Thu Aug 25 11:47:02 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
2.023488	112.327796	0.000000
1.780137	110.844281	0.005005
2.245513	108.028514	0.010010
1.781997	115.017219	0.015014
2.039770	96.408900	0.020019
1.639404	86.534419	0.025024
1.128154	78.063037	0.030029
1.496164	60.307514	0.035034
0.823565	60.140936	0.040038
0.532454	43.782672	0.045043
-0.247050	41.987700	0.050048
-0.529210	36.720113	0.055053
-0.491383	31.604871	0.060058
-1.445252	26.183104	0.065062
-1.393800	19.275056	0.070067
-1.287197	19.201527	0.075072
-1.408422	14.908471	0.080077
-1.881669	9.499990	0.085082
-2.660213	20.141510	0.090086
-2.886673	13.447850	0.095091
-3.152721	15.542919	0.100096
-3.014908	20.760591	0.105101
-3.344443	19.752493	0.110106
-4.190813	32.559151	0.115110
-4.452193	24.573826	0.120115
-4.466134	16.448495	0.125120
-4.798902	15.709821	0.130125
-4.441876	12.945846	0.135130
-4.698024	18.994032	0.140134
-5.105662	19.092823	0.145139
-5.361583	20.623161	0.150144
-5.640148	20.802968	0.155149
-5.741770	10.470436	0.160154
-5.980533	13.842542	0.165158
-6.763788	14.898686	0.170163
-7.009119	14.829679	0.175168
-7.432471	15.987620	0.180173
-7.246215	11.383798	0.185178
-7.434774	22.711158	0.190182
-7.288678	20.660434	0.195187
-7.736842	16.355329	0.200192
-8.508274	16.134636	0.205197
-8.665173	2.118693	0.210202
-9.023321	20.704915	0.215206
-8.760124	8.442293	0.220211
-9.167762	16.795266	0.225216
-9.689878	9.148191	0.230221
-9.988056	2.892876	0.235226
-10.706147	13.566049	0.240230
-10.582075	9.028919	0.245235
-10.412546	16.158843	0.250240
-10.499202	15.906787	0.255245
-10.237415	7.421886	0.260250
-10.831680	23.849477	0.265254
-11.765862	18.415139	0.270259
-11.916439	22.352392	0.275264
-11.923651	12.751709	0.280269
-11.896247	13.396101	0.285274
-13.179538	15.834051	0.290278
-13.054960	12.527533	0.295283
-13.334861	12.622129	0.300288
-13.575974	21.034433	0.305293
-13.135841	9.690044	0.310298
-13.336934	15.504978	0.315302
-13.654988	17.351933	0.320307
-14.120114	9.990157	0.325312
-14.626746	19.323579	0.330317
-14.447884	13.129558	0.335322
-14.810013	26.436139	0.340326
-15.719079	17.552559	0.345331
-15.914526	13.043344	0.350336
-16.082079	20.561440	0.355341
-15.972780	21.281586	0.360346
-16.388321	20.869091	0.365350
-16.024931	18.062989	0.370355
-16.560244	20.592551	0.375360
-17.036946	23.774151	0.380365
-17.603137	23.673160	0.385370
-17.775703	18.223894	0.390374
-17.639233	20.755766	0.395379
-17.576369	25.029734	0.400384
-18.098130	21.963689	0.405389
-18.813991	16.900104	0.410394
-19.253196	21.151497	0.415398
-19.217206	15.637918	0.420403
-19.425884	12.567112	0.425408
-19.471547	21.790345	0.430413
-19.103483	17.860385	0.435418
-20.152564	26.671367	0.440422
-20.842841	22.438998	0.445427
-20.551987	23.178153	0.450432
-20.717385	22.223431	0.455437
-20.857786	18.442741	0.460442
-21.084071	25.134815	0.465446
-21.211882	24.522214	0.470451
-21.564414	16.627106	0.475456
-21.874938	25.689361	0.480461
-21.982702	11.722661	0.485466
-22.810780	13.886808	0.490470
-23.307744	16.018058	0.495475
-23.458498	16.690365	0.500480
-23.787098	20.196770	0.505485
-23.505147	8.997389	0.510490
-23.799564	17.832491	0.515494
-23.493069	14.127313	0.520499
-23.647838	22.937373	0.525504
-24.361494	21.208019	0.530509
-24.719776	12.953147	0.535514
-24.807791	15.858711	0.540518
-25.382113	10.886845	0.545523
-25.955370	18.443197	0.550528
-26.632733	12.063796	0.555533
-26.286942	13.933287	0.560538
-26.512780	21.669321	0.565542
-26.957846	17.142271	0.570547
-26.678661	16.813912	0.575552
-26.947820	24.022064	0.580557
-26.373084	14.871197	0.585562
-27.671067	26.460972	0.590566
-27.725154	18.949370	0.595571
-27.892164	20.804297	0.600576
-28.195290	20.010359	0.605581
-28.397500	18.998131	0.610586
-28.986124	18.695013	0.615590
-28.921495	14.192505	0.620595
-29.055030	14.020561	0.625600
-29.542065	19.427884	0.630605
-29.341709	12.999543	0.635610
-30.509911	16.308471	0.640614
-30.647399	12.492526	0.645619
-30.642860	23.565004	0.650624
-30.944274	23.099827	0.655629
-30.476100	11.640313	0.660634
-31.214168	20.174773	0.665638
-31.235671	15.628814	0.670643
-32.106058	16.179760	0.675648
-32.424005	18.517078	0.680653
-32.381103	13.078346	0.685658
-32.336782	15.605672	0.690662
-32.433352	19.157978	0.695667
-33.362688	10.555989	0.700672
-33.691074	24.255911	0.705677
-33.696029	19.878199	0.710682
-33.848352	32.155333	0.715686
-33.704488	21.265482	0.720691
-34.294653	14.986312	0.725696
-34.840996	29.732783	0.730701
-34.865086	20.201181	0.735706
-35.187025	21.118608	0.740710
-35.138865	20.136752	0.745715
-34.948175	27.361439	0.750720
-35.778927	23.008713	0.755725
-36.014770	20.081368	0.760730
-36.268653	22.753496	0.765734
-36.412661	16.907453	0.770739
-36.822671	27.234971	0.775744
-37.771533	22.220550	0.780749
-37.774907	20.133134	0.785754
-38.121783	26.337906	0.790758
-38.197671	29.279536	0.795763
-37.987067	28.968249	0.800768
-38.390949	28.009766	0.805773
-38.161729	12.604550	0.810778
-38.236295	23.063003	0.815782
-38.807275	20.260935	0.820787
-39.599411	15.823068	0.825792
-39.524456	27.877927	0.830797
-39.557988	16.484367	0.835802
-40.109808	24.673273	0.840806
-40.825600	24.238222	0.845811
-40.886899	23.137477	0.850816
-41.045879	29.382410	0.855821
-41.015558	22.578914	0.860826
-40.983192	24.627227	0.865830
-41.001484	24.570103	0.870835
-41.697714	26.087175	0.875840
-42.120563	22.543729	0.880845
-42.421804	18.452885	0.885850
-42.639836	21.951457	0.890854
-42.351629	23.105475	0.895859
-43.344331	21.337588	0.900864
-43.845145	25.181024	0.905869
-43.770005	21.034370	0.910874
-44.006368	29.221307	0.915878
-44.197128	25.128970	0.920883
-44.381659	10.933858	0.925888
-44.356489	28.014197	0.930893
-44.503453	19.855927	0.935898
-45.259893	30.380096	0.940902
-45.644919	25.214054	0.945907
-45.459264	26.017148	0.950912
-45.607360	33.921338	0.955917
-46.059573	18.325499	0.960922
-46.700093	15.619749	0.965926
-46.974587	22.860374	0.970931
-47.168611	20.597188	0.975936
-47.416198	23.432843	0.980941
-47.245506	19.293364	0.985946
-47.455547	27.783058	0.990950
-47.135127	25.239950	0.995955
-47.836413	31.781827	1.000960
-48.259202	25.792803	1.005965
-48.656408	23.931610	1.010970
-48.874952	33.495145	1.015974
-48.937819	16.392475	1.020979
-49.377682	25.307317	1.025984
-49.916898	18.077372	1.030989
-49.635979	27.689194	1.035994
-50.067971	27.601979	1.040998
-50.280428	19.754526	1.046003
-51.372337	15.964741	1.051008
-51.399771	21.467729	1.056013
-51.059331	21.863757	1.061018
-51.635795	27.006687	1.066022
-51.592259	23.285761	1.071027
-51.747504	17.587012	1.076032
-51.865381	19.605082	1.081037
-52.112298	16.087856	1.086042
-52.863418	29.078901	1.091046
-52.896663	23.424310	1.096051
-53.011912	24.679508	1.101056
-53.333801	25.881665	1.106061
-52.884194	22.464106	1.111066
-53.889105	26.190376	1.116070
-54.588855	21.367877	1.121075
-54.452149	27.224797	1.126080
-54.497844	37.273774	1.131085
-54.393711	24.754496	1.136090
-55.241963	26.592780	1.141094
-56.005903	25.038985	1.146099
-56.433314	25.337028	1.151104
-56.490637	25.706797	1.156109
-56.017929	21.308025	1.161114
-56.110538	27.229348	1.166118
-55.920212	26.582719	1.171123
-56.365935	24.577269	1.176128
-57.129828	33.311933	1.181133
-57.031787	21.853463	1.186138
-57.411976	24.279628	1.191142
-57.844278	19.608212	1.196147
-58.348780	21.920978	1.201152
-58.867922	20.793895	1.206157
-58.927413	14.485363	1.211162
-59.511121	25.286181	1.216166
-59.189250	23.973539	1.221171
-58.777068	22.444266	1.226176
-59.464152	23.551785	1.231181
-59.214466	26.945434	1.236186
-60.348545	37.234551	1.241190
-60.719763	29.003849	1.246195
-60.525617	30.438359	1.251200
-60.776265	38.149813	1.256205
-60.703318	29.393938	1.261210
-61.698444	24.326657	1.266214
-61.896843	32.339968	1.271219
-61.759081	20.141288	1.276224
-61.839977	29.161236	1.281229
-62.016959	22.039048	1.286234
-62.970466	25.928106	1.291238
-62.853784	28.190997	1.296243
-63.099494	26.992597	1.301248
-63.543753	22.949473	1.306253
-63.470600	24.902811	1.311258
-63.770113	22.877616	1.316262
-64.361163	17.383194	1.321267
-64.555000	24.940209	1.326272
-64.634412	33.776430	1.331277
-64.368753	25.205495	1.336282
-65.130423	23.784222	1.341286
-65.608260	24.457160	1.346291
-65.919486	14.641526	1.351296
-66.273851	29.402206	1.356301
-66.614636	22.138006	1.361306
-66.859367	32.680073	1.366310
-66.052760	25.463877	1.371315
-66.147437	21.093897	1.376320
-67.250026	28.688902	1.381325
-67.417108	30.543841	1.386330
-67.829535	27.444850	1.391334
-67.938219	13.664959	1.396339
-67.823158	21.407687	1.401344
-68.741646	28.888425	1.406349
-69.178516	23.781129	1.411354
-69.268263	22.064750	1.416358
-69.263424	23.978171	1.421363
-69.359592	24.091436	1.426368
-69.745448	28.812197	1.431373
-69.435590	19.516172	1.436378
-69.732525	25.080370	1.441382
-70.366892	17.609075	1.446387
-70.822680	18.908142	1.451392
-71.045139	22.021432	1.456397
-71.009489	16.207352	1.461402
-71.441482	19.429404	1.466406
-71.906349	24.668741	1.471411
-72.148506	22.270730	1.476416
-72.927254	28.014828	1.481421
-72.473382	27.523055	1.486426
-72.301094	32.017157	1.491430
-72.613650	26.700558	1.496435
-72.838589	27.507875	1.501440
-73.885923	29.358373	1.506445
-73.840249	19.426704	1.511450
-73.874327	26.996651	1.516454
-73.728104	30.792488	1.521459
-73.987966	15.368996	1.526464
-74.623858	33.432436	1.531469
-75.016250	20.665098	1.536474
-75.758014	28.918569	1.541478
-75.963939	19.507211	1.546483
-75.573901	23.913408	1.551488
-75.579810	23.477859	1.556493
-75.568950	24.150153	1.561498
-76.244609	30.972751	1.566502
-76.315512	18.094930	1.571507
-76.310932	24.697044	1.576512
-77.358674	25.690234	1.581517
-77.443845	23.169549	1.586522
-78.121655	22.333084	1.591526
-78.349818	32.274607	1.596531
-78.202982	31.631628	1.601536
-78.336007	31.472260	1.606541
-77.727475	18.896099	1.611546
-78.859736	24.274812	1.616550
-79.280046	18.813749	1.621555
-79.469907	22.621116	1.626560
-79.635816	22.577631	1.631565
-80.008382	21.718647	1.636570
-80.357847	30.900898	1.641574
-80.632906	17.662764	1.646579
-80.690997	25.783799	1.651584
-80.988543	22.983182	1.656589
-81.051241	19.680698	1.661594
-81.609134	27.427634	1.666598
-82.364248	20.623825	1.671603
-82.310843	16.613456	1.676608
-82.761540	25.751456	1.681613
-82.403874	20.026123	1.686618
-82.535287	21.245890	1.691622
-82.571943	20.609516	1.696627
-82.633016	20.154138	1.701632
-83.256373	26.035238	1.706637
-83.405737	22.205335	1.711642
-84.096203	27.584425	1.716646
-84.031670	24.306297	1.721651
-84.292105	31.763019	1.726656
-85.264478	26.454896	1.731661
-85.201709	17.080531	1.736666
-85.596394	26.693806	1.741670
-85.428826	27.022008	1.746675
-85.184285	14.227641	1.751680
-85.648667	27.224375	1.756685
-85.710407	9.820986	1.761690
-86.566268	15.611964	1.766694
-86.622193	28.921182	1.771699
-87.071419	16.425344	1.776704
-87.114475	26.024650	1.781709
-87.488487	12.153460	1.786714
-87.981596	17.394057	1.791718
-88.151162	22.327697	1.796723
-88.505086	19.931382	1.801728
-89.004831	20.699502	1.806733
-88.338674	23.037643	1.811738
-88.466355	20.865303	1.816742
-88.812342	16.923843	1.821747
-89.162665	16.735249	1.826752
-89.950715	27.428883	1.831757
-89.886209	23.024470	1.836762
-90.380269	20.235663	1.841766
-91.256951	15.959746	1.846771
-90.752951	19.800759	1.851776
-91.198472	23.439380	1.856781
-91.227820	8.830821	1.861786
-91.401544	24.543946	1.866790
-91.528079	19.337407	1.871795
-91.767400	22.545088	1.876800
-92.755907	33.757350	1.881805
-92.835619	19.798912	1.886810
-93.260861	20.204185	1.891814
-92.517736	23.931799	1.896819
-93.101099	17.892014	1.901824
-93.226426	28.339437	1.906829
-93.145977	20.167683	1.911834
-94.155942	22.989921	1.916838
-94.126438	16.202376	1.921843
-94.375921	16.858516	1.926848
-94.703871	30.109119	1.931853
-94.562798	21.291955	1.936858
-95.193365	22.855689	1.941862
-95.676512	17.300072	1.946867
-96.029083	16.501230	1.951872
-96.055963	24.756577	1.956877
-96.020499	18.237015	1.961882
-96.233978	16.388166	1.966886
-96.885043	21.109352	1.971891
-97.096546	23.970991	1.976896
-97.554247	21.739633	1.981901
-97.585170	17.767787	1.986906
-97.605021	21.589643	1.991910
-97.620909	25.183090	1.996915
-98.560135	21.875745	2.006912
-98.013492	15.803221	2.016909
-97.751241	28.151571	2.026906
-96.741811	25.104623	2.036902
-96.676411	22.636416	2.046899
-96.233405	26.545978	2.056896
-94.967725	26.382742	2.066893
-94.988314	22.461325	2.076890
-94.643561	21.941882	2.086886
-94.185273	28.484646	2.096883
-93.206357	29.227982	2.106880
-93.349199	25.401747	2.116877
-92.472049	30.022558	2.126874
-92.114088	31.037421	2.136870
-91.623717	32.522543	2.146867
-90.614885	32.557943	2.156864
-90.438334	24.370306	2.166861
-90.338098	26.211163	2.176858
-89.427626	21.386755	2.186854
-89.178068	28.953743	2.196851
-88.379986	29.982005	2.206848
-87.769948	28.863464	2.216845
-87.891416	26.281987	2.226842
-86.873846	29.220877	2.236838
-86.674318	26.582766	2.246835
-85.840350	24.380601	2.256832
-85.176939	24.235710	2.266829
-85.112418	31.454727	2.276826
-84.510128	33.004675	2.286822
-84.092968	23.996893	2.296819
-83.927752	26.179192	2.306816
-82.929863	24.841490	2.316813
-82.529202	25.501206	2.326810
-81.918113	22.637051	2.336806
-81.150319	28.738515	2.346803
-80.991633	27.497462	2.356800
-80.657222	23.729492	2.366797
-79.751168	30.617078	2.376794
-79.479201	24.118759	2.386790
-79.081661	24.611071	2.396787
-78.598466	23.277990	2.406784
-78.156738	29.934224	2.416781
-77.119204	20.138660	2.426778
-76.827028	27.299830	2.436774
-76.650227	26.987267	2.446771
-76.170097	24.302022	2.456768
-75.696887	21.969485	2.466765
-74.592547	27.733116	2.476762
-73.970572	18.674237	2.486758
-74.055427	18.225278	2.496755
-73.838026	23.978996	2.506752
-73.190464	21.460751	2.516749
-72.605140	16.009388	2.526746
-71.616774	22.488102	2.536742
-71.387083	22.404836	2.546739
-71.300867	27.786305	2.556736
-70.551974	26.484451	2.566733
-69.723996	13.382881	2.576730
-69.523060	21.027177	2.586726
-68.732308	27.137716	2.596723
-68.326294	25.715359	2.606720
-68.194943	22.739476	2.616717
-67.056326	23.638355	2.626714
-66.704192	22.376495	2.636710
-66.415240	21.134037	2.646707
-66.432611	22.119013	2.656704
-65.693997	20.749079	2.666701
-64.813972	17.307431	2.676698
-64.023269	15.523859	2.686694
-64.090929	22.649545	2.696691
-63.789756	28.238086	2.706688
-63.092679	26.443841	2.716685
-62.715620	28.241323	2.726682
-61.612204	25.296859	2.736678
-61.761596	26.061770	2.746675
-60.394745	27.995600	2.756672
-60.114892	26.447293	2.766669
-60.376801	22.674559	2.776666
-59.656422	24.735026	2.786662
-58.378251	21.278510	2.796659
-58.321854	28.701538	2.806656
-58.308867	22.722133	2.816653
-57.124838	25.752153	2.826650
-56.873227	22.339279	2.836646
-56.640451	27.792819	2.846643
-55.738908	25.728953	2.856640
-55.334878	20.727311	2.866637
-55.058876	20.576601	2.876634
-54.278128	22.938052	2.886630
-53.916517	23.971351	2.896627
-53.511911	20.395122	2.906624
-52.432697	24.094129	2.916621
-52.461797	10.841753	2.926618
-52.127688	18.699599	2.936614
-51.323564	22.733145	2.946611
-51.106580	22.734233	2.956608
-50.411199	19.606618	2.966605
-49.826428	21.827716	2.976602
-49.601826	16.984068	2.986598
-48.600199	24.056252	2.996595
-48.273640	20.577782	3.006592
-48.276874	24.769510	3.016589
-47.331645	21.615417	3.026586
-46.776091	21.465255	3.036582
-46.662606	25.765406	3.046579
-45.685336	22.045595	3.056576
-45.529127	14.573899	3.066573
-44.874964	16.822137	3.076570
-43.860946	19.723575	3.086566
-43.943723	14.985110	3.096563
-43.801403	15.910219	3.106560
-42.772378	15.261387	3.116557
-42.247260	22.145307	3.126554
-42.022811	23.086058	3.136550
-41.150335	13.544442	3.146547
-41.115903	16.612039	3.156544
-40.579619	24.520573	3.166541
-39.488298	18.071269	3.176538
-39.357723	16.901145	3.186534
-38.886497	16.361887	3.196531
-38.220784	17.616800	3.206528
-37.812291	17.578379	3.216525
-37.790192	11.901656	3.226522
-36.901900	17.778336	3.236518
-36.229773	9.538396	3.246515
-35.353366	17.567863	3.256512
-35.088025	12.451739	3.266509
-34.829710	13.038727	3.276506
-34.960621	14.174540	3.286502
-34.279555	17.197839	3.296499
-32.983815	18.997097	3.306496
-32.448743	21.555433	3.316493
-32.219942	11.994296	3.326490
-32.152269	14.660711	3.336486
-31.570806	11.186652	3.346483
-31.221656	15.487890	3.356480
-30.132770	9.412770	3.366477
-29.668175	13.185905	3.376474
-29.259478	18.985679	3.386470
-28.997118	11.712760	3.396467
-28.397726	16.307406	3.406464
-27.962625	12.143529	3.416461
-26.849130	8.506915	3.426458
-26.446740	10.547516	3.436454
-26.536459	11.645197	3.446451
-26.255610	18.697270	3.456448
-24.904299	18.273540	3.466445
-24.694403	16.124814	3.476442
-24.674522	16.172624	3.486438
-23.919974	16.780062	3.496435
-23.431461	22.760567	3.506432
-22.910258	15.627654	3.516429
-21.990139	14.644264	3.526426
-21.568639	12.972396	3.536422
-21.655849	14.506838	3.546419
-20.993502	14.153045	3.556416
-20.708901	16.931190	3.566413
-19.246522	21.606032	3.576410
-18.960619	17.180429	3.586406
-19.305281	24.254486	3.596403
-18.113718	22.126176	3.606400
-17.601027	20.693442	3.616397
-17.354006	16.175731	3.626394
-17.070867	14.284790	3.636390
-16.201405	21.279486	3.646387
-15.979359	17.769875	3.656384
-14.990498	19.351125	3.666381
-14.769739	23.238495	3.676378
-14.370169	23.366198	3.686374
-14.132347	12.298948	3.696371
-13.100633	20.193214	3.706368
-12.806511	18.199183	3.716365
-11.950735	20.795970	3.726362
-11.436232	10.952484	3.736358
-11.491384	19.156426	3.746355
-11.182722	15.398828	3.756352
-10.468657	21.141255	3.766349
-9.825938	15.243746	3.776346
-8.762259	9.058537	3.786342
-8.371938	18.713218	3.796339
-8.395233	13.221001	3.806336
-8.339475	8.673071	3.816333
-7.552384	14.369209	3.826330
-6.650028	12.216524	3.836326
-6.203345	28.150432	3.846323
-6.032303	24.705831	3.856320
-5.467936	25.701029	3.866317
-4.812344	24.831947	3.876314
-4.232291	22.843800	3.886310
-3.766204	35.112713	3.896307
-3.582098	35.857049	3.906304
-3.042493	44.297265	3.916301
-2.508219	47.657184	3.926298
-2.117693	60.356103	3.936294
-1.663219	70.475929	3.946291
-1.187004	79.854259	3.956288
-0.753100	92.666781	3.966285
-0.367664	109.662069	3.976282
0.000000	126.164628	3.981286
0.271913	128.798681	3.986291
0.281044	147.378110	3.991296
1.227835	144.053474	3.996301
0.718039	150.650811	4.001306
0.941590	155.339397	4.006310
0.889577	149.225795	4.011315
0.654637	156.061643	4.016320
1.086331	150.106371	4.021325
0.941413	153.723227	4.026330
0.761140	148.572520	4.031334
0.901330	154.922486	4.036339
0.812928	156.439243	4.041344
1.008857	158.927018	4.046349
1.091004	173.214467	4.051354
1.193361	173.932543	4.056358
1.098274	182.401138	4.061363
1.302655	176.864287	4.066368
1.479183	172.477084	4.071373
1.241394	169.499397	4.076378
1.094867	156.971838	4.081382
1.111220	151.587842	4.086387
0.930932	153.739093	4.091392
1.556553	148.136251	4.096397
1.106550	154.208528	4.101402
1.316060	157.776181	4.106406
1.215277	156.884093	4.111411
0.615532	167.516668	4.116416
1.442785	167.608637	4.121421
1.331159	180.379374	4.126426
1.511534	176.108627	4.131430
1.839821	172.222831	4.136435
1.284183	165.239003	4.141440
1.053146	150.896035	4.146445
1.264486	168.026440	4.151450
1.287515	171.860595	4.156454
1.389660	163.909998	4.161459
1.298733	179.249629	4.166464
1.626271	180.176033	4.171469
1.603804	185.358756	4.176474
1.540164	174.257710	4.181478
1.437649	166.560642	4.186483
1.219646	168.297023	4.191488
2.049172	172.726153	4.196493
1.196826	164.387267	4.201498
1.498441	162.818362	4.206502
1.333973	152.903719	4.211507
1.781413	167.769845	4.216512
1.740447	165.020748	4.221517
1.667786	164.687404	4.226522
1.499700	154.308254	4.231526
1.699596	158.064075	4.236531
1.309257	162.155984	4.241536
1.545922	165.434645	4.246541
1.287890	168.711722	4.251546
1.996422	171.337483	4.256550
2.196900	165.370976	4.261555
1.144683	160.113274	4.266560
1.486552	162.438978	4.271565
1.600489	161.712565	4.276570
1.808821	166.245350	4.281574
1.705622	166.976650	4.286579
1.708610	165.963899	4.291584
1.726113	163.091746	4.296589
1.470972	165.827367	4.301594
1.992112	168.507798	4.306598
2.016744	164.644271	4.311603
1.502250	164.266258	4.316608
1.889393	165.262417	4.321613
1.603825	175.149744	4.326618
1.946009	172.460836	4.331622
1.626650	169.913546	4.336627
2.061250	169.810772	4.341632
1.779904	175.426359	4.346637
1.497135	174.047091	4.351642
1.818020	173.946315	4.356646
1.777513	174.345089	4.361651
1.650834	179.031608	4.366656
1.859478	174.490676	4.371661
1.828755	175.647220	4.376666
1.892961	177.785476	4.381670
1.839636	179.214481	4.386675
2.008078	183.728211	4.391680
2.349875	182.241594	4.396685
1.735768	178.800845	4.401690
1.714528	167.088882	4.406694
1.757624	180.958513	4.411699
1.603749	180.346826	4.416704
1.935077	174.445236	4.421709
1.866606	183.061521	4.426714
2.039779	172.869338	4.431718
2.051784	175.218253	4.436723
2.003794	181.809684	4.441728
2.159514	186.841102	4.446733
2.291191	181.122652	4.451738
2.120823	181.617703	4.456742
2.260978	180.551822	4.461747
2.163554	192.731883	4.466752
2.112004	179.379502	4.471757
1.702724	181.130035	4.476762
2.260810	196.355337	4.481766
2.409843	206.737738	4.486771
2.139883	201.132831	4.491776
2.442411	196.029852	4.496781
2.065637	193.529519	4.501786
1.822241	183.257065	4.506790
2.524286	201.854536	4.511795
2.573328	204.368495	4.516800
2.404928	185.096027	4.521805
1.919870	187.247577	4.526810
2.306866	200.411604	4.531814
2.308004	200.424202	4.536819
2.598751	213.106608	4.541824
2.653598	198.769429	4.546829
2.343434	189.491364	4.551834
2.184979	189.158806	4.556838
2.451918	178.746284	4.561843
2.085898	177.522428	4.566848
2.513305	187.956115	4.571853
2.339311	197.949360	4.576858
2.510939	196.625446	4.581862
2.730289	199.128539	4.586867
2.569649	188.083812	4.591872
2.154751	182.988839	4.596877
2.166024	197.072277	4.601882
2.632970	199.245510	4.606886
2.522493	204.154125	4.611891
2.580280	213.032217	4.616896
2.841087	206.113441	4.621901
2.447311	191.830740	4.626906
2.339079	195.887948	4.631910
2.859529	192.358019	4.636915
2.962201	192.661593	4.641920
2.825328	181.470777	4.646925
2.487592	183.902965	4.651930
2.737196	180.456604	4.656934
2.572843	175.445764	4.661939
2.501608	185.309006	4.666944
2.391176	173.547738	4.671949
2.391566	184.364704	4.676954
2.959953	191.185432	4.681958
2.485997	201.940688	4.686963
2.673102	202.287981	4.691968
2.643440	202.071286	4.696973
2.576568	201.604155	4.701978
2.721079	197.497211	4.706982
2.916093	204.493503	4.711987
2.853780	193.945897	4.716992
3.155703	205.566685	4.721997
2.957489	196.818408	4.727002
2.440573	190.904183	4.732006
2.811600	194.715456	4.737011
2.634032	210.571727	4.742016
2.522415	201.930103	4.747021
2.962431	210.147190	4.752026
2.573208	202.801913	4.757030
2.727293	207.681732	4.762035
2.791723	217.716725	4.767040
3.083764	200.640522	4.772045
2.753921	208.895973	4.777050
3.003841	211.663199	4.782054
3.103547	210.091123	4.787059
2.980165	210.534520	4.792064
3.164833	201.210556	4.797069
3.174365	204.439390	4.802074
3.147334	202.811242	4.807078
2.858755	197.215581	4.812083
3.091790	204.655171	4.817088
2.945726	198.154489	4.822093
2.872453	201.719001	4.827098
2.926464	200.606504	4.832102
3.385153	201.325699	4.837107
3.208356	202.479821	4.842112
3.182309	200.380118	4.847117
3.002729	207.318044	4.852122
2.999677	206.938991	4.857126
3.082685	204.635537	4.862131
2.822425	198.671605	4.867136
3.221424	199.491901	4.872141
2.672474	207.367228	4.877146
2.936633	209.255859	4.882150
3.096566	202.761015	4.887155
2.941547	211.814819	4.892160
2.995314	197.819498	4.897165
3.035209	218.735369	4.902170
3.160428	226.574678	4.907174
3.340621	218.178391	4.912179
3.164319	228.184669	4.917184
3.431772	221.135132	4.922189
3.705186	227.622438	4.927194
3.376215	216.907789	4.932198
3.165804	206.130278	4.937203
3.274751	216.882799	4.942208
3.168616	223.056246	4.947213
3.473580	225.492145	4.952218
3.663915	226.123673	4.957222
3.505106	215.157736	4.962227
2.910581	211.913230	4.967232
3.457681	212.852692	4.972237
3.274920	217.057624	4.977242
3.237041	223.217214	4.982246
3.571669	218.529980	4.987251
3.295643	222.379365	4.992256
3.573951	219.507469	4.997261
3.564862	224.463479	5.002266
3.532624	220.517101	5.007270
3.209300	227.714840	5.012275
3.245548	234.207670	5.017280
3.309442	219.214156	5.022285
3.235167	229.916298	5.027290
3.368169	229.680443	5.032294
3.515327	221.991688	5.037299
3.406986	223.483101	5.042304
3.559911	226.297165	5.047309
3.614715	225.845771	5.052314
3.708455	221.870162	5.057318
3.440574	219.270506	5.062323
3.429233	226.805343	5.067328
3.842001	228.654873	5.072333
3.668264	240.163548	5.077338
3.607141	234.510090	5.082342
3.743252	227.199553	5.087347
3.695588	232.069860	5.092352
3.784274	232.853356	5.097357
3.710789	235.664929	5.102362
3.783874	227.962467	5.107366
3.827186	231.024661	5.112371
3.491246	225.477541	5.117376
4.205409	238.678921	5.122381
3.943873	239.007923	5.127386
3.850179	228.000139	5.132390
3.692302	232.606138	5.137395
3.832503	229.524924	5.142400
3.558683	224.898220	5.147405
3.761870	240.046287	5.152410
4.037023	243.591016	5.157414
4.485045	242.543334	5.162419
3.852025	235.302681	5.167424
4.020022	229.262148	5.172429
3.786987	223.401510	5.177434
3.724272	233.234970	5.182438
4.074670	226.640672	5.187443
3.663785	225.496610	5.192448
3.725862	234.247490	5.197453
4.155670	242.988214	5.202458
4.253842	242.450931	5.207462
3.961228	235.830826	5.212467
4.071442	230.571307	5.217472
3.956341	241.517135	5.222477
4.020417	249.052820	5.227482
4.041729	243.269384	5.232486
4.278802	247.022562	5.237491
4.058813	242.457022	5.242496
4.151578	234.333856	5.247501
3.641798	231.471541	5.252506
3.855447	243.131494	5.257510
3.937188	240.796597	5.262515
4.080298	249.227902	5.267520
4.117032	240.521886	5.272525
4.026358	257.706025	5.277530
4.188390	252.470018	5.282534
4.618304	250.197627	5.287539
4.067456	250.094228	5.292544
4.231268	242.260485	5.297549
4.199338	242.939493	5.302554
4.266686	238.582035	5.307558
4.280604	237.959876	5.312563
3.922656	253.107288	5.317568
4.062428	240.829043	5.322573
4.277710	249.438866	5.327578
4.050839	247.190287	5.332582
4.545394	243.468252	5.337587
4.176928	255.260549	5.342592
4.261493	248.774333	5.347597
4.014038	254.422601	5.352602
4.501575	248.585097	5.357606
4.609832	246.385251	5.362611
4.159648	244.032455	5.367616
4.705901	244.962560	5.372621
4.264919	257.047796	5.377626
4.343331	243.184620	5.382630
4.664525	248.038267	5.387635
4.328394	261.590889	5.392640
4.445913	246.535166	5.397645
4.019008	255.713850	5.402650
4.749243	261.272209	5.407654
4.867005	249.797843	5.412659
4.194402	254.218738	5.417664
4.699565	246.185977	5.422669
4.325248	249.993820	5.427674
4.322152	259.438299	5.432678
4.702010	270.521732	5.437683
4.709929	269.274082	5.442688
4.771220	275.854754	5.447693
4.437358	270.212380	5.452698
4.804593	272.201928	5.457702
4.600288	264.827652	5.462707
4.319010	274.151208	5.467712
4.692202	272.355942	5.472717
4.602938	279.017151	5.477722
4.765607	282.456125	5.482726
4.632057	286.333821	5.487731
4.927471	282.307618	5.492736
4.932611	276.349534	5.497741
4.726935	290.973242	5.502746
4.651829	279.908729	5.507750
4.705858	279.938349	5.512755
5.057565	288.273714	5.517760
5.233496	273.319549	5.522765
4.962421	266.300586	5.527770
4.433599	258.619651	5.532774
4.597917	259.188817	5.537779
4.406134	274.161514	5.542784
4.773780	265.166355	5.547789
4.823854	275.994575	5.552794
4.830299	274.914837	5.557798
4.773869	283.089518	5.562803
4.646254	288.253943	5.567808
5.184841	286.331520	5.572813
4.615475	281.112023	5.577818
5.045058	276.827516	5.582822
4.900525	278.599853	5.587827
4.608462	281.572232	5.592832
4.894811	275.886466	5.597837
4.734469	283.922403	5.602842
4.702540	289.843800	5.607846
4.820484	291.268126	5.612851
4.996156	288.921669	5.617856
4.917214	281.784011	5.622861
4.880339	291.391989	5.627866
5.187959	301.572426	5.632870
5.292456	293.093051	5.637875
5.118180	283.426647	5.642880
5.209653	292.331139	5.647885
4.794344	283.341584	5.652890
4.996738	293.019643	5.657894
5.396704	301.328470	5.662899
5.069971	306.780365	5.667904
5.395837	302.613344	5.672909
4.903373	293.888976	5.677914
4.837419	306.133786	5.682918
5.388412	308.176805	5.687923
5.267523	314.222880	5.692928
5.703239	300.351134	5.697933
5.177870	294.640680	5.702938
5.065337	294.778656	5.707942
5.061171	297.484465	5.712947
5.407560	304.368494	5.717952
5.545965	311.300931	5.722957
5.146707	301.337570	5.727962
5.353934	308.303516	5.732966
5.017171	304.610479	5.737971
5.255851	309.644752	5.742976
5.549835	303.774281	5.747981
5.446892	310.513576	5.752986
5.495821	299.777633	5.757990
5.210242	312.993340	5.762995
4.994588	311.306149	5.768000
5.560123	308.977700	5.773005
5.339299	310.999278	5.778010
5.456758	315.106573	5.783014
5.708621	309.394562	5.788019
5.470854	310.748071	5.793024
5.460634	302.561915	5.798029
5.322368	317.580048	5.803034
5.105999	312.510880	5.808038
5.365884	310.758673	5.813043
5.038633	309.221847	5.818048
5.268679	309.382078	5.823053
5.594197	311.045969	5.828058
5.037396	298.987556	5.833062
5.450992	306.354606	5.838067
5.573745	323.514860	5.843072
5.478949	321.128517	5.848077
5.608596	329.210789	5.853082
5.462744	330.945373	5.858086
5.708875	334.773082	5.863091
5.614943	333.759687	5.868096
5.979559	328.903210	5.873101
5.720201	328.722502	5.878106
6.029351	329.319598	5.883110
6.017787	315.691928	5.888115
5.270789	308.753844	5.893120
5.690096	300.633269	5.898125
5.533021	314.224315	5.903130
5.935869	317.201717	5.908134
5.879251	318.368655	5.913139
5.544880	322.727081	5.918144
5.845329	322.860463	5.923149
5.850933	330.202862	5.928154
5.915291	329.152012	5.933158
6.048056	318.159310	5.938163
5.745260	320.022888	5.943168
5.749369	314.735675	5.948173
6.051308	320.234608	5.953178
5.907550	319.814322	5.958182
5.995498	311.271092	5.963187
5.534548	318.569525	5.968192
6.183423	318.373066	5.973197
5.520477	316.844543	5.978202
5.974982	319.418378	5.983206
6.257307	322.424156	5.988211
5.913375	329.321441	5.993216
5.895741	325.480320	5.998221
5.840682	317.753604	6.003226
6.011339	326.506500	6.008230
6.104620	328.905976	6.013235
6.008153	318.414268	6.018240
5.884354	314.020302	6.023245
5.885181	314.656214	6.028250
6.117612	312.506508	6.033254
5.814983	315.853875	6.038259
5.642724	324.938911	6.043264
6.078970	322.738287	6.048269
6.081772	327.660825	6.053274
5.860138	326.806646	6.058278
5.755531	316.762309	6.063283
5.645950	324.154389	6.068288
5.802588	320.187887	6.073293
5.925012	336.940077	6.078298
5.735348	333.015175	6.083302
5.871691	333.054046	6.088307
5.860831	327.965329	6.093312
5.837316	329.465607	6.098317
5.880427	324.267194	6.103322
6.338407	321.389277	6.108326
6.231386	320.880977	6.113331
5.704216	322.191245	6.118336
6.214342	328.416871	6.123341
6.092721	328.866323	6.128346
6.210736	324.909035	6.133350
6.115101	317.353194	6.138355
5.729886	315.673587	6.143360
5.774874	316.134899	6.148365
6.271191	317.136108	6.153370
6.318107	314.597848	6.158374
5.858136	310.737450	6.163379
5.854331	310.795115	6.168384
5.692924	306.840482	6.173389
5.557829	314.875641	6.178394
5.854053	314.794547	6.183398
6.243975	322.443726	6.188403
5.747324	333.427246	6.193408
5.972800	329.462611	6.198413
6.146467	326.420430	6.203418
5.798385	328.246811	6.208422
5.807663	320.215781	6.213427
5.838821	326.193745	6.218432
5.878979	323.371801	6.223437
6.162889	331.123016	6.228442
6.021629	334.372336	6.233446
6.164518	328.807108	6.238451
5.730431	318.216436	6.243456
6.163218	313.520126	6.248461
5.979938	317.794766	6.253466
5.680578	311.716698	6.258470
5.828168	312.794692	6.263475
5.830188	327.303630	6.268480
6.076716	321.994252	6.273485
5.968482	325.943921	6.278490
5.965452	328.409108	6.283494
6.024032	330.247704	6.288499
5.863220	331.949829	6.293504
5.985355	323.711288	6.298509
5.863753	332.146142	6.303514
6.091523	327.232011	6.308518
6.164352	317.688225	6.313523
5.505817	314.292377	6.318528
6.086183	307.443717	6.323533
5.891687	318.746885	6.328538
6.007806	330.456978	6.333542
5.955640	320.258888	6.338547
5.879494	320.796128	6.343552
6.002126	310.172019	6.348557
5.928022	314.540285	6.353562
5.901773	315.411396	6.358566
5.661337	316.433126	6.363571
5.893715	322.626337	6.368576
6.059661	332.458826	6.373581
5.929496	331.166368	6.378586
6.083848	325.675276	6.383590
6.103539	317.573012	6.388595
5.788923	314.727561	6.393600
6.236752	319.099474	6.398605
5.813642	316.188763	6.403610
5.696985	311.844299	6.408614
6.042934	320.038211	6.413619
5.959420	329.213750	6.418624
5.920524	323.499833	6.423629
6.091032	318.857271	6.428634
5.788420	315.003855	6.433638
5.867440	311.372222	6.438643
5.637236	318.460494	6.443648
5.914386	327.323256	6.448653
5.841257	326.211689	6.453658
5.378686	338.037768	6.458662
5.915991	339.431194	6.463667
5.964207	329.372396	6.468672
5.678465	323.121346	6.473677
5.619765	325.244075	6.478682
5.620213	328.455372	6.483686
6.025293	330.499108	6.488691
5.834955	329.421725	6.493696
5.896076	330.671457	6.498701
6.050643	326.461666	6.503706
5.920638	323.887849	6.508710
5.934007	326.932604	6.513715
5.823855	329.047576	6.518720
6.127616	326.089417	6.523725
6.091984	331.925985	6.528730
6.157830	329.289843	6.533734
6.057502	324.060120	6.538739
6.180136	329.799124	6.543744
6.119864	319.447278	6.548749
5.890107	324.678338	6.553754
5.912947	324.292062	6.558758
6.389931	319.671084	6.563763
5.807103	331.740629	6.568768
5.981648	325.550339	6.573773
6.083053	333.311168	6.578778
6.068190	328.741940	6.583782
6.226731	321.184238	6.588787
5.906749	322.009622	6.593792
5.845115	318.659456	6.598797
5.902514	329.280915	6.603802
5.641440	320.656322	6.608806
5.841673	331.448394	6.613811
6.003686	326.680609	6.618816
6.072233	326.344119	6.623821
5.926915	328.616463	6.628826
5.910332	331.444447	6.633830
6.204335	323.182141	6.638835
5.984988	327.275770	6.643840
6.307595	322.356273	6.648845
5.583003	321.739088	6.653850
5.724620	322.887622	6.658854
6.002448	322.372808	6.663859
6.028168	327.136729	6.668864
6.216794	328.088071	6.673869
5.902515	323.284180	6.678874
5.769006	313.706286	6.683878
5.597682	310.863695	6.688883
6.213848	321.312178	6.693888
5.982713	316.140918	6.698893
6.198380	329.977299	6.703898
5.828040	320.904748	6.708902
5.893954	312.890158	6.713907
5.713274	322.663055	6.718912
5.815553	323.327365	6.723917
5.804309	335.481365	6.728922
5.714459	340.532320	6.733926
6.118327	323.818132	6.738931
5.933535	332.186956	6.743936
5.849139	329.004872	6.748941
6.079541	330.379944	6.753946
5.915155	324.144680	6.758950
6.249828	339.060257	6.763955
5.615860	335.524512	6.768960
5.997166	321.784662	6.773965
5.887157	326.822952	6.778970
6.138107	332.032481	6.783974
6.099958	328.140790	6.788979
6.098769	333.449937	6.793984
5.875124	322.604825	6.798989
5.803655	320.312906	6.803994
5.670953	322.918633	6.808998
6.211356	315.658612	6.814003
6.044325	331.295038	6.819008
5.829349	319.480450	6.824013
5.873498	323.222743	6.829018
6.068427	329.861590	6.834022
5.977285	320.166322	6.839027
5.498891	329.618869	6.844032
5.871418	326.162711	6.849037
5.959396	330.932698	6.854042
5.980136	333.033490	6.859046
6.089706	330.349368	6.864051
6.129177	336.816420	6.869056
6.280556	322.508310	6.874061
5.958344	321.695201	6.879066
5.522640	311.237666	6.884070
6.025528	312.361233	6.889075
6.142160	332.777992	6.894080
6.237206	317.314437	6.899085
6.143258	317.509614	6.904090
5.914851	315.868714	6.909094
5.694267	317.086652	6.914099
5.538209	313.453886	6.919104
5.951125	312.019391	6.924109
5.862868	324.688492	6.929114
5.995130	330.856263	6.934118
6.137790	321.684352	6.939123
6.051738	331.761970	6.944128
6.079869	315.337618	6.949133
5.921963	313.046587	6.954138
5.849613	316.579339	6.959142
6.141144	314.331786	6.964147
5.981826	311.654995	6.969152
6.017272	304.885387	6.974157
5.332831	310.510389	6.979162
6.014177	306.132645	6.984166
6.184375	317.195172	6.989171
5.930434	310.885359	6.994176
6.099117	307.005558	6.999181
5.797840	307.008590	7.004186
5.950269	322.370326	7.009190
6.084508	311.212881	7.014195
6.075796	319.693318	7.019200
5.809952	315.581037	7.024205
5.842928	319.527562	7.029210
5.864339	313.440365	7.034214
5.812100	307.348889	7.039219
5.669805	310.955875	7.044224
6.163681	309.242937	7.049229
6.018175	317.131031	7.054234
5.720780	317.927565	7.059238
5.839215	321.367150	7.064243
5.523099	329.974850	7.069248
6.037606	324.439984	7.074253
6.141926	335.677361	7.079258
6.147622	335.882236	7.084262
5.935824	327.658048	7.089267
5.739749	324.790859	7.094272
5.966552	331.756911	7.099277
5.807966	337.565289	7.104282
5.948336	332.329489	7.109286
6.225034	328.619423	7.114291
5.855081	336.745174	7.119296
6.091180	322.553506	7.124301
5.883252	323.386644	7.129306
5.834721	318.114005	7.134310
5.971596	321.474770	7.139315
5.766119	327.246198	7.144320
6.185004	321.685186	7.149325
5.916116	322.483582	7.154330
5.764037	323.194072	7.159334
6.408823	323.472822	7.164339
5.676593	322.942256	7.169344
5.878597	308.689501	7.174349
6.020664	321.455392	7.179354
5.798248	318.421486	7.184358
5.972929	316.024561	7.189363
5.968363	331.297006	7.194368
5.755095	319.811185	7.199373
6.216942	323.424757	7.204378
5.864561	313.631216	7.209382
5.873728	319.302572	7.214387
6.009509	340.788864	7.219392
5.952244	330.841506	7.224397
5.893946	326.063947	7.229402
5.858480	326.006349	7.234406
6.270215	330.251040	7.239411
6.204362	325.927087	7.244416
6.199867	318.698654	7.249421
6.353312	327.751644	7.254426
6.421348	326.083279	7.259430
6.199597	314.551333	7.264435
5.835972	323.074724	7.269440
5.803980	316.711151	7.274445
5.753329	309.154593	7.279450
5.791258	314.425967	7.284454
6.224684	309.520748	7.289459
6.212224	315.227129	7.294464
6.191571	316.780741	7.299469
6.003056	312.805044	7.304474
5.851763	316.116044	7.309478
6.034536	317.005026	7.314483
6.132351	322.532779	7.319488
6.027916	315.139670	7.324493
5.701422	321.714677	7.329498
6.119252	319.868119	7.334502
6.124411	308.414521	7.339507
5.887636	308.211292	7.344512
5.914222	309.425305	7.349517
5.835953	316.989649	7.354522
5.772101	307.271129	7.359526
5.812694	312.244690	7.364531
5.704086	318.652678	7.369536
5.729838	313.725910	7.374541
5.848260	316.229015	7.379546
5.774399	321.717226	7.384550
5.670031	318.041558	7.389555
5.360454	318.919096	7.394560
5.467893	317.820367	7.399565
5.510265	318.699709	7.404570
5.404351	332.665572	7.409574
6.059401	331.990413	7.414579
6.218968	339.175813	7.419584
6.318550	328.653381	7.424589
5.941404	330.092006	7.429594
6.063112	320.138759	7.434598
5.847941	312.029003	7.439603
5.755851	320.490866	7.444608
5.850448	331.492480	7.449613
6.290850	337.773326	7.454618
6.159738	319.228871	7.459622
5.988854	317.752966	7.464627
5.785435	327.111808	7.469632
6.025996	312.982724	7.474637
5.815690	317.179340	7.479642
5.617089	321.181132	7.484646
5.923966	318.836260	7.489651
5.978775	328.967738	7.494656
5.808891	328.380701	7.499661
6.156279	330.060149	7.504666
5.864263	330.903298	7.509670
5.985012	317.732628	7.514675
5.807023	317.311379	7.519680
6.235865	324.141367	7.524685
6.210767	321.639699	7.529690
5.662345	325.126820	7.534694
6.094846	305.168444	7.539699
5.785946	317.849964	7.544704
5.987017	317.764797	7.549709
5.848558	322.152639	7.554714
6.026290	314.721648	7.559718
6.241359	317.022947	7.564723
6.133482	314.376061	7.569728
5.997739	313.650796	7.574733
5.948692	319.894427	7.579738
5.665262	320.040197	7.584742
5.890233	315.265715	7.589747
5.785788	312.494904	7.594752
6.035260	311.029069	7.599757
5.847160	321.628876	7.604762
5.796847	323.345326	7.609766
6.081887	321.456297	7.614771
5.832808	319.223844	7.619776
5.845049	305.054608	7.624781
5.850317	318.844851	7.629786
5.793755	316.904940	7.634790
6.044343	321.339395	7.639795
5.966435	326.575138	7.644800
6.316927	318.623527	7.649805
6.152774	322.942628	7.654810
6.135731	316.848799	7.659814
6.221541	312.153069	7.664819
5.868924	319.412383	7.669824
6.054483	319.971894	7.674829
5.778892	322.517752	7.679834
5.990706	313.784268	7.684838
5.851795	313.296784	7.689843
5.880354	324.150551	7.694848
5.987344	311.969143	7.699853
5.804627	321.217169	7.704858
5.890293	306.005034	7.709862
6.068067	308.441890	7.714867
5.812140	316.910439	7.719872
5.976593	313.787445	7.724877
5.541563	311.182326	7.729882
5.440197	311.131889	7.734886
5.788878	312.896556	7.739891
5.944805	328.324189	7.744896
6.214417	331.939408	7.749901
5.756775	324.063792	7.754906
5.889735	333.328804	7.759910
6.321169	332.514673	7.764915
5.606694	322.575378	7.769920
5.927115	324.271706	7.774925
6.155419	323.745669	7.779930
5.671433	329.513278	7.784934
6.136124	328.187730	7.789939
6.047610	329.068597	7.794944
5.792988	327.653269	7.799949
5.874666	327.048964	7.804954
5.974708	328.336891	7.809958
6.087357	321.311569	7.814963
5.789215	326.062957	7.819968
5.888326	313.164602	7.824973
5.659943	318.215110	7.829978
5.676352	323.309523	7.834982
6.136583	327.160633	7.839987
6.013019	330.426162	7.844992
6.219959	323.952383	7.849997
5.907801	320.470625	7.855002
5.694908	321.497531	7.860006
5.908097	335.046399	7.865011
6.143224	333.174681	7.870016
6.019777	326.151547	7.875021
