541011	642.810789	13.233549
14.678324	641.526929	13.238567
15.096939	656.971922	13.243584
14.663304	653.104577	13.248602
14.721254	647.232035	13.253619
14.824662	655.089447	13.258637
14.918840	666.792043	13.263655
15.064586	654.616283	13.268672
14.994501	655.201577	13.273690
14.607172	639.366604	13.278707
14.957843	650.959575	13.283725
14.688351	661.542044	13.288743
15.359928	669.222080	13.293760
15.079716	654.948197	13.298778
14.778073	644.388871	13.303795
14.990787	648.148742	13.308813
14.999601	660.546355	13.313831
15.017032	658.801599	13.318848
15.232602	664.318793	13.323866
15.365996	653.912203	13.328883
14.954116	645.361440	13.333901
14.656839	639.617140	13.338919
15.174847	643.486966	13.343936
15.149758	669.286150	13.348954
15.281909	661.792532	13.353971
15.021442	663.284960	13.358989
14.715815	670.613181	13.364007
15.317025	657.952651	13.369024
15.154068	662.620289	13.374042
15.148695	661.895264	13.379059
15.346500	662.088294	13.384077
15.289148	657.795922	13.389095
15.625212	660.738060	13.394112
15.216928	666.861079	13.399130
15.443249	661.757407	13.404147
15.247800	644.790999	13.409165
15.284569	645.227008	13.414183
15.459059	637.325983	13.419200
14.981650	639.508801	13.424218
15.387235	651.894734	13.429235
15.355734	656.702718	13.434253
15.468871	656.729135	13.439271
15.582936	650.847799	13.444288
15.284197	645.463484	13.449306
15.361879	646.530549	13.454323
15.446568	663.025091	13.459341
15.218488	663.745592	13.464359
15.856750	652.401530	13.469376
15.416091	654.256701	13.474394
15.398165	640.449815	13.479411
15.531093	652.951052	13.484429
15.324866	662.554787	13.489447
15.332138	651.899718	13.494464
15.220796	648.701393	13.499482
15.536419	657.216671	13.504499
15.565272	653.642933	13.509517
15.826539	657.799138	13.514535
15.143920	650.111294	13.519552
15.405034	652.118441	13.524570
15.321163	651.475143	13.529587
15.442749	655.618520	13.534605
15.581623	657.294529	13.539623
15.334842	652.214493	13.544640
15.359270	664.530768	13.549658
15.770142	675.517882	13.554675
16.047276	682.395042	13.559693
15.775998	670.518139	13.564711
15.741686	655.454653	13.569728
15.748040	665.091354	13.574746
15.970807	664.002384	13.579763
15.659860	659.033384	13.584781
15.702136	657.843307	13.589799
16.104681	664.577736	13.594816
15.485087	660.231446	13.599834
15.874997	675.273858	13.604851
16.014431	675.618044	13.609869
15.794044	680.045378	13.614887
15.844447	669.639159	13.619904
15.673354	680.872091	13.624922
15.892027	681.251198	13.629939
15.817336	675.793901	13.634957
15.520463	674.360318	13.639975
16.245319	671.065687	13.644992
15.730005	687.502783	13.650010
15.674954	681.382849	13.655027
15.958418	679.545916	13.660045
16.036074	688.025910	13.665063
15.918752	686.441119	13.670080
15.900433	682.698042	13.675098
16.304695	679.280073	13.680115
15.868046	683.782317	13.685133
15.901282	674.215066	13.690151
15.928852	688.036171	13.695168
16.080156	698.880933	13.700186
16.119925	696.728733	13.705203
16.651426	701.675734	13.710221
16.497812	700.456387	13.715239
16.685816	679.396779	13.720256
16.022220	680.592612	13.725274
16.111062	680.461891	13.730291
16.113563	672.521526	13.735309
16.328402	691.984224	13.740327
16.431722	690.311213	13.745344
16.301891	691.663257	13.750362
16.182865	691.031777	13.755379
16.594749	699.358425	13.760397
16.480332	697.615388	13.765415
16.638895	687.542504	13.770432
16.500787	680.700287	13.775450
16.572529	680.313471	13.780467
16.345677	670.786972	13.785485
16.518678	671.734963	13.790503
16.675777	672.057447	13.795520
16.327105	679.919431	13.800538
16.478166	669.061943	13.805555
16.916406	664.041831	13.810573
16.440617	672.147788	13.815591
16.504072	664.122138	13.820608
16.939424	672.877438	13.825626
16.617695	664.719636	13.830643
16.522258	673.980974	13.835661
16.494039	679.905595	13.840679
16.668148	671.701660	13.845696
16.149696	676.705865	13.850714
16.420481	677.401852	13.855731
16.558185	672.457227	13.860749
16.511751	677.049808	13.865767
16.965208	685.865393	13.870784
16.511905	684.096560	13.875802
16.606318	693.302916	13.880819
17.106238	701.890324	13.885837
16.732580	689.960021	13.890855
16.815574	696.084972	13.895872
16.747747	685.646775	13.900890
16.541391	699.665485	13.905907
17.361834	693.484113	13.910925
16.990234	698.982863	13.915943
16.698712	680.014931	13.920960
16.681601	681.005332	13.925978
16.847202	691.311367	13.930995
16.764694	687.193342	13.936013
16.372412	699.391896	13.941031
17.005839	699.964794	13.946048
16.829801	704.871176	13.951066
16.537624	697.879524	13.956083
16.650592	694.298910	13.961101
16.586256	698.001216	13.966119
16.941462	697.652037	13.971136
17.170018	698.963707	13.976154
16.999524	702.060957	13.981171
16.923119	700.031100	13.986189
17.119885	718.199632	13.991207
17.403978	712.550410	13.996224
17.320443	706.965102	14.001242
17.208815	695.697479	14.006259
17.130504	693.213489	14.011277
16.834128	702.086606	14.016295
17.168308	711.896029	14.021312
17.339940	716.116784	14.026330
17.317284	717.742369	14.031347
17.565321	718.814305	14.036365
17.228050	707.178089	14.041383
17.487809	703.580786	14.046400
17.125434	699.588657	14.051418
16.969629	703.283204	14.056435
17.577223	708.379230	14.061453
17.350594	717.926232	14.066471
17.542444	717.018827	14.071488
17.567217	710.192104	14.076506
17.279935	714.210208	14.081523
17.476698	710.304040	14.086541
17.572423	716.569013	14.091559
17.613282	701.250715	14.096576
17.264842	701.497774	14.101594
17.108102	704.823241	14.106611
17.393300	704.431383	14.111629
17.525689	720.145338	14.116647
17.644477	713.565813	14.121664
17.474079	718.711154	14.126682
17.287318	719.459897	14.131699
17.414576	717.063615	14.136717
17.185189	714.631694	14.141735
17.343528	717.276641	14.146752
17.264021	715.370344	14.151770
17.483417	720.173748	14.156787
17.609836	703.879529	14.161805
17.717910	709.448292	14.166823
17.511113	713.573706	14.171840
17.992654	729.589568	14.176858
17.600642	719.372557	14.181875
18.120466	719.092259	14.186893
17.776219	717.779703	14.191911
17.879259	710.801862	14.196928
17.868703	715.641294	14.201946
17.583955	719.179324	14.206963
17.642881	711.249036	14.211981
17.832736	722.759954	14.216999
18.146814	726.267277	14.222016
18.225776	725.522725	14.227034
18.051811	716.679032	14.232051
17.984396	708.509767	14.237069
17.853440	720.108817	14.242087
17.649317	724.647222	14.247104
17.900175	725.731340	14.252122
18.007777	733.843748	14.257139
18.192761	732.375688	14.262157
17.884930	740.688889	14.267175
18.060321	737.391975	14.272192
18.265730	727.289637	14.277210
18.369797	729.245661	14.282227
18.280399	716.611243	14.287245
18.132774	710.452155	14.292263
18.170449	707.795356	14.297280
18.186117	710.538394	14.302298
17.773624	707.895324	14.307315
18.158975	713.717289	14.312333
18.181030	736.328155	14.317351
18.034425	732.715620	14.322368
18.495464	731.813375	14.327386
18.192045	738.235567	14.332403
18.677505	729.455807	14.337421
18.599339	732.866798	14.342439
18.229039	724.666086	14.347456
18.508169	716.145876	14.352474
18.489702	723.687901	14.357491
18.198412	716.945410	14.362509
17.942088	717.929112	14.367527
18.169892	733.334641	14.372544
18.363238	737.116501	14.377562
17.865382	737.080858	14.382579
18.067890	733.527233	14.387597
18.375555	733.753544	14.392615
18.191050	733.829751	14.397632
18.365306	733.549948	14.402650
18.472946	751.827152	14.407667
18.881735	752.381600	14.412685
18.882069	742.055766	14.417703
18.909756	743.480963	14.422720
18.824960	725.376836	14.427738
18.704810	738.937105	14.432755
18.750222	735.101981	14.437773
18.678865	746.764294	14.442791
18.517187	737.132875	14.447808
18.890835	735.004097	14.452826
18.621138	732.543776	14.457843
18.874872	734.814020	14.462861
18.706125	736.440405	14.467879
18.490695	732.441025	14.472896
18.689336	726.915640	14.477914
18.787958	730.693405	14.482931
18.687759	726.221538	14.487949
18.748280	739.851329	14.492967
18.941118	740.704698	14.497984
19.054420	732.084231	14.503002
18.926646	737.424870	14.508019
18.701371	730.287024	14.513037
18.763785	732.236951	14.518055
18.885866	748.195541	14.523072
18.756677	748.045332	14.528090
18.710738	752.928187	14.533107
19.363525	748.720188	14.538125
19.102365	744.226199	14.543143
19.126072	756.384862	14.548160
19.043602	753.469171	14.553178
18.964845	757.956385	14.558195
19.090730	747.424685	14.563213
19.069082	750.981458	14.568231
19.449029	747.138099	14.573248
19.198146	738.729322	14.578266
19.021112	752.557288	14.583283
19.173469	739.326401	14.588301
19.165138	737.797111	14.593319
19.402304	739.921629	14.598336
19.254702	746.407773	14.603354
19.161575	757.552799	14.608371
19.220991	745.336855	14.613389
19.084593	746.696242	14.618407
19.453972	749.374400	14.623424
19.416463	738.675803	14.628442
19.097536	760.961430	14.633459
19.427811	744.881385	14.638477
19.331121	748.964309	14.643495
19.080960	749.246462	14.648512
19.443963	748.034530	14.653530
19.468581	758.798193	14.658547
19.328496	752.278149	14.663565
19.625527	743.587864	14.668583
19.107377	761.092129	14.673600
19.537527	751.248054	14.678618
19.365065	768.303690	14.683635
19.592843	767.229708	14.688653
19.197480	778.216974	14.693671
19.303230	776.275332	14.698688
19.729171	760.555824	14.703706
19.982912	759.187441	14.708723
19.954760	775.005493	14.713741
19.734944	768.466377	14.718759
19.967987	772.652278	14.723776
19.843220	771.444185	14.728794
19.975723	766.238418	14.733811
20.234291	772.818723	14.738829
19.953592	752.996952	14.743847
19.382080	756.999639	14.748864
20.284793	756.662506	14.753882
19.719828	755.892611	14.758899
19.637738	743.575763	14.763917
19.888993	760.618652	14.768935
19.742249	767.202499	14.773952
20.037822	761.002355	14.778970
19.918852	774.975875	14.783987
19.980322	770.279852	14.789005
19.988734	758.093981	14.794023
19.898541	768.276037	14.799040
20.138411	771.501507	14.804058
20.227977	768.006596	14.809075
20.124743	772.374572	14.814093
20.079657	765.094871	14.819111
20.130592	772.616576	14.824128
20.117309	766.909789	14.829146
19.917913	765.615559	14.834163
19.938108	778.077743	14.839181
20.254387	766.629423	14.844199
20.055836	769.617472	14.849216
19.910595	766.582227	14.854234
20.152512	766.992408	14.859251
20.033783	766.509201	14.864269
20.116516	764.839410	14.869287
20.000205	765.599207	14.874304
20.017300	761.648594	14.879322
20.304624	776.640894	14.884339
20.560005	773.486074	14.889357
20.284149	783.981250	14.894375
20.336297	787.902008	14.899392
20.743373	784.209024	14.904410
20.436015	784.954574	14.909427
20.341266	785.900341	14.914445
20.850997	780.859528	14.919463
20.432957	779.697384	14.924480
20.533510	770.548722	14.929498
20.669425	773.989295	14.934515
20.454615	773.653686	14.939533
21.012211	782.759115	14.944551
20.499383	774.675384	14.949568
20.559652	765.877018	14.954586
20.827273	776.754096	14.959603
20.389014	769.838952	14.964621
20.887480	784.129149	14.969639
20.452770	781.849309	14.974656
20.812970	780.915524	14.979674
21.023266	792.407505	14.984691
20.743904	785.375941	14.989709
20.652174	772.817588	14.994727
20.606753	785.195383	14.999744
20.710390	790.894255	15.004762
20.658320	787.342637	15.009779
20.752811	787.012215	15.014797
21.084494	786.575202	15.019815
20.714020	792.900622	15.024832
20.763122	782.112690	15.029850
20.569563	780.662910	15.034867
20.795821	777.512653	15.039885
20.764115	781.875736	15.044903
20.472715	787.507113	15.049920
21.398642	788.649567	15.054938
21.227032	782.664625	15.059955
21.215016	781.997441	15.064973
21.097004	774.530347	15.069991
21.199468	780.655432	15.075008
21.225753	769.845836	15.080026
20.935724	781.586614	15.085043
20.983605	784.548678	15.090061
20.969690	781.707448	15.095079
21.411437	809.803696	15.100096
21.616846	800.240959	15.105114
21.300990	792.908997	15.110131
21.122874	787.562544	15.115149
21.891105	789.622796	15.120167
21.403835	786.745277	15.125184
21.232716	773.482996	15.130202
21.090527	777.674041	15.135219
20.874820	788.304962	15.140237
21.264758	787.527463	15.145255
21.193782	797.785420	15.150272
21.454208	794.465705	15.155290
21.544073	807.759591	15.160307
21.525802	802.855148	15.165325
21.819340	807.451300	15.170343
21.703741	804.439806	15.175360
21.966919	797.963859	15.180378
21.670599	807.351415	15.185395
21.723511	805.585306	15.190413
21.901086	793.660084	15.195431
21.388223	779.776002	15.200448
21.599534	779.957450	15.205466
21.498153	790.220167	15.210483
21.609881	797.445179	15.215501
21.695942	793.281783	15.220519
21.747374	794.476046	15.225536
21.712375	786.756100	15.230554
21.923954	788.322901	15.235571
21.597017	796.752729	15.240589
21.564365	792.554285	15.245607
22.043796	801.397416	15.250624
21.688421	792.455877	15.255642
21.735006	792.675757	15.260659
21.511469	798.375401	15.265677
21.835985	793.606600	15.270695
22.013624	792.436331	15.275712
21.814687	794.698611	15.280730
21.733141	791.426164	15.285747
21.763908	795.760528	15.290765
22.316225	814.258458	15.295783
22.111842	813.971707	15.300800
22.053204	797.952548	15.305818
22.392302	806.372702	15.310835
22.127485	808.970353	15.315853
21.926900	800.768262	15.320871
21.941023	809.908363	15.325888
22.151286	814.855235	15.330906
22.406721	810.958787	15.335923
22.078822	815.336727	15.340941
22.611754	809.774720	15.345959
22.368617	820.217454	15.350976
22.359166	820.499763	15.355994
22.484754	815.582243	15.361011
22.317242	815.371766	15.366029
22.540729	821.073960	15.371047
22.514406	825.445678	15.376064
22.721795	813.632537	15.381082
22.517191	800.347080	15.386099
22.222658	794.637012	15.391117
22.727763	795.977944	15.396135
22.335216	798.119081	15.401152
22.352748	811.216021	15.406170
22.489698	813.122720	15.411187
22.544583	819.785448	15.416205
22.899049	803.979270	15.421223
22.433652	814.207516	15.426240
22.590875	814.719331	15.431258
22.952848	815.047587	15.436275
22.309251	820.257631	15.441293
22.814480	812.815949	15.446311
22.656705	823.961677	15.451328
22.718269	816.520079	15.456346
22.764139	815.506154	15.461363
22.743079	816.604478	15.466381
23.049413	813.640484	15.471399
22.805454	821.138985	15.476416
22.983580	814.193520	15.481434
22.774021	810.496159	15.486451
22.554255	813.986156	15.491469
22.813835	811.935202	15.496487
22.747778	807.767234	15.501504
22.518528	816.677227	15.506522
22.834473	811.452173	15.511539
22.912558	819.080097	15.516557
23.063570	814.625653	15.521575
22.726419	823.849200	15.526592
22.905924	836.870288	15.531610
23.206493	834.876026	15.536627
23.416965	840.794861	15.541645
23.240355	834.031200	15.546663
23.303195	840.358174	15.551680
23.234837	841.965684	15.556698
23.718388	836.496612	15.561715
23.572940	825.972664	15.566733
23.420512	815.329896	15.571751
23.066975	811.453122	15.576768
23.059388	815.370622	15.581786
23.217524	802.214522	15.586803
22.933109	819.896817	15.591821
23.084938	834.932486	15.596839
23.180151	835.078476	15.601856
23.490238	840.079143	15.606874
23.535997	820.830997	15.611891
22.990085	828.231644	15.616909
23.366922	834.143345	15.621927
23.553913	833.684820	15.626944
23.536715	836.448807	15.631962
23.476077	829.228321	15.636979
23.119248	839.297559	15.641997
23.288766	834.527786	15.647015
23.502921	850.894921	15.652032
23.440456	859.917659	15.657050
23.546683	857.240631	15.662067
23.305434	856.861824	15.667085
24.132337	854.141309	15.672103
23.873674	859.149042	15.677120
23.898134	850.921134	15.682138
23.877562	860.325474	15.687155
23.729843	853.598305	15.692173
23.787699	859.332774	15.697191
24.000176	859.643429	15.702208
24.115970	859.486393	15.707226
24.268471	862.725569	15.712243
24.265548	853.151264	15.717261
24.013414	850.006520	15.722279
24.026556	854.602435	15.727296
23.809600	858.334998	15.732314
24.182727	847.562530	15.737331
23.878148	851.911579	15.742349
23.910269	841.590175	15.747367
24.405441	854.274639	15.752384
24.001120	850.939144	15.757402
24.293503	838.759219	15.762419
24.071179	847.788063	15.767437
24.271588	846.311265	15.772455
24.313560	850.318838	15.777472
24.200929	853.100935	15.782490
24.465981	842.885046	15.787507
24.165611	849.802262	15.792525
24.316925	848.266884	15.797543
24.215637	847.566348	15.802560
23.867878	846.853936	15.807578
24.192842	845.250325	15.812595
24.178489	856.938493	15.817613
24.222262	847.208552	15.822631
24.051926	855.310915	15.827648
24.286970	882.814814	15.832666
24.776166	873.740907	15.837683
24.520088	883.923774	15.842701
24.878504	872.279435	15.847719
24.985621	881.796324	15.852736
24.634991	868.047700	15.857754
24.989598	862.207502	15.862771
24.331921	861.960214	15.867789
24.566410	856.009450	15.872807
24.654046	856.592129	15.877824
24.279400	869.327679	15.882842
24.602143	870.034469	15.887859
24.708175	874.789405	15.892877
24.881640	867.355499	15.897895
24.847535	869.475198	15.902912
25.180169	865.869601	15.907930
25.217852	869.388700	15.912947
25.027128	876.875727	15.917965
24.930169	870.822255	15.922983
25.027498	871.646413	15.928000
25.013289	869.603636	15.933018
25.279127	871.045178	15.938035
24.822697	875.276013	15.943053
24.651531	876.397860	15.948071
24.969149	874.233664	15.953088
24.802065	873.164738	15.958106
25.190232	869.118092	15.963123
25.106816	871.715733	15.968141
25.106666	873.773308	15.973159
25.139379	868.882949	15.978176
24.924725	870.144153	15.983194
25.195550	870.571899	15.988211
24.978530	873.790077	15.993229
25.031181	872.762463	15.998247
25.625707	876.948556	16.003264
25.386975	875.266005	16.008282
25.421351	872.597076	16.013299
25.231044	872.314430	16.018317
25.468203	877.455922	16.023335
25.748102	890.568617	16.028352
25.439526	875.169219	16.033370
25.374235	874.160084	16.038387
25.296857	890.711788	16.043405
25.550987	887.834856	16.048423
25.736810	887.370201	16.053440
25.767459	891.941292	16.058458
25.882793	882.146471	16.063475
25.732931	889.516649	16.068493
25.436772	880.433243	16.073511
25.738505	879.000528	16.078528
25.721155	887.400828	16.083546
25.920621	887.814508	16.088563
26.034470	885.789535	16.093581
25.768179	887.377568	16.098599
26.165693	883.417818	16.103616
25.699241	883.045893	16.108634
25.909184	872.425210	16.113651
25.995833	885.116899	16.118669
25.956849	890.165960	16.123687
26.091696	876.016217	16.128704
25.693237	878.552767	16.133722
25.826455	892.515268	16.138739
25.702335	888.511013	16.143757
25.955094	884.643371	16.148775
26.245869	887.952405	16.153792
26.030605	887.869329	16.158810
26.144263	875.774186	16.163827
26.022067	868.774768	16.168845
26.010504	880.109063	16.173863
26.269051	866.372293	16.178880
26.268562	881.693799	16.183898
26.315701	868.327822	16.188915
26.653116	886.316699	16.193933
25.952324	876.703400	16.198951
26.485550	879.217051	16.203968
26.010649	877.498918	16.208986
26.272435	871.578586	16.214003
26.139138	873.126846	16.219021
26.067391	876.388535	16.224039
26.305251	878.636038	16.229056
26.383918	896.731738	16.234074
26.528012	896.090584	16.239091
26.702445	891.206416	16.244109
27.023862	903.321690	16.249127
26.811075	884.202347	16.254144
26.715628	880.670129	16.259162
26.460577	868.310867	16.264179
26.381773	879.712501	16.269197
26.528313	891.249250	16.274215
26.892032	885.432864	16.279232
26.549648	898.283301	16.284250
26.419347	891.278832	16.289267
26.657643	887.962567	16.294285
26.354493	900.219877	16.299303
26.700370	902.564068	16.304320
26.403869	895.976959	16.309338
26.412494	903.846177	16.314355
26.806268	908.114224	16.319373
26.603592	927.554233	16.324391
26.857592	928.031953	16.329408
26.903740	919.421918	16.334426
27.170833	920.705476	16.339443
27.142374	919.106741	16.344461
27.030283	922.513616	16.349479
27.603378	912.075854	16.354496
27.447620	919.819354	16.359514
27.441442	911.103911	16.364531
27.620889	916.566883	16.369549
27.662817	913.836804	16.374567
27.573878	904.755633	16.379584
27.199946	905.704122	16.384602
27.361687	900.815629	16.389619
27.457336	899.774964	16.394637
27.407856	899.467097	16.399655
27.514778	889.534734	16.404672
27.507603	899.454549	16.409690
27.553457	892.498220	16.414707
27.691598	886.057611	16.419725
27.277295	885.178898	16.424743
27.637677	896.814690	16.429760
27.166414	909.256136	16.434778
27.259620	902.008361	16.439795
27.512028	911.007038	16.444813
27.347527	912.768475	16.449831
27.667793	912.039757	16.454848
27.588792	911.884838	16.459866
27.652774	909.533159	16.464883
27.751207	915.939790	16.469901
27.416376	921.041524	16.474919
28.086187	912.396894	16.479936
27.750711	910.571706	16.484954
27.869838	906.955370	16.489971
27.888949	908.574429	16.494989
27.455957	905.066690	16.500007
27.954488	913.398798	16.505024
27.946172	929.867134	16.510042
28.507079	939.650628	16.515059
28.133362	927.682304	16.520077
27.769866	909.782602	16.525095
28.496748	905.307337	16.530112
28.084422	906.978213	16.535130
27.890313	905.118253	16.540147
27.828858	913.825279	16.545165
28.267468	920.812933	16.550183
28.321955	919.633549	16.555200
28.177680	933.213524	16.560218
28.526454	930.305978	16.565235
28.342049	926.746663	16.570253
28.208810	932.122930	16.575271
28.735615	922.421410	16.580288
28.320298	935.620973	16.585306
28.527919	932.637711	16.590323
28.490802	927.871886	16.595341
28.550768	928.749239	16.600359
28.483896	922.580580	16.605376
28.401547	921.015535	16.610394
28.471235	914.184852	16.615411
28.678799	929.451711	16.620429
28.490512	923.841720	16.625447
28.805701	921.109852	16.630464
28.658166	920.407091	16.635482
28.388241	916.880112	16.640499
28.691406	920.272418	16.645517
28.639547	922.909304	16.650535
28.700942	926.904384	16.655552
28.274576	927.955764	16.660570
28.590492	922.809578	16.665587
28.999253	924.102499	16.670605
28.539266	921.880250	16.675623
28.950005	921.351952	16.680640
28.902280	940.041858	16.685658
29.134455	947.800330	16.690675
29.169138	946.437853	16.695693
28.961212	944.475912	16.700711
29.242211	945.369127	16.705728
29.219871	950.201002	16.710746
29.018109	943.163528	16.715763
29.197489	951.539347	16.720781
28.873672	947.941910	16.725799
29.546701	950.367395	16.730816
29.120803	939.278246	16.735834
29.619696	941.986635	16.740851
29.702301	939.407970	16.745869
29.116952	931.767877	16.750887
29.356802	928.015858	16.755904
29.546627	938.012127	16.760922
29.528152	935.433520	16.765939
29.602959	933.193751	16.770957
29.451902	937.506143	16.775975
29.667401	932.744919	16.780992
29.664484	942.468429	16.786010
29.562327	927.071359	16.791027
29.301365	932.180458	16.796045
29.090838	932.005121	16.801063
29.467142	935.168219	16.806080
29.415794	947.127331	16.811098
29.200683	943.746394	16.816115
29.307828	946.705512	16.821133
29.629836	938.232128	16.826151
29.818590	948.023441	16.831168
30.044754	966.417996	16.836186
29.751388	970.938888	16.841203
30.208360	970.333917	16.846221
29.863583	966.622995	16.851239
30.173008	955.046239	16.856256
29.967641	947.002620	16.861274
29.936017	936.798446	16.866291
30.095399	937.805391	16.871309
30.117810	957.147049	16.876327
29.881984	957.748853	16.881344
30.140863	959.573348	16.886362
30.069351	963.321014	16.891379
30.270477	962.557312	16.896397
29.965978	975.474453	16.901415
29.918756	967.342930	16.906432
30.081962	964.647490	16.911450
30.021010	970.107118	16.916467
30.373812	959.363014	16.921485
30.207891	969.291961	16.926503
30.461945	962.419750	16.931520
30.113649	966.277055	16.936538
30.229404	958.312507	16.941555
30.403680	965.376308	16.946573
30.205981	963.119270	16.951591
30.321109	964.729602	16.956608
30.235579	967.924039	16.961626
30.328334	972.141435	16.966643
30.480401	969.962141	16.971661
30.649249	977.642184	16.976679
30.619331	973.626306	16.981696
30.441028	984.314600	16.986714
30.565654	981.439009	16.991731
30.520493	973.130434	16.996749
30.494775	982.156944	17.001767
30.555838	989.377350	17.006784
30.839422	990.973913	17.011802
31.140814	991.201211	17.016819
31.044992	992.895090	17.021837
31.263393	991.080943	17.026855
31.275252	991.524020	17.031872
31.187097	989.619048	17.036890
31.369210	992.531713	17.041907
31.330618	971.832313	17.046925
31.418098	966.119142	17.051943
31.360039	956.509239	17.056960
31.151291	961.518646	17.061978
31.068604	967.988388	17.066995
31.195911	965.617312	17.072013
30.830313	975.593326	17.077031
30.881117	985.409430	17.082048
31.341702	982.171929	17.087066
31.470809	987.510265	17.092083
31.567527	990.736113	17.097101
31.295185	993.637930	17.102119
31.917869	990.195149	17.107136
31.672124	990.359847	17.112154
31.511680	992.748666	17.117171
31.421386	989.360787	17.122189
31.554141	1000.416925	17.127207
31.558980	996.335635	17.132224
31.543085	990.411433	17.137242
31.519180	985.356342	17.142259
31.776240	988.904209	17.147277
31.688016	994.712103	17.152295
31.511380	981.475777	17.157312
31.568567	982.473490	17.162330
31.419559	989.086175	17.167347
31.862661	989.666814	17.172365
31.955325	1003.455874	17.177383
31.884788	992.771767	17.182400
31.766862	995.362210	17.187418
31.766631	1006.221434	17.192435
31.945944	1008.121517	17.197453
31.735224	1010.672852	17.202471
31.783907	1008.623360	17.207488
32.124348	1011.192483	17.212506
31.783846	1008.310866	17.217523
32.030275	995.462686	17.222541
32.245244	1014.382913	17.227559
32.224869	1003.441628	17.232576
32.407999	1004.536375	17.237594
32.160320	1005.474556	17.242611
32.788700	1013.903134	17.247629
32.443047	1006.493700	17.252647
32.453344	1003.550810	17.257664
32.371197	1000.830690	17.262682
32.356944	999.728343	17.267699
32.533966	1015.280931	17.272717
32.721822	1006.604469	17.277735
32.715984	1006.807319	17.282752
32.743832	999.913730	17.287770
32.825431	999.455935	17.292787
32.705989	991.420924	17.297805
32.541343	1001.677895	17.302823
32.495087	996.304407	17.307840
32.764248	997.628674	17.312858
32.771456	1009.080032	17.317875
32.799676	995.041575	17.322893
32.393843	1002.483463	17.327911
32.821609	1020.085931	17.332928
32.995303	1026.717498	17.337946
32.804007	1037.253223	17.342963
33.167029	1019.520452	17.347981
33.270697	1031.253359	17.352999
33.149665	1030.877804	17.358016
33.411295	1022.196088	17.363034
32.904362	1034.898832	17.368051
32.981352	1029.897349	17.373069
33.245531	1022.196699	17.378087
32.980187	1030.512844	17.383104
33.127117	1029.650332	17.388122
33.213150	1033.445914	17.393139
33.383098	1023.462576	17.398157
33.280049	1032.674799	17.403175
33.176283	1028.064558	17.408192
33.276065	1024.419671	17.413210
33.353126	1033.676260	17.418227
33.327318	1023.786709	17.423245
33.556600	1025.073044	17.428263
33.124340	1031.916319	17.433280
33.711382	1046.751434	17.438298
33.340585	1047.910881	17.443315
33.687851	1048.465512	17.448333
33.493014	1054.451077	17.453351
33.633940	1059.304739	17.458368
33.988104	1054.278756	17.463386
33.720779	1050.871265	17.468403
33.858415	1041.394759	17.473421
33.824170	1047.844316	17.478439
34.088213	1041.914107	17.483456
34.040815	1038.184979	17.488474
33.787728	1048.014016	17.493491
34.524648	1036.202969	17.498509
34.367188	1039.124664	17.503527
33.947847	1040.717755	17.508544
34.093844	1040.764271	17.513562
34.040100	1042.792392	17.518579
34.306094	1037.972735	17.523597
34.395578	1041.802492	17.528615
34.442253	1033.741434	17.533632
34.675122	1039.697853	17.538650
34.385852	1045.401562	17.543667
34.504234	1030.481095	17.548685
34.444571	1026.211086	17.553703
33.905903	1027.381054	17.558720
34.231558	1021.444354	17.563738
34.055607	1037.023861	17.568755
34.339894	1044.266120	17.573773
34.340571	1039.121954	17.578791
34.148933	1034.869465	17.583808
34.761252	1034.467374	17.588826
34.419949	1043.846322	17.593843
34.412406	1035.831629	17.598861
34.324134	1033.623709	17.603879
34.607813	1055.739550	17.608896
34.724369	1049.378004	17.613914
34.590884	1063.559154	17.618931
34.835404	1067.765418	17.623949
34.570552	1069.116553	17.628967
34.801661	1064.832536	17.633984
34.807479	1054.846493	17.639002
34.740336	1062.762366	17.644019
34.918489	1059.092571	17.649037
35.098279	1052.790545	17.654055
34.793154	1060.544886	17.659072
35.439396	1050.976063	17.664090
35.429298	1057.459711	17.669107
34.965612	1056.629751	17.674125
34.799453	1064.573762	17.679143
35.037450	1074.890768	17.684160
35.342911	1079.368357	17.689178
35.235175	1094.324991	17.694195
35.568894	1090.081698	17.699213
35.526336	1088.939598	17.704231
35.558710	1092.412235	17.709248
35.408721	1083.378408	17.714266
35.909117	1080.980420	17.719283
35.597361	1076.708871	17.724301
35.829518	1069.584427	17.729319
35.446487	1059.678240	17.734336
35.763155	1061.159172	17.739354
35.656810	1075.680066	17.744371
35.842252	1080.479422	17.749389
35.848368	1082.700143	17.754407
35.871322	1079.408114	17.759424
36.033358	1074.582644	17.764442
35.689891	1062.041437	17.769459
35.400193	1067.530622	17.774477
35.999055	1069.513303	17.779495
35.958715	1078.444322	17.784512
35.897732	1072.438793	17.789530
36.154991	1079.442301	17.794547
36.136234	1070.277464	17.799565
36.002351	1069.036064	17.804583
36.006424	1073.955354	17.809600
36.193498	1074.743370	17.814618
36.276105	1069.712592	17.819635
36.094379	1076.036942	17.824653
36.152890	1065.960585	17.829671
35.978362	1072.930755	17.834688
36.208455	1072.282432	17.839706
36.121829	1077.556764	17.844723
36.259864	1080.514220	17.849741
36.538733	1093.586201	17.854759
36.401330	1095.438085	17.859776
36.552399	1095.692093	17.864794
36.519509	1095.271168	17.869811
36.378978	1100.604447	17.874829
36.601935	1093.850669	17.879847
36.649390	1096.926462	17.884864
36.990627	1082.346582	17.889882
36.667622	1088.939227	17.894899
36.495639	1095.725967	17.899917
36.773196	1080.057830	17.904935
36.773759	1091.355645	17.909952
36.755161	1093.397201	17.914970
36.952239	1092.848725	17.919987
36.716614	1097.723524	17.925005
36.731542	1086.694606	17.930023
36.756137	1101.456941	17.935040
36.983305	1097.912004	17.940058
37.088510	1118.736739	17.945075
37.228761	1119.292248	17.950093
37.616081	1106.216783	17.955111
37.192625	1115.596016	17.960128
37.142236	1101.525611	17.965146
37.304606	1109.156232	17.970163
37.356581	1119.088993	17.975181
37.515427	1101.656377	17.980199
37.116688	1107.585543	17.985216
37.739878	1105.304015	17.990234
37.622593	1113.751638	17.995251
37.578282	1112.808631	18.000269
37.664149	1111.819981	18.005287
37.360532	1118.681003	18.010304
37.925503	1113.994366	18.015322
37.676544	1108.302304	18.020339
37.921101	1103.586975	18.025357
37.852639	1099.842199	18.030375
37.533987	1114.156544	18.035392
37.782591	1114.149114	18.040410
37.802621	1116.919934	18.045427
37.965871	1108.711188	18.050445
38.162502	1113.647657	18.055463
37.795341	1113.386404	18.060480
38.097946	1107.901418	18.065498
37.688488	1104.112236	18.070515
37.919279	1111.460736	18.075533
38.168468	1100.896885	18.080551
37.845821	1103.995952	18.085568
38.027810	1111.118565	18.090586
37.860529	1107.218854	18.095603
37.854861	1120.417488	18.100621
38.364036	1122.026056	18.105639
38.227375	1121.217440	18.110656
38.471427	1131.808090	18.115674
38.597882	1125.498617	18.120691
38.585248	1125.210219	18.125709
38.563447	1128.962755	18.130727
38.485909	1130.353975	18.135744
38.784351	1123.275929	18.140762
38.527879	1126.740179	18.145779
38.559793	1123.027010	18.150797
38.887477	1129.691294	18.155815
39.095717	1126.985619	18.160832
38.948545	1125.648465	18.165850
38.703872	1120.129299	18.170867
39.056237	1133.334964	18.175885
38.922685	1127.586943	18.180903
38.687726	1121.952644	18.185920
38.849431	1118.541038	18.190938
38.940891	1124.396562	18.195955
38.620229	1126.617994	18.200973
39.085185	1125.345882	18.205991
38.859815	1121.228048	18.211008
38.944202	1118.933105	18.216026
38.984295	1125.105951	18.221043
39.336217	1138.024506	18.226061
39.555528	1139.104125	18.231079
39.336093	1121.942201	18.236096
39.364115	1115.023293	18.241114
39.287621	1125.209719	18.246131
39.327113	1142.611206	18.251149
39.794528	1137.706315	18.256167
39.553104	1141.477484	18.261184
39.274039	1131.021628	18.266202
39.500390	1132.636640	18.271219
39.231050	1133.669740	18.276237
39.851929	1146.053848	18.281255
39.822132	1140.832375	18.286272
