Thu Aug 25 11:44:03 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.016901	106.164164	0.000000
1.039842	109.473142	0.005005
0.914355	108.509001	0.010010
0.783504	103.081647	0.015014
0.707579	101.302984	0.020019
1.141031	102.573461	0.025024
0.875367	86.824934	0.030029
0.372077	79.927851	0.035034
0.074099	73.716772	0.040038
-0.213165	59.025182	0.045043
-0.313798	51.891014	0.050048
-0.847812	40.234165	0.055053
-1.059562	45.028897	0.060058
-1.334199	38.032729	0.065062
-1.642380	29.769997	0.070067
-1.522486	27.334240	0.075072
-2.137331	9.081029	0.080077
-2.605911	11.723525	0.085082
-3.131723	7.743799	0.090086
-2.991628	4.055205	0.095091
-3.357966	8.886803	0.100096
-4.008285	0.405611	0.105101
-4.732087	-2.733175	0.110106
-4.780218	2.693965	0.115110
-4.839381	-11.852972	0.120115
-4.691438	0.744099	0.125120
-4.627416	-2.910428	0.130125
-4.835411	1.655915	0.135130
-5.542371	5.594925	0.140134
-6.253425	-1.206298	0.145139
-6.528265	10.403500	0.150144
-6.380245	4.018162	0.155149
-6.457855	-6.580713	0.160154
-6.478361	0.398654	0.165158
-7.428425	-6.846005	0.170163
-7.741079	0.919450	0.175168
-8.073933	-0.761999	0.180173
-8.249666	-3.483624	0.185178
-8.074362	2.199571	0.190182
-7.734303	-3.715983	0.195187
-8.369083	-2.597677	0.200192
-8.389002	-2.569122	0.205197
-9.331023	-3.414811	0.210202
-9.242550	5.316009	0.215206
-9.181555	-6.193592	0.220211
-10.263582	6.203895	0.225216
-10.759592	-3.212627	0.230221
-10.732855	-0.438935	0.235226
-10.942692	-4.582059	0.240230
-10.496989	-7.970524	0.245235
-10.495004	-5.006294	0.250240
-11.082381	-3.901743	0.255245
-11.680555	-4.092631	0.260250
-12.071976	9.329268	0.265254
-12.049128	-7.717217	0.270259
-12.589817	-4.032049	0.275264
-12.142172	-13.346486	0.280269
-12.863908	-4.080602	0.285274
-13.407072	-7.421695	0.290278
-13.672345	-8.828996	0.295283
-14.079129	-9.704763	0.300288
-13.668798	-9.326008	0.305293
-13.871162	5.714570	0.310298
-14.020916	-1.570065	0.315302
-14.294920	-7.547591	0.320307
-14.848825	2.900544	0.325312
-15.057938	-5.140412	0.330317
-15.819064	-3.179739	0.335322
-16.385148	10.990858	0.340326
-15.963698	-10.876334	0.345331
-16.487923	-3.409923	0.350336
-16.801624	-6.464267	0.355341
-16.681630	-3.664059	0.360346
-16.941735	-1.598392	0.365350
-16.513699	-0.915529	0.370355
-16.661913	3.593991	0.375360
-17.796558	2.693063	0.380365
-18.122634	7.385475	0.385370
-18.422279	-4.842734	0.390374
-17.891061	2.860103	0.395379
-18.558784	5.005456	0.400384
-18.940098	2.306551	0.405389
-19.109095	1.535894	0.410394
-19.369464	-3.352281	0.415398
-19.395660	-7.239442	0.420403
-20.001526	7.687190	0.425408
-20.491464	0.190103	0.430413
-20.852780	-6.881048	0.435418
-21.011717	-3.167110	0.440422
-20.840070	-15.969025	0.445427
-21.029131	-2.600988	0.450432
-21.106172	-9.083934	0.455437
-21.124673	8.113975	0.460442
-21.914679	8.307484	0.465446
-21.959604	-7.000983	0.470451
-22.230211	2.390370	0.475456
-22.446639	6.964363	0.480461
-22.963718	1.458352	0.485466
-23.462961	0.821697	0.490470
-23.592817	-3.245375	0.495475
-23.648038	0.221361	0.500480
-23.494116	-0.454360	0.505485
-23.941319	3.823598	0.510490
-24.915261	7.611454	0.515494
-24.777109	11.734424	0.520499
-25.038767	9.655844	0.525504
-25.057739	-1.939304	0.530509
-24.880087	-2.694674	0.535514
-25.634014	5.484771	0.540518
-26.245445	-1.363697	0.545523
-26.714025	5.356850	0.550528
-26.159450	11.970869	0.555533
-26.206234	7.549096	0.560538
-26.743608	1.046526	0.565542
-26.999818	-1.441027	0.570547
-27.473170	-6.457180	0.575552
-27.900225	-5.665648	0.580557
-27.919362	-3.666210	0.585562
-27.992932	-0.079542	0.590566
-28.338135	-1.056706	0.595571
-29.180320	-11.956554	0.600576
-29.099349	-7.065334	0.605581
-29.349604	-12.793479	0.610586
-29.575890	-4.639766	0.615590
-29.319386	-2.566459	0.620595
-29.832129	2.974606	0.625600
-30.164890	0.008669	0.630605
-30.522745	-4.000532	0.635610
-30.747812	2.574292	0.640614
-30.842008	-5.206261	0.645619
-31.116109	0.718189	0.650624
-31.455847	-6.577804	0.655629
-31.778370	-2.955292	0.660634
-32.345243	2.515162	0.665638
-32.172171	6.199227	0.670643
-32.521820	7.820185	0.675648
-32.513502	2.611501	0.680653
-32.472901	7.382501	0.685658
-32.991742	6.204754	0.690662
-33.064523	6.934450	0.695667
-33.473667	11.076734	0.700672
-34.050244	0.454799	0.705677
-34.607303	2.459429	0.710682
-35.198844	3.912644	0.715686
-35.151337	5.566285	0.720691
-35.484152	5.080722	0.725696
-35.541924	7.665177	0.730701
-35.263511	6.334039	0.735706
-35.474008	3.671644	0.740710
-35.388771	6.765199	0.745715
-35.819045	17.880502	0.750720
-36.102508	2.008296	0.755725
-36.641239	16.139809	0.760730
-36.925558	18.345314	0.765734
-37.073248	2.907411	0.770739
-37.919038	10.952556	0.775744
-37.916283	13.767972	0.780749
-38.329136	3.958773	0.785754
-38.397783	10.006056	0.790758
-38.395688	-0.402829	0.795763
-38.599493	0.027859	0.800768
-38.589066	1.725274	0.805773
-39.412101	3.844344	0.810778
-39.669909	7.368134	0.815782
-39.592390	6.641108	0.820787
-39.820510	4.905285	0.825792
-40.068457	-0.383466	0.830797
-40.535719	-1.686351	0.835802
-41.047898	8.777396	0.840806
-41.349975	3.838808	0.845811
-41.374769	6.351657	0.850816
-41.289497	3.915001	0.855821
-41.661013	9.196661	0.860826
-41.920647	9.427290	0.865830
-41.618093	-0.955906	0.870835
-42.420438	8.363742	0.875840
-42.807537	3.640955	0.880845
-42.793184	10.105501	0.885850
-43.278106	8.631377	0.890854
-43.357073	-3.821231	0.895859
-44.439666	6.462973	0.900864
-44.269126	4.497008	0.905869
-44.083516	4.901481	0.910874
-44.333607	2.735670	0.915878
-44.391585	-6.347686	0.920883
-44.768768	4.506191	0.925888
-45.115494	4.497368	0.930893
-45.376403	-2.339580	0.935898
-45.474984	0.804921	0.940902
-45.981644	-4.557185	0.945907
-46.426390	11.489474	0.950912
-46.952174	5.238188	0.955917
-47.013104	5.697109	0.960922
-47.198916	9.839201	0.965926
-47.213900	4.925232	0.970931
-47.315020	7.054574	0.975936
-47.203500	0.561064	0.980941
-47.629055	4.645808	0.985946
-48.336781	9.046846	0.990950
-48.526262	1.493192	0.995955
-48.604077	4.710370	1.000960
-48.671567	-2.134738	1.005965
-49.387545	9.151874	1.010970
-50.271641	5.797764	1.015974
-50.052474	6.130541	1.020979
-50.181613	7.299335	1.025984
-50.242166	4.331875	1.030989
-50.236141	1.569117	1.035994
-50.193077	10.069771	1.040998
-50.577664	7.092971	1.046003
-50.971942	11.735960	1.051008
-51.564220	-2.879305	1.056013
-51.520257	4.890384	1.061018
-52.662702	1.722287	1.066022
-52.651141	-4.733412	1.071027
-52.889507	1.970043	1.076032
-52.479768	4.968459	1.081037
-53.027859	-4.009629	1.086042
-53.278096	4.726803	1.091046
-53.115470	-6.558274	1.096051
-53.358472	10.165448	1.101056
-54.058954	-3.300245	1.106061
-54.095319	-0.206621	1.111066
-54.593636	4.955701	1.116070
-54.449334	1.440455	1.121075
-55.441855	6.876365	1.126080
-55.870947	6.630513	1.131085
-55.751217	5.523553	1.136090
-56.020400	6.388426	1.141094
-55.901724	-3.624274	1.146099
-56.158958	6.388239	1.151104
-56.172872	6.289304	1.156109
-56.191399	3.758182	1.161114
-56.988756	8.359924	1.166118
-56.933132	5.424880	1.171123
-57.391379	6.388979	1.176128
-57.599383	5.849060	1.181133
-57.649767	-3.118428	1.186138
-58.408707	2.299864	1.191142
-58.618146	-7.879719	1.196147
-58.807335	-5.837818	1.201152
-58.623666	-14.731243	1.206157
-59.285785	1.947411	1.211162
-59.784768	-1.049427	1.216166
-59.950787	-13.690865	1.221171
-60.120879	-6.637445	1.226176
-60.327245	2.066801	1.231181
-60.132704	-8.043203	1.236186
-60.919920	3.899968	1.241190
-61.077309	-0.441196	1.246195
-61.613108	3.581728	1.251200
-61.896875	-4.545602	1.256205
-61.794761	-0.904205	1.261210
-61.584608	-2.031660	1.266214
-61.526663	-7.257607	1.271219
-62.900836	3.053301	1.276224
-63.372492	-1.216475	1.281229
-63.211726	-0.029832	1.286234
-63.339166	1.714495	1.291238
-63.026381	0.422263	1.296243
-63.680860	7.947052	1.301248
-64.315340	-4.738046	1.306253
-64.856867	-1.859496	1.311258
-65.050076	-1.281773	1.316262
-64.899694	0.672120	1.321267
-64.996716	-0.457824	1.326272
-65.018677	-7.240460	1.331277
-65.112249	-4.362498	1.336282
-65.513364	6.849466	1.341286
-65.636709	2.439693	1.346291
-65.999908	0.165056	1.351296
-66.423212	2.398664	1.356301
-67.158504	-3.905209	1.361306
-67.901189	2.548240	1.366310
-67.200634	-5.869363	1.371315
-67.777830	8.375737	1.376320
-67.541199	4.643544	1.381325
-68.053842	2.278429	1.386330
-68.002778	0.116051	1.391334
-68.079220	0.817847	1.396339
-69.068320	11.637895	1.401344
-69.340906	1.490349	1.406349
-69.039180	6.577933	1.411354
-69.428003	0.279881	1.416358
-69.354818	4.669288	1.421363
-70.160681	8.750349	1.426368
-70.068174	-0.483136	1.431373
-70.512914	1.760158	1.436378
-70.722306	6.165369	1.441382
-70.850711	6.748758	1.446387
-71.810384	6.756885	1.451392
-71.906738	2.266953	1.456397
-72.062956	3.193219	1.461402
-72.219443	6.691641	1.466406
-72.329668	-0.744715	1.471411
-72.525762	-0.157048	1.476416
-72.141580	3.187054	1.481421
-72.765455	3.566505	1.486426
-73.447098	2.183319	1.491430
-73.191253	0.109076	1.496435
-73.399618	5.244948	1.501440
-74.044600	12.132341	1.506445
-74.226055	-4.682810	1.511450
-74.814413	3.056242	1.516454
-74.636821	1.044880	1.521459
-75.265663	2.820316	1.526464
-75.034422	3.220802	1.531469
-75.557530	-3.837649	1.536474
-76.036926	5.725623	1.541478
-76.124892	-7.516502	1.546483
-76.450759	8.720331	1.551488
-76.398471	2.824557	1.556493
-76.227405	2.848497	1.561498
-77.378955	9.315394	1.566502
-77.616082	-7.677691	1.571507
-78.309105	0.795927	1.576512
-78.123567	-1.074312	1.581517
-78.486198	3.797832	1.586522
-78.275918	4.517976	1.591526
-78.117970	0.193840	1.596531
-78.471542	3.947768	1.601536
-78.875003	4.726115	1.606541
-79.550339	-8.800457	1.611546
-79.683722	6.991765	1.616550
-79.621938	-1.860421	1.621555
-79.780237	2.707626	1.626560
-79.968895	2.661381	1.631565
-80.606741	11.787579	1.636570
-80.802525	13.912772	1.641574
-80.703037	0.758328	1.646579
-81.178477	4.468077	1.651584
-82.038696	-0.256501	1.656589
-82.268565	-2.988622	1.661594
-82.372739	4.108255	1.666598
-82.541856	4.334194	1.671603
-82.226474	6.338162	1.676608
-82.533643	-5.604123	1.681613
-82.432378	-4.670747	1.686618
-83.010934	5.755941	1.691622
-83.273969	-0.463743	1.696627
-83.988519	8.655489	1.701632
-84.297906	2.332336	1.706637
-84.757096	-2.705014	1.711642
-85.051668	1.333896	1.716646
-85.061760	-3.625128	1.721651
-85.556212	1.239197	1.726656
-85.518517	1.749103	1.731661
-85.322261	5.160616	1.736666
-85.520101	4.242620	1.741670
-85.172789	-6.191876	1.746675
-86.432188	5.015368	1.751680
-86.865551	7.677657	1.756685
-86.835524	2.566814	1.761690
-86.682481	7.503689	1.766694
-87.204230	-2.528881	1.771699
-87.824499	2.500690	1.776704
-88.256891	1.195508	1.781709
-88.107758	2.083419	1.786714
-88.169482	0.735974	1.791718
-88.154506	0.278175	1.796723
-89.316589	4.646005	1.801728
-89.310694	0.538682	1.806733
-89.484974	2.334641	1.811738
-89.777854	-0.204111	1.816742
-89.773237	-7.851445	1.821747
-90.020162	-1.364948	1.826752
-90.059541	-4.417980	1.831757
-90.217092	-7.851125	1.836762
-91.154621	-3.926604	1.841766
-91.281877	0.589121	1.846771
-91.454317	-6.530601	1.851776
-91.821928	2.043887	1.856781
-91.619368	-6.096369	1.861786
-91.854689	-1.323268	1.866790
-92.297182	-1.332901	1.871795
-92.647550	1.949129	1.876800
-93.128918	0.787661	1.881805
-92.945027	-2.629384	1.886810
-93.184424	0.141715	1.891814
-93.808633	-2.519125	1.896819
-94.225469	6.040932	1.901824
-94.162864	8.476812	1.906829
-94.540229	8.235512	1.911834
-94.380095	2.398770	1.916838
-94.385509	-8.600547	1.921843
-94.883258	1.411683	1.926848
-95.479683	3.602817	1.931853
-95.649958	-2.065093	1.936858
-95.896124	2.595814	1.941862
-95.857212	0.346756	1.946867
-96.390419	7.403294	1.951872
-97.091750	-1.905115	1.956877
-97.114629	-1.815985	1.961882
-97.806364	0.908935	1.966886
-97.548942	-3.209326	1.971891
-97.551201	-3.838429	1.976896
-97.520951	-0.312322	1.981901
-97.493889	11.515917	1.986906
-98.228992	10.849785	1.991910
-98.353491	-2.649205	1.996915
-99.219248	4.692027	2.006912
-98.708175	1.222667	2.016909
-98.134861	4.414903	2.026906
-97.720759	4.765244	2.036902
-96.979112	6.698836	2.046899
-96.572742	3.996647	2.056896
-96.648578	2.754336	2.066893
-95.282937	0.152091	2.076890
-94.831237	2.184968	2.086886
-94.756452	4.701388	2.096883
-94.546300	2.406911	2.106880
-93.690633	3.391309	2.116877
-93.243933	0.980573	2.126874
-92.316728	-1.819066	2.136870
-92.233653	-1.429527	2.146867
-91.749580	0.854868	2.156864
-91.225238	-1.919658	2.166861
-90.698305	3.937614	2.176858
-89.557285	-7.119087	2.186854
-89.464868	-0.145195	2.196851
-89.436976	0.449394	2.206848
-88.941151	-1.056719	2.216845
-88.380291	-5.123086	2.226842
-87.180883	-8.095255	2.236838
-86.922736	-3.906469	2.246835
-86.933649	-2.890821	2.256832
-85.957873	-3.632676	2.266829
-85.306995	-0.680674	2.276826
-85.043700	-2.606511	2.286822
-84.846063	2.808186	2.296819
-83.721111	-4.093037	2.306816
-83.288098	-7.455130	2.316813
-83.514362	-4.093258	2.326810
-82.947797	-6.690668	2.336806
-82.295324	-1.340905	2.346803
-81.647352	2.308465	2.356800
-81.355455	-4.135943	2.366797
-80.487030	-7.778503	2.376794
-79.686593	-8.625930	2.386790
-79.685898	-1.919598	2.396787
-79.450709	-1.256122	2.406784
-78.410200	0.301193	2.416781
-77.888755	-4.528768	2.426778
-77.734439	-9.564129	2.436774
-76.925429	-1.625475	2.446771
-76.553752	-0.805989	2.456768
-76.515900	2.248405	2.466765
-75.553814	0.621717	2.476762
-75.112191	-0.758694	2.486758
-73.978534	5.665579	2.496755
-74.006064	4.368183	2.506752
-73.967853	2.636002	2.516749
-73.048651	-0.564689	2.526746
-72.155830	-5.170909	2.536742
-72.198664	1.225466	2.546739
-72.178284	-6.706436	2.556736
-71.171233	0.070291	2.566733
-70.677347	0.930816	2.576730
-70.087502	2.387687	2.586726
-69.702647	0.433299	2.596723
-68.836742	3.433973	2.606720
-68.300595	0.302806	2.616717
-68.383751	2.435330	2.626714
-67.561950	2.968877	2.636710
-66.939582	-1.496765	2.646707
-66.653962	-1.446236	2.656704
-66.159126	0.750944	2.666701
-65.269157	2.876708	2.676698
-65.346861	5.128754	2.686694
-64.572839	4.561064	2.696691
-64.320515	4.718178	2.706688
-63.275512	6.021370	2.716685
-62.637776	5.646094	2.726682
-62.402057	3.148041	2.736678
-62.442335	7.640181	2.746675
-61.686646	5.215875	2.756672
-61.201854	11.358521	2.766669
-60.168529	4.142205	2.776666
-59.678852	2.557862	2.786662
-59.376117	2.450487	2.796659
-59.545601	10.513958	2.806656
-58.810376	-0.108532	2.816653
-58.369502	7.045182	2.826650
-57.100390	-4.003081	2.836646
-56.461718	-2.674236	2.846643
-56.825770	0.262570	2.856640
-56.376219	6.239676	2.866637
-55.482439	3.619505	2.876634
-54.888585	-3.809880	2.886630
-54.311430	-0.003693	2.896627
-53.910603	-1.289014	2.906624
-53.566390	-0.598271	2.916621
-53.385672	-1.434123	2.926618
-52.476405	3.976777	2.936614
-52.062596	1.900644	2.946611
-51.295603	9.500603	2.956608
-50.964155	4.462825	2.966605
-50.656529	1.240754	2.976602
-50.035371	1.552318	2.986598
-49.193940	-4.354142	2.996595
-48.943378	-0.097641	3.006592
-48.833541	-2.971943	3.016589
-48.113930	-1.880691	3.026586
-47.788023	-3.322165	3.036582
-46.818968	-0.499207	3.046579
-46.636766	-5.789194	3.056576
-45.939382	-0.918463	3.066573
-44.918118	8.013304	3.076570
-45.097424	0.999665	3.086566
-44.736087	2.812288	3.096563
-44.261941	3.241922	3.106560
-43.719002	9.581364	3.116557
-42.569434	1.478863	3.126554
-42.223062	4.960086	3.136550
-42.142206	5.441840	3.146547
-41.803089	7.799636	3.156544
-40.846680	4.384043	3.166541
-40.803364	1.130526	3.176538
-39.995157	-0.893362	3.186534
-39.228263	4.432143	3.196531
-39.200319	2.688900	3.206528
-38.114996	-0.126006	3.216525
-37.793600	-2.577295	3.226522
-37.694681	2.152793	3.236518
-37.330627	4.341957	3.246515
-36.350920	7.812644	3.256512
-36.294916	4.886588	3.266509
-35.327105	1.532565	3.276506
-34.969479	-5.473337	3.286502
-34.429748	-0.375165	3.296499
-33.476337	4.312903	3.306496
-33.476739	-1.670728	3.316493
-33.272559	-4.737208	3.326490
-32.680445	-1.589094	3.336486
-31.968430	-4.351842	3.346483
-31.270619	-8.794456	3.356480
-30.809329	-0.364157	3.366477
-30.349753	0.359196	3.376474
-30.160280	0.370938	3.386470
-29.333878	1.135016	3.396467
-29.026100	4.853535	3.406464
-28.632330	3.331737	3.416461
-27.615674	-0.929590	3.426458
-27.311232	-4.135322	3.436454
-27.344520	0.070622	3.446451
-26.355907	1.683593	3.456448
-26.222488	2.537245	3.466445
-25.375839	3.111252	3.476442
-24.834072	1.727822	3.486438
-24.473140	-0.606118	3.496435
-24.199806	-1.988670	3.506432
-23.594232	3.640879	3.516429
-22.857172	-1.593496	3.526426
-21.777584	-2.820442	3.536422
-21.879945	-1.945687	3.546419
-21.750047	-0.039779	3.556416
-21.100434	-6.755645	3.566413
-20.768697	-11.302457	3.576410
-19.823709	-6.657420	3.586406
-19.071085	-1.972737	3.596403
-18.593435	-0.178337	3.606400
-18.590871	-0.850060	3.616397
-18.390134	1.716318	3.626394
-17.748674	1.476678	3.636390
-16.658259	-4.636686	3.646387
-16.244626	-3.636872	3.656384
-16.223086	-2.740348	3.666381
-15.441614	-5.922622	3.676378
-14.160197	-0.633383	3.686374
-14.199560	-4.523340	3.696371
-14.131585	0.107060	3.706368
-13.847441	-1.337373	3.716365
-12.988919	1.518747	3.726362
-12.479391	2.136073	3.736358
-11.427396	3.197424	3.746355
-10.973427	-5.334607	3.756352
-11.282984	-11.206441	3.766349
-11.082058	-0.863186	3.776346
-10.162983	-2.346914	3.786342
-8.881321	-9.792199	3.796339
-8.323173	-3.252402	3.806336
-8.295800	-7.700841	3.816333
-8.261583	-3.131676	3.826330
-7.819307	-6.149931	3.836326
-6.826315	-6.774099	3.846323
-6.354066	-10.395760	3.856320
-5.688846	-1.414539	3.866317
-5.403783	-10.027807	3.876314
-5.139947	-7.674054	3.886310
-4.289302	-2.589749	3.896307
-3.912427	-0.209356	3.906304
-3.745779	7.481504	3.916301
-3.309244	11.252711	3.926298
-2.275674	17.562805	3.936294
-2.130320	28.320262	3.946291
-1.825878	32.479634	3.956288
-1.892278	51.595236	3.966285
-0.994992	60.574974	3.976282
-0.504521	82.875690	3.986278
0.130075	99.911140	3.996275
0.000000	112.674489	4.001280
0.969312	118.575000	4.006285
0.872072	128.189193	4.011290
1.000923	117.684445	4.016294
1.016214	130.837067	4.021299
0.982610	151.172766	4.026304
1.358361	148.143247	4.031309
1.212010	159.916508	4.036314
1.558746	154.797124	4.041318
1.472137	156.199709	4.046323
1.170181	158.373192	4.051328
1.353681	158.164231	4.056333
1.080204	162.108122	4.061338
1.283122	159.434712	4.066342
0.776606	159.311717	4.071347
1.154698	162.081004	4.076352
1.531727	157.456747	4.081357
1.470928	172.921377	4.086362
1.291898	158.269694	4.091366
1.681799	166.200391	4.096371
1.493551	167.739125	4.101376
1.868961	178.655526	4.106381
1.581666	173.328593	4.111386
1.523372	163.457419	4.116390
1.478791	164.454786	4.121395
1.425342	166.931019	4.126400
1.865654	176.090853	4.131405
1.647030	186.926326	4.136410
1.636025	172.014187	4.141414
1.508947	180.756721	4.146419
1.645742	190.520940	4.151424
1.867031	184.589132	4.156429
1.791897	186.790355	4.161434
2.259064	182.677153	4.166438
1.830403	165.796157	4.171443
1.686498	163.158105	4.176448
1.796479	158.515578	4.181453
1.677100	164.482278	4.186458
1.658446	160.695139	4.191462
1.682250	162.172174	4.196467
1.731112	159.956337	4.201472
1.654737	160.680274	4.206477
1.909573	173.554950	4.211482
1.923865	172.660654	4.216486
1.898009	164.556104	4.221491
1.864358	177.820834	4.226496
1.735564	161.968538	4.231501
1.458448	178.109309	4.236506
2.166831	189.843581	4.241510
2.168866	189.394132	4.246515
2.178718	197.912738	4.251520
1.816866	175.247389	4.256525
1.868965	181.857947	4.261530
2.002127	184.232178	4.266534
2.214045	183.993454	4.271539
2.003710	179.106879	4.276544
1.876419	173.618833	4.281549
1.861312	178.784588	4.286554
2.258000	178.811144	4.291558
2.097404	185.163962	4.296563
1.772377	179.884067	4.301568
2.303929	184.568701	4.306573
2.318446	195.845380	4.311578
1.922334	166.177666	4.316582
1.947240	173.365122	4.321587
1.844843	185.055583	4.326592
2.210169	184.584014	4.331597
2.142138	190.014329	4.336602
2.198911	189.094393	4.341606
2.310367	196.372702	4.346611
2.205423	191.441137	4.351616
2.335549	177.316805	4.356621
1.897621	191.378880	4.361626
2.191265	184.616320	4.366630
2.763619	191.888851	4.371635
2.299204	184.577510	4.376640
2.280026	177.987353	4.381645
1.871345	176.023537	4.386650
2.100544	186.257332	4.391654
2.350563	188.015302	4.396659
2.321636	194.932790	4.401664
2.559959	189.058423	4.406669
2.112434	183.054235	4.411674
2.179360	191.459492	4.416678
2.121152	188.048704	4.421683
1.754000	191.387181	4.426688
2.446992	189.086236	4.431693
2.386711	191.531905	4.436698
2.087044	197.039645	4.441702
2.293330	196.725873	4.446707
2.278199	201.616390	4.451712
2.543153	197.680402	4.456717
2.456330	200.579487	4.461722
2.364842	194.516347	4.466726
2.754573	186.207467	4.471731
2.196998	200.370555	4.476736
2.200624	194.064721	4.481741
2.416031	200.754102	4.486746
2.689128	216.580908	4.491750
2.552068	203.033097	4.496755
2.313338	208.509145	4.501760
2.970623	221.248033	4.506765
2.815524	204.090019	4.511770
2.952392	201.192832	4.516774
2.532035	198.189963	4.521779
2.692170	199.357738	4.526784
2.870655	192.388591	4.531789
2.268697	197.007218	4.536794
2.557425	194.624080	4.541798
2.817027	195.080241	4.546803
2.438644	191.033081	4.551808
2.451323	194.005160	4.556813
2.698174	204.666472	4.561818
2.482498	207.357956	4.566822
2.927098	215.327560	4.571827
2.467667	223.078144	4.576832
2.670089	213.805175	4.581837
2.837164	225.804619	4.586842
2.750736	217.108420	4.591846
2.803766	226.243538	4.596851
2.440864	218.511314	4.601856
2.651855	211.141595	4.606861
2.605210	221.937488	4.611866
2.895631	220.876538	4.616870
2.842346	223.877940	4.621875
2.727168	218.340526	4.626880
3.026609	221.916253	4.631885
2.912463	218.378182	4.636890
2.807626	225.000689	4.641894
2.921614	232.563356	4.646899
2.871007	222.934555	4.651904
3.016479	219.197618	4.656909
3.304071	225.932646	4.661914
2.875502	221.915489	4.666918
3.155798	222.276659	4.671923
2.826288	227.991565	4.676928
3.294757	221.600234	4.681933
3.327066	224.464838	4.686938
2.912908	226.605289	4.691942
3.218880	226.320190	4.696947
2.913665	233.935883	4.701952
3.477660	233.218049	4.706957
3.472246	214.824846	4.711962
3.267859	210.769402	4.716966
2.913790	205.804099	4.721971
2.982021	213.952897	4.726976
3.269571	220.023538	4.731981
3.369887	229.470790	4.736986
3.152571	215.223694	4.741990
3.154181	215.302661	4.746995
3.269999	212.788423	4.752000
3.211726	204.049853	4.757005
3.065108	207.584734	4.762010
3.211982	217.303096	4.767014
3.165985	225.520417	4.772019
3.325141	233.139282	4.777024
3.430849	223.565084	4.782029
3.219299	229.770876	4.787034
3.062457	224.015361	4.792038
3.381281	228.084764	4.797043
3.113958	227.202951	4.802048
3.191643	226.070928	4.807053
3.093628	237.339954	4.812058
3.170060	228.982066	4.817062
3.371076	228.833635	4.822067
2.992141	233.268631	4.827072
2.990348	223.894775	4.832077
2.921394	232.773761	4.837082
2.804685	232.010719	4.842086
3.090041	244.501011	4.847091
3.403764	254.708947	4.852096
3.649973	250.930910	4.857101
3.455181	252.075204	4.862106
3.496363	254.631536	4.867110
3.366018	250.865041	4.872115
3.367006	251.652791	4.877120
3.578045	253.388402	4.882125
3.433251	256.268104	4.887130
3.393840	249.813969	4.892134
3.653319	248.700917	4.897139
3.357696	253.711327	4.902144
3.713258	247.207963	4.907149
3.358992	261.247494	4.912154
3.259975	253.018325	4.917158
3.415709	244.698625	4.922163
3.431267	253.785844	4.927168
3.838463	252.700268	4.932173
3.501625	254.670418	4.937178
3.563668	247.596106	4.942182
3.579702	256.588338	4.947187
3.374342	256.832612	4.952192
3.450465	250.480598	4.957197
3.839829	273.613384	4.962202
3.795080	261.148897	4.967206
3.565171	263.741378	4.972211
3.334400	272.981098	4.977216
3.613020	271.773296	4.982221
3.666408	278.693738	4.987226
3.914222	269.673058	4.992230
3.798004	275.949352	4.997235
3.833988	280.237091	5.002240
4.097306	271.444937	5.007245
4.082922	282.330726	5.012250
4.056474	274.235711	5.017254
3.613461	264.655715	5.022259
3.654668	271.334452	5.027264
4.228275	270.545507	5.032269
4.151599	274.116899	5.037274
3.931873	262.119593	5.042278
3.625227	257.083570	5.047283
3.674580	272.394984	5.052288
4.384680	280.177486	5.057293
4.269949	277.060278	5.062298
3.897913	265.447504	5.067302
4.033372	257.134139	5.072307
3.788878	253.167227	5.077312
4.164817	257.151758	5.082317
3.757613	270.307405	5.087322
3.817050	270.690525	5.092326
4.417774	273.649576	5.097331
3.669092	279.240348	5.102336
3.899932	277.103553	5.107341
3.886220	282.259628	5.112346
3.926579	276.406758	5.117350
4.135954	274.197395	5.122355
4.083486	284.443741	5.127360
3.934700	275.409267	5.132365
3.518813	287.104620	5.137370
4.198078	281.885642	5.142374
4.101037	289.174509	5.147379
4.164066	280.663672	5.152384
4.291787	274.774968	5.157389
3.922770	283.976242	5.162394
4.312031	283.674929	5.167398
4.245589	281.005740	5.172403
3.918793	282.999630	5.177408
4.405094	284.809175	5.182413
3.952308	285.788248	5.187418
4.480544	292.517235	5.192422
4.506563	295.126570	5.197427
4.040457	296.965117	5.202432
4.448016	284.458219	5.207437
4.343008	293.773158	5.212442
4.494748	302.962453	5.217446
4.287134	288.457512	5.222451
4.126025	296.901711	5.227456
4.952438	297.028618	5.232461
4.580742	290.724608	5.237466
4.508014	287.898213	5.242470
4.366041	288.021823	5.247475
4.247347	278.175868	5.252480
4.190005	281.054528	5.257485
4.471522	299.623089	5.262490
4.588789	297.633801	5.267494
4.518208	283.452246	5.272499
4.270046	291.527264	5.277504
4.679473	295.610961	5.282509
4.353200	299.446095	5.287514
4.357396	298.097789	5.292518
4.582680	302.580502	5.297523
4.532467	304.145077	5.302528
4.656537	308.447495	5.307533
4.973675	317.607719	5.312538
4.663506	297.363907	5.317542
4.397123	288.607282	5.322547
4.471057	295.515020	5.327552
4.390171	298.090484	5.332557
4.505946	303.365484	5.337562
4.594495	297.302574	5.342566
5.070074	309.434074	5.347571
4.744035	299.108061	5.352576
5.068901	301.370013	5.357581
4.965518	305.401181	5.362586
4.699128	293.983810	5.367590
4.442618	285.592639	5.372595
4.597142	293.598237	5.377600
4.479579	299.248320	5.382605
4.682449	297.960635	5.387610
4.833402	307.333555	5.392614
4.701553	311.065461	5.397619
4.713803	303.344024	5.402624
5.016350	309.273140	5.407629
4.792783	309.127957	5.412634
4.655352	306.052266	5.417638
4.657882	315.416807	5.422643
4.315762	311.794213	5.427648
4.879298	310.184259	5.432653
5.029823	305.864375	5.437658
4.830560	298.188736	5.442662
5.122808	303.749300	5.447667
4.883714	316.150970	5.452672
5.120055	304.192911	5.457677
4.697541	312.981798	5.462682
4.845580	304.327914	5.467686
4.836482	309.135257	5.472691
4.488263	314.498778	5.477696
4.986998	311.661936	5.482701
4.753501	320.465505	5.487706
4.851259	323.370491	5.492710
5.244028	326.219763	5.497715
5.553570	329.926808	5.502720
4.931939	325.844963	5.507725
5.232538	321.014337	5.512730
4.964162	315.921681	5.517734
5.189884	321.777415	5.522739
4.805500	328.760139	5.527744
5.395760	323.555095	5.532749
5.299086	341.018679	5.537754
5.245497	325.480325	5.542758
5.073978	316.446229	5.547763
4.871229	316.386370	5.552768
5.361642	317.999119	5.557773
5.383795	322.991397	5.562778
5.324558	319.925599	5.567782
5.207804	318.605733	5.572787
5.141153	318.065801	5.577792
5.299786	326.627598	5.582797
5.226507	330.249089	5.587802
5.399775	326.229361	5.592806
5.241344	324.716706	5.597811
5.192301	328.540047	5.602816
5.299163	323.935931	5.607821
4.959517	328.627389	5.612826
4.927238	323.099101	5.617830
5.051308	321.839580	5.622835
5.189450	322.817818	5.627840
5.152055	322.279629	5.632845
5.154885	325.588635	5.637850
4.670994	333.254512	5.642854
5.194893	338.927490	5.647859
5.224085	349.952027	5.652864
5.774715	354.048416	5.657869
6.050853	351.180005	5.662874
5.820220	348.691557	5.667878
5.409395	338.271236	5.672883
5.420633	332.144497	5.677888
5.184742	331.188151	5.682893
5.446866	337.196376	5.687898
5.425146	345.425767	5.692902
5.551038	350.471402	5.697907
5.591248	355.293179	5.702912
5.517316	354.871446	5.707917
5.845370	355.573154	5.712922
5.353373	351.527940	5.717926
5.833845	357.514616	5.722931
5.779145	360.563720	5.727936
5.922483	356.928330	5.732941
5.377598	344.409267	5.737946
5.599047	346.829799	5.742950
5.792871	353.048050	5.747955
5.474317	358.770772	5.752960
5.610649	355.987542	5.757965
5.464419	354.463481	5.762970
5.495367	351.921393	5.767974
5.433336	360.967038	5.772979
5.427863	372.430461	5.777984
5.455441	357.372914	5.782989
5.475527	367.997087	5.787994
5.152024	368.430718	5.792998
6.063365	369.977521	5.798003
5.931327	380.182604	5.803008
5.734027	361.949030	5.808013
5.817043	369.734910	5.813018
5.904278	385.448616	5.818022
5.965106	379.630471	5.823027
5.742951	367.779009	5.828032
6.242821	373.803781	5.833037
5.585788	369.382617	5.838042
5.612006	379.724258	5.843046
5.815265	379.480561	5.848051
5.831777	383.024719	5.853056
5.982397	375.522020	5.858061
5.984003	380.315050	5.863066
5.764712	381.564432	5.868070
6.174818	379.912073	5.873075
5.995487	381.686713	5.878080
6.037694	376.523230	5.883085
5.790944	381.342518	5.888090
5.710875	380.358590	5.893094
5.919942	378.234685	5.898099
5.650121	376.350331	5.903104
5.944107	374.905994	5.908109
6.015825	382.288683	5.913114
6.201003	386.328442	5.918118
6.225824	377.428069	5.923123
5.896406	387.762160	5.928128
6.115243	374.655172	5.933133
6.159879	389.024614	5.938138
6.439809	379.002250	5.943142
6.299483	374.974697	5.948147
6.093146	385.938081	5.953152
6.198140	376.405042	5.958157
5.813734	377.759390	5.963162
5.993334	383.220568	5.968166
6.343616	381.830686	5.973171
5.989500	388.713777	5.978176
6.083508	394.413000	5.983181
6.449531	397.057663	5.988186
6.523986	403.351583	5.993190
6.834447	403.299901	5.998195
6.345696	388.478253	6.003200
6.644916	382.344341	6.008205
6.537816	378.726039	6.013210
6.038406	373.134883	6.018214
6.147337	377.015741	6.023219
6.168564	379.473976	6.028224
6.402232	381.101648	6.033229
6.057067	390.729517	6.038234
6.332620	378.227417	6.043238
6.456017	378.850459	6.048243
5.969020	387.159097	6.053248
6.363786	382.275736	6.058253
6.038571	382.491333	6.063258
6.379721	391.663651	6.068262
6.433687	388.978744	6.073267
6.249882	403.444101	6.078272
6.512043	391.624309	6.083277
6.094777	390.981120	6.088282
5.980414	385.522621	6.093286
6.610560	384.528658	6.098291
6.474860	410.293914	6.103296
6.676156	400.714135	6.108301
6.385327	393.454605	6.113306
6.238321	391.019487	6.118310
6.223574	383.375013	6.123315
6.183145	385.055123	6.128320
6.265800	379.334800	6.133325
6.107645	385.934083	6.138330
6.369354	388.497011	6.143334
6.385791	387.912421	6.148339
6.503201	394.196443	6.153344
6.346308	383.188972	6.158349
6.401465	387.533845	6.163354
6.425659	382.455442	6.168358
6.259795	379.653116	6.173363
6.312482	387.548160	6.178368
6.333050	378.487100	6.183373
6.037336	380.571044	6.188378
6.156128	386.124010	6.193382
6.139489	383.655813	6.198387
6.296848	390.167696	6.203392
6.952321	399.926695	6.208397
6.517581	389.086142	6.213402
6.599932	383.438632	6.218406
6.338766	375.690400	6.223411
5.981725	382.861853	6.228416
6.349001	384.281927	6.233421
6.146771	381.577049	6.238426
6.070081	379.931358	6.243430
6.352450	388.030865	6.248435
6.344065	391.303674	6.253440
6.520724	373.229799	6.258445
6.595863	384.145917	6.263450
6.321413	378.788434	6.268454
6.541343	382.968282	6.273459
6.292223	388.781377	6.278464
6.697759	377.549744	6.283469
6.020576	386.786699	6.288474
6.340545	375.846888	6.293478
6.418858	385.123661	6.298483
6.459456	388.420433	6.303488
6.578620	388.737250	6.308493
6.488522	395.401804	6.313498
6.112376	390.825892	6.318502
6.482536	381.023511	6.323507
6.168965	383.518384	6.328512
6.407240	375.397665	6.333517
6.472997	381.971355	6.338522
6.347094	392.102716	6.343526
6.559908	386.763800	6.348531
6.224143	388.395270	6.353536
6.602101	382.040211	6.358541
6.521499	390.038399	6.363546
6.367577	374.477757	6.368550
6.173914	367.367530	6.373555
6.440014	384.790137	6.378560
6.490096	365.160529	6.383565
5.973200	368.762949	6.388570
6.013304	372.300244	6.393574
6.404925	375.415463	6.398579
6.350009	397.510691	6.403584
6.229798	390.588267	6.408589
6.424332	391.427957	6.413594
6.587855	389.035936	6.418598
6.426750	380.031814	6.423603
6.218302	375.322062	6.428608
6.203601	371.328611	6.433613
6.549612	376.662472	6.438618
6.020386	372.831896	6.443622
6.488735	373.220554	6.448627
6.143492	382.899051	6.453632
6.300298	382.279813	6.458637
6.590141	394.364541	6.463642
6.285245	376.299673	6.468646
6.227877	369.174419	6.473651
5.988347	378.488333	6.478656
6.174999	378.724972	6.483661
6.349126	390.210886	6.488666
6.361849	394.701617	6.493670
6.462853	394.110104	6.498675
6.696510	393.621195	6.503680
6.128484	371.538401	6.508685
6.157792	383.401347	6.513690
6.238491	397.426619	6.518694
6.573262	394.431954	6.523699
6.212628	391.138116	6.528704
6.272465	382.808066	6.533709
6.232345	380.017676	6.538714
6.281929	385.774477	6.543718
6.483937	394.880012	6.548723
5.945787	393.708425	6.553728
6.348412	381.233871	6.558733
6.193706	396.874762	6.563738
6.066301	398.457767	6.568742
6.562571	384.082912	6.573747
6.042838	387.154261	6.578752
6.401267	386.158577	6.583757
6.574411	392.443358	6.588762
6.373644	383.815613	6.593766
6.525242	383.023181	6.598771
6.300006	384.608858	6.603776
6.379704	382.128731	6.608781
6.302853	372.674806	6.613786
6.268773	376.954564	6.618790
6.567709	382.298966	6.623795
5.994603	374.871696	6.628800
6.254201	379.409165	6.633805
6.360275	386.115747	6.638810
6.334480	390.191726	6.643814
6.544798	379.360843	6.648819
5.973062	384.382913	6.653824
6.324555	386.134496	6.658829
6.379214	389.337315	6.663834
6.092103	393.789601	6.668838
6.339799	385.012495	6.673843
6.727074	396.287845	6.678848
6.199260	381.927911	6.683853
6.424914	384.714790	6.688858
6.290777	385.425640	6.693862
6.432846	372.346501	6.698867
6.211522	363.434081	6.703872
6.339885	369.849258	6.708877
5.864722	372.999044	6.713882
6.472194	385.258630	6.718886
6.376168	387.732073	6.723891
6.364360	387.155072	6.728896
6.657720	371.239610	6.733901
6.250095	377.843175	6.738906
6.095847	367.430093	6.743910
5.943171	378.154108	6.748915
6.442908	387.975467	6.753920
6.214497	390.776542	6.758925
6.438710	386.922827	6.763930
6.381066	385.163418	6.768934
6.192060	383.180979	6.773939
5.953127	389.375297	6.778944
6.358370	386.429704	6.783949
6.189878	397.440951	6.788954
6.428624	394.154442	6.793958
6.040861	393.342112	6.798963
5.992078	395.254489	6.803968
6.420620	391.818019	6.808973
6.289556	394.512092	6.813978
6.202201	389.701104	6.818982
6.410253	392.174362	6.823987
5.944536	391.836161	6.828992
6.439127	387.879971	6.833997
6.067482	398.049839	6.839002
6.406665	397.569706	6.844006
6.510492	391.225956	6.849011
6.265830	397.645806	6.854016
6.364742	394.286292	6.859021
6.401438	396.507984	6.864026
6.564212	396.897063	6.869030
6.394229	395.379885	6.874035
6.410118	398.243926	6.879040
6.420876	393.079037	6.884045
6.313768	389.261415	6.889050
6.490025	391.461240	6.894054
6.248933	388.601096	6.899059
5.896203	387.685199	6.904064
6.198926	386.204691	6.909069
6.149852	385.383588	6.914074
6.062605	391.908487	6.919078
6.381148	389.811721	6.924083
6.390410	388.813797	6.929088
6.371922	385.871318	6.934093
6.421834	390.223341	6.939098
6.092725	388.493811	6.944102
6.515110	393.625882	6.949107
6.501157	398.193561	6.954112
6.727646	396.313701	6.959117
6.493496	390.481658	6.964122
6.490604	394.642636	6.969126
6.703036	386.431047	6.974131
6.161367	386.626774	6.979136
6.271383	384.806294	6.984141
5.996351	382.647506	6.989146
5.966799	394.984761	6.994150
6.341284	389.047865	6.999155
6.291404	385.025121	7.004160
6.604887	389.411779	7.009165
6.385952	398.826882	7.014170
6.152503	387.527678	7.019174
6.555920	386.094668	7.024179
6.464323	389.016678	7.029184
6.609471	385.827095	7.034189
6.511753	364.619761	7.039194
6.033043	366.732376	7.044198
6.539588	360.050289	7.049203
6.188867	366.347537	7.054208
6.220197	361.650841	7.059213
6.191359	365.714636	7.064218
6.346631	375.010984	7.069222
6.406364	374.055773	7.074227
6.356126	376.952318	7.079232
6.152953	362.974975	7.084237
6.052907	380.230315	7.089242
6.295587	387.152779	7.094246
6.376595	385.260912	7.099251
6.601384	392.236802	7.104256
6.195513	388.488137	7.109261
6.411400	391.551798	7.114266
6.544349	386.443698	7.119270
6.484216	376.395522	7.124275
6.196670	375.301731	7.129280
6.218025	360.922210	7.134285
5.973941	368.860580	7.139290
6.357420	375.530021	7.144294
6.302164	372.738841	7.149299
5.882217	389.974710	7.154304
6.278640	389.691256	7.159309
5.746226	385.392934	7.164314
5.903256	385.928448	7.169318
6.680090	391.517519	7.174323
6.484599	400.792907	7.179328
6.659978	393.194571	7.184333
6.237132	396.652544	7.189338
6.507855	396.483699	7.194342
6.633528	385.280091	7.199347
6.519457	392.502066	7.204352
6.333260	379.230742	7.209357
6.408571	385.632091	7.214362
5.989750	375.156053	7.219366
6.371308	376.789028	7.224371
6.620484	385.270226	7.229376
6.343810	375.695746	7.234381
6.291460	369.873191	7.239386
6.174275	374.229244	7.244390
6.197760	376.984522	7.249395
6.389962	386.233960	7.254400
6.659801	384.518155	7.259405
6.484762	378.028275	7.264410
6.179756	377.728170	7.269414
6.254201	365.108891	7.274419
6.172159	367.320710	7.279424
6.389843	373.101789	7.284429
6.570016	370.678688	7.289434
6.380772	369.601134	7.294438
6.384798	365.168146	7.299443
6.448290	366.110625	7.304448
6.269195	358.105929	7.309453
6.062677	359.483025	7.314458
6.197009	364.552652	7.319462
6.412906	346.627681	7.324467
6.247313	370.777701	7.329472
6.395885	366.087944	7.334477
6.516625	365.926780	7.339482
6.411037	367.091907	7.344486
6.451099	357.875940	7.349491
6.310526	371.246152	7.354496
6.300878	361.319790	7.359501
6.591612	361.673000	7.364506
6.528690	368.757235	7.369510
6.726963	369.608994	7.374515
6.304362	371.184464	7.379520
6.461569	363.237806	7.384525
6.380758	364.807180	7.389530
6.242262	374.557685	7.394534
6.378731	363.798495	7.399539
6.050612	372.604260	7.404544
6.435175	360.097749	7.409549
6.320722	358.562382	7.414554
6.174409	373.676747	7.419558
6.305901	364.848254	7.424563
5.752145	381.089500	7.429568
6.244624	364.133594	7.434573
6.133964	367.526829	7.439578
6.006838	365.234135	7.444582
6.230671	366.420415	7.449587
6.011253	368.030490	7.454592
6.418564	358.488059	7.459597
5.992431	374.725122	7.464602
6.262029	374.024935	7.469606
6.532962	376.538960	7.474611
6.322651	378.868955	7.479616
6.408852	372.154645	7.484621
6.333408	374.757742	7.489626
6.022582	374.224428	7.494630
6.125016	373.768734	7.499635
6.504763	379.774364	7.504640
6.365306	383.422054	7.509645
6.100561	381.869104	7.514650
6.093171	384.116685	7.519654
6.241928	388.041926	7.524659
6.324369	399.972490	7.529664
6.428458	393.318645	7.534669
6.374415	396.658722	7.539674
6.341368	391.276068	7.544678
6.321381	407.911441	7.549683
6.416794	395.503995	7.554688
6.638194	396.099026	7.559693
6.190640	382.220071	7.564698
6.175970	375.920203	7.569702
6.185486	381.154926	7.574707
6.135994	392.400628	7.579712
6.609503	386.963918	7.584717
6.244134	396.990431	7.589722
6.466290	390.083968	7.594726
6.212086	380.392068	7.599731
6.026681	382.870024	7.604736
6.329629	379.548148	7.609741
6.657602	381.910865	7.614746
6.409681	382.867336	7.619750
6.644316	369.403531	7.624755
6.176220	372.109278	7.629760
6.178419	360.206849	7.634765
5.939147	367.185835	7.639770
6.180790	377.787955	7.644774
6.750519	385.089452	7.649779
6.238844	376.001052	7.654784
6.141062	368.081689	7.659789
6.372676	383.336168	7.664794
5.998482	388.121641	7.669798
6.231363	387.044387	7.674803
6.143286	389.772853	7.679808
6.463131	391.810973	7.684813
6.368209	388.333132	7.689818
6.670724	386.628026	7.694822
6.602239	393.070891	7.699827
6.320688	382.339220	7.704832
5.910973	369.378175	7.709837
6.210792	378.838541	7.714842
6.204885	392.988111	7.719846
6.524821	388.961208	7.724851
6.246474	396.854339	7.729856
6.374068	388.548472	7.734861
6.478824	394.575046	7.739866
6.431937	387.131762	7.744870
6.273269	371.543392	7.749875
6.093766	377.620826	7.754880
6.279053	381.549833	7.759885
6.199709	392.594566	7.764890
6.262732	396.935045	7.769894
6.787624	394.315559	7.774899
6.097157	379.952637	7.779904
6.242749	386.570768	7.784909
6.450596	386.671206	7.789914
6.025060	391.338173	7.794918
6.571822	390.977379	7.799923
6.298919	395.256594	7.804928
6.417446	382.620905	7.809933
6.177717	383.452704	7.814938
6.346340	385.837225	7.819942
6.419056	386.088552	7.824947
5.948287	377.240518	7.829952
5.951303	383.706979	7.834957
6.137955	392.394132	7.839962
5.909180	390.895657	7.844966
6.379449	385.839111	7.849971
6.405219	388.625671	7.854976
6.624300	391.505331	7.859981
6.378612	396.982528	7.864986
6.716708	394.183498	7.869990
6.689492	391.473343	7.874995
6.673579	383.379792	7.880000
6.290167	378.893608	7.885005
6.477182	370.489854	7.890010
6.356914	366.462323	7.895014
6.241220	366.445773	7.900019
5.944738	371.563920	7.905024
6.063951	365.790416	7.910029
6.595215	377.919566	7.915034
5.917122	381.493460	7.920038
6.374940	380.798584	7.925043
6.464519	395.676689	7.930048
6.341479	382.430269	7.935053