6.006721	331.124027	7.880026
6.164050	327.916725	7.885030
6.110269	317.633467	7.890035
5.869571	318.430609	7.895040
5.557229	312.107800	7.900045
6.040033	322.159559	7.905050
5.780051	312.743852	7.910054
6.219616	315.563639	7.915059
5.862525	315.939252	7.920064
5.780407	310.447249	7.925069
6.001538	322.125065	7.930074
5.978391	314.118101	7.935078
5.798304	307.730278	7.940083
6.074236	316.567915	7.945088
6.070390	315.315779	7.950093
6.045826	313.032330	7.955098
5.837872	312.954300	7.960102
6.043014	309.220649	7.965107
6.209398	314.003656	7.970112
6.173772	306.457400	7.975117
5.802125	315.833103	7.980122
5.730770	308.486033	7.985139
6.045962	315.382500	7.990157
6.044450	313.760820	7.995174
6.186811	302.996580	8.000192
5.996723	311.149295	8.005210
6.027388	317.093137	8.010227
6.086539	308.531999	8.015245
5.950309	305.855328	8.020262
6.089083	312.934066	8.025280
6.212918	306.675935	8.030298
5.780448	314.948676	8.035315
6.240385	301.565927	8.040333
6.198923	316.357071	8.045350
6.009717	305.887770	8.050368
6.033836	314.786386	8.055386
5.927441	313.474621	8.060403
5.962286	312.124947	8.065421
5.365357	308.188746	8.070438
5.696902	306.811520	8.075456
5.982992	306.501736	8.080474
5.821175	308.370149	8.085491
5.909484	315.437860	8.090509
5.877130	322.256244	8.095526
6.088073	324.672152	8.100544
6.325901	328.481830	8.105562
6.006847	315.113829	8.110579
6.064791	311.526289	8.115597
5.931455	314.586256	8.120614
5.985555	321.356381	8.125632
5.907091	318.705370	8.130650
6.328635	320.116319	8.135667
6.446289	325.686782	8.140685
6.500113	332.368595	8.145702
5.945216	313.508726	8.150720
6.060438	318.394778	8.155738
5.676805	307.100740	8.160755
6.069831	307.392721	8.165773
6.281343	326.382364	8.170790
6.120888	319.764839	8.175808
5.994022	314.044588	8.180826
5.877836	320.257586	8.185843
6.380620	329.377849	8.190861
5.912195	330.600045	8.195878
6.068497	335.700566	8.200896
6.101440	326.525004	8.205914
5.944642	328.812343	8.210931
6.343962	324.092057	8.215949
6.091208	334.015492	8.220966
6.154078	326.659248	8.225984
6.211271	333.858071	8.231002
5.960818	330.962614	8.236019
6.366166	322.722757	8.241037
6.066234	335.878729	8.246054
6.147578	333.401488	8.251072
6.148998	335.200147	8.256090
5.964937	336.314674	8.261107
6.475627	342.000282	8.266125
6.144025	338.467459	8.271142
6.422454	333.848161	8.276160
6.069636	333.054674	8.281178
5.801713	337.249701	8.286195
6.076820	335.751930	8.291213
6.180834	331.043199	8.296230
6.188257	327.772832	8.301248
6.542954	330.030521	8.306266
6.305221	327.303480	8.311283
6.443260	323.368882	8.316301
6.385991	337.976334	8.321318
6.182507	329.601499	8.326336
6.544797	329.904608	8.331354
6.195814	335.204214	8.336371
6.068977	325.479347	8.341389
6.185072	329.153469	8.346406
6.043532	324.079281	8.351424
6.308900	328.828205	8.356442
6.170610	330.591950	8.361459
6.430504	334.552803	8.366477
6.248285	342.653808	8.371494
6.442202	330.464555	8.376512
6.431471	337.358450	8.381530
6.300253	340.875669	8.386547
6.239134	337.789604	8.391565
6.266739	339.928134	8.396582
6.314649	329.093473	8.401600
6.270126	334.108697	8.406618
6.104872	341.891471	8.411635
6.588295	347.265781	8.416653
6.451898	348.230834	8.421670
6.520446	356.409316	8.426688
6.546212	333.523261	8.431706
6.232273	340.332123	8.436723
6.506793	338.515717	8.441741
6.305913	342.217415	8.446758
6.540285	339.817180	8.451776
6.831674	343.422815	8.456794
6.604248	341.956446	8.461811
6.653090	330.645124	8.466829
6.400696	327.469112	8.471846
6.695566	338.625838	8.476864
6.395654	333.065235	8.481882
6.474290	339.206690	8.486899
6.520021	331.237763	8.491917
6.539077	335.110123	8.496934
6.405874	322.751228	8.501952
6.478279	325.027900	8.506970
5.946538	327.506525	8.511987
6.319851	326.463571	8.517005
6.314713	328.253789	8.522022
6.340289	335.624820	8.527040
6.785662	347.638416	8.532058
6.670042	341.301029	8.537075
6.502352	333.573818	8.542093
6.702696	331.257808	8.547110
6.410205	333.159320	8.552128
6.581070	320.765408	8.557146
6.296975	331.375387	8.562163
6.574548	340.524631	8.567181
6.518970	345.882408	8.572199
6.687404	348.273422	8.577216
6.638516	334.061523	8.582234
6.480017	338.469773	8.587251
6.709656	332.409644	8.592269
6.540562	333.572318	8.597287
6.057184	341.332354	8.602304
6.430104	343.530387	8.607322
6.218990	359.910231	8.612339
6.543229	355.223791	8.617357
6.097824	359.380361	8.622375
6.427637	357.201849	8.627392
6.750085	357.271366	8.632410
6.485061	356.413630	8.637427
6.538775	354.672842	8.642445
6.849625	357.663221	8.647463
6.724236	355.284638	8.652480
7.045872	351.002540	8.657498
6.785408	353.722679	8.662515
6.837059	354.399500	8.667533
6.378581	357.387344	8.672551
6.567634	354.606053	8.677568
6.657540	354.106106	8.682586
6.747413	354.524480	8.687603
6.787273	356.484371	8.692621
7.200258	356.874210	8.697639
6.578380	356.413204	8.702656
6.869210	357.510130	8.707674
6.397298	363.144577	8.712691
6.765780	353.944830	8.717709
6.741758	358.290991	8.722727
6.763060	361.512925	8.727744
6.985172	358.237316	8.732762
6.338633	363.245889	8.737779
6.602349	361.270232	8.742797
6.942485	360.535423	8.747815
6.770949	350.681850	8.752832
6.993616	354.512844	8.757850
7.011575	359.085951	8.762867
6.922589	358.273214	8.767885
6.836865	350.829792	8.772903
6.821871	366.784449	8.777920
6.892178	361.733861	8.782938
6.642509	360.577080	8.787955
6.811176	354.712685	8.792973
6.986250	351.400267	8.797991
6.918349	362.837903	8.803008
7.130778	357.373739	8.808026
7.016184	352.184870	8.813043
6.694660	343.219469	8.818061
6.552807	349.654243	8.823079
6.433709	350.805929	8.828096
6.555613	342.648342	8.833114
6.451876	351.065250	8.838131
6.390740	356.546974	8.843149
6.512549	352.741141	8.848167
6.431026	361.653177	8.853184
6.902879	367.868729	8.858202
6.817336	376.923410	8.863219
7.290233	379.238323	8.868237
7.249481	374.255624	8.873255
7.009606	362.153250	8.878272
6.956386	363.222034	8.883290
6.796702	360.716283	8.888307
6.852546	357.488815	8.893325
7.016148	355.992735	8.898343
6.966171	360.071571	8.903360
6.983218	356.865961	8.908378
7.059531	357.194943	8.913395
7.194770	346.911463	8.918413
7.133571	350.278862	8.923431
6.664492	355.045038	8.928448
7.130196	346.458052	8.933466
6.839441	350.965921	8.938483
7.074790	354.189029	8.943501
7.235262	348.177601	8.948519
6.868193	355.821593	8.953536
7.077696	357.489824	8.958554
7.004595	364.601779	8.963571
6.956473	355.580912	8.968589
6.946934	355.715068	8.973607
6.879659	366.325809	8.978624
6.841379	353.412391	8.983642
6.942831	370.153516	8.988659
7.067979	375.356756	8.993677
7.511483	375.744969	8.998695
6.877426	384.169245	9.003712
7.444517	369.463184	9.008730
6.976537	369.255769	9.013747
7.031580	366.990922	9.018765
6.985536	348.799195	9.023783
6.790043	358.584288	9.028800
6.792537	376.480139	9.033818
7.044465	375.140628	9.038835
7.304169	381.405203	9.043853
7.462239	382.863750	9.048871
7.187320	386.324600	9.053888
7.046247	377.005868	9.058906
6.811175	381.334610	9.063923
7.039518	381.175881	9.068941
6.969755	384.064957	9.073959
7.158609	388.832196	9.078976
7.037300	387.043091	9.083994
7.261690	393.082834	9.089011
7.393728	380.770702	9.094029
7.240699	389.924324	9.099047
7.125183	382.738014	9.104064
7.266237	379.068013	9.109082
7.215382	394.719052	9.114099
6.829999	391.828947	9.119117
6.918662	386.986910	9.124135
7.220763	393.819189	9.129152
7.479440	383.569994	9.134170
7.154695	383.286489	9.139187
7.238262	395.890125	9.144205
7.401976	383.929625	9.149223
7.438791	388.348310	9.154240
7.262105	390.077052	9.159258
7.317345	389.232250	9.164275
7.681720	391.024538	9.169293
7.386441	381.853038	9.174311
7.185274	394.128909	9.179328
7.316138	385.657481	9.184346
7.408175	394.873692	9.189363
7.354971	386.626759	9.194381
7.529740	390.114980	9.199399
7.395607	399.354006	9.204416
7.559836	386.042771	9.209434
7.213691	373.818188	9.214451
7.358648	364.905917	9.219469
6.975026	369.377848	9.224487
7.108668	384.160548	9.229504
7.624014	384.275580	9.234522
7.723538	385.134244	9.239539
7.480699	379.384807	9.244557
7.353923	370.603468	9.249575
7.124315	369.336249	9.254592
7.451973	379.793604	9.259610
7.459208	390.023465	9.264627
7.462629	382.591307	9.269645
7.332015	366.227358	9.274663
6.998510	384.851188	9.279680
7.594557	383.511407	9.284698
7.728861	391.209399	9.289715
7.662066	397.338947	9.294733
7.305247	381.600547	9.299751
7.118335	379.345206	9.304768
7.384484	384.671521	9.309786
7.788153	383.529136	9.314803
7.487066	381.916518	9.319821
7.290773	374.947990	9.324839
7.675332	388.018844	9.329856
7.383195	390.488337	9.334874
7.661001	385.837566	9.339891
7.770299	382.832087	9.344909
7.520799	373.012806	9.349927
6.991501	375.402695	9.354944
7.327776	368.732569	9.359962
7.438403	383.982766	9.364979
7.403249	392.133333	9.369997
7.834833	385.312572	9.375015
7.427582	391.050503	9.380032
7.348700	389.450405	9.385050
7.663184	389.656867	9.390067
7.191856	397.853686	9.395085
7.464933	388.148175	9.400103
7.516001	399.488301	9.405120
7.049061	394.108479	9.410138
7.419249	389.395897	9.415155
7.123041	390.404926	9.420173
7.469647	390.495904	9.425191
7.360732	402.545892	9.430208
7.740937	402.663163	9.435226
7.699922	408.021833	9.440243
7.436506	415.258299	9.445261
7.568995	410.153774	9.450279
7.470197	420.535962	9.455296
8.119670	420.544774	9.460314
8.138663	409.070825	9.465331
7.703936	392.293763	9.470349
7.442143	389.668310	9.475367
7.518687	393.058315	9.480384
7.472114	389.474513	9.485402
7.751684	400.715724	9.490419
7.756069	412.801614	9.495437
7.804315	406.845619	9.500455
7.697391	393.144527	9.505472
7.613230	393.672218	9.510490
7.882410	392.509880	9.515507
7.878914	397.843734	9.520525
8.199085	379.316893	9.525543
7.596399	392.536121	9.530560
7.720886	391.273379	9.535578
7.710231	382.328677	9.540595
7.485143	388.347327	9.545613
7.334303	384.372773	9.550631
7.745052	398.414651	9.555648
8.000298	405.165915	9.560666
8.067769	400.986743	9.565683
8.039966	397.848111	9.570701
8.282080	393.199775	9.575719
8.005073	392.722602	9.580736
7.463395	387.111501	9.585754
7.656307	390.805157	9.590771
7.268280	383.598430	9.595789
7.617800	401.124361	9.600807
7.460778	403.216089	9.605824
7.491839	420.318576	9.610842
8.143590	406.915161	9.615859
7.834465	415.190713	9.620877
8.210719	405.497428	9.625895
8.063099	412.368620	9.630912
8.004186	407.215191	9.635930
8.246510	411.320823	9.640947
7.892688	412.420928	9.645965
8.018268	410.785638	9.650983
8.199900	412.391971	9.656000
7.773356	388.639460	9.661018
7.862272	388.732944	9.666035
8.149261	401.569792	9.671053
8.070672	395.434862	9.676071
7.881290	391.715648	9.681088
7.996103	389.738071	9.686106
7.858775	389.469382	9.691123
7.628014	384.746819	9.696141
8.090798	397.048048	9.701159
8.094115	405.189437	9.706176
8.119741	407.019024	9.711194
8.181196	409.537258	9.716211
7.985770	393.470610	9.721229
7.706372	381.879333	9.726247
7.688806	396.360694	9.731264
7.931204	408.213634	9.736282
8.049724	405.225641	9.741299
7.847488	411.423751	9.746317
8.050109	409.463972	9.751335
8.235945	417.816606	9.756352
8.219607	421.625103	9.761370
8.215932	404.591148	9.766387
8.199770	414.237722	9.771405
7.970592	415.523421	9.776423
7.972520	418.653729	9.781440
7.827791	416.540094	9.786458
8.009930	418.092700	9.791475
7.901598	413.183693	9.796493
8.015359	410.003945	9.801511
8.313450	405.652941	9.806528
7.956530	407.826481	9.811546
8.105239	409.870308	9.816563
7.619195	415.592190	9.821581
8.184993	405.291708	9.826599
8.222043	407.428767	9.831616
8.043277	413.421233	9.836634
8.180255	409.155430	9.841651
7.967036	408.829205	9.846669
7.996171	409.294965	9.851687
7.957890	413.349891	9.856704
7.935787	429.223668	9.861722
8.576160	423.427351	9.866739
8.541462	433.973069	9.871757
8.767220	418.073932	9.876775
8.593300	409.464059	9.881792
8.052852	415.368030	9.886810
8.404625	407.688783	9.891827
8.174265	414.967406	9.896845
8.377226	407.955244	9.901863
8.577509	401.924937	9.906880
8.396793	408.507829	9.911898
8.489516	407.603505	9.916915
8.327158	412.899139	9.921933
8.472805	405.166984	9.926951
8.331920	409.237984	9.931968
8.387460	414.407962	9.936986
8.482568	412.468184	9.942003
7.994148	415.151467	9.947021
8.282479	408.125929	9.952039
8.085638	404.493086	9.957056
8.248322	404.941077	9.962074
8.337888	406.404048	9.967091
8.191163	402.839090	9.972109
8.258135	408.408053	9.977127
8.347372	411.594106	9.982144
7.921679	408.653511	9.987162
8.490744	406.437506	9.992179
8.520907	412.851663	9.997197
8.554838	411.836633	10.002215
8.362451	403.134984	10.007232
8.052638	412.571952	10.012250
8.688627	414.690907	10.017267
8.443119	415.878182	10.022285
8.323830	407.272373	10.027303
8.445231	402.365243	10.032320
8.193965	422.112290	10.037338
8.359381	422.326329	10.042355
8.728254	439.136070	10.047373
8.717434	441.192272	10.052391
8.645067	439.363936	10.057408
8.168536	426.058393	10.062426
8.353482	425.732898	10.067443
8.587047	440.954414	10.072461
8.599808	434.369666	10.077479
8.803046	422.642783	10.082496
8.634697	438.425876	10.087514
8.613897	417.973771	10.092531
8.375348	410.046195	10.097549
8.365439	428.846583	10.102567
8.700721	425.553230	10.107584
8.533841	433.169045	10.112602
8.501994	435.452599	10.117619
8.512033	437.511844	10.122637
8.648289	436.613321	10.127655
8.916646	438.379633	10.132672
8.536676	433.939206	10.137690
8.944658	433.032822	10.142707
8.339963	432.341908	10.147725
8.623671	429.119750	10.152743
8.855417	432.403397	10.157760
8.605303	442.802995	10.162778
9.156590	428.875673	10.167795
8.360630	428.072719	10.172813
8.493919	430.544988	10.177831
8.787635	428.435237	10.182848
8.586134	431.348118	10.187866
8.822110	428.518439	10.192883
8.853614	428.087599	10.197901
8.743388	436.035358	10.202919
8.831931	432.821688	10.207936
8.733330	434.058528	10.212954
8.779466	417.382822	10.217971
8.666214	428.928590	10.222989
8.647333	436.117283	10.228007
9.248212	435.474160	10.233024
8.687128	428.225102	10.238042
8.612912	425.507140	10.243059
8.684800	424.659727	10.248077
8.800247	428.031021	10.253095
8.858415	438.723134	10.258112
8.700110	438.258919	10.263130
9.010737	430.179018	10.268147
9.023692	440.811946	10.273165
8.970899	432.915215	10.278183
8.633020	428.162087	10.283200
8.458504	430.777255	10.288218
8.910082	429.535845	10.293235
9.161040	433.980948	10.298253
8.826824	440.363845	10.303271
8.974663	440.946704	10.308288
8.888012	436.103720	10.313306
9.165293	441.469333	10.318323
9.225212	429.774368	10.323341
8.657541	417.133193	10.328359
8.605029	428.735715	10.333376
9.062898	440.520204	10.338394
9.074355	433.982996	10.343411
9.278414	432.673071	10.348429
8.883432	418.455371	10.353447
8.779010	430.053404	10.358464
8.575688	436.927021	10.363482
9.150405	428.212465	10.368499
9.274971	429.354380	10.373517
8.942574	434.550433	10.378535
9.055444	430.913238	10.383552
9.075889	438.089459	10.388570
9.012049	430.093476	10.393587
8.860503	433.181562	10.398605
8.746387	431.302965	10.403623
9.168835	431.236897	10.408640
9.147741	432.073437	10.413658
9.296837	435.158599	10.418675
8.627137	432.480288	10.423693
8.347470	436.898080	10.428711
8.733224	436.910343	10.433728
8.774411	438.456634	10.438746
8.997502	434.934711	10.443763
8.834332	438.223430	10.448781
9.212267	437.444828	10.453799
9.113844	443.446806	10.458816
9.406275	440.601969	10.463834
9.282247	439.766317	10.468851
9.256927	439.984995	10.473869
8.998683	435.699061	10.478887
9.111559	441.011539	10.483904
8.940927	440.552410	10.488922
8.966423	437.948208	10.493939
9.269093	449.517183	10.498957
9.023018	466.669448	10.503975
9.316192	454.653903	10.508992
9.280478	455.707326	10.514010
9.307099	452.452863	10.519027
9.119479	457.159189	10.524045
9.225480	463.204882	10.529063
9.420009	451.930616	10.534080
9.163849	463.003346	10.539098
9.410360	449.669704	10.544115
9.485148	461.053489	10.549133
9.442247	455.032865	10.554151
9.292544	444.620408	10.559168
9.242032	439.629752	10.564186
9.133610	443.648338	10.569203
9.605443	448.529043	10.574221
9.370443	442.251349	10.579239
9.145903	433.084518	10.584256
9.105842	449.661701	10.589274
9.212667	456.619273	10.594291
9.249080	458.964716	10.599309
9.248785	462.912717	10.604327
9.273953	460.002456	10.609344
9.486062	467.454766	10.614362
9.296304	459.683622	10.619379
9.386869	457.867624	10.624397
9.044271	460.313476	10.629415
9.803973	453.924108	10.634432
9.425089	459.793313	10.639450
9.540243	454.363294	10.644467
9.778498	456.793875	10.649485
9.368060	466.764180	10.654503
9.598157	459.369057	10.659520
9.296270	453.376388	10.664538
9.235863	447.049247	10.669555
9.661445	463.124305	10.674573
9.288463	461.563968	10.679591
9.668538	456.720434	10.684608
9.648123	455.666580	10.689626
9.727757	456.398979	10.694643
9.749997	450.702659	10.699661
9.625868	461.486463	10.704679
9.466596	454.417431	10.709696
9.597516	457.789461	10.714714
9.606351	455.108973	10.719731
9.516076	461.567264	10.724749
9.374968	459.465679	10.729767
9.596416	456.562534	10.734784
9.597660	460.314637	10.739802
9.387754	464.882449	10.744819
9.401749	453.481836	10.749837
9.473946	462.044796	10.754855
9.812496	466.839094	10.759872
9.880127	462.233857	10.764890
9.348352	459.959957	10.769907
9.736665	458.914645	10.774925
9.704840	459.124876	10.779943
9.903972	458.601501	10.784960
9.685237	466.421111	10.789978
9.719794	456.472073	10.794995
9.744731	464.054691	10.800013
9.576532	465.343463	10.805031
9.243346	470.943585	10.810048
9.574112	466.549578	10.815066
9.294521	467.716950	10.820083
9.775578	470.156826	10.825101
9.759558	485.600520	10.830119
10.180893	476.026363	10.835136
10.021623	469.380195	10.840154
9.664058	465.583176	10.845171
9.901288	453.525906	10.850189
9.560794	464.671809	10.855207
9.646414	454.711616	10.860224
9.777447	463.192776	10.865242
9.487982	471.197035	10.870259
9.896832	472.931872	10.875277
10.267863	490.233619	10.880295
10.524329	476.731142	10.885312
10.079499	470.972299	10.890330
9.667357	457.568283	10.895347
9.805031	455.113756	10.900365
9.702814	456.111328	10.905383
10.178972	453.947744	10.910400
9.740517	457.314312	10.915418
9.685807	456.344725	10.920435
10.005168	450.005417	10.925453
9.870986	447.710248	10.930471
10.063291	459.773039	10.935488
10.133136	461.516809	10.940506
9.810976	460.216748	10.945523
9.915237	456.511471	10.950541
9.619411	472.860511	10.955559
10.227179	470.076713	10.960576
10.436947	469.835688	10.965594
10.160310	463.170042	10.970611
10.199675	458.117963	10.975629
9.776594	464.669424	10.980647
10.153254	454.385925	10.985664
9.688640	460.880776	10.990682
9.923875	470.844591	10.995699
10.190350	473.497966	11.000717
9.983541	483.288055	11.005735
10.112639	477.499246	11.010752
10.319238	486.476652	11.015770
10.185548	476.901096	11.020787
10.569505	475.607162	11.025805
10.035893	465.478901	11.030823
10.113499	451.382786	11.035840
9.947421	447.467409	11.040858
9.784432	456.370166	11.045875
9.937612	469.108110	11.050893
10.199131	478.471375	11.055911
10.215509	476.815320	11.060928
10.616992	476.216060	11.065946
10.200091	481.715695	11.070963
10.081221	483.902438	11.075981
10.341756	480.614475	11.080999
10.212810	482.039107	11.086016
10.458894	479.589681	11.091034
10.123890	470.790426	11.096051
10.343022	474.123393	11.101069
10.343681	479.043217	11.106087
9.979129	473.748312	11.111104
10.093896	473.253934	11.116122
10.007366	481.611403	11.121139
10.424021	478.409431	11.126157
10.197943	481.708016	11.131175
10.317620	482.809675	11.136192
10.216311	485.192479	11.141210
9.928161	482.668970	11.146227
10.415008	475.132629	11.151245
10.461795	488.635169	11.156263
10.602399	477.227327	11.161280
10.632532	464.388315	11.166298
10.268164	479.637279	11.171315
10.551012	475.793566	11.176333
10.130080	490.637999	11.181351
10.517401	483.574831	11.186368
10.520938	476.871594	11.191386
10.480565	473.264713	11.196403
10.512621	468.317916	11.201421
10.441246	478.162520	11.206439
10.589537	476.457394	11.211456
10.616540	465.291417	11.216474
10.286363	470.525002	11.221491
10.647455	473.879906	11.226509
10.501742	472.236624	11.231527
10.522501	478.680680	11.236544
10.222158	472.372188	11.241562
10.433740	480.345284	11.246579
10.391366	477.325684	11.251597
10.268387	473.431950	11.256615
10.468770	475.846377	11.261632
10.636350	461.600460	11.266650
10.412072	474.315499	11.271667
10.639185	473.850854	11.276685
10.545173	473.802590	11.281703
10.532870	459.086252	11.286720
10.429336	463.463830	11.291738
10.274277	478.272908	11.296755
10.787500	470.805018	11.301773
10.324924	482.077355	11.306791
10.779484	490.564641	11.311808
10.774022	492.149803	11.316826
10.796792	501.080282	11.321843
10.819326	477.935775	11.326861
10.501275	483.994269	11.331879
10.622428	487.800173	11.336896
10.907714	494.341641	11.341914
10.669987	488.285260	11.346931
11.066921	483.126658	11.351949
11.001963	473.521400	11.356967
10.792117	467.296559	11.361984
10.762876	473.436028	11.367002
10.403700	472.324799	11.372019
10.786534	463.567708	11.377037
10.223759	469.083884	11.382055
10.532247	488.973671	11.387072
11.196503	484.300195	11.392090
10.999459	496.644916	11.397107
11.356569	500.069876	11.402125
10.841942	485.154515	11.407143
10.611902	475.994835	11.412160
11.034133	479.570531	11.417178
10.948685	472.852835	11.422195
11.044572	476.078882	11.427213
11.100069	477.922731	11.432231
10.782781	474.772639	11.437248
10.789451	462.975544	11.442266
10.530517	471.483095	11.447283
10.968630	485.230426	11.452301
10.966562	493.577823	11.457319
10.940206	490.426326	11.462336
11.225450	496.945711	11.467354
10.933533	485.839157	11.472371
11.228140	481.741140	11.477389
11.104855	479.204423	11.482407
10.941419	471.713167	11.487424
10.856126	475.781783	11.492442
11.141407	489.054456	11.497459
11.016588	481.049069	11.502477
10.667559	490.375460	11.507495
11.069194	489.580520	11.512512
11.451154	488.867555	11.517530
11.228628	484.632816	11.522547
11.143071	481.547399	11.527565
10.885063	468.034020	11.532583
11.097278	482.640393	11.537600
11.012944	485.859966	11.542618
11.232235	499.117739	11.547635
11.350881	493.747120	11.552653
11.363481	486.950942	11.557671
11.205025	481.557474	11.562688
11.107870	473.923290	11.567706
10.688248	470.031854	11.572723
11.440695	481.258985	11.577741
11.471706	489.392918	11.582759
11.165257	483.129559	11.587776
11.001599	469.358404	11.592794
11.381563	485.869812	11.597811
11.286664	483.006760	11.602829
11.306613	481.466907	11.607847
11.562905	480.906174	11.612864
11.413918	465.109891	11.617882
11.129564	476.650941	11.622899
11.476295	467.542905	11.627917
11.231171	469.556928	11.632935
11.447170	467.951646	11.637952
11.536471	468.666752	11.642970
11.229063	457.704651	11.647987
11.370955	460.475372	11.653005
11.502582	463.714751	11.658023
11.295121	478.326916	11.663040
11.383039	465.482005	11.668058
11.336501	468.335898	11.673075
11.421276	461.881865	11.678093
11.378721	458.262705	11.683111
11.312162	467.011507	11.688128
11.137323	463.012293	11.693146
11.422797	477.607183	11.698163
11.349897	481.112136	11.703181
11.512338	494.217870	11.708199
11.485426	498.046975	11.713216
11.615544	495.555758	11.718234
11.484570	501.780603	11.723251
11.494739	500.485273	11.728269
11.707755	495.778354	11.733287
11.153343	493.419635	11.738304
11.524381	491.932068	11.743322
11.433950	491.337299	11.748339
11.587245	489.442043	11.753357
11.309193	495.421691	11.758375
11.248917	507.505154	11.763392
11.703633	489.755524	11.768410
11.315103	504.241448	11.773427
11.244442	487.154794	11.778445
11.653482	499.082669	11.783463
11.336791	502.524840	11.788480
11.669460	496.464292	11.793498
11.641929	498.223323	11.798515
11.465394	491.532515	11.803533
11.478169	491.855676	11.808551
11.342376	497.794102	11.813568
11.544656	497.166093	11.818586
11.557852	513.078595	11.823603
11.467162	511.190007	11.828621
11.898291	513.085456	11.833639
11.805483	512.977044	11.838656
12.225907	512.062396	11.843674
11.982589	514.836676	11.848691
11.792229	509.224139	11.853709
11.791266	499.249085	11.858727
11.459174	499.452714	11.863744
11.693899	508.734988	11.868762
11.662841	517.976861	11.873779
11.922265	526.412689	11.878797
12.109914	521.220596	11.883815
11.703491	529.233739	11.888832
12.201234	515.387322	11.893850
12.279499	498.905318	11.898867
11.409577	503.762740	11.903885
11.712657	505.555176	11.908903
11.628605	516.638842	11.913920
11.735198	510.298136	11.918938
11.542907	513.029708	11.923955
11.614801	513.665494	11.928973
11.561902	523.052800	11.933991
12.015692	518.787825	11.939008
12.317546	518.339871	11.944026
12.156932	519.072045	11.949043
11.949607	513.244418	11.954061
12.118617	517.374184	11.959079
12.204462	519.664554	11.964096
12.425289	507.767605	11.969114
12.242895	512.365831	11.974131
11.880905	510.260979	11.979149
12.151630	515.835921	11.984167
12.139127	526.381372	11.989184
12.347118	513.691180	11.994202
12.096590	519.360416	11.999219
12.249426	508.461870	12.004237
12.443970	514.449527	12.009255
12.241106	511.543428	12.014272
12.315190	513.453794	12.019290
12.081994	500.999991	12.024307
11.953957	500.710910	12.029325
12.319981	509.253102	12.034343
12.325364	515.289332	12.039360
12.651825	491.983581	12.044378
12.075034	497.457780	12.049395
11.911296	485.766264	12.054413
12.042148	493.225005	12.059431
11.897538	509.222188	12.064448
12.113136	514.502814	12.069466
11.781780	514.728418	12.074483
12.194401	513.199621	12.079501
12.113305	509.728499	12.084519
12.246341	516.552601	12.089536
12.163408	511.740571	12.094554
12.345925	504.860960	12.099571
12.356317	502.909199	12.104589
12.403203	501.488198	12.109607
12.300371	513.957023	12.114624
12.342024	513.931684	12.119642
12.531508	518.089800	12.124659
12.129321	520.724874	12.129677
12.519625	515.065537	12.134695
11.964072	514.452125	12.139712
12.202749	512.202668	12.144730
12.221573	516.968181	12.149747
12.443358	532.497730	12.154765
12.551971	528.201630	12.159783
12.642567	536.143215	12.164800
12.516931	527.421579	12.169818
12.423514	520.847123	12.174835
12.177222	526.581968	12.179853
12.347957	529.610109	12.184871
12.494241	538.003709	12.189888
12.765916	535.812195	12.194906
12.917519	537.088734	12.199923
12.802450	539.139191	12.204941
12.605998	513.696845	12.209959
12.543009	518.828621	12.214976
12.254879	512.843244	12.219994
12.357707	515.847308	12.225011
12.229965	530.333418	12.230029
12.847474	526.967426	12.235047
12.814522	533.700779	12.240064
12.884050	532.452950	12.245082
12.913281	537.317822	12.250099
12.961390	541.027886	12.255117
12.647649	520.425905	12.260135
12.512008	519.443748	12.265152
12.742552	534.315530	12.270170
12.871317	527.488513	12.275187
12.848128	527.072552	12.280205
12.846103	517.621509	12.285223
12.517904	512.598603	12.290240
12.707746	533.112934	12.295258
12.496805	538.889581	12.300275
12.630974	552.094460	12.305293
12.749548	537.692060	12.310311
12.819319	544.068501	12.315328
12.798540	541.925963	12.320346
12.677908	538.243282	12.325363
12.467373	543.634864	12.330381
12.887054	535.140205	12.335399
12.662628	543.664473	12.340416
12.530030	531.153863	12.345434
12.737990	531.866159	12.350451
12.609391	536.541168	12.355469
12.875833	542.467078	12.360487
12.963501	552.851685	12.365504
13.304631	551.428759	12.370522
13.279925	538.361604	12.375539
12.856502	548.570670	12.380557
12.988660	532.184331	12.385575
12.919210	536.045355	12.390592
12.979230	528.951402	12.395610
13.140337	533.309624	12.400627
12.939361	530.466341	12.405645
12.977570	535.301404	12.410663
12.782874	527.262764	12.415680
12.977459	546.189023	12.420698
13.196611	548.313346	12.425715
13.308565	559.637724	12.430733
13.050583	533.154123	12.435751
13.261026	550.455843	12.440768
13.244012	537.157114	12.445786
13.078608	534.983588	12.450803
13.283829	539.041415	12.455821
13.533509	527.061038	12.460839
12.991880	536.152546	12.465856
12.846847	542.004073	12.470874
13.174069	540.119430	12.475891
13.187872	546.069146	12.480909
13.396938	544.357648	12.485927
13.375649	542.275149	12.490944
12.909271	541.505755	12.495962
13.404503	544.104365	12.500979
13.362749	558.835797	12.505997
13.571092	546.726186	12.511015
13.324347	543.653390	12.516032
13.263022	540.545232	12.521050
13.398730	538.722153	12.526067
13.178345	536.708719	12.531085
13.008016	532.648823	12.536103
13.136803	551.175149	12.541120
13.227255	555.670677	12.546138
13.577577	550.270054	12.551155
13.471871	557.390350	12.556173
13.767607	557.656556	12.561191
13.469907	558.751032	12.566208
13.688392	559.114547	12.571226
13.566102	559.067557	12.576243
13.288927	552.509258	12.581261
13.663836	548.941435	12.586279
13.450489	548.539488	12.591296
13.157592	548.137383	12.596314
13.613364	544.717835	12.601331
13.179197	550.377984	12.606349
13.323989	552.154201	12.611367
13.573866	558.025908	12.616384
13.639602	561.802641	12.621402
13.393608	556.160937	12.626419
13.383688	565.806615	12.631437
13.519799	555.065293	12.636455
13.164381	558.488297	12.641472
13.391038	557.020190	12.646490
13.759403	559.285235	12.651507
13.657388	567.238077	12.656525
13.940478	553.636699	12.661543
13.664882	563.447076	12.666560
13.629534	561.205834	12.671578
14.064201	553.901695	12.676595
13.524265	562.592169	12.681613
13.714762	555.443049	12.686631
13.523229	548.546290	12.691648
13.600526	563.451574	12.696666
14.004137	554.022162	12.701683
13.735556	558.018531	12.706701
13.613960	555.942279	12.711719
13.536418	563.181239	12.716736
13.763338	567.803710	12.721754
13.841411	573.475125	12.726771
13.760694	584.930691	12.731789
14.035189	573.688000	12.736807
14.205341	577.243252	12.741824
14.156188	577.856981	12.746842
13.704336	559.129027	12.751859
13.982686	562.689414	12.756877
14.306783	565.993329	12.761895
13.886884	553.145870	12.766912
13.722563	555.847821	12.771930
14.071285	553.650544	12.776947
13.984158	554.342804	12.781965
13.615697	545.753878	12.786983
13.816097	553.050270	12.792000
14.040951	569.702821	12.797018
14.154079	562.247089	12.802035
13.990060	580.456409	12.807053
14.240831	571.631595	12.812071
14.350666	573.536366	12.817088
14.267903	573.183386	12.822106
14.167273	555.422873	12.827123
13.985515	555.331553	12.832141
14.119733	554.247154	12.837159
14.054784	550.918659	12.842176
14.299444	570.108493	12.847194
14.273407	568.238171	12.852211
14.041871	564.730649	12.857229
13.812199	560.484388	12.862247
14.053548	567.193711	12.867264
13.716845	575.438944	12.872282
14.297761	571.321295	12.877299
14.123477	577.196350	12.882317
14.004925	578.101816	12.887335
13.932731	575.071093	12.892352
14.100937	576.436550	12.897370
14.452462	561.164512	12.902387
14.176600	573.108231	12.907405
14.575957	563.117755	12.912423
14.293111	560.643896	12.917440
14.032487	570.600252	12.922458
14.158169	561.299588	12.927475
14.519344	579.546539	12.932493
14.650399	581.694136	12.937511
14.647440	572.189562	12.942528
14.293254	574.744541	12.947546
14.297912	571.667064	12.952563
14.375782	572.197775	12.957581
14.386878	570.435242	12.962599
14.515994	571.765800	12.967616
14.767635	578.489293	12.972634
14.575706	571.740907	12.977651
14.343692	567.801120	12.982669
14.509321	568.346483	12.987687
14.467959	585.817077	12.992704
14.507721	581.784213	12.997722
14.763246	571.241920	13.002739
14.830702	569.338015	13.007757
14.829510	567.397529	13.012775
14.617298	568.137790	13.017792
14.545775	567.284438	13.022810
14.818383	562.486116	13.027827
14.505733	560.076885	13.032845
14.582476	563.820337	13.037863
14.911760	569.130504	13.042880
14.297052	563.350910	13.047898
14.717322	560.299834	13.052915
14.651424	577.329302	13.057933
14.756722	578.597320	13.062951
14.951262	576.275877	13.067968
14.723121	583.797214	13.072986
14.837451	590.690547	13.078003
14.827597	589.641342	13.083021
14.497761	582.548490	13.088039
14.877898	588.377708	13.093056
14.917055	599.000314	13.098074
14.957866	598.634283	13.103091
14.770538	595.274461	13.108109
14.751816	591.474818	13.113127
14.811758	597.234287	13.118144
14.614095	599.606957	13.123162
15.094288	590.462169	13.128179
15.067413	588.775011	13.133197
15.114367	596.502557	13.138215
15.228491	597.298985	13.143232
15.138340	604.571495	13.148250
15.160244	586.211092	13.153267
14.970436	580.983449	13.158285
14.955840	567.542309	13.163303
14.907738	583.552839	13.168320
14.995002	590.156926	13.173338
15.177256	588.291836	13.178355
15.353373	584.294411	13.183373
14.885323	576.617311	13.188391
14.893387	570.569728	13.193408
14.804771	585.655658	13.198426
15.066884	591.604353	13.203443
14.885086	593.617935	13.208461
14.835488	590.103992	13.213479
14.995114	585.263406	13.218496
15.193645	598.862173	13.223514
15.331893	598.364113	13.228531
15.323542	596.762413	13.233549
14.852788	603.027906	13.238567
15.209084	592.087964	13.243584
14.785653	601.347176	13.248602
15.035458	595.735073	13.253619
15.305495	593.944590	13.258637
15.106823	600.681843	13.263655
15.322243	610.702489	13.268672
15.362621	622.833375	13.273690
15.719231	616.175751	13.278707
15.497182	608.841941	13.283725
15.348230	599.584286	13.288743
15.606508	593.355482	13.293760
15.124810	605.501884	13.298778
14.893074	597.270203	13.303795
15.492417	611.367907	13.308813
15.628276	617.566764	13.313831
15.377534	611.704882	13.318848
15.521716	623.668028	13.323866
15.724944	616.990254	13.328883
15.774666	623.130026	13.333901
15.351905	616.534553	13.338919
15.649095	611.230598	13.343936
15.679634	620.204100	13.348954
15.502986	602.313441	13.353971
15.303039	609.145570	13.358989
15.322682	612.380432	13.364007
15.473145	612.953419	13.369024
15.484443	625.622188	13.374042
15.545827	620.923216	13.379059
15.919616	618.217080	13.384077
15.759037	624.528656	13.389095
15.816075	618.066289	13.394112
15.536688	622.007561	13.399130
15.525015	622.249349	13.404147
15.473829	624.580138	13.409165
15.309964	625.726232	13.414183
15.854678	622.848150	13.419200
15.494808	617.773372	13.424218
15.591030	620.974147	13.429235
15.553839	620.711854	13.434253
15.373194	614.870546	13.439271
15.897068	629.235706	13.444288
16.368720	636.751563	13.449306
15.978895	624.890253	13.454323
15.863396	620.648179	13.459341
15.655251	619.652131	13.464359
15.832300	623.076925	13.469376
15.978335	637.308789	13.474394
16.100759	630.684696	13.479411
16.041192	626.086723	13.484429
15.370706	622.376568	13.489447
16.012301	627.306463	13.494464
15.759661	631.429737	13.499482
16.176348	640.140778	13.504499
16.197318	634.103774	13.509517
15.983230	644.033945	13.514535
16.205156	644.245445	13.519552
16.056273	646.692528	13.524570
16.340353	642.002839	13.529587
16.413810	633.006963	13.534605
15.870647	625.837066	13.539623
16.255536	629.103067	13.544640
16.222142	632.557679	13.549658
16.181104	629.209644	13.554675
16.191323	632.830991	13.559693
16.363497	642.271457	13.564711
16.237982	621.671424	13.569728
15.916610	622.296248	13.574746
16.196851	629.125731	13.579763
16.341798	644.787337	13.584781
16.268393	633.185711	13.589799
16.356407	634.024100	13.594816
16.146879	634.407341	13.599834
16.253058	646.187110	13.604851
16.222215	640.590563	13.609869
16.503444	641.707946	13.614887
16.522412	638.823873	13.619904
16.421562	646.151725	13.624922
16.221802	632.439749	13.629939
16.473046	622.674416	13.634957
16.398694	625.772530	13.639975
16.573199	623.400572	13.644992
16.506485	634.377454	13.650010
16.407209	633.755663	13.655027
16.682228	637.477532	13.660045
16.514368	638.823067	13.665063
16.522587	643.031703	13.670080
16.380471	644.748742	13.675098
16.554935	643.314052	13.680115
16.614242	634.979949	13.685133
16.766751	637.332472	13.690151
16.607620	635.839599	13.695168
16.419072	637.478706	13.700186
16.656191	635.690221	13.705203
16.655993	636.990552	13.710221
16.546635	646.393080	13.715239
16.709463	629.282330	13.720256
16.732091	638.178186	13.725274
16.481664	644.702660	13.730291
16.621271	642.339322	13.735309
16.454634	641.346237	13.740327
16.668772	641.874534	13.745344
16.507497	635.600999	13.750362
16.751270	634.161763	13.755379
16.666089	624.982465	13.760397
16.095165	642.176328	13.765415
16.601981	644.457560	13.770432
17.006280	661.192534	13.775450
16.793349	654.936553	13.780467
17.102106	658.302848	13.785485
16.706794	659.226434	13.790503
16.721109	654.336013	13.795520
16.798735	658.663165	13.800538
16.741864	656.037123	13.805555
17.158413	661.078027	13.810573
16.726789	658.864147	13.815591
17.386587	653.755829	13.820608
17.119666	653.889289	13.825626
16.968743	663.298338	13.830643
17.272611	657.128641	13.835661
17.056260	653.549295	13.840679
17.186572	657.612574	13.845696
17.320675	668.501209	13.850714
16.673897	657.914046	13.855731
17.174022	658.321797	13.860749
17.058384	666.305220	13.865767
17.258503	664.247977	13.870784
17.322985	661.678659	13.875802
16.913784	663.488038	13.880819
17.389806	660.882642	13.885837
17.241048	660.836643	13.890855
17.461684	658.296508	13.895872
17.140975	659.937389	13.900890
17.044218	657.263948	13.905907
17.732708	662.214908	13.910925
17.068286	659.169664	13.915943
17.536126	660.762735	13.920960
17.150527	660.933723	13.925978
16.979480	654.352446	13.930995
17.456791	655.464354	13.936013
17.037740	664.063355	13.941031
17.647806	656.939974	13.946048
17.458857	669.731667	13.951066
17.824510	660.895121	13.956083
17.694584	661.707699	13.961101
17.370132	656.002517	13.966119
17.486825	650.597444	13.971136
17.403042	655.375914	13.976154
17.229493	659.881275	13.981171
17.704601	663.054252	13.986189
17.213131	655.358696	13.991207
17.454552	657.025111	13.996224
17.378897	662.941545	14.001242
16.970745	664.574037	14.006259
17.954900	665.306735	14.011277
17.481244	658.476226	14.016295
17.555524	665.868164	14.021312
18.060908	668.140157	14.026330
17.724008	664.494491	14.031347
17.982009	655.624322	14.036365
17.906421	661.619640	14.041383
17.617840	652.358589	14.046400
17.384992	645.490355	14.051418
17.648866	659.874186	14.056435
18.053848	670.553125	14.061453
17.732975	674.229512	14.066471
17.359421	670.264542	14.071488
17.620458	669.191824	14.076506
17.833442	679.074036	14.081523
18.106192	681.256248	14.086541
18.233101	681.457390	14.091559
18.054307	683.325345	14.096576
18.051698	686.140832	14.101594
17.743287	681.644949	14.106611
17.702823	672.988792	14.111629
17.837675	679.071064	14.116647
18.235843	686.838294	14.121664
18.354416	683.862869	14.126682
18.082680	681.674428	14.131699
18.130733	683.150238	14.136717
18.039485	680.769417	14.141735
18.216835	670.576982	14.146752
18.252612	677.930777	14.151770
17.951807	669.214426	14.156787
18.367196	671.992822	14.161805
18.107716	674.103790	14.166823
18.117603	674.228593	14.171840
17.999579	677.273599	14.176858
17.994481	678.555766	14.181875
18.455148	680.948375	14.186893
18.116260	686.612573	14.191911
17.812553	684.766809	14.196928
17.879231	683.674050	14.201946
18.104136	683.266551	14.206963
18.447116	673.145993	14.211981
18.196983	683.346919	14.216999
18.190785	676.692468	14.222016
18.281757	670.868545	14.227034
18.196531	689.630515	14.232051
18.478111	680.769263	14.237069
18.195466	679.589226	14.242087
18.222975	677.334965	14.247104
18.256665	683.316324	14.252122
17.829935	689.448719	14.257139
18.527968	687.588013	14.262157
19.000409	701.115540	14.267175
18.707902	703.225374	14.272192
18.760541	698.518284	14.277210
18.252758	687.483295	14.282227
18.549851	691.772913	14.287245
18.496781	705.660490	14.292263
18.434830	694.943804	14.297280
18.670642	704.203920	14.302298
18.736332	701.779573	14.307315
18.953923	693.379618	14.312333
18.854356	699.205137	14.317351
18.654270	702.575428	14.322368
18.553614	695.853720	14.327386
18.745492	705.265886	14.332403
18.774208	693.342109	14.337421
18.864912	704.168138	14.342439
18.746756	692.538771	14.347456
18.865420	699.838563	14.352474
18.886753	697.238131	14.357491
18.801873	692.899725	14.362509
18.936511	710.188232	14.367527
18.970701	705.458784	14.372544
18.761101	696.374683	14.377562
18.579844	702.743174	14.382579
18.572266	703.542896	14.387597
18.772244	707.961343	14.392615
18.455397	696.858562	14.397632
18.623055	700.076561	14.402650
18.676359	701.721962	14.407667
18.993423	703.098820	14.412685
19.094309	710.849524	14.417703
18.955686	717.315482	14.422720
18.990369	718.641911	14.427738
19.137199	735.878040	14.432755
19.349774	728.226777	14.437773
19.247651	720.811015	14.442791
18.931727	706.047370	14.447808
19.575372	712.131986	14.452826
18.780992	711.499181	14.457843
19.105640	706.033107	14.462861
19.491052	720.218065	14.467879
19.483062	723.763389	14.472896
19.527429	696.436914	14.477914
19.238992	687.737551	14.482931
18.959205	693.430361	14.487949
19.390601	691.516758	14.492967
19.386863	695.414857	14.497984
19.112112	691.996131	14.503002
19.178793	714.587539	14.508019
19.562971	704.990681	14.513037
19.573618	712.345272	14.518055
19.525638	708.900479	14.523072
19.344016	695.403362	14.528090
19.644343	703.365809	14.533107
19.246431	691.553058	14.538125
19.791223	702.945409	14.543143
19.483518	702.476192	14.548160
19.489865	698.262346	14.553178
19.386447	705.066764	14.558195
19.819648	710.748854	14.563213
19.624395	711.066743	14.568231
19.568424	708.345879	14.573248
19.642275	698.882851	14.578266
19.731966	700.532018	14.583283
19.678579	696.911351	14.588301
19.454565	701.396227	14.593319
19.462085	718.313341	14.598336