40.009484	1145.126511	18.291290
39.829559	1136.958896	18.296307
39.724592	1149.254755	18.301325
39.975926	1133.549652	18.306343
40.163732	1126.482628	18.311360
40.102748	1139.999216	18.316378
40.384947	1136.180557	18.321395
40.023274	1133.576797	18.326413
40.068673	1138.205602	18.331431
39.816403	1138.917287	18.336448
39.610526	1139.874172	18.341466
39.657214	1133.709739	18.346483
39.850577	1143.904388	18.351501
39.832427	1143.553738	18.356519
39.959001	1149.170235	18.361536
39.999296	1155.791193	18.366554
40.283167	1154.282359	18.371571
39.999708	1167.335199	18.376589
40.245911	1169.149079	18.381607
40.205596	1166.400288	18.386624
40.328831	1163.010480	18.391642
40.541791	1165.059946	18.396659
40.531571	1171.146015	18.401677
40.776459	1174.418111	18.406695
40.868620	1183.782868	18.411712
40.600629	1181.366398	18.416730
40.844098	1174.353751	18.421747
40.934201	1179.726658	18.426765
41.322976	1172.823792	18.431783
41.018878	1166.767957	18.436800
40.863640	1160.966518	18.441818
41.077692	1154.324567	18.446835
41.004211	1179.500901	18.451853
41.310769	1175.508000	18.456871
40.916450	1178.662492	18.461888
41.037490	1178.810750	18.466906
41.441065	1174.954131	18.471923
41.206166	1182.849003	18.476941
41.706298	1173.861596	18.481959
41.620178	1179.612415	18.486976
40.980098	1164.324666	18.491994
41.179526	1159.404951	18.497011
41.057487	1169.355536	18.502029
41.297181	1171.388191	18.507047
41.302253	1172.495066	18.512064
41.121018	1171.854381	18.517082
41.324916	1173.037405	18.522099
41.112322	1184.116206	18.527117
41.656293	1176.643058	18.532135
42.153550	1191.331412	18.537152
41.981716	1192.264031	18.542170
42.291944	1180.081078	18.547187
41.782599	1175.903579	18.552205
41.997937	1167.225889	18.557223
41.635456	1180.420510	18.562240
41.958245	1180.136365	18.567258
42.175652	1189.724503	18.572275
42.117429	1190.143850	18.577293
42.291592	1184.546419	18.582311
42.278454	1180.146005	18.587328
41.912747	1168.747475	18.592346
42.098101	1173.307023	18.597363
42.235367	1191.895625	18.602381
42.323614	1189.350754	18.607399
42.409784	1187.547839	18.612416
42.293380	1185.906052	18.617434
42.252597	1189.532184	18.622451
42.362015	1189.028999	18.627469
42.303652	1183.966627	18.632487
42.315137	1182.383700	18.637504
42.418389	1197.840706	18.642522
42.867925	1184.537681	18.647539
42.274312	1186.088659	18.652557
42.168028	1185.650828	18.657575
42.743899	1193.544911	18.662592
42.611940	1205.409527	18.667610
42.637838	1213.516021	18.672627
42.802112	1212.653939	18.677645
42.922349	1215.263904	18.682663
43.100881	1204.026239	18.687680
42.568244	1207.486434	18.692698
42.964442	1210.176241	18.697715
42.645657	1206.177167	18.702733
42.618999	1210.145080	18.707751
42.794063	1220.670851	18.712768
43.302677	1233.031583	18.717786
43.266918	1226.182587	18.722803
43.417962	1231.833147	18.727821
43.525586	1230.437129	18.732839
43.726779	1229.354663	18.737856
43.521841	1228.531492	18.742874
44.116293	1226.371219	18.747891
43.855503	1228.854688	18.752909
43.590142	1213.915294	18.757927
43.532877	1207.296898	18.762944
43.869329	1226.636984	18.767962
44.185563	1210.129522	18.772979
43.441083	1212.117558	18.777997
43.875676	1216.865291	18.783015
43.807438	1218.535934	18.788032
43.931684	1215.584624	18.793050
43.731313	1220.027889	18.798067
43.757314	1219.073860	18.803085
43.941497	1223.526305	18.808103
44.189706	1225.286227	18.813120
44.169424	1219.488871	18.818138
44.220553	1218.101706	18.823155
44.471223	1220.381961	18.828173
44.162399	1222.699381	18.833191
44.048880	1216.673632	18.838208
44.116435	1230.015512	18.843226
43.884700	1221.332101	18.848243
44.329966	1224.793723	18.853261
44.343453	1213.764951	18.858279
44.670813	1226.646393	18.863296
44.379161	1233.133191	18.868314
44.562782	1240.845749	18.873331
44.675038	1243.415942	18.878349
44.505708	1243.922127	18.883367
44.809240	1232.551248	18.888384
44.725047	1232.845274	18.893402
44.567389	1233.479022	18.898419
44.479348	1239.548904	18.903437
44.665293	1233.971703	18.908455
44.806259	1244.203022	18.913472
44.745379	1240.867293	18.918490
44.622933	1244.159084	18.923507
44.905299	1244.925866	18.928525
44.878118	1260.504351	18.933543
45.306187	1258.673107	18.938560
45.094643	1263.269617	18.943578
45.149172	1255.295593	18.948595
45.106682	1256.255288	18.953613
45.124604	1263.350017	18.958631
45.368919	1256.684352	18.963648
45.046767	1258.770331	18.968666
45.317493	1253.905692	18.973683
44.907439	1248.718518	18.978701
45.370675	1265.959059	18.983719
45.695004	1272.529247	18.988736
45.384953	1275.591655	18.993754
45.803876	1266.664264	18.998771
45.985628	1272.354208	19.003789
45.726920	1276.431078	19.008807
45.992216	1277.307836	19.013824
46.056303	1277.745893	19.018842
46.276181	1278.026994	19.023859
46.311242	1278.690510	19.028877
46.081309	1269.063184	19.033895
46.489337	1275.528738	19.038912
46.318247	1275.176800	19.043930
46.387998	1256.391496	19.048947
46.203001	1248.858956	19.053965
46.165450	1243.140039	19.058983
46.534981	1254.156081	19.064000
46.224906	1254.595954	19.069018
46.731132	1261.828777	19.074035
46.591215	1249.915123	19.079053
46.389944	1238.443446	19.084071
46.055277	1248.591495	19.089088
46.489548	1263.277154	19.094106
46.613238	1256.851300	19.099123
46.733101	1262.134361	19.104141
46.651846	1263.166404	19.109159
46.630136	1262.999349	19.114176
46.467512	1268.762183	19.119194
46.400674	1264.322824	19.124211
46.452868	1266.567908	19.129229
46.810072	1284.210098	19.134247
46.585613	1285.826325	19.139264
47.191077	1286.520397	19.144282
47.382772	1282.248816	19.149299
47.309207	1285.504553	19.154317
47.172544	1281.379095	19.159335
47.164482	1281.762182	19.164352
47.055553	1286.822314	19.169370
47.161398	1281.734186	19.174387
47.011118	1290.120789	19.179405
47.291508	1285.352460	19.184423
47.259133	1284.644265	19.189440
47.484782	1283.949293	19.194458
47.891539	1307.043423	19.199475
47.483865	1293.776789	19.204493
47.907704	1296.897791	19.209511
48.033003	1291.951783	19.214528
47.645878	1286.022527	19.219546
47.868930	1286.789137	19.224563
47.986039	1291.286823	19.229581
47.854858	1299.774582	19.234599
48.301163	1292.960489	19.239616
47.667181	1290.929558	19.244634
47.734342	1288.634136	19.249651
48.128945	1287.600261	19.254669
48.096445	1291.730057	19.259687
48.051537	1291.655002	19.264704
48.153070	1302.233369	19.269722
48.547631	1288.162532	19.274739
48.200705	1287.188031	19.279757
47.921092	1288.364764	19.284775
48.388860	1292.397246	19.289792
48.245044	1287.745874	19.294810
48.361222	1293.465034	19.299827
48.421589	1293.556526	19.304845
48.522318	1288.671175	19.309863
48.454455	1294.072022	19.314880
48.313488	1306.127470	19.319898
48.939128	1312.464267	19.324915
48.905187	1313.712967	19.329933
48.863932	1314.227491	19.334951
49.039734	1307.499956	19.339968
48.663361	1325.086702	19.344986
49.382344	1307.017001	19.350003
49.196728	1309.999957	19.355021
49.200930	1319.141874	19.360039
49.162524	1315.026260	19.365056
48.735792	1316.396464	19.370074
49.000340	1310.882664	19.375091
48.896861	1316.244917	19.380109
48.875412	1308.194409	19.385127
49.067521	1314.943123	19.390144
49.136638	1333.807645	19.395162
49.300466	1338.758784	19.400179
49.728026	1338.287803	19.405197
49.430545	1338.492168	19.410215
49.850384	1342.475364	19.415232
49.766290	1344.808085	19.420250
49.957463	1346.280301	19.425267
50.194840	1341.768012	19.430285
50.015905	1342.695439	19.435303
49.896386	1334.044885	19.440320
49.684898	1336.706842	19.445338
49.782233	1337.650946	19.450355
49.838709	1339.122174	19.455373
49.737509	1341.631148	19.460391
49.751464	1333.723409	19.465408
49.949010	1337.387972	19.470426
50.140815	1343.038493	19.475443
50.526091	1351.173954	19.480461
50.494533	1357.260274	19.485479
50.622067	1356.489151	19.490496
50.571011	1356.333005	19.495514
50.576375	1354.189273	19.500531
50.620177	1356.470398	19.505549
50.499686	1359.578862	19.510567
50.745551	1347.478465	19.515584
50.264596	1355.610785	19.520602
50.440625	1349.498598	19.525619
50.433674	1348.941056	19.530637
50.289472	1360.741419	19.535655
50.722280	1348.498120	19.540672
50.565561	1357.592683	19.545690
50.967905	1368.190233	19.550707
51.115505	1372.632668	19.555725
50.898323	1377.075451	19.560743
51.066365	1371.573597	19.565760
51.375574	1374.049834	19.570778
51.201290	1381.465067	19.575795
51.262303	1382.825132	19.580813
51.325640	1376.869452	19.585831
51.065746	1369.111903	19.590848
51.282352	1379.684910	19.595866
51.277740	1376.261442	19.600883
51.310820	1369.152290	19.605901
51.524034	1379.574345	19.610919
51.559619	1385.804794	19.615936
51.628366	1394.103479	19.620954
51.820335	1386.947334	19.625971
52.042484	1390.169383	19.630989
51.594709	1395.096437	19.636007
51.816384	1383.795093	19.641024
51.923801	1399.040175	19.646042
52.044335	1384.210597	19.651059
52.329950	1394.722307	19.656077
52.189877	1395.167106	19.661095
52.403902	1387.218529	19.666112
52.221888	1390.459718	19.671130
51.909794	1396.732020	19.676147
52.250424	1391.635479	19.681165
52.146356	1396.675945	19.686183
52.203653	1387.331767	19.691200
52.364866	1390.156252	19.696218
52.306565	1396.701225	19.701235
52.578462	1393.890860	19.706253
52.272182	1398.028861	19.711271
52.398670	1397.431475	19.716288
52.733929	1413.107946	19.721306
52.658758	1413.062879	19.726323
52.782650	1405.387200	19.731341
53.149221	1409.227274	19.736359
52.680679	1407.138849	19.741376
53.057804	1409.822208	19.746394
52.893276	1406.789874	19.751411
53.144985	1408.722841	19.756429
53.234203	1418.757235	19.761447
53.246451	1401.672353	19.766464
53.283289	1403.051987	19.771482
52.991470	1409.100203	19.776499
53.248249	1415.722055	19.781517
53.446445	1422.469856	19.786535
53.707838	1433.095840	19.791552
53.663586	1431.278619	19.796570
53.326440	1435.263669	19.801587
53.620650	1428.908870	19.806605
53.859054	1437.499740	19.811623
53.693612	1433.094723	19.816640
53.772426	1433.530477	19.821658
53.621308	1436.539607	19.826675
54.079215	1429.808855	19.831693
53.662232	1432.143247	19.836711
54.091584	1429.709008	19.841728
54.026541	1429.252086	19.846746
53.726473	1432.057327	19.851763
54.127906	1420.696237	19.856781
54.095124	1428.802555	19.861799
54.276645	1439.560982	19.866816
54.252755	1450.367377	19.871834
54.025890	1449.629685	19.876851
54.656027	1448.931296	19.881869
54.924907	1448.854416	19.886887
54.381130	1452.975989	19.891904
54.621050	1449.148109	19.896922
54.389640	1448.004015	19.901939
54.393523	1447.116557	19.906957
54.419200	1447.772082	19.911975
54.527570	1445.965663	19.916992
54.743865	1451.192645	19.922010
54.572814	1464.723568	19.927027
54.772771	1462.722910	19.932045
54.721369	1467.206016	19.937063
54.810539	1464.534725	19.942080
54.805449	1468.682360	19.947098
55.190876	1471.200319	19.952115
55.131273	1467.649745	19.957133
55.250150	1477.158798	19.962151
55.388408	1465.507542	19.967168
55.543660	1466.388928	19.972186
55.448800	1482.139161	19.977203
55.749470	1479.194881	19.982221
55.521471	1484.242165	19.987239
55.582162	1489.771259	19.992256
55.801312	1491.851353	19.997274
56.032008	1491.752052	20.002291
56.390681	1488.034951	20.007309
56.219937	1477.476709	20.012327
55.928248	1465.971713	20.017344
55.997507	1461.192234	20.022362
55.725157	1460.196570	20.027379
55.729812	1470.780748	20.032397
55.605892	1489.170731	20.037415
55.830356	1486.383562	20.042432
56.134509	1493.225247	20.047450
55.985543	1493.100220	20.052467
56.366255	1484.888790	20.057485
56.035954	1486.269145	20.062503
55.972482	1503.579815	20.067520
56.356215	1505.223855	20.072538
56.266823	1514.304793	20.077555
56.580422	1516.234388	20.082573
56.792993	1505.653945	20.087591
56.927728	1515.242588	20.092608
56.862834	1510.537765	20.097626
56.927142	1508.832920	20.102643
56.967593	1495.518017	20.107661
57.101584	1502.433704	20.112679
57.071906	1510.732084	20.117696
57.425842	1503.689377	20.122714
56.876516	1506.410601	20.127731
57.073667	1507.787217	20.132749
57.195131	1507.320007	20.137767
56.804136	1522.324535	20.142784
57.382884	1518.367812	20.147802
57.524769	1531.474201	20.152819
57.762801	1517.134208	20.157837
57.836334	1512.344579	20.162855
57.719979	1511.012035	20.167872
57.625698	1516.000506	20.172890
57.803227	1517.676854	20.177907
57.618683	1515.619663	20.182925
57.901430	1507.982170	20.187943
58.045722	1516.704593	20.192960
58.045525	1520.135078	20.197978
57.740628	1524.370725	20.202995
58.091644	1513.673908	20.208013
57.745664	1521.759908	20.213031
58.134114	1514.083761	20.218048
58.310067	1514.220263	20.223066
58.083233	1531.761691	20.228083
58.195740	1532.034372	20.233101
58.231760	1535.904171	20.238119
58.273619	1529.910778	20.243136
58.372442	1534.291466	20.248154
58.363520	1547.276322	20.253171
58.482149	1537.972950	20.258189
58.845345	1528.738568	20.263207
58.313321	1530.671259	20.268224
58.811828	1541.029775	20.273242
58.617870	1551.503101	20.278259
59.385070	1548.892832	20.283277
59.029922	1555.465437	20.288295
58.859586	1553.263998	20.293312
59.244936	1561.181784	20.298330
58.937796	1560.403013	20.303347
59.350480	1537.445191	20.308365
59.175644	1552.030853	20.313383
59.038797	1550.603683	20.318400
59.152490	1547.865420	20.323418
59.148525	1554.884796	20.328435
59.338678	1545.292492	20.333453
59.104674	1557.968625	20.338471
59.368933	1567.360270	20.343488
59.532087	1566.634053	20.348506
59.764079	1574.408607	20.353523
60.227096	1566.130595	20.358541
59.828236	1566.442367	20.363559
59.600561	1572.751999	20.368576
59.883830	1572.186851	20.373594
59.885591	1575.437151	20.378611
59.882776	1570.766769	20.383629
59.993945	1582.678753	20.388647
60.292583	1595.549183	20.393664
60.286470	1596.089768	20.398682
60.343660	1597.526191	20.403699
60.699114	1591.619350	20.408717
60.857200	1589.830375	20.413735
60.462728	1595.446593	20.418752
60.420174	1589.378040	20.423770
60.673523	1593.598826	20.428787
60.612514	1589.764413	20.433805
60.894179	1589.527733	20.438823
60.412168	1586.810209	20.443840
60.758065	1585.828132	20.448858
60.624074	1591.488749	20.453875
61.094362	1590.117938	20.458893
60.838437	1601.711892	20.463911
61.287518	1614.801773	20.468928
61.375782	1599.437405	20.473946
61.170876	1614.835751	20.478963
61.198376	1600.856894	20.483981
61.231502	1598.566766	20.488999
61.352290	1605.967420	20.494016
61.543266	1597.829849	20.499034
61.757273	1604.982359	20.504051
61.833060	1600.381709	20.509069
61.858320	1599.951662	20.514087
61.623214	1611.517113	20.519104
61.878690	1598.790164	20.524122
61.809105	1598.554865	20.529139
61.809772	1606.233127	20.534157
61.951891	1605.330315	20.539175
62.182326	1612.063670	20.544192
62.293451	1630.467468	20.549210
61.782865	1625.355895	20.554227
61.910292	1618.837803	20.559245
62.478131	1619.231659	20.564263
62.344881	1628.530976	20.569280
62.768944	1621.669748	20.574298
62.570545	1623.411317	20.579315
62.365736	1616.951590	20.584333
62.873534	1614.940556	20.589351
62.312832	1627.257649	20.594368
62.611944	1616.354300	20.599386
62.695725	1629.589791	20.604403
62.846867	1631.554319	20.609421
63.114554	1644.985080	20.614439
62.661664	1645.898636	20.619456
63.208937	1642.293973	20.624474
62.761672	1650.736741	20.629491
63.302588	1647.363457	20.634509
63.317310	1643.791735	20.639527
62.981345	1638.122601	20.644544
63.485709	1631.138331	20.649562
63.218818	1635.207095	20.654579
63.305663	1630.153405	20.659597
63.482612	1640.789588	20.664615
63.493814	1638.174670	20.669632
63.695632	1636.845918	20.674650
63.922767	1636.845010	20.679667
63.738739	1633.635803	20.684685
64.067782	1644.393332	20.689703
63.963507	1659.226815	20.694720
64.485837	1648.111740	20.699738
64.172622	1646.769002	20.704755
63.914886	1639.354995	20.709773
64.121522	1650.371558	20.714791
64.096784	1654.443415	20.719808
64.445561	1648.887913	20.724826
64.518996	1658.915446	20.729843
64.399249	1653.903585	20.734861
64.547154	1659.144499	20.739879
64.174055	1664.252439	20.744896
64.506100	1650.336287	20.749914
64.477309	1649.816872	20.754931
64.401003	1658.539212	20.759949
64.650848	1665.831305	20.764967
64.843193	1673.634206	20.769984
65.010652	1673.699455	20.775002
65.108333	1681.223687	20.780019
65.128838	1678.462132	20.785037
65.299532	1662.986961	20.790055
65.089059	1678.840691	20.795072
64.921553	1681.637826	20.800090
64.886117	1682.350273	20.805107
65.173630	1687.291599	20.810125
65.420202	1698.462889	20.815143
65.549634	1709.709345	20.820160
65.679557	1702.259824	20.825178
65.602084	1706.380983	20.830195
65.488650	1702.930318	20.835213
65.713844	1699.669609	20.840231
65.724777	1700.687232	20.845248
65.693431	1693.218798	20.850266
65.793704	1705.804790	20.855283
66.176264	1721.038600	20.860301
66.312732	1718.426136	20.865319
65.547360	1727.878193	20.870336
65.899847	1722.375738	20.875354
65.767222	1716.655785	20.880371
66.447703	1733.253643	20.885389
66.603602	1731.045252	20.890407
66.807075	1744.552425	20.895424
66.916739	1739.851752	20.900442
66.983736	1736.723124	20.905459
66.842160	1737.912975	20.910477
66.696462	1732.621120	20.915495
67.057212	1738.235830	20.920512
67.169354	1726.550624	20.925530
67.325493	1736.988143	20.930547
67.050946	1743.873252	20.935565
67.462524	1738.743406	20.940583
67.066207	1732.016981	20.945600
67.703149	1723.771611	20.950618
67.809352	1734.422089	20.955635
67.476468	1725.564921	20.960653
67.416330	1714.326458	20.965671
66.950092	1722.816416	20.970688
67.101468	1716.638537	20.975706
67.304260	1725.746392	20.980723
67.500296	1735.028889	20.985741
67.385772	1735.144629	20.990759
67.266740	1750.359215	20.995776
67.509123	1755.083557	21.000794
67.456988	1760.384246	21.005811
67.436357	1761.255331	21.010829
67.958991	1767.905094	21.015847
68.038282	1785.430367	21.020864
68.020508	1777.707293	21.025882
68.272361	1775.764746	21.030899
68.095473	1776.193230	21.035917
68.495682	1777.370787	21.040935
68.341604	1781.049504	21.045952
68.791062	1776.775293	21.050970
68.742163	1770.054386	21.055987
68.313832	1788.833216	21.061005
69.140178	1797.442604	21.066023
69.030061	1792.795288	21.071040
69.053832	1788.411034	21.076058
69.103429	1794.797229	21.081075
69.077570	1798.121329	21.086093
69.159308	1796.562057	21.091111
69.269519	1795.891465	21.096128
69.414345	1792.251989	21.101146
69.599511	1790.736477	21.106163
69.370070	1793.726379	21.111181
69.606991	1787.932724	21.116199
69.104174	1784.101214	21.121216
69.383560	1788.343215	21.126234
69.941655	1797.171367	21.131251
69.776365	1812.920301	21.136269
70.112131	1814.521390	21.141287
70.172874	1814.300385	21.146304
70.273304	1812.706623	21.151322
69.949030	1808.812418	21.156339
70.065255	1814.146709	21.161357
70.201935	1807.062179	21.166375
70.041429	1813.774805	21.171392
70.133201	1808.048069	21.176410
70.389474	1814.663837	21.181427
70.623606	1809.650140	21.186445
70.599034	1797.916875	21.191463
70.304120	1797.937795	21.196480
70.565657	1822.194652	21.201498
70.598796	1828.312024	21.206515
70.647829	1832.410235	21.211533
70.707387	1825.170514	21.216551
70.812582	1828.663445	21.221568
70.881787	1829.018659	21.226586
71.055076	1828.316091	21.231603
71.168518	1836.977229	21.236621
71.427641	1844.510952	21.241639
71.434463	1851.724426	21.246656
71.967251	1844.063396	21.251674
71.717482	1836.487104	21.256691
71.503823	1842.693643	21.261709
71.866095	1843.574173	21.266727
71.817216	1842.786486	21.271744
71.982999	1845.575611	21.276762
72.105439	1842.002753	21.281779
71.701022	1857.539869	21.286797
72.228012	1843.978055	21.291815
71.967268	1851.520643	21.296832
72.122559	1844.988635	21.301850
72.002587	1846.070960	21.306867
72.111996	1845.299501	21.311885
72.107749	1836.343449	21.316903
72.005391	1848.188073	21.321920
71.834789	1845.320726	21.326938
72.268565	1848.418179	21.331955
72.074812	1861.334386	21.336973
72.593707	1871.219659	21.341991
72.592400	1868.227949	21.347008
72.544760	1864.003196	21.352026
72.876669	1867.353312	21.357043
72.844285	1888.421421	21.362061
72.670736	1886.431896	21.367079
72.677961	1884.622343	21.372096
72.586081	1883.831922	21.377114
73.137020	1890.240597	21.382131
73.479907	1906.850482	21.387149
73.449327	1914.814655	21.392167
73.594904	1918.216065	21.397184
73.457414	1913.251094	21.402202
74.021227	1905.013943	21.407219
73.828960	1916.235187	21.412237
73.936277	1911.007787	21.417255
74.056861	1907.735025	21.422272
73.848368	1910.219861	21.427290
74.102391	1908.434759	21.432307
74.299763	1904.922736	21.437325
74.242774	1903.388346	21.442343
74.374434	1908.057488	21.447360
74.316334	1898.819490	21.452378
74.401407	1908.308822	21.457395
74.229217	1906.265429	21.462413
74.360368	1908.750703	21.467431
74.572131	1904.627319	21.472448
74.450480	1904.583220	21.477466
74.703816	1909.722479	21.482483
74.915870	1930.948013	21.487501
75.102746	1922.501650	21.492519
74.923875	1922.614849	21.497536
75.059626	1922.088583	21.502554
75.077290	1922.129961	21.507571
75.186328	1917.195797	21.512589
75.162190	1913.768973	21.517607
75.340878	1915.082238	21.522624
75.251052	1917.652630	21.527642
75.457697	1929.209039	21.532659
75.481987	1943.315671	21.537677
75.735535	1946.646519	21.542695
76.118446	1942.758259	21.547712
75.626909	1949.838399	21.552730
76.027799	1951.394582	21.557747
75.491940	1947.132684	21.562765
76.148261	1941.803480	21.567783
75.895337	1943.190681	21.572800
75.787739	1947.158815	21.577818
76.173318	1954.262492	21.582835
76.075947	1969.679011	21.587853
76.103810	1960.954566	21.592871
76.616042	1966.794940	21.597888
76.024251	1968.541366	21.602906
76.245047	1957.987773	21.607923
76.281612	1982.863956	21.612941
76.626578	1976.333744	21.617959
76.693100	1972.454020	21.622976
76.628996	1987.281480	21.627994
76.809051	1976.794222	21.633011
77.186197	1985.934859	21.638029
77.282728	1996.628037	21.643047
77.543288	2002.798206	21.648064
77.556730	1990.904215	21.653082
77.827170	1981.583141	21.658099
77.351872	1984.346488	21.663117
77.233187	1980.820848	21.668135
77.649973	1989.219926	21.673152
77.579946	1997.647937	21.678170
78.029454	2008.257417	21.683187
77.896498	2003.714616	21.688205
77.982621	1996.167687	21.693223
77.858461	1997.402165	21.698240
77.668459	2000.565814	21.703258
77.841817	1990.347859	21.708275
78.111296	1994.581994	21.713293
78.211637	2004.804335	21.718311
78.282740	2015.987535	21.723328
78.583254	2011.080154	21.728346
78.373352	2018.722151	21.733363
78.342225	2016.467284	21.738381
78.542094	2023.549589	21.743399
78.699404	2010.963969	21.748416
78.932126	2022.020859	21.753434
79.052017	2021.635939	21.758451
79.059147	2039.119115	21.763469
79.409920	2046.487076	21.768487
79.259269	2036.035817	21.773504
79.028292	2033.963747	21.778522
79.621167	2045.213550	21.783539
79.503618	2046.456465	21.788557
79.425582	2034.832414	21.793575
79.395787	2038.128770	21.798592
79.406295	2037.972441	21.803610
79.627868	2033.235223	21.808627
79.724849	2053.914006	21.813645
80.183654	2054.691055	21.818663
79.780209	2064.301191	21.823680
80.159130	2067.662915	21.828698
80.486412	2057.032615	21.833715
80.384613	2053.876726	21.838733
80.393280	2051.318953	21.843751
80.421220	2047.135968	21.848768
80.327344	2052.784133	21.853786
80.605392	2050.878481	21.858803
80.462207	2056.120934	21.863821
80.175944	2063.244702	21.868839
80.984781	2074.003065	21.873856
80.534176	2088.187370	21.878874
80.849045	2089.899064	21.883891
81.015648	2090.529377	21.888909
81.459821	2084.403335	21.893927
81.086092	2079.074515	21.898944
81.132579	2079.414356	21.903962
81.157784	2073.656937	21.908979
81.224112	2082.442348	21.913997
81.413253	2091.779763	21.919015
81.767506	2092.090323	21.924032
81.869788	2101.422416	21.929050
81.698716	2102.891485	21.934067
81.672366	2104.312633	21.939085
81.837588	2103.545042	21.944103
82.068366	2098.225656	21.949120
81.939228	2103.860425	21.954138
82.036918	2097.088025	21.959155
82.385815	2118.784683	21.964173
82.211014	2116.504973	21.969191
82.484627	2113.552206	21.974208
82.149976	2121.406309	21.979226
82.539397	2111.567874	21.984243
82.138173	2117.687121	21.989261
82.044717	2119.825734	21.994279
82.135917	2131.368801	21.999296
82.555891	2144.192213	22.004314
82.769118	2138.973401	22.009331
82.995162	2147.285664	22.014349
82.888397	2160.570338	22.019367
83.065940	2166.961869	22.024384
83.091494	2171.606675	22.029402
83.205869	2156.648025	22.034419
83.219873	2162.730637	22.039437
83.566481	2164.465770	22.044455
83.410651	2158.070762	22.049472
83.495251	2160.831628	22.054490
84.181335	2177.984487	22.059507
84.234987	2180.857510	22.064525
84.317561	2180.948685	22.069543
84.450235	2174.211803	22.074560
84.390294	2181.669416	22.079578
84.767280	2174.515532	22.084595
84.348927	2152.349894	22.089613
84.232852	2173.579784	22.094631
84.774358	2179.182095	22.099648
84.453762	2181.327898	22.104666
84.763858	2180.540763	22.109683
84.967591	2175.427578	22.114701
84.791533	2175.338349	22.119719
85.148040	2161.869284	22.124736
85.044051	2163.943276	22.129754
84.997940	2166.683593	22.134771
85.067842	2164.801072	22.139789
84.907237	2169.872705	22.144807
85.603762	2173.411925	22.149824
85.523354	2194.699373	22.154842
85.566270	2184.681639	22.159859
85.629582	2200.887441	22.164877
85.557908	2195.422893	22.169895
85.803710	2195.598956	22.174912
85.747464	2193.423746	22.179930
85.445132	2192.653660	22.184947
85.555032	2200.946272	22.189965
85.649041	2214.344707	22.194983
86.001064	2212.834579	22.200000
85.957245	2221.129192	22.205018
86.263921	2221.103199	22.210035
86.420301	2228.530096	22.215053
86.337035	2238.030196	22.220071
86.609618	2234.162316	22.225088
86.488865	2242.443743	22.230106
86.309086	2239.442061	22.235123
86.584590	2246.910267	22.240141
86.782979	2266.468788	22.245159
87.232580	2264.665634	22.250176
86.851806	2268.067518	22.255194
87.046217	2259.834429	22.260211
87.041710	2258.973493	22.265229
86.919183	2264.932351	22.270247
87.286506	2277.221266	22.275264
87.550011	2283.933913	22.280282
87.708375	2289.315397	22.285299
87.648853	2289.744441	22.290317
87.712538	2287.171704	22.295335
88.219977	2289.856875	22.300352
87.579171	2290.743092	22.305370
88.182155	2294.208622	22.310387
88.360934	2307.104657	22.315405
88.305944	2301.350260	22.320423
88.505639	2294.183077	22.325440
88.356581	2305.287331	22.330458
88.738759	2303.879778	22.335475
88.727492	2298.503572	22.340493
88.657834	2301.702072	22.345511
88.857696	2304.233446	22.350528
88.841451	2304.011872	22.355546
88.741941	2301.392111	22.360563
89.057272	2291.107557	22.365581
88.939819	2307.834122	22.370599
89.317854	2307.670707	22.375616
89.826771	2313.704235	22.380634
89.683867	2321.784025	22.385651
89.657590	2325.938333	22.390669
89.784022	2315.793823	22.395687
90.118714	2321.961957	22.400704
89.555137	2324.928549	22.405722
89.795082	2323.382318	22.410739
90.087423	2314.370092	22.415757
89.533526	2316.542994	22.420775
90.030407	2305.778670	22.425792
89.712457	2312.326785	22.430810
89.994086	2330.392139	22.435827
90.334558	2335.353754	22.440845
90.225867	2336.686826	22.445863
90.098407	2337.356908	22.450880
90.427760	2348.761809	22.455898
91.055608	2360.356657	22.460915
90.854664	2351.229176	22.465933
90.876455	2361.479807	22.470951
91.216549	2350.979882	22.475968
91.058809	2362.906112	22.480986
90.852621	2358.715550	22.486003
91.029588	2360.085928	22.491021
91.224864	2373.500177	22.496039
91.510321	2377.618282	22.501056
91.737448	2380.476783	22.506074
91.543097	2371.073680	22.511091
91.535547	2365.094062	22.516109
92.033314	2372.202423	22.521127
92.160474	2374.584237	22.526144
92.270219	2374.125154	22.531162
92.180675	2379.637032	22.536179
92.401517	2389.304181	22.541197
92.267923	2401.703221	22.546215
92.593218	2398.502449	22.551232
92.414770	2391.760577	22.556250
92.450753	2392.304059	22.561267
93.118414	2388.424747	22.566285
92.970483	2389.691381	22.571303
93.017178	2383.539141	22.576320
92.913888	2384.846122	22.581338
93.141130	2383.529114	22.586355
93.037826	2379.849493	22.591373
93.189924	2410.685782	22.596391
93.517322	2409.473011	22.601408
93.372266	2412.351955	22.606426
93.654348	2411.809062	22.611443
93.442607	2408.581964	22.616461
93.797781	2411.470906	22.621479
93.870853	2408.375926	22.626496
93.954153	2407.131966	22.631514
93.897585	2406.023537	22.636531
94.317845	2414.166629	22.641549
93.870174	2428.609540	22.646567
94.186251	2429.336379	22.651584
94.486477	2431.672150	22.656602
94.349615	2430.330125	22.661619
94.718659	2425.866372	22.666637
94.391680	2430.178279	22.671655
94.523594	2427.004644	22.676672
94.599485	2432.039298	22.681690
94.489587	2446.880625	22.686707
94.771189	2454.985494	22.691725
94.739146	2455.836308	22.696743
95.163782	2452.137082	22.701760
95.115161	2469.818777	22.706778
95.288898	2474.348919	22.711795
95.363998	2467.412646	22.716813
95.197127	2479.450846	22.721831
95.472870	2483.693586	22.726848
95.539319	2471.222874	22.731866
95.249536	2489.504156	22.736883
96.051402	2494.488212	22.741901
96.174519	2505.493138	22.746919
96.157535	2500.452314	22.751936
96.143383	2495.616195	22.756954
96.217873	2495.131072	22.761971
96.294271	2499.581788	22.766989
96.445681	2521.982125	22.772007
96.832935	2513.548277	22.777024
97.133364	2514.952977	22.782042
96.482488	2519.804846	22.787059
96.887572	2511.570196	22.792077
96.909603	2509.070231	22.797095
97.212897	2506.027536	22.802112
97.445186	2518.211529	22.807130
97.655116	2529.546885	22.812147
97.811776	2528.641750	22.817165
97.640693	2531.385922	22.822183
97.987327	2529.172801	22.827200
98.074827	2523.266609	22.832218
98.346105	2523.747983	22.837235
98.275786	2528.688796	22.842253
98.084091	2525.376477	22.847271
98.069404	2514.247167	22.852288
98.131377	2521.190313	22.857306
98.120162	2527.554736	22.862323
98.389671	2520.796286	22.867341
98.433594	2517.948875	22.872359
98.602655	2514.441170	22.877376
98.761434	2534.167150	22.882394
98.888582	2540.958068	22.887411
99.431604	2546.708596	22.892429
99.220156	2553.019184	22.897447
99.062256	2541.025428	22.902464
99.224986	2539.828979	22.907482
99.129682	2545.969876	22.912499
98.914649	2541.629163	22.917517
99.061395	2549.562680	22.922535
99.664370	2565.819975	22.927552
99.757688	2563.539230	22.932570
99.537088	2566.916074	22.937587
99.707324	2563.304024	22.942605
100.086599	2570.307941	22.947623
99.967728	2571.285984	22.952640
99.961532	2589.065302	22.957658
100.444793	2593.748973	22.962675
100.408550	2585.390909	22.967693
100.146557	2586.921604	22.972711
100.265246	2592.063218	22.977728
100.569287	2595.219003	22.982746
100.599405	2598.105249	22.987763
101.109741	2601.257120	22.992781
101.050834	2616.453551	22.997799
101.042943	2612.863086	23.002816
101.111312	2604.879983	23.007834
100.668679	2619.887202	23.012851
101.345252	2617.878025	23.017869
101.284966	2627.617752	23.022887
101.950972	2620.064926	23.027904
101.866195	2627.132100	23.032922
101.687802	2629.119962	23.037939
101.634581	2626.221474	23.042957
101.528003	2629.933952	23.047975
101.913683	2624.350278	23.052992
102.246750	2635.306611	23.058010
102.003791	2648.818130	23.063027
101.934069	2645.199472	23.068045
102.222171	2650.677516	23.073063
102.322134	2658.586850	23.078080
102.746346	2662.919992	23.083098
102.712217	2674.773408	23.088115
103.201874	2679.273044	23.093133
103.226590	2679.196543	23.098151
103.494892	2669.102197	23.103168
103.112617	2668.931653	23.108186
103.253631	2671.153530	23.113203
103.441177	2663.022328	23.118221
103.178004	2675.337706	23.123239
103.411271	2690.491581	23.128256
104.000080	2685.055963	23.133274
103.937104	2691.848319	23.138291
103.881210	2681.489146	23.143309
103.943106	2701.609224	23.148327
104.094735	2692.634636	23.153344
104.088704	2686.922943	23.158362
104.250220	2714.204473	23.163379
104.086293	2703.584472	23.168397
104.206249	2719.750307	23.173415
104.255620	2714.440224	23.178432
104.590290	2735.114114	23.183450
104.808307	2745.018608	23.188467
105.216926	2730.496272	23.193485
105.046221	2730.333609	23.198503
104.758838	2734.181744	23.203520
104.931002	2745.078137	23.208538
105.110216	2753.293867	23.213555