6.482654	371.353957	7.940058
5.909576	375.958613	7.945062
6.350001	381.809202	7.950067
6.378968	395.532525	7.955072
6.827856	393.658949	7.960077
6.291974	378.319503	7.965082
6.104918	372.866071	7.970086
6.057667	375.031310	7.975091
6.272534	382.701622	7.980096
6.612458	384.591061	7.985101
6.493627	376.513638	7.990106
6.255570	366.300353	7.995110
6.040843	367.621787	8.000115
6.337040	374.393280	8.005133
6.459816	378.088461	8.010150
6.332869	364.150690	8.015168
6.171798	368.202760	8.020186
6.346485	372.110707	8.025203
6.292264	379.497421	8.030221
6.410936	377.850596	8.035238
6.130875	369.238437	8.040256
6.202815	385.936876	8.045274
6.709196	384.491229	8.050291
6.424154	391.604852	8.055309
6.580051	378.462179	8.060326
6.281253	380.008091	8.065344
6.148882	372.969590	8.070362
6.407333	373.885406	8.075379
6.447333	383.400099	8.080397
6.800065	383.231351	8.085414
6.409837	374.292477	8.090432
6.012224	375.216414	8.095450
6.520443	369.668033	8.100467
6.323437	362.469254	8.105485
6.285781	368.736241	8.110502
6.461645	389.284167	8.115520
6.229938	393.334687	8.120538
6.491079	387.910217	8.125555
6.675123	395.086041	8.130573
6.938156	383.744280	8.135590
6.454565	375.015689	8.140608
6.090474	370.462341	8.145626
6.410278	360.389769	8.150643
6.212538	378.559999	8.155661
6.670224	390.637975	8.160678
6.607815	401.487819	8.165696
6.297314	385.786335	8.170714
5.951906	385.802710	8.175731
5.919977	390.752868	8.180749
5.995386	393.789614	8.185766
6.185277	393.646380	8.190784
6.450807	395.129120	8.195802
6.355635	390.625148	8.200819
6.641153	391.823895	8.205837
6.575746	391.704883	8.210854
6.607133	393.798652	8.215872
6.533810	399.907140	8.220890
6.629904	388.143418	8.225907
6.909425	389.709170	8.230925
6.875413	387.300489	8.235942
6.920353	394.829460	8.240960
6.525399	389.902254	8.245978
6.648335	392.316186	8.250995
6.800454	397.934926	8.256013
6.745984	400.376655	8.261030
6.687969	397.637226	8.266048
6.698023	393.097833	8.271066
6.965609	389.508989	8.276083
6.618627	385.309554	8.281101
6.541424	373.784428	8.286118
6.757356	374.590144	8.291136
6.637897	372.564074	8.296154
6.560265	357.201660	8.301171
6.586886	371.385762	8.306189
6.639024	383.300062	8.311206
6.653487	380.400961	8.316224
6.308935	385.639935	8.321242
6.777947	388.722305	8.326259
6.990155	396.550109	8.331277
6.836756	382.376633	8.336294
6.463747	370.370849	8.341312
6.483817	375.142446	8.346330
6.903962	373.419985	8.351347
6.608080	375.855355	8.356365
6.657809	374.127816	8.361382
6.323830	370.065199	8.366400
6.605674	387.150463	8.371418
6.800343	391.001636	8.376435
6.832022	395.496871	8.381453
6.927577	392.922726	8.386470
6.670990	381.110128	8.391488
6.506229	383.152579	8.396506
6.709257	382.663312	8.401523
6.723645	388.237358	8.406541
6.498059	398.503711	8.411558
6.871414	390.060557	8.416576
6.981898	394.013282	8.421594
6.936217	393.067533	8.426611
6.859461	384.915807	8.431629
6.781724	378.193784	8.436646
6.814140	370.971678	8.441664
6.333066	381.429527	8.446682
7.155971	382.673460	8.451699
7.021270	386.162837	8.456717
6.586221	374.352960	8.461734
6.478618	369.743646	8.466752
6.814963	389.436472	8.471770
6.609119	384.549064	8.476787
6.650980	398.131210	8.481805
6.710807	400.962121	8.486822
6.975600	394.423103	8.491840
6.836701	394.678515	8.496858
7.028959	388.841970	8.501875
6.903457	392.500317	8.506893
6.807122	393.414919	8.511910
6.820898	389.862688	8.516928
6.616999	387.594231	8.521946
7.028434	394.860656	8.526963
7.007124	396.817518	8.531981
6.933452	398.397585	8.536998
6.692944	387.185209	8.542016
6.650793	386.756447	8.547034
6.888536	393.876521	8.552051
6.677753	385.528049	8.557069
6.595063	389.564686	8.562087
6.985258	394.177313	8.567104
6.811601	393.096985	8.572122
6.718418	395.071419	8.577139
6.988401	397.254034	8.582157
6.715276	397.603058	8.587175
6.953488	396.423484	8.592192
6.859429	388.413320	8.597210
6.652221	387.000586	8.602227
6.514896	394.031106	8.607245
6.654796	392.289437	8.612263
6.917569	401.848129	8.617280
7.264075	413.811000	8.622298
7.163013	401.027300	8.627315
6.841134	398.796262	8.632333
6.858635	402.413271	8.637351
7.465950	408.134258	8.642368
7.004793	405.644181	8.647386
6.683225	386.255378	8.652403
6.717605	399.753493	8.657421
6.921559	403.921943	8.662439
7.284393	404.890832	8.667456
7.111592	414.902776	8.672474
7.084175	411.574740	8.677491
7.242398	412.667204	8.682509
6.854724	397.444850	8.687527
6.943082	401.262191	8.692544
7.172465	404.189609	8.697562
7.183037	407.577336	8.702579
7.300430	400.487068	8.707597
6.949746	402.621767	8.712615
7.264897	390.546016	8.717632
6.943831	397.788360	8.722650
7.051134	381.213550	8.727667
7.314098	390.923681	8.732685
6.835373	393.482374	8.737703
7.082308	387.766647	8.742720
6.863129	396.637162	8.747738
6.916165	402.700607	8.752755
7.203760	408.392796	8.757773
7.387441	416.827823	8.762791
7.093882	406.188624	8.767808
7.065657	413.331443	8.772826
7.332005	411.046108	8.777843
7.304548	414.947868	8.782861
6.995886	405.917305	8.787879
7.263448	398.535272	8.792896
6.934545	411.421299	8.797914
7.032377	415.603224	8.802931
7.252699	412.643461	8.807949
7.449650	420.896535	8.812967
7.385819	416.984080	8.817984
7.363575	406.191920	8.823002
7.006103	393.199097	8.828019
7.279864	401.695741	8.833037
6.911516	396.691784	8.838055
7.190608	401.997147	8.843072
7.340114	414.760884	8.848090
7.464844	415.937490	8.853107
7.457709	405.016733	8.858125
6.944419	401.477654	8.863143
7.105175	405.933734	8.868160
7.229452	416.019050	8.873178
7.545881	419.633406	8.878195
7.313892	402.799319	8.883213
7.011998	402.319737	8.888231
7.320459	402.877433	8.893248
7.229325	417.080021	8.898266
7.522241	420.985233	8.903283
7.723256	415.775299	8.908301
7.275058	415.750976	8.913319
7.304214	401.283800	8.918336
7.108400	396.502113	8.923354
6.990002	400.143569	8.928371
6.928398	402.021540	8.933389
7.201876	419.300646	8.938407
7.219582	419.518898	8.943424
7.213883	422.050816	8.948442
7.722221	419.364655	8.953459
7.834565	419.596481	8.958477
7.313001	429.297013	8.963495
7.677916	421.836601	8.968512
7.631751	426.981500	8.973530
7.136176	404.445268	8.978547
7.199174	399.973315	8.983565
7.213869	410.375593	8.988583
7.413943	412.701704	8.993600
7.403032	427.365090	8.998618
7.404915	423.483363	9.003635
7.273722	419.101790	9.008653
7.108217	422.311985	9.013671
7.324943	413.208566	9.018688
7.007996	418.080315	9.023706
7.106664	412.586623	9.028723
7.397660	416.810864	9.033741
7.249517	419.014814	9.038759
7.151163	416.499449	9.043776
7.120496	423.405974	9.048794
7.754638	436.614490	9.053811
7.499870	430.232603	9.058829
7.172450	433.215709	9.063847
7.246024	433.415741	9.068864
7.368915	434.428538	9.073882
7.269981	433.178712	9.078899
7.336701	434.175064	9.083917
7.170274	446.164675	9.088935
7.713565	433.753355	9.093952
7.493206	451.917736	9.098970
7.525239	442.047995	9.103987
7.866766	443.698708	9.109005
7.888267	441.660011	9.114023
7.793391	438.591843	9.119040
7.792821	443.884234	9.124058
8.054308	442.786215	9.129075
7.594878	429.904013	9.134093
7.693690	428.818860	9.139111
7.715889	425.277925	9.144128
7.615980	424.485835	9.149146
7.416142	419.534361	9.154163
7.599003	417.874319	9.159181
7.253249	423.059845	9.164199
7.655060	428.342833	9.169216
7.765200	442.693782	9.174234
7.583284	445.007166	9.179251
7.671409	439.366798	9.184269
7.759194	437.178864	9.189287
7.809114	430.054975	9.194304
7.564389	428.982624	9.199322
7.519077	425.913004	9.204339
7.769483	437.051521	9.209357
7.849234	433.113410	9.214375
7.910161	417.634563	9.219392
7.576896	428.037722	9.224410
7.542767	420.848113	9.229427
7.564444	417.818489	9.234445
7.646031	428.134559	9.239463
7.635380	424.885942	9.244480
7.748286	434.345059	9.249498
7.668107	440.719718	9.254515
8.132701	440.375656	9.259533
7.508993	441.275061	9.264551
7.621936	438.496217	9.269568
7.875394	441.719665	9.274586
7.553109	442.006967	9.279603
7.574609	442.104706	9.284621
7.665089	457.683175	9.289639
7.882775	436.843389	9.294656
7.751336	441.171693	9.299674
7.875375	444.689969	9.304691
7.956757	435.036556	9.309709
7.928511	444.675581	9.314727
8.017814	436.358961	9.319744
7.945785	445.534641	9.324762
7.653545	440.471410	9.329779
7.825139	431.895751	9.334797
7.619993	441.401548	9.339815
7.564213	440.807666	9.344832
7.868711	443.423527	9.349850
7.594442	439.657646	9.354867
8.004546	447.883646	9.359885
8.042569	446.520844	9.364903
7.971871	434.574946	9.369920
7.367425	435.471334	9.374938
7.805602	441.543874	9.379955
7.999279	443.432344	9.384973
7.964639	451.349340	9.389991
7.972964	446.321063	9.395008
7.600842	439.152846	9.400026
7.581381	431.115196	9.405043
7.941250	442.713083	9.410061
7.887750	438.732734	9.415079
7.979760	441.006354	9.420096
8.124367	442.015749	9.425114
7.762778	446.111876	9.430131
8.041791	433.757742	9.435149
7.828437	431.935721	9.440167
8.053564	436.975001	9.445184
8.347272	436.525173	9.450202
7.800229	440.094946	9.455219
7.779936	430.735171	9.460237
7.985074	438.299019	9.465255
7.938577	438.025568	9.470272
8.226008	433.269138	9.475290
7.769973	440.166580	9.480307
7.865578	435.784181	9.485325
7.686241	443.610239	9.490343
8.101372	447.650939	9.495360
8.192132	454.560542	9.500378
8.064937	451.999198	9.505395
8.310589	440.638034	9.510413
8.301450	442.154346	9.515431
8.109370	439.079318	9.520448
7.843644	441.380586	9.525466
7.336471	449.507316	9.530483
8.004621	451.255174	9.535501
7.861067	462.632155	9.540519
8.255387	455.905567	9.545536
8.191496	455.527546	9.550554
8.576772	460.166207	9.555571
8.671824	459.558159	9.560589
8.049978	446.808687	9.565607
7.901409	437.058761	9.570624
8.345747	442.227795	9.575642
8.010502	450.081439	9.580659
8.005963	446.345877	9.585677
8.035983	463.016243	9.590695
8.351502	456.503968	9.595712
8.386727	454.015004	9.600730
8.355950	465.727760	9.605747
8.367506	447.728871	9.610765
8.317822	442.731775	9.615783
8.554401	437.459459	9.620800
8.570403	440.552857	9.625818
7.986341	436.743999	9.630835
8.585636	430.875223	9.635853
8.013344	433.615835	9.640871
8.106502	435.942923	9.645888
8.230837	439.404347	9.650906
7.875574	435.969887	9.655923
8.146323	430.859473	9.660941
8.311582	444.343427	9.665959
8.265362	449.491496	9.670976
8.438753	440.842969	9.675994
7.779528	440.750726	9.681011
8.220358	447.813755	9.686029
8.312285	461.457532	9.691047
8.332089	455.985650	9.696064
8.740064	460.791165	9.701082
8.599709	461.393937	9.706099
8.131539	450.412848	9.711117
8.042251	449.931511	9.716135
8.295834	455.679535	9.721152
8.691617	451.575142	9.726170
8.104424	453.494443	9.731187
8.429314	454.595510	9.736205
8.862976	459.564254	9.741223
8.259451	458.188363	9.746240
8.472259	462.364907	9.751258
8.369790	463.703344	9.756275
8.305038	456.190321	9.761293
8.490535	462.810533	9.766311
8.405600	463.653927	9.771328
8.472446	458.316682	9.776346
8.363739	457.620641	9.781363
8.597483	450.976017	9.786381
8.503526	458.337432	9.791399
8.287911	463.704547	9.796416
8.512359	452.816903	9.801434
8.371813	468.955433	9.806451
8.264644	466.463532	9.811469
8.486543	466.649791	9.816487
8.487186	467.274653	9.821504
8.747598	466.621761	9.826522
8.649108	467.044408	9.831539
8.819886	464.796131	9.836557
8.396371	447.518649	9.841575
8.264909	455.412948	9.846592
8.598336	455.446036	9.851610
8.428217	468.521817	9.856627
8.619518	462.253061	9.861645
8.613541	460.114528	9.866663
8.224611	460.522722	9.871680
8.476878	464.636281	9.876698
8.245882	467.260309	9.881715
8.489808	460.418430	9.886733
8.622812	460.198903	9.891751
8.425613	472.376387	9.896768
8.162180	463.155675	9.901786
8.426338	472.509065	9.906803
8.637745	471.696596	9.911821
8.768312	465.468913	9.916839
8.487248	470.275094	9.921856
8.628262	467.908406	9.926874
8.590142	464.219126	9.931891
8.735145	462.195790	9.936909
8.498405	463.716207	9.941927
8.647515	477.382593	9.946944
8.599371	475.067632	9.951962
9.001799	484.137436	9.956979
8.900483	475.487753	9.961997
8.687947	471.920472	9.967015
8.352588	471.357770	9.972032
9.064729	474.121200	9.977050
8.445061	472.378615	9.982067
8.739528	473.399245	9.987085
8.895854	477.433166	9.992103
8.583969	488.716620	9.997120
9.100897	478.673055	10.002138
8.453886	480.611199	10.007155
9.009958	480.842928	10.012173
9.030376	483.212976	10.017191
8.744285	471.610064	10.022208
8.752879	467.430635	10.027226
8.590955	463.369441	10.032243
8.533865	466.354378	10.037261
9.015188	485.907832	10.042279
9.194067	483.143896	10.047296
8.910406	473.935815	10.052314
8.564440	469.938168	10.057331
8.795885	476.428113	10.062349
9.129072	474.381602	10.067367
8.644139	477.610297	10.072384
8.788983	462.995560	10.077402
9.009277	489.333743	10.082419
8.971558	479.506467	10.087437
8.665877	476.884724	10.092455
8.940413	490.026548	10.097472
9.088564	481.921589	10.102490
9.113070	479.317538	10.107507
8.904753	477.235952	10.112525
8.966428	467.408888	10.117543
8.816601	473.513609	10.122560
8.927643	468.560749	10.127578
9.342275	483.955912	10.132595
9.390631	467.475463	10.137613
9.055442	472.760332	10.142631
8.496771	467.464288	10.147648
8.868215	460.286855	10.152666
9.075274	475.749246	10.157683
8.847579	466.223137	10.162701
8.867685	464.307730	10.167719
8.850119	491.853966	10.172736
9.134774	486.678243	10.177754
9.344264	489.810760	10.182771
8.844766	479.058620	10.187789
9.447575	483.133038	10.192807
8.915492	482.064682	10.197824
8.858436	470.151336	10.202842
9.132049	480.121774	10.207859
9.062440	485.311387	10.212877
9.453073	482.334396	10.217895
8.904761	473.284543	10.222912
9.116052	475.801406	10.227930
9.062665	484.825865	10.232947
9.245796	486.895869	10.237965
9.143242	484.668325	10.242983
8.990560	490.719852	10.248000
9.031392	483.524784	10.253018
9.422204	491.501368	10.258035
9.302822	491.665362	10.263053
9.364016	478.212411	10.268071
8.874295	478.317667	10.273088
9.400678	481.271147	10.278106
8.996507	475.133555	10.283123
9.235644	482.565864	10.288141
8.948542	478.426452	10.293159
9.048732	485.362990	10.298176
9.401575	496.289838	10.303194
9.238078	491.746054	10.308211
9.252794	482.472284	10.313229
9.460574	486.782163	10.318247
9.299150	489.616196	10.323264
9.238980	495.028391	10.328282
8.904811	491.016268	10.333299
9.109123	492.338198	10.338317
9.309226	496.425224	10.343335
8.886925	494.216219	10.348352
9.381337	493.779123	10.353370
9.282269	497.812040	10.358387
9.483563	500.049610	10.363405
9.538993	498.125509	10.368423
8.985858	499.894315	10.373440
9.390659	499.098881	10.378458
9.356367	500.129997	10.383475
9.173278	490.167704	10.388493
9.386149	484.722367	10.393511
9.031596	489.682077	10.398528
9.210937	485.567408	10.403546
9.374239	496.672274	10.408563
9.392496	493.226615	10.413581
9.387711	482.621018	10.418599
9.147081	487.651238	10.423616
9.136910	485.043153	10.428634
9.247211	494.912957	10.433651
9.480031	506.764317	10.438669
9.621497	516.723923	10.443687
9.389851	512.856675	10.448704
9.722435	516.181346	10.453722
9.638379	505.660738	10.458739
9.135626	497.364272	10.463757
9.541908	495.634503	10.468775
9.433259	511.146391	10.473792
9.507110	511.538881	10.478810
9.480134	513.304142	10.483827
9.788225	517.809747	10.488845
9.528689	508.367498	10.493863
9.455038	511.503358	10.498880
10.036207	515.966176	10.503898
9.622459	507.425389	10.508915
9.248691	495.754149	10.513933
9.541189	506.049841	10.518951
9.593591	502.712437	10.523968
9.383828	495.733350	10.528986
9.405777	498.989926	10.534003
9.551152	520.552620	10.539021
9.881893	509.850256	10.544039
10.052499	518.726030	10.549056
10.085584	504.299181	10.554074
9.498628	501.787775	10.559091
9.562399	502.175533	10.564109
9.649136	491.202147	10.569127
9.549644	500.776627	10.574144
9.081480	495.753567	10.579162
9.520604	503.779390	10.584179
9.476235	519.095023	10.589197
9.602305	517.273460	10.594215
9.818335	509.886832	10.599232
9.868035	514.622266	10.604250
9.770397	517.821844	10.609267
9.578026	518.953468	10.614285
9.683727	517.961903	10.619303
9.806756	522.543842	10.624320
9.782963	512.925800	10.629338
9.728811	520.599736	10.634355
9.576633	524.041386	10.639373
9.758846	509.701618	10.644391
9.796227	523.707432	10.649408
9.753733	513.827237	10.654426
9.961099	516.511975	10.659443
9.742176	513.662043	10.664461
9.594769	515.670232	10.669479
9.208551	522.389511	10.674496
9.570823	522.354965	10.679514
9.998597	509.440992	10.684531
9.887449	525.574967	10.689549
10.123968	508.048846	10.694567
9.521532	519.532475	10.699584
9.421140	509.781272	10.704602
9.950851	532.328317	10.709619
10.266730	533.531785	10.714637
10.215442	534.836961	10.719655
10.025895	516.020614	10.724672
9.832578	518.616655	10.729690
9.822177	514.547487	10.734707
9.904391	521.584685	10.739725
9.939972	511.767996	10.744743
10.019443	507.324993	10.749760
10.093474	512.160754	10.754778
9.884760	512.259851	10.759795
9.763030	517.012679	10.764813
10.291817	515.481462	10.769831
9.964305	516.186142	10.774848
9.932091	518.823213	10.779866
9.947697	512.569345	10.784883
9.866216	521.336297	10.789901
10.230471	527.795984	10.794919
10.424795	531.063427	10.799936
10.301327	515.711214	10.804954
10.167962	513.643126	10.809971
9.421351	516.840246	10.814989
9.848345	518.395526	10.820007
10.090492	533.256032	10.825024
10.044835	539.303430	10.830042
10.199637	535.397718	10.835059
10.155108	538.762546	10.840077
10.275430	535.954129	10.845095
10.081637	535.981461	10.850112
10.264389	534.649624	10.855130
10.065424	530.935040	10.860147
10.018774	543.985219	10.865165
10.618365	527.932736	10.870183
9.964921	531.096326	10.875200
9.804604	537.584559	10.880218
9.944772	532.535601	10.885235
10.183324	544.127316	10.890253
10.168764	540.374370	10.895271
10.482415	537.497792	10.900288
10.290991	540.254484	10.905306
10.437637	537.722805	10.910323
10.138834	536.920847	10.915341
10.541489	529.217797	10.920359
10.519863	542.797377	10.925376
10.280677	543.336743	10.930394
10.164472	533.625874	10.935411
10.180506	539.322785	10.940429
10.301496	533.790845	10.945447
10.302386	537.442041	10.950464
10.171445	527.752418	10.955482
10.540064	528.474259	10.960499
10.561180	534.356561	10.965517
10.784789	535.501903	10.970535
10.473545	533.972916	10.975552
10.349578	520.044024	10.980570
10.388640	508.708874	10.985587
10.651031	522.455374	10.990605
10.319256	510.023320	10.995623
10.340680	512.835019	11.000640
10.562376	521.967874	11.005658
10.506268	503.247395	11.010675
10.354548	511.747642	11.015693
10.255959	508.632707	11.020711
10.333228	516.702608	11.025728
10.326140	531.829378	11.030746
10.834037	528.972859	11.035763
10.632810	530.421447	11.040781
10.433049	530.326640	11.045799
10.362913	523.764315	11.050816
10.436180	532.475469	11.055834
10.476150	527.325448	11.060851
10.602774	533.894953	11.065869
10.519786	533.403159	11.070887
10.591775	536.241653	11.075904
10.678545	540.141322	11.080922
10.912854	539.094892	11.085939
10.545787	525.005273	11.090957
10.244720	506.430467	11.095975
10.341846	527.391669	11.100992
10.267139	540.215872	11.106010
10.374200	532.237246	11.111027
10.296385	537.939393	11.116045
10.429501	539.739533	11.121063
10.552109	535.772595	11.126080
10.393733	527.706175	11.131098
10.497878	528.441052	11.136115
10.417472	536.229559	11.141133
10.470531	535.634399	11.146151
10.037392	545.280114	11.151168
10.138821	547.924651	11.156186
10.874496	559.438486	11.161203
10.415127	560.189074	11.166221
10.432830	560.839668	11.171239
10.598203	564.815388	11.176256
10.524039	567.269693	11.181274
10.828021	556.735593	11.186291
10.793768	564.838768	11.191309
10.815411	563.904552	11.196327
10.765511	555.070052	11.201344
10.735000	563.371454	11.206362
11.280541	564.510538	11.211379
10.884502	559.387798	11.216397
10.707795	555.758082	11.221415
10.872498	555.846008	11.226432
10.731661	563.599815	11.231450
10.706676	553.379188	11.236467
10.805377	556.787849	11.241485
11.104390	556.618049	11.246503
11.173796	554.912655	11.251520
10.870101	563.253704	11.256538
11.038844	555.902868	11.261555
10.982494	561.140918	11.266573
10.797820	553.813898	11.271591
10.963297	557.262588	11.276608
10.987085	554.705975	11.281626
11.239709	548.935659	11.286643
10.742933	552.683767	11.291661
10.969191	554.188453	11.296679
11.159425	553.473971	11.301696
10.904259	561.962048	11.306714
11.177089	550.564998	11.311731
10.750444	552.127800	11.316749
10.887010	558.661042	11.321767
10.932070	560.083667	11.326784
10.997246	561.288548	11.331802
10.865491	555.360706	11.336819
11.022255	554.575731	11.341837
11.009717	551.472552	11.346855
11.433915	552.864174	11.351872
10.768603	559.485186	11.356890
11.186608	558.432064	11.361907
10.653097	553.274061	11.366925
10.927835	572.418172	11.371943
11.232978	580.477645	11.376960
11.225509	576.947640	11.381978
11.539576	577.510774	11.386995
11.157376	569.463625	11.392013
10.923534	569.238460	11.397031
11.119742	561.697128	11.402048
11.315012	567.236578	11.407066
11.503191	567.005250	11.412083
11.397289	563.361283	11.417101
11.153269	564.497846	11.422119
11.194503	560.875007	11.427136
11.166172	563.962750	11.432154
11.252245	550.584741	11.437171
11.504857	563.938336	11.442189
11.314206	565.041291	11.447207
11.473773	559.396003	11.452224
11.334149	560.348954	11.457242
10.959927	557.368714	11.462259
10.840211	551.795588	11.467277
10.872113	556.808373	11.472295
11.550660	560.618482	11.477312
11.381466	576.856271	11.482330
11.773716	573.001709	11.487347
11.211062	575.229599	11.492365
11.102194	559.805634	11.497383
11.479749	572.107724	11.502400
11.534640	579.373285	11.507418
11.260099	563.549247	11.512435
11.220587	579.501635	11.517453
11.371339	586.045287	11.522471
11.496591	580.099260	11.527488
11.057891	586.138829	11.532506
11.782407	587.858936	11.537523
11.754022	579.636427	11.542541
11.609818	578.330569	11.547559
11.368898	566.117767	11.552576
11.125649	574.140085	11.557594
11.527765	577.763138	11.562611
11.562153	579.723916	11.567629
11.300538	580.730695	11.572647
11.227578	574.585354	11.577664
11.342099	586.048209	11.582682
11.551873	577.838878	11.587699
11.864332	583.432555	11.592717
11.430451	589.114768	11.597735
11.925687	585.228289	11.602752
11.428749	585.776483	11.607770
11.720690	580.975128	11.612787
11.805285	586.238438	11.617805
11.685024	588.371769	11.622823
11.801260	573.250190	11.627840
11.503298	587.621017	11.632858
11.560616	576.693213	11.637875
11.718580	585.353253	11.642893
11.675000	587.247354	11.647911
11.686427	581.776746	11.652928
11.300026	585.545437	11.657946
11.699870	575.892544	11.662963
11.445999	579.230219	11.667981
11.608225	582.354380	11.672999
11.637130	581.302261	11.678016
11.589561	583.705065	11.683034
11.481104	579.622844	11.688051
11.538413	573.195165	11.693069
11.258896	589.305085	11.698087
11.974706	586.883035	11.703104
11.864066	599.119625	11.708122
12.057335	598.739178	11.713139
12.122067	582.265525	11.718157
11.741095	581.258692	11.723175
12.185424	580.485463	11.728192
11.708119	586.370137	11.733210
11.808287	577.881337	11.738227
11.911190	581.421886	11.743245
11.913433	588.664142	11.748263
11.846627	576.506102	11.753280
11.646700	584.531105	11.758298
11.990207	574.445232	11.763315
11.787346	582.041509	11.768333
11.374952	585.189431	11.773351
12.062123	591.604858	11.778368
12.334629	597.608737	11.783386
12.321376	600.204980	11.788403
11.849958	583.323030	11.793421
11.718416	586.890846	11.798439
12.359572	583.006750	11.803456
11.816975	589.826294	11.808474
12.119001	585.342090	11.813491
11.809097	581.341923	11.818509
11.927512	595.047923	11.823527
12.292861	595.804992	11.828544
12.178877	605.337619	11.833562
12.020406	592.657449	11.838579
12.170392	584.943471	11.843597
11.843524	582.432328	11.848615
12.018956	591.263202	11.853632
12.254065	603.663371	11.858650
12.253555	603.073447	11.863667
12.308293	591.757878	11.868685
11.758767	586.826434	11.873703
12.155049	592.410136	11.878720
12.509027	608.654343	11.883738
12.542240	598.560270	11.888755
12.292757	588.851319	11.893773
12.145691	584.304936	11.898791
12.316324	573.924262	11.903808
12.120161	576.659611	11.908826
12.131319	578.450462	11.913843
12.269747	579.659646	11.918861
12.007339	572.966484	11.923879
12.386891	577.116929	11.928896
12.650641	591.993034	11.933914
12.467345	588.733569	11.938931
12.551861	578.896553	11.943949
12.237266	575.313684	11.948967
12.540515	578.841776	11.953984
12.195736	579.072644	11.959002
11.986163	577.363623	11.964019
12.038646	577.494378	11.969037
11.949428	589.033337	11.974055
12.357789	591.692906	11.979072
12.248645	600.508412	11.984090
12.060305	589.625402	11.989107
12.332693	592.773329	11.994125
12.278894	600.485112	11.999143
12.349653	604.078039	12.004160
12.657165	604.736874	12.009178
12.573403	601.095742	12.014195
12.796043	607.811174	12.019213
12.435611	616.726020	12.024231
12.606535	605.976056	12.029248
12.691392	604.527010	12.034266
12.281258	600.378443	12.039283
12.613590	599.521777	12.044301
12.464606	603.079705	12.049319
12.998075	595.293015	12.054336
12.600625	603.121759	12.059354
12.796465	603.469891	12.064371
12.877316	603.312183	12.069389
12.603084	601.483903	12.074407
12.662703	592.250377	12.079424
12.303215	599.918539	12.084442
12.432773	604.250169	12.089459
12.734476	596.039050	12.094477
12.428332	609.164648	12.099495
12.561680	603.782227	12.104512
12.790821	610.619716	12.109530
12.658891	597.676612	12.114547
12.774169	610.079782	12.119565
12.547157	611.876395	12.124583
12.910271	596.299554	12.129600
12.831086	611.141044	12.134618
12.876766	614.526465	12.139635
12.780293	600.028320	12.144653
12.707964	606.493325	12.149671
12.826896	605.505994	12.154688
12.927835	602.091540	12.159706
12.341910	611.161633	12.164723
12.745308	600.592996	12.169741
12.447324	609.349733	12.174759
12.376876	603.090381	12.179776
12.519210	611.961164	12.184794
12.095505	604.223456	12.189811
12.336570	606.312799	12.194829
12.743814	617.824483	12.199847
12.998401	625.844562	12.204864
12.967813	622.027838	12.209882
12.911081	629.629642	12.214899
13.118173	623.692867	12.219917
12.919280	625.911105	12.224935
13.050971	626.190395	12.229952
13.027274	625.238033	12.234970
12.593992	624.914729	12.239987
13.021398	627.154757	12.245005
12.817260	624.390852	12.250023
13.163258	621.064229	12.255040
13.017497	629.273267	12.260058
12.964538	616.418760	12.265075
13.364855	622.472049	12.270093
13.101251	628.944941	12.275111
12.972584	622.600031	12.280128
12.683618	619.830482	12.285146
12.891398	624.361298	12.290163
13.287216	626.394839	12.295181
13.130787	627.448255	12.300199
13.246985	628.515760	12.305216
13.355322	626.845285	12.310234
13.447732	628.112175	12.315251
13.515811	618.072588	12.320269
13.149289	620.916686	12.325287
13.274420	618.416768	12.330304
13.473189	614.295870	12.335322
13.322227	623.515567	12.340339
13.186878	616.341738	12.345357
13.072321	618.269053	12.350375
13.346934	618.677427	12.355392
13.569390	614.985157	12.360410
13.710142	609.734117	12.365427
13.384430	588.900399	12.370445
13.094894	590.044095	12.375463
13.374351	583.430129	12.380480
13.125637	592.349549	12.385498
12.738908	599.330866	12.390515
13.304114	605.434052	12.395533
13.502140	617.309872	12.400551
13.458972	621.365616	12.405568
13.469207	620.840279	12.410586
13.510282	629.594393	12.415603
13.478752	622.432697	12.420621
13.343418	634.651091	12.425639
13.197681	623.496300	12.430656
13.392850	612.275479	12.435674
13.326854	614.504451	12.440691
13.743239	608.591693	12.445709
13.400963	616.616923	12.450727
13.583775	619.119333	12.455744
13.546110	620.599105	12.460762
13.542407	620.419930	12.465779
13.372085	611.272914	12.470797
13.349618	623.546199	12.475815
13.571315	616.142860	12.480832
13.497649	609.274947	12.485850
13.354164	613.999651	12.490867
13.494667	613.621159	12.495885
13.528303	621.887291	12.500903
13.555024	614.533437	12.505920
13.802907	622.090666	12.510938
13.482137	621.784447	12.515955
13.487732	627.871181	12.520973
13.584607	627.890840	12.525991
13.389276	627.252546	12.531008
13.558757	618.323682	12.536026
13.636670	622.013319	12.541043
13.527954	613.645592	12.546061
13.666800	627.253743	12.551079
13.651942	623.668081	12.556096
13.572608	619.492926	12.561114
13.772208	621.393110	12.566131
13.733156	622.125181	12.571149
13.598455	634.141506	12.576167
13.584460	635.980484	12.581184
13.552581	645.415061	12.586202
13.794204	647.460141	12.591219
14.030812	637.873815	12.596237
13.700216	643.666094	12.601255
13.873382	641.559431	12.606272
14.032031	639.890539	12.611290
13.821712	637.108665	12.616307
14.092078	630.432991	12.621325
14.177151	637.624419	12.626343
14.165834	638.692969	12.631360
13.962319	637.349063	12.636378
13.645824	641.722188	12.641395
14.263749	648.246315	12.646413
13.719821	647.580588	12.651431
13.714918	647.881280	12.656448
13.917553	638.161422	12.661466
13.899851	636.955659	12.666483
14.001377	639.410848	12.671501
14.155861	640.630144	12.676519
14.199117	648.544490	12.681536
14.635697	641.618709	12.686554
14.438204	637.512555	12.691571
14.427742	633.244556	12.696589
14.214428	619.913403	12.701607
13.870246	616.489794	12.706624
14.073775	610.531491	12.711642
13.693349	618.240811	12.716659
14.350585	625.746527	12.721677
14.313315	634.225743	12.726695
14.331382	640.764959	12.731712
14.183282	630.601447	12.736730
14.189950	627.286965	12.741747
14.337078	619.421942	12.746765
14.006018	622.512946	12.751783
13.931867	633.901252	12.756800
14.415091	631.430433	12.761818
14.078889	629.441448	12.766835
14.307361	631.965108	12.771853
14.555567	645.281585	12.776871
14.342977	627.405996	12.781888
14.291149	631.923841	12.786906
14.345713	635.894849	12.791923
14.548892	627.329926	12.796941
14.479760	641.911094	12.801959
14.405602	638.801775	12.806976
14.511735	623.934198	12.811994
13.909422	630.876722	12.817011
13.941790	631.329362	12.822029
14.278872	642.211433	12.827047
14.152488	639.195504	12.832064
14.446118	640.411932	12.837082
14.085999	639.411296	12.842099
14.265037	639.967187	12.847117
14.287280	647.651298	12.852135
14.097790	649.520930	12.857152
14.351367	640.357974	12.862170
14.581312	665.227470	12.867187
14.961145	653.886172	12.872205
14.470985	651.107116	12.877223
14.568984	637.036059	12.882240
14.881200	633.840958	12.887258
14.557065	634.712370	12.892275
14.608309	632.306077	12.897293
14.488527	638.279916	12.902311
14.596519	634.738120	12.907328
14.701177	631.465087	12.912346
14.618501	640.374295	12.917363
14.498816	633.990104	12.922381
14.753166	645.797159	12.927399
14.543062	657.522359	12.932416
14.866341	652.583532	12.937434
14.533452	658.262566	12.942451
15.031419	662.697434	12.947469
15.282873	660.556411	12.952487
14.795307	645.011827	12.957504
14.726378	633.150725	12.962522
14.627548	642.355951	12.967539
14.808574	629.013499	12.972557
14.608022	628.357087	12.977575
14.675327	646.435570	12.982592
14.875707	645.283998	12.987610
14.714911	650.693072	12.992627
14.835113	662.855669	12.997645
15.128076	650.470798	13.002663
15.031651	664.469286	13.007680
15.536495	658.460602	13.012698
14.560616	648.186937	13.017715
15.019215	645.565341	13.022733
14.868707	653.020902	13.027751
14.833863	660.275310	13.032768
15.284270	658.137829	13.037786
15.160202	656.784629	13.042803
15.165902	647.401733	13.047821
14.806154	644.804215	13.052839
14.957382	654.989585	13.057856
15.032506	653.374804	13.062874
14.903665	659.220683	13.067891
15.225120	662.518724	13.072909
15.035956	654.876788	13.077927
14.884974	645.461639	13.082944
15.195236	659.087136	13.087962
14.967002	664.175424	13.092979
15.278392	657.619543	13.097997
15.137457	652.545167	13.103015
14.786937	666.810685	13.108032
15.512670	654.386406	13.113050
15.283370	660.538357	13.118067
15.337632	657.538301	13.123085
15.544903	658.825066	13.128103
15.150432	654.071279	13.133120
15.494844	651.363432	13.138138
14.924828	655.277670	13.143155
15.058556	652.552340	13.148173
15.158497	654.335599	13.153191
15.383183	652.271355	13.158208
15.301196	642.409899	13.163226
15.379050	656.785015	13.168243
15.267452	656.632212	13.173261
15.462352	651.183329	13.178279
15.486370	655.531508	13.183296
15.445986	651.564836	13.188314
15.587544	662.950921	13.193331
15.380078	650.830648	13.198349
15.564889	656.595825	13.203367
15.180471	644.967181	13.208384
15.317538	646.981306	13.213402
15.449812	652.606391	13.218419
15.154595	646.966060	13.223437
15.423621	653.857276	13.228455
15.271803	649.955401	13.233472
15.769811	654.630098	13.238490
15.241194	655.132766	13.243507
15.598943	651.469784	13.248525
15.755185	640.636893	13.253543
15.683429	649.474967	13.258560
16.107472	654.719827	13.263578
15.897881	654.531886	13.268595
15.454513	651.426765	13.273613
15.899867	649.047082	13.278631
15.497135	650.249543	13.283648
15.636786	654.566982	13.288666
15.613084	651.594921	13.293683
15.390689	664.852604	13.298701
15.878376	661.358608	13.303719
15.586688	655.701943	13.308736
15.698111	650.102038	13.313754
15.384236	651.151722	13.318771
15.651255	667.286534	13.323789
15.739346	669.936335	13.328807
16.093071	677.524341	13.333824
15.864635	671.595830	13.338842
15.838452	680.950639	13.343859
15.727113	676.865691	13.348877
16.274678	685.508918	13.353895
15.827074	679.242361	13.358912
15.828494	675.325938	13.363930
15.987231	685.541707	13.368947
15.989375	679.324603	13.373965
16.061774	678.997805	13.378983
15.890350	680.479605	13.384000
15.679341	673.951919	13.389018
15.923027	677.637686	13.394035
15.889524	671.221044	13.399053
16.241826	674.504787	13.404071
15.787133	684.018254	13.409088
15.931874	680.928279	13.414106
16.184620	668.950481	13.419123
16.029349	683.583049	13.424141
16.208933	672.591848	13.429159
16.115158	686.198621	13.434176
16.086422	674.943415	13.439194
16.357596	685.223618	13.444211
15.828705	682.109801	13.449229
16.157400	678.934200	13.454247
15.731542	681.251122	13.459264
16.180469	678.555297	13.464282
16.411149	687.446989	13.469299
15.610926	688.339349	13.474317
16.004596	694.573584	13.479335
16.323532	706.326378	13.484352
16.476891	694.433562	13.489370
16.209927	691.079890	13.494387
16.035319	699.568033	13.499405
16.618684	697.756853	13.504423
16.371997	699.518687	13.509440
16.392225	700.030036	13.514458
16.371834	709.642727	13.519475
16.651009	699.014601	13.524493
16.502991	689.324410	13.529511
16.218077	677.692777	13.534528
16.534100	683.857124	13.539546
16.608933	681.330364	13.544563
16.587601	686.531407	13.549581
16.756115	676.340352	13.554599
16.464694	678.150218	13.559616
16.348316	678.272718	13.564634
16.392236	681.873021	13.569651
16.826017	687.810637	13.574669
16.969581	684.837610	13.579687
16.742301	676.595727	13.584704
16.525920	676.115361	13.589722
16.437959	677.240103	13.594739
16.164177	678.346623	13.599757
16.646709	682.070706	13.604775
16.441080	678.546482	13.609792
16.045084	683.881965	13.614810
16.260127	680.402281	13.619827
16.209676	697.956471	13.624845
16.945986	696.720927	13.629863
16.860556	698.867748	13.634880
17.115830	694.425555	13.639898
17.202512	689.545878	13.644915
16.951747	699.674338	13.649933
17.334703	698.210137	13.654951
16.763772	687.510086	13.659968
16.514653	679.303181	13.664986
16.752964	683.923903	13.670003
16.590538	694.619183	13.675021
16.872419	697.039811	13.680039
16.866572	702.109045	13.685056
16.859334	707.184809	13.690074
16.758829	702.454377	13.695091
16.558817	691.216529	13.700109
17.124336	692.873197	13.705127
17.019057	693.634582	13.710144
16.763255	689.190416	13.715162
17.047193	691.658057	13.720179
17.368369	694.880409	13.725197
17.175928	696.778911	13.730215
16.773095	695.403113	13.735232
16.999641	695.383521	13.740250
17.178910	691.000575	13.745267
16.996019	691.190300	13.750285
17.392531	689.184336	13.755303
17.112084	699.349004	13.760320
16.674512	700.118272	13.765338
16.980545	700.546971	13.770355
17.041157	698.719866	13.775373
17.106942	695.298280	13.780391
17.141022	693.393282	13.785408
16.878520	696.905899	13.790426
16.999754	699.111858	13.795443
17.048609	712.475399	13.800461
17.298232	711.546480	13.805479
17.374778	721.068250	13.810496
17.248043	726.645579	13.815514
17.486952	720.362962	13.820531
17.174276	721.888987	13.825549
17.370478	716.613448	13.830567
17.264409	720.341400	13.835584
17.471737	719.810426	13.840602
17.491562	713.338076	13.845619
17.598383	713.315153	13.850637
17.402827	713.333294	13.855655
17.395210	707.856164	13.860672
17.316218	715.799161	13.865690
17.408157	721.105542	13.870707
17.412510	706.629382	13.875725
17.612982	713.834319	13.880743
17.537182	715.925984	13.885760
17.549504	713.576272	13.890778
17.600143	713.981870	13.895795
17.398999	723.679694	13.900813
17.559103	712.596847	13.905831
17.478876	719.807897	13.910848
17.983401	715.623290	13.915866
17.792354	711.636029	13.920883
17.595782	720.941817	13.925901
17.829952	710.156635	13.930919
17.844653	709.558012	13.935936
17.567801	707.941570	13.940954
17.977081	708.253107	13.945971
17.720488	714.456689	13.950989
17.933171	717.090132	13.956007
17.680267	707.593089	13.961024
17.981355	705.217069	13.966042
17.574423	691.868861	13.971059
17.515615	697.110492	13.976077
17.693193	694.296235	13.981095
17.592377	708.753034	13.986112
17.262642	714.519955	13.991130
17.743841	708.218315	13.996147
17.636277	713.975671	14.001165
17.889442	712.260406	14.006183
17.680911	709.522422	14.011200
17.667335	714.147903	14.016218
18.099357	705.790084	14.021235
17.974064	717.233793	14.026253
18.220104	707.040041	14.031271
18.132401	708.609710	14.036288
18.034180	715.741527	14.041306
18.089575	702.686945	14.046323
17.971141	713.643586	14.051341
18.117186	705.068643	14.056359
17.976477	710.102205	14.061376
18.019125	719.553547	14.066394
18.149908	725.923656	14.071411
18.058974	724.243368	14.076429
18.393889	732.219351	14.081447
18.431791	727.366242	14.086464
17.866056	726.861717	14.091482
18.140313	719.352271	14.096499
18.193172	741.567199	14.101517
18.385519	743.683126	14.106535
18.192353	730.276150	14.111552
18.168494	731.138389	14.116570
18.508674	732.211832	14.121587
18.626786	737.993797	14.126605
18.275774	729.222168	14.131623
18.467333	729.072359	14.136640
18.193812	728.155978	14.141658
18.270938	714.643549	14.146675
18.038626	725.747427	14.151693
18.235572	728.055135	14.156711
18.170913	726.752582	14.161728
18.433468	731.760835	14.166746
18.396919	727.165543	14.171763
18.292862	734.339307	14.176781
18.595239	734.187914	14.181799
18.434595	726.588815	14.186816
18.645606	730.112456	14.191834
18.974494	725.387324	14.196851
18.197816	731.669243	14.201869
18.618373	727.889108	14.206887
18.428396	727.735962	14.211904
18.422559	727.023793	14.216922
18.718070	723.531493	14.221939
18.185492	737.809813	14.226957
18.479429	737.038051	14.231975
18.197259	742.642894	14.236992
18.451360	748.873770	14.242010
18.769075	742.695562	14.247027
18.895207	749.725969	14.252045
18.697160	757.176399	14.257063
18.930681	753.668560	14.262080
18.923220	760.044563	14.267098
19.225425	756.185136	14.272115
18.738861	759.745495	14.277133
18.693760	744.402897	14.282151
19.131797	750.589175	14.287168
18.613913	743.907573	14.292186
18.905291	749.002834	14.297203
19.206421	752.840562	14.302221
19.116090	752.835905	14.307239
19.395854	750.213911	14.312256
19.285689	744.203729	14.317274
19.286464	726.745888	14.322291
18.723760	722.201476	14.327309
18.652747	724.109357	14.332327
18.843488	728.904801	14.337344
19.205772	740.300534	14.342362
19.268863	743.866287	14.347379
19.295984	741.369086	14.352397
18.785277	725.455673	14.357415
19.283743	728.486152	14.362432
19.002671	742.560969	14.367450
19.551791	738.189490	14.372467
19.166220	741.121798	14.377485
19.107695	735.766244	14.382503
19.502015	736.553495	14.387520
18.871858	751.560324	14.392538
19.330175	732.342439	14.397555
19.362610	745.787472	14.402573
18.938341	742.777172	14.407591
19.161410	736.058376	14.412608
18.840169	748.305976	14.417626
19.369547	739.879238	14.422643
19.093824	749.872782	14.427661
19.426714	749.416808	14.432679
19.092956	748.282647	14.437696
18.915537	747.023005	14.442714
19.234321	742.125883	14.447731
19.534339	762.380233	14.452749
19.426887	772.606201	14.457767
19.654855	763.668100	14.462784
19.399823	771.013856	14.467802
19.542306	760.495473	14.472819
19.647405	766.696052	14.477837
19.858719	760.758571	14.482855
19.751251	760.239048	14.487872
19.228151	760.037110	14.492890
19.822076	761.133914	14.497907
19.940100	770.403060	14.502925
19.741861	762.655203	14.507943
19.365931	752.173868	14.512960
19.775365	751.330361	14.517978
19.627121	755.213251	14.522995
19.568322	754.247447	14.528013
20.072817	762.616595	14.533031
19.943184	748.375988	14.538048
19.641703	753.649346	14.543066
19.900045	750.869763	14.548083
19.935086	754.193762	14.553101
19.708563	755.314972	14.558119
19.872681	753.174999	14.563136
19.978222	758.810619	14.568154
20.096777	752.717260	14.573171
19.683136	750.749862	14.578189
19.843468	768.239538	14.583207
20.284440	765.787944	14.588224
19.880654	762.783898	14.593242
20.122878	763.001691	14.598259
19.728405	757.272734	14.603277
20.135509	769.093807	14.608295
20.343793	770.285748	14.613312
19.998777	772.990801	14.618330
19.872316	756.354439	14.623347
19.965524	754.430703	14.628365
19.926565	771.834843	14.633383
20.125661	762.270107	14.638400
20.109917	759.921630	14.643418
19.980029	766.253700	14.648435
