Fri Mar 05 19:12:35 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.238782	105.356017	0.000000
0.028995	88.114501	0.005005
-0.953035	58.712177	0.010010
-2.832807	26.504197	0.015014
-6.353580	-17.106646	0.020019
-12.089033	-5.671063	0.025024
-17.424729	-17.406185	0.030029
-21.719632	-18.479998	0.035034
-25.974139	-11.487873	0.040038
-29.463939	-18.471157	0.045043
-33.562321	-20.746384	0.050048
-36.866832	-22.071176	0.055053
-40.259475	-19.220354	0.060058
-44.338098	-4.076645	0.065062
-48.114315	-17.820306	0.070067
-52.516451	-15.229492	0.075072
-56.017600	-13.837359	0.080077
-59.340711	-16.966329	0.085082
-63.159934	-11.760865	0.090086
-66.635687	-20.067810	0.095091
-70.371531	-21.289060	0.100096
-74.386685	-15.859939	0.105101
-78.492088	-15.281282	0.110106
-82.208050	-16.540378	0.115110
-85.643607	-12.269707	0.120115
-89.537709	-14.515926	0.125120
-93.490212	-15.623732	0.130125
-97.008536	-18.636354	0.135130
-101.054606	-15.693826	0.140134
-104.462836	-17.583870	0.145139
-108.312518	-9.886641	0.150144
-111.628242	-11.152772	0.155149
-115.678029	-10.537193	0.160154
-119.749422	-12.740887	0.165158
-123.294727	-13.263906	0.170163
-127.422091	-19.043045	0.175168
-131.121053	-7.031659	0.180173
-134.604691	-15.505979	0.185178
-138.381499	-9.704775	0.190182
-142.279589	-20.834760	0.195187
-146.050597	-18.565243	0.200192
-149.869859	-16.951913	0.205197
-153.532887	-12.859321	0.210202
-157.537725	-5.733345	0.215206
-160.479495	-21.018156	0.220211
-164.790684	-16.345898	0.225216
-168.478981	-15.234402	0.230221
-172.070605	-16.306619	0.235226
-176.034096	-14.318578	0.240230
-179.406629	-20.588644	0.245235
-184.161085	-7.338029	0.250240
-188.094291	-16.202577	0.255245
-191.462366	-13.984668	0.260250
-195.092213	-12.865111	0.265254
-198.702647	-17.606981	0.270259
-202.733290	-16.136457	0.275264
-206.160350	-8.970137	0.280269
-209.984161	-13.871906	0.285274
-213.842497	-18.022265	0.290278
-217.447121	-19.715230	0.295283
-221.184926	-12.814693	0.300288
-225.180918	-17.252147	0.305293
-228.624909	-13.113975	0.310298
-232.447978	-7.079745	0.315302
-235.900965	-17.348627	0.320307
-240.240928	-14.642821	0.325312
-243.942644	-14.666043	0.330317
-247.630662	-16.820313	0.335322
-251.655999	-14.992590	0.340326
-255.110017	-14.323624	0.345331
-258.658688	-11.688874	0.350336
-262.411620	-12.129668	0.355341
-266.308479	-14.701585	0.360346
-270.402771	-17.101638	0.365350
-274.005070	-22.458117	0.370355
-278.032462	-17.539223	0.375360
-281.307858	-24.281953	0.380365
-284.977406	-15.924088	0.385370
-289.051185	-15.301238	0.390374
-292.298310	-17.696116	0.395379
-296.403848	-17.844038	0.400384
-300.606658	-21.803656	0.405389
-304.051824	-19.082861	0.410394
-307.953522	-12.473001	0.415398
-311.270751	-16.247525	0.420403
-315.350341	-12.982331	0.425408
-319.166232	-12.820058	0.430413
-322.692563	-11.910798	0.435418
-326.847751	-14.162263	0.440422
-330.522695	-14.181741	0.445427
-334.341717	-6.154752	0.450432
-337.665373	-15.187302	0.455437
-341.405395	-15.811381	0.460442
-345.541353	-6.939008	0.465446
-348.925987	-20.350424	0.470451
-352.982029	-15.330642	0.475456
-357.072507	-17.001033	0.480461
-360.582457	-16.010755	0.485466
-363.965506	-15.245731	0.490470
-367.606634	-20.658945	0.495475
-371.799361	-16.793707	0.500480
-375.659577	-22.045777	0.505485
-379.284831	-14.120620	0.510490
-383.737324	-10.937706	0.515494
-386.889380	-18.567294	0.520499
-390.353282	-16.043657	0.525504
-394.143308	-11.214507	0.530509
-397.887990	-19.578936	0.535514
-401.985825	-11.688684	0.540518
-405.619211	-19.865867	0.545523
-409.547537	-10.197073	0.550528
-413.169027	-22.556601	0.555533
-416.868574	-16.101850	0.560538
-420.688886	-18.338807	0.565542
-424.411096	-22.723438	0.570547
-428.340787	-19.977148	0.575552
-431.800216	-16.438620	0.580557
-435.699005	-22.066050	0.585562
-439.610503	-14.412069	0.590566
-442.796368	-24.119309	0.595571
-446.873125	-12.864017	0.600576
-450.861185	-21.476500	0.605581
-454.553300	-24.684762	0.610586
-458.873148	-25.640270	0.615590
-462.114622	-32.746116	0.620595
-465.672706	-14.835376	0.625600
-469.380469	-19.518706	0.630605
-473.441667	-18.303049	0.635610
-477.147156	-8.893657	0.640614
-480.516634	-26.631240	0.645619
-484.950154	-18.759793	0.650624
-488.453119	-23.210870	0.655629
-491.898826	-19.641334	0.660634
-495.997532	-14.619236	0.665638
-499.347243	-21.020207	0.670643
-503.586197	-5.913276	0.675648
-507.200176	-17.132152	0.680653
-511.128381	-16.590520	0.685658
-514.920691	-12.880445	0.690662
-518.385489	-21.115907	0.695667
-522.393369	-12.386705	0.700672
-525.849742	-18.344832	0.705677
-529.693082	-20.221548	0.710682
-533.447709	-23.653088	0.715686
-537.033123	-24.080781	0.720691
-541.169898	-18.216755	0.725696
-545.022915	-23.181112	0.730701
-548.642595	-14.206367	0.735706
-552.344140	-14.941915	0.740710
-555.907793	-19.305928	0.745715
-560.040297	-14.101709	0.750720
-563.605521	-21.911059	0.755725
-567.171456	-22.354433	0.760730
-571.241979	-14.722156	0.765734
-574.895925	-15.375387	0.770739
-578.919449	-9.813231	0.775744
-582.519890	-15.067027	0.780749
-585.813565	-15.832978	0.785754
-590.061219	-16.487546	0.790758
-593.647706	-20.316427	0.795763
-597.497388	-19.402425	0.800768
-601.131584	-16.944326	0.805773
-605.043902	-17.800664	0.810778
-608.910525	-10.357011	0.815782
-612.258053	-15.701621	0.820787
-616.283521	-11.597758	0.825792
-620.541197	-15.216882	0.830797
-624.043445	-17.729819	0.835802
-627.877886	-15.230231	0.840806
-630.878889	-14.517978	0.845811
-634.970256	-12.824148	0.850816
-638.742305	-4.936667	0.855821
-642.755646	-14.292243	0.860826
-646.496417	-9.263997	0.865830
-650.048785	-23.165377	0.870835
-653.747285	-10.675523	0.875840
-657.672537	-10.419548	0.880845
-661.435616	-7.768882	0.885850
-665.379390	-13.466009	0.890854
-668.815629	-22.123688	0.895859
-672.892719	-18.173910	0.900864
-676.490446	-15.032406	0.905869
-680.403115	-19.307351	0.910874
-684.157958	-7.281529	0.915878
-687.267344	-18.334724	0.920883
-691.152703	-16.869253	0.925888
-695.179444	-18.207047	0.930893
-699.270177	-23.014896	0.935898
-703.339166	-6.586525	0.940902
-706.762803	-16.873556	0.945907
-710.262417	-18.650357	0.950912
-713.875476	-17.712474	0.955917
-717.889887	-18.265311	0.960922
-721.640215	-8.998210	0.965926
-725.456113	-14.308817	0.970931
-729.292261	-10.851598	0.975936
-732.964020	-19.540931	0.980941
-736.400586	-23.778316	0.985946
-740.424441	-16.331416	0.990950
-743.681929	-20.518559	0.995955
-747.884400	-14.402418	1.000960
-751.911800	-16.993669	1.005965
-755.653039	-13.884308	1.010970
-759.561334	-15.054842	1.015974
-762.644392	-15.439469	1.020979
-766.686388	-8.715012	1.025984
-770.519380	-9.427636	1.030989
-774.207373	-22.414596	1.035994
-778.282538	-12.713885	1.040998
-781.908322	-20.295595	1.046003
-785.382488	-15.882170	1.051008
-789.292161	-14.838425	1.056013
-792.658794	-12.427529	1.061018
-796.897485	-12.797734	1.066022
-800.409555	-20.235164	1.071027
-804.551508	-22.122052	1.076032
-808.489718	-17.424700	1.081037
-811.814686	-27.124942	1.086042
-816.170879	-11.565120	1.091046
-819.492021	-10.826695	1.096051
-822.834203	-16.083542	1.101056
-826.877932	-14.933155	1.106061
-830.706242	-17.600244	1.111066
-834.741330	-9.558467	1.116070
-838.350668	-15.154208	1.121075
-841.922756	-10.849629	1.126080
-845.742720	-8.329931	1.131085
-849.268961	-9.450997	1.136090
-853.472522	-6.324355	1.141094
-856.738061	-11.177095	1.146099
-860.808624	-4.534647	1.151104
-864.816996	-12.272690	1.156109
-868.237268	-11.406389	1.161114
-872.416886	-3.186906	1.166118
-875.910828	-10.483619	1.171123
-879.549431	-10.437097	1.176128
-883.449382	-11.252373	1.181133
-887.045970	-8.380392	1.186138
-891.032363	-7.754717	1.191142
-894.571008	-17.619376	1.196147
-898.140964	-4.399101	1.201152
-901.901947	-14.002707	1.206157
-905.610590	-19.437387	1.211162
-909.599734	-6.426048	1.216166
-913.327926	-14.981488	1.221171
-917.196779	-12.373438	1.226176
-921.092865	-2.627003	1.231181
-924.284513	-17.634259	1.236186
-928.662217	-11.540254	1.241190
-932.417575	-12.395911	1.246195
-936.173910	-9.157701	1.251200
-940.212611	-10.269239	1.256205
-943.470248	-11.530876	1.261210
-947.452846	-9.122207	1.266214
-950.991096	-20.915418	1.271219
-954.656949	-13.121713	1.276224
-958.576926	-9.552958	1.281229
-962.284477	-19.075115	1.286234
-966.479520	-11.050128	1.291238
-969.865839	-24.498139	1.296243
-973.930148	-18.271241	1.301248
-977.676007	-15.608643	1.306253
-980.966218	-8.936231	1.311258
-984.735246	-8.815077	1.316262
-988.391823	-18.521957	1.321267
-992.512201	-19.503651	1.326272
-996.276652	-18.460709	1.331277
-1000.238627	-21.571337	1.336282
-1003.892200	-16.799336	1.341286
-1006.922162	-19.056060	1.346291
-1011.125914	-14.000533	1.351296
-1015.165861	-21.909868	1.356301
-1018.451775	-21.523720	1.361306
-1022.553427	-23.717857	1.366310
-1026.311016	-21.950578	1.371315
-1030.408387	-24.131193	1.376320
-1034.129863	-11.867355	1.381325
-1037.337375	-16.946728	1.386330
-1041.170522	-16.304305	1.391334
-1044.619877	-20.597528	1.396339
-1048.980571	-16.961301	1.401344
-1052.929691	-16.289275	1.406349
-1056.322835	-15.944272	1.411354
-1060.625610	-12.586940	1.416358
-1063.419813	-21.307262	1.421363
-1067.702811	-14.520116	1.426368
-1071.741774	-5.318291	1.431373
-1075.116778	-13.354368	1.436378
-1079.055655	-9.856509	1.441382
-1082.539434	-13.057669	1.446387
-1086.459311	-12.311417	1.451392
-1090.241832	-16.426709	1.456397
-1093.956277	-15.867840	1.461402
-1098.181914	-6.374347	1.466406
-1101.475412	-18.196998	1.471411
-1105.083850	-17.522604	1.476416
-1109.446905	-16.987699	1.481421
-1112.627792	-21.640720	1.486426
-1116.623805	-5.661767	1.491430
-1120.449809	-3.697318	1.496435
-1124.031690	-0.871487	1.501440
-1127.724824	-11.551562	1.506445
-1131.516638	-19.309569	1.511450
-1135.842962	-13.141411	1.516454
-1138.993341	-11.665044	1.521459
-1143.050605	1.756523	1.526464
-1146.525684	0.236645	1.531469
-1150.294573	-12.064968	1.536474
-1154.091208	-18.841319	1.541478
-1158.050444	-18.727305	1.546483
-1161.739293	-9.958229	1.551488
-1165.802950	-1.654300	1.556493
-1169.337940	-9.270410	1.561498
-1173.143211	-11.883848	1.566502
-1176.539314	-16.910774	1.571507
-1180.299412	-15.518158	1.576512
-1184.409907	-11.145862	1.581517
-1188.023118	-10.703963	1.586522
-1192.132731	-6.070025	1.591526
-1195.621743	-16.240175	1.596531
-1199.348827	-16.349309	1.601536
-1203.303181	-15.398654	1.606541
-1206.552368	-13.253542	1.611546
-1210.358012	-7.512321	1.616550
-1214.163844	-13.536485	1.621555
-1217.964313	-17.737000	1.626560
-1222.114622	-11.089079	1.631565
-1225.605554	-15.884721	1.636570
-1229.465250	-11.703861	1.641574
-1232.958074	-16.994342	1.646579
-1236.865856	-16.603004	1.651584
-1240.921101	-14.986451	1.656589
-1244.639319	-22.858537	1.661594
-1248.359881	-13.574915	1.666598
-1251.675996	-10.919148	1.671603
-1255.704520	-8.756498	1.676608
-1259.456771	-8.393163	1.681613
-1262.935869	-16.130023	1.686618
-1266.836509	-12.951781	1.691622
-1270.682373	-20.510092	1.696627
-1274.785197	-11.140030	1.701632
-1278.532868	-7.090554	1.706637
-1282.148360	-15.035789	1.711642
-1285.862463	-10.218982	1.716646
-1289.582283	-16.118011	1.721651
-1293.278206	-14.088945	1.726656
-1297.222127	-15.986143	1.731661
-1301.014045	-19.617040	1.736666
-1304.852121	-11.763716	1.741670
-1308.578462	-13.046023	1.746675
-1311.910507	-13.188234	1.751680
-1315.609367	-13.055698	1.756685
-1319.439634	-11.481321	1.761690
-1323.689656	-2.609576	1.766694
-1327.264318	-14.301729	1.771699
-1330.931202	-9.435641	1.776704
-1334.841691	-11.377548	1.781709
-1338.639235	-16.992825	1.786714
-1342.380995	0.481710	1.791718
-1346.084852	-6.340707	1.796723
-1349.837659	-5.980291	1.801728
-1353.623906	-8.500281	1.806733
-1357.061429	-16.726184	1.811738
-1361.066822	-10.377180	1.816742
-1364.777768	-14.177047	1.821747
-1368.430914	-13.838860	1.826752
-1372.528508	-2.736432	1.831757
-1375.770333	-8.872675	1.836762
-1380.138963	-4.182762	1.841766
-1383.897320	-8.533240	1.846771
-1387.394063	-14.882543	1.851776
-1391.134168	-7.506801	1.856781
-1394.607555	-14.769714	1.861786
-1398.813358	-12.950596	1.866790
-1402.375428	-16.102463	1.871795
-1406.119468	-9.416760	1.876800
-1409.963489	-12.152907	1.881805
-1413.571430	-17.322178	1.886810
-1417.417346	-14.403178	1.891814
-1421.173719	-21.303784	1.896819
-1424.987259	-7.304216	1.901824
-1428.828386	-8.676760	1.906829
-1432.362807	-13.398888	1.911834
-1436.459908	-3.576892	1.916838
-1439.895889	-13.170102	1.921843
-1443.791324	-14.527618	1.926848
-1447.651934	-5.033618	1.931853
-1451.117209	-13.696468	1.936858
-1455.202938	-12.866275	1.941862
-1458.765518	-14.059440	1.946867
-1462.558852	-10.664670	1.951872
-1466.532849	-7.805506	1.956877
-1470.160202	-22.584468	1.961882
-1474.222881	-8.179094	1.966886
-1477.640987	-11.587277	1.971891
-1481.307738	-21.069353	1.976896
-1485.142567	-19.632742	1.981901
-1488.685348	-12.958636	1.986906
-1493.039130	-19.985814	1.991910
-1496.475795	-20.109430	1.996915
-1500.729051	-16.246500	2.006912
-1501.337397	-17.801720	2.016909
-1498.545848	-12.155056	2.026906
-1495.711890	-18.167729	2.036902
-1493.925895	-16.267923	2.046899
-1492.057602	-20.581775	2.056896
-1490.261201	-19.717836	2.066893
-1488.021524	-22.515369	2.076890
-1486.058387	-16.540265	2.086886
-1484.721781	-18.583736	2.096883
-1482.383612	-14.156031	2.106880
-1480.515051	-11.288914	2.116877
-1478.468443	-15.596570	2.126874
-1476.356743	-19.560962	2.136870
-1475.371079	-20.938770	2.146867
-1473.232673	-16.438021	2.156864
-1470.959109	-16.384668	2.166861
-1469.157225	-14.818962	2.176858
-1467.105216	-16.037493	2.186854
-1465.388887	-16.659126	2.196851
-1463.554086	-15.992364	2.206848
-1461.669612	-12.384100	2.216845
-1459.727523	-17.859208	2.226842
-1457.950506	-11.349019	2.236838
-1455.793241	-14.207539	2.246835
-1454.353507	-15.675401	2.256832
-1452.395039	-11.597399	2.266829
-1450.211768	-17.071639	2.276826
-1448.175249	-17.556625	2.286822
-1446.349244	-10.511114	2.296819
-1444.629940	-12.765829	2.306816
-1442.918971	-13.350271	2.316813
-1440.905491	-14.174192	2.326810
-1439.032382	-14.816167	2.336806
-1436.898359	-13.728341	2.346803
-1435.417186	-12.908630	2.356800
-1433.625936	-14.001704	2.366797
-1431.480739	-16.267747	2.376794
-1429.562736	-21.191083	2.386790
-1427.927792	-13.781816	2.396787
-1425.898357	-18.868251	2.406784
-1423.585990	-16.441604	2.416781
-1422.133777	-16.708294	2.426778
-1420.130962	-13.084201	2.436774
-1418.272800	-17.487954	2.446771
-1416.458927	-19.498840	2.456768
-1414.692163	-19.735353	2.466765
-1412.802387	-24.267317	2.476762
-1410.921084	-18.361149	2.486758
-1408.958418	-12.283266	2.496755
-1407.042173	-17.687881	2.506752
-1405.061272	-19.596022	2.516749
-1403.344096	-20.214586	2.526746
-1401.319805	-20.571259	2.536742
-1399.631207	-18.134738	2.546739
-1397.792263	-24.731699	2.556736
-1395.654674	-18.209704	2.566733
-1393.617977	-17.624151	2.576730
-1392.016395	-13.943701	2.586726
-1390.089688	-21.366281	2.596723
-1388.407566	-21.110807	2.606720
-1386.675597	-15.689131	2.616717
-1384.457946	-20.197767	2.626714
-1382.678391	-19.578940	2.636710
-1380.867149	-18.046240	2.646707
-1378.559367	-17.194593	2.656704
-1376.909341	-13.292940	2.666701
-1375.150440	-17.882877	2.676698
-1373.180103	-14.023017	2.686694
-1371.387294	-11.244735	2.696691
-1369.353015	-16.177164	2.706688
-1367.616056	-16.694657	2.716685
-1365.834916	-20.560255	2.726682
-1363.824003	-18.066349	2.736678
-1362.050487	-13.966557	2.746675
-1360.261760	-14.539699	2.756672
-1358.196355	-22.357083	2.766669
-1356.047065	-16.650073	2.776666
-1354.470398	-22.164505	2.786662
-1352.449695	-14.670078	2.796659
-1350.811427	-13.215458	2.806656
-1348.868466	-14.973797	2.816653
-1347.044161	-9.270024	2.826650
-1344.885107	-13.177145	2.836646
-1343.218901	-14.783817	2.846643
-1341.194772	-15.873039	2.856640
-1339.550881	-22.715056	2.866637
-1337.734020	-21.420062	2.876634
-1335.855617	-17.971770	2.886630
-1333.578106	-20.127848	2.896627
-1331.975631	-11.750153	2.906624
-1329.843167	-11.656709	2.916621
-1328.162241	-14.479931	2.926618
-1326.498173	-19.847282	2.936614
-1324.459084	-15.076282	2.946611
-1322.723492	-17.474040	2.956608
-1320.285436	-20.426321	2.966605
-1318.558837	-15.226360	2.976602
-1316.885925	-19.129864	2.986598
-1315.087402	-23.790833	2.996595
-1313.384109	-16.185573	3.006592
-1311.380447	-18.553592	3.016589
-1309.275680	-19.988846	3.026586
-1307.572510	-20.638255	3.036582
-1305.669903	-17.718019	3.046579
-1303.747142	-14.718900	3.056576
-1301.678400	-13.961552	3.066573
-1299.720357	-16.634891	3.076570
-1298.165471	-16.208990	3.086566
-1296.542701	-7.321357	3.096563
-1294.345277	-11.801413	3.106560
-1292.326366	-11.133976	3.116557
-1290.654025	-16.090525	3.126554
-1289.025253	-18.595901	3.136550
-1286.821942	-9.782215	3.146547
-1285.011199	-10.295665	3.156544
-1283.113523	-10.395131	3.166541
-1281.212280	-15.855670	3.176538
-1279.478660	-10.696272	3.186534
-1277.360607	-10.663631	3.196531
-1275.674638	-13.951832	3.206528
-1273.749718	-13.529864	3.216525
-1271.859747	-17.600702	3.226522
-1269.990601	-20.654526	3.236518
-1268.126924	-8.041227	3.246515
-1266.001023	-14.718751	3.256512
-1264.262717	-11.448504	3.266509
-1262.864153	-19.383318	3.276506
-1260.439238	-16.578197	3.286502
-1258.549705	-13.565827	3.296499
-1256.887567	-15.842837	3.306496
-1255.184138	-23.152219	3.316493
-1253.098192	-15.450243	3.326490
-1251.068682	-18.831290	3.336486
-1249.214374	-14.842228	3.346483
-1247.536657	-16.070150	3.356480
-1245.620090	-17.023657	3.366477
-1243.561480	-16.600949	3.376474
-1241.764303	-13.971681	3.386470
-1240.191689	-9.961222	3.396467
-1238.132520	-18.814877	3.406464
-1236.261212	-15.824836	3.416461
-1234.270465	-20.020716	3.426458
-1232.337966	-19.113612	3.436454
-1230.597784	-15.537325	3.446451
-1228.668565	-15.693899	3.456448
-1226.778349	-15.444758	3.466445
-1224.767421	-10.834946	3.476442
-1223.132462	-14.086528	3.486438
-1221.291125	-15.519030	3.496435
-1219.084206	-14.049507	3.506432
-1217.446096	-17.069484	3.516429
-1215.705837	-16.970026	3.526426
-1213.845566	-17.557660	3.536422
-1211.795335	-13.445176	3.546419
-1209.914284	-18.507693	3.556416
-1207.949200	-15.010001	3.566413
-1206.231746	-8.306910	3.576410
-1204.221193	-12.423831	3.586406
-1202.537003	-13.987492	3.596403
-1200.494871	-9.565807	3.606400
-1198.498756	-3.908339	3.616397
-1196.789392	-10.454430	3.626394
-1195.016181	-15.790209	3.636390
-1192.771080	-10.281519	3.646387
-1191.102287	-6.644830	3.656384
-1189.479847	-4.957034	3.666381
-1187.694082	-10.800080	3.676378
-1185.454724	-15.976744	3.686374
-1183.650087	-19.727547	3.696371
-1181.746542	-10.502638	3.706368
-1179.821327	-9.584849	3.716365
-1177.926571	-12.661648	3.726362
-1176.373534	-8.385905	3.736358
-1174.241062	-12.894936	3.746355
-1172.214455	-14.862300	3.756352
-1170.409034	-18.291115	3.766349
-1168.718401	-15.469481	3.776346
-1166.528285	-9.189338	3.786342
-1164.861200	-7.338141	3.796339
-1163.428667	-7.543099	3.806336
-1161.149115	-14.207219	3.816333
-1159.346227	-11.111431	3.826330
-1157.605820	-12.475632	3.836326
-1155.258457	-12.763771	3.846323
-1153.546855	-12.024947	3.856320
-1151.620090	-15.256844	3.866317
-1149.842728	-13.683802	3.876314
-1148.213613	-11.513888	3.886310
-1146.223539	-15.043276	3.896307
-1144.114121	-13.242295	3.906304
-1142.210525	-14.212590	3.916301
-1140.335978	-11.530879	3.926298
-1138.573458	-14.168074	3.936294
-1136.971397	-13.645399	3.946291
-1135.045348	-11.737709	3.956288
-1132.766846	-17.266374	3.966285
-1131.291258	-20.931347	3.976282
-1129.120338	-22.545968	3.986278
-1127.184385	-19.545650	3.996275
-1125.561564	-13.522093	4.006272
-1123.423605	-15.256174	4.016269
-1121.545476	-12.683968	4.026266
-1119.994708	-14.944648	4.036262
-1117.852375	-15.817321	4.046259
-1116.206461	-17.659008	4.056256
-1114.331742	-17.107297	4.066253
-1112.238232	-18.567417	4.076250
-1110.428197	-17.899568	4.086246
-1108.514668	-14.783541	4.096243
-1106.831472	-14.141191	4.106240
-1104.789647	-19.164607	4.116237
-1102.829692	-16.449158	4.126234
-1101.115403	-17.485457	4.136230
-1099.321739	-11.369204	4.146227
-1097.224241	-16.049415	4.156224
-1095.576664	-15.106097	4.166221
-1093.459674	-24.728354	4.176218
-1091.645138	-17.000178	4.186214
-1089.885552	-15.394246	4.196211
-1088.073156	-12.920445	4.206208
-1086.245832	-15.877439	4.216205
-1084.403404	-14.728436	4.226202
-1082.030868	-24.161029	4.236198
-1080.538844	-22.436509	4.246195
-1078.547173	-15.758227	4.256192
-1076.607334	-12.578485	4.266189
-1074.789490	-18.072896	4.276186
-1072.856507	-17.892048	4.286182
-1070.943115	-21.063320	4.296179
-1069.221915	-18.443868	4.306176
-1067.546756	-20.763881	4.316173
-1065.252064	-20.816138	4.326170
-1063.368217	-19.479532	4.336166
-1061.945863	-18.454381	4.346163
-1059.984196	-22.233364	4.356160
-1057.771945	-16.016653	4.366157
-1056.027654	-22.383495	4.376154
-1054.192950	-27.247427	4.386150
-1052.233158	-21.879284	4.396147
-1050.464484	-19.739514	4.406144
-1048.555420	-20.745344	4.416141
-1046.732934	-17.963652	4.426138
-1044.559393	-22.591240	4.436134
-1042.919416	-14.001422	4.446131
-1041.003891	-16.047225	4.456128
-1039.284635	-15.996380	4.466125
-1037.427689	-19.884914	4.476122
-1035.436924	-20.614853	4.486118
-1033.412896	-19.000640	4.496115
-1031.651469	-11.611283	4.506112
-1029.869172	-14.973139	4.516109
-1027.841912	-19.346795	4.526106
-1026.019153	-18.980914	4.536102
-1023.800454	-17.963084	4.546099
-1022.277206	-18.392461	4.556096
-1020.646522	-17.348494	4.566093
-1018.327831	-21.844534	4.576090
-1016.629984	-15.856575	4.586086
-1014.756051	-19.245704	4.596083
-1012.894945	-17.865946	4.606080
-1011.123264	-13.326629	4.616077
-1009.104806	-17.397284	4.626074
-1007.265404	-16.102472	4.636070
-1005.277771	-19.953458	4.646067
-1003.595573	-16.956666	4.656064
-1001.470985	-14.946399	4.666061
-999.603616	-19.084466	4.676058
-998.121449	-11.994637	4.686054
-995.975410	-15.378314	4.696051
-994.278097	-22.839706	4.706048
-992.358891	-19.550804	4.716045
-990.653248	-22.398268	4.726042
-988.375341	-18.216193	4.736038
-986.290482	-18.147978	4.746035
-984.992030	-15.655075	4.756032
-983.254768	-12.319703	4.766029
-980.670148	-14.142443	4.776026
-978.900677	-20.289049	4.786022
-977.346623	-26.123313	4.796019
-975.556564	-19.257964	4.806016
-973.523502	-21.309874	4.816013
-971.701153	-15.471260	4.826010
-969.417562	-20.615325	4.836006
-967.927720	-17.264067	4.846003
-965.833987	-19.101461	4.856000
-964.253277	-18.491568	4.865997
-962.211147	-26.655435	4.875994
-960.068355	-18.076472	4.885990
-958.633456	-12.242214	4.895987
-956.848887	-17.503852	4.905984
-954.821070	-14.838596	4.915981
-952.527796	-21.937350	4.925978
-951.023063	-16.324253	4.935974
-949.087336	-15.010057	4.945971
-947.292386	-18.631244	4.955968
-945.149556	-15.864368	4.965965
-943.338899	-14.995961	4.975962
-941.727056	-18.213658	4.985958
-939.612236	-18.240191	4.995955
-937.795387	-18.050138	5.005952
-936.085320	-16.688802	5.015949
-933.937078	-25.515401	5.025946
-932.225403	-16.700116	5.035942
-930.378208	-18.177539	5.045939
-928.565445	-18.957877	5.055936
-926.475717	-23.564067	5.065933
-924.905433	-22.365112	5.075930
-922.674763	-18.429628	5.085926
-920.789913	-11.745172	5.095923
-919.302104	-17.946183	5.105920
-917.454190	-15.326344	5.115917
-915.293051	-18.690259	5.125914
-913.107840	-24.126438	5.135910
-911.335925	-19.070763	5.145907
-909.924957	-17.851066	5.155904
-907.658114	-21.715029	5.165901
-905.940750	-17.305891	5.175898
-904.215728	-24.465338	5.185894
-902.264721	-19.469865	5.195891
-900.349790	-21.104934	5.205888
-898.452341	-19.517735	5.215885
-896.439083	-19.155362	5.225882
-894.647304	-15.629689	5.235878
-892.703596	-20.210931	5.245875
-890.875520	-5.352634	5.255872
-889.205134	-11.622290	5.265869
-887.406735	-17.973984	5.275866
-885.063157	-19.720193	5.285862
-883.251358	-20.522448	5.295859
-881.449582	-15.915205	5.305856
-880.169229	-23.647766	5.315853
-877.888940	-16.415433	5.325850
-875.635112	-13.198865	5.335846
-873.975796	-15.893580	5.345843
-872.248671	-14.545975	5.355840
-870.491110	-16.332708	5.365837
-868.116442	-19.318607	5.375834
-866.558751	-21.269178	5.385830
-864.697273	-15.960938	5.395827
-862.701899	-20.831467	5.405824
-860.895448	-16.733376	5.415821
-859.016642	-22.829479	5.425818
-857.231387	-22.125892	5.435814
-855.225042	-15.219221	5.445811
-853.705560	-9.355778	5.455808
-851.748290	-10.230208	5.465805
-849.507249	-11.489467	5.475802
-847.890134	-17.229526	5.485798
-845.806394	-9.550477	5.495795
-844.077836	-12.254661	5.505792
-842.216076	-10.560657	5.515789
-839.903645	-14.187108	5.525786
-838.426836	-14.577365	5.535782
-836.372183	-11.687344	5.545779
-834.787020	-14.177550	5.555776
-832.798173	-8.455426	5.565773
-830.660968	-16.359655	5.575770
-829.211320	-22.077672	5.585766
-827.328736	-11.104349	5.595763
-825.303088	-15.551793	5.605760
-823.225615	-17.459095	5.615757
-821.615412	-18.364872	5.625754
-819.683712	-16.582555	5.635750
-817.544336	-13.944479	5.645747
-815.749362	-12.364518	5.655744
-813.893236	-15.016436	5.665741
-812.300363	-10.355221	5.675738
-810.074809	-12.889338	5.685734
-808.427007	-20.181645	5.695731
-806.247002	-18.664791	5.705728
-804.484708	-22.574338	5.715725
-802.938224	-27.249919	5.725722
-801.044329	-20.552596	5.735718
-799.102578	-16.345025	5.745715
-797.038436	-18.286489	5.755712
-795.266190	-19.895514	5.765709
-793.214949	-18.157542	5.775706
-791.490727	-20.590995	5.785702
-789.769526	-22.093962	5.795699
-787.842488	-16.208765	5.805696
-785.858786	-21.236841	5.815693
-783.802452	-22.078099	5.825690
-782.229736	-23.146805	5.835686
-780.135148	-18.011536	5.845683
-778.187947	-17.899031	5.855680
-776.544150	-19.733831	5.865677
-774.802726	-22.106862	5.875674
-772.836041	-23.151679	5.885670
-770.703876	-18.232406	5.895667
-768.876242	-28.308689	5.905664
-767.049800	-20.574241	5.915661
-765.194513	-24.577567	5.925658
-763.541050	-19.932318	5.935654
-761.525182	-15.412872	5.945651
-759.437107	-15.862864	5.955648
-757.653182	-13.508985	5.965645
-755.749204	-18.623773	5.975642
-753.759693	-24.338015	5.985638
-751.999186	-21.997759	5.995635
-750.303931	-22.692867	6.005632
-748.649287	-19.546217	6.015629
-746.609255	-16.896938	6.025626
-744.315834	-22.287104	6.035622
-742.446658	-25.961053	6.045619
-740.812398	-22.482720	6.055616
-738.880619	-16.528763	6.065613
-737.305055	-18.627371	6.075610
-735.166932	-16.933230	6.085606
-733.338209	-13.159119	6.095603
-731.260363	-12.161133	6.105600
-729.682310	-26.489098	6.115597
-727.745180	-11.193341	6.125594
-725.851801	-15.551675	6.135590
-724.051598	-23.643544	6.145587
-722.350758	-21.189521	6.155584
-720.433361	-16.366936	6.165581
-718.337929	-23.274392	6.175578
-716.104403	-24.377587	6.185574
-714.401510	-17.504405	6.195571
-712.523665	-21.372350	6.205568
-710.815925	-24.227849	6.215565
-709.004683	-20.474611	6.225562
-707.052646	-19.922293	6.235558
-704.890237	-14.950946	6.245555
-703.238146	-10.739640	6.255552
-701.507639	-15.960882	6.265549
-699.653709	-15.255514	6.275546
-697.548449	-13.200824	6.285542
-695.916683	-18.598917	6.295539
-693.650220	-17.416296	6.305536
-692.042984	-13.832554	6.315533
-690.190962	-17.402673	6.325530
-688.221284	-19.804216	6.335526
-686.540336	-22.129627	6.345523
-684.434415	-18.293975	6.355520
-682.700994	-22.636192	6.365517
-680.837135	-18.135020	6.375514
-678.901732	-19.998974	6.385510
-676.764468	-14.311475	6.395507
-675.287058	-23.840692	6.405504
-673.305381	-24.415715	6.415501
-671.252036	-16.786906	6.425498
-669.671242	-24.332105	6.435494
-667.678686	-21.597803	6.445491
-665.879395	-24.628950	6.455488
-664.109899	-25.492173	6.465485
-661.959883	-19.091435	6.475482
-659.782202	-20.141445	6.485478
-658.128713	-14.716117	6.495475
-656.656133	-11.690312	6.505472
-654.638764	-16.750507	6.515469
-652.521818	-16.543436	6.525466
-650.701015	-16.205370	6.535462
-648.739249	-24.146156	6.545459
-647.284100	-21.589668	6.555456
-645.240511	-20.677713	6.565453
-643.466396	-19.507970	6.575450
-641.380903	-18.078494	6.585446
-639.406285	-18.235518	6.595443
-637.332104	-29.069521	6.605440
-635.786748	-19.172684	6.615437
-634.089055	-23.714424	6.625434
-631.945972	-30.638893	6.635430
-629.938545	-24.971665	6.645427
-628.161762	-20.151802	6.655424
-626.530520	-24.663974	6.665421
-624.410186	-28.895850	6.675418
-622.631575	-21.813639	6.685414
-620.599162	-21.820406	6.695411
-618.799293	-21.051075	6.705408
-617.283434	-22.680592	6.715405
-615.324768	-20.242409	6.725402
-613.066950	-17.351483	6.735398
-611.334771	-20.826608	6.745395
-609.426943	-19.913462	6.755392
-607.720345	-22.670812	6.765389
-605.885682	-17.790702	6.775386
-603.673838	-22.455602	6.785382
-601.894919	-22.785020	6.795379
-599.983634	-21.981366	6.805376
-598.147722	-20.057247	6.815373
-596.436246	-18.915358	6.825370
-594.415437	-21.623414	6.835366
-592.533550	-19.149264	6.845363
-590.751397	-21.689723	6.855360
-589.099365	-18.869381	6.865357
-587.129762	-17.602924	6.875354
-584.959370	-20.465918	6.885350
-583.191065	-26.460485	6.895347
-581.338620	-20.942141	6.905344
-579.291661	-17.415921	6.915341
-577.484866	-22.582946	6.925338
-575.945240	-17.679371	6.935334
-573.772455	-17.736939	6.945331
-571.711754	-18.862922	6.955328
-570.258247	-17.427178	6.965325
-568.384196	-22.227569	6.975322
-566.224791	-15.348233	6.985318
-564.435458	-20.842462	6.995315
-562.701768	-18.246722	7.005312
-560.705405	-15.102405	7.015309
-558.740947	-13.997735	7.025306
-556.996740	-21.073178	7.035302
-555.094256	-21.924403	7.045299
-552.978875	-23.040155	7.055296
-551.343302	-16.696092	7.065293
-549.631991	-20.519949	7.075290
-547.502443	-28.204822	7.085286
-545.461988	-23.858058	7.095283
-543.846781	-24.646025	7.105280
-541.894712	-21.608303	7.115277
-540.090563	-24.442765	7.125274
-538.176515	-22.758447	7.135270
-536.420279	-16.888381	7.145267
-534.613099	-15.588046	7.155264
-532.587322	-15.761046	7.165261
-530.706511	-17.680899	7.175258
-528.551239	-19.586162	7.185254
-526.862475	-24.473774	7.195251
-525.097199	-24.687271	7.205248
-523.085966	-25.974260	7.215245
-521.424663	-24.825882	7.225242
-519.306335	-17.276781	7.235238
-517.684815	-17.295209	7.245235
-515.408734	-13.671309	7.255232
-513.908894	-18.732429	7.265229
-511.782100	-16.442586	7.275226
-510.243790	-15.748244	7.285222
-508.299270	-17.735097	7.295219
-506.235807	-17.786197	7.305216
-504.448227	-20.608514	7.315213
-502.455903	-19.835090	7.325210
-500.388046	-23.943219	7.335206
-499.021708	-23.354040	7.345203
-497.041712	-19.774422	7.355200
-494.805055	-18.629480	7.365197
-492.863519	-18.207939	7.375194
-491.348382	-17.753044	7.385190
-489.355362	-21.422896	7.395187
-487.674787	-20.519151	7.405184
-485.808001	-13.746167	7.415181
-483.935986	-24.702512	7.425178
-481.804335	-21.646047	7.435174
-479.805585	-15.317290	7.445171
-478.110133	-17.076451	7.455168
-476.297892	-9.912640	7.465165
-474.212037	-14.817838	7.475162
-472.371881	-19.098008	7.485158
-470.812500	-21.317017	7.495155
-468.715662	-19.346038	7.505152
-466.902641	-14.397618	7.515149
-465.172367	-12.044417	7.525146
-463.063347	-16.084878	7.535142
-461.230991	-25.541184	7.545139
-459.138862	-18.663634	7.555136
-457.704391	-13.561604	7.565133
-455.772402	-16.304312	7.575130
-453.470999	-26.023402	7.585126
-451.950402	-25.761986	7.595123
-450.157270	-22.330912	7.605120
-448.010604	-21.493664	7.615117
-446.026769	-21.326734	7.625114
-444.314653	-29.205400	7.635110
-442.350049	-25.669068	7.645107
-440.520202	-18.574358	7.655104
-438.832208	-24.267056	7.665101
-437.085608	-16.540100	7.675098
-434.807437	-26.264938	7.685094
-432.975346	-28.568517	7.695091
-431.136060	-22.034258	7.705088
-429.826610	-22.797015	7.715085
-427.700296	-22.630713	7.725082
-425.437184	-20.373608	7.735078
-423.580028	-23.516450	7.745075
-421.719492	-19.429796	7.755072
-420.258310	-22.162045	7.765069
-418.110059	-19.291329	7.775066
-416.346395	-24.685039	7.785062
-414.107752	-24.459290	7.795059
-412.423504	-19.035529	7.805056
-410.829679	-18.179458	7.815053
-408.618490	-15.618782	7.825050
-406.742680	-22.037765	7.835046
-405.054270	-17.849405	7.845043
-403.218491	-20.183552	7.855040
-401.331622	-23.539544	7.865037
-399.352598	-23.632334	7.875034
-397.370971	-26.390815	7.885030
-395.509625	-24.199015	7.895027
-393.658320	-23.993516	7.905024
-391.837998	-19.908312	7.915021
-389.965241	-25.032050	7.925018
-388.111022	-20.502252	7.935014
-386.058060	-23.940011	7.945011
-384.207743	-24.498560	7.955008
-382.612480	-25.302182	7.965005
-380.765950	-26.207495	7.975002
-378.596051	-24.363361	7.984998
-376.683975	-16.108559	7.994995
-375.027360	-14.889854	8.004992
-373.139636	-18.926491	8.014989
-371.072641	-23.564905	8.024986
-369.233468	-16.771624	8.034982
-367.361796	-28.387839	8.044979
-365.405615	-25.120096	8.054976
-363.893628	-13.957714	8.064973
-361.887103	-19.140683	8.074970
-359.949642	-18.181537	8.084966
-358.132361	-21.098490	8.094963
-356.106710	-29.257678	8.104960
-354.017158	-20.855925	8.114957
-352.510095	-24.208093	8.124954
-350.405000	-25.718344	8.134950
-348.719577	-26.991074	8.144947
-347.060368	-25.472763	8.154944
-345.027663	-18.190878	8.164941
-342.867482	-24.135730	8.174938
-341.067902	-19.586119	8.184934
-339.021842	-31.166991	8.194931
-337.439654	-19.952641	8.204928
-335.864584	-15.171397	8.214925
-333.819249	-18.138946	8.224922
-331.856927	-22.185880	8.234918
-329.642686	-18.536136	8.244915
-328.097900	-25.639596	8.254912
-326.100920	-20.463057	8.264909
-324.047385	-20.837680	8.274906
-322.482188	-18.105916	8.284902
-320.725410	-17.285268	8.294899
-318.593415	-13.189750	8.304896
-316.666951	-24.175202	8.314893
-314.962767	-21.181406	8.324890
-312.856402	-20.009179	8.334886
-310.939847	-23.246681	8.344883
-309.295360	-23.346002	8.354880
-307.549137	-24.749989	8.364877
-305.565620	-17.187057	8.374874
-303.560950	-19.445454	8.384870
-301.791096	-18.336350	8.394867
-299.688486	-19.781424	8.404864
-297.984697	-24.481809	8.414861
-296.114555	-22.389228	8.424858
-294.438376	-22.160437	8.434854
-292.448944	-23.259017	8.444851
-290.736299	-19.050755	8.454848
-288.545322	-17.310955	8.464845
-286.674468	-14.861634	8.474842
-284.775363	-20.665297	8.484838
-283.032695	-18.656571	8.494835
-281.327899	-18.394443	8.504832
-279.472573	-15.680532	8.514829
-277.282234	-16.388004	8.524826
-275.222088	-21.928411	8.534822
-273.658970	-22.561040	8.544819
-271.841836	-18.521020	8.554816
-269.881258	-13.597567	8.564813
-267.229430	-21.746099	8.574810
-265.959501	-26.716697	8.584807
-264.399452	-20.068258	8.594803
-262.298389	-23.197800	8.604800
-260.459556	-29.606037	8.614797
-258.599022	-29.406642	8.624794
-256.897906	-28.021271	8.634791
-254.701229	-27.902359	8.644787
-252.932673	-28.761972	8.654784
-251.286833	-22.416165	8.664781
-249.076840	-25.072023	8.674778
-247.152865	-25.820644	8.684775
-245.272060	-23.994990	8.694771
-244.022755	-28.220176	8.704768
-241.863679	-23.821014	8.714765
-240.178434	-22.720468	8.724762
-237.896352	-23.352543	8.734759
-236.068144	-27.943266	8.744755
-234.270825	-28.851667	8.754752
-232.480146	-30.758486	8.764749
-230.398937	-26.465310	8.774746
-228.562802	-19.481952	8.784743
-226.668076	-27.250674	8.794739
-224.671727	-22.484473	8.804736
-223.075166	-21.090287	8.814733
-220.979292	-25.227920	8.824730
-219.238165	-27.005244	8.834727
-217.468439	-30.151348	8.844723
-215.455026	-26.365238	8.854720
-213.489214	-23.168376	8.864717
-211.784199	-19.410419	8.874714
-209.904228	-29.123630	8.884711
-208.204369	-29.814353	8.894707
-205.947435	-29.738170	8.904704
-204.125066	-28.515794	8.914701
-202.312671	-25.708130	8.924698
-200.219950	-27.036275	8.934695
-198.736152	-28.241993	8.944691
-196.999161	-22.074900	8.954688
-194.622206	-25.952622	8.964685
-193.207473	-27.257844	8.974682
-191.003887	-29.835258	8.984679
-188.910033	-22.741410	8.994675
-186.992315	-20.084749	9.004672
-185.847247	-29.589104	9.014669
-183.904661	-25.071659	9.024666
-181.799716	-14.876916	9.034663
-179.682163	-23.734327	9.044659
-177.935207	-24.885704	9.054656
-175.973888	-21.437038	9.064653
-174.302128	-19.600077	9.074650
-172.221662	-18.960439	9.084647
-170.343113	-23.203883	9.094643
-168.636717	-19.458745	9.104640
-166.653456	-9.571413	9.114637
-164.681490	-14.598714	9.124634
-162.910566	-12.288087	9.134631
-161.093060	-11.432798	9.144627
-159.080697	-12.155978	9.154624
-157.353145	-10.637381	9.164621
-155.618331	-15.151571	9.174618
-153.644518	-10.392760	9.184615
-151.543046	-12.710690	9.194611
-149.779969	-16.750960	9.204608
-147.931858	-13.876316	9.214605
-146.104796	-16.084145	9.224602
-144.097469	-15.001757	9.234599
-142.401316	-10.031268	9.244595
-140.391691	-14.815083	9.254592
-138.604269	-17.266058	9.264589
-136.828018	-16.326799	9.274586
-134.696098	-13.784794	9.284583
-132.605933	-18.260922	9.294579
-131.193456	-13.908333	9.304576
-129.168854	-15.212919	9.314573
-127.324285	-10.237675	9.324570
-125.253235	-20.128162	9.334567
-123.444217	-17.970427	9.344563
-121.811089	-15.830420	9.354560
-120.003817	-17.125591	9.364557
-118.008083	-20.094524	9.374554
-115.953252	-15.062815	9.384551
-114.075739	-12.827577	9.394547
-112.208031	-22.846667	9.404544
-110.291018	-22.373533	9.414541
-108.699302	-12.780531	9.424538
-106.822505	-10.538857	9.434535
-104.607890	-20.248545	9.444531
-102.929226	-15.166290	9.454528
-101.087468	-18.953811	9.464525
-99.111179	-13.012707	9.474522
-97.265843	-17.205011	9.484519
-95.320414	-17.494299	9.494515
-93.491443	-17.795008	9.504512
-91.546516	-17.239469	9.514509
-89.846993	-18.823747	9.524506
-87.895907	-20.113414	9.534503
-85.844965	-23.296392	9.544499
-84.303454	-16.190123	9.554496
-82.233843	-17.948696	9.564493
-80.185210	-18.736017	9.574490
-78.674815	-14.997441	9.584487
-76.876871	-24.725902	9.594483
-74.487921	-26.238562	9.604480
-73.017740	-18.258795	9.614477
-71.253703	-24.643919	9.624474
-69.069114	-26.234503	9.634471
-66.869329	-23.635368	9.644467
-65.209337	-25.341220	9.654464
-63.581710	-23.656615	9.664461
-61.793804	-26.510246	9.674458
-59.728510	-18.729606	9.684455
-57.751552	-21.510757	9.694451
-55.895145	-26.792700	9.704448
-54.200379	-32.825705	9.714445
-52.155572	-22.223348	9.724442
-50.123310	-28.371764	9.734439
-48.310827	-27.442956	9.744435
-46.637287	-24.630390	9.754432
-44.876611	-24.160689	9.764429
-42.991731	-26.625560	9.774426
-40.974670	-24.347785	9.784423
-39.088734	-24.624381	9.794419
-37.331272	-21.602560	9.804416
-35.692944	-18.328049	9.814413
-33.474543	-18.400296	9.824410
-31.518047	-22.930811	9.834407
-29.547152	-22.065149	9.844403
-27.746476	-23.817099	9.854400
-26.046342	-22.624037	9.864397
-23.977676	-20.345004	9.874394
-22.487790	-19.142091	9.884391
-20.538513	-24.839877	9.894387
-18.576424	-20.266979	9.904384
-16.442420	-27.887398	9.914381
-14.855181	-20.916270	9.924378
-12.797049	-18.469757	9.934375
-10.977540	-12.595149	9.944371
-9.335901	-10.139048	9.954368
-7.775209	1.364798	9.964365
-5.913822	24.173468	9.974362
-4.110383	50.833052	9.984359
-2.677877	83.730369	9.994355
-1.183949	123.638101	10.004352
0.000000	160.463313	10.009357
1.011303	178.742517	10.014362
1.749589	203.603393	10.019367
2.122941	217.636690	10.024371
2.490313	222.228056	10.029376
2.897092	233.728155	10.034381
2.974410	228.758877	10.039386
2.793936	231.958419	10.044391
3.031166	232.656503	10.049395
3.309469	234.038750	10.054400
3.068878	244.437295	10.059405
3.589450	251.301887	10.064410
3.473286	258.219143	10.069415
3.123134	253.275452	10.074419
3.558598	250.925173	10.079424
3.286214	237.945449	10.084429
3.488560	243.386319	10.089434
3.196026	248.600183	10.094439
3.592698	260.614432	10.099443
3.781247	253.654612	10.104448
3.423185	256.994447	10.109453
3.511511	255.084311	10.114458
3.882893	275.810654	10.119463
3.728546	270.263288	10.124467
4.021505	258.078068	10.129472
3.538685	259.230036	10.134477
3.816922	247.143368	10.139482
3.936041	262.727994	10.144487
4.281467	270.970418	10.149491
4.248893	258.562719	10.154496
3.995758	262.059288	10.159501
4.144422	247.681440	10.164506
3.925078	253.025561	10.169511
3.686949	262.158993	10.174515
4.397392	272.483159	10.179520
4.497812	280.624311	10.184525
4.685448	266.413697	10.189530
4.317685	262.242375	10.194535
4.344859	264.164575	10.199539
4.387303	266.391851	10.204544
3.924720	271.421528	10.209549
4.289247	272.930378	10.214554
4.546134	294.428803	10.219559
4.640423	303.222237	10.224563
5.102332	286.719091	10.229568
4.923847	284.433603	10.234573
4.710870	272.726455	10.239578
4.536843	273.557939	10.244583
4.799293	276.757817	10.249587
4.859957	276.052168	10.254592
4.480054	293.974640	10.259597
4.963365	301.789809	10.264602
4.800094	306.060546	10.269607
4.751122	306.160869	10.274611
4.978299	307.292653	10.279616
4.955741	311.782228	10.284621
5.133394	304.064018	10.289626
5.053217	316.901850	10.294631
4.970511	310.131922	10.299635
5.327808	310.263650	10.304640
4.946824	313.783775	10.309645
5.325171	302.993142	10.314650
5.335655	314.166993	10.319655
5.068627	320.206306	10.324659
5.734437	316.746935	10.329664
5.604215	323.988168	10.334669
5.605738	324.067823	10.339674
5.865345	321.710886	10.344679
5.512348	324.769225	10.349683
5.799452	314.057792	10.354688
5.548141	325.888425	10.359693
6.103181	336.059221	10.364698
6.148183	330.710279	10.369703
5.872495	330.127656	10.374707
5.674446	322.940871	10.379712
6.119142	326.354550	10.384717
6.159255	330.879870	10.389722
6.058960	328.553519	10.394727
5.748379	325.327133	10.399731
6.474253	340.662110	10.404736
6.262528	346.793541	10.409741
6.088715	337.426647	10.414746
6.314151	342.433356	10.419751
6.495986	351.819997	10.424755
6.694430	344.678780	10.429760
6.320175	342.932292	10.434765
6.193659	327.287779	10.439770
6.239339	330.779287	10.444775
6.218373	353.829707	10.449779
6.627810	350.220399	10.454784
6.457346	360.451722	10.459789
6.565427	360.687852	10.464794
6.919515	360.753859	10.469799
6.590786	364.048037	10.474803
6.858814	360.037070	10.479808
6.685484	361.040339	10.484813
6.840745	361.346217	10.489818
6.580621	368.021550	10.494823
6.626080	366.914613	10.499827
6.891334	367.108331	10.504832
6.925537	381.821938	10.509837
7.135594	391.628313	10.514842
7.556207	390.827407	10.519847
7.197499	387.726955	10.524851
7.172604	372.318505	10.529856
6.849976	387.339766	10.534861
7.621328	394.229089	10.539866
7.571493	393.168888	10.544871
7.332759	399.508080	10.549875
7.700852	398.095792	10.554880
7.561529	403.086576	10.559885
7.549474	401.533059	10.564890
7.622798	393.982831	10.569895
7.398176	401.146115	10.574899
7.788595	404.152145	10.579904
7.665002	414.916938	10.584909
7.979677	413.021147	10.589914