105.449110	2751.861500	23.218573
105.543346	2759.276260	23.223591
105.562320	2777.834545	23.228608
106.018390	2780.792957	23.233626
105.975893	2780.884793	23.238643
105.944565	2770.379693	23.243661
106.205544	2768.962688	23.248679
106.128747	2777.461560	23.253696
106.153758	2764.949795	23.258714
106.756144	2786.380307	23.263731
106.934891	2792.866558	23.268749
106.917920	2789.930803	23.273767
107.202483	2790.763593	23.278784
107.229018	2790.251257	23.283802
107.169800	2793.580767	23.288819
107.402817	2792.275450	23.293837
106.729568	2790.253644	23.298855
107.152775	2790.960560	23.303872
107.107257	2787.382267	23.308890
107.239299	2802.006081	23.313907
107.825980	2807.895038	23.318925
107.793916	2811.131924	23.323943
107.873471	2814.187204	23.328960
107.872038	2804.081388	23.333978
107.845385	2808.772412	23.338995
108.267983	2819.560180	23.344013
108.394779	2833.256932	23.349031
108.343516	2832.523229	23.354048
108.561258	2833.382270	23.359066
108.472869	2837.527490	23.364083
108.666868	2835.284592	23.369101
108.839846	2837.409954	23.374119
108.503450	2842.471442	23.379136
108.788460	2841.880737	23.384154
108.857559	2859.657994	23.389171
109.082134	2859.338717	23.394189
109.247817	2863.781848	23.399207
108.992913	2860.716082	23.404224
109.308226	2878.284350	23.409242
109.756556	2885.429068	23.414259
109.669945	2879.827780	23.419277
109.970332	2875.595606	23.424295
109.738836	2871.816033	23.429312
109.922999	2882.417107	23.434330
110.085142	2905.895650	23.439347
110.246392	2901.915668	23.444365
110.569070	2891.844241	23.449383
110.358871	2899.795962	23.454400
110.456397	2904.691644	23.459418
110.686497	2913.069908	23.464435
111.081856	2918.048336	23.469453
111.062002	2918.423837	23.474471
111.211544	2920.893747	23.479488
111.243296	2906.319847	23.484506
111.216362	2912.958299	23.489523
111.683862	2925.421336	23.494541
111.751933	2931.704045	23.499559
111.482950	2935.978579	23.504576
112.077212	2926.410602	23.509594
111.966796	2937.468163	23.514611
112.137745	2927.647732	23.519629
111.787913	2930.539902	23.524647
112.278023	2942.292425	23.529664
112.585333	2949.730694	23.534682
112.418907	2952.736162	23.539699
112.423827	2944.974312	23.544717
112.824459	2948.698920	23.549735
112.435711	2957.912705	23.554752
112.841992	2963.681636	23.559770
112.934540	2985.687781	23.564787
113.356548	2974.092091	23.569805
113.415345	2981.206346	23.574823
113.232685	2983.166510	23.579840
113.448791	2975.248470	23.584858
113.734315	2986.026252	23.589875
114.196657	2996.331316	23.594893
113.863516	2989.528236	23.599911
114.376046	2994.339988	23.604928
114.125604	2984.364612	23.609946
114.364109	2984.159930	23.614963
114.362006	2981.692086	23.619981
114.820630	2982.254589	23.624999
114.707704	2986.160662	23.630016
114.582681	2989.178586	23.635034
114.029034	2983.344286	23.640051
114.757484	3004.578562	23.645069
115.273711	3006.164115	23.650087
114.971782	3006.413376	23.655104
115.397808	3008.243462	23.660122
115.131643	3017.649536	23.665139
115.341845	3018.875886	23.670157
115.625780	3023.549869	23.675175
115.894859	3031.148814	23.680192
115.624053	3033.081763	23.685210
115.722321	3038.419232	23.690227
115.648466	3035.691189	23.695245
115.907482	3036.947767	23.700263
115.593837	3053.049273	23.705280
116.381048	3052.723908	23.710298
116.269144	3055.010707	23.715315
116.447634	3054.771240	23.720333
116.757697	3055.221304	23.725351
116.667977	3066.824879	23.730368
117.269192	3070.922082	23.735386
117.432317	3070.142156	23.740403
117.162321	3082.402068	23.745421
117.537282	3073.559580	23.750439
117.526741	3078.680550	23.755456
117.522591	3066.539263	23.760474
117.446247	3071.133986	23.765491
117.402145	3068.454933	23.770509
118.050545	3089.291545	23.775527
117.917177	3098.323362	23.780544
118.076857	3095.789125	23.785562
118.097125	3097.569167	23.790579
117.791274	3096.900588	23.795597
118.158793	3101.769806	23.800615
118.365984	3109.984472	23.805632
118.700299	3111.781594	23.810650
118.944326	3120.823733	23.815667
118.506042	3124.168504	23.820685
118.884163	3128.007144	23.825703
119.051138	3135.113981	23.830720
119.198400	3140.661584	23.835738
119.122988	3147.020503	23.840755
119.453206	3157.974446	23.845773
119.632847	3168.674240	23.850791
119.379481	3171.683896	23.855808
119.567212	3168.122640	23.860826
119.883418	3180.527496	23.865843
120.259003	3193.819424	23.870861
120.415886	3195.284544	23.875879
120.396553	3195.789374	23.880896
120.376967	3181.538917	23.885914
120.383895	3194.522480	23.890931
120.497911	3197.294679	23.895949
120.883733	3202.817552	23.900967
121.068026	3218.623414	23.905984
121.548235	3213.725432	23.911002
121.675084	3211.006950	23.916019
121.273913	3202.336494	23.921037
122.005823	3203.367498	23.926055
121.874806	3209.504746	23.931072
122.070450	3208.909093	23.936090
121.972188	3222.436246	23.941107
122.009630	3227.972676	23.946125
122.336647	3223.991903	23.951143
122.158321	3223.565307	23.956160
122.370779	3220.508319	23.961178
122.718497	3228.066622	23.966195
122.654114	3236.488017	23.971213
122.675395	3215.640927	23.976231
122.304438	3231.180293	23.981248
122.703766	3241.823619	23.986266
122.625335	3247.602300	23.991283
122.665089	3256.518698	23.996301
123.089563	3259.567360	24.001319
122.940287	3266.786919	24.006336
123.569959	3270.257933	24.011354
123.457732	3291.112946	24.016371
123.256758	3299.691487	24.021389
124.076868	3306.531942	24.026407
123.618234	3296.330198	24.031424
123.905218	3307.527724	24.036442
124.391314	3319.795591	24.041459
124.287819	3326.815471	24.046477
124.542034	3318.058063	24.051495
124.298968	3327.564835	24.056512
124.481860	3332.412541	24.061530
124.933836	3334.898252	24.066547
125.000040	3348.020983	24.071565
125.684723	3337.119315	24.076583
125.587789	3343.822549	24.081600
125.299160	3340.812483	24.086618
125.570250	3333.958796	24.091635
125.425200	3336.029886	24.096653
125.635747	3342.353542	24.101671
125.465908	3360.168726	24.106688
125.767656	3352.518011	24.111706
126.244078	3355.751082	24.116723
126.278953	3355.108018	24.121741
126.771026	3368.669045	24.126759
126.743473	3372.697544	24.131776
126.565566	3383.166262	24.136794
126.982654	3381.150316	24.141811
127.015870	3380.090886	24.146829
127.274936	3380.637324	24.151847
127.191260	3380.997583	24.156864
127.023153	3381.257444	24.161882
127.417642	3384.736920	24.166899
127.405495	3394.671519	24.171917
127.780849	3398.103495	24.176935
128.042121	3399.258745	24.181952
127.723215	3407.268750	24.186970
127.875096	3400.711465	24.191987
127.496065	3419.354858	24.197005
127.900906	3411.631153	24.202023
127.713840	3429.846794	24.207040
128.060209	3440.337565	24.212058
128.604912	3446.312218	24.217075
128.367034	3461.016616	24.222093
128.709353	3463.705744	24.227111
129.262464	3462.473327	24.232128
129.170401	3461.780708	24.237146
129.187686	3469.741227	24.242163
129.688387	3479.724934	24.247181
129.954661	3483.155077	24.252199
129.850419	3487.927872	24.257216
130.175621	3471.060276	24.262234
130.026165	3474.252548	24.267251
130.227949	3477.617043	24.272269
130.519554	3473.723828	24.277287
130.518372	3491.613720	24.282304
130.588674	3495.049318	24.287322
130.910342	3493.471249	24.292339
130.954726	3499.536928	24.297357
131.042714	3504.210173	24.302375
131.052177	3502.412732	24.307392
130.946380	3498.872148	24.312410
131.165811	3512.416028	24.317427
131.371632	3520.198687	24.322445
131.465824	3512.252168	24.327463
131.603694	3517.924454	24.332480
131.839198	3533.586850	24.337498
131.715556	3544.495352	24.342515
132.047444	3548.098293	24.347533
132.340934	3542.787597	24.352551
132.472048	3543.294117	24.357568
132.354403	3544.982183	24.362586
132.849313	3561.014280	24.367603
132.704636	3564.250006	24.372621
132.777298	3566.810957	24.377639
133.005523	3569.921981	24.382656
132.996148	3564.706072	24.387674
132.736565	3563.780878	24.392691
133.618280	3574.516111	24.397709
133.759854	3585.591402	24.402727
133.620077	3583.937273	24.407744
133.759726	3584.773868	24.412762
134.278083	3590.209815	24.417779
134.087602	3588.345845	24.422797
133.821397	3585.398506	24.427815
134.126344	3600.409355	24.432832
134.292935	3603.507947	24.437850
134.361714	3606.255733	24.442867
134.290486	3617.579011	24.447885
134.927056	3624.836568	24.452903
135.125898	3624.382435	24.457920
135.059373	3625.232394	24.462938
134.986774	3622.642942	24.467955
135.646392	3641.770883	24.472973
135.401399	3652.755275	24.477991
135.596323	3657.575934	24.483008
135.577128	3656.736171	24.488026
136.101770	3643.634201	24.493043
136.214947	3662.835148	24.498061
136.540468	3669.368160	24.503079
137.013224	3668.246165	24.508096
136.613956	3672.462375	24.513114
137.125382	3659.968473	24.518131
136.773844	3670.663407	24.523149
137.223849	3671.173629	24.528167
136.933919	3671.263201	24.533184
136.967678	3679.047634	24.538202
137.178506	3677.682606	24.543219
137.691343	3681.796954	24.548237
137.572936	3689.592606	24.553255
137.638013	3692.489332	24.558272
137.913205	3708.634891	24.563290
138.202959	3715.296619	24.568307
138.063084	3720.021400	24.573325
138.069743	3715.080690	24.578343
138.317422	3713.028123	24.583360
138.672088	3725.856588	24.588378
138.659508	3724.595996	24.593395
138.999973	3742.025447	24.598413
139.064792	3736.043505	24.603431
139.010338	3737.406057	24.608448
139.143116	3753.059487	24.613466
139.448280	3751.108381	24.618483
139.986582	3745.506767	24.623501
139.983188	3744.980156	24.628519
139.798375	3757.066206	24.633536
139.833952	3754.065248	24.638554
140.245511	3761.351800	24.643571
140.034479	3768.982087	24.648589
140.238669	3772.466202	24.653607
140.674108	3774.373803	24.658624
140.279686	3783.399514	24.663642
140.810330	3789.275483	24.668659
140.689543	3794.142483	24.673677
140.907780	3797.823251	24.678695
141.026904	3806.736955	24.683712
141.116599	3819.749034	24.688730
141.623872	3821.134061	24.693747
141.455941	3833.719375	24.698765
141.870499	3836.829661	24.703783
141.776318	3835.345120	24.708800
141.923842	3841.259032	24.713818
142.382982	3835.906518	24.718835
142.134356	3842.930397	24.723853
142.507543	3850.863733	24.728871
142.614150	3871.577816	24.733888
142.603762	3861.232929	24.738906
142.629473	3867.396347	24.743923
142.659426	3872.334443	24.748941
143.236329	3883.272277	24.753959
143.339913	3889.003709	24.758976
143.306566	3885.189722	24.763994
143.868744	3882.134649	24.769011
143.641470	3885.092989	24.774029
143.989046	3890.880887	24.779047
144.053347	3900.245115	24.784064
143.896109	3906.809656	24.789082
144.312243	3904.964246	24.794099
144.496503	3918.217245	24.799117
144.542975	3922.568843	24.804135
144.601017	3925.343611	24.809152
144.513902	3929.362627	24.814170
144.955387	3940.760444	24.819187
145.222299	3951.178740	24.824205
145.496814	3949.592239	24.829223
145.747157	3945.541258	24.834240
145.666569	3952.624074	24.839258
146.150575	3953.495116	24.844275
146.094783	3968.521754	24.849293
146.300401	3961.053130	24.854311
146.628026	3956.794344	24.859328
146.826699	3964.603566	24.864346
146.675536	3960.189375	24.869363
146.720305	3969.654546	24.874381
146.895124	3961.016583	24.879399
147.219871	3980.238380	24.884416
146.809962	3988.187144	24.889434
147.351948	3974.725550	24.894451
147.419894	3978.723441	24.899469
147.422989	3993.611464	24.904487
147.888459	3999.324112	24.909504
147.898943	4008.295969	24.914522
148.110330	4003.701871	24.919539
147.878745	4016.767581	24.924557
148.302728	4025.930332	24.929575
148.532052	4029.016013	24.934592
148.560745	4029.431277	24.939610
148.829406	4032.839058	24.944627
148.720650	4053.770159	24.949645
149.099452	4048.897312	24.954663
149.286078	4037.893341	24.959680
149.362573	4059.593988	24.964698
149.506961	4061.544062	24.969715
149.516505	4076.986664	24.974733
149.904405	4078.046369	24.979751
150.144019	4078.491718	24.984768
149.714971	4078.909254	24.989786
149.883150	4093.591582	24.994803
150.266458	4092.309976	24.999821
150.219747	4097.926139	25.004839
150.862574	4103.560534	25.009856
150.383014	4119.281805	25.014874
150.741757	4113.862873	25.019891
151.018107	4128.477781	25.024909
151.309885	4139.993869	25.029927
151.426659	4134.941102	25.034944
151.475030	4146.492172	25.039962
151.465199	4150.833706	25.044979
151.799631	4163.829786	25.049997
151.529275	4169.881871	25.055015
152.105181	4163.759747	25.060032
152.358866	4176.632761	25.065050
152.390946	4181.270751	25.070067
152.680426	4187.033126	25.075085
152.696292	4187.589284	25.080103
153.191248	4189.225626	25.085120
153.125905	4209.155841	25.090138
153.209944	4202.640459	25.095155
153.442031	4205.870932	25.100173
153.526897	4208.164925	25.105191
153.795175	4201.892130	25.110208
154.080175	4221.101472	25.115226
154.102695	4223.935510	25.120243
154.448777	4229.228197	25.125261
154.470561	4225.528600	25.130279
154.735673	4218.542949	25.135296
154.644788	4221.767208	25.140314
154.901050	4229.172972	25.145331
155.186357	4254.284773	25.150349
155.093810	4243.112935	25.155367
155.579115	4248.371191	25.160384
155.523988	4245.090816	25.165402
155.551087	4250.723871	25.170419
155.441099	4260.768966	25.175437
155.332896	4273.222127	25.180455
155.734314	4278.761828	25.185472
155.750773	4291.583709	25.190490
155.683955	4304.320798	25.195507
156.369185	4308.452474	25.200525
156.207805	4316.450825	25.205543
156.526629	4323.849983	25.210560
156.824245	4343.777142	25.215578
156.992492	4346.594682	25.220595
157.561833	4348.190978	25.225613
157.582301	4339.971569	25.230631
157.968303	4352.442053	25.235648
158.325750	4361.599616	25.240666
158.608045	4364.989543	25.245683
158.680862	4362.348796	25.250701
158.218756	4368.102718	25.255719
158.598411	4357.718537	25.260736
158.718423	4358.902295	25.265754
159.001957	4354.476722	25.270771
159.043059	4373.740218	25.275789
159.106819	4386.437969	25.280807
159.180853	4386.700942	25.285824
159.260560	4375.085389	25.290842
159.733673	4384.145933	25.295859
160.150140	4392.489377	25.300877
159.939792	4405.324776	25.305895
160.371015	4404.225028	25.310912
160.140393	4403.484638	25.315930
160.223139	4406.716449	25.320947
160.468176	4402.959746	25.325965
160.638147	4431.691350	25.330983
161.135031	4415.209476	25.336000
160.794686	4428.731265	25.341018
161.242626	4426.760877	25.346035
161.292901	4424.477173	25.351053
161.507890	4438.757894	25.356071
161.299523	4441.650232	25.361088
161.571501	4449.350330	25.366106
161.913063	4462.216094	25.371123
162.133295	4465.691517	25.376141
162.255234	4471.246655	25.381159
162.452759	4478.822702	25.386176
162.479481	4481.368885	25.391194
162.543664	4481.800695	25.396211
162.885661	4485.045564	25.401229
162.891193	4493.781704	25.406247
163.084727	4502.829291	25.411264
163.552577	4503.753396	25.416282
163.197395	4501.567923	25.421299
163.398684	4517.419608	25.426317
163.788401	4528.140957	25.431335
164.200982	4526.977837	25.436352
164.286149	4531.774892	25.441370
164.663873	4531.043354	25.446387
164.781019	4544.051654	25.451405
164.590020	4551.808544	25.456423
165.075069	4550.583567	25.461440
165.105171	4562.276647	25.466458
164.636643	4553.300444	25.471475
164.931772	4569.794016	25.476493
165.405189	4579.451182	25.481511
165.606351	4576.023276	25.486528
165.754663	4588.512222	25.491546
165.922330	4598.163637	25.496563
166.075378	4598.834045	25.501581
165.784858	4612.505988	25.506599
166.387415	4615.836320	25.511616
166.402020	4618.810544	25.516634
166.651392	4628.392359	25.521651
167.053770	4636.012135	25.526669
167.192040	4646.596184	25.531687
167.455838	4642.700765	25.536704
167.378699	4658.457307	25.541722
167.429585	4663.919471	25.546739
168.069102	4671.274845	25.551757
168.087643	4695.523140	25.556775
168.224038	4695.340754	25.561792
168.277046	4702.431342	25.566810
168.680181	4700.537387	25.571827
168.550601	4699.894788	25.576845
169.053633	4721.014897	25.581863
169.174808	4709.743004	25.586880
169.131268	4716.482570	25.591898
169.356932	4730.572460	25.596915
169.761135	4735.726775	25.601933
169.942032	4738.248841	25.606951
170.170046	4740.166949	25.611968
170.220893	4750.726878	25.616986
170.210315	4763.499668	25.622003
170.473198	4759.307657	25.627021
170.444515	4765.265260	25.632039
170.854316	4773.215363	25.637056
171.152045	4786.451222	25.642074
170.969115	4787.133237	25.647091
171.464907	4788.583273	25.652109
171.485148	4794.804680	25.657127
171.783824	4789.814774	25.662144
171.731732	4809.172244	25.667162
171.715125	4807.205151	25.672180
172.061828	4812.816719	25.677197
172.176434	4825.150126	25.682215
172.245991	4823.807146	25.687232
172.420022	4829.177468	25.692250
172.886614	4850.492828	25.697268
172.997753	4850.970951	25.702285
172.697193	4857.583539	25.707303
173.395087	4875.267427	25.712320
173.354031	4875.330638	25.717338
173.161816	4882.191409	25.722356
173.602599	4891.714969	25.727373
173.990035	4904.905295	25.732391
174.019826	4900.569847	25.737408
174.361066	4913.912617	25.742426
174.355954	4919.061665	25.747444
174.620335	4919.894565	25.752461
174.696248	4925.059331	25.757479
174.963860	4942.491883	25.762496
175.133231	4959.321164	25.767514
175.237834	4954.295329	25.772532
175.400993	4950.986943	25.777549
175.518193	4965.930487	25.782567
175.747094	4973.665966	25.787584
176.199547	4974.914476	25.792602
176.159041	4981.347482	25.797620
176.393526	4984.751329	25.802637
176.119785	4998.357801	25.807655
176.499084	5009.898611	25.812672
176.666811	5018.167678	25.817690
176.713140	5029.867986	25.822708
177.092644	5029.148778	25.827725
177.362609	5050.211087	25.832743
177.415108	5054.268454	25.837760
177.918591	5067.595390	25.842778
177.933820	5070.818957	25.847796
178.420775	5066.705409	25.852813
178.414282	5080.169065	25.857831
178.748933	5078.626709	25.862848
179.227851	5087.708794	25.867866
178.972620	5088.948230	25.872884
179.317671	5092.552578	25.877901
179.710218	5104.514351	25.882919
180.083701	5103.038511	25.887936
180.516656	5101.878479	25.892954
180.218356	5103.733878	25.897972
180.494942	5093.731587	25.902989
180.621593	5097.572171	25.908007
180.599393	5093.017550	25.913024
180.981726	5095.091444	25.918042
181.034157	5108.362810	25.923060
181.080661	5112.774663	25.928077
181.270837	5131.141243	25.933095
181.203868	5125.798175	25.938112
181.569271	5123.938499	25.943130
181.587945	5148.566164	25.948148
182.098546	5144.155334	25.953165
182.197176	5153.862053	25.958183
182.096187	5164.455478	25.963200
182.281546	5174.091802	25.968218
182.460830	5175.487288	25.973236
182.464863	5179.003033	25.978253
182.399155	5193.451429	25.983271
182.827066	5194.489153	25.988288
182.997108	5208.281940	25.993306
182.940559	5224.057842	25.998324
183.286986	5230.263020	26.003341
183.816449	5240.669338	26.008359
184.200896	5240.236596	26.013376
184.936266	5249.146011	26.018394
184.667304	5256.905944	26.023412
185.017658	5256.544832	26.028429
184.873710	5250.342571	26.033447
184.798167	5260.117668	26.038464
185.312541	5264.194264	26.043482
185.438411	5280.708686	26.048500
185.375239	5281.435090	26.053517
185.630953	5294.081307	26.058535
185.948269	5302.143987	26.063552
186.068705	5307.317668	26.068570
186.140988	5313.559509	26.073588
186.189131	5318.435174	26.078605
186.687249	5321.507379	26.083623
186.794231	5328.072074	26.088640
186.855329	5329.672327	26.093658
187.030833	5340.771786	26.098676
187.313542	5349.187133	26.103693
187.258261	5345.982341	26.108711
187.499077	5358.425759	26.113728
187.718045	5368.334702	26.118746
187.760005	5375.433596	26.123764
188.106114	5379.514483	26.128781
188.381315	5396.542238	26.133799
188.694052	5404.911872	26.138816
188.917655	5409.289739	26.143834
189.024972	5421.807776	26.148852
189.227738	5410.311175	26.153869
189.560521	5431.869143	26.158887
189.889271	5440.567728	26.163904
189.824858	5441.957221	26.168922
189.661711	5454.072568	26.173940
190.048579	5459.820094	26.178957
190.095259	5473.496674	26.183975
190.267875	5473.507474	26.188992
190.642657	5484.424284	26.194010
191.163461	5503.433899	26.199028
191.064057	5495.579976	26.204045
191.341338	5513.049441	26.209063
191.077697	5511.537646	26.214080
191.670441	5522.912767	26.219098
191.707716	5542.692631	26.224116
192.139673	5536.106485	26.229133
192.572382	5555.994872	26.234151
192.383328	5567.599823	26.239168
192.776401	5560.202192	26.244186
192.921982	5575.422730	26.249204
193.255748	5575.701851	26.254221
193.318815	5589.170769	26.259239
193.248156	5597.925688	26.264256
193.821728	5603.669264	26.269274
193.859940	5613.246801	26.274292
193.889557	5607.771664	26.279309
194.322037	5616.700302	26.284327
194.055526	5637.790516	26.289344
194.560561	5636.571811	26.294362
194.440490	5658.945960	26.299380
194.910977	5658.916409	26.304397
195.279740	5669.932130	26.309415
195.641883	5676.782113	26.314432
195.787533	5678.523826	26.319450
195.804473	5685.374229	26.324468
195.802129	5710.400527	26.329485
196.472878	5703.322354	26.334503
196.435604	5704.991713	26.339520
196.580348	5716.875915	26.344538
196.657114	5732.312548	26.349556
197.000580	5738.082745	26.354573
197.190509	5742.560668	26.359591
197.591134	5755.313928	26.364608
197.610472	5756.302054	26.369626
197.968031	5760.371764	26.374644
198.134865	5771.747475	26.379661
198.040270	5780.430470	26.384679
198.221960	5781.314247	26.389696
198.670509	5791.547315	26.394714
198.872597	5803.956067	26.399732
198.890373	5799.953739	26.404749
199.129901	5815.431234	26.409767
199.518530	5826.557578	26.414784
199.750974	5826.094975	26.419802
199.767494	5825.457857	26.424820
200.064768	5822.614432	26.429837
200.284606	5849.070811	26.434855
200.360145	5851.057120	26.439872
200.671885	5847.684259	26.444890
200.830426	5853.442426	26.449908
200.940209	5865.527916	26.454925
201.558894	5854.982332	26.459943
201.415666	5854.360768	26.464960
201.584179	5857.045922	26.469978
201.432753	5880.937306	26.474996
201.948838	5890.013972	26.480013
202.399434	5890.830375	26.485031
202.431234	5895.939192	26.490048
202.630008	5903.026353	26.495066
202.639604	5907.696716	26.500084
202.454531	5910.465680	26.505101
202.865344	5927.639992	26.510119
202.890803	5943.507838	26.515136
203.543936	5944.377745	26.520154
203.587653	5952.988648	26.525172
204.059678	5960.714871	26.530189
204.215402	5974.248475	26.535207
204.165540	5987.637521	26.540224
204.944660	5989.396824	26.545242
204.921816	5989.324604	26.550260
205.170217	6002.022967	26.555277
205.565501	6006.699225	26.560295
205.504544	6019.212466	26.565312
205.741256	6019.197442	26.570330
205.857623	6025.808270	26.575348
206.013428	6040.251044	26.580365
206.267619	6044.573766	26.585383
206.336562	6048.436218	26.590400
206.808916	6064.489854	26.595418
207.040139	6070.116749	26.600436
207.118172	6067.118229	26.605453
207.214792	6080.550686	26.610471
207.728024	6107.750659	26.615488
207.591546	6104.725760	26.620506
207.758316	6114.753773	26.625524
207.841321	6126.158620	26.630541
208.426481	6133.160086	26.635559
208.598740	6146.306106	26.640576
208.863849	6148.448997	26.645594
209.177602	6152.825548	26.650612
209.217064	6163.968918	26.655629
209.514944	6160.370887	26.660647
209.590233	6169.696682	26.665664
210.000480	6183.547279	26.670682
210.092304	6195.042334	26.675700
209.919284	6200.173853	26.680717
210.791537	6199.169066	26.685735
210.822803	6213.038019	26.690752
210.985186	6218.817797	26.695770
211.075360	6222.294994	26.700788
211.234712	6244.600831	26.705805
211.864013	6235.316067	26.710823
211.746730	6249.422978	26.715840
211.933946	6256.366876	26.720858
211.958170	6273.213795	26.725876
212.450009	6275.526371	26.730893
213.034869	6273.546971	26.735911
212.959774	6283.152080	26.740928
212.815202	6278.366949	26.745946
213.206781	6285.787082	26.750964
213.206554	6301.135241	26.755981
213.503259	6302.673415	26.760999
213.121219	6314.930953	26.766016
213.677383	6327.634994	26.771034
214.012399	6335.632225	26.776052
214.106265	6352.657714	26.781069
214.655457	6359.661746	26.786087
214.809865	6367.942983	26.791104
215.209041	6384.311415	26.796122
215.375944	6384.689298	26.801140
214.879324	6394.587787	26.806157
215.505553	6404.070464	26.811175
215.621305	6409.788159	26.816192
215.694151	6429.771757	26.821210
216.053978	6434.715694	26.826228
216.211680	6452.428924	26.831245
216.731606	6456.040876	26.836263
216.565966	6478.435792	26.841280
217.144629	6479.266885	26.846298
217.308448	6493.077403	26.851316
217.578257	6502.076156	26.856333
217.768043	6497.484819	26.861351
217.825423	6527.045504	26.866368
217.475995	6535.143732	26.871386
217.813849	6550.293924	26.876404
218.298559	6570.525678	26.881421
219.313736	6581.263905	26.886439
219.338888	6591.986765	26.891456
219.637053	6600.236117	26.896474
219.868227	6610.052275	26.901492
220.159283	6610.095033	26.906509
220.609693	6605.178727	26.911527
220.542251	6621.898271	26.916544
220.552876	6633.482084	26.921562
220.772840	6634.536689	26.926580
221.145319	6651.357811	26.931597
221.591103	6645.233158	26.936615
221.567821	6664.616492	26.941632
221.847116	6672.382681	26.946650
222.138947	6674.941306	26.951668
222.069538	6680.640740	26.956685
222.313825	6689.438390	26.961703
222.530906	6700.535320	26.966720
222.666361	6707.010817	26.971738
222.960121	6712.760701	26.976756
223.349338	6728.152384	26.981773
223.432635	6724.890915	26.986791
223.291842	6743.715041	26.991808
223.442809	6744.796246	26.996826
223.980563	6761.490559	27.001844
224.249374	6780.834570	27.006861
224.672264	6789.755818	27.011879
224.980888	6813.841521	27.016896
225.073011	6808.094216	27.021914
225.475411	6825.321201	27.026932
225.307556	6840.812875	27.031949
225.535052	6839.416595	27.036967
225.579829	6853.179739	27.041984
226.130435	6854.220443	27.047002
226.235946	6879.793362	27.052020
226.091328	6887.468209	27.057037
226.503813	6899.907883	27.062055
226.743841	6913.605760	27.067072
226.794977	6921.486720	27.072090
227.387029	6936.610038	27.077108
227.505078	6958.894803	27.082125
227.910634	6952.305977	27.087143
227.972617	6973.096871	27.092160
228.385469	6977.761157	27.097178
228.982895	6983.002652	27.102196
229.040726	6987.747812	27.107213
229.252056	6995.837318	27.112231
229.258121	7005.651071	27.117248
229.294706	6999.918720	27.122266
229.895162	7014.055839	27.127284
229.877904	7021.174120	27.132301
230.181504	7028.627279	27.137319
230.444001	7050.580152	27.142336
230.381200	7057.156282	27.147354
230.887613	7053.484372	27.152372
230.935459	7064.317600	27.157389
231.426665	7064.152220	27.162407
231.437088	7088.316568	27.167424
231.843566	7094.213072	27.172442
231.833730	7103.789445	27.177460
231.978616	7116.192265	27.182477
232.127890	7119.392038	27.187495
232.537703	7144.892401	27.192512
232.841857	7149.750547	27.197530
233.363813	7160.503247	27.202548
233.282905	7179.154277	27.207565
233.648008	7186.856733	27.212583
234.185541	7200.419825	27.217600
234.308006	7195.939882	27.222618
234.825517	7210.677334	27.227636
234.763343	7230.521952	27.232653
234.973679	7225.447364	27.237671
235.285653	7237.101156	27.242688
235.300889	7251.642672	27.247706
235.596753	7251.088021	27.252724
235.610191	7271.148137	27.257741
235.846255	7270.795426	27.262759
236.232368	7286.895217	27.267776
236.529914	7302.633221	27.272794
236.729706	7298.999826	27.277812
237.002601	7321.961612	27.282829
237.408639	7325.130669	27.287847
237.396689	7346.624936	27.292864
237.631791	7348.201265	27.297882
238.080906	7359.628450	27.302900
238.138503	7380.227918	27.307917
238.304243	7379.554743	27.312935
238.627603	7398.991883	27.317952
238.719200	7409.689026	27.322970
239.257614	7418.744018	27.327988
239.236702	7425.054847	27.333005
239.479557	7445.091841	27.338023
239.578885	7455.920392	27.343040
240.079071	7466.035820	27.348058
240.252550	7480.432762	27.353076
240.608736	7491.258980	27.358093
240.857402	7491.987130	27.363111
241.414332	7499.694394	27.368128
241.694526	7523.239328	27.373146
241.832905	7519.621824	27.378164
241.759736	7526.206059	27.383181
241.846164	7529.302098	27.388199
242.458279	7540.069311	27.393216
242.785185	7563.537525	27.398234
243.455216	7561.434158	27.403252
243.123332	7571.730503	27.408269
243.252175	7568.603815	27.413287
243.959914	7591.696708	27.418304
243.569602	7581.926976	27.423322
244.276400	7598.999666	27.428340
244.506692	7620.039582	27.433357
244.756862	7612.859252	27.438375
244.812364	7621.203905	27.443392
244.544579	7635.518559	27.448410
245.169982	7651.126577	27.453428
245.101145	7661.220758	27.458445
245.632010	7670.030811	27.463463
245.856261	7663.211262	27.468480
245.841406	7693.719610	27.473498
246.190362	7695.316017	27.478516
246.245210	7710.524131	27.483533
246.408969	7723.438995	27.488551
246.889559	7742.236253	27.493568
246.946136	7762.103881	27.498586
247.252370	7765.841128	27.503604
247.320888	7785.536432	27.508621
247.763760	7789.845797	27.513639
248.554937	7824.461651	27.518656
248.638139	7828.890510	27.523674
249.284132	7839.018030	27.528692
249.546005	7846.039233	27.533709
249.468986	7857.328158	27.538727
249.784491	7861.970038	27.543744
249.642663	7867.873762	27.548762
250.351202	7869.764286	27.553780
250.690190	7891.952429	27.558797
250.628283	7894.806577	27.563815
250.983058	7897.598607	27.568832
250.877093	7912.519532	27.573850
251.478912	7921.081814	27.578868
251.574647	7933.982226	27.583885
252.116159	7941.616324	27.588903
252.464934	7950.859140	27.593920
252.325998	7971.909943	27.598938
252.817478	7971.094164	27.603956
252.763557	7989.375568	27.608973
253.284844	7988.760328	27.613991
253.533805	8003.887762	27.619008
253.753661	8021.899003	27.624026
253.669149	8022.322621	27.629044
254.110866	8045.419874	27.634061
254.351588	8048.188752	27.639079
255.088469	8064.351088	27.644096
255.362868	8071.970257	27.649114
255.964995	8088.917733	27.654132
256.093094	8087.723199	27.659149
255.880151	8083.323999	27.664167
256.226592	8088.706158	27.669184
256.350162	8099.989065	27.674202
256.656235	8111.767463	27.679220
256.986781	8118.181326	27.684237
257.382571	8128.900690	27.689255
257.490122	8123.731461	27.694272
257.765139	8147.426386	27.699290
258.000161	8150.496095	27.704308
257.885552	8169.027122	27.709325
257.811674	8186.418393	27.714343
258.577625	8191.251832	27.719360
258.730913	8202.700629	27.724378
259.158884	8210.804089	27.729396
259.469173	8231.677475	27.734413
259.915507	8245.141973	27.739431
259.723198	8245.822422	27.744448
260.034888	8258.556633	27.749466
260.249505	8268.903509	27.754484
260.230562	8286.437809	27.759501
260.571218	8303.192817	27.764519
261.098929	8310.920788	27.769536
261.179790	8328.587877	27.774554
261.785509	8335.823758	27.779572
262.088589	8350.617817	27.784589
262.524165	8364.674468	27.789607
262.760755	8360.561534	27.794624
263.257206	8362.889447	27.799642
263.308260	8366.471050	27.804660
263.462599	8386.080938	27.809677
263.734759	8380.472268	27.814695
264.194924	8390.221937	27.819712
264.137936	8401.173401	27.824730
264.261121	8401.274037	27.829748
264.375407	8409.559324	27.834765
264.622464	8427.241515	27.839783
264.852488	8439.897089	27.844800
264.805896	8448.428594	27.849818
265.269750	8463.835298	27.854836
265.421057	8486.309285	27.859853
265.793761	8502.008128	27.864871
266.682016	8505.622781	27.869888
266.804433	8512.817628	27.874906
267.156016	8516.074353	27.879924
267.535492	8531.693232	27.884941
268.063641	8551.191066	27.889959
268.553063	8543.464598	27.894976
268.006344	8552.873253	27.899994
268.610831	8552.364936	27.905012
268.742259	8571.233523	27.910029
268.935085	8577.969051	27.915047
269.496254	8586.765328	27.920064
269.644165	8604.074891	27.925082
269.942755	8612.066197	27.930100
270.269758	8617.707287	27.935117
270.498107	8625.823259	27.940135
270.917810	8630.007010	27.945152
270.728121	8642.943158	27.950170
271.186077	8653.725705	27.955188
271.300914	8658.781239	27.960205
271.325903	8668.352968	27.965223
271.688359	8682.566545	27.970240
271.615822	8697.050334	27.975258
272.364316	8710.846700	27.980276
272.604022	8727.658952	27.985293
272.641175	8733.838002	27.990311
272.953847	8757.897201	27.995328