20.270641	768.508869	14.653453
20.016415	766.879408	14.658471
20.526106	760.484924	14.663488
20.268594	769.159658	14.668506
20.394126	754.983208	14.673523
20.225810	762.299595	14.678541
20.326261	773.313495	14.683559
20.223666	758.244981	14.688576
19.816267	771.538041	14.693594
20.289979	763.363010	14.698611
20.322300	763.165567	14.703629
19.987135	769.324675	14.708647
20.308851	769.662556	14.713664
20.276824	793.263620	14.718682
20.400486	786.134347	14.723699
20.488733	795.947814	14.728717
20.516954	783.033131	14.733735
20.660015	789.180433	14.738752
20.620446	788.596622	14.743770
20.833182	789.103057	14.748787
21.100883	780.518485	14.753805
20.579486	774.023615	14.758823
20.726097	763.147978	14.763840
20.461177	761.135186	14.768858
20.432991	759.340922	14.773875
20.706854	778.236085	14.778893
20.726729	789.590824	14.783911
21.108182	786.558417	14.788928
20.693546	783.909518	14.793946
20.736559	782.280821	14.798963
21.052396	786.696919	14.803981
20.770846	772.060374	14.808999
20.977783	769.222571	14.814016
20.658152	768.215583	14.819034
20.612968	774.061015	14.824051
20.705422	781.967712	14.829069
20.665833	790.494703	14.834087
20.992801	777.236571	14.839104
20.717944	784.427649	14.844122
20.847940	783.091437	14.849139
20.842217	783.430129	14.854157
20.712593	787.739297	14.859175
20.885140	786.134486	14.864192
20.986639	797.081966	14.869210
20.739717	788.098338	14.874227
20.620913	783.572723	14.879245
21.100895	794.981608	14.884263
21.197776	792.861633	14.889280
21.135850	796.440673	14.894298
21.059054	811.300891	14.899315
21.210112	805.937725	14.904333
20.983849	817.100673	14.909351
21.247690	811.861845	14.914368
21.027891	813.086147	14.919386
21.065759	819.612859	14.924403
21.203778	807.034405	14.929421
21.219157	807.212001	14.934439
21.549557	806.194683	14.939456
21.511681	810.227549	14.944474
21.530037	798.475737	14.949491
21.732705	806.740718	14.954509
21.207826	819.903897	14.959527
21.610059	809.035519	14.964544
21.887596	804.043857	14.969562
21.415031	790.156748	14.974579
21.567540	786.267120	14.979597
21.362544	792.670928	14.984615
21.828283	796.501809	14.989632
21.543558	795.041227	14.994650
21.154967	781.809998	14.999667
21.736261	802.417955	15.004685
21.590396	809.541495	15.009703
21.970412	802.769681	15.014720
21.509283	798.878366	15.019738
21.501932	795.963679	15.024755
21.572815	803.050101	15.029773
21.308034	814.736634	15.034791
21.599379	807.420134	15.039808
21.530418	802.233453	15.044826
21.957220	805.612845	15.049843
21.929467	807.327764	15.054861
21.639725	809.711738	15.059879
22.325571	807.641493	15.064896
22.115937	805.074080	15.069914
21.811182	805.043058	15.074931
22.153302	795.844060	15.079949
21.736310	803.025856	15.084967
22.185868	807.847042	15.089984
22.176183	805.011615	15.095002
21.928797	809.758962	15.100019
21.886979	805.988139	15.105037
21.763911	812.871424	15.110055
21.885774	796.855680	15.115072
21.715911	805.983758	15.120090
21.975573	810.919904	15.125107
22.162009	804.269939	15.130125
22.030335	807.020465	15.135143
21.857230	802.569625	15.140160
22.038842	802.686462	15.145178
22.096309	810.033764	15.150195
22.190572	799.172619	15.155213
21.976261	804.249297	15.160231
22.212739	807.961467	15.165248
22.326288	809.641624	15.170266
22.167260	806.596066	15.175283
22.142695	811.431578	15.180301
21.996508	827.628120	15.185319
22.346636	822.691351	15.190336
22.419487	825.949479	15.195354
22.444795	822.490029	15.200371
22.380910	817.715959	15.205389
22.393175	818.146507	15.210407
22.686288	822.664005	15.215424
22.453856	819.910813	15.220442
22.731355	831.326200	15.225459
22.540092	819.544100	15.230477
22.343648	825.488988	15.235495
22.414872	828.905161	15.240512
22.396023	837.463640	15.245530
22.314051	820.949635	15.250547
22.556238	819.539038	15.255565
22.204334	831.425425	15.260583
22.309105	818.328308	15.265600
22.529527	832.384582	15.270618
22.510208	829.929358	15.275635
22.798981	827.012452	15.280653
22.762834	836.870677	15.285671
22.940640	836.385351	15.290688
22.996350	826.757839	15.295706
22.565546	831.786394	15.300723
23.066339	825.806692	15.305741
23.104969	825.156979	15.310759
23.182179	821.724111	15.315776
22.848174	821.176964	15.320794
22.519587	829.967005	15.325811
22.852606	820.939833	15.330829
22.661693	827.559197	15.335847
22.760604	842.082642	15.340864
23.118257	841.840537	15.345882
23.010927	846.802635	15.350899
23.374285	851.050357	15.355917
23.192188	853.376445	15.360935
23.376966	842.788270	15.365952
23.429481	832.189266	15.370970
23.403011	828.883094	15.375987
23.233099	819.537090	15.381005
22.896211	824.118583	15.386023
22.793698	825.529636	15.391040
23.382056	841.197692	15.396058
22.883600	840.455403	15.401075
23.127421	838.126207	15.406093
23.284134	844.612217	15.411111
23.352079	850.638765	15.416128
23.438882	844.989009	15.421146
23.343877	846.323148	15.426163
23.311261	838.022288	15.431181
23.440923	838.958307	15.436199
23.312643	844.523292	15.441216
23.546855	846.367584	15.446234
23.239662	845.765742	15.451251
23.466864	834.631281	15.456269
23.117796	835.506608	15.461287
23.286406	837.938692	15.466304
23.406938	843.370017	15.471322
23.100518	845.917555	15.476339
23.555651	849.305140	15.481357
23.410814	868.777242	15.486375
23.600717	865.973650	15.491392
23.789271	869.283086	15.496410
23.613993	880.592719	15.501427
24.082743	864.434202	15.506445
23.888951	868.485199	15.511463
24.210859	864.398599	15.516480
24.142143	862.989374	15.521498
23.452382	846.605287	15.526515
23.724372	841.295747	15.531533
23.874275	855.000169	15.536551
24.213823	856.076875	15.541568
24.090216	843.757138	15.546586
23.704192	849.179470	15.551603
23.775854	841.048463	15.556621
24.024559	851.045103	15.561639
24.061409	853.314795	15.566656
24.134581	854.436392	15.571674
24.090276	851.158257	15.576691
24.007281	837.970624	15.581709
23.938992	847.338430	15.586727
24.041763	858.519278	15.591744
24.093181	860.890831	15.596762
24.094538	863.929792	15.601779
23.834389	860.477190	15.606797
24.147917	871.334690	15.611815
24.005693	852.712544	15.616832
24.141219	856.967562	15.621850
23.992158	858.635220	15.626867
24.247112	856.559899	15.631885
24.073516	859.809309	15.636903
24.122482	861.004127	15.641920
24.448871	860.334574	15.646938
24.447375	858.514028	15.651955
24.665779	862.203794	15.656973
24.292126	872.013933	15.661991
24.176974	865.089305	15.667008
24.204852	857.236550	15.672026
24.451822	876.038200	15.677043
24.729977	866.726110	15.682061
24.841249	877.552187	15.687079
24.689793	865.867962	15.692096
24.498229	852.870898	15.697114
24.401549	859.901545	15.702131
24.918097	863.932764	15.707149
24.485314	866.080379	15.712167
24.726022	878.091698	15.717184
24.664812	883.226462	15.722202
24.627243	887.284545	15.727219
25.173327	882.506407	15.732237
24.676509	883.174510	15.737255
24.618853	890.590377	15.742272
24.970178	878.893640	15.747290
24.780647	886.481646	15.752307
24.944604	876.559435	15.757325
24.967287	879.632928	15.762343
25.073957	883.337050	15.767360
24.953924	882.330340	15.772378
24.627723	880.361850	15.777395
24.854217	879.824713	15.782413
24.927410	882.401140	15.787431
24.995907	885.297042	15.792448
24.920689	876.829268	15.797466
24.943493	885.955602	15.802483
25.055891	882.577169	15.807501
25.009439	885.087137	15.812519
24.778195	886.568858	15.817536
24.965440	877.880079	15.822554
24.903269	882.481660	15.827571
25.264606	892.804661	15.832589
24.961080	908.874449	15.837607
24.955362	908.563043	15.842624
25.527963	907.842288	15.847642
25.218516	898.830531	15.852659
25.352523	893.747723	15.857677
25.227297	907.608902	15.862695
25.169551	908.482770	15.867712
25.612026	910.303906	15.872730
25.448508	906.735168	15.877747
25.519761	902.732013	15.882765
25.252742	905.866680	15.887783
25.333334	903.888101	15.892800
25.848673	906.606697	15.897818
25.486419	906.739319	15.902835
25.513034	907.069791	15.907853
25.598482	908.719646	15.912871
25.707772	908.144067	15.917888
25.961638	900.246418	15.922906
25.956013	907.537374	15.927923
26.079886	914.079047	15.932941
26.041000	911.914058	15.937959
25.952114	913.067362	15.942976
25.681935	906.940183	15.947994
25.925245	911.402390	15.953011
25.754504	904.565351	15.958029
25.978865	903.599355	15.963047
25.673976	906.919838	15.968064
25.841175	913.779773	15.973082
25.530542	914.074721	15.978099
25.596475	909.722102	15.983117
25.875979	909.665811	15.988135
26.012860	917.297363	15.993152
26.141138	913.427283	15.998170
25.936631	913.188049	16.003187
26.108911	910.314628	16.008205
26.061488	899.611321	16.013223
25.684676	901.967923	16.018240
26.036608	905.172871	16.023258
25.836698	921.245371	16.028275
25.766867	930.067503	16.033293
25.980037	940.814537	16.038311
26.025254	940.864382	16.043328
26.292483	923.314107	16.048346
26.276701	933.740400	16.053363
26.273539	932.156795	16.058381
26.195081	924.939213	16.063399
26.147518	936.392975	16.068416
26.137241	926.845177	16.073434
26.224870	935.336526	16.078451
26.227036	945.614845	16.083469
26.439294	951.464181	16.088487
26.184822	951.803980	16.093504
26.329503	948.638229	16.098522
26.427162	956.386397	16.103539
26.564084	953.370185	16.108557
27.023689	945.695903	16.113575
26.688700	952.227434	16.118592
26.990834	951.842546	16.123610
26.726745	956.901820	16.128627
26.956613	960.826498	16.133645
27.020264	955.275009	16.138663
26.714635	955.376669	16.143680
27.205135	943.112126	16.148698
27.059156	952.375393	16.153715
26.771251	955.125173	16.158733
26.678842	950.838379	16.163751
26.533712	953.496361	16.168768
26.864750	943.749909	16.173786
26.808792	950.329239	16.178803
26.578389	948.525614	16.183821
26.803373	957.200581	16.188839
26.680915	957.308256	16.193856
26.922703	951.050354	16.198874
26.685395	955.158682	16.203891
27.121175	957.037677	16.208909
27.306403	966.047085	16.213927
26.997195	968.503557	16.218944
27.279857	971.526865	16.223962
27.224991	974.640927	16.228979
27.399810	974.055079	16.233997
27.024847	959.048004	16.239015
27.201713	976.563696	16.244032
27.218046	974.301684	16.249050
27.581934	979.960013	16.254067
27.520802	978.852550	16.259085
27.593278	975.395147	16.264103
27.407906	965.480282	16.269120
27.454766	955.522725	16.274138
27.345300	952.586143	16.279155
27.222992	972.455618	16.284173
27.514238	968.234942	16.289191
27.431912	980.811344	16.294208
27.579709	972.800893	16.299226
26.940711	978.228185	16.304243
27.399068	972.838913	16.309261
27.580844	971.463016	16.314279
27.296042	981.344501	16.319296
27.752865	973.689579	16.324314
27.606196	970.140279	16.329331
27.745181	980.715921	16.334349
27.559996	982.379784	16.339367
27.647578	979.762622	16.344384
28.051817	996.494776	16.349402
28.029405	992.007654	16.354419
27.997052	992.034939	16.359437
28.181313	968.937034	16.364455
27.934131	977.102160	16.369472
27.894266	971.879313	16.374490
27.580560	982.901428	16.379507
27.917538	986.784084	16.384525
28.008830	993.286709	16.389543
27.987229	1001.050426	16.394560
28.270346	995.483474	16.399578
28.204642	1003.733789	16.404595
27.905161	992.388258	16.409613
27.954353	992.813025	16.414631
28.253581	994.934328	16.419648
28.200554	994.586151	16.424666
28.333695	991.450603	16.429683
28.314371	995.941357	16.434701
28.278277	995.874553	16.439719
28.303007	988.770167	16.444736
28.345662	993.197561	16.449754
28.502123	995.820920	16.454771
28.620581	1001.457748	16.459789
28.532437	993.866111	16.464807
28.125193	987.179706	16.469824
28.442390	988.259922	16.474842
28.475908	976.385695	16.479859
28.415251	993.430530	16.484877
28.920387	989.466674	16.489895
28.287615	990.007758	16.494912
28.544503	990.586178	16.499930
28.425515	998.475606	16.504947
28.574359	1004.274934	16.509965
28.712120	1010.363182	16.514983
28.473387	1016.674524	16.520000
28.867384	1013.343466	16.525018
28.593878	1013.967118	16.530035
28.779710	1016.756294	16.535053
28.986845	1018.983548	16.540071
28.760537	1019.012818	16.545088
28.864932	1019.908625	16.550106
28.792544	1020.503923	16.555123
28.757342	1017.158058	16.560141
29.080835	1011.944541	16.565159
28.877668	1023.211296	16.570176
28.975173	1014.943615	16.575194
29.211052	1014.641692	16.580211
29.225021	1008.463646	16.585229
29.389686	1017.410029	16.590247
29.058761	1019.112509	16.595264
29.111042	1014.960821	16.600282
29.082374	1013.273906	16.605299
28.899451	1012.759886	16.610317
29.254060	1010.302856	16.615335
28.971563	1009.700294	16.620352
29.159114	1021.748441	16.625370
29.661241	1036.398219	16.630387
29.593566	1036.958065	16.635405
29.586452	1022.363523	16.640423
29.300359	1019.669200	16.645440
29.588358	1022.268798	16.650458
29.686496	1014.868875	16.655475
29.444275	1010.441435	16.660493
29.325918	1004.902668	16.665511
29.426267	1024.882485	16.670528
29.775664	1026.020775	16.675546
29.613090	1031.868905	16.680563
29.787471	1031.308370	16.685581
30.074776	1032.951857	16.690599
29.610376	1034.388069	16.695616
29.748851	1037.768499	16.700634
29.539353	1032.670042	16.705651
29.526413	1037.304976	16.710669
29.482385	1033.149438	16.715687
29.231980	1028.442406	16.720704
29.661579	1028.182715	16.725722
29.980380	1026.166799	16.730739
29.808825	1031.407258	16.735757
30.266726	1036.334498	16.740775
29.581377	1040.216394	16.745792
29.926724	1051.163695	16.750810
30.085086	1047.105834	16.755827
30.271959	1056.885056	16.760845
30.748670	1046.711775	16.765863
30.430330	1048.424909	16.770880
30.140057	1035.837659	16.775898
30.086880	1020.420348	16.780915
29.932496	1034.431363	16.785933
30.458513	1048.900681	16.790951
30.240987	1052.920724	16.795968
30.400580	1052.056388	16.800986
30.468499	1057.606477	16.806003
30.471315	1051.433320	16.811021
30.847498	1035.074555	16.816039
30.662856	1038.953741	16.821056
30.420989	1040.112087	16.826074
30.403335	1032.723986	16.831091
30.233839	1047.933445	16.836109
30.516526	1051.341776	16.841127
30.555143	1052.961112	16.846144
30.368361	1050.238602	16.851162
30.887663	1056.049333	16.856179
30.488947	1061.214937	16.861197
30.325607	1057.709257	16.866215
30.547835	1060.167685	16.871232
30.375281	1064.417373	16.876250
30.781768	1058.095759	16.881267
30.425206	1053.228624	16.886285
30.819395	1058.058554	16.891303
31.166739	1070.779141	16.896320
31.044706	1068.642939	16.901338
31.178365	1060.741963	16.906355
30.609740	1057.511225	16.911373
30.691612	1068.345180	16.916391
31.024320	1073.093227	16.921408
31.025521	1078.151995	16.926426
31.092458	1075.743184	16.931443
31.668505	1078.518569	16.936461
31.525805	1068.839962	16.941479
31.321896	1064.191907	16.946496
31.178253	1049.890137	16.951514
31.099005	1051.076654	16.956531
30.990779	1052.166724	16.961549
31.516298	1068.917815	16.966567
31.488729	1065.886330	16.971584
31.300192	1066.777542	16.976602
31.503045	1068.610992	16.981619
31.552840	1076.047970	16.986637
31.736643	1067.318613	16.991655
31.877583	1067.694293	16.996672
31.499978	1054.751477	17.001690
31.654064	1044.521447	17.006707
31.266642	1051.001267	17.011725
31.195891	1050.561190	17.016743
31.434233	1069.244474	17.021760
31.451736	1064.003143	17.026778
31.754446	1068.774824	17.031795
31.350022	1082.045557	17.036813
31.892021	1072.348034	17.041831
31.798535	1071.917830	17.046848
31.809545	1071.231410	17.051866
31.669364	1069.748157	17.056883
31.648778	1071.746005	17.061901
31.613009	1070.173808	17.066919
31.541236	1075.086217	17.071936
31.681798	1085.393427	17.076954
31.829334	1080.579849	17.081971
31.941673	1092.589335	17.086989
31.758576	1088.790094	17.092007
31.864790	1090.957429	17.097024
31.624358	1093.191700	17.102042
32.059556	1092.842767	17.107059
32.534122	1105.963176	17.112077
32.281790	1085.679121	17.117095
32.148195	1101.116533	17.122112
32.217015	1108.493738	17.127130
32.376019	1105.824341	17.132147
32.153659	1112.357217	17.137165
32.756317	1103.751569	17.142183
32.481168	1110.532560	17.147200
32.472265	1114.134915	17.152218
32.727359	1110.734082	17.157235
32.300285	1112.956572	17.162253
32.539015	1109.201691	17.167271
32.631379	1110.683221	17.172288
32.612820	1114.602675	17.177306
33.055028	1110.591847	17.182323
32.669595	1117.570005	17.187341
32.659799	1109.511599	17.192359
32.897091	1109.168427	17.197376
32.544214	1112.610077	17.202394
32.461166	1111.578624	17.207411
32.739010	1115.609431	17.212429
32.905586	1111.670191	17.217447
32.697953	1112.652761	17.222464
32.543038	1104.778043	17.227482
33.011610	1105.556835	17.232499
32.607332	1106.898423	17.237517
32.670771	1097.506245	17.242535
32.905422	1099.776536	17.247552
32.750800	1130.160256	17.252570
33.175079	1115.157215	17.257587
33.309013	1130.079357	17.262605
33.243939	1124.368100	17.267623
33.478897	1130.507434	17.272640
33.008975	1126.109328	17.277658
33.529353	1118.258192	17.282675
33.437713	1131.849190	17.287693
33.480892	1122.958799	17.292711
33.301048	1121.292403	17.297728
33.083459	1115.614513	17.302746
33.343681	1120.421267	17.307763
33.293697	1136.180131	17.312781
33.273197	1131.815753	17.317799
33.462939	1124.871655	17.322816
33.416023	1135.028384	17.327834
33.554376	1130.228855	17.332851
33.309230	1140.710141	17.337869
33.364733	1129.476164	17.342887
33.727529	1134.033317	17.347904
33.524265	1137.268490	17.352922
33.627835	1130.000215	17.357939
33.369421	1142.153031	17.362957
33.801188	1143.552984	17.367975
34.021727	1148.649992	17.372992
33.886632	1152.464634	17.378010
34.144312	1152.111955	17.383027
34.049242	1154.740032	17.388045
34.266089	1154.737740	17.393063
34.366048	1150.316614	17.398080
33.956906	1144.624544	17.403098
34.143936	1136.809848	17.408115
33.996349	1140.743212	17.413133
34.068545	1147.987358	17.418151
34.034675	1150.940368	17.423168
34.365792	1157.175100	17.428186
34.247794	1155.394869	17.433203
34.407697	1156.799548	17.438221
34.403806	1150.592693	17.443239
34.592250	1152.115978	17.448256
34.438603	1151.199728	17.453274
34.346508	1152.467161	17.458291
33.938342	1160.723867	17.463309
33.959609	1157.132438	17.468327
34.301953	1156.387790	17.473344
34.109154	1166.438003	17.478362
34.262913	1164.548918	17.483379
34.171752	1169.177206	17.488397
34.483921	1172.861814	17.493415
34.614394	1174.539355	17.498432
34.240088	1179.000564	17.503450
34.594497	1176.322632	17.508467
34.739598	1180.011327	17.513485
34.565542	1175.519516	17.518503
34.713810	1174.795807	17.523520
34.926775	1176.154303	17.528538
34.840525	1185.152707	17.533555
34.946557	1188.863304	17.538573
35.164568	1198.593544	17.543591
35.107657	1200.032196	17.548608
34.947957	1206.204987	17.553626
35.287115	1194.973865	17.558643
35.523026	1188.754672	17.563661
34.939705	1178.072044	17.568679
35.189560	1176.193149	17.573696
35.021170	1168.797051	17.578714
35.242038	1174.948075	17.583731
35.650078	1184.856822	17.588749
34.944615	1187.094535	17.593767
35.165216	1184.387072	17.598784
35.245268	1189.793288	17.603802
35.531195	1190.152565	17.608819
35.473827	1195.280505	17.613837
35.713697	1186.264589	17.618855
35.652687	1190.351660	17.623872
35.310089	1195.956643	17.628890
35.370544	1194.561867	17.633907
35.414826	1196.805192	17.638925
35.885302	1195.926856	17.643943
35.689159	1182.993386	17.648960
35.618950	1202.062830	17.653978
35.665772	1199.120655	17.658995
35.792806	1188.039540	17.664013
35.682812	1194.901987	17.669031
36.348363	1181.871380	17.674048
35.902362	1191.301701	17.679066
36.137278	1184.511452	17.684083
36.265391	1187.603194	17.689101
35.967516	1183.370627	17.694119
35.947868	1180.931185	17.699136
35.939935	1192.091717	17.704154
36.332053	1189.133314	17.709171
36.253588	1184.055311	17.714189
36.108207	1181.544048	17.719207
35.943084	1191.305910	17.724224
35.956078	1193.162808	17.729242
36.123407	1185.906611	17.734259
36.445306	1200.019862	17.739277
36.351801	1209.013102	17.744295
36.689706	1205.523536	17.749312
36.356016	1194.801786	17.754330
36.239630	1188.622011	17.759347
36.169490	1196.560679	17.764365
36.300921	1204.114310	17.769383
36.253713	1202.581764	17.774400
36.336463	1212.623545	17.779418
36.175588	1216.877751	17.784435
36.651036	1214.486969	17.789453
36.369298	1206.155540	17.794471
36.617400	1222.726174	17.799488
36.806191	1235.938791	17.804506
36.826010	1227.986148	17.809523
37.171389	1226.944369	17.814541
37.169669	1228.453274	17.819559
37.502853	1224.270150	17.824576
37.117572	1221.534531	17.829594
37.078484	1203.227226	17.834611
36.987574	1200.306631	17.839629
36.896412	1205.468271	17.844647
37.139039	1211.966201	17.849664
37.057723	1226.035347	17.854682
37.248047	1219.962144	17.859699
37.194410	1219.014442	17.864717
37.347436	1220.518036	17.869735
37.383195	1220.597766	17.874752
37.390611	1231.049001	17.879770
37.469566	1223.711959	17.884787
37.606387	1223.368747	17.889805
37.384263	1216.823667	17.894823
37.395531	1223.307357	17.899840
37.343339	1228.112595	17.904858
37.430886	1217.782435	17.909875
37.430060	1224.015549	17.914893
37.235401	1225.185445	17.919911
37.687787	1219.086963	17.924928
37.767788	1229.826633	17.929946
37.761001	1225.248639	17.934963
37.868102	1220.633868	17.939981
37.553318	1228.980119	17.944999
37.584677	1224.307785	17.950016
37.709493	1228.444646	17.955034
37.508959	1230.587474	17.960051
37.813961	1220.977498	17.965069
37.917830	1245.343681	17.970087
38.089870	1241.476142	17.975104
37.954844	1254.859432	17.980122
37.895384	1249.440752	17.985139
38.378740	1246.824660	17.990157
38.095399	1248.630161	17.995175
38.303961	1236.390656	18.000192
38.504408	1240.916468	18.005210
38.263399	1237.350337	18.010227
38.588614	1246.546242	18.015245
38.284476	1244.694177	18.020263
38.733760	1241.818329	18.025280
38.595581	1241.761206	18.030298
38.026867	1237.492163	18.035315
38.839600	1233.303332	18.040333
38.221504	1244.449040	18.045351
38.501863	1230.554075	18.050368
38.524739	1238.260433	18.055386
38.539675	1248.398067	18.060403
38.692593	1239.234798	18.065421
38.400087	1249.016649	18.070439
38.434123	1241.658234	18.075456
38.435334	1246.164769	18.080474
38.714712	1241.595586	18.085491
38.744953	1238.198400	18.090509
38.622453	1261.211484	18.095527
38.883984	1258.614366	18.100544
38.736465	1272.435138	18.105562
39.067663	1272.654778	18.110579
39.487636	1265.863907	18.115597
39.290463	1272.380272	18.120615
39.258504	1265.745418	18.125632
39.006875	1267.836293	18.130650
39.331284	1273.630293	18.135667
39.397075	1260.712534	18.140685
38.999675	1263.959211	18.145703
39.297483	1261.911844	18.150720
39.634278	1267.268390	18.155738
39.044358	1268.800026	18.160755
39.363688	1263.407203	18.165773
39.347213	1266.679407	18.170791
39.490968	1265.385186	18.175808
39.311733	1263.983777	18.180826
39.311095	1271.226761	18.185843
39.795697	1279.892769	18.190861
39.519724	1284.247078	18.195879
39.959314	1289.770565	18.200896
39.879335	1285.049386	18.205914
39.673358	1287.827407	18.210931
39.969000	1287.339386	18.215949
39.865025	1295.179255	18.220967
40.008990	1280.551364	18.225984
39.784268	1290.723415	18.231002
39.768022	1289.482664	18.236019
39.970230	1282.271458	18.241037
40.156048	1294.925992	18.246055
40.337763	1285.480469	18.251072
40.007860	1288.303153	18.256090
40.265966	1282.421287	18.261107
40.127014	1285.829452	18.266125
40.027045	1294.514471	18.271143
40.358308	1288.845208	18.276160
40.333873	1287.441634	18.281178
39.730642	1282.720384	18.286195
39.870617	1280.767173	18.291213
40.017599	1295.643227	18.296231
40.400848	1298.486726	18.301248
40.438581	1309.242534	18.306266
40.116775	1304.729656	18.311283
40.531792	1307.322019	18.316301
40.504136	1314.278912	18.321319
40.692692	1314.950103	18.326336
40.560258	1308.845386	18.331354
40.595787	1310.667206	18.336371
41.170805	1299.443247	18.341389
40.624617	1306.030087	18.346407
40.965403	1295.723323	18.351424
40.815658	1307.590975	18.356442
40.569246	1302.659175	18.361459
41.215252	1308.046183	18.366477
41.222609	1320.750788	18.371495
41.209431	1303.127307	18.376512
41.218188	1298.837201	18.381530
40.924806	1299.372456	18.386547
41.528588	1315.145815	18.391565
41.297901	1319.635051	18.396583
41.515307	1307.324683	18.401600
41.330695	1300.666394	18.406618
40.967720	1304.851297	18.411635
41.346492	1317.825920	18.416653
41.561018	1319.278860	18.421671
41.758799	1314.094420	18.426688
41.737034	1320.902065	18.431706
41.567463	1315.431188	18.436723
41.962424	1322.924646	18.441741
41.579587	1324.354411	18.446759
41.763411	1315.069493	18.451776
41.713756	1316.077816	18.456794
41.623721	1311.298243	18.461811
41.685167	1308.991249	18.466829
41.649674	1315.614846	18.471847
41.960104	1316.825535	18.476864
42.122300	1311.523591	18.481882
41.621341	1316.010990	18.486899
41.663274	1312.283745	18.491917
41.547884	1315.735562	18.496935
41.545873	1313.665734	18.501952
41.922864	1318.037670	18.506970
42.065037	1337.733565	18.511987
42.197775	1330.621589	18.517005
42.036444	1342.393246	18.522023
42.117724	1334.143740	18.527040
42.191902	1340.418793	18.532058
42.195425	1344.035027	18.537075
42.336270	1330.742529	18.542093
42.303872	1335.017660	18.547111
42.207146	1344.257633	18.552128
42.527463	1344.586280	18.557146
42.539318	1363.235927	18.562163
42.810875	1348.600613	18.567181
42.996699	1364.452124	18.572199
43.214809	1366.958578	18.577216
43.058272	1340.218025	18.582234
42.920504	1342.108027	18.587251
42.769100	1333.812924	18.592269
42.535995	1340.252890	18.597287
42.968162	1343.562116	18.602304
43.056211	1356.566538	18.607322
43.132175	1363.538774	18.612339
43.414498	1338.152778	18.617357
43.168973	1351.288356	18.622375
43.031012	1330.512718	18.627392
43.612035	1331.627363	18.632410
43.370893	1333.435728	18.637427
43.579683	1330.143097	18.642445
43.131567	1324.561219	18.647463
43.069415	1330.286412	18.652480
43.030062	1329.368024	18.657498
43.259006	1346.172156	18.662515
43.492484	1351.560694	18.667533
43.219140	1353.954792	18.672551
43.529247	1355.389604	18.677568
43.647185	1347.358416	18.682586
43.576404	1351.664812	18.687603
43.891812	1354.345375	18.692621
43.767525	1357.233687	18.697639
43.917264	1354.436313	18.702656
44.298920	1355.250826	18.707674
43.720298	1363.827831	18.712691
43.858380	1359.583722	18.717709
43.814098	1362.866612	18.722727
43.964200	1364.679956	18.727744
43.755282	1353.799701	18.732762
43.394242	1352.717112	18.737779
43.600317	1348.345585	18.742797
43.600483	1364.652231	18.747815
43.715120	1373.575072	18.752832
44.224098	1382.710698	18.757850
43.816609	1369.721840	18.762867
44.324285	1375.165257	18.767885
44.245379	1368.402017	18.772903
44.053038	1372.392937	18.777920
44.156412	1382.283255	18.782938
44.289823	1396.987945	18.787955
44.394939	1396.457187	18.792973
44.669140	1400.337146	18.797991
44.744842	1395.989190	18.803008
44.796030	1392.001694	18.808026
44.878515	1388.602605	18.813043
44.969411	1389.617314	18.818061
45.175875	1387.672611	18.823079
44.861601	1388.678215	18.828096
45.102065	1387.889559	18.833114
45.018152	1382.386304	18.838131
45.050078	1382.024809	18.843149
45.085783	1383.710906	18.848167
44.981442	1391.743384	18.853184
45.145150	1375.843647	18.858202
44.886318	1381.546020	18.863219
44.985851	1387.059700	18.868237
45.237469	1376.236668	18.873255
45.310105	1381.969162	18.878272
45.751420	1378.412866	18.883290
45.246661	1380.663339	18.888307
45.340064	1381.147462	18.893325
45.306146	1383.232644	18.898343
45.273489	1377.459420	18.903360
45.068599	1382.427484	18.908378
44.892642	1402.208010	18.913395
45.293805	1404.569021	18.918413
44.993781	1411.543378	18.923431
45.512503	1403.654506	18.928448
45.846263	1406.777185	18.933466
45.738423	1410.174187	18.938483
45.627330	1406.843295	18.943501
45.870222	1417.314551	18.948519
46.044535	1425.458026	18.953536
46.470356	1421.837875	18.958554
45.971766	1418.255257	18.963571
46.119321	1403.393166	18.968589
46.289514	1415.400116	18.973607
46.183907	1412.516504	18.978624
46.021718	1417.566253	18.983642
46.434274	1424.892889	18.988659
46.456117	1418.445216	18.993677
46.625508	1413.593410	18.998695
46.444226	1412.539459	19.003712
46.343424	1399.404696	19.008730
46.394171	1418.285000	19.013747
46.701013	1429.569938	19.018765
46.633549	1421.583545	19.023783
46.601331	1424.324895	19.028800
46.532692	1412.179196	19.033818
46.360531	1417.748077	19.038835
46.653425	1411.144326	19.043853
46.676313	1415.518115	19.048871
46.561911	1412.613789	19.053888
46.849748	1406.200186	19.058906
46.870130	1416.226606	19.063923
46.869715	1406.907387	19.068941
47.091891	1413.992439	19.073959
47.071802	1413.604378	19.078976
47.114093	1418.555816	19.083994
47.056202	1429.736948	19.089011
47.231315	1429.239405	19.094029
47.255848	1437.901831	19.099047
47.272245	1447.042080	19.104064
47.535945	1436.393850	19.109082
47.316121	1447.104885	19.114099
47.603930	1434.344726	19.119117
47.576015	1445.233982	19.124135
47.700385	1447.073457	19.129152
47.581970	1434.051885	19.134170
47.549595	1446.175803	19.139187
47.843662	1437.656216	19.144205
47.279034	1441.916928	19.149223
47.494415	1449.889871	19.154240
47.614313	1435.701141	19.159258
47.585297	1442.816092	19.164275
47.785214	1439.348101	19.169293
48.042707	1453.389589	19.174311
47.832288	1459.270602	19.179328
47.809971	1455.335634	19.184346
48.199580	1468.756811	19.189363
48.202972	1469.220325	19.194381
47.872441	1457.690005	19.199399
48.030271	1457.286691	19.204416
48.230968	1457.277463	19.209434
47.941215	1463.552772	19.214451
48.013558	1455.465562	19.219469
48.156133	1464.226275	19.224487
48.386534	1475.674703	19.229504
48.509227	1480.017091	19.234522
48.458392	1475.057757	19.239539
48.665466	1483.533809	19.244557
48.881049	1472.110428	19.249575
48.704461	1486.210485	19.254592
48.805631	1471.270394	19.259610
48.883656	1474.338475	19.264627
48.907544	1469.455800	19.269645
48.596544	1472.865709	19.274663
48.305993	1466.861453	19.279680
48.769601	1460.142571	19.284698
49.156214	1474.757160	19.289715
49.114676	1482.902920	19.294733
48.911558	1483.357763	19.299751
49.207542	1490.431281	19.304768
49.551896	1491.696631	19.309786
49.355289	1492.150453	19.314803
49.384073	1500.102160	19.319821
49.937382	1492.753806	19.324839
49.419344	1484.932657	19.329856
49.668507	1470.919313	19.334874
49.324758	1463.834600	19.339891
49.265758	1462.398556	19.344909
49.603179	1479.132167	19.349927
49.167605	1489.419421	19.354944
49.592576	1487.724505	19.359962
49.796224	1491.741776	19.364979
49.911887	1492.108802	19.369997
50.051981	1486.412622	19.375015
49.676034	1490.145146	19.380032
50.100424	1477.130020	19.385050
49.954418	1486.627105	19.390067
49.969745	1487.341224	19.395085
50.250945	1486.098039	19.400103
49.847692	1490.440780	19.405120
49.706938	1494.663495	19.410138
49.836381	1502.050301	19.415155
50.060235	1517.630891	19.420173
50.494196	1516.638337	19.425191
50.236760	1521.349574	19.430208
50.663421	1510.088765	19.435226
50.522801	1517.672530	19.440243
50.766104	1510.581031	19.445261
50.710810	1508.241808	19.450279
50.388804	1517.542414	19.455296
50.822940	1508.622136	19.460314
50.685706	1503.243968	19.465331
50.802228	1514.700795	19.470349
50.977766	1509.623929	19.475367
50.741611	1502.187815	19.480384
51.036242	1505.783719	19.485402
51.209096	1509.490226	19.490419
50.822722	1509.418337	19.495437
51.144202	1509.052500	19.500455
50.887022	1524.882040	19.505472
51.225447	1522.749383	19.510490
51.549915	1530.601126	19.515507
51.105381	1530.623559	19.520525
51.268759	1528.628784	19.525543
50.977708	1540.906909	19.530560
51.147609	1533.015827	19.535578
51.487408	1536.566789	19.540595
51.443247	1536.829463	19.545613
51.484888	1525.152423	19.550631
51.016690	1535.470062	19.555648
51.323223	1542.690278	19.560666
51.577081	1550.243811	19.565683
51.739371	1552.238308	19.570701
51.843454	1549.407029	19.575719
51.813957	1561.644189	19.580736
51.722275	1552.250828	19.585754
52.093740	1544.981439	19.590771
51.760460	1551.102645	19.595789
52.364581	1564.667018	19.600807
52.152677	1568.279178	19.605824
52.375233	1558.072843	19.610842
52.397667	1554.392785	19.615859
52.231956	1558.045045	19.620877
52.599169	1555.974148	19.625895
52.426615	1558.049512	19.630912
51.991107	1551.222147	19.635930
52.611504	1561.479702	19.640947
52.385393	1572.160236	19.645965
52.712430	1566.232762	19.650983
52.737056	1567.560835	19.656000
52.840176	1563.240102	19.661018
52.975674	1563.430445	19.666035
52.820064	1562.782735	19.671053
52.792079	1569.433653	19.676071
52.940008	1566.961591	19.681088
52.918659	1567.066051	19.686106
53.137944	1561.161772	19.691123
53.329640	1561.447457	19.696141
53.357131	1563.021243	19.701159
53.117595	1567.997943	19.706176
53.260356	1562.200331	19.711194
53.071514	1557.575034	19.716211
52.797408	1560.291184	19.721229
53.322108	1556.283114	19.726247
53.211312	1562.593538	19.731264
53.512493	1563.663678	19.736282
53.328297	1578.989504	19.741299
53.164097	1586.662203	19.746317
53.493410	1583.230718	19.751335
53.473295	1585.989132	19.756352
53.700815	1587.203363	19.761370
53.579498	1580.724410	19.766387
53.627685	1584.131714	19.771405
53.993485	1582.543894	19.776423
54.171876	1590.869851	19.781440
54.261931	1598.486939	19.786458
54.374261	1591.971375	19.791475
54.005542	1586.780935	19.796493
53.988721	1580.071006	19.801511
54.165787	1595.636904	19.806528
54.324435	1598.089589	19.811546
54.723100	1604.099291	19.816563
54.389248	1598.120711	19.821581
54.370256	1595.431790	19.826599
54.679580	1605.299432	19.831616
54.888580	1602.145580	19.836634
54.919131	1604.750886	19.841651
54.693977	1602.198411	19.846669
54.980128	1597.151529	19.851687
54.783425	1598.425915	19.856704
55.030897	1599.015300	19.861722
55.070580	1597.125108	19.866739
55.153607	1599.801089	19.871757
55.292768	1596.509852	19.876775
54.969548	1597.229678	19.881792
55.195312	1588.297824	19.886810
55.239395	1593.937026	19.891827
55.109512	1596.475943	19.896845
55.241762	1593.132138	19.901863
55.234931	1599.419975	19.906880
55.177613	1593.656857	19.911898
55.569879	1596.776715	19.916915
55.367115	1610.278186	19.921933
55.545408	1595.430054	19.926951
55.565460	1594.593868	19.931968
55.097536	1594.844038	19.936986
55.536127	1588.135340	19.942003
55.098952	1604.479166	19.947021
55.563349	1609.449734	19.952039
55.573136	1617.830522	19.957056
55.500649	1619.135943	19.962074
55.563294	1621.591049	19.967091
55.278907	1621.383254	19.972109
56.008761	1639.333690	19.977127
55.663533	1643.509578	19.982144
56.049600	1645.368035	19.987162
56.335496	1647.239030	19.992179
56.373415	1647.810753	19.997197
56.622440	1642.416209	20.002215
56.438376	1645.837822	20.007232
56.559761	1652.165552	20.012250
56.759301	1645.629992	20.017267
56.557167	1648.369595	20.022285
56.800245	1633.523905	20.027303
56.720571	1647.176540	20.032320
56.663610	1642.085568	20.037338
56.656598	1642.437102	20.042355
56.716156	1647.224945	20.047373
57.034190	1643.097750	20.052391
56.629329	1642.088282	20.057408
56.597128	1648.099231	20.062426
56.888200	1656.909360	20.067443
56.940056	1668.243868	20.072461
57.294482	1664.442342	20.077479
57.213206	1661.444418	20.082496
57.240468	1662.731057	20.087514
57.455822	1668.542273	20.092531
57.625284	1657.589926	20.097549
57.466019	1662.749744	20.102567
57.741838	1662.365811	20.107584
57.321710	1659.335767	20.112602
57.634068	1658.662073	20.117619
57.187731	1662.049038	20.122637
57.664302	1663.173759	20.127655
57.486470	1675.156513	20.132672
57.651103	1673.650699	20.137690
57.748960	1668.440785	20.142707
57.741119	1681.018633	20.147725
57.997450	1678.412802	20.152743
58.361435	1667.556210	20.157760
58.242936	1678.062150	20.162778
58.380020	1673.701353	20.167795
58.230336	1674.958910	20.172813
58.605658	1669.181635	20.177831
58.499829	1669.930522	20.182848
58.569032	1671.437820	20.187866
58.848367	1668.295029	20.192883
58.248543	1678.201006	20.197901
58.736938	1672.440730	20.202919
58.635821	1676.146012	20.207936
58.384135	1671.255963	20.212954
58.438238	1673.718726	20.217971
58.387955	1689.639078	20.222989
58.576850	1694.362486	20.228007
58.602890	1696.706567	20.233024
58.610952	1700.211703	20.238042
58.921623	1698.540988	20.243059
58.953321	1716.998538	20.248077
59.281927	1711.051835	20.253095
59.140407	1709.855930	20.258112
59.055787	1708.957238	20.263130
59.520741	1712.191967	20.268147
59.175813	1719.703681	20.273165
59.567638	1712.408943	20.278183
59.555738	1715.279704	20.283200
59.422794	1713.795262	20.288218
59.463563	1703.544739	20.293235
59.490341	1717.540528	20.298253
59.716852	1726.764771	20.303271
60.020874	1727.294805	20.308288
60.060946	1736.582979	20.313306
60.188072	1729.298146	20.318323
59.840491	1723.649894	20.323341
60.140202	1725.439835	20.328359
60.268270	1733.562292	20.333376
60.223406	1729.889587	20.338394
60.306665	1734.026765	20.343411
60.116217	1725.447247	20.348429
60.533011	1731.510960	20.353447
60.480715	1723.064441	20.358464
60.289819	1730.110190	20.363482
60.642647	1719.804453	20.368499
60.714050	1716.489094	20.373517
60.852009	1716.890504	20.378535
60.996586	1711.420780	20.383552
60.841243	1725.808046	20.388570
61.139517	1716.173612	20.393587
60.768310	1725.646144	20.398605
60.743654	1719.767409	20.403623
60.945916	1721.670452	20.408640
60.659880	1714.390394	20.413658
61.330656	1711.467147	20.418675
61.081169	1709.215130	20.423693
61.091066	1712.786256	20.428711
61.077265	1715.190233	20.433728
60.978485	1725.424854	20.438746
61.432354	1734.616636	20.443763
61.495668	1739.473346	20.448781
61.761740	1739.595894	20.453799
61.862119	1737.670930	20.458816
61.747917	1748.438183	20.463834
61.958578	1738.347224	20.468851
61.833249	1746.499921	20.473869
61.814813	1734.904743	20.478887
61.645046	1738.434592	20.483904
61.513289	1747.487748	20.488922
61.672755	1737.644664	20.493939
61.781055	1739.303641	20.498957
61.736695	1752.127114	20.503975
62.030641	1761.075708	20.508992
62.029721	1765.147183	20.514010
62.349517	1766.905577	20.519027
62.487881	1772.691018	20.524045
62.605801	1768.664579	20.529063
62.737540	1763.578724	20.534080
62.419750	1759.497469	20.539098
62.479527	1756.272291	20.544115
62.709208	1769.409466	20.549133
62.779933	1779.084201	20.554151
63.027022	1779.392770	20.559168
62.893527	1781.354736	20.564186
62.972204	1777.580610	20.569203
63.051250	1781.286091	20.574221
62.650205	1786.281842	20.579239
63.250720	1779.803339	20.584256
62.937920	1787.619332	20.589274
63.089469	1779.203968	20.594291
62.892331	1774.179105	20.599309
62.868111	1778.743411	20.604327
63.437302	1797.984726	20.609344
63.732895	1793.930444	20.614362
63.705741	1792.621936	20.619379
64.076997	1800.867278	20.624397
63.854756	1797.695746	20.629415
63.854743	1798.674226	20.634432
63.913086	1803.762119	20.639450
64.033456	1793.985093	20.644467
64.084439	1798.742760	20.649485
64.084147	1798.250598	20.654503
64.318358	1800.729344	20.659520
64.079691	1797.216384	20.664538
64.198910	1794.758257	20.669555
64.261058	1792.129182	20.674573
64.266303	1787.072606	20.679591
64.497716	1789.173072	20.684608
64.215501	1791.316139	20.689626
64.212318	1794.150832	20.694643
64.188244	1801.836384	20.699661
64.419911	1790.940485	20.704679
64.539516	1794.434476	20.709696
64.369216	1797.317444	20.714714
64.714001	1811.651669	20.719731
64.638683	1809.646921	20.724749
65.031516	1823.093109	20.729767
65.264704	1818.761404	20.734784
65.007333	1817.217548	20.739802
65.109914	1813.455449	20.744819
65.164125	1810.691907	20.749837
64.863833	1803.625496	20.754855
65.212157	1801.810010	20.759872
65.027812	1838.331662	20.764890
65.330762	1831.738806	20.769907
65.549146	1837.376023	20.774925
65.576409	1832.685236	20.779943
65.419965	1841.262597	20.784960
65.297812	1839.855353	20.789978
65.287496	1835.501832	20.794995
65.844059	1848.953946	20.800013
65.807574	1845.705962	20.805031
65.908232	1853.261535	20.810048
65.834987	1860.345710	20.815066
66.473173	1852.513670	20.820083
66.309341	1846.618827	20.825101
66.202844	1851.148702	20.830119
66.601821	1846.229250	20.835136
66.174562	1850.910371	20.840154
66.206690	1847.269762	20.845171
66.466639	1852.073603	20.850189
66.328759	1861.733726	20.855207
66.819895	1868.890436	20.860224
66.910263	1868.421940	20.865242
66.764476	1878.951208	20.870259
67.252840	1871.054266	20.875277
66.968567	1873.677376	20.880295
67.010431	1859.102880	20.885312
67.006858	1877.768106	20.890330
67.180492	1865.107586	20.895347
66.884670	1874.069738	20.900365
66.916373	1880.032881	20.905383
67.224517	1865.511341	20.910400
67.349592	1873.438660	20.915418
67.473405	1869.695314	20.920435
67.596421	1868.186536	20.925453
67.324027	1883.340238	20.930471
67.556722	1884.376943	20.935488
67.515624	1891.954742	20.940506
67.551490	1898.983966	20.945523
68.047935	1889.659238	20.950541
67.602086	1901.627326	20.955559
67.977205	1895.865791	20.960576
67.914183	1899.899687	20.965594
68.321421	1890.314364	20.970611
68.255054	1894.421371	20.975629
68.026260	1888.763923	20.980647
68.484346	1887.953774	20.985664
68.721259	1885.893787	20.990682
68.729108	1889.932357	20.995699
68.460644	1885.695013	21.000717
68.355307	1886.301812	21.005735
68.736235	1879.598885	21.010752
68.501771	1885.707879	21.015770
68.994444	1895.243980	21.020787
69.171762	1900.196489	21.025805
68.859200	1902.820878	21.030823
69.209971	1895.592462	21.035840
69.295514	1909.471891	21.040858
69.415197	1891.681838	21.045875
68.998636	1879.224235	21.050893
68.685979	1892.500124	21.055911
69.304055	1897.901160	21.060928