7.801825	408.537213	10.594919
7.738213	411.077899	10.599923
7.874656	407.821205	10.604928
7.624547	419.058774	10.609933
7.949101	407.128594	10.614938
7.983362	416.819516	10.619943
8.170235	416.109503	10.624947
8.389599	414.285683	10.629952
8.039233	415.813941	10.634957
8.136713	411.142591	10.639962
8.132002	413.263866	10.644967
7.838569	411.187505	10.649971
8.159422	406.098902	10.654976
8.332729	411.140758	10.659981
8.254105	414.220016	10.664986
8.250768	416.729012	10.669991
8.260732	417.587932	10.674995
8.937641	424.479717	10.680000
8.554575	427.437214	10.685005
8.592738	420.114935	10.690010
8.745234	428.312522	10.695015
8.782280	444.889745	10.700019
8.892433	435.821285	10.705024
9.088076	432.928891	10.710029
8.908276	421.523845	10.715034
8.610993	422.810242	10.720039
8.613507	431.257260	10.725043
8.909065	428.721103	10.730048
8.644636	445.614494	10.735053
8.851585	439.161021	10.740058
9.082292	442.358114	10.745063
8.899597	440.275127	10.750067
9.330335	442.648669	10.755072
9.155667	448.141858	10.760077
9.097932	449.178738	10.765082
9.245037	445.808368	10.770087
9.020663	447.657166	10.775091
9.192705	455.850075	10.780096
9.435800	477.289468	10.785101
9.761906	467.949999	10.790106
9.703860	481.795301	10.795111
9.631759	481.159703	10.800115
10.011490	476.929034	10.805120
9.605274	459.441318	10.810125
9.422036	459.413240	10.815130
9.397174	468.627911	10.820135
9.585530	481.711654	10.825139
10.087928	470.508442	10.830144
9.587548	482.192837	10.835149
10.064199	476.689845	10.840154
10.450105	476.676661	10.845159
9.855621	489.066794	10.850163
10.235216	483.809519	10.855168
9.932094	482.835438	10.860173
10.036104	474.439734	10.865178
9.893534	480.645350	10.870183
9.983468	478.774353	10.875187
10.151366	483.378692	10.880192
10.159382	494.592501	10.885197
10.444598	492.926909	10.890202
10.219353	489.923425	10.895207
10.025490	502.291470	10.900211
10.429983	509.893812	10.905216
10.686715	509.440743	10.910221
10.728534	505.215069	10.915226
10.946276	514.490430	10.920231
10.817475	510.936958	10.925235
11.103373	504.538677	10.930240
10.738104	512.598104	10.935245
10.803105	504.090329	10.940250
10.737508	510.871903	10.945255
10.858208	510.500455	10.950259
10.903443	513.435398	10.955264
10.888766	519.554400	10.960269
10.926159	514.632394	10.965274
10.911454	510.925104	10.970279
10.715843	513.601980	10.975283
11.122369	509.490035	10.980288
11.271985	518.356781	10.985293
11.353231	511.144284	10.990298
11.317233	513.790974	10.995303
11.236651	518.600537	11.000307
11.463522	512.812503	11.005312
11.310121	524.323321	11.010317
11.427141	514.723844	11.015322
11.370504	526.433704	11.020327
11.523299	546.521917	11.025331
11.815013	536.249571	11.030336
11.833361	545.380126	11.035341
11.756298	536.223184	11.040346
11.685073	521.921135	11.045351
11.803408	521.433365	11.050355
11.685412	526.179509	11.055360
11.903880	544.227643	11.060365
11.874562	542.921299	11.065370
12.143922	541.844877	11.070375
11.955270	551.248152	11.075379
12.379046	541.979795	11.080384
12.139021	549.028909	11.085389
11.994237	546.247555	11.090394
12.471378	549.886359	11.095399
12.149633	552.446157	11.100403
12.048720	548.582290	11.105408
12.069459	554.090089	11.110413
12.200810	553.620743	11.115418
12.265852	545.053012	11.120423
11.978492	552.265800	11.125427
12.386833	545.409566	11.130432
11.999967	547.940325	11.135437
12.304792	551.116160	11.140442
12.331827	556.954127	11.145447
12.577877	568.991078	11.150451
12.787110	572.658419	11.155456
12.820933	571.912881	11.160461
12.976349	575.696042	11.165466
12.848356	575.849972	11.170471
12.845804	583.335910	11.175475
13.003171	577.994190	11.180480
12.784274	578.936928	11.185485
12.982255	576.212873	11.190490
13.132195	579.657852	11.195495
12.815264	581.089327	11.200499
12.685795	585.946133	11.205504
12.834851	579.626414	11.210509
12.994105	580.060975	11.215514
13.016645	591.475977	11.220519
13.379243	605.818885	11.225523
13.661903	599.402154	11.230528
13.536674	616.339779	11.235533
13.619911	607.346470	11.240538
13.882481	605.460541	11.245543
13.549757	583.936421	11.250547
13.998146	570.694789	11.255552
13.443524	575.712436	11.260557
13.764724	570.120656	11.265562
13.991322	568.453365	11.270567
13.577057	576.713036	11.275571
13.638198	574.056537	11.280576
13.885585	576.669085	11.285581
13.725699	578.261601	11.290586
13.997228	588.711189	11.295591
13.900593	605.503887	11.300595
14.237891	602.666143	11.305600
14.044898	617.406760	11.310605
14.132609	606.570787	11.315610
14.114431	611.824608	11.320615
13.922474	608.959298	11.325619
14.093520	606.334154	11.330624
14.251055	611.845392	11.335629
14.171758	603.601854	11.340634
14.704663	604.189724	11.345639
14.661371	609.248845	11.350643
14.408149	605.442369	11.355648
14.381039	621.763511	11.360653
14.412840	610.510658	11.365658
14.388038	610.996651	11.370663
14.011716	616.048958	11.375667
14.273918	609.786879	11.380672
14.535443	620.591336	11.385677
14.800868	632.888612	11.390682
14.935642	634.640732	11.395687
14.871499	639.214314	11.400691
15.065502	638.821711	11.405696
14.741508	648.480031	11.410701
14.821868	636.445099	11.415706
15.348038	634.903498	11.420711
15.197073	646.417179	11.425715
15.371490	639.923072	11.430720
15.411475	637.244704	11.435725
15.521711	631.760663	11.440730
15.292996	624.132322	11.445735
15.217139	610.676203	11.450739
15.511967	612.970520	11.455744
15.354089	623.854480	11.460749
15.483319	630.306985	11.465754
15.364023	632.083853	11.470759
15.389460	639.109600	11.475763
15.179029	642.023837	11.480768
15.359949	649.117838	11.485773
15.381632	640.858174	11.490778
15.682262	638.064120	11.495783
15.664773	638.574180	11.500787
15.809524	628.911855	11.505792
15.453739	634.916564	11.510797
15.504054	637.562128	11.515802
15.735099	642.733635	11.520807
15.924985	657.216106	11.525811
15.903982	659.347901	11.530816
16.302882	668.051977	11.535821
16.437978	663.149034	11.540826
16.370513	651.781087	11.545831
15.840876	643.603036	11.550835
16.196829	644.584995	11.555840
16.331581	658.708815	11.560845
16.420357	656.131477	11.565850
16.722766	654.348004	11.570855
16.230163	655.443210	11.575859
16.603804	654.302839	11.580864
16.612036	660.255815	11.585869
16.322575	648.428089	11.590874
16.691096	650.109818	11.595879
16.490269	668.079888	11.600883
16.810341	655.573032	11.605888
16.564508	670.175466	11.610893
16.807913	665.259981	11.615898
16.670582	657.347379	11.620903
16.638748	667.252444	11.625907
16.817489	660.377578	11.630912
16.407195	663.839377	11.635917
16.571945	660.890362	11.640922
16.817616	658.709066	11.645927
16.642526	659.890837	11.650931
16.873900	660.865856	11.655936
17.154418	676.213869	11.660941
17.096053	675.733773	11.665946
17.396734	674.101966	11.670951
17.318714	678.726662	11.675955
17.505760	674.075639	11.680960
17.479974	679.751761	11.685965
17.489452	676.414326	11.690970
17.440700	674.940752	11.695975
17.167360	675.698204	11.700979
17.330908	679.506905	11.705984
17.382652	686.156303	11.710989
17.260453	682.458227	11.715994
17.840310	676.083958	11.720999
17.310412	683.095782	11.726003
17.583515	681.301209	11.731008
17.608762	673.812121	11.736013
17.633269	679.781434	11.741018
17.776315	687.512301	11.746023
17.905592	712.401792	11.751027
18.307986	703.483687	11.756032
18.012755	717.666674	11.761037
17.993988	707.773319	11.766042
18.332548	709.209086	11.771047
18.386454	702.712091	11.776051
18.559516	693.341689	11.781056
18.248777	691.539293	11.786061
18.036776	680.787333	11.791066
18.022744	690.863048	11.796071
18.045110	701.309873	11.801075
18.429739	695.867209	11.806080
18.156544	708.739323	11.811085
18.258755	714.185302	11.816090
18.613703	703.128436	11.821095
18.543101	713.785647	11.826099
18.569869	712.628047	11.831104
18.568077	710.326928	11.836109
18.936390	706.165828	11.841114
18.979414	712.457068	11.846119
18.882723	712.057202	11.851123
18.792717	706.464712	11.856128
18.780161	720.473307	11.861133
18.765761	713.832652	11.866138
18.843071	708.890021	11.871143
18.931473	709.350079	11.876147
18.848339	711.851351	11.881152
18.773913	724.600313	11.886157
19.236590	729.220802	11.891162
19.506874	732.938376	11.896167
19.174992	739.726251	11.901171
19.576339	723.762151	11.906176
19.619833	730.575319	11.911181
19.518746	722.030822	11.916186
19.440536	713.369136	11.921191
19.245162	720.603609	11.926195
19.553944	721.511092	11.931200
19.334320	734.642780	11.936205
19.530051	732.876310	11.941210
19.674752	736.867813	11.946215
19.617553	740.787431	11.951219
19.908663	731.459683	11.956224
19.776548	739.081487	11.961229
19.865348	735.237779	11.966234
19.700808	729.064205	11.971239
19.743228	731.335713	11.976243
19.892573	722.122046	11.981248
19.868247	735.457566	11.986253
19.592979	728.024259	11.991258
19.974312	731.284134	11.996263
19.745021	735.619143	12.001267
19.802176	742.707694	12.006272
20.213000	751.870412	12.011277
20.212360	762.630048	12.016282
20.682479	762.150829	12.021287
20.109257	745.954174	12.026291
20.487154	730.979447	12.031296
19.964978	739.846225	12.036301
19.779830	737.752546	12.041306
20.332679	752.576217	12.046311
20.437074	757.182886	12.051315
20.426102	745.350095	12.056320
20.242912	737.821671	12.061325
20.080003	736.579194	12.066330
20.025034	727.249866	12.071335
20.257138	741.935434	12.076339
20.687248	749.022862	12.081344
20.414439	737.861067	12.086349
20.461984	728.666784	12.091354
20.664399	734.047904	12.096359
20.337869	737.657219	12.101363
20.505958	728.423211	12.106368
20.703380	733.967560	12.111373
20.422609	734.869710	12.116378
20.536939	735.527493	12.121383
20.383779	718.279816	12.126387
20.406086	705.374105	12.131392
20.080126	706.887459	12.136397
20.026818	703.678307	12.141402
20.230132	705.228686	12.146407
20.017560	702.738822	12.151411
20.107611	695.766114	12.156416
20.437666	706.394120	12.161421
20.019186	701.267194	12.166426
20.406295	709.348676	12.171431
20.243000	711.157802	12.176435
20.580961	697.471599	12.181440
20.292757	703.467135	12.186445
20.110757	707.707858	12.191450
20.226921	701.885363	12.196455
19.948739	714.904940	12.201459
19.895328	708.150655	12.206464
20.075838	714.642331	12.211469
20.197124	724.500938	12.216474
20.120961	715.204961	12.221479
19.896547	724.487890	12.226483
20.524759	737.402367	12.231488
20.374347	739.433380	12.236493
20.497431	723.125707	12.241498
20.687049	707.182774	12.246503
20.258849	705.676664	12.251507
20.241725	703.163517	12.256512
20.047122	706.759670	12.261517
20.270942	710.554037	12.266522
20.488260	710.627667	12.271527
19.848679	716.012163	12.276531
20.116099	712.967914	12.281536
20.054835	707.008124	12.286541
19.978933	714.589411	12.291546
20.399179	709.478545	12.296551
20.057976	711.877463	12.301555
20.471943	706.409615	12.306560
20.495442	707.737924	12.311565
20.443404	703.837833	12.316570
20.387334	706.047770	12.321575
20.073714	712.304418	12.326579
20.746641	704.355619	12.331584
20.522143	708.828634	12.336589
20.254997	700.190778	12.341594
20.516016	700.676927	12.346599
20.466428	710.338838	12.351603
20.274530	693.795989	12.356608
20.218167	680.409238	12.361613
19.862788	678.377410	12.366618
20.186439	690.072490	12.371623
20.002571	703.313570	12.376627
20.175335	701.801513	12.381632
20.319004	703.656307	12.386637
20.205188	706.993562	12.391642
20.721034	703.857655	12.396647
20.350246	699.260889	12.401651
20.382449	679.999803	12.406656
20.026942	680.628427	12.411661
20.109692	677.315578	12.416666
20.360653	674.534169	12.421671
20.284246	673.009810	12.426675
20.138444	669.290268	12.431680
20.117359	676.481155	12.436685
19.900908	679.866311	12.441690
20.302786	684.078572	12.446695
20.348661	693.454001	12.451699
20.153090	683.710288	12.456704
20.202448	680.405917	12.461709
20.341188	682.326152	12.466714
20.490206	678.545399	12.471719
20.274560	685.645887	12.476723
20.407870	679.756009	12.481728
20.317362	676.155386	12.486733
20.151546	681.784451	12.491738
20.308995	673.865833	12.496743
20.125263	684.430672	12.501747
20.482425	679.900758	12.506752
19.957933	683.637828	12.511757
20.136242	687.295938	12.516762
20.444018	678.627914	12.521767
20.123256	689.536322	12.526771
20.149784	683.808556	12.531776
20.227998	688.602313	12.536781
19.968265	688.474465	12.541786
20.489376	682.295651	12.546791
20.156679	682.909598	12.551795
20.172178	682.788322	12.556800
20.039579	675.102046	12.561805
19.896758	686.606574	12.566810
20.418545	672.000062	12.571815
20.051371	677.968756	12.576819
20.048916	675.439081	12.581824
20.001504	685.504345	12.586829
20.171824	686.460717	12.591834
20.016703	670.951285	12.596839
20.586194	703.745545	12.601843
20.705900	699.961576	12.606848
20.448139	691.907303	12.611853
20.332918	689.971221	12.616858
20.490104	691.087389	12.621863
20.135531	691.534507	12.626867
20.274654	683.005345	12.631872
20.391423	684.902275	12.636877
20.138451	691.803705	12.641882
20.257808	688.546520	12.646887
20.320979	687.755292	12.651891
20.419758	686.065793	12.656896
20.624437	679.380755	12.661901
20.494433	687.503687	12.666906
20.549883	681.138926	12.671911
20.266417	683.654793	12.676915
19.997026	675.952483	12.681920
20.112646	672.188097	12.686925
20.053295	669.497178	12.691930
20.041450	672.557955	12.696935
20.222243	693.427263	12.701939
20.186056	690.186997	12.706944
20.264551	689.620417	12.711949
20.529081	689.722790	12.716954
20.213291	675.823881	12.721959
20.053663	668.375317	12.726963
20.494131	670.875087	12.731968
20.420579	665.024511	12.736973
20.004476	668.632324	12.741978
20.150075	670.031047	12.746983
20.394442	672.305036	12.751987
20.093743	660.218884	12.756992
20.215117	663.775676	12.761997
20.242932	674.604829	12.767002
20.237170	667.215311	12.772007
20.115053	673.258468	12.777011
20.293188	666.076176	12.782016
20.233566	662.563676	12.787021
19.972384	672.032214	12.792026
20.308515	659.885508	12.797031
20.040823	669.347197	12.802035
20.284456	672.734678	12.807040
20.241309	666.467651	12.812045
20.149466	674.759541	12.817050
20.368942	669.098786	12.822055
20.148763	678.131841	12.827059
19.932264	670.485756	12.832064
20.320238	683.427458	12.837069
20.112187	685.190100	12.842074
20.293667	687.745367	12.847079
20.163607	683.614863	12.852083
20.275012	691.172575	12.857088
20.093990	679.125672	12.862093
20.360232	692.673446	12.867098
20.654211	679.002158	12.872103
20.332813	683.470117	12.877107
20.276273	669.118269	12.882112
20.325450	679.660155	12.887117
20.643493	672.711026	12.892122
20.479673	675.315049	12.897127
20.441709	679.701535	12.902131
20.483222	663.607219	12.907136
20.607626	671.211736	12.912141
20.375895	681.708531	12.917146
20.268450	663.053235	12.922151
20.084891	652.381918	12.927155
20.015839	660.689089	12.932160
20.440168	670.368441	12.937165
20.086921	666.338192	12.942170
20.197832	669.708989	12.947175
20.172368	677.365794	12.952179
20.220614	676.979088	12.957184
20.197873	675.573908	12.962189
20.248320	681.723596	12.967194
20.121874	668.415845	12.972199
20.256505	683.966912	12.977203
20.248791	679.534611	12.982208
19.876906	672.898942	12.987213
20.082435	677.263944	12.992218
20.246181	675.844795	12.997223
20.052537	681.688042	13.002227
20.101163	681.958892	13.007232
20.305646	680.506437	13.012237
20.006806	677.940445	13.017242
20.282197	678.861135	13.022247
20.184461	677.573576	13.027251
20.340459	682.958925	13.032256
20.430136	681.488506	13.037261
20.116244	677.051415	13.042266
20.279251	676.752068	13.047271
20.274955	690.582690	13.052275
20.552904	682.693738	13.057280
20.337879	682.683344	13.062285
20.064219	677.744652	13.067290
20.117776	670.545954	13.072295
19.883943	678.059363	13.077299
20.050094	680.397868	13.082304
20.401418	678.543511	13.087309
20.039893	677.186050	13.092314
20.109875	673.477829	13.097319
20.059743	685.196243	13.102323
20.138489	684.249562	13.107328
20.366363	680.669130	13.112333
20.217676	693.656998	13.117338
20.392128	683.419019	13.122343
20.264853	687.406571	13.127347
20.199706	689.797733	13.132352
20.388760	696.917270	13.137357
20.219475	695.462915	13.142362
20.369366	691.593706	13.147367
20.251084	695.527785	13.152371
20.289931	685.940660	13.157376
20.547002	689.942617	13.162381
20.129776	674.274698	13.167386
20.027849	658.364119	13.172391
20.004883	663.468905	13.177395
20.097488	682.239058	13.182400
20.390609	682.205978	13.187405
20.359644	684.624806	13.192410
20.472048	664.759568	13.197415
19.899062	664.240110	13.202419
19.950848	663.425467	13.207424
20.320559	669.492696	13.212429
20.327198	687.730916	13.217434
20.084468	679.112835	13.222439
20.006824	690.567547	13.227443
20.257483	688.245097	13.232448
20.457609	689.693477	13.237453
20.256331	687.361093	13.242458
20.497275	665.212332	13.247463
20.238069	663.050046	13.252467
19.987580	661.252239	13.257472
20.194604	648.547365	13.262477
20.072863	651.553121	13.267482
20.071267	662.527310	13.272487
20.333965	682.680192	13.277491
20.428459	676.378594	13.282496
20.153265	660.192857	13.287501
19.828204	665.276431	13.292506
20.216592	670.189458	13.297511
20.339018	680.790631	13.302515
20.367447	678.350651	13.307520
20.268895	664.729358	13.312525
19.930195	665.801598	13.317530
20.172965	671.729792	13.322535
19.974771	681.998880	13.327539
20.340922	683.591101	13.332544
20.390536	687.301274	13.337549
20.173669	692.548961	13.342554
20.293362	682.614618	13.347559
20.478731	685.448397	13.352563
19.919187	683.069065	13.357568
20.315182	680.157289	13.362573
20.017166	678.810201	13.367578
20.246823	676.229317	13.372583
20.036273	684.245239	13.377587
20.379445	687.340871	13.382592
20.657073	684.873766	13.387597
20.202430	674.075345	13.392602
20.193927	658.501542	13.397607
19.846493	662.935798	13.402611
19.904009	678.115941	13.407616
20.316050	680.503546	13.412621
20.337761	685.776265	13.417626
20.375071	682.218338	13.422631
20.186843	678.620682	13.427635
20.329643	671.925014	13.432640
20.398426	674.968202	13.437645
20.113721	660.854607	13.442650
20.339199	652.269111	13.447655
20.008732	664.308192	13.452659
19.961964	668.462680	13.457664
20.123380	663.170748	13.462669
20.203486	672.501278	13.467674
20.481025	683.740064	13.472679
20.151156	680.067221	13.477683
20.313711	664.412514	13.482688
20.028401	662.320626	13.487693
19.964798	669.773766	13.492698
20.424464	677.733269	13.497703
20.234993	677.252002	13.502707
19.939654	673.081623	13.507712
20.193002	680.257133	13.512717
20.232404	703.142357	13.517722
20.410115	695.370313	13.522727
20.531279	700.480514	13.527731
20.466488	676.420253	13.532736
20.587876	662.685038	13.537741
20.046277	671.362475	13.542746
20.029575	658.340019	13.547751
20.240402	657.146763	13.552755
19.990557	661.775199	13.557760
20.359942	665.871206	13.562765
20.108861	673.606569	13.567770
20.499004	662.290221	13.572775
20.082119	667.077767	13.577779
19.878569	658.319403	13.582784
20.054285	658.503750	13.587789
19.820868	674.022033	13.592794
20.282089	668.521432	13.597799
20.665157	681.498609	13.602803
20.397110	674.221880	13.607808
20.362009	669.336614	13.612813
20.448055	664.731664	13.617818
20.559704	660.816521	13.622823
20.322193	668.964473	13.627827
19.996778	664.712157	13.632832
20.189071	655.821279	13.637837
20.211955	658.081699	13.642842
20.162614	659.965690	13.647847
19.871697	660.199220	13.652851
19.876858	663.403946	13.657856
19.997652	669.074037	13.662861
19.818628	666.337545	13.667866
20.675199	670.089344	13.672871
20.275624	670.859042	13.677875
20.204225	665.448111	13.682880
20.268101	663.589132	13.687885
20.063673	669.730573	13.692890
20.227767	651.744801	13.697895
20.372401	662.011245	13.702899
20.160383	659.910823	13.707904
20.541069	665.392804	13.712909
20.401104	654.060071	13.717914
20.495381	654.257405	13.722919
20.219016	670.689318	13.727923
20.446315	666.747845	13.732928
20.606470	660.901004	13.737933
20.075419	667.167074	13.742938
20.502833	663.539056	13.747943
20.469341	669.785707	13.752947
20.661350	656.390910	13.757952
20.194430	646.920739	13.762957
20.080172	639.821360	13.767962
20.228706	638.008810	13.772967
20.139330	646.264018	13.777971
20.283872	651.734764	13.782976
20.406388	647.393674	13.787981
20.165717	640.588855	13.792986
20.223689	631.635831	13.797991
20.251514	635.046679	13.802995
20.213954	633.886727	13.808000
20.215399	630.383419	13.813005
19.712085	641.510145	13.818010
20.194778	645.425645	13.823015
20.354959	655.577636	13.828019
20.417745	662.774065	13.833024
20.285016	640.478343	13.838029
20.288039	638.283704	13.843034
20.203218	631.001433	13.848039
19.945027	642.106416	13.853043
20.113360	651.011263	13.858048
20.055198	656.389752	13.863053
20.185929	659.342631	13.868058
20.440348	658.727495	13.873063
20.276879	662.031656	13.878067
20.117482	661.635484	13.883072
20.182063	653.772688	13.888077
20.243161	658.591243	13.893082
20.053443	664.653062	13.898087
20.090116	666.996443	13.903091
20.462873	672.153248	13.908096
20.554522	657.825089	13.913101
20.173895	650.859650	13.918106
20.251065	636.260998	13.923111
20.327061	641.947683	13.928115
20.146438	640.398945	13.933120
20.224925	638.611758	13.938125
20.234421	636.480745	13.943130
20.232724	642.673427	13.948135
20.133469	642.453752	13.953139
20.050514	640.980905	13.958144
20.527509	631.322367	13.963149
19.950310	640.885438	13.968154
20.173974	633.814177	13.973159
20.014398	636.155732	13.978163
20.052183	649.153249	13.983168
20.386679	651.824463	13.988173
20.378829	654.999721	13.993178
20.181551	641.671750	13.998183
20.031516	644.363459	14.003187
19.935688	638.951702	14.008192
20.328485	646.069696	14.013210
20.268027	669.879784	14.018227
20.579863	661.255130	14.023245
20.403659	652.456630	14.028263
20.232709	649.233558	14.033280
20.226533	638.795634	14.038298
20.052370	639.209835	14.043315
20.534957	648.771646	14.048333
19.973968	649.491349	14.053351
20.458826	659.302911	14.058368
20.654981	659.813783	14.063386
20.399221	663.254855	14.068403
20.313855	652.195633	14.073421
20.445404	653.371173	14.078439
20.676008	665.681875	14.083456
20.518014	645.289080	14.088474
20.475940	647.398352	14.093491
20.378065	639.293643	14.098509
20.347401	648.728095	14.103527
20.532174	668.945683	14.108544
20.742989	660.782296	14.113562
20.563222	677.072062	14.118579
20.362412	669.864629	14.123597
20.523186	672.295480	14.128615
20.473725	678.212584	14.133632
20.672803	666.909793	14.138650
20.335148	667.675677	14.143667
20.438421	662.467795	14.148685
20.530654	665.372035	14.153703
20.594796	675.150029	14.158720
20.536884	666.796690	14.163738
20.451160	678.431124	14.168755
20.544947	672.828356	14.173773
20.693429	674.193104	14.178791
20.581400	677.686762	14.183808
21.102864	693.573714	14.188826
20.943962	691.784859	14.193843
20.640503	681.350269	14.198861
20.938192	685.547785	14.203879
20.991767	699.028742	14.208896
20.931100	698.542393	14.213914
21.095922	714.531860	14.218931
20.742014	704.232712	14.223949
21.036261	697.646302	14.228967
20.771268	699.076990	14.233984
20.901080	699.194183	14.239002
20.848873	698.195260	14.244019
20.679021	705.614913	14.249037
20.789697	703.959241	14.254055
20.711685	710.061807	14.259072
21.045315	706.569496	14.264090
21.122310	710.410537	14.269107
21.033650	708.033187	14.274125
21.255845	709.703929	14.279143
20.726576	711.582596	14.284160
20.984076	711.448195	14.289178
21.400653	728.729861	14.294195
21.284377	727.582280	14.299213
21.332029	708.196356	14.304231
20.815236	713.324425	14.309248
21.300659	718.594686	14.314266
21.552330	734.677289	14.319283
21.739086	721.125454	14.324301
21.599879	705.494199	14.329319
21.235899	709.223095	14.334336
21.396850	696.619198	14.339354
21.527925	699.745336	14.344371
21.384250	703.190565	14.349389
21.134009	700.728873	14.354407
20.754781	702.948548	14.359424
21.532628	704.502364	14.364442
21.378620	718.681822	14.369459
21.478714	720.752703	14.374477
21.816944	715.216328	14.379495
21.384960	737.062895	14.384512
21.595304	716.078013	14.389530
21.644555	727.497483	14.394547
21.506820	725.634463	14.399565
21.665026	718.420088	14.404583
21.531934	720.598941	14.409600
21.831474	709.689075	14.414618
21.374492	726.337704	14.419635
21.780283	726.736498	14.424653
21.803422	719.877139	14.429671
21.652884	727.567425	14.434688
21.492072	720.057864	14.439706
21.802425	734.606871	14.444723
21.692203	724.286150	14.449741
21.582560	731.548352	14.454759
21.569817	737.212664	14.459776
21.928383	721.786724	14.464794
22.126347	725.713870	14.469811
21.852739	730.348566	14.474829
21.879510	721.678101	14.479847
21.974926	724.684091	14.484864
21.674256	724.786565	14.489882
21.886525	727.961109	14.494899
21.808321	730.661311	14.499917
22.198693	742.117627	14.504935
22.298844	751.487241	14.509952
22.173367	729.821300	14.514970
22.052278	728.580106	14.519987
21.534461	727.870934	14.525005
22.048051	734.772631	14.530023
21.824444	758.410684	14.535040
22.167768	750.081399	14.540058
22.413770	757.527569	14.545075
22.379841	762.062705	14.550093
22.583229	752.849684	14.555111
22.091723	770.114194	14.560128
22.513503	759.828157	14.565146
22.312928	753.490516	14.570163
22.016052	744.152788	14.575181
22.478941	758.957489	14.580199
22.401488	753.136610	14.585216
22.350655	759.901816	14.590234
22.490624	756.937446	14.595251
22.182525	744.911669	14.600269
22.313985	747.455745	14.605287
21.986434	763.673221	14.610304
22.289721	753.240919	14.615322
22.037191	760.396936	14.620339
22.078745	758.865538	14.625357
22.203535	756.746719	14.630375
22.421635	756.011422	14.635392
22.315271	750.920309	14.640410
22.354050	757.284264	14.645427
22.515581	773.340387	14.650445
23.114271	769.456584	14.655463
22.526338	772.829532	14.660480
22.618346	752.694016	14.665498
22.829445	757.643101	14.670515
22.712132	760.525722	14.675533
22.579002	755.375956	14.680551
22.596446	764.530682	14.685568
22.687649	772.690521	14.690586
22.740714	777.100106	14.695603
22.576111	782.716295	14.700621
22.824151	779.692215	14.705639
22.456982	794.398091	14.710656
22.905588	785.312683	14.715674
23.521052	776.938412	14.720691
23.337831	775.071628	14.725709
23.231195	751.931887	14.730727
23.111440	758.513031	14.735744
23.314436	751.127906	14.740762
23.251934	748.496270	14.745779
23.072420	744.706688	14.750797
23.567289	743.062102	14.755815
22.968554	748.030220	14.760832
22.939771	736.153386	14.765850
23.376498	742.608028	14.770867
22.906575	748.087279	14.775885
23.177467	741.207276	14.780903
23.174652	745.366217	14.785920
23.144727	733.989783	14.790938
23.395240	739.525599	14.795955
23.177302	749.649070	14.800973
23.339639	744.793530	14.805991
23.210801	756.522991	14.811008
23.333681	748.686606	14.816026
23.814489	744.966325	14.821043
23.255798	747.101369	14.826061
23.225367	741.414565	14.831079
23.218805	747.559235	14.836096
23.183168	744.836800	14.841114
23.338746	750.222594	14.846131
22.968698	747.136642	14.851149
23.405849	739.412164	14.856167
23.100826	744.872982	14.861184
22.862269	745.624640	14.866202
23.238052	744.730492	14.871219
22.902356	749.900478	14.876237
23.331307	765.676424	14.881255
23.387266	781.700629	14.886272
23.391467	782.613347	14.891290
23.568596	776.268946	14.896307
23.308455	774.032188	14.901325
23.736675	773.686520	14.906343
23.708025	784.991045	14.911360
23.497367	782.851786	14.916378
24.005625	779.385092	14.921395
23.828674	782.785309	14.926413
23.743127	771.996582	14.931431
23.592020	786.697882	14.936448
23.786232	781.546241	14.941466
23.623526	784.286670	14.946483
23.300229	789.129080	14.951501
23.772817	778.171118	14.956519
23.830316	782.018434	14.961536
23.458057	784.741944	14.966554
23.939695	789.610146	14.971571
23.586480	796.706732	14.976589
23.963616	812.228299	14.981607
24.236358	808.701629	14.986624
24.396504	798.554815	14.991642
24.059691	793.105611	14.996659
23.704731	785.615966	15.001677
24.066128	790.523791	15.006695
24.231511	806.901805	15.011712
24.266019	804.970408	15.016730
24.431746	791.289728	15.021747
23.986014	782.262000	15.026765
23.787874	782.075994	15.031783
24.250618	788.498193	15.036800
24.199534	799.334404	15.041818
24.620100	793.361730	15.046835
23.985179	801.458059	15.051853
24.376709	792.710508	15.056871
24.427636	799.130746	15.061888
24.504605	801.784194	15.066906
24.201437	768.740640	15.071923
24.116784	787.363860	15.076941
24.441896	793.101729	15.081959
24.713417	809.887532	15.086976
24.542197	797.218544	15.091994
24.623331	778.793013	15.097011
24.162903	783.416620	15.102029
24.170900	785.961515	15.107047
24.487851	800.372685	15.112064
24.399572	812.182238	15.117082
24.592207	798.346252	15.122099
24.135077	813.970974	15.127117
24.608278	810.704917	15.132135
24.641252	811.098674	15.137152
24.466735	809.578132	15.142170
24.799395	802.648926	15.147187
24.539152	817.792374	15.152205
24.463070	804.968209	15.157223
24.809144	806.021463	15.162240
24.489877	807.215426	15.167258
24.835467	797.924644	15.172275
24.422230	803.657568	15.177293
24.661286	793.328288	15.182311
24.764704	807.598914	15.187328
24.650585	810.561259	15.192346
25.061915	801.354372	15.197363
24.741142	802.367679	15.202381
24.897000	799.948174	15.207399
25.189817	807.852515	15.212416
24.580395	810.539919	15.217434
24.865238	810.833736	15.222451
25.006644	826.620997	15.227469
25.301562	825.189186	15.232487
25.173841	824.145668	15.237504
25.088044	832.195343	15.242522
25.624046	816.239216	15.247539
25.128119	809.415400	15.252557
24.892293	804.791648	15.257575
25.078695	805.322958	15.262592
25.120280	825.898651	15.267610
25.315932	827.183532	15.272627
25.392815	831.199228	15.277645
25.225890	816.943940	15.282663
25.175208	819.786060	15.287680
24.851167	828.210350	15.292698
25.406397	831.119440	15.297715
25.417814	826.022102	15.302733
25.415292	822.353710	15.307751
25.531635	828.117021	15.312768
25.289388	836.912088	15.317786
25.520743	833.332238	15.322803
25.637720	831.980712	15.327821
25.383321	832.113560	15.332839
25.497743	837.095393	15.337856
25.530636	826.534701	15.342874
25.717615	823.731133	15.347891
25.634482	826.512363	15.352909
25.515716	826.670771	15.357927
25.790785	824.546854	15.362944
25.561332	831.186423	15.367962
25.724119	825.655963	15.372979
25.677703	830.649285	15.377997
25.672333	822.680731	15.383015
25.722349	820.635175	15.388032
25.550431	823.790783	15.393050
25.698307	822.391859	15.398067
25.749361	824.928322	15.403085
25.644908	825.551632	15.408103
25.913520	829.519450	15.413120
25.647756	829.639953	15.418138
25.899460	821.073557	15.423155
25.964184	828.743725	15.428173
25.386865	822.167262	15.433191
25.590840	824.380466	15.438208
25.762009	850.455230	15.443226
26.104540	838.421572	15.448243
26.064666	854.424961	15.453261
26.142491	857.013789	15.458279
26.307586	850.447906	15.463296
26.309801	861.755434	15.468314
26.085370	849.708361	15.473331
25.842193	842.680629	15.478349
25.779786	847.287974	15.483367
26.118734	849.298761	15.488384
26.050799	852.436219	15.493402
26.141654	858.666074	15.498419
25.869326	855.193282	15.503437
26.060240	853.814234	15.508455
26.207661	846.950725	15.513472
25.966012	862.223388	15.518490
25.989509	854.822790	15.523507
26.258167	868.568479	15.528525
26.579741	875.982209	15.533543
26.673991	872.147363	15.538560
26.819323	881.988054	15.543578
27.053593	860.456456	15.548595
26.985924	853.344102	15.553613
26.578212	839.617971	15.558631
26.908733	833.477171	15.563648
26.955521	838.785966	15.568666
27.268200	844.912801	15.573683
26.932388	847.779947	15.578701
27.043438	833.258519	15.583719
26.899332	820.116428	15.588736
26.326824	808.705338	15.593754
26.602644	817.752828	15.598771
26.725375	827.378437	15.603789
26.761092	840.846645	15.608807
27.097770	827.838660	15.613824
26.703521	846.635595	15.618842
26.833953	839.669408	15.623859
26.995994	838.963496	15.628877
26.888268	847.005664	15.633895
27.321777	841.128434	15.638912
27.142466	834.559280	15.643930
27.082388	814.713769	15.648947
27.062446	804.208709	15.653965
26.861471	812.003036	15.658983
26.886693	808.143035	15.664000
27.084524	819.669444	15.669018
27.168153	828.234787	15.674035
26.983339	826.311622	15.679053
27.070824	826.572418	15.684071
27.510786	835.533970	15.689088
27.376385	833.531978	15.694106
27.296667	811.444914	15.699123
27.246649	808.356676	15.704141
26.676939	825.932594	15.709159
27.142592	829.195740	15.714176
27.253210	836.251411	15.719194
27.122474	833.621203	15.724211
27.050094	837.338236	15.729229
26.909958	850.180121	15.734247
27.165910	841.336186	15.739264
26.808391	847.555741	15.744282
26.924240	846.685736	15.749299
27.613956	863.683336	15.754317
27.651661	875.370604	15.759335
27.820522	868.025470	15.764352
27.906081	873.666294	15.769370
27.586463	849.533180	15.774387
27.851626	851.349670	15.779405
27.511528	844.708624	15.784423
27.923992	838.721494	15.789440
27.440285	847.827204	15.794458
27.256455	843.182563	15.799475
27.565129	861.530798	15.804493
27.412653	864.761964	15.809511
27.907628	861.756691	15.814528
27.469318	869.769794	15.819546
27.668357	865.929249	15.824563
27.520297	871.085086	15.829581
27.820617	862.709113	15.834599
27.535929	859.496266	15.839616
27.665738	875.628348	15.844634
27.970978	877.029465	15.849651
28.191533	889.820159	15.854669
28.139614	906.841696	15.859687
28.379065	897.157219	15.864704
27.993263	872.380246	15.869722
28.104025	868.141648	15.874739
28.438936	872.586540	15.879757
28.359571	867.195353	15.884775
28.434950	858.723120	15.889792
27.992782	863.965181	15.894810
28.409102	869.367641	15.899827
28.646944	870.737034	15.904845
28.207808	872.613930	15.909863
28.495998	858.004455	15.914880
28.394222	860.722597	15.919898
28.228480	856.976406	15.924915
28.293589	860.372647	15.929933
28.112766	867.168070	15.934951
28.225480	858.743367	15.939968
28.135568	865.639122	15.944986
28.154460	879.984647	15.950003
28.675828	887.454611	15.955021
28.438997	897.881645	15.960039
28.602075	899.299142	15.965056
28.592195	899.394570	15.970074
28.802954	899.953460	15.975091
28.943211	892.872422	15.980109
28.467305	898.769533	15.985127
28.809318	891.223742	15.990144
28.884753	899.898973	15.995162
28.459489	896.755725	16.000179
28.812373	889.971116	16.005197
28.759285	893.994972	16.010215
29.008847	892.376907	16.015232
28.656224	897.323129	16.020250
28.838496	888.121255	16.025267
28.888338	892.496783	16.030285
28.601691	899.633139	16.035303
29.036355	884.630619	16.040320
28.921263	889.062335	16.045338
28.653842	895.376080	16.050355
28.531622	884.761430	16.055373
28.463184	896.044072	16.060391
28.837505	887.547746	16.065408
29.063705	905.325598	16.070426
29.343348	913.515242	16.075443
29.622034	904.694384	16.080461
29.128128	898.474242	16.085479
29.206591	886.561307	16.090496
28.994502	882.882274	16.095514
29.376053	905.280478	16.100531
29.813658	896.903042	16.105549
29.443513	893.933476	16.110567
29.567457	899.263023	16.115584
29.584351	888.330458	16.120602
29.227360	885.122843	16.125619
29.454852	889.869587	16.130637
29.153923	891.565571	16.135655
29.566956	885.955856	16.140672
29.249006	891.288228	16.145690
29.177985	895.406179	16.150707
29.454414	903.542848	16.155725
29.661375	907.396250	16.160743
29.324245	913.482020	16.165760
29.335462	916.072043	16.170778
29.561082	918.731695	16.175795
29.798783	906.779192	16.180813
29.455272	927.455765	16.185831
29.677508	922.935107	16.190848
29.750516	920.517783	16.195866
29.516138	917.378697	16.200883
29.803117	909.531788	16.205901
29.518372	924.858579	16.210919
29.724389	928.913484	16.215936
30.373262	931.511935	16.220954
30.091403	931.388040	16.225971
30.301662	920.401020	16.230989
30.067893	921.258887	16.236007
30.064703	922.295488	16.241024
30.221065	914.200419	16.246042
30.080443	924.082020	16.251059
30.020404	914.020574	16.256077
29.764872	914.623936	16.261095
29.919459	907.987345	16.266112
29.736934	918.589776	16.271130
30.180340	934.656185	16.276147
30.285591	943.694775	16.281165
30.101583	955.312071	16.286183
30.197035	942.274813	16.291200
30.301282	942.989116	16.296218
29.942329	941.519994	16.301235
30.471070	946.446806	16.306253
30.116762	940.401013	16.311271
30.276356	944.641077	16.316288
30.494980	941.903227	16.321306
30.324486	937.967437	16.326323
30.142272	938.250795	16.331341
30.330111	944.002751	16.336359
30.721650	947.581338	16.341376
30.591706	946.204684	16.346394
30.328557	948.501837	16.351411
30.942230	951.514892	16.356429
30.881667	963.170710	16.361447
31.090983	956.077057	16.366464
30.935400	939.392659	16.371482
30.922681	935.173733	16.376499
31.131990	924.397647	16.381517
30.913401	926.870162	16.386535
30.873047	922.676095	16.391552
31.022764	929.572994	16.396570
30.999367	927.995307	16.401587
31.095521	927.433605	16.406605
30.945576	923.131173	16.411623
31.057917	927.581688	16.416640
30.977533	931.115978	16.421658
30.719744	931.442848	16.426675
31.022168	921.122249	16.431693
30.665885	930.374430	16.436711
30.788111	943.232761	16.441728
31.286509	944.908250	16.446746
31.258675	957.436593	16.451763
31.434508	955.534549	16.456781
31.408365	963.039954	16.461799
31.420078	955.033996	16.466816
31.622127	951.565757	16.471834
31.150766	944.406050	16.476851
31.281072	942.561605	16.481869
31.454034	949.933006	16.486887
31.085904	953.749141	16.491904
31.397917	946.131027	16.496922
31.123733	958.991239	16.501939
31.140214	951.144972	16.506957
31.041299	954.447841	16.511975
31.018958	952.500322	16.516992
31.283094	959.575617	16.522010
31.488239	971.110419	16.527027
31.990454	978.083263	16.532045
32.029465	991.486591	16.537063
31.764844	980.007390	16.542080
32.108785	965.863970	16.547098
31.951697	961.306263	16.552115
31.820710	951.661946	16.557133
31.881064	953.651108	16.562151
31.808855	958.335556	16.567168
31.648790	954.596299	16.572186
31.639457	963.708230	16.577203
31.989040	960.708820	16.582221
31.968812	965.405430	16.587239
31.892419	987.507127	16.592256
32.264538	979.901434	16.597274
32.057993	992.429991	16.602291
31.966419	988.300703	16.607309
32.263066	991.661625	16.612327
32.352020	990.932754	16.617344
32.452881	974.625848	16.622362
32.159684	970.750514	16.627379
32.239095	966.019810	16.632397
32.332216	966.363082	16.637415
32.229470	974.237786	16.642432
32.605001	972.541422	16.647450
32.209393	957.675947	16.652467
32.305533	976.830577	16.657485
32.570586	977.597890	16.662503
32.201760	984.925145	16.667520
32.399351	983.291763	16.672538
32.295538	996.475624	16.677555
32.452812	988.234077	16.682573
32.798914	981.895675	16.687591
32.675352	988.079553	16.692608
32.731600	982.751640	16.697626
32.860356	980.795753	16.702643
32.681342	986.071397	16.707661
32.951526	975.375228	16.712679
32.783937	991.647673	16.717696
32.718251	982.757415	16.722714
32.500990	983.213104	16.727731
32.439827	988.391304	16.732749
32.711303	983.121878	16.737767
32.347785	997.174568	16.742784
32.756711	983.034927	16.747802
32.808643	986.708579	16.752819
33.030843	1008.097299	16.757837
33.162472	1006.713534	16.762855
33.133694	1014.518262	16.767872
33.237650	1005.830600	16.772890
33.236515	998.828688	16.777907
32.987986	991.273198	16.782925
33.543063	987.086409	16.787943
32.965334	993.382040	16.792960
33.074620	981.541189	16.797978
33.207656	1005.103894	16.802995
32.878933	1013.204992	16.808013
33.493359	1008.944238	16.813031
33.100261	1009.964371	16.818048
33.298211	1001.634532	16.823066
32.943516	1002.316631	16.828083
33.234586	1005.514851	16.833101
33.399151	1007.152347	16.838119
33.030218	1014.636936	16.843136
33.549123	1004.947150	16.848154
33.393500	1004.320202	16.853171
33.245050	1019.902212	16.858189
33.630507	1025.326957	16.863207
33.627371	1045.973015	16.868224
33.917003	1037.814154	16.873242
33.578864	1038.024850	16.878259
33.557258	1037.423720	16.883277
33.921333	1027.244227	16.888295
33.952302	1044.218101	16.893312
33.927233	1032.864253	16.898330
33.859402	1038.298366	16.903347
33.578118	1036.060218	16.908365
34.049649	1034.151909	16.913383
33.870857	1041.549563	16.918400
33.918300	1037.256519	16.923418
34.021332	1043.508107	16.928435
33.809889	1033.914318	16.933453
34.048160	1030.957813	16.938471
34.001915	1033.225109	16.943488
33.659807	1032.064752	16.948506
34.066196	1043.930891	16.953523
34.249422	1054.220264	16.958541
34.796788	1054.340089	16.963559
34.681335	1047.004024	16.968576
34.755864	1029.979230	16.973594
34.330039	1026.423907	16.978611
34.228612	1019.990113	16.983629
34.787492	1011.281813	16.988647
34.444096	1016.992671	16.993664
34.407362	1014.696652	16.998682
34.819414	1010.600304	17.003699
34.283891	1016.941124	17.008717
34.565795	1020.493169	17.013735
34.069319	1019.366867	17.018752
34.778543	1037.642013	17.023770
35.138490	1042.337799	17.028787
34.417728	1037.638717	17.033805
34.750266	1034.629426	17.038823
34.777513	1044.934228	17.043840
35.228487	1044.639985	17.048858
35.155157	1030.097426	17.053875
34.530637	1021.120079	17.058893
34.725877	1019.361225	17.063911
34.799268	1034.830796	17.068928
35.197782	1043.865156	17.073946
35.067308	1046.978022	17.078963
34.800514	1049.857795	17.083981
35.460046	1041.271854	17.088999
35.072436	1043.815386	17.094016
35.102653	1043.467117	17.099034
35.148696	1040.063061	17.104051
35.197561	1045.923737	17.109069
35.219697	1045.510688	17.114087
35.302813	1043.785441	17.119104
35.325360	1037.825803	17.124122
35.262010	1046.317185	17.129139
34.850908	1049.992332	17.134157
35.405927	1043.444408	17.139175
35.356396	1045.767287	17.144192
35.236888	1047.034806	17.149210
35.383176	1045.598362	17.154227
35.447383	1038.060617	17.159245
35.622740	1043.043817	17.164263
35.442525	1045.209782	17.169280
35.642563	1039.876222	17.174298
35.739002	1042.581666	17.179315
35.388353	1046.969195	17.184333
35.821515	1041.664527	17.189351
35.263519	1042.662194	17.194368
35.542359	1060.705551	17.199386
35.727510	1060.697519	17.204403
35.716086	1077.901565	17.209421
36.199556	1067.761207	17.214439
36.041894	1077.604730	17.219456
35.747158	1076.046701	17.224474
36.141024	1062.587364	17.229491
35.985816	1079.789172	17.234509
36.101658	1074.020710	17.239527
36.083294	1070.968267	17.244544
36.116311	1071.300676	17.249562
36.143030	1072.560610	17.254579
36.055196	1073.838811	17.259597
36.335202	1074.117676	17.264615
36.135248	1077.881856	17.269632
36.162431	1073.514953	17.274650
36.070161	1072.898349	17.279667
36.123076	1070.160158	17.284685
36.329211	1069.129451	17.289703
36.397293	1065.567717	17.294720
36.367106	1073.043936	17.299738
36.599112	1075.894510	17.304755
36.293032	1085.370020	17.309773
36.608711	1085.756456	17.314791
36.756143	1091.205026	17.319808
36.830457	1091.740065	17.324826
36.937426	1088.338866	17.329843
36.331273	1084.750936	17.334861
36.951770	1076.241986	17.339879
36.974668	1088.214935	17.344896
36.775514	1084.609293	17.349914
36.832957	1072.550118	17.354931
36.715993	1078.577252	17.359949
37.007200	1076.658368	17.364967
36.883182	1088.448676	17.369984
37.147837	1093.527766	17.375002
37.249713	1086.765790	17.380019
36.837649	1084.502871	17.385037
36.908045	1078.666148	17.390055
37.255278	1082.942400	17.395072
37.102283	1077.095682	17.400090