273.223344	8776.015060	28.000346
273.807436	8784.495280	28.005364
273.929211	8805.802966	28.010381
274.102795	8823.260257	28.015399
274.776159	8831.379224	28.020416
274.776375	8850.117104	28.025434
275.035339	8846.793015	28.030452
275.417853	8863.418845	28.035469
275.552121	8881.532733	28.040487
276.309430	8893.114657	28.045504
276.325640	8904.433816	28.050522
276.605346	8917.953323	28.055540
277.049425	8936.864865	28.060557
276.784389	8949.652012	28.065575
277.734519	8962.722394	28.070592
277.430509	8979.961026	28.075610
277.890532	8978.098783	28.080628
278.349202	8988.985603	28.085645
278.407797	8998.002881	28.090663
278.859916	9007.037448	28.095680
278.946086	9034.185523	28.100698
279.477670	9042.178404	28.105716
279.910748	9043.581793	28.110733
279.658516	9051.476456	28.115751
280.480541	9060.563607	28.120768
280.772827	9069.661130	28.125786
280.716778	9079.365740	28.130804
281.238845	9091.660289	28.135821
281.475240	9093.324971	28.140839
281.618345	9093.772944	28.145856
281.652024	9112.673181	28.150874
281.925630	9126.657911	28.155892
282.453192	9130.319722	28.160909
282.276524	9145.606327	28.165927
282.867735	9155.717901	28.170944
283.227889	9175.009075	28.175962
283.123491	9186.334670	28.180980
283.722632	9204.947515	28.185997
283.886000	9223.413949	28.191015
284.162662	9238.130768	28.196032
284.416007	9254.401470	28.201050
284.724502	9266.344404	28.206068
285.143509	9273.480457	28.211085
285.384622	9290.716073	28.216103
285.601965	9298.875110	28.221120
285.847782	9308.627271	28.226138
286.265553	9327.000282	28.231156
286.872087	9331.701137	28.236173
286.491322	9366.752895	28.241191
286.861273	9364.967870	28.246208
287.479747	9390.018734	28.251226
287.800769	9394.224433	28.256244
288.092938	9416.611180	28.261261
288.367212	9429.279443	28.266279
288.894760	9434.501021	28.271296
288.878151	9449.930139	28.276314
289.320677	9448.717838	28.281332
289.807500	9466.811801	28.286349
289.679774	9476.073195	28.291367
290.435510	9488.565044	28.296384
290.871130	9505.018952	28.301402
290.554540	9509.772897	28.306420
290.999064	9524.015310	28.311437
291.317933	9540.872731	28.316455
291.464031	9545.393182	28.321472
292.179059	9559.833206	28.326490
292.227524	9578.649510	28.331508
292.442624	9590.670430	28.336525
292.436559	9604.879298	28.341543
292.549824	9623.148752	28.346560
293.168563	9643.861749	28.351578
293.958111	9653.497344	28.356596
294.248964	9664.006712	28.361613
294.474908	9691.733746	28.366631
294.879993	9686.590094	28.371648
295.029367	9697.383702	28.376666
295.141816	9714.081017	28.381684
295.757264	9726.651837	28.386701
295.931747	9737.226835	28.391719
296.440461	9740.418121	28.396736
296.403002	9759.513285	28.401754
296.258994	9765.648438	28.406772
296.603823	9766.071144	28.411789
296.983889	9802.213804	28.416807
297.523092	9810.881500	28.421824
297.971855	9830.996176	28.426842
298.116500	9835.441149	28.431860
298.696444	9856.008908	28.436877
298.640400	9870.393148	28.441895
298.882032	9880.645130	28.446912
299.234979	9886.636171	28.451930
299.670934	9909.727184	28.456948
299.972350	9902.973664	28.461965
300.290035	9913.895744	28.466983
300.706879	9926.924057	28.472000
300.853839	9935.931105	28.477018
301.040468	9954.700887	28.482036
301.522312	9948.626341	28.487053
301.456431	9969.011227	28.492071
301.738173	9976.825792	28.497088
302.285010	9988.201415	28.502106
302.388246	10002.396622	28.507124
302.521590	10018.554181	28.512141
302.854225	10032.489301	28.517159
303.012393	10047.503176	28.522176
303.480816	10064.650227	28.527194
303.591377	10083.851990	28.532212
304.111467	10096.384322	28.537229
304.337090	10112.600128	28.542247
304.573016	10131.501292	28.547264
305.083682	10146.434770	28.552282
305.399299	10164.287851	28.557300
305.904595	10179.708439	28.562317
305.734148	10201.742346	28.567335
306.511146	10218.847518	28.572352
306.706872	10232.898958	28.577370
306.600401	10244.500216	28.582388
307.444535	10253.625544	28.587405
307.747289	10272.854229	28.592423
308.275551	10289.152236	28.597440
308.392137	10304.431741	28.602458
308.521165	10316.621328	28.607476
308.991434	10330.958210	28.612493
309.330438	10347.778476	28.617511
309.646987	10367.415567	28.622528
310.063315	10378.312996	28.627546
309.928783	10389.836646	28.632564
310.255533	10410.226816	28.637581
310.902221	10439.054157	28.642599
311.464699	10440.570002	28.647616
311.517671	10458.720264	28.652634
311.692514	10470.100777	28.657652
312.191799	10488.174839	28.662669
312.248994	10507.707460	28.667687
312.866092	10512.817437	28.672704
313.084493	10540.935286	28.677722
313.183074	10552.485670	28.682740
313.841410	10569.148760	28.687757
313.853056	10591.100924	28.692775
314.251303	10593.305582	28.697792
314.678890	10611.621491	28.702810
314.668427	10635.695850	28.707828
315.483901	10649.006393	28.712845
315.509298	10667.176963	28.717863
315.807644	10667.468044	28.722880
316.388369	10691.926651	28.727898
316.794573	10704.297257	28.732916
317.158328	10719.939388	28.737933
317.276507	10728.626104	28.742951
317.552950	10740.676048	28.747968
318.173957	10745.697068	28.752986
318.421663	10768.212391	28.758004
318.554878	10775.463259	28.763021
319.309146	10792.193617	28.768039
319.500641	10795.286376	28.773056
319.675239	10809.736250	28.778074
320.129221	10820.590150	28.783092
320.241010	10827.102375	28.788109
320.493240	10839.291950	28.793127
320.559405	10854.567173	28.798144
320.991149	10860.110447	28.803162
320.964192	10885.548609	28.808180
321.472092	10894.562733	28.813197
321.889666	10908.576772	28.818215
321.779256	10923.980753	28.823232
322.555032	10933.622335	28.828250
322.680582	10949.797708	28.833268
322.963055	10962.200496	28.838285
323.368474	10971.682241	28.843303
324.023767	10996.852648	28.848320
324.270720	11002.939594	28.853338
324.233324	11016.131393	28.858356
325.055550	11032.049302	28.863373
325.211535	11037.149560	28.868391
325.654919	11058.327348	28.873408
325.991060	11070.036608	28.878426
326.078611	11082.719459	28.883444
326.599930	11088.431909	28.888461
326.599944	11106.726870	28.893479
327.139242	11118.154889	28.898496
327.568425	11135.476426	28.903514
327.675131	11144.468261	28.908532
328.253244	11156.275449	28.913549
328.225461	11186.782077	28.918567
328.450229	11192.158944	28.923584
329.089360	11207.164721	28.928602
329.305533	11238.921518	28.933620
329.469326	11244.229012	28.938637
329.800883	11272.387072	28.943655
330.119607	11288.598787	28.948672
330.650267	11305.358320	28.953690
330.913998	11335.178529	28.958708
331.162299	11346.923827	28.963725
331.593477	11365.400953	28.968743
332.082321	11385.874156	28.973760
332.382842	11400.247924	28.978778
332.343191	11426.067723	28.983796
332.773491	11440.964307	28.988813
332.783621	11462.320935	28.993831
333.348788	11490.647976	28.998848
333.970161	11493.973490	29.003866
334.209359	11512.392419	29.008884
334.887692	11531.737239	29.013901
335.504546	11554.154632	29.018919
335.246414	11560.024059	29.023936
336.025949	11574.228197	29.028954
336.418722	11600.510986	29.033972
336.627961	11607.901836	29.038989
336.920882	11628.942797	29.044007
337.308579	11649.353191	29.049024
337.867294	11654.921022	29.054042
338.058213	11671.813043	29.059060
338.347954	11681.480625	29.064077
338.810871	11698.491105	29.069095
338.861873	11713.118921	29.074112
339.174909	11731.122316	29.079130
339.598362	11743.503539	29.084148
339.914010	11748.591612	29.089165
340.315242	11767.591687	29.094183
340.819897	11781.065407	29.099200
341.549448	11786.502314	29.104218
341.395052	11808.001941	29.109236
341.799892	11814.875949	29.114253
341.826783	11824.297428	29.119271
342.442550	11846.371153	29.124288
343.396572	11858.738813	29.129306
343.564182	11876.739866	29.134324
343.812154	11874.856884	29.139341
344.193758	11877.133775	29.144359
344.521653	11900.061030	29.149376
344.775400	11890.478642	29.154394
344.756500	11902.360874	29.159412
344.810238	11913.657032	29.164429
345.404895	11925.181079	29.169447
345.600210	11942.915766	29.174464
346.008834	11946.085225	29.179482
346.227661	11977.280782	29.184500
346.298533	11990.001593	29.189517
347.007078	12004.791886	29.194535
346.964457	12022.440767	29.199552
347.566050	12031.649176	29.204570
347.946313	12050.728608	29.209588
348.291990	12076.788927	29.214605
348.702381	12083.491646	29.219623
348.557902	12116.992656	29.224640
349.467550	12127.337014	29.229658
349.537910	12154.548936	29.234676
350.008972	12162.164244	29.239693
349.920083	12182.798286	29.244711
350.489038	12205.792360	29.249728
350.828426	12224.136296	29.254746
351.218445	12249.151003	29.259764
351.650496	12270.038263	29.264781
352.156736	12292.802277	29.269799
352.350006	12307.373534	29.274816
353.011479	12322.313552	29.279834
353.065617	12345.211603	29.284852
353.684074	12369.887539	29.289869
354.152648	12378.441189	29.294887
354.639995	12409.936443	29.299904
354.646473	12423.425505	29.304922
354.845124	12434.721380	29.309940
355.374699	12451.226327	29.314957
355.760636	12477.372470	29.319975
356.258386	12504.101119	29.324992
357.169264	12512.702387	29.330010
357.174609	12526.321170	29.335028
357.396877	12547.882636	29.340045
357.904094	12559.319722	29.345063
358.050345	12579.882629	29.350080
358.479163	12594.871939	29.355098
358.791408	12619.226703	29.360116
358.995653	12627.038729	29.365133
359.356935	12649.930089	29.370151
359.739696	12671.330770	29.375168
359.936244	12682.996591	29.380186
360.228789	12708.071385	29.385204
360.728212	12728.699132	29.390221
361.284359	12754.291636	29.395239
361.821163	12769.842059	29.400256
362.363579	12775.453832	29.405274
362.315958	12803.951472	29.410292
362.448418	12812.349551	29.415309
363.240256	12829.319007	29.420327
363.453419	12851.580136	29.425344
364.034249	12861.594306	29.430362
364.154912	12888.458357	29.435380
364.605907	12897.596047	29.440397
365.161216	12916.980516	29.445415
365.332080	12938.345218	29.450432
365.490981	12951.788676	29.455450
365.809383	12976.038725	29.460468
366.139251	12996.380693	29.465485
366.372191	13015.430495	29.470503
367.056766	13030.222196	29.475520
367.369569	13053.491114	29.480538
367.771544	13064.926046	29.485556
367.604706	13086.476445	29.490573
368.669029	13093.528676	29.495591
368.681861	13116.115181	29.500608
369.282566	13127.452706	29.505626
369.747696	13148.743131	29.510644
369.811577	13163.066893	29.515661
370.306488	13186.572716	29.520679
370.461835	13205.208544	29.525696
370.834133	13212.741855	29.530714
371.499621	13230.258840	29.535732
371.973166	13256.960769	29.540749
372.392300	13270.647906	29.545767
372.653055	13290.941015	29.550784
373.074816	13291.042284	29.555802
373.457095	13307.264734	29.560820
373.817757	13316.492569	29.565837
374.477689	13335.737921	29.570855
374.624395	13357.770051	29.575872
375.479901	13356.735991	29.580890
375.625565	13382.778917	29.585908
375.546308	13384.768176	29.590925
376.100910	13394.729897	29.595943
375.948035	13418.053260	29.600960
376.857795	13437.632223	29.605978
376.966978	13456.907124	29.610996
377.263959	13483.425445	29.616013
378.170155	13498.602812	29.621031
378.256025	13521.967855	29.626048
378.586672	13534.810073	29.631066
378.664528	13550.903569	29.636084
379.541006	13582.352459	29.641101
379.752394	13591.528019	29.646119
379.604984	13617.809812	29.651136
380.196918	13636.927170	29.656154
380.815518	13660.003668	29.661172
381.177128	13682.754118	29.666189
381.810168	13703.463058	29.671207
381.745155	13729.972108	29.676224
382.190771	13736.913070	29.681242
382.777109	13766.383423	29.686260
383.093543	13784.154554	29.691277
383.737306	13808.013639	29.696295
383.790040	13829.252581	29.701312
384.962303	13846.131786	29.706330
385.019930	13869.129033	29.711348
385.341937	13878.754795	29.716365
385.752530	13895.049107	29.721383
385.862506	13921.085730	29.726400
386.477037	13940.367232	29.731418
386.699673	13956.349969	29.736436
387.057898	13969.004995	29.741453
387.766378	13993.643692	29.746471
388.019770	14008.614234	29.751488
388.498348	14034.956453	29.756506
388.848157	14040.080854	29.761524
389.173428	14054.948590	29.766541
389.707591	14070.598400	29.771559
390.232887	14094.151121	29.776576
390.354846	14115.682715	29.781594
390.939653	14121.117718	29.786612
391.404323	14146.644327	29.791629
392.009945	14154.921516	29.796647
392.386843	14169.800204	29.801664
392.561620	14182.964137	29.806682
392.870332	14196.119733	29.811700
392.981379	14222.374509	29.816717
393.679371	14225.066375	29.821735
393.745295	14246.439515	29.826752
394.473741	14256.421834	29.831770
394.503811	14272.757126	29.836788
394.792244	14296.119816	29.841805
395.185311	14306.890534	29.846823
395.294298	14338.552484	29.851840
395.863582	14350.053573	29.856858
396.305110	14374.642995	29.861876
396.923716	14396.532935	29.866893
397.323750	14412.191405	29.871911
397.470313	14443.313918	29.876928
397.480440	14452.290876	29.881946
398.073551	14469.810875	29.886964
398.396027	14489.874530	29.891981
399.019147	14501.894689	29.896999
399.485435	14526.363578	29.902016
400.024719	14555.346698	29.907034
400.421427	14568.264540	29.912052
400.729721	14591.261293	29.917069
401.086358	14609.712221	29.922087
401.738018	14636.716644	29.927104
401.724655	14662.530421	29.932122
402.486417	14682.692855	29.937140
402.732906	14705.096215	29.942157
403.231181	14723.547175	29.947175
403.550855	14756.929610	29.952192
403.921135	14772.905698	29.957210
404.584092	14796.576688	29.962228
404.574242	14816.007413	29.967245
405.491420	14831.721029	29.972263
405.285609	14865.309132	29.977280
405.692401	14882.880803	29.982298
406.474734	14910.676807	29.987316
406.412840	14931.789655	29.992333
407.498857	14958.537007	29.997351
407.549414	14982.863157	30.002368
407.865985	15012.203997	30.007386
408.286002	15025.573284	30.012404
408.698632	15064.620198	30.017421
409.257349	15073.176746	30.022439
409.846850	15101.625406	30.027456
410.116672	15123.349738	30.032474
410.709519	15142.117907	30.037492
410.909870	15172.156220	30.042509
411.575617	15190.085555	30.047527
412.059390	15216.207519	30.052544
412.443315	15241.915633	30.057562
413.203000	15250.712394	30.062580
413.254067	15269.960334	30.067597
413.844205	15289.035425	30.072615
414.371710	15309.806866	30.077632
414.672372	15325.023702	30.082650
415.142132	15343.482887	30.087668
415.514662	15365.055601	30.092685
415.864112	15367.792754	30.097703
416.222863	15389.986679	30.102720
416.892918	15413.875248	30.107738
417.541149	15418.558494	30.112756
417.378423	15451.471317	30.117773
418.063127	15466.596530	30.122791
418.402205	15483.244503	30.127808
418.576076	15511.528321	30.132826
419.052845	15525.397558	30.137844
419.339955	15546.140586	30.142861
419.860180	15557.555343	30.147879
420.137157	15595.999244	30.152896
420.431679	15615.818955	30.157914
420.983997	15635.961516	30.162932
421.402345	15662.776539	30.167949
421.810736	15673.586691	30.172967
422.289591	15690.784611	30.177984
422.723240	15715.866540	30.183002
423.337206	15719.418225	30.188020
423.640685	15747.846324	30.193037
424.419855	15755.395879	30.198055
424.585370	15769.399322	30.203072
425.058938	15788.846907	30.208090
425.235862	15794.358918	30.213108
425.603833	15814.612659	30.218125
426.413034	15837.592465	30.223143
426.560705	15854.362335	30.228160
427.035404	15876.475496	30.233178
427.367112	15888.867493	30.238196
427.414279	15917.421267	30.243213
428.156707	15941.397070	30.248231
428.533725	15963.452989	30.253248
428.883752	15989.461149	30.258266
429.175522	16004.976808	30.263284
429.545998	16032.636821	30.268301
429.843809	16060.661998	30.273319
430.686901	16086.242476	30.278336
431.102361	16111.394100	30.283354
431.689259	16136.635765	30.288372
432.287609	16162.712650	30.293389
432.656584	16184.621638	30.298407
432.907818	16205.955308	30.303424
433.357845	16226.556693	30.308442
433.905824	16246.902717	30.313460
434.121920	16278.004690	30.318477
434.720174	16299.584162	30.323495
434.976705	16312.683065	30.328512
435.496157	16343.693411	30.333530
436.088697	16368.157519	30.338548
436.368169	16389.047945	30.343565
437.158030	16408.036019	30.348583
437.702202	16449.702469	30.353600
437.549853	16467.817997	30.358618
438.386246	16492.540965	30.363636
438.647786	16519.795508	30.368653
439.313632	16536.440593	30.373671
439.531308	16558.838003	30.378688
439.898792	16585.254839	30.383706
440.699303	16609.487695	30.388724
440.668282	16638.544352	30.393741
441.347394	16658.822897	30.398759
442.108931	16676.767052	30.403776
442.348693	16691.564957	30.408794
443.156543	16723.806782	30.413812
443.384298	16740.596468	30.418829
444.277185	16759.941459	30.423847
444.478834	16777.196409	30.428864
444.806138	16806.159292	30.433882
445.607707	16811.640087	30.438900
445.815905	16836.329235	30.443917
446.211791	16853.866525	30.448935
446.684615	16872.134036	30.453952
447.208776	16891.012597	30.458970
447.798477	16903.266926	30.463988
447.595758	16924.381911	30.469005
448.278023	16936.053224	30.474023
449.296598	16956.613720	30.479040
448.859625	16976.217763	30.484058
449.668909	16996.668949	30.489076
449.759816	17032.058958	30.494093
450.689689	17050.412980	30.499111
450.949628	17067.646426	30.504128
451.494535	17087.182071	30.509146
451.764883	17099.211750	30.514164
451.715109	17125.783123	30.519181
452.125452	17140.519911	30.524199
452.903534	17172.937716	30.529216
453.040659	17188.386955	30.534234
453.931484	17206.175537	30.539252
454.231468	17238.061887	30.544269
454.514981	17245.793906	30.549287
455.114714	17270.962405	30.554304
455.653887	17305.414089	30.559322
456.128423	17313.034092	30.564340
456.510181	17345.400553	30.569357
456.881713	17368.494969	30.574375
457.065850	17388.725469	30.579392
457.643016	17418.199736	30.584410
458.278014	17444.070470	30.589428
458.840673	17468.992344	30.594445
459.287932	17498.891387	30.599463
460.081641	17516.366971	30.604480
460.146874	17536.395144	30.609498
460.475623	17551.618823	30.614516
460.775936	17585.862046	30.619533
461.085942	17613.337967	30.624551
462.301808	17644.279235	30.629568
462.350330	17669.717793	30.634586
463.234022	17687.318419	30.639604
463.810979	17723.666451	30.644621
463.929529	17738.430448	30.649639
464.776692	17764.306284	30.654656
465.163412	17783.576815	30.659674
465.605300	17799.654766	30.664692
466.108857	17832.047187	30.669709
466.355924	17859.242716	30.674727
467.248255	17880.563112	30.679744
467.667741	17901.250043	30.684762
468.050552	17914.235496	30.689780
468.321134	17946.373999	30.694797
468.834430	17965.504854	30.699815
469.373404	17984.183168	30.704832
470.064690	18009.622577	30.709850
470.422580	18032.682020	30.714868
470.665813	18055.367766	30.719885
470.791145	18079.247054	30.724903
471.609549	18107.098905	30.729920
471.848224	18143.822901	30.734938
472.531928	18155.144112	30.739956
472.647507	18189.764799	30.744973
473.023559	18210.515721	30.749991
473.761530	18238.424582	30.755008
474.259928	18273.907817	30.760026
474.913218	18299.239842	30.765044
475.599529	18327.826582	30.770061
476.174073	18357.315328	30.775079
476.673507	18374.913594	30.780096
477.045328	18405.211225	30.785114
477.530428	18416.835353	30.790132
477.954614	18440.573513	30.795149
478.244595	18458.754291	30.800167
478.984867	18479.536901	30.805184
479.141011	18514.094954	30.810202
479.937488	18533.687427	30.815220
480.541378	18564.182709	30.820237
480.816077	18586.415597	30.825255
480.971646	18607.795335	30.830272
481.727556	18631.330149	30.835290
482.215707	18651.634386	30.840308
482.434391	18691.154951	30.845325
482.829693	18704.884463	30.850343
483.362367	18717.208900	30.855360
483.652999	18743.729172	30.860378
484.208826	18754.451632	30.865396
485.067836	18783.125714	30.870413
485.658678	18819.429403	30.875431
485.774545	18829.753304	30.880448
486.260282	18851.056326	30.885466
486.888864	18863.435329	30.890484
487.509847	18883.314670	30.895501
488.003071	18909.759214	30.900519
488.605771	18932.206469	30.905536
488.834724	18961.257478	30.910554
489.692345	18985.907670	30.915572
490.145684	19007.860350	30.920589
489.938040	19029.758638	30.925607
490.777815	19045.194071	30.930624
491.350674	19081.355757	30.935642
491.373451	19099.269414	30.940660
492.215193	19130.676003	30.945677
492.481216	19152.329658	30.950695
493.420481	19181.200247	30.955712
493.870368	19207.083379	30.960730
494.441926	19229.182057	30.965748
494.820785	19259.593638	30.970765
494.897446	19284.815096	30.975783
495.987041	19316.347429	30.980800
496.654540	19343.573954	30.985818
496.876321	19372.873097	30.990836
497.173555	19389.012933	30.995853
497.595776	19418.697732	31.000871
498.461043	19433.270248	31.005888
498.381168	19469.117907	31.010906
499.400077	19487.419242	31.015924
499.877480	19524.177951	31.020941
500.035844	19545.779408	31.025959
500.910460	19578.678924	31.030976
501.408861	19613.235865	31.035994
501.506468	19634.859573	31.041012
502.234702	19661.078790	31.046029
502.895386	19693.209624	31.051047
503.990147	19720.066493	31.056064
504.074100	19751.889719	31.061082
504.502931	19764.749163	31.066100
505.176083	19791.425762	31.071117
505.458313	19817.493915	31.076135
505.927363	19841.473162	31.081152
506.256263	19867.894200	31.086170
506.559190	19887.009355	31.091188
507.226873	19931.484960	31.096205
507.625317	19962.779099	31.101223
508.187382	19992.613456	31.106240
508.615674	20022.184496	31.111258
509.260692	20051.468913	31.116276
509.421271	20082.345595	31.121293
510.158651	20126.273687	31.126311
510.904402	20140.202050	31.131328
511.330558	20171.492183	31.136346
511.754063	20202.738554	31.141364
512.606142	20226.279193	31.146381
512.752517	20258.403055	31.151399
513.273862	20285.426332	31.156416
514.103013	20323.603588	31.161434
514.445077	20348.968076	31.166452
515.288884	20369.610130	31.171469
515.796781	20390.386954	31.176487
516.264331	20417.418840	31.181504
516.740496	20456.744694	31.186522
516.886695	20473.825226	31.191540
517.933240	20496.097358	31.196557
518.127641	20519.242216	31.201575
518.529450	20541.931293	31.206592
519.286311	20557.880060	31.211610
519.744987	20579.574625	31.216628
520.200142	20606.172752	31.221645
520.448733	20634.749301	31.226663
521.135393	20650.355314	31.231680
521.284925	20694.364115	31.236698
521.922160	20712.562108	31.241716
522.779916	20743.880332	31.246733
522.598734	20779.101782	31.251751
523.349585	20807.745240	31.256768
524.404580	20841.212557	31.261786
525.019523	20859.091942	31.266804
525.854644	20891.424885	31.271821
526.084149	20907.488125	31.276839
526.362497	20927.480083	31.281856
526.986501	20962.335653	31.286874
527.226420	20986.453284	31.291892
527.864011	21009.541944	31.296909
528.542841	21048.350724	31.301927
529.508287	21080.846802	31.306944
529.737365	21104.618763	31.311962
530.176013	21139.465767	31.316980
531.022904	21166.274992	31.321997
531.422605	21191.738956	31.327015
532.205913	21218.008504	31.332032
532.439734	21251.554588	31.337050
532.988267	21268.598071	31.342068
533.506567	21300.115675	31.347085
533.942355	21321.448172	31.352103
534.360654	21351.016463	31.357120
535.059789	21382.208906	31.362138
534.953471	21422.999044	31.367156
536.025742	21439.802684	31.372173
536.792952	21477.555909	31.377191
537.007712	21504.951131	31.382208
537.694926	21525.347234	31.387226
538.537984	21566.096392	31.392244
538.946221	21593.132868	31.397261
539.269648	21626.128474	31.402279
540.115462	21650.253121	31.407296
540.692909	21673.484673	31.412314
541.343174	21709.613817	31.417332
541.862074	21722.220334	31.422349
542.424109	21766.230109	31.427367
542.858422	21780.069411	31.432384
543.422814	21811.454242	31.437402
543.825727	21844.241885	31.442420
544.747520	21863.432644	31.447437
544.845562	21883.377987	31.452455
545.410941	21915.584259	31.457472
545.880943	21949.416793	31.462490
546.476965	21984.739823	31.467508
546.808561	22014.259500	31.472525
547.452169	22042.138032	31.477543
548.245044	22063.529144	31.482560
548.246237	22109.226165	31.487578
548.856669	22137.141621	31.492596
549.495517	22155.726146	31.497613
550.016310	22204.387659	31.502631
550.764580	22236.060306	31.507648
551.001222	22265.727925	31.512666
551.719983	22296.305817	31.517684
552.497691	22326.672321	31.522701
553.096520	22361.989267	31.527719
553.957665	22384.463195	31.532736
554.245781	22403.406190	31.537754
554.688772	22427.974012	31.542772
555.435223	22446.207060	31.547789
555.634200	22485.744668	31.552807
556.328842	22498.911816	31.557824
556.873702	22536.278526	31.562842
557.185114	22561.486373	31.567860
558.148867	22586.111847	31.572877
558.233029	22609.870403	31.577895
558.963910	22644.080316	31.582912
559.302582	22672.974293	31.587930
559.611326	22710.801682	31.592948
560.480475	22739.581080	31.597965
560.726864	22777.165603	31.602983
561.119978	22812.724097	31.608000
562.089257	22850.088118	31.613018
562.445884	22885.235403	31.618036
563.461435	22911.805745	31.623053
564.171577	22950.518578	31.628071
564.547246	22979.470398	31.633088
565.417771	23009.823415	31.638106
565.893966	23037.577914	31.643124
566.798086	23062.377617	31.648141
567.240476	23092.058482	31.653159
567.976639	23118.129418	31.658176
568.695345	23153.871337	31.663194
568.941288	23179.747410	31.668212
569.646991	23198.922763	31.673229
569.869365	23235.564047	31.678247
570.724932	23261.003516	31.683264
571.378536	23291.308789	31.688282
571.676362	23322.769362	31.693300
572.343194	23342.033090	31.698317
572.928304	23377.954314	31.703335
573.550383	23403.708578	31.708352
574.236853	23428.858787	31.713370
574.792455	23447.204799	31.718388
575.528095	23478.875094	31.723405
576.239879	23509.689763	31.728423
576.623588	23530.742118	31.733440
577.324216	23568.042142	31.738458
577.595388	23583.070997	31.743476
578.401861	23608.765051	31.748493
578.913318	23647.162802	31.753511
579.206979	23671.357439	31.758528
579.998363	23696.643218	31.763546
580.678469	23735.210623	31.768564
581.564401	23753.302966	31.773581
581.518972	23794.031563	31.778599
582.421348	23824.823191	31.783616
583.403721	23847.349310	31.788634
583.810950	23869.112422	31.793652
584.338353	23893.624604	31.798669
584.747736	23909.586279	31.803687
585.587066	23950.303015	31.808704
586.083639	23973.998608	31.813722
586.619330	24002.705679	31.818740
587.356306	24030.085795	31.823757
587.939951	24052.769385	31.828775
588.383876	24070.495205	31.833792
589.002403	24092.971158	31.838810
589.406533	24131.228665	31.843828
589.915277	24149.007598	31.848845
590.558151	24181.862633	31.853863
591.053329	24206.020039	31.858880
591.439092	24244.640848	31.863898
592.121797	24276.383897	31.868916
592.628516	24296.514115	31.873933
593.099945	24324.738796	31.878951
594.058179	24351.357964	31.883968
594.750813	24373.961655	31.888986
595.150663	24405.610181	31.894004
595.695493	24422.511617	31.899021
596.235425	24449.638793	31.904039
596.462907	24488.329098	31.909056
597.035370	24504.543768	31.914074
597.458632	24547.589275	31.919092
598.346232	24576.842414	31.924109
598.916439	24611.276783	31.929127
599.171701	24644.920034	31.934144
600.050471	24676.013696	31.939162
600.417572	24723.106586	31.944180
601.557444	24751.625317	31.949197
601.953289	24785.322622	31.954215
602.582260	24817.176060	31.959232
603.685946	24848.967843	31.964250
604.097254	24884.919002	31.969268
604.717382	24916.925656	31.974285
605.004974	24942.639500	31.979303
605.532526	24986.876673	31.984320
606.515042	25012.570248	31.989338
606.732244	25045.310097	31.994356
607.407434	25071.007640	31.999373
607.733915	25109.911149	32.004391
608.919705	25155.404344	32.009408
609.611890	25188.006840	32.014426
610.052459	25228.599040	32.019444
610.881924	25255.245900	32.024461
611.366361	25287.084804	32.029479
611.909694	25309.428547	32.034496
612.655103	25345.612597	32.039514
613.212086	25386.464956	32.044532
613.918409	25418.003885	32.049549
614.559710	25462.091575	32.054567
615.120550	25492.673833	32.059584
615.622996	25518.051413	32.064602
616.168360	25557.547173	32.069620
616.821853	25585.827275	32.074637
618.184110	25623.735342	32.079655
618.393464	25660.857096	32.084672
619.009578	25686.431963	32.089690
619.381218	25725.165272	32.094708
620.039433	25757.508577	32.099725
620.926036	25789.399052	32.104743
621.238646	25817.568548	32.109760
622.024914	25851.301296	32.114778
622.922058	25893.163161	32.119796
623.539709	25921.259751	32.124813
623.754367	25956.561068	32.129831
624.468139	25986.766208	32.134848
625.101525	26017.862463	32.139866
625.479019	26055.615890	32.144884
626.288918	26089.212616	32.149901
626.922742	26136.140642	32.154919
627.663932	26158.195222	32.159936
628.591559	26182.596967	32.164954
628.674691	26236.525606	32.169972
629.346470	26255.506972	32.174989
630.030077	26292.574575	32.180007
630.392990	26338.319402	32.185024
631.534757	26369.835871	32.190042
631.757060	26417.265087	32.195060
632.147152	26439.697287	32.200077
633.300817	26482.329180	32.205095
634.073653	26514.560948	32.210112
634.734096	26541.267587	32.215130
635.290083	26568.622637	32.220148
635.649355	26594.915141	32.225165
636.566769	26628.691854	32.230183
636.939715	26658.679610	32.235200
637.492799	26671.302877	32.240218
638.339086	26709.287478	32.245236
638.818390	26736.553642	32.250253
639.352983	26762.837868	32.255271
639.652619	26800.750246	32.260288
640.740857	26827.699960	32.265306
641.186836	26877.105063	32.270324
641.733934	26906.433886	32.275341
642.560306	26944.687501	32.280359
642.656510	26982.549915	32.285376
643.559781	27016.854077	32.290394
644.220877	27061.586833	32.295412
644.658176	27099.256999	32.300429
645.476830	27134.990368	32.305447
646.463190	27180.601540	32.310464
647.087514	27210.278969	32.315482
647.760338	27259.624197	32.320500
648.225390	27294.465167	32.325517
649.050300	27329.490015	32.330535
649.455799	27375.982645	32.335552
650.087105	27408.200080	32.340570
650.893271	27452.045080	32.345588
651.513323	27495.647541	32.350605
652.521364	27532.426430	32.355623
653.192964	27570.345198	32.360640
653.835666	27596.278590	32.365658
654.192904	27646.407357	32.370676
655.094044	27688.082701	32.375693
655.824852	27726.201064	32.380711
656.182109	27773.732404	32.385728
657.104076	27803.528423	32.390746
657.643585	27833.788897	32.395764
658.602038	27882.894969	32.400781
659.364844	27914.846112	32.405799
659.613825	27956.086888	32.410816
660.564134	27977.187898	32.415834
661.184961	28019.306018	32.420852
661.832433	28059.517542	32.425869
662.581168	28087.097282	32.430887
663.203642	28144.132123	32.435904
663.903401	28165.203039	32.440922
664.419028	28209.227906	32.445940
665.277474	28248.186872	32.450957
665.869682	28283.136036	32.455975
666.618327	28319.919050	32.460992
667.401595	28352.758897	32.466010
667.873930	28394.970577	32.471028
668.369315	28432.830058	32.476045
669.425083	28462.327976	32.481063
670.106655	28505.474192	32.486080
670.687735	28532.309657	32.491098
671.324247	28579.950841	32.496116
672.029587	28610.685842	32.501133
673.166995	28641.795683	32.506151
673.594814	28668.592120	32.511168
674.802293	28704.305283	32.516186
675.322086	28725.929594	32.521204
675.635818	28756.751426	32.526221
676.588912	28785.715980	32.531239
676.835586	28822.843989	32.536256
677.794941	28849.361476	32.541274
678.259211	28877.568356	32.546292
678.551492	28909.127000	32.551309
679.305734	28943.166993	32.556327
679.884113	28973.107027	32.561344
680.521480	28999.833157	32.566362
681.281008	29027.172285	32.571380
681.650215	29065.033734	32.576397
682.526794	29088.227038	32.581415
682.942300	29136.694248	32.586432
683.853192	29162.998499	32.591450
684.344039	29195.676906	32.596468
684.943399	29245.563088	32.601485
685.434549	29275.928089	32.606503
686.621438	29321.070183	32.611520
687.416063	29361.981823	32.616538
688.110334	29398.705765	32.621556
688.536204	29438.246750	32.626573
689.528215	29467.876209	32.631591
689.680018	29510.646071	32.636608
690.989282	29536.553400	32.641626
691.413823	29568.275658	32.646644
691.839135	29615.585703	32.651661