69.141992	1892.627756	21.065946
69.481322	1891.738377	21.070963
69.077752	1897.166926	21.075981
68.907343	1895.136039	21.080999
69.981350	1906.297929	21.086016
69.802303	1927.518654	21.091034
69.594623	1913.892140	21.096051
70.045252	1924.908697	21.101069
70.016734	1924.616626	21.106087
69.987304	1930.526243	21.111104
69.956289	1933.627267	21.116122
70.027188	1923.747461	21.121139
70.187837	1922.971288	21.126157
70.003195	1932.007574	21.131175
70.150180	1916.933693	21.136192
70.243883	1923.458373	21.141210
70.593016	1938.937648	21.146227
70.691424	1950.678478	21.151245
70.736172	1949.873122	21.156263
70.955774	1937.290561	21.161280
70.971647	1950.044775	21.166298
71.247012	1949.645128	21.171315
71.117622	1948.936488	21.176333
71.096103	1947.027444	21.181351
71.137009	1943.445404	21.186368
71.047859	1938.892756	21.191386
71.189726	1933.095166	21.196403
71.324146	1939.203191	21.201421
70.906897	1941.348496	21.206439
71.301430	1940.747130	21.211456
71.435832	1953.081963	21.216474
71.156984	1944.948562	21.221491
71.517520	1942.641968	21.226509
71.582537	1958.295170	21.231527
71.664054	1958.882165	21.236544
71.842927	1967.665843	21.241562
71.766711	1961.795107	21.246579
71.818862	1959.846115	21.251597
71.943118	1957.996287	21.256615
72.038870	1959.360586	21.261632
71.874376	1954.567257	21.266650
71.708382	1960.779166	21.271667
71.946085	1968.568952	21.276685
71.981997	1981.272709	21.281703
72.497825	1978.140153	21.286720
72.615255	1975.533950	21.291738
72.356398	1979.825779	21.296755
72.638198	1980.438203	21.301773
72.740816	1985.894777	21.306791
72.811158	1998.157621	21.311808
72.844219	1994.147583	21.316826
72.695182	1996.866294	21.321843
73.088215	1991.373340	21.326861
72.738154	1993.198834	21.331879
72.932288	1991.742024	21.336896
73.083988	2008.871328	21.341914
72.995819	2004.170177	21.346931
73.086539	2011.433864	21.351949
73.434383	2014.879515	21.356967
73.420806	2025.798438	21.361984
73.450546	2024.802913	21.367002
73.801049	2030.829775	21.372019
73.577164	2019.822061	21.377037
73.544729	2026.404414	21.382055
73.919547	2022.760575	21.387072
73.810530	2021.862534	21.392090
73.607366	2021.288533	21.397107
73.943258	2030.707250	21.402125
73.877982	2050.133455	21.407143
74.291297	2047.417764	21.412160
74.428630	2050.905871	21.417178
74.546649	2048.832934	21.422195
74.425808	2043.616147	21.427213
74.750266	2047.084404	21.432231
74.892821	2039.383589	21.437248
74.918925	2046.512237	21.442266
74.818720	2038.663251	21.447283
74.755322	2050.596766	21.452301
74.668949	2041.981853	21.457319
74.768099	2034.202628	21.462336
74.878440	2057.413802	21.467354
74.916218	2066.064989	21.472371
75.309793	2059.391574	21.477389
75.257338	2056.909813	21.482407
75.222238	2071.382665	21.487424
75.078474	2065.471982	21.492442
75.118357	2070.875289	21.497459
75.371686	2072.931327	21.502477
75.688482	2088.633565	21.507495
75.847300	2093.664770	21.512512
76.088791	2084.600809	21.517530
75.901545	2088.373323	21.522547
76.093715	2086.048905	21.527565
75.951324	2082.407187	21.532583
75.656026	2085.600139	21.537600
76.014997	2082.277531	21.542618
75.942471	2091.864417	21.547635
76.448702	2099.410204	21.552653
76.719072	2102.612372	21.557671
76.456657	2106.002162	21.562688
76.603325	2101.605045	21.567706
76.619324	2107.810582	21.572723
76.681111	2106.765847	21.577741
76.422534	2107.816415	21.582759
76.818665	2110.553880	21.587776
76.737402	2097.374513	21.592794
76.657248	2119.441568	21.597811
76.792810	2125.729373	21.602829
77.253264	2129.192119	21.607847
77.123104	2128.625614	21.612864
77.276385	2119.862655	21.617882
77.458193	2130.687909	21.622899
77.428770	2117.686612	21.627917
77.637697	2128.816909	21.632935
77.796696	2129.006733	21.637952
77.921696	2131.228061	21.642970
77.918180	2123.199775	21.647987
77.983449	2119.462394	21.653005
77.876130	2116.976595	21.658023
78.165774	2120.169434	21.663040
78.192528	2112.231092	21.668058
77.984431	2124.824846	21.673075
78.144660	2130.559637	21.678093
78.507299	2136.029171	21.683111
78.831558	2138.522261	21.688128
78.814039	2127.545270	21.693146
78.375676	2133.777818	21.698163
78.579405	2132.142756	21.703181
78.342093	2140.827611	21.708199
78.237368	2132.515354	21.713216
78.414162	2131.272704	21.718234
78.584433	2135.711948	21.723251
78.958290	2144.364171	21.728269
78.884889	2157.836317	21.733287
79.306766	2155.523242	21.738304
79.604279	2158.781132	21.743322
79.380770	2151.705709	21.748339
79.847904	2153.134923	21.753357
79.911861	2151.382891	21.758375
79.856253	2145.597235	21.763392
79.896892	2140.844307	21.768410
79.724820	2148.846707	21.773427
79.862556	2143.636720	21.778445
79.758307	2146.537799	21.783463
79.858593	2144.284579	21.788480
80.452574	2145.005901	21.793498
80.089762	2146.580925	21.798515
80.112360	2148.767802	21.803533
80.129509	2154.382996	21.808551
80.074906	2151.819500	21.813568
79.950506	2151.043792	21.818586
80.049824	2171.968711	21.823603
80.306106	2171.228041	21.828621
80.285742	2167.860699	21.833639
80.251962	2174.995624	21.838656
80.915367	2188.339732	21.843674
80.935763	2195.677632	21.848691
80.963285	2194.957022	21.853709
80.808586	2198.951695	21.858727
81.149472	2192.324359	21.863744
80.990510	2189.474228	21.868762
81.034235	2200.857687	21.873779
81.302708	2201.143979	21.878797
81.544644	2212.127133	21.883815
81.483380	2211.783379	21.888832
81.755351	2211.690396	21.893850
81.818103	2207.331648	21.898867
82.075587	2216.361929	21.903885
82.036983	2221.294703	21.908903
81.916269	2216.453416	21.913920
82.242895	2213.798623	21.918938
82.150567	2215.804683	21.923955
82.270120	2211.632711	21.928973
82.324725	2207.022755	21.933991
82.179970	2202.655491	21.939008
82.510484	2211.226168	21.944026
82.338030	2228.952466	21.949043
82.543129	2234.834908	21.954061
82.509433	2237.636578	21.959079
82.638085	2244.301078	21.964096
83.059314	2237.645358	21.969114
82.843847	2233.689984	21.974131
83.073064	2228.591882	21.979149
82.981896	2237.137112	21.984167
82.908868	2235.128801	21.989184
83.431632	2241.135059	21.994202
83.602483	2250.507160	21.999219
83.714365	2251.752180	22.004237
83.698290	2232.228289	22.009255
83.417773	2234.229118	22.014272
83.882594	2239.023059	22.019290
83.422714	2246.956976	22.024307
83.817587	2249.783030	22.029325
83.862724	2249.911793	22.034343
83.924662	2249.637105	22.039360
83.713994	2243.449643	22.044378
83.829177	2246.739271	22.049395
83.917615	2246.836002	22.054413
84.052046	2253.581658	22.059431
83.792986	2254.723835	22.064448
83.919924	2260.123029	22.069466
84.259111	2275.796675	22.074483
84.590669	2267.554868	22.079501
84.544030	2283.219535	22.084519
85.112355	2283.402041	22.089536
85.081699	2279.483979	22.094554
85.229017	2279.243255	22.099571
85.407208	2272.338397	22.104589
85.489052	2271.855446	22.109607
85.228861	2278.457793	22.114624
85.348220	2272.969758	22.119642
85.445206	2270.597108	22.124659
85.294001	2268.878775	22.129677
85.401317	2260.362810	22.134695
85.214292	2272.214847	22.139712
85.636730	2283.431719	22.144730
85.808512	2293.296044	22.149747
85.463675	2294.659963	22.154765
85.833950	2299.295149	22.159783
85.781273	2303.336983	22.164800
86.185480	2297.539202	22.169818
86.106964	2311.308935	22.174835
86.216540	2315.353756	22.179853
86.489440	2318.221023	22.184871
86.294973	2322.111492	22.189888
86.726675	2316.940612	22.194906
86.772142	2325.912639	22.199923
86.741814	2311.194440	22.204941
86.977295	2316.314691	22.209959
87.251950	2319.623533	22.214976
86.978629	2325.902880	22.219994
87.189779	2331.434081	22.225011
87.434899	2337.452310	22.230029
87.405827	2338.050331	22.235047
87.568176	2338.814039	22.240064
87.427057	2341.045527	22.245082
87.124518	2348.863311	22.250099
87.670888	2331.804459	22.255117
87.441479	2339.285707	22.260135
87.589664	2341.585487	22.265152
88.072947	2351.640901	22.270170
87.869133	2363.760740	22.275187
87.865293	2365.131205	22.280205
88.040064	2359.094773	22.285223
88.142376	2368.061071	22.290240
88.363484	2362.326673	22.295258
88.272273	2363.909660	22.300275
88.361443	2360.626116	22.305293
88.935921	2378.308128	22.310311
88.503022	2382.106565	22.315328
88.550415	2379.220917	22.320346
88.689734	2376.301931	22.325363
88.756567	2383.960866	22.330381
88.962645	2373.488383	22.335399
88.586665	2383.006192	22.340416
88.986722	2391.285169	22.345434
89.414751	2412.367170	22.350451
89.712418	2407.236201	22.355469
89.755562	2405.055022	22.360487
89.718057	2403.410389	22.365504
89.853593	2405.712159	22.370522
89.834062	2394.378682	22.375539
89.808925	2400.556049	22.380557
89.848455	2395.676983	22.385575
90.042221	2402.249282	22.390592
89.945781	2399.130523	22.395610
89.953687	2403.055580	22.400627
89.862577	2400.911216	22.405645
89.903411	2396.839904	22.410663
89.890144	2413.010742	22.415680
90.160853	2422.512469	22.420698
90.309986	2417.796123	22.425715
90.063619	2424.064968	22.430733
90.503803	2436.535280	22.435751
90.222175	2436.254450	22.440768
90.785102	2447.480976	22.445786
90.747481	2454.499838	22.450803
90.935885	2467.849141	22.455821
91.187700	2469.028067	22.460839
90.860479	2465.456257	22.465856
91.555306	2466.950820	22.470874
91.725589	2468.508628	22.475891
91.363412	2462.685685	22.480909
91.924868	2480.063696	22.485927
91.689134	2480.435300	22.490944
91.858048	2483.555593	22.495962
91.665548	2484.993498	22.500979
91.982194	2482.475943	22.505997
92.312112	2476.793896	22.511015
92.295277	2478.002288	22.516032
92.458524	2477.512890	22.521050
92.347684	2487.071273	22.526067
92.598169	2495.929206	22.531085
92.578806	2503.046222	22.536103
92.884430	2504.109413	22.541120
93.031203	2497.818520	22.546138
93.001193	2500.717493	22.551155
93.103848	2502.920276	22.556173
93.176296	2494.867298	22.561191
93.180628	2504.234060	22.566208
93.330468	2488.180861	22.571226
93.329007	2491.094297	22.576243
93.056188	2506.384301	22.581261
93.281420	2509.173852	22.586279
93.115106	2522.288408	22.591296
93.967319	2520.952538	22.596314
93.640695	2522.155815	22.601331
93.910183	2526.532270	22.606349
94.415183	2513.683665	22.611367
93.813609	2518.969834	22.616384
94.488825	2529.815867	22.621402
94.416989	2532.033367	22.626419
94.381213	2541.125538	22.631437
94.812431	2536.106166	22.636455
94.555984	2537.651933	22.641472
94.630253	2527.667116	22.646490
94.839477	2537.708763	22.651507
94.994196	2537.520530	22.656525
95.162643	2529.837541	22.661543
94.825835	2530.269167	22.666560
95.059102	2534.392498	22.671578
95.063187	2530.803486	22.676595
95.196996	2554.393516	22.681613
95.476096	2552.680329	22.686631
95.330722	2558.923930	22.691648
95.464589	2549.519956	22.696666
95.596795	2554.113605	22.701683
95.648458	2561.052243	22.706701
95.585504	2553.509650	22.711719
95.603516	2555.372216	22.716736
95.851325	2569.485535	22.721754
96.155633	2564.009464	22.726771
96.204262	2574.347719	22.731789
96.381943	2565.492349	22.736807
96.241437	2568.512797	22.741824
96.593969	2572.806818	22.746842
96.418701	2572.332579	22.751859
96.397169	2592.967623	22.756877
96.477616	2592.513288	22.761895
96.535399	2605.466549	22.766912
96.738581	2600.482886	22.771930
96.960632	2603.983078	22.776947
97.208816	2612.118677	22.781965
97.075401	2619.742808	22.786983
97.124503	2625.826561	22.792000
97.763337	2619.041926	22.797018
97.563844	2623.245703	22.802035
97.780197	2631.954401	22.807053
97.695150	2623.973382	22.812071
97.575511	2629.026272	22.817088
97.761475	2639.904838	22.822106
98.287675	2642.962870	22.827123
97.929135	2647.882763	22.832141
98.431294	2640.523024	22.837159
98.192366	2642.356419	22.842176
98.336778	2632.789787	22.847194
98.579521	2651.489818	22.852211
98.872774	2652.760105	22.857229
99.180701	2649.663164	22.862247
99.031841	2666.717097	22.867264
99.051673	2660.029426	22.872282
99.505140	2652.487943	22.877299
99.116757	2660.082602	22.882317
99.481714	2661.101789	22.887335
99.432440	2653.954683	22.892352
99.406045	2648.659800	22.897370
99.632659	2665.566535	22.902387
99.398030	2656.450636	22.907405
99.538432	2661.415452	22.912423
99.569973	2675.187157	22.917440
99.797695	2683.474334	22.922458
100.443214	2678.708556	22.927475
99.818731	2681.094717	22.932493
100.047656	2675.658828	22.937511
99.995123	2685.703694	22.942528
100.370050	2699.134411	22.947546
100.463003	2691.605208	22.952563
100.680784	2701.841287	22.957581
100.827678	2703.645803	22.962599
100.895323	2699.548129	22.967616
100.845551	2696.917519	22.972634
101.080930	2699.074284	22.977651
101.236733	2719.252454	22.982669
101.511261	2722.110064	22.987687
101.830136	2712.711737	22.992704
101.439369	2723.144167	22.997722
101.665915	2715.638209	23.002739
101.935585	2723.622155	23.007757
101.561186	2714.341912	23.012775
101.856199	2712.206451	23.017792
101.875754	2713.226101	23.022810
102.361881	2694.822361	23.027827
102.573058	2705.993694	23.032845
102.337945	2695.063071	23.037863
102.139295	2710.060731	23.042880
102.277561	2706.065613	23.047898
102.324746	2704.136256	23.052915
102.379533	2723.086739	23.057933
102.400119	2722.471346	23.062951
102.799425	2736.901926	23.067968
102.938846	2728.996158	23.072986
103.232286	2726.595826	23.078003
102.912928	2730.316580	23.083021
103.097027	2722.302818	23.088039
103.324380	2737.101201	23.093056
103.350852	2744.678242	23.098074
103.649447	2746.380091	23.103091
103.592030	2754.235394	23.108109
103.244773	2748.630950	23.113127
103.721510	2750.828811	23.118144
103.781616	2771.845788	23.123162
103.831345	2774.972181	23.128179
103.700540	2768.292289	23.133197
104.214342	2777.178543	23.138215
104.167762	2774.247588	23.143232
104.089844	2792.783386	23.148250
104.607398	2792.033320	23.153267
104.564456	2802.749010	23.158285
104.768353	2796.032451	23.163303
104.911035	2788.760533	23.168320
105.006794	2795.906971	23.173338
105.336107	2805.358690	23.178355
105.442693	2812.203604	23.183373
105.524483	2808.536083	23.188391
105.493883	2809.620408	23.193408
105.458664	2811.724896	23.198426
105.686753	2802.104034	23.203443
105.568905	2804.417148	23.208461
105.648793	2796.227155	23.213479
105.576043	2819.799397	23.218496
105.543816	2837.056149	23.223514
105.806054	2838.779484	23.228531
106.112303	2834.256190	23.233549
106.316459	2841.328853	23.238567
106.904630	2853.407000	23.243584
107.064278	2851.920808	23.248602
107.253107	2843.849441	23.253619
106.982933	2850.930141	23.258637
107.476316	2838.859543	23.263655
107.276721	2835.665339	23.268672
106.960273	2847.752651	23.273690
107.251445	2842.641514	23.278707
107.110061	2849.427449	23.283725
107.612226	2840.290708	23.288743
107.431032	2846.628393	23.293760
107.809492	2850.994168	23.298778
107.800860	2843.588126	23.303795
107.860960	2844.762396	23.308813
108.063205	2853.205139	23.313831
108.178287	2866.013896	23.318848
108.015341	2869.804858	23.323866
108.444513	2860.291334	23.328883
108.113784	2871.149993	23.333901
108.433380	2859.157107	23.338919
108.665713	2860.165524	23.343936
108.332185	2881.746131	23.348954
108.901350	2877.721340	23.353971
108.549272	2882.381478	23.358989
108.956856	2882.630207	23.364007
108.908942	2877.348097	23.369024
108.940489	2891.110498	23.374042
109.079103	2894.649069	23.379059
109.103079	2901.241841	23.384077
109.330115	2901.954409	23.389095
109.484842	2902.627807	23.394112
109.676144	2915.879148	23.399130
110.046301	2915.294199	23.404147
110.294813	2933.589629	23.409165
110.031603	2930.471655	23.414183
110.203576	2927.932518	23.419200
110.110174	2934.729906	23.424218
110.161561	2929.845682	23.429235
110.277754	2927.943364	23.434253
110.589207	2943.347352	23.439271
110.437438	2947.092393	23.444288
110.399488	2949.957965	23.449306
110.945564	2941.947363	23.454323
110.736684	2961.374958	23.459341
111.163896	2962.305506	23.464359
111.209177	2964.507866	23.469376
111.341555	2973.476069	23.474394
111.617136	2961.234360	23.479411
111.535831	2970.097167	23.484429
111.360207	2974.256255	23.489447
111.731163	2985.106048	23.494464
111.966417	2993.089194	23.499482
112.373481	2986.706852	23.504499
112.204051	2990.754507	23.509517
112.491586	2984.390892	23.514535
112.352149	2981.512325	23.519552
112.314427	3001.323453	23.524570
112.627937	3003.117676	23.529587
112.779905	3011.448434	23.534605
112.775701	3013.655397	23.539623
113.026207	3007.367012	23.544640
112.589935	3011.074578	23.549658
113.032342	3026.249812	23.554675
113.222138	3029.496334	23.559693
113.245687	3029.470676	23.564711
113.729581	3031.711638	23.569728
113.474953	3032.556485	23.574746
114.033528	3038.213378	23.579763
113.844136	3056.451292	23.584781
113.727768	3056.542240	23.589799
114.191372	3047.158941	23.594816
114.013993	3051.514006	23.599834
114.239375	3044.443650	23.604851
114.308643	3059.314409	23.609869
114.501918	3073.540823	23.614887
114.569464	3070.610877	23.619904
114.611982	3073.643765	23.624922
115.024649	3065.461481	23.629939
114.841982	3079.642644	23.634957
114.742513	3093.444663	23.639975
115.570013	3088.347274	23.644992
115.108385	3100.372281	23.650010
115.640638	3089.179166	23.655027
115.785773	3089.402736	23.660045
115.799996	3083.365965	23.665063
115.946264	3098.404597	23.670080
116.046593	3111.263183	23.675098
116.182840	3123.390223	23.680115
116.279276	3122.043317	23.685133
116.116939	3115.099958	23.690151
116.576954	3116.429371	23.695168
116.378748	3118.338494	23.700186
116.745570	3106.300171	23.705203
116.573677	3112.169372	23.710221
116.622313	3132.219611	23.715239
117.111870	3132.547033	23.720256
117.145761	3142.799549	23.725274
117.411327	3135.763893	23.730291
117.492028	3137.913382	23.735309
117.168085	3134.315673	23.740327
117.416154	3140.598833	23.745344
117.241728	3138.827242	23.750362
117.868150	3142.267344	23.755379
117.631454	3152.186668	23.760397
117.578767	3156.017228	23.765415
117.946228	3164.592044	23.770432
117.915911	3181.122896	23.775450
118.282920	3175.763067	23.780467
118.009664	3192.284647	23.785485
118.431407	3185.716875	23.790503
118.882593	3191.583172	23.795520
118.625765	3209.093248	23.800538
118.836734	3206.090310	23.805555
119.001589	3216.202413	23.810573
119.014798	3200.450890	23.815591
119.038210	3208.921817	23.820608
119.017906	3217.917219	23.825626
119.410914	3222.700585	23.830643
119.669224	3215.874346	23.835661
119.619177	3223.072204	23.840679
119.859252	3235.741705	23.845696
120.333771	3244.274537	23.850714
120.340462	3253.196290	23.855731
120.354625	3244.612392	23.860749
120.241684	3246.489233	23.865767
120.815974	3245.847044	23.870784
120.777852	3240.831572	23.875802
120.754994	3239.026756	23.880819
120.874348	3244.376936	23.885837
121.278705	3258.927082	23.890855
121.898932	3251.188788	23.895872
121.715122	3252.694828	23.900890
121.297562	3248.407923	23.905907
121.709082	3244.363563	23.910925
121.458613	3257.261432	23.915943
122.156713	3252.967017	23.920960
121.837971	3253.364265	23.925978
121.874700	3251.322863	23.930995
122.015487	3251.496617	23.936013
122.116941	3251.114724	23.941031
122.368897	3256.043291	23.946048
122.547512	3272.380525	23.951066
122.785479	3265.892016	23.956083
122.646412	3265.674054	23.961101
122.507895	3280.691174	23.966119
122.884654	3272.504954	23.971136
122.650031	3292.997435	23.976154
122.896542	3295.152529	23.981171
122.931810	3294.537973	23.986189
122.991956	3305.240967	23.991207
123.494882	3314.949818	23.996224
123.424316	3319.730087	24.001242
123.892855	3322.838305	24.006259
123.851119	3324.621936	24.011277
123.812826	3331.799057	24.016295
124.240497	3338.811649	24.021312
124.260390	3345.351566	24.026330
124.948619	3348.008745	24.031347
124.791768	3342.036564	24.036365
124.885411	3355.679123	24.041383
124.791037	3332.161020	24.046400
125.269228	3350.992173	24.051418
125.210611	3335.501129	24.056435
125.040566	3344.598960	24.061453
124.943767	3346.432251	24.066471
125.135354	3345.477579	24.071488
125.313878	3354.956368	24.076506
125.508574	3362.093844	24.081523
125.871312	3365.411176	24.086541
125.509961	3363.889785	24.091559
125.925416	3367.154671	24.096576
125.849853	3380.432382	24.101594
126.054788	3379.049521	24.106611
125.960412	3386.071326	24.111629
125.936940	3398.198323	24.116647
125.987386	3403.638252	24.121664
126.602906	3404.810762	24.126682
127.005786	3412.622645	24.131699
126.627541	3425.026181	24.136717
126.871280	3434.870391	24.141735
126.963360	3438.722518	24.146752
127.015389	3437.152138	24.151770
127.243814	3451.038780	24.156787
127.586921	3453.374448	24.161805
127.450997	3464.799478	24.166823
127.545228	3458.690077	24.171840
128.088113	3476.485438	24.176858
128.357350	3482.102584	24.181875
128.501021	3481.430008	24.186893
128.270800	3478.584521	24.191911
128.690547	3481.498409	24.196928
128.853489	3479.440364	24.201946
128.551742	3482.126409	24.206963
128.964982	3494.424930	24.211981
128.846292	3506.188164	24.216999
129.024334	3507.028372	24.222016
129.352160	3504.590989	24.227034
129.174603	3503.400607	24.232051
129.310587	3518.207636	24.237069
129.644459	3534.429252	24.242087
129.826746	3523.577920	24.247104
130.163291	3525.485371	24.252122
129.924909	3530.522396	24.257139
130.068602	3551.268372	24.262157
130.203534	3550.991698	24.267175
130.394020	3551.930960	24.272192
130.435580	3552.189702	24.277210
130.606754	3551.500188	24.282227
130.781383	3560.986009	24.287245
130.651629	3562.736109	24.292263
130.966296	3555.550565	24.297280
131.158271	3574.335261	24.302298
131.420045	3592.537751	24.307315
132.099301	3585.004698	24.312333
131.510207	3594.026271	24.317351
131.560623	3587.462873	24.322368
131.924572	3594.895867	24.327386
131.749184	3598.117640	24.332403
132.013048	3606.055545	24.337421
132.209687	3608.038580	24.342439
132.563728	3606.354589	24.347456
132.838153	3612.820007	24.352474
132.875947	3611.321281	24.357491
133.138691	3607.410621	24.362509
132.822474	3615.960199	24.367527
133.000731	3620.007179	24.372544
133.219250	3629.804947	24.377562
133.193668	3629.919549	24.382579
133.347679	3627.900763	24.387597
133.566742	3638.639028	24.392615
133.795769	3646.746536	24.397632
133.838765	3660.684484	24.402650
134.028943	3648.686101	24.407667
134.361831	3651.623094	24.412685
134.084285	3656.394848	24.417703
134.345340	3650.417062	24.422720
134.385123	3646.329852	24.427738
134.527258	3674.149493	24.432755
134.686648	3670.662176	24.437773
134.601251	3673.065005	24.442791
134.981210	3682.228341	24.447808
135.204387	3682.606978	24.452826
135.146854	3695.800032	24.457843
135.584450	3700.526040	24.462861
135.359466	3705.980804	24.467879
135.513185	3700.064007	24.472896
135.733757	3705.013396	24.477914
135.939395	3716.874302	24.482931
136.024378	3708.234901	24.487949
136.056269	3727.193182	24.492967
136.026503	3722.864345	24.497984
136.216567	3735.977606	24.503002
136.492805	3745.447605	24.508019
136.772354	3735.376302	24.513037
136.675908	3754.319998	24.518055
137.423754	3755.074105	24.523072
137.344514	3753.486388	24.528090
137.269827	3755.928583	24.533107
137.488577	3752.353042	24.538125
137.288421	3769.971565	24.543143
137.711180	3772.774558	24.548160
138.408025	3779.012885	24.553178
138.165266	3780.932213	24.558195
138.434960	3775.091912	24.563213
138.453180	3779.324974	24.568231
138.615180	3780.874726	24.573248
138.613691	3784.590083	24.578266
138.642992	3799.546621	24.583283
138.835067	3803.944988	24.588301
138.771171	3809.254605	24.593319
138.872531	3808.437141	24.598336
139.135316	3817.271707	24.603354
139.303643	3829.873959	24.608371
139.460212	3825.844163	24.613389
139.263286	3837.105386	24.618407
139.677592	3840.165378	24.623424
139.782064	3843.163439	24.628442
139.796670	3850.566048	24.633459
140.292702	3861.661909	24.638477
140.250652	3880.723469	24.643495
140.494835	3878.930411	24.648512
140.707428	3877.959795	24.653530
140.768950	3881.438043	24.658547
140.645189	3889.234794	24.663565
140.679746	3896.669016	24.668583
140.700384	3898.414524	24.673600
141.366467	3909.177607	24.678618
141.489274	3922.276289	24.683635
141.751934	3918.128850	24.688653
141.921041	3922.556094	24.693671
142.004278	3917.625582	24.698688
141.974499	3925.385530	24.703706
142.062781	3941.974250	24.708723
142.042155	3946.803675	24.713741
142.298430	3945.390635	24.718759
142.634465	3957.439590	24.723776
143.143595	3966.484987	24.728794
143.131042	3973.535232	24.733811
143.384080	3963.862501	24.738829
143.239451	3968.117964	24.743847
143.224424	3955.343499	24.748864
143.689938	3961.289870	24.753882
143.416701	3960.512148	24.758899
143.698403	3950.105815	24.763917
144.038666	3972.068240	24.768935
143.887898	3978.991792	24.773952
144.274007	3983.154640	24.778970
143.907710	3978.000996	24.783987
144.762621	3979.521119	24.789005
144.723624	3987.778087	24.794023
145.414195	4009.177501	24.799040
145.299862	3995.550565	24.804058
144.930022	3998.332574	24.809075
145.114657	3988.793645	24.814093
145.332268	4000.220440	24.819111
145.102371	3990.493943	24.824128
145.736130	3999.945941	24.829146
145.967727	4005.613338	24.834163
145.839330	4008.366992	24.839181
145.967830	4020.123397	24.844199
145.942203	4031.537817	24.849216
146.335432	4028.944926	24.854234
146.473610	4038.215763	24.859251
146.584018	4037.892422	24.864269
146.250778	4046.485901	24.869287
146.723423	4061.464734	24.874304
147.331413	4065.444491	24.879322
147.078523	4068.170312	24.884339
147.214979	4074.906866	24.889357
147.636449	4083.107520	24.894375
147.750947	4084.216535	24.899392
148.177362	4073.774834	24.904410
148.044253	4086.588621	24.909427
147.811474	4086.249605	24.914445
148.130899	4103.348315	24.919463
148.438728	4104.982566	24.924480
148.918288	4105.074849	24.929498
148.598137	4113.751531	24.934515
148.775169	4115.794510	24.939533
149.065052	4127.055400	24.944551
148.758153	4136.351826	24.949568
149.458145	4133.385753	24.954586
149.575998	4149.143056	24.959603
149.642465	4151.705228	24.964621
149.610969	4150.936970	24.969639
149.688509	4163.389546	24.974656
150.249864	4163.273318	24.979674
150.198543	4176.314242	24.984691
150.232088	4178.515433	24.989709
150.794791	4169.087624	24.994727
150.633468	4181.517662	24.999744
150.833685	4173.500735	25.004762
150.607948	4200.715975	25.009779
150.943682	4192.466330	25.014797
151.336303	4206.274171	25.019815
151.118216	4209.644779	25.024832
151.443913	4223.393677	25.029850
151.529221	4226.290642	25.034867
151.590613	4223.626612	25.039885
151.909179	4229.854920	25.044903
151.674349	4247.703443	25.049920
151.753912	4245.860386	25.054938
152.242098	4263.740849	25.059955
152.598948	4258.114001	25.064973
152.979232	4263.284723	25.069991
152.984348	4260.623191	25.075008
153.023734	4259.900640	25.080026
153.014097	4277.777042	25.085043
153.514935	4275.486056	25.090061
153.447171	4285.745677	25.095079
153.475214	4289.128243	25.100096
153.921949	4287.619054	25.105114
153.962400	4292.454785	25.110131
154.122531	4303.107985	25.115149
154.284186	4308.366631	25.120167
154.454744	4316.319466	25.125184
154.558029	4300.350863	25.130202
154.549346	4306.280103	25.135219
154.730586	4314.654225	25.140237
154.585502	4328.773661	25.145255
154.801111	4336.324895	25.150272
155.003557	4347.138783	25.155290
155.703498	4357.136132	25.160307
155.709309	4350.522630	25.165325
155.898491	4358.179019	25.170343
155.760397	4375.400166	25.175360
156.017666	4370.328634	25.180378
156.330891	4379.351272	25.185395
156.618643	4368.842746	25.190413
156.768776	4382.625583	25.195431
156.818604	4390.919321	25.200448
157.473600	4395.567266	25.205466
157.121136	4393.236344	25.210483
157.346402	4392.800310	25.215501
157.430051	4384.924653	25.220519
157.544817	4391.914081	25.225536
157.812086	4395.464357	25.230554
157.503447	4407.570421	25.235571
157.515103	4413.187179	25.240589
157.964428	4422.750362	25.245607
157.901705	4432.961930	25.250624
159.001362	4426.303291	25.255642
159.146330	4436.750621	25.260659
159.037331	4432.512938	25.265677
159.060965	4443.433808	25.270695
159.200496	4462.192921	25.275712
159.427494	4451.248807	25.280730
159.331652	4454.653969	25.285747
159.685112	4464.592028	25.290765
160.036177	4474.622005	25.295783
159.886352	4482.836588	25.300800
160.225710	4473.778197	25.305818
160.411851	4482.400988	25.310835
160.274848	4479.493391	25.315853
160.627530	4488.213195	25.320871
160.688649	4504.257463	25.325888
160.587248	4496.568571	25.330906
160.816504	4512.507594	25.335923
160.994196	4526.494548	25.340941
161.387515	4531.900040	25.345959
161.366205	4527.629658	25.350976
161.545504	4543.529188	25.355994
161.549398	4550.788564	25.361011
161.823295	4555.404718	25.366029
161.972421	4554.977452	25.371047
162.537113	4582.006303	25.376064
162.743289	4571.920781	25.381082
162.671216	4579.258355	25.386099
162.115269	4583.840386	25.391117
163.197694	4588.626590	25.396135
163.457248	4601.644367	25.401152
163.139420	4598.364207	25.406170
163.157416	4603.263512	25.411187
163.247713	4596.406262	25.416205
163.487274	4606.264392	25.421223
163.783668	4626.122805	25.426240
163.982812	4623.695966	25.431258
164.268250	4623.604026	25.436275
164.279736	4638.532483	25.441293
164.455549	4637.062554	25.446311
164.633422	4642.580744	25.451328
164.804355	4643.182229	25.456346
165.049243	4663.108724	25.461363
164.614990	4660.724294	25.466381
164.854804	4665.169053	25.471399
165.535878	4683.073373	25.476416
166.032743	4683.667989	25.481434
165.795461	4691.435521	25.486451
165.879218	4682.069856	25.491469
166.068843	4698.043659	25.496487
166.156004	4717.111107	25.501504
166.677160	4702.661245	25.506522
166.915533	4714.050517	25.511539
166.678860	4727.218725	25.516557
167.137572	4736.420764	25.521575
166.937365	4737.740104	25.526592
167.194641	4736.314221	25.531610
167.432470	4754.133384	25.536627
167.498933	4760.562353	25.541645
168.064150	4763.292682	25.546663
167.855036	4775.165599	25.551680
168.313579	4789.193983	25.556698
168.500407	4786.207195	25.561715
168.398021	4789.449306	25.566733
168.542603	4794.704455	25.571751
168.985402	4808.826859	25.576768
168.989738	4812.854007	25.581786
169.122900	4810.191274	25.586803
169.276131	4828.263657	25.591821
169.831035	4826.216656	25.596839
169.953191	4833.179845	25.601856
170.361184	4826.787249	25.606874
170.143736	4840.583828	25.611891
170.360680	4848.065624	25.616909
170.719874	4848.072606	25.621927
170.609271	4852.581778	25.626944
170.774459	4851.441774	25.631962
171.098220	4864.860029	25.636979
171.084907	4868.728973	25.641997
171.437377	4870.223729	25.647015
171.463952	4875.907736	25.652032
171.411189	4873.454042	25.657050
171.968679	4893.798982	25.662067
171.530576	4899.723090	25.667085
171.971078	4890.901169	25.672103
172.113272	4908.839632	25.677120
172.644752	4915.423074	25.682138
172.678476	4916.847821	25.687156
172.454866	4926.516696	25.692173
173.120835	4935.812629	25.697191
173.039449	4953.653588	25.702208
173.029664	4947.900889	25.707226
173.218127	4965.147191	25.712244
173.409503	4972.509939	25.717261
173.766039	4965.882302	25.722279
174.156156	4982.017494	25.727296
174.296035	4982.374490	25.732314
174.364380	4988.673826	25.737332
174.480681	4990.265565	25.742349
174.311372	4985.737330	25.747367
174.862496	5012.424886	25.752384
175.301127	5002.447910	25.757402
174.788657	5005.438650	25.762420
174.685439	5012.689738	25.767437
175.182381	5021.295661	25.772455
175.319643	5036.072165	25.777472
175.730164	5053.056491	25.782490
176.404467	5059.163068	25.787508
176.224390	5065.914858	25.792525
176.555013	5061.355631	25.797543
176.325794	5077.748919	25.802560
176.987869	5069.015306	25.807578
177.008834	5080.366268	25.812596
176.932340	5085.854998	25.817613
177.374802	5085.741614	25.822631
177.258311	5100.311713	25.827648
177.413277	5105.530603	25.832666
177.930623	5104.954099	25.837684
177.736891	5124.700448	25.842701
178.253389	5129.240864	25.847719
178.334058	5126.488455	25.852736
178.848388	5128.317724	25.857754
179.249958	5141.218944	25.862772
179.104186	5146.424986	25.867789
179.556858	5144.696997	25.872807
179.334541	5147.920081	25.877824
179.252072	5143.996889	25.882842
179.432563	5145.588055	25.887860
179.484728	5158.834430	25.892877
179.825642	5160.403623	25.897895
179.813408	5171.084336	25.902912
180.106790	5181.852910	25.907930
180.810567	5193.336871	25.912948
180.749438	5213.589690	25.917965
180.751827	5212.752948	25.922983
180.913998	5219.160772	25.928000
181.453060	5221.522794	25.933018
181.445272	5239.118916	25.938036
181.678558	5237.223267	25.943053
181.736518	5237.599415	25.948071
181.917058	5248.066891	25.953088
181.901056	5253.467281	25.958106
182.662411	5251.911885	25.963124
182.302137	5255.494355	25.968141
182.909374	5275.307937	25.973159
182.954836	5289.360387	25.978176
183.598322	5290.935852	25.983194
183.436440	5278.798998	25.988212
183.112895	5294.361292	25.993229
183.587051	5294.328170	25.998247
183.776254	5303.708455	26.003264
184.088072	5316.920581	26.008282
184.118749	5321.666575	26.013300
183.936791	5329.173183	26.018317
184.759998	5335.297563	26.023335
185.158941	5351.980950	26.028352
184.901260	5350.730393	26.033370
185.350628	5352.007988	26.038388
184.814166	5352.518297	26.043405
185.270922	5362.727918	26.048423
185.616125	5362.364616	26.053440
185.657381	5374.148193	26.058458
186.335077	5394.260215	26.063476
186.110620	5409.008461	26.068493
186.554382	5402.707916	26.073511
186.787821	5404.578063	26.078528
186.397474	5418.948259	26.083546
186.914170	5426.130805	26.088564
186.904016	5427.950730	26.093581
187.165619	5431.808290	26.098599
187.407321	5437.875444	26.103616
187.422687	5451.029941	26.108634
187.857630	5449.127933	26.113652
187.719107	5469.298461	26.118669
188.161991	5459.847727	26.123687
188.005886	5471.820117	26.128704
188.533783	5486.087549	26.133722
188.865541	5498.526467	26.138740
188.648587	5509.157378	26.143757
188.986029	5504.461239	26.148775
189.048597	5514.208700	26.153792
189.315997	5526.771358	26.158810
189.730188	5530.923855	26.163828
189.838278	5545.752693	26.168845
190.129434	5538.361717	26.173863
190.030163	5544.965289	26.178880
190.230724	5562.614311	26.183898
190.867176	5565.706090	26.188916
191.024579	5561.587397	26.193933
191.304052	5566.458624	26.198951
191.412209	5582.651149	26.203968
191.414207	5582.808793	26.208986
192.032014	5580.903377	26.214004
191.953730	5587.611001	26.219021
192.006688	5591.160365	26.224039
192.333649	5610.427930	26.229056
192.175997	5604.341487	26.234074
192.705951	5613.662236	26.239092
192.837303	5630.675055	26.244109
193.014159	5623.112553	26.249127
193.321639	5627.730034	26.254144
193.694460	5638.164456	26.259162
193.883469	5641.758806	26.264180
194.003681	5644.738917	26.269197
193.858180	5647.242964	26.274215
194.257702	5658.323486	26.279232
193.972812	5659.769795	26.284250
194.516697	5663.242265	26.289268
194.506047	5678.443358	26.294285
195.001012	5688.331512	26.299303
195.197214	5696.767062	26.304320
195.385567	5705.093362	26.309338
195.560980	5708.752988	26.314356
195.299969	5722.891664	26.319373
195.692890	5731.586825	26.324391
196.099315	5726.731460	26.329408
196.120775	5743.079759	26.334426
196.659862	5742.061057	26.339444
196.622890	5760.561904	26.344461
197.046055	5752.777675	26.349479
196.942248	5769.726449	26.354496
197.056333	5781.760884	26.359514
197.808319	5785.178680	26.364532
197.582036	5787.105103	26.369549
197.975116	5805.103002	26.374567
198.207549	5810.082678	26.379584
198.200564	5810.049173	26.384602
198.358938	5808.913336	26.389620
198.810729	5827.839594	26.394637
199.226244	5824.258079	26.399655
199.049563	5836.350728	26.404672
199.126960	5842.721546	26.409690
199.620876	5849.178635	26.414708
199.810066	5852.848759	26.419725
200.004595	5863.573246	26.424743
200.139717	5857.248295	26.429760
199.889199	5875.596468	26.434778
200.744097	5871.668322	26.439796
200.523780	5888.998479	26.444813
200.516905	5878.705705	26.449831
200.991126	5898.496613	26.454848
200.764473	5902.437078	26.459866
201.387727	5908.068968	26.464884
201.594508	5924.839806	26.469901
201.546871	5932.196192	26.474919
201.875846	5930.380184	26.479936
201.982848	5944.837026	26.484954
202.548396	5945.190491	26.489972
202.594783	5953.984241	26.494989
202.652753	5972.296810	26.500007
203.066195	5970.742199	26.505024
202.879537	5979.496708	26.510042
203.401614	5989.251354	26.515060
203.642012	5998.182037	26.520077
203.408021	6007.392228	26.525095
203.787286	6012.456286	26.530112
204.312333	6029.947599	26.535130
204.365880	6031.258843	26.540148
204.663232	6048.691143	26.545165
204.779533	6051.602486	26.550183
204.977716	6059.943192	26.555200
205.170429	6068.328954	26.560218
205.409180	6073.721243	26.565236
205.799341	6073.451902	26.570253
206.176131	6086.465005	26.575271
206.230752	6099.942120	26.580288
206.109973	6105.965268	26.585306
206.581160	6106.216720	26.590324
206.592993	6121.528302	26.595341
206.728040	6128.606766	26.600359
207.352607	6123.748691	26.605376
207.205985	6143.214123	26.610394
207.253126	6141.530635	26.615412
207.444419	6161.091515	26.620429
207.989166	6159.285877	26.625447
208.300018	6176.220576	26.630464
208.432351	6179.972278	26.635482
208.468864	6182.454197	26.640500
208.533806	6195.585680	26.645517
209.093435	6203.756186	26.650535
209.394085	6210.123725	26.655552
209.425753	6217.167911	26.660570
209.729537	6222.180717	26.665588
209.805788	6235.979689	26.670605
209.969458	6244.780459	26.675623
210.206867	6259.491758	26.680640
210.487427	6266.519070	26.685658
210.886268	6260.446244	26.690676
210.952718	6280.604497	26.695693
211.075552	6288.616182	26.700711
211.487486	6278.150243	26.705728
211.263790	6287.901924	26.710746
211.612140	6297.573466	26.715764
211.683522	6299.323882	26.720781
212.155665	6326.745483	26.725799
212.555644	6321.180700	26.730816
212.548703	6334.945427	26.735834
212.671973	6341.659634	26.740852
213.256064	6355.410707	26.745869
213.126055	6355.529058	26.750887
213.597578	6359.202406	26.755904
213.689935	6374.763597	26.760922
214.373070	6378.646871	26.765940
214.010096	6382.596166	26.770957
213.979732	6400.477896	26.775975
214.377264	6407.505878	26.780992
214.584393	6411.005995	26.786010
215.121345	6416.714702	26.791028
215.322698	6422.794820	26.796045
215.560966	6436.656952	26.801063
215.627140	6430.023769	26.806080
215.447610	6436.248793	26.811098
215.761694	6441.616763	26.816116
216.102268	6452.757512	26.821133
216.432355	6450.051065	26.826151
216.517824	6468.066241	26.831168
216.406708	6468.421549	26.836186
216.834447	6475.293300	26.841204
217.163865	6483.111710	26.846221
217.252584	6488.006755	26.851239
217.572215	6506.641899	26.856256
217.644945	6509.759020	26.861274
218.061148	6522.829397	26.866292
218.052184	6523.762182	26.871309
218.399697	6533.424510	26.876327
218.875177	6548.225018	26.881344
218.775257	6554.601765	26.886362
219.422335	6562.910260	26.891380
219.412047	6577.600639	26.896397
219.540252	6587.272097	26.901415
219.617558	6586.366733	26.906432
220.050106	6612.690081	26.911450
220.147596	6620.554354	26.916468
220.439496	6622.024024	26.921485
220.669066	6638.125857	26.926503
221.016126	6639.517437	26.931520
220.978251	6656.182059	26.936538
221.324952	6658.293454	26.941556
221.528170	6661.513274	26.946573
221.554453	6682.963090	26.951591
222.042394	6687.814589	26.956608
222.267543	6699.516546	26.961626
222.630998	6702.948035	26.966644
222.891343	6708.141406	26.971661
223.213833	6724.923263	26.976679
223.369118	6724.453947	26.981696
223.507866	6732.273923	26.986714
224.148520	6734.235101	26.991732
224.321078	6752.846183	26.996749
224.005128	6760.986793	27.001767
224.483954	6764.210809	27.006784
224.745367	6763.639632	27.011802
224.974046	6766.151506	27.016820
225.316554	6765.766506	27.021837
225.380837	6775.315490	27.026855
225.904632	6793.082378	27.031872
226.208895	6793.344209	27.036890
226.164934	6785.219177	27.041908
226.397357	6788.794326	27.046925
226.146039	6817.861070	27.051943
226.608732	6810.843634	27.056960
226.852387	6816.311141	27.061978
226.935078	6823.656939	27.066996
227.264253	6834.989118	27.072013
227.306898	6858.330691	27.077031
227.587041	6853.851540	27.082048
227.537778	6872.352278	27.087066
227.688318	6881.805726	27.092084
228.257763	6892.680438	27.097101
227.909725	6913.279986	27.102119
228.460840	6918.513102	27.107136
228.812638	6937.162587	27.112154
229.172587	6938.018660	27.117172
229.378153	6957.710744	27.122189
229.904251	6964.270525	27.127207
230.120621	6964.066283	27.132224
230.047135	6967.556800	27.137242
230.361603	6990.795978	27.142260
230.595360	6995.343278	27.147277
230.734691	6996.240229	27.152295
231.209726	7010.498199	27.157312
231.223743	7015.035731	27.162330
231.374298	7031.301819	27.167348
231.453187	7038.777731	27.172365
231.538573	7046.079000	27.177383
231.927873	7058.535224	27.182400
232.356638	7068.125125	27.187418
232.509305	7091.920136	27.192436
232.984557	7094.001973	27.197453
233.173824	7101.006025	27.202471
233.623330	7123.816976	27.207488
233.799630	7127.697733	27.212506
233.761733	7123.464069	27.217524
233.878803	7134.488716	27.222541
234.169578	7143.803524	27.227559
234.394968	7156.550673	27.232576
234.747844	7160.034417	27.237594
235.263897	7179.024618	27.242612
235.459704	7180.856649	27.247629
235.337547	7186.179530	27.252647
235.750809	7192.605538	27.257664
236.321193	7206.779271	27.262682
236.425738	7215.933875	27.267700
236.994090	7216.656294	27.272717
236.937061	7226.969550	27.277735