37.129468	1080.111055	17.405107
36.903751	1082.289000	17.410125
36.936715	1070.394180	17.415143
36.779727	1085.367283	17.420160
36.866239	1079.729339	17.425178
37.130408	1078.159262	17.430195
37.112790	1094.901842	17.435213
37.148297	1105.002447	17.440231
37.498840	1105.495010	17.445248
37.492115	1113.116948	17.450266
37.679331	1111.214642	17.455283
37.474801	1114.523378	17.460301
37.458340	1115.972674	17.465319
37.583800	1116.557761	17.470336
37.410361	1117.069386	17.475354
37.512299	1111.444701	17.480371
37.207681	1121.162248	17.485389
37.542756	1114.320601	17.490407
37.753206	1114.140219	17.495424
37.435803	1114.918624	17.500442
37.881618	1128.611143	17.505459
38.093564	1139.704543	17.510477
38.490625	1134.954592	17.515495
38.430277	1127.817339	17.520512
37.879862	1119.771940	17.525530
38.288993	1107.812386	17.530547
37.853648	1112.507599	17.535565
37.927771	1104.718124	17.540583
38.649528	1116.346842	17.545600
38.296385	1117.115216	17.550618
38.586560	1105.689017	17.555635
38.210744	1107.577866	17.560653
38.310247	1103.182119	17.565671
38.366805	1102.312116	17.570688
38.065160	1103.828910	17.575706
38.344216	1108.016940	17.580723
38.328870	1127.471122	17.585741
38.360912	1132.974288	17.590759
38.733255	1136.137555	17.595776
38.527863	1133.365037	17.600794
38.724753	1130.345897	17.605811
38.498238	1130.036992	17.610829
38.526750	1133.503628	17.615847
38.555786	1132.485427	17.620864
38.400526	1142.375803	17.625882
38.872270	1131.556141	17.630899
38.399462	1136.392618	17.635917
38.817192	1122.482676	17.640935
38.724614	1135.869369	17.645952
38.391367	1132.340155	17.650970
38.762081	1128.124524	17.655987
38.724008	1146.319200	17.661005
39.206661	1152.206701	17.666023
39.283773	1166.966375	17.671040
38.958639	1172.067183	17.676058
39.256134	1161.860460	17.681075
39.238268	1171.593664	17.686093
39.205210	1162.495169	17.691111
39.277936	1158.053337	17.696128
39.372978	1160.417675	17.701146
39.739372	1146.750281	17.706163
39.379611	1148.926015	17.711181
39.362646	1140.060925	17.716199
39.393134	1142.997131	17.721216
39.261445	1159.021790	17.726234
39.604288	1157.651521	17.731251
39.552483	1160.954789	17.736269
39.510774	1163.732623	17.741287
39.849367	1151.570347	17.746304
39.895541	1167.665754	17.751322
39.686858	1158.798190	17.756339
39.770126	1163.001727	17.761357
39.667508	1152.210718	17.766375
39.994072	1143.504780	17.771392
39.481683	1162.762986	17.776410
39.513621	1154.885829	17.781427
39.694393	1155.366141	17.786445
39.748135	1162.456210	17.791463
39.915574	1154.829583	17.796480
39.756275	1159.759221	17.801498
39.877273	1148.646262	17.806515
39.995731	1158.612552	17.811533
39.869479	1165.168173	17.816551
40.355455	1173.413155	17.821568
40.031504	1186.564652	17.826586
40.348612	1179.878425	17.831603
40.299206	1183.239519	17.836621
40.330001	1189.403588	17.841639
40.395412	1182.505808	17.846656
40.317347	1178.824204	17.851674
40.161956	1187.679563	17.856691
40.231135	1181.227930	17.861709
40.243148	1180.152665	17.866727
40.312264	1178.720649	17.871744
40.098783	1185.736936	17.876762
40.465207	1176.950688	17.881779
40.536526	1199.260391	17.886797
40.770083	1208.388801	17.891815
40.559315	1210.062576	17.896832
40.521068	1213.749093	17.901850
40.785087	1206.265917	17.906867
40.830145	1209.281612	17.911885
40.756823	1210.722681	17.916903
41.099370	1199.959752	17.921920
40.775427	1216.789073	17.926938
40.680240	1204.584238	17.931955
41.387702	1198.509023	17.936973
41.306904	1197.737998	17.941991
41.344482	1202.239846	17.947008
41.511958	1203.176892	17.952026
41.614102	1197.245395	17.957043
41.458661	1206.173135	17.962061
41.605295	1206.685634	17.967079
41.410378	1190.496438	17.972096
41.258221	1184.602352	17.977114
41.491415	1195.514652	17.982131
41.318443	1205.156206	17.987149
41.354199	1202.573313	17.992167
41.036942	1199.423784	17.997184
41.236983	1212.562535	18.002202
41.470080	1205.158223	18.007219
41.307257	1205.578495	18.012237
41.497147	1205.788362	18.017255
41.668782	1199.191393	18.022272
41.386161	1206.338267	18.027290
41.578503	1218.833299	18.032307
42.195283	1220.920963	18.037325
41.715684	1223.716725	18.042343
41.814145	1222.135304	18.047360
41.958543	1218.651027	18.052378
42.164618	1226.342912	18.057395
42.036229	1215.206748	18.062413
41.995985	1226.842234	18.067431
42.379178	1223.429991	18.072448
41.728933	1227.525568	18.077466
41.915562	1226.521556	18.082483
42.273085	1222.614748	18.087501
42.069695	1225.415230	18.092519
42.156295	1225.803594	18.097536
42.186360	1229.381692	18.102554
41.958008	1220.767342	18.107571
42.077878	1224.905284	18.112589
42.371074	1244.610876	18.117607
42.935140	1240.410000	18.122624
43.083728	1237.964841	18.127642
42.519602	1226.043982	18.132659
42.637324	1216.204096	18.137677
42.163117	1218.214042	18.142695
42.283256	1231.791849	18.147712
42.659310	1252.737965	18.152730
42.765173	1242.404439	18.157747
43.202754	1243.982697	18.162765
42.610966	1246.893882	18.167783
43.070237	1242.689267	18.172800
43.021784	1245.836287	18.177818
43.035775	1249.151107	18.182835
42.970778	1241.668467	18.187853
42.834096	1257.867066	18.192871
43.079693	1237.682790	18.197888
42.730828	1246.721624	18.202906
43.115010	1244.276649	18.207923
43.230697	1246.139050	18.212941
43.182945	1246.992440	18.217959
43.395282	1234.121902	18.222976
43.206431	1240.739451	18.227994
43.067795	1245.127837	18.233011
43.371028	1238.550765	18.238029
43.183457	1256.769418	18.243047
43.666934	1256.512464	18.248064
43.479648	1273.066796	18.253082
43.716071	1263.091543	18.258099
43.773549	1264.524345	18.263117
43.661273	1270.822949	18.268135
43.814569	1268.631871	18.273152
43.680918	1267.929046	18.278170
43.889256	1268.502496	18.283187
44.137041	1257.315752	18.288205
43.846555	1267.753178	18.293223
44.130112	1261.449799	18.298240
44.163560	1264.826015	18.303258
44.063324	1260.268585	18.308275
44.280039	1257.998180	18.313293
43.796367	1253.413804	18.318311
43.975492	1252.708296	18.323328
43.946917	1268.818881	18.328346
43.730018	1263.771954	18.333363
44.015660	1265.387027	18.338381
44.023295	1258.636854	18.343399
43.962483	1257.121727	18.348416
44.087423	1272.045346	18.353434
44.174490	1286.499954	18.358451
44.513911	1287.873641	18.363469
44.138798	1298.516496	18.368487
44.343323	1291.330634	18.373504
44.491097	1297.505983	18.378522
44.262740	1296.278698	18.383539
44.640105	1293.092317	18.388557
44.528984	1293.947950	18.393575
44.466134	1296.751203	18.398592
44.532133	1302.505429	18.403610
44.605288	1313.421315	18.408627
45.014296	1316.451358	18.413645
44.780060	1325.361846	18.418663
45.162694	1319.116578	18.423680
45.166593	1315.566591	18.428698
45.108567	1322.138145	18.433715
45.277295	1316.262051	18.438733
45.282581	1315.533923	18.443751
45.424249	1310.036536	18.448768
45.345991	1310.336357	18.453786
45.068889	1312.799389	18.458803
45.424527	1305.608300	18.463821
45.122075	1312.015901	18.468839
45.072815	1312.691779	18.473856
45.406188	1309.691739	18.478874
45.073985	1309.478336	18.483891
45.233444	1311.491071	18.488909
45.296177	1311.117160	18.493927
45.428533	1311.112829	18.498944
45.325286	1314.808163	18.503962
45.539012	1328.149335	18.508979
45.773235	1341.208818	18.513997
45.721800	1345.179050	18.519015
45.933572	1336.864120	18.524032
46.088003	1344.035752	18.529050
46.147141	1346.646525	18.534067
45.911014	1343.647627	18.539085
46.077196	1341.630666	18.544103
45.827996	1336.282116	18.549120
46.097052	1337.185670	18.554138
45.871931	1339.667160	18.559155
46.428369	1335.969282	18.564173
45.971814	1333.368914	18.569191
46.001860	1329.591378	18.574208
46.316842	1329.842650	18.579226
46.103243	1332.098926	18.584243
46.057905	1326.832705	18.589261
46.032049	1336.361222	18.594279
46.558259	1351.384534	18.599296
46.566832	1357.984812	18.604314
46.564374	1361.604309	18.609331
46.676489	1360.266096	18.614349
46.903655	1355.709912	18.619367
46.851035	1357.783215	18.624384
46.840383	1346.736716	18.629402
46.765969	1355.981971	18.634419
47.006685	1351.820041	18.639437
46.878185	1358.078798	18.644455
47.049414	1357.033188	18.649472
47.354007	1345.949006	18.654490
47.047615	1343.546493	18.659507
47.027551	1333.220398	18.664525
46.523505	1347.180999	18.669543
46.796177	1349.993683	18.674560
46.988419	1345.421048	18.679578
47.012197	1351.141126	18.684595
46.950350	1354.884926	18.689613
47.236960	1358.738334	18.694631
47.205946	1367.465428	18.699648
47.241487	1360.286028	18.704666
47.315198	1361.744566	18.709683
47.726684	1372.112602	18.714701
47.871804	1373.699757	18.719719
47.566366	1363.696007	18.724736
47.520635	1355.330890	18.729754
47.431350	1362.487910	18.734771
47.605321	1370.829951	18.739789
47.371392	1386.653293	18.744807
47.528614	1385.905652	18.749824
47.728539	1393.081852	18.754842
47.719950	1394.912178	18.759859
47.706947	1392.352758	18.764877
47.986645	1393.139784	18.769895
47.817701	1383.126053	18.774912
47.919362	1381.626692	18.779930
47.851532	1390.742713	18.784947
48.095083	1409.369452	18.789965
48.097174	1420.868564	18.794983
48.321374	1413.423093	18.800000
48.511848	1417.689049	18.805018
48.252797	1427.258743	18.810035
48.710320	1414.655699	18.815053
48.516797	1412.338213	18.820071
48.337398	1416.932144	18.825088
48.606441	1408.016565	18.830106
48.668393	1414.982748	18.835123
48.537995	1413.036667	18.840141
48.696744	1412.439797	18.845159
48.589884	1417.912523	18.850176
48.656390	1404.438219	18.855194
48.545537	1409.806969	18.860211
48.633122	1407.478479	18.865229
48.712483	1408.995111	18.870247
48.597542	1415.633201	18.875264
49.099827	1422.608613	18.880282
48.978516	1441.359643	18.885299
49.213018	1440.465179	18.890317
49.161284	1444.887746	18.895335
49.027694	1449.007178	18.900352
49.309459	1445.437234	18.905370
49.171622	1448.604844	18.910387
49.289900	1442.856298	18.915405
49.246834	1441.531811	18.920423
49.303331	1445.684641	18.925440
49.772349	1437.828872	18.930458
49.311349	1435.789209	18.935475
49.260636	1438.665276	18.940493
49.414315	1438.364165	18.945511
49.282169	1441.527720	18.950528
49.634392	1438.297339	18.955546
49.526626	1458.682233	18.960563
49.808501	1453.716160	18.965581
50.173232	1456.155523	18.970599
49.894900	1462.929017	18.975616
50.022845	1458.537280	18.980634
49.860706	1461.596292	18.985651
49.954161	1458.992355	18.990669
49.969228	1453.292511	18.995687
50.060369	1457.888149	19.000704
49.984995	1458.738091	19.005722
49.976047	1454.956515	19.010739
49.806307	1459.684205	19.015757
50.298532	1463.445864	19.020775
50.137752	1459.522539	19.025792
50.498429	1457.027007	19.030810
50.263233	1471.069128	19.035827
50.377423	1480.133371	19.040845
50.640551	1481.416206	19.045863
50.528124	1494.090640	19.050880
50.580070	1481.752780	19.055898
50.536126	1484.219561	19.060915
50.541286	1486.143663	19.065933
50.790810	1479.728424	19.070951
50.474304	1486.482847	19.075968
50.795539	1483.432010	19.080986
50.647942	1487.845493	19.086003
50.624993	1485.581809	19.091021
51.016809	1497.457727	19.096039
50.967903	1511.135900	19.101056
51.371341	1505.404782	19.106074
51.182908	1511.371128	19.111091
51.502001	1511.569051	19.116109
51.887042	1505.401189	19.121127
51.306253	1487.890448	19.126144
51.394301	1483.634058	19.131162
51.409600	1489.892751	19.136179
51.737996	1490.767189	19.141197
51.498437	1494.183059	19.146215
51.735554	1497.950012	19.151232
51.738312	1502.284467	19.156250
51.361513	1505.602669	19.161267
51.498545	1508.372517	19.166285
51.760367	1500.558407	19.171303
51.624524	1506.856938	19.176320
51.492199	1500.438869	19.181338
51.658555	1496.938440	19.186355
51.830073	1505.313198	19.191373
51.804846	1502.809192	19.196391
51.904824	1518.637637	19.201408
52.244661	1529.261040	19.206426
52.040032	1532.683147	19.211443
52.007293	1529.250639	19.216461
52.215066	1535.626530	19.221479
52.046938	1536.677678	19.226496
52.320201	1527.534828	19.231514
52.244666	1534.780192	19.236531
52.328490	1527.075465	19.241549
52.378663	1524.811127	19.246567
52.102196	1527.520281	19.251584
52.842502	1534.562405	19.256602
52.690559	1532.015676	19.261619
52.639703	1544.954054	19.266637
53.070610	1538.234575	19.271655
52.956013	1544.344896	19.276672
52.815582	1529.280045	19.281690
52.668654	1524.059054	19.286707
53.171572	1543.641946	19.291725
53.216214	1557.144790	19.296743
52.979904	1548.245998	19.301760
53.082683	1543.829145	19.306778
53.115809	1548.928013	19.311795
52.965175	1555.477472	19.316813
53.003247	1546.927414	19.321831
52.908654	1552.273174	19.326848
53.064033	1554.329855	19.331866
53.150991	1556.649140	19.336883
53.402173	1557.577583	19.341901
53.167051	1556.726535	19.346919
53.742248	1577.590242	19.351936
53.766408	1572.885457	19.356954
53.732915	1575.518907	19.361971
53.399608	1580.636889	19.366989
53.940625	1565.887287	19.372007
54.150285	1578.026708	19.377024
54.248167	1574.876182	19.382042
54.417942	1564.970342	19.387059
54.242341	1552.718259	19.392077
54.402494	1540.157020	19.397095
54.071400	1543.150178	19.402112
54.171238	1539.497531	19.407130
53.895290	1531.565440	19.412147
53.897650	1557.430073	19.417165
54.357123	1571.447254	19.422183
54.133368	1559.527686	19.427200
54.326272	1567.511303	19.432218
54.365344	1568.525481	19.437235
54.295394	1568.539252	19.442253
54.530281	1572.000614	19.447271
54.349798	1576.995120	19.452288
54.447368	1573.085626	19.457306
54.534212	1569.424032	19.462323
54.178091	1586.947138	19.467341
54.778604	1597.773642	19.472359
54.643757	1602.557951	19.477376
54.573695	1599.047217	19.482394
54.963926	1597.341364	19.487411
54.651362	1604.262747	19.492429
54.980664	1593.929524	19.497447
54.778409	1606.059143	19.502464
55.190687	1616.496446	19.507482
55.396464	1620.981043	19.512499
55.277594	1628.640010	19.517517
55.492919	1629.737777	19.522535
55.641212	1621.607422	19.527552
55.526376	1629.308220	19.532570
55.737877	1622.659084	19.537587
55.818503	1630.883232	19.542605
55.943931	1616.773242	19.547623
55.940602	1597.092226	19.552640
55.593398	1583.863844	19.557658
55.465557	1587.880147	19.562675
55.440245	1606.430456	19.567693
56.088706	1611.093797	19.572711
55.851420	1627.055580	19.577728
55.749095	1624.417549	19.582746
56.012045	1622.295454	19.587763
56.001597	1626.941952	19.592781
56.000238	1614.124032	19.597799
56.080310	1623.187513	19.602816
55.863281	1621.998506	19.607834
55.841204	1618.414046	19.612851
55.813586	1623.222950	19.617869
56.261761	1644.521520	19.622887
56.209310	1652.489249	19.627904
56.433006	1651.985838	19.632922
56.283399	1652.048493	19.637939
56.370343	1659.317563	19.642957
56.722497	1651.297050	19.647975
56.696128	1655.445850	19.652992
56.565633	1658.557275	19.658010
56.715936	1648.614371	19.663027
56.466444	1673.221559	19.668045
56.854411	1676.185819	19.673063
56.974880	1685.593699	19.678080
56.764919	1683.543071	19.683098
56.899180	1683.133363	19.688115
57.108109	1685.309732	19.693133
57.067743	1679.888426	19.698151
56.819672	1680.183083	19.703168
57.224624	1691.882452	19.708186
57.437425	1699.272267	19.713203
57.339107	1711.488439	19.718221
57.677200	1706.312746	19.723239
57.721821	1701.383634	19.728256
57.419884	1705.734486	19.733274
57.620945	1702.598942	19.738291
57.733935	1702.412073	19.743309
57.862553	1698.244325	19.748327
57.759259	1701.996396	19.753344
57.957487	1701.922571	19.758362
58.177835	1686.800028	19.763379
57.938050	1701.618642	19.768397
57.928748	1694.679835	19.773415
58.233035	1695.178227	19.778432
58.238183	1700.814892	19.783450
58.572279	1686.927191	19.788467
58.126933	1698.051106	19.793485
58.259663	1690.115900	19.798503
58.434787	1688.117918	19.803520
58.291795	1702.774014	19.808538
58.338323	1691.264295	19.813555
58.204014	1703.844081	19.818573
58.418318	1707.727991	19.823591
58.731183	1714.928817	19.828608
58.625247	1717.758685	19.833626
58.910730	1718.435478	19.838643
58.636962	1720.726576	19.843661
59.006607	1719.455024	19.848679
59.057891	1717.972314	19.853696
58.865855	1719.533828	19.858714
58.643796	1717.341971	19.863731
58.900987	1723.953897	19.868749
58.974626	1719.377249	19.873767
59.077668	1729.342457	19.878784
59.169920	1717.492714	19.883802
59.324827	1725.198530	19.888819
59.045877	1743.958568	19.893837
59.562956	1748.280302	19.898855
59.598614	1740.929227	19.903872
59.255931	1757.767664	19.908890
59.769350	1751.632715	19.913907
59.684957	1747.673533	19.918925
59.419411	1749.815452	19.923943
59.721959	1751.722845	19.928960
59.674697	1748.132144	19.933978
60.050387	1738.936649	19.938995
59.700107	1740.200123	19.944013
60.129064	1742.626936	19.949031
60.085172	1746.242124	19.954048
59.882933	1748.486426	19.959066
60.216246	1760.410431	19.964083
60.121430	1766.087444	19.969101
60.236817	1772.121861	19.974119
60.467877	1760.470972	19.979136
60.485009	1772.572826	19.984154
60.335251	1761.777082	19.989171
60.475180	1773.714629	19.994189
60.360570	1778.605100	19.999207
60.398516	1776.404811	20.004224
60.395118	1774.061668	20.009242
60.570229	1777.012697	20.014259
60.705283	1784.026394	20.019277
60.615364	1799.516528	20.024295
60.695095	1804.178592	20.029312
60.802193	1804.306499	20.034330
60.954381	1800.131817	20.039347
60.833783	1804.246131	20.044365
61.077611	1795.411420	20.049383
61.232752	1789.225827	20.054400
60.964382	1810.414728	20.059418
61.561241	1821.903480	20.064435
61.740160	1824.009933	20.069453
61.567086	1821.456297	20.074471
61.713096	1821.719580	20.079488
61.873057	1821.773774	20.084506
61.864420	1808.903357	20.089523
61.679101	1800.281013	20.094541
61.789673	1809.918654	20.099559
61.819003	1809.693998	20.104576
61.877347	1819.676621	20.109594
62.073673	1815.108696	20.114611
62.266431	1815.946579	20.119629
62.068891	1819.683819	20.124647
62.099192	1822.912006	20.129664
62.058844	1824.848916	20.134682
62.325088	1818.986175	20.139699
62.312777	1822.763097	20.144717
61.999403	1823.496844	20.149735
62.395189	1810.947353	20.154752
62.201067	1820.585606	20.159770
62.130889	1814.782016	20.164787
62.356974	1818.060786	20.169805
62.242770	1826.027445	20.174823
62.422553	1831.751152	20.179840
62.427742	1845.944076	20.184858
62.439868	1836.085215	20.189875
62.810184	1843.662360	20.194893
62.606477	1841.968597	20.199911
63.064103	1846.523225	20.204928
62.634971	1874.916016	20.209946
63.033575	1876.565062	20.214963
62.932864	1875.166351	20.219981
62.734354	1880.370701	20.224999
63.028999	1874.568694	20.230016
62.935224	1888.513154	20.235034
63.126563	1893.965252	20.240051
63.431158	1905.096380	20.245069
63.636377	1907.986789	20.250087
63.890138	1901.344947	20.255104
63.852470	1906.607821	20.260122
63.735562	1901.433034	20.265139
63.693194	1903.967279	20.270157
63.843825	1902.158016	20.275175
64.037195	1906.997062	20.280192
64.064310	1908.898056	20.285210
64.298041	1904.291103	20.290227
63.863808	1904.702755	20.295245
63.981981	1899.134957	20.300263
64.439253	1890.692473	20.305280
64.049665	1902.250487	20.310298
64.213584	1920.935415	20.315315
64.520217	1930.213089	20.320333
64.313268	1929.735077	20.325351
64.501281	1929.150039	20.330368
64.562582	1933.423374	20.335386
64.685630	1926.625386	20.340403
64.662334	1923.652993	20.345421
64.588808	1925.383620	20.350439
64.960295	1923.808931	20.355456
64.719125	1928.396353	20.360474
64.711352	1928.990134	20.365491
64.828435	1931.229167	20.370509
64.748878	1948.252397	20.375527
64.932331	1945.959663	20.380544
64.775241	1954.883402	20.385562
64.884425	1946.931361	20.390579
65.294003	1949.200841	20.395597
65.162214	1956.722030	20.400615
65.616520	1968.784228	20.405632
65.584939	1980.827164	20.410650
65.602166	1980.476225	20.415667
65.706657	1977.174324	20.420685
65.909419	1981.329942	20.425703
65.724709	1976.698446	20.430720
65.910604	1989.173933	20.435738
65.836523	1980.663528	20.440755
66.240295	1968.343881	20.445773
65.311833	1983.827123	20.450791
66.164920	1972.769062	20.455808
66.019227	1975.503065	20.460826
65.985986	1980.212303	20.465843
66.012916	1968.851005	20.470861
65.918097	1986.837900	20.475879
66.486103	1996.527791	20.480896
66.457584	2006.393822	20.485914
66.429493	2003.299472	20.490931
66.697817	2017.692084	20.495949
66.387461	2013.838078	20.500967
66.723949	2001.281362	20.505984
66.485113	2007.251227	20.511002
66.890517	2022.009764	20.516019
67.194061	2023.666906	20.521037
67.041409	2036.942873	20.526055
67.381495	2042.328047	20.531072
67.211564	2041.156665	20.536090
67.208707	2035.531029	20.541107
67.752765	2028.576981	20.546125
67.442717	2040.256923	20.551143
67.418278	2019.317828	20.556160
67.109763	2029.906545	20.561178
67.387560	2036.103952	20.566195
67.375689	2031.826366	20.571213
67.320329	2035.576385	20.576231
67.567626	2028.892255	20.581248
67.223915	2037.406108	20.586266
67.714947	2056.622688	20.591283
67.825675	2061.109206	20.596301
67.807517	2061.433281	20.601319
68.232304	2057.909604	20.606336
67.783827	2055.259829	20.611354
67.965437	2054.535012	20.616371
68.133067	2047.906051	20.621389
68.042700	2068.993792	20.626407
68.545658	2072.608388	20.631424
68.577118	2075.314949	20.636442
68.349188	2077.068641	20.641459
68.529835	2080.265047	20.646477
68.471399	2087.444247	20.651495
68.748821	2079.441711	20.656512
68.474139	2076.930187	20.661530
68.247823	2084.855870	20.666547
68.656388	2081.289152	20.671565
68.798714	2088.378921	20.676583
69.107878	2102.458340	20.681600
68.975346	2120.949316	20.686618
69.202077	2112.188719	20.691635
69.297813	2104.919911	20.696653
69.373464	2113.309520	20.701671
69.432250	2105.392959	20.706688
69.476322	2104.996048	20.711706
69.258330	2107.693622	20.716723
69.608398	2106.583263	20.721741
69.456521	2110.061591	20.726759
69.363723	2112.669985	20.731776
69.479630	2114.237498	20.736794
69.273508	2126.036229	20.741811
69.916386	2128.186735	20.746829
69.666134	2142.828125	20.751847
69.963913	2137.225306	20.756864
70.095222	2132.693607	20.761882
70.023525	2140.265089	20.766899
70.241580	2129.879223	20.771917
70.223290	2140.250269	20.776935
70.256776	2149.737605	20.781952
70.679635	2155.303909	20.786970
70.526196	2162.378734	20.791987
70.998052	2156.498019	20.797005
70.719915	2159.213845	20.802023
70.941778	2160.296454	20.807040
71.049338	2157.274832	20.812058
71.039937	2161.565800	20.817075
70.892419	2152.281999	20.822093
71.114435	2155.595319	20.827111
71.207156	2151.665993	20.832128
71.292529	2161.331483	20.837146
71.175802	2157.104402	20.842163
71.272241	2147.541012	20.847181
71.434922	2148.418322	20.852199
71.351322	2148.169192	20.857216
71.546127	2138.540569	20.862234
71.391041	2153.033864	20.867251
71.740699	2145.166864	20.872269
71.371120	2152.229739	20.877287
71.249648	2153.959386	20.882304
71.719885	2170.234485	20.887322
71.562732	2176.778968	20.892339
71.812455	2175.049048	20.897357
71.976952	2184.256733	20.902375
71.869407	2180.889486	20.907392
72.177609	2179.201369	20.912410
72.105820	2186.912115	20.917427
72.376397	2200.371665	20.922445
71.885709	2207.483767	20.927463
72.258775	2214.630409	20.932480
72.354929	2216.581788	20.937498
71.855112	2220.288668	20.942515
72.343346	2211.763193	20.947533
72.658580	2231.433577	20.952551
72.668278	2238.797059	20.957568
73.221482	2246.337389	20.962586
72.989767	2245.194718	20.967603
73.050913	2238.628272	20.972621
72.807999	2244.604388	20.977639
72.960042	2246.828457	20.982656
73.030279	2236.338659	20.987674
73.090915	2247.782681	20.992691
73.068017	2238.049480	20.997709
73.175372	2234.110719	21.002727
73.321768	2251.047933	21.007744
73.730570	2250.841423	21.012762
73.618465	2265.461694	21.017779
73.843286	2258.376740	21.022797
73.706810	2266.830151	21.027815
73.760585	2257.890174	21.032832
73.953518	2252.334706	21.037850
73.917826	2259.523735	21.042867
74.210161	2253.567778	21.047885
74.314896	2251.138097	21.052903
74.301642	2257.572361	21.057920
74.565064	2256.025095	21.062938
74.407918	2252.703497	21.067955
74.189679	2250.838953	21.072973
74.491556	2252.586847	21.077991
74.717011	2264.242936	21.083008
74.694087	2274.248267	21.088026
74.303490	2282.363859	21.093043
74.868223	2284.758893	21.098061
74.862649	2277.094770	21.103079
74.803076	2272.449518	21.108096
75.200056	2274.156293	21.113114
75.205270	2280.928214	21.118131
75.055752	2274.665926	21.123149
74.877625	2273.584715	21.128167
75.143814	2280.158492	21.133184
75.511609	2294.075366	21.138202
75.004273	2310.388507	21.143219
75.508578	2298.460006	21.148237
75.420637	2303.554058	21.153255
75.517603	2306.741047	21.158272
75.702583	2307.083865	21.163290
75.555456	2303.353992	21.168307
75.878129	2296.992021	21.173325
75.996923	2315.123814	21.178343
76.016995	2326.470536	21.183360
76.083872	2327.229413	21.188378
75.801025	2332.139813	21.193395
76.255730	2332.576491	21.198413
76.160436	2327.877924	21.203431
76.277121	2331.969496	21.208448
76.098339	2328.184096	21.213466
76.294068	2325.784731	21.218483
76.768724	2336.626355	21.223501
76.832416	2345.904490	21.228519
76.910769	2350.208265	21.233536
77.241790	2347.207608	21.238554
77.046982	2343.077088	21.243571
77.261684	2342.714318	21.248589
77.434696	2331.644081	21.253607
77.067088	2327.077031	21.258624
77.425958	2320.050905	21.263642
77.068723	2328.087264	21.268659
77.548645	2337.109459	21.273677
77.728453	2339.136401	21.278695
77.690974	2345.337803	21.283712
78.053909	2335.848213	21.288730
77.484931	2337.194587	21.293747
77.493450	2340.188813	21.298765
78.159995	2339.787821	21.303783
77.703383	2345.717820	21.308800
77.786974	2342.085656	21.313818
78.055010	2348.334310	21.318835
78.033232	2350.446098	21.323853
78.205773	2341.321162	21.328871
77.550387	2344.306405	21.333888
78.061113	2355.909216	21.338906
78.192744	2381.683120	21.343923
78.352331	2367.562240	21.348941
78.249326	2369.620907	21.353959
78.194166	2379.217705	21.358976
78.423694	2384.711881	21.363994
78.559374	2399.427286	21.369011
78.864790	2393.366929	21.374029
78.989072	2385.951844	21.379047
79.215946	2388.081411	21.384064
79.374925	2381.040719	21.389082
79.225645	2384.261482	21.394099
79.368065	2389.996088	21.399117
79.543652	2383.647307	21.404135
79.205975	2391.590910	21.409152
79.602399	2389.235833	21.414170
79.440438	2391.969360	21.419187
80.035276	2396.805912	21.424205
80.117503	2391.548857	21.429223
79.561198	2379.834237	21.434240
80.231467	2393.508690	21.439258
80.218034	2407.601300	21.444275
80.254198	2419.192518	21.449293
80.397243	2403.050339	21.454311
80.140712	2402.549538	21.459328
80.082864	2406.368482	21.464346
80.288736	2398.460560	21.469363
80.424905	2403.818605	21.474381
80.574384	2405.016605	21.479399
80.306842	2407.654487	21.484416
80.769407	2406.056575	21.489434
80.149888	2408.852835	21.494451
80.371152	2408.406426	21.499469
80.687081	2422.130325	21.504487
80.508519	2437.701343	21.509504
80.960360	2432.652781	21.514522
80.992690	2434.047233	21.519539
81.117199	2428.752745	21.524557
81.369865	2434.905563	21.529575
81.013655	2435.215113	21.534592
81.066278	2432.951031	21.539610
81.434411	2453.769573	21.544627
81.222686	2462.947750	21.549645
81.501715	2467.326540	21.554663
81.307505	2462.280294	21.559680
81.645926	2465.324202	21.564698
81.740786	2482.790629	21.569715
81.861482	2491.894583	21.574733
81.948625	2486.579288	21.579751
81.897744	2492.152825	21.584768
82.097607	2494.584835	21.589786
82.159359	2495.727611	21.594803
81.970301	2487.797658	21.599821
82.387078	2502.639038	21.604839
82.506623	2506.100140	21.609856
83.141846	2499.021214	21.614874
83.553171	2503.658950	21.619891
83.376846	2504.753947	21.624909
83.654716	2485.039482	21.629927
83.427509	2480.730811	21.634944
83.473329	2469.075072	21.639962
83.038981	2465.867629	21.644979
83.271004	2463.902948	21.649997
83.280893	2457.435034	21.655015
83.407153	2466.730014	21.660032
83.496643	2468.940494	21.665050
83.442503	2465.908407	21.670067
83.390152	2488.484437	21.675085
83.983278	2489.785545	21.680103
83.607190	2496.807932	21.685120
83.962607	2496.272483	21.690138
84.044265	2491.881525	21.695155
84.031070	2498.226213	21.700173
84.352945	2483.254992	21.705191
84.205016	2494.269944	21.710208
84.114498	2490.945532	21.715226
83.942749	2492.495238	21.720243
84.245252	2497.023681	21.725261
84.909882	2499.579024	21.730279
84.601260	2513.961861	21.735296
84.642759	2511.315681	21.740314
84.822485	2519.638589	21.745331
84.561898	2520.344284	21.750349
84.687044	2517.784663	21.755367
84.801052	2522.251137	21.760384
84.721582	2516.963183	21.765402
84.550027	2530.529718	21.770419
84.651049	2543.589499	21.775437
85.138062	2549.300689	21.780455
84.845145	2557.124760	21.785472
85.309234	2552.012851	21.790490
85.519992	2562.571070	21.795507
85.438789	2577.147396	21.800525
85.668036	2575.700727	21.805543
85.820512	2583.449077	21.810560
85.893638	2585.830516	21.815578
85.795244	2580.894021	21.820595
86.148756	2575.865022	21.825613
86.144762	2576.889284	21.830631
85.859491	2579.283030	21.835648
86.112545	2592.250179	21.840666
86.681776	2601.454951	21.845683
86.706920	2612.507684	21.850701
87.095081	2599.313725	21.855719
86.681042	2605.951273	21.860736
86.981222	2599.233282	21.865754
87.244338	2598.191029	21.870771
87.128655	2597.283901	21.875789
87.003906	2603.957130	21.880807
87.206301	2597.639379	21.885824
87.250851	2591.603230	21.890842
87.605865	2591.693978	21.895859
87.250774	2596.438212	21.900877
87.179103	2592.875578	21.905895
87.237756	2597.485410	21.910912
87.433228	2596.733973	21.915930
87.299602	2592.230216	21.920947
87.555200	2613.660816	21.925965
87.901203	2613.859978	21.930983
87.620593	2611.649787	21.936000
87.584439	2623.227526	21.941018
88.139381	2619.615319	21.946035
87.903578	2627.087362	21.951053
87.906706	2629.632570	21.956071
88.141482	2650.599302	21.961088
88.318032	2647.735699	21.966106
88.378405	2655.896796	21.971123
88.328568	2659.886795	21.976141
88.491870	2666.012270	21.981159
88.411731	2677.742588	21.986176
88.734138	2680.451641	21.991194
88.536286	2677.212736	21.996211
88.766036	2673.780582	22.001229
89.057594	2694.910590	22.006247
89.164629	2701.329017	22.011264
89.433312	2706.634581	22.016282
89.305601	2701.784526	22.021299
89.203132	2715.330778	22.026317
89.708362	2708.243375	22.031335
89.565928	2704.767511	22.036352
89.522533	2702.689390	22.041370
89.633488	2700.707011	22.046387
89.409189	2711.678453	22.051405
90.138854	2722.865148	22.056423
90.281264	2732.327630	22.061440
90.004642	2730.223763	22.066458
90.508671	2722.497819	22.071475
90.349825	2731.572552	22.076493
90.329783	2719.969591	22.081511
90.653685	2724.115549	22.086528
90.476540	2730.132505	22.091546
90.733619	2723.470886	22.096563
90.763572	2721.082943	22.101581
90.793598	2719.815120	22.106599
91.155279	2731.983972	22.111616
91.076010	2743.625317	22.116634
91.477890	2736.753392	22.121651
91.650914	2752.784703	22.126669
91.697332	2743.920330	22.131687
91.631917	2746.882378	22.136704
91.773922	2743.417789	22.141722
92.214751	2735.412442	22.146739
91.782221	2723.249105	22.151757
91.836999	2707.874235	22.156775
92.108180	2722.949080	22.161792
91.774663	2725.772164	22.166810
92.338292	2725.032817	22.171827
92.115656	2727.320633	22.176845
92.163290	2725.233501	22.181863
92.106361	2725.188559	22.186880
91.939458	2732.924197	22.191898
92.259354	2727.137496	22.196915
92.312225	2750.363411	22.201933
92.574143	2756.077536	22.206951
92.477854	2757.794585	22.211968
92.448100	2762.137744	22.216986
92.557448	2761.361488	22.222003
92.425394	2782.789642	22.227021
92.886543	2792.024355	22.232039
92.993783	2794.442867	22.237056
92.849211	2796.663184	22.242074
93.482041	2808.063611	22.247091
93.377785	2819.388062	22.252109
93.346345	2821.359867	22.257127
93.551581	2825.530281	22.262144
93.452464	2822.911184	22.267162
93.559271	2813.672938	22.272179
93.395574	2839.944682	22.277197
93.788214	2849.548265	22.282215
94.080346	2852.587838	22.287232
93.968875	2851.446397	22.292250
94.026706	2853.612426	22.297267
94.479152	2869.885643	22.302285
94.443464	2880.755557	22.307303
94.805244	2887.865003	22.312320
94.800851	2880.873719	22.317338
94.896070	2873.185346	22.322355
94.617758	2877.320385	22.327373
94.896310	2880.004218	22.332391
94.772707	2887.392428	22.337408
95.159094	2880.617301	22.342426
95.672699	2870.726556	22.347443
95.747737	2867.757958	22.352461
95.483316	2865.619874	22.357479
95.393693	2864.622045	22.362496
95.318761	2867.224578	22.367514
95.622463	2879.830718	22.372531
95.247022	2893.209843	22.377549
96.115572	2898.432421	22.382567
96.329675	2899.026264	22.387584
95.843148	2903.389589	22.392602
96.299533	2895.232219	22.397619
96.272782	2895.025142	22.402637
96.132756	2894.047147	22.407655
96.213530	2888.543933	22.412672
96.266298	2902.076620	22.417690
96.650543	2903.479510	22.422707
96.734613	2916.381071	22.427725
96.625808	2912.428610	22.432743
96.995402	2918.791111	22.437760
96.416729	2921.153028	22.442778
96.819736	2934.765988	22.447795
96.798395	2943.601035	22.452813
97.210132	2945.219801	22.457831
97.286466	2948.908938	22.462848
97.025013	2952.120177	22.467866
97.628383	2965.089229	22.472883
97.641096	2978.972126	22.477901
97.896956	2980.336497	22.482919
98.409821	2972.816684	22.487936
97.973337	2972.769327	22.492954
98.040829	2971.383808	22.497971
98.217951	2975.061602	22.502989
98.049250	2976.890122	22.508007
98.502904	2961.799864	22.513024
98.359636	2970.655153	22.518042
98.725624	2970.174642	22.523059
98.641751	2982.628705	22.528077
98.709201	3003.473163	22.533095
98.656647	3001.721336	22.538112
98.853915	2994.580638	22.543130
98.813833	3004.719785	22.548147
98.952177	2999.424459	22.553165
98.784212	2996.441089	22.558183
99.359625	3008.681504	22.563200
99.197165	3019.522176	22.568218
99.460099	3015.099799	22.573235
99.547259	3017.165209	22.578253
99.528039	3020.322895	22.583271
99.808343	3009.285386	22.588288
99.705289	3013.855842	22.593306
99.940039	3018.888466	22.598323
99.655078	3036.775601	22.603341
99.849945	3040.662972	22.608359
100.259758	3040.287173	22.613376
99.960997	3045.832793	22.618394
100.132327	3052.133355	22.623411
100.265968	3058.893026	22.628429
100.495901	3073.687693	22.633447
100.726314	3069.284645	22.638464
101.341278	3072.102096	22.643482
101.316408	3064.117332	22.648499
101.437245	3057.027334	22.653517
101.359148	3060.726963	22.658535
101.562901	3059.775955	22.663552
101.479982	3060.929255	22.668570
101.656460	3052.044746	22.673587
101.707465	3053.476398	22.678605
101.531291	3066.620173	22.683623
101.836278	3055.135036	22.688640
101.611405	3070.639380	22.693658
101.944337	3078.388328	22.698675
101.996378	3090.565159	22.703693
102.053426	3096.386812	22.708711
102.118549	3089.973530	22.713728
102.096979	3096.691888	22.718746
102.209894	3097.912297	22.723763
102.355302	3105.318296	22.728781
102.453504	3122.674828	22.733799
102.453605	3123.651277	22.738816
102.589545	3120.772820	22.743834
102.799489	3125.222610	22.748851
102.807645	3133.697512	22.753869
102.724946	3155.451086	22.758887
103.307361	3149.719909	22.763904
102.851210	3156.048976	22.768922
103.263190	3163.486447	22.773939
103.677812	3173.081234	22.778957
103.348562	3187.866054	22.783975
103.600552	3188.954955	22.788992
103.878997	3184.441166	22.794010
103.414437	3188.729487	22.799027
103.907244	3204.243836	22.804045
103.780671	3219.814474	22.809063
104.425966	3219.801525	22.814080
104.295233	3224.433884	22.819098
104.347935	3214.676180	22.824115
104.525035	3219.632322	22.829133
104.192143	3235.006960	22.834151
104.664049	3242.786544	22.839168
104.810487	3240.015732	22.844186
104.866921	3240.611916	22.849203
105.068693	3237.744966	22.854221
105.119194	3238.710241	22.859239
105.322663	3244.356001	22.864256
105.358976	3250.809545	22.869274
105.496794	3268.489534	22.874291
105.673957	3277.048488	22.879309
105.358780	3284.048949	22.884327
105.776860	3273.636679	22.889344
106.048334	3278.462946	22.894362
106.120602	3271.078520	22.899379
106.099806	3269.233494	22.904397
106.094401	3274.857503	22.909415
105.923485	3280.026480	22.914432
106.178254	3297.847546	22.919450
106.200463	3301.041166	22.924467
106.623205	3295.884465	22.929485
106.227091	3294.973231	22.934503
106.635854	3309.765584	22.939520
106.952754	3318.426573	22.944538
107.098502	3322.863060	22.949555
107.423750	3320.108564	22.954573
107.404950	3333.712058	22.959591
107.479195	3314.713324	22.964608
107.281693	3324.446711	22.969626
107.502574	3325.884344	22.974643
108.133929	3333.473361	22.979661
107.856339	3353.712551	22.984679
107.836627	3344.067783	22.989696
108.110669	3349.935178	22.994714
107.811041	3345.684207	22.999731
108.054442	3352.409995	23.004749
107.973410	3353.161043	23.009767
107.979913	3361.679605	23.014784
108.126838	3375.417190	23.019802
108.290777	3386.777196	23.024819
108.314968	3377.115181	23.029837
108.471453	3404.695421	23.034855
108.558566	3414.230880	23.039872
108.995059	3415.346235	23.044890
108.775043	3412.388383	23.049907
109.257751	3427.228065	23.054925
109.036200	3451.227277	23.059943
109.244828	3437.981742	23.064960
109.564631	3443.485528	23.069978
109.619626	3442.572373	23.074995
110.050200	3447.734402	23.080013
110.359714	3458.978431	23.085031
110.273653	3450.105647	23.090048
110.932067	3452.432460	23.095066
110.531220	3451.282041	23.100083
110.788825	3432.801428	23.105101
110.571955	3439.852367	23.110119
110.575505	3426.980942	23.115136
110.868819	3439.372896	23.120154
110.754933	3446.796022	23.125171
111.038193	3443.632062	23.130189
110.981595	3444.307633	23.135207
110.732899	3439.232760	23.140224
110.837977	3446.181240	23.145242
110.829273	3444.488447	23.150259
111.098050	3457.111669	23.155277
111.164595	3479.339877	23.160295
111.645714	3474.431829	23.165312
111.492803	3479.402915	23.170330
111.486740	3481.098582	23.175347
111.668727	3494.676506	23.180365
112.036638	3499.961823	23.185383
111.949653	3499.876830	23.190400
112.403822	3495.164229	23.195418
112.532703	3502.997856	23.200435
112.377794	3491.289922	23.205453
112.480069	3514.804953	23.210471
112.345440	3522.864679	23.215488
112.945933	3520.598827	23.220506
112.720714	3532.905974	23.225523
113.199581	3521.565030	23.230541
112.992351	3532.477722	23.235559
112.894086	3555.640905	23.240576
113.159267	3561.403600	23.245594
113.020226	3569.989540	23.250611
113.238017	3568.734188	23.255629
113.382183	3589.125936	23.260647
113.636597	3591.498303	23.265664
113.601129	3589.714575	23.270682
113.910231	3601.595970	23.275699
114.443105	3605.729320	23.280717
114.208486	3618.727148	23.285735
114.574404	3618.422057	23.290752
114.803656	3612.120831	23.295770
114.952086	3621.129816	23.300787
114.853935	3615.790163	23.305805
114.780690	3614.589860	23.310823
114.614272	3625.242024	23.315840
115.116886	3629.661042	23.320858
115.296274	3642.259343	23.325875
115.207640	3642.205292	23.330893
115.576078	3643.013706	23.335911
115.534601	3647.869538	23.340928
115.636068	3640.590403	23.345946
115.698496	3644.429826	23.350963
115.595903	3647.051852	23.355981
115.998750	3667.160176	23.360999
115.769437	3665.954858	23.366016
116.283742	3663.751500	23.371034
116.062685	3672.205830	23.376051
116.477071	3673.601635	23.381069
116.558793	3695.008051	23.386087
116.469779	3694.297985	23.391104
117.029860	3692.942425	23.396122
116.929085	3695.272319	23.401139
117.248870	3689.748794	23.406157
117.069573	3698.972129	23.411175
117.235811	3683.466761	23.416192
117.337226	3689.816506	23.421210
117.396423	3697.320723	23.426227
117.573534	3719.532454	23.431245
117.772761	3710.698202	23.436263
117.944108	3718.242762	23.441280
117.851668	3720.259813	23.446298
117.655783	3731.214109	23.451315
117.847624	3728.645221	23.456333
118.005323	3743.322283	23.461351
117.989128	3748.050611	23.466368
118.343171	3754.670840	23.471386
118.072819	3760.216129	23.476403
118.227908	3777.615500	23.481421
118.623438	3789.117469	23.486439
118.778929	3787.434646	23.491456
118.887953	3788.415800	23.496474
118.945393	3807.205080	23.501491
119.075990	3824.764958	23.506509
119.183047	3826.264844	23.511527
119.105760	3829.952736	23.516544
119.516961	3834.957513	23.521562
119.262767	3856.663159	23.526579
119.506901	3849.996018	23.531597
120.055017	3854.473146	23.536615
120.490040	3871.422864	23.541632
120.584089	3877.853319	23.546650
120.451100	3871.099186	23.551667
121.005079	3876.553217	23.556685
121.084110	3882.336278	23.561703
120.669842	3880.535025	23.566720
120.968184	3866.869666	23.571738
120.775886	3877.310590	23.576755
121.139657	3871.665919	23.581773
121.121698	3881.531529	23.586791
120.916915	3885.022640	23.591808
121.392785	3891.817817	23.596826
121.358783	3895.199102	23.601843
121.509077	3889.079482	23.606861
121.502473	3910.067623	23.611879
121.346198	3922.582798	23.616896
121.668493	3923.127184	23.621914
121.713368	3930.163373	23.626931
122.034205	3946.466644	23.631949
122.460203	3953.700112	23.636967
122.565068	3960.987141	23.641984
122.492107	3951.959350	23.647002
122.819762	3962.861031	23.652019
123.429934	3971.870566	23.657037
123.669913	3969.047733	23.662055
123.543664	3954.541374	23.667072
123.576763	3943.703061	23.672090
123.696461	3943.298765	23.677107
123.736848	3936.198358	23.682125
123.799328	3932.574675	23.687143
123.757719	3933.931498	23.692160
123.784441	3954.926191	23.697178
123.824795	3958.961951	23.702195
124.144705	3964.359718	23.707213
124.044224	3971.162644	23.712231
123.955688	3974.647043	23.717248
124.485709	3968.387397	23.722266
124.692509	3980.120209	23.727283
124.822578	3993.563699	23.732301
124.855195	4001.932147	23.737319
124.888749	3991.637320	23.742336
125.027101	3988.836191	23.747354
124.823020	3996.181146	23.752371
125.332175	3996.908148	23.757389
125.702244	4012.532608	23.762407
125.460366	4027.877040	23.767424
125.757868	4015.502618	23.772442
125.898811	4014.936025	23.777459
125.884104	4022.335762	23.782477
126.307614	4017.347042	23.787495
126.264315	4024.958235	23.792512
126.353717	4016.265605	23.797530
126.526277	4039.235330	23.802547
126.748228	4036.637989	23.807565
127.114614	4039.373333	23.812583
127.007423	4035.400642	23.817600
127.199532	4042.300131	23.822618
127.053510	4040.503292	23.827635
126.892570	4036.675265	23.832653
127.432270	4029.317421	23.837671
127.465945	4034.851316	23.842688
127.718533	4049.888017	23.847706
127.807541	4073.817492	23.852723
127.875081	4062.530699	23.857741
128.076287	4059.343504	23.862759
127.734381	4069.809988	23.867776
127.830070	4068.837600	23.872794
128.130303	4080.661799	23.877811
127.879495	4102.139916	23.882829
128.051710	4091.145579	23.887847
128.019018	4119.639194	23.892864
128.335573	4121.514000	23.897882
128.477214	4135.907662	23.902899
128.531688	4151.806790	23.907917
129.107317	4142.987007	23.912935
129.047023	4152.945297	23.917952
129.718583	4157.673461	23.922970
130.463493	4162.127179	23.927987
130.119716	4156.943703	23.933005
130.282727	4148.814326	23.938023
130.167714	4143.139680	23.943040
130.411819	4162.414934	23.948058
130.275505	4160.684187	23.953075
130.511673	4180.898461	23.958093
130.786769	4179.085603	23.963111
130.392071	4185.770329	23.968128
130.449392	4175.186803	23.973146
130.556989	4177.115383	23.978163