692.576213	29652.802764	32.656679
693.523932	29707.464853	32.661696
694.537147	29734.777841	32.666714
695.222249	29778.330741	32.671732
696.076842	29814.360277	32.676749
696.879168	29838.880865	32.681767
697.277250	29884.362651	32.686784
698.253523	29912.370671	32.691802
698.444232	29947.790111	32.696820
699.567064	29985.674306	32.701837
700.646756	30007.073222	32.706855
701.061950	30055.820784	32.711872
701.766231	30092.967924	32.716890
702.170035	30127.456683	32.721908
703.121906	30170.058374	32.726925
703.687331	30192.650566	32.731943
704.299263	30240.217280	32.736960
705.413178	30272.237230	32.741978
705.795260	30306.931973	32.746996
706.568809	30343.265909	32.752013
707.510140	30370.376077	32.757031
707.881843	30415.774667	32.762048
708.494541	30461.622363	32.767066
709.287847	30501.076242	32.772084
710.080450	30540.871662	32.777101
710.816918	30572.388584	32.782119
711.385378	30618.079199	32.787136
712.022538	30652.715613	32.792154
712.999126	30692.880765	32.797172
713.867584	30739.675171	32.802189
714.700047	30768.528671	32.807207
715.281023	30817.479643	32.812224
715.932776	30854.434094	32.817242
716.763227	30887.972302	32.822260
717.237681	30928.128045	32.827277
718.010394	30961.517377	32.832295
718.572961	31012.829623	32.837312
718.967571	31047.365609	32.842330
719.838694	31082.889053	32.847348
720.497763	31127.302291	32.852365
721.800327	31161.898573	32.857383
722.399621	31196.744121	32.862400
723.242422	31245.256843	32.867418
724.433300	31275.622684	32.872436
724.503150	31305.045194	32.877453
725.410150	31335.468221	32.882471
726.247160	31388.097572	32.887488
726.716319	31412.337163	32.892506
727.658508	31433.436696	32.897524
727.960918	31462.456354	32.902541
728.960064	31502.644835	32.907559
729.383842	31533.927716	32.912576
729.787830	31560.674758	32.917594
730.685870	31604.356209	32.922612
731.174973	31640.345025	32.927629
731.959836	31682.957027	32.932647
732.774076	31722.934665	32.937664
733.867170	31759.884838	32.942682
734.236446	31791.827785	32.947700
734.890983	31834.055913	32.952717
735.123980	31862.720336	32.957735
736.361013	31915.288381	32.962752
736.847417	31959.060328	32.967770
737.938855	32001.941067	32.972788
738.660782	32046.694132	32.977805
739.735839	32086.163810	32.982823
740.188070	32131.692628	32.987840
741.119167	32177.039084	32.992858
741.794021	32209.522756	32.997876
742.561228	32251.557075	33.002893
743.699595	32283.317120	33.007911
744.249331	32324.254016	33.012928
745.078743	32362.479333	33.017946
745.953545	32402.240171	33.022964
746.464213	32447.223161	33.027981
747.185993	32476.918233	33.032999
747.654811	32520.580318	33.038016
748.535325	32573.572535	33.043034
749.733744	32615.306147	33.048052
750.451553	32663.462433	33.053069
751.156525	32692.964462	33.058087
751.465279	32730.791513	33.063104
752.357790	32776.745914	33.068122
753.172534	32807.324634	33.073140
754.111217	32856.477278	33.078157
754.554630	32899.151563	33.083175
755.287508	32947.622251	33.088192
756.089432	32990.588298	33.093210
757.385813	33035.259851	33.098228
757.620183	33082.228377	33.103245
758.561946	33115.841266	33.108263
759.568889	33163.466621	33.113280
760.284441	33200.579632	33.118298
761.113982	33235.474728	33.123316
761.952914	33283.297365	33.128333
762.715237	33314.277016	33.133351
763.372993	33361.192511	33.138368
764.312290	33400.224415	33.143386
765.238435	33440.080348	33.148404
765.816771	33474.711712	33.153421
766.582802	33512.013362	33.158439
767.264668	33553.791808	33.163456
767.846569	33599.512155	33.168474
768.884258	33639.724017	33.173492
769.424780	33674.823164	33.178509
770.232533	33719.104843	33.183527
770.911298	33752.544981	33.188544
771.722875	33800.543787	33.193562
772.618127	33843.996440	33.198580
773.137111	33885.990727	33.203597
774.112160	33926.446878	33.208615
774.669235	33966.810499	33.213632
775.528142	34017.647485	33.218650
776.694516	34052.699839	33.223668
777.431653	34094.755218	33.228685
777.966931	34126.682061	33.233703
778.615309	34158.831495	33.238720
779.413047	34191.735259	33.243738
780.070329	34224.509327	33.248756
780.833429	34266.934014	33.253773
781.310985	34304.004055	33.258791
782.185170	34342.339786	33.263808
783.006564	34384.300357	33.268826
784.022028	34422.645724	33.273844
784.299158	34470.280848	33.278861
785.452832	34499.563419	33.283879
786.062318	34549.568231	33.288896
787.055711	34593.101905	33.293914
787.627277	34626.199831	33.298932
788.391204	34676.243985	33.303949
789.078982	34715.785599	33.308967
789.677177	34764.831645	33.313984
790.360664	34802.679617	33.319002
791.659623	34857.237011	33.324020
792.067978	34901.659595	33.329037
793.210831	34957.822373	33.334055
794.132889	34996.069602	33.339072
794.808698	35043.308483	33.344090
795.879729	35080.976136	33.349108
796.528564	35132.689637	33.354125
797.434290	35183.066864	33.359143
798.352905	35234.883794	33.364160
799.051019	35272.249784	33.369178
800.334622	35305.793685	33.374196
800.888815	35360.652366	33.379213
801.795307	35399.041866	33.384231
802.407704	35442.048927	33.389248
803.209866	35477.660197	33.394266
804.031747	35516.474147	33.399284
805.080919	35563.687339	33.404301
806.249120	35598.451130	33.409319
806.936547	35641.611243	33.414336
807.443899	35689.282612	33.419354
808.604818	35725.141622	33.424372
809.161897	35767.848181	33.429389
810.156720	35816.480471	33.434407
811.134452	35847.455414	33.439424
811.848312	35892.205293	33.444442
812.309445	35927.788523	33.449460
813.143726	35966.949123	33.454477
813.997492	36011.070334	33.459495
815.142761	36056.884831	33.464512
815.658133	36091.131999	33.469530
816.682853	36133.816652	33.474548
817.292066	36174.290141	33.479565
818.109528	36220.137352	33.484583
819.011325	36257.801987	33.489600
819.791722	36305.375075	33.494618
821.158447	36342.220928	33.499636
821.797482	36389.715169	33.504653
822.468641	36430.388110	33.509671
823.140874	36468.487426	33.514688
823.674284	36508.271547	33.519706
824.472068	36542.108474	33.524724
825.188318	36580.251683	33.529741
825.920689	36640.580641	33.534759
827.037723	36682.588001	33.539776
827.481619	36731.081016	33.544794
828.868347	36771.313749	33.549812
829.583599	36824.772516	33.554829
830.648297	36870.361099	33.559847
831.243063	36906.822948	33.564864
832.137500	36954.189928	33.569882
833.849938	36983.103901	33.574900
834.657822	37006.898536	33.579917
834.961679	37033.592335	33.584935
835.891712	37051.373362	33.589952
836.724155	37091.206597	33.594970
837.515308	37120.201785	33.599988
838.142609	37154.635485	33.605005
838.445867	37193.255480	33.610023
839.423862	37238.782548	33.615040
840.134320	37276.624386	33.620058
841.150540	37308.076014	33.625076
841.794402	37359.125425	33.630093
842.627033	37407.849984	33.635111
843.634181	37443.116277	33.640128
843.787519	37490.809168	33.645146
845.213008	37538.404140	33.650164
845.844927	37581.867758	33.655181
846.774274	37630.482826	33.660199
848.220016	37682.830238	33.665216
848.551211	37733.752442	33.670234
849.344438	37762.558471	33.675252
849.931855	37819.195198	33.680269
850.538685	37860.582853	33.685287
852.160216	37906.851612	33.690304
852.803718	37958.054272	33.695322
853.693525	38011.887060	33.700340
854.412566	38062.888432	33.705357
855.416809	38114.376455	33.710375
856.158165	38156.976731	33.715392
857.272722	38215.226706	33.720410
858.012851	38264.796100	33.725428
858.884367	38307.256143	33.730445
859.839464	38356.577081	33.735463
860.949803	38407.878454	33.740480
861.719542	38459.119454	33.745498
862.901317	38500.867302	33.750516
863.580540	38548.853296	33.755533
864.242805	38602.685250	33.760551
865.324994	38645.188858	33.765568
866.355039	38687.409818	33.770586
866.961421	38732.157176	33.775604
867.623525	38782.049848	33.780621
868.647665	38846.392920	33.785639
869.885608	38873.189374	33.790656
870.183062	38927.167796	33.795674
871.344520	38968.078654	33.800692
872.301054	39023.440235	33.805709
873.118309	39071.684032	33.810727
874.101511	39115.949478	33.815744
874.879657	39174.703726	33.820762
876.002346	39227.200348	33.825780
876.698458	39268.722181	33.830797
877.577669	39315.685697	33.835815
878.877039	39363.557426	33.840832
879.519832	39403.506859	33.845850
880.667797	39453.944761	33.850868
881.166868	39494.795911	33.855885
881.860913	39540.277457	33.860903
883.192044	39570.766102	33.865920
883.890613	39634.005191	33.870938
884.884578	39678.289076	33.875956
885.562227	39731.084276	33.880973
886.439595	39773.457751	33.885991
887.770609	39814.318368	33.891008
888.502027	39860.547309	33.896026
889.769380	39889.655074	33.901044
890.561008	39939.580728	33.906061
891.217702	39985.246134	33.911079
891.972240	40023.629782	33.916096
892.724343	40058.314203	33.921114
893.509141	40088.275676	33.926132
894.586028	40134.002085	33.931149
895.129617	40181.703051	33.936167
896.002661	40209.665054	33.941184
896.831473	40257.511254	33.946202
897.408545	40298.060786	33.951220
898.628132	40349.084043	33.956237
899.335645	40382.549047	33.961255
900.310681	40429.702353	33.966272
900.627008	40478.830910	33.971290
901.538516	40534.304593	33.976308
902.483674	40577.358380	33.981325
903.368078	40647.831713	33.986343
904.652375	40700.268654	33.991360
905.322213	40769.903208	33.996378
906.080825	40814.827086	34.001396
907.313220	40871.857795	34.006413
907.879264	40917.381239	34.011431
909.524138	40972.823426	34.016448
910.260870	41023.601321	34.021466
911.080707	41078.161039	34.026484
912.224528	41136.844362	34.031501
913.193663	41181.356559	34.036519
914.232182	41224.517174	34.041536
915.279113	41286.877998	34.046554
916.065833	41324.759260	34.051572
917.351562	41374.288283	34.056589
918.172710	41420.930237	34.061607
919.238614	41465.326667	34.066624
920.083510	41520.010056	34.071642
920.635106	41569.426784	34.076660
922.160769	41623.630684	34.081677
922.908429	41667.229846	34.086695
923.726466	41712.639593	34.091712
924.907215	41768.150150	34.096730
925.917456	41816.116830	34.101748
927.092160	41846.443429	34.106765
927.872179	41898.038794	34.111783
928.761204	41942.362692	34.116800
929.417815	41988.462388	34.121818
930.312485	42038.446284	34.126836
931.188316	42089.887953	34.131853
932.103821	42145.169029	34.136871
933.421072	42190.185357	34.141888
933.972098	42240.394291	34.146906
934.789080	42289.511767	34.151924
935.965061	42336.903371	34.156941
936.252528	42393.497787	34.161959
937.574857	42436.135661	34.166976
938.481535	42502.057533	34.171994
939.534920	42557.571055	34.177012
940.644223	42599.236933	34.182029
941.468882	42661.573220	34.187047
943.046035	42707.467038	34.192064
943.589284	42749.702532	34.197082
944.745360	42797.566297	34.202100
945.896839	42849.491559	34.207117
946.658133	42896.455947	34.212135
947.468852	42942.558812	34.217152
948.066400	42988.783702	34.222170
949.205214	43044.639281	34.227188
950.453440	43078.934559	34.232205
951.411488	43133.578946	34.237223
952.190358	43181.673386	34.242240
953.311207	43229.126145	34.247258
954.459670	43276.682212	34.252276
955.303379	43313.691436	34.257293
956.039615	43351.887707	34.262311
956.890124	43377.668781	34.267328
957.643449	43416.861869	34.272346
958.581787	43461.041951	34.277364
959.333950	43506.219031	34.282381
959.934932	43549.509652	34.287399
960.987314	43598.479333	34.292416
961.988645	43653.504069	34.297434
962.903553	43709.851807	34.302452
964.024468	43747.008112	34.307469
964.932927	43799.764323	34.312487
965.994063	43846.291613	34.317504
967.068002	43898.528774	34.322522
967.895977	43946.319896	34.327540
969.010040	43989.733454	34.332557
970.043126	44046.303908	34.337575
970.966596	44095.041856	34.342592
972.393128	44147.401508	34.347610
972.753576	44197.315805	34.352628
973.966335	44247.748284	34.357645
975.044644	44297.126604	34.362663
976.157595	44346.708349	34.367680
976.972706	44397.576632	34.372698
977.703505	44452.392689	34.377716
979.221791	44508.761843	34.382733
979.965285	44561.577320	34.387751
980.475323	44604.833635	34.392768
981.569138	44654.368458	34.397786
982.782883	44713.233801	34.402804
984.251142	44761.660193	34.407821
985.048318	44822.735420	34.412839
985.995704	44873.324730	34.417856
986.882361	44937.302369	34.422874
988.177724	44989.330308	34.427892
989.030531	45040.181506	34.432909
989.636173	45100.294353	34.437927
991.004600	45147.339240	34.442944
991.941162	45196.260995	34.447962
993.201651	45248.623937	34.452980
994.173313	45303.499259	34.457997
995.186746	45361.265370	34.463015
995.970966	45411.033796	34.468032
997.053330	45468.637573	34.473050
998.315490	45514.295549	34.478068
999.492560	45566.090324	34.483085
1000.092222	45622.789574	34.488103
1001.285705	45672.020065	34.493120
1002.221265	45735.701343	34.498138
1003.450609	45784.224296	34.503156
1004.298970	45835.742215	34.508173
1005.329892	45881.373888	34.513191
1006.414553	45934.063282	34.518208
1007.437597	45982.391233	34.523226
1008.233657	46030.457507	34.528244
1009.525886	46072.316352	34.533261
1010.196259	46127.493905	34.538279
1011.144633	46181.293284	34.543296
1012.452095	46231.974789	34.548314
1013.184334	46290.837438	34.553332
1014.450981	46344.252098	34.558349
1015.093662	46404.875050	34.563367
1016.361449	46454.747210	34.568384
1017.293850	46499.161983	34.573402
1018.615705	46561.462972	34.578420
1019.831429	46605.909511	34.583437
1020.352267	46656.525350	34.588455
1021.000656	46710.708249	34.593472
1022.259417	46757.691453	34.598490
1023.088423	46804.122078	34.603508
1024.204151	46859.870639	34.608525
1025.079814	46901.802579	34.613543
1025.780444	46946.551854	34.618560
1027.100524	46994.291421	34.623578
1028.039872	47048.296725	34.628596
1029.288703	47098.932428	34.633613
1030.097102	47152.534626	34.638631
1030.622511	47199.000944	34.643648
1032.327266	47256.714301	34.648666
1033.442734	47307.086669	34.653684
1034.380970	47350.293885	34.658701
1035.337056	47419.373053	34.663719
1035.895565	47475.172417	34.668736
1037.024750	47526.466773	34.673754
1038.031143	47586.979016	34.678772
1039.331084	47640.847036	34.683789
1040.227649	47700.959238	34.688807
1041.346473	47753.508359	34.693824
1042.596707	47814.596695	34.698842
1043.315098	47875.009291	34.703860
1044.579446	47932.995775	34.708877
1045.567157	47985.477391	34.713895
1047.039634	48056.040292	34.718912
1047.786665	48114.551089	34.723930
1049.155471	48179.265921	34.728948
1050.217563	48226.757464	34.733965
1051.179602	48287.740359	34.738983
1052.734322	48347.283062	34.744000
1053.457504	48393.043917	34.749018
1054.530525	48457.767892	34.754036
1055.811033	48507.395855	34.759053
1056.784146	48563.234205	34.764071
1057.908988	48616.385413	34.769088
1059.173269	48673.627254	34.774106
1060.330092	48731.063209	34.779124
1061.417926	48775.034227	34.784141
1062.201799	48831.200218	34.789159
1063.662861	48886.665611	34.794176
1064.566239	48940.035723	34.799194
1065.936463	48990.359290	34.804212
1066.829013	49037.303334	34.809229
1067.901159	49086.123720	34.814247
1068.771774	49147.350994	34.819264
1069.936970	49213.903786	34.824282
1071.187237	49259.001790	34.829300
1072.233744	49304.226686	34.834317
1073.032828	49374.683991	34.839335
1074.267630	49414.710575	34.844352
1075.742252	49462.121127	34.849370
1076.468943	49516.488263	34.854388
1077.762299	49565.173810	34.859405
1078.859895	49624.791422	34.864423
1079.663327	49664.297575	34.869440
1080.960376	49725.807616	34.874458
1081.911929	49771.174842	34.879476
1083.228153	49815.390495	34.884493
1084.515941	49871.011948	34.889511
1085.457014	49927.504005	34.894528
1086.422024	49966.599434	34.899546
1087.388898	50019.139608	34.904564
1088.642321	50068.452529	34.909581
1089.571217	50112.008111	34.914599
1090.615704	50166.839527	34.919616
1091.900045	50220.444027	34.924634
1093.011033	50274.898318	34.929652
1093.667078	50316.636834	34.934669
1094.851798	50370.409132	34.939687
1096.017018	50418.996339	34.944704
1096.821528	50461.211719	34.949722
1097.587639	50502.560037	34.954740
1098.922612	50543.395446	34.959757
1099.911917	50590.681848	34.964775
1100.933801	50647.492037	34.969792
1101.990986	50699.798176	34.974810
1102.657386	50750.071296	34.979828
1104.028567	50806.536138	34.984845
1105.058125	50866.066387	34.989863
1106.496079	50916.908750	34.994880
1107.579472	50971.792939	34.999898
1108.310448	51025.131620	35.004916
1109.742200	51075.551374	35.009933
1111.181630	51137.675636	35.014951
1111.833252	51193.963022	35.019968
1113.357318	51237.484502	35.024986
1114.056993	51309.266732	35.030004
1115.017122	51360.558198	35.035021
1116.431478	51418.833748	35.040039
1117.636133	51482.375073	35.045056
1118.652165	51544.642645	35.050074
1119.883046	51599.967140	35.055092
1121.283028	51660.023570	35.060109
1122.242405	51721.047642	35.065127
1123.244225	51770.587096	35.070144
1124.663718	51832.013990	35.075162
1125.720952	51894.788583	35.080180
1126.907419	51944.179276	35.085197
1128.079152	52005.455591	35.090215
1129.058197	52057.258173	35.095232
1130.242456	52119.690780	35.100250
1131.749550	52171.695690	35.105268
1133.009680	52227.921956	35.110285
1133.795258	52295.011324	35.115303
1134.839716	52349.531541	35.120320
1136.138000	52403.316101	35.125338
1137.086578	52467.634227	35.130356
1138.314269	52515.412442	35.135373
1139.635067	52575.724092	35.140391
1140.853398	52645.689121	35.145408
1141.893082	52699.103546	35.150426
1143.176779	52755.118581	35.155444
1144.506009	52815.372581	35.160461
1145.830109	52871.311964	35.165479
1146.568935	52929.855261	35.170496
1148.606949	52983.942992	35.175514
1149.540068	53027.794483	35.180532
1150.358181	53077.599612	35.185549
1151.522960	53124.743483	35.190567
1152.810454	53188.744766	35.195584
1154.021722	53236.090405	35.200602
1155.294711	53293.937180	35.205620
1156.146413	53343.149118	35.210637
1157.573853	53390.461227	35.215655
1158.497151	53446.743167	35.220672
1159.781888	53494.033531	35.225690
1161.127035	53554.451475	35.230708
1162.269256	53601.340391	35.235725
1163.392694	53645.884641	35.240743
1164.497481	53700.272008	35.245760
1165.760395	53762.095532	35.250778
1166.946088	53804.947074	35.255796
1167.790008	53847.504155	35.260813
1169.201841	53905.596485	35.265831
1170.186236	53956.567135	35.270848
1171.754783	54003.491364	35.275866
1173.072102	54058.346211	35.280884
1173.925187	54093.359157	35.285901
1174.737401	54136.712746	35.290919
1175.820090	54184.339887	35.295936
1177.171090	54225.122317	35.300954
1178.026605	54263.470093	35.305972
1179.055098	54313.485383	35.310989
1180.014183	54351.209579	35.316007
1181.037340	54408.484380	35.321024
1182.446012	54466.654532	35.326042
1183.174419	54517.128571	35.331060
1184.186547	54568.589811	35.336077
1185.491671	54619.239571	35.341095
1186.783964	54691.705134	35.346112
1187.786139	54739.497884	35.351130
1189.265199	54810.263895	35.356148
1190.126666	54872.450617	35.361165
1191.615594	54935.539158	35.366183
1192.767254	54994.396343	35.371200
1194.541076	55050.181924	35.376218
1195.472711	55103.460528	35.381236
1196.669364	55161.684573	35.386253
1197.951623	55220.452263	35.391271
1198.991095	55285.649864	35.396288
1200.342532	55342.628728	35.401306
1201.443990	55406.247491	35.406324
1202.901227	55458.615579	35.411341
1204.570867	55527.157906	35.416359
1205.498713	55593.266151	35.421376
1207.006444	55637.880582	35.426394
1208.072808	55693.620220	35.431412
1209.053619	55747.867176	35.436429
1210.638065	55801.412212	35.441447
1211.364870	55875.919140	35.446464
1212.606940	55923.803299	35.451482
1214.081761	55980.245433	35.456500
1215.894226	56045.874705	35.461517
1217.049235	56094.462664	35.466535
1218.140316	56148.971736	35.471552
1219.700600	56193.452414	35.476570
1220.867119	56256.854424	35.481588
1222.067105	56304.435832	35.486605
1223.539419	56357.449077	35.491623
1224.428999	56413.964873	35.496640
1225.703465	56462.496911	35.501658
1227.281976	56515.304020	35.506676
1228.473875	56564.539031	35.511693
1229.376085	56622.464669	35.516711
1230.517321	56660.113401	35.521728
1232.538487	56706.301294	35.526746
1233.113410	56767.392313	35.531764
1234.279959	56816.726746	35.536781
1235.774234	56864.655595	35.541799
1236.698027	56916.844595	35.546816
1238.321097	56973.044366	35.551834
1239.434718	57014.495333	35.556852
1240.547250	57074.028334	35.561869
1241.723614	57124.007419	35.566887
1242.988805	57187.453417	35.571904
1244.140471	57232.316454	35.576922
1245.252083	57288.590705	35.581940
1246.310117	57348.531647	35.586957
1247.920496	57398.924369	35.591975
1249.263092	57453.232493	35.596992
1250.848582	57517.376052	35.602010
1251.984511	57559.451050	35.607028
1253.567248	57611.538410	35.612045
1254.616350	57646.918323	35.617063
1255.971221	57703.826353	35.622080
1257.090815	57732.245992	35.627098
1258.438362	57763.465431	35.632116
1259.475574	57810.651272	35.637133
1260.615746	57839.618453	35.642151
1261.423959	57884.409895	35.647168
1262.271778	57928.593949	35.652186
1263.345042	57972.869376	35.657204
1264.677311	58031.294395	35.662221
1265.946885	58087.134394	35.667239
1266.993422	58136.370080	35.672256
1268.630195	58200.032746	35.677274
1269.927361	58248.419284	35.682292
1270.420337	58317.293069	35.687309
1272.057680	58368.708953	35.692327
1273.189770	58434.603200	35.697344
1274.824303	58479.658813	35.702362
1275.954164	58557.345260	35.707380
1277.309593	58625.895036	35.712397
1278.424968	58675.026106	35.717415
1279.640100	58728.255756	35.722432
1281.366546	58788.899485	35.727450
1282.477673	58861.178209	35.732468
1283.729366	58927.244960	35.737485
1285.451923	58986.718850	35.742503
1286.953936	59056.474813	35.747520
1288.180592	59112.108702	35.752538
1289.474711	59175.441484	35.757556
1290.663976	59238.879457	35.762573
1292.232055	59288.270042	35.767591
1293.702072	59363.703155	35.772608
1295.019766	59409.170887	35.777626
1296.530323	59465.425749	35.782644
1297.587456	59524.302545	35.787661
1299.346386	59578.290775	35.792679
1300.481412	59636.060627	35.797696
1301.581244	59680.892034	35.802714
1303.113983	59733.694400	35.807732
1304.092876	59795.761581	35.812749
1305.386356	59846.842002	35.817767
1306.902036	59911.914331	35.822784
1308.170215	59963.372409	35.827802
1309.788556	60009.180316	35.832820
1310.883251	60077.711715	35.837837
1312.348514	60129.000039	35.842855
1313.677446	60181.031404	35.847872
1315.383827	60238.162559	35.852890
1316.365529	60302.040905	35.857908
1317.689879	60354.269582	35.862925
1319.116849	60410.071312	35.867943
1320.331478	60459.665196	35.872960
1321.576596	60508.444189	35.877978
1322.895870	60573.473073	35.882996
1324.039497	60632.794759	35.888013
1325.356484	60681.379281	35.893031
1326.791604	60741.617745	35.898048
1328.123129	60798.543037	35.903066
1329.655053	60849.100832	35.908084
1330.897965	60911.863795	35.913101
1332.221570	60957.618345	35.918119
1333.674128	61026.476185	35.923136
1334.821813	61087.260562	35.928154
1335.984824	61136.313191	35.933172
1337.368218	61197.902836	35.938189
1338.918680	61242.894457	35.943207
1339.760673	61310.158550	35.948224
1341.162869	61359.978103	35.953242
1342.737103	61418.930445	35.958260
1343.661324	61474.306896	35.963277
1345.225378	61524.012824	35.968295
1346.538643	61570.447460	35.973312
1347.854163	61608.095616	35.978330
1348.980184	61665.542511	35.983348
1350.388472	61721.786937	35.988365
1351.747808	61762.517587	35.993383
1352.809114	61813.657455	35.998400
1354.066668	61866.773380	36.003418
1355.608375	61928.681908	36.008436
1357.125373	61982.884249	36.013453
1358.433802	62033.137641	36.018471
1359.744317	62093.417921	36.023488
1360.918646	62150.212700	36.028506
1362.317978	62205.636700	36.033524
1363.706638	62265.664619	36.038541
1365.343332	62319.095659	36.043559
1366.619576	62386.130127	36.048576
1368.094951	62432.648632	36.053594
1369.469249	62500.427702	36.058612
1371.002032	62558.946141	36.063629
1372.756097	62613.252029	36.068647
1373.800829	62671.986400	36.073664
1375.061340	62722.470261	36.078682
1376.634712	62778.108860	36.083700
1377.462021	62841.986320	36.088717
1379.551491	62905.463803	36.093735
1380.766422	62962.519972	36.098752
1381.987059	63018.923340	36.103770
1383.480644	63075.239798	36.108788
1384.909979	63136.307996	36.113805
1386.845377	63202.095673	36.118823
1388.153339	63267.437311	36.123840
1389.558587	63322.597007	36.128858
1390.994154	63372.149520	36.133876
1392.294348	63440.189653	36.138893
1393.606085	63495.047840	36.143911
1395.244598	63555.229694	36.148928
1396.928631	63612.505139	36.153946
1398.291366	63661.271970	36.158964
1399.466579	63722.786549	36.163981
1400.698471	63762.502220	36.168999
1402.287216	63832.511414	36.174016
1403.593251	63889.023673	36.179034
1405.430747	63948.118105	36.184052
1406.508413	64009.249825	36.189069
1407.871467	64063.100975	36.194087
1408.818887	64129.014100	36.199104
1410.457414	64188.133914	36.204122
1411.902605	64240.668450	36.209140
1413.161669	64310.445704	36.214157
1414.824307	64379.014101	36.219175
1416.567077	64433.920842	36.224192
1417.902963	64494.108019	36.229210
1419.541133	64554.096084	36.234228
1421.055073	64610.685059	36.239245
1422.606803	64655.765000	36.244263
1423.949630	64704.733247	36.249280
1425.001219	64767.073774	36.254298
1426.685095	64811.854753	36.259316
1427.794878	64871.318515	36.264333
1429.662463	64932.164242	36.269351
1430.570599	64977.991263	36.274368
1432.128080	65037.511963	36.279386
1433.730039	65094.075592	36.284404
1434.853441	65160.774253	36.289421
1436.388732	65204.990407	36.294439
1437.719303	65261.894452	36.299456
1438.962302	65331.037623	36.304474
1440.703920	65365.035078	36.309492
1441.995592	65420.267834	36.314509
1443.347156	65461.486938	36.319527
1444.453535	65512.475407	36.324544
1445.902179	65565.917533	36.329562
1447.253580	65607.947287	36.334580
1448.322482	65663.000187	36.339597
1449.462966	65722.359858	36.344615
1451.147543	65781.634505	36.349632
1452.428901	65856.775076	36.354650
1454.386357	65904.294583	36.359668
1455.583119	65969.825291	36.364685
1457.029432	66029.384732	36.369703
1458.531312	66102.509838	36.374720
1459.819875	66160.758385	36.379738
1461.529668	66221.802878	36.384756
1462.751311	66295.700504	36.389773
1464.499049	66360.873738	36.394791
1465.816024	66418.700564	36.399808
1467.884641	66490.953000	36.404826
1469.513138	66541.893482	36.409844
1470.996434	66606.374301	36.414861
1472.467352	66655.649196	36.419879
1474.141643	66729.445581	36.424896
1475.457140	66786.918919	36.429914
1477.176325	66845.791766	36.434932
1478.567776	66906.615486	36.439949
1479.982752	66976.306069	36.444967
1481.865034	67031.114336	36.449984
1482.987905	67087.827069	36.455002
1484.437726	67150.668319	36.460020
1485.922947	67209.806565	36.465037
1487.406245	67269.375796	36.470055
1489.406557	67323.900295	36.475072
1490.511356	67406.525344	36.480090
1492.466979	67451.591394	36.485108
1493.903131	67515.252460	36.490125
1495.196318	67570.312385	36.495143
1496.745341	67627.573786	36.500160
1498.684238	67700.198208	36.505178
1500.093397	67756.873952	36.510196
1501.744120	67820.229933	36.515213
1502.676368	67876.562697	36.520231
1504.709472	67936.769247	36.525248
1505.786681	68001.646410	36.530266
1507.450356	68061.125941	36.535284
1508.977928	68118.480446	36.540301
1510.266822	68169.857251	36.545319
1511.879076	68238.937883	36.550336
1513.839695	68306.691483	36.555354
1515.489030	68362.735789	36.560372
1516.617323	68427.916295	36.565389
1518.165776	68488.377293	36.570407
1519.960099	68550.395581	36.575424
1520.998154	68601.717534	36.580442
1522.809721	68667.576859	36.585460
1523.928174	68730.587832	36.590477
1525.467506	68794.356237	36.595495
1527.374881	68855.762368	36.600512
1528.562049	68912.139820	36.605530
1529.914388	68976.659787	36.610548
1531.739317	69036.173330	36.615565
1533.341378	69102.769411	36.620583
1534.924322	69164.619643	36.625600
1536.088478	69230.556411	36.630618
1537.687560	69298.020951	36.635636
1539.552413	69354.388285	36.640653
1541.168403	69417.342062	36.645671
1542.428056	69459.240570	36.650688
1543.352782	69514.666278	36.655706
1544.877423	69555.219053	36.660724
1546.193388	69620.455521	36.665741
1547.551019	69670.336516	36.670759
1548.762746	69726.015368	36.675776
1550.529355	69796.709720	36.680794
1551.954973	69860.789840	36.685812
1553.559502	69928.375486	36.690829
1555.066377	69991.715008	36.695847
1556.227668	70055.020123	36.700864
1558.004416	70137.403126	36.705882
1559.985822	70195.907022	36.710900
1561.480062	70284.185724	36.715917
1563.070636	70349.298726	36.720935
1564.852732	70412.076951	36.725952
1566.817936	70482.045533	36.730970
1568.309573	70542.944504	36.735988
1569.988790	70609.399409	36.741005
1571.284954	70688.338578	36.746023
1572.978891	70744.761023	36.751040
1574.543731	70814.210581	36.756058
1576.249022	70880.674761	36.761076
1577.871816	70947.835929	36.766093
1579.190993	71024.302857	36.771111
1580.907314	71090.297243	36.776128
1582.620469	71169.539889	36.781146
1584.246866	71232.610427	36.786164
1585.731901	71310.850671	36.791181
1587.371543	71372.007047	36.796199
1589.827794	71439.051699	36.801216
1591.183532	71518.705966	36.806234
1592.968887	71582.360399	36.811252
1594.488688	71645.410621	36.816269
1595.925197	71703.838543	36.821287
1597.645172	71765.401220	36.826304
1599.525696	71836.311257	36.831322
1600.849487	71897.391641	36.836340
1602.518890	71962.952286	36.841357
1604.110108	72035.187345	36.846375
1605.939244	72092.402130	36.851392
1607.154611	72179.818966	36.856410
1609.056015	72228.942153	36.861428
1610.914157	72289.331874	36.866445
1611.927554	72363.406113	36.871463
1614.222257	72431.897139	36.876480
1615.469978	72507.201671	36.881498
1616.999256	72566.706240	36.886516
1618.872199	72624.751264	36.891533
1620.298540	72697.849883	36.896551
1622.313907	72761.547172	36.901568
1624.127288	72836.409473	36.906586
1625.634430	72889.547334	36.911604
1627.209472	72944.599886	36.916621
1628.626577	73019.081419	36.921639
1630.141169	73075.460958	36.926656
1631.668935	73147.253023	36.931674
1633.544975	73215.304972	36.936692
1635.448722	73276.601770	36.941709
1636.680197	73344.222956	36.946727
1638.237163	73401.609843	36.951744
1639.814292	73475.928289	36.956762
1641.464191	73540.279963	36.961780
1643.549686	73606.590208	36.966797
1645.059554	73670.495464	36.971815
1646.603110	73732.888320	36.976832
1648.135757	73803.782096	36.981850
1649.669321	73860.818985	36.986868
1651.318049	73909.174208	36.991885
1652.660240	73966.431269	36.996903
1654.654027	74008.538828	37.001920
1655.607923	74066.084867	37.006938
1656.879431	74130.927850	37.011956
1659.020110	74190.479714	37.016973
1660.282513	74256.793737	37.021991
1661.931062	74312.141623	37.027008
1663.701357	74384.823732	37.032026
1665.437962	74444.008741	37.037044
1667.222653	74508.620329	37.042061
1668.303758	74586.452156	37.047079
1670.165394	74663.351387	37.052096
1671.891894	74733.393964	37.057114
1673.408204	74807.662311	37.062132
1675.220957	74872.245054	37.067149
1677.189036	74953.739168	37.072167
1678.635423	75027.195725	37.077184
1680.688001	75095.566862	37.082202
1682.326059	75172.667216	37.087220
1684.181044	75244.629061	37.092237
1685.504932	75318.713601	37.097255
1687.792183	75384.452018	37.102272
1689.298200	75464.487288	37.107290
1691.223876	75539.820965	37.112308
1692.959933	75616.083895	37.117325
1694.295415	75686.899516	37.122343
1696.684831	75760.717182	37.127360
1698.009726	75838.552484	37.132378
1699.666014	75896.271207	37.137396
1701.545856	75970.498545	37.142413
1703.074433	76052.546131	37.147431
1704.973949	76115.471534	37.152448
1707.050174	76201.664765	37.157466
1708.510025	76276.617378	37.162484
1710.565462	76348.069441	37.167501
1712.486705	76420.632100	37.172519
1714.213735	76483.902044	37.177536
1715.845090	76552.583490	37.182554
1717.424659	76619.398411	37.187572
1719.174383	76689.455115	37.192589
1720.734930	76769.397046	37.197607
1722.588009	76840.730068	37.202624
1724.326633	76916.717579	37.207642
1726.601567	76985.172726	37.212660