237.098265	7226.647670	27.282752
237.304596	7230.511117	27.287770
237.617104	7244.873653	27.292788
237.818051	7241.988436	27.297805
237.632430	7255.437740	27.302823
238.356406	7277.808112	27.307840
238.632080	7289.136327	27.312858
238.603158	7285.112734	27.317876
238.982984	7302.018729	27.322893
238.942150	7302.375671	27.327911
239.069029	7318.999299	27.332928
239.346620	7332.906460	27.337946
239.645156	7352.357104	27.342964
239.935904	7361.959310	27.347981
240.014356	7374.376050	27.352999
240.196853	7378.053845	27.358016
240.684009	7388.843880	27.363034
240.824409	7411.334248	27.368052
241.151029	7414.364395	27.373069
240.994407	7435.619598	27.378087
241.635776	7436.485279	27.383104
242.242975	7455.480431	27.388122
242.346274	7464.783731	27.393140
242.738479	7468.485518	27.398157
242.929202	7481.569805	27.403175
242.915224	7489.322476	27.408192
243.180751	7494.035401	27.413210
243.520275	7508.659097	27.418228
243.760505	7510.124308	27.423245
243.788955	7514.855435	27.428263
244.221738	7526.080260	27.433280
244.370997	7538.122967	27.438298
244.818464	7550.965036	27.443316
245.230086	7553.233687	27.448333
245.239065	7566.352818	27.453351
245.497887	7568.885338	27.458368
245.472095	7569.924994	27.463386
245.532791	7583.455915	27.468404
246.144314	7596.821632	27.473421
246.321464	7612.272722	27.478439
246.196318	7605.182910	27.483456
246.408978	7619.059420	27.488474
246.605162	7628.922825	27.493492
247.379276	7643.607985	27.498509
247.290279	7653.535020	27.503527
247.521931	7661.053551	27.508544
247.651047	7674.712729	27.513562
247.905101	7692.342797	27.518580
248.474442	7703.975691	27.523597
248.536812	7715.230246	27.528615
248.847093	7729.811344	27.533632
249.086221	7740.757250	27.538650
249.334620	7751.326026	27.543668
249.720505	7756.796790	27.548685
249.698130	7777.283144	27.553703
250.264258	7782.747779	27.558720
250.497072	7799.487840	27.563738
250.363628	7810.697359	27.568756
250.909490	7816.525080	27.573773
250.972813	7836.985447	27.578791
251.193903	7852.603492	27.583808
251.782364	7858.067808	27.588826
252.085944	7872.599556	27.593844
252.400193	7889.087008	27.598861
252.327868	7900.069171	27.603879
253.021930	7906.738733	27.608896
253.380995	7912.018008	27.613914
253.292770	7918.898520	27.618932
253.826515	7932.096715	27.623949
253.834851	7936.461727	27.628967
254.079888	7945.004318	27.633984
254.526332	7951.605348	27.639002
254.526916	7959.507474	27.644020
255.104113	7976.623107	27.649037
255.268088	7984.253399	27.654055
255.532251	7999.208153	27.659072
256.291695	8011.041928	27.664090
256.179239	8013.389578	27.669108
256.372623	8013.915051	27.674125
256.417630	8023.360362	27.679143
256.612708	8023.276257	27.684160
256.787095	8031.880469	27.689178
257.220906	8045.381693	27.694196
257.438692	8049.031995	27.699213
257.524325	8060.564095	27.704231
257.772280	8083.581450	27.709248
258.504151	8093.951560	27.714266
258.775186	8101.154709	27.719284
258.902655	8107.013338	27.724301
258.993637	8123.232895	27.729319
259.513801	8128.152347	27.734336
259.319810	8136.078715	27.739354
259.876326	8155.480324	27.744372
260.290299	8150.335853	27.749389
260.349249	8175.918068	27.754407
260.559272	8186.553091	27.759424
260.674927	8189.755328	27.764442
260.914856	8206.396776	27.769460
261.615045	8207.714220	27.774477
261.703016	8225.045635	27.779495
261.872419	8238.070657	27.784512
262.234898	8233.350967	27.789530
262.153698	8251.817049	27.794548
262.538659	8247.223274	27.799565
262.579064	8265.234640	27.804583
263.016821	8277.283150	27.809600
263.559167	8285.514129	27.814618
263.384930	8296.660876	27.819636
263.731055	8306.917894	27.824653
264.326995	8318.445985	27.829671
264.220946	8326.346030	27.834688
264.582982	8323.375427	27.839706
264.543324	8344.234498	27.844724
264.939980	8345.751044	27.849741
265.426929	8376.103191	27.854759
265.508672	8386.019658	27.859776
265.993708	8385.583889	27.864794
265.866309	8404.341501	27.869812
266.311140	8402.898593	27.874829
266.561060	8428.849041	27.879847
266.628388	8435.541206	27.884864
267.243571	8442.580078	27.889882
267.358008	8467.674121	27.894900
268.046540	8473.975374	27.899917
268.192012	8476.320564	27.904935
268.308694	8486.029554	27.909952
268.696001	8502.411396	27.914970
268.847691	8518.820691	27.919988
269.554287	8525.548504	27.925005
269.810090	8536.321785	27.930023
269.798378	8548.301968	27.935040
270.051555	8546.803829	27.940058
270.261160	8570.692858	27.945076
270.400357	8574.693392	27.950093
270.727085	8589.364152	27.955111
270.933451	8600.925033	27.960128
271.433663	8611.622186	27.965146
271.224726	8625.480253	27.970164
271.375512	8640.712176	27.975181
271.996756	8651.257791	27.980199
272.347265	8676.286722	27.985216
272.827525	8684.155059	27.990234
272.976281	8696.609034	27.995252
273.148025	8702.836620	28.000269
273.674552	8715.411388	28.005287
274.037500	8726.253240	28.010304
274.226028	8742.723263	28.015322
274.387587	8753.937655	28.020340
274.693020	8772.959341	28.025357
274.930819	8782.570584	28.030375
275.065909	8787.099058	28.035392
275.855287	8791.793400	28.040410
275.781998	8806.609082	28.045428
276.447974	8827.737024	28.050445
276.580747	8827.498503	28.055463
276.765570	8834.930134	28.060480
276.822672	8848.620405	28.065498
277.014570	8855.151134	28.070516
277.566089	8870.336257	28.075533
277.720757	8869.478650	28.080551
277.401947	8892.137474	28.085568
278.086147	8910.594814	28.090586
278.203746	8927.243445	28.095604
278.770537	8931.979006	28.100621
279.197068	8941.551296	28.105639
279.235320	8960.030943	28.110656
279.758708	8969.086076	28.115674
279.723537	8982.247858	28.120692
280.009873	8999.517352	28.125709
280.389073	9012.074357	28.130727
280.869519	9029.228227	28.135744
281.109074	9037.052334	28.140762
281.185260	9046.130201	28.145780
281.680724	9059.111039	28.150797
281.708842	9061.743052	28.155815
281.925693	9076.936569	28.160832
282.485660	9078.244475	28.165850
282.468511	9098.747259	28.170868
282.966005	9110.026060	28.175885
282.974317	9115.723712	28.180903
283.477876	9129.195862	28.185920
283.225212	9146.063710	28.190938
284.122984	9158.015477	28.195956
284.183269	9165.984540	28.200973
284.589483	9175.822187	28.205991
284.810221	9194.361884	28.211008
285.201268	9199.058743	28.216026
285.828322	9217.525342	28.221044
286.037347	9233.421126	28.226061
286.729617	9234.948272	28.231079
286.312338	9234.170772	28.236096
286.869906	9243.937387	28.241114
287.288262	9258.569066	28.246132
287.303680	9273.563819	28.251149
287.333400	9281.540877	28.256167
287.520981	9296.729688	28.261184
287.878836	9300.285680	28.266202
288.432381	9323.663997	28.271220
288.523850	9341.077998	28.276237
288.893844	9348.572390	28.281255
289.374071	9363.216562	28.286272
289.544408	9375.067727	28.291290
289.659360	9380.780328	28.296308
290.171256	9401.551030	28.301325
290.835638	9415.711745	28.306343
290.575739	9424.589861	28.311360
291.242703	9439.574245	28.316378
291.392217	9452.038080	28.321396
291.429518	9467.509471	28.326413
291.812246	9477.972947	28.331431
292.052552	9495.010158	28.336448
292.103811	9510.349948	28.341466
292.665876	9524.836191	28.346484
293.044241	9539.114423	28.351501
293.645865	9548.864826	28.356519
293.485035	9564.133693	28.361536
293.902787	9577.010247	28.366554
294.400265	9596.290012	28.371572
294.088293	9600.945549	28.376589
294.769493	9621.465806	28.381607
294.948655	9628.927060	28.386624
295.296996	9641.280943	28.391642
295.339643	9658.886014	28.396660
295.627396	9673.797383	28.401677
296.098661	9690.583895	28.406695
296.587661	9704.390266	28.411712
296.842406	9719.278425	28.416730
297.279137	9738.668889	28.421748
297.502885	9753.142004	28.426765
298.037253	9751.239784	28.431783
298.014956	9770.923202	28.436800
298.416289	9778.185530	28.441818
298.998326	9788.245392	28.446836
299.644519	9790.114485	28.451853
299.745515	9789.129479	28.456871
299.909342	9805.042305	28.461888
300.277027	9816.771275	28.466906
300.548372	9821.338648	28.471924
300.554307	9832.006587	28.476941
300.821285	9830.133617	28.481959
301.038585	9843.193311	28.486976
301.780431	9855.109968	28.491994
301.767794	9864.663126	28.497012
301.774771	9882.008776	28.502029
302.233154	9885.905919	28.507047
302.189407	9895.694454	28.512064
302.292895	9913.451262	28.517082
302.804342	9931.769344	28.522100
303.177495	9947.535835	28.527117
303.984433	9959.881241	28.532135
303.965752	9979.169639	28.537152
304.011498	9991.650091	28.542170
304.260077	10004.783934	28.547188
304.580331	10015.210139	28.552205
305.073272	10030.370661	28.557223
304.983159	10055.088429	28.562240
305.461901	10064.021641	28.567258
306.077096	10088.603710	28.572276
306.440254	10107.273564	28.577293
306.630590	10113.356629	28.582311
306.893507	10132.020109	28.587328
307.237207	10146.859945	28.592346
307.644745	10149.448464	28.597364
307.657990	10170.077120	28.602381
308.446145	10182.621377	28.607399
308.640446	10190.610933	28.612416
308.898444	10206.294645	28.617434
309.527958	10224.490325	28.622452
309.690360	10234.935066	28.627469
310.464181	10254.361673	28.632487
310.620566	10260.383798	28.637504
310.755582	10270.883368	28.642522
311.121722	10290.875908	28.647540
310.999950	10300.247465	28.652557
311.718951	10303.428178	28.657575
311.864793	10317.926566	28.662592
311.976715	10329.086536	28.667610
312.673576	10341.073703	28.672628
312.976409	10355.803282	28.677645
313.374142	10367.979409	28.682663
313.428760	10372.767159	28.687680
313.892696	10386.132763	28.692698
314.306730	10395.423593	28.697716
314.551901	10407.705739	28.702733
314.669904	10421.027675	28.707751
314.669213	10432.978927	28.712768
315.078245	10436.887076	28.717786
315.631810	10452.265784	28.722804
315.539411	10470.003287	28.727821
316.180308	10488.349002	28.732839
316.361195	10495.608255	28.737856
316.668961	10516.090118	28.742874
317.585755	10527.083079	28.747892
317.200971	10549.672152	28.752909
318.122340	10563.919791	28.757927
317.954138	10576.579393	28.762944
318.509059	10586.697616	28.767962
318.885282	10597.882652	28.772980
319.272116	10613.499163	28.777997
319.765046	10623.200854	28.783015
319.630431	10633.452374	28.788032
320.088466	10643.475292	28.793050
320.426833	10652.358155	28.798068
320.811243	10667.911941	28.803085
321.226413	10679.447725	28.808103
321.268506	10690.694630	28.813120
321.617226	10700.892578	28.818138
322.064653	10705.419957	28.823156
322.156174	10731.316338	28.828173
322.751534	10726.420615	28.833191
322.843641	10747.084917	28.838208
323.087466	10761.438842	28.843226
323.601914	10770.237344	28.848244
324.009077	10774.714213	28.853261
324.304206	10786.505681	28.858279
324.131145	10805.452841	28.863296
324.603145	10821.555076	28.868314
325.324467	10827.678343	28.873332
325.288445	10842.742407	28.878349
325.876753	10847.907680	28.883367
325.697817	10863.212018	28.888384
326.210267	10875.591536	28.893402
326.432546	10892.645481	28.898420
326.768106	10902.248824	28.903437
326.851931	10926.441604	28.908455
327.456063	10940.369793	28.913472
327.470741	10960.276016	28.918490
328.071962	10975.969763	28.923508
328.288377	11007.322174	28.928525
328.957634	11024.830378	28.933543
328.867673	11045.804553	28.938560
329.252081	11051.349156	28.943578
329.640687	11070.306486	28.948596
330.115187	11095.331881	28.953613
330.584042	11108.135184	28.958631
331.061955	11119.926649	28.963648
331.409592	11142.588003	28.968666
331.777014	11146.202850	28.973684
332.088692	11171.736964	28.978701
332.420040	11184.438713	28.983719
332.646851	11203.348898	28.988736
333.177102	11215.009079	28.993754
333.503011	11220.850237	28.998772
333.116409	11248.937822	29.003789
334.125742	11259.714638	29.008807
334.188249	11267.763192	29.013824
334.633290	11297.858281	29.018842
335.370216	11306.413785	29.023860
335.570839	11328.965774	29.028877
335.906172	11336.917941	29.033895
336.117663	11344.147469	29.038912
336.544340	11356.894397	29.043930
336.944060	11376.955467	29.048948
337.166945	11388.120791	29.053965
337.338062	11404.700098	29.058983
337.657463	11419.083739	29.064000
337.934797	11438.930381	29.069018
338.416738	11448.902623	29.074036
338.712536	11467.312833	29.079053
338.928963	11481.778963	29.084071
339.119181	11509.113476	29.089088
339.651714	11512.614117	29.094106
340.181214	11530.091008	29.099124
340.200416	11551.212846	29.104141
340.754502	11566.554501	29.109159
340.884347	11588.723181	29.114176
341.088627	11614.448393	29.119194
341.887960	11624.371012	29.124212
341.994853	11643.489885	29.129229
342.447138	11657.211886	29.134247
342.704388	11671.491780	29.139264
342.743702	11687.450975	29.144282
343.531369	11694.426185	29.149300
343.806393	11725.966393	29.154317
344.181327	11740.900493	29.159335
344.483554	11751.602056	29.164352
344.547612	11764.466060	29.169370
345.351895	11773.497514	29.174388
345.627498	11785.927369	29.179405
345.819395	11798.161935	29.184423
346.154890	11813.095956	29.189440
346.295143	11817.235962	29.194458
347.235550	11833.455160	29.199476
347.805922	11856.458255	29.204493
347.907140	11851.658595	29.209511
348.210513	11867.775516	29.214528
348.743285	11884.317543	29.219546
348.819526	11892.272640	29.224564
348.797540	11910.897265	29.229581
349.202537	11918.106177	29.234599
349.601010	11934.729283	29.239616
349.594092	11955.928294	29.244634
350.122970	11973.209918	29.249652
350.576274	11994.554766	29.254669
351.080197	12013.220265	29.259687
351.491670	12029.506698	29.264704
351.659034	12047.846022	29.269722
352.169806	12059.235058	29.274740
352.480588	12079.576062	29.279757
352.610373	12094.826726	29.284775
353.121074	12111.066109	29.289792
353.323490	12125.152842	29.294810
353.920150	12140.728288	29.299828
353.734652	12158.841953	29.304845
354.116864	12186.627356	29.309863
354.817800	12205.101139	29.314880
355.203985	12224.944192	29.319898
355.598419	12240.905069	29.324916
356.109386	12256.415091	29.329933
356.426153	12272.069225	29.334951
356.410721	12294.261493	29.339968
356.842209	12319.929976	29.344986
357.403106	12324.954699	29.350004
357.660418	12342.572876	29.355021
358.270334	12358.604307	29.360039
358.706384	12379.431259	29.365056
358.819970	12394.163667	29.370074
359.648059	12399.323394	29.375092
359.608337	12430.756195	29.380109
360.122501	12442.031253	29.385127
360.672630	12458.991057	29.390144
360.778385	12478.483578	29.395162
361.412138	12482.565377	29.400180
361.705238	12503.238020	29.405197
362.069698	12514.176580	29.410215
362.608982	12541.078976	29.415232
362.533128	12551.556014	29.420250
363.278020	12561.503452	29.425268
363.684673	12571.020729	29.430285
364.087971	12593.236177	29.435303
364.237357	12599.661198	29.440320
364.477935	12622.546368	29.445338
364.689912	12631.860490	29.450356
365.261691	12653.440156	29.455373
365.240145	12670.969691	29.460391
366.023235	12683.652221	29.465408
365.986487	12702.722039	29.470426
366.311761	12717.216280	29.475444
366.670159	12737.733691	29.480461
366.803120	12760.550623	29.485479
367.659780	12791.167833	29.490496
367.851621	12806.766192	29.495514
368.155966	12818.440655	29.500532
368.417674	12844.401707	29.505549
368.790037	12854.101340	29.510567
369.494110	12866.625846	29.515584
369.447535	12877.979527	29.520602
369.941954	12896.726339	29.525620
370.340310	12917.736633	29.530637
370.650611	12928.409182	29.535655
371.150084	12954.588932	29.540672
371.429051	12971.057989	29.545690
371.715482	12976.236407	29.550708
372.681351	12996.311578	29.555725
372.768288	13010.262324	29.560743
372.987043	13024.002958	29.565760
373.305918	13052.175349	29.570778
373.849920	13069.919826	29.575796
374.025458	13082.003052	29.580813
374.291051	13097.432202	29.585831
374.898535	13116.082575	29.590848
375.218635	13140.316980	29.595866
375.697644	13157.414871	29.600884
375.923076	13177.691481	29.605901
376.265203	13197.431932	29.610919
376.964113	13222.475538	29.615936
377.464655	13241.847006	29.620954
377.782377	13247.538501	29.625972
377.532513	13275.667678	29.630989
378.079881	13297.182430	29.636007
378.744295	13306.343910	29.641024
379.244455	13323.495482	29.646042
379.705722	13342.740572	29.651060
380.282602	13365.757126	29.656077
379.804064	13379.743034	29.661095
380.692078	13395.668631	29.666112
381.056250	13411.322602	29.671130
381.772765	13421.720217	29.676148
382.162283	13449.335805	29.681165
382.037335	13467.965460	29.686183
382.670666	13475.385530	29.691200
383.291007	13506.438824	29.696218
383.693392	13520.517382	29.701236
384.319326	13532.050332	29.706253
384.616888	13542.589430	29.711271
385.057283	13551.858754	29.716288
384.853921	13570.788170	29.721306
385.541702	13590.143299	29.726324
385.736984	13602.959579	29.731341
386.046889	13626.450915	29.736359
386.569918	13643.236026	29.741376
386.963272	13658.711941	29.746394
387.161227	13675.380624	29.751412
387.601663	13694.844081	29.756429
387.929113	13725.804660	29.761447
388.779452	13742.529116	29.766464
388.587538	13758.441012	29.771482
389.092686	13785.770547	29.776500
389.657301	13800.657622	29.781517
390.048640	13815.044459	29.786535
390.671128	13827.310795	29.791552
390.377395	13850.126400	29.796570
390.755325	13870.591453	29.801588
391.573365	13891.423402	29.806605
392.005708	13909.558808	29.811623
392.200256	13919.795289	29.816640
392.705581	13941.228935	29.821658
393.052729	13970.449897	29.826676
393.377033	13985.482134	29.831693
394.142862	14000.631550	29.836711
394.790087	14009.214982	29.841728
394.576994	14029.835945	29.846746
395.026614	14045.293889	29.851764
395.287626	14059.897127	29.856781
395.759674	14078.617036	29.861799
396.285380	14091.170299	29.866816
396.327328	14118.996051	29.871834
396.709196	14129.042241	29.876852
397.074889	14138.080382	29.881869
397.811063	14155.258903	29.886887
398.160148	14173.995010	29.891904
398.476847	14203.401111	29.896922
398.933309	14212.892468	29.901940
399.541086	14231.758649	29.906957
399.709049	14258.184774	29.911975
400.098976	14269.022462	29.916992
400.394256	14286.099625	29.922010
400.924487	14309.089894	29.927028
401.214509	14330.699820	29.932045
401.403432	14352.631945	29.937063
401.764019	14365.486010	29.942080
402.277501	14392.685631	29.947098
402.726052	14425.501154	29.952116
403.415020	14438.123819	29.957133
403.677561	14460.382457	29.962151
403.908144	14475.988755	29.967168
404.207016	14508.562582	29.972186
404.839606	14531.514981	29.977204
405.375792	14544.546942	29.982221
405.606088	14578.480164	29.987239
406.136811	14593.887954	29.992256
406.930246	14620.652438	29.997274
407.053923	14632.372112	30.002292
407.558707	14658.603917	30.007309
407.733020	14672.346391	30.012327
408.363118	14691.537983	30.017344
408.900922	14714.612828	30.022362
409.084850	14729.017056	30.027380
409.508963	14747.653547	30.032397
409.820525	14775.611727	30.037415
410.857837	14780.012965	30.042432
410.818450	14807.555592	30.047450
411.652267	14822.672912	30.052468
411.840808	14836.836475	30.057485
411.993776	14859.273811	30.062503
412.462444	14869.013085	30.067520
412.654514	14896.437472	30.072538
413.581294	14918.977906	30.077556
414.300805	14942.665685	30.082573
414.099974	14952.408805	30.087591
414.687182	14969.311368	30.092608
415.171106	14989.400987	30.097626
415.367237	15011.275892	30.102644
415.873060	15028.633408	30.107661
416.364727	15043.507622	30.112679
416.826365	15056.422124	30.117696
416.868456	15077.983302	30.122714
417.541501	15110.152143	30.127732
418.219376	15126.033161	30.132749
418.412627	15143.196555	30.137767
418.817958	15153.031169	30.142784
419.191085	15172.951999	30.147802
419.272948	15186.832497	30.152820
419.844136	15207.363467	30.157837
420.327144	15232.519347	30.162855
421.002603	15257.316654	30.167872
421.571272	15270.277703	30.172890
421.522630	15283.389144	30.177908
422.334221	15309.690646	30.182925
422.388003	15326.907634	30.187943
422.951433	15342.228792	30.192960
423.728970	15360.080960	30.197978
423.750173	15369.742140	30.202996
424.525662	15378.650360	30.208013
424.775278	15391.531976	30.213031
425.036196	15413.678284	30.218048
425.237619	15434.614830	30.223066
425.363798	15447.986406	30.228084
425.754884	15469.231221	30.233101
426.350960	15485.794914	30.238119
426.746532	15509.407806	30.243136
427.309042	15535.148554	30.248154
427.716902	15558.784849	30.253172
428.180922	15573.407984	30.258189
428.426039	15590.377315	30.263207
428.920081	15615.967821	30.268224
429.152892	15640.869703	30.273242
429.378402	15673.314884	30.278260
430.121448	15701.172093	30.283277
430.641244	15730.444511	30.288295
431.147898	15748.361581	30.293312
431.378005	15778.462720	30.298330
431.718667	15803.477413	30.303348
432.112844	15820.278315	30.308365
432.903109	15848.684216	30.313383
433.333854	15877.907641	30.318400
433.992542	15895.917896	30.323418
434.363706	15924.531681	30.328436
435.038889	15937.362800	30.333453
434.977408	15963.100793	30.338471
435.987816	15983.086885	30.343488
436.753361	15996.371332	30.348506
436.781125	16020.503591	30.353524
437.521600	16031.318962	30.358541
438.121761	16054.331969	30.363559
438.156115	16059.083273	30.368576
438.610729	16079.949283	30.373594
438.847863	16109.064416	30.378612
439.652541	16117.042998	30.383629
439.598472	16152.122682	30.388647
440.455495	16166.643654	30.393664
440.753767	16181.075285	30.398682
440.957250	16206.911073	30.403700
441.580821	16220.559025	30.408717
441.927742	16255.980370	30.413735
442.433274	16275.774224	30.418752
442.811004	16295.354391	30.423770
443.030224	16313.250684	30.428788
443.951320	16337.192882	30.433805
444.122407	16373.071534	30.438823
444.838150	16393.407423	30.443840
445.011143	16403.228539	30.448858
445.349305	16435.433112	30.453876
445.737912	16444.607734	30.458893
446.319012	16470.504752	30.463911
446.749539	16492.098274	30.468928
447.044744	16523.592750	30.473946
447.452027	16536.065105	30.478964
448.280710	16557.924820	30.483981
448.301409	16588.707520	30.488999
449.090208	16615.475531	30.494016
448.983566	16633.132580	30.499034
449.940402	16668.007488	30.504052
450.306422	16690.075636	30.509069
450.958120	16712.345429	30.514087
451.124829	16736.886381	30.519104
451.775687	16753.139376	30.524122
452.251918	16773.620574	30.529140
452.766367	16793.176676	30.534157
452.634520	16814.609122	30.539175
453.346877	16828.091992	30.544192
453.501664	16837.549791	30.549210
453.825434	16874.612023	30.554228
454.762878	16893.558704	30.559245
455.251657	16925.964764	30.564263
455.535642	16941.852137	30.569280
456.071337	16960.861811	30.574298
456.748570	16980.231520	30.579316
457.472900	16990.977319	30.584333
457.719996	17010.698702	30.589351
458.190606	17028.976375	30.594368
459.216575	17036.699585	30.599386
459.165510	17064.054604	30.604404
459.454578	17072.139618	30.609421
460.138462	17088.286650	30.614439
460.652463	17110.278407	30.619456
461.132656	17125.661413	30.624474
461.634977	17148.773182	30.629492
461.912664	17168.932138	30.634509
462.182245	17187.336207	30.639527
462.583710	17207.444229	30.644544
463.500886	17230.434263	30.649562
463.699420	17262.797911	30.654580
464.396732	17273.939768	30.659597
464.649852	17298.531073	30.664615
464.963856	17314.091874	30.669632
465.465800	17335.624620	30.674650
465.687452	17364.327139	30.679668
466.421008	17372.734329	30.684685
466.661876	17413.278749	30.689703
466.854064	17427.323627	30.694720
467.531070	17460.061188	30.699738
467.965915	17496.008011	30.704756
468.305458	17521.685271	30.709773
468.699284	17551.750906	30.714791
468.876467	17590.461020	30.719808
469.704388	17611.254429	30.724826
470.627574	17643.044047	30.729844
471.057120	17665.858285	30.734861
471.636131	17694.378975	30.739879
472.018753	17724.617202	30.744896
472.966351	17749.965785	30.749914
473.380410	17765.043793	30.754932
473.613097	17788.381765	30.759949
474.240131	17806.016572	30.764967
474.711019	17826.815597	30.769984
475.438069	17846.165742	30.775002
475.504168	17870.875512	30.780020
476.066850	17893.574405	30.785037
476.490379	17914.968462	30.790055
477.018902	17937.104189	30.795072
477.634844	17956.408673	30.800090
477.865066	17977.201333	30.805108
478.307001	17999.230662	30.810125
478.813175	18020.934081	30.815143
478.972877	18036.222712	30.820160
479.518301	18063.934255	30.825178
479.935233	18095.115308	30.830196
480.234309	18119.833127	30.835213
480.867449	18149.476841	30.840231
481.160999	18182.894802	30.845248
481.589054	18192.266242	30.850266
481.851573	18226.775750	30.855284
482.609462	18253.607740	30.860301
483.545428	18292.484699	30.865319
484.282629	18314.708207	30.870336
484.650910	18321.265126	30.875354
484.776110	18349.087120	30.880372
485.670283	18365.454991	30.885389
486.204642	18385.170689	30.890407
486.136653	18402.289461	30.895424
487.131141	18424.498068	30.900442
487.323947	18446.762772	30.905460
487.748353	18475.441499	30.910477
488.317169	18492.151048	30.915495
488.934332	18504.380167	30.920512
489.262466	18528.563277	30.925530
489.831225	18554.168100	30.930548
490.611379	18571.192085	30.935565
491.244876	18594.202910	30.940583
491.234387	18615.274025	30.945600
491.899147	18631.817044	30.950618
492.488968	18658.960215	30.955636
492.753318	18674.220322	30.960653
493.190287	18710.105889	30.965671
493.497857	18725.580386	30.970688
494.220492	18749.840971	30.975706
494.663673	18778.870996	30.980724
495.340896	18797.256973	30.985741
496.088345	18819.188842	30.990759
496.432745	18852.587356	30.995776
496.995600	18871.642043	31.000794
496.682302	18896.469400	31.005812
497.430736	18920.719840	31.010829
498.221851	18939.422955	31.015847
498.787881	18980.595721	31.020864
499.511099	18994.103683	31.025882
499.536092	19028.298023	31.030900
499.990963	19053.870801	31.035917
500.959145	19084.335325	31.040935
500.914161	19107.642560	31.045952
501.860214	19126.315270	31.050970
502.510806	19156.292635	31.055988
503.022708	19180.150835	31.061005
503.595020	19197.662810	31.066023
503.478808	19225.416464	31.071040
504.483955	19245.962753	31.076058
505.097563	19281.884887	31.081076
505.336606	19297.086268	31.086093
505.997095	19321.843779	31.091111
506.072193	19352.758179	31.096128
507.425066	19376.276412	31.101146
507.493536	19404.614231	31.106164
507.866014	19417.204466	31.111181
508.437762	19442.721542	31.116199
509.256144	19472.243496	31.121216
509.819225	19488.999029	31.126234
510.264100	19521.991242	31.131252
510.518548	19541.701413	31.136269
511.164461	19567.402893	31.141287
511.567819	19590.570986	31.146304
512.092990	19608.482428	31.151322
512.282730	19638.002006	31.156340
512.929303	19662.395687	31.161357
513.420800	19687.963562	31.166375
513.921496	19710.756426	31.171392
514.735475	19736.722435	31.176410
514.924937	19769.584484	31.181428
515.386693	19790.665038	31.186445
516.245503	19812.359457	31.191463
516.647828	19846.388723	31.196480
517.349584	19865.725896	31.201498
517.545065	19899.181117	31.206516
517.856201	19920.228539	31.211533
518.534194	19937.029641	31.216551
519.302733	19962.971478	31.221568
519.596212	19978.682948	31.226586
519.822908	20012.196654	31.231604
520.171056	20031.128153	31.236621
520.716245	20050.351033	31.241639
520.753148	20082.346648	31.246656
521.449701	20106.341332	31.251674
522.239888	20147.645726	31.256692
522.599272	20182.630024	31.261709
523.816670	20214.131372	31.266727
523.763284	20240.751991	31.271744
524.697538	20258.429369	31.276762
525.119004	20295.514417	31.281780
525.315689	20329.147093	31.286797
525.953509	20354.661333	31.291815
526.501400	20394.405689	31.296832
527.469202	20415.635116	31.301850
527.884789	20447.584652	31.306868
527.927530	20473.899892	31.311885
528.745704	20498.659474	31.316903
528.964297	20535.991572	31.321920
529.858245	20562.003020	31.326938
530.415369	20599.143215	31.331956
530.793503	20615.277899	31.336973
531.530920	20637.440848	31.341991
532.276079	20680.933235	31.347008
532.925234	20706.079695	31.352026
533.544818	20740.297628	31.357044
533.853734	20770.975457	31.362061
534.610678	20788.990687	31.367079
534.992096	20818.690528	31.372096
535.665443	20836.560935	31.377114
536.054459	20865.621502	31.382132
536.667096	20897.490362	31.387149
537.613213	20928.593065	31.392167
537.885872	20951.119807	31.397184
538.139320	20972.265853	31.402202
538.798899	20998.004986	31.407220
539.099017	21024.470205	31.412237
539.861007	21051.052674	31.417255
540.397286	21078.795213	31.422272
541.104767	21099.914514	31.427290
541.594747	21127.809698	31.432308
542.336552	21157.118728	31.437325
542.585821	21183.851183	31.442343
543.231749	21209.959204	31.447360
543.573816	21243.280024	31.452378
544.352778	21267.844529	31.457396
544.888533	21300.939238	31.462413
545.541703	21327.987740	31.467431
545.779765	21349.964328	31.472448
546.717478	21387.697216	31.477466
546.887590	21411.175690	31.482484
547.200960	21438.770411	31.487501
547.949860	21458.000681	31.492519
548.375413	21496.862874	31.497536
549.449249	21525.614966	31.502554
549.894747	21552.633117	31.507572
550.278686	21578.852165	31.512589
550.860866	21597.249353	31.517607
551.027458	21630.130733	31.522624
551.515725	21650.804745	31.527642
552.210273	21693.163627	31.532660
552.796043	21727.293795	31.537677
553.661122	21747.706696	31.542695
553.699599	21777.215267	31.547712
554.369833	21798.448571	31.552730
555.421685	21827.577351	31.557748
555.673071	21842.620806	31.562765
556.504234	21850.205875	31.567783
556.900057	21880.081985	31.572800
557.945991	21896.675497	31.577818
558.399801	21906.038376	31.582836
558.739461	21928.821129	31.587853
559.639369	21955.395860	31.592871
559.685414	21970.199868	31.597888
560.520903	21999.773507	31.602906
560.950852	22020.058961	31.607924
561.124982	22051.581332	31.612941
561.679593	22068.037102	31.617959
561.979049	22101.037469	31.622976
562.770938	22127.509293	31.627994
563.417225	22155.179252	31.633012
563.727149	22191.861985	31.638029
564.317549	22222.156774	31.643047
564.814737	22257.375930	31.648064
565.548319	22290.687752	31.653082
565.913060	22320.266092	31.658100
566.522463	22357.515156	31.663117
567.267748	22376.209788	31.668135
567.707451	22421.965462	31.673152
568.314980	22447.777833	31.678170
569.394507	22471.797577	31.683188
569.627802	22510.647644	31.688205
570.667655	22544.038303	31.693223
570.928527	22561.128148	31.698240
571.452846	22596.488994	31.703258
571.890002	22632.160544	31.708276
572.532209	22664.842775	31.713293
573.057236	22685.954442	31.718311
573.922823	22718.380613	31.723328
573.887003	22751.801076	31.728346
574.427298	22777.485389	31.733364
575.166503	22822.101895	31.738381
576.012109	22848.275599	31.743399
576.856006	22878.519053	31.748416
577.473198	22905.183575	31.753434
578.450487	22933.649532	31.758452
578.877541	22966.226938	31.763469
579.337320	22983.873667	31.768487
579.765491	23011.869662	31.773504
580.209362	23039.288201	31.778522
581.005031	23068.844402	31.783540
581.650911	23095.100266	31.788557
582.396566	23119.811317	31.793575
582.603529	23156.347664	31.798592
583.196519	23177.727252	31.803610
583.963003	23210.239260	31.808628
584.497152	23236.929873	31.813645
585.235481	23269.250495	31.818663
585.462963	23296.008174	31.823680
586.269977	23327.964261	31.828698
587.005263	23349.258557	31.833716
587.746454	23380.371951	31.838733
588.083670	23411.573939	31.843751
588.528316	23437.697474	31.848768
589.180411	23469.128282	31.853786
589.567179	23488.998617	31.858804
589.968930	23529.208199	31.863821
590.670134	23553.408577	31.868839
591.321623	23592.915656	31.873856
591.831225	23624.432218	31.878874
592.602603	23650.865060	31.883892
593.078315	23680.168957	31.888909
593.679449	23709.946158	31.893927
593.748506	23738.467045	31.898944
594.292327	23764.923038	31.903962
595.197847	23776.977597	31.908980
595.389674	23815.988371	31.913997
596.177104	23832.396508	31.919015
596.717018	23869.033680	31.924032
597.501478	23900.810961	31.929050
598.598034	23933.708495	31.934068
598.867891	23963.733858	31.939085
599.283723	23993.376201	31.944103
599.948543	24026.834415	31.949120
600.826044	24052.593955	31.954138
601.255208	24083.839470	31.959156
601.588058	24117.830102	31.964173
602.212302	24146.397329	31.969191
603.421189	24178.399276	31.974208
604.128713	24203.117648	31.979226
604.725826	24222.595565	31.984244
604.915535	24256.229685	31.989261
605.836702	24284.617899	31.994279
606.549943	24323.181474	31.999296
606.678758	24346.947945	32.004314
607.264142	24376.627498	32.009332
608.018922	24409.623582	32.014349
608.569859	24440.983293	32.019367
608.595316	24479.863431	32.024384
609.427273	24522.503850	32.029402
610.456039	24552.822014	32.034420
610.667497	24591.995535	32.039437
611.510643	24626.191493	32.044455
612.265975	24657.690162	32.049472
612.984190	24692.992768	32.054490
613.619323	24710.992743	32.059508
614.026641	24758.800087	32.064525
614.721788	24788.014368	32.069543
615.384972	24822.927685	32.074560
615.886408	24862.132156	32.079578
617.091327	24890.040738	32.084596
617.352120	24932.468140	32.089613
618.150808	24965.293954	32.094631
618.504131	24996.723403	32.099648
619.453824	25024.071774	32.104666
619.964640	25062.308254	32.109684
620.562231	25097.845335	32.114701
621.457258	25122.573399	32.119719
621.919933	25151.123129	32.124736
622.099512	25185.999062	32.129754
623.491380	25206.200317	32.134772
623.787542	25242.353640	32.139789
624.564920	25268.825607	32.144807
625.248631	25292.942359	32.149824
625.661159	25329.741192	32.154842
626.537205	25353.726780	32.159860
626.714520	25398.279052	32.164877
627.682067	25424.045221	32.169895
628.299532	25451.142855	32.174912
628.808183	25478.984350	32.179930
629.332570	25503.189506	32.184948
629.960137	25540.498554	32.189965
630.500975	25571.419227	32.194983
631.315680	25593.733624	32.200000
631.458849	25628.439070	32.205018
632.786993	25654.395538	32.210036
633.000834	25698.279165	32.215053
633.877282	25725.595727	32.220071
634.450763	25753.345289	32.225088
635.008139	25781.192211	32.230106
635.502541	25799.455363	32.235124
636.361182	25833.505598	32.240141
636.881538	25857.680213	32.245159
637.142629	25884.366567	32.250176
637.836255	25922.790933	32.255194
638.280645	25941.744605	32.260212
638.824078	25981.867401	32.265229
639.329636	26013.811799	32.270247
640.377178	26047.371451	32.275264
640.880095	26089.959295	32.280282
641.521877	26116.902338	32.285300
642.076375	26149.047847	32.290317
642.573110	26181.954540	32.295335
643.403993	26224.048900	32.300352
644.063389	26262.245431	32.305370
644.881923	26295.221994	32.310388
644.994465	26334.673522	32.315405
646.034812	26371.338015	32.320423
646.729217	26402.488718	32.325440
647.179856	26437.678294	32.330458
648.387673	26483.746414	32.335476
648.806065	26513.632243	32.340493
649.454077	26541.232175	32.345511
650.256188	26577.548823	32.350528
650.887482	26612.470244	32.355546
651.662545	26641.870632	32.360564
652.496886	26670.920489	32.365581
653.065768	26717.620103	32.370599
653.778683	26737.499465	32.375616
654.151778	26777.915969	32.380634
655.215855	26809.622472	32.385652
655.788119	26844.648342	32.390669
656.722263	26870.920901	32.395687
657.107510	26903.536536	32.400704
657.497329	26938.572181	32.405722
658.468255	26963.891056	32.410740
658.669889	26987.282660	32.415757
659.793932	27035.299173	32.420775
660.276335	27069.126003	32.425792
660.850816	27100.606261	32.430810
661.638940	27140.370699	32.435828
662.331020	27177.571546	32.440845
663.236369	27207.963614	32.445863
664.108611	27240.977554	32.450880
664.135216	27281.228110	32.455898
665.092799	27300.109009	32.460916
665.712579	27338.244253	32.465933
666.581727	27374.469668	32.470951
667.424009	27404.688616	32.475968
667.738631	27437.474182	32.480986
668.577590	27465.140279	32.486004
669.298279	27487.578948	32.491021
669.810435	27521.054247	32.496039
670.459367	27549.742534	32.501056
670.814494	27588.046103	32.506074
671.458304	27622.916743	32.511092
672.212998	27657.460372	32.516109
673.114503	27692.638403	32.521127
673.747540	27723.370956	32.526144
674.108923	27764.593967	32.531162
674.819107	27794.164205	32.536180
675.467320	27836.960507	32.541197
676.436296	27872.577045	32.546215
677.329813	27908.135936	32.551232
677.660941	27942.424032	32.556250
678.437080	27966.466303	32.561268
679.096452	28000.033106	32.566285
679.688930	28039.754099	32.571303
680.349929	28060.439293	32.576320
681.040956	28094.317326	32.581338
681.682579	28127.849196	32.586356
682.053483	28149.635462	32.591373
682.843936	28177.638803	32.596391
684.095088	28218.236698	32.601408
684.216668	28251.445688	32.606426
684.871237	28267.246197	32.611444
685.747733	28298.592526	32.616461
686.390629	28334.109241	32.621479
687.381103	28368.389608	32.626496
687.604620	28402.050615	32.631514
688.421070	28429.721552	32.636532
688.776170	28467.293571	32.641549
689.192352	28503.067312	32.646567
690.272411	28531.474562	32.651584
690.742589	28587.340113	32.656602
691.392641	28616.718698	32.661620
692.107151	28657.685947	32.666637
693.089282	28703.358319	32.671655
693.745056	28740.156856	32.676672
694.482271	28789.919444	32.681690
695.407686	28810.475500	32.686708
696.098323	28861.737284	32.691725
696.524011	28894.166470	32.696743
697.325475	28928.755499	32.701760
698.136717	28974.853458	32.706778
698.749803	29002.607588	32.711796
699.651622	29053.476487	32.716813
700.261923	29084.025025	32.721831
701.116305	29119.048556	32.726848
701.633911	29157.222168	32.731866
702.524419	29194.755923	32.736884
703.289078	29229.325940	32.741901
704.012482	29271.658363	32.746919
705.090874	29294.788891	32.751936
705.696758	29327.139975	32.756954
706.101357	29357.240735	32.761972
706.769294	29398.292613	32.766989
707.594346	29438.485588	32.772007
708.586405	29467.464178	32.777024
708.834987	29509.308875	32.782042
709.599175	29541.016039	32.787060
710.701625	29575.426284	32.792077
711.257468	29618.145966	32.797095
712.062912	29648.114847	32.802112
712.823085	29683.166740	32.807130
713.289122	29721.083989	32.812148
714.245184	29752.287346	32.817165
714.887275	29786.182170	32.822183
715.933726	29825.980926	32.827200
716.555931	29854.891562	32.832218
716.966963	29885.453536	32.837236
717.785594	29911.160245	32.842253
718.481324	29954.117889	32.847271
719.651631	29982.513028	32.852288
720.008310	30017.476969	32.857306
720.778302	30047.091675	32.862324
721.500236	30085.645898	32.867341
722.092166	30123.518889	32.872359
722.925076	30153.914056	32.877376
723.527271	30200.186574	32.882394
724.073961	30228.300434	32.887412
725.106445	30266.787400	32.892429
725.266349	30304.165782	32.897447
726.316595	30336.701723	32.902464
726.931507	30378.554031	32.907482
727.436010	30415.872329	32.912500
728.778289	30450.467734	32.917517
728.842216	30480.155705	32.922535
729.376686	30502.538355	32.927552
730.197959	30545.559752	32.932570
730.599887	30576.610926	32.937588
731.475635	30622.519161	32.942605
731.777956	30654.635408	32.947623
732.560115	30687.005279	32.952640
733.514033	30739.185055	32.957658
734.707258	30774.632460	32.962676
735.188622	30813.282610	32.967693
735.760715	30858.783776	32.972711
736.339030	30896.129312	32.977728
737.026173	30950.614502	32.982746
737.608013	30992.700809	32.987764
738.887916	31035.436473	32.992781
739.517463	31075.954055	32.997799
740.378407	31113.205151	33.002816
741.074108	31151.676972	33.007834
741.921749	31197.338023	33.012852
742.750757	31243.855511	33.017869
743.382507	31283.203654	33.022887
744.202062	31310.719954	33.027904
744.971121	31362.323375	33.032922
745.525208	31408.119364	33.037940
746.461346	31446.933382	33.042957
747.123756	31488.831074	33.047975
748.059013	31529.851657	33.052992
749.022811	31577.429799	33.058010
749.752234	31612.578292	33.063028
750.734334	31648.850477	33.068045
751.171087	31705.892917	33.073063
751.776822	31730.914556	33.078080
752.910856	31772.922297	33.083098
753.581471	31811.740649	33.088116
754.582051	31848.155690	33.093133
755.110930	31892.148659	33.098151
756.380877	31922.041786	33.103168
757.247926	31965.021035	33.108186
758.030105	31997.133758	33.113204
758.587727	32030.369055	33.118221
759.029518	32065.803589	33.123239
759.888769	32096.551516	33.128256
760.405346	32136.469316	33.133274
761.491553	32171.607138	33.138292
762.501616	32211.637462	33.143309
762.946527	32250.706923	33.148327
763.725734	32278.527959	33.153344
764.622127	32322.451642	33.158362
765.162382	32358.320114	33.163380
766.283401	32397.378804	33.168397
766.989002	32441.098702	33.173415
767.312520	32467.575226	33.178432
768.297213	32513.413692	33.183450
769.191505	32552.154146	33.188468
769.849869	32586.879196	33.193485
770.713444	32629.860363	33.198503
771.522455	32661.988878	33.203520
772.281858	32698.847790	33.208538
772.897876	32736.437293	33.213556
773.567847	32768.543490	33.218573
774.544575	32810.021620	33.223591
775.238378	32852.543030	33.228608
776.113662	32887.797281	33.233626
776.957171	32925.756117	33.238644
777.834588	32966.832850	33.243661
778.015695	33018.899134	33.248679
779.236314	33047.473956	33.253696
779.708794	33067.485627	33.258714
780.510615	33104.857032	33.263732
781.513267	33133.984525	33.268749
781.923743	33174.091625	33.273767
782.636184	33199.319599	33.278784
783.373870	33242.631530	33.283802
784.332122	33265.665213	33.288820
784.693209	33305.135429	33.293837