19.570682	711.707163	14.603354
20.035210	716.522817	14.608371
19.924530	721.311831	14.613389
19.979938	718.535644	14.618407
19.904136	715.353984	14.623424
19.573114	709.122798	14.628442
19.555089	713.742659	14.633459
19.888531	709.578546	14.638477
19.886149	718.661396	14.643495
19.939308	717.930513	14.648512
20.153066	705.141452	14.653530
19.843024	712.865023	14.658547
19.974573	712.857156	14.663565
20.119803	720.383167	14.668583
20.034738	715.344199	14.673600
20.192145	708.654636	14.678618
20.016070	711.484682	14.683635
20.321494	710.322957	14.688653
20.246828	708.816843	14.693671
19.923851	713.598092	14.698688
19.883198	704.250832	14.703706
19.648558	708.753153	14.708723
19.706513	707.178924	14.713741
20.229602	706.383880	14.718759
19.913033	713.183828	14.723776
20.486380	711.863361	14.728794
19.892383	714.140353	14.733811
19.756340	719.608679	14.738829
19.892917	714.774825	14.743847
19.773488	719.666194	14.748864
20.384247	728.141745	14.753882
20.424645	736.820272	14.758899
20.425297	735.886177	14.763917
20.625413	734.374878	14.768935
20.212879	739.955957	14.773952
20.357197	726.256270	14.778970
20.397741	735.603801	14.783987
20.418244	735.089471	14.789005
20.305820	739.525315	14.794023
20.236395	734.578565	14.799040
20.553271	740.714389	14.804058
20.140488	740.391022	14.809075
20.459986	727.834686	14.814093
20.800547	731.098183	14.819111
20.429157	731.222765	14.824128
20.662354	718.291794	14.829146
20.509165	726.571460	14.834163
20.429367	727.859023	14.839181
20.811775	735.357346	14.844199
20.237132	731.259767	14.849216
20.540112	723.143064	14.854234
20.385188	731.050621	14.859251
20.527648	729.390566	14.864269
20.512459	731.646301	14.869287
20.987558	752.778908	14.874304
21.259050	739.557900	14.879322
20.920335	734.621785	14.884339
20.605039	731.190469	14.889357
20.722221	732.279912	14.894375
20.290210	735.838025	14.899392
21.117261	734.307393	14.904410
20.902633	750.003339	14.909427
20.876177	747.902691	14.914445
21.342574	743.862905	14.919463
21.012125	744.697437	14.924480
21.237682	732.108479	14.929498
21.118310	730.697730	14.934515
20.932264	728.925045	14.939533
21.027101	729.566711	14.944551
20.934592	734.400218	14.949568
21.021191	721.104052	14.954586
20.976326	749.525945	14.959603
21.150769	748.034446	14.964621
21.492686	738.983831	14.969639
21.362994	733.667829	14.974656
21.095430	729.209715	14.979674
20.762412	732.727071	14.984691
21.269645	747.858636	14.989709
21.226560	750.311247	14.994727
21.123754	755.676547	14.999744
21.471012	748.963534	15.004762
21.154117	756.195894	15.009779
21.541042	749.861673	15.014797
21.234146	752.570212	15.019815
21.294791	756.609716	15.024832
21.337193	748.047835	15.029850
21.672900	748.642296	15.034867
21.622542	752.942186	15.039885
21.353681	743.179382	15.044903
21.475720	749.815950	15.049920
21.574162	740.686717	15.054938
21.545358	749.792658	15.059955
21.310149	751.265517	15.064973
21.475413	744.334869	15.069991
21.398125	744.230335	15.075008
21.423910	746.173540	15.080026
21.845078	752.987303	15.085043
21.507631	759.493895	15.090061
21.672477	757.454791	15.095079
21.643061	754.657175	15.100096
21.534822	747.838805	15.105114
21.523297	751.624528	15.110131
21.618711	756.769424	15.115149
21.475041	754.011800	15.120167
21.195309	763.109725	15.125184
21.836861	756.107604	15.130202
21.857705	770.387592	15.135219
21.648508	775.005864	15.140237
22.109380	771.348790	15.145255
22.164541	778.885781	15.150272
22.274416	774.636761	15.155290
21.842615	759.948031	15.160307
21.968004	773.864504	15.165325
22.164921	765.735997	15.170343
21.756649	759.371729	15.175360
21.953211	759.315807	15.180378
22.162016	774.576203	15.185395
22.017938	777.009928	15.190413
22.215010	783.404378	15.195431
22.031706	781.161044	15.200448
22.240326	770.755370	15.205466
22.186192	770.334784	15.210483
22.119650	764.743791	15.215501
22.312877	766.449326	15.220519
22.157273	774.754639	15.225536
22.252531	771.779696	15.230554
22.653480	766.320584	15.235571
21.867092	766.327151	15.240589
22.331148	766.548053	15.245607
22.357040	768.595385	15.250624
22.267863	769.218547	15.255642
22.248311	770.064330	15.260659
22.307695	766.274502	15.265677
22.465412	763.236126	15.270695
22.293612	769.890337	15.275712
22.475700	770.824447	15.280730
22.604373	763.555543	15.285747
22.416642	774.112816	15.290765
22.384393	765.351185	15.295783
22.522888	761.593145	15.300800
22.442757	773.468460	15.305818
22.112977	763.784617	15.310835
21.904251	766.925901	15.315853
22.485100	760.536046	15.320871
22.417773	761.531324	15.325888
22.546173	773.481264	15.330906
22.503030	782.131877	15.335923
22.540944	793.004101	15.340941
22.876364	784.787613	15.345959
22.701667	801.184247	15.350976
22.997973	789.988495	15.355994
23.050128	791.053417	15.361011
23.041021	794.270726	15.366029
23.034783	781.399315	15.371047
22.551139	772.430694	15.376064
23.064456	781.486426	15.381082
22.935658	784.410062	15.386099
22.743637	790.209072	15.391117
23.474824	780.769242	15.396135
22.853836	772.450145	15.401152
22.538567	776.428630	15.406170
22.915388	777.180751	15.411187
22.555110	792.423029	15.416205
22.725664	783.664328	15.421223
22.990589	781.341298	15.426240
22.914711	786.632960	15.431258
22.842629	785.186395	15.436275
22.905550	787.126942	15.441293
22.881188	779.345523	15.446311
23.296408	797.849318	15.451328
23.387560	798.712470	15.456346
23.429594	791.741151	15.461363
23.187690	792.299880	15.466381
23.357368	780.814706	15.471399
23.511463	788.541328	15.476416
23.191109	778.142789	15.481434
23.520103	772.963192	15.486451
23.277039	782.137432	15.491469
23.536650	776.571074	15.496487
23.777810	789.020909	15.501504
23.457221	789.014455	15.506522
23.767877	781.562396	15.511539
23.432020	781.144925	15.516557
23.733109	777.033203	15.521575
23.335309	783.120071	15.526592
23.376530	782.362653	15.531610
24.059725	788.343270	15.536627
23.498647	787.295212	15.541645
23.931136	784.816540	15.546663
23.764050	782.788414	15.551680
23.338430	786.036267	15.556698
23.587670	784.457306	15.561715
23.432870	783.361372	15.566733
23.911434	786.909371	15.571751
23.700937	781.422979	15.576768
23.886654	782.359676	15.581786
23.741009	777.891915	15.586803
23.701179	787.173171	15.591821
23.674466	789.212968	15.596839
23.940095	783.778208	15.601856
23.453766	780.174865	15.606874
23.896893	795.155569	15.611891
23.985987	814.969644	15.616909
24.168688	813.934437	15.621927
23.888944	811.845064	15.626944
24.345590	809.927493	15.631962
24.387648	796.186969	15.636979
23.963751	789.048812	15.641997
24.001784	780.582274	15.647015
23.695676	785.335653	15.652032
24.222574	791.990854	15.657050
24.281856	794.383252	15.662067
24.358744	806.382311	15.667085
23.940556	796.043271	15.672103
24.030152	805.569346	15.677120
23.989125	806.465832	15.682138
24.616659	802.227218	15.687155
24.361299	803.763199	15.692173
24.353378	800.447812	15.697191
24.112299	799.674663	15.702208
24.189393	801.123842	15.707226
24.656325	789.200769	15.712243
24.480296	796.092338	15.717261
24.580289	792.188845	15.722279
24.695422	806.558230	15.727296
24.630778	810.936112	15.732314
24.622991	798.708715	15.737331
24.521067	803.480600	15.742349
24.713262	801.812747	15.747367
24.419753	799.933815	15.752384
24.392713	807.856082	15.757402
24.420832	798.087743	15.762419
24.315344	813.937058	15.767437
24.284477	804.010700	15.772455
24.354001	804.593219	15.777472
24.223126	798.971270	15.782490
24.472483	797.802545	15.787507
24.799283	809.926552	15.792525
24.849821	817.533712	15.797543
25.055236	830.939074	15.802560
24.995715	808.529675	15.807578
25.000265	792.330348	15.812595
24.687307	801.922648	15.817613
25.011640	809.057718	15.822631
24.901366	798.301204	15.827648
24.676279	803.534199	15.832666
25.203965	807.017700	15.837683
24.924256	819.154690	15.842701
25.204555	819.704186	15.847719
25.025379	809.838930	15.852736
24.511931	815.543142	15.857754
25.035775	806.435587	15.862771
24.830408	819.286764	15.867789
24.990818	824.311042	15.872807
24.958661	822.406938	15.877824
24.646299	820.884408	15.882842
25.055397	817.598354	15.887859
24.892850	822.496507	15.892877
24.621982	819.619947	15.897895
25.184183	838.697203	15.902912
25.468412	852.090233	15.907930
25.502190	833.778207	15.912947
25.319750	843.034499	15.917965
25.642604	838.723692	15.922983
25.632673	839.959291	15.928000
25.638170	843.956962	15.933018
25.557743	835.505802	15.938035
25.247094	836.211004	15.943053
25.741434	837.560098	15.948071
25.979649	833.066894	15.953088
26.037807	815.618914	15.958106
25.390171	810.851099	15.963123
25.579120	817.811724	15.968141
25.398306	809.833897	15.973159
25.563318	810.565557	15.978176
25.519151	826.597780	15.983194
25.671274	825.680973	15.988211
25.638399	833.642036	15.993229
25.506240	839.551603	15.998247
25.928392	833.530571	16.003264
25.683188	835.241688	16.008282
25.759445	833.563595	16.013299
25.469312	830.478611	16.018317
25.563286	830.075844	16.023335
25.784592	836.883084	16.028352
25.774495	836.638634	16.033370
25.917273	825.921351	16.038387
25.963698	832.257372	16.043405
26.031403	827.835065	16.048423
25.828421	830.151794	16.053440
25.920937	840.349617	16.058458
26.263641	847.989909	16.063475
26.024903	854.588368	16.068493
26.190662	849.664698	16.073511
26.375921	855.682328	16.078528
26.239998	859.834704	16.083546
26.497903	845.094646	16.088563
26.220187	837.876760	16.093581
26.095045	836.791955	16.098599
26.831458	841.896405	16.103616
25.983359	835.313842	16.108634
26.240129	830.846134	16.113651
26.359780	838.104803	16.118669
26.351812	836.802823	16.123687
26.626118	844.113003	16.128704
26.608308	855.025554	16.133722
26.425850	841.477963	16.138739
26.778648	850.274857	16.143757
26.104627	843.848054	16.148775
26.739100	846.020950	16.153792
26.367474	850.330174	16.158810
27.019710	842.376447	16.163827
26.480730	848.763168	16.168845
26.791279	847.297674	16.173863
26.741336	851.190423	16.178880
26.397946	855.798183	16.183898
26.572816	845.031679	16.188915
26.758217	844.365278	16.193933
26.769098	850.078868	16.198951
26.753940	843.094398	16.203968
26.883292	850.159048	16.208986
26.864520	853.497803	16.214003
26.583191	853.396835	16.219021
26.702210	848.471021	16.224039
26.674724	847.468745	16.229056
26.417079	854.423616	16.234074
26.646102	843.345671	16.239091
26.813037	838.951996	16.244109
26.924905	858.787798	16.249127
27.170535	862.198738	16.254144
27.102692	865.608300	16.259162
27.496415	860.109266	16.264179
27.398190	852.143727	16.269197
27.287018	857.160073	16.274215
27.301286	845.856997	16.279232
26.906654	845.379304	16.284250
26.908583	839.436733	16.289267
26.683748	848.854305	16.294285
26.696097	868.279675	16.299303
26.911105	874.134860	16.304320
27.263228	865.928341	16.309338
27.297304	861.321946	16.314355
27.423798	860.869902	16.319373
27.388848	867.218685	16.324391
27.269705	864.700198	16.329408
27.637590	876.514856	16.334426
27.586414	876.576644	16.339443
27.660233	873.160074	16.344461
27.580732	860.830261	16.349479
27.924641	863.610419	16.354496
27.874228	876.020791	16.359514
27.781124	868.805527	16.364531
27.740789	863.620653	16.369549
27.554091	863.246081	16.374567
27.649083	860.381619	16.379584
27.577319	870.141294	16.384602
27.585877	865.879724	16.389619
27.679442	872.915276	16.394637
27.867529	892.808602	16.399655
27.681743	889.435859	16.404672
27.842617	890.868762	16.409690
28.143122	895.729099	16.414707
28.138197	890.582851	16.419725
27.991249	894.478186	16.424743
28.295589	874.593154	16.429760
28.128508	888.874279	16.434778
28.168353	883.294983	16.439795
28.018967	871.149682	16.444813
28.216624	870.197336	16.449831
28.261544	868.233814	16.454848
28.122423	869.281372	16.459866
28.339110	875.514992	16.464883
28.190069	882.850492	16.469901
28.293006	873.060921	16.474919
28.209521	872.326194	16.479936
28.343247	879.393326	16.484954
28.349129	878.458404	16.489971
28.431708	889.323689	16.494989
28.578701	884.585987	16.500007
28.431141	874.977675	16.505024
28.437394	882.796930	16.510042
28.449891	878.982866	16.515059
28.572543	882.267910	16.520077
28.396662	873.276265	16.525095
28.745390	882.004385	16.530112
28.817393	876.991255	16.535130
28.246145	868.616981	16.540147
28.429499	870.658589	16.545165
28.437070	876.909194	16.550183
28.690515	884.755992	16.555200
28.433626	890.088669	16.560218
28.758445	884.631982	16.565235
28.719969	885.865744	16.570253
28.621737	887.626423	16.575271
28.774326	881.300469	16.580288
29.087639	880.715012	16.585306
28.801464	876.427034	16.590323
28.794689	874.553662	16.595341
28.916273	880.294098	16.600359
29.196145	877.227097	16.605376
29.018867	878.072350	16.610394
29.155946	891.242311	16.615411
29.331258	882.691100	16.620429
29.018106	889.029830	16.625447
29.335144	886.225249	16.630464
28.977648	878.164620	16.635482
28.978661	875.015078	16.640499
29.131648	874.189652	16.645517
28.934251	886.032923	16.650535
28.863088	881.995280	16.655552
29.111202	887.485519	16.660570
29.126033	883.699491	16.665587
29.216888	887.402930	16.670605
29.071182	902.046791	16.675623
29.383266	896.450083	16.680640
29.384075	904.380654	16.685658
29.153956	904.511504	16.690675
29.051421	891.932813	16.695693
29.320150	898.666374	16.700711
29.205632	899.489172	16.705728
29.224305	900.824435	16.710746
29.744636	900.582085	16.715763
29.479659	898.395713	16.720781
29.747247	915.202839	16.725799
29.940453	913.443298	16.730816
30.010146	899.284952	16.735834
29.756957	900.735394	16.740851
29.693184	889.280415	16.745869
29.396733	905.008252	16.750887
29.754573	905.652899	16.755904
29.927770	920.328862	16.760922
29.988813	918.880363	16.765939
30.001360	925.745591	16.770957
29.964076	929.611128	16.775975
30.084853	917.013210	16.780992
30.196506	920.101168	16.786010
30.054020	922.967011	16.791027
30.116159	911.751067	16.796045
30.382299	919.397075	16.801063
30.062348	912.223646	16.806080
29.917760	901.898482	16.811098
30.177645	913.622788	16.816115
30.467000	918.058842	16.821133
30.008031	914.236587	16.826151
30.384831	915.380041	16.831168
30.382590	922.474804	16.836186
30.453689	922.791991	16.841203
30.364707	924.191461	16.846221
30.132438	928.087547	16.851239
30.337182	926.622844	16.856256
30.634173	925.392999	16.861274
30.518030	927.008164	16.866291
30.501252	920.061789	16.871309
30.004596	923.955116	16.876327
30.763309	920.664760	16.881344
30.265314	920.405233	16.886362
30.540730	923.265560	16.891379
30.580033	915.676079	16.896397
30.595750	923.137261	16.901415
30.632488	920.676394	16.906432
30.729402	920.162711	16.911450
30.719927	918.352874	16.916467
30.696991	920.414185	16.921485
30.199014	921.931384	16.926503
30.688427	922.274549	16.931520
31.036790	931.207879	16.936538
30.799090	920.458633	16.941555
31.224983	917.330877	16.946573
30.717335	929.756120	16.951591
30.634103	928.087227	16.956608
31.013412	931.792819	16.961626
31.385924	945.358281	16.966643
31.696251	944.031670	16.971661
31.127805	926.514498	16.976679
30.809940	930.319853	16.981696
31.367015	935.995231	16.986714
31.069473	942.375716	16.991731
31.452444	936.944616	16.996749
31.197066	945.650651	17.001767
31.335796	938.872409	17.006784
31.515391	944.490167	17.011802
31.382371	949.124951	17.016819
31.912086	935.140656	17.021837
31.166827	924.205841	17.026855
31.345439	932.323163	17.031872
31.698954	942.265555	17.036890
31.102966	941.626902	17.041907
31.602886	934.728955	17.046925
31.182800	928.688371	17.051943
31.502101	929.048722	17.056960
31.469936	929.505165	17.061978
31.237824	930.949151	17.066995
31.877935	931.805196	17.072013
31.401591	941.167548	17.077031
31.519263	927.203636	17.082048
31.342255	934.653992	17.087066
31.573095	939.055038	17.092083
32.088579	947.880141	17.097101
31.889126	946.219987	17.102119
31.871154	944.010689	17.107136
31.876010	941.924046	17.112154
32.015970	947.948806	17.117171
32.067195	939.887228	17.122189
32.239992	946.935641	17.127207
32.130875	953.280296	17.132224
32.277712	940.002931	17.137242
32.038884	947.513472	17.142259
32.325289	940.459625	17.147277
32.057739	948.429106	17.152295
32.014663	942.534577	17.157312
32.075759	943.437160	17.162330
32.083254	947.813240	17.167347
32.351107	939.657761	17.172365
32.237127	946.337693	17.177383
32.063774	947.223359	17.182400
32.301300	948.820985	17.187418
32.150930	962.540968	17.192435
32.733749	964.759843	17.197453
32.546563	964.924993	17.202471
32.722135	967.384401	17.207488
32.718339	965.314891	17.212506
32.752055	956.628038	17.217523
32.617563	944.142680	17.222541
32.626340	952.570644	17.227559
32.547357	951.257692	17.232576
32.994878	951.623201	17.237594
32.711891	966.345428	17.242611
33.117199	968.753063	17.247629
33.035454	954.075598	17.252647
32.588194	940.907093	17.257664
32.864038	944.307003	17.262682
32.966735	955.598370	17.267699
33.073347	955.326165	17.272717
33.366694	953.601423	17.277735
32.864902	950.249777	17.282752
33.255250	933.273503	17.287770
32.983111	939.959277	17.292787
33.142422	942.926162	17.297805
33.399967	944.719468	17.302823
33.311211	938.835253	17.307840
33.036328	933.292629	17.312858
32.642479	944.245217	17.317875
33.412955	943.490300	17.322893
33.079731	961.038549	17.327911
33.349761	954.722571	17.332928
33.183273	962.366952	17.337946
33.257359	966.530630	17.342963
33.383439	959.445091	17.347981
33.422546	959.612655	17.352999
33.417650	962.624206	17.358016
33.341119	962.383852	17.363034
33.411114	966.724898	17.368051
33.175584	965.824639	17.373069
33.820775	975.314249	17.378087
33.457016	983.816375	17.383104
33.631880	984.174111	17.388122
33.616172	985.331729	17.393139
33.802259	979.249803	17.398157
33.887719	983.717819	17.403175
33.745128	971.527203	17.408192
34.177307	968.540466	17.413210
33.796450	971.112302	17.418227
33.946585	970.022229	17.423245
34.102801	976.514670	17.428263
33.949666	983.383788	17.433280
33.887804	980.376624	17.438298
34.046329	975.633935	17.443315
33.942762	971.516141	17.448333
33.983338	971.626671	17.453351
34.059092	971.602300	17.458368
34.056098	967.607605	17.463386
33.743808	986.080413	17.468403
34.116690	993.154302	17.473421
34.516728	1000.773054	17.478439
34.383323	1003.397643	17.483456
34.783370	991.361838	17.488474
34.225730	987.857988	17.493491
34.611570	980.971584	17.498509
34.519295	985.751474	17.503527
34.903258	990.409411	17.508544
34.743923	973.819026	17.513562
34.463198	969.820508	17.518579
34.647904	961.059503	17.523597
34.762625	966.554887	17.528615
34.450351	964.502151	17.533632
34.758322	975.259590	17.538650
34.510292	991.352305	17.543667
35.141148	984.591616	17.548685
35.091543	980.121379	17.553703
34.825517	970.733549	17.558720
34.663215	966.801685	17.563738
34.678118	978.772702	17.568755
35.102656	990.752131	17.573773
35.439082	987.717277	17.578791
35.151983	981.734734	17.583808
34.641483	962.706269	17.588826
34.682956	979.485768	17.593843
35.089840	971.172790	17.598861
34.876859	985.249742	17.603879
34.998753	979.708054	17.608896
35.190185	983.215873	17.613914
35.072969	996.151196	17.618931
35.394515	987.551777	17.623949
35.274488	983.054703	17.628967
34.949235	987.217837	17.633984
35.185873	979.284983	17.639002
35.230398	990.386668	17.644019
35.504811	1001.670095	17.649037
35.789567	988.853928	17.654055
35.261799	997.741523	17.659072
35.328309	999.558454	17.664090
35.156928	1012.609574	17.669107
35.716785	1005.168872	17.674125
35.979998	999.261050	17.679143
35.771500	1005.760151	17.684160
36.032004	991.609706	17.689178
35.849907	1000.799753	17.694195
35.545461	999.096084	17.699213
35.613958	989.681078	17.704231
35.655956	998.047055	17.709248
35.621771	1000.195345	17.714266
35.563733	999.570236	17.719283
35.766179	997.913382	17.724301
36.008550	1004.234543	17.729319
36.109624	1021.872599	17.734336
36.303805	1020.845050	17.739354
36.205441	1025.313475	17.744371
36.252881	1019.701388	17.749389
36.510801	1006.239310	17.754407
36.030585	1002.726481	17.759424
36.533562	1011.616692	17.764442
36.430720	1008.928372	17.769459
36.228391	1004.579888	17.774477
36.485421	996.527065	17.779495
36.499479	997.702111	17.784512
36.444297	999.582290	17.789530
36.695088	1006.141976	17.794547
36.037435	1006.289318	17.799565
36.668847	1012.300216	17.804583
36.401058	1025.003529	17.809600
36.736197	1016.436681	17.814618
36.655511	1020.766634	17.819635
36.637496	1013.839351	17.824653
36.900897	1004.144489	17.829671
36.741920	1014.369192	17.834688
36.984058	1012.835507	17.839706
36.805140	1018.547330	17.844723
36.726115	1015.927861	17.849741
37.001064	1017.712135	17.854759
36.964657	1017.153065	17.859776
36.529225	1017.237188	17.864794
36.837092	1020.206057	17.869811
36.846992	1020.838951	17.874829
36.828900	1013.744420	17.879847
36.898468	1017.662663	17.884864
37.093353	1027.715165	17.889882
37.405002	1033.687807	17.894899
37.209430	1040.263792	17.899917
37.458536	1030.877272	17.904935
37.156469	1043.513384	17.909952
37.262130	1037.677572	17.914970
37.609971	1047.892316	17.919987
37.567419	1048.309364	17.925005
37.835808	1037.285092	17.930023
37.382616	1029.128933	17.935040
37.390089	1025.546001	17.940058
37.381527	1034.289150	17.945075
37.357263	1046.048595	17.950093
37.629425	1039.536591	17.955111
37.625919	1044.356237	17.960128
37.800154	1044.805592	17.965146
37.611773	1049.483790	17.970163
37.442400	1042.400327	17.975181
37.697590	1041.445270	17.980199
37.753788	1045.318276	17.985216
37.811714	1045.946802	17.990234
37.659876	1035.916190	17.995251
37.766310	1049.665434	18.000269
37.794024	1059.598977	18.005287
37.755307	1057.790551	18.010304
38.001819	1068.002247	18.015322
38.665656	1060.403218	18.020339
38.174372	1064.608162	18.025357
38.497803	1059.186354	18.030375
38.339006	1064.244934	18.035392
38.363047	1064.238132	18.040410
38.408542	1063.476877	18.045427
38.177335	1057.330915	18.050445
38.531152	1049.193476	18.055463
38.126659	1058.680333	18.060480
38.444080	1056.740368	18.065498
38.331093	1059.077740	18.070515
38.469518	1055.909792	18.075533
38.664739	1055.901417	18.080551
38.711489	1057.219670	18.085568
38.602699	1045.506552	18.090586
38.783274	1057.076119	18.095603
38.377757	1054.735019	18.100621
38.892153	1049.977580	18.105639
38.645671	1062.961608	18.110656
38.718158	1053.785788	18.115674
38.563686	1049.556030	18.120691
38.670376	1065.249247	18.125709
39.081712	1064.162426	18.130727
39.141911	1071.237998	18.135744
39.346733	1075.614752	18.140762
39.283432	1064.598249	18.145779
38.798984	1061.316449	18.150797
39.298937	1065.918363	18.155815
39.292931	1071.255968	18.160832
39.241057	1077.831542	18.165850
39.444184	1074.606116	18.170867
39.186726	1077.632011	18.175885
39.345512	1074.615506	18.180903
39.000970	1072.839215	18.185920
39.552561	1060.609205	18.190938
39.362252	1064.871136	18.195955
39.437544	1074.951870	18.200973
39.502997	1066.506148	18.205991
39.424333	1067.645232	18.211008
39.589182	1072.886639	18.216026
39.682972	1065.503155	18.221043
39.314753	1073.939750	18.226061
39.718496	1064.456401	18.231079
39.401697	1071.865599	18.236096
39.877288	1070.017618	18.241114
39.483527	1067.106622	18.246131
39.341353	1087.156053	18.251149
40.192294	1087.420488	18.256167
39.843331	1093.629199	18.261184
40.121325	1089.334829	18.266202
40.317048	1085.337377	18.271219
40.034369	1089.070980	18.276237
40.056291	1085.296421	18.281255
40.141569	1082.556524	18.286272
40.221801	1084.680587	18.291290
40.405249	1082.928871	18.296307
40.158780	1093.107365	18.301325
40.416462	1081.412546	18.306343
40.535632	1089.542409	18.311360
40.146899	1082.016764	18.316378
40.556276	1085.600911	18.321395
40.474061	1076.979501	18.326413
40.592049	1074.452234	18.331431
40.479897	1080.668020	18.336448
40.491514	1082.029649	18.341466
40.285186	1072.973244	18.346483
40.656748	1082.284873	18.351501
40.481273	1078.970440	18.356519
40.452271	1081.635488	18.361536
40.843825	1081.807795	18.366554
40.844942	1081.971845	18.371571
40.529378	1094.591173	18.376589
41.174547	1095.209745	18.381607
41.286754	1102.431819	18.386624
40.983070	1092.784732	18.391642
41.056479	1097.134743	18.396659
41.025632	1107.225813	18.401677
41.330152	1108.472125	18.406695
40.958637	1104.819166	18.411712
40.977264	1101.764655	18.416730
40.938057	1108.619128	18.421747
40.988207	1105.272495	18.426765
41.530942	1105.749324	18.431783
41.339290	1100.635427	18.436800
40.914724	1099.777402	18.441818
41.165444	1091.015458	18.446835
41.069848	1105.951441	18.451853
40.999894	1117.203688	18.456871
41.336842	1117.734851	18.461888
41.367938	1125.600813	18.466906
42.035001	1118.616647	18.471923
41.514964	1129.084181	18.476941
41.528560	1129.583953	18.481959
41.516856	1130.097158	18.486976
41.756036	1124.672751	18.491994
41.866050	1125.289963	18.497011
41.618433	1124.634590	18.502029
41.828294	1121.073580	18.507047
42.204489	1134.786936	18.512064
41.802394	1136.368025	18.517082
42.192054	1133.823432	18.522099
42.165523	1138.271164	18.527117
42.328060	1141.098719	18.532135
42.377656	1134.697292	18.537152
42.404093	1141.958066	18.542170
42.197742	1126.646718	18.547187
42.135893	1125.848629	18.552205
42.518416	1126.694549	18.557223
42.941668	1130.929795	18.562240
42.349958	1115.262259	18.567258
42.498212	1114.106199	18.572275
42.112689	1120.320647	18.577293
42.191246	1123.767282	18.582311
42.687556	1130.869226	18.587328
42.311111	1132.481010	18.592346
42.657241	1131.300258	18.597363
42.605141	1128.187396	18.602381
42.665883	1138.343030	18.607399
42.683298	1126.720540	18.612416
42.517896	1130.255893	18.617434
42.864600	1129.529495	18.622451
42.779032	1137.536821	18.627469
42.821150	1133.393007	18.632487
42.711614	1131.598826	18.637504
42.852652	1149.464280	18.642522
43.104603	1153.612759	18.647539
42.797957	1169.200411	18.652557
43.007035	1159.523445	18.657575
43.197046	1153.614418	18.662592
43.425792	1147.399516	18.667610
43.448367	1146.802798	18.672627
43.531103	1154.057912	18.677645
43.456231	1147.609709	18.682663
43.490547	1151.066437	18.687680
43.419412	1148.988520	18.692698
43.609621	1149.836170	18.697715
43.390098	1153.395787	18.702733
43.379798	1155.903279	18.707751
43.480876	1150.273279	18.712768
43.400277	1156.133846	18.717786
43.732615	1153.831765	18.722803
43.360838	1162.325765	18.727821
43.927442	1177.618813	18.732839
43.878280	1174.817913	18.737856
43.851210	1176.927240	18.742874
43.903409	1169.909998	18.747891
43.959283	1184.573002	18.752909
44.120389	1180.341106	18.757927
44.279093	1176.324187	18.762944
44.211338	1175.063108	18.767962
44.129187	1170.045646	18.772979
44.031983	1176.776685	18.777997
44.443106	1173.152573	18.783015
44.406304	1165.802131	18.788032
44.179512	1174.077757	18.793050
44.373959	1169.973186	18.798067
44.162647	1177.599435	18.803085
44.382276	1166.566944	18.808103
44.703875	1167.709596	18.813120
44.341148	1181.687085	18.818138
44.466483	1169.167172	18.823155
44.356497	1176.701804	18.828173
44.594420	1183.938928	18.833191
44.899490	1198.717538	18.838208
44.928752	1200.862224	18.843226
44.873349	1192.507963	18.848243
45.105105	1191.373529	18.853261
44.959519	1189.853239	18.858279
45.147744	1188.268025	18.863296
45.016611	1188.042533	18.868314
45.321215	1184.864306	18.873331
45.141302	1183.478785	18.878349
45.211344	1183.146033	18.883367
45.081477	1177.615326	18.888384
45.089284	1186.277088	18.893402
45.564224	1183.091108	18.898419
45.414997	1193.866663	18.903437
45.413629	1185.765876	18.908455
45.420571	1184.205909	18.913472
45.378540	1191.262832	18.918490
45.347923	1184.883422	18.923507
45.359538	1181.981479	18.928525
45.430795	1197.576220	18.933543
45.630213	1185.559096	18.938560
45.451856	1191.520199	18.943578
45.297359	1190.957534	18.948595
45.384079	1182.136032	18.953613
45.247271	1176.398125	18.958631
45.853540	1189.532667	18.963648
45.503222	1193.093848	18.968666
45.929375	1193.674155	18.973683
45.905653	1199.866659	18.978701
45.951459	1204.142124	18.983719
46.303281	1199.274415	18.988736
45.843637	1206.437800	18.993754
45.752354	1202.605213	18.998771
45.734780	1200.982812	19.003789
45.612772	1202.037175	19.008807
46.176390	1208.800394	19.013824
46.301842	1223.477775	19.018842
46.616596	1220.389472	19.023859
46.585523	1221.003546	19.028877
46.670799	1233.001578	19.033895
46.643731	1226.782548	19.038912
46.709901	1222.669660	19.043930
46.537986	1219.158978	19.048947
46.965515	1230.118752	19.053965
46.722120	1217.590302	19.058983
47.018537	1228.337083	19.064000
46.646864	1230.421510	19.069018
47.255641	1225.955359	19.074035
46.676449	1225.781132	19.079053
46.907041	1224.845699	19.084071
47.206135	1218.392528	19.089088
46.726778	1227.622954	19.094106
47.358224	1218.375253	19.099123
46.948109	1212.601259	19.104141
46.799890	1220.397525	19.109159
47.095706	1219.966282	19.114176
46.836803	1222.446460	19.119194
47.341493	1218.681444	19.124211
46.979005	1220.429908	19.129229
47.049575	1233.878793	19.134247
47.548411	1235.419724	19.139264
47.366050	1245.544079	19.144282
47.920221	1237.271020	19.149299
47.674836	1241.636299	19.154317
47.793418	1237.931773	19.159335
48.055599	1237.430058	19.164352
47.717002	1238.672995	19.169370
47.820298	1240.458940	19.174387
47.875832	1233.179213	19.179405
47.699935	1239.657511	19.184423
48.165216	1231.363667	19.189440
47.809477	1233.272025	19.194458
47.782640	1242.276921	19.199475
48.099814	1233.712783	19.204493
47.950596	1240.196369	19.209511
47.770194	1227.617017	19.214528
47.590534	1238.955958	19.219546
47.957078	1244.885356	19.224563
48.198429	1261.176201	19.229581
48.094062	1260.031308	19.234599
48.499869	1256.490065	19.239616
48.189158	1269.730464	19.244634
48.656339	1266.709792	19.249651
48.576090	1255.534877	19.254669
48.435970	1257.163296	19.259687
48.428419	1253.317578	19.264704
48.426624	1251.408671	19.269722
48.515084	1259.281485	19.274739
48.750256	1256.126747	19.279757
48.559226	1256.478698	19.284775
48.823646	1259.397610	19.289792
49.052290	1277.198972	19.294810
49.058615	1282.102352	19.299827
49.267196	1274.391519	19.304845
49.058650	1282.238291	19.309863
49.589811	1275.811858	19.314880
49.065121	1270.570205	19.319898
49.138632	1248.682221	19.324915
49.172397	1256.336379	19.329933
49.102938	1266.913284	19.334951
49.512332	1268.155799	19.339968
48.972288	1273.236299	19.344986
49.094861	1272.011667	19.350003
49.303984	1267.273598	19.355021
49.310453	1270.286576	19.360039
49.649153	1264.568817	19.365056
49.307569	1274.020683	19.370074
49.643110	1269.389042	19.375091
49.612854	1273.386100	19.380109
49.820331	1294.034250	19.385127
50.134508	1289.762566	19.390144
50.023471	1289.360351	19.395162
50.171891	1295.996146	19.400179
49.847309	1284.250406	19.405197
49.835715	1288.383402	19.410215
50.203526	1283.784572	19.415232
49.755708	1295.345448	19.420250
50.078082	1296.131372	19.425267
50.109008	1293.775509	19.430285
50.185922	1303.183914	19.435303
50.237047	1289.993870	19.440320
49.790228	1292.298366	19.445338
49.995873	1299.534283	19.450355
50.446355	1307.934238	19.455373
50.229344	1312.430792	19.460391
50.510434	1313.819649	19.465408
50.523698	1313.915524	19.470426
50.777608	1318.543431	19.475443
50.708430	1310.093440	19.480461
50.589608	1322.164536	19.485479
50.918492	1313.989857	19.490496
50.999207	1322.946384	19.495514
50.724836	1313.767969	19.500531
51.079431	1309.136488	19.505549
50.904906	1308.703193	19.510567
50.762564	1314.665006	19.515584
51.059599	1334.541757	19.520602
51.242544	1336.911697	19.525619
51.529812	1339.075938	19.530637
51.431743	1341.445724	19.535655
51.502109	1340.043070	19.540672
51.666925	1329.363059	19.545690
51.412866	1335.591698	19.550707
51.997109	1334.010699	19.555725
51.349353	1329.520478	19.560743
51.547494	1313.773198	19.565760
51.818701	1325.540185	19.570778
52.007759	1323.582433	19.575795
52.140047	1325.770955	19.580813
51.569927	1319.482336	19.585831
51.827651	1322.247668	19.590848
51.986461	1316.857887	19.595866
51.936515	1330.136373	19.600883
51.906078	1325.423198	19.605901
51.875815	1326.336958	19.610919
52.060776	1323.609809	19.615936
51.776879	1331.985976	19.620954
51.865353	1323.931012	19.625971
52.033323	1321.458997	19.630989
52.160876	1324.364649	19.636007
52.010693	1316.230312	19.641024
52.306003	1320.990592	19.646042
51.995872	1334.019503	19.651059
52.381868	1347.169738	19.656077
52.664389	1345.061637	19.661095
52.951280	1340.832087	19.666112
52.807107	1344.903815	19.671130
52.865082	1341.388649	19.676147
52.741366	1340.515034	19.681165
52.547134	1345.232096	19.686183
52.767462	1343.493511	19.691200
52.608261	1345.175422	19.696218
52.781352	1343.564163	19.701235
52.956322	1340.753368	19.706253
52.767299	1345.621097	19.711271
53.011756	1336.074196	19.716288
53.202988	1350.264835	19.721306
53.334747	1355.751359	19.726323
53.905760	1358.230920	19.731341
53.510439	1350.804025	19.736359
53.145639	1334.311769	19.741376
53.273769	1337.880071	19.746394
53.541611	1346.883033	19.751411
53.630348	1349.618040	19.756429
53.399475	1354.293506	19.761447
53.547801	1343.937972	19.766464
53.881010	1359.141509	19.771482
53.740761	1368.811197	19.776499
54.101773	1359.681537	19.781517
53.668246	1365.588000	19.786535
53.856127	1358.410566	19.791552
53.842145	1345.653573	19.796570
54.052472	1347.271276	19.801587
54.065250	1353.997774	19.806605
53.736966	1366.931720	19.811623
54.175669	1355.681747	19.816640
54.203903	1368.105387	19.821658
54.510870	1378.800111	19.826675
54.744859	1368.421674	19.831693
54.390759	1371.084050	19.836711
54.388954	1359.694801	19.841728
54.661963	1368.933657	19.846746
54.661474	1378.392100	19.851763
54.412828	1372.718990	19.856781
54.193244	1380.324530	19.861799
54.698854	1372.516624	19.866816
54.663351	1384.123414	19.871834
54.574075	1388.757769	19.876851
54.752687	1382.935662	19.881869
54.386538	1391.018620	19.886887
54.849939	1391.425835	19.891904
55.290654	1402.945402	19.896922
55.124530	1406.196890	19.901939
55.549821	1397.016113	19.906957
55.424101	1399.611153	19.911975
55.716395	1385.758383	19.916992
55.298831	1372.966768	19.922010
55.220587	1374.213107	19.927027
55.176413	1387.793698	19.932045
55.448427	1395.394809	19.937063
55.688204	1391.586053	19.942080
55.802927	1387.711681	19.947098
55.642427	1382.807423	19.952115
55.910162	1386.268652	19.957133
55.712404	1391.415482	19.962151
55.772830	1391.005336	19.967168
55.594577	1391.188024	19.972186
55.722058	1390.293985	19.977203
55.966642	1381.034228	19.982221
55.651886	1392.416524	19.987239
55.813495	1394.455288	19.992256
55.894997	1383.911378	19.997274
56.114973	1397.400097	20.002291
56.029156	1397.568303	20.007309
55.940449	1408.852074	20.012327
56.111431	1406.234404	20.017344
56.364883	1418.196745	20.022362
56.236116	1416.105736	20.027379
56.507538	1410.272235	20.032397
56.105947	1413.453315	20.037415
56.364973	1418.216150	20.042432
56.915609	1427.632454	20.047450
56.583260	1426.381253	20.052467
56.907219	1432.986441	20.057485
57.038241	1443.049184	20.062503
57.009745	1439.254047	20.067520
57.180541	1430.498147	20.072538
57.156602	1435.734525	20.077555
57.429887	1437.383400	20.082573
57.464435	1426.720585	20.087591
57.336465	1429.117159	20.092608
57.438674	1428.498487	20.097626
57.197940	1426.526008	20.102643
57.504729	1420.295629	20.107661
57.479640	1426.336942	20.112679
56.923175	1427.929618	20.117696
57.117030	1424.178545	20.122714
56.911824	1428.957310	20.127731
57.566116	1432.039237	20.132749
57.643279	1443.836705	20.137767
57.571151	1449.393073	20.142784
58.032717	1448.576081	20.147802
57.495133	1455.306792	20.152819
57.800069	1452.144245	20.157837
57.606132	1456.050219	20.162855
57.591049	1448.270209	20.167872
58.125642	1455.199023	20.172890
58.230757	1475.345850	20.177907
58.474010	1472.915670	20.182925
58.263594	1476.477079	20.187943
58.671038	1483.580465	20.192960
58.654602	1475.197874	20.197978
58.158220	1474.660361	20.202995
58.632471	1466.298729	20.208013
58.730981	1482.580597	20.213031
58.742950	1474.487057	20.218048
59.025490	1469.159899	20.223066
58.956621	1474.920899	20.228083
58.939643	1463.350917	20.233101
58.882811	1465.957265	20.238119
58.674326	1468.218130	20.243136
58.679774	1467.617772	20.248154
58.517102	1466.519872	20.253171
58.763109	1467.655453	20.258189
59.006590	1470.003302	20.263207
59.054294	1481.483506	20.268224
59.180958	1478.705505	20.273242
59.469784	1487.276046	20.278259
59.275635	1480.180509	20.283277
59.580488	1487.331530	20.288295
59.398785	1485.655920	20.293312
59.922801	1485.785388	20.298330
59.550253	1479.320584	20.303347
59.938145	1480.919947	20.308365
60.137364	1482.564651	20.313383
59.698071	1471.799316	20.318400
59.586904	1477.516449	20.323418
59.426882	1476.452848	20.328435
59.662312	1480.174787	20.333453
59.692602	1480.160695	20.338471
59.842251	1475.602309	20.343488
59.872341	1482.607020	20.348506
59.848432	1505.071608	20.353523
60.190611	1500.650315	20.358541
60.053522	1510.821377	20.363559
60.106548	1498.104271	20.368576
60.688412	1498.559204	20.373594
60.597663	1498.447306	20.378611
60.368600	1502.475563	20.383629
60.336889	1499.880168	20.388647
60.431880	1516.582357	20.393664
60.935537	1519.223979	20.398682
61.106569	1530.817441	20.403699
61.397603	1523.342902	20.408717
60.988314	1504.862910	20.413735
60.763098	1512.617716	20.418752
61.049899	1517.344668	20.423770
61.072338	1528.125088	20.428787
60.657952	1525.709570	20.433805
61.093309	1529.829403	20.438823
61.249291	1530.215356	20.443840
60.971585	1528.958743	20.448858
60.872287	1534.096499	20.453875
61.097550	1541.506173	20.458893
61.772977	1541.624543	20.463911
61.708521	1544.001714	20.468928
62.243342	1537.795530	20.473946
61.973309	1543.281944	20.478963
62.140272	1541.561170	20.483981
61.788823	1539.533438	20.488999
61.800307	1540.737326	20.494016
62.115269	1532.586821	20.499034
62.233741	1539.899612	20.504051
62.542444	1526.123062	20.509069
62.254037	1535.377378	20.514087
61.868526	1539.139808	20.519104
62.257551	1523.965220	20.524122
62.255007	1540.310312	20.529139
62.070578	1542.374906	20.534157
61.963728	1532.516853	20.539175
62.003263	1535.682492	20.544192
62.105911	1543.903517	20.549210
62.520888	1554.101723	20.554227
62.844923	1544.564335	20.559245
63.233667	1552.368139	20.564263
63.081754	1554.613840	20.569280
63.391843	1545.539403	20.574298
63.004826	1556.686961	20.579315
63.492176	1553.319086	20.584333
63.914640	1547.695415	20.589351
63.354329	1539.543178	20.594368
63.434272	1515.151204	20.599386
63.059570	1520.988539	20.604403
63.391675	1526.478442	20.609421
63.445486	1522.118103	20.614439
63.380623	1540.571654	20.619456
64.072794	1522.373526	20.624474
63.480129	1517.663177	20.629491
63.306090	1511.006308	20.634509
63.683138	1525.448852	20.639527
63.298738	1537.444934	20.644544
63.661844	1521.813642	20.649562
63.661552	1534.188216	20.654579
63.655003	1528.230964	20.659597
63.883051	1524.098957	20.664615
64.118556	1533.230161	20.669632
64.055912	1530.166219	20.674650
63.889220	1536.138233	20.679667
64.028010	1548.500494	20.684685
64.233526	1550.901642	20.689703
64.216939	1558.936220	20.694720
64.441131	1550.563232	20.699738
64.309144	1557.782722	20.704755
64.510508	1551.732925	20.709773
64.216138	1558.602300	20.714791
64.282516	1575.006056	20.719808
65.071006	1576.047183	20.724826
64.634806	1575.724309	20.729843
64.812424	1568.172842	20.734861
64.883595	1567.625303	20.739879
65.168660	1575.410647	20.744896
64.993116	1569.091677	20.749914
64.929545	1577.379787	20.754931
64.652096	1576.984701	20.759949
65.334615	1586.853819	20.764967
65.470920	1599.705676	20.769984
65.884184	1597.652804	20.775002
65.659321	1601.913965	20.780019
65.493865	1596.230906	20.785037
65.535918	1594.255129	20.790055
65.704856	1589.337071	20.795072
65.751353	1590.320873	20.800090
65.875057	1590.162751	20.805107
65.617413	1587.833126	20.810125
65.821745	1588.763796	20.815143
66.020237	1590.594824	20.820160
66.109631	1581.671716	20.825178
65.860585	1592.778744	20.830195
65.829759	1595.349476	20.835213
66.259463	1598.523428	20.840231
66.021520	1612.292346	20.845248
66.284785	1606.258079	20.850266
66.545744	1616.467827	20.855283
66.447270	1614.189003	20.860301
66.697980	1614.373917	20.865319
66.621745	1620.344410	20.870336
66.689447	1607.416635	20.875354
67.253394	1610.443318	20.880371
66.875055	1608.703826	20.885389
66.937963	1607.605290	20.890407
66.595194	1619.153071	20.895424
66.514838	1620.131501	20.900442
66.925835	1631.157234	20.905459
66.810296	1633.974784	20.910477
67.173873	1631.184889	20.915495
67.012284	1640.286841	20.920512
67.265452	1638.009727	20.925530
67.360827	1654.699361	20.930547
67.782067	1660.184809	20.935565
67.765275	1654.967612	20.940583
67.919987	1657.158974	20.945600
67.947201	1649.744652	20.950618
68.164721	1649.600235	20.955635
67.942724	1647.590079	20.960653
67.813850	1646.231240	20.965671
68.091610	1643.445321	20.970688
68.093939	1638.622783	20.975706
68.164438	1643.263731	20.980723
68.383591	1642.203833	20.985741
68.649474	1636.595199	20.990759
68.207365	1647.325391	20.995776
68.502363	1646.569204	21.000794
68.416174	1642.666292	21.005811
68.557048	1651.720862	21.010829
68.573304	1647.009754	21.015847
68.337655	1646.794319	21.020864
68.272134	1643.288974	21.025882
68.748749	1637.508462	21.030899
68.488449	1639.095781	21.035917
69.077764	1652.025031	21.040935
68.920957	1659.352597	21.045952