130.326665	4181.098381	23.983181
130.727233	4189.951090	23.988199
130.806746	4201.172571	23.993216
131.067626	4204.887674	23.998234
131.159102	4217.692437	24.003251
131.393330	4235.923066	24.008269
131.642711	4227.499816	24.013287
131.485611	4242.479304	24.018304
131.315918	4251.905206	24.023322
131.682690	4267.625654	24.028339
131.752057	4272.049434	24.033357
132.199238	4286.653355	24.038375
132.237758	4298.397516	24.043392
132.291616	4307.844455	24.048410
132.524782	4305.515902	24.053427
132.478629	4323.608826	24.058445
132.853195	4325.062183	24.063463
132.842284	4332.868979	24.068480
133.133112	4336.790175	24.073498
133.558513	4344.984489	24.078515
133.711041	4353.976752	24.083533
133.634992	4348.386285	24.088551
133.783125	4355.417230	24.093568
133.681564	4355.222844	24.098586
133.835190	4361.319894	24.103603
134.067331	4372.866467	24.108621
134.635224	4365.950021	24.113639
134.505835	4382.051783	24.118656
134.493613	4379.527903	24.123674
134.944487	4386.086569	24.128691
134.709879	4403.941372	24.133709
134.897187	4408.278734	24.138727
134.916321	4405.054409	24.143744
134.977937	4415.065817	24.148762
135.340410	4427.462532	24.153779
135.488985	4435.056721	24.158797
135.707830	4429.799974	24.163815
135.964822	4436.956783	24.168832
135.811880	4444.397651	24.173850
136.497509	4462.353629	24.178867
136.356410	4466.630865	24.183885
136.099024	4473.416555	24.188903
136.304873	4473.069314	24.193920
136.256695	4473.288876	24.198938
136.680803	4487.153242	24.203955
136.472649	4498.180079	24.208973
137.037775	4497.936049	24.213991
137.059515	4504.313010	24.219008
136.970646	4524.303441	24.224026
137.372100	4533.078333	24.229043
137.489192	4531.713871	24.234061
137.412486	4523.421108	24.239079
137.656454	4541.693833	24.244096
137.901942	4550.274109	24.249114
137.963309	4549.578576	24.254131
137.825188	4561.660282	24.259149
137.999932	4555.478273	24.264167
138.242816	4571.699476	24.269184
138.877599	4590.341860	24.274202
138.992426	4587.485367	24.279219
138.774315	4596.346482	24.284237
138.902704	4596.345940	24.289255
139.071399	4599.330826	24.294272
139.699690	4593.324310	24.299290
139.877975	4584.245062	24.304307
139.857255	4590.901031	24.309325
140.374616	4582.980833	24.314343
140.727118	4592.029474	24.319360
140.298802	4589.245407	24.324378
140.702821	4590.454151	24.329395
140.730746	4594.851593	24.334413
140.888962	4582.921365	24.339431
140.615220	4586.142778	24.344448
140.948185	4579.217271	24.349466
141.394173	4578.432098	24.354483
140.807349	4590.378456	24.359501
140.944380	4588.374363	24.364519
141.304213	4586.318229	24.369536
141.227757	4598.583666	24.374554
141.312053	4606.266076	24.379571
141.519777	4620.336568	24.384589
141.417167	4619.259657	24.389607
141.607926	4633.166083	24.394624
141.610463	4650.162838	24.399642
141.987722	4643.880063	24.404659
141.939630	4658.748190	24.409677
142.268282	4670.680836	24.414695
142.509976	4669.007773	24.419712
142.608031	4691.568717	24.424730
143.181287	4696.293852	24.429747
143.159910	4699.017189	24.434765
143.435566	4702.555414	24.439783
143.411490	4708.136532	24.444800
143.164002	4714.686312	24.449818
143.785082	4719.635911	24.454835
143.436413	4740.288770	24.459853
143.765420	4738.137617	24.464871
143.998220	4743.786364	24.469888
143.950663	4754.146615	24.474906
144.488054	4756.555097	24.479923
144.452393	4764.907329	24.484941
144.688485	4760.641341	24.489959
144.622545	4772.986278	24.494976
144.890965	4788.725325	24.499994
145.225563	4789.196197	24.505011
145.316205	4800.817588	24.510029
145.367376	4794.634725	24.515047
145.654400	4783.421745	24.520064
145.574306	4791.339726	24.525082
145.550803	4784.965010	24.530099
145.734033	4805.361660	24.535117
145.427488	4816.384751	24.540135
146.047989	4817.300173	24.545152
146.042108	4831.038307	24.550170
146.289970	4840.973898	24.555187
146.137773	4848.499815	24.560205
146.212744	4851.836413	24.565223
146.399858	4873.742259	24.570240
146.666325	4881.359583	24.575258
147.147399	4887.807454	24.580275
147.245365	4910.509572	24.585293
147.412148	4913.944048	24.590311
147.430418	4909.567984	24.595328
147.469918	4919.838161	24.600346
148.179015	4926.971127	24.605363
148.028730	4943.915483	24.610381
147.971917	4939.965198	24.615399
148.272129	4934.648098	24.620416
148.408599	4959.376269	24.625434
148.814415	4959.132458	24.630451
148.798019	4981.409988	24.635469
149.210989	4970.329415	24.640487
149.353924	4974.176807	24.645504
148.903601	4976.358074	24.650522
149.318621	4985.578727	24.655539
149.092948	5005.871693	24.660557
149.036676	5010.956123	24.665575
149.542271	5017.223916	24.670592
149.653883	5040.196266	24.675610
150.110393	5033.369650	24.680627
150.244129	5047.461000	24.685645
150.236491	5058.931474	24.690663
150.362177	5061.813170	24.695680
150.661059	5068.375921	24.700698
150.917123	5083.144850	24.705715
150.892249	5087.469035	24.710733
150.911019	5097.118758	24.715751
151.128579	5091.385221	24.720768
150.992846	5115.843926	24.725786
151.248420	5117.805687	24.730803
151.206757	5127.856859	24.735821
151.757284	5147.366995	24.740839
152.234716	5148.275352	24.745856
151.871637	5151.305002	24.750874
152.419685	5164.720693	24.755891
152.426031	5173.484218	24.760909
152.318073	5182.959875	24.765927
152.513251	5192.662572	24.770944
152.648903	5207.549951	24.775962
152.881426	5213.642646	24.780979
153.104294	5214.653742	24.785997
153.392085	5226.942668	24.791015
153.436175	5230.261459	24.796032
153.428398	5254.264139	24.801050
153.684245	5236.108839	24.806067
153.961655	5243.184114	24.811085
154.197770	5258.622771	24.816103
154.653947	5257.255327	24.821120
154.555082	5266.503005	24.826138
155.039283	5264.563850	24.831155
154.794757	5264.129468	24.836173
155.015746	5255.673185	24.841191
155.304138	5254.738448	24.846208
155.329633	5292.391410	24.851226
155.325281	5292.724368	24.856243
155.366924	5284.967753	24.861261
155.183902	5296.064344	24.866279
155.796323	5293.278661	24.871296
155.909777	5314.700468	24.876314
156.059745	5315.295203	24.881331
156.495931	5309.729711	24.886349
156.242758	5322.392116	24.891367
156.586887	5328.179904	24.896384
156.486133	5343.984692	24.901402
156.620357	5338.866994	24.906419
156.981784	5359.103043	24.911437
156.812127	5377.049368	24.916455
157.275335	5385.985655	24.921472
157.499736	5403.167411	24.926490
157.611503	5408.667345	24.931507
157.788769	5411.025564	24.936525
158.207997	5415.146089	24.941543
158.305401	5401.754456	24.946560
158.585785	5420.355263	24.951578
159.017762	5417.485032	24.956595
159.283543	5422.486007	24.961613
159.135046	5421.919872	24.966631
159.512460	5417.945083	24.971648
159.329641	5418.868235	24.976666
159.540460	5413.513291	24.981683
159.636525	5412.006552	24.986701
159.805334	5412.397665	24.991719
159.960277	5415.317251	24.996736
159.928859	5430.786936	25.001754
160.292809	5439.822475	25.006771
160.205306	5440.473953	25.011789
160.017041	5450.880725	25.016807
160.364632	5453.902570	25.021824
160.311265	5481.682229	25.026842
160.501675	5476.451676	25.031859
160.349968	5490.603113	25.036877
160.760774	5512.426257	25.041895
160.996725	5517.044149	25.046912
161.209430	5533.475781	25.051930
161.354276	5544.304719	25.056947
161.548497	5535.764427	25.061965
161.820171	5563.879511	25.066983
161.829075	5571.232202	25.072000
162.424933	5566.484570	25.077018
162.351682	5567.716771	25.082035
162.720823	5583.682935	25.087053
163.088749	5591.636138	25.092071
163.412979	5595.568087	25.097088
163.114647	5594.085649	25.102106
163.502451	5595.330899	25.107123
163.474858	5587.755890	25.112141
163.291342	5598.351617	25.117159
163.673643	5604.238070	25.122176
163.377570	5616.581844	25.127194
163.454513	5629.267416	25.132211
164.195223	5628.063863	25.137229
164.010330	5648.137207	25.142247
164.288299	5656.865587	25.147264
164.240321	5665.391805	25.152282
164.557818	5677.065055	25.157299
165.090794	5678.901635	25.162317
164.806284	5698.362301	25.167335
165.077519	5709.904480	25.172352
165.283830	5712.623966	25.177370
165.487776	5722.624587	25.182387
165.617906	5729.884077	25.187405
165.470162	5745.415906	25.192423
166.176395	5747.184751	25.197440
166.075650	5777.749817	25.202458
166.151795	5784.256344	25.207475
166.467721	5782.300677	25.212493
166.715226	5795.303022	25.217511
166.826722	5793.835484	25.222528
166.835783	5807.112667	25.227546
167.245473	5824.498263	25.232563
167.529668	5832.428752	25.237581
167.298435	5833.995360	25.242599
167.621072	5840.357977	25.247616
168.089520	5857.432911	25.252634
168.293339	5865.169308	25.257651
168.544506	5864.004437	25.262669
168.564981	5868.611942	25.267687
168.648286	5885.218015	25.272704
168.625457	5886.439843	25.277722
168.997280	5893.442161	25.282739
169.206925	5902.209902	25.287757
169.433676	5918.328159	25.292775
169.699352	5916.128717	25.297792
169.876678	5920.885900	25.302810
169.860521	5915.695203	25.307827
170.294994	5893.081060	25.312845
170.682212	5908.800795	25.317863
170.406044	5915.603508	25.322880
170.590269	5912.372995	25.327898
170.718929	5909.546302	25.332915
170.889101	5907.895522	25.337933
170.989348	5907.458086	25.342951
171.177555	5911.749332	25.347968
171.277999	5927.032505	25.352986
171.143512	5940.950313	25.358003
171.152031	5942.728911	25.363021
171.182157	5968.447396	25.368039
171.411415	5967.219134	25.373056
171.657521	5982.355620	25.378074
171.805926	5998.901089	25.383091
172.060816	6008.123522	25.388109
171.969568	6029.222582	25.393127
172.429540	6038.218007	25.398144
172.719292	6053.765392	25.403162
172.691163	6066.713565	25.408179
172.853098	6071.384343	25.413197
172.947396	6091.054219	25.418215
173.184651	6102.356644	25.423232
173.584945	6115.526892	25.428250
173.538042	6124.884053	25.433267
174.082760	6137.327908	25.438285
173.964788	6159.487286	25.443303
174.375577	6156.761918	25.448320
174.633140	6171.798422	25.453338
174.677295	6187.352837	25.458355
174.947184	6191.110287	25.463373
174.986182	6194.762134	25.468391
175.197837	6217.751051	25.473408
175.795877	6224.577417	25.478426
175.775459	6233.234897	25.483443
175.939221	6243.769431	25.488461
175.941269	6251.656214	25.493479
176.176595	6254.799981	25.498496
176.440307	6264.223375	25.503514
176.439144	6285.601128	25.508531
176.632000	6280.395868	25.513549
177.135718	6289.674016	25.518567
176.946763	6303.554425	25.523584
177.146509	6319.948084	25.528602
177.320802	6323.154310	25.533619
177.647730	6337.840814	25.538637
177.666324	6357.624609	25.543655
177.827184	6356.540975	25.548672
177.957010	6354.423709	25.553690
177.764550	6382.237455	25.558707
178.106057	6392.086780	25.563725
178.681386	6406.235709	25.568743
178.707670	6415.600270	25.573760
178.710088	6417.998326	25.578778
178.983666	6445.752065	25.583795
179.464168	6445.859842	25.588813
179.565956	6464.046673	25.593831
179.551016	6469.331944	25.598848
180.366203	6472.487185	25.603866
179.969726	6480.407716	25.608883
180.610183	6488.307735	25.613901
180.877957	6496.521304	25.618919
181.011256	6506.397600	25.623936
181.076734	6497.040901	25.628954
181.305502	6490.421454	25.633971
181.596961	6486.161887	25.638989
181.637027	6488.200676	25.644007
182.133101	6465.960596	25.649024
182.148125	6472.672297	25.654042
182.254722	6486.040760	25.659059
182.283016	6509.612486	25.664077
182.488652	6510.933279	25.669095
182.800231	6516.858126	25.674112
182.900639	6512.495248	25.679130
182.611205	6515.946960	25.684148
182.829506	6526.422646	25.689165
183.010411	6546.732374	25.694183
183.403026	6548.172861	25.699200
183.486580	6555.792673	25.704218
183.395458	6577.924790	25.709236
183.455863	6581.186207	25.714253
183.617298	6594.029875	25.719271
184.012243	6609.195207	25.724288
184.219374	6611.952497	25.729306
184.145767	6628.493931	25.734324
184.522999	6632.299690	25.739341
184.616197	6651.186027	25.744359
184.914940	6674.102759	25.749376
185.312008	6671.270119	25.754394
185.026822	6700.316449	25.759412
185.434514	6703.568957	25.764429
185.635248	6724.647640	25.769447
185.497537	6740.966517	25.774464
185.790317	6751.971824	25.779482
185.807594	6765.128171	25.784500
186.476542	6773.034031	25.789517
186.705939	6786.424105	25.794535
186.812807	6793.226745	25.799552
187.460599	6807.317300	25.804570
187.460547	6825.782034	25.809588
187.628744	6827.156821	25.814605
187.980821	6833.354665	25.819623
188.066998	6849.327962	25.824640
188.340495	6855.053654	25.829658
188.134747	6863.547482	25.834676
188.684426	6872.266319	25.839693
188.705117	6877.786039	25.844711
189.009722	6889.371032	25.849728
189.468721	6883.913843	25.854746
189.668106	6898.421381	25.859764
189.563733	6913.513970	25.864781
190.082213	6921.452551	25.869799
189.876230	6917.974009	25.874816
190.342611	6917.357012	25.879834
189.921620	6926.639758	25.884852
190.432427	6933.881648	25.889869
190.754001	6935.783568	25.894887
190.729670	6946.669612	25.899904
190.785582	6939.492903	25.904922
191.108876	6957.273645	25.909940
191.010485	6964.533186	25.914957
191.470486	6973.589767	25.919975
191.392743	6985.301088	25.924992
191.827410	6998.239250	25.930010
191.933195	7005.458397	25.935028
192.112742	7010.594047	25.940045
192.353608	7023.875497	25.945063
192.366083	7041.845155	25.950080
192.780523	7048.464337	25.955098
192.596600	7069.475781	25.960116
192.838843	7078.206763	25.965133
192.771419	7085.374874	25.970151
193.411150	7093.239929	25.975168
193.817577	7107.075359	25.980186
193.519958	7120.427779	25.985204
194.043350	7125.877691	25.990221
194.243105	7147.230164	25.995239
194.292178	7155.346771	26.000256
194.537329	7163.374688	26.005274
194.832174	7178.677734	26.010292
194.951875	7185.765707	26.015309
195.068075	7201.855772	26.020327
195.189041	7214.420803	26.025344
195.555797	7218.128456	26.030362
195.349250	7245.067933	26.035380
195.933184	7253.691836	26.040397
196.457741	7258.625439	26.045415
196.227829	7270.436776	26.050432
196.485555	7274.205886	26.055450
196.644350	7291.076109	26.060468
196.934187	7299.186678	26.065485
197.171654	7313.934836	26.070503
197.110195	7331.780503	26.075520
197.681131	7325.603440	26.080538
197.776177	7345.403115	26.085556
197.885818	7368.970316	26.090573
198.206520	7357.432934	26.095591
198.223437	7387.159500	26.100608
198.852372	7389.240677	26.105626
199.059353	7395.960753	26.110644
199.153780	7406.841580	26.115661
199.551262	7420.701155	26.120679
199.550157	7430.903217	26.125696
199.933188	7423.527779	26.130714
199.774039	7441.495374	26.135732
200.123760	7446.385304	26.140749
200.218269	7448.516266	26.145767
200.320424	7462.478821	26.150784
200.316275	7472.363505	26.155802
200.221117	7488.271182	26.160820
200.462037	7507.657536	26.165837
200.940413	7519.735441	26.170855
201.121001	7524.546916	26.175872
201.170570	7543.007777	26.180890
201.539046	7562.621734	26.185908
201.897857	7588.252859	26.190925
202.411311	7589.093485	26.195943
202.190929	7604.938625	26.200960
202.382944	7603.529683	26.205978
202.642071	7618.753107	26.210996
202.621085	7627.033790	26.216013
203.025979	7634.610804	26.221031
202.996883	7655.181352	26.226048
203.359607	7665.030505	26.231066
203.570888	7681.268816	26.236084
203.886960	7676.766570	26.241101
204.451213	7690.621061	26.246119
204.439727	7700.530672	26.251136
205.013044	7694.492358	26.256154
204.947307	7696.630799	26.261172
204.951538	7712.304908	26.266189
205.034396	7716.072891	26.271207
205.057235	7734.365136	26.276224
205.526331	7740.811461	26.281242
205.687176	7753.361935	26.286260
205.609881	7769.314276	26.291277
205.911574	7782.909330	26.296295
206.301620	7808.069237	26.301312
206.861800	7819.482812	26.306330
206.984145	7822.582761	26.311348
206.689867	7838.224321	26.316365
207.404539	7850.966731	26.321383
207.092193	7875.495104	26.326400
207.416809	7880.245181	26.331418
207.917266	7895.882094	26.336436
207.456747	7914.437307	26.341453
208.116868	7930.960807	26.346471
208.565443	7943.866892	26.351488
208.580068	7958.583536	26.356506
208.785874	7969.572923	26.361524
208.876418	7987.580456	26.366541
209.304701	7991.795485	26.371559
209.830294	8002.636352	26.376576
209.596567	8006.638213	26.381594
210.127551	8017.940529	26.386612
210.101049	8025.951229	26.391629
210.484945	8032.100834	26.396647
210.799557	8054.487587	26.401664
211.059931	8061.684967	26.406682
211.229370	8067.387977	26.411700
211.316656	8071.848203	26.416717
211.699065	8079.024173	26.421735
211.650568	8087.082477	26.426752
211.757236	8083.128510	26.431770
212.038464	8101.870650	26.436788
212.048796	8113.233992	26.441805
212.615563	8108.542937	26.446823
212.524953	8131.107313	26.451840
212.525081	8150.535638	26.456858
212.937995	8139.845792	26.461876
213.032783	8167.451829	26.466893
213.264101	8184.169469	26.471911
213.277819	8185.472219	26.476928
213.487394	8201.854584	26.481946
213.582255	8223.189120	26.486964
213.853444	8248.520194	26.491981
214.538522	8249.466101	26.496999
214.331561	8274.526800	26.502016
214.576209	8287.074989	26.507034
215.003331	8309.100314	26.512052
215.304861	8318.047633	26.517069
215.705534	8320.987649	26.522087
215.788208	8342.302264	26.527104
215.717902	8346.424533	26.532122
216.093680	8369.831678	26.537140
216.161385	8389.173999	26.542157
216.584260	8395.457219	26.547175
216.776792	8411.787447	26.552192
216.927808	8424.462023	26.557210
217.061111	8438.090810	26.562228
217.317097	8443.328090	26.567245
217.577714	8456.340515	26.572263
217.840350	8471.225878	26.577280
218.221541	8488.905975	26.582298
218.248900	8539.798444	26.587316
218.788336	8558.072704	26.592333
218.953061	8580.794183	26.597351
219.587627	8583.127243	26.602368
219.522150	8604.581128	26.607386
219.725286	8593.759931	26.612404
220.026244	8612.218636	26.617421
220.875269	8613.797880	26.622439
220.777594	8618.708753	26.627456
220.911051	8623.482062	26.632474
221.382972	8617.108579	26.637492
221.691325	8616.971555	26.642509
221.603229	8612.299342	26.647527
221.421245	8619.222826	26.652544
221.368681	8632.204662	26.657562
221.837205	8633.445192	26.662580
221.545981	8654.270967	26.667597
222.055399	8661.347104	26.672615
221.791109	8682.039176	26.677632
222.256822	8699.867371	26.682650
222.419353	8712.362904	26.687668
222.408655	8743.265546	26.692685
223.017223	8759.128511	26.697703
223.154403	8766.893964	26.702720
222.985956	8791.515002	26.707738
223.555112	8814.094862	26.712756
223.325560	8822.209567	26.717773
224.024907	8842.906838	26.722791
224.229732	8860.968425	26.727808
224.773282	8881.676023	26.732826
224.875935	8888.752573	26.737844
224.650008	8903.083539	26.742861
224.968840	8916.049314	26.747879
225.058129	8943.992500	26.752896
225.564360	8955.301837	26.757914
225.778839	8971.683084	26.762932
226.090529	8983.764355	26.767949
226.538590	8985.219471	26.772967
227.154930	9008.443692	26.777984
227.016442	9015.401347	26.783002
227.669360	9013.408485	26.788020
227.624160	9026.941135	26.793037
227.722280	9039.658502	26.798055
227.989447	9039.081843	26.803072
228.162939	9067.646903	26.808090
228.537727	9064.876400	26.813108
228.606181	9071.385590	26.818125
228.906758	9087.371966	26.823143
229.183454	9096.399258	26.828160
229.465047	9104.787167	26.833178
229.884953	9116.867824	26.838196
230.020169	9134.400990	26.843213
230.279583	9139.415262	26.848231
230.514148	9132.155124	26.853248
230.169331	9150.330633	26.858266
230.543996	9153.918295	26.863284
230.683494	9174.208691	26.868301
231.252521	9187.175747	26.873319
231.415113	9197.130608	26.878336
231.377438	9221.448598	26.883354
231.984324	9220.818969	26.888372
232.123643	9239.534788	26.893389
232.285684	9260.806189	26.898407
232.363881	9258.719569	26.903424
232.400707	9279.870482	26.908442
232.578758	9287.978707	26.913460
232.908790	9306.194794	26.918477
233.061242	9332.750280	26.923495
233.562620	9347.147538	26.928512
234.000761	9352.576850	26.933530
234.471630	9355.881662	26.938548
234.200192	9381.203948	26.943565
234.508082	9384.899499	26.948583
234.850416	9396.810958	26.953600
234.989128	9416.451383	26.958618
235.314768	9419.760076	26.963636
235.718070	9454.562529	26.968653
235.822303	9450.630627	26.973671
236.022050	9463.472629	26.978688
236.086039	9484.767844	26.983706
236.174000	9479.602596	26.988724
236.572328	9501.605939	26.993741
236.697243	9513.183448	26.998759
236.875113	9522.808319	27.003776
236.839737	9547.957116	27.008794
237.116873	9556.960220	27.013812
237.470474	9582.631406	27.018829
237.744946	9596.905708	27.023847
237.596153	9615.146151	27.028864
237.819010	9633.042498	27.033882
238.305454	9652.836359	27.038900
238.752983	9675.502618	27.043917
238.836394	9692.644121	27.048935
239.133255	9710.601955	27.053952
239.058200	9724.367034	27.058970
239.295669	9741.702819	27.063988
239.668566	9765.885817	27.069005
240.039299	9781.021256	27.074023
240.484161	9802.807500	27.079040
240.484072	9825.650783	27.084058
241.062346	9830.838367	27.089076
241.030842	9858.131993	27.094093
241.246324	9865.021425	27.099111
241.679196	9885.255794	27.104128
241.814620	9899.412460	27.109146
242.106945	9926.718345	27.114164
242.339479	9934.280330	27.119181
242.662256	9957.364722	27.124199
243.367970	9968.576930	27.129216
243.246393	9983.790643	27.134234
244.043239	9990.075933	27.139252
244.377407	9992.825417	27.144269
244.310160	10011.400406	27.149287
244.631663	10013.000146	27.154304
244.663899	10017.688511	27.159322
245.026952	10025.990371	27.164340
244.980839	10047.679720	27.169357
245.049560	10059.963492	27.174375
245.643486	10077.218458	27.179392
245.408555	10098.975356	27.184410
246.171212	10109.617466	27.189428
246.297389	10114.367621	27.194445
246.370116	10138.458579	27.199463
246.588144	10146.437733	27.204480
246.869718	10174.022019	27.209498
247.144517	10185.367602	27.214516
247.161568	10202.586764	27.219533
247.319684	10216.273811	27.224551
247.809862	10224.301712	27.229568
247.862341	10261.813369	27.234586
248.339558	10275.920639	27.239604
248.636893	10290.111681	27.244621
248.706177	10313.259057	27.249639
249.096365	10328.547383	27.254656
249.172273	10349.671139	27.259674
249.481712	10357.238395	27.264692
249.263402	10375.992950	27.269709
249.620453	10404.505126	27.274727
250.107425	10408.157439	27.279744
250.197287	10435.880973	27.284762
250.637991	10443.679985	27.289780
250.943492	10459.685141	27.294797
250.698130	10475.039096	27.299815
251.045481	10496.677794	27.304832
251.390829	10513.340508	27.309850
251.847142	10536.331314	27.314868
252.106014	10558.262414	27.319885
252.277793	10570.985864	27.324903
252.969297	10581.000981	27.329920
252.871836	10609.594443	27.334938
253.142834	10618.089564	27.339956
253.427167	10643.367495	27.344973
253.646550	10661.024395	27.349991
254.185854	10671.097672	27.355008
254.281618	10695.431794	27.360026
254.716287	10706.847917	27.365044
254.697553	10723.422894	27.370061
254.817736	10750.213475	27.375079
255.302921	10753.521439	27.380096
255.448335	10764.894376	27.385114
255.559334	10782.176355	27.390132
255.803281	10798.992097	27.395149
256.259161	10825.130376	27.400167
256.635692	10833.404958	27.405184
256.467658	10865.355453	27.410202
256.638507	10874.565571	27.415220
257.210589	10901.574425	27.420237
257.079773	10930.150983	27.425255
257.465112	10936.798582	27.430272
257.726879	10966.691543	27.435290
257.767933	10989.467065	27.440308
258.222411	11011.574643	27.445325
258.349312	11044.221877	27.450343
258.651790	11066.685894	27.455360
258.768052	11094.493790	27.460378
259.420078	11105.811038	27.465396
259.984165	11129.541537	27.470413
259.994813	11145.985578	27.475431
260.878329	11159.206850	27.480448
260.951552	11178.864336	27.485466
260.905612	11184.874789	27.490484
261.569200	11199.651738	27.495501
261.810412	11209.533226	27.500519
262.374220	11231.235290	27.505536
262.467716	11240.522498	27.510554
262.794567	11237.787584	27.515572
262.932629	11256.614330	27.520589
263.104235	11280.103613	27.525607
263.377641	11285.598847	27.530624
263.483148	11300.115577	27.535642
263.584660	11304.041263	27.540660
264.015183	11317.471620	27.545677
263.973914	11337.980468	27.550695
264.404106	11338.350956	27.555712
264.891869	11357.535699	27.560730
264.771390	11371.673926	27.565748
264.967779	11387.827323	27.570765
264.834430	11407.900935	27.575783
265.309655	11422.657751	27.580800
265.935538	11445.276216	27.585818
265.900999	11467.303015	27.590836
266.290020	11484.440743	27.595853
266.905049	11499.466964	27.600871
267.136322	11512.092590	27.605888
267.368844	11528.991444	27.610906
267.593779	11545.672523	27.615924
267.671253	11553.964467	27.620941
267.376651	11583.458932	27.625959
267.906370	11593.963709	27.630976
268.344557	11613.068525	27.635994
268.767528	11632.417423	27.641012
269.349779	11645.335707	27.646029
269.699173	11668.275425	27.651047
270.071600	11664.332678	27.656064
270.393063	11681.504813	27.661082
270.978051	11696.453572	27.666100
271.341421	11687.742348	27.671117
271.215803	11702.259894	27.676135
271.142299	11719.202614	27.681152
271.811833	11731.832567	27.686170
271.592529	11739.092816	27.691188
271.898092	11757.548354	27.696205
272.063191	11769.338035	27.701223
272.125377	11798.946857	27.706240
272.405497	11815.878784	27.711258
272.822682	11837.233189	27.716276
273.221053	11848.252188	27.721293
272.943308	11867.603651	27.726311
273.643906	11885.589465	27.731328
274.057230	11907.867057	27.736346
273.917657	11929.960064	27.741364
274.386689	11951.069845	27.746381
274.473750	11973.204918	27.751399
274.981044	11996.151060	27.756416
274.892693	12015.855649	27.761434
275.115089	12038.254572	27.766452
275.856747	12060.020003	27.771469
275.749439	12089.332510	27.776487
276.341581	12111.361516	27.781504
276.367862	12125.703741	27.786522
276.823129	12154.119150	27.791540
276.890763	12168.696271	27.796557
277.451329	12192.331795	27.801575
277.704532	12221.086503	27.806592
278.086626	12223.496017	27.811610
278.146410	12250.585777	27.816628
278.481132	12259.414851	27.821645
278.813885	12286.026688	27.826663
279.193752	12304.763465	27.831680
279.523881	12307.608480	27.836698
279.329071	12326.446900	27.841716
280.270668	12354.226135	27.846733
280.244134	12371.519053	27.851751
280.529899	12381.775370	27.856768
280.847934	12394.933773	27.861786
280.696611	12413.856283	27.866804
281.418248	12424.695297	27.871821
281.417930	12456.527758	27.876839
281.504747	12467.323924	27.881856
282.118986	12481.193986	27.886874
282.369396	12508.029889	27.891892
282.625471	12522.582632	27.896909
282.860774	12543.946553	27.901927
283.381536	12558.870785	27.906944
283.436265	12583.758776	27.911962
283.404106	12605.873821	27.916980
284.005353	12624.644195	27.921997
284.313494	12651.573479	27.927015
284.515264	12678.119899	27.932032
284.860688	12699.124873	27.937050
285.077289	12726.632465	27.942068
285.413195	12744.177590	27.947085
285.708827	12772.183916	27.952103
285.719899	12787.993856	27.957120
285.786198	12809.535228	27.962138
286.129106	12846.689778	27.967156
286.696930	12866.174008	27.972173
287.097219	12903.951433	27.977191
287.283799	12928.238455	27.982208
287.775929	12939.093555	27.987226
287.983673	12960.912700	27.992244
288.550223	12974.941062	27.997261
288.816004	13005.639210	28.002279
289.229194	13013.399078	28.007296
289.596463	13037.706284	28.012314
289.458205	13049.769541	28.017332
289.939365	13061.224024	28.022349
290.248513	13079.868927	28.027367
290.429644	13108.719744	28.032384
291.049718	13124.913150	28.037402
291.008750	13143.108963	28.042420
291.269481	13165.434660	28.047437
291.758475	13200.179933	28.052455
292.010228	13210.828628	28.057472
292.625096	13220.123799	28.062490
292.435754	13245.448788	28.067508
293.381706	13256.910823	28.072525
293.335803	13269.016113	28.077543
293.491321	13292.899365	28.082560
294.189431	13307.429158	28.087578
294.257562	13315.719813	28.092596
294.527389	13319.340741	28.097613
294.425513	13346.571070	28.102631
294.996428	13349.713249	28.107648
295.114449	13369.362690	28.112666
295.128150	13397.224499	28.117684
295.468183	13403.626353	28.122701
295.802590	13427.186785	28.127719
295.904382	13458.477069	28.132736
296.318900	13469.191813	28.137754
296.561580	13503.468514	28.142772
296.849155	13523.989893	28.147789
297.153475	13547.508271	28.152807
297.077098	13568.169179	28.157824
297.920092	13595.077483	28.162842
297.734487	13625.831492	28.167860
298.379867	13643.205341	28.172877
298.862723	13670.643475	28.177895
298.768224	13696.558063	28.182912
299.411784	13712.381232	28.187930
299.835109	13735.671348	28.192948
300.133767	13756.679823	28.197965
300.296462	13772.785825	28.202983
300.767850	13806.510759	28.208000
301.003240	13826.561953	28.213018
301.263561	13848.924337	28.218036
301.796980	13860.822356	28.223053
302.194932	13873.849161	28.228071
302.418817	13899.002126	28.233088
303.085961	13910.571869	28.238106
303.232571	13936.254889	28.243124
303.244736	13952.880118	28.248141
303.548805	13968.785007	28.253159
303.975454	13991.377624	28.258176
304.200275	14016.351741	28.263194
304.205462	14039.849566	28.268212
304.632503	14050.133207	28.273229
305.097023	14062.220075	28.278247
305.197013	14085.770366	28.283264
305.549823	14110.473788	28.288282
305.760590	14137.010783	28.293300
306.155620	14148.934328	28.298317
306.409242	14168.512512	28.303335
306.468344	14203.445966	28.308352
306.783046	14225.455830	28.313370
307.099865	14250.425313	28.318388
307.493289	14275.889695	28.323405
307.695523	14299.942798	28.328423
307.820857	14332.584835	28.333440
308.430606	14362.702678	28.338458
308.432365	14396.330658	28.343476
309.020594	14418.354975	28.348493
309.154893	14444.200320	28.353511
309.546640	14458.646404	28.358528
310.019633	14496.778309	28.363546
310.149850	14520.176157	28.368564
310.520422	14541.424196	28.373581
310.901049	14566.558005	28.378599
310.712969	14594.869605	28.383616
311.394054	14608.202437	28.388634
311.529819	14639.231409	28.393652
311.991838	14660.697669	28.398669
312.519205	14676.900025	28.403687
312.314745	14706.590726	28.408704
313.125640	14723.698542	28.413722
313.221687	14751.384962	28.418740
313.953708	14765.272888	28.423757
314.895923	14774.619690	28.428775
314.911026	14787.413755	28.433792
315.105002	14799.328614	28.438810
316.075771	14817.233729	28.443828
315.969491	14816.578224	28.448845
316.398067	14838.164606	28.453863
316.463105	14853.630057	28.458880
317.199151	14862.679222	28.463898
317.352936	14889.238408	28.468916
317.477386	14892.397542	28.473933
317.868160	14902.806611	28.478951
317.884870	14924.269411	28.483968
318.355938	14935.142976	28.488986
318.626393	14944.059628	28.494004
318.926856	14968.569494	28.499021
319.081452	14986.500944	28.504039
319.043572	15014.194122	28.509056
319.426114	15033.999674	28.514074
319.578653	15053.816118	28.519092
319.541223	15085.144503	28.524109
320.278501	15117.644942	28.529127
320.391770	15145.151603	28.534144
320.713053	15167.111781	28.539162
321.012973	15189.986454	28.544180
321.466102	15228.676200	28.549197
321.877470	15250.459179	28.554215
322.092008	15274.412064	28.559232
322.290840	15299.956588	28.564250
322.641968	15330.984427	28.569268
322.789918	15367.628129	28.574285
323.357752	15399.683801	28.579303
323.440945	15432.057671	28.584320
324.022664	15452.949858	28.589338
324.245745	15478.150318	28.594356
324.774198	15520.541594	28.599373
325.147290	15540.504301	28.604391
325.185114	15578.090416	28.609408
325.710754	15603.777042	28.614426
326.174313	15629.158887	28.619444
326.199294	15663.381418	28.624461
326.979165	15681.984406	28.629479
327.141372	15720.475324	28.634496
327.379197	15741.232767	28.639514
327.569392	15753.355338	28.644532
328.082950	15777.625679	28.649549
328.356955	15802.782537	28.654567
328.467263	15834.789595	28.659584
328.739973	15852.658555	28.664602
329.320997	15877.725480	28.669620
329.424154	15903.296681	28.674637
330.191182	15925.352349	28.679655
329.821688	15955.856196	28.684672
330.017164	15980.955001	28.689690
330.597350	16008.535342	28.694708
330.900221	16040.545407	28.699725
331.158572	16072.159532	28.704743
331.877310	16098.928683	28.709760
332.500018	16110.824765	28.714778
332.814123	16148.027931	28.719796
333.573904	16163.822235	28.724813
334.014611	16164.037673	28.729831
334.409138	16190.428377	28.734848
334.823982	16195.907387	28.739866
335.032358	16216.277293	28.744884
335.489451	16232.385223	28.749901
335.794803	16252.019528	28.754919
335.770895	16266.558841	28.759936
336.073153	16280.396463	28.764954
336.655134	16294.811116	28.769972
336.513929	16322.989395	28.774989
336.934639	16339.329392	28.780007
337.397850	16362.217089	28.785024
337.573838	16380.466210	28.790042
337.918736	16409.280113	28.795060
338.115384	16441.875598	28.800077
338.338148	16460.195502	28.805095
338.356460	16489.723931	28.810112
339.001051	16522.796391	28.815130
339.295194	16551.407839	28.820148
339.133601	16580.864131	28.825165
339.645094	16612.653971	28.830183
340.379723	16655.514689	28.835200
340.182212	16690.038898	28.840218
340.547974	16718.713451	28.845236
340.727425	16747.145322	28.850253
341.373934	16789.667724	28.855271
341.927478	16829.317072	28.860288
342.084973	16862.642268	28.865306
342.653067	16875.933772	28.870324
342.793424	16920.421699	28.875341
343.203213	16941.620847	28.880359
343.754097	16974.209827	28.885376
343.798086	17003.701878	28.890394
344.684620	17029.272754	28.895412
344.803055	17052.694138	28.900429
345.477926	17073.867962	28.905447
345.561902	17108.784842	28.910464
346.206787	17132.831878	28.915482
346.764135	17144.541944	28.920500
347.076975	17173.231480	28.925517
347.297531	17181.965463	28.930535
347.348819	17209.655058	28.935552
347.577068	17226.474869	28.940570
347.998165	17252.158068	28.945588
348.333087	17277.622767	28.950605
348.917663	17282.640300	28.955623
349.127777	17318.304845	28.960640
349.306281	17343.257981	28.965658
349.797267	17361.147451	28.970676
349.595246	17393.848026	28.975693
350.012990	17429.556907	28.980711
350.230861	17448.536417	28.985728
350.712018	17481.941292	28.990746
351.075463	17506.770739	28.995764
351.318486	17536.381889	29.000781
351.698578	17574.240355	29.005799
351.759437	17605.940457	29.010816
352.097043	17647.097534	29.015834
352.759429	17671.823711	29.020852
353.247443	17713.362898	29.025869
353.575378	17738.332229	29.030887
354.022470	17778.332854	29.035904
354.054965	17810.441825	29.040922
354.801972	17836.531937	29.045940
355.369497	17874.831743	29.050957
355.972808	17898.401163	29.055975
356.204167	17929.659799	29.060992
356.386692	17946.067991	29.066010
356.815265	17971.573632	29.071028
357.198964	18005.843591	29.076045
357.781853	18023.968006	29.081063
358.306220	18048.708114	29.086080
358.347258	18082.067081	29.091098
358.688025	18095.017114	29.096116
358.657030	18129.547121	29.101133
359.506837	18155.396192	29.106151
359.610221	18188.688367	29.111168
359.881587	18216.103347	29.116186
360.467438	18236.544117	29.121204
360.555251	18275.537496	29.126221
360.908169	18310.808722	29.131239
361.290422	18337.418828	29.136256
361.133756	18366.158601	29.141274
361.729855	18398.228988	29.146292
362.224126	18440.830966	29.151309
362.657220	18471.240412	29.156327
363.261887	18499.594949	29.161344
363.704850	18537.269359	29.166362
364.536843	18563.013678	29.171380
364.810665	18579.936360	29.176397
364.841529	18599.098652	29.181415
365.481577	18618.285174	29.186432
365.572592	18643.179529	29.191450
365.926519	18654.114848	29.196468
366.381878	18682.276962	29.201485
366.953630	18693.275641	29.206503
366.750749	18705.648201	29.211520
367.165705	18738.883641	29.216538
368.026838	18754.447128	29.221556
368.258574	18773.446915	29.226573
368.564782	18799.312406	29.231591
368.668751	18816.923468	29.236608
369.194853	18849.593374	29.241626
369.572523	18866.527384	29.246644
369.881618	18898.511845	29.251661
370.277363	18925.083797	29.256679
370.770556	18949.008601	29.261696
370.770439	18978.711630	29.266714
371.279975	18997.622546	29.271732
371.582400	19029.847725	29.276749
372.064303	19062.249116	29.281767
372.378186	19088.224501	29.286784
372.624836	19119.811067	29.291802
372.729243	19141.083728	29.296820
373.180364	19175.703816	29.301837
373.655539	19208.436136	29.306855
374.199667	19238.509285	29.311872
374.040011	19269.908504	29.316890
374.501996	19295.480291	29.321908
375.042078	19330.454691	29.326925
375.425109	19368.910808	29.331943
375.740425	19396.429533	29.336960
376.010195	19447.298362	29.341978
376.433156	19478.941429	29.346996
376.822776	19514.208349	29.352013
377.505527	19533.577014	29.357031
378.425657	19565.991925	29.362048
378.463920	19607.273138	29.367066
379.149397	19621.906720	29.372084
379.614364	19644.840918	29.377101
379.831774	19676.942379	29.382119
379.939189	19696.752160	29.387136
380.479292	19724.326605	29.392154
380.854682	19758.958476	29.397172
381.037925	19780.506881	29.402189
381.360215	19798.715050	29.407207
382.043945	19828.979327	29.412224
382.476449	19851.131897	29.417242
382.767832	19882.853052	29.422260
382.908499	19905.972781	29.427277
382.996207	19949.474857	29.432295
383.582480	19976.846305	29.437312
383.873154	20010.879157	29.442330
384.575863	20036.473657	29.447348
384.800910	20068.742049	29.452365
384.932954	20106.164226	29.457383
385.410895	20132.923591	29.462400
385.684117	20169.339430	29.467418
386.183005	20200.773408	29.472436
386.505063	20225.525187	29.477453
386.768934	20253.280420	29.482471
387.354476	20283.019407	29.487488
387.335219	20324.447122	29.492506
387.921573	20359.748393	29.497524
388.127920	20388.887259	29.502541
387.950272	20424.693130	29.507559
388.810700	20454.497328	29.512576
388.914545	20514.288431	29.517594
389.400909	20549.291046	29.522612
389.759913	20584.108483	29.527629
389.970564	20636.353414	29.532647
390.756398	20677.374220	29.537664
390.649859	20722.686859	29.542682
391.268435	20762.264193	29.547700
391.957075	20804.920007	29.552717
392.675148	20854.207918	29.557735
392.584392	20880.541739	29.562752
393.129883	20925.339195	29.567770
393.622645	20958.078277	29.572788
394.056288	20992.145213	29.577805
394.513186	21032.944495	29.582823
394.860121	21063.854695	29.587840
395.308024	21101.625062	29.592858
395.891340	21126.775311	29.597876
396.180748	21164.007971	29.602893
396.419607	21213.029973	29.607911
397.167625	21247.843609	29.612928
397.533227	21285.043152	29.617946
397.915022	21313.137451	29.622964
399.026375	21331.301633	29.627981
399.375761	21362.219904	29.632999
400.127358	21376.209030	29.638016
400.245771	21399.134850	29.643034
400.692015	21427.721560	29.648052
401.102688	21446.020340	29.653069
401.215032	21476.292193	29.658087
401.565268	21492.971942	29.663104
402.071958	21528.112901	29.668122
402.264447	21547.427885	29.673140
402.907700	21581.179962	29.678157
402.892670	21608.181043	29.683175
403.338972	21633.609898	29.688192
403.497855	21678.541970	29.693210
404.145861	21699.547199	29.698228
404.375994	21740.831793	29.703245
404.676649	21785.124110	29.708263
404.945236	21808.880354	29.713280
405.707501	21840.701745	29.718298
406.155772	21873.653807	29.723316
406.976124	21904.500477	29.728333
407.236370	21937.815783	29.733351
407.855241	21961.024990	29.738368
408.305801	21995.458425	29.743386
408.541583	22004.124952	29.748404
408.681903	22029.051865	29.753421
408.889013	22063.263534	29.758439
409.552570	22073.710470	29.763456
409.960091	22106.704954	29.768474
409.941294	22143.735414	29.773492
410.292375	22174.602237	29.778509
410.344482	22207.895349	29.783527
410.713089	22244.305121	29.788544
411.240176	22275.137802	29.793562
411.683549	22319.246630	29.798580
412.299915	22362.949176	29.803597
412.473486	22399.225762	29.808615
412.981689	22433.376087	29.813632
413.525339	22469.373343	29.818650
414.140738	22496.655146	29.823668
414.480745	22533.209550	29.828685
414.709069	22574.798271	29.833703
415.159629	22601.245630	29.838720
415.524887	22639.666104	29.843738
415.560475	22685.030245	29.848756
416.440400	22710.887184	29.853773
416.975448	22751.916328	29.858791
417.940601	22773.340329	29.863808
418.337434	22800.350294	29.868826
418.671114	22832.312061	29.873844
419.286493	22868.303525	29.878861
419.602668	22902.102655	29.883879
419.578739	22920.985142	29.888896
420.259981	22968.298283	29.893914
420.555073	22995.773752	29.898932
421.037723	23029.804986	29.903949
421.043073	23063.582298	29.908967
421.347903	23106.552018	29.913984
421.972712	23149.263725	29.919002
422.217779	23187.729090	29.924020
422.579075	23224.777138	29.929037
423.210375	23270.626201	29.934055
423.258477	23308.146525	29.939072
423.179659	23352.170488	29.944090
423.661947	23400.345242	29.949108
424.149697	23438.396046	29.954125
424.154430	23497.183925	29.959143
425.101565	23552.163111	29.964160
425.760464	23600.660857	29.969178
425.916098	23648.097561	29.974196
426.321543	23691.112696	29.979213
426.858429	23746.090164	29.984231
427.472535	23804.444972	29.989248
427.885099	23854.583329	29.994266
428.206415	23891.120991	29.999284
429.040738	23938.674154	30.004301
429.170177	23990.003356	30.009319
429.842972	24023.653537	30.014336
430.165245	24066.775097	30.019354
430.213561	24110.150732	30.024372
431.088159	24142.383436	30.029389
431.253293	24182.845820	30.034407
432.117718	24219.391458	30.039424
432.448405	24262.120711	30.044442
432.911691	24296.547661	30.049460
433.938120	24321.618233	30.054477
433.732125	24370.659411	30.059495
434.320916	24399.517085	30.064512
434.782999	24428.988152	30.069530
435.211912	24468.590794	30.074548
435.651004	24498.330329	30.079565
435.855071	24542.782786	30.084583
436.670767	24584.684147	30.089600
437.096086	24618.012650	30.094618
437.549100	24648.276453	30.099636
438.127384	24675.177200	30.104653
438.318312	24714.233072	30.109671
438.824372	24749.322977	30.114688
439.657643	24772.032660	30.119706
439.510428	24822.137187	30.124724
440.017528	24857.511540	30.129741
440.642050	24890.926255	30.134759
440.891626	24926.322876	30.139776
441.596826	24962.829415	30.144794
441.635920	24999.815537	30.149812
442.291645	25038.439734	30.154829
442.738158	25077.347857	30.159847
442.938633	25122.939231	30.164864
443.644644	25159.469723	30.169882
443.577035	25203.784530	30.174900
444.512567	25246.320022	30.179917
444.819015	25288.165702	30.184935
445.152086	25326.719887	30.189952
445.292691	25367.953312	30.194970
445.769316	25414.965997	30.199988
446.394686	25459.487022	30.205005
446.707513	25517.607754	30.210023
447.082326	25553.427756	30.215040
448.091723	25602.008889	30.220058
448.195497	25644.104422	30.225076
448.779803	25685.419240	30.230093
449.067294	25739.952502	30.235111
449.780924	25785.366333	30.240128
450.008868	25825.785836	30.245146
450.166192	25878.741868	30.250164
450.945073	25913.591556	30.255181
451.072881	25962.495402	30.260199
451.556190	26016.086136	30.265216
452.318592	26049.983140	30.270234
453.164267	26096.020454	30.275252
453.641690	26128.904205	30.280269
453.964473	26173.204404	30.285287
454.529498	26211.667832	30.290304
455.030095	26248.346185	30.295322
454.981204	26287.140775	30.300340