785.221290	33347.253885	33.298855
786.504663	33384.126791	33.303872
787.033378	33429.058721	33.308890
787.651014	33471.865176	33.313908
788.920298	33506.091462	33.318925
789.080123	33557.460640	33.323943
790.248540	33590.722900	33.328960
791.270296	33651.820174	33.333978
791.729996	33685.022862	33.338996
792.620299	33719.321488	33.344013
793.514414	33771.075670	33.349031
794.532173	33813.630495	33.354048
795.325326	33853.678970	33.359066
796.347616	33898.547260	33.364084
797.325837	33932.560604	33.369101
797.787039	33972.003753	33.374119
798.676085	34006.088082	33.379136
799.388344	34055.165432	33.384154
799.856558	34091.952270	33.389172
801.267395	34139.396707	33.394189
801.631579	34184.096795	33.399207
802.726066	34226.937602	33.404224
803.280889	34267.321344	33.409242
804.247977	34300.957677	33.414260
804.981298	34345.884819	33.419277
805.817694	34395.544167	33.424295
806.702189	34435.592093	33.429312
807.477703	34484.875507	33.434330
808.275328	34527.017345	33.439348
809.258394	34568.181836	33.444365
810.228805	34618.807054	33.449383
811.077587	34646.525509	33.454400
811.785769	34694.637623	33.459418
812.669575	34728.831431	33.464436
813.419628	34765.651185	33.469453
814.689847	34798.994263	33.474471
815.960911	34837.521879	33.479488
816.854875	34870.298041	33.484506
817.145387	34911.527392	33.489524
818.184538	34937.913940	33.494541
818.476533	34972.750894	33.499559
819.708544	35006.707269	33.504576
820.378036	35050.179029	33.509594
821.089156	35098.057660	33.514612
822.180156	35131.378748	33.519629
822.964500	35161.415791	33.524647
823.454666	35205.428097	33.529664
824.357953	35239.132827	33.534682
824.570523	35280.242322	33.539700
825.802177	35317.563003	33.544717
826.405876	35362.354536	33.549735
826.878250	35415.177811	33.554752
828.259433	35453.531239	33.559770
828.989537	35505.081417	33.564788
829.981519	35542.560161	33.569805
830.351654	35585.548772	33.574823
831.133905	35625.197654	33.579840
832.299879	35666.651794	33.584858
833.031925	35719.707053	33.589876
834.215589	35765.028272	33.594893
834.731835	35795.734173	33.599911
835.086342	35831.631336	33.604928
836.096748	35865.977883	33.609946
836.565941	35913.636998	33.614964
837.789309	35950.112809	33.619981
838.352377	35992.863373	33.624999
839.398792	36036.461503	33.630016
840.244512	36078.497735	33.635034
840.576670	36120.532268	33.640052
841.524656	36167.674363	33.645069
842.467349	36208.051660	33.650087
843.316508	36263.170242	33.655104
844.144349	36299.417726	33.660122
845.152711	36343.091999	33.665140
845.943748	36387.799453	33.670157
846.837488	36437.385059	33.675175
847.772985	36483.846908	33.680192
848.578928	36527.060046	33.685210
849.427744	36583.349304	33.690228
850.441505	36619.498666	33.695245
851.296279	36677.608331	33.700263
851.810715	36727.032692	33.705280
853.072986	36758.350341	33.710298
853.954486	36815.336978	33.715316
854.662193	36866.223694	33.720333
855.648883	36905.767074	33.725351
856.398289	36955.370163	33.730368
857.681276	37001.051545	33.735386
858.342748	37051.402135	33.740404
859.214245	37092.430918	33.745421
860.334525	37145.017918	33.750439
861.006346	37183.479230	33.755456
862.222296	37229.317036	33.760474
862.977559	37273.260492	33.765492
863.880103	37313.974992	33.770509
864.779755	37352.337699	33.775527
865.346863	37406.466354	33.780544
866.695619	37439.706446	33.785562
867.252068	37502.089150	33.790580
868.096146	37533.296366	33.795597
869.343215	37576.796673	33.800615
870.106974	37619.240836	33.805632
870.833607	37662.626781	33.810650
871.900619	37714.483668	33.815668
872.728561	37753.136559	33.820685
873.565595	37799.553454	33.825703
874.521435	37836.251453	33.830720
875.304130	37880.097005	33.835738
876.083134	37916.968275	33.840756
877.024277	37963.362899	33.845773
877.865754	38008.862625	33.850791
878.691851	38066.265982	33.855808
880.049182	38099.910474	33.860826
880.806990	38148.553814	33.865844
881.487435	38169.271296	33.870861
882.437386	38224.259002	33.875879
883.139466	38272.038677	33.880896
884.318513	38314.570958	33.885914
884.821147	38354.983280	33.890932
885.333420	38398.631933	33.895949
886.776664	38442.994932	33.900967
887.393192	38498.756459	33.905984
888.552878	38545.118120	33.911002
889.291033	38590.470837	33.916020
890.238677	38621.638127	33.921037
891.291972	38679.279468	33.926055
892.016689	38721.301902	33.931072
892.858060	38763.932214	33.936090
893.597320	38800.893435	33.941108
894.651469	38838.640165	33.946125
895.472449	38871.263173	33.951143
896.325449	38907.175971	33.956160
897.096600	38936.771405	33.961178
898.289265	38980.542360	33.966196
898.772393	39015.874539	33.971213
899.813551	39053.288512	33.976231
900.725596	39103.870284	33.981248
901.951748	39117.806157	33.986266
902.745970	39158.553766	33.991284
903.559055	39187.523229	33.996301
904.423183	39219.906022	34.001319
905.539225	39263.923539	34.006336
906.360307	39294.934550	34.011354
907.248581	39345.735628	34.016372
908.282476	39380.615370	34.021389
909.183322	39426.658989	34.026407
910.135551	39478.443242	34.031424
910.970665	39506.733009	34.036442
911.654306	39553.221973	34.041460
913.022394	39593.052090	34.046477
913.824117	39638.188361	34.051495
914.079465	39689.803977	34.056512
915.172283	39736.640334	34.061530
916.116169	39776.866067	34.066548
917.086576	39830.102873	34.071565
917.740631	39878.557662	34.076583
918.816978	39937.147380	34.081600
920.091300	39981.274383	34.086618
920.758560	40027.785902	34.091636
921.815505	40081.686468	34.096653
922.851798	40126.508760	34.101671
923.614356	40166.428423	34.106688
924.673068	40208.249667	34.111706
925.653123	40270.156640	34.116724
925.996102	40323.454951	34.121741
927.336539	40373.333856	34.126759
927.912091	40430.472830	34.131776
929.027063	40471.115768	34.136794
930.280051	40526.953619	34.141812
931.345162	40580.069920	34.146829
932.380495	40622.414224	34.151847
933.412469	40671.273287	34.156864
934.314998	40708.831995	34.161882
935.116797	40759.143968	34.166900
935.870902	40802.987280	34.171917
937.433067	40849.170699	34.176935
938.065331	40900.818711	34.181952
939.109547	40943.699830	34.186970
939.909960	40995.536771	34.191988
940.721128	41031.662027	34.197005
941.829754	41074.210767	34.202023
942.693257	41130.281914	34.207040
943.925207	41168.757492	34.212058
944.734804	41215.565489	34.217076
945.577961	41263.886234	34.222093
946.421973	41301.069325	34.227111
946.917922	41362.049586	34.232128
948.202303	41399.518072	34.237146
949.324669	41448.345751	34.242164
950.184020	41504.639870	34.247181
951.514299	41554.156241	34.252199
951.953422	41592.630212	34.257216
953.330562	41638.528042	34.262234
953.942078	41686.525482	34.267252
954.888711	41735.798749	34.272269
956.111641	41777.888233	34.277287
956.968850	41819.440536	34.282304
957.685649	41857.858845	34.287322
958.641749	41894.456167	34.292340
959.574481	41932.328490	34.297357
960.139723	41974.685775	34.302375
961.213335	42015.211573	34.307392
961.884673	42056.002825	34.312410
962.890386	42104.945106	34.317428
963.937809	42150.478198	34.322445
964.935208	42197.195640	34.327463
965.707124	42246.408863	34.332480
966.998591	42296.337784	34.337498
967.781931	42340.951236	34.342516
968.690326	42387.050529	34.347533
970.033634	42427.711959	34.352551
970.578891	42483.292453	34.357568
971.952465	42538.091923	34.362586
973.173565	42590.923037	34.367604
973.899208	42636.014170	34.372621
975.182143	42686.388063	34.377639
975.910672	42725.293078	34.382656
976.980942	42778.255784	34.387674
977.830132	42828.742190	34.392692
978.401657	42882.883794	34.397709
980.020407	42933.066521	34.402727
980.661094	42984.243737	34.407744
981.920925	43038.018623	34.412762
983.087779	43082.782259	34.417780
983.939495	43135.780044	34.422797
984.783957	43179.696186	34.427815
985.996598	43238.241781	34.432832
986.885917	43275.262995	34.437850
988.191842	43328.955472	34.442868
988.710485	43386.174303	34.447885
989.560605	43435.978831	34.452903
990.524268	43497.669776	34.457920
991.909386	43538.250812	34.462938
992.872005	43596.045846	34.467956
993.847390	43648.911642	34.472973
995.082709	43705.551016	34.477991
995.990682	43754.044192	34.483008
997.042516	43813.002331	34.488026
998.004949	43855.990499	34.493044
999.137414	43915.670025	34.498061
1000.608793	43956.541940	34.503079
1001.265388	44008.225062	34.508096
1002.479177	44052.673372	34.513114
1003.352767	44106.074879	34.518132
1004.253078	44154.525854	34.523149
1005.628055	44196.279888	34.528167
1006.494581	44235.950309	34.533184
1007.427372	44289.406243	34.538202
1008.493297	44329.747737	34.543220
1009.264001	44393.754881	34.548237
1010.354541	44428.867851	34.553255
1011.313576	44485.653684	34.558272
1012.466823	44535.463825	34.563290
1013.351014	44581.059116	34.568308
1014.314196	44635.586465	34.573325
1015.349122	44680.936966	34.578343
1016.022812	44742.727377	34.583360
1017.275478	44776.974210	34.588378
1018.571317	44821.006375	34.593396
1019.388112	44872.723353	34.598413
1020.666729	44923.337065	34.603431
1021.782712	44980.852339	34.608448
1022.782168	45016.125988	34.613466
1023.637977	45061.511634	34.618484
1024.346305	45096.350240	34.623501
1025.251193	45134.131202	34.628519
1026.143417	45192.099551	34.633536
1027.041852	45228.211695	34.638554
1028.253636	45275.711765	34.643572
1028.946113	45315.253217	34.648589
1029.599127	45366.358081	34.653607
1031.049412	45421.348776	34.658624
1031.848066	45470.836981	34.663642
1032.944396	45517.583895	34.668660
1033.848581	45570.155441	34.673677
1035.300681	45628.448440	34.678695
1035.758839	45677.522300	34.683712
1037.039973	45733.191809	34.688730
1038.218826	45779.736575	34.693748
1038.819413	45830.622975	34.698765
1040.312819	45902.504567	34.703783
1041.442853	45961.759791	34.708800
1042.398768	46010.939900	34.713818
1043.826908	46053.770834	34.718836
1044.564943	46114.745235	34.723853
1045.904789	46157.817927	34.728871
1046.941527	46213.191616	34.733888
1048.017108	46280.154950	34.738906
1048.961504	46317.248515	34.743924
1050.046896	46382.635436	34.748941
1051.210931	46431.081690	34.753959
1052.222683	46492.710128	34.758976
1053.671025	46540.346650	34.763994
1055.115819	46580.506373	34.769012
1056.155563	46639.410608	34.774029
1057.414512	46681.358270	34.779047
1058.461858	46724.224800	34.784064
1059.333169	46772.831492	34.789082
1060.645190	46814.682528	34.794100
1061.271913	46862.796309	34.799117
1062.236251	46910.351239	34.804135
1063.281110	46956.957383	34.809152
1064.784166	47006.060333	34.814170
1065.865826	47041.324304	34.819188
1066.754382	47094.566118	34.824205
1068.162744	47141.691422	34.829223
1069.009045	47177.745280	34.834240
1069.954024	47231.048171	34.839258
1071.129640	47273.743835	34.844276
1072.116141	47333.297174	34.849293
1073.118774	47368.751168	34.854311
1074.412376	47419.728772	34.859328
1075.299625	47466.221466	34.864346
1076.806885	47519.981073	34.869364
1077.509923	47569.659676	34.874381
1078.690198	47618.580420	34.879399
1079.729450	47664.132396	34.884416
1080.635721	47716.841484	34.889434
1082.139436	47751.591313	34.894452
1082.909023	47817.582235	34.899469
1084.026973	47856.871748	34.904487
1084.941232	47910.813696	34.909504
1085.828940	47954.770406	34.914522
1087.236704	48009.381850	34.919540
1088.536614	48056.089514	34.924557
1089.929074	48110.874415	34.929575
1090.619320	48151.465074	34.934592
1091.408653	48197.348271	34.939610
1092.490826	48243.046529	34.944628
1093.408134	48290.972339	34.949645
1094.220414	48356.660794	34.954663
1095.342052	48399.866836	34.959680
1096.532309	48455.228314	34.964698
1097.772058	48496.612960	34.969716
1098.347103	48546.168226	34.974733
1099.633071	48574.550843	34.979751
1100.832948	48629.613886	34.984768
1101.610508	48684.534401	34.989786
1102.735853	48728.569283	34.994804
1103.820166	48791.578169	34.999821
1104.815578	48837.512640	35.004839
1106.170462	48882.688657	35.009856
1107.409185	48938.271485	35.014874
1108.592727	48987.036500	35.019892
1109.251933	49046.487404	35.024909
1110.274532	49097.346711	35.029927
1111.393508	49145.635010	35.034944
1112.231941	49206.393228	35.039962
1113.967885	49262.278611	35.044980
1115.183735	49320.776303	35.049997
1116.503032	49372.019998	35.055015
1117.447437	49433.812492	35.060032
1118.585433	49492.227908	35.065050
1120.133385	49537.406631	35.070068
1120.951649	49598.656222	35.075085
1122.283618	49636.226011	35.080103
1123.783960	49694.256213	35.085120
1124.757947	49750.192486	35.090138
1125.660367	49787.848755	35.095156
1126.995132	49856.813030	35.100173
1128.321879	49904.051754	35.105191
1129.281779	49954.720319	35.110208
1130.636232	50014.843116	35.115226
1131.688414	50052.273908	35.120244
1132.478509	50110.283491	35.125261
1133.499401	50148.491242	35.130279
1135.146258	50206.904740	35.135296
1135.574996	50265.509091	35.140314
1137.019395	50327.010591	35.145332
1138.045382	50376.543510	35.150349
1139.354874	50430.537096	35.155367
1141.013434	50488.399014	35.160384
1141.944833	50549.829572	35.165402
1143.143136	50594.831016	35.170420
1144.305144	50646.317313	35.175437
1145.380580	50694.495475	35.180455
1146.703357	50752.075283	35.185472
1148.187396	50808.313915	35.190490
1149.519525	50854.098480	35.195508
1150.550564	50897.525900	35.200525
1151.937186	50935.260102	35.205543
1152.970558	50972.328355	35.210560
1154.164554	51029.948001	35.215578
1155.749409	51060.716619	35.220596
1157.117604	51087.286200	35.225613
1158.048222	51136.266224	35.230631
1159.531217	51158.698803	35.235648
1160.071958	51217.553787	35.240666
1161.269156	51255.545956	35.245684
1162.333943	51301.164461	35.250701
1163.015507	51342.040539	35.255719
1164.381252	51388.643469	35.260736
1165.245022	51447.290280	35.265754
1166.206607	51487.230606	35.270772
1167.343011	51543.829175	35.275789
1168.602948	51589.120305	35.280807
1169.687556	51647.138265	35.285824
1170.445770	51705.245434	35.290842
1171.697729	51763.098279	35.295860
1172.878562	51817.216495	35.300877
1174.180911	51860.204617	35.305895
1174.925395	51907.589230	35.310912
1175.930001	51962.501010	35.315930
1177.442418	52004.089753	35.320948
1178.572208	52054.723681	35.325965
1179.372253	52107.826494	35.330983
1180.582526	52158.555618	35.336000
1181.810188	52209.307441	35.341018
1183.118089	52258.920488	35.346036
1184.000725	52323.381686	35.351053
1185.032830	52372.348435	35.356071
1186.447803	52432.892013	35.361088
1187.547575	52506.735367	35.366106
1188.935115	52550.464432	35.371124
1190.230238	52617.570145	35.376141
1191.278282	52667.794245	35.381159
1192.760222	52717.324075	35.386176
1193.440293	52787.171580	35.391194
1195.034896	52839.455614	35.396212
1196.413037	52890.495429	35.401229
1197.912353	52947.869552	35.406247
1199.300032	53009.507293	35.411264
1200.227085	53067.743298	35.416282
1201.706152	53121.438188	35.421300
1202.664505	53174.651534	35.426317
1203.841655	53225.780500	35.431335
1205.196159	53292.435902	35.436352
1206.353116	53358.641495	35.441370
1207.604299	53404.342524	35.446388
1208.871924	53457.976369	35.451405
1210.086974	53526.154003	35.456423
1211.536242	53569.160253	35.461440
1212.566593	53634.386618	35.466458
1214.046068	53683.159521	35.471476
1215.218905	53731.455300	35.476493
1216.615980	53780.994346	35.481511
1217.949631	53842.718679	35.486528
1219.272918	53895.984113	35.491546
1220.596373	53936.903474	35.496564
1221.742928	53987.589598	35.501581
1222.786085	54041.487732	35.506599
1224.418760	54096.717539	35.511616
1225.197717	54148.568985	35.516634
1226.464337	54198.002773	35.521652
1228.012003	54256.220513	35.526669
1228.977577	54306.423072	35.531687
1230.587495	54343.697543	35.536704
1231.569932	54405.301146	35.541722
1232.632392	54448.622695	35.546740
1234.113102	54502.105334	35.551757
1235.145648	54560.606974	35.556775
1236.394777	54616.802993	35.561792
1237.652577	54667.700987	35.566810
1239.012516	54713.653333	35.571828
1240.525900	54765.891104	35.576845
1241.352965	54822.609327	35.581863
1242.839589	54868.263695	35.586880
1243.961556	54920.278307	35.591898
1245.555380	54967.650064	35.596916
1246.771854	55014.973406	35.601933
1247.700960	55060.114224	35.606951
1249.075699	55104.533538	35.611968
1250.534847	55161.438405	35.616986
1251.295807	55215.560599	35.622004
1252.289603	55269.266758	35.627021
1253.534164	55316.776162	35.632039
1255.104599	55366.835663	35.637056
1256.353219	55418.723961	35.642074
1257.778637	55458.997159	35.647092
1258.947227	55499.563773	35.652109
1259.767264	55543.001225	35.657127
1261.138519	55574.796516	35.662144
1262.289078	55626.548736	35.667162
1263.306437	55670.189689	35.672180
1264.411462	55711.646290	35.677197
1265.247369	55769.789332	35.682215
1267.019308	55811.426495	35.687232
1268.145329	55874.517662	35.692250
1269.288525	55932.916774	35.697268
1270.584252	55980.995410	35.702285
1271.311815	56038.915581	35.707303
1272.673563	56092.034395	35.712320
1274.446736	56154.968041	35.717338
1275.670115	56216.772804	35.722356
1277.047898	56275.262609	35.727373
1278.392340	56341.162427	35.732391
1280.020584	56383.848351	35.737408
1281.092093	56444.405396	35.742426
1282.511634	56498.085661	35.747444
1283.687374	56554.297767	35.752461
1284.701990	56616.110931	35.757479
1286.537648	56663.859602	35.762496
1287.857957	56725.739116	35.767514
1288.980282	56773.694607	35.772532
1290.430437	56841.882972	35.777549
1291.850834	56897.855065	35.782567
1293.244707	56948.027818	35.787584
1294.456395	57010.678216	35.792602
1295.457810	57059.045601	35.797620
1297.110332	57116.197028	35.802637
1298.208797	57184.479399	35.807655
1299.637675	57239.931988	35.812672
1301.199670	57303.319441	35.817690
1302.551092	57356.885722	35.822708
1303.934687	57415.307793	35.827725
1304.870926	57474.667117	35.832743
1306.401883	57524.585447	35.837760
1307.673279	57577.133109	35.842778
1308.818920	57636.270181	35.847796
1310.613638	57694.160222	35.852813
1311.673751	57747.342598	35.857831
1312.418243	57807.815043	35.862848
1314.264893	57868.051818	35.867866
1315.601075	57927.786368	35.872884
1317.143184	57980.495071	35.877901
1318.406226	58035.709636	35.882919
1320.230959	58085.317321	35.887936
1321.575731	58143.424453	35.892954
1322.659779	58195.268604	35.897972
1324.007656	58244.622143	35.902989
1325.160787	58316.044817	35.908007
1326.416848	58349.228976	35.913024
1328.192013	58408.301049	35.918042
1329.492930	58456.244609	35.923060
1330.802448	58508.060469	35.928077
1331.891405	58566.949200	35.933095
1333.253186	58623.434515	35.938112
1334.471644	58676.486558	35.943130
1335.482862	58717.266828	35.948148
1337.150009	58771.634980	35.953165
1338.355856	58825.031111	35.958183
1339.962723	58879.668449	35.963200
1341.111509	58930.320444	35.968218
1342.126033	58996.361484	35.973236
1343.788981	59040.762004	35.978253
1345.188663	59092.527029	35.983271
1346.551308	59125.980402	35.988288
1347.687148	59172.944838	35.993306
1348.795940	59215.565221	35.998324
1350.198119	59254.240765	36.003341
1350.948864	59305.519181	36.008359
1352.565739	59342.496590	36.013376
1353.749488	59403.746102	36.018394
1354.984451	59464.019325	36.023412
1356.270706	59507.688472	36.028429
1357.576696	59572.508154	36.033447
1358.880324	59625.308421	36.038464
1360.477374	59680.145323	36.043482
1361.487916	59746.189028	36.048500
1363.131993	59809.747457	36.053517
1364.313220	59867.574181	36.058535
1365.868467	59919.278644	36.063552
1367.296546	59977.326506	36.068570
1368.787082	60042.441369	36.073588
1370.134828	60105.160794	36.078605
1371.306990	60164.869578	36.083623
1372.941282	60225.379680	36.088640
1374.188995	60290.058481	36.093658
1375.823767	60350.948608	36.098676
1377.338933	60412.072823	36.103693
1378.496289	60477.836006	36.108711
1380.247221	60539.898432	36.113728
1381.617411	60588.411386	36.118746
1383.284473	60648.467989	36.123764
1384.885771	60699.939026	36.128781
1386.096428	60760.643367	36.133799
1387.599732	60809.541039	36.138816
1388.883897	60861.688722	36.143834
1390.385586	60923.316393	36.148852
1392.057988	60980.581465	36.153869
1393.318157	61037.360490	36.158887
1394.419784	61085.802531	36.163904
1396.022702	61149.263285	36.168922
1397.205228	61207.903224	36.173940
1399.174159	61262.926021	36.178957
1400.402521	61317.203975	36.183975
1401.917429	61371.487836	36.188992
1403.356921	61430.024783	36.194010
1404.586561	61473.630355	36.199028
1406.059628	61527.826162	36.204045
1407.316063	61593.114732	36.209063
1408.787287	61654.046365	36.214080
1410.110438	61715.779937	36.219098
1411.428097	61770.456376	36.224116
1412.844649	61828.149618	36.229133
1414.088500	61883.439230	36.234151
1415.846098	61940.978070	36.239168
1417.177170	61994.703375	36.244186
1418.316408	62058.916396	36.249204
1420.295617	62109.717210	36.254221
1421.470497	62181.793489	36.259239
1422.838313	62246.382687	36.264256
1424.209960	62306.768126	36.269274
1425.521138	62372.018540	36.274292
1427.313796	62416.829046	36.279309
1428.764996	62476.404825	36.284327
1429.834863	62535.882177	36.289344
1431.369325	62591.931846	36.294362
1433.054937	62647.128700	36.299380
1434.617373	62698.451755	36.304397
1435.755305	62769.351743	36.309415
1437.428187	62821.702287	36.314432
1438.962575	62880.170851	36.319450
1440.244798	62931.291362	36.324468
1441.776376	62975.213170	36.329485
1442.700811	63002.334004	36.334503
1444.019928	63052.385468	36.339520
1445.196050	63093.887898	36.344538
1446.675603	63148.624347	36.349556
1448.227388	63206.844070	36.354573
1449.254415	63256.751749	36.359591
1450.936661	63311.247923	36.364608
1452.076307	63363.860335	36.369626
1453.514993	63429.049262	36.374644
1454.693668	63484.909749	36.379661
1456.520906	63541.510820	36.384679
1457.993238	63597.097693	36.389696
1459.535475	63668.145875	36.394714
1460.527191	63734.608390	36.399732
1462.229131	63792.913605	36.404749
1463.835149	63856.880961	36.409767
1465.496811	63925.271279	36.414784
1466.700534	63983.218103	36.419802
1468.462760	64056.100526	36.424820
1470.436792	64107.944504	36.429837
1471.556847	64182.763735	36.434855
1473.114150	64237.655012	36.439872
1475.236402	64297.218759	36.444890
1476.587280	64355.580240	36.449908
1478.372874	64409.429561	36.454925
1479.588530	64467.755493	36.459943
1481.033570	64531.395247	36.464960
1482.700140	64581.230800	36.469978
1483.883334	64643.031549	36.474996
1485.485473	64695.327475	36.480013
1487.070957	64768.917050	36.485031
1488.282713	64834.290779	36.490048
1490.218939	64883.863146	36.495066
1491.588282	64961.418646	36.500084
1493.196751	65004.192427	36.505101
1494.778243	65068.255357	36.510119
1496.133457	65132.841358	36.515136
1497.875058	65185.996493	36.520154
1498.934561	65253.630003	36.525172
1500.390343	65301.663976	36.530189
1501.909156	65371.625387	36.535207
1503.367351	65435.955467	36.540224
1505.198134	65497.986176	36.545242
1506.191621	65567.827761	36.550260
1507.612460	65631.227177	36.555277
1509.035935	65701.850205	36.560295
1510.855216	65770.645079	36.565312
1512.583903	65835.693584	36.570330
1513.952453	65899.665337	36.575348
1515.724366	65968.651770	36.580365
1517.071906	66030.379553	36.585383
1518.697929	66097.394827	36.590400
1520.342552	66151.326934	36.595418
1521.684829	66227.516677	36.600436
1523.582784	66293.204655	36.605453
1524.528648	66350.937715	36.610471
1526.236101	66417.827130	36.615488
1528.022891	66471.478083	36.620506
1529.499737	66547.508436	36.625524
1531.083731	66614.898880	36.630541
1532.606993	66665.685380	36.635559
1533.978565	66743.682873	36.640576
1536.013967	66801.873240	36.645594
1537.300226	66864.695325	36.650612
1538.628047	66918.406399	36.655629
1540.137143	66977.850868	36.660647
1541.434653	67031.560594	36.665664
1543.351146	67073.460253	36.670682
1544.350497	67135.840387	36.675700
1545.813678	67187.821333	36.680717
1547.069798	67238.340547	36.685735
1548.534861	67301.224366	36.690752
1550.143862	67352.467358	36.695770
1551.175297	67423.029909	36.700788
1552.971543	67480.594447	36.705805
1554.672200	67540.060902	36.710823
1556.113762	67610.477469	36.715840
1557.663649	67677.673456	36.720858
1558.982085	67745.697304	36.725876
1560.629264	67808.528544	36.730893
1562.243614	67877.240904	36.735911
1563.928728	67950.311266	36.740928
1565.879931	68017.457998	36.745946
1566.966758	68081.529990	36.750964
1568.991909	68150.577690	36.755981
1570.471347	68220.325171	36.760999
1572.163840	68293.408021	36.766016
1573.974503	68359.526567	36.771034
1575.857514	68434.169290	36.776052
1576.969917	68484.206913	36.781069
1578.696387	68556.576027	36.786087
1580.588580	68623.701926	36.791104
1581.966873	68694.530285	36.796122
1583.870044	68755.683819	36.801140
1585.502038	68812.726188	36.806157
1587.195561	68880.998275	36.811175
1588.499813	68947.666160	36.816192
1590.675281	69010.867236	36.821210
1592.052794	69077.802600	36.826228
1593.847515	69137.872248	36.831245
1595.510331	69206.593247	36.836263
1596.925560	69264.867300	36.841280
1598.874809	69333.993385	36.846298
1600.131349	69398.124411	36.851316
1601.742332	69463.890793	36.856333
1603.703344	69521.206175	36.861351
1605.216938	69591.160987	36.866368
1606.729371	69645.387118	36.871386
1608.406862	69718.115430	36.876404
1609.958024	69784.018633	36.881421
1611.692656	69844.947846	36.886439
1613.050101	69905.834920	36.891456
1614.931927	69966.811037	36.896474
1616.476721	70033.931660	36.901492
1617.927925	70099.319401	36.906509
1619.599857	70167.003037	36.911527
1621.302895	70233.187562	36.916544
1622.440585	70298.156283	36.921562
1624.084121	70366.326138	36.926580
1626.278103	70436.752988	36.931597
1628.017710	70503.515054	36.936615
1629.677219	70568.238140	36.941632
1631.298650	70623.494101	36.946650
1632.691286	70702.507152	36.951668
1634.907864	70757.201656	36.956685
1636.060653	70828.286449	36.961703
1637.341272	70895.957237	36.966720
1638.985877	70956.212913	36.971738
1640.655220	71025.558295	36.976756
1642.372899	71086.499408	36.981773
1644.169926	71148.036166	36.986791
1645.628745	71222.708998	36.991808
1647.861344	71276.211572	36.996826
1649.187285	71342.926545	37.001844
1650.772529	71404.155094	37.006861
1652.338550	71450.479894	37.011879
1653.563585	71501.683578	37.016896
1655.161984	71552.600956	37.021914
1656.353481	71613.233027	37.026932
1658.024050	71661.910240	37.031949
1659.902193	71723.790288	37.036967
1660.943515	71786.080085	37.041984
1662.363453	71848.792059	37.047002
1663.861087	71932.630559	37.052020
1665.484005	71997.527565	37.057037
1667.476382	72073.018562	37.062055
1668.787796	72150.541504	37.067072
1670.735419	72214.007688	37.072090
1672.673955	72292.243496	37.077108
1674.147026	72376.720534	37.082125
1676.246271	72447.015646	37.087143
1678.117575	72530.670915	37.092160
1679.893202	72591.315149	37.097178
1681.138363	72661.161877	37.102196
1683.086100	72736.699762	37.107213
1684.972292	72810.942916	37.112231
1686.536425	72890.429682	37.117248
1688.524803	72960.566194	37.122266
1690.286515	73042.340352	37.127284
1691.570272	73108.319113	37.132301
1693.965702	73170.007616	37.137319
1695.275829	73254.766281	37.142336
1696.852759	73323.460891	37.147354
1698.964156	73391.464062	37.152372
1700.812099	73472.326760	37.157389
1702.598238	73535.606074	37.162407
1704.273036	73620.524161	37.167424
1705.894170	73683.196340	37.172442
1707.758042	73752.569131	37.177460
1709.127560	73824.223405	37.182477
1711.385491	73893.940216	37.187495
1712.850193	73990.570724	37.192512
1714.872399	74049.127759	37.197530
1716.815609	74120.173725	37.202548
1718.244732	74189.438363	37.207565
1720.210110	74249.372713	37.212583
1721.754801	74317.922941	37.217600
1723.733670	74398.742634	37.222618
1725.697766	74460.919644	37.227636
1727.207763	74534.783165	37.232653
1729.125065	74599.754481	37.237671
1730.763919	74673.902221	37.242688
1732.548953	74730.889203	37.247706
1734.255792	74799.605293	37.252724
1736.124236	74862.950885	37.257741
1737.804208	74942.830991	37.262759
1739.271191	75009.457130	37.267776
1740.860530	75076.000953	37.272794
1742.646320	75143.286879	37.277812
1744.668422	75213.424057	37.282829
1746.404272	75277.728735	37.287847
1747.964558	75362.011597	37.292864
1749.675982	75422.254330	37.297882
1751.702805	75490.846115	37.302900
1752.831449	75565.519514	37.307917
1755.085492	75636.254857	37.312935
1756.459929	75718.541176	37.317952
1758.080608	75789.870060	37.322970
1759.859717	75866.089237	37.327988
1761.118373	75936.233772	37.333005
1763.057171	76002.801205	37.338023
1764.815960	76093.477623	37.343040
1767.101734	76158.306381	37.348058
1768.772149	76217.341242	37.353076
1770.483657	76280.790742	37.358093
1772.467412	76320.078910	37.363111
1774.425488	76370.277866	37.368128
1775.943058	76428.450384	37.373146
1777.096659	76472.441664	37.378164
1779.094208	76548.020541	37.383181
1781.004559	76601.622308	37.388199
1782.333482	76659.001450	37.393216
1783.894469	76728.670030	37.398234
1786.015580	76804.939677	37.403252
1787.436338	76876.429394	37.408269
1789.306908	76930.924780	37.413287
1790.935375	77013.491977	37.418304
1792.659770	77103.239743	37.423322
1794.272051	77174.725609	37.428340
1796.264597	77253.334856	37.433357
1798.250219	77325.586108	37.438375
1800.080942	77416.901761	37.443392
1801.979851	77499.390107	37.448410
1803.745262	77572.347879	37.453428
1805.418475	77657.849016	37.458445
1807.454101	77736.250226	37.463463
1809.212846	77831.252287	37.468480
1810.981762	77905.515223	37.473498
1812.948517	77987.361016	37.478516
1814.960923	78064.968704	37.483533
1816.771391	78149.715139	37.488551
1818.683962	78238.373050	37.493568
1820.613429	78312.662641	37.498586
1822.777878	78402.130448	37.503604
1824.170507	78476.985894	37.508621
1826.499514	78546.754295	37.513639
1828.252846	78633.968858	37.518656
1830.029496	78709.474281	37.523674
1831.857210	78793.611914	37.528692
1833.830671	78868.491551	37.533709
1835.980506	78949.994851	37.538727
1837.918225	79022.764830	37.543744
1839.554567	79101.587153	37.548762
1841.733732	79180.565464	37.553780
1843.469693	79252.379457	37.558797
1845.321013	79330.053935	37.563815
1847.045124	79406.671683	37.568832
1848.944625	79476.813712	37.573850
1850.758671	79558.903454	37.578868
1852.975169	79636.280938	37.583885
1854.536723	79707.223907	37.588903
1856.358151	79779.824046	37.593920
1858.643082	79849.298592	37.598938
1860.584267	79928.506320	37.603956
1861.962120	79995.095253	37.608973
1863.873354	80070.494656	37.613991
1865.715029	80155.774482	37.619008
1867.767567	80221.840297	37.624026
1870.009849	80285.950845	37.629044
1871.777371	80366.669307	37.634061
1873.492771	80454.275629	37.639079
1875.373627	80514.376394	37.644096
1876.918226	80592.001052	37.649114
1879.088638	80667.754272	37.654132
1880.677414	80737.669388	37.659149
1882.753743	80818.087446	37.664167
1884.178261	80898.962482	37.669184
1886.094094	80977.226948	37.674202
1888.060588	81058.929849	37.679220
1889.549863	81132.333006	37.684237
1891.976999	81209.922639	37.689255
1893.394451	81280.499409	37.694272
1895.071865	81335.413845	37.699290
1896.979412	81395.119571	37.704308
1899.085001	81465.196363	37.709325
1900.682752	81533.857753	37.714343
1902.075746	81597.014611	37.719360
1903.993449	81673.608308	37.724378
1905.845968	81746.994245	37.729396
1907.527482	81835.294374	37.734413
1909.682576	81910.888653	37.739431
1911.572703	81995.368302	37.744448
1912.873031	82072.034352	37.749466
1914.830826	82158.303057	37.754484
1916.369333	82256.053468	37.759501
1918.429699	82349.744106	37.764519
1920.529442	82447.483380	37.769536
1922.303769	82546.528274	37.774554
1924.474065	82645.486213	37.779572
1926.714352	82743.736675	37.784589
1928.662933	82832.327564	37.789607
1930.720519	82935.282672	37.794624
1932.564437	83031.112739	37.799642
1934.825665	83124.736503	37.804660
1936.969367	83217.669412	37.809677
1939.114605	83304.127682	37.814695
1941.186800	83391.446581	37.819712
1943.254922	83485.228458	37.824730
1945.226994	83570.700977	37.829748
1946.986081	83658.855280	37.834765
1948.900007	83745.161024	37.839783
1951.105570	83842.711156	37.844800
1953.266070	83936.023911	37.849818
1955.068928	84016.101087	37.854836
1957.299586	84098.519038	37.859853
1959.392917	84184.468594	37.864871
1961.541180	84275.706324	37.869888
1963.321283	84364.366360	37.874906
1965.523189	84446.270298	37.879924
1967.327011	84537.144610	37.884941
1969.280530	84615.362567	37.889959
1971.421723	84712.330192	37.894976
1973.122928	84805.046073	37.899994
1974.716546	84887.477279	37.905012
1976.608033	84982.976999	37.910029
1978.709235	85075.580478	37.915047
1980.759422	85175.402307	37.920064
1982.451530	85280.437820	37.925082
1984.703886	85379.138969	37.930100
1986.985865	85481.599290	37.935117
1988.874718	85565.354772	37.940135
1991.078408	85665.813205	37.945152
1992.791893	85773.977076	37.950170
1994.718435	85866.977905	37.955188
1996.693208	85952.381068	37.960205
1998.708136	86051.945335	37.965223
2000.621701	86153.768731	37.970240
2002.515625	86256.964128	37.975258
2004.846266	86348.750127	37.980276
2006.732695	86448.906101	37.985293
2008.780351	86543.588202	37.990311
2010.528084	86640.484471	37.995328
2012.576690	86757.926246	38.000346
2014.558447	86851.276409	38.005364
2016.210574	86953.625055	38.010381
2018.085621	87060.374482	38.015399
2019.890777	87158.594078	38.020416
2021.775790	87264.024766	38.025434
2023.923231	87366.018562	38.030452
2025.976051	87467.545964	38.035469
2027.680805	87561.866829	38.040487
2029.653789	87658.401742	38.045504
2031.178373	87751.294063	38.050522
2033.280452	87844.159681	38.055540
2034.930343	87946.550162	38.060557
2036.611584	88055.272455	38.065575
2038.797792	88167.603916	38.070592
2040.633739	88278.799363	38.075610
2043.142241	88390.548986	38.080628
2044.690056	88514.387238	38.085645
2046.561939	88632.751270	38.090663
2048.904824	88744.211320	38.095680
2051.114344	88855.908101	38.100698
2053.740260	88983.685702	38.105716
2055.432431	89104.512977	38.110733
2057.627251	89232.384449	38.115751
2059.856697	89344.105297	38.120768
2061.901757	89475.270951	38.125786
2064.228893	89576.319118	38.130804
2066.008770	89703.509809	38.135821
2068.387028	89827.933313	38.140839
2070.361680	89943.510994	38.145856
2072.535957	90070.096576	38.150874
2074.586809	90185.194347	38.155892
2076.543886	90311.890978	38.160909
2078.602382	90442.412419	38.165927
2081.039037	90568.540822	38.170944
2083.086681	90700.585938	38.175962
2085.227270	90818.042108	38.180980
2086.901665	90950.374851	38.185997
2089.219491	91081.847062	38.191015
2091.233540	91209.641201	38.196032
2093.067495	91341.329666	38.201050
2095.582950	91480.617972	38.206068
2097.635409	91616.278486	38.211085
2099.354455	91745.806722	38.216103
2101.704849	91879.736121	38.221120
2103.571949	92019.533928	38.226138
2106.121922	92161.671706	38.231156
2108.026314	92297.295060	38.236173
2110.194263	92434.778967	38.241191
2112.590879	92563.241408	38.246208
2114.868018	92703.776705	38.251226
2117.381099	92839.307235	38.256244
2119.353621	92973.503366	38.261261
2121.605988	93093.409773	38.266279
2124.144232	93217.619412	38.271296
2125.673206	93343.318333	38.276314
2128.252516	93472.655935	38.281332
2130.395534	93606.511288	38.286349
2132.307835	93739.300588	38.291367
2134.835481	93860.814691	38.296384
2136.724778	93996.118380	38.301402
2138.734159	94121.707294	38.306420
2141.107392	94255.770281	38.311437
2142.971899	94395.034298	38.316455
2145.065507	94511.954338	38.321472
2146.965362	94650.504150	38.326490
2149.182757	94784.885350	38.331508
2151.666004	94920.543800	38.336525
2153.457928	95056.729301	38.341543
2155.714604	95190.370923	38.346560
2157.616877	95319.543324	38.351578
2160.072619	95462.953332	38.356596
2161.945076	95598.330026	38.361613
2163.646248	95740.135447	38.366631
2166.143835	95856.971990	38.371648
2167.964285	95992.903597	38.376666
2169.809026	96113.519289	38.381684
2171.879355	96231.387460	38.386701
2173.785537	96356.938164	38.391719
2175.859537	96490.854777	38.396736
2177.577199	96624.523480	38.401754
2179.815416	96757.654960	38.406772
2181.766230	96897.677219	38.411789
2183.597642	97046.503560	38.416807
2186.216007	97187.284661	38.421824
2188.013609	97345.980026	38.426842
2190.280407	97489.948593	38.431860
2192.304914	97642.487131	38.436877
2194.459152	97804.500994	38.441895
2196.980246	97964.442672	38.446912
2199.302843	98136.002882	38.451930
2201.305862	98284.656060	38.456948
2203.683420	98447.398871	38.461965
2205.360001	98623.144768	38.466983
2208.137563	98778.473980	38.472000
2210.004830	98960.112117	38.477018
2212.436456	99118.526954	38.482036
2214.402061	99289.616757	38.487053
2216.514982	99461.369001	38.492071
2219.214253	99620.783987	38.497088
2221.298615	99796.662665	38.502106
2223.478402	99974.695243	38.507124
2226.179426	100144.609605	38.512141
2227.887360	100322.793984	38.517159
2230.620903	100498.587589	38.522176
2232.765102	100680.661157	38.527194
2235.323029	100849.511300	38.532212
2237.642949	101028.199664	38.537229
2239.649504	101202.513379	38.542247
2241.806854	101375.752145	38.547264
2244.215137	101570.416806	38.552282
2246.909618	101727.218487	38.557300
2249.340748	101902.648586	38.562317
2251.281853	102088.514562	38.567335
2253.948685	102250.293011	38.572352
2256.265908	102421.001940	38.577370
2258.330595	102596.873426	38.582388
2260.834943	102762.584826	38.587405
2263.368214	102942.619523	38.592423
2265.747144	103092.034639	38.597440
2268.991826	103250.469131	38.602458
2271.461658	103396.967938	38.607476
2274.531107	103538.175200	38.612493
2276.779347	103681.958593	38.617511
2278.919417	103835.737976	38.622528
2281.039439	103979.136978	38.627546
2283.502746	104125.601975	38.632564
2285.772789	104280.390087	38.637581
2287.450569	104433.141445	38.642599
2289.570152	104572.853378	38.647616
2290.934979	104733.643069	38.652634
2293.445732	104892.986305	38.657652
2295.584663	105051.133189	38.662669
2297.570462	105223.670777	38.667687
2300.140335	105388.015554	38.672704
2302.172048	105560.801274	38.677722
2304.412984	105734.937242	38.682740
2306.712667	105905.641348	38.687757
2308.390565	106071.904169	38.692775
2311.070512	106241.815037	38.697792
2313.144164	106419.049240	38.702810
2315.755609	106588.325870	38.707828
2317.943591	106767.623538	38.712845
2319.693496	106924.812911	38.717863
2322.238207	107080.027339	38.722880
2323.961351	107236.398106	38.727898
2325.698746	107408.351601	38.732916
2328.408360	107572.089066	38.737933
2330.072448	107736.979956	38.742951
2332.467231	107915.896208	38.747968
2334.418704	108103.416837	38.752986
2336.965290	108292.405114	38.758004
2339.340249	108478.314470	38.763021
2341.054923	108672.228311	38.768039
2343.764955	108856.286583	38.773056
2345.801104	109059.117725	38.778074
2347.881751	109264.136915	38.783092
2350.539837	109471.501758	38.788109
2352.170569	109679.726016	38.793127
2354.765539	109886.012596	38.798144
2357.478828	110107.562974	38.803162
2359.633041	110316.026140	38.808180
2362.251536	110520.385169	38.813197
2364.537359	110742.196625	38.818215
2367.254372	110957.867473	38.823232
2369.367550	111169.132058	38.828250
2371.827285	111388.447396	38.833268
2374.052333	111608.916808	38.838285
2376.624414	111823.981478	38.843303
2379.579129	112037.630599	38.848320
2382.615316	112264.685992	38.853338
2384.543294	112468.238416	38.858356
2387.123234	112681.683672	38.863373
2389.637798	112905.413164	38.868391
2392.333294	113119.020484	38.873408
2394.883456	113322.670633	38.878426
2397.139184	113547.547967	38.883444
2399.803035	113754.657796	38.888461
2402.234034	113969.135872	38.893479
2404.702837	114175.466908	38.898496
2407.413621	114395.205149	38.903514
2409.500838	114613.900787	38.908532
2412.218897	114811.876374	38.913549
2414.082247	115030.343167	38.918567
2416.388108	115247.004431	38.923584
2418.633283	115477.070016	38.928602
2421.089167	115703.172225	38.933620
2423.912102	115927.214410	38.938637
2425.830141	116154.925521	38.943655
2428.441992	116374.779811	38.948672
2430.958595	116601.981461	38.953690
2433.052287	116832.003024	38.958708
2435.306806	117058.462052	38.963725
2437.929724	117290.572575	38.968743
2440.312105	117528.911945	38.973760
2442.718657	117758.294088	38.978778
2445.218372	118000.194986	38.983796
2447.890408	118235.461991	38.988813
2450.128584	118469.022521	38.993831
2452.701727	118698.663350	38.998848
2454.964474	118928.138483	39.003866
2457.290764	119177.519774	39.008884
2459.564548	119414.847829	39.013901
2462.055558	119656.443483	39.018919
2464.034740	119895.748667	39.023936
2466.594262	120148.245596	39.028954
2469.197581	120400.952969	39.033972
2471.557929	120649.120704	39.038989
2473.720607	120892.031258	39.044007
2476.679333	121139.055654	39.049024
2478.924145	121388.971363	39.054042
2481.241725	121605.349938	39.059060
2484.262824	121831.159082	39.064077
2486.627845	122053.926156	39.069095
2488.880063	122276.293512	39.074112
2491.077137	122494.890434	39.079130
2493.303247	122723.328117	39.084148
2495.896288	122954.081958	39.089165
2498.175428	123189.389714	39.094183
2500.753581	123420.224705	39.099200
2503.262050	123660.814770	39.104218
2505.205817	123913.876218	39.109236
2508.173291	124146.519353	39.114253
2510.101756	124408.238260	39.119271
2512.276969	124664.553960	39.124288