69.330172	1660.610950	21.050970
69.171791	1666.815246	21.055987
68.606955	1675.579587	21.061005
69.157843	1662.576069	21.066023
68.968190	1664.508945	21.071040
69.188066	1664.992193	21.076058
69.060159	1666.180058	21.081075
69.333354	1682.346373	21.086093
69.550048	1685.032980	21.091111
69.284349	1699.977175	21.096128
69.631399	1688.621426	21.101146
69.837701	1688.074804	21.106163
69.458379	1689.463013	21.111181
69.781982	1695.755915	21.116199
69.859111	1713.502554	21.121216
70.164162	1721.038665	21.126234
70.388649	1716.998695	21.131251
70.107128	1712.242701	21.136269
70.221881	1709.605393	21.141287
70.470416	1715.323054	21.146304
70.627316	1704.495729	21.151322
70.648249	1711.139029	21.156339
70.314507	1720.630929	21.161357
70.464984	1711.549855	21.166375
70.616012	1717.162866	21.171392
70.581806	1733.109132	21.176410
70.832800	1735.190739	21.181427
70.685131	1731.710872	21.186445
71.320052	1736.058276	21.191463
71.165020	1730.973175	21.196480
71.094491	1734.493782	21.201498
71.183175	1733.400667	21.206515
71.215904	1732.676100	21.211533
71.602785	1728.765327	21.216551
71.550088	1725.762912	21.221568
71.696648	1731.133618	21.226586
71.365829	1727.411033	21.231603
71.273566	1736.508484	21.236621
71.915766	1744.660848	21.241639
71.745423	1744.258445	21.246656
72.038187	1755.558412	21.251674
72.174511	1745.539060	21.256691
71.837133	1758.348473	21.261709
72.110373	1750.311709	21.266727
72.415542	1752.599437	21.271744
72.204886	1749.031599	21.276762
72.424376	1753.497747	21.281779
72.369834	1753.544285	21.286797
72.401434	1755.183716	21.291815
72.434073	1745.354186	21.296832
72.163408	1744.711868	21.301850
72.449329	1741.198782	21.306867
72.701051	1760.934778	21.311885
72.803176	1759.647042	21.316903
72.737662	1768.721382	21.321920
72.659133	1765.401098	21.326938
72.677284	1765.013347	21.331955
72.889007	1768.467647	21.336973
73.133766	1766.908242	21.341991
73.034477	1769.133100	21.347008
73.152566	1768.900114	21.352026
73.250191	1781.736070	21.357043
73.033690	1792.632984	21.362061
73.613217	1786.527016	21.367079
73.402696	1788.343247	21.372096
73.081621	1785.941477	21.377114
73.790522	1782.280059	21.382131
73.763913	1783.565675	21.387149
73.897483	1796.774728	21.392167
74.328561	1805.351539	21.397184
74.193077	1801.939180	21.402202
74.490675	1796.426519	21.407219
74.331893	1781.331229	21.412237
74.131386	1785.105752	21.417255
74.239942	1785.688501	21.422272
74.828509	1801.003895	21.427290
74.984888	1797.416415	21.432307
74.441684	1793.304190	21.437325
74.703023	1798.401299	21.442343
74.452944	1802.691705	21.447360
74.937463	1810.060874	21.452378
74.750009	1797.763105	21.457395
74.439813	1798.149515	21.462413
74.855528	1798.598929	21.467431
74.963137	1801.075415	21.472448
74.805828	1805.234516	21.477466
75.518003	1812.971983	21.482483
75.480780	1827.691129	21.487501
75.773353	1821.986732	21.492519
75.256657	1821.534444	21.497536
75.226091	1821.233224	21.502554
75.462264	1818.810420	21.507571
75.480934	1817.706178	21.512589
75.577276	1817.419790	21.517607
75.433678	1825.430202	21.522624
75.520390	1824.230088	21.527642
75.962124	1832.634820	21.532659
76.230622	1832.917941	21.537677
76.179281	1827.841814	21.542695
76.589294	1823.157336	21.547712
76.134313	1831.737274	21.552730
76.306099	1827.866492	21.557747
76.086034	1833.181053	21.562765
76.548674	1828.169575	21.567783
76.560769	1837.547389	21.572800
76.470710	1836.040435	21.577818
76.832462	1831.278305	21.582835
77.022346	1843.837905	21.587853
77.209773	1845.831649	21.592871
77.226281	1835.815238	21.597888
76.905473	1847.170365	21.602906
76.932219	1842.082000	21.607923
76.967431	1848.880913	21.612941
76.981409	1856.200738	21.617959
77.371596	1851.891766	21.622976
77.116954	1861.137804	21.627994
77.122313	1851.858477	21.633011
77.060477	1846.635657	21.638029
77.453469	1861.053884	21.643047
77.802463	1879.783791	21.648064
77.859867	1882.656341	21.653082
77.966515	1875.529300	21.658099
78.001834	1879.661394	21.663117
78.261017	1878.831910	21.668135
78.115777	1872.085182	21.673152
78.298018	1876.875951	21.678170
78.320300	1880.287366	21.683187
78.255630	1878.170479	21.688205
78.540986	1877.194875	21.693223
78.736483	1874.368157	21.698240
78.318600	1880.045105	21.703258
78.520978	1868.364750	21.708275
78.416211	1871.401569	21.713293
78.978360	1887.169328	21.718311
78.572046	1884.970259	21.723328
78.582941	1893.010149	21.728346
79.190157	1896.781231	21.733363
78.861636	1901.778269	21.738381
78.944834	1904.406925	21.743399
79.012851	1901.745352	21.748416
78.775680	1901.236644	21.753434
79.281308	1908.574142	21.758451
79.367180	1911.937728	21.763469
79.359517	1910.982782	21.768487
79.479468	1909.061042	21.773504
79.653041	1919.982132	21.778522
79.817380	1909.983546	21.783539
80.020857	1919.700671	21.788557
80.179244	1938.258518	21.793575
79.892649	1936.469903	21.798592
80.049901	1940.964784	21.803610
80.048523	1931.708563	21.808627
80.038086	1936.513756	21.813645
79.931554	1933.257792	21.818663
80.302797	1933.117693	21.823680
80.124871	1949.468545	21.828698
80.832838	1951.144046	21.833715
80.884069	1956.223623	21.838733
81.029620	1954.234748	21.843751
81.242681	1944.998575	21.848768
80.968924	1957.772915	21.853786
81.365584	1945.017434	21.858803
81.512961	1950.905663	21.863821
81.287546	1957.941123	21.868839
81.242086	1946.116499	21.873856
81.548266	1948.334662	21.878874
81.622597	1936.355568	21.883891
81.364122	1948.240670	21.888909
81.353472	1940.554432	21.893927
81.924483	1952.918688	21.898944
81.449061	1951.222775	21.903962
81.967507	1942.333259	21.908979
81.317505	1950.883843	21.913997
81.718828	1960.825630	21.919015
82.180861	1968.905334	21.924032
82.015988	1969.606671	21.929050
82.309284	1970.375092	21.934067
82.019983	1965.986345	21.939085
82.006511	1970.990851	21.944103
82.330101	1973.723876	21.949120
82.491164	1995.794003	21.954138
82.852566	1990.365967	21.959155
82.914521	2000.471406	21.964173
82.951141	1993.462594	21.969191
82.653607	1992.729795	21.974208
82.725249	1994.347194	21.979226
83.281415	1992.218239	21.984243
83.168666	1989.329337	21.989261
82.624854	1995.354275	21.994279
83.144987	1992.167388	21.999296
83.144986	2007.483648	22.004314
83.254257	2001.094655	22.009331
83.439330	2015.069023	22.014349
83.429620	2021.944473	22.019367
83.793287	2016.793804	22.024384
83.959793	2018.374251	22.029402
83.858622	2005.886084	22.034419
83.532102	2009.320611	22.039437
83.733230	2017.444369	22.044455
84.376165	2023.144521	22.049472
84.217516	2028.793525	22.054490
84.335195	2031.849172	22.059507
84.044053	2043.092470	22.064525
84.468469	2036.856075	22.069543
84.804318	2027.569062	22.074560
84.656482	2032.619885	22.079578
84.647288	2032.911800	22.084595
84.807307	2023.128438	22.089613
84.790172	2029.799912	22.094631
85.036082	2021.057205	22.099648
84.593684	2030.048704	22.104666
84.914818	2037.916968	22.109683
85.248838	2041.254325	22.114701
85.217074	2047.722956	22.119719
85.891372	2055.182423	22.124736
85.673897	2051.451479	22.129754
85.706539	2048.770178	22.134771
85.711742	2049.728915	22.139789
85.680926	2050.245140	22.144807
85.992854	2044.291471	22.149824
85.588504	2052.544823	22.154842
85.938206	2039.787163	22.159859
85.818238	2053.149745	22.164877
86.189513	2068.338456	22.169895
86.132009	2058.715395	22.174912
85.948123	2064.238967	22.179930
86.279288	2063.148871	22.184947
86.182521	2061.920678	22.189965
86.168829	2072.700775	22.194983
86.785729	2080.636337	22.200000
86.827365	2084.840078	22.205018
86.924211	2081.848890	22.210035
86.828457	2083.394687	22.215053
86.773484	2083.867357	22.220071
87.292153	2078.083273	22.225088
87.212718	2081.684244	22.230106
87.348325	2075.575140	22.235123
87.234801	2081.384360	22.240141
87.239859	2100.780653	22.245159
87.555347	2101.801241	22.250176
87.835520	2105.349033	22.255194
87.750921	2103.585561	22.260211
87.646826	2111.245904	22.265229
87.384072	2104.451222	22.270247
88.111516	2095.516263	22.275264
87.720891	2100.649327	22.280282
88.108382	2113.519009	22.285299
88.097491	2121.900111	22.290317
87.946326	2130.615640	22.295335
87.998851	2124.570033	22.300352
87.950093	2126.809111	22.305370
88.224778	2137.171654	22.310387
89.099744	2145.650681	22.315405
88.854261	2143.593651	22.320423
89.317025	2144.909928	22.325440
88.803989	2141.225271	22.330458
88.990245	2137.686696	22.335475
89.025880	2148.449642	22.340493
89.317183	2143.831021	22.345511
89.346425	2137.489234	22.350528
89.328529	2141.626570	22.355546
89.449583	2128.011511	22.360563
89.583715	2129.445551	22.365581
89.757759	2138.163787	22.370599
89.899297	2139.729220	22.375616
89.744470	2138.472246	22.380634
89.569848	2134.747195	22.385651
90.037615	2143.993815	22.390669
90.192279	2161.902333	22.395687
90.313037	2156.780213	22.400704
90.149561	2160.757312	22.405722
90.513881	2163.080011	22.410739
90.267692	2156.241685	22.415757
90.175468	2150.831019	22.420775
90.501775	2150.505442	22.425792
90.778499	2163.947977	22.430810
90.526615	2167.430805	22.435827
90.770806	2178.473543	22.440845
90.946818	2183.896580	22.445863
91.240301	2167.559213	22.450880
91.202235	2173.179902	22.455898
90.992397	2169.214189	22.460915
91.585858	2163.531978	22.465933
91.313326	2170.518094	22.470951
91.184144	2161.628942	22.475968
91.260948	2188.585439	22.480986
91.284425	2195.695615	22.486003
91.504994	2191.962290	22.491021
91.502868	2199.360524	22.496039
92.002173	2203.612519	22.501056
91.724680	2217.211357	22.506074
92.049758	2219.776916	22.511091
92.421992	2224.212939	22.516109
92.309434	2216.021800	22.521127
92.349540	2216.776246	22.526144
92.276415	2209.781388	22.531162
91.932987	2228.642235	22.536179
92.578941	2230.494752	22.541197
92.394256	2230.343913	22.546215
93.301895	2224.757639	22.551232
93.265583	2232.205426	22.556250
93.373529	2233.387936	22.561267
93.293017	2235.508917	22.566285
93.127698	2239.218056	22.571303
93.639841	2245.131292	22.576320
93.606043	2249.154371	22.581338
93.409144	2262.538628	22.586355
94.304805	2259.034065	22.591373
94.239721	2260.082727	22.596391
94.018302	2246.713753	22.601408
93.813455	2246.531356	22.606426
93.980017	2250.791309	22.611443
94.095137	2251.505600	22.616461
93.991481	2250.701385	22.621479
94.087255	2249.007478	22.626496
94.344945	2253.985360	22.631514
94.394254	2253.734739	22.636531
94.599019	2254.393957	22.641549
94.473032	2269.963728	22.646567
94.479213	2270.246926	22.651584
94.716076	2277.169056	22.656602
94.676515	2270.191008	22.661619
95.246613	2270.584689	22.666637
94.869628	2273.923022	22.671655
95.160862	2271.488375	22.676672
94.923863	2278.068146	22.681690
95.363809	2290.674096	22.686707
95.642965	2288.272901	22.691725
95.538845	2292.985560	22.696743
95.585830	2282.118299	22.701760
95.609769	2285.744144	22.706778
95.923030	2292.101999	22.711795
96.031421	2278.091147	22.716813
95.836019	2285.810054	22.721831
96.334389	2298.681435	22.726848
96.245281	2305.929224	22.731866
96.040037	2306.002530	22.736883
96.503147	2311.677297	22.741901
96.552179	2302.375113	22.746919
96.277992	2310.841739	22.751936
96.515171	2306.566100	22.756954
96.327258	2330.370342	22.761971
96.839177	2322.229652	22.766989
97.009813	2331.586043	22.772007
97.153542	2336.360877	22.777024
97.292488	2336.077275	22.782042
97.133429	2335.373263	22.787059
97.154880	2328.496096	22.792077
97.279210	2345.595284	22.797095
97.845373	2358.143634	22.802112
97.983391	2356.515689	22.807130
97.704039	2352.462988	22.812147
97.947553	2349.079516	22.817165
97.915180	2354.626780	22.822183
98.206229	2339.441606	22.827200
98.059401	2346.297633	22.832218
97.676612	2356.750686	22.837235
98.282358	2366.572303	22.842253
98.516368	2366.396894	22.847271
98.486662	2369.920698	22.852288
98.528056	2369.169499	22.857306
98.619896	2377.162207	22.862323
98.863328	2378.320344	22.867341
98.536758	2385.434940	22.872359
98.624865	2386.055630	22.877376
98.857401	2389.576225	22.882394
99.293117	2404.041851	22.887411
99.486757	2406.467070	22.892429
99.487537	2408.266038	22.897447
99.405027	2409.039702	22.902464
99.690086	2410.001955	22.907482
99.708706	2417.327594	22.912499
99.844841	2402.494871	22.917517
99.807067	2416.173078	22.922535
99.924509	2428.798092	22.927552
100.512978	2430.056824	22.932570
100.446568	2444.216108	22.937587
100.857393	2425.628765	22.942605
100.682127	2425.839399	22.947623
100.911331	2429.303714	22.952640
100.952876	2417.149539	22.957658
101.063746	2420.392529	22.962675
101.424202	2420.131032	22.967693
101.082124	2420.566633	22.972711
101.126332	2418.246415	22.977728
101.250282	2413.158439	22.982746
101.092730	2414.022763	22.987763
101.366436	2414.851083	22.992781
101.201238	2420.330806	22.997799
101.425253	2421.791816	23.002816
101.562425	2432.428562	23.007834
101.249043	2442.728766	23.012851
101.768255	2442.982088	23.017869
101.857714	2443.356393	23.022887
101.982649	2433.950723	23.027904
102.013998	2442.082338	23.032922
102.157787	2449.413628	23.037939
102.589784	2457.668690	23.042957
102.424388	2463.009588	23.047975
102.272007	2458.548771	23.052992
102.687933	2462.327853	23.058010
102.379044	2457.872619	23.063027
102.598507	2456.377085	23.068045
102.798410	2471.368905	23.073063
103.240949	2478.719681	23.078080
103.277066	2478.168138	23.083098
103.030769	2489.979099	23.088115
103.273524	2482.041469	23.093133
103.374351	2476.549962	23.098151
103.406441	2479.035217	23.103168
103.832755	2493.751721	23.108186
103.459853	2499.671146	23.113203
103.980072	2493.653137	23.118221
103.646990	2491.354146	23.123239
103.797099	2500.887426	23.128256
103.765460	2513.826218	23.133274
103.827605	2525.913958	23.138291
104.090475	2518.635943	23.143309
104.510701	2526.100697	23.148327
104.538583	2541.700251	23.153344
105.137389	2543.774805	23.158362
105.179332	2544.917179	23.163379
105.407887	2541.577045	23.168397
104.998815	2549.585185	23.173415
105.510792	2548.315241	23.178432
105.478673	2545.984872	23.183450
105.564937	2539.195310	23.188467
105.814479	2544.272389	23.193485
105.543922	2545.454254	23.198503
105.459147	2538.369565	23.203520
105.757894	2537.167746	23.208538
105.797576	2538.562962	23.213555
105.834136	2536.060873	23.218573
106.041412	2558.411659	23.223591
106.338275	2557.244851	23.228608
106.359363	2557.715085	23.233626
106.234227	2564.201687	23.238643
106.614506	2566.588219	23.243661
106.314068	2568.065129	23.248679
106.425304	2584.674242	23.253696
106.745583	2581.622718	23.258714
107.020952	2590.776624	23.263731
106.822208	2582.952305	23.268749
106.883153	2590.183012	23.273767
107.225411	2597.833598	23.278784
107.286446	2596.451245	23.283802
107.106662	2613.693017	23.288819
107.707766	2605.421452	23.293837
107.522609	2610.882266	23.298855
107.241204	2624.573552	23.303872
107.793121	2618.806181	23.308890
107.963455	2631.987998	23.313907
108.001169	2626.004509	23.318925
108.394289	2629.193849	23.323943
108.142448	2622.400416	23.328960
108.376058	2630.844445	23.333978
108.380847	2648.966298	23.338995
108.794454	2654.955075	23.344013
108.797725	2654.014157	23.349031
108.955135	2647.459586	23.354048
108.838028	2645.890521	23.359066
109.158720	2641.058866	23.364083
109.098941	2638.426674	23.369101
109.248664	2647.354116	23.374119
109.227666	2667.619884	23.379136
109.754452	2666.647444	23.384154
109.459275	2668.480181	23.389171
109.819621	2663.452939	23.394189
109.966595	2669.871699	23.399207
109.539744	2667.618937	23.404224
109.794355	2665.878014	23.409242
109.775144	2678.941222	23.414259
110.253585	2690.320001	23.419277
110.228963	2687.407710	23.424295
110.413592	2688.445679	23.429312
110.538577	2682.473748	23.434330
111.074583	2694.455800	23.439347
111.217218	2694.181084	23.444365
111.333203	2685.925518	23.449383
111.450027	2689.016130	23.454400
111.321795	2674.890546	23.459418
111.268587	2680.681040	23.464435
111.221536	2694.013737	23.469453
111.493586	2701.385003	23.474471
111.386425	2697.109565	23.479488
111.322194	2698.789346	23.484506
111.604824	2704.751318	23.489523
111.821582	2710.180757	23.494541
111.921808	2713.908358	23.499559
112.172017	2724.606471	23.504576
112.302050	2721.565792	23.509594
111.926892	2726.308403	23.514611
112.100656	2735.626641	23.519629
112.201630	2735.188019	23.524647
112.503809	2744.546109	23.529664
112.887373	2744.233646	23.534682
113.103856	2760.573942	23.539699
113.242966	2761.372867	23.544717
113.325025	2768.871767	23.549735
113.362458	2766.120173	23.554752
113.903857	2764.236469	23.559770
113.756483	2765.863003	23.564787
113.664563	2762.490977	23.569805
113.729446	2755.338569	23.574823
113.513538	2762.502255	23.579840
113.741184	2766.017378	23.584858
114.029064	2773.979550	23.589875
114.532058	2786.452884	23.594893
114.540944	2783.570045	23.599911
114.189878	2781.756725	23.604928
114.364502	2772.706051	23.609946
114.337408	2784.451301	23.614963
114.592344	2797.768324	23.619981
114.815784	2796.354200	23.624999
115.047202	2801.724558	23.630016
115.467720	2790.397638	23.635034
115.357102	2789.935354	23.640051
115.249347	2792.073292	23.645069
116.059568	2809.223272	23.650087
115.932025	2813.677776	23.655104
116.067893	2813.385181	23.660122
116.030804	2805.832117	23.665139
116.222332	2794.790405	23.670157
116.227448	2804.466497	23.675175
116.265773	2808.686707	23.680192
116.267008	2803.703063	23.685210
116.277828	2812.112647	23.690227
115.905273	2810.031261	23.695245
116.610968	2806.376458	23.700263
116.198333	2814.950225	23.705280
116.527346	2818.162268	23.710298
116.557640	2833.001062	23.715315
116.730101	2822.300030	23.720333
117.330543	2831.321071	23.725351
117.093787	2840.242880	23.730368
117.263839	2841.835470	23.735386
117.260347	2855.060465	23.740403
117.175699	2854.543612	23.745421
117.786583	2849.303478	23.750439
117.490244	2873.829251	23.755456
117.689332	2875.856003	23.760474
117.877614	2880.598754	23.765491
118.019424	2881.558226	23.770509
118.329891	2880.231458	23.775527
118.301926	2898.415505	23.780544
118.837742	2896.624192	23.785562
118.685158	2901.508724	23.790579
118.828247	2893.078384	23.795597
119.135007	2896.713698	23.800615
119.284164	2897.072348	23.805632
119.420403	2894.867053	23.810650
119.145341	2896.478885	23.815667
119.568795	2907.803294	23.820685
119.829578	2912.537851	23.825703
119.721840	2916.345418	23.830720
119.614817	2915.948847	23.835738
119.527861	2927.198580	23.840755
119.948160	2921.988285	23.845773
119.959622	2921.961360	23.850791
119.931036	2944.589449	23.855808
120.254279	2944.516835	23.860826
120.368097	2945.837345	23.865843
120.301539	2951.522707	23.870861
120.578294	2954.742962	23.875879
120.635444	2963.167451	23.880896
120.841386	2963.772856	23.885914
120.948265	2975.020657	23.890931
120.900684	2984.499949	23.895949
121.228467	2987.734309	23.900967
121.186122	2997.736715	23.905984
121.600166	2988.067685	23.911002
121.623352	2998.438567	23.916019
121.714000	3002.751624	23.921037
122.411080	2999.928211	23.926055
122.470852	2998.198844	23.931072
122.621155	3003.316852	23.936090
122.277807	2995.432946	23.941107
122.097356	2999.034144	23.946125
122.463850	2999.907924	23.951143
122.346643	3011.973590	23.956160
123.250473	3014.931491	23.961178
123.084010	3017.353242	23.966195
123.111611	3027.650857	23.971213
123.355603	3017.714927	23.976231
123.309795	3022.364986	23.981248
123.289203	3026.442980	23.986266
123.781007	3026.220867	23.991283
124.036111	3040.080909	23.996301
124.411107	3039.119608	24.001319
123.849497	3045.270771	24.006336
124.176032	3034.674879	24.011354
124.176907	3048.562133	24.016371
124.189601	3048.954790	24.021389
124.627506	3033.645027	24.026407
124.666502	3040.689983	24.031424
124.696711	3033.492398	24.036442
124.908952	3019.906566	24.041459
125.296003	3022.172164	24.046477
125.213197	3027.891658	24.051495
124.958875	3034.130392	24.056512
125.403559	3024.589102	24.061530
125.385498	3037.699734	24.066547
125.259891	3056.205389	24.071565
125.344361	3057.290634	24.076583
125.365615	3064.054320	24.081600
125.716166	3053.265283	24.086618
126.099370	3065.255743	24.091635
125.799535	3072.937692	24.096653
126.216541	3070.817794	24.101671
126.221416	3081.510370	24.106688
126.011245	3073.220507	24.111706
126.258412	3097.516249	24.116723
126.168697	3101.040128	24.121741
126.783947	3105.062712	24.126759
126.946042	3116.286169	24.131776
126.964391	3127.257564	24.136794
127.395463	3124.983958	24.141811
127.163607	3135.931432	24.146829
127.775324	3132.613223	24.151847
127.682192	3132.719465	24.156864
127.673896	3139.538308	24.161882
127.624394	3153.708126	24.166899
127.733902	3160.240242	24.171917
128.310453	3156.681353	24.176935
127.956632	3163.636400	24.181952
128.150390	3169.514608	24.186970
128.562827	3165.650025	24.191987
128.402170	3184.319114	24.197005
128.767294	3178.028493	24.202023
128.649747	3197.492521	24.207040
128.852394	3207.589223	24.212058
129.103164	3203.118715	24.217075
129.214101	3200.175634	24.222093
129.453306	3208.372874	24.227111
129.349810	3217.352896	24.232128
129.267819	3222.081268	24.237146
129.759140	3221.572012	24.242163
129.790402	3232.664540	24.247181
130.081432	3239.499651	24.252199
130.318368	3245.083903	24.257216
130.379556	3250.563128	24.262234
130.419411	3243.827915	24.267251
130.507823	3245.682675	24.272269
131.112288	3254.968425	24.277287
131.144304	3267.326506	24.282304
131.335522	3257.149370	24.287322
131.716684	3259.794670	24.292339
131.642401	3263.199382	24.297357
131.603258	3254.301895	24.302375
131.739886	3258.276405	24.307392
131.758585	3250.610258	24.312410
131.992965	3251.807747	24.317427
131.943545	3256.310089	24.322445
131.944605	3248.047022	24.327463
132.120193	3263.365249	24.332480
132.158981	3270.296703	24.337498
132.521981	3272.537695	24.342515
132.106116	3282.911244	24.347533
132.713038	3278.110328	24.352551
132.411796	3299.263427	24.357568
132.658219	3297.943507	24.362586
132.855119	3288.791242	24.367603
132.889740	3304.055839	24.372621
133.424864	3315.580791	24.377639
133.329272	3329.249812	24.382656
133.239289	3326.148814	24.387674
133.488749	3325.270291	24.392691
133.434183	3334.084893	24.397709
134.091943	3333.855715	24.402727
134.110159	3344.773606	24.407744
134.003186	3340.949330	24.412762
134.380777	3343.165951	24.417779
134.006481	3353.037497	24.422797
134.493054	3360.129239	24.427815
134.494051	3374.092474	24.432832
134.443163	3367.223087	24.437850
135.318589	3371.473253	24.442867
135.355221	3390.512490	24.447885
135.498332	3383.663204	24.452903
135.398550	3388.198719	24.457920
135.364260	3378.135751	24.462938
135.707908	3387.168898	24.467955
135.654153	3401.298545	24.472973
136.280206	3400.648239	24.477991
136.349656	3410.002107	24.483008
136.392873	3400.387798	24.488026
136.647730	3399.615739	24.493043
136.708529	3410.255561	24.498061
136.900046	3405.898443	24.503079
137.210966	3422.840016	24.508096
136.946422	3429.203581	24.513114
137.233797	3425.753070	24.518131
136.949173	3432.981442	24.523149
137.370498	3417.039544	24.528167
137.467223	3427.367589	24.533184
137.414183	3436.118877	24.538202
137.736777	3439.111099	24.543219
137.678225	3443.081509	24.548237
137.823766	3446.751663	24.553255
137.981612	3464.250666	24.558272
138.145632	3465.557037	24.563290
138.750689	3461.428652	24.568307
138.474796	3473.614175	24.573325
138.885930	3483.185990	24.578343
139.177249	3485.094205	24.583360
139.022862	3499.640542	24.588378
139.335578	3489.081269	24.593395
139.470961	3484.452018	24.598413
139.537581	3490.072498	24.603431
139.897468	3500.918018	24.608448
139.823909	3507.993414	24.613466
140.585158	3505.204062	24.618483
139.942895	3503.108033	24.623501
140.082794	3499.914177	24.628519
140.473805	3502.116092	24.633536
140.406086	3512.245853	24.638554
141.003725	3520.191391	24.643571
140.819899	3523.992068	24.648589
141.023022	3525.046128	24.653607
141.098192	3522.323226	24.658624
140.802372	3522.890478	24.663642
141.276201	3528.595520	24.668659
141.185291	3538.552177	24.673677
141.234710	3532.020517	24.678695
141.484887	3548.094278	24.683712
141.625772	3557.878911	24.688730
142.278415	3562.388123	24.693747
142.139644	3570.256520	24.698765
142.359690	3571.424714	24.703783
142.536102	3562.477523	24.708800
142.705125	3570.231417	24.713818
142.558571	3568.464882	24.718835
143.118464	3582.081903	24.723853
142.971514	3580.893029	24.728871
143.180147	3583.104588	24.733888
142.911992	3587.489779	24.738906
143.274192	3584.968091	24.743923
143.168676	3594.021211	24.748941
143.255098	3599.976346	24.753959
143.386891	3610.008623	24.758976
143.637616	3624.778816	24.763994
143.951493	3626.219537	24.769011
144.009769	3642.765329	24.774029
144.114768	3633.134904	24.779047
144.458515	3643.604283	24.784064
144.579519	3645.958987	24.789082
145.107065	3655.941914	24.794099
144.600877	3669.331480	24.799117
145.163921	3651.242980	24.804135
145.020885	3665.715076	24.809152
145.218856	3679.218431	24.814170
145.587868	3672.904937	24.819187
145.608382	3680.404390	24.824205
145.827715	3682.364936	24.829223
146.172352	3686.789869	24.834240
145.953875	3692.824365	24.839258
146.049476	3687.898288	24.844275
146.193805	3705.323892	24.849293
146.116138	3719.542754	24.854311
146.848685	3726.368851	24.859328
146.807273	3719.119088	24.864346
147.106867	3731.410317	24.869363
146.965852	3742.050388	24.874381
147.228644	3747.646527	24.879399
147.411313	3739.222218	24.884416
147.590507	3745.437467	24.889434
148.324279	3750.678909	24.894451
148.389310	3756.921516	24.899469
148.178871	3764.813850	24.904487
148.282225	3758.693450	24.909504
148.365364	3765.024756	24.914522
148.656885	3764.849797	24.919539
148.274176	3772.589213	24.924557
148.873722	3783.817149	24.929575
148.886769	3784.468586	24.934592
149.152591	3798.106591	24.939610
149.049171	3788.013192	24.944627
149.324451	3798.111472	24.949645
149.430048	3808.646663	24.954663
149.677119	3802.765708	24.959680
149.855111	3806.048935	24.964698
150.025165	3809.406002	24.969715
149.649368	3823.390738	24.974733
150.180770	3827.612848	24.979751
150.716530	3829.741626	24.984768
150.579415	3835.782360	24.989786
150.996465	3841.903565	24.994803
151.077555	3840.590571	24.999821
151.387557	3840.194929	25.004839
151.437083	3840.073663	25.009856
151.787471	3835.792555	25.014874
151.783347	3838.750810	25.019891
151.798735	3836.428612	25.024909
151.768590	3836.540771	25.029927
152.222445	3855.982273	25.034944
151.984984	3856.190038	25.039962
152.555206	3855.611593	25.044979
152.333477	3856.817453	25.049997
152.488952	3858.368231	25.055015
152.703088	3850.235636	25.060032
152.642434	3868.438407	25.065050
153.179424	3872.394519	25.070067
152.841274	3875.357765	25.075085
153.071465	3878.471854	25.080103
153.542470	3883.053793	25.085120
153.535310	3897.422723	25.090138
153.641936	3892.236043	25.095155
153.442313	3897.708980	25.100173
153.758374	3906.560487	25.105191
154.052349	3918.366647	25.110208
153.966685	3926.147969	25.115226
154.561659	3920.073593	25.120243
154.512728	3926.362519	25.125261
154.821485	3936.585043	25.130279
154.961489	3944.520400	25.135296
154.691858	3951.825538	25.140314
154.937476	3955.057165	25.145331
155.531901	3962.687770	25.150349
156.088457	3973.872058	25.155367
156.115075	3972.798003	25.160384
155.921141	3978.203789	25.165402
155.989870	3965.523513	25.170419
155.988810	3988.622050	25.175437
156.334173	3992.485113	25.180455
156.612275	3996.961579	25.185472
156.727208	3998.231491	25.190490
156.749428	4001.040452	25.195507
156.948995	4004.755914	25.200525
157.074299	4001.943021	25.205543
157.422686	4006.383227	25.210560
157.295550	4025.344629	25.215578
157.835549	4029.716947	25.220595
157.727894	4025.520179	25.225613
157.891643	4031.034076	25.230631
157.907510	4038.007292	25.235648
158.365822	4050.059240	25.240666
158.180892	4058.383285	25.245683
158.771213	4060.361506	25.250701
158.551670	4062.520263	25.255719
158.992715	4071.945669	25.260736
159.029704	4082.592773	25.265754
159.281870	4073.380953	25.270771
159.160314	4084.810427	25.275789
159.839389	4102.146325	25.280807
159.778630	4094.072470	25.285824
159.786253	4102.795637	25.290842
159.550609	4099.777296	25.295859
160.351383	4112.498447	25.300877
159.980737	4126.179596	25.305895
160.477798	4110.720778	25.310912
160.591783	4134.609513	25.315930
160.470369	4134.432959	25.320947
160.805944	4138.881518	25.325965
161.128542	4146.431687	25.330983
161.123096	4155.876584	25.336000
161.019363	4183.558756	25.341018
161.179040	4172.448598	25.346035
161.614873	4193.165314	25.351053
161.854992	4200.365441	25.356071
162.214464	4198.244961	25.361088
162.289253	4209.754227	25.366106
162.516625	4209.557751	25.371123
162.852639	4213.990478	25.376141
162.702271	4215.122054	25.381159
163.031951	4213.426040	25.386176
162.911386	4221.588569	25.391194
163.206407	4239.874873	25.396211
163.527684	4233.628636	25.401229
163.563797	4241.116408	25.406247
164.213286	4227.098185	25.411264
164.220302	4228.706973	25.416282
164.096919	4227.552241	25.421299
164.261017	4225.118317	25.426317
164.403111	4240.635163	25.431335
164.815858	4243.465047	25.436352
164.829367	4250.028381	25.441370
164.684626	4247.592335	25.446387
164.955698	4250.346567	25.451405
165.129524	4261.351108	25.456423
165.437133	4253.399387	25.461440
165.173278	4270.267670	25.466458
165.661953	4268.190069	25.471475
165.714831	4266.925654	25.476493
166.051386	4285.663177	25.481511
166.146831	4289.398167	25.486528
166.374462	4291.682592	25.491546
165.881011	4296.999670	25.496563
166.685594	4311.554243	25.501581
166.552706	4319.794501	25.506599
166.681335	4318.461399	25.511616
167.172048	4339.441138	25.516634
167.276209	4335.141673	25.521651
167.321338	4340.620589	25.526669
167.322611	4351.364983	25.531687
167.955176	4359.258078	25.536704
167.770865	4359.066123	25.541722
167.828492	4376.711125	25.546739
168.559131	4376.416865	25.551757
168.153153	4395.801110	25.556775
168.571755	4405.091325	25.561792
168.692011	4411.322350	25.566810
168.846389	4406.977124	25.571827
169.105432	4426.326659	25.576845
169.360982	4442.198363	25.581863
169.654879	4436.480316	25.586880
169.581520	4441.851567	25.591898
169.754536	4446.155222	25.596915
170.081238	4452.148750	25.601933
170.462224	4461.710028	25.606951
170.765336	4455.722234	25.611968
170.692197	4453.177093	25.616986
171.144984	4456.903482	25.622003
171.357003	4464.366945	25.627021
171.255452	4471.870067	25.632039
171.569551	4473.812698	25.637056
171.777820	4476.602056	25.642074
171.957441	4465.775831	25.647091
171.922348	4470.866486	25.652109
171.806113	4479.969073	25.657127
172.351695	4489.703437	25.662144
172.452398	4492.967334	25.667162
172.412508	4494.836010	25.672180
172.578088	4490.946695	25.677197
172.678672	4504.488019	25.682215
172.975743	4494.782857	25.687232
172.798876	4519.847674	25.692250
173.048485	4527.747179	25.697268
173.533670	4530.767774	25.702285
173.716604	4541.512229	25.707303
174.377388	4535.515722	25.712320
173.901425	4548.320409	25.717338
173.917244	4554.750920	25.722356
174.451683	4562.220729	25.727373
174.218309	4567.440323	25.732391
174.666478	4562.906994	25.737408
174.920088	4579.255748	25.742426
174.936318	4577.387855	25.747444
175.393473	4587.565404	25.752461
175.334364	4590.917484	25.757479
175.437429	4589.247470	25.762496
175.441725	4599.073004	25.767514
175.553746	4611.529947	25.772532
175.666748	4610.918948	25.777549
175.813131	4627.701198	25.782567
175.908318	4628.544968	25.787584
176.135648	4641.280576	25.792602
176.635168	4651.104311	25.797620
177.018099	4652.531143	25.802637
177.035811	4670.555148	25.807655
177.372235	4674.643869	25.812672
177.113103	4680.965987	25.817690
177.095313	4685.410068	25.822708
177.426794	4701.734106	25.827725
177.534489	4702.127699	25.832743
178.016733	4712.121468	25.837760
178.266541	4720.491343	25.842778
178.328541	4725.980358	25.847796
178.535337	4729.167703	25.852813
178.741649	4754.469525	25.857831
179.001705	4746.616579	25.862848
179.364255	4760.833578	25.867866
179.677221	4765.497321	25.872884
180.138059	4764.913894	25.877901
179.882387	4765.373883	25.882919
180.104305	4770.575869	25.887936
180.268119	4770.231521	25.892954
180.772769	4782.207257	25.897972
181.080795	4779.024717	25.902989
181.006834	4784.310938	25.908007
181.072810	4782.277405	25.913024
181.398119	4782.766325	25.918042
181.233343	4790.042745	25.923060
181.806826	4791.449206	25.928077
182.018118	4797.827084	25.933095
181.855330	4806.466808	25.938112
182.155126	4802.660566	25.943130
181.800083	4808.761015	25.948148
182.339496	4822.347463	25.953165
182.274068	4827.654456	25.958183
182.663013	4829.891583	25.963200
182.972918	4841.755825	25.968218
182.990329	4850.986016	25.973236
182.927367	4844.310507	25.978253
183.358073	4857.014406	25.983271
183.453557	4871.368026	25.988288
184.021511	4877.652179	25.993306
183.755454	4899.300358	25.998324
184.461740	4900.840692	26.003341
184.637408	4902.644076	26.008359
184.669243	4900.754766	26.013376
185.065164	4912.119474	26.018394
185.455718	4918.412494	26.023412
185.633588	4914.104503	26.028429
185.420388	4925.943428	26.033447
185.462484	4916.135943	26.038464
185.516552	4916.774681	26.043482
185.530498	4939.982557	26.048500
185.930220	4934.778073	26.053517
185.650926	4947.435437	26.058535
186.122995	4956.888013	26.063552
186.510398	4955.388065	26.068570
186.392608	4957.117479	26.073588
187.181822	4975.671168	26.078605
187.562366	4980.419076	26.083623
187.506713	4978.773891	26.088640
187.567954	4987.069264	26.093658
187.202869	4982.903134	26.098676
187.902221	4995.132598	26.103693
187.734746	5001.816096	26.108711
187.891964	5006.987251	26.113728
188.908719	5009.227058	26.118746
188.557837	5023.641257	26.123764
189.297877	5023.503348	26.128781
189.083450	5034.155675	26.133799
189.173833	5021.550183	26.138816
189.413896	5035.556160	26.143834
189.536163	5050.180345	26.148852
189.750579	5049.259886	26.153869
189.953802	5058.978748	26.158887
190.127177	5063.667593	26.163904
190.218239	5068.931201	26.168922
189.970170	5078.083149	26.173940
190.355291	5084.582254	26.178957
190.480955	5094.764673	26.183975
191.012801	5110.076002	26.188992
191.133042	5113.374829	26.194010
191.028306	5127.226559	26.199028
191.479309	5127.998828	26.204045
191.740791	5142.534991	26.209063
191.848379	5143.370529	26.214080
192.420230	5154.941415	26.219098
192.558375	5163.234290	26.224116
192.707817	5158.334104	26.229133
192.610241	5165.552797	26.234151
192.857156	5180.602636	26.239168
193.185246	5177.492642	26.244186
193.100971	5186.521131	26.249204
193.600210	5199.132463	26.254221
194.228012	5205.833493	26.259239
194.108871	5208.333347	26.264256
194.427275	5202.595439	26.269274
194.509781	5229.246236	26.274292
194.748596	5222.049825	26.279309
194.787347	5228.334935	26.284327
194.849290	5242.495239	26.289344
195.269745	5245.848069	26.294362
195.405450	5253.257525	26.299380
195.629880	5250.267926	26.304397
195.566445	5260.338015	26.309415
196.115899	5266.524193	26.314432
196.217827	5272.704724	26.319450
196.153074	5282.418337	26.324468
196.451302	5295.465270	26.329485
196.912629	5300.607807	26.334503
196.739417	5300.164731	26.339520
196.961741	5313.990620	26.344538
196.982870	5323.905450	26.349556
197.453852	5330.889935	26.354573
197.732421	5339.678574	26.359591
197.690676	5342.043214	26.364608
198.104874	5340.406461	26.369626
198.229067	5361.659452	26.374644
198.824545	5368.952735	26.379661
199.092994	5374.703169	26.384679
198.998291	5371.043839	26.389696
199.059116	5381.246046	26.394714
199.612696	5395.651423	26.399732
199.465421	5397.161378	26.404749
199.889170	5394.588769	26.409767
199.778750	5393.523472	26.414784
200.124876	5408.624246	26.419802
200.088150	5419.321561	26.424820
200.094135	5418.720988	26.429837
200.519347	5426.470268	26.434855
200.700272	5439.791366	26.439872
200.981312	5428.696153	26.444890
200.864976	5449.930109	26.449908
201.112939	5460.128296	26.454925
201.542861	5468.075723	26.459943
201.679855	5480.178964	26.464960
201.827074	5482.514019	26.469978
201.882115	5493.392711	26.474996
202.447088	5505.750899	26.480013
202.440757	5514.615821	26.485031
202.400430	5527.813813	26.490048
202.849659	5535.177425	26.495066
202.738630	5545.794911	26.500084
202.580614	5557.243647	26.505101
203.126246	5574.961723	26.510119
203.710131	5584.965306	26.515136
204.207801	5586.244818	26.520154
204.192877	5600.761516	26.525172
204.486036	5615.854977	26.530189
204.638013	5610.600728	26.535207
204.943118	5612.911066	26.540224
205.134611	5624.974299	26.545242
205.581871	5636.075731	26.550260
205.743801	5626.299598	26.555277
205.583297	5631.397596	26.560295
205.783603	5651.044894	26.565312
206.181132	5650.095719	26.570330
206.370339	5654.554958	26.575348
206.538557	5669.803774	26.580365
206.769767	5681.264214	26.585383
206.528016	5685.642611	26.590400
207.083996	5694.223818	26.595418
207.461697	5705.165729	26.600436
207.822910	5715.330535	26.605453
208.037577	5717.153144	26.610471
208.086830	5729.999486	26.615488
208.159705	5722.945671	26.620506
208.452239	5731.823856	26.625524
208.510018	5744.921406	26.630541
209.177453	5743.595338	26.635559
209.314472	5761.216618	26.640576
209.339874	5766.860044	26.645594
209.549564	5782.699068	26.650612
209.828628	5767.891711	26.655629
209.832308	5777.885281	26.660647
209.941893	5800.170147	26.665664
210.453172	5796.055939	26.670682
210.743899	5807.699693	26.675700
210.516973	5821.299618	26.680717
210.829707	5819.053697	26.685735
211.162942	5840.751157	26.690752
211.488955	5845.062744	26.695770
211.766273	5842.939165	26.700788
212.064086	5861.138279	26.705805
212.310112	5861.140895	26.710823
212.253571	5869.376205	26.715840
212.507730	5863.793364	26.720858
212.569675	5885.012523	26.725876
212.708297	5889.176702	26.730893
213.241868	5892.193108	26.735911
213.298335	5903.431684	26.740928
213.779510	5908.056746	26.745946
213.704024	5920.853316	26.750964
213.933654	5915.624696	26.755981
214.047780	5926.481764	26.760999
213.784142	5932.101074	26.766016
214.363750	5929.788078	26.771034
214.779875	5954.067496	26.776052
215.042848	5962.268576	26.781069
215.394383	5951.228295	26.786087
215.241861	5966.410806	26.791104
215.680931	5976.210010	26.796122
215.761774	5982.921255	26.801140
215.979443	5973.631809	26.806157
216.303335	5990.747373	26.811175
216.034218	6013.940981	26.816192
216.358813	6012.987432	26.821210
216.860781	6026.460695	26.826228
217.032561	6034.177332	26.831245
217.177836	6037.434525	26.836263
217.536818	6057.654023	26.841280
217.748262	6053.981320	26.846298
217.804260	6059.537969	26.851316
218.161525	6066.101769	26.856333
218.353508	6077.638053	26.861351
218.391653	6082.367287	26.866368
218.890372	6088.037679	26.871386
219.067510	6102.559412	26.876404
219.066284	6111.897333	26.881421
219.491155	6116.995309	26.886439
219.603936	6127.347630	26.891456
219.616910	6141.399503	26.896474
219.664979	6145.082319	26.901492
220.216165	6159.482364	26.906509
220.644733	6169.371707	26.911527
220.985547	6177.655392	26.916544
221.394467	6187.105878	26.921562
221.353583	6201.194645	26.926580
221.520848	6192.099232	26.931597
222.008757	6199.535974	26.936615
221.976864	6210.599177	26.941632
222.139287	6209.478462	26.946650
222.259088	6224.378612	26.951668
222.438249	6232.084707	26.956685
222.886661	6231.351664	26.961703
222.732131	6250.325984	26.966720
223.108144	6263.850723	26.971738
223.248459	6274.473452	26.976756
223.361237	6273.297375	26.981773
224.280722	6290.566144	26.986791
224.427242	6312.495448	26.991808
224.438084	6308.806769	26.996826
224.689705	6315.810216	27.001844
224.896399	6324.004492	27.006861
225.191937	6331.414603	27.011879
225.140296	6346.935183	27.016896
225.537712	6352.488945	27.021914
225.731142	6352.174654	27.026932
225.798848	6374.700382	27.031949
226.354699	6382.798950	27.036967
226.416836	6389.756347	27.041984
226.750502	6400.393054	27.047002
226.442443	6401.240100	27.052020
226.616769	6421.400538	27.057037
227.336757	6428.974641	27.062055
227.267971	6441.821033	27.067072
227.608233	6449.738742	27.072090
228.132413	6455.812488	27.077108
228.273350	6480.795484	27.082125
228.678078	6478.790774	27.087143
228.948467	6485.658761	27.092160
228.806415	6473.044487	27.097178
229.369098	6499.331489	27.102196
229.536303	6505.751599	27.107213
229.648807	6495.944864	27.112231
229.632835	6514.904065	27.117248
229.861016	6525.431099	27.122266
230.227686	6532.246139	27.127284
230.327337	6533.616486	27.132301
230.543724	6537.392972	27.137319
230.913328	6556.077150	27.142336
230.917041	6570.279173	27.147354
231.231140	6574.558076	27.152372
231.274059	6576.795967	27.157389
231.721766	6589.905644	27.162407
231.832011	6603.421759	27.167424
232.314706	6621.766294	27.172442
232.676946	6620.358549	27.177460
232.721190	6634.475352	27.182477
233.031514	6641.182458	27.187495
233.095562	6659.706259	27.192512
233.528362	6658.839903	27.197530
233.720497	6668.394050	27.202548
233.501348	6676.642567	27.207565
234.010442	6695.185077	27.212583
233.866970	6704.204646	27.217600
234.784599	6714.604842	27.222618
235.172769	6722.455184	27.227636
235.001640	6731.021358	27.232653
235.458385	6747.652764	27.237671
235.669554	6751.193348	27.242688
235.820328	6774.034866	27.247706
236.155847	6779.077575	27.252724
236.394842	6787.008138	27.257741