1728.210575	77048.817158	37.217677
1729.533208	77126.871870	37.222695
1731.090991	77193.995643	37.227712
1732.831559	77269.261768	37.232730
1734.914682	77349.567001	37.237748
1736.592494	77413.936260	37.242765
1738.159943	77487.671923	37.247783
1740.023661	77569.050915	37.252800
1742.108086	77630.114036	37.257818
1743.509910	77707.119235	37.262836
1745.356174	77777.873051	37.267853
1747.036434	77850.439239	37.272871
1748.762333	77917.006422	37.277888
1750.811475	77992.846997	37.282906
1752.180707	78067.134642	37.287924
1754.187613	78127.197547	37.292941
1755.770513	78203.035659	37.297959
1757.618675	78277.971021	37.302976
1759.356046	78343.739341	37.307994
1761.117360	78419.347437	37.313012
1762.906566	78492.164316	37.318029
1764.551425	78564.788613	37.323047
1766.143757	78624.081367	37.328064
1768.135828	78680.942675	37.333082
1769.250828	78747.658153	37.338100
1770.878712	78809.124739	37.343117
1772.237166	78877.259322	37.348135
1774.428307	78941.729206	37.353152
1776.189518	79000.160213	37.358170
1777.712412	79068.902972	37.363188
1779.417749	79134.070100	37.368205
1780.901763	79208.279524	37.373223
1782.669096	79280.848540	37.378240
1784.367063	79362.993588	37.383258
1786.173761	79442.588086	37.388276
1788.116693	79521.046628	37.393293
1789.632832	79604.348382	37.398311
1791.557448	79693.236842	37.403328
1793.402847	79767.910645	37.408346
1795.181929	79863.283638	37.413364
1797.272966	79942.429667	37.418381
1798.962489	80021.904807	37.423399
1800.823049	80106.877179	37.428416
1802.848432	80188.251294	37.433434
1804.528411	80287.340669	37.438452
1806.643153	80361.910577	37.443469
1808.419613	80450.279866	37.448487
1810.345400	80537.625187	37.453504
1812.184533	80606.233588	37.458522
1813.941179	80695.569633	37.463540
1815.978787	80778.172499	37.468557
1817.608953	80859.965172	37.473575
1819.943070	80947.868687	37.478592
1821.903391	81034.424646	37.483610
1823.804371	81109.625479	37.488628
1825.400200	81184.848929	37.493645
1826.696620	81268.405431	37.498663
1829.243497	81346.647920	37.503680
1831.139467	81423.826866	37.508698
1832.994609	81505.598891	37.513716
1835.133865	81579.129293	37.518733
1837.086341	81674.785423	37.523751
1839.023880	81738.325915	37.528768
1840.923726	81809.233700	37.533786
1842.747063	81892.342177	37.538804
1844.684232	81964.486173	37.543821
1846.251150	82050.055219	37.548839
1848.326366	82123.584400	37.553856
1850.091360	82196.870905	37.558874
1851.933375	82279.407446	37.563892
1854.083465	82337.708593	37.568909
1856.186195	82419.267151	37.573927
1857.565895	82500.368926	37.578944
1859.257022	82569.055979	37.583962
1861.156364	82651.698672	37.588980
1863.670044	82723.551674	37.593997
1865.123689	82798.168172	37.599015
1867.332984	82862.847028	37.604032
1869.084181	82936.923183	37.609050
1870.632088	83020.838314	37.614068
1872.493168	83094.923029	37.619085
1874.289175	83174.251067	37.624103
1876.536372	83246.476535	37.629120
1878.237310	83318.698974	37.634138
1880.128481	83393.058513	37.639156
1882.139490	83470.769903	37.644173
1883.561596	83545.836777	37.649191
1885.215382	83627.177643	37.654208
1887.524330	83698.076838	37.659226
1888.942051	83783.281674	37.664244
1890.893059	83855.364978	37.669261
1892.574596	83917.518627	37.674279
1894.394730	83989.027216	37.679296
1896.010344	84046.934029	37.684314
1897.798858	84124.872086	37.689332
1899.509147	84190.823132	37.694349
1901.382074	84270.192874	37.699367
1903.023467	84349.903173	37.704384
1904.747045	84424.697106	37.709402
1906.541088	84509.401731	37.714420
1908.481907	84591.866178	37.719437
1910.473444	84681.520191	37.724455
1912.279098	84773.268991	37.729472
1914.177671	84849.848645	37.734490
1916.135228	84958.452465	37.739508
1918.200924	85036.539701	37.744525
1920.154064	85129.064857	37.749543
1921.718994	85224.121994	37.754560
1923.813109	85307.971045	37.759578
1925.527268	85410.583015	37.764596
1927.916697	85497.706358	37.769613
1929.837852	85599.665702	37.774631
1931.755557	85690.462188	37.779648
1933.652886	85785.849313	37.784666
1935.790101	85893.212055	37.789684
1938.100092	85987.762296	37.794701
1940.352858	86080.459037	37.799719
1942.245711	86169.879685	37.804736
1944.547600	86260.529141	37.809754
1945.870524	86353.853788	37.814772
1948.482501	86441.135232	37.819789
1950.434977	86545.069835	37.824807
1952.619970	86631.797734	37.829824
1954.537685	86717.845402	37.834842
1956.265780	86803.035943	37.839860
1958.429179	86892.137693	37.844877
1960.070812	86988.265749	37.849895
1962.155980	87076.594624	37.854912
1964.345876	87164.983414	37.859930
1966.330842	87268.041121	37.864948
1968.290717	87357.961827	37.869965
1970.363008	87448.942377	37.874983
1972.184625	87549.517490	37.880000
1974.278117	87640.419283	37.885018
1976.284436	87737.607921	37.890036
1978.240540	87817.595333	37.895053
1980.244762	87908.283818	37.900071
1981.995519	88011.532858	37.905088
1984.135068	88101.478421	37.910106
1985.808598	88196.312831	37.915124
1987.852266	88294.042394	37.920141
1990.331198	88392.464546	37.925159
1992.293103	88484.403368	37.930176
1994.398420	88571.048098	37.935194
1995.922672	88676.654056	37.940212
1998.170864	88761.274659	37.945229
2000.234997	88855.403745	37.950247
2002.511664	88956.026518	37.955264
2004.675568	89036.504324	37.960282
2006.374496	89124.861772	37.965300
2008.191864	89222.097542	37.970317
2010.558341	89313.139207	37.975335
2012.137750	89413.872635	37.980352
2014.303641	89492.741861	37.985370
2015.944634	89597.116191	37.990388
2017.721662	89693.295252	37.995405
2020.037884	89791.950293	38.000423
2021.744396	89890.409571	38.005440
2023.783121	89971.175642	38.010458
2025.542915	90070.058076	38.015476
2027.278358	90147.399520	38.020493
2029.310301	90242.273106	38.025511
2030.925112	90329.848853	38.030528
2033.079785	90407.847776	38.035546
2034.751848	90517.657483	38.040564
2036.499550	90609.877198	38.045581
2038.649449	90721.691389	38.050599
2040.699207	90819.973281	38.055616
2042.292890	90923.687926	38.060634
2044.142312	91041.988678	38.065652
2046.537421	91156.820549	38.070669
2048.081198	91272.914055	38.075687
2050.236763	91382.701964	38.080704
2052.555235	91506.076840	38.085722
2054.216261	91631.392849	38.090740
2056.462606	91743.018301	38.095757
2058.682776	91869.096984	38.100775
2060.349407	92006.593694	38.105792
2062.987123	92130.783023	38.110810
2065.129730	92263.795723	38.115828
2067.002502	92386.711592	38.120845
2069.216534	92505.467997	38.125863
2071.212882	92640.051525	38.130880
2073.328576	92762.816832	38.135898
2075.445212	92888.485002	38.140916
2077.836232	93017.431555	38.145933
2080.683332	93151.123737	38.150951
2082.368493	93275.656897	38.155968
2084.984039	93397.332553	38.160986
2086.486487	93526.825879	38.166004
2088.727098	93646.343060	38.171021
2090.861854	93769.743176	38.176039
2092.858830	93898.336810	38.181056
2094.769365	94026.906480	38.186074
2097.458619	94160.209474	38.191092
2099.570734	94279.052078	38.196109
2102.133643	94404.669306	38.201127
2103.831131	94536.836213	38.206144
2106.683396	94651.026643	38.211162
2108.492978	94784.229132	38.216180
2110.343663	94900.389790	38.221197
2112.327054	95022.474985	38.226215
2114.439345	95154.224706	38.231232
2117.061642	95276.185584	38.236250
2118.974843	95410.680146	38.241268
2120.834632	95537.730257	38.246285
2123.252656	95665.961132	38.251303
2125.096341	95796.399276	38.256320
2127.048110	95935.440726	38.261338
2129.319832	96072.163722	38.266356
2131.080000	96196.341958	38.271373
2133.335721	96327.199539	38.276391
2135.404978	96468.253155	38.281408
2136.982163	96607.799860	38.286426
2139.462673	96752.086234	38.291444
2141.539123	96890.098299	38.296461
2143.743545	97030.182558	38.301479
2145.900840	97173.114345	38.306496
2148.062980	97315.031897	38.311514
2149.919010	97462.233416	38.316532
2152.611633	97591.595435	38.321549
2154.405283	97734.219028	38.326567
2156.158872	97884.518976	38.331584
2158.370236	98030.894255	38.336602
2160.649918	98184.345901	38.341620
2162.571385	98323.871655	38.346637
2164.640931	98471.437426	38.351655
2166.776087	98603.451538	38.356672
2168.907723	98728.316857	38.361690
2170.913277	98845.659484	38.366708
2173.035354	98980.669008	38.371725
2175.125498	99113.579672	38.376743
2176.736088	99257.290922	38.381760
2178.980887	99390.761694	38.386778
2181.350137	99538.146037	38.391796
2183.011867	99681.508889	38.396813
2185.239857	99826.736126	38.401831
2187.295684	99984.960135	38.406848
2189.427687	100137.582152	38.411866
2191.603530	100288.004784	38.416884
2193.725203	100451.887714	38.421901
2196.115344	100613.079800	38.426919
2198.426531	100778.620883	38.431936
2200.942062	100929.931510	38.436954
2203.182945	101097.678504	38.441972
2205.112373	101254.483178	38.446989
2207.699674	101410.437668	38.452007
2209.961135	101583.787684	38.457024
2212.350036	101743.540234	38.462042
2214.569891	101904.841412	38.467060
2216.782243	102065.231711	38.472077
2219.320586	102236.120279	38.477095
2221.401595	102404.253970	38.482112
2223.665400	102549.931480	38.487130
2225.824487	102720.387428	38.492148
2227.558705	102882.669555	38.497165
2230.076307	103059.068194	38.502183
2232.391548	103227.232817	38.507200
2234.217193	103411.779980	38.512218
2236.993660	103583.348273	38.517236
2239.292123	103753.724329	38.522253
2241.558432	103923.725912	38.527271
2244.085808	104099.063490	38.532288
2246.115498	104279.729060	38.537306
2248.574434	104446.178331	38.542324
2250.728691	104619.941379	38.547341
2252.937535	104788.168548	38.552359
2255.117326	104961.891330	38.557376
2257.748663	105143.316945	38.562394
2260.144346	105320.887752	38.567412
2262.340185	105499.365658	38.572429
2264.805705	105659.530761	38.577447
2266.892263	105844.735182	38.582464
2268.850411	106012.703352	38.587482
2271.439780	106190.806333	38.592500
2273.507051	106365.086476	38.597517
2275.553058	106542.654980	38.602535
2278.157753	106723.091483	38.607552
2280.557135	106898.945455	38.612570
2282.831675	107091.431050	38.617588
2284.820867	107267.566650	38.622605
2287.306333	107444.956958	38.627623
2289.461474	107627.307211	38.632640
2291.664964	107802.372221	38.637658
2294.334592	107980.725562	38.642676
2296.255502	108160.693276	38.647693
2298.414394	108328.831592	38.652711
2300.684998	108528.312917	38.657728
2302.951025	108709.801912	38.662746
2305.328574	108888.053444	38.667764
2307.672798	109086.816321	38.672781
2309.986913	109265.548904	38.677799
2312.049585	109451.144202	38.682816
2313.863717	109639.936992	38.687834
2316.387485	109823.065372	38.692852
2318.447362	110003.160346	38.697869
2321.076121	110175.038451	38.702887
2323.201839	110343.584774	38.707904
2325.212721	110517.323936	38.712922
2327.016773	110693.277545	38.717940
2329.174959	110879.486828	38.722957
2331.675183	111060.012888	38.727975
2333.602394	111249.709680	38.732992
2336.124726	111435.357638	38.738010
2338.450563	111627.593866	38.743028
2340.448648	111831.993723	38.748045
2342.955470	112026.816281	38.753063
2345.264589	112218.538336	38.758080
2347.647061	112434.612488	38.763098
2349.898611	112633.194165	38.768116
2351.898078	112839.818945	38.773133
2354.538695	113049.768866	38.778151
2356.960176	113268.809605	38.783168
2359.160384	113480.035758	38.788186
2361.826568	113700.372495	38.793204
2363.812435	113913.283444	38.798221
2366.152256	114125.290516	38.803239
2368.623933	114358.243014	38.808256
2371.164139	114569.511073	38.813274
2373.757159	114803.487424	38.818292
2376.027530	115028.954627	38.823309
2379.121090	115239.784849	38.828327
2381.510783	115460.822274	38.833344
2383.694073	115683.986063	38.838362
2386.199629	115907.937888	38.843380
2388.518230	116133.987723	38.848397
2391.121104	116347.856274	38.853415
2393.739997	116572.948580	38.858432
2395.958605	116790.545358	38.863450
2398.488985	117026.067582	38.868468
2400.966572	117256.234259	38.873485
2403.218859	117472.726228	38.878503
2405.538637	117705.038558	38.883520
2407.980840	117937.041432	38.888538
2410.274002	118165.251102	38.893556
2413.032617	118393.059542	38.898573
2415.459431	118610.672306	38.903591
2418.362931	118855.128076	38.908608
2420.560823	119078.005301	38.913626
2423.239603	119302.051687	38.918644
2426.213072	119524.302804	38.923661
2428.941958	119728.644601	38.928679
2431.344308	119944.175800	38.933696
2433.760486	120150.687114	38.938714
2436.150740	120366.768015	38.943732
2438.684802	120590.362510	38.948749
2440.724488	120806.526072	38.953767
2443.119734	121033.100451	38.958784
2445.601086	121258.609806	38.963802
2447.991487	121479.009838	38.968820
2450.160605	121700.917226	38.973837
2452.503173	121931.551681	38.978855
2454.747048	122160.452329	38.983872
2457.009116	122391.038642	38.988890
2459.548617	122628.496581	38.993908
2461.783360	122853.355952	38.998925
2464.339711	123090.509568	39.003943
2466.692670	123327.062121	39.008960
2468.614681	123574.365060	39.013978
2471.219617	123823.846186	39.018996
2473.513178	124067.453162	39.024013
2475.906476	124307.811037	39.029031
2477.933543	124555.623725	39.034048
2480.040344	124799.568815	39.039066
2482.899839	125013.406965	39.044084
2484.931014	125254.880094	39.049101
2487.031976	125480.840774	39.054119
2489.529808	125716.001860	39.059136
2491.647729	125960.865619	39.064154
2494.247235	126201.088273	39.069172
2496.280519	126459.327424	39.074189
2499.123118	126706.137543	39.079207
2501.291131	126965.120006	39.084224
2503.553417	127231.371732	39.089242
2506.162651	127491.354184	39.094260
2508.352061	127772.528206	39.099277
2510.819290	128046.974437	39.104295
2512.960957	128331.255398	39.109312
2515.455101	128608.606520	39.114330
2517.924017	128891.964648	39.119348
2520.112978	129190.733251	39.124365
2522.717553	129480.367195	39.129383
2525.318591	129778.441093	39.134400
2527.472798	130086.813457	39.139418
2530.703838	130389.677941	39.144436
2533.033907	130700.437946	39.149453
2536.498790	131009.956875	39.154471
2538.850116	131334.104201	39.159488
2541.107122	131634.287616	39.164506
2543.886891	131938.921126	39.169524
2546.101928	132251.410514	39.174541
2549.108118	132570.617578	39.179559
2551.808336	132874.648306	39.184576
2554.227622	133198.126335	39.189594
2556.999661	133495.260060	39.194612
2559.551245	133810.182213	39.199629
2562.589586	134121.705907	39.204647
2565.546835	134431.239568	39.209664
2567.926525	134737.858346	39.214682
2570.825586	135031.213714	39.219700
2573.474625	135343.542776	39.224717
2576.166435	135639.573923	39.229735
2579.274867	135941.137962	39.234752
2581.849126	136235.084897	39.239770
2584.753769	136531.964147	39.244788
2586.954838	136833.574487	39.249805
2589.801015	137132.103758	39.254823
2592.797860	137428.136835	39.259840
2594.863604	137728.200622	39.264858
2597.308161	138023.854353	39.269876
2599.711546	138327.549349	39.274893
2602.435556	138632.122562	39.279911
2605.085036	138939.691664	39.284928
2607.229239	139249.143862	39.289946
2610.071801	139561.991461	39.294964
2612.357844	139878.012010	39.299981
2614.808543	140194.262715	39.304999
2617.011762	140506.543906	39.310016
2619.497136	140830.103324	39.315034
2622.283688	141147.234213	39.320052
2624.737492	141479.153621	39.325069
2627.620330	141809.700996	39.330087
2630.019103	142132.901918	39.335104
2631.973998	142475.592213	39.340122
2634.316519	142802.436079	39.345140
2636.689557	143151.766767	39.350157
2639.303966	143499.298024	39.355175
2641.928485	143846.576292	39.360192
2644.363851	144202.478920	39.365210
2646.928822	144560.013748	39.370228
2649.169039	144898.957356	39.375245
2652.091417	145245.881392	39.380263
2654.324599	145576.530002	39.385280
2656.702872	145917.197627	39.390298
2659.317836	146258.985495	39.395316
2661.724792	146598.637761	39.400333
2664.212555	146944.549713	39.405351
2666.839003	147299.479399	39.410368
2668.940185	147663.518145	39.415386
2672.025315	148021.617617	39.420404
2674.151011	148389.516154	39.425421
2676.676371	148764.805490	39.430439
2679.305406	149149.943742	39.435456
2681.809913	149538.531387	39.440474
2684.509001	149922.991496	39.445492
2686.734696	150310.917495	39.450509
2689.482620	150711.610300	39.455527
2692.355833	151106.206266	39.460544
2695.008484	151511.172140	39.465562
2698.131250	151912.513226	39.470580
2700.181155	152333.103751	39.475597
2702.650862	152757.249534	39.480615
2705.463728	153173.880796	39.485632
2708.054220	153598.420225	39.490650
2711.003888	154017.181586	39.495668
2714.107839	154441.545432	39.500685
2716.992975	154871.455977	39.505703
2719.850786	155304.623763	39.510720
2722.376911	155740.626750	39.515738
2725.306594	156163.900632	39.520756
2727.782374	156596.909219	39.525773
2730.548106	157038.914316	39.530791
2733.612787	157480.165013	39.535808
2736.434567	157917.546884	39.540826
2738.768221	158365.126242	39.545844
2741.350111	158813.863409	39.550861
2744.254941	159252.828774	39.555879
2747.080548	159699.325305	39.560896
2749.629645	160164.124349	39.565914
2752.491562	160607.397055	39.570932
2755.482606	161067.702919	39.575949
2758.279056	161526.125501	39.580967
2761.060254	161984.845759	39.585984
2763.497251	162449.222012	39.591002
2766.154913	162901.163087	39.596020
2769.085553	163377.999705	39.601037
2771.799659	163843.574042	39.606055
2774.758662	164315.359907	39.611072
2777.572645	164786.473482	39.616090
2780.682362	165249.126355	39.621108
2783.369088	165719.606115	39.626125
2786.068136	166191.483809	39.631143
2788.531209	166657.611940	39.636160
2791.361001	167133.017978	39.641178
2794.488418	167598.819945	39.646196
2797.341397	168079.536041	39.651213
2800.055567	168553.611140	39.656231
2803.110904	169023.204711	39.661248
2805.794777	169508.705537	39.666266
2808.344491	169975.210024	39.671284
2811.456846	170461.323092	39.676301
2813.961711	170939.776200	39.681319
2816.894555	171415.892564	39.686336
2819.435016	171901.647292	39.691354
2822.271196	172382.978153	39.696372
2825.017422	172869.430593	39.701389
2827.743051	173352.143427	39.706407
2830.594731	173830.433333	39.711424
2833.189963	174317.845306	39.716442
2835.743516	174792.594078	39.721460
2838.176683	175244.126842	39.726477
2841.178592	175718.379172	39.731495
2843.862593	176186.131632	39.736512
2846.473250	176649.999796	39.741530
2849.029994	177134.323446	39.746548
2852.095633	177616.538514	39.751565
2854.234941	178104.691727	39.756583
2857.372682	178591.802640	39.761600
2859.741421	179091.379699	39.766618
2862.355046	179599.988229	39.771636
2865.375807	180109.196324	39.776653
2867.924029	180627.548238	39.781671
2870.659706	181146.000765	39.786688
2873.021931	181675.410424	39.791706
2875.658840	182199.319479	39.796724
2878.735903	182747.037151	39.801741
2881.721653	183277.450380	39.806759
2884.486480	183886.967377	39.811776
2887.557299	184446.607619	39.816794
2890.894307	184990.969938	39.821812
2894.119960	185546.858428	39.826829
2896.622891	186093.389007	39.831847
2900.119304	186644.034192	39.836864
2903.289253	187193.006132	39.841882
2906.010365	187737.326733	39.846900
2908.920305	188286.878294	39.851917
2911.607350	188857.930421	39.856935
2914.512342	189404.567285	39.861952
2917.244815	189983.669829	39.866970
2920.350497	190550.042136	39.871988
2923.361269	191108.862679	39.877005
2926.384586	191685.134073	39.882023
2929.365637	192255.090036	39.887040
2932.087475	192833.395232	39.892058
2935.081451	193406.275530	39.897076
2938.192880	193979.089221	39.902093
2940.631247	194568.496036	39.907111
2944.114306	195157.056255	39.912128
2947.846272	195734.759120	39.917146
2950.890778	196310.184170	39.922164
2953.683919	196878.208216	39.927181
2956.897156	197455.948459	39.932199
2960.264910	198021.042128	39.937216
2963.314574	198596.094406	39.942234
2966.602805	199156.734023	39.947252
2969.886732	199723.498221	39.952269
2972.648844	200301.319763	39.957287
2975.865594	200863.170449	39.962304
2978.588048	201429.520326	39.967322
2981.640728	201996.557106	39.972340
2984.674403	202560.118551	39.977357
2987.517450	203123.813186	39.982375
2990.927739	203686.404733	39.987392
2993.631949	204259.371069	39.992410
2996.277503	204837.962285	39.997428
2998.672321	205415.552870	40.002445
3001.236935	205991.543543	40.007463
3004.409735	206579.049846	40.012480
3007.364519	207181.579636	40.017498
3010.234732	207768.780766	40.022516
3012.943808	208359.463408	40.027533
3015.392473	208965.862031	40.032551
3017.991097	209573.102385	40.037568
3021.239014	210192.944313	40.042586
3024.096914	210808.682487	40.047604
3027.211922	211414.652261	40.052621
3030.156809	212028.194737	40.057639
3033.324642	212615.385451	40.062656
3036.032451	213201.506008	40.067674
3038.825890	213788.046053	40.072692
3042.002750	214371.351644	40.077709
3044.595190	214976.139498	40.082727
3047.700369	215555.672932	40.087744
3050.698201	216166.267435	40.092762
3053.376773	216773.254537	40.097780
3056.400909	217377.368537	40.102797
3059.067541	218004.072428	40.107815
3062.032084	218627.021457	40.112832
3064.884799	219261.369587	40.117850
3067.650930	219890.422413	40.122868
3070.805961	220533.133118	40.127885
3073.296749	221196.449231	40.132903
3076.637556	221845.736847	40.137920
3079.372290	222516.281178	40.142938
3082.466168	223180.291613	40.147956
3085.130602	223847.722767	40.152973
3088.680644	224537.549019	40.157991
3091.526020	225227.307718	40.163008
3094.456721	225915.554240	40.168026
3097.382879	226610.381057	40.173044
3101.298175	227300.124653	40.178061
3103.846976	228010.404947	40.183079
3107.188989	228715.632482	40.188096
3110.794966	229417.566606	40.193114
3114.187488	230116.535936	40.198132
3117.868456	230814.418019	40.203149
3120.998347	231517.847468	40.208167
3124.043398	232208.993921	40.213184
3127.649200	232910.213442	40.218202
3130.627868	233622.504583	40.223220
3134.249126	234314.752196	40.228237
3137.378956	235014.544309	40.233255
3140.724274	235705.740495	40.238272
3143.972301	236422.557609	40.243290
3146.970406	237118.200351	40.248308
3150.168859	237819.932630	40.253325
3153.672368	238518.668885	40.258343
3156.549668	239217.780915	40.263360
3160.097233	239932.714415	40.268378
3162.951553	240643.308894	40.273396
3166.452013	241349.507285	40.278413
3169.552823	242059.906929	40.283431
3172.762750	242757.712884	40.288448
3175.924544	243472.112481	40.293466
3178.459305	244184.042149	40.298484
3182.196930	244895.247925	40.303501
3185.237940	245616.518097	40.308519
3188.454165	246333.516028	40.313536
3191.594850	247057.737464	40.318554
3194.839871	247770.280034	40.323572
3198.509341	248487.503691	40.328589
3201.528718	249206.629639	40.333607
3205.000323	249924.335529	40.338624
3208.358522	250640.862145	40.343642
3211.266756	251359.691304	40.348660
3214.778090	252066.839615	40.353677
3217.758793	252786.666877	40.358695
3220.547198	253497.376137	40.363712
3223.699222	254227.812808	40.368730
3227.136366	254958.912354	40.373748
3230.420530	255677.737746	40.378765
3233.618590	256404.066073	40.383783
3236.960721	257126.913326	40.388800
3240.229552	257843.798778	40.393818
3242.808199	258559.187808	40.398836
3246.234959	259264.940271	40.403853
3248.932469	259960.540872	40.408871
3252.400175	260658.379156	40.413888
3255.483698	261353.428486	40.418906
3258.532802	262049.748923	40.423924
3261.861781	262759.051291	40.428941
3264.011572	263473.841923	40.433959
3267.080544	264191.455783	40.438976
3270.092621	264919.715899	40.443994
3273.193897	265663.170932	40.449012
3276.405157	266408.025637	40.454029
3279.489633	267169.683074	40.459047
3282.435391	267917.336312	40.464064
3285.921000	268683.922582	40.469082
3289.031354	269455.767872	40.474100
3292.566895	270216.466791	40.479117
3296.002016	270982.025981	40.484135
3299.888492	271753.578012	40.489152
3303.460206	272518.721602	40.494170
3306.886507	273293.658968	40.499188
3310.295583	274068.464980	40.504205
3313.913584	274851.662772	40.509223
3316.991328	275635.902641	40.514240
3320.356924	276413.004445	40.519258
3323.165658	277206.946917	40.524276
3326.565403	277996.700299	40.529293
3330.073232	278796.942333	40.534311
3333.442056	279589.782387	40.539328
3336.739281	280390.548401	40.544346
3339.654293	281199.872631	40.549364
3342.985935	282011.890701	40.554381
3346.216350	282832.930228	40.559399
3349.368848	283670.173480	40.564416
3352.712137	284494.858033	40.569434
3355.765693	285334.915317	40.574452
3359.688419	286171.093615	40.579469
3362.643135	287013.760886	40.584487
3366.063441	287853.322984	40.589504
3369.329691	288700.769751	40.594522
3372.641417	289546.801728	40.599540
3376.213516	290388.744568	40.604557
3379.926191	291254.394291	40.609575
3383.553195	292109.229066	40.614592
3386.937123	292955.508106	40.619610
3390.242542	293813.949105	40.624628
3394.042619	294666.867116	40.629645
3397.546000	295521.215521	40.634663
3401.125338	296378.332203	40.639680
3404.646719	297222.141833	40.644698
3408.332263	298070.305296	40.649716
3411.862046	298921.907549	40.654733
3415.892201	299762.756006	40.659751
3419.440970	300606.205455	40.664768
3422.919617	301453.714496	40.669786
3426.449198	302286.326169	40.674804
3429.948741	303127.052726	40.679821
3433.515008	303966.460732	40.684839
3436.673139	304805.132033	40.689856
3440.039098	305633.806595	40.694874
3443.310453	306479.870174	40.699892
3447.060982	307318.635766	40.704909
3450.441911	308147.291893	40.709927
3453.910337	308995.617048	40.714944
3457.572132	309825.571495	40.719962
3461.000507	310663.086430	40.724980
3464.746514	311498.608061	40.729997
3467.862413	312336.015453	40.735015
3471.092433	313151.287364	40.740020
3474.566806	313937.038454	40.745024
3477.960981	314683.910024	40.750029
3480.823472	315372.688095	40.755034
3484.064027	316022.977076	40.760039
3486.987742	316607.790356	40.765044
3489.738884	317149.446632	40.770048
3492.357599	317644.277451	40.775053
3495.137803	318084.427647	40.780058
3497.394170	318479.394070	40.785063
3499.125901	318818.543392	40.790068
3501.358902	319107.059254	40.795072
3503.018499	319367.600924	40.800077
3505.047460	319588.776447	40.805082
3506.730060	319760.699917	40.810087
3507.644455	319883.132578	40.815092
3509.581478	319993.905646	40.820096
3511.132285	320063.702419	40.825101
3511.984112	320098.805044	40.830106
3513.091247	320118.857531	40.835111
3514.390177	320109.800949	40.840116
3514.938186	320058.426112	40.845120
3515.157463	319994.763680	40.850125
3516.253131	319912.366677	40.855130
3517.119230	319804.869509	40.860135
3517.698335	319683.475128	40.865140
3518.591156	319556.510590	40.870144
3519.008505	319399.802659	40.875149
3519.476389	319217.797375	40.880154
3519.878580	319044.375434	40.885159
3520.233817	318853.379892	40.890164
3521.123145	318631.515345	40.895168
3520.753093	318423.534362	40.900173
3520.862988	318196.293989	40.905178
3521.499225	317971.972341	40.910183
3521.284454	317743.457387	40.915188
3521.361132	317499.910031	40.920192
3521.397179	317248.785767	40.925197
3521.302614	316990.632836	40.930202
3521.732062	316725.247007	40.935207
3521.502969	316476.602362	40.940212
3521.583550	316204.347449	40.945216
3521.361390	315952.289410	40.950221
3521.543736	315682.050897	40.955226
3521.342287	315402.507475	40.960231
3521.304812	315142.528482	40.965236
3521.322876	314862.921971	40.970240
3521.221005	314601.092535	40.975245
3521.465761	314312.287302	40.980250
3520.985925	314036.468447	40.985255
3520.883993	313763.438655	40.990260
3521.100067	313491.935109	40.995264
3520.671727	313212.413777	41.000269
3520.371227	312941.114986	41.005274
3520.113488	312674.871533	41.010279
3520.052457	312408.010564	41.015284
3520.130541	312139.879495	41.020288
3519.521266	311866.892447	41.025293
3519.920907	311598.402673	41.030298
3519.253391	311340.002138	41.035303
3519.158512	311085.098571	41.040308
3519.514469	310810.784009	41.045312
3519.201177	310564.207276	41.050317
3519.166314	310299.009787	41.055322
3519.010167	310034.262387	41.060327
3518.530771	309779.361084	41.065332
3518.947318	309517.116884	41.070336
3518.612482	309261.375949	41.075341
3518.517771	309000.913842	41.080346
3518.191282	308754.609849	41.085351
3517.909936	308501.630323	41.090356
3518.026192	308253.829536	41.095360
3517.641516	307995.875830	41.100365
3517.922340	307748.148562	41.105370
3517.390829	307513.881792	41.110375
3516.940197	307272.882974	41.115380
3516.972556	307031.756583	41.120384
3516.806403	306797.480218	41.125389
3516.485949	306560.020373	41.130394
3516.647307	306327.395655	41.135399
3516.155681	306097.849446	41.140404
3516.434140	305866.171344	41.145408
3515.735431	305645.817028	41.150413
3515.819230	305411.546043	41.155418
3515.532739	305186.289972	41.160423
3515.198140	304972.772537	41.165428
3514.814760	304745.341035	41.170432
3514.904688	304539.746529	41.175437
3514.743463	304320.880338	41.180442
3514.708862	304129.199131	41.185447
3514.115303	303930.224168	41.190452
3514.225850	303715.613941	41.195456
3513.711244	303516.370550	41.200461
3513.550492	303315.722223	41.205466
3513.603974	303135.119812	41.210471
3513.251591	302948.472172	41.215476
3513.333302	302751.474066	41.220480
3513.176691	302571.284318	41.225485
3512.941389	302376.039549	41.230490
3512.920502	302201.350086	41.235495
3512.857765	302009.334665	41.240500
3512.700126	301823.365226	41.245504
3512.551993	301649.737327	41.250509
3512.418435	301467.860474	41.255514
3512.632601	301291.604225	41.260519
3512.235174	301119.286133	41.265524
3512.255147	300944.738880	41.270528
3511.873676	300770.991911	41.275533
3511.988928	300595.741451	41.280538
3511.697164	300428.953034	41.285543
3511.565283	300257.659641	41.290548
3511.759501	300087.332791	41.295552
3511.413825	299927.346845	41.300557
3511.000963	299765.003921	41.305562
3511.239668	299611.950377	41.310567
3511.032763	299449.625225	41.315572
3511.148875	299282.235053	41.320576
3510.770427	299146.864017	41.325581
3510.378593	298982.530237	41.330586
3510.419113	298823.498789	41.335591
3510.244969	298680.128134	41.340596
3510.168661	298530.938684	41.345600
3509.842809	298392.274234	41.350605
3509.927461	298247.742102	41.355610
3509.632203	298099.272945	41.360615
3509.544398	297963.497256	41.365620
3509.417735	297815.739116	41.370624
3509.107309	297694.123800	41.375629
3509.121232	297556.065933	41.380634
3509.003332	297429.100318	41.385639
3509.129611	297300.594524	41.390644
3508.897143	297165.017700	41.395648
3508.808553	297051.714887	41.400653
3508.399434	296918.481314	41.405658
3508.965680	296790.491003	41.410663
3508.580241	296669.114295	41.415668
3508.586607	296542.687244	41.420672
3508.055124	296438.208362	41.425677
3507.976921	296311.972196	41.430682
3508.144796	296194.325976	41.435687
3507.955297	296093.865543	41.440692
3508.372941	295968.721962	41.445696
3507.542240	295846.980419	41.450701
3507.767248	295728.280723	41.455706
3507.552491	295626.958005	41.460711
3507.687630	295521.660543	41.465716
3507.656348	295405.214724	41.470720
3507.739333	295307.561144	41.475725
3507.457619	295194.717584	41.480730
3507.585955	295092.576683	41.485735
3507.302943	294982.329208	41.490740
3507.276944	294879.702986	41.495744
3506.939752	294780.281531	41.500749
3507.070300	294672.845122	41.505754
3507.008713	294576.078362	41.510759
3506.741071	294489.958028	41.515764
3506.633114	294386.656497	41.520768
3506.662783	294293.744041	41.525773
3506.306389	294192.670073	41.530778
3506.476589	294097.368093	41.535783
3506.357616	294010.002011	41.540788
3506.475575	293919.035147	41.545792
3506.313321	293842.468236	41.550797
3506.071522	293750.819182	41.555802
3506.254567	293655.081760	41.560807
3506.003351	293574.430241	41.565812
3505.987850	293482.159942	41.570816
3505.790803	293402.899723	41.575821
3505.799425	293312.890850	41.580826
3505.809930	293239.147075	41.585831
3505.688564	293160.052886	41.590836
3505.530768	293071.087856	41.595840
3505.039415	293003.938662	41.600845
3505.577738	292923.061013	41.605850
3505.517995	292849.607747	41.610855
3504.997518	292774.520946	41.615860
3505.476894	292695.714052	41.620864
3505.185937	292618.783878	41.625869
3505.450235	292552.126963	41.630874