455.607990	26322.796306	30.305357
456.407421	26354.961159	30.310375
456.293624	26401.335741	30.315392
456.966410	26440.162282	30.320410
457.283597	26477.518751	30.325428
457.611951	26513.392412	30.330445
457.826760	26555.214233	30.335463
458.380614	26601.985681	30.340480
458.663267	26640.424207	30.345498
459.229154	26702.930238	30.350516
459.862509	26737.310134	30.355533
460.083916	26783.342496	30.360551
460.606761	26833.890952	30.365568
461.082656	26885.189195	30.370586
461.386994	26934.621728	30.375604
461.911543	26980.127353	30.380621
462.433340	27029.806015	30.385639
462.881664	27078.432928	30.390656
463.325444	27129.622825	30.395674
463.836105	27178.277926	30.400692
464.283167	27227.589352	30.405709
464.566648	27275.291375	30.410727
464.944093	27328.821398	30.415744
465.597171	27380.908438	30.420762
465.956751	27433.724692	30.425780
466.677512	27479.597559	30.430797
467.130170	27536.501001	30.435815
467.507311	27586.180778	30.440832
468.482370	27630.850660	30.445850
468.651086	27684.497046	30.450868
469.290562	27727.583423	30.455885
469.603537	27771.990421	30.460903
470.087381	27823.648866	30.465920
470.611161	27863.585133	30.470938
471.200135	27915.279127	30.475956
471.863328	27962.590203	30.480973
472.149352	28012.025793	30.485991
472.861296	28058.963800	30.491008
473.228107	28104.562323	30.496026
473.342344	28161.721992	30.501044
473.841346	28204.022042	30.506061
474.333581	28246.082178	30.511079
474.781090	28305.274086	30.516096
475.222949	28356.356283	30.521114
475.652577	28406.829164	30.526132
476.367905	28452.992460	30.531149
477.180715	28510.787465	30.536167
477.529878	28541.153137	30.541184
478.893364	28568.643686	30.546202
479.419033	28610.715202	30.551220
479.741030	28648.904822	30.556237
480.369253	28676.397626	30.561255
480.487919	28710.803030	30.566272
480.838173	28742.000964	30.571290
481.206623	28771.568180	30.576308
481.432085	28800.404955	30.581325
481.989488	28847.521145	30.586343
482.009460	28882.015120	30.591360
482.743580	28923.230056	30.596378
483.245082	28971.064658	30.601396
483.479651	29008.958597	30.606413
483.918472	29056.664754	30.611431
483.849793	29106.907147	30.616448
484.948907	29143.521167	30.621466
485.501663	29198.321683	30.626484
485.796613	29241.695464	30.631501
486.315274	29288.872684	30.636519
486.614382	29338.920107	30.641536
487.183642	29382.312034	30.646554
487.526272	29444.235397	30.651572
488.144220	29497.857189	30.656589
488.751327	29529.617734	30.661607
489.472471	29584.376969	30.666624
490.094649	29623.575378	30.671642
490.613901	29673.590341	30.676660
491.049768	29707.282270	30.681677
491.602480	29744.898733	30.686695
491.585032	29803.979452	30.691712
492.335989	29838.915343	30.696730
493.034641	29898.140810	30.701748
493.100953	29951.984336	30.706765
494.301961	29989.359422	30.711783
494.353474	30042.773782	30.716800
494.788306	30083.613805	30.721818
495.092318	30143.557055	30.726836
495.206572	30187.143367	30.731853
496.150702	30247.505132	30.736871
496.585691	30302.321806	30.741888
496.875350	30352.520408	30.746906
497.203660	30415.187311	30.751924
497.880624	30471.493190	30.756941
498.322379	30520.391490	30.761959
498.787714	30580.507651	30.766976
499.644558	30628.014705	30.771994
499.847355	30698.658605	30.777012
500.235832	30759.734876	30.782029
501.007725	30805.028991	30.787047
501.395464	30866.611697	30.792064
502.037440	30921.611823	30.797082
502.216049	30977.027943	30.802100
502.717665	31036.548963	30.807117
503.593518	31075.680507	30.812135
503.970200	31142.293757	30.817152
504.444157	31197.408253	30.822170
505.015816	31253.970006	30.827188
505.521522	31304.225373	30.832205
506.438881	31352.766706	30.837223
507.167231	31402.944360	30.842240
507.648210	31449.292158	30.847258
508.627540	31478.702362	30.852276
508.842069	31516.772368	30.857293
509.519557	31559.410471	30.862311
509.877456	31595.831247	30.867328
510.461732	31625.901992	30.872346
510.706106	31667.554911	30.877364
511.269985	31697.034825	30.882381
511.892908	31730.329152	30.887399
511.917870	31785.077377	30.892416
512.428250	31833.234165	30.897434
512.719253	31880.839695	30.902452
513.537300	31922.417656	30.907469
514.035875	31965.616479	30.912487
514.059448	32021.235761	30.917504
514.684641	32070.880217	30.922522
515.243509	32128.362783	30.927540
515.661443	32184.419462	30.932557
516.179418	32218.005750	30.937575
516.431533	32289.953720	30.942592
516.906643	32340.308543	30.947610
517.514830	32401.534028	30.952628
517.812523	32467.440152	30.957645
518.461035	32524.405426	30.962663
518.768547	32583.468012	30.967680
519.039390	32649.905603	30.972698
520.222758	32713.769127	30.977716
520.784165	32774.856854	30.982733
521.185465	32825.877482	30.987751
521.731893	32889.283549	30.992768
522.390984	32942.607396	30.997786
523.538142	32987.250351	31.002804
523.800821	33045.691214	31.007821
524.612996	33095.041004	31.012839
525.205016	33149.315668	31.017856
525.738294	33199.931815	31.022874
526.523648	33241.753179	31.027892
526.926461	33286.802373	31.032909
527.499521	33326.577035	31.037927
527.850483	33373.589349	31.042944
528.189319	33426.002626	31.047962
528.984921	33468.382526	31.052980
529.007181	33521.677245	31.057997
529.691327	33569.223448	31.063015
529.958372	33620.452334	31.068032
530.568209	33673.100670	31.073050
531.112582	33732.889429	31.078068
531.512659	33788.903941	31.083085
532.310368	33836.773318	31.088103
532.877826	33894.341044	31.093120
533.532290	33958.473310	31.098138
534.022354	34003.573610	31.103156
534.131784	34063.185331	31.108173
535.088220	34115.239173	31.113191
535.387215	34161.325619	31.118208
536.070969	34213.227721	31.123226
536.276292	34263.472135	31.128244
536.622467	34316.541257	31.133261
537.609297	34352.847450	31.138279
538.016102	34419.090757	31.143296
539.034568	34453.817295	31.148314
539.542898	34494.134740	31.153332
539.895536	34549.784180	31.158349
540.410726	34592.069727	31.163367
541.083186	34641.354935	31.168384
541.472746	34674.432243	31.173402
542.027789	34718.746949	31.178420
542.664664	34787.362311	31.183437
543.109829	34823.932356	31.188455
543.311772	34877.462911	31.193472
543.649882	34927.338205	31.198490
544.735325	34979.282774	31.203508
544.645525	35035.552902	31.208525
545.477364	35081.268541	31.213543
545.942687	35147.245301	31.218560
546.632570	35202.307207	31.223578
547.369920	35246.007828	31.228596
547.575392	35307.796871	31.233613
548.311422	35355.358835	31.238631
548.665066	35421.264600	31.243648
549.041981	35482.806276	31.248666
549.610783	35542.164093	31.253684
550.383445	35604.062549	31.258701
550.732588	35659.497103	31.263719
551.269180	35728.742417	31.268736
551.744305	35784.228266	31.273754
552.206910	35853.742854	31.278772
552.504955	35929.142422	31.283789
553.364827	35988.075518	31.288807
553.401741	36062.437321	31.293824
553.950210	36132.243667	31.298842
554.810270	36193.379932	31.303860
555.262053	36266.952924	31.308877
555.869577	36336.892610	31.313895
556.562900	36404.748846	31.318912
557.262189	36473.458928	31.323930
557.991294	36528.512641	31.328948
558.396603	36603.311652	31.333965
559.122782	36657.864889	31.338983
559.986468	36734.571733	31.344000
559.991269	36790.243011	31.349018
560.711826	36852.092880	31.354036
561.047533	36925.460199	31.359053
561.589137	36990.274795	31.364071
562.340869	37054.341952	31.369088
563.208972	37105.853157	31.374106
564.387827	37169.777059	31.379124
564.767879	37231.587943	31.384141
565.432809	37285.689427	31.389159
566.374833	37334.611684	31.394176
566.317897	37399.163678	31.399194
567.385455	37434.014736	31.404212
567.501422	37480.692873	31.409229
567.902168	37529.085396	31.414247
568.161525	37574.796512	31.419264
568.973770	37631.901357	31.424282
569.600338	37679.272904	31.429300
569.950473	37739.472695	31.434317
570.386128	37789.369333	31.439335
571.277310	37843.693585	31.444352
571.861655	37903.147134	31.449370
572.503939	37953.303050	31.454388
572.879473	38021.381958	31.459405
573.618376	38075.945645	31.464423
573.981333	38129.095098	31.469440
574.158607	38189.191567	31.474458
575.005315	38239.254286	31.479476
575.476847	38309.599080	31.484493
576.173050	38368.319016	31.489511
576.840235	38422.805365	31.494528
577.216736	38493.766812	31.499546
578.057978	38554.615050	31.504564
578.593905	38618.878609	31.509581
579.431610	38685.100066	31.514599
579.838529	38744.595858	31.519616
580.290031	38799.584500	31.524634
580.999375	38860.685056	31.529652
581.127391	38924.975305	31.534669
581.891311	38986.827660	31.539687
582.495612	39051.969732	31.544704
582.862205	39123.756926	31.549722
583.535247	39184.877044	31.554740
584.460290	39260.972183	31.559757
584.938731	39319.670165	31.564775
585.608223	39384.333222	31.569792
586.388545	39448.570464	31.574810
586.833995	39501.641695	31.579828
586.895291	39569.381043	31.584845
587.697652	39634.233620	31.589863
588.320779	39698.709717	31.594880
588.541203	39778.139411	31.599898
589.448669	39840.751010	31.604916
589.874041	39911.280087	31.609933
590.644711	39978.441334	31.614951
591.359280	40051.496921	31.619968
591.945181	40119.247958	31.624986
592.808785	40170.474315	31.630004
593.629290	40244.362259	31.635021
593.861503	40300.385724	31.640039
594.740228	40361.482043	31.645056
595.172944	40433.893431	31.650074
595.597693	40492.419491	31.655092
595.847807	40572.628753	31.660109
596.919310	40636.499246	31.665127
597.098944	40704.823506	31.670144
597.651144	40781.648713	31.675162
598.282629	40836.011269	31.680180
598.666048	40902.162284	31.685197
599.219246	40973.777723	31.690215
600.092007	41023.570087	31.695232
600.377599	41095.783759	31.700250
600.731883	41165.293208	31.705268
601.084950	41235.411872	31.710285
602.069452	41310.634570	31.715303
602.827763	41392.930471	31.720320
603.046812	41473.256127	31.725338
603.655262	41536.601264	31.730356
604.433664	41611.962185	31.735373
604.895846	41681.201052	31.740391
605.578285	41743.106326	31.745408
606.458941	41824.277691	31.750426
607.247915	41894.774382	31.755444
607.862536	41971.055598	31.760461
608.612567	42038.754966	31.765479
609.256596	42114.997440	31.770496
609.596403	42188.557089	31.775514
610.454488	42254.517868	31.780532
610.935008	42325.680520	31.785549
611.677025	42388.859276	31.790567
612.146469	42457.030794	31.795584
612.699511	42537.014876	31.800602
613.400123	42610.399011	31.805620
614.233897	42675.523060	31.810637
614.904120	42746.127308	31.815655
615.645546	42807.146943	31.820672
615.788143	42880.327713	31.825690
616.723655	42948.972677	31.830708
617.231791	43017.279038	31.835725
617.462056	43101.676540	31.840743
618.665614	43164.816195	31.845760
618.738639	43246.974543	31.850778
619.471905	43316.066400	31.855796
620.017495	43386.992783	31.860813
620.862741	43467.571852	31.865831
621.954540	43543.679939	31.870848
622.431140	43614.671865	31.875866
623.123660	43677.528831	31.880884
623.821623	43747.599630	31.885901
624.116146	43814.413183	31.890919
625.124315	43886.208021	31.895936
625.550041	43952.073766	31.900954
625.927641	44035.837206	31.905972
626.598533	44106.762354	31.910989
627.401442	44177.367082	31.916007
628.172487	44238.759292	31.921024
628.749684	44311.318525	31.926042
629.337540	44370.825489	31.931060
630.158320	44447.766204	31.936077
630.357844	44520.048886	31.941095
630.949488	44584.956821	31.946112
631.503049	44659.344690	31.951130
632.364946	44737.693456	31.956148
633.022751	44798.824898	31.961165
633.614340	44865.689831	31.966183
634.146236	44920.986515	31.971200
634.413551	45000.623629	31.976218
635.809650	45048.047598	31.981236
636.833360	45112.516444	31.986253
637.234712	45165.295069	31.991271
638.054237	45218.250199	31.996288
638.523515	45284.978471	32.001306
638.711651	45334.967976	32.006324
639.754370	45397.261161	32.011341
640.296833	45466.265743	32.016359
640.817889	45525.045887	32.021376
641.007661	45600.388513	32.026394
641.845652	45671.157762	32.031412
642.521848	45734.800859	32.036429
642.533210	45810.254818	32.041447
643.802593	45880.382036	32.046464
644.400676	45953.566293	32.051482
645.048573	46026.717686	32.056500
645.585770	46090.753336	32.061517
646.642478	46161.619101	32.066535
647.686364	46217.917384	32.071552
647.917335	46287.126231	32.076570
648.749644	46346.171923	32.081588
649.670828	46410.936368	32.086605
649.882044	46486.585423	32.091623
650.688697	46547.421636	32.096640
651.278653	46620.603659	32.101658
651.838189	46686.701347	32.106676
652.307692	46761.830892	32.111693
653.098408	46825.813087	32.116711
653.663262	46904.272480	32.121728
654.061315	46972.031303	32.126746
655.018913	47048.469472	32.131764
656.364769	47101.248695	32.136781
656.495407	47170.379176	32.141799
657.527667	47240.707345	32.146816
658.415973	47297.254722	32.151834
658.703623	47364.108157	32.156852
659.395824	47432.090113	32.161869
659.816517	47507.009740	32.166887
660.615392	47567.980086	32.171904
660.993419	47641.379936	32.176922
662.025409	47697.949899	32.181940
662.766145	47774.675009	32.186957
662.910807	47849.782020	32.191975
663.450513	47918.796666	32.196992
664.047215	47994.223584	32.202010
664.686948	48069.391547	32.207028
665.289206	48145.067495	32.212045
665.844681	48232.261974	32.217063
666.727064	48312.100141	32.222080
667.222899	48385.768307	32.227098
667.521147	48460.099315	32.232116
668.369545	48525.274387	32.237133
668.703547	48602.954508	32.242151
669.231331	48678.322734	32.247168
669.880043	48757.247161	32.252186
670.064618	48844.876039	32.257204
671.071532	48935.226998	32.262221
671.433363	49015.283728	32.267239
672.509193	49101.427745	32.272256
673.273968	49195.018267	32.277274
673.862291	49281.979161	32.282292
674.858890	49362.031068	32.287309
675.202809	49451.928506	32.292327
675.940165	49536.374010	32.297344
676.936532	49632.883603	32.302362
677.329045	49711.013652	32.307380
678.108331	49792.563143	32.312397
678.841692	49889.273773	32.317415
679.817416	49957.718868	32.322432
680.173064	50043.477182	32.327450
680.840586	50139.764166	32.332468
681.886089	50207.656331	32.337485
682.392180	50305.468869	32.342503
683.028954	50388.366018	32.347520
683.776145	50477.775240	32.352538
684.192994	50553.090158	32.357556
685.051428	50652.101343	32.362573
685.637485	50737.018418	32.367591
686.390788	50830.183837	32.372608
687.421589	50916.094476	32.377626
687.698541	50997.416998	32.382644
688.999829	51081.764253	32.387661
689.499274	51178.560113	32.392679
689.942823	51260.463235	32.397696
690.800208	51345.043343	32.402714
691.369078	51438.727290	32.407732
692.222429	51518.300396	32.412749
693.210759	51612.347685	32.417767
694.302555	51688.819154	32.422784
695.074810	51766.342263	32.427802
695.646249	51850.597861	32.432820
696.443234	51910.459836	32.437837
697.063335	51987.184396	32.442855
697.666121	52074.683602	32.447872
698.400614	52151.305439	32.452890
699.086180	52228.452986	32.457908
699.826192	52303.531274	32.462925
700.343857	52385.784354	32.467943
701.289533	52469.086939	32.472960
702.116147	52545.973527	32.477978
702.121534	52625.576040	32.482996
703.254599	52697.172148	32.488013
703.768768	52779.796847	32.493031
704.268585	52861.900282	32.498048
705.102838	52941.473243	32.503066
705.648934	53022.133971	32.508084
706.239546	53099.688564	32.513101
706.957283	53183.838719	32.518119
707.560767	53264.172609	32.523136
708.314202	53335.077330	32.528154
709.028185	53418.746265	32.533172
709.996471	53490.785217	32.538189
710.636457	53572.752777	32.543207
710.869514	53653.857524	32.548224
711.897139	53736.234411	32.553242
712.738504	53821.197958	32.558260
713.378541	53895.067787	32.563277
714.087617	53983.742934	32.568295
714.921810	54054.849089	32.573312
715.688947	54142.802426	32.578330
715.972940	54230.271251	32.583348
716.765511	54311.870650	32.588365
717.504898	54407.859642	32.593383
717.880636	54485.018761	32.598400
719.146309	54571.840559	32.603418
719.507240	54667.730179	32.608436
720.278200	54757.361970	32.613453
721.008525	54862.783285	32.618471
721.495467	54946.564825	32.623488
722.887999	55030.562453	32.628506
722.985824	55137.178194	32.633524
723.776307	55224.485932	32.638541
724.409880	55322.472597	32.643559
724.914847	55417.326793	32.648576
725.810118	55507.374931	32.653594
726.534225	55608.041324	32.658612
727.288153	55695.704360	32.663629
727.901452	55800.925580	32.668647
728.689999	55892.454143	32.673664
729.749996	55990.363878	32.678682
730.514600	56099.006704	32.683700
731.226703	56185.109836	32.688717
732.048048	56272.768055	32.693735
732.503847	56379.674961	32.698752
733.227517	56469.310026	32.703770
734.225453	56580.251432	32.708788
735.118000	56662.776659	32.713805
736.068188	56768.120261	32.718823
736.625424	56852.543309	32.723840
737.528818	56934.749185	32.728858
737.969141	57035.436991	32.733876
738.616614	57132.900735	32.738893
739.313982	57233.359292	32.743911
739.630591	57322.248805	32.748928
740.294305	57430.391485	32.753946
741.483409	57524.670948	32.758964
742.266774	57612.433133	32.763981
743.066731	57730.137365	32.768999
743.541798	57815.345044	32.774016
744.874750	57912.025030	32.779034
745.286123	57992.880625	32.784052
746.302408	58087.313588	32.789069
746.885815	58165.575851	32.794087
747.435825	58258.552710	32.799104
748.428814	58340.659021	32.804122
748.999579	58431.284545	32.809140
749.692118	58518.730821	32.814157
750.140954	58612.164396	32.819175
750.721177	58721.890692	32.824192
751.508589	58796.804946	32.829210
751.896524	58913.830846	32.834228
752.708858	59007.312738	32.839245
753.815771	59107.485784	32.844263
754.614546	59200.490902	32.849280
755.868112	59307.474006	32.854298
756.293193	59407.229916	32.859316
757.215205	59495.490414	32.864333
758.423016	59595.097493	32.869351
758.818589	59705.537791	32.874368
759.589167	59780.045063	32.879386
760.176633	59881.965715	32.884404
760.987623	59984.378632	32.889421
761.795459	60076.104765	32.894439
762.310894	60183.204049	32.899456
762.907064	60281.241848	32.904474
763.685187	60393.251402	32.909492
764.710216	60491.383077	32.914509
765.738861	60589.618887	32.919527
766.533074	60692.751941	32.924544
767.428561	60779.232404	32.929562
768.204428	60889.754925	32.934580
769.092693	60986.578470	32.939597
769.526697	61080.939272	32.944615
770.499111	61173.449761	32.949632
771.415663	61267.052657	32.954650
772.107490	61371.872950	32.959668
772.746042	61467.668276	32.964685
773.369052	61573.400571	32.969703
773.616665	61680.945715	32.974720
775.078020	61772.361401	32.979738
775.647324	61888.303372	32.984756
776.488293	61985.070106	32.989773
777.573990	62083.055172	32.994791
778.099369	62196.242992	32.999808
779.329779	62285.446430	33.004826
779.777472	62398.742558	33.009844
780.649727	62492.718572	33.014861
781.757342	62585.407094	33.019879
782.017220	62687.401378	33.024896
782.993293	62782.568607	33.029914
783.856077	62877.312240	33.034932
784.581991	62976.404448	33.039949
785.645701	63063.863346	33.044967
786.159746	63178.805160	33.049984
787.023128	63266.486348	33.055002
787.688048	63362.072323	33.060020
788.745564	63435.433624	33.065037
790.258226	63511.287062	33.070055
791.071267	63586.143684	33.075072
792.411250	63659.953550	33.080090
792.617519	63729.927118	33.085108
793.198285	63815.015706	33.090125
794.057899	63891.767257	33.095143
794.634391	63966.009302	33.100160
795.243457	64044.759340	33.105178
795.901355	64133.721507	33.110196
796.658541	64221.449260	33.115213
797.281264	64308.620879	33.120231
797.877494	64407.460099	33.125248
798.665821	64498.790760	33.130266
799.395679	64596.378013	33.135284
800.095258	64694.036903	33.140301
800.838642	64797.146688	33.145319
801.320474	64899.711223	33.150336
802.020462	64996.149358	33.155354
802.872239	65102.205956	33.160372
803.862247	65204.375425	33.165389
804.977537	65301.232221	33.170407
805.563827	65417.050843	33.175424
806.397022	65537.678893	33.180442
807.624219	65640.848869	33.185460
808.069230	65740.429648	33.190477
808.975064	65838.323681	33.195495
810.194999	65942.011244	33.200512
810.876310	66034.632758	33.205530
811.723273	66141.886576	33.210548
812.103035	66246.243249	33.215565
813.022093	66348.913329	33.220583
813.743982	66464.283960	33.225600
814.324344	66573.673511	33.230618
815.161250	66688.774500	33.235636
815.807429	66798.758126	33.240653
816.705541	66912.776809	33.245671
817.269506	67042.699017	33.250688
817.862445	67161.543480	33.255706
818.704508	67279.395128	33.260724
819.703359	67403.040731	33.265741
820.977544	67525.626224	33.270759
821.036108	67649.821014	33.275776
822.101956	67764.247590	33.280794
823.632089	67877.406970	33.285812
824.371492	67984.299587	33.290829
825.293092	68097.506544	33.295847
826.380186	68199.613229	33.300864
827.697223	68308.153024	33.305882
828.607535	68414.351147	33.310900
829.096298	68524.552801	33.315917
830.191604	68624.177583	33.320935
831.062847	68715.290712	33.325952
831.790881	68810.994755	33.330970
832.786356	68900.288432	33.335988
833.182734	69013.022001	33.341005
833.947125	69101.961669	33.346023
834.547832	69203.595038	33.351040
835.502557	69291.500746	33.356058
836.090493	69398.254626	33.361076
836.756183	69503.006567	33.366093
837.801392	69589.465044	33.371111
838.404147	69711.558278	33.376128
838.892061	69827.447279	33.381146
839.524787	69921.478680	33.386164
840.369200	70056.443412	33.391181
841.195313	70170.220916	33.396199
841.848143	70288.310378	33.401216
842.803120	70407.508704	33.406234
843.787457	70525.584748	33.411252
844.564360	70649.551568	33.416269
845.591838	70763.597419	33.421287
846.348967	70894.007303	33.426304
846.990215	71011.110951	33.431322
847.878903	71145.343156	33.436340
848.631988	71274.473548	33.441357
849.615236	71391.177510	33.446375
850.467935	71531.041554	33.451392
851.237529	71658.099327	33.456410
852.294071	71780.221614	33.461428
853.109928	71914.622270	33.466445
854.352388	72017.684520	33.471463
855.151098	72140.924238	33.476480
856.169795	72265.936897	33.481498
857.413298	72369.323067	33.486516
857.928057	72492.976640	33.491533
858.968844	72606.234803	33.496551
859.629740	72737.651553	33.501568
860.649991	72857.890549	33.506586
861.750503	72972.980123	33.511604
862.410028	73098.446937	33.516621
863.483007	73199.532812	33.521639
864.283703	73326.672119	33.526656
865.118138	73444.201702	33.531674
866.138874	73556.343635	33.536692
866.944044	73687.882703	33.541709
867.946571	73797.286324	33.546727
868.601964	73918.537648	33.551744
869.885119	74040.707243	33.556762
870.663450	74154.723712	33.561780
871.087290	74279.331748	33.566797
872.390259	74377.094547	33.571815
873.134404	74506.386317	33.576832
873.717561	74626.869791	33.581850
874.638657	74735.229794	33.586868
875.427349	74855.896802	33.591885
876.419682	74980.235457	33.596903
877.035724	75103.573038	33.601920
877.824877	75218.611286	33.606938
879.190591	75324.249425	33.611956
879.687804	75447.386821	33.616973
880.724616	75552.086272	33.621991
881.800706	75667.289978	33.627008
882.224816	75777.308301	33.632026
883.592114	75888.674987	33.637044
883.701367	76002.460759	33.642061
884.784618	76114.290997	33.647079
885.945156	76237.270779	33.652096
886.752167	76361.893899	33.657114
887.792538	76464.391787	33.662132
888.371240	76584.306178	33.667149
888.998938	76707.430465	33.672167
890.027104	76829.069727	33.677184
890.721107	76948.392776	33.682202
891.873488	77070.190686	33.687220
892.688269	77197.352135	33.692237
893.928652	77308.512950	33.697255
894.669649	77437.830250	33.702272
895.252716	77567.293584	33.707290
896.980401	77678.675951	33.712308
898.040578	77805.201698	33.717325
898.796945	77916.227930	33.722343
899.885786	78024.749471	33.727360
900.617935	78142.126678	33.732378
901.842827	78264.489034	33.737396
902.460371	78380.185573	33.742413
903.456192	78498.963999	33.747431
904.150653	78617.715207	33.752448
904.952773	78743.744216	33.757466
905.993542	78862.606086	33.762484
906.578303	78996.407970	33.767501
907.351587	79114.726006	33.772519
908.309379	79250.290626	33.777536
909.143517	79388.574891	33.782554
910.272302	79511.073738	33.787572
910.859142	79651.674693	33.792589
911.607337	79777.067525	33.797607
912.594773	79913.004730	33.802624
913.346055	80041.173675	33.807642
914.808303	80174.653958	33.812660
915.543936	80309.205217	33.817677
916.468822	80441.438911	33.822695
917.376290	80569.093210	33.827712
918.083140	80708.240967	33.832730
919.341078	80830.998902	33.837748
920.328382	80964.755796	33.842765
921.221873	81086.985323	33.847783
922.300876	81230.553028	33.852800
923.024794	81359.998786	33.857818
923.999403	81485.150983	33.862836
924.589367	81626.706743	33.867853
925.562759	81762.399094	33.872871
926.804614	81880.519289	33.877888
927.900335	82019.904744	33.882906
929.338066	82135.643500	33.887924
930.109132	82253.214833	33.892941
931.648218	82338.751530	33.897959
932.461418	82455.716714	33.902976
933.488603	82558.341833	33.907994
934.792194	82641.919485	33.913012
936.313403	82728.598587	33.918029
937.033876	82825.590289	33.923047
937.805441	82913.350363	33.928064
938.538598	83015.929665	33.933082
939.473613	83126.892155	33.938100
939.867474	83222.964034	33.943117
940.445033	83326.423098	33.948135
941.454587	83449.665842	33.953152
941.833538	83564.000347	33.958170
942.881446	83685.550316	33.963188
943.715819	83811.459455	33.968205
944.006899	83946.762355	33.973223
945.145607	84076.418107	33.978240
945.840131	84207.232781	33.983258
946.426625	84347.403823	33.988276
947.367358	84491.945243	33.993293
948.366821	84642.965311	33.998311
949.169859	84796.578379	34.003328
949.808494	84955.087196	34.008346
950.703876	85092.147506	34.013364
951.528762	85259.790636	34.018381
952.651596	85417.947677	34.023399
953.920294	85562.140709	34.028416
954.732262	85721.500219	34.033434
955.498880	85867.760588	34.038452
956.689061	86020.012040	34.043469
958.014000	86188.151995	34.048487
959.370011	86332.171943	34.053504
959.975585	86485.695805	34.058522
960.689754	86632.134145	34.063540
962.189207	86786.358958	34.068557
962.871367	86937.926312	34.073575
963.839740	87091.624438	34.078592
964.985987	87239.281828	34.083610
965.893048	87384.240234	34.088628
967.052210	87540.257209	34.093645
968.018485	87691.607622	34.098663
969.381587	87829.395174	34.103680
969.813523	87986.346792	34.108698
971.035447	88122.337473	34.113716
972.045445	88274.443854	34.118733
973.336644	88436.314689	34.123751
974.320781	88574.938772	34.128768
975.179551	88712.584520	34.133786
976.450664	88855.964531	34.138804
977.133985	89000.324332	34.143821
978.354368	89149.304679	34.148839
979.146325	89285.314137	34.153856
979.719252	89435.771735	34.158874
981.091896	89566.745200	34.163892
982.096758	89695.147126	34.168909
983.102490	89834.022446	34.173927
984.043768	89970.752357	34.178944
984.776111	90103.525774	34.183962
985.793115	90242.098335	34.188980
986.778945	90380.796895	34.193997
987.747736	90496.345648	34.199015
988.797596	90639.114856	34.204032
989.426915	90787.289692	34.209050
990.607587	90925.948065	34.214068
991.559465	91078.329920	34.219085
992.422669	91225.572434	34.224103
993.517424	91363.627430	34.229120
994.490853	91519.974433	34.234138
995.590595	91659.181573	34.239156
996.336071	91814.333611	34.244173
997.291378	91961.591694	34.249191
998.419086	92106.831028	34.254208
998.984680	92267.934872	34.259226
999.927433	92419.366074	34.264244
1001.266682	92577.104452	34.269261
1002.075245	92737.799899	34.274279
1003.338697	92896.324252	34.279296
1004.105633	93056.244323	34.284314
1004.963217	93214.626776	34.289332
1005.935247	93384.402738	34.294349
1006.872967	93544.166325	34.299367
1008.366670	93696.201730	34.304384
1009.209868	93864.648240	34.309402
1010.027232	94025.737432	34.314420
1011.640037	94186.511510	34.319437
1012.402786	94351.622033	34.324455
1013.454932	94509.248982	34.329472
1014.490272	94671.269627	34.334490
1015.705750	94824.546160	34.339508
1016.941327	94990.180790	34.344525
1017.844770	95149.303432	34.349543
1019.332050	95290.812154	34.354560
1020.449659	95453.533838	34.359578
1021.355493	95602.873385	34.364596
1022.490436	95754.865961	34.369613
1023.357962	95913.898505	34.374631
1024.740455	96051.171362	34.379648
1025.750010	96194.735427	34.384666
1026.845211	96343.126166	34.389684
1027.977233	96493.422485	34.394701
1028.934836	96640.078418	34.399719
1030.121296	96776.766902	34.404736
1030.897752	96931.841959	34.409754
1031.944534	97071.799753	34.414772
1032.953219	97229.180599	34.419789
1033.495291	97384.023988	34.424807
1034.378846	97535.644632	34.429824
1035.552206	97689.162389	34.434842
1036.325361	97836.892899	34.439860
1037.405748	97980.589843	34.444877
1038.150638	98133.950982	34.449895
1039.257787	98279.923088	34.454912
1040.057710	98444.817153	34.459930
1041.114186	98585.099020	34.464948
1042.135809	98733.542346	34.469965
1043.218678	98892.169203	34.474983
1045.026162	99035.295285	34.480000
1046.189175	99181.080771	34.485018
1047.303872	99325.653790	34.490036
1048.656376	99472.182858	34.495053
1049.463083	99621.937800	34.500071
1050.981602	99748.961714	34.505088
1051.712447	99903.266959	34.510106
1052.650071	100046.373165	34.515124
1053.704699	100181.559160	34.520141
1054.814063	100319.432581	34.525159
1056.142436	100459.227078	34.530176
1057.084678	100608.416397	34.535194
1058.065129	100743.149257	34.540212
1059.352107	100889.887554	34.545229
1060.149530	101048.859349	34.550247
1061.188783	101185.730377	34.555264
1062.169770	101343.276653	34.560282
1063.209771	101494.550473	34.565300
1064.234794	101640.613839	34.570317
1064.917777	101791.883088	34.575335
1066.022378	101940.232552	34.580352
1067.232585	102112.845065	34.585370
1068.780605	102258.164728	34.590388
1069.959310	102415.889283	34.595405
1070.521558	102572.086710	34.600423
1071.632730	102716.763657	34.605440
1072.671494	102870.659930	34.610458
1073.480858	103045.184434	34.615476
1074.807870	103200.384855	34.620493
1075.529618	103362.504038	34.625511
1076.780725	103527.893975	34.630528
1077.886405	103692.770316	34.635546
1078.787274	103859.623088	34.640564
1079.872050	104031.383704	34.645581
1080.641464	104207.574786	34.650599
1082.098737	104360.977588	34.655616
1082.870181	104531.013432	34.660634
1083.501795	104716.855441	34.665652
1084.793512	104887.235098	34.670669
1085.625378	105066.270363	34.675687
1086.623549	105252.077247	34.680704
1087.986219	105431.657365	34.685722
1088.749009	105621.073806	34.690740
1090.093212	105798.887638	34.695757
1091.004240	105988.346701	34.700775
1092.181668	106166.341670	34.705792
1093.458256	106344.277893	34.710810
1094.206318	106521.938737	34.715828
1096.042088	106686.650096	34.720845
1097.151765	106844.509991	34.725863
1098.331056	107009.226687	34.730880
1099.192822	107163.590251	34.735898
1100.236809	107331.666006	34.740916
1101.481627	107490.850387	34.745933
1102.469157	107660.101942	34.750951
1103.891708	107833.007018	34.755968
1104.945087	107994.364389	34.760986
1105.347952	108167.680827	34.766004
1106.659256	108327.986736	34.771021
1107.813297	108514.971266	34.776039
1108.549781	108696.048748	34.781056
1109.835325	108871.856522	34.786074
1110.909943	109049.521973	34.791092
1112.197096	109215.483406	34.796109
1113.180029	109409.217557	34.801127
1114.207182	109586.856487	34.806144
1115.511610	109770.763228	34.811162
1116.173439	109960.767699	34.816180
1117.946320	110139.349114	34.821197
1119.250880	110316.290933	34.826215
1120.678132	110489.207765	34.831232
1121.912951	110666.973410	34.836250
1122.917261	110841.479123	34.841268
1124.418267	111000.778596	34.846285
1125.212763	111184.745342	34.851303
1126.485410	111351.818603	34.856320
1127.825125	111516.603513	34.861338
1129.009459	111707.044767	34.866356
1130.097497	111857.819155	34.871373
1131.767297	112034.613935	34.876391
1132.859022	112198.461629	34.881408
1134.169777	112361.300717	34.886426
1135.018300	112531.791737	34.891444
1136.036252	112690.767405	34.896461
1137.387134	112864.865091	34.901479
1138.646907	113026.191004	34.906496
1139.601037	113194.390803	34.911514
1140.473560	113379.481866	34.916532
1141.296951	113535.980625	34.921549
1142.778646	113706.265033	34.926567
1143.717977	113885.765619	34.931584
1144.840114	114058.331637	34.936602
1145.728193	114241.641324	34.941620
1147.297199	114406.358207	34.946637
1148.387233	114572.988256	34.951655
1149.474903	114754.389683	34.956672
1151.290779	114932.511183	34.961690
1152.250326	115105.698989	34.966708
1153.484624	115264.890787	34.971725
1154.721186	115430.604189	34.976743
1155.765654	115600.572040	34.981760
1157.253872	115755.035217	34.986778
1158.097247	115915.584794	34.991796
1159.205079	116070.920753	34.996813
1160.083853	116213.865871	35.001831
1160.994234	116368.532268	35.006848
1162.426501	116524.674133	35.011866
1163.257357	116692.454607	35.016884
1164.137823	116856.473781	35.021901
1165.366711	117029.017699	35.026919
1166.261945	117199.247851	35.031936
1167.514301	117372.277870	35.036954
1167.979319	117557.977041	35.041972
1169.388434	117731.320126	35.046989
1170.443000	117914.750071	35.052007
1171.411368	118109.585742	35.057024
1172.697209	118296.540045	35.062042
1173.788839	118501.470866	35.067060
1175.342600	118678.666041	35.072077
1176.187477	118868.189319	35.077095
1177.261959	119066.244576	35.082112
1178.217752	119265.320664	35.087130
1179.128089	119466.843329	35.092148
1180.627428	119659.541987	35.097165
1181.857158	119869.571621	35.102183
1182.929803	120077.323004	35.107200
1184.433061	120271.608599	35.112218
1185.312124	120479.609244	35.117236
1186.795174	120671.026162	35.122253
1188.397057	120879.269676	35.127271
1189.571579	121088.621295	35.132288
1190.957391	121277.791084	35.137306
1191.711489	121480.842196	35.142324
1193.555654	121669.853279	35.147341
1195.114007	121861.596174	35.152359
1195.673894	122072.041183	35.157376
1197.179305	122251.509974	35.162394
1198.382142	122456.599688	35.167412
1199.791361	122649.587877	35.172429
1201.068926	122845.828141	35.177447
1202.115202	123039.155494	35.182464
1203.708567	123237.640945	35.187482
1204.789614	123421.795462	35.192500
1206.071385	123611.125078	35.197517
1207.484759	123793.608073	35.202535
1208.509614	123990.910208	35.207552
1209.727133	124173.312924	35.212570
1211.042202	124360.717262	35.217588
1212.151078	124556.844886	35.222605
1213.433821	124747.309675	35.227623
1214.302426	124944.174970	35.232640
1215.737143	125139.811703	35.237658
1216.583394	125342.003485	35.242676
1217.667779	125536.812095	35.247693
1219.057236	125735.247049	35.252711
1219.836826	125940.341968	35.257728
1221.400835	126132.114499	35.262746
1222.379703	126333.443873	35.267764
1223.390871	126520.012076	35.272781
1224.681690	126700.912739	35.277799
1225.697256	126896.375386	35.282816
1227.302463	127082.992348	35.287834
1228.276939	127291.676715	35.292852
1229.300982	127478.692775	35.297869
1230.770473	127677.205119	35.302887
1231.780447	127868.178457	35.307904
1233.510157	128059.469430	35.312922
1235.244131	128248.062728	35.317940
1236.563955	128437.394563	35.322957
1237.938490	128614.671384	35.327975
1238.826282	128813.816436	35.332992
1240.471542	129005.241393	35.338010
1241.193554	129199.652191	35.343028
1242.436860	129389.471426	35.348045
1244.077029	129582.472087	35.353063
1244.936980	129779.145388	35.358080
1246.231096	129967.212172	35.363098
1247.472760	130168.920471	35.368116
1248.425279	130368.269041	35.373133
1249.745893	130570.297078	35.378151
1251.021974	130776.451181	35.383168
1252.348504	130972.045142	35.388186
1253.400470	131186.663043	35.393204
1254.399094	131406.320893	35.398221
1256.043633	131604.757371	35.403239
1257.028624	131802.856628	35.408256
1258.433212	132010.760423	35.413274
1259.898897	132232.985789	35.418292
1261.182205	132438.922808	35.423309
1262.705791	132644.924489	35.428327
1263.752397	132860.354129	35.433344
1265.023665	133062.851256	35.438362
1266.077298	133281.336510	35.443380
1267.331800	133499.956221	35.448397
1268.833638	133702.991405	35.453415
1269.779244	133923.652730	35.458432
1271.161206	134143.701548	35.463450
1272.534712	134361.675359	35.468468
1273.807209	134566.184899	35.473485
1274.760074	134781.504462	35.478503
1276.004028	135008.170784	35.483520
1277.725849	135212.385396	35.488538
1278.880173	135441.299497	35.493556
1279.673461	135659.844133	35.498573
1281.380036	135876.053072	35.503591
1282.654686	136101.063054	35.508608
1284.083125	136318.041758	35.513626
1285.336609	136532.908330	35.518644
1286.486510	136764.291849	35.523661
1287.768004	136979.017844	35.528679
1288.559780	137203.682181	35.533696
1290.333129	137413.999300	35.538714
1291.945143	137621.454266	35.543732
1293.249937	137827.692271	35.548749
1294.724044	138020.421246	35.553767
1295.972050	138218.281794	35.558784
1297.079545	138421.475846	35.563802
1298.854952	138609.598600	35.568820
1300.505518	138812.265470	35.573837
1301.646930	139004.534117	35.578855
1302.932170	139201.406796	35.583872
1304.631932	139382.449562	35.588890
1305.441963	139579.641041	35.593908
1306.523561	139781.188280	35.598925
1307.926094	139974.460868	35.603943
1308.990156	140175.265810	35.608960
1310.307661	140378.072250	35.613978
1311.530721	140591.604257	35.618996
1312.377940	140802.143141	35.624013
1313.885853	141017.356508	35.629031
1315.055829	141245.489091	35.634048
1316.225564	141457.223311	35.639066
1317.719516	141673.774319	35.644084
1318.842257	141897.698840	35.649101
1320.132654	142116.883545	35.654119
1321.238047	142348.482045	35.659136
1322.706818	142574.067568	35.664154
1323.713657	142805.216226	35.669172
1324.894649	143038.569681	35.674189
1326.565736	143274.103122	35.679207
1327.431049	143516.458712	35.684224
1329.031483	143752.171803	35.689242
1330.814160	143982.838427	35.694260
1331.788944	144231.583098	35.699277
1333.333294	144458.488600	35.704295
1334.731161	144701.592712	35.709312
1336.177931	144939.012371	35.714330
1337.737340	145174.894878	35.719348
1338.889994	145410.374803	35.724365
1340.484749	145636.279484	35.729383
1342.149981	145859.259166	35.734400
1344.356545	146066.588462	35.739418
1345.841161	146282.907001	35.744436
1346.856625	146502.546635	35.749453
1348.712503	146705.397842	35.754471
1350.087145	146929.255213	35.759488
1351.120985	147145.980865	35.764506
1352.647337	147355.771820	35.769524
1353.611324	147580.130026	35.774541
1354.962743	147801.335171	35.779559
1355.572448	148028.402221	35.784576
1356.941015	148259.102607	35.789594
1358.516743	148484.358737	35.794612
1359.615142	148725.880702	35.799629
1360.889154	148958.768891	35.804647
1362.502256	149182.198482	35.809664
1363.737668	149407.084122	35.814682
1365.096406	149623.597414	35.819700
1366.307102	149851.773481	35.824717
1367.691782	150062.606130	35.829735
1368.748011	150279.856447	35.834752
1370.041037	150495.904248	35.839770
1371.374556	150727.109558	35.844788
1372.358552	150961.820395	35.849805
1373.671720	151189.076735	35.854823
1374.965683	151424.933355	35.859840
1375.919963	151675.488789	35.864858
1377.295715	151914.949169	35.869876
1378.587184	152170.817644	35.874893
1380.002195	152418.009161	35.879911
1381.495723	152681.836833	35.884928
1382.349174	152936.614396	35.889946
1384.182995	153188.030444	35.894964
1385.319454	153456.852978	35.899981
1386.551703	153706.809029	35.904999
1387.972824	153981.587633	35.910016
1389.343127	154250.670993	35.915034
1390.539690	154508.119306	35.920052
1391.795513	154784.642410	35.925069
1393.267774	155053.563822	35.930087
1395.058307	155330.399487	35.935104
1396.824778	155595.842326	35.940122
1398.258411	155861.187961	35.945140
1399.982862	156143.721218	35.950157
1401.641933	156396.596372	35.955175
1402.978437	156664.892717	35.960192
1404.345464	156923.042284	35.965210
1406.023169	157185.100624	35.970228
1407.117510	157455.254859	35.975245
1408.913656	157708.980131	35.980263
1409.991924	157977.403788	35.985280
1411.486830	158250.936974	35.990298
1412.816041	158506.200513	35.995316
1414.320455	158785.911840	36.000333
1415.993113	159042.151866	36.005351
1417.460413	159304.132794	36.010368
1418.902678	159561.770073	36.015386
1420.406509	159825.067899	36.020404
1421.751067	160088.963645	36.025421
1423.427464	160347.165474	36.030439
1424.968240	160620.519597	36.035456
1426.252346	160880.284028	36.040474
1428.127128	161133.514285	36.045492
1429.005306	161396.187627	36.050509
1430.789564	161656.613781	36.055527
1432.482424	161911.844117	36.060544
1433.914272	162169.996525	36.065562
1435.795263	162412.759570	36.070580
1436.863771	162668.994879	36.075597
1438.413965	162916.531596	36.080615
1440.355103	163170.932413	36.085632
1441.422687	163405.613225	36.090650
1443.103774	163641.580470	36.095668
1444.158296	163873.691835	36.100685
1445.302725	164110.216612	36.105703
1446.493377	164349.525759	36.110720
1447.682956	164595.457033	36.115738
1449.196785	164836.709200	36.120756
1450.415656	165086.837117	36.125773
1452.080710	165328.005054	36.130791
1453.462208	165575.700666	36.135808
1454.907419	165822.715598	36.140826
1456.353050	166070.987744	36.145844
1457.870051	166328.762714	36.150861
1458.883305	166586.898517	36.155879
1460.584436	166850.127068	36.160896
1461.658853	167113.951678	36.165914
1463.250975	167364.428744	36.170932
1464.390479	167630.491637	36.175949
1465.907265	167903.066714	36.180967
1467.819160	168179.436910	36.185984
1469.151400	168447.288715	36.191002
1470.954425	168703.233306	36.196020
1472.482724	168971.565006	36.201037
1474.266683	169228.467452	36.206055
1476.004728	169488.385113	36.211072
1477.339953	169750.613667	36.216090
1478.904063	170009.002270	36.221108
1480.159681	170282.358759	36.226125
1481.396847	170543.238308	36.231143
1483.058336	170822.216885	36.236160
1484.321453	171089.260795	36.241178
1486.250294	171358.458710	36.246196
1487.487599	171639.146853	36.251213
1488.871627	171906.062945	36.256231
1490.277637	172170.199275	36.261248
1491.721367	172450.657433	36.266266
1493.309970	172728.253021	36.271284
1495.237929	172990.294917	36.276301
1497.032173	173249.568939	36.281319
1498.826473	173515.022570	36.286336
1500.233411	173789.140449	36.291354
1501.803513	174045.144230	36.296372
1502.988952	174315.660031	36.301389
1504.518070	174584.638787	36.306407
1505.853886	174857.062598	36.311424
1506.902604	175139.949212	36.316442
1508.839565	175403.007576	36.321460
1510.003462	175698.185467	36.326477
1511.240478	175982.824096	36.331495
1512.703869	176260.666805	36.336512
1513.817314	176552.040183	36.341530
1515.676537	176844.654642	36.346548
1517.328256	177138.560119	36.351565
1518.574995	177434.117859	36.356583
1519.917167	177718.333042	36.361600
1521.536500	178015.954447	36.366618
1523.071888	178282.659963	36.371636
1524.402475	178555.248520	36.376653
1526.212821	178832.520388	36.381671
1527.791314	179111.835510	36.386688
1528.693117	179388.519444	36.391706
1530.274242	179667.013107	36.396724
1531.720382	179952.064173	36.401741
1533.423174	180229.958545	36.406759