236.941907	6794.366406	27.262759
236.784329	6810.440639	27.267776
237.122497	6808.477889	27.272794
237.350470	6819.226104	27.277812
237.623276	6824.704825	27.282829
237.969311	6823.678427	27.287847
237.995381	6839.105172	27.292864
238.207732	6850.970223	27.297882
238.548357	6855.851154	27.302900
238.691380	6867.919645	27.307917
238.779158	6876.379033	27.312935
239.260673	6882.377527	27.317952
239.420165	6896.763752	27.322970
239.849429	6900.005024	27.327988
240.089180	6916.689518	27.333005
240.600971	6917.269251	27.338023
240.493207	6923.663132	27.343040
240.680380	6937.388423	27.348058
240.703774	6948.339233	27.353076
241.024959	6957.494489	27.358093
241.135435	6962.013736	27.363111
241.564802	6979.587235	27.368128
241.536491	6988.822512	27.373146
242.051433	7000.201451	27.378164
242.304761	7018.796983	27.383181
242.793168	7023.635868	27.388199
242.932540	7038.097964	27.393216
243.137187	7040.597853	27.398234
243.374967	7042.855784	27.403252
243.690420	7058.998192	27.408269
243.989145	7059.024125	27.413287
244.011306	7058.553554	27.418304
244.666540	7076.966223	27.423322
244.743699	7079.533442	27.428340
244.723756	7094.895001	27.433357
244.829784	7089.723295	27.438375
245.272288	7104.545197	27.443392
245.735523	7108.248406	27.448410
245.722543	7115.025274	27.453428
245.715316	7134.441496	27.458445
246.071918	7132.182233	27.463463
246.179103	7141.579462	27.468480
246.481876	7152.533981	27.473498
247.272566	7165.438811	27.478516
246.859252	7179.078408	27.483533
247.373528	7188.613931	27.488551
247.324812	7207.247499	27.493568
247.537029	7207.223847	27.498586
247.744707	7223.114943	27.503604
248.115031	7238.077695	27.508621
248.305078	7244.361895	27.513639
248.599625	7258.528361	27.518656
248.809946	7286.443842	27.523674
249.145766	7294.990844	27.528692
249.686277	7306.984728	27.533709
249.585849	7310.662629	27.538727
249.894157	7328.081795	27.543744
250.289971	7337.800114	27.548762
251.076939	7343.223702	27.553780
251.100470	7360.100319	27.558797
251.256599	7359.008934	27.563815
251.497064	7373.654345	27.568832
251.716037	7385.341916	27.573850
251.977517	7383.814152	27.578868
252.455110	7401.569918	27.583885
253.009858	7404.125506	27.588903
252.910700	7410.818118	27.593920
252.940154	7410.292727	27.598938
253.024932	7422.629578	27.603956
253.577168	7434.700633	27.608973
253.882435	7450.093624	27.613991
254.113830	7457.457415	27.619008
254.208870	7459.100053	27.624026
254.521206	7477.453191	27.629044
254.613641	7488.153578	27.634061
255.062669	7495.956837	27.639079
255.141946	7502.416327	27.644096
255.743778	7512.961162	27.649114
256.302229	7516.677952	27.654132
256.720156	7519.166595	27.659149
256.634296	7517.207058	27.664167
256.837832	7528.369923	27.669184
257.286236	7531.873497	27.674202
257.596119	7523.089725	27.679220
257.513184	7540.068423	27.684237
257.853542	7542.989099	27.689255
258.126819	7558.696576	27.694272
258.266561	7560.688959	27.699290
259.071743	7570.138071	27.704308
259.186527	7577.813777	27.709325
259.230169	7582.252094	27.714343
259.297669	7577.436712	27.719360
259.530213	7595.764585	27.724378
259.838268	7603.252176	27.729396
259.536498	7602.522951	27.734413
259.990216	7611.654617	27.739431
260.102184	7637.571880	27.744448
260.439939	7648.271814	27.749466
260.519326	7666.055490	27.754484
260.548314	7691.038728	27.759501
261.250737	7696.393585	27.764519
261.438474	7703.477027	27.769536
261.465661	7726.721086	27.774554
262.000808	7733.914282	27.779572
262.171088	7749.202389	27.784589
262.572927	7755.257853	27.789607
262.803170	7775.417333	27.794624
263.043969	7786.432452	27.799642
263.617751	7780.899989	27.804660
263.589347	7802.710095	27.809677
263.861111	7815.905040	27.814695
263.904917	7819.162662	27.819712
264.115319	7843.748316	27.824730
264.679750	7841.538495	27.829748
264.532290	7866.180239	27.834765
264.911814	7876.914804	27.839783
265.058034	7893.955798	27.844800
265.340827	7912.664430	27.849818
265.776798	7922.698788	27.854836
265.768607	7936.136568	27.859853
266.565994	7956.538892	27.864871
267.124766	7964.593509	27.869888
267.100310	7987.909127	27.874906
267.375727	7989.321506	27.879924
267.390791	8000.485768	27.884941
267.820520	8014.038114	27.889959
268.363643	8026.900253	27.894976
268.337989	8044.918585	27.899994
269.109548	8050.752063	27.905012
269.269586	8064.311965	27.910029
269.616002	8067.980001	27.915047
269.873876	8088.031311	27.920064
269.676429	8099.165782	27.925082
270.024567	8102.811456	27.930100
269.997870	8118.001286	27.935117
270.449029	8129.735042	27.940135
271.101194	8129.468833	27.945152
270.876277	8154.296733	27.950170
271.831364	8167.290175	27.955188
271.755470	8184.277833	27.960205
271.748151	8195.332064	27.965223
272.151807	8204.632880	27.970240
272.703149	8219.031369	27.975258
273.261003	8226.821050	27.980276
273.357279	8233.063451	27.985293
273.715245	8242.927092	27.990311
274.067647	8250.455357	27.995328
274.179324	8267.142198	28.000346
274.671355	8265.325679	28.005364
275.029904	8275.950108	28.010381
275.033487	8271.823335	28.015399
275.233414	8280.199502	28.020416
275.911872	8300.043088	28.025434
276.027056	8306.083654	28.030452
276.233467	8314.316750	28.035469
276.334699	8329.458300	28.040487
276.770429	8332.758802	28.045504
276.771042	8355.089095	28.050522
277.384360	8355.624563	28.055540
277.613891	8358.865815	28.060557
277.527708	8378.049459	28.065575
277.735607	8380.318553	28.070592
278.148155	8402.634887	28.075610
278.459747	8408.025923	28.080628
278.857248	8416.841614	28.085645
279.298507	8432.390923	28.090663
279.368497	8440.989573	28.095680
279.149929	8434.933829	28.100698
279.592071	8451.711140	28.105716
280.287536	8471.122877	28.110733
280.552009	8475.656259	28.115751
280.824999	8482.174147	28.120768
280.739571	8500.060215	28.125786
281.624515	8507.470435	28.130804
281.332466	8513.518033	28.135821
281.918746	8530.973723	28.140839
282.181870	8522.392548	28.145856
282.107240	8545.180014	28.150874
282.285614	8546.241409	28.155892
282.438074	8554.890336	28.160909
282.792351	8574.731331	28.165927
283.330741	8588.595422	28.170944
283.509463	8597.937987	28.175962
283.910084	8616.780420	28.180980
284.288272	8620.004745	28.185997
284.497118	8633.004917	28.191015
285.015303	8640.270585	28.196032
285.390052	8660.638868	28.201050
285.438429	8686.393921	28.206068
285.651716	8687.734000	28.211085
285.536014	8689.864395	28.216103
286.239147	8695.055265	28.221120
286.702554	8726.399859	28.226138
286.529505	8730.591407	28.231156
286.804545	8752.263540	28.236173
287.409756	8766.941324	28.241191
287.893209	8770.594350	28.246208
287.991359	8776.524080	28.251226
288.050608	8797.207140	28.256244
288.619784	8814.290072	28.261261
288.943809	8824.768680	28.266279
289.071850	8839.950649	28.271296
289.350029	8863.046317	28.276314
289.954125	8864.580924	28.281332
290.021131	8880.438656	28.286349
290.122927	8891.046831	28.291367
290.577949	8902.205863	28.296384
290.954172	8914.305466	28.301402
291.429782	8930.029775	28.306420
291.501079	8939.657704	28.311437
291.902117	8955.561049	28.316455
292.416339	8969.725993	28.321472
292.407898	8981.955356	28.326490
292.926916	8983.752721	28.331508
293.187922	8993.543551	28.336525
293.318468	9005.002895	28.341543
294.144224	9011.649073	28.346560
293.856910	9027.208825	28.351578
293.947917	9031.829505	28.356596
294.297349	9052.211657	28.361613
294.293248	9060.462277	28.366631
294.971740	9082.084225	28.371648
295.653719	9097.593230	28.376666
296.290966	9101.474811	28.381684
296.577152	9108.792794	28.386701
296.566220	9127.498152	28.391719
297.071779	9124.176586	28.396736
297.072923	9128.135716	28.401754
297.145895	9140.614482	28.406772
297.712944	9149.823879	28.411789
297.719231	9159.739944	28.416807
298.347071	9174.114569	28.421824
298.409722	9185.436269	28.426842
298.731821	9195.741741	28.431860
299.001488	9200.410251	28.436877
299.288485	9226.419141	28.441895
299.262317	9225.795066	28.446912
299.194014	9249.169656	28.451930
299.708660	9263.382118	28.456948
300.220782	9278.797907	28.461965
300.189075	9295.665999	28.466983
300.854473	9311.458779	28.472000
301.244712	9330.193060	28.477018
301.420135	9336.549727	28.482036
301.655948	9334.340698	28.487053
301.720318	9358.256639	28.492071
302.069494	9365.075477	28.497088
302.560061	9384.712868	28.502106
302.840825	9401.611040	28.507124
303.182396	9409.324600	28.512141
303.113212	9427.190072	28.517159
303.506898	9447.802525	28.522176
303.520597	9467.262119	28.527194
304.081587	9487.772634	28.532212
304.685258	9505.428589	28.537229
304.767908	9520.359325	28.542247
305.413643	9535.328161	28.547264
305.620748	9553.993479	28.552282
306.103594	9564.299234	28.557300
306.197995	9571.120170	28.562317
306.780251	9597.847402	28.567335
307.009246	9607.151029	28.572352
307.640560	9625.753125	28.577370
307.637964	9616.032230	28.582388
308.531074	9637.715929	28.587405
308.378182	9649.434769	28.592423
309.167403	9655.111289	28.597440
308.917048	9664.894172	28.602458
309.066529	9675.271154	28.607476
309.909643	9688.592637	28.612493
309.770007	9704.148764	28.617511
310.665107	9708.406854	28.622528
310.743836	9722.422736	28.627546
310.676169	9742.381596	28.632564
311.136777	9743.537774	28.637581
311.423296	9755.364661	28.642599
312.069253	9764.375721	28.647616
312.307601	9780.207382	28.652634
312.421489	9795.941730	28.657652
312.936838	9807.537048	28.662669
312.894036	9821.796215	28.667687
313.397041	9837.564366	28.672704
313.937223	9846.740432	28.677722
313.974184	9864.779139	28.682740
314.405546	9855.615301	28.687757
314.531399	9875.209307	28.692775
315.046654	9891.708096	28.697792
315.253222	9904.415880	28.702810
315.815896	9911.368818	28.707828
315.701299	9927.499010	28.712845
315.970043	9944.109080	28.717863
316.729163	9950.627115	28.722880
317.043039	9973.806980	28.727898
317.030209	9993.744889	28.732916
317.041605	9991.520419	28.737933
317.356870	10015.344227	28.742951
318.218225	10038.214237	28.747968
318.097615	10043.067234	28.752986
318.639871	10062.444655	28.758004
318.936281	10068.406889	28.763021
319.128382	10100.437257	28.768039
319.503447	10111.120146	28.773056
319.817026	10134.262369	28.778074
320.497846	10149.065178	28.783092
320.538491	10151.616443	28.788109
320.783554	10164.940387	28.793127
321.297539	10172.257839	28.798144
321.762133	10181.098596	28.803162
321.982557	10200.952827	28.808180
322.715731	10193.787561	28.813197
322.575833	10205.788883	28.818215
322.948396	10219.563351	28.823232
323.017157	10221.248243	28.828250
323.585680	10229.804361	28.833268
323.943073	10242.286674	28.838285
323.755566	10261.860710	28.843303
324.146524	10267.710317	28.848320
324.730643	10286.121551	28.853338
324.807444	10301.227490	28.858356
325.559706	10318.327336	28.863373
325.747163	10333.153898	28.868391
325.666023	10350.122254	28.873408
325.647332	10362.755125	28.878426
326.246937	10386.118083	28.883444
326.942233	10400.445206	28.888461
326.906344	10414.981601	28.893479
327.234275	10428.684278	28.898496
328.025934	10442.469042	28.903514
327.998892	10464.108398	28.908532
328.374919	10480.812654	28.913549
328.492350	10502.947250	28.918567
328.892157	10514.204314	28.923584
329.379874	10541.181366	28.928602
329.865260	10561.278650	28.933620
330.014467	10565.398026	28.938637
330.203082	10590.745374	28.943655
330.571961	10613.415378	28.948672
330.831410	10622.152707	28.953690
331.182131	10642.236440	28.958708
332.083045	10653.882404	28.963725
332.023690	10680.718013	28.968743
332.725984	10692.635085	28.973760
333.196299	10704.841105	28.978778
332.936596	10719.362274	28.983796
333.574269	10736.540449	28.988813
333.451807	10763.461841	28.993831
334.217900	10773.919669	28.998848
334.588843	10800.602792	29.003866
335.080872	10816.420857	29.008884
335.785671	10821.640493	29.013901
335.608976	10831.538746	29.018919
336.183066	10846.137803	29.023936
336.441566	10865.554193	29.028954
336.609005	10880.889532	29.033972
337.156873	10892.357292	29.038989
337.359180	10910.216388	29.044007
337.890625	10919.902721	29.049024
338.159286	10935.888493	29.054042
338.512538	10946.234264	29.059060
339.431637	10962.626539	29.064077
339.560187	10971.090884	29.069095
339.637420	10974.015437	29.074112
340.237793	10986.311784	29.079130
339.996818	11003.975171	29.084148
340.546490	11018.054032	29.089165
340.859793	11032.627776	29.094183
340.966373	11048.263282	29.099200
341.860081	11051.754619	29.104218
342.279719	11075.784463	29.109236
342.387175	11080.049427	29.114253
342.497390	11098.463074	29.119271
342.520633	11112.526582	29.124288
343.227056	11127.809272	29.129306
343.294796	11148.866207	29.134324
343.775387	11160.669902	29.139341
344.169008	11174.744907	29.144359
344.599246	11188.274238	29.149376
344.564169	11204.816191	29.154394
344.968918	11219.940968	29.159412
345.175183	11236.100966	29.164429
345.618760	11247.329514	29.169447
345.568762	11276.823215	29.174464
346.116054	11289.068081	29.179482
346.142179	11308.912876	29.184500
346.707443	11331.606668	29.189517
347.006694	11341.168554	29.194535
347.837870	11357.754935	29.199552
348.294275	11377.974470	29.204570
348.494796	11394.299700	29.209588
348.926623	11395.264724	29.214605
349.242478	11422.080512	29.219623
349.574113	11434.656073	29.224640
349.945977	11442.668867	29.229658
350.232644	11473.133215	29.234676
350.775518	11476.496447	29.239693
351.008009	11500.079346	29.244711
351.506263	11517.857930	29.249728
351.702382	11527.173981	29.254746
352.083294	11546.177196	29.259764
352.452087	11553.072709	29.264781
353.083283	11580.559274	29.269799
353.273019	11586.181890	29.274816
353.194771	11604.398203	29.279834
353.817357	11624.737227	29.284852
354.035928	11639.822037	29.289869
354.435413	11661.026515	29.294887
354.897063	11679.341476	29.299904
355.301304	11694.886687	29.304922
355.331149	11717.128010	29.309940
355.987010	11733.145385	29.314957
356.499332	11750.609375	29.319975
356.896532	11773.402656	29.324992
357.136978	11776.601751	29.330010
357.438349	11800.771042	29.335028
357.869087	11807.375911	29.340045
358.440501	11832.595508	29.345063
358.396287	11840.894688	29.350080
358.850605	11869.830350	29.355098
359.265091	11877.944018	29.360116
360.095428	11881.565437	29.365133
360.107165	11906.459141	29.370151
360.210840	11926.857671	29.375168
361.147201	11939.727247	29.380186
361.209875	11957.034507	29.385204
361.996995	11961.584767	29.390221
362.166982	11982.563466	29.395239
362.399873	11998.748370	29.400256
362.878227	12005.930031	29.405274
363.355745	12012.006619	29.410292
363.936532	12023.002574	29.415309
364.270803	12035.274984	29.420327
364.067216	12049.516822	29.425344
364.871692	12064.276525	29.430362
364.578154	12080.742897	29.435380
365.368045	12092.179801	29.440397
365.979060	12100.676447	29.445415
365.987560	12120.499596	29.450432
366.565166	12115.852605	29.455450
366.706578	12142.033618	29.460468
366.840459	12157.618405	29.465485
367.250820	12176.797639	29.470503
367.597598	12197.849933	29.475520
368.557997	12202.272063	29.480538
368.358734	12224.534084	29.485556
368.513479	12230.465521	29.490573
369.324797	12245.906375	29.495591
369.415962	12248.787894	29.500608
369.787597	12275.299332	29.505626
369.634892	12289.539697	29.510644
370.072382	12311.989438	29.515661
370.552439	12333.336786	29.520679
371.023819	12343.175370	29.525696
371.338272	12364.532905	29.530714
371.424089	12385.594709	29.535732
371.958793	12405.632567	29.540749
372.355293	12424.545812	29.545767
372.676051	12449.334987	29.550784
373.259119	12468.657988	29.555802
373.367467	12501.536081	29.560820
373.817631	12517.898972	29.565837
374.320903	12533.460945	29.570855
374.905477	12566.030877	29.575872
375.608975	12570.089135	29.580890
375.460275	12594.699411	29.585908
376.035781	12611.844840	29.590925
376.173944	12640.262800	29.595943
376.700939	12662.916831	29.600960
377.355145	12675.764798	29.605978
377.440013	12688.253539	29.610996
378.137533	12705.569412	29.616013
378.150384	12710.920078	29.621031
378.503867	12738.489733	29.626048
379.108584	12764.156938	29.631066
379.464520	12781.479018	29.636084
379.833742	12804.517929	29.641101
380.536520	12812.618424	29.646119
380.878218	12842.596373	29.651136
381.106561	12852.103823	29.656154
381.576765	12878.032251	29.661172
381.739455	12883.918439	29.666189
382.233454	12906.950562	29.671207
382.738142	12934.695767	29.676224
383.033799	12938.517991	29.681242
383.530009	12963.548781	29.686260
383.883356	12980.078818	29.691277
384.445801	12996.452959	29.696295
384.714987	13013.021471	29.701312
385.237540	13026.433459	29.706330
385.160164	13040.529957	29.711348
385.475812	13066.176537	29.716365
386.927382	13079.559887	29.721383
386.647563	13089.904952	29.726400
387.160682	13107.654293	29.731418
387.640340	13118.982526	29.736436
387.790288	13129.408717	29.741453
388.648821	13150.874553	29.746471
388.631983	13171.981734	29.751488
389.343216	13182.484249	29.756506
389.452339	13200.789596	29.761524
389.826457	13210.653344	29.766541
390.696384	13218.974154	29.771559
390.691245	13231.009978	29.776576
391.008827	13247.460587	29.781594
391.001037	13271.212816	29.786612
391.382272	13289.305097	29.791629
391.973182	13302.254988	29.796647
392.334022	13331.415964	29.801664
392.901648	13344.107421	29.806682
393.239800	13357.918011	29.811700
393.183376	13379.716901	29.816717
393.907919	13402.978787	29.821735
394.206883	13412.197556	29.826752
394.285468	13420.588723	29.831770
395.057301	13454.277200	29.836788
395.480598	13471.017769	29.841805
395.768698	13479.515095	29.846823
395.968207	13505.240464	29.851840
396.478258	13514.419903	29.856858
396.427637	13537.443364	29.861876
397.019447	13553.115474	29.866893
397.760956	13569.421011	29.871911
397.588849	13597.402677	29.876928
398.406829	13614.741574	29.881946
399.048004	13635.840943	29.886964
399.047332	13656.264001	29.891981
399.790495	13678.686439	29.896999
400.044229	13704.390952	29.902016
400.648549	13711.960923	29.907034
401.095559	13733.052917	29.912052
401.047758	13757.917330	29.917069
401.625648	13773.872868	29.922087
402.245779	13794.527270	29.927104
402.837339	13815.227225	29.932122
403.084703	13831.439856	29.937140
403.336525	13851.141438	29.942157
404.175416	13866.910903	29.947175
404.213484	13891.547294	29.952192
404.848550	13898.174584	29.957210
405.341685	13917.282621	29.962228
405.634070	13946.966871	29.967245
405.989404	13953.404300	29.972263
406.039162	13974.764061	29.977280
406.595974	13992.058946	29.982298
407.132717	14021.054475	29.987316
407.057403	14039.351624	29.992333
407.626090	14058.994316	29.997351
408.372958	14082.629353	30.002368
408.784112	14101.260914	30.007386
409.207143	14127.792165	30.012404
409.783936	14146.419932	30.017421
410.273512	14156.206087	30.022439
410.570862	14178.329450	30.027456
410.819456	14191.033552	30.032474
411.458811	14211.581182	30.037492
411.679617	14243.721478	30.042509
412.444886	14244.700752	30.047527
413.044213	14276.664964	30.052544
413.199125	14277.847220	30.057562
413.820677	14294.879592	30.062580
414.241184	14319.210300	30.067597
414.619401	14325.467418	30.072615
415.267938	14343.932552	30.077632
415.316596	14348.463275	30.082650
415.801325	14359.204048	30.087668
415.907435	14377.580480	30.092685
416.231018	14387.247481	30.097703
416.477299	14413.361521	30.102720
417.277413	14424.463488	30.107738
418.105181	14442.929068	30.112756
418.040241	14469.129830	30.117773
418.705975	14477.817948	30.122791
419.113732	14501.579263	30.127808
419.424416	14515.240251	30.132826
419.701029	14523.045053	30.137844
420.162898	14540.390050	30.142861
420.736454	14565.344523	30.147879
421.016661	14586.498334	30.152896
421.391925	14597.404822	30.157914
421.968391	14622.750527	30.162932
422.272152	14639.574016	30.167949
422.879215	14644.794255	30.172967
422.705072	14659.055543	30.177984
423.536988	14669.701055	30.183002
423.599880	14678.919520	30.188020
423.497411	14704.889620	30.193037
424.163727	14725.926261	30.198055
424.547205	14750.575982	30.203072
424.641773	14776.218446	30.208090
425.496532	14797.873081	30.213108
425.678374	14826.274841	30.218125
426.208451	14846.252849	30.223143
426.795581	14876.394538	30.228160
426.931738	14899.494610	30.233178
427.410179	14913.031702	30.238196
427.870898	14948.113808	30.243213
428.331149	14971.516924	30.248231
428.727650	15002.219253	30.253248
429.154137	15026.635201	30.258266
429.736696	15058.878122	30.263284
430.112667	15076.748698	30.268301
430.384711	15100.566758	30.273319
431.172079	15128.510923	30.278336
431.566817	15153.983706	30.283354
432.028934	15181.157747	30.288372
432.468846	15197.132938	30.293389
433.109902	15216.992889	30.298407
433.532196	15236.770269	30.303424
434.002973	15263.744100	30.308442
434.449179	15286.391817	30.313460
434.807625	15312.167374	30.318477
435.389635	15331.427144	30.323495
436.085327	15364.808794	30.328512
436.338445	15371.528014	30.333530
436.869124	15397.636754	30.338548
437.295302	15419.501351	30.343565
437.921620	15429.727858	30.348583
437.739342	15457.878075	30.353600
438.564404	15480.653022	30.358618
439.154925	15489.331280	30.363636
439.434226	15522.835277	30.368653
440.213955	15537.898466	30.373671
440.045407	15557.408674	30.378688
440.458289	15571.654494	30.383706
441.227754	15601.481362	30.388724
441.623647	15626.825103	30.393741
441.819546	15652.812921	30.398759
442.528739	15674.854564	30.403776
442.876835	15686.283900	30.408794
443.337942	15704.839724	30.413812
443.722186	15727.608212	30.418829
444.623396	15745.943541	30.423847
444.845980	15769.691223	30.428864
445.430518	15787.166585	30.433882
445.730252	15808.056547	30.438900
445.818169	15834.405786	30.443917
446.693006	15849.466959	30.448935
446.912341	15873.941705	30.453952
447.356869	15903.001919	30.458970
447.741011	15918.291607	30.463988
448.414308	15939.871738	30.469005
448.759153	15963.812123	30.474023
449.457152	15977.277682	30.479040
450.082976	16005.472682	30.484058
450.292330	16020.186574	30.489076
450.780213	16039.986097	30.494093
451.196315	16055.327740	30.499111
451.178963	16075.746522	30.504128
451.850722	16094.651897	30.509146
452.630599	16111.019942	30.514164
452.554269	16128.965505	30.519181
452.951412	16143.087880	30.524199
453.342628	16162.220452	30.529216
453.832204	16177.582268	30.534234
454.389765	16187.033506	30.539252
454.667595	16213.470381	30.544269
455.356471	16231.751001	30.549287
455.420089	16263.069694	30.554304
456.159648	16289.728089	30.559322
456.493326	16306.084069	30.564340
456.759478	16336.632083	30.569357
457.368080	16367.019119	30.574375
457.961932	16387.336183	30.579392
458.313968	16408.695535	30.584410
459.119179	16421.512924	30.589428
459.131023	16453.061129	30.594445
459.710658	16469.309238	30.599463
460.034839	16498.894561	30.604480
460.400352	16529.247285	30.609498
461.182025	16557.712426	30.614516
461.218575	16582.633625	30.619533
461.925128	16606.894018	30.624551
462.350312	16635.140322	30.629568
462.931774	16657.379981	30.634586
463.610321	16684.184296	30.639604
463.943947	16722.492287	30.644621
464.408561	16746.973947	30.649639
464.964763	16765.623293	30.654656
465.349438	16791.042977	30.659674
465.992912	16812.710885	30.664692
466.586242	16840.545813	30.669709
467.046644	16868.543736	30.674727
467.473579	16889.247549	30.679744
468.137799	16906.234514	30.684762
468.637207	16923.187296	30.689780
468.993768	16954.578096	30.694797
469.617635	16969.704733	30.699815
470.037174	16985.744623	30.704832
470.778065	16998.086056	30.709850
471.022030	17019.355623	30.714868
471.465317	17037.536501	30.719885
472.039519	17063.656489	30.724903
472.304411	17091.208414	30.729920
472.840521	17104.093679	30.734938
473.336253	17126.498921	30.739956
473.628702	17159.056137	30.744973
474.063683	17176.960493	30.749991
474.707852	17201.578855	30.755008
474.664221	17228.130646	30.760026
475.700787	17254.380623	30.765044
476.110924	17283.047170	30.770061
476.435293	17303.116820	30.775079
477.163315	17324.134024	30.780096
477.126150	17351.657825	30.785114
477.943398	17375.219590	30.790132
478.240738	17407.422694	30.795149
478.798777	17421.410257	30.800167
479.634390	17447.407697	30.805184
480.122513	17474.369285	30.810202
480.419242	17485.125475	30.815220
481.081880	17514.138171	30.820237
481.031157	17531.765162	30.825255
482.079517	17549.902292	30.830272
482.218580	17577.973687	30.835290
483.160252	17589.993459	30.840308
483.445570	17616.949108	30.845325
484.013225	17630.562596	30.850343
484.494353	17643.084113	30.855360
484.723926	17660.225106	30.860378
484.990345	17675.774691	30.865396
485.103025	17701.847801	30.870413
485.853773	17724.548617	30.875431
486.332751	17746.085408	30.880448
486.628798	17764.214226	30.885466
487.381280	17784.741666	30.890484
487.849691	17810.733936	30.895501
488.601365	17843.157205	30.900519
489.187801	17855.611827	30.905536
489.003585	17872.356649	30.910554
490.104202	17904.169435	30.915572
490.257798	17921.373099	30.920589
490.728330	17939.285230	30.925607
491.148272	17959.321641	30.930624
491.720701	17992.531327	30.935642
492.295267	18010.559896	30.940660
492.526992	18047.594558	30.945677
493.213805	18072.845417	30.950695
493.741096	18088.727206	30.955712
494.361173	18124.008105	30.960730
494.534425	18153.041554	30.965748
495.608209	18178.036099	30.970765
496.000906	18195.884849	30.975783
496.338583	18214.013886	30.980800
496.570318	18246.759333	30.985818
497.350905	18270.852292	30.990836
497.770236	18299.626304	30.995853
498.456142	18322.666492	31.000871
499.263961	18346.016126	31.005888
499.501662	18370.901805	31.010906
500.278893	18389.107465	31.015924
500.678623	18411.522919	31.020941
501.354755	18430.382528	31.025959
501.592340	18448.445332	31.030976
501.630518	18483.824344	31.035994
502.411199	18496.217369	31.041012
502.802943	18534.188173	31.046029
503.231795	18557.426842	31.051047
504.146618	18591.259914	31.056064
504.598236	18611.336263	31.061082
505.237581	18631.263194	31.066100
505.241894	18668.473647	31.071117
505.963632	18678.317368	31.076135
506.832302	18699.851046	31.081152
507.444227	18737.402384	31.086170
508.057116	18752.273117	31.091188
508.375487	18781.455354	31.096205
508.541998	18800.035034	31.101223
509.095866	18817.625358	31.106240
509.303408	18850.217669	31.111258
509.952468	18866.794928	31.116276
510.663603	18892.959120	31.121293
511.009630	18917.765356	31.126311
511.648435	18943.309170	31.131328
512.114009	18976.594138	31.136346
512.561430	18995.047876	31.141364
513.177887	19027.639616	31.146381
513.622270	19050.889078	31.151399
514.084710	19070.553551	31.156416
514.551345	19108.576925	31.161434
515.483250	19129.968504	31.166452
515.978019	19152.388881	31.171469
516.366598	19175.350296	31.176487
516.967242	19206.851829	31.181504
517.111121	19218.713273	31.186522
517.672341	19235.986934	31.191540
518.112275	19261.524407	31.196557
518.598678	19287.850686	31.201575
519.162352	19302.363114	31.206592
519.605796	19327.521052	31.211610
520.116335	19344.101462	31.216628
520.304689	19380.216726	31.221645
520.589512	19402.499690	31.226663
521.397644	19429.691867	31.231680
522.400324	19464.100267	31.236698
522.532405	19484.802496	31.241716
523.453461	19519.198506	31.246733
523.584405	19548.594468	31.251751
524.095778	19566.950281	31.256768
524.229266	19597.893818	31.261786
525.301327	19636.088753	31.266804
525.906469	19658.012260	31.271821
526.168844	19692.682325	31.276839
526.704083	19719.172124	31.281856
527.334431	19743.119858	31.286874
527.692590	19768.121136	31.291892
528.453824	19800.362957	31.296909
528.849905	19837.691184	31.301927
529.953545	19859.644248	31.306944
530.274610	19881.163917	31.311962
530.735582	19914.760793	31.316980
531.294742	19947.363046	31.321997
531.857551	19969.887433	31.327015
532.918728	19991.847298	31.332032
533.134121	20024.415068	31.337050
533.349543	20045.370198	31.342068
534.335850	20073.919035	31.347085
534.550362	20097.553246	31.352103
535.426180	20118.752520	31.357120
535.857978	20145.025328	31.362138
536.655479	20160.013544	31.367156
537.535786	20185.735982	31.372173
537.220332	20222.614069	31.377191
538.274831	20229.740199	31.382208
538.562085	20262.840473	31.387226
538.972903	20285.717575	31.392244
539.829125	20307.842580	31.397261
540.055608	20328.733099	31.402279
540.698677	20353.437775	31.407296
541.306123	20381.553580	31.412314
541.948013	20412.690462	31.417332
542.206531	20427.087250	31.422349
542.664027	20461.488025	31.427367
543.604550	20483.258840	31.432384
543.984650	20509.597099	31.437402
544.541622	20548.152497	31.442420
545.196973	20569.298336	31.447437
545.530538	20596.686515	31.452455
546.658054	20601.046576	31.457472
546.970017	20625.632860	31.462490
547.489682	20655.355017	31.467508
548.226259	20663.023931	31.472525
548.375947	20696.702493	31.477543
549.362612	20717.202680	31.482560
549.762958	20737.958994	31.487578
550.165339	20769.197138	31.492596
550.914881	20792.691527	31.497613
550.887851	20822.613292	31.502631
551.457061	20836.949084	31.507648
552.338541	20868.598865	31.512666
552.398905	20887.885856	31.517684
552.972526	20929.149982	31.522701
553.430233	20951.413952	31.527719
553.893217	20974.466922	31.532736
554.510873	21005.362124	31.537754
554.956019	21033.921301	31.542772
555.903762	21049.505879	31.547789
556.040716	21096.468470	31.552807
556.906215	21098.481310	31.557824
557.322624	21122.243096	31.562842
557.776219	21153.821346	31.567860
558.585629	21189.267694	31.572877
558.752950	21215.949831	31.577895
559.192546	21243.429721	31.582912
559.741805	21280.168039	31.587930
560.269838	21303.072200	31.592948
560.916016	21343.100039	31.597965
561.286524	21377.136930	31.602983
562.045265	21406.506855	31.608000
562.747971	21446.930439	31.613018
563.491377	21478.944031	31.618036
564.192629	21513.081003	31.623053
564.108154	21536.106639	31.628071
564.940139	21571.189980	31.633088
565.406463	21603.247171	31.638106
566.440823	21628.277607	31.643124
567.121170	21665.293087	31.648141
567.331178	21701.864172	31.653159
568.106657	21725.418803	31.658176
568.720295	21765.300949	31.663194
569.562963	21798.752808	31.668212
570.079818	21810.892297	31.673229
570.485119	21847.938560	31.678247
571.257692	21870.267994	31.683264
571.856823	21901.300198	31.688282
572.360178	21934.457901	31.693300
573.105639	21948.311955	31.698317
573.750065	21972.670929	31.703335
574.318856	21993.547518	31.708352
575.030417	22028.555754	31.713370
575.125644	22061.398465	31.718388
575.891897	22084.632715	31.723405
576.403183	22123.356325	31.728423
576.915261	22144.444156	31.733440
577.733566	22170.614908	31.738458
577.897637	22210.896941	31.743476
578.575410	22229.172321	31.748493
579.124696	22266.828700	31.753511
580.015961	22292.653290	31.758528
580.446280	22329.367959	31.763546
581.419562	22362.414870	31.768564
582.225965	22385.030257	31.773581
582.361095	22415.775764	31.778599
582.797451	22429.084595	31.783616
583.715511	22453.584555	31.788634
584.356330	22486.727975	31.793652
584.670380	22516.257665	31.798669
585.034512	22549.014838	31.803687
585.775867	22571.179346	31.808704
586.099837	22609.130741	31.813722
586.771904	22639.091100	31.818740
587.666178	22660.896856	31.823757
588.000052	22698.524604	31.828775
588.587984	22726.375103	31.833792
589.259115	22747.735660	31.838810
590.008863	22780.761409	31.843828
590.495160	22812.387743	31.848845
591.371930	22836.483911	31.853863
591.916986	22861.055433	31.858880
592.662088	22882.846883	31.863898
593.176626	22901.458082	31.868916
594.102288	22914.279872	31.873933
594.338426	22937.617108	31.878951
594.755536	22946.872482	31.883968
595.299164	22978.174150	31.888986
596.203264	23004.812820	31.894004
596.707387	23025.650076	31.899021
596.907351	23043.634537	31.904039
597.295274	23065.678019	31.909056
597.948808	23095.749397	31.914074
598.701567	23123.467216	31.919092
599.240326	23152.968981	31.924109
599.630262	23183.840068	31.929127
600.502160	23201.283419	31.934144
601.191965	23224.126560	31.939162
601.483548	23255.404948	31.944180
602.160511	23294.521963	31.949197
602.523295	23325.334331	31.954215
603.195707	23360.502716	31.959232
603.700795	23383.728843	31.964250
604.458070	23412.735472	31.969268
604.991632	23438.750285	31.974285
605.634431	23481.140042	31.979303
606.500696	23508.619450	31.984320
607.387287	23540.411745	31.989338
607.625986	23576.217167	31.994356
608.313198	23607.939687	31.999373
608.961959	23638.214851	32.004391
609.492321	23655.882712	32.009408
610.004341	23701.674226	32.014426
610.287702	23728.872393	32.019444
611.221944	23763.450706	32.024461
611.716070	23812.284859	32.029479
612.305111	23845.773583	32.034496
613.091395	23870.782525	32.039514
613.212610	23915.706794	32.044532
614.275128	23945.532146	32.049549
615.183084	23978.130672	32.054567
615.608462	24015.259990	32.059584
616.204236	24044.084293	32.064602
616.609520	24094.430744	32.069620
617.651959	24121.207234	32.074637
617.996192	24155.783840	32.079655
618.455531	24180.882292	32.084672
619.412904	24224.304986	32.089690
620.156561	24260.121024	32.094708
620.968252	24287.907072	32.099725
621.073763	24320.145232	32.104743
622.065786	24352.528982	32.109760
622.598979	24383.663869	32.114778
622.976895	24425.187110	32.119796
624.071676	24459.324403	32.124813
624.422178	24488.668044	32.129831
625.114517	24520.751428	32.134848
625.944658	24553.002868	32.139866
626.548676	24584.461912	32.144884
627.041664	24619.167692	32.149901
627.713791	24648.018828	32.154919
628.356694	24677.512860	32.159936
629.235816	24704.751764	32.164954
629.501112	24739.449174	32.169972
630.299198	24762.624704	32.174989
630.770666	24805.277931	32.180007
631.407046	24830.494824	32.185024
632.466447	24866.546885	32.190042
632.543603	24900.698951	32.195060
633.442402	24918.386068	32.200077
634.163926	24956.829481	32.205095
634.759539	24990.805710	32.210112
635.282442	25013.259945	32.215130
635.810793	25043.663533	32.220148
636.556977	25061.709622	32.225165
636.921940	25080.807625	32.230183
637.542656	25114.697977	32.235200
638.433265	25141.746087	32.240218
639.011256	25169.456207	32.245236
639.726739	25198.825886	32.250253
640.220887	25227.642533	32.255271
640.685028	25253.310358	32.260288
641.197040	25271.671380	32.265306
641.894434	25317.538678	32.270324
642.729307	25343.685740	32.275341
643.457842	25374.601982	32.280359
643.555798	25404.207708	32.285376
644.293663	25444.520162	32.290394
644.839522	25484.925966	32.295412
645.471222	25525.166730	32.300429
646.484715	25555.337121	32.305447
646.908874	25597.190497	32.310464
647.446093	25626.626640	32.315482
647.805770	25668.970575	32.320500
648.835835	25702.854692	32.325517
649.984539	25738.654181	32.330535
650.608519	25772.955928	32.335552
651.533311	25805.851837	32.340570
651.858617	25842.222857	32.345588
652.766310	25869.073356	32.350605
652.979989	25910.498989	32.355623
654.198066	25935.228016	32.360640
654.875452	25967.246538	32.365658
655.365526	25996.583166	32.370676
655.899799	26031.316522	32.375693
656.419175	26065.868990	32.380711
656.926023	26106.636072	32.385728
657.774710	26132.055195	32.390746
658.085335	26170.615841	32.395764
659.438815	26200.417955	32.400781
659.944625	26232.571210	32.405799
660.417490	26267.870757	32.410816
661.367843	26295.998123	32.415834
661.897838	26339.321687	32.420852
662.338563	26370.385656	32.425869
663.368912	26410.926006	32.430887
663.894034	26450.945146	32.435904
664.874354	26478.063171	32.440922
665.212537	26512.499417	32.445940
665.911374	26541.740942	32.450957
666.876524	26584.655596	32.455975
667.561099	26614.379794	32.460992
668.246719	26649.943739	32.466010
668.710954	26682.843686	32.471028
669.137654	26705.586647	32.476045
670.251656	26739.509928	32.481063
670.842564	26779.272927	32.486080
671.467115	26802.294704	32.491098
672.227701	26840.432227	32.496116
672.582734	26860.898651	32.501133
673.372725	26895.700892	32.506151
673.802732	26928.341147	32.511168
675.032140	26965.368958	32.516186
675.520988	27007.758674	32.521204
676.373866	27044.453738	32.526221
676.843391	27073.883633	32.531239
677.095290	27107.032413	32.536256
678.040118	27133.954628	32.541274
678.353500	27169.211200	32.546292
679.123938	27203.549326	32.551309
679.689727	27243.494141	32.556327
680.426683	27266.208105	32.561344
681.174743	27293.704902	32.566362
681.788820	27328.320542	32.571380
682.400545	27359.719514	32.576397
683.070418	27392.190223	32.581415
683.910548	27432.174611	32.586432
684.386667	27453.166230	32.591450
684.828144	27497.612215	32.596468
685.755859	27538.063452	32.601485
686.633228	27564.206744	32.606503
687.034159	27595.733900	32.611520
687.855390	27622.151519	32.616538
688.543058	27668.543962	32.621556
689.538267	27696.552487	32.626573
690.091909	27731.083471	32.631591
690.551106	27767.531789	32.636608
691.495530	27805.035566	32.641626
692.398632	27842.305701	32.646644
692.904083	27877.710400	32.651661
694.092917	27907.679878	32.656679
694.489719	27944.928361	32.661696
695.673692	27964.077810	32.666714
696.006439	28000.931907	32.671732
696.694997	28026.757730	32.676749
697.441673	28053.939744	32.681767
697.953364	28095.955235	32.686784
698.900877	28122.644481	32.691802
699.793766	28156.636370	32.696820
700.361273	28190.913137	32.701837
701.169778	28212.270653	32.706855
701.372869	28250.144174	32.711872
702.407299	28281.238187	32.716890
702.980713	28327.921816	32.721908
703.838351	28358.986748	32.726925
704.672279	28382.647530	32.731943
705.529668	28420.222959	32.736960
706.589051	28441.724731	32.741978
706.825719	28467.293202	32.746996
707.180495	28495.257745	32.752013
708.325588	28523.996113	32.757031
708.684682	28571.820001	32.762048
709.688420	28605.258013	32.767066
709.996213	28645.163812	32.772084
710.597199	28672.521167	32.777101
711.511356	28714.424339	32.782119
712.231634	28751.465616	32.787136
712.933385	28790.437726	32.792154
713.774645	28822.220188	32.797172
714.296956	28856.151181	32.802189
715.473188	28891.458916	32.807207
715.782022	28935.726539	32.812224
716.633694	28959.777110	32.817242
717.317915	28996.141818	32.822260
718.098012	29035.045237	32.827277
718.714749	29066.939092	32.832295
719.263200	29109.241675	32.837312
719.890098	29144.597948	32.842330
720.588350	29181.200985	32.847348
721.248664	29225.136067	32.852365
722.177306	29268.593074	32.857383
722.907136	29307.606019	32.862400
723.805508	29340.284250	32.867418
724.443637	29379.773129	32.872436
724.941305	29413.354926	32.877453
725.847111	29452.820990	32.882471
726.354015	29490.857823	32.887488
726.736127	29522.921872	32.892506
728.106911	29554.230642	32.897524
728.587530	29588.510716	32.902541
729.483383	29621.783976	32.907559
729.828188	29650.927388	32.912576
730.450496	29680.969234	32.917594
731.166069	29714.283518	32.922612
731.486707	29748.709015	32.927629
732.855489	29782.161321	32.932647
733.285202	29829.376571	32.937664
734.396724	29862.591163	32.942682
735.032099	29908.516470	32.947700
735.731365	29944.703511	32.952717
736.747736	29972.446362	32.957735
737.335595	30020.231480	32.962752
737.897589	30051.838341	32.967770
738.894669	30086.051011	32.972788
739.313775	30126.871485	32.977805
740.265444	30159.586925	32.982823
740.890444	30205.735765	32.987840
741.607452	30253.829908	32.992858
742.157714	30290.502348	32.997876
742.865818	30333.490439	33.002893
743.560722	30376.316331	33.007911
744.332373	30423.119078	33.012928
745.073530	30454.647929	33.017946
745.935092	30501.386202	33.022964
746.646085	30547.623483	33.027981
747.906329	30587.131045	33.032999
748.575335	30628.659305	33.038016
749.282920	30672.735471	33.043034
749.786679	30716.976400	33.048052
750.812054	30762.425320	33.053069
751.699349	30798.457987	33.058087
752.210720	30841.629661	33.063104
753.237461	30874.517805	33.068122
754.080038	30916.025784	33.073140
754.989909	30946.144555	33.078157
755.871322	30983.910567	33.083175
756.880360	31023.534162	33.088192
757.797443	31054.467443	33.093210
758.403303	31086.954040	33.098228
758.769559	31127.721551	33.103245
759.597391	31147.346995	33.108263
760.402448	31198.817923	33.113280
760.816858	31230.702566	33.118298
761.987346	31260.724090	33.123316
762.850211	31317.224596	33.128333
763.565402	31335.053546	33.133351
764.301600	31389.506906	33.138368
765.284010	31412.629562	33.143386
766.085271	31446.672864	33.148404
766.570855	31475.076135	33.153421
767.461961	31511.134737	33.158439
768.203014	31549.909948	33.163456
768.578688	31591.808484	33.168474
769.341766	31626.825285	33.173492
769.906793	31672.057495	33.178509
770.598814	31706.067756	33.183527
771.629277	31754.211131	33.188544
772.494152	31786.639299	33.193562
773.423530	31830.632626	33.198580
773.905623	31872.913337	33.203597
774.778227	31907.047373	33.208615
775.219019	31949.872063	33.213632
775.906852	31988.441485	33.218650
776.944805	32030.875703	33.223668
777.508363	32073.093490	33.228685
778.382451	32108.150617	33.233703
779.049885	32152.185644	33.238720
780.106777	32183.775163	33.243738
780.925161	32220.124549	33.248756
781.642062	32256.312876	33.253773
782.635857	32291.130300	33.258791
783.439040	32317.190126	33.263808
783.991983	32350.249641	33.268826
784.335541	32378.233851	33.273844
785.669003	32417.948396	33.278861