3505.174659	292474.914197	41.635879
3505.158902	292398.831644	41.640884
3505.298787	292324.099235	41.645888
3505.189441	292259.282267	41.650893
3505.096050	292180.844257	41.655898
3505.358798	292105.965097	41.660903
3505.162641	292036.248623	41.665908
3505.005410	291967.926019	41.670912
3504.906346	291893.866821	41.675917
3504.647161	291827.418231	41.680922
3504.697520	291764.535824	41.685927
3504.502823	291698.866126	41.690932
3505.034163	291625.853536	41.695936
3504.635988	291570.906751	41.700941
3504.642770	291506.350840	41.705946
3504.674491	291434.587081	41.710951
3504.670552	291377.542056	41.715956
3504.576770	291317.303637	41.720960
3504.222909	291253.847518	41.725965
3504.510134	291188.356488	41.730970
3504.534815	291129.804886	41.735975
3504.428660	291073.411950	41.740980
3504.367910	291017.648253	41.745984
3504.015944	290961.726391	41.750989
3504.366576	290886.984745	41.755994
3504.368300	290830.803823	41.760999
3504.242115	290778.766669	41.766004
3504.287997	290713.516516	41.771008
3504.065940	290671.218339	41.776013
3503.927076	290610.578992	41.781018
3503.798141	290555.334656	41.786023
3503.788567	290498.238795	41.791028
3504.009741	290440.317675	41.796032
3503.696556	290400.884614	41.801037
3503.973596	290342.700113	41.806042
3503.858342	290292.315475	41.811047
3503.793545	290244.646690	41.816052
3503.849877	290191.587733	41.821056
3503.675919	290142.790420	41.826061
3503.793665	290090.561822	41.831066
3503.229571	290042.640016	41.836071
3503.409774	290001.347650	41.841076
3503.577421	289945.980044	41.846080
3503.038643	289909.254825	41.851085
3503.318555	289856.644296	41.856090
3503.732799	289810.554933	41.861095
3503.348713	289770.979826	41.866100
3503.270932	289719.672453	41.871104
3503.558610	289676.784794	41.876109
3503.726970	289624.344249	41.881114
3503.423364	289579.690666	41.886119
3503.232871	289543.063521	41.891124
3503.534996	289487.827228	41.896128
3503.195136	289448.626847	41.901133
3502.817454	289400.599042	41.906138
3503.254119	289369.754139	41.911143
3502.880510	289330.126206	41.916148
3503.045887	289281.911585	41.921152
3502.881187	289252.917126	41.926157
3503.032197	289214.276266	41.931162
3502.883457	289177.744209	41.936167
3503.084025	289145.357816	41.941172
3503.093112	289088.385046	41.946176
3502.996872	289056.579594	41.951181
3502.768574	289016.317796	41.956186
3503.070742	288979.282372	41.961191
3503.136500	288938.719988	41.966196
3503.114149	288903.695399	41.971200
3503.018391	288866.569383	41.976205
3503.168345	288813.494639	41.981210
3503.128180	288774.908859	41.986215
3502.862364	288740.889592	41.991220
3502.968788	288700.855287	41.996224
3503.048202	288673.909835	42.001229
3502.832770	288635.784134	42.006234
3503.102371	288603.793980	42.011239
3502.821387	288560.052584	42.016244
3503.105526	288507.694850	42.021248
3502.578978	288477.865631	42.026253
3502.600565	288437.691686	42.031258
3502.537793	288398.167320	42.036263
3502.956932	288374.503450	42.041268
3503.181600	288340.941880	42.046272
3502.778668	288306.841993	42.051277
3502.771399	288266.036036	42.056282
3503.060638	288231.344219	42.061287
3502.672152	288188.383080	42.066292
3502.762449	288151.863983	42.071296
3502.664228	288121.407586	42.076301
3502.722335	288083.086054	42.081306
3502.435151	288047.389616	42.086311
3502.232938	288022.015328	42.091316
3502.372553	287988.746897	42.096320
3502.419523	287964.861038	42.101325
3502.214290	287935.948693	42.106330
3502.252553	287904.223473	42.111335
3502.193087	287873.760902	42.116340
3502.439366	287837.904577	42.121344
3502.354844	287814.013764	42.126349
3501.988422	287769.597856	42.131354
3501.984284	287768.682018	42.136359
3501.863949	287747.622492	42.141364
3502.357401	287713.789465	42.146368
3502.283385	287708.073195	42.151373
3502.244841	287675.825277	42.156378
3502.222670	287653.502986	42.161383
3501.684205	287620.518576	42.166388
3502.197106	287580.878257	42.171392
3501.818364	287569.812742	42.176397
3501.690785	287537.985987	42.181402
3501.824099	287517.319500	42.186407
3501.497551	287495.044741	42.191412
3502.117072	287472.062012	42.196416
3501.737305	287456.948975	42.201421
3501.893647	287436.380691	42.206426
3502.257001	287414.558100	42.211431
3501.946915	287394.190008	42.216436
3501.780025	287364.354963	42.221440
3501.961004	287355.467581	42.226445
3501.737743	287327.779724	42.231450
3502.342227	287300.038817	42.236455
3501.999004	287282.374321	42.241460
3501.835785	287251.291254	42.246464
3501.678193	287229.855530	42.251469
3501.460879	287216.397208	42.256474
3501.559835	287193.037539	42.261479
3501.435837	287175.822426	42.266484
3501.567090	287155.792576	42.271488
3501.422400	287148.610794	42.276493
3501.463719	287119.481343	42.281498
3501.527907	287105.571674	42.286503
3501.436269	287091.559078	42.291508
3501.812024	287075.411379	42.296512
3501.628383	287066.886449	42.301517
3501.711394	287051.904625	42.306522
3501.912062	287040.213836	42.311527
3501.820993	287011.130492	42.316532
3501.944721	286984.381072	42.321536
3501.484219	286965.283766	42.326541
3501.613868	286944.108529	42.331546
3501.990703	286924.931217	42.336551
3501.834762	286911.514152	42.341556
3501.922419	286887.239682	42.346560
3501.712442	286868.688697	42.351565
3501.691355	286840.714456	42.356570
3501.684714	286821.291579	42.361575
3501.323521	286810.834166	42.366580
3501.471965	286787.772104	42.371584
3501.417540	286780.321598	42.376589
3502.137393	286762.185274	42.381594
3501.856723	286740.463147	42.386599
3501.538101	286725.849528	42.391604
3501.624248	286706.335740	42.396608
3501.725880	286695.042232	42.401613
3501.700390	286663.682784	42.406618
3501.768354	286649.186911	42.411623
3501.426477	286631.445658	42.416628
3501.450477	286617.796743	42.421632
3501.547387	286608.107770	42.426637
3501.580301	286581.856075	42.431642
3501.552747	286566.815056	42.436647
3501.299575	286553.667693	42.441652
3501.486888	286534.723558	42.446656
3501.399608	286521.575710	42.451661
3501.334328	286507.966188	42.456666
3501.359219	286492.535093	42.461671
3501.342298	286486.707962	42.466676
3501.468396	286460.441651	42.471680
3501.075096	286449.760084	42.476685
3501.174558	286445.416740	42.481690
3501.349160	286432.737081	42.486695
3501.341596	286421.256939	42.491700
3501.577335	286394.286111	42.496704
3501.804265	286380.579964	42.501709
3501.733321	286357.399308	42.506714
3501.688743	286349.412608	42.511719
3501.475185	286328.443577	42.516724
3501.879734	286305.214021	42.521728
3501.718935	286290.193772	42.526733
3501.388085	286276.523892	42.531738
3501.951037	286254.338768	42.536743
3501.380377	286242.208363	42.541748
3501.012173	286217.037534	42.546752
3501.469292	286205.357419	42.551757
3501.577330	286195.182955	42.556762
3501.584121	286182.860431	42.561767
3501.402280	286172.476707	42.566772
3501.583259	286159.235934	42.571776
3501.635078	286137.843492	42.576781
3501.402960	286124.387263	42.581786
3501.605435	286104.727825	42.586791
3501.367058	286092.469071	42.591796
3501.476168	286081.021545	42.596800
3501.515799	286073.556255	42.601805
3501.270850	286048.315178	42.606810
3501.377163	286047.687538	42.611815
3501.483454	286031.428969	42.616820
3501.605262	286005.035863	42.621824
3501.545656	285995.753135	42.626829
3501.590684	285973.139738	42.631834
3501.481046	285965.519570	42.636839
3501.351909	285947.261181	42.641844
3501.559901	285918.308809	42.646848
3501.183706	285914.345286	42.651853
3501.330431	285890.366710	42.656858
3501.495790	285883.110861	42.661863
3501.495148	285877.815741	42.666868
3501.747796	285851.860357	42.671872
3501.574830	285845.497498	42.676877
3501.458812	285820.159806	42.681882
3501.425682	285811.916675	42.686887
3501.308003	285804.705068	42.691892
3501.414436	285784.678687	42.696896
3501.409907	285768.870160	42.701901
3501.347110	285750.295855	42.706906
3501.619371	285730.396278	42.711911
3501.677598	285718.829358	42.716916
3501.817591	285704.831174	42.721920
3501.744714	285694.226679	42.726925
3501.838753	285671.121824	42.731930
3501.754805	285650.437810	42.736935
3501.623260	285640.478922	42.741940
3501.818188	285602.821924	42.746944
3501.407687	285600.416666	42.751949
3501.582385	285577.095506	42.756954
3501.564976	285558.310391	42.761959
3501.272018	285542.877854	42.766964
3501.811400	285527.773426	42.771968
3501.475807	285512.271174	42.776973
3501.119829	285493.997212	42.781978
3501.536662	285475.806085	42.786983
3501.360109	285468.781851	42.791988
3501.448036	285444.837767	42.796993
3501.527972	285442.101251	42.801997
3501.656583	285429.097642	42.807002
3501.834131	285407.914432	42.812007
3501.256419	285401.182027	42.817012
3501.568674	285376.184537	42.822017
3501.408763	285358.516330	42.827021
3501.440448	285345.171449	42.832026
3501.330224	285330.015789	42.837031
3501.247472	285323.486031	42.842036
3501.454939	285315.612550	42.847041
3501.255858	285291.815115	42.852045
3501.290332	285281.601098	42.857050
3501.463886	285277.984373	42.862055
3501.353483	285263.185136	42.867060
3501.750446	285242.934969	42.872065
3501.418891	285220.227449	42.877069
3501.473433	285201.227323	42.882074
3501.534006	285203.254444	42.887079
3501.232604	285182.069669	42.892084
3501.318713	285158.278516	42.897089
3501.462367	285160.470855	42.902093
3501.282022	285148.839304	42.907098
3501.640984	285132.311896	42.912103
3501.266790	285116.510095	42.917108
3501.428088	285096.474933	42.922113
3501.231606	285084.896810	42.927117
3500.907237	285074.815238	42.932122
3501.324582	285065.177778	42.937127
3501.340743	285047.176468	42.942132
3501.425321	285037.769235	42.947137
3501.264130	285028.756835	42.952141
3501.468439	285009.784157	42.957146
3501.708714	284996.381140	42.962151
3501.619228	284982.418683	42.967156
3501.327406	284965.585651	42.972161
3501.258663	284962.388659	42.977165
3501.159684	284947.383903	42.982170
3501.077221	284926.343026	42.987175
3501.256478	284911.320221	42.992180
3501.300726	284914.648260	42.997185
3501.051891	284899.794212	43.002189
3501.154552	284877.731516	43.007194
3501.498957	284871.160391	43.012199
3501.088559	284872.904741	43.017204
3501.466759	284848.380450	43.022209
3501.263758	284836.777846	43.027213
3501.409036	284829.626856	43.032218
3501.624347	284802.582215	43.037223
3501.358699	284801.325350	43.042228
3501.505266	284780.274079	43.047233
3501.394696	284764.940141	43.052237
3501.459263	284749.400614	43.057242
3501.600565	284736.267599	43.062247
3501.503585	284721.618894	43.067252
3501.449504	284717.834063	43.072257
3501.211869	284700.610624	43.077261
3501.166261	284686.844911	43.082266
3501.356998	284681.952566	43.087271
3501.213071	284660.182932	43.092276
3501.667563	284644.175091	43.097281
3501.299653	284639.319165	43.102285
3501.167613	284622.511984	43.107290
3501.578652	284602.844964	43.112295
3501.290988	284601.209665	43.117300
3501.175345	284581.217651	43.122305
3501.131681	284574.885374	43.127309
3501.231998	284556.641656	43.132314
3501.402057	284553.916473	43.137319
3500.977730	284539.980817	43.142324
3501.158486	284521.088061	43.147329
3501.248683	284510.890675	43.152333
3501.131797	284516.025993	43.157338
3501.577045	284492.382127	43.162343
3501.286431	284485.324706	43.167348
3501.378989	284467.795005	43.172353
3501.131178	284452.635203	43.177357
3501.250976	284447.677557	43.182362
3501.422101	284433.241457	43.187367
3501.157864	284428.292933	43.192372
3501.381660	284399.082864	43.197377
3501.070262	284388.311792	43.202381
3501.110120	284388.229148	43.207386
3501.153449	284371.623613	43.212391
3501.187910	284361.434919	43.217396
3501.224242	284351.856928	43.222401
3500.913127	284357.939117	43.227405
3501.167960	284331.091777	43.232410
3501.378240	284313.238134	43.237415
3500.969185	284314.040335	43.242420
3501.272589	284310.225051	43.247425
3501.229420	284289.839748	43.252429
3500.723674	284278.513505	43.257434
3500.994245	284268.084219	43.262439
3500.816667	284264.853293	43.267444
3501.015930	284267.291549	43.272449
3501.225902	284266.596771	43.277453
3501.167784	284244.762674	43.282458
3501.139079	284230.281398	43.287463
3500.739943	284233.016874	43.292468
3501.038226	284225.510944	43.297473
3500.918637	284209.058131	43.302477
3501.077014	284188.768581	43.307482
3501.119670	284186.572466	43.312487
3501.294209	284187.079764	43.317492
3501.104697	284172.012618	43.322497
3501.110126	284162.413974	43.327501
3501.101472	284146.147469	43.332506
3501.160242	284149.167775	43.337511
3501.214554	284155.880224	43.342516
3501.449641	284138.048115	43.347521
3501.074868	284129.501779	43.352525
3501.009768	284115.535334	43.357530
3501.339139	284101.583590	43.362535
3501.240999	284088.386053	43.367540
3501.209945	284080.346056	43.372545
3501.152403	284075.645233	43.377549
3501.085716	284057.885741	43.382554
3501.169842	284038.931586	43.387559
3501.393787	284033.804878	43.392564
3501.577938	284023.796399	43.397569
3501.399939	284012.698914	43.402573
3500.997791	284002.298385	43.407578
3501.762219	283991.664557	43.412583
3501.308084	283967.677413	43.417588
3501.454851	283957.547478	43.422593
3501.059028	283942.334329	43.427597
3501.189560	283916.779178	43.432602
3501.327736	283915.993788	43.437607
3501.266950	283914.297545	43.442612
3501.435542	283896.221187	43.447617
3501.120029	283884.101387	43.452621
3501.244178	283873.924059	43.457626
3501.503954	283863.318192	43.462631
3501.063941	283854.629271	43.467636
3501.358082	283832.765431	43.472641
3501.331813	283827.346868	43.477645
3501.046758	283807.432032	43.482650
3501.300391	283794.306736	43.487655
3501.314792	283795.500990	43.492660
3501.102714	283784.637922	43.497665
3501.139463	283764.647304	43.502669
3501.021224	283754.202353	43.507674
3501.061140	283756.614622	43.512679
3501.134823	283740.258774	43.517684
3501.071294	283720.538406	43.522689
3501.319012	283725.336737	43.527693
3501.331078	283720.752300	43.532698
3501.364939	283689.993206	43.537703
3501.053942	283688.870702	43.542708
3501.459406	283668.160494	43.547713
3501.025251	283665.173321	43.552717
3500.956040	283638.529125	43.557722
3501.021733	283631.186787	43.562727
3500.825625	283632.795832	43.567732
3501.172239	283628.770088	43.572737
3500.907132	283628.175036	43.577741
3501.032911	283623.445523	43.582746
3501.170104	283594.146822	43.587751
3501.029525	283590.935538	43.592756
3501.044364	283592.995315	43.597761
3501.049271	283584.440470	43.602765
3501.067579	283556.051385	43.607770
3501.095596	283562.233374	43.612775
3501.004886	283549.849245	43.617780
3501.216643	283542.102185	43.622785
3501.013452	283535.234667	43.627789
3500.636508	283524.066373	43.632794
3501.203982	283520.693473	43.637799
3501.271239	283513.707296	43.642804
3501.207898	283501.446172	43.647809
3501.191777	283493.149187	43.652813
3501.068842	283488.611299	43.657818
3501.276558	283482.850627	43.662823
3501.465523	283480.631616	43.667828
3501.306855	283454.383214	43.672833
3501.045690	283452.871037	43.677837
3500.969637	283429.461062	43.682842
3501.333948	283416.165640	43.687847
3501.139359	283403.415848	43.692852
3501.528593	283398.619672	43.697857
3501.046454	283380.135745	43.702861
3501.078500	283363.455358	43.707866
3501.210195	283362.569141	43.712871
3501.177642	283362.752402	43.717876
3501.407738	283354.900620	43.722881
3501.321476	283331.008496	43.727885
3501.535577	283327.283496	43.732890
3501.240453	283306.606335	43.737895
3500.872169	283296.404076	43.742900
3501.214260	283283.137561	43.747905
3500.981223	283282.842995	43.752909
3501.010392	283267.563256	43.757914
3501.110805	283247.384329	43.762919
3501.131208	283247.024681	43.767924
3501.285418	283242.036111	43.772929
3501.449826	283238.420710	43.777933
3501.443429	283218.513059	43.782938
3501.541252	283201.771432	43.787943
3501.194070	283185.939508	43.792948
3501.113396	283171.771640	43.797953
3500.946386	283169.175477	43.802957
3500.858244	283162.977319	43.807962
3501.142997	283166.853388	43.812967
3501.031417	283147.445875	43.817972
3501.162165	283130.164453	43.822977
3501.287479	283128.108134	43.827981
3501.522380	283125.449134	43.832986
3501.420185	283092.496150	43.837991
3500.980293	283089.662600	43.842996
3501.336670	283082.656639	43.848001
3501.313232	283064.610089	43.853005
3501.264846	283051.175450	43.858010
3501.198292	283039.245710	43.863015
3501.162667	283022.932243	43.868020
3501.258590	283000.411750	43.873025
3501.115373	283013.799902	43.878029
3501.419188	283002.194132	43.883034
3501.306790	282979.197028	43.888039
3501.338289	282963.611355	43.893044
3501.203425	282961.162909	43.898049
3500.950942	282946.639977	43.903053
3501.126931	282931.184459	43.908058
3501.458827	282930.470607	43.913063
3500.963603	282917.258554	43.918068
3501.018387	282902.127483	43.923073
3500.980191	282904.017361	43.928077
3500.985640	282888.282992	43.933082
3501.374055	282879.897231	43.938087
3501.165408	282876.976603	43.943092
3501.049570	282859.988253	43.948097
3500.838591	282856.507897	43.953101
3501.000950	282856.991651	43.958106
3501.104470	282852.367400	43.963111
3501.083957	282852.854285	43.968116
3501.134103	282837.418421	43.973121
3501.042652	282812.584960	43.978125
3500.882772	282813.144551	43.983130
3501.068394	282798.451261	43.988135
3500.855683	282798.433560	43.993140
3500.761510	282766.853942	43.998145
3501.063000	282765.992089	44.003149
3500.697450	282761.644837	44.008154
3501.123680	282756.002696	44.013159
3500.701747	282758.181700	44.018164
3500.887099	282756.217819	44.023169
3500.766702	282760.539133	44.028173
3500.901377	282737.146901	44.033178
3501.280574	282725.427466	44.038183
3500.834819	282731.709056	44.043188
3501.116549	282722.474358	44.048193
3501.050658	282722.280952	44.053197
3501.032104	282697.079630	44.058202
3501.134875	282690.469702	44.063207
3500.993768	282694.412377	44.068212
3501.315696	282679.672293	44.073217
3500.790080	282661.933279	44.078221
3501.185083	282655.175825	44.083226
3501.240588	282645.569145	44.088231
3500.801650	282644.313873	44.093236
3500.975825	282635.095979	44.098241
3500.889394	282622.863771	44.103245
3500.944955	282610.532985	44.108250
3501.076274	282604.300468	44.113255
3500.956104	282607.297898	44.118260
3500.909505	282604.224630	44.123265
3501.105394	282596.861829	44.128269
3500.903026	282577.901153	44.133274
3500.947879	282569.569069	44.138279
3500.856780	282564.058709	44.143284
3500.740712	282568.430276	44.148289
3500.715575	282568.586921	44.153293
3500.823743	282567.729831	44.158298
3500.941128	282552.792570	44.163303
3500.932457	282547.880334	44.168308
3500.843051	282525.923300	44.173313
3501.092574	282521.887215	44.178317
3500.962571	282517.554040	44.183322
3500.759573	282523.364895	44.188327
3500.585210	282524.155883	44.193332
3500.752680	282508.319722	44.198337
3500.689292	282501.379330	44.203341
3500.679152	282484.603496	44.208346
3500.864069	282486.993139	44.213351
3501.111832	282485.605047	44.218356
3500.900479	282485.485299	44.223361
3500.817674	282478.191516	44.228365
3500.524854	282481.648744	44.233370
3500.655180	282477.402162	44.238375
3500.677875	282481.166486	44.243380
3500.629451	282454.747724	44.248385
3500.658748	282452.273596	44.253389
3500.536112	282440.174311	44.258394
3500.972764	282438.069298	44.263399
3500.568636	282441.212965	44.268404
3500.538194	282440.657591	44.273409
3500.803889	282439.979543	44.278413
3500.807650	282438.069502	44.283418
3500.785112	282429.544266	44.288423
3500.887773	282445.796396	44.293428
3501.095101	282439.068263	44.298433
3500.736199	282426.649489	44.303437
3500.675200	282417.544711	44.308442
3500.790059	282405.917467	44.313447
3500.997504	282399.825784	44.318452
3500.918774	282401.798389	44.323457
3500.853907	282405.652783	44.328461
3500.856224	282396.181679	44.333466
3500.835221	282378.490999	44.338471
3500.733022	282369.927292	44.343476
3500.813024	282363.575482	44.348481
3500.754421	282359.256594	44.353485
3500.572349	282360.659802	44.358490
3501.073505	282356.686202	44.363495
3501.049633	282364.760367	44.368500
3500.663831	282359.117852	44.373505
3501.038508	282352.083500	44.378509
3501.028238	282334.696637	44.383514
3500.922824	282329.952264	44.388519
3500.835011	282330.933394	44.393524
3501.166238	282325.458825	44.398529
3500.868127	282315.983761	44.403533
3500.835894	282307.689157	44.408538
3500.661798	282303.591993	44.413543
3500.913550	282287.258887	44.418548
3501.052186	282277.715538	44.423553
3501.039127	282295.513329	44.428557
3500.663857	282291.447615	44.433562
3500.374072	282290.576361	44.438567
3500.637154	282298.605671	44.443572
3501.053355	282275.576617	44.448577
3501.383777	282262.133524	44.453581
3500.912626	282255.638741	44.458586
3500.781132	282257.772353	44.463591
3500.863237	282252.438562	44.468596
3500.711248	282245.053735	44.473601
3500.562420	282240.927158	44.478605
3500.604670	282222.997420	44.483610
3500.949227	282221.339601	44.488615
3500.887996	282220.534449	44.493620
3500.928584	282216.378258	44.498625
3500.723737	282216.308410	44.503629
3500.748406	282220.479783	44.508634
3500.783840	282223.147395	44.513639
3500.931950	282212.940623	44.518644
3501.095667	282188.067051	44.523649
3500.686184	282186.247069	44.528653
3500.704916	282179.650232	44.533658
3500.766718	282177.476520	44.538663
3501.029928	282185.251233	44.543668
3500.816494	282170.136482	44.548673
3501.221593	282169.309342	44.553677
3501.001433	282153.711918	44.558682
3501.321291	282144.853070	44.563687
3500.636452	282141.650433	44.568692
3500.946360	282133.531449	44.573697
3500.646010	282141.597945	44.578701
3500.797232	282131.263380	44.583706
3501.035775	282104.774166	44.588711
3500.799734	282106.134898	44.593716
3501.135934	282093.327345	44.598721
3501.040984	282101.616324	44.603725
3501.183134	282093.752693	44.608730
3501.035094	282074.987062	44.613735
3500.611259	282070.521585	44.618740
3501.338020	282056.838278	44.623745
3501.083932	282057.718111	44.628749
3501.040282	282055.713636	44.633754
3501.359365	282036.213031	44.638759
3500.994914	282027.053808	44.643764
3500.831176	282022.267615	44.648769
3501.218896	282012.659830	44.653773
3501.166913	281995.101193	44.658778
3501.277303	281979.350217	44.663783
3501.065124	281973.044052	44.668788
3501.528384	281969.101816	44.673793
3501.002604	281960.400610	44.678797
3500.629096	281941.491980	44.683802
3500.916094	281933.911196	44.688807
3500.707061	281938.730139	44.693812
3500.908787	281938.851318	44.698817
3500.876311	281938.881817	44.703821
3500.951504	281922.117969	44.708826
3500.762548	281908.552337	44.713831
3500.677649	281907.190784	44.718836
3500.889919	281895.802819	44.723841
3501.050454	281903.415402	44.728845
3500.701106	281907.594348	44.733850
3501.310807	281892.910949	44.738855
3500.963846	281886.218503	44.743860
3501.132225	281865.952182	44.748865
3501.140655	281866.027204	44.753869
3501.202609	281859.194448	44.758874
3501.027606	281851.685884	44.763879
3501.034840	281837.605845	44.768884
3500.851509	281811.920792	44.773889
3500.956479	281825.295823	44.778893
3500.863245	281829.281979	44.783898
3500.861588	281818.182039	44.788903
3500.995058	281798.939520	44.793908
3501.003889	281787.761558	44.798913
3501.178542	281792.393230	44.803917
3501.096035	281790.598495	44.808922
3501.312289	281783.436101	44.813927
3500.983514	281768.237461	44.818932
3501.230726	281749.664542	44.823937
3500.971443	281743.518476	44.828941
3501.073301	281739.607269	44.833946
3501.451191	281723.534366	44.838951
3501.166513	281717.672318	44.843956
3501.183276	281712.399621	44.848961
3501.267147	281693.954062	44.853965
3501.128483	281671.240694	44.858970
3501.002739	281677.548722	44.863975
3500.767139	281676.287102	44.868980
3501.290097	281665.283334	44.873985
3501.240613	281640.111936	44.878989
3501.018680	281635.029306	44.883994
3500.675098	281627.674370	44.888999
3500.722952	281637.723216	44.894004
3500.924649	281628.322677	44.899009
3500.828927	281626.835514	44.904013
3500.822560	281604.254197	44.909018
3500.980889	281593.638393	44.914023
3501.231793	281605.997743	44.919028
3500.975268	281601.302405	44.924033
3500.663680	281594.400729	44.929037
3500.784042	281590.053815	44.934042
3501.138405	281560.949459	44.939047
3501.048593	281561.574483	44.944052
3500.753174	281548.458234	44.949057
3500.900409	281553.934361	44.954061
3501.278234	281558.890713	44.959066
3501.193972	281539.707625	44.964071
3501.047117	281531.634524	44.969076
3500.824493	281518.354134	44.974081
3500.850691	281511.628773	44.979085
3500.590226	281516.557622	44.984090
3500.855609	281510.405888	44.989095
3500.681136	281508.803738	44.994100
3500.701578	281491.819218	44.999105
3500.862444	281481.355756	45.004109
3500.771231	281480.427988	45.009114
3500.975481	281476.373463	45.014119
3500.784678	281478.694584	45.019124
3501.079436	281462.558243	45.024129
3501.287684	281459.215950	45.029133
3500.863560	281444.006689	45.034138
3501.223495	281432.493730	45.039143
3501.004539	281438.001656	45.044148
3501.026312	281437.514489	45.049153
3500.718968	281415.158383	45.054157
3500.984353	281401.165195	45.059162
3500.747386	281396.543165	45.064167
3500.918675	281402.677483	45.069172
3501.072446	281401.176769	45.074177
3500.843172	281403.809418	45.079181
3500.975571	281394.546978	45.084186
3501.070959	281368.741816	45.089191
3500.878916	281371.801452	45.094196
3500.809839	281359.693612	45.099201
3501.009976	281359.509529	45.104205
3500.850071	281360.120054	45.109210
3500.807594	281352.285208	45.114215
3500.848650	281333.260687	45.119220
3501.079567	281317.668940	45.124225
3501.021198	281314.622915	45.129229
3500.716257	281307.491039	45.134234
3501.074603	281313.086935	45.139239
3500.820804	281307.296404	45.144244
3501.121305	281301.444672	45.149249
3501.140808	281291.563388	45.154253
3500.776392	281284.949993	45.159258
3500.693336	281279.030929	45.164263
3500.608976	281287.038293	45.169268
3500.665515	281276.234682	45.174273
3500.860059	281277.655409	45.179277
3500.835170	281258.157452	45.184282
3500.873412	281249.113389	45.189287
3500.869359	281241.934465	45.194292
3500.709070	281242.443214	45.199297
3500.541811	281237.733897	45.204301
3500.656528	281238.581540	45.209306
3500.703163	281235.391800	45.214311
3500.838219	281245.197934	45.219316
3500.795924	281242.225772	45.224321
3501.075034	281226.906522	45.229325
3500.916346	281210.280913	45.234330
3500.665809	281207.544980	45.239335
3501.029314	281208.048216	45.244340
3500.739340	281199.717402	45.249345
3501.179205	281192.927339	45.254349
3500.750587	281203.254412	45.259354
3501.288414	281184.279484	45.264359
3500.938935	281174.786842	45.269364
3501.135560	281160.727980	45.274369
3501.320299	281163.474126	45.279373
3500.849403	281152.116474	45.284378
3501.135786	281123.124408	45.289383
3500.767388	281125.346009	45.294388
3500.895000	281125.656991	45.299393
3500.942448	281124.325651	45.304397
3500.973942	281120.068980	45.309402
3501.260909	281097.747159	45.314407
3500.885876	281087.112829	45.319412
3500.824803	281074.672719	45.324417
3501.311879	281077.957166	45.329421
3501.026252	281075.735901	45.334426
3501.322815	281050.764793	45.339431
3501.088697	281043.927330	45.344436
3501.198884	281045.997733	45.349441
3501.299463	281042.901388	45.354445
3501.030046	281022.194090	45.359450
3501.286158	281011.944805	45.364455
3500.712443	281007.680909	45.369460
3501.080415	280998.381590	45.374465
3501.273578	280974.699590	45.379469
3501.213363	280975.345450	45.384474
3501.244249	280968.822982	45.389479
3501.175364	280969.393820	45.394484
3500.967954	280934.394086	45.399489
3500.933965	280933.966552	45.404493
3500.946712	280930.629340	45.409498
3501.010938	280920.995608	45.414503
3500.801412	280927.673231	45.419508
3501.044251	280911.748561	45.424513
3501.112863	280903.794461	45.429517
3500.632544	280901.705467	45.434522
3500.771591	280888.724850	45.439527
3500.437084	280896.313095	45.444532
3500.450092	280894.197892	45.449537
3500.301152	280891.166010	45.454541
3500.322594	280891.340836	45.459546
3500.741588	280894.941449	45.464551
3500.754639	280894.481101	45.469556
3500.908723	280894.966162	45.474561
3500.959728	280879.555205	45.479565
3500.771986	280877.496847	45.484570
3500.699053	280860.908669	45.489575
3500.851473	280861.241234	45.494580
3500.688571	280861.750393	45.499585
3500.831079	280854.039330	45.504589
3500.748614	280853.033808	45.509594
3501.149510	280843.194674	45.514599
3500.695823	280860.119706	45.519604
3500.477773	280847.271288	45.524609
3500.690056	280853.271946	45.529613
3501.142673	280845.359643	45.534618
3500.873409	280828.700315	45.539623
3500.391018	280827.273588	45.544628
3500.687826	280820.098505	45.549633
3500.715700	280812.634494	45.554637
3500.698255	280815.692316	45.559642
3500.735140	280811.103813	45.564647
3500.731637	280816.756318	45.569652
3500.700979	280820.987340	45.574657
3500.821232	280818.600775	45.579661
3500.514742	280807.599256	45.584666
3500.966563	280786.473620	45.589671
3500.728740	280778.338280	45.594676
3500.800193	280769.925452	45.599681
3500.809972	280780.362261	45.604685
3500.560230	280782.132510	45.609690
3500.911007	280766.292771	45.614695
3500.616166	280779.017637	45.619700
3500.809979	280771.451300	45.624705
3500.699170	280774.014532	45.629709
3500.428680	280775.482512	45.634714
3500.627437	280751.061241	45.639719
3500.627428	280755.822123	45.644724
3500.599399	280735.637114	45.649729
3500.303878	280734.919493	45.654733
3500.370529	280739.593577	45.659738
3500.482757	280734.967831	45.664743
3500.728343	280746.640752	45.669748
3500.909814	280740.247477	45.674753
3500.565652	280731.441351	45.679757
3500.563525	280738.697594	45.684762
3500.789000	280727.892951	45.689767
3500.936510	280735.431314	45.694772
3501.064769	280729.224573	45.699777
3500.886021	280728.335940	45.704781
3500.800347	280729.393135	45.709786
3500.954662	280699.810523	45.714791
3501.224644	280698.393464	45.719796
3501.243913	280691.592733	45.724801
3501.151560	280690.334159	45.729805
3500.933617	280679.013265	45.734810
3501.067273	280666.364425	45.739815
3500.933357	280663.762996	45.744820
3500.534167	280634.394190	45.749825
3500.608470	280589.802935	45.754829
3500.691641	280491.770689	45.759834
3500.659534	280345.637706	45.764839
3500.475288	280167.652731	45.769844
3500.135145	279930.497824	45.774849
3499.808719	279650.236526	45.779853
3499.794179	279321.806133	45.784858
3499.606800	278934.130294	45.789863
3498.910369	278526.571258	45.794868
3498.482188	278052.745720	45.799873
3498.117249	277539.519948	45.804877
3497.091379	276994.084492	45.809882
3496.820487	276389.432484	45.814887
3496.101389	275752.943205	45.819892
3495.385930	275053.457042	45.824897
3495.082052	274323.219400	45.829901
3493.794181	273543.402326	45.834906
3493.296646	272716.349744	45.839911
3492.275477	271856.830279	45.844916
3491.304531	270951.742043	45.849921
3490.582988	270003.267946	45.854925
3489.728120	269010.600923	45.859930
3488.579582	267980.970991	45.864935
3487.417525	266901.779829	45.869940
3486.301759	265770.088385	45.874945
3485.096466	264604.148849	45.879949
3483.932949	263400.833239	45.884954
3482.999153	262150.816663	45.889959
3481.396075	260868.040631	45.894964
3479.881048	259538.940409	45.899969
3478.864975	258168.849476	45.904973
3477.370269	256760.873969	45.909978
3475.537580	255314.965853	45.914983
3474.190907	253837.387895	45.919988
3472.351600	252307.308262	45.924993
3470.518276	250754.877602	45.929997
3468.657833	249165.330317	45.935002
3467.316074	247543.165140	45.940007
3465.080311	245890.360357	45.945012
3463.648364	244197.940792	45.950017
3461.425969	242480.239793	45.955021
3459.483349	240717.581968	45.960026
3457.971388	238922.449139	45.965031
3455.503073	237117.904305	45.970036
3453.604836	235263.214784	45.975041
3451.448218	233376.058957	45.980045
3449.114399	231466.460129	45.985050
3447.145657	229528.426185	45.990055
3444.762382	227571.682409	45.995060
3442.298828	225571.906270	46.000065
3439.847970	223545.105137	46.005069