1535.385850	180501.418773	36.411776
1536.943896	180780.151711	36.416794
1538.683836	181059.783781	36.421812
1539.973659	181346.467586	36.426829
1541.463970	181625.178651	36.431847
1543.434243	181900.275252	36.436864
1544.525312	182201.118252	36.441882
1546.103281	182481.609906	36.446900
1547.692758	182773.343521	36.451917
1548.863680	183071.578645	36.456935
1550.833273	183360.971825	36.461952
1551.993805	183656.319513	36.466970
1553.861919	183955.071588	36.471988
1554.938634	184251.045584	36.477005
1556.465721	184551.556110	36.482023
1558.372792	184854.914095	36.487040
1559.490067	185173.575791	36.492058
1560.962619	185470.865353	36.497076
1562.899989	185782.612332	36.502093
1564.403105	186097.184009	36.507111
1566.489415	186410.675448	36.512128
1567.911406	186741.735417	36.517146
1569.601519	187047.743798	36.522164
1571.042875	187353.260735	36.527181
1572.400640	187673.348220	36.532199
1574.430960	187975.349445	36.537216
1575.776287	188286.940849	36.542234
1577.321932	188597.753790	36.547252
1578.857519	188900.791290	36.552269
1580.397639	189217.548197	36.557287
1582.447367	189527.728825	36.562304
1584.010607	189844.410091	36.567322
1585.935108	190146.340459	36.572340
1587.444166	190466.080163	36.577357
1588.585973	190774.192183	36.582375
1590.709960	191071.121920	36.587392
1592.316729	191376.841526	36.592410
1594.404695	191679.859617	36.597428
1596.458762	191970.130516	36.602445
1598.310055	192250.599753	36.607463
1600.247224	192544.902991	36.612480
1601.718065	192826.273533	36.617498
1603.809361	193107.674061	36.622516
1605.012740	193394.395251	36.627533
1606.473841	193680.645655	36.632551
1608.344403	193960.816901	36.637568
1609.607472	194239.410885	36.642586
1611.062329	194499.078097	36.647604
1612.948816	194773.920844	36.652621
1614.590398	195030.477043	36.657639
1616.124417	195289.919969	36.662656
1617.529048	195546.681383	36.667674
1619.185579	195801.246450	36.672692
1620.854953	196059.440658	36.677709
1621.686905	196337.848020	36.682727
1623.587883	196599.092328	36.687744
1624.953577	196881.339732	36.692762
1626.408795	197162.559065	36.697780
1628.090659	197435.633501	36.702797
1629.161223	197740.791349	36.707815
1630.611531	198035.140110	36.712832
1631.722190	198338.784634	36.717850
1633.451357	198654.961874	36.722868
1635.192806	198958.801705	36.727885
1636.676065	199263.788527	36.732903
1638.349407	199575.550275	36.737920
1639.748422	199897.943297	36.742938
1641.332718	200211.956805	36.747956
1643.040761	200535.434217	36.752973
1644.962011	200856.226816	36.757991
1647.029808	201170.651398	36.763008
1648.421148	201484.893230	36.768026
1650.126928	201798.871130	36.773044
1652.131208	202118.058498	36.778061
1653.336267	202453.508062	36.783079
1655.207294	202770.879742	36.788096
1656.743701	203094.208896	36.793114
1658.505685	203416.082378	36.798132
1660.374779	203735.262278	36.803149
1661.983763	204073.386464	36.808167
1663.861904	204387.046713	36.813184
1665.251367	204719.408401	36.818202
1666.934456	205045.708368	36.823220
1668.726594	205377.603676	36.828237
1670.282032	205711.645690	36.833255
1671.898331	206027.057367	36.838272
1674.027483	206362.065610	36.843290
1675.557384	206693.146737	36.848308
1677.317085	207017.046195	36.853325
1678.975133	207347.894793	36.858343
1681.189131	207672.982427	36.863360
1682.922583	208004.990562	36.868378
1684.475274	208320.424401	36.873396
1686.422632	208645.711904	36.878413
1688.294207	208964.932285	36.883431
1690.042125	209287.030325	36.888448
1691.640667	209601.092383	36.893466
1693.394473	209913.722214	36.898484
1695.402763	210235.441051	36.903501
1696.870463	210548.360671	36.908519
1698.483226	210870.945340	36.913536
1700.076210	211178.021025	36.918554
1701.404618	211488.859953	36.923572
1703.132026	211777.496085	36.928589
1704.517090	212087.338660	36.933607
1706.241290	212380.281788	36.938624
1708.050570	212684.638838	36.943642
1709.994723	213005.404180	36.948660
1711.412932	213306.931571	36.953677
1712.796081	213619.206598	36.958695
1714.587380	213920.410940	36.963712
1716.095984	214241.568806	36.968730
1717.576942	214570.350219	36.973748
1719.299400	214887.427182	36.978765
1720.215004	215226.712330	36.983783
1722.307790	215553.928630	36.988800
1724.644987	215883.151795	36.993818
1726.467566	216205.208613	36.998836
1729.045440	216522.220828	37.003853
1730.637851	216842.031781	37.008871
1733.147660	217160.035323	37.013888
1734.641299	217484.283264	37.018906
1735.934422	217797.442268	37.023924
1738.108182	218107.783858	37.028941
1739.716000	218435.623858	37.033959
1741.013420	218767.933105	37.038976
1742.857578	219085.746157	37.043994
1744.343208	219415.463721	37.049012
1746.304250	219750.224182	37.054029
1747.789976	220101.694716	37.059047
1749.642357	220430.914203	37.064064
1750.891420	220779.911476	37.069082
1752.502572	221174.702509	37.074100
1754.249512	221502.254689	37.079117
1755.990933	221850.061381	37.084135
1757.882675	222202.175595	37.089152
1759.762813	222550.712579	37.094170
1761.678600	222900.172383	37.099188
1763.183626	223249.533878	37.104205
1765.004721	223594.720029	37.109223
1766.969381	223930.767975	37.114240
1769.137185	224290.301261	37.119258
1770.739399	224641.646977	37.124276
1772.793349	224986.027597	37.129293
1774.516867	225344.544067	37.134311
1776.026251	225688.188713	37.139328
1778.126098	226036.782168	37.144346
1779.489309	226396.731767	37.149364
1781.507515	226739.360332	37.154381
1782.881247	227100.276320	37.159399
1784.869728	227453.096400	37.164416
1786.753218	227807.204420	37.169434
1787.956443	228172.647159	37.174452
1790.070951	228523.064322	37.179469
1791.597131	228883.379430	37.184487
1793.438777	229248.649129	37.189504
1795.211349	229599.454985	37.194522
1797.146477	229945.461753	37.199540
1798.841385	230287.368223	37.204557
1800.569248	230633.664477	37.209575
1802.551993	230965.064105	37.214592
1804.695950	231302.458537	37.219610
1806.318219	231639.784600	37.224628
1808.401678	231970.359091	37.229645
1810.084111	232315.195728	37.234663
1811.922042	232652.846736	37.239680
1813.859575	232989.391009	37.244698
1815.284471	233334.551543	37.249716
1817.275228	233685.388863	37.254733
1818.840291	234036.650562	37.259751
1820.677790	234385.152646	37.264768
1822.705310	234724.736348	37.269786
1824.313180	235082.395302	37.274804
1826.410968	235427.938841	37.279821
1828.077002	235784.295683	37.284839
1829.910384	236146.748282	37.289856
1831.647091	236501.572429	37.294874
1833.677336	236858.535486	37.299892
1835.627216	237218.738160	37.304909
1837.961964	237561.304803	37.309927
1839.855085	237903.383825	37.314944
1842.051129	238259.004427	37.319962
1843.725160	238614.201021	37.324980
1845.636281	238960.979317	37.329997
1847.386174	239318.655232	37.335015
1848.917467	239676.773347	37.340032
1851.041902	240034.417454	37.345050
1852.568007	240393.605386	37.350068
1854.592910	240747.355907	37.355085
1856.438133	241110.610136	37.360103
1858.439001	241476.533156	37.365120
1860.044585	241836.550999	37.370138
1861.760175	242210.954284	37.375156
1863.343595	242577.785021	37.380173
1865.483914	242948.592494	37.385191
1867.247590	243325.175882	37.390208
1869.057716	243699.466965	37.395226
1870.922471	244072.810637	37.400244
1873.053411	244445.554316	37.405261
1874.840044	244826.862868	37.410279
1876.604789	245200.174758	37.415296
1878.539601	245581.182503	37.420314
1880.275612	245961.283009	37.425332
1882.389406	246339.038520	37.430349
1884.463089	246717.690431	37.435367
1886.197577	247103.357031	37.440384
1888.300347	247472.379314	37.445402
1890.088857	247854.330753	37.450420
1892.229058	248227.311539	37.455437
1893.960483	248605.311344	37.460455
1895.981837	248981.767392	37.465472
1898.284128	249339.103334	37.470490
1900.072686	249693.117800	37.475508
1901.731424	250035.316548	37.480525
1903.837597	250388.367682	37.485543
1905.091796	250732.257763	37.490560
1907.263925	251084.131430	37.495578
1909.042087	251448.489761	37.500596
1910.626783	251801.905998	37.505613
1912.440638	252172.839230	37.510631
1914.092547	252534.400240	37.515648
1916.064373	252901.499629	37.520666
1917.972344	253274.223711	37.525684
1919.715277	253637.880800	37.530701
1921.671255	254015.399702	37.535719
1923.456187	254406.689012	37.540736
1925.567304	254790.941750	37.545754
1927.153130	255188.589313	37.550772
1928.850671	255570.648340	37.555789
1930.720938	255970.843298	37.560807
1932.329698	256365.085538	37.565824
1934.895361	256759.786330	37.570842
1936.805964	257164.600303	37.575860
1938.956845	257567.674905	37.580877
1941.020075	257957.453188	37.585895
1942.647108	258374.202618	37.590912
1944.853492	258765.178811	37.595930
1947.015507	259174.096916	37.600948
1949.097762	259570.250774	37.605965
1951.141541	259974.159159	37.610983
1953.136883	260376.551663	37.616000
1955.393190	260772.146204	37.621018
1956.875765	261178.202988	37.626036
1958.832250	261586.522210	37.631053
1960.944852	261996.366790	37.636071
1962.548846	262413.481619	37.641088
1964.483209	262814.235875	37.646106
1966.522484	263232.883073	37.651124
1969.044259	263628.362891	37.656141
1971.731022	264033.216099	37.661159
1973.581075	264431.369054	37.666176
1976.196793	264828.435641	37.671194
1978.025180	265221.410601	37.676212
1979.706799	265618.753151	37.681229
1981.963776	266004.116110	37.686247
1983.755656	266415.057977	37.691264
1986.018335	266811.267864	37.696282
1988.126649	267205.241666	37.701300
1990.190588	267594.650219	37.706317
1991.826203	267992.611681	37.711335
1993.764631	268379.830599	37.716352
1995.968655	268775.847977	37.721370
1997.490396	269183.379909	37.726388
1999.335476	269571.579663	37.731405
2001.562189	269966.501772	37.736423
2003.354905	270379.148244	37.741440
2005.398662	270769.552550	37.746458
2007.260282	271153.508045	37.751476
2009.560062	271531.068737	37.756493
2011.596552	271890.152245	37.761511
2013.610333	272265.573835	37.766528
2015.812228	272636.012019	37.771546
2017.569359	273011.042635	37.776564
2019.365005	273393.383393	37.781581
2021.619985	273771.053333	37.786599
2023.254985	274153.140234	37.791616
2025.598058	274534.327350	37.796634
2027.736254	274904.115442	37.801652
2029.538865	275299.893653	37.806669
2031.649829	275673.547376	37.811687
2033.697531	276065.603182	37.816704
2036.218706	276447.905152	37.821722
2037.945485	276832.517761	37.826740
2039.866361	277228.124594	37.831757
2042.066835	277618.961964	37.836775
2043.974881	278015.358152	37.841792
2046.111052	278396.221982	37.846810
2048.082850	278803.023199	37.851828
2049.605726	279211.165630	37.856845
2052.327168	279608.118143	37.861863
2054.014384	280021.162401	37.866880
2055.999041	280418.688651	37.871898
2057.796203	280830.902137	37.876916
2059.646704	281254.868645	37.881933
2062.116155	281672.614524	37.886951
2063.585293	282103.703055	37.891968
2065.786469	282519.788866	37.896986
2067.696780	282951.492661	37.902004
2069.595840	283392.165204	37.907021
2071.974825	283826.003992	37.912039
2073.844167	284272.421547	37.917056
2075.889357	284688.174597	37.922074
2078.617853	285124.751021	37.927092
2080.987920	285546.116574	37.932109
2083.403868	285973.698136	37.937127
2085.832900	286405.290808	37.942144
2087.715271	286812.303362	37.947162
2090.076462	287243.016662	37.952180
2092.071963	287653.820708	37.957197
2094.120152	288074.268970	37.962215
2096.118566	288512.658968	37.967232
2098.491768	288920.429317	37.972250
2100.811139	289339.791300	37.977268
2102.770188	289763.579077	37.982285
2105.160461	290166.950261	37.987303
2107.492189	290589.051884	37.992320
2109.344580	290998.248102	37.997338
2111.694489	291420.447095	38.002356
2113.658075	291837.016466	38.007373
2115.890556	292238.377197	38.012391
2117.754387	292656.713734	38.017408
2119.955846	293065.165247	38.022426
2121.929534	293453.508076	38.027444
2123.691319	293848.971068	38.032461
2125.750947	294239.178647	38.037479
2128.196227	294643.727408	38.042496
2129.841749	295035.345489	38.047514
2131.824779	295434.809356	38.052532
2133.666095	295831.983308	38.057549
2135.765888	296235.415167	38.062567
2137.722784	296645.854375	38.067584
2139.508286	297068.309563	38.072602
2141.682925	297488.619131	38.077620
2143.633292	297923.493105	38.082637
2145.635428	298346.291993	38.087655
2147.611696	298786.443289	38.092672
2149.399570	299229.315896	38.097690
2151.689009	299679.296439	38.102708
2153.564849	300133.507176	38.107725
2156.598269	300566.881779	38.112743
2158.605961	301017.893943	38.117760
2160.754911	301463.903771	38.122778
2162.758132	301913.669386	38.127796
2164.874741	302372.509276	38.132813
2167.443194	302835.060861	38.137831
2169.265308	303303.495330	38.142848
2171.483558	303764.321422	38.147866
2173.559768	304228.927848	38.152884
2175.786884	304700.849596	38.157901
2178.571605	305152.716459	38.162919
2180.901728	305625.152089	38.167936
2183.567103	306076.552158	38.172954
2186.015335	306527.883503	38.177972
2188.049887	306986.543326	38.182989
2190.349118	307430.351257	38.188007
2192.588411	307893.699762	38.193024
2194.644299	308333.352060	38.198042
2196.778116	308795.799497	38.203060
2198.784494	309258.011371	38.208077
2201.506346	309711.446736	38.213095
2203.786615	310174.373599	38.218112
2205.887499	310630.646995	38.223130
2208.145690	311082.093157	38.228148
2210.396778	311544.993708	38.233165
2213.259393	311999.616866	38.238183
2215.479453	312447.710866	38.243200
2217.748484	312903.668932	38.248218
2220.085707	313348.387973	38.253236
2221.899244	313804.820792	38.258253
2224.411141	314244.784211	38.263271
2226.451485	314700.085026	38.268288
2228.518714	315154.770002	38.273306
2230.840156	315589.297205	38.278324
2232.802308	316060.579840	38.283341
2234.984633	316498.807878	38.288359
2236.977017	316978.234120	38.293376
2239.042084	317439.614035	38.298394
2241.160430	317877.922193	38.303412
2243.036602	318327.619435	38.308429
2245.112959	318763.923739	38.313447
2247.696393	319215.206235	38.318464
2249.721066	319665.457622	38.323482
2251.573851	320105.727590	38.328500
2253.883643	320571.751670	38.333517
2256.073600	321014.046296	38.338535
2258.568013	321479.731600	38.343552
2260.525481	321943.188462	38.348570
2262.726055	322412.166132	38.353588
2264.535950	322886.434807	38.358605
2266.759242	323358.679811	38.363623
2269.056972	323847.824101	38.368640
2271.197362	324334.349299	38.373658
2273.673847	324819.548577	38.378676
2275.981168	325302.511592	38.383693
2278.584676	325783.901060	38.388711
2280.835587	326284.847068	38.393728
2283.005122	326764.496358	38.398746
2285.594791	327254.564236	38.403764
2287.569956	327746.402493	38.408781
2290.413819	328241.655174	38.413799
2292.869103	328733.918914	38.418816
2295.022817	329232.245700	38.423834
2297.779945	329705.739699	38.428852
2300.129096	330203.089467	38.433869
2302.709560	330690.140149	38.438887
2304.733471	331182.481489	38.443904
2306.985333	331670.237940	38.448922
2309.573627	332165.073265	38.453940
2311.891087	332663.198396	38.458957
2314.454741	333149.803416	38.463975
2316.886600	333636.984589	38.468992
2319.240868	334132.808107	38.474010
2321.712739	334616.522665	38.479028
2323.997977	335108.084170	38.484045
2326.509231	335592.420363	38.489063
2328.952283	336081.816848	38.494080
2331.325218	336562.257619	38.499098
2333.816014	337045.875548	38.504116
2335.941961	337549.225951	38.509133
2338.244023	338028.880105	38.514151
2340.825413	338513.920079	38.519168
2342.759363	339013.277766	38.524186
2345.142130	339496.792935	38.529204
2347.839716	339992.721136	38.534221
2350.127040	340478.148167	38.539239
2352.454376	340960.035882	38.544256
2354.920945	341455.354300	38.549274
2357.385631	341939.192982	38.554292
2359.831847	342434.176633	38.559309
2362.206424	342904.311701	38.564327
2364.845980	343384.734362	38.569344
2367.225656	343861.081374	38.574362
2369.883613	344315.673328	38.579380
2372.039310	344763.054930	38.584397
2374.645376	345195.535105	38.589415
2377.306257	345635.289696	38.594432
2379.220653	346078.104200	38.599450
2382.055441	346510.842927	38.604468
2383.906431	346943.302681	38.609485
2386.757848	347377.961606	38.614503
2389.556164	347826.740711	38.619520
2391.000052	348272.633664	38.624538
2394.021266	348700.984895	38.629556
2395.893722	349145.711301	38.634573
2398.231301	349584.623150	38.639591
2400.664022	350043.672793	38.644608
2402.540433	350502.629008	38.649626
2405.442885	350953.396937	38.654644
2407.752519	351413.622168	38.659661
2409.788410	351883.736189	38.664679
2412.139577	352340.088299	38.669696
2414.378470	352819.934973	38.674714
2417.150175	353288.066803	38.679732
2419.753190	353768.024760	38.684749
2421.962766	354238.597806	38.689767
2424.530180	354709.338302	38.694784
2426.794945	355185.452931	38.699802
2429.486121	355666.318339	38.704820
2431.944008	356157.800806	38.709837
2434.399592	356633.414663	38.714855
2436.812407	357113.091953	38.719872
2439.068601	357608.196402	38.724890
2441.724126	358078.916732	38.729908
2444.911212	358556.934393	38.734925
2447.894658	359028.228172	38.739943
2450.523265	359477.948814	38.744960
2453.169423	359956.342958	38.749978
2455.787198	360405.092171	38.754996
2458.672811	360875.774207	38.760013
2461.205007	361331.457103	38.765031
2463.923778	361780.456489	38.770048
2466.101477	362232.227552	38.775066
2469.113996	362672.796533	38.780084
2471.677642	363123.178078	38.785101
2474.033886	363556.127344	38.790119
2476.709583	363999.325702	38.795136
2479.170139	364449.355291	38.800154
2481.894693	364865.737790	38.805172
2484.399502	365307.833843	38.810189
2487.231768	365734.926175	38.815207
2489.948438	366158.505278	38.820224
2492.212302	366580.172668	38.825242
2495.069035	367013.745489	38.830260
2497.354611	367433.396543	38.835277
2499.904781	367853.661475	38.840295
2502.558395	368277.230293	38.845312
2505.095773	368675.640336	38.850330
2507.928650	369055.475533	38.855348
2510.632356	369441.671773	38.860365
2512.477258	369810.542305	38.865383
2515.285019	370185.397944	38.870400
2517.212988	370562.140538	38.875418
2519.777959	370938.017652	38.880436
2521.865990	371320.158374	38.885453
2524.255390	371721.912980	38.890471
2526.839846	372106.759111	38.895488
2529.126335	372500.834230	38.900506
2531.838444	372893.188929	38.905524
2534.439319	373286.648599	38.910541
2536.792822	373689.201910	38.915559
2539.344067	374092.760256	38.920576
2541.626568	374495.113950	38.925594
2544.159279	374901.179161	38.930612
2546.637542	375320.797642	38.935629
2548.964963	375735.615032	38.940647
2551.710393	376154.066200	38.945664
2554.025292	376592.396183	38.950682
2556.431576	377014.697793	38.955700
2558.790632	377445.247903	38.960717
2560.870744	377898.138159	38.965735
2563.904674	378321.671095	38.970752
2566.568922	378782.044370	38.975770
2568.966959	379227.258025	38.980788
2571.230383	379670.027102	38.985805
2573.568816	380129.751122	38.990823
2575.871481	380585.999836	38.995840
2578.273145	381068.052494	39.000858
2580.924549	381532.048210	39.005876
2583.627969	382010.210632	39.010893
2586.182119	382479.258403	39.015911
2588.933645	382956.893926	39.020928
2591.351486	383438.685667	39.025946
2593.855360	383935.195513	39.030964
2596.640181	384416.003363	39.035981
2599.257935	384902.716321	39.040999
2602.488970	385384.328754	39.046016
2604.757790	385863.195657	39.051034
2608.037817	386345.497967	39.056052
2610.534711	386828.628140	39.061069
2612.798825	387307.324674	39.066087
2615.470025	387787.041056	39.071104
2618.658194	388273.973863	39.076122
2621.187975	388755.322995	39.081140
2624.015066	389233.930110	39.086157
2626.395771	389708.391318	39.091175
2629.392273	390192.944220	39.096192
2631.806148	390672.561112	39.101210
2634.600167	391153.303248	39.106228
2637.101516	391639.309507	39.111245
2639.788323	392121.932010	39.116263
2642.310811	392597.422209	39.121280
2645.282613	393068.498158	39.126298
2647.931965	393518.975961	39.131316
2650.486271	393957.188978	39.136333
2652.499035	394412.827697	39.141351
2655.344711	394851.185964	39.146368
2658.142472	395300.069866	39.151386
2660.838211	395743.486632	39.156404
2663.597304	396192.111206	39.161421
2666.359843	396643.772113	39.166439
2669.145673	397091.011113	39.171456
2671.738328	397550.293742	39.176474
2673.983006	398001.156111	39.181492
2676.860963	398461.065549	39.186509
2678.769833	398925.939571	39.191527
2681.894311	399385.594190	39.196544
2684.364803	399855.766744	39.201562
2686.760020	400335.173461	39.206580
2689.795333	400809.629103	39.211597
2692.199360	401299.719573	39.216615
2695.161826	401771.054091	39.221632
2697.544372	402256.164109	39.226650
2700.411015	402754.779094	39.231668
2703.624452	403238.779198	39.236685
2705.826390	403728.915086	39.241703
2709.021175	404214.373615	39.246720
2711.628665	404710.260848	39.251738
2714.531609	405197.093985	39.256756
2717.546233	405686.335465	39.261773
2720.182962	406185.946449	39.266791
2723.034429	406670.660623	39.271808
2726.025622	407171.213537	39.276826
2728.544557	407657.942039	39.281844
2731.537233	408144.511757	39.286861
2734.025828	408635.285209	39.291879
2736.773626	409136.807680	39.296896
2739.799792	409627.606708	39.301914
2742.190866	410136.950572	39.306932
2745.433517	410620.424688	39.311949
2747.999298	411128.532791	39.316967
2750.973803	411620.726745	39.321984
2753.977593	412127.101022	39.327002
2756.359175	412617.319377	39.332020
2759.286621	413113.246946	39.337037
2762.269131	413609.436210	39.342055
2764.681986	414097.141271	39.347072
2767.252002	414607.621737	39.352090
2769.988846	415119.333945	39.357108
2773.192759	415600.375608	39.362125
2776.069884	416110.299489	39.367143
2778.869542	416608.848515	39.372160
2781.912616	417096.960731	39.377178
2784.625832	417602.854868	39.382196
2787.678294	418092.671675	39.387213
2790.096488	418599.456315	39.392231
2793.120577	419090.349936	39.397248
2795.962678	419576.728256	39.402266
2798.211003	420048.825574	39.407284
2801.382340	420501.740401	39.412301
2803.537613	420966.615764	39.417319
2806.303453	421440.026487	39.422336
2808.965924	421904.805850	39.427354
2811.688861	422383.679825	39.432372
2814.392857	422845.447143	39.437389
2816.823720	423330.076639	39.442407
2819.643939	423816.485330	39.447424
2822.197227	424298.747490	39.452442
2824.311167	424815.498848	39.457460
2827.320824	425306.892230	39.462477
2830.263367	425823.999816	39.467495
2832.956173	426349.243238	39.472512
2835.825383	426855.677770	39.477530
2838.390887	427380.313142	39.482548
2841.355962	427906.445424	39.487565
2843.820777	428436.040675	39.492583
2846.904579	428969.884024	39.497600
2850.021244	429503.103454	39.502618
2852.976950	430036.312196	39.507636
2856.294128	430567.198664	39.512653
2859.265457	431115.326404	39.517671
2861.882164	431650.556640	39.522688
2864.605690	432190.697551	39.527706
2867.995321	432731.152267	39.532724
2871.036828	433263.951805	39.537741
2873.799886	433808.661668	39.542759
2876.312207	434358.489766	39.547776
2879.472325	434902.480296	39.552794
2882.360382	435453.086232	39.557812
2885.609042	435997.140505	39.562829
2888.854132	436535.410148	39.567847
2891.516046	437075.457074	39.572864
2894.624546	437613.320018	39.577882
2897.585417	438164.234739	39.582900
2900.847018	438701.239673	39.587917
2903.707011	439240.398014	39.592935
2906.895964	439777.618922	39.597952
2909.807112	440316.239235	39.602970
2912.367326	440865.739203	39.607988
2915.281739	441401.499527	39.613005
2918.463741	441952.851330	39.618023
2921.157380	442498.040159	39.623040
2924.324619	443044.306258	39.628058
2927.196114	443594.555884	39.633076
2930.152086	444135.210757	39.638093
2933.063915	444701.325936	39.643111
2935.921604	445237.566853	39.648128
2939.138826	445783.560032	39.653146
2941.628355	446336.641867	39.658164
2944.745796	446879.233764	39.663181
2947.226780	447438.517701	39.668199
2949.940873	448009.697796	39.673216
2952.744992	448549.668411	39.678234
2955.409882	449076.639766	39.683252
2958.461100	449604.297300	39.688269
2961.002976	450132.175260	39.693287
2963.985254	450668.828998	39.698304
2967.172125	451192.683329	39.703322
2970.393479	451718.544735	39.708340
2973.260861	452238.275537	39.713357
2976.061381	452786.397151	39.718375
2978.977128	453315.509139	39.723392
2981.884333	453857.666832	39.728410
2984.648517	454404.489919	39.733428
2987.671743	454949.841823	39.738445
2990.569686	455508.863297	39.743463
2993.633907	456067.237289	39.748480
2996.642259	456621.608675	39.753498
2999.686108	457189.673193	39.758516
3002.659130	457746.805098	39.763533
3005.678654	458317.323887	39.768551
3008.694403	458894.304793	39.773568
3011.484286	459466.702185	39.778586
3014.288783	460052.944866	39.783604
3018.163512	460632.122004	39.788621
3020.696526	461210.585371	39.793639
3023.568989	461805.623461	39.798656
3027.281848	462381.137115	39.803674
3030.065093	462969.277326	39.808692
3033.128188	463554.777342	39.813709
3036.331727	464154.301397	39.818727
3038.949136	464745.909364	39.823744
3042.269199	465342.296078	39.828762
3045.478354	465939.341113	39.833780
3048.572065	466533.201152	39.838797
3051.642863	467135.443799	39.843815
3054.540199	467736.735711	39.848832
3058.142966	468340.629755	39.853850
3060.955062	468952.267809	39.858868
3063.924146	469561.081681	39.863885
3067.326172	470152.716828	39.868903
3070.260845	470767.922981	39.873920
3073.795164	471361.575856	39.878938
3076.731728	471970.374444	39.883956
3080.183093	472557.078497	39.888973
3083.411380	473165.694257	39.893991
3085.997228	473760.691616	39.899008
3089.418257	474366.662377	39.904026
3092.777762	474974.647023	39.909044
3096.027038	475558.262900	39.914061
3099.437920	476153.564892	39.919079
3102.389371	476744.523793	39.924096
3105.798533	477333.876297	39.929114
3108.720984	477933.095033	39.934132
3112.292814	478518.191116	39.939149
3115.265088	479097.602418	39.944167
3118.021540	479695.378831	39.949184
3121.388879	480248.561910	39.954202
3124.380557	480808.359352	39.959220
3127.250628	481350.875003	39.964237
3130.578836	481890.624533	39.969255
3133.713239	482430.490843	39.974272
3136.619591	482964.364340	39.979290
3139.529930	483509.946734	39.984308
3142.653735	484052.346863	39.989325
3146.192096	484600.123693	39.994343
3148.818395	485156.669990	39.999360
3152.221454	485699.838518	40.004378
3155.150395	486259.387225	40.009396
3158.312157	486820.499557	40.014413
3161.734783	487381.048831	40.019431
3164.610014	487951.722338	40.024448
3167.879631	488507.361688	40.029466
3170.914673	489083.836311	40.034484
3173.980089	489649.073221	40.039501
3177.331867	490221.168739	40.044519
3180.189043	490807.772583	40.049536
3183.360113	491387.893018	40.054554
3186.864807	491976.428779	40.059572
3189.636478	492571.880819	40.064589
3192.887847	493161.833317	40.069607
3195.779962	493757.834227	40.074624
3199.238423	494353.271725	40.079642
3202.278185	494966.634785	40.084660
3206.209440	495559.079576	40.089677
3209.570062	496147.454251	40.094695
3212.840192	496756.428119	40.099712
3216.326875	497347.016516	40.104730
3219.701980	497951.691787	40.109748
3223.025965	498548.831173	40.114765
3226.338495	499149.588061	40.119783
3229.162225	499754.542427	40.124800
3232.665896	500340.889624	40.129818
3235.888125	500945.791161	40.134836
3239.122458	501548.246894	40.139853
3242.610122	502145.391735	40.144871
3245.928193	502760.616110	40.149888
3249.527910	503348.464249	40.154906
3252.859517	503951.024668	40.159924
3255.898087	504558.103260	40.164941
3259.174357	505145.740474	40.169959
3262.314596	505752.912957	40.174976
3265.982370	506348.422681	40.179994
3269.526210	506953.672439	40.185012
3272.950684	507536.814514	40.190029
3277.102747	508108.365793	40.195047
3280.327299	508691.298603	40.200064
3283.893244	509256.091581	40.205082
3287.092660	509835.103815	40.210100
3290.144708	510416.087717	40.215117
3293.712913	510969.671981	40.220135
3296.987360	511548.311479	40.225152
3300.623023	512082.624631	40.230170
3303.513585	512618.552345	40.235188
3306.755886	513136.496841	40.240205
3310.304371	513643.681422	40.245223
3312.997669	514170.913426	40.250240
3316.479375	514683.626609	40.255258
3319.699935	515199.039034	40.260276
3322.679628	515721.737682	40.265293
3325.516455	516254.026723	40.270311
3328.437254	516796.121549	40.275328
3331.917778	517346.281438	40.280346
3334.964654	517899.517887	40.285364
3338.224606	518454.719585	40.290381
3341.187176	519016.960015	40.295399
3344.155162	519589.720851	40.300416
3347.296972	520169.343282	40.305434
3350.718736	520749.354795	40.310452
3353.777780	521346.699678	40.315469
3356.914560	521939.673758	40.320487
3360.383893	522550.574920	40.325504
3363.573519	523157.463512	40.330522
3366.985827	523768.882335	40.335540
3370.340698	524383.513801	40.340557
3374.265008	524990.519761	40.345575
3377.387590	525621.878695	40.350592
3381.106865	526231.491567	40.355610
3384.327209	526856.081451	40.360628
3387.755532	527481.017218	40.365645
3390.982837	528115.839788	40.370663
3394.453321	528745.356430	40.375680
3397.729300	529379.616533	40.380698
3401.345812	530017.980491	40.385716
3404.743293	530676.461974	40.390733
3408.560815	531297.858725	40.395751
3411.994687	531945.697873	40.400768
3415.323267	532579.568182	40.405786
3418.960380	533225.054335	40.410804
3422.639204	533880.433411	40.415821
3426.253742	534499.819539	40.420839
3429.741597	535164.797971	40.425856
3433.159293	535804.870357	40.430874
3436.663273	536423.289674	40.435892
3440.412062	537066.279828	40.440909
3444.425898	537706.682264	40.445927
3447.816507	538334.714121	40.450944
3451.397231	538972.310835	40.455962
3455.016845	539596.929785	40.460980
3458.828485	540217.513605	40.465997
3462.434685	540838.456908	40.471015
3465.162121	541473.061007	40.476032
3468.907961	542088.944674	40.481050
3472.446429	542717.878617	40.486068
3475.954680	543342.208426	40.491085
3479.460688	543947.025336	40.496103
3483.097053	544583.166446	40.501120
3486.570676	545176.377489	40.506125
3490.400125	545738.701634	40.511130
3493.071927	546246.219866	40.516135
3496.665707	546694.016088	40.521140
3499.965960	547076.786299	40.526144
3502.936867	547393.027087	40.531149
3505.499729	547659.006650	40.536154
3507.707620	547857.307301	40.541159
3510.690321	548012.129887	40.546164
3512.537169	548105.104243	40.551168
3514.251017	548151.617445	40.556173
3516.384430	548155.721057	40.561178
3517.674045	548120.037247	40.566183
3519.436744	548031.488028	40.571188
3520.362939	547915.816959	40.576192
3521.173769	547757.970327	40.581197
3522.913139	547579.383272	40.586202
3523.222072	547372.049550	40.591207
3524.099089	547129.141234	40.596212
3524.649123	546881.182803	40.601216
3524.951119	546602.318865	40.606221
3525.758373	546309.590149	40.611226
3525.821117	546008.998060	40.616231
3526.268258	545690.773092	40.621236
3526.644564	545365.838871	40.626240
3527.045193	545014.190091	40.631245
3526.896237	544661.206357	40.636250
3526.826700	544305.728071	40.641255
3526.730599	543943.935103	40.646260
3527.044681	543577.070583	40.651264
3527.256807	543195.218938	40.656269
3527.186852	542823.903366	40.661274
3527.389766	542435.419984	40.666279
3527.056965	542044.234253	40.671284
3526.793800	541657.773447	40.676288
3526.523375	541267.113000	40.681293
3526.453600	540883.176814	40.686298
3526.302352	540510.554515	40.691303
3526.397465	540113.090596	40.696308
3526.135161	539734.205187	40.701312
3525.802575	539349.362576	40.706317
3525.514367	538962.533686	40.711322
3525.148548	538592.574548	40.716327
3524.968300	538220.506490	40.721332
3524.602488	537846.741540	40.726336
3524.243413	537478.925917	40.731341
3524.084503	537116.978994	40.736346
3523.676617	536762.941949	40.741351
3523.590455	536401.320150	40.746356
3523.250934	536061.852981	40.751360
3523.167428	535701.274960	40.756365
3522.790736	535348.766176	40.761370
3522.647161	535013.639418	40.766375
3522.333567	534674.491127	40.771380
3521.774140	534351.488519	40.776384
3521.415144	534009.554476	40.781389
3521.447929	533689.121810	40.786394
3520.919482	533374.934422	40.791399
3520.704087	533041.898052	40.796404
3520.330814	532731.108423	40.801408
3519.906473	532418.198762	40.806413
3519.866403	532122.955409	40.811418
3519.453664	531835.545924	40.816423
3519.941871	531529.496955	40.821428
3519.291174	531249.793966	40.826432
3519.287992	530946.489068	40.831437
3518.652185	530658.486891	40.836442
3518.236199	530386.462023	40.841447
3518.412503	530112.418760	40.846452
3517.842129	529835.507464	40.851456
3517.582818	529567.132324	40.856461
3517.269903	529300.479149	40.861466
3516.815713	529053.096539	40.866471
3516.866940	528788.347923	40.871476
3516.531395	528550.287289	40.876480
3516.558446	528309.184240	40.881485
3516.445430	528049.098385	40.886490
3515.727091	527826.955450	40.891495
3515.320729	527581.866946	40.896500
3515.445133	527348.769269	40.901504
3515.245036	527138.916514	40.906509
3514.937189	526921.295028	40.911514
3514.660342	526698.510630	40.916519
3514.213906	526479.944763	40.921524
3514.389019	526278.967027	40.926528
3513.874005	526067.077747	40.931533
3513.776468	525866.845494	40.936538
3513.369758	525674.241022	40.941543
3513.161388	525479.783325	40.946548
3512.844013	525295.297675	40.951552
3512.412261	525108.654557	40.956557
3512.543322	524930.715199	40.961562
3512.295746	524753.541344	40.966567
3512.625002	524573.645975	40.971572
3512.253335	524409.983806	40.976576
3511.923138	524241.764156	40.981581
3512.076545	524077.156326	40.986586
3511.833585	523909.778739	40.991591
3511.617574	523740.524846	40.996596
3511.499401	523583.284486	41.001600
3511.496203	523413.993541	41.006605
3511.182195	523265.273423	41.011610
3510.742909	523125.215933	41.016615
3510.845415	522960.453114	41.021620
3510.581996	522813.945113	41.026624
3510.427893	522683.595238	41.031629
3510.684574	522531.947278	41.036634
3510.253345	522401.537822	41.041639
3510.268834	522257.457823	41.046644
3510.318748	522133.744362	41.051648
3510.049704	521984.044857	41.056653
3509.802006	521865.027385	41.061658
3509.701895	521730.465280	41.066663
3509.708077	521605.238053	41.071668
3509.574953	521479.526317	41.076672
3509.324763	521357.320500	41.081677
3509.363956	521219.445997	41.086682
3509.080733	521114.989007	41.091687
3509.451627	520993.289003	41.096692
3509.178324	520874.116667	41.101696
3508.992580	520756.244140	41.106701
3508.783592	520639.385607	41.111706
3508.709367	520542.880186	41.116711
3508.744720	520422.543488	41.121716
3508.401549	520312.327083	41.126720
3508.359219	520211.517102	41.131725
3508.662135	520101.601662	41.136730
3508.150158	519999.499465	41.141735
3508.429927	519887.917752	41.146740
3508.318497	519797.430566	41.151744
3508.310465	519688.673843	41.156749
3508.466202	519584.188278	41.161754
3507.775861	519506.583110	41.166759
3508.016253	519380.240037	41.171764
3508.006095	519297.824088	41.176768
3507.894186	519209.963003	41.181773
3507.773219	519107.641780	41.186778
3507.370851	519010.167932	41.191783
3507.472701	518930.007803	41.196788
3507.373593	518846.187861	41.201792
3507.276486	518752.052042	41.206797
3507.201106	518671.868099	41.211802
3507.051705	518594.577662	41.216807
3507.600582	518498.669676	41.221812
3507.099019	518420.068811	41.226816
3507.084204	518347.559663	41.231821
3507.432602	518254.867576	41.236826
3507.082604	518179.073304	41.241831
3507.214199	518105.781467	41.246836
3506.616083	518023.047525	41.251840
3506.716820	517946.473026	41.256845
3507.234831	517866.292537	41.261850
3507.011645	517802.309197	41.266855
3507.521276	517714.240795	41.271860
3507.236423	517636.967283	41.276864
3506.929897	517552.313899	41.281869
3507.313394	517469.776049	41.286874
3506.782036	517396.737540	41.291879
3506.904885	517322.128834	41.296884
3506.898696	517238.134348	41.301888
3506.719780	517162.814076	41.306893
3506.484621	517096.705994	41.311898
3506.476443	517031.876591	41.316903
3506.869567	516950.902299	41.321908
3506.982328	516873.208406	41.326912
3506.477306	516801.123944	41.331917
3506.909191	516730.458804	41.336922
3506.808060	516653.505672	41.341927
3506.733846	516583.273878	41.346932
3506.528741	516517.866737	41.351936
3506.302992	516445.736602	41.356941
3506.434241	516373.600312	41.361946
3506.396040	516316.257467	41.366951
3506.248349	516247.148446	41.371956
3506.484927	516175.348657	41.376960
3506.099051	516116.239463	41.381965
3506.412471	516045.185558	41.386970
3505.911073	515998.332778	41.391975
3506.112957	515930.330377	41.396980
3505.935057	515867.091020	41.401984
3506.059775	515813.715984	41.406989
3506.151834	515740.470534	41.411994
3506.087922	515687.883507	41.416999
3505.853817	515630.316393	41.422004
3506.016050	515568.235929	41.427008
3505.694593	515509.063830	41.432013
3505.954214	515455.868630	41.437018
3505.949516	515395.584009	41.442023
3505.964506	515333.020194	41.447028
3506.142441	515269.317746	41.452032
3505.918264	515212.860275	41.457037
3506.090498	515150.827257	41.462042
3506.034878	515101.827927	41.467047
3505.624028	515033.058919	41.472052
3505.777087	514988.679247	41.477056
3505.664499	514930.989371	41.482061
3505.808117	514872.095556	41.487066
3505.589234	514815.534756	41.492071
3505.734453	514752.948195	41.497076
3505.354083	514705.769204	41.502080
3505.380302	514661.661594	41.507085
3505.847482	514599.579928	41.512090
3505.695900	514557.270336	41.517095
3505.774860	514504.505283	41.522100
3505.593241	514431.701975	41.527104
3505.198711	514386.345114	41.532109
3505.593892	514338.030979	41.537114
3505.108643	514299.971424	41.542119
3505.109925	514252.477958	41.547124
3505.062331	514201.451606	41.552128
3504.864866	514167.544265	41.557133
3505.237881	514112.910695	41.562138
3505.113966	514082.835525	41.567143
3504.891240	514033.050223	41.572148
3505.255792	513991.871534	41.577152
3505.418566	513938.787988	41.582157
3505.312436	513902.033253	41.587162
3505.238458	513846.963665	41.592167
3505.293705	513806.693249	41.597172
3504.978603	513741.697273	41.602176
3505.031632	513713.970724	41.607181
3505.679994	513668.396542	41.612186
3504.841047	513627.255406	41.617191
3504.723055	513577.755685	41.622196
3505.233317	513534.630811	41.627200
3505.182194	513496.551412	41.632205
3505.297471	513452.730041	41.637210
3505.100657	513417.202510	41.642215
3505.449440	513353.364640	41.647220
3505.268046	513311.258947	41.652224
3505.176629	513263.929085	41.657229
3505.293328	513221.118508	41.662234
3505.352738	513171.690725	41.667239
3505.345566	513122.121574	41.672244
3505.380725	513077.452004	41.677248
3505.137650	513034.748389	41.682253
3505.444167	512992.514218	41.687258
3505.206045	512945.156063	41.692263
3505.296447	512901.337191	41.697268
3505.467224	512847.844292	41.702272
3505.208711	512809.846700	41.707277
3505.093455	512759.686577	41.712282
3505.279370	512725.058177	41.717287
3505.354501	512669.860019	41.722292
3505.554103	512635.077523	41.727296
3505.093033	512582.240044	41.732301
3505.135736	512539.439434	41.737306
3505.001443	512489.939102	41.742311
3505.053990	512449.008292	41.747316
3504.958096	512396.112524	41.752320
3504.848977	512368.004721	41.757325
3504.944894	512319.630937	41.762330
3504.988743	512276.677731	41.767335
3504.782707	512246.258177	41.772340
3504.923853	512200.608447	41.777344
3504.648098	512166.254197	41.782349
3504.955700	512115.721838	41.787354
3504.639710	512087.545091	41.792359
3504.745004	512050.297656	41.797364
3505.000771	512018.135422	41.802368
3504.732984	511983.425449	41.807373
3504.821703	511935.506971	41.812378
3504.935814	511910.549989	41.817383
3504.625900	511856.067634	41.822388
3504.941948	511829.156381	41.827392
3504.824497	511788.655524	41.832397
3505.254247	511751.609089	41.837402
3504.965957	511707.745804	41.842407
3505.023932	511667.773381	41.847412
3505.328984	511623.006741	41.852416
3504.824925	511585.905167	41.857421
3505.107676	511532.491597	41.862426
3504.917294	511502.422339	41.867431
3505.026788	511451.211103	41.872436
3504.921555	511420.065928	41.877440
3504.864462	511385.017917	41.882445
3505.108940	511327.208713	41.887450
3504.740885	511298.431841	41.892455
3505.017734	511253.011056	41.897460
3504.961067	511209.716927	41.902464
3504.624609	511188.168839	41.907469
3504.972457	511131.759078	41.912474
3504.633934	511094.023222	41.917479
3504.922025	511061.651723	41.922484
3504.755378	511012.405134	41.927488
3504.887489	510977.275797	41.932493
3504.730527	510937.740328	41.937498
3504.559475	510904.985796	41.942503
3504.735339	510877.032844	41.947508
3504.862009	510827.031134	41.952512
3504.553178	510798.142880	41.957517
3504.524381	510764.556184	41.962522
3504.602585	510733.836063	41.967527
3504.480030	510695.053422	41.972532
3504.336925	510657.639838	41.977536
3504.415411	510633.141913	41.982541
3504.623994	510590.765485	41.987546
3504.389455	510572.185262	41.992551
3504.620638	510538.000558	41.997556
3504.615647	510497.478858	42.002560
3504.608617	510466.063475	42.007565
3504.419834	510443.074604	42.012570
3504.314477	510411.168763	42.017575
3504.194694	510384.020567	42.022580
3504.324951	510351.065588	42.027584
3504.251950	510324.921699	42.032589
3504.500708	510282.791109	42.037594
3504.192752	510264.930411	42.042599
3504.211932	510222.937132	42.047604
3504.378341	510204.242558	42.052608
3504.257341	510172.288153	42.057613
3504.453175	510148.276891	42.062618
3504.234262	510119.322688	42.067623
3504.451005	510084.532275	42.072628
3504.519354	510056.392609	42.077632
3504.197000	510038.179816	42.082637
3504.617478	509987.623314	42.087642
3504.439401	509958.864750	42.092647
3504.268422	509938.351339	42.097652
3504.385167	509904.335226	42.102656
3504.444966	509870.783365	42.107661
3504.225496	509845.521939	42.112666
3504.409945	509814.378647	42.117671
3504.548354	509780.156499	42.122676
3504.409325	509745.118070	42.127680
3504.439761	509721.537080	42.132685
3504.388815	509685.725736	42.137690
3504.093150	509674.894721	42.142695
3504.322521	509634.586902	42.147700
3504.548639	509601.109414	42.152704
3504.282635	509587.136956	42.157709
3504.460849	509551.187934	42.162714
3504.144446	509521.742205	42.167719
3504.397962	509496.152559	42.172724
3504.639091	509464.949084	42.177728
3504.707528	509432.558624	42.182733
3504.597360	509387.042267	42.187738
3504.749181	509352.766555	42.192743
3504.485341	509320.630763	42.197748
3504.662458	509281.595192	42.202752
3504.411384	509256.084926	42.207757
3504.572223	509217.962456	42.212762
3504.302102	509191.544429	42.217767
3504.351163	509155.260836	42.222772
3504.444981	509135.716485	42.227776
3504.361703	509098.543006	42.232781
3504.291256	509058.078840	42.237786
3504.500772	509037.403036	42.242791
3504.538522	509001.475061	42.247796
3504.701799	508968.208646	42.252800
3504.585077	508940.855304	42.257805
3504.583641	508916.165180	42.262810
3504.405569	508874.098582	42.267815
3504.503370	508848.836144	42.272820
3504.737013	508806.805509	42.277824
3504.056942	508788.445537	42.282829
3504.543772	508744.705127	42.287834