786.653413	32447.577211	33.283879
787.140001	32482.651396	33.288896
787.603102	32517.558625	33.293914
788.831425	32554.811670	33.298932
789.069439	32596.114226	33.303949
790.113641	32632.839904	33.308967
790.974957	32683.698787	33.313984
791.724388	32720.262150	33.319002
792.398173	32759.619138	33.324020
793.557357	32792.066012	33.329037
793.899418	32831.007245	33.334055
794.649261	32877.483874	33.339072
795.449522	32916.992051	33.344090
796.719809	32962.135591	33.349108
797.280335	33007.965687	33.354125
798.139461	33041.414582	33.359143
798.914760	33088.444045	33.364160
799.510451	33135.103441	33.369178
800.586876	33174.360227	33.374196
801.464780	33218.927224	33.379213
802.362970	33255.721120	33.384231
803.080773	33292.840474	33.389248
803.943408	33340.324673	33.394266
805.036540	33377.290569	33.399284
805.718993	33424.480739	33.404301
806.780348	33455.799633	33.409319
807.482404	33496.373783	33.414336
808.193211	33536.807551	33.419354
809.190127	33564.589882	33.424372
810.253542	33603.400627	33.429389
811.052987	33640.387689	33.434407
811.894868	33671.159618	33.439424
813.009535	33708.223886	33.444442
813.778876	33741.789119	33.449460
814.134158	33771.082089	33.454477
815.230499	33800.891296	33.459495
816.211679	33847.574107	33.464512
816.605127	33878.340692	33.469530
817.425142	33917.531545	33.474548
818.244333	33960.522386	33.479565
818.777053	33987.081868	33.484583
819.316661	34033.733079	33.489600
820.030565	34079.421375	33.494618
821.250661	34113.188486	33.499636
822.031021	34171.720193	33.504653
823.020531	34211.030470	33.509671
823.832375	34244.115663	33.514688
824.467954	34296.461670	33.519706
825.618972	34334.058769	33.524724
826.274329	34378.580888	33.529741
827.045394	34418.880467	33.534759
828.026540	34457.180903	33.539776
828.579831	34498.595899	33.544794
829.652230	34537.659871	33.549812
830.294043	34578.865163	33.554829
830.856864	34623.737389	33.559847
831.587979	34673.673093	33.564864
832.318844	34713.612817	33.569882
833.781494	34756.687885	33.574900
834.532323	34794.866933	33.579917
835.267778	34820.719194	33.584935
835.958975	34857.289082	33.589952
836.516684	34891.414076	33.594970
837.687203	34919.733743	33.599988
837.889186	34972.143000	33.605005
839.081477	34998.733256	33.610023
840.319365	35041.527965	33.615040
840.733836	35087.796447	33.620058
841.403657	35134.790103	33.625076
842.163729	35170.622629	33.630093
843.147577	35212.679760	33.635111
843.868346	35249.536547	33.640128
844.469218	35301.985325	33.645146
845.468943	35342.320415	33.650164
846.263463	35397.173404	33.655181
847.270132	35438.430730	33.660199
848.312491	35491.272416	33.665216
848.951302	35534.749962	33.670234
850.316261	35568.540989	33.675252
850.974441	35632.027755	33.680269
851.773910	35672.312634	33.685287
852.641801	35719.592721	33.690304
853.576027	35758.326505	33.695322
854.328288	35802.159891	33.700340
855.101845	35857.213366	33.705357
856.678614	35907.342039	33.710375
857.139607	35946.599204	33.715392
857.841449	35999.552384	33.720410
858.734892	36036.086319	33.725428
859.671337	36080.517422	33.730445
860.540762	36132.521525	33.735463
861.425509	36175.753212	33.740480
862.835279	36224.928706	33.745498
863.695294	36253.121738	33.750516
864.881501	36296.059865	33.755533
865.320535	36340.474553	33.760551
866.478600	36377.334382	33.765568
867.662702	36425.375892	33.770586
868.241333	36458.791939	33.775604
869.145446	36500.023128	33.780621
869.708029	36532.316274	33.785639
870.462029	36569.372494	33.790656
871.690952	36614.644168	33.795674
872.871800	36652.322928	33.800692
873.295987	36696.026155	33.805709
874.006917	36733.285426	33.810727
875.165667	36775.311948	33.815744
875.700967	36825.548960	33.820762
876.558372	36853.717905	33.825780
877.344842	36915.930076	33.830797
878.251636	36947.170869	33.835815
879.028078	36999.653253	33.840832
880.197752	37053.338864	33.845850
881.283850	37096.035025	33.850868
881.765498	37135.695843	33.855885
882.536690	37180.913926	33.860903
883.830892	37220.131498	33.865920
884.513666	37268.329291	33.870938
885.514355	37311.235282	33.875956
886.269768	37349.234829	33.880973
887.098918	37396.278093	33.885991
888.068321	37443.893906	33.891008
889.067499	37496.077046	33.896026
890.259750	37532.819702	33.901044
890.921073	37577.227449	33.906061
891.758934	37621.253527	33.911079
893.103437	37646.185486	33.916096
893.531130	37675.681186	33.921114
894.284092	37703.854962	33.926132
894.959494	37746.932910	33.931149
895.721113	37780.531050	33.936167
896.752618	37824.957230	33.941184
897.353192	37868.483466	33.946202
898.222914	37905.233000	33.951220
899.069239	37951.478019	33.956237
899.897784	37992.553187	33.961255
900.762632	38035.216308	33.966272
901.504059	38072.580641	33.971290
902.971850	38130.237802	33.976308
904.045142	38175.220972	33.981325
904.887695	38217.268225	33.986343
905.816434	38256.127560	33.991360
906.562266	38307.878068	33.996378
907.476665	38344.343115	34.001396
908.613147	38395.077780	34.006413
909.552155	38443.668108	34.011431
910.642710	38483.147542	34.016448
911.034685	38531.197668	34.021466
911.842013	38572.998181	34.026484
913.228966	38622.239688	34.031501
913.880188	38662.996092	34.036519
914.672067	38708.916104	34.041536
915.808577	38763.970823	34.046554
917.065909	38809.622130	34.051572
917.983879	38851.481746	34.056589
918.473500	38899.188560	34.061607
919.278274	38936.727869	34.066624
920.523913	38995.946201	34.071642
921.349246	39044.062417	34.076660
922.395659	39090.474598	34.081677
923.350746	39143.927113	34.086695
924.416513	39182.317664	34.091712
925.249489	39244.560919	34.096730
926.289900	39276.859269	34.101748
927.190079	39326.298761	34.106765
927.527429	39373.233636	34.111783
928.860794	39419.013458	34.116800
929.780736	39479.346555	34.121818
931.281379	39524.063260	34.126836
932.474067	39571.395861	34.131853
932.981610	39606.497503	34.136871
933.946616	39644.721254	34.141888
934.793473	39697.515404	34.146906
936.097046	39734.143213	34.151924
936.983445	39773.707572	34.156941
937.880622	39830.326606	34.161959
938.847444	39860.038117	34.166976
939.794888	39912.001221	34.171994
940.794715	39947.778916	34.177012
941.486298	39989.284083	34.182029
942.874805	40028.985313	34.187047
943.803871	40069.707191	34.192064
944.314201	40114.093211	34.197082
945.370752	40151.633153	34.202100
946.440553	40194.641587	34.207117
947.358279	40244.137346	34.212135
948.143275	40284.161215	34.217152
949.105087	40337.293084	34.222170
950.032379	40375.833924	34.227188
950.781449	40426.178668	34.232205
951.403431	40461.978427	34.237223
952.486333	40512.954133	34.242240
953.491639	40567.717768	34.247258
954.748924	40601.305938	34.252276
955.523967	40651.432108	34.257293
956.364668	40694.211778	34.262311
957.586987	40729.140075	34.267328
958.265918	40766.044518	34.272346
959.033975	40809.152010	34.277364
959.843035	40845.112842	34.282381
960.683040	40887.608400	34.287399
961.843428	40934.708705	34.292416
962.721271	40970.823411	34.297434
963.834729	41021.940989	34.302452
964.876715	41064.164935	34.307469
965.539370	41116.301998	34.312487
966.430383	41162.142115	34.317504
967.420961	41210.047524	34.322522
968.439139	41248.664223	34.327540
969.267462	41301.515766	34.332557
970.105207	41367.274505	34.337575
971.398383	41412.735949	34.342592
972.231003	41473.107222	34.347610
973.370452	41525.120010	34.352628
974.925034	41565.386242	34.357645
975.341016	41611.598938	34.362663
976.774218	41663.003163	34.367680
977.590226	41711.386058	34.372698
978.750903	41745.889233	34.377716
979.479840	41801.553074	34.382733
980.484619	41854.441571	34.387751
981.997638	41902.228749	34.392768
982.850485	41957.203158	34.397786
983.710421	41996.933820	34.402804
985.067678	42033.683600	34.407821
985.988473	42090.715919	34.412839
986.923600	42124.243034	34.417856
988.024446	42171.481825	34.422874
989.069004	42221.695893	34.427892
990.041535	42259.385445	34.432909
990.831103	42317.431905	34.437927
991.931517	42359.788353	34.442944
993.400049	42397.198086	34.447962
993.985954	42436.789028	34.452980
995.118151	42487.907098	34.457997
995.963187	42538.886824	34.463015
996.864041	42568.979209	34.468032
997.912220	42620.414340	34.473050
999.099675	42664.035394	34.478068
1000.269042	42712.523295	34.483085
1001.065291	42763.517505	34.488103
1002.317210	42792.372452	34.493120
1003.030981	42847.231712	34.498138
1003.994805	42894.537788	34.503156
1005.191569	42931.200351	34.508173
1006.017025	42982.171519	34.513191
1007.111139	43027.863561	34.518208
1008.188604	43071.040911	34.523226
1009.048701	43119.046821	34.528244
1010.026125	43166.673933	34.533261
1010.719267	43224.446923	34.538279
1012.022431	43265.286961	34.543296
1012.874327	43309.777778	34.548314
1013.814887	43369.814775	34.553332
1015.034772	43415.064139	34.558349
1016.253587	43469.763644	34.563367
1017.026483	43508.384775	34.568384
1017.908234	43550.278057	34.573402
1019.049177	43601.568123	34.578420
1020.251074	43645.100305	34.583437
1021.022878	43697.093566	34.588455
1022.048029	43732.848190	34.593472
1023.044426	43789.221562	34.598490
1023.827573	43835.286553	34.603508
1025.224630	43863.588855	34.608525
1025.928162	43913.139083	34.613543
1027.027889	43954.271587	34.618560
1028.142441	43991.941868	34.623578
1028.945360	44031.545969	34.628596
1030.173960	44072.860929	34.633613
1030.627080	44119.926993	34.638631
1031.637782	44156.361383	34.643648
1033.110399	44204.444534	34.648666
1033.941585	44256.644875	34.653684
1034.934403	44311.717093	34.658701
1035.499225	44361.979515	34.663719
1036.660173	44413.805995	34.668736
1037.689036	44463.331816	34.673754
1039.043294	44526.368718	34.678772
1040.166123	44566.505635	34.683789
1040.883846	44628.124357	34.688807
1042.161425	44674.626048	34.693824
1043.367782	44724.978614	34.698842
1044.332273	44783.592434	34.703860
1045.474014	44825.877561	34.708877
1046.460393	44879.788282	34.713895
1047.515087	44932.258843	34.718912
1048.663932	44988.269804	34.723930
1049.406971	45041.807847	34.728948
1050.924136	45097.628578	34.733965
1052.365712	45148.438678	34.738983
1053.297557	45198.620220	34.744000
1054.578724	45248.411920	34.749018
1055.137435	45302.858724	34.754036
1056.653100	45341.600804	34.759053
1057.477802	45401.825898	34.764071
1059.080546	45444.122257	34.769088
1059.833944	45495.907526	34.774106
1060.435459	45539.025030	34.779124
1061.625129	45591.653132	34.784141
1062.384182	45652.749491	34.789159
1063.956141	45699.188255	34.794176
1065.198593	45755.306675	34.799194
1066.062875	45806.834919	34.804212
1067.199291	45860.888990	34.809229
1068.499448	45908.509405	34.814247
1069.663077	45946.795254	34.819264
1071.079425	45995.979145	34.824282
1071.740737	46048.336790	34.829300
1072.980516	46085.010487	34.834317
1074.180727	46130.445588	34.839335
1075.354194	46176.163311	34.844352
1076.068974	46225.052682	34.849370
1076.936501	46283.065664	34.854388
1078.557401	46318.130200	34.859405
1079.629654	46370.177543	34.864423
1080.551029	46403.365354	34.869440
1081.815277	46450.448504	34.874458
1082.563555	46506.646175	34.879476
1084.012047	46538.518074	34.884493
1084.837149	46593.033846	34.889511
1085.877783	46634.990290	34.894528
1087.017486	46684.851617	34.899546
1087.794619	46734.459838	34.904564
1088.921109	46786.733721	34.909581
1090.215346	46840.050585	34.914599
1091.182076	46888.225051	34.919616
1092.428485	46930.345942	34.924634
1093.275753	46979.235187	34.929652
1094.580569	47020.037576	34.934669
1095.707591	47066.175587	34.939687
1096.610474	47107.313089	34.944704
1098.155623	47140.537183	34.949722
1098.964889	47176.622137	34.954740
1100.035939	47208.554082	34.959757
1100.772368	47247.813692	34.964775
1101.831620	47287.908511	34.969792
1102.943774	47329.956275	34.974810
1103.926175	47376.535100	34.979828
1104.944496	47422.115163	34.984845
1105.741749	47466.831586	34.989863
1107.220687	47510.277324	34.994880
1108.394210	47555.858664	34.999898
1109.337534	47617.114969	35.004916
1110.518699	47656.881364	35.009933
1111.387164	47703.459721	35.014951
1112.370621	47756.599658	35.019968
1113.875808	47809.898443	35.024986
1114.606572	47865.317758	35.030004
1115.966990	47919.272111	35.035021
1117.046952	47983.367582	35.040039
1117.960345	48020.000638	35.045056
1119.202416	48079.300817	35.050074
1120.569864	48134.716009	35.055092
1121.636846	48188.331024	35.060109
1122.667962	48251.871837	35.065127
1123.835294	48307.875520	35.070144
1124.803730	48358.988386	35.075162
1126.350649	48411.446942	35.080180
1127.878301	48460.821243	35.085197
1129.010154	48526.453819	35.090215
1130.050517	48575.012600	35.095232
1131.212805	48625.741424	35.100250
1132.084513	48679.331229	35.105268
1133.615506	48731.128716	35.110285
1134.653899	48774.234615	35.115303
1135.614203	48834.422330	35.120320
1137.144775	48883.683212	35.125338
1137.755880	48941.173745	35.130356
1139.352476	48979.498189	35.135373
1140.433190	49041.496036	35.140391
1141.557714	49090.593171	35.145408
1143.034995	49133.612060	35.150426
1143.653395	49195.012060	35.155444
1145.181118	49237.219741	35.160461
1146.672966	49298.388373	35.165479
1147.833265	49340.843573	35.170496
1149.011170	49383.738979	35.175514
1149.835247	49443.873705	35.180532
1151.089124	49475.255092	35.185549
1152.239490	49537.629323	35.190567
1153.274028	49588.215789	35.195584
1154.476612	49625.616004	35.200602
1155.367594	49676.940086	35.205620
1156.577411	49741.981872	35.210637
1158.013701	49787.773303	35.215655
1159.099605	49835.739228	35.220672
1160.120583	49886.897907	35.225690
1161.102397	49944.256999	35.230708
1162.589674	49984.327530	35.235725
1163.671845	50045.821707	35.240743
1164.869357	50095.213273	35.245760
1166.298031	50139.614645	35.250778
1167.381700	50194.718627	35.255796
1168.247113	50240.619319	35.260813
1169.184189	50295.215015	35.265831
1170.663572	50353.345069	35.270848
1172.043130	50383.556488	35.275866
1173.057672	50443.429911	35.280884
1174.266475	50485.386123	35.285901
1175.322251	50512.630336	35.290919
1176.372509	50562.944422	35.295936
1177.438062	50588.693975	35.300954
1178.426182	50638.771193	35.305972
1179.400529	50667.021712	35.310989
1180.832759	50726.855792	35.316007
1181.683584	50778.435385	35.321024
1183.319132	50820.743002	35.326042
1183.944042	50869.820930	35.331060
1185.635949	50906.381031	35.336077
1186.450299	50967.394435	35.341095
1187.765667	51012.403674	35.346112
1189.207769	51071.515790	35.351130
1190.356194	51118.474885	35.356148
1191.510282	51166.578443	35.361165
1192.510028	51214.592370	35.366183
1193.433724	51275.570487	35.371200
1194.744153	51320.676013	35.376218
1195.911025	51382.343995	35.381236
1197.407370	51432.729348	35.386253
1198.207746	51489.152593	35.391271
1199.935092	51546.563476	35.396288
1201.098133	51601.354678	35.401306
1202.225782	51665.098643	35.406324
1203.309397	51724.154654	35.411341
1205.095480	51767.263023	35.416359
1205.994650	51820.722978	35.421376
1207.595674	51876.654828	35.426394
1208.526419	51933.988898	35.431412
1210.070612	51980.786547	35.436429
1211.472314	52028.258341	35.441447
1212.763810	52084.416322	35.446464
1214.042450	52129.363885	35.451482
1214.936502	52184.122643	35.456500
1216.348343	52228.568645	35.461517
1217.737044	52277.219929	35.466535
1218.814501	52333.734732	35.471552
1220.315376	52374.984251	35.476570
1221.304635	52432.677398	35.481588
1222.283696	52469.111122	35.486605
1223.795668	52529.025971	35.491623
1224.789255	52580.245529	35.496640
1226.396922	52636.519871	35.501658
1227.356799	52686.030114	35.506676
1228.539028	52741.865089	35.511693
1229.926551	52793.479049	35.516711
1230.889063	52840.761818	35.521728
1232.332147	52889.962720	35.526746
1233.764230	52943.575962	35.531764
1234.683131	53000.370318	35.536781
1235.938370	53040.431866	35.541799
1237.321444	53103.196933	35.546816
1238.438648	53154.322466	35.551834
1239.719779	53210.522755	35.556852
1240.958751	53254.402957	35.561869
1242.676391	53315.236822	35.566887
1243.543424	53363.731581	35.571904
1244.871449	53400.099477	35.576922
1246.086315	53457.032122	35.581940
1247.414005	53513.004371	35.586957
1248.676945	53546.421178	35.591975
1249.647009	53604.993494	35.596992
1251.231297	53652.161586	35.602010
1252.106372	53709.995997	35.607028
1253.294449	53764.320095	35.612045
1254.907243	53811.243580	35.617063
1256.038844	53861.273646	35.622080
1257.632758	53901.751934	35.627098
1258.311188	53950.391338	35.632116
1259.029071	53986.292458	35.637133
1260.290117	54016.773981	35.642151
1261.325534	54065.908288	35.647168
1262.751361	54123.012029	35.652186
1263.931703	54177.901503	35.657204
1264.941578	54234.336559	35.662221
1266.759185	54284.266466	35.667239
1267.414615	54339.447320	35.672256
1268.970637	54380.710742	35.677274
1270.247007	54442.110216	35.682292
1271.477993	54491.613479	35.687309
1272.759349	54546.082991	35.692327
1274.061528	54600.169672	35.697344
1275.374104	54665.702769	35.702362
1276.853343	54721.021344	35.707380
1277.886049	54778.764095	35.712397
1279.320335	54827.786928	35.717415
1280.516589	54901.325278	35.722432
1281.998010	54944.626450	35.727450
1283.371732	54998.829414	35.732468
1284.503730	55068.163626	35.737485
1286.144232	55125.925993	35.742503
1287.208866	55182.215521	35.747520
1288.658153	55234.888369	35.752538
1289.789400	55301.489485	35.757556
1291.456537	55354.198110	35.762573
1292.670057	55398.940653	35.767591
1293.821295	55468.576794	35.772608
1295.503912	55519.182293	35.777626
1296.637479	55576.930191	35.782644
1298.153850	55639.092607	35.787661
1299.748274	55689.984406	35.792679
1300.792108	55746.341816	35.797696
1302.366459	55797.888836	35.802714
1303.733237	55850.797474	35.807732
1305.054277	55903.245070	35.812749
1306.377175	55950.705509	35.817767
1307.609474	56003.198861	35.822784
1308.779958	56056.866483	35.827802
1310.156934	56115.254758	35.832820
1311.589355	56174.071178	35.837837
1313.073433	56220.266496	35.842855
1313.941325	56277.564045	35.847872
1315.533469	56322.957883	35.852890
1316.783528	56372.278564	35.857908
1317.946834	56430.099826	35.862925
1319.650965	56475.052397	35.867943
1320.832948	56539.389662	35.872960
1322.141258	56590.885118	35.877978
1323.781230	56658.081259	35.882996
1324.908794	56695.074210	35.888013
1326.752704	56745.948209	35.893031
1327.726945	56800.395034	35.898048
1328.986125	56841.943394	35.903066
1330.406649	56891.738449	35.908084
1331.880913	56941.088502	35.913101
1332.996471	56981.988722	35.918119
1333.885350	57041.329065	35.923136
1335.424294	57095.890694	35.928154
1336.813112	57146.014021	35.933172
1337.889274	57203.015373	35.938189
1339.546640	57251.160213	35.943207
1340.537345	57313.637134	35.948224
1341.965450	57359.185208	35.953242
1343.447766	57412.376696	35.958260
1344.845569	57467.853663	35.963277
1345.836356	57504.862952	35.968295
1346.894725	57545.975621	35.973312
1348.166984	57595.567506	35.978330
1349.377510	57640.131190	35.983348
1350.850213	57689.451388	35.988365
1352.454845	57729.383926	35.993383
1353.522917	57785.546156	35.998400
1354.488970	57834.718111	36.003418
1356.067229	57891.781748	36.008436
1357.420704	57944.545215	36.013453
1358.551011	57989.337298	36.018471
1359.533087	58059.811287	36.023488
1361.335433	58124.834199	36.028506
1362.670169	58177.322625	36.033524
1364.122414	58246.698226	36.038541
1365.677233	58294.487791	36.043559
1366.903356	58359.658500	36.048576
1368.251110	58409.398481	36.053594
1369.891785	58466.510676	36.058612
1371.292895	58541.116820	36.063629
1372.755321	58591.548114	36.068647
1374.336063	58648.670123	36.073664
1375.821205	58719.485032	36.078682
1377.380515	58770.515486	36.083700
1378.659631	58818.830283	36.088717
1379.909705	58866.782617	36.093735
1381.584492	58922.928482	36.098752
1382.629050	58989.471153	36.103770
1383.836950	59039.715365	36.108788
1385.338376	59102.610682	36.113805
1386.894613	59159.940281	36.118823
1388.266414	59224.628466	36.123840
1389.757828	59277.094761	36.128858
1391.297559	59330.534686	36.133876
1392.621409	59394.889036	36.138893
1394.237607	59447.627328	36.143911
1395.918493	59511.166552	36.148928
1396.950996	59564.142044	36.153946
1398.547264	59619.839757	36.158964
1399.950993	59675.865229	36.163981
1401.492965	59728.425863	36.168999
1402.417985	59789.634556	36.174016
1404.038685	59839.119549	36.179034
1405.654207	59895.549124	36.184052
1406.851900	59965.203698	36.189069
1408.682627	60016.903225	36.194087
1410.033359	60062.987562	36.199104
1411.644748	60128.640753	36.204122
1413.329995	60184.186580	36.209140
1414.118452	60228.852759	36.214157
1415.721852	60274.435874	36.219175
1416.992012	60333.427122	36.224192
1418.687622	60381.667183	36.229210
1420.235967	60438.545292	36.234228
1421.097249	60491.112845	36.239245
1422.103929	60553.867818	36.244263
1424.119885	60606.027005	36.249280
1425.505947	60677.546762	36.254298
1427.226932	60720.763918	36.259316
1428.474126	60784.557920	36.264333
1429.896533	60832.037737	36.269351
1431.678286	60887.949860	36.274368
1433.093580	60942.393950	36.279386
1434.154460	60986.740355	36.284404
1435.242073	61046.863315	36.289421
1436.777365	61097.858114	36.294439
1438.675062	61152.486694	36.299456
1439.851290	61195.821611	36.304474
1441.386708	61238.467378	36.309492
1442.018840	61297.155697	36.314509
1443.498282	61326.226087	36.319527
1444.703115	61379.058275	36.324544
1446.211338	61428.867947	36.329562
1447.279368	61477.980680	36.334580
1448.328313	61545.061365	36.339597
1449.979233	61607.540955	36.344615
1451.710802	61671.729880	36.349632
1453.045885	61717.452642	36.354650
1454.485639	61775.749824	36.359668
1455.926195	61843.643592	36.364685
1457.626390	61914.351833	36.369703
1458.920455	61976.824915	36.374720
1460.420362	62034.885408	36.379738
1462.114243	62097.657040	36.384756
1463.759934	62159.214632	36.389773
1465.115152	62224.179228	36.394791
1466.520515	62274.025705	36.399808
1467.969790	62343.584356	36.404826
1469.815500	62402.585450	36.409844
1471.204367	62477.749952	36.414861
1472.787795	62531.095087	36.419879
1474.136306	62591.965951	36.424896
1475.771350	62657.818456	36.429914
1477.384983	62718.350606	36.434932
1478.836257	62782.352072	36.439949
1480.654582	62841.276206	36.444967
1481.842203	62903.185891	36.449984
1483.239070	62967.683798	36.455002
1485.127111	63020.159348	36.460020
1486.630888	63089.376049	36.465037
1488.285027	63151.656471	36.470055
1490.133082	63199.897208	36.475072
1491.261480	63254.777480	36.480090
1492.790846	63312.481854	36.485108
1494.365194	63377.453163	36.490125
1495.444523	63435.892974	36.495143
1497.569418	63503.089110	36.500160
1498.960528	63562.119811	36.505178
1500.570220	63615.862003	36.510196
1501.959317	63676.811477	36.515213
1503.380425	63728.386690	36.520231
1504.971652	63789.019922	36.525248
1506.271504	63854.744479	36.530266
1507.707718	63917.035607	36.535284
1508.884495	63979.456127	36.540301
1510.560337	64040.000757	36.545319
1512.509490	64098.964379	36.550336
1513.969307	64165.329448	36.555354
1515.790374	64227.592769	36.560372
1517.639468	64283.736292	36.565389
1518.993938	64333.309990	36.570407
1520.272356	64390.897871	36.575424
1521.544697	64447.752457	36.580442
1523.098566	64500.372073	36.585460
1524.800789	64573.354030	36.590477
1526.089400	64629.560732	36.595495
1527.925271	64690.404769	36.600512
1528.940453	64748.452515	36.605530
1530.577688	64809.119009	36.610548
1531.891564	64875.958303	36.615565
1533.334462	64939.453816	36.620583
1535.096945	65014.276271	36.625600
1536.584683	65082.355101	36.630618
1538.330926	65132.065324	36.635636
1539.418384	65200.118489	36.640653
1541.034492	65256.319655	36.645671
1542.861150	65314.355660	36.650688
1544.162998	65355.512959	36.655706
1545.459190	65410.150115	36.660724
1546.872815	65465.275499	36.665741
1548.375941	65515.663976	36.670759
1550.150638	65568.479193	36.675776
1551.186209	65634.597994	36.680794
1552.853533	65675.901214	36.685812
1553.847308	65743.464017	36.690829
1555.747162	65799.913223	36.695847
1557.362005	65862.782692	36.700864
1558.793395	65930.739682	36.705882
1560.952383	65993.074793	36.710900
1562.351924	66052.926775	36.715917
1564.211040	66121.311171	36.720935
1565.699307	66181.029276	36.725952
1567.159703	66235.845123	36.730970
1569.191876	66301.999629	36.735988
1570.679483	66369.569121	36.741005
1572.215441	66417.478711	36.746023
1574.245252	66472.972045	36.751040
1575.449447	66538.591967	36.756058
1577.106471	66606.065929	36.761076
1579.163484	66661.042576	36.766093
1580.645568	66729.481296	36.771111
1582.060463	66777.410515	36.776128
1583.650540	66837.747379	36.781146
1585.215681	66905.382142	36.786164
1586.586409	66974.579733	36.791181
1588.342693	67038.658297	36.796199
1590.264709	67104.806816	36.801216
1591.513680	67171.010195	36.806234
1593.290470	67219.554752	36.811252
1594.834155	67288.941401	36.816269
1596.467343	67353.204644	36.821287
1598.420091	67413.562093	36.826304
1599.699714	67483.978331	36.831322
1601.405335	67539.018211	36.836340
1603.227225	67606.418373	36.841357
1604.638803	67666.038005	36.846375
1606.425742	67729.379039	36.851392
1608.056727	67784.469121	36.856410
1609.791776	67850.946431	36.861428
1611.402709	67916.499914	36.866445
1612.778551	67982.723532	36.871463
1614.931960	68036.307754	36.876480
1616.130617	68095.429845	36.881498
1617.616241	68153.905641	36.886516
1619.316416	68228.323112	36.891533
1621.143273	68277.083464	36.896551
1622.983780	68331.287140	36.901568
1624.084337	68406.799401	36.906586
1626.050429	68461.673869	36.911604
1627.851488	68535.899152	36.916621
1629.316951	68587.528008	36.921639
1631.064425	68636.846013	36.926656
1632.301403	68707.759846	36.931674
1634.178464	68768.689553	36.936692
1635.659391	68823.919334	36.941709
1637.457363	68898.038504	36.946727
1639.407282	68961.420400	36.951744
1640.693859	69017.174907	36.956762
1642.304303	69082.490832	36.961780
1643.936893	69138.406736	36.966797
1645.205725	69199.578293	36.971815
1647.143645	69263.868294	36.976832
1648.290091	69327.079231	36.981850
1650.156711	69382.078881	36.986868
1651.878140	69448.125549	36.991885
1653.581912	69494.418967	36.996903
1654.975026	69544.769319	37.001920
1656.345472	69596.567043	37.006938
1657.707681	69653.666166	37.011956
1659.351007	69716.774964	37.016973
1660.913466	69769.024228	37.021991
1662.178299	69831.958253	37.027008
1663.568881	69901.698869	37.032026
1665.175614	69967.061938	37.037044
1667.101175	70044.837124	37.042061
1668.434310	70118.044716	37.047079
1670.400962	70190.760766	37.052096
1671.814610	70266.147143	37.057114
1673.689470	70340.840991	37.062132
1675.689584	70426.381734	37.067149
1677.152156	70496.125344	37.072167
1679.498116	70562.944648	37.077184
1680.952161	70648.077657	37.082202
1682.755681	70704.609769	37.087220
1684.554675	70778.835486	37.092237
1686.296498	70843.014454	37.097255
1688.171102	70922.801292	37.102272
1689.746241	70998.367154	37.107290
1691.672029	71061.530004	37.112308
1693.320951	71137.692641	37.117325
1694.911246	71215.751767	37.122343
1696.505435	71284.324368	37.127360
1698.367054	71362.290810	37.132378
1700.284737	71434.080779	37.137396
1701.925424	71510.929710	37.142413
1703.533037	71581.616077	37.147431
1705.727702	71651.970122	37.152448
1707.396094	71727.751472	37.157466
1709.242021	71797.691870	37.162484
1711.070583	71864.076205	37.167501
1712.448533	71933.938219	37.172519
1714.597333	71997.182419	37.177536
1716.034127	72076.433351	37.182554
1717.937530	72135.359369	37.187572
1719.917306	72203.050774	37.192589
1721.328415	72273.896414	37.197607
1723.504783	72339.467588	37.202624
1725.089538	72416.606568	37.207642
1726.601386	72483.270015	37.212660
1728.460177	72551.956508	37.217677
1730.337231	72621.184949	37.222695
1732.151959	72694.527032	37.227712
1733.559392	72759.548304	37.232730
1735.470575	72820.906474	37.237748
1737.169237	72896.939771	37.242765
1739.275958	72975.113293	37.247783
1740.603449	73030.445670	37.252800
1742.249422	73099.116230	37.257818
1744.150218	73175.815324	37.262836
1745.798399	73243.143318	37.267853
1747.278401	73307.495948	37.272871
1749.396236	73376.144048	37.277888
1751.006381	73461.059080	37.282906
1752.670359	73532.223172	37.287924
1754.590878	73596.811554	37.292941
1756.213056	73669.806489	37.297959
1758.124031	73735.030012	37.302976
1759.988760	73803.630166	37.307994
1761.755865	73873.702401	37.313012
1763.688968	73937.846323	37.318029
1764.930102	73997.817452	37.323047
1766.929500	74061.229314	37.328064
1768.528100	74131.619926	37.333082
1770.324785	74180.155396	37.338100
1772.044135	74229.197049	37.343117
1773.270909	74281.381175	37.348135
1775.213163	74341.230691	37.353152
1776.813766	74388.365907	37.358170
1778.480246	74451.514135	37.363188
1780.193294	74514.161227	37.368205
1781.943258	74587.860680	37.373223
1783.726457	74654.563122	37.378240
1785.209193	74728.659449	37.383258
1786.636445	74798.736635	37.388276
1788.947575	74864.140975	37.393293
1791.006987	74950.586462	37.398311
1792.403573	75016.172292	37.403328
1794.013092	75097.875252	37.408346
1795.849313	75177.212267	37.413364
1797.936651	75239.397144	37.418381
1799.700236	75330.108249	37.423399
1801.462783	75403.972650	37.428416
1803.188315	75490.294787	37.433434
1805.144504	75581.014599	37.438452
1807.073385	75654.448311	37.443469
1809.119762	75742.785795	37.448487
1810.697096	75810.296027	37.453504
1812.949785	75888.024566	37.458522
1814.694892	75960.816507	37.463540
1816.497611	76048.521757	37.468557
1818.044561	76135.988634	37.473575
1820.400288	76215.032066	37.478592
1822.138738	76292.652232	37.483610
1824.038359	76371.083455	37.488628
1826.248377	76441.827811	37.493645
1828.011527	76524.435783	37.498663
1829.739006	76599.145006	37.503680
1831.868932	76678.541820	37.508698
1833.733318	76752.229297	37.513716
1835.953804	76827.672732	37.518733
1837.471578	76900.553448	37.523751
1839.617046	76963.252587	37.528768
1841.325730	77045.161275	37.533786
1843.122851	77121.710539	37.538804
1845.075475	77195.360076	37.543821
1846.682086	77272.534967	37.548839
1848.656616	77328.725058	37.553856
1850.850628	77407.898624	37.558874
1852.443623	77485.684313	37.563892
1854.368727	77559.402483	37.568909
1856.084405	77633.178960	37.573927
1858.046098	77709.197400	37.578944
1859.721743	77779.078757	37.583962
1861.096775	77867.629566	37.588980
1863.653744	77936.043252	37.593997
1865.252566	78025.649020	37.599015
1867.359781	78093.487399	37.604032
1868.861124	78160.065245	37.609050
1871.057601	78240.355654	37.614068
1873.278800	78319.945669	37.619085
1874.896417	78391.940626	37.624103
1876.821813	78464.216991	37.629120
1878.529497	78543.596637	37.634138
1880.693375	78619.915351	37.639156
1882.494739	78683.090358	37.644173
1884.067579	78764.201998	37.649191
1885.340047	78836.277467	37.654208
1887.823525	78913.953206	37.659226
1889.655838	78995.949740	37.664244
1891.474770	79063.366889	37.669261
1892.933579	79123.150614	37.674279
1894.745855	79191.874003	37.679296
1896.424317	79262.341463	37.684314
1897.852539	79335.964801	37.689332
1899.688805	79402.480578	37.694349
1901.339935	79478.565188	37.699367
1903.193541	79557.012758	37.704384
1905.499160	79636.998782	37.709402
1907.214117	79708.791916	37.714420
1909.251502	79786.577928	37.719437
1910.924616	79877.901090	37.724455
1912.749484	79963.144952	37.729472
1914.943674	80051.131175	37.734490
1916.524409	80133.347818	37.739508
1918.630560	80207.842922	37.744525
1920.561114	80306.855461	37.749543
1922.442172	80391.965153	37.754560
1924.594769	80482.746508	37.759578
1926.215682	80580.022086	37.764596
1928.032767	80669.044821	37.769613
1930.051004	80768.311337	37.774631
1932.272050	80863.314839	37.779648
1934.454920	80943.767272	37.784666
1936.378229	81042.922923	37.789684
1938.585612	81135.648955	37.794701
1940.237671	81226.473044	37.799719
1942.095864	81315.871498	37.804736
1944.477700	81417.186604	37.809754
1946.591053	81519.684374	37.814772
1948.682086	81603.928693	37.819789
1950.681248	81695.206782	37.824807
1952.802961	81782.842380	37.829824
1955.047284	81867.582974	37.834842
1956.891840	81948.750074	37.839860
1959.095591	82047.041839	37.844877
1960.476473	82137.784606	37.849895
1962.483441	82219.294507	37.854912
1964.842151	82310.873099	37.859930
1966.708422	82414.755835	37.864948
1968.975636	82494.553336	37.869965
1971.036325	82589.080961	37.874983
1973.078680	82673.323429	37.880000
1975.214014	82758.767958	37.885018
1976.444941	82844.823067	37.890036
1978.900686	82935.387537	37.895053
1980.436614	83031.493868	37.900071
1982.413966	83128.228334	37.905088
1984.612589	83211.472318	37.910106
1986.565185	83302.610844	37.915124
1988.686711	83400.438696	37.920141
1990.584577	83492.891478	37.925159
1992.358417	83573.428099	37.930176
1994.561013	83676.540598	37.935194
1996.134937	83780.119294	37.940212
1998.279758	83869.506321	37.945229
2000.451931	83965.465567	37.950247
2002.349941	84059.580058	37.955264
2004.604070	84157.301063	37.960282
2006.119851	84253.135903	37.965300
2008.277735	84340.330265	37.970317
2010.250684	84443.836259	37.975335
2012.693427	84542.263994	37.980352
2014.809252	84633.077121	37.985370
2016.410451	84728.139909	37.990388
2018.544293	84828.276897	37.995405
2020.601432	84922.305967	38.000423
2022.203098	85021.703259	38.005440
2024.195477	85108.190911	38.010458
2025.857027	85184.479359	38.015476
2028.034421	85266.718936	38.020493
2029.993488	85352.236827	38.025511
2031.418825	85433.124652	38.030528
2033.831112	85516.646036	38.035546
2035.213464	85607.222197	38.040564
2037.207156	85702.125413	38.045581
2039.356626	85799.919068	38.050599
2041.203873	85904.007535	38.055616
2042.966771	86000.861283	38.060634
2044.971453	86113.187906	38.065652
2046.800394	86226.822326	38.070669
2048.848671	86335.278048	38.075687
2051.167924	86448.291721	38.080704
2053.469017	86560.155517	38.085722
2055.004353	86669.820558	38.090740
2057.235961	86783.584231	38.095757
2059.197564	86901.268295	38.100775
2061.229876	87023.795252	38.105792
2063.766649	87143.316484	38.110810
2065.416883	87270.504313	38.115828
2067.774237	87381.462714	38.120845
2069.974988	87512.367187	38.125863
2072.135648	87626.018513	38.130880
2074.507488	87736.633834	38.135898
2076.067434	87863.838360	38.140916
2078.716578	87982.876546	38.145933
2080.858392	88104.643196	38.150951
2083.169757	88219.946041	38.155968
2085.224231	88338.331014	38.160986
2087.055931	88470.488740	38.166004
2089.101399	88581.944022	38.171021
2091.244797	88703.358052	38.176039
2093.284070	88824.269276	38.181056
2095.608651	88953.120411	38.186074
2097.541280	89079.473453	38.191092
2100.028569	89194.486436	38.196109
2102.586582	89317.384242	38.201127
2104.271299	89441.838605	38.206144
2106.796534	89559.647868	38.211162
2108.753828	89688.661046	38.216180
2110.619171	89800.998207	38.221197
2112.961638	89921.232782	38.226215
2114.438663	90049.220065	38.231232
2116.979926	90174.063082	38.236250
2118.912145	90298.634375	38.241268
2121.494071	90425.968795	38.246285
2124.074537	90551.542330	38.251303
2125.883486	90676.425976	38.256320
2128.430976	90796.441881	38.261338
2130.327825	90918.625917	38.266356
2132.209594	91027.429077	38.271373
2134.270173	91153.606103	38.276391
2136.276143	91281.173676	38.281408
2138.677635	91409.529073	38.286426
2140.656684	91536.658342	38.291444
2142.923618	91651.601175	38.296461
2145.058413	91778.871860	38.301479
2147.245674	91902.231170	38.306496
2149.693995	92023.496886	38.311514
2151.279278	92153.440696	38.316532
2153.702652	92268.602208	38.321549
2155.958774	92395.108699	38.326567
2157.932742	92526.273419	38.331584
2159.969941	92636.743767	38.336602
2162.117279	92769.073824	38.341620
2164.517939	92899.286160	38.346637
2166.169940	93013.417771	38.351655
2168.164456	93123.110719	38.356672
2170.487038	93236.136931	38.361690
2172.281292	93348.105475	38.366708
2173.752052	93462.330489	38.371725
2176.315090	93563.697321	38.376743
2178.168260	93700.361591	38.381760
2180.253210	93808.534506	38.386778
2181.954058	93942.194323	38.391796
2184.004053	94075.039579	38.396813
2186.293650	94217.721983	38.401831
2188.092726	94349.682381	38.406848
2190.099563	94481.788293	38.411866
2192.236605	94640.543594	38.416884
2194.512355	94781.329442	38.421901
2196.553283	94934.295889	38.426919
2198.775601	95091.405002	38.431936
2200.880754	95240.319371	38.436954
2202.908849	95401.820887	38.441972
2205.120254	95564.929745	38.446989
2207.575724	95725.985799	38.452007
2209.236174	95888.688184	38.457024
2212.112041	96050.770274	38.462042
2214.336944	96222.918476	38.467060
2216.603921	96392.120164	38.472077
2219.267255	96552.564842	38.477095
2221.379963	96725.227723	38.482112
2223.748131	96888.192174	38.487130
2226.073505	97050.897956	38.492148
2228.458574	97209.526076	38.497165
2230.884327	97378.796955	38.502183
2232.608142	97530.862256	38.507200
2235.176296	97699.922422	38.512218
2237.562631	97867.465367	38.517236
2239.720325	98029.124880	38.522253
2242.247252	98193.617783	38.527271
2244.582724	98360.740267	38.532288
2246.933053	98517.630932	38.537306
2249.161879	98686.178956	38.542324
2251.729837	98845.268352	38.547341
2254.241295	99008.195901	38.552359
2256.175414	99178.719560	38.557376
2258.664368	99328.480547	38.562394
2260.911806	99493.315434	38.567412
2263.370808	99655.607924	38.572429
2265.784151	99817.312529	38.577447
2267.677011	99971.708326	38.582464
2269.970542	100126.599994	38.587482
2272.125578	100298.172610	38.592500
2274.466722	100465.457277	38.597517
2276.980241	100626.136027	38.602535
2279.018327	100789.526960	38.607552
2280.830109	100957.797110	38.612570
2283.094680	101126.441022	38.617588
2285.806926	101291.896952	38.622605
2287.900497	101466.274527	38.627623
2290.030732	101632.140186	38.632640
2292.526268	101804.136554	38.637658
2294.797656	101976.688704	38.642676
2296.814695	102163.113745	38.647693
2299.350886	102320.475519	38.652711
2301.753221	102505.942048	38.657728
2304.047763	102671.267419	38.662746
2306.206530	102838.288449	38.667764
2308.468063	103009.275382	38.672781
2310.945374	103176.298997	38.677799
2313.172027	103353.670621	38.682816
2315.475335	103530.232424	38.687834
2317.401944	103699.715791	38.692852
2319.588836	103854.831912	38.697869
2321.818789	104013.276636	38.702887
2323.850264	104176.140173	38.707904
2325.848967	104326.850196	38.712922
2327.631784	104493.456526	38.717940
2329.710135	104658.571996	38.722957
2331.935822	104842.621039	38.727975
2334.251708	105025.997641	38.732992
2336.656631	105199.369777	38.738010
2339.050787	105382.241566	38.743028
2340.929182	105578.648242	38.748045
2343.513128	105760.414604	38.753063
2345.348468	105961.813403	38.758080
2347.923462	106155.984221	38.763098
2350.319375	106360.239434	38.768116
2352.375483	106562.114446	38.773133
2354.887512	106757.566552	38.778151
2357.135857	106969.012796	38.783168
2359.826691	107177.601446	38.788186
2362.818475	107370.978503	38.793204
2365.353923	107569.538274	38.798221
2367.858729	107767.672842	38.803239
2370.341667	107978.936428	38.808256
2372.960176	108169.675384	38.813274
2375.658979	108370.103627	38.818292
2377.900793	108570.033880	38.823309
2380.498078	108752.879193	38.828327
2382.775499	108956.445520	38.833344
2384.948299	109152.433443	38.838362
2387.641143	109343.940757	38.843380
2390.055092	109539.449285	38.848397
2392.518703	109742.407725	38.853415
2394.644116	109953.029057	38.858432
2397.243981	110154.484843	38.863450
2399.551666	110355.809948	38.868468
2402.047889	110571.551018	38.873485
2404.536815	110765.659652	38.878503
2406.765304	110976.486550	38.883520
2409.013222	111185.231845	38.888538
2411.177648	111393.801198	38.893556
2413.742678	111608.333027	38.898573
2416.217988	111817.870782	38.903591
2418.476367	112040.480894	38.908608
2420.742815	112261.696086	38.913626
2423.720241	112469.218729	38.918644
2425.569486	112694.458710	38.923661
2428.394355	112908.222090	38.928679
2430.492380	113136.812114	38.933696
2432.894845	113357.213753	38.938714
2435.702494	113577.971874	38.943732
2437.770376	113794.408109	38.948749
2440.798411	114020.930444	38.953767
2442.761048	114259.986647	38.958784
2444.952946	114477.891431	38.963802
2447.588108	114699.545761	38.968820
2449.873831	114934.750915	38.973837
2452.014623	115163.410353	38.978855
2454.486357	115404.842221	38.983872
2456.681528	115632.024795	38.988890
2459.562985	115867.053914	38.993908
2461.580072	116102.612922	38.998925
2464.102166	116338.652502	39.003943
2466.504130	116578.606254	39.008960
2468.950974	116818.757466	39.013978
2471.915033	117054.910008	39.018996
2474.410187	117292.367725	39.024013
2476.879622	117524.706634	39.029031
2479.381660	117746.361894	39.034048
2481.774526	117966.855908	39.039066
2484.371472	118163.067084	39.044084
2486.346593	118372.428657	39.049101
2489.479799	118572.946826	39.054119
2491.511555	118782.390588	39.059136
2494.202533	118993.952164	39.064154
2496.408448	119210.055749	39.069172
2499.067162	119424.466093	39.074189
2501.101931	119642.780643	39.079207
2503.631380	119869.454420	39.084224
2505.601382	120098.956968	39.089242
2507.824697	120326.340928	39.094260
2510.032663	120568.481270	39.099277
2512.411312	120816.000265	39.104295