3437.730913	221496.681238	46.010074
3435.357530	219426.550744	46.015079
3432.504760	217335.209295	46.020084
3430.071499	215211.847405	46.025089
3427.458705	213078.617328	46.030093
3424.850958	210900.601009	46.035098
3421.895854	208720.261592	46.040103
3419.006717	206517.799368	46.045108
3416.422591	204292.059626	46.050113
3413.501518	202054.530106	46.055117
3410.410594	199778.269182	46.060122
3407.273699	197498.380477	46.065127
3404.621229	195211.448045	46.070132
3401.537989	192895.921368	46.075137
3398.293105	190562.713013	46.080141
3395.054935	188217.122924	46.085146
3392.022911	185855.355136	46.090151
3388.016588	183495.754081	46.095156
3385.088086	181122.214919	46.100161
3381.671572	178734.630301	46.105165
3377.814107	176347.701412	46.110170
3374.676727	173935.623633	46.115175
3370.341714	171534.944891	46.120180
3367.144274	169111.123363	46.125185
3363.628580	166717.562266	46.130189
3359.782695	164295.520574	46.135194
3355.742942	161865.590575	46.140199
3351.840106	159443.952886	46.145204
3347.811635	157027.621997	46.150209
3344.161576	154609.827656	46.155213
3339.893368	152198.466873	46.160218
3335.418604	149782.063008	46.165223
3331.023813	147374.763881	46.170228
3326.433357	144982.429885	46.175233
3321.773570	142607.281971	46.180237
3317.018752	140249.414080	46.185242
3312.798697	137800.853163	46.190247
3308.246173	135461.716196	46.195252
3303.312742	133133.228798	46.200257
3298.576643	130826.140017	46.205261
3292.476863	128549.801079	46.210266
3287.801701	126291.995975	46.215271
3281.946972	124076.025162	46.220276
3276.565995	121871.306561	46.225281
3270.595217	119728.278281	46.230285
3263.978184	117626.912963	46.235290
3257.883633	115549.767979	46.240295
3251.156888	113536.693146	46.245300
3244.354887	111568.597588	46.250305
3237.399044	109656.599937	46.255309
3230.583183	107816.449261	46.260314
3223.272793	106019.149026	46.265319
3215.788966	104305.054388	46.270324
3208.250612	102656.314407	46.275329
3200.202761	101070.131815	46.280333
3192.705580	99562.881137	46.285338
3185.020348	98140.298025	46.290343
3177.292800	96795.168710	46.295348
3169.528334	95518.434831	46.300353
3161.738693	94331.804428	46.305357
3153.708440	93201.194762	46.310362
3146.768264	92152.352215	46.315367
3139.180642	91181.423464	46.320372
3131.247871	90291.365381	46.325377
3124.388522	89463.970469	46.330381
3118.007999	88696.048645	46.335386
3111.976542	87975.926969	46.340391
3105.767901	87326.426076	46.345396
3100.191645	86718.422825	46.350401
3094.611051	86146.348110	46.355405
3089.474048	85626.581689	46.360410
3084.837148	85129.435569	46.365415
3079.689999	84671.301969	46.370420
3075.484524	84245.663765	46.375425
3071.177905	83836.587444	46.380429
3066.606601	83451.478444	46.385434
3063.036255	83075.681854	46.390439
3059.463377	82724.191180	46.395444
3055.718144	82379.629373	46.400449
3052.132402	82048.918004	46.405453
3048.411896	81734.223919	46.410458
3044.634746	81413.953197	46.415463
3040.800371	81102.307113	46.420468
3037.052413	80801.244438	46.425473
3033.725078	80504.196517	46.430477
3030.108793	80211.909278	46.435482
3026.715198	79924.277164	46.440487
3023.384806	79652.794413	46.445492
3019.811428	79368.866880	46.450497
3016.669350	79087.491253	46.455501
3013.434488	78811.137224	46.460506
3009.861433	78521.706045	46.465511
3006.361382	78247.926613	46.470516
3002.816594	77972.556608	46.475521
2999.663167	77686.624778	46.480525
2996.143039	77426.433587	46.485530
2992.761522	77133.164232	46.490535
2989.251137	76864.150143	46.495540
2986.054781	76588.955461	46.500545
2982.212579	76317.776144	46.505549
2978.794663	76056.096144	46.510554
2975.563228	75775.847951	46.515559
2971.805181	75506.949523	46.520564
2968.426371	75235.137089	46.525569
2964.771958	74974.571288	46.530573
2961.172629	74702.951099	46.535578
2957.699961	74429.066113	46.540583
2954.024716	74167.139899	46.545588
2950.424691	73908.582367	46.550593
2946.705061	73645.398322	46.555597
2942.939383	73403.252900	46.560602
2939.533890	73136.291372	46.565607
2935.773381	72891.889472	46.570612
2932.452393	72635.865716	46.575617
2928.853713	72392.751023	46.580621
2925.699554	72147.943703	46.585626
2921.811809	71898.961504	46.590631
2918.072117	71660.459529	46.595636
2914.622732	71416.149594	46.600641
2910.694200	71183.192249	46.605645
2906.771092	70937.805378	46.610650
2902.983964	70713.134192	46.615655
2899.104669	70499.335435	46.620660
2895.573924	70266.489103	46.625665
2892.242136	70056.823773	46.630669
2888.392054	69837.953436	46.635674
2884.822129	69612.667361	46.640679
2881.592273	69410.399854	46.645684
2878.050855	69197.339802	46.650689
2874.383965	68984.954992	46.655693
2870.891950	68785.729727	46.660698
2867.304902	68578.382571	46.665703
2863.428832	68374.675292	46.670708
2859.971747	68168.885428	46.675713
2856.000717	67961.850865	46.680717
2852.467035	67778.465404	46.685722
2849.153957	67579.653153	46.690727
2845.594138	67387.165383	46.695732
2842.205240	67191.827569	46.700737
2838.549521	67006.549699	46.705741
2834.563077	66822.061233	46.710746
2831.320332	66626.774712	46.715751
2827.165695	66437.072194	46.720756
2823.890157	66247.303427	46.725761
2820.185395	66083.539091	46.730765
2816.815300	65903.930993	46.735770
2813.671289	65722.149730	46.740775
2810.142299	65550.363616	46.745780
2806.458054	65366.016208	46.750785
2803.075040	65183.635121	46.755789
2799.257222	65003.805125	46.760794
2796.045509	64816.550619	46.765799
2792.610413	64644.546538	46.770804
2789.174807	64464.133812	46.775809
2785.819171	64283.525811	46.780813
2782.086006	64114.612222	46.785818
2778.746703	63932.366671	46.790823
2774.890822	63752.361194	46.795828
2771.572447	63576.208008	46.800833
2768.424764	63390.585291	46.805837
2764.804540	63213.288676	46.810842
2761.634361	63021.255635	46.815847
2757.673834	62862.521822	46.820852
2754.131703	62667.338265	46.825857
2751.039815	62486.029289	46.830861
2747.571233	62301.842103	46.835866
2744.062521	62119.103221	46.840871
2740.622057	61943.101297	46.845876
2736.938970	61748.968807	46.850881
2733.354855	61565.185968	46.855885
2730.005937	61379.482859	46.860890
2726.644484	61199.012433	46.865895
2722.976636	61026.511337	46.870900
2719.414213	60844.932627	46.875905
2716.220988	60657.478117	46.880909
2712.204826	60476.480796	46.885914
2708.843497	60292.012650	46.890919
2705.776109	60119.887283	46.895924
2702.187700	59919.338666	46.900929
2698.951618	59734.023827	46.905933
2695.342731	59554.727451	46.910938
2691.880509	59359.284800	46.915943
2688.237082	59174.310804	46.920948
2684.613462	58980.203670	46.925953
2681.318455	58791.472214	46.930957
2677.908251	58605.628453	46.935962
2674.375888	58420.566692	46.940967
2670.345232	58238.122487	46.945972
2667.079907	58047.716981	46.950977
2663.650314	57867.313637	46.955981
2660.171527	57677.039628	46.960986
2656.606421	57482.649835	46.965991
2652.939583	57310.650880	46.970996
2649.484114	57119.622552	46.976001
2646.019391	56928.146687	46.981005
2642.877636	56748.436419	46.986010
2639.630126	56559.264527	46.991015
2635.896640	56370.328772	46.996020
2632.357945	56182.055644	47.001025
2629.069149	55985.204675	47.006029
2624.987722	55800.337840	47.011034
2621.404400	55601.144106	47.016039
2618.295341	55418.786617	47.021044
2614.873225	55219.012533	47.026049
2611.566295	55032.127128	47.031053
2607.792223	54844.351887	47.036058
2604.054429	54650.469009	47.041063
2600.588474	54466.480683	47.046068
2597.269079	54272.922473	47.051073
2593.637288	54088.442792	47.056077
2590.427922	53895.206727	47.061082
2587.165183	53703.078160	47.066087
2583.460871	53513.196309	47.071092
2579.675055	53317.454025	47.076097
2576.497949	53124.276354	47.081101
2573.119817	52940.654193	47.086106
2569.447721	52734.520070	47.091111
2566.124207	52550.226310	47.096116
2562.389751	52354.242983	47.101121
2558.822635	52150.857204	47.106125
2555.573234	51969.474624	47.111130
2552.077030	51765.757583	47.116135
2548.245115	51578.467969	47.121140
2545.122801	51385.017013	47.126145
2541.648885	51194.712009	47.131149
2537.792933	50995.669812	47.136154
2534.566870	50798.617812	47.141159
2530.968197	50605.178110	47.146164
2527.158730	50413.650650	47.151169
2524.082948	50208.371825	47.156173
2520.422064	50015.828526	47.161178
2516.912208	49819.412872	47.166183
2513.556975	49626.647412	47.171188
2509.925371	49420.111472	47.176193
2506.541487	49228.134048	47.181197
2502.984393	49031.377321	47.186202
2499.788811	48820.833224	47.191207
2496.000549	48644.388100	47.196212
2492.752915	48438.543082	47.201217
2489.638652	48236.782850	47.206221
2485.406814	48032.199109	47.211226
2482.051997	47826.661813	47.216231
2478.365615	47643.764349	47.221236
2475.230766	47437.714124	47.226241
2471.657592	47242.611761	47.231245
2468.213692	47049.818544	47.236250
2465.120443	46840.145701	47.241255
2460.970938	46639.969634	47.246260
2457.696520	46429.498097	47.251265
2454.173060	46227.838796	47.256269
2450.799074	46038.734467	47.261274
2447.208643	45829.212225	47.266279
2443.569826	45631.280123	47.271284
2440.072546	45427.125140	47.276289
2436.597156	45221.750938	47.281293
2432.871462	45016.950496	47.286298
2429.417301	44811.805046	47.291303
2425.802674	44621.133161	47.296308
2422.052677	44425.068249	47.301313
2418.859479	44231.835130	47.306317
2415.406457	44037.020880	47.311322
2411.734056	43830.339547	47.316327
2408.154440	43635.231548	47.321332
2404.509676	43429.830608	47.326337
2401.346869	43240.888176	47.331341
2397.814048	43038.720145	47.336346
2394.582645	42829.588480	47.341351
2391.110579	42633.870066	47.346356
2387.600018	42431.272913	47.351361
2383.972135	42224.897657	47.356365
2380.521572	42037.627525	47.361370
2377.351412	41826.923217	47.366375
2373.519087	41625.899316	47.371380
2370.063485	41419.631494	47.376385
2366.796562	41211.446536	47.381389
2363.242004	41015.451092	47.386394
2360.045904	40806.098555	47.391399
2356.255052	40603.739675	47.396404
2352.933290	40389.680681	47.401409
2349.136223	40180.111140	47.406413
2345.877469	39970.560852	47.411418
2341.977368	39768.220492	47.416423
2338.448077	39568.024104	47.421428
2335.322297	39358.636449	47.426433
2331.776024	39151.954126	47.431437
2328.166224	38938.715324	47.436442
2325.068921	38730.261294	47.441447
2321.387148	38531.803834	47.446452
2317.729304	38311.592033	47.451457
2314.569865	38097.035781	47.456461
2310.977252	37887.266274	47.461466
2307.478389	37677.084744	47.466471
2304.333193	37471.154608	47.471476
2300.512662	37255.410545	47.476481
2296.886863	37040.253132	47.481485
2293.198390	36838.496770	47.486490
2289.874339	36619.448291	47.491495
2286.147583	36415.762038	47.496500
2282.914584	36191.828704	47.501505
2279.208044	35991.243285	47.506509
2275.915438	35783.767663	47.511514
2272.309391	35564.622010	47.516519
2268.671072	35348.279206	47.521524
2265.361631	35147.132513	47.526529
2262.141453	34922.468890	47.531533
2258.286501	34717.050426	47.536538
2254.883815	34506.314649	47.541543
2250.978867	34302.524446	47.546548
2247.398401	34076.392209	47.551553
2244.574029	33866.706978	47.556557
2240.679786	33652.728858	47.561562
2237.242295	33436.069992	47.566567
2234.160511	33224.092534	47.571572
2230.845693	33014.955244	47.576577
2227.312485	32788.049867	47.581581
2223.331494	32566.560155	47.586586
2219.946876	32346.849253	47.591591
2216.451886	32134.738323	47.596596
2213.077436	31908.337397	47.601601
2209.865407	31692.447251	47.606605
2205.838588	31478.537497	47.611610
2202.964519	31256.115317	47.616615
2199.123011	31026.114784	47.621620
2195.846361	30809.730569	47.626625
2192.472614	30584.795306	47.631629
2188.891251	30359.559081	47.636634
2185.591433	30137.519732	47.641639
2181.866603	29900.174636	47.646644
2178.619130	29692.619280	47.651649
2175.064432	29464.726965	47.656653
2171.601864	29230.884775	47.661658
2168.082181	29003.277278	47.666663
2164.506189	28782.892730	47.671668
2160.649965	28553.986741	47.676673
2157.546662	28321.290081	47.681677
2153.838778	28095.661231	47.686682
2150.676592	27854.677785	47.691687
2147.170422	27626.741313	47.696692
2143.568898	27395.482890	47.701697
2140.201632	27169.766648	47.706701
2136.357969	26939.178627	47.711706
2133.161970	26706.717688	47.716711
2129.620424	26480.979351	47.721716
2126.233148	26243.877403	47.726721
2122.806788	26012.854462	47.731725
2118.888069	25774.814700	47.736730
2116.125369	25540.189437	47.741735
2112.441544	25306.490355	47.746740
2108.946075	25063.279619	47.751745
2105.460061	24822.471638	47.756749
2101.764484	24600.573647	47.761754
2098.159196	24350.413028	47.766759
2094.687733	24125.849576	47.771764
2090.778771	23881.526775	47.776769
2087.758218	23648.972342	47.781773
2084.119847	23420.540275	47.786778
2080.407427	23173.046699	47.791783
2076.790434	22956.165942	47.796788
2073.079877	22723.812632	47.801793
2069.581071	22496.471669	47.806797
2066.048086	22276.664702	47.811802
2062.254301	22052.542514	47.816807
2057.812781	21846.337992	47.821812
2053.974272	21640.662091	47.826817
2049.945811	21432.091385	47.831821
2046.114625	21250.110519	47.836826
2042.253174	21060.952562	47.841831
2038.167509	20882.125243	47.846836
2034.252898	20707.973025	47.851841
2030.554521	20533.687169	47.856845
2026.580622	20378.145247	47.861850
2023.351596	20203.237796	47.866855
2019.507480	20046.417662	47.871860
2015.923154	19888.310285	47.876865
2013.009290	19729.047796	47.881869
2009.384316	19572.526562	47.886874
2005.760958	19407.721287	47.891879
2002.197117	19252.352206	47.896884
1999.043421	19095.241672	47.901889
1995.532104	18942.229443	47.906893
1992.070642	18779.076333	47.911898
1988.843967	18619.175136	47.916903
1985.001393	18464.926393	47.921908
1981.591935	18300.103377	47.926913
1978.570782	18145.152276	47.931917
1974.849669	17987.309781	47.936922
1971.962692	17812.642642	47.941927
1968.474161	17648.287237	47.946932
1965.226285	17487.493005	47.951937
1961.334465	17321.620110	47.956941
1957.926516	17156.755940	47.961946
1954.644524	16983.754125	47.966951
1951.287055	16830.484367	47.971956
1947.834873	16659.393087	47.976961
1944.324569	16483.277547	47.981965
1940.746128	16313.098918	47.986970
1937.309154	16133.992207	47.991975
1933.854483	15979.170690	47.996980
1930.045401	15802.405190	48.001985
1926.527042	15631.802069	48.006989
1922.988752	15470.085400	48.011994
1919.252739	15300.941015	48.016999
1915.676244	15135.556975	48.022004
1912.190218	14968.615039	48.027009
1908.959542	14796.872476	48.032013
1905.411758	14635.772300	48.037018
1902.241870	14480.022321	48.042023
1898.669167	14302.920269	48.047028
1895.227176	14140.072645	48.052033
1891.684711	13967.100886	48.057037
1888.053445	13794.356732	48.062042
1884.721255	13620.006457	48.067047
1881.153675	13454.888937	48.072052
1877.271930	13275.204328	48.077057
1874.538464	13107.755736	48.082061
1870.687220	12936.855305	48.087066
1867.555811	12765.726637	48.092071
1864.059849	12599.202864	48.097076
1860.684127	12422.913892	48.102081
1856.995104	12234.699056	48.107085
1853.475815	12072.026979	48.112090
1849.964683	11894.029263	48.117095
1846.728512	11718.921732	48.122100
1843.207592	11546.063769	48.127105
1840.060121	11369.942066	48.132109
1836.007532	11190.750463	48.137114
1832.516903	11020.732248	48.142119
1828.942727	10843.504638	48.147124
1824.796289	10670.708327	48.152129
1821.706266	10492.534571	48.157133
1818.056127	10318.252006	48.162138
1814.928156	10136.320572	48.167143
1811.861282	9966.989541	48.172148
1807.781172	9796.951272	48.177153
1804.937189	9606.851636	48.182157
1800.786374	9437.780518	48.187162
1797.519366	9254.318919	48.192167
1793.862672	9080.666229	48.197172
1790.101014	8910.310867	48.202177
1786.743292	8728.634915	48.207181
1782.691087	8561.670780	48.212186
1779.871274	8390.872109	48.217191
1776.702772	8217.423334	48.222196
1773.094910	8042.706076	48.227201
1769.667994	7862.749165	48.232205
1766.125304	7679.232388	48.237210
1762.990118	7498.726960	48.242215
1759.195291	7322.526554	48.247220
1755.737953	7133.554811	48.252225
1752.004808	6952.094377	48.257229
1748.390234	6780.925446	48.262234
1745.143267	6595.825545	48.267239
1741.405295	6412.772918	48.272244
1737.690260	6246.995526	48.277249
1734.558105	6076.450790	48.282253
1730.964328	5890.659064	48.287258
1727.993752	5711.759517	48.292263
1724.077004	5526.594866	48.297268
1720.357824	5354.234079	48.302273
1716.923711	5158.164837	48.307277
1713.629979	4990.842368	48.312282
1710.045165	4800.841876	48.317287
1706.307833	4624.329379	48.322292
1702.948762	4440.911308	48.327297
1699.702921	4260.689359	48.332301
1695.622806	4086.707235	48.337306
1692.590321	3902.411239	48.342311
1688.944754	3719.497826	48.347316
1685.217630	3546.247273	48.352321
1681.704038	3364.990762	48.357325
1678.167286	3188.764659	48.362330
1674.652328	3004.024892	48.367335
1671.253205	2837.096397	48.372340
1667.560293	2656.061772	48.377345
1664.058781	2472.423349	48.382349
1660.546433	2306.700913	48.387354
1657.208352	2126.457763	48.392359
1653.572818	1951.553381	48.397364
1649.979977	1776.808557	48.402369
1646.768144	1603.676429	48.407373
1642.723773	1432.887929	48.412378
1639.423989	1263.794334	48.417383
1635.679050	1087.956827	48.422388
1632.480895	916.841493	48.427393
1628.980337	745.069578	48.432397
1625.145820	577.562704	48.437402
1621.563424	411.875124	48.442407
1617.759981	257.986759	48.447412
1613.930687	99.019562	48.452417
1608.248313	-7.378100	48.457421
1596.194207	59.887931	48.462426
1589.467673	60.440804	48.467431
1585.687337	68.125642	48.472436
1582.759809	65.442165	48.477441
1580.607521	61.273763	48.482445
1577.872647	68.845595	48.487450
1576.091525	66.704033	48.492455
1573.202290	72.227749	48.497460
1569.589103	73.489261	48.502465
1566.514642	68.054147	48.507469
1562.185101	68.178087	48.512474
1559.155767	60.669964	48.517479
1555.437467	68.291318	48.522484
1552.263589	57.319333	48.527489
1549.215412	54.164366	48.532493
1545.457316	71.897071	48.537498
1542.484611	58.549239	48.542503
1538.491445	61.657771	48.547508
1535.038964	62.201273	48.552513
1531.986290	55.623804	48.557517
1528.287958	68.705890	48.562522
1524.908895	64.590308	48.567527
1521.339098	73.909527	48.572532
1517.913603	68.051642	48.577537
1514.605683	62.956812	48.582541
1511.451123	65.927769	48.587546
1507.971914	58.774820	48.592551
1504.274070	69.170787	48.597556
1500.589173	69.323568	48.602561
1497.450114	67.160449	48.607565
1493.560585	75.539458	48.612570
1490.354834	71.637208	48.617575
1486.979216	73.965724	48.622580
1483.641326	69.913314	48.627585
1480.030568	63.476998	48.632589
1476.119930	63.456312	48.637594
1473.044548	57.958103	48.642599
1469.842670	71.525651	48.647604
1466.152119	70.451783	48.652609
1462.356089	68.866074	48.657613
1458.993207	65.621187	48.662618
1455.828630	68.812029	48.667623
1451.817272	64.747988	48.672628
1448.719530	73.683288	48.677633
1445.371530	68.275213	48.682637
1441.421767	67.264075	48.687642
1438.255722	71.787103	48.692647
1434.850665	73.977874	48.697652
1431.276687	66.823968	48.702657
1428.082386	57.509888	48.707661
1424.370171	71.989402	48.712666
1420.913113	59.729844	48.717671
1417.180449	64.097959	48.722676
1413.619610	60.589844	48.727681
1410.503857	67.512642	48.732685
1406.945138	70.341247	48.737690
1403.564602	62.891318	48.742695
1399.793513	67.202178	48.747700
1396.351425	68.066806	48.752705
1392.959540	66.006573	48.757709
1389.426024	62.990903	48.762714
1385.934607	59.044823	48.767719
1382.708111	57.404798	48.772724
1378.913878	61.830019	48.777729
1375.571481	65.197416	48.782733
1371.781570	56.077833	48.787738
1368.135212	56.787783	48.792743
1365.097123	57.965671	48.797748
1361.358295	66.390731	48.802753
1358.082134	51.154250	48.807757
1354.638980	60.314479	48.812762
1351.200402	69.916925	48.817767
1347.686377	67.290528	48.822772
1344.000393	71.028097	48.827777
1340.678110	72.367539	48.832781
1336.932004	72.137654	48.837786
1333.669606	58.167699	48.842791
1329.930245	64.950852	48.847796
1326.617414	59.910647	48.852801
1323.180498	59.395083	48.857805
1319.527994	69.853607	48.862810
1316.049402	59.049643	48.867815
1312.337561	64.847723	48.872820
1309.070668	63.252012	48.877825
1305.826884	65.066398	48.882829
1301.852395	70.323464	48.887834
1298.761073	68.444005	48.892839
1294.862585	64.077625	48.897844
1291.447808	68.168228	48.902849
1288.441203	67.256282	48.907853
1284.494993	68.313760	48.912858
1281.088586	65.920480	48.917863
1277.544784	64.592756	48.922868
1274.035635	64.695962	48.927873
1270.587053	60.898245	48.932877
1267.034492	61.100000	48.937882
1263.573574	68.867813	48.942887
1260.429498	61.738432	48.947892
1256.657110	65.837572	48.952897
1253.365905	58.715409	48.957901
1249.487964	58.503032	48.962906
1246.106756	57.270090	48.967911
1242.637019	61.875514	48.972916
1239.201479	65.361939	48.977921
1236.215730	64.342340	48.982925
1232.088329	59.638499	48.987930
1228.703258	70.162750	48.992935
1225.356359	67.304591	48.997940
1221.513992	68.915317	49.002945
1218.234834	57.365163	49.007949
1214.567368	62.830460	49.012954
1211.049101	63.147089	49.017959
1207.370935	61.008353	49.022964
1203.932575	57.142624	49.027969
1200.634227	60.876503	49.032973
1197.259741	59.044573	49.037978
1194.068014	56.772743	49.042983
1190.338966	58.466981	49.047988
1186.508607	62.799847	49.052993
1183.245812	56.685673	49.057997
1179.253364	63.565443	49.063002
1176.100320	58.952699	49.068007
1173.004903	60.544582	49.073012
1169.084814	57.807818	49.078017
1165.458257	55.983726	49.083021
1161.982590	55.885577	49.088026
1158.550751	60.336397	49.093031
1155.476760	54.474251	49.098036
1151.807648	65.106264	49.103041
1148.510287	57.833246	49.108045
1144.503715	59.928455	49.113050
1140.820797	62.862014	49.118055
1137.487498	55.974281	49.123060
1133.958762	62.740340	49.128065
1130.657134	52.544676	49.133069
1126.852870	62.052568	49.138074
1123.690343	49.671112	49.143079
1120.262938	60.341220	49.148084
1116.787126	53.934554	49.153089
1113.052891	54.696320	49.158093
1109.149325	55.693407	49.163098
1106.017136	59.344354	49.168103
1102.559151	50.906928	49.173108
1099.344405	63.293312	49.178113
1095.989126	50.783856	49.183117
1092.169484	62.904276	49.188122
1088.647277	60.582982	49.193127
1084.829627	59.108379	49.198132
1081.155748	63.593956	49.203137
1078.122009	60.702642	49.208141
1074.810127	60.183410	49.213146
1071.074587	62.767728	49.218151
1067.780831	59.996221	49.223156
1064.167901	59.558928	49.228161
1060.920714	55.489316	49.233165
1056.917173	66.233828	49.238170
1053.643214	58.099803	49.243175
1049.954983	55.886777	49.248180
1046.467561	57.530582	49.253185
1043.143477	61.616554	49.258189
1039.531299	61.647391	49.263194
1036.393423	57.794792	49.268199
1032.597702	61.132031	49.273204
1028.799546	63.893847	49.278209
1025.346066	62.900091	49.283213
1021.883459	67.165947	49.288218
1018.442458	64.031533	49.293223
1015.129085	67.413481	49.298228
1011.306290	64.224951	49.303233
1008.259426	66.717284	49.308237
1004.545118	71.696439	49.313242
1001.226051	64.142138	49.318247
997.720374	63.381192	49.323252
994.106161	68.493374	49.328257
990.660738	59.259920	49.333261
987.125325	62.236879	49.338266
983.896575	62.944859	49.343271
980.298411	63.979601	49.348276
976.490818	64.620028	49.353281
973.129724	61.242165	49.358285
969.145979	58.293991	49.363290
966.091044	59.310121	49.368295
962.652808	59.680748	49.373300
959.228304	58.498982	49.378305
956.004208	51.239884	49.383309
952.260345	69.362800	49.388314
948.335571	64.943740	49.393319
944.737086	61.467016	49.398324
941.358692	72.923609	49.403329
938.369045	60.708147	49.408333
934.220425	65.255454	49.413338
930.786811	60.284933	49.418343
927.447731	61.070320	49.423348
923.875552	54.526963	49.428353
920.590237	58.901132	49.433357
916.958613	62.760051	49.438362
913.409352	55.672106	49.443367
910.058345	58.550613	49.448372
906.476090	57.317637	49.453377
903.289959	54.716002	49.458381
899.632959	59.683053	49.463386
896.048404	49.035084	49.468391
892.631425	45.428724	49.473396
888.856122	59.431024	49.478401
885.579181	60.042179	49.483405
881.797975	70.005288	49.488410
878.669894	60.171698	49.493415
874.710665	62.927156	49.498420
871.432161	61.118281	49.503425
868.122440	50.528530	49.508429
864.299327	58.612599	49.513434
861.011769	59.361466	49.518439
857.625855	65.092845	49.523444
853.780387	61.366930	49.528449
850.587177	55.080640	49.533453
846.972110	60.199331	49.538458
843.604628	58.119661	49.543463
840.155055	65.031605	49.548468
836.354568	57.733095	49.553473
832.963751	55.432457	49.558477
829.409944	56.602679	49.563482
826.015032	59.079964	49.568487
822.293003	55.432812	49.573492
818.717480	57.463817	49.578497
815.507903	63.360584	49.583501
811.600578	61.501503	49.588506
808.355626	63.423800	49.593511
804.916248	65.357562	49.598516
801.174678	68.088458	49.603521
797.977051	58.604315	49.608525
794.265271	61.077446	49.613530
790.611963	66.796934	49.618535
787.633129	59.236903	49.623540
784.019658	61.549111	49.628545
780.524932	64.867784	49.633549
777.059362	59.604937	49.638554
773.534505	54.291266	49.643559
770.253175	59.582349	49.648564
766.070927	57.741030	49.653569
762.718002	53.159742	49.658573
759.160017	55.140566	49.663578
755.964319	54.122363	49.668583
752.314356	48.565702	49.673588
748.961991	62.660001	49.678593
745.582702	56.858472	49.683597
741.856383	66.566256	49.688602
738.292293	62.622322	49.693607
735.007201	57.296429	49.698612
731.223796	66.073519	49.703617
727.544538	56.699632	49.708621
724.188532	54.665668	49.713626
720.819661	58.081711	49.718631
717.464453	51.890446	49.723636
713.726795	65.595839	49.728641
710.627223	51.768360	49.733645
706.694476	52.349400	49.738650
703.292926	53.464187	49.743655
699.849911	60.352999	49.748660
695.871082	59.944677	49.753665
692.882193	50.911949	49.758669
689.592529	60.551363	49.763674
686.252352	57.999242	49.768679
682.373259	50.985201	49.773684
678.750837	50.192040	49.778689
675.401177	52.595851	49.783693
671.792385	52.271958	49.788698
668.222674	50.540403	49.793703
664.692320	49.631589	49.798708
661.009152	61.964882	49.803713
657.789756	61.551538	49.808717
654.268254	60.913425	49.813722
651.167263	56.969770	49.818727
647.456150	57.674313	49.823732
643.347701	62.205955	49.828737
640.097272	61.781658	49.833741
636.500502	61.683687	49.838746
633.342657	56.353726	49.843751
629.517577	56.076378	49.848756
626.375729	66.828452	49.853761
622.973068	62.669459	49.858765
619.131567	61.309518	49.863770
616.062913	58.395361	49.868775
612.504928	61.429770	49.873780
608.940977	61.295032	49.878785
605.200444	58.514577	49.883789
601.711731	64.360212	49.888794
598.406666	55.098627	49.893799
594.771984	54.275783	49.898804
591.155528	59.397944	49.903809
587.804462	53.468676	49.908813
583.639185	57.044296	49.913818
580.440293	57.867960	49.918823
576.887101	55.839625	49.923828
573.751662	53.113113	49.928833
570.429319	61.128346	49.933837
566.716943	64.009782	49.938842
562.881147	61.617588	49.943847
559.824624	58.739516	49.948852
556.154377	59.706614	49.953857
552.843751	61.190029	49.958861
549.353629	62.296598	49.963866
545.624556	57.552847	49.968871
542.297323	58.080250	49.973876
538.808177	60.401551	49.978881
535.474882	65.564806	49.983885
531.291235	63.087901	49.988890
528.014101	56.343485	49.993895
524.542676	59.766165	49.998900
521.281202	66.107747	50.003905
518.187149	59.182799	50.008909
514.058840	51.429590	50.013914
510.601515	56.102912	50.018919
507.108254	57.289082	50.023924
503.191347	64.011736	50.028929
499.975365	55.998580	50.033933
496.260947	61.158264	50.038938
493.234211	62.780734	50.043943
489.649374	64.199553	50.048948
485.787571	71.631757	50.053953
482.709067	60.047342	50.058957
479.101811	67.885767	50.063962
475.568887	66.774949	50.068967
472.010773	63.858412	50.073972
468.622531	61.152551	50.078977
465.156525	62.299667	50.083981
461.910604	62.475842	50.088986
458.323783	60.022552	50.093991
454.566364	54.381613	50.098996
450.817163	67.184059	50.104001
447.619548	62.553261	50.109005
444.025176	67.156325	50.114010
440.728982	64.407584	50.119015
437.291239	66.622795	50.124020
433.208391	75.798069	50.129025
430.325086	56.618572	50.134029
426.241694	58.817858	50.139034
423.083054	61.720183	50.144039
419.594388	54.951999	50.149044
416.263274	66.720861	50.154049
412.698202	59.331896	50.159053
409.098884	63.125827	50.164058
405.525751	56.478446	50.169063
401.745899	57.257130	50.174068
398.030561	71.035053	50.179073
394.565554	72.723041	50.184077
391.470734	67.323189	50.189082
388.208137	61.114391	50.194087
384.961105	68.244690	50.199092
381.206156	70.813329	50.204097
377.605913	68.634257	50.209101
373.770606	59.699436	50.214106
370.157539	61.160688	50.219111
367.193013	62.102739	50.224116
363.554721	59.619586	50.229121
360.210250	50.538290	50.234125
356.525563	62.470116	50.239130
352.907884	59.233931	50.244135
349.253658	59.160893	50.249140
345.619747	68.307002	50.254145
342.723213	62.790690	50.259149
338.901639	67.207920	50.264154
335.255002	71.129514	50.269159
331.937408	62.629308	50.274164
328.623164	63.825469	50.279169
325.638791	67.823660	50.284173
321.616383	67.112283	50.289178
317.916956	66.299693	50.294183
314.101651	58.949972	50.299188
310.847109	64.322425	50.304193
307.392790	56.558657	50.309197
304.063816	62.357223	50.314202
300.149719	58.427177	50.319207
297.002990	58.141785	50.324212
293.462070	59.784754	50.329217
290.387351	59.643108	50.334221
286.599610	64.662497	50.339226
282.959662	59.765699	50.344231
279.248062	60.372392	50.349236
275.763426	62.550716	50.354241
272.562150	56.288070	50.359245
268.775122	62.300770	50.364250
265.219135	57.428793	50.369255
261.631906	55.418576	50.374260
258.298107	62.818767	50.379265
255.161648	56.647214	50.384269
251.521576	60.045792	50.389274
247.599912	57.334999	50.394279
244.144514	61.081135	50.399284
240.485027	64.112601	50.404289
237.529173	59.428196	50.409293
233.941548	58.819591	50.414298
231.022584	59.359081	50.419303
227.058155	58.224214	50.424308
223.444662	66.278836	50.429313
219.797653	60.990869	50.434317
215.790997	67.053815	50.439322
212.822999	60.656572	50.444327
209.660652	60.864038	50.449332
205.729398	63.637536	50.454337
202.253797	53.206952	50.459341
198.589792	56.495404	50.464346
195.189141	60.849912	50.469351
191.934822	53.867949	50.474356
188.309944	66.537104	50.479361
184.974704	59.893685	50.484365
180.936492	59.026661	50.489370
177.892165	63.050108	50.494375
174.301398	58.873316	50.499380
170.434428	57.194863	50.504385
167.066623	51.018463	50.509389
163.197562	64.197276	50.514394
160.169635	63.387123	50.519399
156.981902	52.111036	50.524404
153.499237	60.692511	50.529409
150.193221	48.403580	50.534413
146.534112	49.571578	50.539418
142.752058	54.697697	50.544423
139.686454	55.835991	50.549428
135.759680	62.164863	50.554433
132.217678	53.222184	50.559437
128.434132	65.644133	50.564442
125.116663	55.198303	50.569447
121.709543	60.129651	50.574452
118.054505	65.166280	50.579457
115.001054	69.010844	50.584461
111.282704	71.029694	50.589466
107.682544	65.361115	50.594471
104.145910	58.818887	50.599476
100.524052	67.608850	50.604481
97.178554	58.559469	50.609485
94.083233	69.782117	50.614490
90.142422	69.368110	50.619495
86.946589	63.164798	50.624500
82.928447	58.732304	50.629505
80.023712	54.482875	50.634509
76.536574	67.443696	50.639514
73.007401	60.084067	50.644519
69.158768	66.394396	50.649524
65.488749	63.403817	50.654529
62.057739	59.524748	50.659533
58.556005	59.121058	50.664538
54.988878	67.260222	50.669543
51.993342	56.887372	50.674548
48.072426	56.299426	50.679553
44.899213	57.720367	50.684557
41.232367	63.015138	50.689562
37.497816	67.168918	50.694567
33.915149	63.006738	50.699572
30.352691	69.259592	50.704577
26.941874	66.161980	50.709581
23.730340	68.250155	50.714586
20.319271	60.119076	50.719591
16.891168	57.837260	50.724596
13.138506	58.855457	50.729601
9.616701	54.095300	50.734605
6.114236	59.550988	50.739610
2.664818	65.659590	50.744615