3504.149045	508733.231442	42.292839
3504.313075	508692.172822	42.297844
3504.366922	508667.321821	42.302848
3504.233520	508637.693873	42.307853
3504.346313	508605.547819	42.312858
3504.237392	508576.826605	42.317863
3504.288013	508552.431302	42.322868
3504.490664	508521.889934	42.327872
3504.171047	508494.466755	42.332877
3504.189048	508458.692554	42.337882
3504.308455	508443.443972	42.342887
3504.292692	508413.544071	42.347892
3504.476250	508378.047113	42.352896
3504.158742	508352.495409	42.357901
3504.354483	508317.856527	42.362906
3504.339716	508288.664591	42.367911
3504.125469	508257.075528	42.372916
3504.188890	508231.969407	42.377920
3504.271708	508216.422831	42.382925
3504.407544	508182.299104	42.387930
3504.167055	508154.053340	42.392935
3504.088254	508137.014347	42.397940
3504.573388	508103.442421	42.402944
3504.061166	508075.239469	42.407949
3504.501961	508040.763693	42.412954
3504.311622	508021.718351	42.417959
3503.985342	507985.390415	42.422964
3504.332407	507956.444319	42.427968
3503.924218	507951.752204	42.432973
3504.025312	507906.299740	42.437978
3504.315014	507880.347800	42.442983
3504.065541	507855.897741	42.447988
3503.997527	507831.064793	42.452992
3503.967500	507809.160444	42.457997
3504.069516	507785.110115	42.463002
3503.927188	507767.423032	42.468007
3503.825847	507741.785665	42.473012
3503.989876	507708.010728	42.478016
3503.850260	507685.263382	42.483021
3504.223404	507666.836970	42.488026
3504.115738	507646.665002	42.493031
3504.134958	507625.511603	42.498036
3504.168652	507587.810404	42.503040
3503.880703	507581.125870	42.508045
3504.204493	507545.959228	42.513050
3504.099308	507532.162078	42.518055
3504.112411	507496.842041	42.523060
3504.194138	507466.166122	42.528064
3504.166961	507442.793511	42.533069
3504.196894	507414.908591	42.538074
3504.065233	507404.809201	42.543079
3503.531048	507383.287573	42.548084
3504.065464	507354.209667	42.553088
3504.028458	507334.329761	42.558093
3504.113475	507309.117690	42.563098
3504.119425	507277.036649	42.568103
3503.650843	507267.901199	42.573108
3503.936900	507224.036876	42.578112
3503.730861	507223.714720	42.583117
3503.850093	507199.863254	42.588122
3503.821757	507189.646212	42.593127
3503.835464	507154.679576	42.598132
3503.692592	507136.232946	42.603136
3503.661871	507113.164045	42.608141
3503.516920	507106.102534	42.613146
3503.697963	507081.380950	42.618151
3503.760604	507071.706055	42.623156
3503.714522	507047.526309	42.628160
3503.551622	507024.275779	42.633165
3503.587214	507012.834144	42.638170
3503.944888	507002.960789	42.643175
3504.137658	506974.088035	42.648180
3504.073279	506964.331954	42.653184
3503.778779	506933.056750	42.658189
3504.205013	506904.804785	42.663194
3504.112960	506885.995660	42.668199
3503.857184	506870.147183	42.673204
3504.336781	506825.644069	42.678208
3504.056571	506805.650189	42.683213
3504.176888	506779.520968	42.688218
3504.091514	506768.958491	42.693223
3504.178537	506732.157809	42.698228
3504.486684	506706.757802	42.703232
3503.967481	506692.620605	42.708237
3504.100539	506655.104078	42.713242
3504.384059	506634.717313	42.718247
3504.035676	506617.314620	42.723252
3504.200569	506585.713190	42.728256
3504.134241	506564.976822	42.733261
3504.491217	506530.511292	42.738266
3503.980766	506505.645159	42.743271
3504.093004	506466.107475	42.748276
3504.355349	506439.803496	42.753280
3504.059986	506425.984917	42.758285
3504.185663	506399.651874	42.763290
3503.944288	506367.051621	42.768295
3503.440887	506360.957276	42.773300
3504.030599	506328.529225	42.778304
3503.940922	506301.369840	42.783309
3504.073688	506294.061705	42.788314
3503.744725	506272.253256	42.793319
3504.140414	506250.380867	42.798324
3504.449284	506218.503010	42.803329
3503.902000	506198.145819	42.808333
3504.260627	506159.276928	42.813338
3504.407810	506134.559350	42.818343
3504.300073	506116.713310	42.823348
3504.353120	506073.439530	42.828353
3504.245437	506059.945216	42.833357
3504.421256	506015.589243	42.838362
3504.065987	506001.020755	42.843367
3503.921892	505967.645343	42.848372
3504.419395	505939.076936	42.853377
3504.080919	505929.464793	42.858381
3504.124847	505887.659470	42.863386
3504.133295	505872.375561	42.868391
3503.914928	505856.216630	42.873396
3504.345852	505836.058652	42.878401
3504.088846	505807.508056	42.883405
3504.031664	505784.947604	42.888410
3503.701326	505757.622988	42.893415
3503.819342	505738.779425	42.898420
3504.062370	505708.176122	42.903425
3503.876458	505700.159049	42.908429
3503.994210	505675.698488	42.913434
3504.115606	505648.251712	42.918439
3503.996153	505627.573226	42.923444
3504.183338	505597.029156	42.928449
3503.941020	505575.357951	42.933453
3503.871229	505540.553077	42.938458
3503.650129	505526.317215	42.943463
3503.579691	505498.192064	42.948468
3504.046811	505481.772648	42.953473
3503.798675	505469.868796	42.958477
3503.819554	505440.818250	42.963482
3504.205332	505425.727342	42.968487
3504.012782	505397.368305	42.973492
3504.207131	505374.969992	42.978497
3504.006102	505346.156773	42.983501
3504.065253	505321.502559	42.988506
3504.110198	505295.889071	42.993511
3503.959529	505278.808025	42.998516
3504.208638	505251.340443	43.003521
3504.022802	505233.708259	43.008525
3503.822143	505206.868334	43.013530
3504.188256	505191.173075	43.018535
3503.738376	505164.473679	43.023540
3503.743837	505145.799078	43.028545
3503.839991	505128.729486	43.033549
3503.980759	505101.380000	43.038554
3503.872631	505084.443856	43.043559
3503.691443	505064.837167	43.048564
3503.857777	505045.934617	43.053569
3503.825726	505029.947898	43.058573
3503.623823	505004.676623	43.063578
3503.897462	504987.224608	43.068583
3503.826551	504973.116377	43.073588
3503.706655	504951.526263	43.078593
3503.504057	504933.643398	43.083597
3503.850810	504903.578957	43.088602
3503.649398	504895.614568	43.093607
3503.695784	504872.884756	43.098612
3504.060028	504852.736185	43.103617
3503.625636	504840.254066	43.108621
3503.895167	504809.391974	43.113626
3503.942306	504798.503726	43.118631
3503.670064	504773.091414	43.123636
3503.934178	504763.737643	43.128641
3503.536906	504737.130492	43.133645
3503.711744	504709.775011	43.138650
3503.786984	504698.426804	43.143655
3503.918994	504686.563557	43.148660
3503.850540	504649.732447	43.153665
3504.002181	504627.441140	43.158669
3504.095707	504617.203333	43.163674
3504.001941	504587.056144	43.168679
3504.159304	504557.678925	43.173684
3504.424313	504536.837181	43.178689
3504.378297	504528.392608	43.183693
3504.088558	504485.472707	43.188698
3504.214382	504454.480880	43.193703
3504.146293	504435.462897	43.198708
3504.416055	504397.919920	43.203713
3504.246601	504383.017073	43.208717
3504.060862	504347.823292	43.213722
3504.160893	504327.412229	43.218727
3504.060622	504307.437653	43.223732
3504.231193	504285.598388	43.228737
3503.928576	504271.374386	43.233741
3504.236552	504239.897928	43.238746
3504.087199	504215.123285	43.243751
3503.644744	504197.125748	43.248756
3504.163997	504164.097537	43.253761
3504.069375	504150.447861	43.258765
3503.946806	504130.375392	43.263770
3503.880037	504098.907294	43.268775
3503.857449	504079.982951	43.273780
3504.164864	504059.488196	43.278785
3503.741754	504039.412508	43.283789
3504.144599	504007.009696	43.288794
3503.821867	503982.413948	43.293799
3503.736541	503977.163644	43.298804
3503.817506	503941.623252	43.303809
3503.752114	503928.019393	43.308813
3503.682002	503907.634730	43.313818
3503.658815	503893.416872	43.318823
3503.789856	503860.854308	43.323828
3503.950958	503855.261374	43.328833
3503.621367	503836.941980	43.333837
3503.719460	503807.117394	43.338842
3504.185848	503796.870796	43.343847
3503.812396	503768.689536	43.348852
3503.902834	503753.947521	43.353857
3503.804498	503725.975761	43.358861
3503.815281	503711.904216	43.363866
3503.805878	503681.236050	43.368871
3503.841273	503673.891603	43.373876
3503.888261	503640.430949	43.378881
3503.423281	503630.280827	43.383885
3503.645204	503607.268590	43.388890
3503.904199	503595.536369	43.393895
3503.639608	503569.615010	43.398900
3503.639351	503560.555426	43.403905
3503.811124	503546.711356	43.408909
3503.786362	503516.197158	43.413914
3503.624165	503510.250328	43.418919
3503.640010	503487.877818	43.423924
3503.363374	503464.691133	43.428929
3503.323252	503466.316463	43.433933
3503.431294	503447.067138	43.438938
3503.585299	503420.876971	43.443943
3503.488617	503425.547837	43.448948
3503.798311	503411.732476	43.453953
3503.612303	503384.229517	43.458957
3503.923289	503365.605963	43.463962
3503.446423	503358.899046	43.468967
3503.578326	503338.329969	43.473972
3503.988141	503324.498717	43.478977
3503.647906	503304.257262	43.483981
3503.828846	503273.355866	43.488986
3503.830679	503264.295800	43.493991
3503.241259	503245.409525	43.498996
3503.535730	503224.257910	43.504001
3503.533886	503229.318725	43.509005
3503.535000	503196.016309	43.514010
3503.658602	503188.657720	43.519015
3503.346291	503188.807772	43.524020
3503.865733	503152.639782	43.529025
3503.723880	503136.769913	43.534029
3503.380745	503128.523453	43.539034
3503.214353	503099.802293	43.544039
3503.701935	503080.239535	43.549044
3503.960277	503067.596071	43.554049
3503.427547	503054.014777	43.559053
3503.607872	503027.212536	43.564058
3503.758877	503026.783261	43.569063
3503.486299	503006.631994	43.574068
3503.731177	502978.604812	43.579073
3503.932416	502968.247803	43.584077
3503.669069	502949.309680	43.589082
3503.644214	502927.803283	43.594087
3503.794213	502922.566089	43.599092
3503.769230	502886.686034	43.604097
3503.597944	502877.096401	43.609101
3503.834673	502865.215380	43.614106
3503.736009	502832.990888	43.619111
3503.359792	502837.503638	43.624116
3503.748870	502811.072973	43.629121
3503.731187	502799.282722	43.634125
3503.846442	502776.387484	43.639130
3503.866550	502751.988897	43.644135
3503.573988	502740.900000	43.649140
3503.534000	502731.238927	43.654145
3503.838557	502702.088414	43.659149
3503.482137	502693.388341	43.664154
3503.367838	502683.587150	43.669159
3503.497349	502662.207871	43.674164
3503.666403	502634.748859	43.679169
3503.398010	502643.091143	43.684173
3503.379309	502622.393196	43.689178
3503.893751	502596.650972	43.694183
3503.304399	502590.012148	43.699188
3503.130735	502575.159047	43.704193
3503.297841	502572.500275	43.709197
3503.352468	502555.333526	43.714202
3503.218871	502544.371221	43.719207
3502.992092	502554.579630	43.724212
3503.449229	502531.427599	43.729217
3503.546969	502510.053157	43.734221
3503.316074	502494.196782	43.739226
3503.636938	502482.454046	43.744231
3503.445749	502478.637178	43.749236
3503.560008	502455.033104	43.754241
3503.342969	502453.649724	43.759245
3503.213229	502433.677681	43.764250
3503.387887	502433.194043	43.769255
3502.932065	502410.439190	43.774260
3503.554071	502390.500140	43.779265
3503.408209	502390.522667	43.784269
3503.119425	502388.593878	43.789274
3503.258600	502377.588365	43.794279
3503.077241	502357.928071	43.799284
3503.683233	502344.520571	43.804289
3503.675606	502340.927730	43.809293
3503.786533	502322.688985	43.814298
3503.826272	502297.679313	43.819303
3503.530726	502298.079786	43.824308
3503.860597	502253.689977	43.829313
3503.345997	502241.775428	43.834317
3503.093590	502237.613889	43.839322
3503.194777	502230.967031	43.844327
3503.111435	502217.010396	43.849332
3503.610546	502185.044553	43.854337
3503.362800	502186.804038	43.859341
3503.488381	502176.762204	43.864346
3503.722091	502162.806037	43.869351
3503.128991	502150.448310	43.874356
3503.618475	502136.552930	43.879361
3503.710153	502126.263357	43.884365
3503.491930	502106.406155	43.889370
3503.692160	502087.444464	43.894375
3503.535537	502075.270779	43.899380
3503.675250	502056.166777	43.904385
3503.466372	502044.001327	43.909389
3503.735406	502017.689678	43.914394
3503.580054	502006.123111	43.919399
3503.249040	501991.547456	43.924404
3503.859168	501986.439729	43.929409
3503.497077	501960.683257	43.934413
3503.328029	501946.436268	43.939418
3503.666889	501940.359113	43.944423
3503.374013	501908.214242	43.949428
3503.296809	501894.458840	43.954433
3503.140765	501885.524246	43.959437
3503.362641	501879.364328	43.964442
3503.766977	501876.364278	43.969447
3503.572656	501852.909396	43.974452
3503.902226	501832.408562	43.979457
3503.977624	501819.236360	43.984461
3503.723368	501789.059136	43.989466
3503.735041	501778.073401	43.994471
3503.610625	501755.417177	43.999476
3503.599092	501736.842880	44.004481
3503.508822	501739.083670	44.009485
3503.535607	501708.052060	44.014490
3503.429030	501692.883929	44.019495
3503.318290	501690.673852	44.024500
3503.697346	501667.077500	44.029505
3503.371882	501650.425475	44.034509
3503.755312	501642.367191	44.039514
3503.756092	501633.002767	44.044519
3503.518002	501607.782952	44.049524
3503.936569	501593.037899	44.054529
3503.593045	501575.882506	44.059533
3503.759370	501555.407150	44.064538
3503.943347	501538.269592	44.069543
3503.293794	501522.782197	44.074548
3503.367337	501499.436365	44.079553
3503.555544	501493.939635	44.084557
3503.747075	501482.773448	44.089562
3503.436824	501459.538829	44.094567
3503.831862	501455.426637	44.099572
3503.783515	501435.946763	44.104577
3503.574749	501414.113283	44.109581
3503.281086	501404.694037	44.114586
3503.784843	501380.571444	44.119591
3503.497389	501366.494548	44.124596
3503.507433	501357.027283	44.129601
3503.856042	501338.395657	44.134605
3503.977006	501311.600205	44.139610
3503.623542	501293.990567	44.144615
3503.695809	501276.060553	44.149620
3504.059789	501249.024140	44.154625
3503.848519	501234.783252	44.159629
3503.795319	501208.723794	44.164634
3503.803550	501201.686312	44.169639
3503.705090	501184.036267	44.174644
3503.457676	501167.877617	44.179649
3503.520176	501159.363669	44.184653
3503.567829	501127.112955	44.189658
3503.403295	501123.443430	44.194663
3503.394281	501121.318440	44.199668
3503.634800	501088.176697	44.204673
3503.099794	501076.467053	44.209677
3503.254007	501072.443448	44.214682
3503.711649	501068.473124	44.219687
3503.479581	501045.529308	44.224692
3503.704315	501024.588562	44.229697
3503.796957	501017.588285	44.234701
3503.774728	500995.269262	44.239706
3503.623999	500980.816136	44.244711
3503.568578	500972.371349	44.249716
3503.818147	500942.619239	44.254721
3503.583767	500927.926204	44.259725
3503.364965	500913.382547	44.264730
3503.679839	500883.164464	44.269735
3503.599967	500881.050641	44.274740
3503.406953	500859.416460	44.279745
3503.276446	500852.957554	44.284749
3503.489433	500833.030785	44.289754
3503.577567	500823.044723	44.294759
3503.362925	500816.447248	44.299764
3503.464914	500783.883623	44.304769
3503.366224	500783.999930	44.309773
3503.148805	500775.276946	44.314778
3503.423787	500767.184789	44.319783
3503.252552	500744.534677	44.324788
3503.367969	500737.226986	44.329793
3503.447615	500726.482947	44.334797
3503.694595	500714.902577	44.339802
3503.860644	500693.262070	44.344807
3503.366316	500686.101332	44.349812
3504.028403	500664.331784	44.354817
3503.800375	500645.081911	44.359821
3503.757566	500629.244764	44.364826
3503.536837	500594.504605	44.369831
3503.491976	500584.944371	44.374836
3503.639308	500581.529159	44.379841
3503.728388	500561.874758	44.384845
3503.656397	500540.221064	44.389850
3503.811876	500529.211833	44.394855
3503.548540	500506.778446	44.399860
3503.560450	500486.883066	44.404865
3503.830106	500478.943476	44.409869
3503.447949	500461.742494	44.414874
3503.522479	500436.269143	44.419879
3503.383733	500437.859717	44.424884
3503.579288	500418.694517	44.429889
3503.475025	500410.155946	44.434893
3503.621013	500397.376486	44.439898
3503.684799	500385.014955	44.444903
3503.504529	500353.254429	44.449908
3503.431916	500339.193387	44.454913
3503.494303	500336.550832	44.459917
3503.382628	500308.525170	44.464922
3503.555252	500292.754918	44.469927
3503.754908	500293.026556	44.474932
3503.631863	500253.410889	44.479937
3503.253637	500250.837950	44.484941
3503.476822	500239.210414	44.489946
3503.930831	500227.445156	44.494951
3503.572878	500209.987011	44.499956
3503.355659	500198.429044	44.504961
3503.622498	500191.907107	44.509965
3503.428914	500167.336267	44.514970
3503.474173	500142.828888	44.519975
3503.327159	500145.230702	44.524980
3503.621315	500127.720045	44.529985
3503.408562	500106.543643	44.534989
3503.226444	500099.434568	44.539994
3503.596404	500091.833292	44.544999
3503.251990	500077.612519	44.550004
3503.521953	500052.107737	44.555009
3503.231633	500036.359798	44.560013
3503.639089	500040.344449	44.565018
3503.555955	500020.058614	44.570023
3503.459863	500003.571277	44.575028
3503.632262	499988.458848	44.580033
3503.693269	499985.057164	44.585037
3503.441300	499956.800023	44.590042
3503.421476	499940.654914	44.595047
3503.385827	499941.520562	44.600052
3503.194426	499916.493454	44.605057
3503.202489	499908.443091	44.610061
3503.293951	499885.497276	44.615066
3503.569593	499892.236270	44.620071
3503.612288	499884.281664	44.625076
3503.766794	499854.795868	44.630081
3503.649244	499844.538043	44.635085
3503.132562	499837.684215	44.640090
3503.466309	499812.118392	44.645095
3503.331271	499806.824088	44.650100
3503.468836	499800.474299	44.655105
3503.908300	499779.396922	44.660109
3503.554390	499768.164000	44.665114
3503.802761	499749.090978	44.670119
3503.354431	499733.671464	44.675124
3503.816539	499705.199841	44.680129
3503.857268	499709.090659	44.685133
3503.436325	499676.557036	44.690138
3503.437136	499660.813379	44.695143
3503.317255	499653.137464	44.700148
3503.659119	499639.972167	44.705153
3503.311221	499626.915861	44.710157
3503.374163	499615.515727	44.715162
3503.500697	499604.662364	44.720167
3503.588646	499593.055781	44.725172
3503.683552	499569.957156	44.730177
3503.568553	499559.951870	44.735181
3503.385318	499544.085332	44.740186
3503.892902	499518.592862	44.745191
3503.356896	499508.400973	44.750196
3503.660502	499496.203416	44.755201
3503.817179	499474.512296	44.760205
3503.859933	499453.800957	44.765210
3503.767713	499438.729882	44.770215
3503.522782	499419.127011	44.775220
3503.508793	499415.990177	44.780225
3503.506403	499387.996426	44.785229
3503.662140	499375.012212	44.790234
3503.993345	499361.848395	44.795239
3503.522520	499338.079551	44.800244
3503.450340	499320.828484	44.805249
3503.485663	499318.341922	44.810253
3503.707965	499298.867570	44.815258
3503.943938	499266.280012	44.820263
3503.574981	499257.580233	44.825268
3503.702263	499225.009777	44.830273
3503.679601	499216.963959	44.835277
3503.521136	499209.800171	44.840282
3503.891150	499179.317393	44.845287
3503.736806	499171.292365	44.850292
3503.822388	499143.638684	44.855297
3504.051868	499131.655083	44.860301
3503.684710	499111.362481	44.865306
3503.697907	499087.618060	44.870311
3503.867063	499088.502006	44.875316
3503.884099	499067.490552	44.880321
3503.808512	499041.785831	44.885325
3503.642448	499022.068818	44.890330
3503.751816	498992.892474	44.895335
3503.557590	498982.595651	44.900340
3503.378035	498967.487359	44.905345
3503.652008	498950.788707	44.910349
3503.539536	498930.303784	44.915354
3503.609796	498923.964322	44.920359
3503.412497	498903.442152	44.925364
3503.678296	498878.543836	44.930369
3503.624447	498881.336078	44.935373
3503.291956	498863.619480	44.940378
3503.613625	498844.635163	44.945383
3503.662263	498834.957974	44.950388
3503.924442	498823.778967	44.955393
3503.598588	498804.238835	44.960397
3503.584002	498781.105877	44.965402
3503.564868	498757.264883	44.970407
3503.475948	498749.229326	44.975412
3503.602273	498723.492243	44.980417
3503.608505	498728.350567	44.985421
3503.482434	498698.704721	44.990426
3503.729108	498679.985198	44.995431
3503.383136	498670.977761	45.000436
3503.470099	498646.613620	45.005441
3503.481250	498641.802103	45.010445
3503.559447	498638.954307	45.015450
3503.544546	498603.317162	45.020455
3503.597255	498592.221738	45.025460
3503.513016	498584.691605	45.030465
3503.379269	498568.259524	45.035469
3503.436621	498547.595458	45.040474
3503.599050	498539.671960	45.045479
3503.362838	498530.292740	45.050484
3503.569772	498509.402497	45.055489
3503.462876	498501.369671	45.060493
3503.367439	498487.057664	45.065498
3503.644248	498474.610532	45.070503
3503.327752	498458.308478	45.075508
3503.499499	498443.549223	45.080513
3503.436719	498428.523273	45.085517
3503.436773	498419.309155	45.090522
3503.638973	498396.090820	45.095527
3503.502943	498393.884329	45.100532
3503.616232	498379.033011	45.105537
3503.441743	498361.949065	45.110541
3503.408702	498346.513353	45.115546
3503.539912	498339.657811	45.120551
3503.325014	498320.150243	45.125556
3503.197799	498306.804979	45.130561
3503.210640	498287.717006	45.135565
3503.348027	498293.668460	45.140570
3503.606436	498285.982805	45.145575
3503.876576	498261.791696	45.150580
3503.553399	498244.528637	45.155585
3503.328441	498235.198109	45.160589
3503.282821	498210.955581	45.165594
3503.537565	498196.790505	45.170599
3503.425758	498198.731391	45.175604
3503.387281	498180.765159	45.180609
3503.566869	498162.359450	45.185613
3503.661579	498162.040211	45.190618
3503.634012	498141.794099	45.195623
3503.498089	498121.058838	45.200628
3503.549025	498092.700271	45.205633
3503.591978	498084.036078	45.210637
3503.276520	498067.429756	45.215642
3503.668471	498052.787258	45.220647
3503.514425	498067.745489	45.225652
3503.807747	498040.411664	45.230657
3503.647857	498024.641346	45.235661
3503.441972	498004.777636	45.240666
3503.430640	497982.098765	45.245671
3503.368623	497970.666712	45.250676
3503.636044	497958.828214	45.255681
3503.710901	497949.956413	45.260685
3503.558023	497928.312352	45.265690
3503.839304	497913.839108	45.270695
3503.667160	497904.601314	45.275700
3503.598799	497880.615064	45.280705
3503.776859	497866.107468	45.285709
3503.083842	497855.686320	45.290714
3503.352933	497825.166580	45.295719
3503.174748	497822.865429	45.300724
3503.628586	497808.820464	45.305729
3503.722678	497807.539426	45.310733
3503.420140	497782.121903	45.315738
3503.753991	497762.729518	45.320743
3503.565212	497756.531834	45.325748
3503.564912	497726.003872	45.330753
3503.780904	497710.072627	45.335757
3503.675956	497701.937885	45.340762
3503.543173	497672.645795	45.345767
3503.252227	497669.248667	45.350772
3503.571517	497657.351149	45.355777
3503.187208	497640.249051	45.360781
3503.175998	497625.619294	45.365786
3503.519366	497612.705415	45.370791
3503.019939	497612.328178	45.375796
3503.417183	497598.848884	45.380801
3503.473193	497583.702207	45.385805
3503.378739	497577.084543	45.390810
3503.205889	497574.934397	45.395815
3503.108516	497566.089625	45.400820
3503.567720	497549.613540	45.405825
3503.431573	497530.801446	45.410829
3503.247069	497529.210028	45.415834
3503.552044	497514.935228	45.420839
3503.275610	497507.283137	45.425844
3503.194808	497480.615109	45.430849
3503.703794	497469.143131	45.435853
3503.586525	497466.376667	45.440858
3503.666840	497435.936730	45.445863
3503.749966	497426.253336	45.450868
3503.682092	497404.696469	45.455873
3503.253917	497391.043700	45.460877
3503.198700	497386.090456	45.465882
3503.613425	497368.608696	45.470887
3503.517507	497360.725508	45.475892
3503.332329	497348.755627	45.480897
3503.669391	497332.096139	45.485901
3503.289478	497326.384155	45.490906
3503.507911	497311.819109	45.495911
3503.159765	497314.658099	45.500916
3503.314832	497282.737903	45.505921
3503.488239	497277.495364	45.510925
3503.284076	497270.540535	45.515930
3503.495138	497244.028545	45.520935
3503.268124	497235.912883	45.525940
3503.130285	497226.314928	45.530945
3503.448028	497230.061251	45.535949
3503.258582	497212.522935	45.540954
3503.544498	497186.910328	45.545959
3503.194635	497184.433714	45.550964
3503.522078	497175.065971	45.555969
3503.638149	497156.314885	45.560973
3502.940006	497139.413790	45.565978
3503.320426	497122.291608	45.570983
3503.158323	497125.708760	45.575988
3503.308656	497123.760626	45.580993
3503.278662	497097.691539	45.585997
3503.036641	497089.831321	45.591002
3503.525652	497076.640907	45.596007
3503.252559	497077.544214	45.601012
3503.495581	497062.772571	45.606017
3503.654878	497045.027097	45.611021
3503.169710	497035.078905	45.616026
3503.417293	497011.497228	45.621031
3503.105228	497025.215589	45.626036
3503.586979	497004.027041	45.631041
3503.478730	496981.260977	45.636045
3503.394540	496985.374637	45.641050
3503.571845	496966.309910	45.646055
3503.289541	496938.103453	45.651060
3503.413300	496928.919655	45.656065
3503.649169	496919.920650	45.661069
3503.247192	496913.756368	45.666074
3503.316013	496887.114450	45.671079
3503.276270	496877.399552	45.676084
3503.233008	496868.900288	45.681089
3503.277199	496877.043960	45.686093
3503.242083	496857.152003	45.691098
3503.551807	496824.599020	45.696103
3503.043813	496828.020260	45.701108
3503.287668	496806.919706	45.706113
3503.498971	496812.657453	45.711117
3503.505422	496805.466647	45.716122
3503.743454	496774.190618	45.721127
3503.261921	496759.685115	45.726132
3503.276979	496760.036614	45.731137
3503.378839	496728.933913	45.736141
3503.254443	496732.851468	45.741146
3503.334220	496714.308177	45.746151
3503.249434	496729.459081	45.751156
3503.227098	496700.654256	45.756161
3503.376901	496693.491380	45.761165
3503.005106	496684.031368	45.766170
3503.226553	496678.831695	45.771175
3503.162330	496668.209232	45.776180
3503.068772	496662.451786	45.781185
3503.092947	496636.322847	45.786189
3502.986612	496625.858901	45.791194
3503.765149	496621.431871	45.796199
3503.172325	496619.753010	45.801204
3503.154057	496619.299712	45.806209
3503.233063	496613.008688	45.811213
3503.144154	496591.656696	45.816218
3503.150574	496569.631433	45.821223
3503.248443	496585.107998	45.826228
3503.310616	496572.339077	45.831233
3503.467057	496562.086715	45.836237
3503.257959	496549.310017	45.841242
3503.446987	496515.965485	45.846247
3503.081992	496531.667130	45.851252
3503.260956	496519.588527	45.856257
3503.238681	496515.389281	45.861261
3503.134004	496494.495331	45.866266
3502.999009	496485.655978	45.871271
3502.975656	496481.507524	45.876276
3503.197872	496475.143192	45.881281
3503.124592	496478.242651	45.886285
3503.165541	496473.881516	45.891290
3503.178954	496460.259520	45.896295
3503.268600	496447.030503	45.901300
3503.164790	496437.173605	45.906305
3503.487693	496429.932642	45.911309
3502.893981	496422.634008	45.916314
3503.411793	496424.070547	45.921319
3503.512380	496404.713577	45.926324
3503.495177	496393.779745	45.931329
3503.488264	496394.489131	45.936333
3503.460497	496374.544855	45.941338
3503.539448	496338.888423	45.946343
3503.480815	496338.795905	45.951348
3502.963739	496335.079850	45.956353
3503.361544	496325.498032	45.961357
3503.149530	496299.405933	45.966362
3503.393788	496281.494399	45.971367
3503.213709	496283.648797	45.976372
3503.198396	496273.018374	45.981377
3503.305454	496272.038960	45.986381
3502.980364	496247.230409	45.991386
3503.308254	496231.482707	45.996391
3503.400691	496233.340895	46.001396
3503.172804	496232.566301	46.006401
3503.448547	496230.598254	46.011405
3502.979980	496208.799507	46.016410
3503.478422	496196.518312	46.021415
3503.194512	496201.777577	46.026420
3503.222899	496186.684730	46.031425
3503.204328	496181.624106	46.036429
3503.212055	496166.483877	46.041434
3503.175659	496143.148474	46.046439
3503.254947	496131.996715	46.051444
3502.985841	496128.443952	46.056449
3503.211790	496133.521403	46.061453
3503.321539	496127.832920	46.066458
3503.422066	496103.817633	46.071463
3503.070121	496097.847687	46.076468
3503.361078	496091.826773	46.081473
3503.486592	496079.351280	46.086477
3502.967165	496089.964013	46.091482
3503.009360	496050.464897	46.096487
3503.026664	496043.930274	46.101492
3503.018834	496033.045375	46.106497
3503.150064	496033.125376	46.111501
3502.860027	496019.804157	46.116506
3502.861190	496021.575528	46.121511
3502.746937	496028.175064	46.126516
3502.918043	496020.400989	46.131521
3503.311924	496023.730486	46.136525
3503.192601	496023.445034	46.141530
3503.376650	496017.592883	46.146535
3503.386673	495993.591752	46.151540
3503.201288	495984.152547	46.156545
3503.178897	495982.029064	46.161549
3503.023408	495969.091593	46.166554
3503.301638	495957.655134	46.171559
3503.029809	495941.445014	46.176564
3502.953271	495928.900086	46.181569
3503.163339	495924.157677	46.186573
3502.943310	495920.343962	46.191578
3502.893667	495925.313130	46.196583
3503.239029	495923.941622	46.201588
3503.176466	495922.837102	46.206593
3503.171013	495899.800284	46.211597
3502.956366	495890.365654	46.216602
3503.322179	495871.624410	46.221607
3502.897921	495879.589401	46.226612
3503.053196	495881.235170	46.231617
3503.508268	495861.517818	46.236621
3503.088689	495864.925262	46.241626
3503.339965	495836.379619	46.246631
3503.494838	495814.886928	46.251636
3503.162854	495818.888115	46.256641
3503.372493	495826.196010	46.261645
3503.142742	495807.346291	46.266650
3503.442587	495781.526983	46.271655
3503.234515	495781.761867	46.276660
3503.373607	495770.246015	46.281665
3503.296357	495774.612009	46.286669
3503.048036	495754.448750	46.291674
3503.024461	495738.604271	46.296679
3503.023167	495723.515732	46.301684
3503.093797	495719.149726	46.306689
3503.238304	495723.176898	46.311693
3503.037827	495729.638272	46.316698
3503.402320	495712.264128	46.321703
3503.184349	495711.032258	46.326708
3503.297205	495699.368613	46.331713
3503.385527	495679.911549	46.336717
3502.904325	495688.341307	46.341722
3503.384833	495677.581552	46.346727
3503.504117	495661.562535	46.351732
3503.332982	495640.981899	46.356737
3503.415115	495636.917847	46.361741
3503.259969	495641.194919	46.366746
3503.441027	495619.292806	46.371751
3503.483391	495600.754294	46.376756
3503.381235	495587.757493	46.381761
3503.398714	495581.273309	46.386765
3503.046257	495568.164152	46.391770
3503.383701	495546.490399	46.396775
3503.234047	495530.412502	46.401780
3503.298520	495538.857361	46.406785
3503.626754	495524.172271	46.411789
3503.188634	495513.557589	46.416794
3503.116833	495494.783851	46.421799
3502.816853	495494.628204	46.426804
3503.182045	495489.810536	46.431809
3503.046519	495489.375740	46.436813
3502.828614	495485.510965	46.441818
3503.144889	495485.460462	46.446823
3503.227578	495487.522795	46.451828
3503.107092	495468.098503	46.456833
3503.217354	495449.599742	46.461837
3503.122323	495442.272538	46.466842
3503.697635	495434.484970	46.471847
3503.293922	495430.953342	46.476852
3503.141657	495408.698592	46.481857
3503.607057	495397.080307	46.486861
3503.459137	495389.457645	46.491866
3503.025509	495383.753534	46.496871
3503.002155	495375.807386	46.501876
3503.217353	495361.393192	46.506881
3503.258832	495344.829234	46.511885
3502.916867	495351.920693	46.516890
3503.138093	495338.821978	46.521895
3503.291265	495348.721255	46.526900
3503.160032	495338.614934	46.531905
3503.468025	495322.616431	46.536909
3503.497696	495299.877103	46.541914
3503.581560	495295.407639	46.546919
3503.636529	495287.854138	46.551924
3503.443663	495262.517022	46.556929
3503.301871	495253.526246	46.561933
3503.307598	495252.815957	46.566938
3503.491839	495225.140713	46.571943
3503.044780	495211.286754	46.576948
3503.223292	495197.992156	46.581953
3503.709371	495190.826185	46.586957
3503.387300	495188.041104	46.591962
3503.445068	495157.246491	46.596967
3503.377565	495160.142727	46.601972
3503.334571	495151.237554	46.606977
3503.553039	495139.151797	46.611981
3503.196804	495129.232815	46.616986
3503.117559	495102.105357	46.621991
3503.286272	495107.141508	46.626996
3503.470423	495103.668816	46.632001
3503.567641	495083.399578	46.637005
3503.432692	495064.989812	46.642010
3503.360359	495050.823346	46.647015
3503.379755	495049.351386	46.652020
3503.093276	495024.940138	46.657025
3503.130329	495002.098006	46.662029
3503.329996	495014.066096	46.667034
3503.330201	495003.989452	46.672039
3503.214215	495007.197176	46.677044
3503.135964	494998.196233	46.682049
3503.029206	494973.807149	46.687053
3503.521301	494961.323598	46.692058
3503.590149	494955.539947	46.697063
3503.171781	494952.364977	46.702068
3503.330156	494950.263441	46.707073
3503.773303	494923.913941	46.712077
3503.172072	494925.476811	46.717082
3503.372229	494911.368444	46.722087
3503.104922	494889.890750	46.727092
3502.865901	494872.104843	46.732097
3503.562610	494867.842233	46.737101
3503.171749	494866.688261	46.742106
3503.207046	494863.289681	46.747111
3503.427485	494866.899971	46.752116
3503.480073	494842.688067	46.757121
3503.509973	494826.884982	46.762125
3503.412837	494822.747811	46.767130
3503.392079	494804.218469	46.772135
3503.450518	494798.689584	46.777140
3503.289407	494774.005019	46.782145
3503.530263	494757.763463	46.787149
3503.279039	494750.865739	46.792154
3503.133572	494727.495131	46.797159
3503.260258	494720.841481	46.802164
3503.380875	494712.619122	46.807169
3503.446900	494715.544961	46.812173
3503.181810	494696.092067	46.817178
3503.169528	494675.485241	46.822183
3503.402155	494672.663057	46.827188
3503.073590	494673.068898	46.832193
3503.489095	494664.850551	46.837197
3503.136100	494643.689917	46.842202
3503.526533	494619.626869	46.847207
3503.059483	494622.130618	46.852212
3502.966434	494613.384997	46.857217
3503.310967	494608.519731	46.862221
3503.289266	494616.117843	46.867226
3503.008682	494591.958259	46.872231
3503.529057	494569.241749	46.877236
3503.147562	494574.162455	46.882241
3503.320030	494562.741841	46.887245
3503.164481	494562.563360	46.892250
3503.391922	494536.247391	46.897255
3503.118765	494519.833679	46.902260
3502.963075	494523.351572	46.907265
3503.555842	494513.181016	46.912269
3503.158352	494514.154737	46.917274
3503.214933	494504.473990	46.922279
3503.579914	494473.376505	46.927284
3503.503882	494472.729741	46.932289
3503.459172	494455.976060	46.937293
3503.249874	494442.235849	46.942298
3503.275197	494414.685768	46.947303
3503.448900	494421.341647	46.952308
3503.251630	494419.144348	46.957313
3503.474610	494400.221633	46.962317
3503.300478	494385.766929	46.967322
3503.237800	494368.053936	46.972327
3503.295037	494366.879754	46.977332
3503.265571	494358.377141	46.982337
3503.326357	494348.341198	46.987341
3503.002494	494332.441686	46.992346
3503.257195	494316.754543	46.997351
3502.988110	494322.670263	47.002356
3502.918197	494316.553891	47.007361
3503.504512	494314.891012	47.012365
3502.998619	494317.350304	47.017370
3503.098445	494295.661990	47.022375
3503.065260	494267.462671	47.027380
3503.155050	494259.396887	47.032385
3503.220950	494262.829176	47.037389
3503.008074	494266.862511	47.042394
3503.094084	494254.392019	47.047399
3503.051439	494261.740409	47.052404
3502.639235	494259.678328	47.057409
3503.430769	494235.551392	47.062413
3502.994434	494231.417055	47.067418
3503.126065	494210.938873	47.072423
3502.902464	494220.138765	47.077428
3503.036918	494214.698965	47.082433
3503.021148	494210.143711	47.087437
3502.891519	494215.024710	47.092442
3503.149441	494204.906901	47.097447
3502.743951	494207.552884	47.102452
3502.906618	494213.197866	47.107457
3503.336076	494181.937792	47.112461
3502.849625	494169.507073	47.117466
3502.907209	494159.572805	47.122471
3502.996286	494165.887698	47.127476
3502.984853	494154.445257	47.132481
3503.292439	494147.610905	47.137485
3502.832362	494169.000826	47.142490
3503.145554	494154.620836	47.147495
3503.324796	494148.768850	47.152500
3502.718045	494139.699095	47.157505
3502.887544	494128.025501	47.162509
3503.248999	494124.119518	47.167514
3503.178475	494118.610809	47.172519
3503.282482	494120.669928	47.177524
3503.022926	494119.748337	47.182529
3503.512608	494115.670181	47.187533
3503.063077	494103.031037	47.192538
3503.411581	494076.948461	47.197543
3503.622164	494061.926344	47.202548
3503.357979	494069.917455	47.207553
3503.317232	494031.642363	47.212557
3503.123330	494026.558214	47.217562
3503.114147	494017.090148	47.222567
3503.332049	494013.460009	47.227572
3503.174042	494015.104819	47.232577
3503.768252	493995.464752	47.237581
3503.428462	493981.846090	47.242586
3503.254563	493967.036564	47.247591
3503.330946	493965.352966	47.252596
3503.456995	493952.065759	47.257601
3503.333993	493927.272760	47.262605
3502.787630	493917.585712	47.267610
3503.241210	493913.108124	47.272615
3503.028314	493911.470235	47.277620
3503.176815	493908.813139	47.282625
3503.299347	493879.322702	47.287629
3503.172283	493881.266454	47.292634
3503.103528	493866.744052	47.297639
3503.254861	493856.946717	47.302644
3503.027714	493863.919328	47.307649
3503.308078	493860.329925	47.312653
3503.287946	493836.735830	47.317658
3503.186891	493814.471052	47.322663
3503.391088	493825.274554	47.327668
3503.324052	493823.664245	47.332673
3503.299406	493804.374955	47.337677
3503.276182	493784.832236	47.342682
3503.272908	493769.894314	47.347687
3503.336955	493758.085239	47.352692
3502.997198	493765.632690	47.357697
3502.986672	493764.215993	47.362701
3503.232132	493764.429865	47.367706
3503.156100	493738.768360	47.372711
3503.168839	493729.651141	47.377716
3503.192878	493713.544203	47.382721
3503.265125	493718.444068	47.387725
3503.426113	493728.849358	47.392730
3503.354085	493701.870603	47.397735
3503.221310	493677.635821	47.402740
3502.999818	493672.555934	47.407745
3502.990118	493665.771545	47.412749
3503.059652	493660.848213	47.417754
3503.144421	493661.340668	47.422759
3503.036419	493662.268684	47.427764
3503.096384	493646.510470	47.432769
3503.417951	493621.342980	47.437773
3503.267711	493624.201895	47.442778
3503.227117	493612.611813	47.447783
3503.194629	493616.920607	47.452788
3502.998900	493597.506225	47.457793
3503.572299	493576.147327	47.462797
3503.037683	493566.711425	47.467802
3503.286994	493557.607373	47.472807
3503.258921	493562.826960	47.477812
3503.098552	493573.435034	47.482817
3503.347814	493542.556817	47.487821
3502.953906	493527.022139	47.492826
3503.157034	493523.292964	47.497831
3503.386430	493513.331197	47.502836
3503.505470	493514.780357	47.507841
3503.169982	493489.260780	47.512845
3503.094285	493488.107550	47.517850
3503.211436	493468.035934	47.522855
3503.362813	493466.087251	47.527860
3503.123416	493467.238592	47.532865
3503.022165	493456.670754	47.537869
3503.141214	493462.221585	47.542874
3503.127047	493426.422291	47.547879
3503.225800	493417.443239	47.552884
3503.164790	493408.286878	47.557889
3503.145218	493407.276687	47.562893
3503.265080	493418.245670	47.567898
3503.381453	493396.503046	47.572903
3503.614130	493374.286273	47.577908
3503.032297	493374.327058	47.582913
3503.160846	493362.001155	47.587917
3503.303571	493363.345307	47.592922
3503.223166	493359.508991	47.597927
3503.211982	493340.723471	47.602932
3503.573251	493332.665019	47.607937
3503.519873	493321.127412	47.612941
3503.161591	493311.460960	47.617946
3503.139279	493293.386086	47.622951
3503.053914	493281.549679	47.627956
3502.982313	493279.889405	47.632961
3503.134190	493273.383168	47.637965
3503.104177	493276.476329	47.642970
3503.065399	493271.316819	47.647975
3503.482710	493265.426932	47.652980
3503.127904	493247.961580	47.657985
3503.206137	493230.174587	47.662989
3503.093229	493236.319164	47.667994
3503.565519	493229.458447	47.672999
3503.303575	493212.839242	47.678004
3502.881151	493202.828398	47.683009
3503.289830	493184.685310	47.688013
3503.262382	493183.575074	47.693018
3503.236543	493170.210030	47.698023
3502.947609	493171.369217	47.703028
3502.975883	493165.945887	47.708033
3503.469698	493147.688031	47.713037
3503.084998	493141.317181	47.718042
3503.294947	493132.320419	47.723047
3503.304662	493130.951114	47.728052
3502.999351	493136.974213	47.733057
3503.048039	493121.521167	47.738061
3503.323339	493101.221606	47.743066
3503.021341	493088.609087	47.748071
3503.352623	493089.568990	47.753076
3503.243247	493081.179693	47.758081
3503.237479	493081.737110	47.763085
3502.971079	493065.219753	47.768090
3502.907655	493039.454005	47.773095
3503.129117	493031.063042	47.778100
3502.734775	493038.670054	47.783105
3503.381083	493034.769468	47.788109
3503.338788	493035.889687	47.793114
3503.248167	493035.498373	47.798119
3503.158203	493024.928504	47.803124
3502.847314	492998.239662	47.808129
3503.402378	492981.541777	47.813133
3503.275306	492983.181788	47.818138
3503.341010	492975.828199	47.823143
3503.029401	492973.344959	47.828148
3503.106823	492980.219132	47.833153
3503.367097	492951.971427	47.838157
3503.423232	492931.250560	47.843162
3503.217227	492933.105607	47.848167
3503.429363	492938.844442	47.853172
3503.420555	492924.058628	47.858177
3502.928440	492895.828457	47.863181
3503.250648	492889.953481	47.868186
3503.352263	492889.936900	47.873191
3503.371546	492874.387015	47.878196
3503.268858	492864.730576	47.883201
3503.708911	492834.833818	47.888205
3503.384519	492837.467177	47.893210
3503.003396	492824.411226	47.898215
3503.123805	492819.986027	47.903220
3503.557247	492800.420740	47.908225
3503.726204	492787.986790	47.913229
3503.226656	492789.381842	47.918234
3503.349937	492771.739209	47.923239
3503.406330	492749.043146	47.928244
3503.200898	492738.947119	47.933249
3502.999641	492736.142569	47.938253
3503.033650	492727.730453	47.943258
3503.319832	492722.924555	47.948263
3503.354800	492705.143894	47.953268
3502.881060	492697.520962	47.958273
3503.265168	492685.255503	47.963277
3502.872202	492683.494040	47.968282
3502.946854	492683.481720	47.973287
3503.028308	492672.530080	47.978292
3502.868808	492681.821887	47.983297
3503.038359	492674.502407	47.988301
3503.103197	492678.593479	47.993306
3503.198746	492663.385845	47.998311
3503.056946	492650.291951	48.003316
3502.740297	492649.429946	48.008321
3502.995038	492628.930556	48.013325
3503.015516	492637.535620	48.018330
3502.870501	492632.797841	48.023335
3503.187348	492622.062174	48.028340
3503.175091	492621.050784	48.033345
3503.091695	492622.380084	48.038349
3503.180010	492600.083917	48.043354
3503.546727	492583.769920	48.048359
3503.350635	492576.305623	48.053364
3503.103636	492573.457635	48.058369
3503.456906	492570.869270	48.063373
3503.426075	492554.618072	48.068378
3503.383753	492553.560789	48.073383
3503.444466	492545.853336	48.078388
3503.182491	492534.348202	48.083393
3503.035889	492512.696737	48.088397
3503.183800	492496.366602	48.093402
3503.098322	492495.468057	48.098407
3503.579909	492489.719691	48.103412
3503.320289	492496.495385	48.108417
3503.520457	492462.736616	48.113421
3503.180930	492454.737889	48.118426
3502.901191	492452.097619	48.123431
3503.123370	492436.920429	48.128436
3503.254041	492445.761373	48.133441
3503.221974	492431.383966	48.138445
3503.124691	492405.622686	48.143450
3503.096120	492395.447882	48.148455
3502.995950	492391.158721	48.153460