2515.289260	124916.718761	39.129306
2517.758209	125170.581307	39.134324
2520.693599	125421.086663	39.139341
2523.000158	125677.362845	39.144359
2525.809052	125937.621803	39.149376
2528.036235	126207.945222	39.154394
2530.700182	126474.637091	39.159412
2533.211486	126728.490000	39.164429
2535.847589	127006.912409	39.169447
2538.211054	127266.475540	39.174464
2540.276219	127540.753349	39.179482
2543.321486	127817.328300	39.184500
2545.687177	128100.291630	39.189517
2548.137606	128380.300130	39.194535
2550.718103	128663.982225	39.199552
2553.414980	128950.185551	39.204570
2555.790898	129239.321131	39.209588
2558.386656	129524.250014	39.214605
2560.661405	129815.651086	39.219623
2563.292500	130110.030834	39.224640
2565.713145	130406.818195	39.229658
2568.105075	130709.207571	39.234676
2570.824687	131004.049072	39.239693
2573.433364	131322.789358	39.244711
2576.089486	131629.737031	39.249728
2579.174430	131939.220940	39.254746
2581.444640	132249.710000	39.259764
2584.207089	132547.473653	39.264781
2586.742823	132867.162914	39.269799
2589.458764	133174.632313	39.274816
2592.302467	133470.993730	39.279834
2594.916939	133775.704299	39.284852
2597.931748	134064.315295	39.289869
2600.603852	134370.251761	39.294887
2603.914615	134654.011070	39.299904
2606.248654	134954.205401	39.304922
2608.658879	135255.189250	39.309940
2611.032223	135556.904175	39.314957
2613.226218	135857.532473	39.319975
2615.880478	136154.601096	39.324992
2618.669836	136460.520679	39.330010
2620.844430	136769.419063	39.335028
2623.153900	137085.430180	39.340045
2625.528053	137410.544795	39.345063
2628.025325	137714.830616	39.350080
2630.509837	138040.376535	39.355098
2633.383959	138380.927180	39.360116
2635.970422	138698.657196	39.365133
2638.474879	139020.856544	39.370151
2640.744483	139354.744770	39.375168
2643.369021	139675.686121	39.380186
2646.034786	140015.468947	39.385204
2648.551974	140331.938984	39.390221
2650.804356	140678.885354	39.395239
2653.194437	141003.984146	39.400256
2655.796630	141322.807931	39.405274
2658.163739	141626.491939	39.410292
2660.701562	141951.332841	39.415309
2662.780528	142272.922541	39.420327
2664.910110	142617.490602	39.425344
2667.839995	142953.978315	39.430362
2670.275491	143308.085439	39.435380
2673.034847	143631.468615	39.440397
2675.894620	143982.963150	39.445415
2678.424204	144342.494979	39.450432
2681.687289	144691.393019	39.455450
2683.818006	145060.079789	39.460468
2686.516134	145416.318346	39.465485
2688.822337	145773.788376	39.470503
2691.253504	146154.836366	39.475520
2694.076013	146516.508121	39.480538
2697.222263	146889.326551	39.485556
2699.821058	147257.257788	39.490573
2702.456565	147646.598425	39.495591
2705.008653	148026.308488	39.500608
2707.633830	148409.627320	39.505626
2710.329956	148807.763202	39.510644
2713.306900	149200.818994	39.515661
2715.589402	149586.014990	39.520679
2718.474042	149982.962353	39.525696
2721.475992	150388.144945	39.530714
2724.370701	150782.012099	39.535732
2727.359286	151177.758740	39.540749
2729.842473	151589.060785	39.545767
2732.403644	151999.820554	39.550784
2735.123541	152406.521903	39.555802
2737.673039	152821.300786	39.560820
2740.459214	153234.522432	39.565837
2742.780939	153657.061024	39.570855
2745.362853	154076.464680	39.575872
2748.146214	154505.500235	39.580890
2750.767307	154933.688455	39.585908
2753.428498	155370.480405	39.590925
2755.912727	155814.589974	39.595943
2758.964271	156257.255846	39.600960
2762.384866	156684.303567	39.605978
2765.403555	157117.574208	39.610996
2768.166656	157556.562592	39.616013
2771.059743	157985.847552	39.621031
2774.198553	158424.148730	39.626048
2777.157853	158844.123886	39.631066
2780.458874	159272.465441	39.636084
2783.088528	159695.697173	39.641101
2785.953552	160129.622631	39.646119
2788.156960	160552.723715	39.651136
2791.105254	160984.763119	39.656154
2793.935072	161426.142648	39.661172
2796.356307	161867.462172	39.666189
2798.692966	162304.836833	39.671207
2801.103870	162746.163979	39.676224
2804.147336	163195.203255	39.681242
2806.764839	163634.752023	39.686260
2809.361595	164100.283442	39.691277
2812.192134	164563.293070	39.696295
2814.429166	165025.421088	39.701312
2817.538956	165479.924831	39.706330
2820.010862	165946.948618	39.711348
2822.754393	166426.705942	39.716365
2825.283370	166894.031929	39.721383
2827.567279	167376.165792	39.726400
2831.026141	167853.434028	39.731418
2833.439888	168329.764283	39.736436
2835.826272	168776.885978	39.741453
2838.561397	169241.020893	39.746471
2841.244008	169702.018061	39.751488
2844.264683	170157.251455	39.756506
2846.983925	170629.155697	39.761524
2849.475658	171101.492124	39.766541
2852.206792	171576.612932	39.771559
2854.717542	172062.157853	39.776576
2857.493552	172536.020546	39.781594
2860.166895	173038.624635	39.786612
2862.915492	173525.906534	39.791629
2865.977174	174014.158317	39.796647
2868.503649	174526.661177	39.801664
2871.944185	175020.446991	39.806682
2874.858112	175529.073477	39.811700
2878.252181	176030.275722	39.816717
2881.432606	176524.073174	39.821735
2884.384883	177021.261606	39.826752
2887.406291	177535.331161	39.831770
2889.928885	178046.662732	39.836788
2893.111590	178554.490852	39.841805
2895.773366	179075.203713	39.846823
2898.571160	179592.495091	39.851840
2901.642456	180115.537378	39.856858
2903.666030	180643.826126	39.861876
2906.600231	181181.347392	39.866893
2909.282614	181721.019211	39.871911
2912.340756	182259.467048	39.876928
2915.436152	182798.013707	39.881946
2918.454003	183351.408313	39.886964
2921.473514	183892.919176	39.891981
2924.515292	184511.286668	39.896999
2927.075427	185087.189837	39.902016
2930.515398	185631.920831	39.907034
2933.387213	186185.912724	39.912052
2936.198488	186743.244354	39.917069
2939.217177	187301.714860	39.922087
2942.270985	187861.097164	39.927104
2945.587218	188413.862728	39.932122
2948.613589	188987.605982	39.937140
2951.229302	189542.290084	39.942157
2954.068045	190103.292061	39.947175
2956.604287	190679.304875	39.952192
2960.029270	191237.782173	39.957210
2963.366689	191797.342589	39.962228
2966.207236	192373.315944	39.967245
2969.816888	192928.495407	39.972263
2972.447063	193501.661957	39.977280
2975.708835	194055.249672	39.982298
2978.733999	194629.807298	39.987316
2981.713611	195197.643183	39.992333
2984.495431	195761.651363	39.997351
2987.601223	196334.704910	40.002368
2990.364246	196900.955957	40.007386
2993.477543	197474.800362	40.012404
2996.141498	198046.100893	40.017421
2999.172962	198629.539032	40.022439
3002.066600	199200.122139	40.027456
3005.207373	199790.482295	40.032474
3008.051053	200377.969834	40.037492
3010.678540	200968.033509	40.042509
3013.696832	201544.498691	40.047527
3016.415970	202136.914504	40.052544
3019.538040	202718.371616	40.057562
3022.276579	203318.967917	40.062580
3025.294620	203919.725669	40.067597
3028.452507	204506.999978	40.072615
3031.677251	205095.027669	40.077632
3034.595023	205659.988434	40.082650
3037.802321	206221.577665	40.087668
3040.561653	206784.610183	40.092685
3044.285319	207326.180139	40.097703
3047.418941	207875.947258	40.102720
3050.249619	208430.081584	40.107738
3053.177261	208989.765326	40.112756
3056.478965	209561.712434	40.117773
3059.650796	210116.101971	40.122791
3062.440366	210679.138782	40.127808
3065.307752	211253.088052	40.132826
3068.056293	211839.403152	40.137844
3070.753493	212414.041763	40.142861
3073.880991	213002.103447	40.147879
3076.444577	213595.309681	40.152896
3079.568661	214187.794177	40.157914
3082.316291	214804.980130	40.162932
3084.982234	215420.884237	40.167949
3087.759930	216033.596303	40.172967
3090.453322	216670.202028	40.177984
3093.554729	217307.659341	40.183002
3096.586807	217954.680160	40.188020
3099.054899	218608.598179	40.193037
3102.336589	219266.454304	40.198055
3105.284674	219921.340154	40.203072
3108.447090	220596.846517	40.208090
3111.841877	221258.649690	40.213108
3114.746838	221935.924743	40.218125
3117.924240	222605.206093	40.223143
3121.003258	223297.925676	40.228160
3124.343215	223982.272146	40.233178
3127.313430	224673.408660	40.238196
3130.308534	225373.839247	40.243213
3133.544431	226064.578612	40.248231
3137.066539	226758.016768	40.253248
3140.533422	227451.895251	40.258266
3143.873261	228145.005814	40.263284
3146.809454	228850.195269	40.268301
3150.387905	229541.616488	40.273319
3153.439856	230241.883916	40.278336
3156.730330	230949.201159	40.283354
3159.881659	231641.754356	40.288372
3162.864268	232350.921952	40.293389
3166.399375	233044.658326	40.298407
3169.357967	233751.770150	40.303424
3172.688025	234469.848108	40.308442
3176.213638	235179.485671	40.313460
3179.145026	235884.947098	40.318477
3182.667419	236592.601149	40.323495
3185.724613	237299.970898	40.328512
3188.796503	237993.669745	40.333530
3192.042033	238713.226132	40.338548
3195.420884	239424.783278	40.343565
3198.960474	240124.704178	40.348583
3201.793933	240841.982570	40.353600
3204.994150	241560.675040	40.358618
3208.466413	242263.750754	40.363636
3211.462390	242983.385502	40.368653
3215.207292	243678.488584	40.373671
3218.604502	244391.502124	40.378688
3221.494006	245102.306410	40.383706
3224.909170	245806.548340	40.388724
3227.475189	246529.388295	40.393741
3231.522978	247223.288915	40.398759
3234.200003	247944.708953	40.403776
3237.257508	248651.485638	40.408794
3240.588001	249362.535164	40.413812
3243.727572	250072.874893	40.418829
3246.858980	250761.468665	40.423847
3250.129435	251437.616178	40.428864
3253.081768	252114.039116	40.433882
3256.320910	252803.572294	40.438900
3259.355566	253484.777107	40.443917
3262.312247	254168.429447	40.448935
3265.405440	254871.616180	40.453952
3268.167175	255572.184022	40.458970
3271.070982	256279.431896	40.463988
3274.351418	257005.058172	40.469005
3277.313188	257722.424115	40.474023
3280.361406	258463.141056	40.479040
3283.377102	259203.045804	40.484058
3286.875443	259951.582852	40.489076
3290.149595	260698.168977	40.494093
3293.501438	261441.385313	40.499111
3297.047312	262182.915424	40.504128
3300.257908	262945.879508	40.509146
3303.790671	263698.272455	40.514164
3306.758023	264475.766793	40.519181
3310.084436	265237.477130	40.524199
3313.748709	266006.748636	40.529216
3316.826498	266782.455614	40.534234
3320.569787	267561.506616	40.539252
3323.884778	268334.421103	40.544269
3327.879861	269107.603923	40.549287
3331.050504	269890.814400	40.554304
3334.918841	270655.622757	40.559322
3338.382961	271433.796075	40.564340
3341.486945	272206.583841	40.569357
3344.890000	272980.384652	40.574375
3348.625911	273757.986727	40.579392
3351.927511	274533.541608	40.584410
3355.362724	275321.563313	40.589428
3358.420276	276122.690014	40.594445
3362.008330	276900.488624	40.599463
3365.257163	277681.354684	40.604480
3368.427253	278470.478689	40.609498
3372.564503	279259.976654	40.614516
3376.084638	280048.267722	40.619533
3379.664384	280837.302959	40.624551
3382.829902	281629.137054	40.629568
3386.523228	282424.003417	40.634586
3390.074793	283200.345732	40.639604
3393.011469	283997.801326	40.644621
3396.614838	284780.212407	40.649639
3399.936264	285575.202668	40.654656
3403.313110	286369.768641	40.659674
3407.028763	287165.110127	40.664692
3410.264826	287966.204771	40.669709
3413.593750	288755.391789	40.674727
3417.201860	289566.488877	40.679744
3420.301903	290369.885411	40.684762
3423.950168	291169.555080	40.689780
3426.789371	291988.510540	40.694797
3430.117587	292791.890737	40.699815
3433.310584	293608.737855	40.704832
3436.860067	294415.413153	40.709850
3440.677421	295218.938094	40.714868
3443.932638	296037.671397	40.719885
3447.259789	296850.771041	40.724903
3450.789759	297666.620025	40.729920
3454.053635	298488.388672	40.734938
3458.186939	299307.902141	40.739956
3461.785369	300117.560852	40.744973
3465.018330	300919.902645	40.749991
3468.321238	301744.916549	40.755008
3471.824063	302537.654176	40.760013
3475.385629	303308.799965	40.765018
3478.702990	304029.353100	40.770023
3482.107959	304695.878945	40.775028
3485.220102	305314.953964	40.780032
3488.184405	305876.174049	40.785037
3491.109927	306382.654193	40.790042
3493.921242	306851.967136	40.795047
3496.477186	307251.104349	40.800052
3498.717929	307612.599295	40.805056
3500.673026	307928.712051	40.810061
3502.839400	308199.493030	40.815066
3505.069341	308428.554164	40.820071
3506.370576	308609.969236	40.825076
3507.775997	308759.863581	40.830080
3509.117903	308870.425951	40.835085
3510.528714	308945.987385	40.840090
3511.422761	309006.259393	40.845095
3512.589375	309031.015367	40.850100
3514.038808	309019.795709	40.855104
3514.851146	308998.725801	40.860109
3515.778269	308944.098517	40.865114
3516.158634	308878.385307	40.870119
3516.912941	308782.611188	40.875124
3517.505885	308675.919746	40.880128
3517.859604	308554.607759	40.885133
3518.836294	308417.420636	40.890138
3519.185617	308264.833642	40.895143
3519.537785	308086.518150	40.900148
3519.806646	307914.526080	40.905152
3520.087861	307728.280687	40.910157
3520.516235	307534.326307	40.915162
3520.610839	307328.411870	40.920167
3520.812423	307110.646461	40.925172
3521.035187	306901.045685	40.930176
3521.088598	306679.077146	40.935181
3521.280076	306431.866573	40.940186
3521.598711	306202.143562	40.945191
3521.056986	305961.280218	40.950196
3521.363815	305718.577991	40.955200
3521.117432	305472.449130	40.960205
3521.093235	305214.043317	40.965210
3521.121035	304976.216505	40.970215
3521.390516	304721.096137	40.975220
3521.158622	304454.702412	40.980224
3521.323207	304202.039021	40.985229
3521.193161	303936.670134	40.990234
3521.162336	303683.678468	40.995239
3520.997510	303430.375672	41.000244
3520.830378	303172.974538	41.005248
3520.419736	302913.879591	41.010253
3520.657340	302653.689456	41.015258
3520.623389	302395.627434	41.020263
3520.267787	302135.349333	41.025268
3520.340591	301874.595768	41.030272
3519.811334	301624.497164	41.035277
3519.924627	301368.137795	41.040282
3519.729813	301105.997063	41.045287
3519.374015	300850.472093	41.050292
3519.404706	300607.738425	41.055296
3519.319106	300358.022696	41.060301
3519.308829	300108.370400	41.065306
3519.037949	299863.339008	41.070311
3518.777101	299610.440339	41.075316
3519.019802	299370.544074	41.080320
3518.371806	299124.473909	41.085325
3519.029829	298873.667982	41.090330
3518.175423	298642.313834	41.095335
3518.301578	298395.075858	41.100340
3518.397343	298151.124909	41.105344
3517.758505	297913.752703	41.110349
3518.014497	297686.471583	41.115354
3517.482746	297457.938250	41.120359
3517.289408	297218.991753	41.125364
3517.206581	296982.903163	41.130368
3516.944296	296764.251580	41.135373
3517.185693	296535.670022	41.140378
3516.727602	296314.883810	41.145383
3516.621750	296092.616289	41.150388
3516.483691	295882.494268	41.155392
3516.255839	295661.185938	41.160397
3516.076055	295447.403543	41.165402
3515.828917	295228.081965	41.170407
3515.748662	295016.471453	41.175412
3515.660250	294802.010607	41.180416
3515.385490	294601.348758	41.185421
3515.379154	294396.087968	41.190426
3515.093246	294198.557351	41.195431
3515.047061	293991.112321	41.200436
3514.761958	293796.329306	41.205440
3514.648863	293601.620579	41.210445
3514.693812	293400.064684	41.215450
3514.348962	293201.954521	41.220455
3514.177894	293022.143949	41.225460
3514.272875	292832.898420	41.230464
3513.982414	292643.610738	41.235469
3513.853879	292455.391713	41.240474
3513.704903	292272.342676	41.245479
3513.533249	292092.834897	41.250484
3513.468427	291908.727953	41.255488
3513.155700	291730.004820	41.260493
3513.168705	291545.299146	41.265498
3512.811497	291385.851666	41.270503
3512.848494	291219.367342	41.275508
3512.534817	291043.417015	41.280512
3512.605081	290875.730155	41.285517
3512.596814	290708.309678	41.290522
3512.046451	290551.894024	41.295527
3512.321263	290385.395744	41.300532
3512.084133	290232.315946	41.305536
3511.672130	290070.964474	41.310541
3511.673514	289916.471997	41.315546
3511.460568	289765.551045	41.320551
3511.358813	289603.920770	41.325556
3511.117784	289452.545253	41.330560
3511.242088	289309.181894	41.335565
3511.142666	289159.438198	41.340570
3510.739479	289017.047622	41.345575
3510.722207	288865.024776	41.350580
3510.737372	288732.623456	41.355584
3510.285002	288604.978961	41.360589
3510.247976	288448.910629	41.365594
3510.229720	288317.150095	41.370599
3510.065283	288183.324697	41.375604
3510.337914	288051.670888	41.380608
3510.010620	287928.231325	41.385613
3509.910342	287798.493651	41.390618
3509.978015	287668.220323	41.395623
3509.713962	287538.507736	41.400628
3509.488242	287413.142048	41.405632
3509.285781	287297.878936	41.410637
3509.327302	287158.062288	41.415642
3509.061556	287043.063194	41.420647
3508.820337	286926.048947	41.425652
3509.004169	286812.582970	41.430656
3509.087093	286704.071286	41.435661
3508.790858	286576.882111	41.440666
3508.885668	286471.601271	41.445671
3509.046929	286358.850855	41.450676
3509.068332	286240.979707	41.455680
3508.765316	286132.578347	41.460685
3508.803302	286008.543483	41.465690
3508.482405	285904.548705	41.470695
3508.350207	285787.260841	41.475700
3508.472936	285687.116846	41.480704
3508.034479	285576.088167	41.485709
3508.393543	285468.422333	41.490714
3508.148420	285375.769049	41.495719
3508.110508	285261.545926	41.500724
3508.465712	285168.569385	41.505728
3507.893857	285065.630868	41.510733
3507.872456	284950.615447	41.515738
3507.986838	284860.196473	41.520743
3507.686373	284758.895291	41.525748
3507.989917	284655.997504	41.530752
3507.668678	284556.175837	41.535757
3507.956697	284453.840253	41.540762
3507.598801	284360.261275	41.545767
3507.758871	284259.472895	41.550772
3507.435786	284171.183524	41.555776
3507.381785	284064.751143	41.560781
3507.482360	283979.297535	41.565786
3507.220620	283897.235508	41.570791
3506.977093	283801.397562	41.575796
3507.368965	283714.345127	41.580800
3507.027584	283628.680142	41.585805
3507.332054	283535.251083	41.590810
3506.729449	283457.238808	41.595815
3506.886524	283369.407981	41.600820
3506.901873	283288.905807	41.605824
3506.880327	283200.313479	41.610829
3506.813910	283109.131276	41.615834
3507.089839	283036.200201	41.620839
3506.897672	282949.136292	41.625844
3506.745507	282871.791248	41.630848
3506.468588	282789.603006	41.635853
3506.122205	282693.041326	41.640858
3506.018127	282626.661225	41.645863
3506.204272	282547.760868	41.650868
3506.220253	282480.801767	41.655872
3506.000400	282400.335355	41.660877
3506.109173	282330.713883	41.665882
3506.053540	282254.549645	41.670887
3505.962020	282181.344174	41.675892
3506.065729	282110.526710	41.680896
3505.923856	282038.729210	41.685901
3506.068971	281976.561200	41.690906
3505.533053	281894.972519	41.695911
3505.646830	281831.892757	41.700916
3505.474000	281761.907415	41.705920
3505.525988	281697.844291	41.710925
3505.433737	281640.041152	41.715930
3505.411828	281573.952740	41.720935
3505.597947	281519.492053	41.725940
3505.395361	281458.498160	41.730944
3505.181243	281388.340698	41.735949
3505.608779	281322.283629	41.740954
3505.339364	281258.193988	41.745959
3505.140656	281199.897955	41.750964
3505.192046	281137.031018	41.755968
3504.960676	281071.764137	41.760973
3505.200765	281017.371014	41.765978
3504.755588	280964.230658	41.770983
3504.674946	280903.242696	41.775988
3504.846249	280854.894084	41.780992
3504.624458	280808.796408	41.785997
3504.956369	280744.968739	41.791002
3504.909158	280698.996456	41.796007
3504.868761	280648.109400	41.801012
3504.550912	280584.204958	41.806016
3504.590104	280532.668890	41.811021
3504.633491	280483.194355	41.816026
3504.790640	280435.280493	41.821031
3504.603074	280387.802386	41.826036
3504.962600	280334.943122	41.831040
3504.710841	280283.452368	41.836045
3504.942507	280226.743155	41.841050
3504.476655	280169.659215	41.846055
3504.294013	280119.303227	41.851060
3504.381696	280064.856851	41.856064
3504.178584	280023.211210	41.861069
3504.353822	279971.347967	41.866074
3504.394674	279930.427925	41.871079
3504.510638	279878.650264	41.876084
3504.302925	279832.269722	41.881088
3504.012938	279791.910522	41.886093
3504.029702	279737.322237	41.891098
3503.717454	279702.287567	41.896103
3503.632856	279653.570823	41.901108
3503.585091	279622.644718	41.906112
3503.705705	279591.183080	41.911117
3503.977709	279554.834926	41.916122
3503.749046	279514.644209	41.921127
3503.548227	279472.768764	41.926132
3503.470826	279435.787762	41.931136
3503.677543	279414.165569	41.936141
3503.852004	279363.855082	41.941146
3503.552965	279337.245412	41.946151
3503.650453	279292.802696	41.951156
3503.779971	279257.469614	41.956160
3503.934064	279215.665839	41.961165
3503.629084	279169.580155	41.966170
3503.632528	279144.247046	41.971175
3503.474174	279097.578274	41.976180
3503.730816	279077.144800	41.981184
3503.582193	279037.144995	41.986189
3503.839639	278995.070341	41.991194
3503.577382	278973.292201	41.996199
3503.457051	278927.228421	42.001204
3504.052281	278885.508258	42.006208
3503.376711	278868.097460	42.011213
3503.519331	278819.624717	42.016218
3503.533167	278795.282811	42.021223
3503.381508	278755.257872	42.026228
3503.318590	278732.862916	42.031232
3503.340784	278697.902794	42.036237
3503.470630	278665.395462	42.041242
3503.098845	278635.334336	42.046247
3503.353476	278598.886600	42.051252
3503.316190	278559.200121	42.056256
3503.207101	278535.946678	42.061261
3503.458901	278503.420211	42.066266
3503.398348	278483.265311	42.071271
3503.603163	278443.668222	42.076276
3503.468168	278402.545704	42.081280
3502.996325	278381.844032	42.086285
3503.239972	278351.686578	42.091290
3503.227629	278324.828049	42.096295
3503.362590	278293.414551	42.101300
3503.344821	278268.695515	42.106304
3503.098548	278237.596199	42.111309
3503.406940	278191.184887	42.116314
3503.271005	278169.361308	42.121319
3503.407740	278131.786069	42.126324
3503.074779	278108.567497	42.131328
3502.880882	278075.499481	42.136333
3503.237955	278046.699035	42.141338
3502.967637	278023.623406	42.146343
3502.703341	278000.699592	42.151348
3503.247976	277973.932086	42.156352
3503.022126	277943.796953	42.161357
3503.173325	277914.748580	42.166362
3502.624530	277889.425012	42.171367
3502.972266	277861.007862	42.176372
3503.653868	277838.165262	42.181376
3503.146803	277806.902861	42.186381
3503.421938	277780.839394	42.191386
3503.167961	277752.083449	42.196391
3503.197034	277717.300030	42.201396
3503.049857	277692.702884	42.206400
3503.001668	277665.238679	42.211405
3502.952848	277636.425156	42.216410
3503.026233	277618.413233	42.221415
3502.829787	277589.571851	42.226420
3503.262767	277566.615278	42.231424
3502.824207	277542.063639	42.236429
3503.000294	277516.372015	42.241434
3502.820824	277488.419062	42.246439
3503.146248	277461.074598	42.251444
3502.915521	277431.983913	42.256448
3502.707836	277409.942193	42.261453
3502.700012	277386.239744	42.266458
3502.260143	277368.664453	42.271463
3502.968074	277343.678903	42.276468
3503.012488	277323.507290	42.281472
3502.392198	277305.298216	42.286477
3503.069873	277268.529111	42.291482
3502.707234	277254.149758	42.296487
3502.569404	277223.924205	42.301492
3502.961075	277206.931772	42.306496
3502.747255	277189.321100	42.311501
3503.032282	277164.376150	42.316506
3502.731535	277135.092616	42.321511
3502.865687	277115.747122	42.326516
3502.712203	277089.826817	42.331520
3502.634820	277074.588093	42.336525
3502.711283	277061.744078	42.341530
3502.860731	277030.098660	42.346535
3502.707127	277014.871841	42.351540
3502.871951	276996.896400	42.356544
3502.856763	276969.630478	42.361549
3502.845929	276938.010081	42.366554
3502.627382	276920.272785	42.371559
3502.596636	276903.219024	42.376564
3502.320109	276876.885053	42.381568
3502.491068	276866.674151	42.386573
3502.823819	276827.285387	42.391578
3502.683435	276816.104723	42.396583
3502.576627	276792.646717	42.401588
3502.608226	276783.297797	42.406592
3502.489159	276759.969002	42.411597
3502.755819	276736.045219	42.416602
3502.401276	276713.313362	42.421607
3502.450929	276705.311033	42.426612
3502.466922	276678.396586	42.431616
3502.300947	276660.039953	42.436621
3502.605198	276650.648391	42.441626
3502.371624	276632.480545	42.446631
3502.533621	276615.803962	42.451636
3502.573799	276592.781213	42.456640
3502.368598	276586.677356	42.461645
3502.849077	276555.820203	42.466650
3502.687629	276543.216986	42.471655
3502.630936	276516.212005	42.476660
3502.658339	276496.093763	42.481664
3502.558724	276474.798712	42.486669
3502.457441	276452.485481	42.491674
3502.493710	276437.279788	42.496679
3502.581155	276421.633255	42.501684
3502.867550	276400.048688	42.506688
3502.394795	276389.887441	42.511693
3502.682402	276366.749560	42.516698
3502.581691	276351.132430	42.521703
3502.364984	276323.617721	42.526708
3502.491522	276310.791218	42.531712
3502.470806	276298.064116	42.536717
3502.396577	276271.290942	42.541722
3502.118858	276264.765563	42.546727
3502.583278	276244.247941	42.551732
3502.477691	276226.187298	42.556736
3502.167025	276215.873383	42.561741
3502.545206	276186.661582	42.566746
3502.498228	276173.327504	42.571751
3502.155614	276151.128302	42.576756
3502.475733	276140.486611	42.581760
3502.572883	276131.560203	42.586765
3502.415049	276098.663946	42.591770
3502.220666	276094.442473	42.596775
3502.399691	276070.710419	42.601780
3502.151285	276056.949515	42.606784
3502.404724	276045.528945	42.611789
3502.453399	276011.607386	42.616794
3502.485723	276013.002813	42.621799
3501.981588	275987.213353	42.626804
3502.347174	275977.964889	42.631808
3502.369767	275968.337210	42.636813
3502.600870	275933.648728	42.641818
3502.333003	275931.806613	42.646823
3502.168448	275904.512757	42.651828
3502.690061	275886.328520	42.656832
3502.330606	275882.132844	42.661837
3502.406022	275858.315081	42.666842
3502.118588	275850.314444	42.671847
3502.027041	275836.401673	42.676852
3502.309503	275819.196869	42.681856
3502.351179	275800.145586	42.686861
3502.267521	275785.264052	42.691866
3502.010135	275767.685338	42.696871
3502.161356	275758.623130	42.701876
3502.133437	275756.819880	42.706880
3502.148714	275742.661243	42.711885
3502.102704	275736.099594	42.716890
3502.283624	275724.257478	42.721895
3502.218540	275705.324708	42.726900
3502.595863	275692.637126	42.731904
3502.330494	275674.474034	42.736909
3502.345317	275658.609557	42.741914
3502.424698	275645.153791	42.746919
3502.379263	275625.250408	42.751924
3502.543063	275611.934206	42.756928
3502.095515	275595.785547	42.761933
3502.060522	275572.417801	42.766938
3502.010903	275574.819032	42.771943
3501.992948	275560.054489	42.776948
3502.357548	275534.485522	42.781952
3502.231873	275532.213789	42.786957
3502.273314	275507.535555	42.791962
3501.984867	275491.107390	42.796967
3502.153336	275491.972317	42.801972
3502.664670	275472.567457	42.806977
3502.119855	275456.714051	42.811981
3502.268737	275441.006801	42.816986
3502.230620	275426.499998	42.821991
3502.208202	275405.854587	42.826996
3502.374134	275406.567145	42.832001
3501.910910	275395.640445	42.837005
3502.416448	275370.405849	42.842010
3502.460692	275365.383195	42.847015
3502.588427	275346.674808	42.852020
3502.588088	275328.037363	42.857025
3502.294256	275310.184174	42.862029
3502.549069	275287.305724	42.867034
3502.279595	275266.902592	42.872039
3502.198265	275250.849378	42.877044
3502.662111	275243.673293	42.882049
3502.547118	275228.745632	42.887053
3502.654773	275203.165810	42.892058
3502.225151	275184.264449	42.897063
3502.187245	275171.947239	42.902068
3502.261270	275162.235040	42.907073
3502.171076	275142.134845	42.912077
3502.328571	275124.007365	42.917082
3502.591720	275116.684416	42.922087
3502.380179	275102.357437	42.927092
3502.784050	275095.801786	42.932097
3502.312689	275071.534589	42.937101
3502.700417	275047.616839	42.942106
3502.076288	275033.608966	42.947111
3502.312192	275014.578056	42.952116
3502.032617	275000.439925	42.957121
3502.233742	274989.994917	42.962125
3502.328252	274972.411938	42.967130
3502.040850	274970.445548	42.972135
3501.961663	274947.491914	42.977140
3502.123067	274938.097026	42.982145
3502.094309	274930.132240	42.987149
3502.490050	274912.833152	42.992154
3502.079013	274901.185309	42.997159
3502.201405	274886.195012	43.002164
3502.476355	274867.463500	43.007169
3502.053686	274859.916752	43.012173
3502.396106	274849.093177	43.017178
3502.073513	274838.246262	43.022183
3501.982455	274816.389287	43.027188
3502.410743	274806.290662	43.032193
3502.328840	274795.737110	43.037197
3502.305107	274772.494682	43.042202
3501.900610	274766.931074	43.047207
3501.767047	274744.724265	43.052212
3502.188673	274726.173482	43.057217
3502.047624	274727.646958	43.062221
3502.362653	274720.214018	43.067226
3502.288607	274698.303429	43.072231
3502.507339	274685.742331	43.077236
3502.290286	274665.891006	43.082241
3502.507031	274644.240478	43.087245
3502.272142	274631.317447	43.092250
3502.087680	274615.967691	43.097255
3501.803285	274608.857608	43.102260
3501.912866	274614.263891	43.107265
3502.267204	274592.668222	43.112269
3502.391162	274570.191953	43.117274
3502.150773	274563.915214	43.122279
3502.129986	274548.718088	43.127284
3502.226439	274529.861637	43.132289
3502.230267	274533.374847	43.137293
3502.400108	274501.878020	43.142298
3502.036462	274492.132322	43.147303
3501.866317	274479.504683	43.152308
3502.225179	274479.346856	43.157313
3502.000296	274466.447697	43.162317
3502.270334	274446.214629	43.167322
3502.319843	274449.822547	43.172327
3502.307777	274417.182898	43.177332
3502.301904	274406.999333	43.182337
3502.353748	274391.128822	43.187341
3502.439068	274367.538232	43.192346
3502.615083	274352.437609	43.197351
3502.554578	274339.156268	43.202356
3502.418483	274318.528357	43.207361
3502.147169	274299.194658	43.212365
3502.239828	274292.280215	43.217370
3502.301922	274281.169392	43.222375
3502.236522	274255.030715	43.227380
3502.107263	274245.121036	43.232385
3502.301766	274243.563057	43.237389
3502.178453	274221.761891	43.242394
3502.134368	274207.866885	43.247399
3502.298210	274199.693687	43.252404
3502.454413	274178.052503	43.257409
3502.148656	274180.570203	43.262413
3501.995023	274147.112349	43.267418
3501.847183	274139.522567	43.272423
3501.819122	274124.937579	43.277428
3502.134514	274110.680817	43.282433
3502.135035	274109.484163	43.287437
3502.372153	274089.765388	43.292442
3502.147510	274088.578475	43.297447
3502.162517	274074.088591	43.302452
3502.280363	274059.480780	43.307457
3502.076970	274053.249143	43.312461
3502.566103	274038.175895	43.317466
3502.211109	274021.579609	43.322471
3502.690056	274005.973253	43.327476
3502.634577	273977.414083	43.332481
3502.416070	273976.149824	43.337485
3502.343579	273943.290282	43.342490
3502.435807	273933.753325	43.347495
3502.436848	273914.096878	43.352500
3502.448665	273891.179648	43.357505
3502.357807	273884.599402	43.362509
3502.604051	273857.953568	43.367514
3502.305332	273854.232064	43.372519
3502.451409	273830.198974	43.377524
3502.501705	273819.166320	43.382529
3502.434708	273811.029174	43.387533
3502.358542	273782.906020	43.392538
3502.534976	273779.161151	43.397543
3502.530306	273751.765198	43.402548
3502.406653	273732.382821	43.407553
3502.316942	273719.156872	43.412557
3502.337831	273697.256640	43.417562
3502.108050	273703.734507	43.422567
3502.199704	273665.731385	43.427572
3502.395650	273649.965514	43.432577
3502.401277	273647.265813	43.437581
3502.132630	273624.341434	43.442586
3502.139171	273618.942643	43.447591
3502.210200	273601.286660	43.452596
3502.104199	273581.443177	43.457601
3502.320011	273586.043603	43.462605
3502.318754	273560.531226	43.467610
3502.636667	273545.586506	43.472615
3502.328198	273532.623885	43.477620
3502.576448	273508.931195	43.482625
3502.499204	273496.899966	43.487629
3502.520876	273475.177786	43.492634
3502.268255	273456.783057	43.497639
3502.071884	273446.960161	43.502644
3502.401920	273429.543730	43.507649
3502.048716	273419.821736	43.512653
3502.191267	273399.353729	43.517658
3502.337070	273390.674037	43.522663
3502.060391	273380.328990	43.527668
3502.161390	273365.443613	43.532673
3501.893746	273351.838035	43.537677
3502.036789	273337.353469	43.542682
3502.063834	273330.143662	43.547687
3502.041203	273315.150295	43.552692
3502.460546	273291.583567	43.557697
3502.313216	273287.329132	43.562701
3502.351744	273269.347158	43.567706
3501.946398	273266.355230	43.572711
3501.994027	273250.205083	43.577716
3502.276193	273241.427671	43.582721
3502.188463	273231.205837	43.587725
3502.075962	273209.555489	43.592730
3501.893945	273214.574599	43.597735
3502.255984	273185.415186	43.602740
3502.254660	273180.068520	43.607745
3502.110878	273175.686215	43.612749
3502.350228	273144.534480	43.617754
3502.180843	273133.001381	43.622759
3502.246896	273126.167388	43.627764
3502.471786	273108.258091	43.632769
3501.974878	273102.861590	43.637773
3502.420199	273091.792545	43.642778
3502.203774	273071.558815	43.647783
3502.074937	273057.320403	43.652788
3502.018895	273045.565877	43.657793
3502.001246	273025.835760	43.662797
3502.083914	273006.675580	43.667802
3501.909185	273011.057014	43.672807
3501.845250	273002.893850	43.677812
3502.239862	272981.749787	43.682817
3501.764244	272979.940085	43.687821
3502.120638	272973.391692	43.692826
3502.154743	272966.868224	43.697831
3502.142891	272949.479684	43.702836
3501.964161	272931.378833	43.707841
3501.696388	272934.578104	43.712845
3501.887143	272922.224813	43.717850
3502.146965	272908.485776	43.722855
3501.760882	272900.067423	43.727860
3502.139801	272891.147539	43.732865
3501.875729	272889.559382	43.737869
3502.142335	272861.382334	43.742874
3501.991939	272855.422404	43.747879
3501.730566	272844.081881	43.752884
3502.026866	272845.359705	43.757889
3502.029832	272827.077653	43.762893
3502.096993	272801.477967	43.767898
3501.777036	272809.752340	43.772903
3501.755998	272804.637891	43.777908
3501.944528	272781.056183	43.782913
3501.794427	272775.376283	43.787917
3501.956138	272766.235725	43.792922
3502.007559	272766.889822	43.797927
3501.903788	272751.297953	43.802932
3501.912800	272740.959088	43.807937
3501.706242	272734.091297	43.812941
3502.241295	272718.628706	43.817946
3501.770253	272730.313157	43.822951
3501.938738	272707.625735	43.827956
3501.633247	272692.192702	43.832961
3501.757027	272690.976759	43.837965
3501.967393	272678.594905	43.842970
3501.652048	272682.871029	43.847975
3502.010310	272671.713692	43.852980
3501.941490	272661.998074	43.857985
3501.791694	272646.999009	43.862989
3501.967137	272641.751984	43.867994
3501.781821	272635.950270	43.872999
3501.716949	272610.498479	43.878004
3501.832709	272596.578219	43.883009
3502.021056	272605.587929	43.888013
3501.965616	272597.856253	43.893018
3502.056594	272594.302927	43.898023
3501.975745	272567.707828	43.903028
3502.070082	272556.566276	43.908033
3501.709046	272561.638874	43.913037
3501.865883	272567.470755	43.918042
3502.050160	272552.393982	43.923047
3502.074151	272543.453166	43.928052
3502.163315	272533.076282	43.933057
3502.033565	272525.890921	43.938061
3502.105617	272499.220973	43.943066
3502.088843	272497.772380	43.948071
3502.095891	272481.781205	43.953076
3501.982049	272469.781016	43.958081
3501.927305	272455.429071	43.963085
3502.028364	272443.038811	43.968090
3501.956530	272453.285933	43.973095
3501.840385	272433.698390	43.978100
3502.476237	272416.972344	43.983105
3502.274882	272406.666327	43.988109
3502.450741	272391.005213	43.993114
3502.275755	272378.479866	43.998119
3502.104340	272364.910011	44.003124
3502.469196	272344.050528	44.008129
3502.002851	272333.276688	44.013133
3502.204186	272325.021063	44.018138
3502.040013	272317.000815	44.023143
3502.069470	272290.159226	44.028148
3501.876191	272289.833098	44.033153
3501.679617	272280.417494	44.038157
3502.105988	272255.856359	44.043162
3501.733279	272259.886851	44.048167
3502.117149	272257.611752	44.053172
3502.025096	272236.874601	44.058177
3502.135656	272231.612232	44.063181
3502.449452	272215.318430	44.068186
3501.923654	272204.121012	44.073191
3502.008885	272189.416132	44.078196
3501.540937	272181.850759	44.083201
3502.040228	272176.069294	44.088205
3502.019946	272166.829813	44.093210
3501.854034	272159.675538	44.098215
3501.576462	272145.893085	44.103220
3501.991081	272132.638968	44.108225
3502.126684	272135.647894	44.113229
3502.061042	272122.188776	44.118234
3501.996638	272102.771304	44.123239
3501.735310	272106.147834	44.128244
3502.200011	272086.800412	44.133249
3502.064029	272085.981542	44.138253
3502.073439	272054.814438	44.143258
3502.196308	272053.675015	44.148263
3502.118610	272047.780050	44.153268
3502.136897	272029.342662	44.158273
3501.830663	272018.009044	44.163277
3502.032045	272016.628185	44.168282
3502.299516	272007.623786	44.173287
3502.190542	271978.919537	44.178292
3502.478917	271969.046149	44.183297
3501.797062	271968.592705	44.188301
3502.043805	271933.976512	44.193306
3501.630983	271936.358242	44.198311
3501.690602	271928.455745	44.203316
3501.967042	271928.514499	44.208321
3501.841281	271918.578540	44.213325
3501.902470	271904.921323	44.218330
3502.109932	271889.637113	44.223335
3501.910467	271889.490186	44.228340
3502.299316	271877.258550	44.233345
3501.665079	271860.832812	44.238349
3501.905844	271852.978374	44.243354
3501.757094	271844.599200	44.248359
3501.983076	271836.696148	44.253364
3502.163871	271818.131459	44.258369
3501.805470	271813.578940	44.263373
3502.024783	271815.530836	44.268378
3502.041401	271812.625660	44.273383
3502.121608	271788.805996	44.278388
3502.036696	271778.176152	44.283393
3501.628789	271775.082723	44.288397
3501.911004	271761.849250	44.293402
3501.708646	271745.712443	44.298407
3501.830747	271727.818931	44.303412
3501.805657	271725.582293	44.308417
3502.276853	271731.568782	44.313421
3501.815302	271717.305779	44.318426
3501.480700	271694.773132	44.323431
3501.801574	271693.933758	44.328436
3502.168619	271685.244769	44.333441
3501.344467	271691.535625	44.338445
3501.634582	271681.661932	44.343450
3501.808319	271684.181128	44.348455
3501.868417	271677.933585	44.353460
3501.762047	271654.474064	44.358465
3501.782590	271648.945648	44.363469
3502.065104	271645.566037	44.368474
3501.959437	271646.830336	44.373479
3501.755020	271644.392571	44.378484
3502.069201	271620.358045	44.383489
3501.641009	271610.800344	44.388493
3501.933785	271603.447000	44.393498
3501.881231	271601.265577	44.398503
3501.874061	271590.190697	44.403508
3502.166077	271573.034460	44.408513
3501.418147	271575.825064	44.413517
3501.708925	271564.627212	44.418522
3502.082100	271562.837553	44.423527
3501.722783	271539.213848	44.428532
3501.745243	271532.462931	44.433537
3501.427388	271536.535804	44.438541
3501.796517	271522.804922	44.443546
3501.743732	271524.570203	44.448551
3501.784415	271532.762852	44.453556
3501.789910	271507.681673	44.458561
3501.747248	271493.556843	44.463565
3501.392002	271494.019905	44.468570
3501.592055	271485.713476	44.473575
3501.663152	271486.211733	44.478580
3502.136248	271477.073282	44.483585
3501.797804	271476.158747	44.488589
3502.174192	271456.621295	44.493594
3501.949670	271448.228467	44.498599
3501.888115	271443.145734	44.503604
3501.759695	271439.397500	44.508609
3501.621573	271421.086286	44.513613
3501.914602	271408.869566	44.518618
3501.975622	271406.874082	44.523623
3502.098397	271404.181458	44.528628
3501.947866	271391.524834	44.533633
3501.898597	271378.419515	44.538637
3501.955761	271376.297321	44.543642
3501.993167	271372.752321	44.548647
3501.706353	271365.260408	44.553652
3501.750699	271343.483224	44.558657
3501.651175	271334.205120	44.563661
3502.302903	271324.045691	44.568666
3501.922248	271322.195645	44.573671
3501.558003	271320.623119	44.578676
3501.649203	271301.817704	44.583681
3501.419071	271293.323889	44.588685
3501.345762	271289.974431	44.593690
3501.805916	271284.071714	44.598695
3501.752336	271285.684349	44.603700
3501.825426	271280.453245	44.608705
3502.037964	271282.889998	44.613709
3502.326482	271265.759711	44.618714
3502.118241	271257.033307	44.623719
3501.397450	271257.808144	44.628724
3501.725330	271248.183124	44.633729
3501.837673	271248.063834	44.638733
3501.750852	271229.057074	44.643738
3501.705460	271223.004228	44.648743
3501.877012	271210.730085	44.653748
3501.755775	271205.682132	44.658753
3501.684425	271210.607668	44.663757
3502.180227	271195.252796	44.668762
3501.814769	271182.171419	44.673767
3501.644980	271172.318646	44.678772
3501.925354	271168.862964	44.683777
3501.537917	271169.254673	44.688781
3501.920186	271163.211349	44.693786
3501.578452	271141.876413	44.698791
3501.760152	271134.565858	44.703796
3501.942096	271127.637202	44.708801
3501.744524	271130.672788	44.713805
3501.787238	271128.705623	44.718810
3501.771333	271122.037060	44.723815
3501.584502	271106.203258	44.728820
3501.536332	271088.285313	44.733825
3501.585739	271092.097088	44.738829
3501.893042	271085.301605	44.743834
3501.845603	271088.568346	44.748839
3501.465553	271079.410461	44.753844
3501.623944	271082.135772	44.758849