2514.660007	121058.492471	39.109312
2517.222969	121317.922556	39.114330
2520.323164	121578.094874	39.119348
2522.350539	121838.449419	39.124365
2524.703807	122101.152268	39.129383
2526.885068	122360.775809	39.134400
2529.569535	122636.483875	39.139418
2532.400949	122908.897950	39.144436
2534.492332	123186.326386	39.149453
2537.036908	123457.114554	39.154471
2539.535022	123742.640287	39.159488
2542.373411	124022.583688	39.164506
2545.024199	124306.846319	39.169524
2547.291686	124592.071640	39.174541
2549.934877	124881.287159	39.179559
2552.331945	125171.215624	39.184576
2555.006145	125458.654305	39.189594
2557.780637	125739.291974	39.194612
2560.347004	126039.755424	39.199629
2563.497349	126317.318826	39.204647
2565.794336	126610.571733	39.209664
2568.488251	126905.223643	39.214682
2571.594309	127192.492737	39.219700
2573.806139	127484.585265	39.224717
2576.759202	127766.667835	39.229735
2579.628529	128051.987998	39.234752
2582.376428	128329.868892	39.239770
2584.770979	128621.750478	39.244788
2587.462670	128900.189499	39.249805
2590.428107	129185.185138	39.254823
2593.246340	129478.389336	39.259840
2595.684713	129756.416854	39.264858
2598.104428	130033.332567	39.269876
2600.399157	130328.908337	39.274893
2603.333814	130615.745444	39.279911
2606.143587	130914.568973	39.284928
2608.452276	131200.581650	39.289946
2611.426324	131488.027440	39.294964
2613.476195	131779.286654	39.299981
2616.544914	132068.713566	39.304999
2618.419009	132366.056628	39.310016
2620.912583	132668.837090	39.315034
2623.666431	132958.484088	39.320052
2625.991507	133257.995872	39.325069
2628.368802	133560.394602	39.330087
2630.911105	133860.701267	39.335104
2633.213434	134178.634644	39.340122
2635.809849	134485.040528	39.345140
2638.083775	134809.720813	39.350157
2640.707130	135128.562412	39.355175
2643.480204	135444.781498	39.360192
2645.978642	135766.172342	39.365210
2648.629120	136084.191600	39.370228
2651.220839	136394.354611	39.375245
2653.863772	136693.002019	39.380263
2656.845567	136987.118822	39.385280
2658.856746	137292.721497	39.390298
2661.251571	137584.675093	39.395316
2663.652764	137892.504937	39.400333
2665.935289	138215.799425	39.405351
2668.694404	138524.326179	39.410368
2670.528036	138840.905856	39.415386
2673.527476	139166.442489	39.420404
2675.912330	139505.098057	39.425421
2678.175864	139842.011008	39.430439
2680.760812	140189.447498	39.435456
2683.178670	140537.128389	39.440474
2685.673869	140894.165640	39.445492
2688.050314	141257.303131	39.450509
2690.554398	141630.017901	39.455527
2693.311742	142011.592492	39.460544
2695.906014	142394.883517	39.465562
2698.560219	142772.177785	39.470580
2701.289209	143165.264238	39.475597
2703.896841	143557.103620	39.480615
2706.345624	143948.679016	39.485632
2708.651997	144351.232827	39.490650
2711.847164	144751.252061	39.495668
2714.333896	145162.770049	39.500685
2716.868371	145574.068132	39.505703
2719.842992	145987.483754	39.510720
2722.314238	146397.300644	39.515738
2725.567565	146817.342832	39.520756
2728.631359	147240.502360	39.525773
2731.403758	147648.048124	39.530791
2733.998871	148065.334756	39.535808
2736.771916	148492.954251	39.540826
2739.560510	148906.003214	39.545844
2742.689554	149333.713408	39.550861
2745.378346	149750.922447	39.555879
2748.336080	150176.508294	39.560896
2751.006493	150599.476807	39.565914
2753.961585	151030.959478	39.570932
2757.025818	151444.644769	39.575949
2759.554798	151874.157029	39.580967
2762.846665	152293.715622	39.585984
2765.544873	152717.343397	39.591002
2768.783010	153131.597943	39.596020
2772.021481	153545.728535	39.601037
2775.172066	153964.763137	39.606055
2778.112001	154363.688007	39.611072
2780.650911	154769.152471	39.616090
2783.544779	155185.062541	39.621108
2786.249140	155587.891804	39.626125
2788.854856	156001.085359	39.631143
2791.656670	156415.215941	39.636160
2793.919477	156844.261210	39.641178
2796.418004	157260.793654	39.646196
2799.133598	157690.015381	39.651213
2801.782906	158122.881309	39.656231
2804.461971	158542.199968	39.661248
2807.046418	158989.783159	39.666266
2809.585404	159421.863048	39.671284
2811.992286	159862.789913	39.676301
2814.281131	160311.266781	39.681319
2817.286100	160764.052914	39.686336
2819.968809	161224.154616	39.691354
2823.027424	161677.205486	39.696372
2825.852436	162126.500033	39.701389
2828.377945	162582.586091	39.706407
2831.730729	163039.015717	39.711424
2834.257553	163496.098240	39.716442
2837.054743	163916.513104	39.721460
2839.718703	164357.532133	39.726477
2842.549476	164782.822577	39.731495
2845.092649	165218.762213	39.736512
2847.847863	165647.244018	39.741530
2850.375143	166084.804136	39.746548
2853.168006	166529.080132	39.751565
2855.409304	166980.149125	39.756583
2858.448307	167435.476682	39.761600
2861.183353	167909.887417	39.766618
2863.910590	168367.085384	39.771636
2866.553165	168843.853037	39.776653
2869.128303	169319.593211	39.781671
2871.698307	169797.876745	39.786688
2874.364509	170305.568104	39.791706
2877.465370	170788.511141	39.796724
2880.340118	171290.704000	39.801741
2882.980524	171794.803391	39.806759
2886.377089	172294.686504	39.811776
2889.104988	172798.080437	39.816794
2892.184259	173305.638364	39.821812
2894.870060	173828.435138	39.826829
2897.590614	174346.772917	39.831847
2900.675675	174860.358747	39.836864
2903.334890	175396.731478	39.841882
2905.919046	175914.376826	39.846900
2909.381104	176454.770534	39.851917
2911.832693	176979.567016	39.856935
2915.448674	177521.607005	39.861952
2918.236763	178058.827457	39.866970
2921.297175	178597.278526	39.871988
2924.166680	179142.518495	39.877005
2927.026750	179696.322304	39.882023
2930.129671	180234.954473	39.887040
2932.679594	180783.708512	39.892058
2935.867106	181325.762618	39.897076
2938.823733	181885.228392	39.902093
2941.852503	182436.533326	39.907111
2944.765213	182997.384052	39.912128
2947.983330	183560.095175	39.917146
2950.615580	184127.523742	39.922164
2954.003246	184751.654946	39.927181
2956.952029	185311.802020	39.932199
2959.844629	185870.030606	39.937216
2962.529849	186439.317973	39.942234
2966.107171	186989.597052	39.947252
2969.084681	187566.337632	39.952269
2972.236533	188114.250638	39.957287
2975.775366	188669.954438	39.962304
2978.763739	189227.017092	39.967322
2981.864916	189777.816400	39.972340
2985.192536	190334.272602	39.977357
2987.824716	190889.062178	39.982375
2990.686238	191449.762206	39.987392
2993.874865	192012.394936	39.992410
2996.667559	192564.474638	39.997428
2999.523939	193125.335527	40.002445
3002.247373	193689.572613	40.007463
3005.417561	194252.218231	40.012480
3007.857300	194823.261276	40.017498
3011.026361	195386.623106	40.022516
3013.913173	195962.478094	40.027533
3016.324210	196544.353821	40.032551
3019.490896	197124.894481	40.037568
3022.244664	197707.076943	40.042586
3025.227987	198296.566923	40.047604
3028.291966	198873.929865	40.052621
3030.772886	199462.054988	40.057639
3033.679094	200025.755163	40.062656
3036.608986	200590.723707	40.067674
3038.493261	201156.187920	40.072692
3041.988791	201738.624863	40.077709
3044.804825	202317.461259	40.082727
3048.021653	202890.597499	40.087744
3050.692145	203485.032157	40.092762
3053.924796	204065.739543	40.097780
3057.093432	204658.423395	40.102797
3059.873638	205257.368054	40.107815
3062.625992	205857.487360	40.112832
3065.581367	206467.788632	40.117850
3068.553678	207087.665924	40.122868
3071.141703	207701.990925	40.127885
3074.483277	208337.817836	40.132903
3077.506228	208958.149447	40.137920
3080.423835	209596.789462	40.142938
3083.814512	210223.188842	40.147956
3086.941913	210869.902786	40.152973
3089.882962	211511.388818	40.157991
3092.752426	212164.344433	40.163008
3096.471523	212815.034652	40.168026
3099.404192	213468.389502	40.173044
3102.448310	214118.324060	40.178061
3105.699980	214779.023907	40.183079
3108.707005	215436.587656	40.188096
3111.865155	216111.987704	40.193114
3115.225311	216773.715309	40.198132
3118.473279	217439.678414	40.203149
3121.243351	218114.557664	40.208167
3124.509024	218791.290913	40.213184
3127.282661	219467.034859	40.218202
3130.505729	220144.208011	40.223220
3133.860792	220835.028464	40.228237
3136.881881	221522.649938	40.233255
3140.809636	222208.809059	40.238272
3143.960257	222883.048521	40.243290
3147.659894	223560.860584	40.248308
3151.090977	224244.252923	40.253325
3154.166494	224926.811833	40.258343
3157.519355	225606.431346	40.263360
3160.931930	226275.168533	40.268378
3164.345892	226954.270256	40.273396
3168.006820	227622.714269	40.278413
3170.909591	228288.761570	40.283431
3174.136492	228952.014221	40.288448
3177.448333	229618.123848	40.293466
3181.016425	230290.594741	40.298484
3184.014657	230962.188832	40.303501
3187.161827	231632.692037	40.308519
3190.278791	232304.723499	40.313536
3193.293338	232961.350026	40.318554
3195.935013	233648.975957	40.323572
3198.834204	234324.824078	40.328589
3202.249019	235019.262348	40.333607
3205.246991	235692.958973	40.338624
3208.532214	236387.415156	40.343642
3211.398490	237086.990858	40.348660
3214.706385	237769.297852	40.353677
3217.701752	238472.915054	40.358695
3220.823386	239167.035410	40.363712
3223.789849	239868.799415	40.368730
3227.262279	240577.366853	40.373748
3230.620267	241284.146668	40.378765
3233.518362	241994.552882	40.383783
3237.288436	242691.306212	40.388800
3240.015548	243408.085743	40.393818
3243.410708	244102.607134	40.398836
3247.148335	244784.828551	40.403853
3249.736147	245451.630196	40.408871
3252.944032	246122.752763	40.413888
3256.029454	246788.125775	40.418906
3258.750708	247460.793122	40.423924
3261.936122	248145.070565	40.428941
3264.779745	248830.059285	40.433959
3267.800499	249527.109076	40.438976
3271.076337	250225.259190	40.443994
3274.087635	250936.224912	40.449012
3277.335208	251652.078485	40.454029
3280.142940	252379.834755	40.459047
3283.702581	253102.745230	40.464064
3286.672563	253823.864623	40.469082
3289.899019	254566.785496	40.474100
3293.189816	255313.070717	40.479117
3296.739782	256058.447676	40.484135
3299.720789	256810.031043	40.489152
3303.434262	257555.018304	40.494170
3306.339772	258311.126003	40.499188
3309.715257	259078.738233	40.504205
3312.748688	259863.061703	40.509223
3315.833879	260632.512753	40.514240
3319.229339	261410.012769	40.519258
3321.914634	262207.760545	40.524276
3325.304318	263004.859035	40.529293
3328.335264	263804.242894	40.534311
3331.861023	264619.392501	40.539328
3335.552708	265424.908909	40.544346
3338.926712	266239.129615	40.549364
3342.657608	267045.515876	40.554381
3346.334261	267858.964729	40.559399
3350.473425	268659.152681	40.564416
3354.146947	269453.133317	40.569434
3357.457023	270256.992898	40.574452
3361.391764	271050.639458	40.579469
3364.868260	271851.868208	40.584487
3368.262138	272642.207189	40.589504
3371.854365	273451.022224	40.594522
3375.132039	274262.164410	40.599540
3378.850758	275050.982516	40.604557
3382.321525	275849.583909	40.609575
3385.648498	276643.273079	40.614592
3389.134829	277436.192929	40.619610
3392.473608	278229.102415	40.624628
3396.126988	279025.128939	40.629645
3399.446401	279839.661369	40.634663
3402.451085	280626.376310	40.639680
3406.420832	281430.987303	40.644698
3409.512533	282243.649586	40.649716
3412.663143	283036.740286	40.654733
3416.388839	283839.203912	40.659751
3419.969140	284636.450041	40.664768
3423.278180	285436.141648	40.669786
3426.377166	286246.115244	40.674804
3430.205739	287049.236030	40.679821
3433.226205	287867.099124	40.684839
3436.365229	288674.649829	40.689856
3440.152325	289482.977769	40.694874
3443.557460	290297.956783	40.699892
3447.429921	291105.234962	40.704909
3450.690594	291913.207636	40.709927
3453.995616	292730.760104	40.714944
3457.668636	293538.646719	40.719962
3460.564887	294360.912603	40.724980
3464.265931	295177.303323	40.729997
3467.493482	296001.754030	40.735015
3470.707412	296807.805086	40.740020
3473.917808	297576.541637	40.745024
3476.848557	298316.779275	40.750029
3480.568257	299010.408237	40.755034
3483.305308	299643.530498	40.760039
3486.018157	300234.552412	40.765044
3489.037692	300780.191251	40.770048
3492.078003	301246.923111	40.775053
3494.338495	301679.363286	40.780058
3496.777671	302068.073248	40.785063
3498.755268	302414.859220	40.790068
3500.955745	302700.069135	40.795072
3503.152008	302943.234379	40.800077
3504.677570	303141.940164	40.805082
3506.600751	303316.354579	40.810087
3508.516317	303438.088123	40.815092
3509.908968	303539.441377	40.820096
3511.106338	303597.560111	40.825101
3512.374557	303627.240163	40.830106
3513.459952	303631.447979	40.835111
3514.166361	303603.520905	40.840116
3514.963006	303564.127237	40.845120
3516.094577	303504.753857	40.850125
3516.937996	303402.313145	40.855130
3517.575668	303287.128463	40.860135
3518.189338	303158.967712	40.865140
3518.938841	303018.747467	40.870144
3519.250216	302856.631754	40.875149
3519.442240	302680.587400	40.880154
3519.820085	302499.652372	40.885159
3520.328036	302295.460033	40.890164
3520.780960	302095.042208	40.895168
3520.684501	301886.158065	40.900173
3521.086593	301656.732673	40.905178
3521.506728	301432.164612	40.910183
3521.259148	301191.869429	40.915188
3521.605036	300951.149525	40.920192
3521.631267	300704.217500	40.925197
3521.749968	300450.932485	40.930202
3521.418874	300204.308560	40.935207
3521.659640	299948.202452	40.940212
3521.621990	299677.452990	40.945216
3521.670263	299419.541974	40.950221
3521.655863	299162.403109	40.955226
3521.550850	298895.707205	40.960231
3521.959642	298625.875419	40.965236
3521.496374	298356.993138	40.970240
3521.305988	298091.172107	40.975245
3521.379278	297799.779590	40.980250
3520.994366	297540.578600	40.985255
3520.833371	297258.662890	40.990260
3520.738850	296997.123251	40.995264
3520.691871	296726.742742	41.000269
3520.852036	296464.575421	41.005274
3520.192375	296199.964282	41.010279
3520.371319	295932.471843	41.015284
3520.440735	295668.864237	41.020288
3520.185263	295395.582905	41.025293
3520.213995	295133.201007	41.030298
3520.164777	294885.593406	41.035303
3519.744725	294607.828771	41.040308
3519.498193	294348.031801	41.045312
3519.115518	294078.276892	41.050317
3519.406966	293818.368037	41.055322
3519.009355	293572.387572	41.060327
3518.660206	293316.598492	41.065332
3518.562330	293071.358202	41.070336
3518.328016	292815.879949	41.075341
3518.396309	292574.557158	41.080346
3518.083023	292326.318384	41.085351
3518.104594	292077.389869	41.090356
3518.120858	291831.235790	41.095360
3517.575416	291583.004835	41.100365
3517.443412	291340.690272	41.105370
3517.377558	291115.037794	41.110375
3517.222106	290875.194260	41.115380
3517.078001	290653.599784	41.120384
3516.753269	290416.937462	41.125389
3516.489821	290185.763142	41.130394
3516.381212	289961.996917	41.135399
3516.188164	289734.628336	41.140404
3516.482797	289518.867082	41.145408
3516.174185	289301.366556	41.150413
3516.053472	289081.773946	41.155418
3515.687364	288864.280920	41.160423
3515.661909	288637.976853	41.165428
3515.369483	288429.049685	41.170432
3515.112821	288226.124030	41.175437
3515.067348	288005.014042	41.180442
3514.842693	287806.893404	41.185447
3514.777240	287607.448973	41.190452
3514.530304	287404.239212	41.195456
3514.117007	287210.575783	41.200461
3514.182603	287011.236339	41.205466
3513.957532	286818.306046	41.210471
3513.635363	286632.289305	41.215476
3513.514101	286442.549313	41.220480
3513.368754	286248.713897	41.225485
3513.571831	286066.228420	41.230490
3512.975358	285890.486423	41.235495
3512.959503	285711.190952	41.240500
3513.193771	285527.298967	41.245504
3512.447931	285349.771415	41.250509
3512.631859	285180.320930	41.255514
3512.442211	285013.245099	41.260519
3512.123245	284837.380614	41.265524
3512.294301	284672.767900	41.270528
3512.222452	284513.997217	41.275533
3512.204002	284339.892001	41.280538
3511.514045	284172.561387	41.285543
3511.386094	284020.595689	41.290548
3511.413811	283864.786570	41.295552
3511.190379	283704.306562	41.300557
3511.344870	283547.560412	41.305562
3511.041108	283401.399922	41.310567
3510.915683	283249.610362	41.315572
3510.929722	283095.023680	41.320576
3510.681620	282947.300569	41.325581
3510.449726	282795.908558	41.330586
3510.425698	282667.803973	41.335591
3510.214644	282519.157662	41.340596
3510.301681	282372.755738	41.345600
3509.894162	282245.092231	41.350605
3510.472897	282099.605775	41.355610
3510.322977	281967.191589	41.360615
3509.683558	281827.725146	41.365620
3510.033194	281685.736106	41.370624
3509.748997	281550.974450	41.375629
3509.653191	281418.347124	41.380634
3509.590663	281292.333764	41.385639
3509.817295	281160.292040	41.390644
3509.449109	281028.877718	41.395648
3509.383172	280906.199400	41.400653
3509.187163	280770.149544	41.405658
3508.999428	280661.976284	41.410663
3508.732041	280531.054502	41.415668
3508.737159	280402.152110	41.420672
3508.083842	280293.109094	41.425677
3508.390951	280185.647022	41.430682
3508.391868	280065.146384	41.435687
3508.259338	279949.351006	41.440692
3508.453901	279840.505746	41.445696
3508.292776	279724.408972	41.450701
3507.788965	279616.003547	41.455706
3508.168752	279509.522074	41.460711
3507.778296	279411.333502	41.465716
3507.775545	279297.299021	41.470720
3507.996073	279200.109432	41.475725
3507.830764	279093.254313	41.480730
3507.778993	278993.637407	41.485735
3507.663844	278876.182758	41.490740
3507.404220	278780.264322	41.495744
3507.311083	278688.469742	41.500749
3507.787030	278587.394955	41.505754
3507.175271	278488.450523	41.510759
3507.007242	278387.908975	41.515764
3507.352716	278300.399061	41.520768
3507.067064	278205.145942	41.525773
3507.372361	278100.430909	41.530778
3506.899338	278012.335742	41.535783
3507.098949	277920.392636	41.540788
3507.034924	277826.122817	41.545792
3506.976297	277733.252366	41.550797
3506.827882	277632.681309	41.555802
3506.674809	277550.136908	41.560807
3506.330450	277467.775088	41.565812
3506.421318	277381.653353	41.570816
3506.253956	277297.201375	41.575821
3506.257097	277219.291494	41.580826
3506.160067	277139.640411	41.585831
3506.340014	277060.022327	41.590836
3506.030118	276974.064644	41.595840
3506.407870	276889.934377	41.600845
3505.996125	276814.304044	41.605850
3505.877329	276738.118623	41.610855
3505.818887	276667.525072	41.615860
3506.000215	276579.045924	41.620864
3505.664396	276510.965301	41.625869
3505.902776	276432.941486	41.630874
3505.662714	276364.107402	41.635879
3505.806080	276294.933242	41.640884
3505.788839	276212.493512	41.645888
3505.443381	276146.272736	41.650893
3505.737805	276067.654200	41.655898
3505.547902	275992.574008	41.660903
3505.568584	275924.004313	41.665908
3505.531325	275851.115236	41.670912
3505.267662	275785.059601	41.675917
3505.092599	275707.303408	41.680922
3505.035066	275656.670340	41.685927
3505.232807	275598.078913	41.690932
3505.040754	275527.301559	41.695936
3504.917354	275469.905999	41.700941
3505.418190	275394.819107	41.705946
3505.398991	275329.361413	41.710951
3504.504006	275275.141693	41.715956
3505.020852	275203.744004	41.720960
3504.901687	275140.491456	41.725965
3504.941195	275077.825125	41.730970
3504.758106	275030.928650	41.735975
3504.642341	274960.877256	41.740980
3504.822387	274896.737518	41.745984
3504.806884	274850.018430	41.750989
3504.819657	274787.687055	41.755994
3504.535851	274731.436357	41.760999
3504.563009	274681.273212	41.766004
3504.659054	274620.507301	41.771008
3504.298007	274557.597658	41.776013
3504.380508	274503.886608	41.781018
3504.470082	274450.836417	41.786023
3504.327919	274394.385115	41.791028
3504.227059	274346.787934	41.796032
3504.111765	274304.539909	41.801037
3503.937946	274246.947687	41.806042
3503.941342	274197.271734	41.811047
3504.094205	274150.042159	41.816052
3504.385415	274093.522900	41.821056
3504.056062	274047.361660	41.826061
3504.255436	273999.437265	41.831066
3504.103217	273950.905807	41.836071
3503.825529	273900.713466	41.841076
3503.773927	273853.897616	41.846080
3503.864468	273811.107928	41.851085
3504.002082	273754.306913	41.856090
3504.014865	273719.829857	41.861095
3503.754394	273677.884292	41.866100
3503.707508	273623.378129	41.871104
3503.437904	273581.408482	41.876109
3503.877822	273548.010357	41.881114
3503.782539	273505.809725	41.886119
3503.625107	273461.607306	41.891124
3504.158695	273407.239408	41.896128
3504.056765	273373.976851	41.901133
3504.026314	273323.185353	41.906138
3503.867057	273273.050509	41.911143
3503.609515	273225.248032	41.916148
3503.747109	273174.582945	41.921152
3503.248348	273146.703875	41.926157
3503.375145	273096.727901	41.931162
3503.384823	273060.621499	41.936167
3503.433348	273026.953354	41.941172
3503.251817	272981.303122	41.946176
3502.980864	272962.936609	41.951181
3503.292934	272912.600556	41.956186
3503.473995	272887.365011	41.961191
3503.354369	272856.396597	41.966196
3503.536930	272815.094278	41.971200
3503.004779	272776.475342	41.976205
3502.665979	272739.633963	41.981210
3503.070196	272711.435345	41.986215
3503.072221	272681.924647	41.991220
3503.518908	272650.663924	41.996224
3503.036868	272611.120445	42.001229
3503.456504	272568.635151	42.006234
3503.113425	272535.995597	42.011239
3502.971608	272499.759871	42.016244
3503.029695	272463.518340	42.021248
3503.213658	272423.768803	42.026253
3503.249141	272397.893860	42.031258
3503.041878	272361.897467	42.036263
3502.771842	272337.343378	42.041268
3502.995685	272306.677538	42.046272
3502.397061	272279.934133	42.051277
3503.054053	272248.767698	42.056282
3502.984119	272226.422963	42.061287
3502.968496	272186.042505	42.066292
3503.063076	272161.304050	42.071296
3502.587159	272129.550825	42.076301
3503.048155	272098.414978	42.081306
3503.074017	272068.263788	42.086311
3502.757808	272037.631361	42.091316
3503.021180	272001.943174	42.096320
3502.657248	271965.716489	42.101325
3502.824483	271939.387953	42.106330
3502.480994	271918.893727	42.111335
3502.565347	271892.832758	42.116340
3502.497690	271860.710060	42.121344
3502.170747	271838.481794	42.126349
3502.764936	271805.746357	42.131354
3502.479671	271789.877138	42.136359
3502.644592	271756.852322	42.141364
3502.664100	271735.053650	42.146368
3502.543610	271710.170455	42.151373
3502.593061	271681.619571	42.156378
3502.399962	271656.493090	42.161383
3502.470425	271632.954987	42.166388
3502.754158	271607.932180	42.171392
3502.472721	271587.020778	42.176397
3502.711774	271558.160126	42.181402
3502.537383	271534.813051	42.186407
3502.219994	271511.768413	42.191412
3502.674115	271486.540697	42.196416
3502.511546	271466.552791	42.201421
3502.704915	271436.731670	42.206426
3502.571590	271412.257797	42.211431
3502.584544	271379.180211	42.216436
3502.708502	271355.786445	42.221440
3502.597718	271325.427202	42.226445
3502.577809	271303.201724	42.231450
3502.657810	271282.361056	42.236455
3502.283852	271263.577425	42.241460
3502.379344	271227.431384	42.246464
3502.354423	271208.262162	42.251469
3502.487882	271175.445748	42.256474
3502.583774	271168.988869	42.261479
3502.458495	271140.617903	42.266484
3502.329570	271117.798322	42.271488
3501.995469	271104.661101	42.276493
3502.633817	271064.610749	42.281498
3502.331457	271050.704682	42.286503
3502.143964	271036.144092	42.291508
3502.259878	271017.512986	42.296512
3502.438200	270997.751767	42.301517
3502.426867	270981.890501	42.306522
3502.594640	270943.161328	42.311527
3502.801154	270930.601588	42.316532
3502.579433	270895.650821	42.321536
3502.301198	270874.433200	42.326541
3502.540827	270849.646238	42.331546
3502.581270	270833.012974	42.336551
3502.683993	270811.150139	42.341556
3502.584862	270779.261133	42.346560
3502.542411	270749.858590	42.351565
3502.319540	270724.176322	42.356570
3502.485458	270707.447029	42.361575
3502.199800	270675.816312	42.366580
3502.346742	270653.488199	42.371584
3502.115107	270639.239997	42.376589
3502.293069	270614.971864	42.381594
3502.174939	270599.305465	42.386599
3502.091476	270576.147624	42.391604
3502.400056	270558.046480	42.396608
3502.121203	270539.808007	42.401613
3501.991344	270525.823964	42.406618
3502.367855	270503.383535	42.411623
3502.643312	270490.558329	42.416628
3502.639723	270455.726063	42.421632
3502.400044	270446.240610	42.426637
3502.373456	270418.210464	42.431642
3502.653799	270399.095194	42.436647
3502.377581	270371.231374	42.441652
3502.810662	270344.529788	42.446656
3501.975327	270322.609790	42.451661
3502.329136	270295.054851	42.456666
3502.266522	270286.814835	42.461671
3502.170500	270266.128764	42.466676
3502.208036	270241.373230	42.471680
3502.304260	270222.057544	42.476685
3502.164673	270202.269465	42.481690
3502.561126	270182.626742	42.486695
3502.333148	270154.093281	42.491700
3502.366413	270127.428677	42.496704
3502.044830	270118.872654	42.501709
3502.219157	270091.422102	42.506714
3502.145091	270074.730212	42.511719
3502.485409	270054.994386	42.516724
3502.382820	270031.763008	42.521728
3502.341659	270013.716434	42.526733
3502.326462	269986.422795	42.531738
3502.212680	269972.512542	42.536743
3502.096107	269958.959203	42.541748
3502.476651	269927.580549	42.546752
3502.282041	269906.349627	42.551757
3502.379354	269883.112421	42.556762
3502.276983	269868.156391	42.561767
3502.404975	269844.532437	42.566772
3502.348905	269814.495148	42.571776
3502.476847	269799.681340	42.576781
3502.296543	269773.355576	42.581786
3501.991359	269752.905791	42.586791
3501.901258	269745.637614	42.591796
3502.423821	269728.979698	42.596800
3502.010252	269712.773689	42.601805
3502.033301	269692.603592	42.606810
3502.307236	269676.722961	42.611815
3501.881077	269665.662418	42.616820
3502.212395	269639.536721	42.621824
3502.027327	269621.869048	42.626829
3501.908868	269599.021985	42.631834
3502.181751	269582.632244	42.636839
3502.530835	269560.170408	42.641844
3502.338599	269540.288566	42.646848
3502.170429	269527.150636	42.651853
3502.050470	269503.819988	42.656858
3502.460312	269489.624095	42.661863
3502.145263	269464.516068	42.666868
3502.015586	269434.490162	42.671872
3501.650723	269431.491769	42.676877
3501.842889	269406.686372	42.681882
3501.746515	269396.287202	42.686887
3501.689949	269396.856351	42.691892
3501.992987	269372.415556	42.696896
3501.929271	269359.414051	42.701901
3501.955934	269339.854424	42.706906
3501.502905	269321.566549	42.711911
3501.982946	269303.718444	42.716916
3502.047120	269310.176134	42.721920
3501.721866	269290.671516	42.726925
3501.481067	269270.364336	42.731930
3501.746592	269260.850702	42.736935
3501.433165	269246.436828	42.741940
3501.885625	269232.361548	42.746944
3502.002231	269226.283238	42.751949
3501.884167	269227.905988	42.756954
3501.799256	269208.516555	42.761959
3501.817395	269195.553155	42.766964
3501.915191	269166.993919	42.771968
3501.926335	269161.925151	42.776973
3501.976704	269140.248344	42.781978
3501.596010	269125.361170	42.786983
3501.960772	269098.542589	42.791988
3501.691383	269104.059384	42.796993
3501.748176	269093.050582	42.801997
3501.480888	269073.460466	42.807002
3501.345703	269064.034923	42.812007
3501.402310	269055.139581	42.817012
3501.861935	269046.766881	42.822017
3501.446554	269032.445303	42.827021
3501.449522	269009.757352	42.832026
3501.620100	269008.966912	42.837031
3501.583044	269014.065443	42.842036
3501.647467	268993.022980	42.847041
3501.279082	268977.038946	42.852045
3501.616482	268963.134392	42.857050
3501.490187	268970.767724	42.862055
3501.429655	268960.108270	42.867060
3502.159751	268935.142258	42.872065
3501.685157	268927.755886	42.877069
3501.990484	268923.124912	42.882074
3501.377141	268910.158346	42.887079
3501.892970	268886.931849	42.892084
3501.878472	268879.142521	42.897089
3501.646710	268860.794499	42.902093
3501.746582	268853.343772	42.907098
3501.965620	268844.473942	42.912103
3501.318290	268826.318199	42.917108
3501.936279	268807.811854	42.922113
3501.507870	268814.321126	42.927117
3501.659513	268796.524266	42.932122
3501.609018	268775.372405	42.937127
3501.742581	268772.830792	42.942132
3501.653944	268753.925647	42.947137
3501.430366	268760.148269	42.952141
3501.740289	268741.970168	42.957146
3501.897911	268731.378434	42.962151
3501.723114	268721.042375	42.967156
3501.925292	268715.408991	42.972161
3501.478595	268698.393162	42.977165
3501.478090	268687.877071	42.982170
3501.549317	268675.872900	42.987175
3501.352588	268660.625869	42.992180
3501.628091	268655.541208	42.997185
3501.566106	268655.627408	43.002189
3501.707371	268649.876227	43.007194
3501.943199	268630.945794	43.012199
3501.725989	268620.947376	43.017204
3501.845558	268603.715683	43.022209
3501.490485	268588.977198	43.027213
3501.785125	268566.523635	43.032218
3501.822285	268565.168396	43.037223
3501.647522	268561.732842	43.042228
3501.914384	268541.702621	43.047233
3501.761346	268525.302894	43.052237
3501.724300	268520.801816	43.057242
3501.490690	268505.280431	43.062247
3501.282374	268487.947200	43.067252
3501.596126	268486.497791	43.072257
3501.786702	268477.937935	43.077261
3502.093088	268467.704862	43.082266
3501.976889	268446.435884	43.087271
3501.864043	268436.752152	43.092276
3501.758443	268421.287130	43.097281
3501.763558	268413.469234	43.102285
3501.764900	268399.260651	43.107290
3502.054750	268385.516226	43.112295
3501.792613	268374.786371	43.117300
3501.579970	268358.268617	43.122305
3501.641765	268345.094569	43.127309
3501.963557	268329.308080	43.132314
3502.111814	268318.284889	43.137319
3501.432045	268298.810025	43.142324
3501.740486	268286.208527	43.147329
3501.073290	268298.204308	43.152333
3501.419536	268290.995115	43.157338
3501.599042	268286.281928	43.162343
3501.526327	268266.890393	43.167348
3501.520885	268246.215173	43.172353
3501.583675	268239.763264	43.177357
3501.930543	268239.148962	43.182362
3501.862556	268228.592444	43.187367
3501.589097	268210.021645	43.192372
3501.918368	268201.923883	43.197377
3501.549527	268192.076442	43.202381
3501.808675	268175.281190	43.207386
3501.577657	268161.541775	43.212391
3501.425007	268150.463754	43.217396
3501.673529	268140.112376	43.222401
3501.582446	268133.939149	43.227405
3501.354900	268115.870420	43.232410
3501.407009	268127.295427	43.237415
3501.680617	268122.516593	43.242420
3501.677383	268094.813117	43.247425
3501.705956	268087.984596	43.252429
3501.460154	268082.039262	43.257434
3501.279352	268063.683118	43.262439
3501.668413	268053.589855	43.267444
3501.942046	268044.405855	43.272449
3501.944739	268044.914821	43.277453
3501.666043	268018.527555	43.282458
3501.473583	268004.323749	43.287463
3501.427504	268007.437603	43.292468
3501.449647	267996.917895	43.297473
3501.228671	267986.614438	43.302477
3501.440513	267966.007041	43.307482
3501.547246	267965.735841	43.312487
3501.688183	267961.512471	43.317492
3501.722728	267947.094923	43.322497
3501.364327	267928.562812	43.327501
3501.586917	267916.942295	43.332506
3501.318917	267919.683433	43.337511
3501.335789	267919.706379	43.342516
3501.561900	267911.497404	43.347521
3501.440542	267895.321785	43.352525
3501.531982	267882.957867	43.357530
3501.394869	267875.645967	43.362535
3501.154153	267877.822646	43.367540
3501.504653	267875.170703	43.372545
3501.273783	267880.299596	43.377549
3501.570676	267853.338493	43.382554
3501.616733	267837.671422	43.387559
3501.589254	267836.682765	43.392564
3501.848677	267826.304186	43.397569
3501.740878	267816.110334	43.402573
3501.439585	267810.530145	43.407578
3501.603426	267797.951189	43.412583
3501.325123	267803.876868	43.417588
3501.740637	267785.300125	43.422593
3501.367955	267767.457728	43.427597
3501.864265	267758.875472	43.432602
3501.650799	267762.295601	43.437607
3501.526328	267741.893515	43.442612
3501.460327	267727.364336	43.447617
3501.524718	267721.192239	43.452621
3501.576627	267712.985018	43.457626
3501.614511	267705.823991	43.462631
3501.580276	267690.475010	43.467636
3501.515406	267677.167892	43.472641
3501.676300	267685.291160	43.477645
3501.487668	267670.399193	43.482650
3501.287231	267657.342437	43.487655
3501.694986	267644.699864	43.492660
3501.916938	267633.486828	43.497665
3501.630387	267631.520135	43.502669
3501.818542	267614.735884	43.507674
3501.594030	267600.180540	43.512679
3501.685408	267609.715173	43.517684
3501.876219	267585.877122	43.522689
3501.369902	267580.099802	43.527693
3501.916701	267564.609036	43.532698
3501.877397	267541.978270	43.537703
3501.695630	267535.131668	43.542708
3501.477840	267523.681807	43.547713
3501.466509	267520.882715	43.552717
3501.453522	267508.331367	43.557722
3501.581728	267496.470921	43.562727
3501.541579	267486.852117	43.567732
3501.572215	267480.252403	43.572737
3501.311212	267483.807291	43.577741
3501.795458	267463.641004	43.582746
3501.624601	267438.458968	43.587751
3501.595870	267446.942928	43.592756
3501.968714	267432.701584	43.597761
3501.397056	267406.920149	43.602765
3501.331900	267404.638740	43.607770
3501.716608	267399.766110	43.612775
3501.616355	267385.802432	43.617780
3501.864996	267372.599039	43.622785
3501.588910	267361.896715	43.627789
3501.144359	267354.530986	43.632794
3501.322918	267358.679209	43.637799
3501.272251	267352.677858	43.642804
3501.380953	267330.176685	43.647809
3501.259617	267325.281312	43.652813
3501.212881	267310.545350	43.657818
3501.471299	267315.241288	43.662823
3501.299630	267317.814601	43.667828
3501.499139	267307.063380	43.672833
3501.512303	267304.922505	43.677837
3501.311397	267289.319419	43.682842
3501.398211	267272.270852	43.687847
3501.669432	267287.073819	43.692852
3501.749877	267281.892263	43.697857
3501.395744	267251.340558	43.702861
3501.634194	267235.872483	43.707866
3501.681777	267241.543538	43.712871
3501.389459	267225.852879	43.717876
3501.550154	267215.209570	43.722881
3501.376826	267211.519108	43.727885
3501.440893	267199.897825	43.732890
3501.255677	267204.306636	43.737895
3501.505472	267200.117142	43.742900
3501.638029	267190.878725	43.747905
3501.542987	267180.428176	43.752909
3501.687970	267162.886689	43.757914
3501.471635	267153.753742	43.762919
3501.728499	267152.847942	43.767924
3501.875228	267128.329154	43.772929
3501.407993	267121.909107	43.777933
3501.447144	267122.667014	43.782938
3501.594768	267114.648487	43.787943
3501.460202	267102.243412	43.792948
3501.512308	267083.188615	43.797953
3501.483131	267092.563901	43.802957
3501.370531	267083.261949	43.807962
3501.471303	267073.137264	43.812967
3501.463987	267055.339469	43.817972
3501.394334	267040.276022	43.822977
3501.296232	267038.559954	43.827981
3501.274275	267033.496248	43.832986
3501.697438	267037.071508	43.837991
3501.607407	267035.761596	43.842996
3501.722029	267009.261636	43.848001
3501.842469	267000.738077	43.853005
3501.944308	266978.899950	43.858010
3502.136771	266976.145372	43.863015
3502.094370	266958.836853	43.868020
3501.999316	266948.411744	43.873025
3502.050327	266935.901244	43.878029
3501.772078	266912.976661	43.883034
3501.636324	266893.365534	43.888039
3501.564115	266892.994988	43.893044
3501.796977	266880.863469	43.898049
3501.610424	266867.040527	43.903053
3501.661166	266858.553316	43.908058
3501.783945	266856.675394	43.913063
3501.924005	266846.366299	43.918068
3502.006985	266815.211383	43.923073
3501.669913	266821.961146	43.928077
3501.602413	266794.751154	43.933082
3501.787924	266776.286570	43.938087
3501.897293	266775.098262	43.943092
3501.591372	266768.321943	43.948097
3501.474958	266747.485506	43.953101
3501.777298	266734.018995	43.958106
3502.031891	266723.717444	43.963111
3501.697153	266710.121357	43.968116
3501.456277	266689.100656	43.973121
3501.456237	266688.107698	43.978125
3501.542747	266684.733085	43.983130
3501.504063	266676.539940	43.988135
3501.304391	266666.309403	43.993140
3501.566516	266660.106326	43.998145
3501.204822	266657.743941	44.003149
3501.404538	266643.096667	44.008154
3501.577501	266647.984243	44.013159
3501.497520	266640.510535	44.018164
3501.443087	266617.652747	44.023169
3501.449624	266627.022494	44.028173
3501.564965	266613.890766	44.033178
3501.697032	266599.534163	44.038183
3501.494710	266577.183297	44.043188
3501.840591	266568.089717	44.048193
3501.517142	266568.496898	44.053197
3501.699806	266557.468127	44.058202
3501.536687	266536.842657	44.063207
3501.424821	266537.395005	44.068212
3501.676437	266525.209583	44.073217
3501.974962	266521.114296	44.078221
3501.620750	266510.755122	44.083226
3501.892352	266499.534193	44.088231
3501.620042	266491.734051	44.093236
3501.862747	266464.271761	44.098241
3501.786216	266462.093963	44.103245
3501.567846	266453.546935	44.108250
3501.703833	266443.544000	44.113255
3501.408472	266425.230920	44.118260
3501.741070	266420.926592	44.123265
3501.829480	266418.977644	44.128269
3501.810293	266397.922223	44.133274
3501.968504	266379.181730	44.138279
3501.467099	266374.905933	44.143284
3501.654096	266348.241698	44.148289
3501.255991	266348.151275	44.153293
3501.518851	266330.896776	44.158298
3501.308569	266332.304817	44.163303
3501.364867	266335.351791	44.168308
3501.433883	266325.155604	44.173313
3501.570409	266311.460320	44.178317
3501.610667	266296.939780	44.183322
3501.517735	266293.593207	44.188327
3501.141134	266287.948313	44.193332
3501.398398	266262.724506	44.198337
3501.554046	266264.788325	44.203341
3501.316569	266257.873952	44.208346
3501.243180	266252.894638	44.213351
3501.512394	266252.547104	44.218356
3501.705316	266241.032882	44.223361
3501.498622	266225.685170	44.228365
3501.826918	266222.145421	44.233370
3501.773758	266217.646755	44.238375
3501.451725	266207.384373	44.243380
3501.769200	266183.678962	44.248385
3501.634749	266175.398893	44.253389
3501.685196	266170.985883	44.258394
3501.641394	266152.124148	44.263399
3501.300818	266147.594023	44.268404
3501.550200	266138.133533	44.273409
3501.502287	266144.914526	44.278413
3501.555320	266123.134768	44.283418
3501.618983	266117.548352	44.288423
3501.342343	266105.343611	44.293428
3501.546373	266094.260520	44.298433
3501.481489	266093.175839	44.303437
3501.125593	266093.155209	44.308442
3501.177870	266079.855023	44.313447
3501.482376	266071.633638	44.318452
3501.612851	266060.460188	44.323457
3501.668211	266058.414544	44.328461
3501.279902	266057.023933	44.333466
3501.218676	266037.299128	44.338471
3501.355318	266027.728934	44.343476
3501.752331	266017.405045	44.348481
3501.455019	266023.028235	44.353485
3501.574866	266017.433031	44.358490
3501.420783	266010.963952	44.363495
3501.525222	265993.504988	44.368500
3501.521524	265985.891986	44.373505
3501.393607	265981.965203	44.378509
3501.479365	265980.093052	44.383514
3501.809537	265961.478380	44.388519
3501.508000	265951.161840	44.393524
3501.470552	265940.498444	44.398529
3501.506045	265938.990645	44.403533
3501.701565	265926.635672	44.408538
3501.774808	265899.276112	44.413543
3501.468925	265895.911891	44.418548
3501.847797	265897.482469	44.423553
3501.533092	265887.371691	44.428557
3501.356124	265874.412885	44.433562
3501.351853	265863.591511	44.438567
3501.427660	265862.459367	44.443572
3501.751554	265852.045037	44.448577
3501.479060	265855.067037	44.453581
3501.456567	265838.009849	44.458586
3501.380669	265829.338638	44.463591
3501.159588	265826.215796	44.468596
3501.709144	265820.884430	44.473601
3501.364947	265805.303512	44.478605
3501.326444	265788.910881	44.483610
3501.015052	265789.596282	44.488615
3501.280498	265784.589436	44.493620
3501.250650	265783.983088	44.498625
3501.270720	265790.677085	44.503629
3501.187228	265791.097682	44.508634
3501.784950	265786.115279	44.513639
3501.401282	265769.343721	44.518644
3501.163914	265747.405571	44.523649
3501.496252	265750.587655	44.528653
3501.393046	265746.886175	44.533658
3501.592928	265744.970714	44.538663
3501.444348	265724.011771	44.543668
3501.500591	265713.231848	44.548673
3501.550837	265718.800718	44.553677
3501.125306	265718.689118	44.558682
3501.434929	265712.427628	44.563687
3501.431403	265710.569431	44.568692
3501.726367	265685.721545	44.573697
3501.730483	265673.803888	44.578701
3501.643396	265663.122759	44.583706
3501.576853	265651.419859	44.588711
3501.530673	265638.185935	44.593716
3501.339314	265619.168921	44.598721
3501.558500	265630.033355	44.603725
3501.269539	265622.439459	44.608730
3501.187899	265625.253380	44.613735
3501.242075	265604.670138	44.618740
3501.574652	265593.439576	44.623745
3501.126379	265596.132569	44.628749
3501.264167	265588.624737	44.633754
3501.636615	265592.589938	44.638759
3501.414551	265590.562194	44.643764
3501.703479	265569.076468	44.648769
3501.478195	265561.294364	44.653773
3501.537339	265552.551089	44.658778
3501.754137	265544.674406	44.663783
3501.323427	265530.532954	44.668788
3501.463101	265511.413237	44.673793
3501.435625	265511.290333	44.678797
3501.425600	265499.782291	44.683802
3501.485968	265501.657310	44.688807
3501.331452	265500.408387	44.693812
3501.283079	265468.917091	44.698817
3501.302737	265466.851553	44.703821
3501.242387	265469.764006	44.708826
3501.149542	265456.664675	44.713831
3501.178678	265466.998630	44.718836
3501.228027	265463.909889	44.723841
3501.201224	265470.280203	44.728845
3500.725378	265461.926129	44.733850
3501.536208	265458.387306	44.738855