3501.458457	271092.423158	44.763853
3501.898121	271067.401289	44.768858
3501.634383	271052.954477	44.773863
3501.649796	271049.845765	44.778868
3501.792292	271045.163970	44.783873
3501.408260	271044.842196	44.788877
3501.787694	271033.146629	44.793882
3501.926443	271042.928131	44.798887
3501.804227	271027.644388	44.803892
3502.070906	271007.156413	44.808897
3502.042982	271007.975704	44.813901
3502.054817	271007.668427	44.818906
3501.601231	270983.575524	44.823911
3501.562807	270968.813385	44.828916
3501.924369	270960.634433	44.833921
3501.883356	270962.372421	44.838925
3501.726925	270959.774360	44.843930
3501.677988	270963.423278	44.848935
3501.706306	270944.958633	44.853940
3501.833500	270925.587335	44.858945
3501.819539	270926.353518	44.863949
3502.193595	270923.672520	44.868954
3501.967692	270924.140825	44.873959
3501.509744	270910.513692	44.878964
3501.943166	270892.749578	44.883969
3501.747733	270891.507128	44.888973
3501.784041	270880.578137	44.893978
3501.942406	270883.354384	44.898983
3501.785092	270872.939451	44.903988
3501.804846	270852.439120	44.908993
3502.016902	270848.001067	44.913997
3502.103965	270841.825637	44.919002
3501.924106	270844.272824	44.924007
3501.747161	270810.409921	44.929012
3501.968184	270806.326940	44.934017
3501.841810	270805.455630	44.939021
3501.785978	270803.733028	44.944026
3501.569880	270793.301814	44.949031
3501.594028	270772.724389	44.954036
3501.919980	270769.567118	44.959041
3501.503079	270765.303779	44.964045
3501.854570	270756.362505	44.969050
3502.075320	270767.633509	44.974055
3501.342924	270751.553925	44.979060
3501.712086	270728.172590	44.984065
3501.709094	270738.358224	44.989069
3501.816745	270720.619544	44.994074
3501.529455	270724.534900	44.999079
3501.590584	270720.578762	45.004084
3501.913768	270721.215850	45.009089
3501.665046	270720.287280	45.014093
3501.870575	270705.385108	45.019098
3501.548735	270692.169526	45.024103
3501.663117	270688.841628	45.029108
3501.550018	270684.938191	45.034113
3501.626133	270692.819826	45.039117
3501.630186	270686.300887	45.044122
3502.120598	270676.497619	45.049127
3501.831171	270664.651948	45.054132
3502.109014	270646.224617	45.059137
3501.927456	270658.169636	45.064141
3502.149421	270647.848156	45.069146
3501.883673	270629.582196	45.074151
3501.464165	270619.208225	45.079156
3501.751319	270616.999132	45.084161
3501.651103	270616.072806	45.089165
3501.320715	270618.212519	45.094170
3501.504021	270608.559108	45.099175
3501.834171	270603.975266	45.104180
3501.869074	270607.178226	45.109185
3501.688613	270592.540082	45.114189
3501.934379	270578.166313	45.119194
3501.906460	270576.362954	45.124199
3501.426827	270575.623259	45.129204
3501.699732	270572.296035	45.134209
3501.678327	270576.628156	45.139213
3501.642972	270543.532358	45.144218
3501.544705	270543.064055	45.149223
3501.777401	270535.669090	45.154228
3502.052807	270524.728138	45.159233
3501.598820	270528.440400	45.164237
3501.706616	270528.703760	45.169242
3501.669830	270517.633376	45.174247
3501.565675	270506.293435	45.179252
3501.809635	270492.047248	45.184257
3501.866280	270491.834814	45.189261
3502.275924	270481.560362	45.194266
3501.866160	270486.538845	45.199271
3501.897819	270467.487937	45.204276
3502.060927	270450.326176	45.209281
3501.464203	270455.563054	45.214285
3501.611278	270453.044842	45.219290
3501.812001	270446.011346	45.224295
3501.817909	270438.397204	45.229300
3501.705470	270420.107232	45.234305
3501.850080	270411.198267	45.239309
3501.620514	270407.669504	45.244314
3501.855449	270407.989376	45.249319
3501.748895	270411.901952	45.254324
3502.150061	270394.193708	45.259329
3501.693854	270384.054612	45.264333
3501.630413	270369.678226	45.269338
3502.114106	270361.989380	45.274343
3501.614405	270367.414796	45.279348
3501.515141	270350.650513	45.284353
3501.557096	270343.234428	45.289357
3501.603214	270323.137258	45.294362
3501.585022	270322.783748	45.299367
3501.669860	270326.284464	45.304372
3501.771653	270332.456114	45.309377
3501.813852	270316.713680	45.314381
3502.186466	270316.044444	45.319386
3501.954109	270296.321820	45.324391
3501.622948	270293.038101	45.329396
3501.896826	270285.152886	45.334401
3501.560707	270285.689351	45.339405
3501.963444	270283.131164	45.344410
3501.627029	270266.836808	45.349415
3501.522361	270254.783958	45.354420
3501.776736	270249.320749	45.359425
3501.431737	270240.615627	45.364429
3501.797546	270247.458964	45.369434
3501.471194	270245.880494	45.374439
3501.471754	270248.961523	45.379444
3501.604255	270243.364591	45.384449
3501.536290	270245.004956	45.389453
3501.583837	270231.629706	45.394458
3501.861172	270222.929138	45.399463
3501.683215	270210.251171	45.404468
3501.863485	270200.572728	45.409473
3501.824042	270208.752563	45.414477
3501.428338	270211.742768	45.419482
3501.525203	270214.706890	45.424487
3501.230761	270196.343477	45.429492
3501.306631	270174.230064	45.434497
3501.838086	270185.987284	45.439501
3501.724047	270171.771554	45.444506
3501.877141	270168.539435	45.449511
3501.586845	270169.756231	45.454516
3501.840989	270168.239782	45.459521
3501.564943	270167.086313	45.464525
3501.654041	270155.970742	45.469530
3501.733563	270138.745601	45.474535
3501.879514	270124.540142	45.479540
3501.522418	270122.609998	45.484545
3501.694160	270114.307869	45.489549
3501.912909	270107.806248	45.494554
3501.800369	270114.979008	45.499559
3501.809933	270105.276318	45.504564
3502.035305	270086.398747	45.509569
3501.861781	270082.275565	45.514573
3501.897256	270075.624355	45.519578
3501.817682	270076.095250	45.524583
3501.754600	270057.517399	45.529588
3502.181922	270047.596613	45.534593
3501.856083	270050.219421	45.539597
3501.696936	270039.117184	45.544602
3501.777463	270036.431124	45.549607
3501.915620	270011.685266	45.554612
3502.038242	270009.298178	45.559617
3501.807466	270008.188555	45.564621
3502.242168	270007.025817	45.569626
3502.045756	269995.547458	45.574631
3501.722241	269991.778739	45.579636
3502.381830	269980.701269	45.584641
3501.816290	269966.250541	45.589645
3501.914856	269947.520081	45.594650
3502.166816	269931.210066	45.599655
3501.712550	269944.190864	45.604660
3501.893831	269929.878000	45.609665
3501.655920	269911.683931	45.614669
3501.921784	269901.533744	45.619674
3501.912437	269890.458994	45.624679
3501.920325	269893.691665	45.629684
3502.043309	269892.323032	45.634689
3501.716627	269874.855793	45.639693
3501.762045	269864.867380	45.644698
3501.999550	269863.531768	45.649703
3501.761617	269859.316794	45.654708
3501.883751	269843.969187	45.659713
3501.595126	269838.361681	45.664717
3501.771750	269822.037963	45.669722
3501.591187	269819.800121	45.674727
3501.470494	269820.633926	45.679732
3501.848368	269810.313440	45.684737
3501.201278	269816.118412	45.689741
3501.650859	269821.777392	45.694746
3501.823851	269819.687979	45.699751
3501.651278	269804.080885	45.704756
3501.856172	269786.963391	45.709761
3501.389996	269792.409063	45.714765
3501.495320	269775.841855	45.719770
3501.796971	269785.572561	45.724775
3501.582705	269770.608552	45.729780
3501.681672	269765.882572	45.734785
3501.473400	269767.672195	45.739789
3501.654755	269756.694929	45.744794
3501.821166	269739.023260	45.749799
3501.478857	269734.519045	45.754804
3501.644887	269726.319625	45.759809
3501.740088	269729.996984	45.764813
3501.696778	269704.973859	45.769818
3501.914070	269662.187805	45.774823
3501.724324	269551.148337	45.779828
3501.692599	269409.757633	45.784833
3501.451924	269228.116884	45.789837
3500.983974	268986.265660	45.794842
3501.310939	268697.131754	45.799847
3500.584673	268381.374283	45.804852
3500.325236	267996.868124	45.809857
3499.765201	267576.860418	45.814861
3499.282570	267103.085152	45.819866
3498.841822	266592.582351	45.824871
3498.367424	266034.413823	45.829876
3498.021482	265432.729564	45.834881
3497.276191	264791.863883	45.839885
3496.984751	264105.571277	45.844890
3496.104160	263364.286544	45.849895
3495.099434	262576.899508	45.854900
3494.517308	261754.324642	45.859905
3493.302598	260877.423727	45.864909
3492.633493	259964.932181	45.869914
3492.005183	259005.697991	45.874919
3490.508495	258015.218209	45.879924
3489.984660	256967.254686	45.884929
3488.805915	255882.662868	45.889933
3487.573043	254745.228033	45.894938
3486.296401	253577.791097	45.899943
3484.848141	252378.257950	45.904948
3483.866382	251124.499539	45.909953
3482.475982	249831.957619	45.914957
3480.979746	248499.438413	45.919962
3479.500142	247133.696790	45.924967
3478.183521	245728.546543	45.929972
3477.014787	244277.597401	45.934977
3475.163663	242802.448560	45.939981
3473.335157	241274.287378	45.944986
3471.921056	239719.412274	45.949991
3470.233550	238129.679430	45.954996
3468.089298	236507.792144	45.960001
3465.974239	234850.236738	45.965005
3464.856783	233153.347761	45.970010
3462.963312	231427.183350	45.975015
3460.644912	229670.594438	45.980020
3458.762792	227872.241121	45.985025
3456.621328	226053.652858	45.990029
3454.652677	224200.373490	45.995034
3452.456096	222319.776844	46.000039
3450.130601	220404.539537	46.005044
3447.816850	218468.522045	46.010049
3445.257923	216504.023956	46.015053
3443.170590	214515.010371	46.020058
3440.324159	212497.117100	46.025063
3437.786834	210472.337140	46.030068
3435.611950	208401.876274	46.035073
3432.874967	206328.260985	46.040077
3430.435831	204211.909633	46.045082
3427.851457	202077.955051	46.050087
3425.005411	199933.803880	46.055092
3422.252191	197760.838256	46.060097
3419.570391	195570.525093	46.065101
3416.198628	193352.622176	46.070106
3413.471821	191122.025855	46.075111
3410.247890	188886.481183	46.080116
3407.673673	186619.965475	46.085121
3404.637546	184343.384893	46.090125
3401.426025	182043.457303	46.095130
3398.264352	179726.696020	46.100135
3394.563846	177411.071689	46.105140
3391.343923	175075.384162	46.110145
3387.846296	172740.850819	46.115149
3384.286861	170394.354632	46.120154
3381.235494	168038.904028	46.125159
3377.105206	165685.672701	46.130164
3373.254851	163317.636735	46.135169
3369.957611	160947.982736	46.140173
3366.594055	158583.212983	46.145178
3362.607243	156209.379233	46.150183
3358.383875	153821.576559	46.155188
3354.440524	151453.555134	46.160193
3350.004079	149080.825458	46.165197
3345.783277	146714.783974	46.170202
3341.642164	144360.175030	46.175207
3336.972063	142011.827802	46.180212
3333.037606	139662.956282	46.185217
3328.154169	137337.274711	46.190221
3323.250634	134966.855452	46.195226
3318.600830	132620.894554	46.200231
3313.436120	130333.259043	46.205236
3309.071539	128077.801315	46.210241
3303.376048	125844.130021	46.215245
3298.186467	123630.787131	46.220250
3292.580395	121446.996701	46.225255
3286.708345	119297.133014	46.230260
3280.443953	117189.541889	46.235265
3273.970801	115125.067320	46.240269
3267.289064	113114.702766	46.245274
3260.685872	111153.043752	46.250279
3254.021561	109244.568504	46.255284
3247.205257	107386.652798	46.260289
3239.572952	105595.894462	46.265293
3232.562376	103871.996064	46.270298
3225.291873	102211.107969	46.275303
3217.443448	100630.138262	46.280308
3209.610299	99107.987144	46.285313
3201.814304	97673.925755	46.290317
3193.878087	96302.731401	46.295322
3185.945548	95009.191736	46.300327
3177.537567	93817.809387	46.305332
3170.052388	92694.146702	46.310337
3162.268431	91652.250675	46.315341
3155.282651	90657.596515	46.320346
3147.946716	89755.274821	46.325351
3140.938408	88910.154913	46.330356
3134.673080	88125.902480	46.335361
3127.951666	87411.987629	46.340365
3121.916155	86727.800598	46.345370
3115.934430	86117.192061	46.350375
3110.192762	85547.427909	46.355380
3105.005618	85015.267939	46.360385
3099.813861	84530.846161	46.365389
3095.211863	84056.896882	46.370394
3090.679239	83625.170240	46.375399
3086.082690	83226.780322	46.380404
3082.510996	82836.657740	46.385409
3078.203971	82462.660966	46.390413
3074.070229	82108.115106	46.395418
3070.528157	81765.192816	46.400423
3066.406563	81443.146277	46.405428
3062.734430	81121.668241	46.410433
3058.760494	80826.115093	46.415437
3055.668291	80532.815130	46.420442
3052.044774	80235.270025	46.425447
3048.323990	79953.404406	46.430452
3044.921313	79665.369768	46.435457
3041.397001	79387.873868	46.440461
3038.058782	79109.297436	46.445466
3034.597778	78829.663409	46.450471
3031.100813	78564.732883	46.455476
3028.377206	78286.576658	46.460481
3024.788994	78015.835974	46.465485
3021.538773	77739.037706	46.470490
3017.995393	77456.191839	46.475495
3014.370011	77183.712507	46.480500
3011.302631	76909.027688	46.485505
3007.500713	76644.125285	46.490509
3004.026781	76370.550877	46.495514
3000.865654	76103.864423	46.500519
2996.974817	75841.726913	46.505524
2993.728247	75571.553929	46.510529
2990.209407	75306.620310	46.515533
2986.892096	75033.961964	46.520538
2983.527251	74767.015763	46.525543
2979.425841	74500.225498	46.530548
2976.494882	74234.308856	46.535553
2972.618128	73977.076394	46.540557
2969.331914	73719.233404	46.545562
2965.869487	73454.360032	46.550567
2961.978790	73198.496003	46.555572
2958.684118	72936.204739	46.560577
2954.443598	72681.149602	46.565581
2951.275066	72430.830748	46.570586
2947.466375	72178.252545	46.575591
2943.484034	71930.960838	46.580596
2940.207325	71683.713469	46.585601
2936.251010	71451.519837	46.590605
2932.518633	71211.865175	46.595610
2929.085300	70968.217036	46.600615
2925.376492	70750.288199	46.605620
2921.990288	70505.532327	46.610625
2918.461143	70291.489954	46.615629
2914.783986	70058.401617	46.620634
2911.116789	69835.045957	46.625639
2907.086072	69623.411046	46.630644
2903.874724	69396.826367	46.635649
2899.659442	69185.604794	46.640653
2896.272677	68968.008718	46.645658
2892.638973	68759.943609	46.650663
2889.006146	68571.089463	46.655668
2885.413800	68361.307108	46.660673
2881.928166	68162.212542	46.665677
2878.031337	67967.830546	46.670682
2874.563794	67764.057778	46.675687
2870.800230	67574.279215	46.680692
2868.008300	67365.084430	46.685697
2863.596351	67193.622025	46.690701
2860.331150	66991.912180	46.695706
2856.702766	66814.413688	46.700711
2852.774710	66631.358329	46.705716
2849.624162	66448.944400	46.710721
2846.048139	66260.847438	46.715725
2842.379055	66081.056270	46.720730
2838.869583	65897.248860	46.725735
2835.112090	65726.144677	46.730740
2831.778146	65535.241418	46.735745
2828.363566	65370.319135	46.740749
2824.836909	65194.022074	46.745754
2821.290688	65006.202715	46.750759
2817.624982	64830.951849	46.755764
2814.753099	64661.188934	46.760769
2810.808449	64480.379604	46.765773
2807.471314	64310.101547	46.770778
2804.533316	64127.055485	46.775783
2800.615846	63950.422068	46.780788
2797.345077	63763.597137	46.785793
2793.313913	63582.490480	46.790797
2789.975866	63408.531167	46.795802
2786.241118	63232.337574	46.800807
2783.157285	63059.553176	46.805812
2779.704887	62881.204442	46.810817
2776.081275	62714.796448	46.815821
2772.805173	62533.782426	46.820826
2769.431006	62356.808788	46.825831
2765.719190	62169.772867	46.830836
2761.818628	61993.341110	46.835841
2758.358361	61819.735722	46.840845
2755.212121	61637.254616	46.845850
2752.023287	61461.971925	46.850855
2748.231513	61286.689591	46.855860
2745.152989	61091.420501	46.860865
2741.361174	60916.039277	46.865869
2738.266358	60739.680868	46.870874
2734.660336	60558.644103	46.875879
2730.929683	60370.203279	46.880884
2727.882759	60185.997638	46.885889
2724.166648	60006.892325	46.890893
2720.524787	59810.845808	46.895898
2717.388173	59633.270810	46.900903
2713.829250	59437.277784	46.905908
2710.268348	59262.716311	46.910913
2706.390578	59088.351607	46.915917
2703.126922	58895.959213	46.920922
2699.644305	58708.323740	46.925927
2695.776203	58527.603242	46.930932
2692.813055	58331.729022	46.935937
2689.274065	58156.144122	46.940941
2685.058657	57964.402950	46.945946
2681.845267	57781.885055	46.950951
2678.225682	57593.537259	46.955956
2674.912032	57422.681463	46.960961
2671.457361	57246.899649	46.965965
2668.088029	57050.598104	46.970970
2664.565836	56860.489552	46.975975
2660.903829	56683.018425	46.980980
2657.516206	56495.030026	46.985985
2654.015313	56311.686325	46.990989
2650.526485	56131.647864	46.995994
2646.970647	55948.302861	47.000999
2643.729085	55766.965845	47.006004
2640.314140	55576.527158	47.011009
2636.648596	55387.924761	47.016013
2633.194690	55193.269637	47.021018
2629.793951	55007.725056	47.026023
2626.117066	54835.682026	47.031028
2622.688296	54634.467244	47.036033
2619.164012	54445.780465	47.041037
2615.829702	54259.209905	47.046042
2612.212383	54068.681771	47.051047
2609.124995	53882.703663	47.056052
2605.495662	53681.763122	47.061057
2601.675770	53501.396768	47.066061
2598.324605	53303.594420	47.071066
2595.178932	53117.136643	47.076071
2591.444710	52931.406820	47.081076
2588.065261	52731.126846	47.086081
2584.337016	52543.242201	47.091085
2580.646112	52354.934528	47.096090
2577.390667	52150.605394	47.101095
2573.812289	51963.755062	47.106100
2570.322270	51768.486903	47.111105
2566.885430	51580.107697	47.116109
2563.633781	51385.535000	47.121114
2560.016905	51182.983701	47.126119
2556.316179	51004.806583	47.131124
2552.924205	50795.213855	47.136129
2549.507537	50611.286177	47.141133
2545.565599	50417.089686	47.146138
2542.397105	50217.680134	47.151143
2538.388516	50024.017539	47.156148
2535.121376	49834.046544	47.161153
2531.543366	49649.257393	47.166157
2528.276420	49452.185147	47.171162
2525.002737	49255.261539	47.176167
2521.209593	49074.265786	47.181172
2518.045113	48866.729223	47.186177
2514.352814	48683.196287	47.191181
2510.958446	48498.007133	47.196186
2507.352974	48286.238016	47.201191
2503.913972	48093.060840	47.206196
2500.161054	47890.896046	47.211201
2496.771760	47711.636590	47.216205
2493.128297	47501.834263	47.221210
2489.800269	47314.659137	47.226215
2486.335644	47127.836737	47.231220
2483.091669	46913.588359	47.236225
2479.695351	46725.122253	47.241229
2476.001193	46525.916008	47.246234
2472.774298	46319.002333	47.251239
2468.795762	46129.947316	47.256244
2465.457800	45930.956988	47.261249
2461.970540	45742.589439	47.266253
2458.568860	45536.534781	47.271258
2454.462826	45336.623437	47.276263
2451.260617	45134.746013	47.281268
2447.830704	44940.471895	47.286273
2444.307076	44752.245206	47.291277
2440.410407	44549.156268	47.296282
2437.478651	44353.033640	47.301287
2433.861106	44158.954225	47.306292
2430.913336	43962.133620	47.311297
2427.296697	43751.753358	47.316301
2424.016473	43564.709873	47.321306
2420.278113	43353.306085	47.326311
2416.229979	43152.631648	47.331316
2412.724733	42950.840471	47.336321
2409.224512	42746.050935	47.341325
2405.762841	42546.571195	47.346330
2402.247194	42355.985648	47.351335
2398.530308	42155.281148	47.356340
2395.153971	41950.936182	47.361345
2391.798154	41759.798152	47.366349
2388.441785	41557.749153	47.371354
2384.719397	41356.868925	47.376359
2381.210582	41164.618666	47.381364
2378.071119	40966.478828	47.386369
2374.203302	40765.848707	47.391373
2371.152961	40561.161356	47.396378
2367.486867	40358.753408	47.401383
2364.144859	40157.380870	47.406388
2360.673698	39947.267897	47.411393
2357.142491	39748.686838	47.416397
2353.655730	39547.069964	47.421402
2349.949123	39334.539706	47.426407
2346.424446	39130.206325	47.431412
2343.068507	38929.259479	47.436417
2339.480765	38723.145549	47.441421
2336.241651	38522.139833	47.446426
2332.583516	38312.889839	47.451431
2328.976899	38108.103456	47.456436
2326.257680	37893.245648	47.461441
2322.189509	37694.450493	47.466445
2318.814145	37485.551039	47.471450
2315.097056	37273.638683	47.476455
2311.680195	37072.217880	47.481460
2308.131679	36856.745778	47.486465
2304.310611	36660.127734	47.491469
2301.385156	36445.462513	47.496474
2298.015923	36239.293887	47.501479
2294.381558	36019.837194	47.506484
2291.026023	35810.317092	47.511489
2287.408039	35606.399570	47.516493
2283.555237	35392.669766	47.521498
2280.166032	35178.140599	47.526503
2276.548077	34974.127731	47.531508
2273.185378	34762.660357	47.536513
2269.667395	34556.315836	47.541517
2266.103156	34347.825378	47.546522
2262.898319	34127.401969	47.551527
2259.103008	33919.953416	47.556532
2255.753789	33694.670013	47.561537
2252.414837	33495.705024	47.566541
2248.650309	33277.292329	47.571546
2245.691896	33065.284355	47.576551
2241.800176	32849.653227	47.581556
2238.657737	32632.018289	47.586561
2235.014842	32420.979599	47.591565
2231.269296	32202.911080	47.596570
2227.761710	31994.137275	47.601575
2224.526670	31766.999705	47.606580
2221.033118	31541.647996	47.611585
2217.757295	31337.452212	47.616589
2214.095542	31112.112466	47.621594
2210.877867	30887.041592	47.626599
2207.108511	30666.020529	47.631604
2203.976631	30437.461733	47.636609
2199.861152	30226.652380	47.641613
2196.399859	30013.803563	47.646618
2193.223502	29787.578441	47.651623
2189.718785	29572.256715	47.656628
2186.559826	29335.247681	47.661633
2182.636354	29135.262550	47.666637
2179.080034	28895.469017	47.671642
2176.189221	28664.997384	47.676647
2172.425374	28445.532888	47.681652
2169.414667	28214.527429	47.686657
2165.781648	27979.369916	47.691661
2162.336260	27744.128727	47.696666
2158.607665	27517.843981	47.701671
2155.266769	27288.421485	47.706676
2151.555731	27041.564228	47.711681
2148.041195	26816.654179	47.716685
2144.842438	26579.271495	47.721690
2141.485814	26342.847734	47.726695
2137.875426	26117.529575	47.731700
2134.454738	25875.393312	47.736705
2130.591648	25635.863622	47.741709
2127.062908	25407.676689	47.746714
2123.778183	25163.867653	47.751719
2120.238809	24938.165076	47.756724
2116.801073	24698.738391	47.761729
2113.169546	24461.251948	47.766733
2110.208065	24222.282303	47.771738
2106.999422	23979.102992	47.776743
2103.324602	23742.943316	47.781748
2099.745225	23481.226967	47.786753
2095.943481	23249.673520	47.791757
2092.598864	23004.322653	47.796762
2089.212439	22764.005182	47.801767
2085.495189	22519.972972	47.806772
2082.223227	22282.310516	47.811777
2078.484235	22041.816225	47.816781
2074.827893	21800.038608	47.821786
2071.261049	21546.302452	47.826791
2067.699853	21318.585504	47.831796
2064.542323	21063.220495	47.836801
2060.689851	20826.401206	47.841805
2056.885710	20589.919273	47.846810
2053.516219	20345.941873	47.851815
2049.354257	20113.759409	47.856820
2046.316814	19877.349796	47.861825
2042.766944	19659.449464	47.866829
2038.917900	19429.170769	47.871834
2035.249236	19200.551430	47.876839
2030.672163	19000.054213	47.881844
2026.421126	18802.174641	47.886849
2021.911302	18623.636923	47.891853
2017.314813	18439.242952	47.896858
2014.003005	18259.355709	47.901863
2009.904988	18094.167029	47.906868
2006.464521	17922.441872	47.911873
2003.122204	17762.439051	47.916877
1999.421373	17600.352912	47.921882
1996.021716	17450.672676	47.926887
1992.393946	17293.137811	47.931892
1989.468297	17118.007853	47.936897
1985.744792	16965.905698	47.941901
1982.073622	16808.676088	47.946906
1978.894695	16655.500015	47.951911
1975.385970	16495.172760	47.956916
1971.850067	16332.279843	47.961921
1968.497878	16173.311408	47.966925
1965.006380	16012.605506	47.971930
1961.734246	15847.170722	47.976935
1958.417571	15695.303132	47.981940
1955.510122	15537.502136	47.986945
1951.317451	15371.306744	47.991949
1948.171159	15201.380549	47.996954
1944.746775	15025.131844	48.001959
1941.377467	14870.641476	48.006964
1938.039444	14693.882039	48.011969
1933.951967	14526.303383	48.016973
1931.180836	14358.862176	48.021978
1928.174185	14195.467726	48.026983
1924.386474	14018.968568	48.031988
1920.966153	13843.629367	48.036993
1916.913414	13675.543034	48.041997
1913.654807	13510.142260	48.047002
1910.361725	13327.391912	48.052007
1906.701197	13168.522137	48.057012
1903.089864	12986.572069	48.062017
1899.502453	12821.279429	48.067021
1896.147501	12649.126054	48.072026
1893.084469	12466.940063	48.077031
1889.233161	12306.233177	48.082036
1886.009560	12124.005979	48.087041
1882.474400	11948.572541	48.092045
1878.498334	11780.342311	48.097050
1874.941259	11588.102044	48.102055
1871.790208	11418.476477	48.107060
1868.049535	11251.575430	48.112065
1864.941233	11086.517485	48.117069
1861.703797	10910.300065	48.122074
1858.059237	10729.940884	48.127079
1854.696707	10548.013489	48.132084
1850.960562	10363.202348	48.137089
1847.368028	10196.667411	48.142093
1843.936731	10017.889838	48.147098
1840.633583	9837.314923	48.152103
1836.428155	9668.250109	48.157108
1833.512410	9481.853726	48.162113
1829.852925	9314.685087	48.167117
1826.251595	9140.602023	48.172122
1823.162015	8964.474835	48.177127
1819.072121	8781.007251	48.182132
1816.049913	8604.664030	48.187137
1812.359821	8424.654036	48.192141
1808.884171	8251.604196	48.197146
1805.831420	8068.867635	48.202151
1802.121049	7889.644666	48.207156
1798.716659	7705.703835	48.212161
1795.260043	7534.363747	48.217165
1791.622022	7338.647858	48.222170
1788.377043	7169.582211	48.227175
1784.645034	6984.642740	48.232180
1781.480776	6805.484131	48.237185
1777.713655	6620.224671	48.242189
1774.393110	6442.575256	48.247194
1770.568037	6255.198577	48.252199
1766.849332	6077.573872	48.257204
1763.448143	5890.621979	48.262209
1759.799099	5719.433410	48.267213
1756.560284	5531.326793	48.272218
1753.086614	5349.825655	48.277223
1748.883917	5171.706372	48.282228
1746.033972	4994.908824	48.287233
1742.494162	4815.265197	48.292237
1738.682075	4642.878066	48.297242
1735.375184	4455.653990	48.302247
1731.818652	4275.309462	48.307252
1728.657846	4103.480590	48.312257
1725.024642	3920.471262	48.317261
1721.594482	3735.517525	48.322266
1717.763969	3552.454196	48.327271
1714.648422	3375.163399	48.332276
1710.966892	3195.238421	48.337281
1707.248768	3007.068447	48.342285
1703.425035	2836.042035	48.347290
1700.099962	2654.013059	48.352295
1696.319335	2483.369293	48.357300
1693.415536	2298.439683	48.362305
1689.792590	2128.597298	48.367309
1685.849717	1946.232364	48.372314
1682.633974	1778.750118	48.377319
1678.945305	1606.977045	48.382324
1675.386347	1417.577489	48.387329
1671.734162	1248.194159	48.392333
1668.168537	1075.846905	48.397338
1664.512477	904.989864	48.402343
1660.925870	739.056126	48.407348
1657.355798	570.818040	48.412353
1653.668341	413.973960	48.417357
1649.643906	250.786753	48.422362
1645.913652	100.434815	48.427367
1639.843574	10.698126	48.432372
1629.825290	59.204120	48.437377
1623.414311	65.503813	48.442381
1618.407689	67.641632	48.447386
1615.641408	56.064968	48.452391
1613.010189	66.066353	48.457396
1610.502533	61.096333	48.462401
1608.173002	57.560107	48.467405
1605.062909	54.892703	48.472410
1601.975396	63.671515	48.477415
1598.519416	58.897381	48.482420
1594.941711	61.305117	48.487425
1591.494033	59.576414	48.492429
1587.852244	58.839886	48.497434
1584.956243	56.929927	48.502439
1581.455811	68.310731	48.507444
1578.210773	53.831890	48.512449
1575.210154	63.457658	48.517453
1570.995694	69.125689	48.522458
1567.376187	65.101668	48.527463
1563.928841	69.681516	48.532468
1560.790952	61.421735	48.537473
1557.348750	66.718960	48.542477
1553.530826	68.417654	48.547482
1550.527110	61.244203	48.552487
1546.951313	60.228438	48.557492
1543.678356	53.960847	48.562497
1540.265726	60.636021	48.567501
1536.636204	63.074033	48.572506
1533.255993	64.656767	48.577511
1529.588902	65.294140	48.582516
1526.347976	71.417257	48.587521
1522.736327	67.066152	48.592525
1519.194147	68.788139	48.597530
1515.651136	58.927635	48.602535
1512.440935	75.192211	48.607540
1509.066762	59.898369	48.612545
1505.429902	57.430508	48.617549
1501.965931	63.730912	48.622554
1498.568664	63.500314	48.627559
1494.955390	63.819224	48.632564
1491.671539	52.994343	48.637569
1488.296347	66.731568	48.642573
1484.533047	63.524197	48.647578
1481.200420	53.586487	48.652583
1477.271694	59.890039	48.657588
1474.178574	60.478720	48.662593
1470.861319	64.111244	48.667597
1467.268480	63.344951	48.672602
1464.338428	57.536248	48.677607
1460.114282	60.880453	48.682612
1456.723610	52.312267	48.687617
1453.085090	62.373270	48.692621
1449.644241	57.406998	48.697626
1446.535076	52.999422	48.702631
1442.595496	53.473832	48.707636
1439.317414	55.224109	48.712641
1435.635529	56.091623	48.717645
1432.120903	56.176814	48.722650
1428.791899	48.911958	48.727655
1425.086426	58.546845	48.732660
1422.055671	55.386188	48.737665
1418.564134	67.088346	48.742669
1414.740321	61.656844	48.747674
1411.584121	61.027870	48.752679
1407.997946	61.968998	48.757684
1404.386017	56.798567	48.762689
1400.583023	56.378410	48.767693
1397.224778	59.508003	48.772698
1393.856175	56.748256	48.777703
1390.651851	62.523989	48.782708
1386.862961	51.218220	48.787713
1383.259763	52.181004	48.792717
1379.629239	59.232019	48.797722
1376.662618	54.128268	48.802727
1373.208514	57.595579	48.807732
1369.604348	57.966893	48.812737
1366.330539	60.864977	48.817741
1362.312450	58.618200	48.822746
1359.025753	46.167642	48.827751
1355.179868	61.718652	48.832756
1352.004671	48.814039	48.837761
1348.582361	55.886253	48.842765
1344.839497	58.373710	48.847770
1341.427817	45.721260	48.852775
1337.817613	55.426679	48.857780
1334.510950	52.258622	48.862785
1331.014734	56.960085	48.867789
1327.629785	58.088043	48.872794
1324.448252	62.604206	48.877799
1320.493355	65.308363	48.882804
1317.211580	64.626310	48.887809
1313.536379	59.165261	48.892813
1309.662591	57.307210	48.897818
1306.471585	52.045619	48.902823
1302.574514	56.534592	48.907828
1299.417645	57.310477	48.912833
1296.203582	52.833953	48.917837
1292.820913	49.712611	48.922842
1289.579039	48.521281	48.927847
1285.543556	59.147512	48.932852
1282.233260	49.892933	48.937857
1278.462063	61.123205	48.942861
1275.138407	62.886997	48.947866
1271.614973	55.608345	48.952871
1267.773621	54.662729	48.957876
1264.431710	53.670567	48.962881
1260.814928	55.176528	48.967885
1257.162188	58.966040	48.972890
1254.224475	56.936161	48.977895
1250.263515	60.751780	48.982900
1247.022988	53.074509	48.987905
1243.812924	53.042484	48.992909
1239.767082	56.083614	48.997914
1236.751447	44.628396	49.002919
1233.147017	65.058147	49.007924
1229.453794	56.955037	49.012929
1226.140183	55.322539	49.017933
1222.103714	51.095013	49.022938
1219.252057	45.467117	49.027943
1215.570185	57.800234	49.032948
1212.273375	49.287061	49.037953
1208.652376	50.777881	49.042957
1204.919881	55.392986	49.047962
1201.557341	59.867918	49.052967
1197.607517	57.268837	49.057972
1194.653690	53.912715	49.062977
1191.094623	57.020027	49.067981
1187.391468	54.407645	49.072986
1184.387412	57.105365	49.077991
1180.667299	52.926407	49.082996
1177.120844	56.705634	49.088001
1173.430200	55.847194	49.093005
1169.743193	68.940440	49.098010
1166.530478	63.777210	49.103015
1162.872880	59.199326	49.108020
1159.403242	49.435067	49.113025
1156.294664	50.250894	49.118029
1152.607790	55.102485	49.123034
1149.335049	49.597484	49.128039
1145.406290	55.568957	49.133044
1141.805511	59.499071	49.138049
1138.395674	53.094877	49.143053
1134.798595	53.319634	49.148058
1131.739549	53.529760	49.153063
1128.384917	64.017812	49.158068
1124.645919	56.231967	49.163073
1120.811574	58.534509	49.168077
1117.280484	59.100120	49.173082
1114.446813	55.782160	49.178087
1110.359792	53.897464	49.183092
1106.954270	55.860789	49.188097
1103.709029	58.820921	49.193101
1099.586549	49.978317	49.198106
1097.102276	45.444557	49.203111
1093.327354	53.454742	49.208116
1089.916541	54.105936	49.213121
1085.875189	52.676012	49.218125
1082.425593	53.270005	49.223130
1079.205039	49.819640	49.228135
1075.441208	53.104584	49.233140
1071.937389	51.505084	49.238145
1068.057508	56.130657	49.243149
1064.876936	51.911568	49.248154
1061.623258	36.118201	49.253159
1057.905069	46.871992	49.258164
1054.656074	52.056857	49.263169
1050.730627	53.845339	49.268173
1047.037239	52.398917	49.273178
1043.962993	50.001340	49.278183
1040.474525	53.869610	49.283188
1037.289837	49.733434	49.288193
1033.480457	43.325404	49.293197
1030.099125	51.160089	49.298202
1026.862192	45.386937	49.303207
1022.772311	54.541123	49.308212
1019.304041	52.521624	49.313217
1016.556470	56.792757	49.318221
1012.164134	60.954419	49.323226
1009.066346	55.324001	49.328231
1004.972741	54.164886	49.333236
1001.467012	47.905480	49.338241
998.327701	51.465993	49.343245
994.838493	46.374598	49.348250
991.736231	48.730244	49.353255
988.193324	49.560344	49.358260
984.560609	48.006371	49.363265
980.801200	52.913670	49.368269
977.393004	47.249610	49.373274
974.203649	54.690420	49.378279
970.296950	57.643430	49.383284
966.785518	51.976555	49.388289
963.286663	55.466825	49.393293
959.836945	52.178936	49.398298
956.517865	45.732136	49.403303
952.851494	59.334734	49.408308
949.420314	43.414183	49.413313
945.872612	49.974633	49.418317
942.455905	50.281951	49.423322
938.859981	52.711746	49.428327
935.267743	59.510131	49.433332
931.961196	45.373421	49.438337
928.246967	53.064107	49.443341
924.504668	46.095127	49.448346
921.551570	44.453747	49.453351
917.724075	55.300629	49.458356
914.502549	44.959792	49.463361
911.015262	51.880955	49.468365
907.265084	53.373130	49.473370
903.997611	45.855245	49.478375
900.282483	58.971943	49.483380
897.227423	50.272351	49.488385
893.990719	50.323709	49.493389
889.816775	54.274054	49.498394
886.426624	40.159952	49.503399
883.131572	43.143770	49.508404
879.128799	42.619061	49.513409
875.739629	49.262277	49.518413
872.045581	53.947408	49.523418
868.528991	35.445991	49.528423
865.319498	52.934935	49.533428
861.818677	44.393745	49.538433
858.250622	50.751766	49.543437
854.621935	42.698840	49.548442
851.274817	41.717133	49.553447
847.825956	47.509161	49.558452
844.314726	46.657559	49.563457
841.012019	46.159285	49.568461
837.394706	51.661318	49.573466
833.908268	50.372401	49.578471
830.392528	50.442166	49.583476
826.826634	42.230724	49.588481
823.166241	45.895032	49.593485
819.574627	50.497702	49.598490
816.643764	37.178587	49.603495
812.812365	37.987489	49.608500
809.312823	38.212913	49.613505
806.015514	41.415409	49.618509
802.183253	40.066764	49.623514
798.985012	40.216537	49.628519
795.101226	40.369259	49.633524
791.862731	39.841965	49.638529
788.151901	46.655801	49.643533
784.524505	40.757229	49.648538
781.441072	33.542776	49.653543
777.848528	43.894158	49.658548
774.333716	41.752329	49.663553
770.835589	39.443373	49.668557
766.888419	45.047704	49.673562
763.861981	44.249930	49.678567
760.390944	49.776538	49.683572
756.798019	40.610742	49.688577
753.284035	47.017275	49.693581
749.835144	43.419294	49.698586
746.279042	44.324317	49.703591
742.539036	44.419743	49.708596
739.200203	37.346541	49.713601
735.623346	43.639539	49.718605
732.308910	31.171474	49.723610
728.588812	37.081942	49.728615
725.093051	43.700766	49.733620
721.794221	46.546023	49.738625
718.104823	45.997619	49.743629
714.599981	46.458027	49.748634
711.369623	44.556415	49.753639
707.476113	47.229050	49.758644
704.216693	52.153061	49.763649
700.630659	53.385493	49.768653
697.017969	45.364935	49.773658
693.815906	47.356651	49.778663
690.107598	42.957759	49.783668
686.761078	44.889842	49.788673
683.283403	42.163266	49.793677
679.836445	54.772954	49.798682
676.492822	51.047783	49.803687
672.148253	45.030620	49.808692
669.047817	42.735353	49.813697
665.640328	39.592831	49.818701
662.090665	42.702017	49.823706
658.755855	41.278692	49.828711
655.097715	38.124809	49.833716
651.673953	40.325265	49.838721
648.080632	47.111254	49.843725
644.383477	52.195586	49.848730
641.224709	41.016138	49.853735
637.607917	43.828961	49.858740
634.439270	44.901137	49.863745
630.928201	48.368124	49.868749
626.852752	47.019674	49.873754
623.428125	46.790510	49.878759
619.643638	39.031015	49.883764
616.704209	43.904936	49.888769
612.990549	44.341139	49.893773
609.156464	47.763809	49.898778
606.191281	46.731868	49.903783
602.580880	47.503080	49.908788
599.768050	45.631030	49.913793
595.836939	40.612178	49.918797
592.437212	47.684241	49.923802
588.913470	41.098806	49.928807
585.070555	56.475546	49.933812
581.238254	46.483614	49.938817
577.885532	49.963784	49.943821
574.295387	46.463926	49.948826
571.092309	42.713623	49.953831
567.277860	54.431770	49.958836
563.920824	45.134205	49.963841
560.555143	51.311932	49.968845
557.012828	49.987582	49.973850
554.038728	43.705219	49.978855
550.085901	55.005282	49.983860
546.434383	52.774223	49.988865
542.927915	46.350616	49.993869
539.408089	45.744088	49.998874
536.151831	42.451381	50.003879
532.467360	48.729666	50.008884
528.861960	42.666412	50.013889
525.407485	41.011943	50.018893
521.862109	43.016358	50.023898
519.020416	43.717825	50.028903
515.003890	44.192013	50.033908
511.386429	41.449435	50.038913
507.750129	48.207402	50.043917
504.378873	53.538134	50.048922
501.129719	41.075765	50.053927
497.344206	47.211699	50.058932
493.941216	46.235713	50.063937
490.478331	40.982222	50.068941
486.818286	47.541435	50.073946
483.539531	45.324785	50.078951
480.219645	39.052319	50.083956
476.612358	41.496718	50.088961
473.230565	43.678010	50.093965
469.409118	40.204936	50.098970
466.330198	35.011540	50.103975
462.373210	39.975282	50.108980
458.446117	39.565454	50.113985
455.476327	41.628436	50.118989
452.080903	43.074716	50.123994
448.227298	50.287520	50.128999
444.853498	44.121588	50.134004
441.349021	40.611534	50.139009
438.432226	37.132818	50.144013
434.751758	40.404944	50.149018
431.283374	37.547302	50.154023
427.069324	43.475139	50.159028
423.611917	32.877244	50.164033
420.745053	36.847675	50.169037
416.997203	39.624162	50.174042
413.544113	32.761987	50.179047
409.184191	49.921853	50.184052
406.217829	36.994456	50.189057
402.833434	36.980538	50.194061
399.330366	41.610613	50.199066
395.664052	42.931666	50.204071
392.105151	40.939267	50.209076
388.811285	41.290823	50.214081
385.815000	38.890761	50.219085
381.856046	42.291950	50.224090
378.625093	37.853229	50.229095
374.767022	53.283022	50.234100
371.490858	38.113610	50.239105
368.084604	45.740423	50.244109
364.316766	40.810001	50.249114
360.659591	32.258739	50.254119
356.996591	39.353131	50.259124
353.994801	33.521275	50.264129
350.370614	46.187281	50.269133
346.750177	25.984511	50.274138
343.290640	35.391372	50.279143
339.595294	43.971473	50.284148
336.266029	32.050083	50.289153
332.782625	42.204170	50.294157
328.973072	46.866462	50.299162
326.184594	41.102440	50.304167
322.388336	48.151283	50.309172
319.141218	42.038328	50.314177
315.279464	46.854335	50.319181
311.638777	41.049808	50.324186
308.447946	41.866143	50.329191
304.554847	48.518875	50.334196
300.900023	40.539908	50.339201
297.907513	37.826075	50.344205
294.681893	36.040936	50.349210
291.223769	44.492145	50.354215
287.738105	48.369726	50.359220
284.126247	41.443892	50.364225
280.378744	37.057654	50.369229
276.658146	40.712614	50.374234
273.071152	37.177593	50.379239
269.335302	45.697626	50.384244
266.047977	46.383560	50.389249
262.464116	43.620006	50.394253
259.079010	46.229001	50.399258
255.856628	45.914512	50.404263
252.420784	42.264072	50.409268
248.875678	43.262478	50.414273
245.042953	45.327832	50.419277
241.383187	42.218675	50.424282
238.464499	42.805742	50.429287
234.824253	42.676944	50.434292
231.297798	37.651824	50.439297
227.443792	34.791403	50.444301
223.963939	43.287165	50.449306
220.953928	40.497008	50.454311
217.304867	43.027145	50.459316
213.618262	40.469534	50.464321
210.133745	36.950125	50.469325
206.006578	48.843926	50.474330
203.266895	38.589276	50.479335
199.565991	43.968586	50.484340
196.356097	42.952975	50.489345
192.756246	37.303458	50.494349
189.307789	46.585251	50.499354
186.098404	39.542628	50.504359
182.093484	37.322800	50.509364
178.878181	43.429634	50.514369
175.056778	48.353270	50.519373
171.438053	50.635065	50.524378
168.193076	45.787336	50.529383
164.663827	48.380982	50.534388
161.389396	45.287423	50.539393
157.709660	35.433166	50.544397
153.835308	50.109439	50.549402
150.823967	36.132514	50.554407
147.205920	38.189586	50.559412
143.615586	42.766985	50.564417
140.487533	40.305398	50.569421
136.884858	38.560409	50.574426
133.055242	41.251744	50.579431
129.385474	51.732488	50.584436
126.104430	31.713950	50.589441
122.660603	38.207778	50.594445
118.986129	45.228124	50.599450
115.362256	34.672277	50.604455
111.939259	53.302133	50.609460
108.956917	44.942654	50.614465
105.326085	40.019364	50.619469
101.457480	48.111004	50.624474
98.236033	42.892624	50.629479
94.238432	43.531715	50.634484
90.603768	35.809121	50.639489
87.612425	47.942627	50.644493
84.109579	44.910195	50.649498
80.993585	41.048367	50.654503
76.939324	45.508652	50.659508
73.068946	36.149377	50.664513
69.628950	42.781829	50.669517
66.406985	42.356614	50.674522
63.172347	35.175635	50.679527
59.770153	42.213453	50.684532
56.025013	37.735201	50.689537
52.805505	38.954753	50.694541
49.419957	41.105150	50.699546
45.719392	30.912533	50.704551
42.013902	41.092014	50.709556
38.373517	38.574696	50.714561
34.772755	37.832358	50.719565
31.096467	43.846951	50.724570
28.203952	36.609219	50.729575
24.553029	33.017887	50.734580
21.306099	35.801470	50.739585
17.717888	33.285479	50.744589
13.772139	33.843717	50.749594
10.876812	30.940758	50.754599
6.810731	31.653893	50.759604
3.406102	35.525207	50.764609