3501.173746	265451.466953	44.743860
3501.345326	265431.247281	44.748865
3501.270124	265432.506896	44.753869
3501.222570	265426.377621	44.758874
3501.284371	265427.997777	44.763879
3501.417165	265429.606834	44.768884
3501.678318	265420.118973	44.773889
3501.456292	265409.306129	44.778893
3501.219686	265384.974163	44.783898
3501.708385	265381.154667	44.788903
3501.380991	265389.456319	44.793908
3501.737849	265384.537018	44.798913
3501.492843	265374.389829	44.803917
3501.322141	265357.610371	44.808922
3501.608731	265346.896252	44.813927
3501.191341	265348.795039	44.818932
3501.654018	265338.664526	44.823937
3501.471720	265329.398770	44.828941
3501.594176	265314.228636	44.833946
3501.646629	265304.060399	44.838951
3501.060359	265307.513432	44.843956
3501.770629	265298.668338	44.848961
3501.658994	265286.565020	44.853965
3501.420906	265272.164241	44.858970
3501.712169	265277.364422	44.863975
3501.443978	265263.070204	44.868980
3501.636833	265246.463066	44.873985
3501.341660	265247.808002	44.878989
3501.562546	265236.111045	44.883994
3501.837693	265228.250678	44.888999
3501.420847	265215.125578	44.894004
3501.665989	265197.593551	44.899009
3501.466831	265195.918714	44.904013
3501.635849	265184.306253	44.909018
3501.666532	265168.030025	44.914023
3501.640018	265155.531422	44.919028
3501.914388	265144.870121	44.924033
3501.909089	265150.040281	44.929037
3501.589603	265125.975851	44.934042
3501.795325	265119.348607	44.939047
3501.405526	265116.583154	44.944052
3501.195587	265091.177456	44.949057
3501.215649	265078.722491	44.954061
3501.427880	265064.302208	44.959066
3501.411878	265063.006160	44.964071
3501.443973	265064.809215	44.969076
3501.273945	265067.586041	44.974081
3501.479921	265069.158199	44.979085
3501.645391	265048.964870	44.984090
3501.705915	265026.139676	44.989095
3501.688757	265028.026824	44.994100
3501.515522	265004.117750	44.999105
3501.293726	265001.555205	45.004109
3501.233948	264994.612963	45.009114
3501.589692	264985.823269	45.014119
3501.066313	264995.887155	45.019124
3501.358085	264983.517019	45.024129
3501.250331	264988.041137	45.029133
3501.466808	264979.935283	45.034138
3501.324350	264966.767253	45.039143
3501.212430	264953.492590	45.044148
3501.463370	264951.365419	45.049153
3501.057361	264950.537770	45.054157
3501.472826	264942.502659	45.059162
3501.306509	264948.309142	45.064167
3501.423790	264933.037904	45.069172
3501.849880	264909.849962	45.074177
3501.295631	264911.973866	45.079181
3500.810356	264903.315650	45.084186
3501.740993	264903.170275	45.089191
3501.570387	264901.007150	45.094196
3501.170456	264885.409340	45.099201
3501.388486	264878.550979	45.104205
3501.474330	264875.634764	45.109210
3501.701351	264863.860413	45.114215
3501.419691	264864.311995	45.119220
3501.492448	264850.117201	45.124225
3501.384178	264836.510918	45.129229
3501.573881	264832.305256	45.134234
3501.693443	264834.247425	45.139239
3501.385272	264824.135520	45.144244
3501.600693	264801.591630	45.149249
3501.537343	264794.828183	45.154253
3501.359535	264792.258755	45.159258
3501.526746	264788.616820	45.164263
3501.241303	264779.214355	45.169268
3501.109702	264755.655212	45.174273
3501.301299	264746.789304	45.179277
3501.627878	264751.907598	45.184282
3501.421827	264745.726669	45.189287
3501.361459	264746.933045	45.194292
3501.503742	264739.144342	45.199297
3501.527051	264720.195455	45.204301
3501.758474	264715.295733	45.209306
3501.645184	264706.502952	45.214311
3501.436673	264700.016835	45.219316
3501.730029	264673.157281	45.224321
3501.358184	264668.453729	45.229325
3501.165252	264675.232028	45.234330
3501.587614	264673.434550	45.239335
3501.107551	264672.643940	45.244340
3501.456138	264669.457465	45.249345
3501.250638	264646.495527	45.254349
3501.276399	264637.451823	45.259354
3501.485339	264632.224577	45.264359
3501.345312	264635.098582	45.269364
3501.513984	264632.016625	45.274369
3501.532934	264620.045599	45.279373
3501.327196	264607.142058	45.284378
3501.480296	264605.590389	45.289383
3501.286410	264606.435677	45.294388
3501.425175	264596.101090	45.299393
3501.257959	264601.092878	45.304397
3501.231144	264582.228196	45.309402
3501.407006	264567.380637	45.314407
3501.182195	264567.364976	45.319412
3501.382615	264566.111479	45.324417
3501.460017	264567.016211	45.329421
3501.431312	264558.897728	45.334426
3501.628450	264560.725917	45.339431
3501.268507	264539.188635	45.344436
3501.531198	264525.753493	45.349441
3501.268124	264529.970879	45.354445
3501.217460	264529.189528	45.359450
3501.472273	264515.832010	45.364455
3501.063965	264525.699701	45.369460
3501.576996	264498.474723	45.374465
3501.632655	264485.377515	45.379469
3501.351471	264490.972803	45.384474
3501.662454	264485.474954	45.389479
3501.369620	264489.111316	45.394484
3501.440930	264462.133637	45.399489
3501.303006	264461.671500	45.404493
3501.595971	264449.530293	45.409498
3501.925382	264450.726662	45.414503
3501.365574	264440.450346	45.419508
3501.514842	264408.240291	45.424513
3501.595057	264403.516980	45.429517
3501.492030	264399.458923	45.434522
3501.394634	264402.428126	45.439527
3501.306257	264396.941780	45.444532
3501.410073	264364.178603	45.449537
3501.182807	264369.943718	45.454541
3500.987115	264357.853433	45.459546
3501.275296	264357.019106	45.464551
3501.051940	264368.029253	45.469556
3501.231709	264357.560911	45.474561
3501.259809	264359.517389	45.479565
3501.110668	264356.230468	45.484570
3501.264368	264366.545060	45.489575
3501.336380	264343.386883	45.494580
3501.548328	264333.015365	45.499585
3501.188103	264324.235693	45.504589
3501.207028	264321.024353	45.509594
3501.215046	264311.754216	45.514599
3501.334180	264316.293820	45.519604
3501.489588	264319.707324	45.524609
3501.275195	264304.080419	45.529613
3501.260270	264290.179363	45.534618
3501.281357	264290.481759	45.539623
3500.836523	264294.141891	45.544628
3500.647724	264286.557702	45.549633
3501.100170	264282.947548	45.554637
3501.012228	264273.106731	45.559642
3501.408957	264271.185932	45.564647
3501.211579	264265.080012	45.569652
3501.418661	264276.634017	45.574657
3501.165104	264272.268454	45.579661
3501.253368	264268.868022	45.584666
3501.496485	264251.030579	45.589671
3501.412316	264256.289507	45.594676
3501.437064	264234.462840	45.599681
3501.414986	264240.094027	45.604685
3501.235975	264241.675457	45.609690
3501.261524	264243.505014	45.614695
3501.032074	264225.766913	45.619700
3501.175041	264202.674005	45.624705
3501.133144	264212.229797	45.629709
3501.233819	264204.040130	45.634714
3501.301257	264210.064752	45.639719
3501.006251	264206.724239	45.644724
3501.335403	264194.500952	45.649729
3501.467954	264200.948288	45.654733
3501.237390	264200.245989	45.659738
3501.391555	264203.532370	45.664743
3501.229049	264186.038439	45.669748
3501.375485	264175.167861	45.674753
3501.313309	264171.281659	45.679757
3501.339882	264159.742281	45.684762
3501.882154	264152.425751	45.689767
3501.396097	264143.589343	45.694772
3501.316782	264131.302587	45.699777
3501.333557	264128.906437	45.704781
3501.172382	264119.204376	45.709786
3501.192045	264118.870385	45.714791
3501.330915	264122.261017	45.719796
3501.061548	264120.775390	45.724801
3501.424623	264122.577644	45.729805
3501.419516	264106.459631	45.734810
3501.677705	264095.062286	45.739815
3501.207787	264089.661038	45.744820
3501.125421	264059.957131	45.749825
3501.215358	264012.273898	45.754829
3501.157329	263909.508837	45.759834
3501.452124	263773.508369	45.764839
3501.094856	263597.681387	45.769844
3500.871110	263350.787225	45.774849
3500.545410	263069.149264	45.779853
3500.390423	262735.255843	45.784858
3500.080959	262347.985950	45.789863
3499.464625	261925.570237	45.794868
3499.244440	261462.525301	45.799873
3498.636939	260958.871291	45.804877
3498.007272	260404.619180	45.809882
3497.583060	259789.597492	45.814887
3497.090454	259141.529116	45.819892
3496.420094	258449.200339	45.824897
3495.571806	257713.832873	45.829901
3495.088663	256933.634929	45.834906
3494.313668	256105.703519	45.839911
3493.596878	255235.407458	45.844916
3492.515528	254309.518705	45.849921
3491.458924	253343.739299	45.854925
3490.391018	252350.069134	45.859930
3489.852290	251310.087194	45.864935
3488.605205	250220.191695	45.869940
3487.418902	249090.626868	45.874945
3486.022750	247921.816587	45.879949
3485.017997	246700.932646	45.884954
3484.011807	245447.238590	45.889959
3482.319499	244154.092311	45.894964
3481.298008	242817.843265	45.899969
3479.459306	241449.191352	45.904973
3477.885483	240033.297688	45.909978
3476.587866	238579.711124	45.914983
3474.876009	237098.599896	45.919988
3473.418957	235575.571865	45.924993
3471.772562	234011.537286	45.929997
3470.290638	232415.559191	45.935002
3468.621494	230784.789800	45.940007
3466.381838	229132.584656	45.945012
3464.380443	227416.692490	45.950017
3462.806852	225692.530805	45.955021
3460.931191	223929.066293	45.960026
3458.909177	222129.230380	45.965031
3456.733161	220303.111509	45.970036
3454.738065	218439.146995	45.975041
3452.408662	216561.232631	45.980045
3450.011019	214644.012684	45.985050
3448.083744	212697.770908	45.990055
3445.554903	210737.525258	45.995060
3443.246469	208739.693106	46.000065
3440.770154	206712.920676	46.005069
3438.471952	204666.095842	46.010074
3436.101271	202598.038027	46.015079
3433.663849	200503.375622	46.020084
3431.062578	198376.091387	46.025089
3428.230302	196232.116020	46.030093
3425.171442	194059.151875	46.035098
3422.571684	191875.252624	46.040103
3419.643052	189679.780621	46.045108
3417.052858	187459.596877	46.050113
3413.553588	185218.312778	46.055117
3410.519198	182952.763854	46.060122
3407.599589	180671.946819	46.065127
3404.181093	178393.250494	46.070132
3401.230577	176089.257124	46.075137
3398.068882	173784.749482	46.080141
3394.477557	171464.043172	46.085146
3391.327903	169130.583516	46.090151
3387.516052	166794.374372	46.095156
3384.095888	164443.531160	46.100161
3380.668475	162092.580324	46.105165
3377.043356	159736.018226	46.110170
3373.521563	157370.568887	46.115175
3369.451538	155000.016523	46.120180
3365.828408	152620.098833	46.125185
3361.592931	150252.848804	46.130189
3357.367449	147877.186887	46.135194
3353.727662	145518.209549	46.140199
3348.931945	143165.349161	46.145204
3344.471876	140809.786559	46.150209
3340.182388	138477.060402	46.155213
3335.467243	136148.434858	46.160218
3331.201996	133832.171746	46.165223
3326.914748	131443.586958	46.170228
3321.927552	129140.544030	46.175233
3316.569859	126871.517727	46.180237
3311.046421	124626.387425	46.185242
3305.987079	122406.070968	46.190247
3300.057952	120217.986241	46.195252
3294.072369	118064.101548	46.200257
3288.398905	115951.883819	46.205261
3281.991255	113888.854097	46.210266
3275.534081	111854.047477	46.215271
3268.055636	109884.394288	46.220276
3261.746366	107962.774549	46.225281
3254.625045	106111.535231	46.230285
3247.250727	104312.897123	46.235290
3240.055092	102578.429181	46.240295
3231.659584	100920.654715	46.245300
3224.203977	99323.036400	46.250305
3216.155531	97825.636791	46.255309
3208.001529	96388.753595	46.260314
3200.270013	95048.400544	46.265319
3191.873639	93781.175994	46.270324
3184.108350	92571.429739	46.275329
3176.301070	91458.473380	46.280333
3168.565847	90421.987018	46.285338
3161.609225	89453.682767	46.290343
3154.137917	88562.510523	46.295348
3147.282458	87730.194757	46.300353
3140.777460	86963.238860	46.305357
3134.254422	86259.738983	46.310362
3128.466016	85600.656470	46.315367
3122.285184	84987.981272	46.320372
3116.821511	84431.941274	46.325377
3111.427652	83913.871543	46.330381
3106.754585	83433.706374	46.335386
3101.940083	82976.779734	46.340391
3097.461406	82536.728019	46.345396
3092.998966	82125.236030	46.350401
3088.609720	81744.834124	46.355405
3084.588313	81387.586872	46.360410
3080.828476	81041.785961	46.365415
3076.670990	80711.090620	46.370420
3072.937080	80394.546286	46.375425
3068.916989	80086.560417	46.380429
3065.297363	79797.199309	46.385434
3061.616361	79491.694595	46.390439
3058.218598	79220.251903	46.395444
3055.050758	78931.337210	46.400449
3051.458714	78656.818633	46.405453
3048.072572	78380.721075	46.410458
3044.508322	78104.730338	46.415463
3040.998507	77845.105007	46.420468
3038.016503	77571.683006	46.425473
3034.652045	77311.747876	46.430477
3031.247194	77044.963372	46.435482
3027.725766	76768.191972	46.440487
3024.502391	76506.172316	46.445492
3021.305359	76235.007121	46.450497
3017.701382	75956.885287	46.455501
3014.085966	75696.560321	46.460506
3010.706863	75426.752444	46.465511
3007.303301	75172.965049	46.470516
3003.985373	74891.355197	46.475521
3000.138581	74625.196977	46.480525
2996.666902	74366.411670	46.485530
2993.508908	74102.309753	46.490535
2989.956780	73837.878414	46.495540
2986.050505	73579.168681	46.500545
2982.817234	73312.216442	46.505549
2979.217703	73062.187655	46.510554
2975.467493	72806.178487	46.515559
2971.715384	72550.629221	46.520564
2968.348898	72309.116959	46.525569
2964.825153	72059.149268	46.530573
2961.200191	71806.774489	46.535578
2957.271489	71561.890481	46.540583
2953.461718	71315.517234	46.545588
2950.129401	71082.696013	46.550593
2946.489936	70845.087199	46.555597
2942.705686	70610.601312	46.560602
2939.601856	70384.886413	46.565607
2935.733691	70155.229951	46.570612
2932.078712	69923.110716	46.575617
2928.058557	69699.005206	46.580621
2924.562869	69480.285535	46.585626
2921.107775	69256.044692	46.590631
2917.366482	69040.782521	46.595636
2914.099583	68818.103099	46.600641
2910.201793	68604.379906	46.605645
2906.494212	68405.445162	46.610650
2903.182540	68188.440669	46.615655
2899.227300	67991.052345	46.620660
2895.603407	67777.077358	46.625665
2891.856513	67584.369744	46.630669
2888.562755	67388.444188	46.635674
2884.787907	67190.259387	46.640679
2881.141939	66994.899754	46.645684
2877.832908	66805.557312	46.650689
2874.185538	66618.459128	46.655693
2870.434054	66433.974770	46.660698
2867.242585	66243.373995	46.665703
2863.520151	66055.733111	46.670708
2859.645200	65870.300994	46.675713
2856.240799	65684.891854	46.680717
2852.513168	65498.493658	46.685722
2849.356957	65319.529041	46.690727
2845.444005	65151.607705	46.695732
2842.094389	64966.468206	46.700737
2838.678726	64783.333414	46.705741
2835.162374	64612.472029	46.710746
2831.315808	64436.433444	46.715751
2827.653595	64274.597357	46.720756
2824.135602	64094.809451	46.725761
2820.818720	63916.933554	46.730765
2817.275916	63748.379802	46.735770
2813.949524	63576.727799	46.740775
2810.206442	63410.613120	46.745780
2806.859361	63230.233493	46.750785
2803.478893	63056.854507	46.755789
2800.081783	62879.988648	46.760794
2796.631421	62715.146600	46.765799
2792.783061	62547.607118	46.770804
2789.835102	62368.783362	46.775809
2786.208694	62191.913846	46.780813
2782.925178	62013.614781	46.785818
2779.492882	61836.647636	46.790823
2775.825278	61673.985254	46.795828
2772.559080	61484.378031	46.800833
2768.809399	61308.238575	46.805837
2765.051613	61133.263015	46.810842
2761.648845	60955.104493	46.815847
2758.416721	60783.266738	46.820852
2755.127101	60596.811377	46.825857
2751.771203	60426.321822	46.830861
2747.736020	60241.946711	46.835866
2744.829599	60062.035356	46.840871
2741.416712	59887.871459	46.845876
2737.711746	59696.315994	46.850881
2733.944765	59528.289408	46.855885
2730.352318	59346.637647	46.860890
2727.202547	59163.769426	46.865895
2723.288091	58987.450378	46.870900
2720.188873	58806.493343	46.875905
2716.822077	58626.417130	46.880909
2712.813385	58455.929268	46.885914
2709.474087	58267.075522	46.890919
2706.062370	58094.352057	46.895924
2702.588119	57912.362608	46.900929
2699.184674	57734.602166	46.905933
2695.951248	57550.433049	46.910938
2692.198196	57366.492559	46.915943
2688.333752	57186.029050	46.920948
2684.949294	56994.191062	46.925953
2681.339272	56819.490011	46.930957
2677.825028	56644.603937	46.935962
2674.613976	56455.395390	46.940967
2670.826760	56288.530328	46.945972
2667.595728	56100.907618	46.950977
2664.027292	55921.701725	46.955981
2660.682957	55743.654959	46.960986
2657.498506	55559.023999	46.965991
2653.728834	55377.652039	46.970996
2650.463783	55189.236057	46.976001
2647.083624	55005.236418	46.981005
2642.925691	54819.875228	46.986010
2639.996345	54638.954844	46.991015
2636.165852	54458.037219	46.996020
2632.630352	54272.157889	47.001025
2629.207596	54092.004076	47.006029
2625.716488	53907.763878	47.011034
2622.191345	53711.507993	47.016039
2618.536748	53538.436860	47.021044
2615.410910	53349.322273	47.026049
2611.788265	53165.914185	47.031053
2608.296077	52975.762378	47.036058
2604.867481	52790.334832	47.041063
2601.026177	52602.448400	47.046068
2597.696463	52414.140885	47.051073
2594.566114	52231.659127	47.056077
2590.827281	52037.322162	47.061082
2587.566068	51855.828084	47.066087
2583.661357	51670.141361	47.071092
2580.404196	51478.607443	47.076097
2576.678437	51284.217643	47.081101
2573.279148	51106.696769	47.086106
2570.022278	50905.379379	47.091111
2566.300418	50721.346358	47.096116
2562.904325	50531.713339	47.101121
2559.452794	50347.317501	47.106125
2555.848024	50150.095512	47.111130
2552.674421	49956.169708	47.116135
2549.065966	49775.228372	47.121140
2545.497983	49575.011559	47.126145
2541.812408	49388.649236	47.131149
2538.115366	49195.452392	47.136154
2534.880172	48997.858999	47.141159
2531.764593	48817.685408	47.146164
2527.876934	48629.077419	47.151169
2524.565777	48442.036299	47.156173
2521.109742	48244.991395	47.161178
2517.785395	48044.686452	47.166183
2514.191202	47851.630787	47.171188
2510.621469	47661.782315	47.176193
2506.835570	47468.487165	47.181197
2503.416504	47274.806469	47.186202
2500.280515	47075.768149	47.191207
2496.338165	46891.597520	47.196212
2492.986002	46690.985427	47.201217
2489.560880	46509.020266	47.206221
2486.175755	46301.770038	47.211226
2482.865455	46096.190697	47.216231
2479.319354	45913.044260	47.221236
2475.531620	45708.564236	47.226241
2471.867500	45516.503484	47.231245
2468.286142	45317.613794	47.236250
2464.757259	45122.205725	47.241255
2461.388323	44935.399298	47.246260
2457.935279	44739.741718	47.251265
2454.407436	44541.751101	47.256269
2450.942398	44350.829769	47.261274
2447.442360	44152.920701	47.266279
2443.934696	43959.123945	47.271284
2440.267252	43763.166040	47.276289
2436.848293	43566.340261	47.281293
2433.212648	43378.948133	47.286298
2430.138419	43175.102663	47.291303
2426.441996	42992.561788	47.296308
2423.088855	42778.484317	47.301313
2419.648808	42586.306022	47.306317
2415.873508	42402.951668	47.311322
2412.609193	42193.913538	47.316327
2408.925181	42002.355545	47.321332
2404.938496	41802.584267	47.326337
2401.437434	41601.400904	47.331341
2398.001715	41402.174834	47.336346
2394.642169	41217.452784	47.341351
2390.794720	41027.330202	47.346356
2387.801405	40843.549518	47.351361
2384.286425	40638.756640	47.356365
2380.935305	40456.696438	47.361370
2377.468173	40243.054662	47.366375
2374.090594	40051.351698	47.371380
2370.411161	39850.751313	47.376385
2367.272828	39651.044547	47.381389
2363.530923	39452.232920	47.386394
2360.023617	39259.790066	47.391399
2356.350701	39057.496816	47.396404
2353.043722	38854.336676	47.401409
2349.730207	38658.730492	47.406413
2346.197388	38458.050339	47.411418
2342.840601	38254.396437	47.416423
2338.994058	38054.060766	47.421428
2335.586593	37849.397903	47.426433
2332.419120	37643.697761	47.431437
2329.006135	37448.568264	47.436442
2325.342950	37235.747668	47.441447
2322.017665	37033.431746	47.446452
2318.435874	36824.317510	47.451457
2314.617666	36617.600591	47.456461
2311.222601	36423.606070	47.461466
2307.923288	36215.271395	47.466471
2304.471995	36008.426910	47.471476
2300.840074	35797.612643	47.476481
2297.038000	35593.064827	47.481485
2293.488517	35389.056325	47.486490
2290.391951	35179.235755	47.491495
2286.506212	34982.700455	47.496500
2283.218103	34767.063055	47.501505
2280.075647	34553.256014	47.506509
2276.481853	34355.375073	47.511514
2272.849511	34140.799455	47.516519
2269.160690	33945.396662	47.521524
2265.531768	33725.113603	47.526529
2262.477541	33523.676174	47.531533
2259.053742	33311.028671	47.536538
2255.501123	33094.308860	47.541543
2251.648420	32890.188182	47.546548
2248.241683	32671.054032	47.551553
2244.999476	32460.960101	47.556557
2241.403346	32260.798515	47.561562
2238.075372	32041.576253	47.566567
2234.770282	31836.416818	47.571572
2230.876830	31617.667773	47.576577
2227.390080	31410.855058	47.581581
2223.963293	31192.417758	47.586586
2220.691143	30970.745313	47.591591
2216.905064	30763.668996	47.596596
2213.442705	30548.374882	47.601601
2210.213851	30336.082178	47.606605
2206.539226	30125.864054	47.611610
2202.874141	29898.865020	47.616615
2199.161812	29692.073106	47.621620
2196.175065	29471.081897	47.626625
2192.478074	29253.334783	47.631629
2188.867189	29043.922577	47.636634
2185.671931	28830.138243	47.641639
2182.383841	28605.711747	47.646644
2178.919121	28391.593928	47.651649
2175.441772	28168.247446	47.656653
2172.009185	27945.479394	47.661658
2168.405388	27717.449357	47.666663
2165.103995	27499.443581	47.671668
2161.686128	27274.418362	47.676673
2158.244144	27046.269145	47.681677
2154.871047	26826.241436	47.686682
2151.124953	26581.511734	47.691687
2147.796048	26359.853716	47.696692
2144.497996	26119.856113	47.701697
2140.637934	25889.789412	47.706701
2137.169810	25665.784716	47.711706
2133.972754	25428.301314	47.716711
2130.388515	25203.641967	47.721716
2126.816060	24976.303194	47.726721
2123.680400	24736.169946	47.731725
2120.031441	24498.172670	47.736730
2116.687691	24262.284603	47.741735
2112.936148	24030.346853	47.746740
2109.189156	23789.015474	47.751745
2105.953077	23554.386022	47.756749
2102.084527	23321.188721	47.761754
2099.063360	23091.574064	47.766759
2095.309424	22855.583081	47.771764
2092.070463	22615.934955	47.776769
2088.623994	22385.368704	47.781773
2084.717011	22141.941079	47.786778
2081.515751	21906.806158	47.791783
2077.492269	21670.516705	47.796788
2074.567419	21435.825588	47.801793
2070.882987	21202.725764	47.806797
2067.012336	20974.681209	47.811802
2063.736333	20739.584562	47.816807
2059.581751	20522.808199	47.821812
2055.796235	20284.046704	47.826817
2052.175688	20056.176383	47.831821
2048.292598	19838.617657	47.836826
2045.467576	19617.424650	47.841831
2041.620060	19398.155024	47.846836
2038.010721	19181.681921	47.851841
2034.619602	18961.205663	47.856845
2030.670483	18737.633248	47.861850
2027.309119	18521.882416	47.866855
2023.425764	18312.321422	47.871860
2020.039918	18101.690453	47.876865
2016.711600	17896.290697	47.881869
2012.626694	17694.735650	47.886874
2009.565397	17477.271087	47.891879
2005.920677	17273.092821	47.896884
2002.139289	17073.966803	47.901889
1998.956634	16874.790322	47.906893
1994.804786	16668.680648	47.911898
1990.879374	16477.525227	47.916903
1987.251565	16299.428373	47.921908
1983.301043	16100.446560	47.926913
1979.377494	15927.630544	47.931917
1976.009841	15754.741770	47.936922
1972.359874	15564.891765	47.941927
1968.992929	15391.258883	47.946932
1965.194643	15227.776845	47.951937
1961.709448	15052.341709	47.956941
1958.323355	14883.228504	47.961946
1954.524451	14715.343427	47.966951
1951.174904	14550.736269	47.971956
1947.632733	14375.667737	47.976961
1944.337934	14212.850197	47.981965
1940.538108	14041.729007	47.986970
1937.002786	13867.604445	47.991975
1934.035855	13710.932917	47.996980
1930.756794	13529.191637	48.001985
1927.201336	13362.853984	48.006989
1923.396172	13207.387924	48.011994
1920.304270	13018.501814	48.016999
1916.088162	12854.785832	48.022004
1912.830710	12686.159651	48.027009
1909.387345	12517.051188	48.032013
1905.812051	12360.479723	48.037018
1902.490097	12182.949774	48.042023
1898.591673	12008.452782	48.047028
1895.373582	11849.379309	48.052033
1892.346448	11683.907719	48.057037
1888.678800	11503.576404	48.062042
1885.085116	11332.697635	48.067047
1881.535470	11168.477349	48.072052
1877.885570	10996.682891	48.077057
1874.615106	10836.771474	48.082061
1870.798663	10660.963625	48.087066
1867.892491	10492.327509	48.092071
1863.980441	10330.900041	48.097076
1860.845664	10166.579326	48.102081
1856.893756	9993.578312	48.107085
1853.435036	9831.653724	48.112090
1850.191046	9652.432557	48.117095
1846.740642	9493.548447	48.122100
1842.789666	9323.567012	48.127105
1839.792602	9143.197897	48.132109
1836.187835	8972.950253	48.137114
1832.988146	8800.279465	48.142119
1829.519119	8626.987726	48.147124
1825.745544	8454.428964	48.152129
1822.112000	8289.133072	48.157133
1818.679245	8122.278451	48.162138
1815.327099	7939.852788	48.167143
1811.720257	7769.470962	48.172148
1808.183679	7600.329932	48.177153
1804.963792	7436.584826	48.182157
1801.157871	7260.139773	48.187162
1797.898269	7087.969145	48.192167
1794.486358	6916.111980	48.197172
1790.574049	6743.005453	48.202177
1787.169858	6569.779901	48.207181
1783.546187	6415.525916	48.212186
1780.286249	6239.002083	48.217191
1776.644419	6072.097532	48.222196
1773.298483	5899.419893	48.227201
1769.676115	5727.527706	48.232205
1766.375095	5555.055171	48.237210
1762.673637	5379.273343	48.242215
1758.987184	5221.108700	48.247220
1755.377234	5051.243191	48.252225
1751.875714	4873.162735	48.257229
1748.683601	4708.390226	48.262234
1745.057784	4536.968694	48.267239
1742.029492	4367.670452	48.272244
1738.273231	4197.085836	48.277249
1734.496869	4022.819349	48.282253
1731.199306	3858.868515	48.287258
1728.079443	3670.699324	48.292263
1723.951327	3510.577679	48.297268
1720.365531	3340.313061	48.302273
1716.851449	3173.937290	48.307277
1713.203863	3002.777366	48.312282
1710.000041	2821.253067	48.317287
1706.685614	2667.254692	48.322292
1703.188461	2498.588434	48.327297
1699.413740	2320.667651	48.332301
1695.966653	2157.866326	48.337306
1692.512486	1986.040326	48.342311
1688.503209	1824.073587	48.347316
1685.035467	1653.768503	48.352321
1681.922202	1492.297352	48.357325
1678.140711	1339.959170	48.362330
1674.826573	1168.770889	48.367335
1670.945157	1010.287719	48.372340
1667.137925	847.285752	48.377345
1663.494836	700.056940	48.382349
1659.455721	539.406896	48.387354
1655.983113	378.571562	48.392359
1651.616227	241.217130	48.397364
1647.609800	120.094576	48.402369
1642.447670	23.350312	48.407373
1632.878353	71.317797	48.412378
1626.812433	63.225185	48.417383
1622.407883	74.089407	48.422388
1619.367748	68.604762	48.427393
1617.155637	63.768817	48.432397
1614.377784	72.268199	48.437402
1611.538771	68.134655	48.442407
1608.406284	66.926092	48.447412
1605.101517	69.579005	48.452417
1601.790441	67.272087	48.457421
1598.099578	70.611861	48.462426
1594.557391	64.883096	48.467431
1591.247224	65.413957	48.472436
1588.044239	66.067250	48.477441
1584.559156	72.431040	48.482445
1581.093906	67.285031	48.487450
1577.707773	69.223017	48.492455
1574.298953	74.375799	48.497460
1570.882607	66.659471	48.502465
1567.684750	71.500822	48.507469
1564.553971	69.516877	48.512474
1560.904436	73.495608	48.517479
1557.033043	72.788694	48.522484
1553.319827	73.290901	48.527489
1550.325037	68.884362	48.532493
1546.671899	69.367677	48.537498
1543.095566	69.465644	48.542503
1539.617784	68.804699	48.547508
1536.544223	77.878735	48.552513
1533.317327	75.897188	48.557517
1529.579033	79.987901	48.562522
1525.952890	67.761229	48.567527
1522.457877	65.495783	48.572532
1518.846270	74.470537	48.577537
1515.808187	64.527833	48.582541
1512.079807	70.562725	48.587546
1508.600181	66.029606	48.592551
1505.014130	70.950717	48.597556
1501.365551	84.208706	48.602561
1498.246084	71.994488	48.607565
1494.935516	73.446105	48.612570
1491.533416	68.796451	48.617575
1487.862971	75.828368	48.622580
1484.494565	60.938600	48.627585
1480.518743	68.945305	48.632589
1476.856685	78.570217	48.637594
1473.672420	71.257367	48.642599
1470.403234	77.827846	48.647604
1466.735340	69.315694	48.652609
1463.489651	73.515985	48.657613
1460.184498	68.291179	48.662618
1456.751008	62.498000	48.667623
1452.833816	62.959404	48.672628
1449.109569	66.924555	48.677633
1446.096972	66.725507	48.682637
1442.435607	73.192863	48.687642
1439.053846	68.422986	48.692647
1435.360328	73.933586	48.697652
1431.773418	73.251795	48.702657
1428.649301	69.036384	48.707661
1424.584526	72.672029	48.712666
1421.450643	62.352049	48.717671
1418.226462	70.244284	48.722676
1415.101335	68.901751	48.727681
1411.596041	59.994013	48.732685
1407.563173	69.025245	48.737690
1404.023442	63.748594	48.742695
1400.436566	71.435013	48.747700
1396.910407	66.845945	48.752705
1393.829175	72.314500	48.757709
1389.562798	80.224350	48.762714
1386.665345	68.696771	48.767719
1383.313975	73.960840	48.772724
1379.552440	68.880271	48.777729
1376.327793	65.683535	48.782733
1372.568972	65.345053	48.787738
1369.352633	63.422023	48.792743
1365.737925	75.007425	48.797748
1362.294642	73.486920	48.802753
1358.774042	72.899180	48.807757
1354.850366	73.757110	48.812762
1351.689533	67.804230	48.817767
1348.252929	70.639212	48.822772
1344.140169	61.035648	48.827777
1341.325549	68.250017	48.832781
1337.677583	62.053857	48.837786
1334.140074	60.389924	48.842791
1330.669519	66.242144	48.847796
1327.151291	68.479300	48.852801
1323.664154	70.259170	48.857805
1319.585556	75.184677	48.862810
1316.626282	65.685298	48.867815
1313.715418	63.268376	48.872820
1309.872499	65.037505	48.877825
1306.455132	58.824244	48.882829
1302.623146	69.589452	48.887834
1298.868241	64.602794	48.892839
1295.590278	66.818167	48.897844
1292.159150	60.186284	48.902849
1288.914400	68.553174	48.907853
1284.863794	65.419329	48.912858
1281.845453	66.973964	48.917863
1278.042118	69.179838	48.922868
1274.542799	64.295549	48.927873
1271.084746	69.165060	48.932877
1267.750269	64.729535	48.937882
1264.567243	58.099953	48.942887
1260.610705	63.329077	48.947892
1257.189052	70.379064	48.952897
1253.891394	70.711922	48.957901
1250.073274	66.513470	48.962906
1247.140801	55.845657	48.967911
1243.482436	67.842885	48.972916
1239.363443	76.289704	48.977921
1236.372430	71.060096	48.982925
1232.619010	71.613008	48.987930
1228.970186	61.180731	48.992935
1225.673749	71.194566	48.997940
1222.311944	67.383437	49.002945
1218.450067	68.804389	49.007949
1214.763198	67.382184	49.012954
1211.966605	63.261111	49.017959
1208.398706	61.364700	49.022964
1204.773512	67.415175	49.027969
1201.477850	68.064116	49.032973
1197.474597	69.763475	49.037978
1193.725039	75.241799	49.042983
1190.650856	70.683294	49.047988
1187.279313	71.166948	49.052993
1183.725817	72.770591	49.057997
1180.138975	74.037769	49.063002
1176.902312	69.422448	49.068007
1173.486136	72.681399	49.073012
1169.952654	81.666171	49.078017
1166.468335	74.235897	49.083021
1162.640200	80.919278	49.088026
1159.051237	75.995283	49.093031
1155.637605	71.762018	49.098036
1152.091983	74.667916	49.103041
1148.590178	80.022047	49.108045
1144.708116	81.620196	49.113050
1141.667042	79.495796	49.118055
1138.466137	73.473337	49.123060
1134.584353	71.467905	49.128065
1131.135054	67.964740	49.133069
1127.090222	79.465687	49.138074
1124.038515	66.867697	49.143079
1120.719059	71.721883	49.148084
1117.280116	72.946945	49.153089
1113.713965	70.506126	49.158093
1110.175110	76.429221	49.163098
1106.953250	75.462605	49.168103
1103.278029	77.667469	49.173108
1099.531886	82.003169	49.178113
1095.858040	70.973748	49.183117
1092.475987	76.745748	49.188122
1089.273208	68.309643	49.193127
1085.730837	76.969960	49.198132
1082.161902	78.645660	49.203137
1078.871163	67.474010	49.208141
1075.271946	74.456939	49.213146
1071.922153	79.224142	49.218151
1068.106050	77.088231	49.223156
1064.239067	77.048379	49.228161
1061.106628	59.198541	49.233165
1057.641627	71.576837	49.238170
1054.199779	69.176692	49.243175
1050.708837	72.589758	49.248180
1046.832867	76.142204	49.253185
1043.662318	63.866579	49.258189
1040.156489	67.528753	49.263194
1036.713998	62.717922	49.268199
1032.925381	59.872203	49.273204
1029.394892	61.399532	49.278209
1026.556189	62.606576	49.283213
1022.460415	76.358645	49.288218
1019.335143	66.572158	49.293223
1015.683896	76.113252	49.298228
1012.037899	76.576663	49.303233
1008.415508	70.822729	49.308237
1005.026006	74.681839	49.313242
1001.523641	72.563273	49.318247
998.520413	76.969350	49.323252
994.572441	74.746549	49.328257
991.027103	76.371130	49.333261
987.335838	70.653300	49.338266
984.159994	67.002971	49.343271
980.436922	70.756129	49.348276
977.211674	65.291207	49.353281
973.483203	62.255760	49.358285
969.699142	71.852463	49.363290
966.237600	65.019829	49.368295
962.981952	65.991617	49.373300
959.641351	74.652016	49.378305
956.684667	57.543508	49.383309
952.646804	67.572261	49.388314
949.250429	69.885381	49.393319
945.566261	65.077625	49.398324
941.999372	70.926067	49.403329
938.721534	62.043033	49.408333
934.996866	68.545771	49.413338
931.810125	72.246605	49.418343
927.920094	66.651674	49.423348
924.220931	65.759859	49.428353
921.072259	65.680358	49.433357
917.701385	68.160339	49.438362
914.084086	60.836423	49.443367
910.411367	68.833825	49.448372
906.818618	68.991544	49.453377
903.653003	65.096034	49.458381
900.028684	68.242132	49.463386
896.404309	70.559333	49.468391
893.099792	70.770002	49.473396
889.525720	67.302287	49.478401
886.181515	58.999147	49.483405
882.649633	61.023458	49.488410
878.816600	66.299822	49.493415
875.413553	62.574380	49.498420
871.693613	64.587013	49.503425
868.791822	65.835620	49.508429
864.936749	61.146411	49.513434
861.490046	65.273952	49.518439
858.217086	61.344648	49.523444
854.423093	59.328754	49.528449
851.379134	61.346276	49.533453
847.200188	73.776313	49.538458
843.708753	72.798217	49.543463
840.264782	61.027409	49.548468
836.950190	66.725646	49.553473
833.280825	67.876157	49.558477
829.744589	67.183494	49.563482
826.717475	66.784433	49.568487
823.081473	70.773950	49.573492
819.765922	75.099269	49.578497
816.299418	64.334914	49.583501
811.958060	68.786066	49.588506
808.791908	68.582790	49.593511
805.145756	64.961882	49.598516
801.772437	77.800457	49.603521
798.306012	74.600661	49.608525
794.716379	73.261473	49.613530
791.504157	59.850370	49.618535
788.154686	75.080181	49.623540
784.615630	70.050453	49.628545
781.154585	63.141891	49.633549
777.193925	68.789457	49.638554
773.833038	74.260845	49.643559
770.927909	75.620736	49.648564
767.031665	70.121765	49.653569
763.383464	66.782771	49.658573
759.678699	62.440232	49.663578
756.266588	64.430014	49.668583
752.875647	69.516971	49.673588
748.980086	65.732663	49.678593
745.802169	67.897747	49.683597
742.317011	80.304598	49.688602
739.025852	69.712134	49.693607
735.559660	67.834781	49.698612
732.177387	64.890755	49.703617
728.271943	53.780733	49.708621
724.906689	64.077555	49.713626
721.044824	67.026799	49.718631
717.542522	63.924406	49.723636
714.595488	62.937036	49.728641
711.168485	62.138727	49.733645
707.356821	64.858652	49.738650
703.640311	53.276128	49.743655
700.120041	51.948264	49.748660
696.612550	60.185612	49.753665
693.766732	53.857789	49.758669
689.852881	66.034387	49.763674
686.240320	64.926624	49.768679
682.820918	69.242940	49.773684
679.413064	72.051497	49.778689
675.915059	72.580446	49.783693
672.109095	74.720524	49.788698
668.364205	69.716753	49.793703
665.040276	67.260327	49.798708
661.622500	59.405405	49.803713
658.396672	62.125350	49.808717
654.960488	73.072384	49.813722
651.254100	69.644473	49.818727
647.808505	73.477683	49.823732
644.147795	75.990495	49.828737
640.804390	68.449798	49.833741
637.119578	74.566747	49.838746
633.677061	69.521964	49.843751
630.569325	69.436152	49.848756
626.538855	69.475869	49.853761
623.468128	68.574340	49.858765
619.701315	74.299176	49.863770
616.171144	72.191444	49.868775
612.914484	66.823334	49.873780
609.196390	67.374122	49.878785
605.799115	66.188382	49.883789
602.114152	77.579357	49.888794
598.642041	72.871418	49.893799
595.228360	70.960587	49.898804
591.366181	76.228969	49.903809
588.159781	69.669750	49.908813
584.699140	72.347402	49.913818
581.654975	67.708490	49.918823
578.396235	67.440701	49.923828
574.220286	74.564738	49.928833
570.453532	64.268303	49.933837
566.833677	75.734512	49.938842
563.590324	71.152112	49.943847
560.281436	61.287012	49.948852
556.745931	71.145476	49.953857
553.460547	62.137240	49.958861
549.501762	71.539980	49.963866
546.280487	64.359849	49.968871
543.292955	58.579460	49.973876
539.220890	70.977041	49.978881
535.480872	66.276290	49.983885
531.617434	69.143598	49.988890
528.787208	64.556621	49.993895
525.285637	58.534045	49.998900
521.818432	67.568735	50.003905
518.347730	64.414017	50.008909
514.773360	69.653168	50.013914
511.251187	67.158248	50.018919
507.530420	61.499041	50.023924
503.833721	67.263556	50.028929
500.697587	63.344599	50.033933
496.647785	68.395629	50.038938
493.732143	58.494277	50.043943
490.305988	62.697819	50.048948
487.034414	68.430555	50.053953
483.366193	65.847791	50.058957
479.204743	68.005659	50.063962
476.266821	59.009475	50.068967
472.723425	68.834398	50.073972
469.065677	63.007150	50.078977
465.443767	50.622158	50.083981
462.106994	71.143013	50.088986
458.605700	64.832519	50.093991
454.773471	57.023623	50.098996
451.522099	65.796738	50.104001
448.142799	66.990552	50.109005
444.751519	65.671058	50.114010
441.411858	66.089873	50.119015
437.605739	63.566693	50.124020
434.020452	58.452613	50.129025
430.510314	55.196543	50.134029
426.609387	59.607348	50.139034
423.450981	59.855410	50.144039
419.875347	62.547969	50.149044
416.434551	65.415562	50.154049
413.330889	59.204158	50.159053
409.931123	60.214530	50.164058
406.490401	59.000872	50.169063
402.746359	60.188560	50.174068
398.609055	61.257514	50.179073
395.264858	59.696547	50.184077
391.955530	69.975214	50.189082
388.617942	56.283383	50.194087
385.271431	66.770354	50.199092
381.466505	63.003658	50.204097
377.991527	58.862578	50.209101
374.229695	68.013067	50.214106
370.677806	58.692318	50.219111
367.551364	64.149257	50.224116
364.014897	78.244201	50.229121
360.325320	66.461473	50.234125
356.964444	59.505772	50.239130
353.551808	58.879357	50.244135
350.196220	66.017347	50.249140
346.497584	66.666434	50.254145
343.013150	64.054942	50.259149
339.402909	61.789026	50.264154
335.849497	60.656323	50.269159
332.664825	72.690346	50.274164
328.686331	63.676886	50.279169
325.265725	66.063622	50.284173
321.794054	68.268534	50.289178
318.693719	65.312147	50.294183
314.973825	69.188441	50.299188
311.349213	72.502482	50.304193
308.153247	66.577660	50.309197
304.316546	66.625133	50.314202
300.832777	69.784238	50.319207
297.477622	74.894215	50.324212
293.984778	78.450213	50.329217
291.007871	64.584866	50.334221
286.568056	65.052690	50.339226
283.406445	63.447346	50.344231
280.128037	62.005832	50.349236
276.026338	72.335891	50.354241
272.547564	67.385529	50.359245
269.021068	77.881752	50.364250
265.833496	70.933739	50.369255
262.548151	74.754636	50.374260
259.095008	73.232934	50.379265
255.493599	67.381139	50.384269
252.213995	72.928548	50.389274
248.771825	71.253271	50.394279
245.001363	69.297230	50.399284
241.358714	67.628053	50.404289
237.753548	74.672301	50.409293
234.150826	72.250226	50.414298
230.598800	64.745557	50.419303
227.354260	70.198895	50.424308
223.644082	79.388805	50.429313
220.241913	66.207041	50.434317
217.019319	73.526721	50.439322
213.638715	60.930043	50.444327
209.594293	58.710054	50.449332
206.178765	66.107416	50.454337
203.074312	69.773444	50.459341
199.337854	71.855369	50.464346
195.578340	72.865232	50.469351
192.179220	65.722604	50.474356
188.800083	63.493313	50.479361
185.672859	61.227723	50.484365
181.831008	62.345403	50.489370
178.185727	60.423566	50.494375
174.607305	61.537945	50.499380
171.338478	60.506259	50.504385
167.945432	57.924817	50.509389
164.412869	64.489479	50.514394
160.838409	62.265490	50.519399
157.417442	59.372051	50.524404
153.638087	67.028909	50.529409
150.131672	55.227095	50.534413
146.497902	65.964782	50.539418
143.416335	59.303938	50.544423
139.898731	60.086101	50.549428
136.132209	66.962673	50.554433
132.752245	59.484879	50.559437
129.271449	65.079665	50.564442
125.971138	55.675331	50.569447
122.365660	57.202093	50.574452
118.785932	64.628371	50.579457
115.373190	51.182573	50.584461
111.515196	64.084598	50.589466
108.473880	62.928707	50.594471
104.858121	58.708562	50.599476
101.240018	61.667323	50.604481
97.559867	63.322853	50.609485
94.221230	61.998415	50.614490
91.084599	55.643613	50.619495
87.455944	54.975218	50.624500
83.564099	65.114282	50.629505
80.087898	59.141714	50.634509
76.306855	65.640934	50.639514
73.038002	63.751915	50.644519
69.840223	61.826452	50.649524
65.955536	67.573125	50.654529
62.621118	62.132006	50.659533
58.776038	71.991673	50.664538
55.621759	70.859827	50.669543
52.406387	65.010919	50.674548
48.436600	69.084657	50.679553
45.488992	61.102566	50.684557
41.657766	65.774690	50.689562
37.972060	62.549458	50.694567
34.552116	64.917216	50.699572
30.995424	69.799432	50.704577
28.216835	67.422330	50.709581
24.055610	73.136419	50.714586
20.522408	73.582553	50.719591
17.357241	71.212239	50.724596
13.766758	66.763547	50.729601
10.021306	63.126911	50.734605
6.785637	67.541223	50.739610
3.166283	65.074399	50.744615