3503.446748	492395.644630	48.158465
3503.165501	492382.623224	48.163469
3502.799039	492380.604338	48.168474
3502.692233	492380.671334	48.173479
3503.100338	492377.010820	48.178484
3503.048801	492369.017186	48.183489
3502.854647	492353.551234	48.188493
3502.641698	492338.695931	48.193498
3502.861761	492348.890100	48.198503
3502.972670	492341.123988	48.203508
3503.045391	492339.288899	48.208513
3503.400608	492337.864936	48.213517
3503.087470	492336.749156	48.218522
3503.046227	492335.641049	48.223527
3503.077704	492332.647735	48.228532
3503.031581	492312.651310	48.233537
3503.024625	492286.824950	48.238541
3503.153612	492281.436087	48.243546
3503.124643	492283.263221	48.248551
3503.350957	492283.986550	48.253556
3502.956613	492285.263731	48.258561
3502.934489	492277.670539	48.263565
3503.258097	492283.290680	48.268570
3503.039124	492257.295219	48.273575
3503.155082	492244.413510	48.278580
3503.056751	492237.338756	48.283585
3503.286408	492232.997437	48.288589
3502.955201	492227.276152	48.293594
3502.686594	492232.787331	48.298599
3503.211044	492225.107743	48.303604
3503.228602	492225.155086	48.308609
3503.265681	492195.624828	48.313613
3503.270939	492191.825374	48.318618
3503.125314	492191.493374	48.323623
3503.182698	492180.595890	48.328628
3503.218125	492188.084690	48.333633
3503.335708	492158.491010	48.338637
3503.077279	492150.479336	48.343642
3503.085521	492143.742195	48.348647
3503.288907	492135.505610	48.353652
3503.398566	492136.601870	48.358657
3503.405709	492117.913497	48.363661
3503.385479	492099.533280	48.368666
3503.015873	492097.211010	48.373671
3503.200088	492086.040219	48.378676
3503.270175	492085.977978	48.383681
3503.224530	492071.906289	48.388685
3503.169589	492056.721940	48.393690
3502.954391	492041.157769	48.398695
3503.237346	492038.074025	48.403700
3502.920070	492038.478133	48.408705
3502.963912	492032.900087	48.413709
3503.157410	492032.362568	48.418714
3502.757262	492029.133563	48.423719
3503.067218	492037.389310	48.428724
3502.941934	492009.403667	48.433729
3503.180989	491979.739864	48.438733
3503.169781	491991.388751	48.443738
3502.988239	491988.479687	48.448743
3503.030542	491982.699301	48.453748
3503.054856	491986.442437	48.458753
3503.061051	491986.289009	48.463757
3503.374391	491985.935118	48.468762
3503.319438	491962.850555	48.473767
3503.116975	491951.740790	48.478772
3503.009431	491947.857827	48.483777
3503.167436	491938.716770	48.488781
3503.107283	491942.827758	48.493786
3503.061802	491944.657535	48.498791
3503.012050	491921.926593	48.503796
3502.794520	491907.679373	48.508801
3503.051805	491893.458392	48.513805
3503.084429	491894.111062	48.518810
3503.130513	491892.735918	48.523815
3503.028096	491895.334329	48.528820
3502.810438	491900.280491	48.533825
3503.139698	491879.920425	48.538829
3503.061130	491893.251211	48.543834
3503.173209	491883.712248	48.548839
3503.268102	491853.665888	48.553844
3503.182271	491848.867913	48.558849
3503.172063	491848.869003	48.563853
3502.753865	491844.174192	48.568858
3502.951718	491841.154507	48.573863
3503.264395	491835.787129	48.578868
3502.939345	491842.269546	48.583873
3502.947351	491828.290478	48.588877
3502.766966	491809.378218	48.593882
3502.933271	491795.576679	48.598887
3503.152784	491783.488565	48.603892
3502.879635	491783.531207	48.608897
3502.975046	491780.882198	48.613901
3503.224653	491783.678208	48.618906
3503.032869	491784.568914	48.623911
3503.105454	491776.606053	48.628916
3503.170969	491779.988222	48.633921
3503.039375	491758.080293	48.638925
3502.902692	491743.566958	48.643930
3503.068032	491742.628741	48.648935
3502.983129	491739.906936	48.653940
3503.001549	491743.397839	48.658945
3503.050517	491741.769015	48.663949
3502.987134	491736.207825	48.668954
3502.800334	491737.148388	48.673959
3503.031941	491740.301747	48.678964
3502.760014	491746.725159	48.683969
3503.057640	491735.029811	48.688973
3503.119058	491737.652996	48.693978
3502.950861	491713.573168	48.698983
3503.291108	491693.666947	48.703988
3503.224633	491693.423715	48.708993
3503.353082	491682.514709	48.713997
3503.236670	491682.887081	48.719002
3503.324678	491669.604249	48.724007
3503.204332	491655.037621	48.729012
3502.733245	491652.579403	48.734017
3503.480268	491632.558192	48.739021
3503.263923	491640.897286	48.744026
3503.036673	491639.160175	48.749031
3502.920686	491634.772053	48.754036
3503.023523	491612.320476	48.759041
3502.946819	491596.227617	48.764045
3503.036456	491603.910659	48.769050
3503.063120	491583.192945	48.774055
3503.071958	491582.836524	48.779060
3502.964943	491585.435705	48.784065
3503.286265	491580.269461	48.789069
3503.344848	491579.905179	48.794074
3503.209121	491573.443798	48.799079
3503.430804	491549.200858	48.804084
3503.288099	491556.160989	48.809089
3503.135523	491542.612228	48.814093
3503.198711	491538.752842	48.819098
3503.276035	491523.293940	48.824103
3503.236559	491503.042377	48.829108
3502.958191	491495.793219	48.834113
3503.105168	491487.210760	48.839117
3503.346148	491492.945486	48.844122
3503.406272	491472.830081	48.849127
3503.368554	491459.415038	48.854132
3502.825305	491450.080700	48.859137
3502.832627	491444.103101	48.864141
3502.826539	491435.646094	48.869146
3502.827910	491436.151788	48.874151
3503.470513	491426.781970	48.879156
3502.962903	491443.877848	48.884161
3503.003075	491437.844413	48.889165
3503.364451	491427.404882	48.894170
3502.968237	491407.766669	48.899175
3502.910084	491389.847535	48.904180
3502.927782	491384.931792	48.909185
3502.876224	491388.687038	48.914189
3502.832821	491377.551793	48.919194
3503.211590	491377.491414	48.924199
3503.461053	491370.057507	48.929204
3503.012691	491374.331254	48.934209
3503.160443	491354.758953	48.939213
3503.250374	491339.196619	48.944218
3503.181391	491336.421596	48.949223
3503.136183	491328.021365	48.954228
3503.280147	491336.354299	48.959233
3503.085233	491323.622368	48.964237
3503.125108	491306.953755	48.969242
3503.103232	491288.218491	48.974247
3503.255344	491281.357015	48.979252
3503.054013	491284.680156	48.984257
3503.110612	491275.605443	48.989261
3503.364314	491270.297868	48.994266
3503.403006	491264.922981	48.999271
3503.303200	491243.617149	49.004276
3503.153960	491231.029868	49.009281
3503.085195	491233.623054	49.014285
3503.060748	491232.714803	49.019290
3502.899574	491234.411000	49.024295
3503.474965	491224.595907	49.029300
3503.343908	491206.941338	49.034305
3503.049033	491189.869725	49.039309
3503.093627	491182.518763	49.044314
3502.966499	491194.692908	49.049319
3503.409181	491177.909881	49.054324
3503.087579	491165.552371	49.059329
3503.435501	491147.315611	49.064333
3503.162277	491150.954002	49.069338
3503.055885	491137.093782	49.074343
3503.520954	491141.172590	49.079348
3502.945783	491128.905770	49.084353
3503.013540	491106.408484	49.089357
3503.019005	491095.012127	49.094362
3502.916687	491087.329833	49.099367
3503.154010	491084.354433	49.104372
3503.152983	491088.810776	49.109377
3503.357817	491083.764092	49.114381
3503.263293	491084.538172	49.119386
3503.056860	491078.492947	49.124391
3503.243445	491051.064311	49.129396
3503.154050	491039.632266	49.134401
3503.038105	491035.497217	49.139405
3503.649708	491032.563952	49.144410
3503.104226	491023.128462	49.149415
3503.236996	491002.190757	49.154420
3502.915137	490996.872770	49.159425
3503.275995	490990.383356	49.164429
3503.215107	490995.608850	49.169434
3503.059775	490991.935817	49.174439
3503.102445	490981.799626	49.179444
3502.796395	490972.478208	49.184449
3502.871268	490955.347949	49.189453
3503.035025	490946.357432	49.194458
3502.867872	490947.294929	49.199463
3503.081835	490941.081935	49.204468
3502.840143	490954.894972	49.209473
3502.994309	490941.753102	49.214477
3503.125144	490938.946442	49.219482
3502.910712	490942.170424	49.224487
3503.321517	490932.836992	49.229492
3503.312476	490922.202493	49.234497
3503.004131	490895.459579	49.239501
3502.979264	490886.954645	49.244506
3502.882082	490889.856239	49.249511
3503.188732	490886.971142	49.254516
3503.225904	490890.864401	49.259521
3503.256550	490872.981383	49.264525
3503.178153	490872.436154	49.269530
3502.796344	490852.187338	49.274535
3503.291864	490833.876304	49.279540
3502.906207	490835.608012	49.284545
3503.025940	490838.222109	49.289549
3503.097431	490832.234174	49.294554
3503.016197	490822.370702	49.299559
3503.216050	490827.403103	49.304564
3502.886068	490833.126972	49.309569
3503.225825	490796.861518	49.314573
3502.937692	490789.208466	49.319578
3502.928036	490789.006888	49.324583
3503.370402	490782.200651	49.329588
3503.084629	490783.004966	49.334593
3503.164988	490771.495285	49.339597
3502.989845	490779.473736	49.344602
3503.147239	490768.407686	49.349607
3503.199237	490750.470531	49.354612
3503.228969	490754.871446	49.359617
3503.175425	490743.585490	49.364621
3503.245287	490744.181670	49.369626
3503.143939	490737.562630	49.374631
3503.247218	490707.158582	49.379636
3503.155899	490689.142725	49.384641
3503.173949	490684.328033	49.389645
3503.034760	490674.878805	49.394650
3502.963747	490683.094068	49.399655
3503.063831	490678.114475	49.404660
3502.945190	490692.313424	49.409665
3502.880124	490676.319223	49.414669
3502.994053	490673.160676	49.419674
3502.926849	490666.738797	49.424679
3502.752695	490652.635698	49.429684
3502.777719	490651.820892	49.434689
3503.023441	490637.702074	49.439693
3503.234313	490638.073392	49.444698
3502.840781	490642.237349	49.449703
3503.091872	490630.751247	49.454708
3502.835940	490637.324448	49.459713
3503.027103	490627.974928	49.464717
3503.177091	490623.696472	49.469722
3502.959708	490627.275494	49.474727
3503.143688	490612.659959	49.479732
3503.155506	490594.171901	49.484737
3503.114103	490586.023964	49.489741
3503.120699	490583.996570	49.494746
3503.121184	490581.413038	49.499751
3503.183395	490581.250747	49.504756
3503.285009	490577.435736	49.509761
3503.269947	490556.926060	49.514765
3503.372863	490544.804926	49.519770
3502.902286	490538.092226	49.524775
3503.126323	490529.598442	49.529780
3503.297433	490535.749673	49.534785
3503.258516	490508.001356	49.539789
3503.120955	490491.967807	49.544794
3503.049106	490495.118688	49.549799
3503.370609	490478.911291	49.554804
3502.908486	490479.338319	49.559809
3502.933443	490481.157108	49.564813
3503.070322	490477.741672	49.569818
3502.895043	490478.325954	49.574823
3503.364979	490458.245986	49.579828
3503.410025	490454.642474	49.584833
3503.473953	490429.713968	49.589837
3503.224975	490430.816359	49.594842
3503.255289	490423.568648	49.599847
3503.490341	490395.219761	49.604852
3502.977048	490384.512704	49.609857
3503.185245	490388.936149	49.614861
3503.230892	490380.622427	49.619866
3503.025223	490387.035834	49.624871
3503.176741	490378.857319	49.629876
3503.058834	490355.527483	49.634881
3503.055939	490344.131989	49.639885
3503.088460	490337.339713	49.644890
3502.954876	490340.297790	49.649895
3503.345875	490334.056619	49.654900
3503.211405	490341.522364	49.659905
3503.365379	490325.189370	49.664909
3503.325586	490306.050780	49.669914
3503.330483	490294.248853	49.674919
3503.268087	490290.358409	49.679924
3503.050847	490294.038765	49.684929
3503.219483	490271.321947	49.689933
3503.240672	490246.551891	49.694938
3503.077549	490248.349777	49.699943
3503.255032	490231.861047	49.704948
3503.199060	490235.971749	49.709953
3503.211358	490234.804409	49.714957
3503.081286	490204.892242	49.719962
3503.030980	490202.316684	49.724967
3503.211040	490193.323230	49.729972
3503.011842	490196.899460	49.734977
3503.277088	490187.082192	49.739981
3503.104450	490186.197309	49.744986
3503.081602	490188.884676	49.749991
3503.103971	490171.508763	49.754996
3503.122630	490164.819908	49.760001
3502.947526	490164.188648	49.765005
3503.053395	490156.776953	49.770010
3502.937500	490154.464988	49.775015
3503.238508	490159.177703	49.780020
3502.991527	490153.138585	49.785025
3502.990280	490145.895754	49.790029
3503.032426	490147.002802	49.795034
3502.817664	490130.778557	49.800039
3503.331835	490105.423939	49.805044
3502.963901	490100.568800	49.810049
3502.987412	490100.463267	49.815053
3503.126424	490102.365363	49.820058
3502.867379	490099.721484	49.825063
3503.184388	490099.822806	49.830068
3503.049492	490108.251004	49.835073
3503.210423	490095.310059	49.840077
3503.219446	490067.756102	49.845082
3503.040812	490057.907619	49.850087
3503.092738	490051.162820	49.855092
3502.990322	490053.761486	49.860097
3502.914567	490054.279406	49.865101
3502.977848	490052.496232	49.870106
3503.110005	490054.652652	49.875111
3503.363560	490031.516947	49.880116
3502.835828	490015.139471	49.885121
3502.918469	489999.222644	49.890125
3503.073547	489988.814915	49.895130
3502.835784	490003.640978	49.900135
3503.087577	489991.090781	49.905140
3503.127443	489997.870698	49.910145
3502.954787	489991.313309	49.915149
3502.986984	489991.662229	49.920154
3502.641576	489995.109660	49.925159
3503.116648	489988.146027	49.930164
3503.238302	489980.883710	49.935169
3502.929867	489958.393846	49.940173
3503.100062	489951.680969	49.945178
3502.753158	489958.977847	49.950183
3503.149491	489952.887649	49.955188
3503.025562	489951.032756	49.960193
3503.285610	489949.724952	49.965197
3503.297975	489949.722475	49.970202
3503.092416	489924.937179	49.975207
3503.243821	489900.146088	49.980212
3502.974353	489906.012617	49.985217
3503.247375	489896.447207	49.990221
3503.218371	489893.260470	49.995226
3503.070080	489896.018350	50.000231
3503.014980	489876.324618	50.005236
3502.978658	489857.944737	50.010241
3502.891974	489850.006225	50.015245
3503.157607	489852.901291	50.020250
3502.840492	489857.813059	50.025255
3503.304961	489842.848713	50.030260
3503.018203	489847.046618	50.035265
3502.873355	489840.788669	50.040269
3503.369832	489841.925233	50.045274
3502.865861	489824.378937	50.050279
3503.030719	489804.852961	50.055284
3502.995260	489796.247910	50.060289
3502.947848	489796.254879	50.065293
3503.028828	489793.303984	50.070298
3502.825675	489796.222492	50.075303
3503.064671	489794.512822	50.080308
3502.843886	489798.497721	50.085313
3502.843635	489797.028450	50.090317
3503.095914	489788.175333	50.095322
3503.084819	489787.619436	50.100327
3502.918600	489774.476731	50.105332
3503.118005	489755.806259	50.110337
3502.756175	489751.203303	50.115341
3503.012652	489749.288274	50.120346
3503.011673	489742.906260	50.125351
3503.070549	489743.048377	50.130356
3503.093173	489743.652055	50.135361
3502.877286	489743.381760	50.140365
3503.005554	489739.714311	50.145370
3502.908221	489746.009520	50.150375
3502.926447	489742.511406	50.155380
3502.681901	489742.600176	50.160385
3502.785973	489742.026079	50.165389
3502.796742	489742.226446	50.170394
3502.274717	489740.637034	50.175399
3502.866309	489732.236749	50.180404
3502.585161	489739.016840	50.185409
3502.781110	489747.747453	50.190413
3503.005180	489735.404059	50.195418
3502.895080	489738.561111	50.200423
3502.864114	489739.932977	50.205428
3502.685849	489734.591937	50.210433
3502.859036	489725.244809	50.215437
3503.239622	489700.265293	50.220442
3503.021325	489693.512420	50.225447
3503.251741	489680.104376	50.230452
3503.002396	489683.030201	50.235457
3502.806240	489684.529472	50.240461
3502.972404	489670.625094	50.245466
3502.976544	489676.752345	50.250471
3503.382234	489673.902062	50.255476
3503.275676	489664.092630	50.260481
3503.147662	489640.560909	50.265485
3503.422783	489635.097544	50.270490
3503.166597	489631.288236	50.275495
3503.337404	489626.499781	50.280500
3503.093388	489609.317389	50.285505
3502.955862	489593.232418	50.290509
3503.384438	489571.537292	50.295514
3503.315450	489588.717487	50.300519
3503.121935	489581.150283	50.305524
3502.964691	489587.657606	50.310529
3503.099828	489571.681473	50.315533
3503.199157	489554.546069	50.320538
3502.788367	489549.393667	50.325543
3503.274492	489540.250237	50.330548
3503.153506	489540.268833	50.335553
3503.042370	489544.996186	50.340557
3503.397635	489535.265651	50.345562
3502.949580	489522.927035	50.350567
3503.116695	489498.082282	50.355572
3503.095109	489501.073440	50.360577
3502.985206	489486.199579	50.365581
3503.184697	489480.697473	50.370586
3502.900906	489482.615798	50.375591
3503.057090	489479.399726	50.380596
3503.126126	489487.897272	50.385601
3503.267852	489473.338177	50.390605
3503.353552	489450.886717	50.395610
3503.034770	489444.706771	50.400615
3503.278280	489438.691208	50.405620
3503.259134	489436.718407	50.410625
3503.320357	489428.553748	50.415629
3503.104550	489411.062824	50.420634
3502.953405	489397.562930	50.425639
3503.427625	489392.523872	50.430644
3503.173213	489396.159627	50.435649
3503.126494	489392.266519	50.440653
3503.391942	489384.677355	50.445658
3503.001851	489372.228182	50.450663
3503.056601	489355.504834	50.455668
3502.903512	489358.567445	50.460673
3502.965238	489358.506519	50.465677
3502.932605	489350.052764	50.470682
3503.280316	489358.101138	50.475687
3503.093530	489346.987344	50.480692
3502.786804	489337.108075	50.485697
3502.860284	489331.271295	50.490701
3502.808287	489316.692043	50.495706
3502.743225	489317.157644	50.500711
3503.102244	489310.921190	50.505716
3502.847487	489298.298634	50.510721
3502.943917	489292.204969	50.515725
3503.160974	489287.003925	50.520730
3502.246319	489281.829776	50.525735
3502.991684	489259.881633	50.530740
3502.769586	489221.524008	50.535745
3502.871336	489188.686571	50.540749
3502.734832	489139.071064	50.545754
3502.288375	489076.183520	50.550759
3502.597935	488998.589101	50.555764
3502.248892	488919.832186	50.560769
3502.136167	488828.172387	50.565773
3502.119043	488720.542060	50.570778
3501.518222	488614.472240	50.575783
3501.543961	488499.844037	50.580788
3501.741072	488371.917325	50.585793
3501.382880	488240.531859	50.590797
3501.017765	488090.506492	50.595802
3500.662894	487951.875198	50.600807
3500.798745	487791.688385	50.605812
3500.289289	487611.796608	50.610817
3499.961850	487442.055849	50.615821
3499.899678	487260.823706	50.620826
3499.497410	487086.988573	50.625831
3499.182756	486870.334001	50.630836
3498.900503	486675.200740	50.635841
3498.618845	486472.517534	50.640845
3498.062731	486266.126909	50.645850
3497.683498	486051.702159	50.650855
3497.625399	485816.808898	50.655860
3496.998050	485593.603644	50.660865
3496.617698	485357.134579	50.665869
3496.353370	485110.157574	50.670874
3496.015561	484871.294763	50.675879
3495.588863	484621.145489	50.680884
3494.937477	484370.420525	50.685889
3494.404267	484103.714785	50.690893
3494.102949	483842.187071	50.695898
3493.468501	483578.479229	50.700903
3493.153098	483299.669844	50.705908
3492.653255	483038.466628	50.710913
3491.951606	482748.361212	50.715917
3491.860000	482467.680505	50.720922
3490.916299	482187.181077	50.725927
3490.441092	481897.533863	50.730932
3489.930630	481608.749301	50.735937
3489.771497	481308.808158	50.740941
3489.199745	481017.592375	50.745946
3488.360170	480719.624566	50.750951
3488.106124	480400.125186	50.755956
3487.446595	480092.795643	50.760961
3486.461410	479783.080404	50.765965
3486.399420	479467.994870	50.770970
3485.752027	479157.811029	50.775975
3485.037818	478846.923407	50.780980
3484.529573	478533.616514	50.785985
3483.981890	478213.266632	50.790989
3483.375617	477887.346146	50.795994
3482.293718	477566.563477	50.800999
3482.242559	477229.699001	50.806004
3481.184479	476905.455643	50.811009
3480.636683	476583.407088	50.816013
3480.386561	476251.676502	50.821018
3479.744393	475921.928385	50.826023
3479.271093	475586.116668	50.831028
3478.352541	475251.231375	50.836033
3477.789143	474909.796508	50.841037
3477.318651	474570.064559	50.846042
3476.345004	474234.157361	50.851047
3476.102622	473885.659495	50.856052
3475.587314	473550.530256	50.861057
3474.823150	473204.333533	50.866061
3474.456442	472843.823735	50.871066
3473.761485	472503.585805	50.876071
3473.237399	472163.416597	50.881076
3472.493913	471807.763961	50.886081
3471.395894	471453.023012	50.891085
3471.221206	471090.626996	50.896090
3470.116556	470751.337298	50.901095
3469.669565	470385.879422	50.906100
3468.983876	470040.833683	50.911105
3468.136505	469690.687100	50.916109
3467.733570	469334.785925	50.921114
3466.916602	468980.059522	50.926119
3466.492647	468621.513008	50.931124
3465.786052	468271.776620	50.936129
3465.041890	467911.544628	50.941133
3464.496167	467552.644105	50.946138
3463.661276	467202.960854	50.951143
3462.876254	466835.973019	50.956148
3462.149583	466474.598080	50.961153
3461.484840	466127.658990	50.966157
3460.737936	465769.419091	50.971162
3460.004238	465420.298818	50.976167
3459.178060	465060.639600	50.981172
3458.526331	464715.855916	50.986177
3457.878707	464361.379948	50.991181
3457.323127	464009.571346	50.996186
3456.551686	463669.252440	51.001191
3456.024431	463314.740102	51.006196
3455.086329	462960.438993	51.011201
3454.322431	462618.530052	51.016205
3454.108264	462266.030323	51.021210
3453.484751	461920.335049	51.026215
3452.721233	461557.614815	51.031220
3452.086904	461214.395210	51.036225
3451.387927	460854.239724	51.041229
3450.829416	460499.026776	51.046234
3450.096688	460153.624970	51.051239
3449.196755	459788.107076	51.056244
3448.662109	459435.054148	51.061249
3447.928342	459079.541498	51.066253
3446.975935	458724.564908	51.071258
3446.463775	458372.911676	51.076263
3445.987646	458022.058778	51.081268
3445.026368	457675.487411	51.086273
3444.189752	457324.883346	51.091277
3443.554806	456970.031312	51.096282
3442.729518	456624.436624	51.101287
3442.034118	456275.112670	51.106292
3441.567882	455929.247532	51.111297
3440.930461	455596.848265	51.116301
3440.156285	455243.157632	51.121306
3439.341603	454900.527898	51.126311
3438.666146	454547.926872	51.131316
3438.218431	454208.526382	51.136321
3436.771825	453863.190288	51.141325
3436.484567	453517.411985	51.146330
3435.575165	453185.426038	51.151335
3434.979354	452842.578295	51.156340
3434.456506	452499.003500	51.161345
3433.923178	452161.818474	51.166349
3433.014570	451814.742526	51.171354
3432.389421	451477.764892	51.176359
3431.846402	451125.850986	51.181364
3431.237581	450786.932411	51.186369
3430.496300	450454.728015	51.191373
3430.027755	450111.514828	51.196378
3429.027908	449779.950534	51.201383
3428.456041	449424.310804	51.206388
3427.780695	449090.655504	51.211393
3426.860455	448758.759552	51.216397
3426.046798	448415.068352	51.221402
3425.255701	448081.822890	51.226407
3425.002418	447743.818665	51.231412
3424.238416	447410.356365	51.236417
3423.211795	447071.348175	51.241421
3422.825823	446737.258306	51.246426
3421.960416	446401.463135	51.251431
3421.466933	446065.096865	51.256436
3420.825443	445745.092122	51.261441
3420.123114	445403.674038	51.266445
3419.308742	445062.421028	51.271450
3418.828994	444728.368420	51.276455
3418.173139	444398.196523	51.281460
3417.412333	444059.661595	51.286465
3416.451644	443736.990179	51.291469
3416.064168	443391.940466	51.296474
3415.183511	443072.699115	51.301479
3414.880994	442737.524802	51.306484
3413.750878	442404.862445	51.311489
3413.005446	442075.992628	51.316493
3412.369782	441745.984217	51.321498
3411.343622	441420.703293	51.326503
3410.850241	441088.074525	51.331508
3410.374801	440765.286772	51.336513
3409.368842	440446.132204	51.341517
3409.289138	440116.064626	51.346522
3408.463401	439786.161306	51.351527
3407.378290	439467.996481	51.356532
3406.829933	439139.284448	51.361537
3406.091715	438821.716436	51.366541
3405.593680	438492.074000	51.371546
3405.019509	438169.902438	51.376551
3404.058525	437843.116922	51.381556
3403.465736	437523.859256	51.386561
3402.285833	437202.278633	51.391565
3401.639088	436879.365656	51.396570
3401.064286	436575.274098	51.401575
3400.375110	436257.183289	51.406580
3399.824211	435940.615224	51.411585
3398.859571	435629.566936	51.416589
3398.496576	435308.619939	51.421594
3397.546353	434998.526345	51.426599
3396.731254	434683.025204	51.431604
3396.435725	434375.664027	51.436609
3395.589723	434065.872619	51.441613
3395.111928	433749.316396	51.446618
3394.083568	433442.186755	51.451623
3393.488922	433128.688102	51.456628
3393.000945	432820.932393	51.461633
3392.180762	432511.295813	51.466637
3391.739463	432192.302474	51.471642
3390.639549	431893.671644	51.476647
3390.137264	431581.993125	51.481652
3389.465655	431261.450419	51.486657
3388.359328	430957.071204	51.491661
3388.093028	430646.283657	51.496666
3387.479433	430344.790325	51.501671
3386.579785	430038.260089	51.506676
3385.991757	429731.575426	51.511681
3385.175199	429421.596712	51.516685
3384.929885	429115.409333	51.521690
3383.661739	428815.550921	51.526695
3383.085749	428512.481529	51.531700
3382.672039	428202.373993	51.536705
3381.361397	427895.452050	51.541709
3380.895513	427604.620770	51.546714
3380.229837	427310.618018	51.551719
3379.819942	427007.403589	51.556724
3379.113973	426706.137250	51.561729
3378.639639	426409.148335	51.566733
3377.935867	426095.709763	51.571738
3376.680735	425804.094756	51.576743
3376.358232	425502.297121	51.581748
3375.469264	425197.766501	51.586753
3374.740062	424900.750428	51.591757
3374.504963	424589.582275	51.596762
3373.386338	424294.272012	51.601767
3372.930822	423995.704238	51.606772
3372.050063	423708.198283	51.611777
3371.160196	423412.994691	51.616781
3370.631992	423114.504965	51.621786
3369.945818	422830.159384	51.626791
3369.439304	422538.670370	51.631796
3368.631789	422238.919863	51.636801
3367.954505	421947.451586	51.641805
3367.330308	421649.570757	51.646810
3366.467482	421369.759434	51.651815
3365.949787	421073.100236	51.656820
3365.404642	420788.304906	51.661825
3364.879304	420493.114040	51.666829
3364.180510	420196.956778	51.671834
3362.913072	419917.906093	51.676839
3362.120569	419620.792242	51.681844
3361.831020	419330.200574	51.686849
3360.878663	419046.315598	51.691853
3360.549503	418757.553332	51.696858
3359.862483	418471.435898	51.701863
3359.196622	418181.730224	51.706868
3358.865942	417904.137365	51.711873
3357.579656	417613.888866	51.716877
3357.445605	417317.332627	51.721882
3356.601096	417037.094207	51.726887
3355.835011	416742.410291	51.731892
3355.236886	416455.750429	51.736897
3354.622538	416161.417638	51.741901
3353.481167	415879.385595	51.746906
3353.051376	415601.455781	51.751911
3352.155440	415310.639516	51.756916
3351.674784	415023.133812	51.761921
3350.655610	414735.634174	51.766925
3350.473033	414456.968297	51.771930
3349.574057	414171.425868	51.776935
3348.988491	413898.687569	51.781940
3348.504764	413613.963320	51.786945
3347.477862	413333.158869	51.791949
3347.042457	413037.216212	51.796954
3346.071608	412765.112684	51.801959
3345.607922	412475.978477	51.806964
3344.941259	412193.962788	51.811969
3344.003913	411917.297847	51.816973
3343.838952	411634.740139	51.821978
3342.711735	411352.941727	51.826983
3341.988850	411073.287433	51.831988
3341.630283	410789.354739	51.836993
3340.868726	410513.284228	51.841997
3340.142086	410233.648086	51.847002
3339.244537	409962.523778	51.852007
3338.778851	409673.311882	51.857012
3338.408721	409405.656807	51.862017
3337.133858	409119.972737	51.867021
3336.937875	408837.647713	51.872026
3335.991859	408570.432079	51.877031
3335.272765	408295.859327	51.882036
3335.063303	408013.096762	51.887041
3333.939629	407740.616023	51.892045
3332.838610	407462.284168	51.897050
3332.401527	407183.539847	51.902055
3331.933435	406912.574576	51.907060
3331.343970	406642.744335	51.912065
3330.534143	406372.260386	51.917069
3329.971634	406093.221065	51.922074
3329.401258	405822.313231	51.927079
3328.600932	405552.633901	51.932084
3327.941183	405278.024852	51.937089
3327.243753	404999.174949	51.942093
3326.281504	404720.008607	51.947098
3325.683116	404456.794313	51.952103
3325.397827	404182.726427	51.957108
3324.687963	403910.095769	51.962113
3323.824624	403634.767438	51.967117
3323.113207	403350.593036	51.972122
3322.471334	403088.162110	51.977127
3321.841849	402817.085177	51.982132
3321.290010	402539.664694	51.987137
3320.275364	402278.633153	51.992141
3319.988546	401991.736025	51.997146
3319.240107	401732.081334	52.002151
3318.673578	401465.558237	52.007156
3318.171663	401192.515557	52.012161
3317.222606	400909.297484	52.017165
3316.857883	400639.914158	52.022170
3316.043677	400365.490393	52.027175
3315.552427	400096.859713	52.032180
3314.545179	399815.217274	52.037185
3313.605444	399547.644336	52.042189
3313.314743	399260.977775	52.047194
3312.114994	399005.465210	52.052199
3311.836061	398731.959865	52.057204
3311.101759	398466.150460	52.062209
3310.394551	398202.927557	52.067213
3309.778708	397922.681376	52.072218
3309.276595	397656.650786	52.077223
3308.511170	397379.855540	52.082228
3307.836567	397113.415702	52.087233
3306.905712	396838.167408	52.092237
3306.320344	396564.260434	52.097242
3305.558123	396306.039359	52.102247
3305.084955	396039.813328	52.107252
3304.569219	395774.227486	52.112257
3303.469405	395505.909953	52.117261
3302.933519	395229.772472	52.122266
3302.205219	394961.290174	52.127271
3301.665335	394695.013232	52.132276
3300.867583	394441.995338	52.137281
3300.135521	394176.075227	52.142285
3299.423576	393911.293949	52.147290
3298.786309	393659.821174	52.152295
3298.186871	393389.602683	52.157300
3297.506659	393125.445928	52.162305
3296.596317	392859.086138	52.167309
3296.283262	392597.536899	52.172314
3295.517805	392346.227345	52.177319
3294.739716	392072.340111	52.182324
3294.009746	391815.961424	52.187329
3293.354117	391558.221522	52.192333
3292.728767	391288.117848	52.197338
3291.990013	391042.540952	52.202343
3291.481848	390773.813225	52.207348
3290.817673	390522.093114	52.212353
3290.188715	390258.745572	52.217357
3289.560588	389997.938634	52.222362
3288.768754	389737.359077	52.227367
3287.879916	389481.522439	52.232372
3287.266842	389226.377750	52.237377
3286.764334	388971.874872	52.242381
3286.239337	388706.566858	52.247386
3285.337892	388450.267106	52.252391
3284.740318	388184.305566	52.257396
3284.126448	387916.488354	52.262401
3283.347787	387668.885587	52.267405
3282.787910	387395.766803	52.272410
3281.850531	387139.590546	52.277415
3281.120760	386883.049071	52.282420
3280.579311	386636.393474	52.287425
3279.880489	386390.498551	52.292429
3279.855024	386123.795673	52.297434
3278.534676	385861.288113	52.302439
3277.985874	385613.151839	52.307444
3277.338742	385342.065881	52.312449
3276.555771	385098.540621	52.317453
3275.937199	384838.559562	52.322458
3275.248881	384592.600091	52.327463
3274.618293	384326.183341	52.332468
3274.124468	384063.684889	52.337473
3273.282555	383822.271362	52.342477
3272.733656	383557.260355	52.347482
3272.169110	383309.009438	52.352487
3271.195868	383055.480818	52.357492
3270.590862	382789.532286	52.362497
3269.570839	382536.109297	52.367501
3269.270866	382280.180099	52.372506
3268.299583	382032.570047	52.377511
3267.777908	381784.505792	52.382516
3267.485141	381532.207297	52.387521
3266.453472	381286.992639	52.392525
3265.796916	381022.082644	52.397530
3265.020586	380780.003515	52.402535
3264.102589	380522.507098	52.407540
3263.809525	380273.837373	52.412545
3262.942217	380030.572539	52.417549
3262.272996	379776.668856	52.422554
3261.626936	379528.762323	52.427559
3261.072038	379279.262863	52.432564
3260.477204	379027.072063	52.437569
3259.367297	378781.675849	52.442573
3259.124701	378533.673761	52.447578
3258.469569	378295.120867	52.452583
3257.608828	378045.763661	52.457588
3256.988063	377795.603870	52.462593
3256.240586	377547.828037	52.467597
3255.781566	377297.207118	52.472602
3254.674358	377057.904315	52.477607
3254.125164	376796.662338	52.482612
3253.643162	376562.548376	52.487617
3252.704304	376334.279326	52.492621
3252.476931	376076.517400	52.497626
3251.607593	375833.939240	52.502631
3250.716280	375593.067357	52.507636
3250.385616	375342.032370	52.512641
3249.506189	375094.542051	52.517645
3248.801988	374856.485150	52.522650
3248.219765	374619.425062	52.527655
3247.405519	374371.792857	52.532660
3246.728188	374120.220104	52.537665
3245.642048	373895.267521	52.542669
3245.392904	373640.190012	52.547674
3245.196380	373403.341721	52.552679
3244.003117	373166.929524	52.557684
3243.680496	372920.177497	52.562689
3242.934083	372681.046271	52.567693
3242.302640	372425.716486	52.572698
3241.587086	372195.455699	52.577703
3240.819155	371951.032418	52.582708
3240.334896	371706.537413	52.587713
3239.514217	371462.424902	52.592717
3239.121752	371209.670171	52.597722
3238.386351	370979.812900	52.602727
3237.678714	370727.486728	52.607732
3236.953811	370483.633264	52.612737
3236.198371	370242.454435	52.617741
3235.451335	370003.715169	52.622746
3235.021532	369763.957671	52.627751
3234.317387	369520.909525	52.632756
3233.909311	369274.149740	52.637761
3232.901701	369032.139013	52.642765
3232.000966	368789.346804	52.647770
3231.417942	368549.225178	52.652775
3230.832649	368310.018467	52.657780
3230.299360	368064.060278	52.662785
3229.308156	367829.469120	52.667789
3229.118122	367580.960671	52.672794
3228.360229	367339.791514	52.677799
3227.670258	367099.348108	52.682804
3226.958021	366850.943573	52.687809
3226.260070	366614.391418	52.692813
3225.541496	366368.020552	52.697818
3225.101400	366122.443879	52.702823
3224.320171	365884.450801	52.707828
3224.023837	365639.688345	52.712833
3222.889914	365400.272801	52.717837
3222.301035	365148.251849	52.722842
3221.542615	364918.697112	52.727847
3220.930373	364670.493653	52.732852
3220.414988	364416.446989	52.737857
3219.567495	364180.338215	52.742861
3218.975734	363944.085999	52.747866
3218.517412	363709.745186	52.752871
3217.525154	363457.956776	52.757876
3217.269680	363211.978922	52.762881
3216.115370	362978.914887	52.767885
3215.549061	362723.085809	52.772890
3215.176186	362488.827058	52.777895
3214.143490	362245.282439	52.782900
3213.403705	362004.641806	52.787905
3212.573770	361780.553330	52.792909
3212.219351	361537.304866	52.797914
3211.463257	361302.439213	52.802919
3210.917526	361062.857203	52.807924
3210.247761	360826.092583	52.812929
3209.291001	360589.499399	52.817933
3208.951453	360340.797101	52.822938
3208.085917	360100.573785	52.827943
3207.226440	359875.819379	52.832948
3207.126055	359619.823440	52.837953
3206.093188	359392.447814	52.842957
3205.449241	359160.836423	52.847962
3204.947126	358919.659111	52.852967
3203.929529	358688.130003	52.857972
3203.533440	358458.791686	52.862977
3202.669151	358223.062879	52.867981
3202.201373	357976.633446	52.872986
3201.233484	357754.481931	52.877991
3200.743732	357514.822545	52.882996
3200.052626	357278.272953	52.888001
3199.200284	357044.699620	52.893005
3198.822831	356805.477088	52.898010
3198.166870	356571.921367	52.903015
3197.544118	356343.016225	52.908020
3197.063700	356106.300499	52.913025
3196.021693	355868.909044	52.918029
3195.783863	355625.994290	52.923034
3195.528420	355387.025619	52.928039
3194.374791	355150.742712	52.933044
3194.027415	354898.196897	52.938049
3193.072207	354663.890768	52.943053
3192.302419	354413.343452	52.948058
3191.425816	354186.301016	52.953063
3190.625070	353939.090069	52.958068
3190.381975	353703.547171	52.963073
3189.453657	353479.080148	52.968077
3188.603246	353231.339243	52.973082
3188.255284	353013.827851	52.978087
3187.332394	352778.006540	52.983092
3187.116588	352540.927097	52.988097
3186.049059	352308.867639	52.993101
3185.407181	352076.205387	52.998106
3184.768265	351839.062459	53.003111
3184.117624	351606.424976	53.008116
3183.720447	351368.758160	53.013121
3182.578659	351139.352137	53.018125
3182.289260	350905.152891	53.023130
3181.168557	350670.982311	53.028135
3180.300347	350439.570336	53.033140
3179.958548	350210.873680	53.038145
3179.417024	349986.025265	53.043149
3178.608709	349745.998486	53.048154
3178.239876	349519.110206	53.053159
3177.351846	349281.130070	53.058164
3176.742997	349052.827107	53.063169
3175.672557	348827.853977	53.068173
3175.610418	348591.699973	53.073178
3174.952933	348363.834524	53.078183
3174.001003	348131.128000	53.083188
3173.790217	347897.870591	53.088193
3172.828585	347663.458382	53.093197
3172.095680	347434.939319	53.098202
3171.393742	347211.301224	53.103207
3170.630033	346971.993480	53.108212
3170.055580	346740.901324	53.113217
3169.329857	346511.002964	53.118221
3168.762305	346282.096755	53.123226
3167.970247	346044.087664	53.128231
3167.391694	345826.176885	53.133236
3166.957105	345604.882741	53.138241
3166.032200	345368.597203	53.143245
3165.362913	345130.284933	53.148250
3164.735372	344901.357271	53.153255
3164.118897	344671.459737	53.158260
3163.749717	344435.082501	53.163265
3163.106173	344217.786843	53.168269
3162.467228	343975.214348	53.173274
3161.550789	343735.001027	53.178279
3160.812718	343503.692764	53.183284
3160.088968	343267.112400	53.188289
3159.417817	343043.682437	53.193293
3158.800940	342811.283253	53.198298
3158.068183	342585.214112	53.203303
3157.209652	342363.414864	53.208308
3156.971181	342117.233345	53.213313
3155.805628	341897.720933	53.218317
3155.369997	341670.506838	53.223322
3154.943943	341442.679473	53.228327
3153.999927	341212.769549	53.233332
3153.362325	340987.824881	53.238337
3152.680835	340767.493660	53.243341
3151.768249	340531.670703	53.248346
3151.215633	340306.175561	53.253351
3150.886695	340087.211640	53.258356
3150.387605	339848.826090	53.263361
3149.368813	339626.813240	53.268365
3148.760054	339401.781919	53.273370
3148.358977	339170.887639	53.278375
3147.591592	338940.559576	53.283380
3146.730770	338705.307060	53.288385
3146.004450	338487.291407	53.293389
3145.824993	338251.522148	53.298394
3144.815439	338025.047476	53.303399
3144.102177	337792.950269	53.308404
3143.573276	337562.528627	53.313409
3142.601564	337347.577225	53.318413
3141.879303	337114.613510	53.323418
3141.453277	336891.886486	53.328423
3140.510575	336651.319084	53.333428
3140.057366	336421.797892	53.338433
3139.131948	336207.471854	53.343437
3138.700997	335975.807241	53.348442
3138.283569	335753.966018	53.353447
3137.709191	335529.985052	53.358452
3137.454817	335298.519276	53.363457
3136.385543	335066.036050	53.368461
3135.538267	334831.862191	53.373466
3134.789999	334599.861188	53.378471
3133.798992	334382.688510	53.383476
3133.475142	334155.481211	53.388481
3132.833565	333930.436397	53.393485
3132.432972	333692.598476	53.398490
3131.760380	333470.357408	53.403495
3130.740702	333239.209407	53.408500
3130.247613	333001.358300	53.413505
3129.728380	332784.182357	53.418509
3129.071892	332549.563269	53.423514
3128.392344	332329.687283	53.428519
3128.018013	332091.865240	53.433524
3127.197973	331856.302324	53.438529
3126.223398	331628.858831	53.443533
3125.619029	331397.384539	53.448538
3124.613749	331172.286635	53.453543
3123.879722	330949.130889	53.458548
3123.908243	330707.701805	53.463553
3122.737364	330489.196318	53.468557
3122.110088	330265.945221	53.473562
3121.620531	330041.118668	53.478567
3120.883925	329808.641906	53.483572
3120.162492	329589.171589	53.488577
3119.385891	329359.856674	53.493581
3118.948505	329138.710714	53.498586
3118.233321	328906.635104	53.503591
3117.420744	328690.180770	53.508596
3117.021046	328458.664901	53.513601
3116.180758	328226.759758	53.518605
3115.567714	328005.994716	53.523610
3114.936846	327786.988575	53.528615
3114.111335	327563.022500	53.533620
3113.436954	327331.673986	53.538625
3112.713563	327108.301478	53.543629
3112.032830	326882.171908	53.548634
3111.523072	326664.671043	53.553639
3110.869806	326443.653329	53.558644
3110.290416	326210.453355	53.563649
3109.534557	325985.173286	53.568653
3108.824466	325761.260198	53.573658
3108.456021	325537.368816	53.578663
3107.430954	325312.816878	53.583668
3106.976596	325085.271529	53.588673
3106.135333	324867.589079	53.593677
3105.326898	324639.945739	53.598682
3105.002983	324407.947711	53.603687
3104.215372	324199.268096	53.608692
3103.591783	323967.443544	53.613697
3103.103274	323746.850707	53.618701
3102.360939	323511.886517	53.623706
3101.864875	323284.444647	53.628711
3100.888565	323064.385488	53.633716
3100.585842	322831.233975	53.638721
3099.530499	322607.214186	53.643725
3099.026597	322377.148613	53.648730
3098.628033	322159.185389	53.653735
3097.729204	321932.873013	53.658740
3097.328891	321700.523176	53.663745
3096.566018	321474.646406	53.668749
3095.705876	321244.659650	53.673754
3095.107452	321020.232470	53.678759
3094.326657	320792.498076	53.683764
3093.878731	320550.884639	53.688769
3093.044345	320338.714768	53.693773
3092.564109	320109.454288	53.698778
3091.553749	319875.464768	53.703783
3090.805359	319657.372489	53.708788
3090.439889	319425.927843	53.713793
3089.651722	319208.782887	53.718797
3088.650113	318982.402906	53.723802
3088.201216	318761.867659	53.728807
3087.452405	318543.187171	53.733812
3087.072695	318321.977914	53.738817
3086.128956	318101.366623	53.743821
3085.657329	317879.941706	53.748826
3085.315835	317650.704105	53.753831
3084.133436	317430.689193	53.758836
3083.575982	317202.986988	53.763841
3082.974150	316981.937071	53.768845
3082.479131	316756.846610	53.773850
3081.632288	316539.068240	53.778855
3080.653154	316324.187637	53.783860
3080.684028	316091.882797	53.788865
3079.513882	315871.047604	53.793869
3078.777552	315646.171026	53.798874
3078.182650	315419.081726	53.803879
3077.331534	315211.613736	53.808884
3077.075113	314987.958385	53.813889
3076.497637	314772.348852	53.818893
3075.722655	314544.216622	53.823898
3075.103721	314327.059440	53.828903
3074.272559	314102.016207	53.833908
3074.051735	313867.989110	53.838913
3073.292909	313644.435800	53.843917
3072.216550	313416.043215	53.848922
3071.801673	313199.615320	53.853927
3070.645701	312976.378073	53.858932
3070.512387	312753.666080	53.863937
3069.903422	312532.811362	53.868941
3069.259331	312303.966052	53.873946
3068.625809	312078.046956	53.878951
3067.427652	311862.606092	53.883956
3067.136028	311629.858526	53.888961
3066.251446	311422.108297	53.893965
3065.728824	311197.315745	53.898970
3065.210516	310970.408523	53.903975
3064.234973	310757.247557	53.908980
3063.833256	310533.554987	53.913985
3063.003868	310311.635767	53.918989
3062.340542	310080.446226	53.923994
3061.919529	309861.389945	53.928999
3060.962085	309635.364432	53.934004
3060.717035	309409.072977	53.939009
3059.610154	309199.342190	53.944013
3058.938937	308973.830346	53.949018
3058.254569	308744.271254	53.954023
3057.582175	308533.808467	53.959028
3056.879631	308314.131795	53.964033
3056.427529	308096.783339	53.969037
3055.714048	307874.128210	53.974042
3055.320445	307660.283896	53.979047
3054.620945	307427.185089	53.984052
3053.861789	307202.447848	53.989057
3053.004960	306983.098812	53.994061
3052.323304	306758.323055	53.999066
3051.846932	306535.500711	54.004071
3050.977222	306307.927278	54.009076
3050.439444	306088.551696	54.014081
3049.826350	305877.285655	54.019085
3049.216090	305657.946287	54.024090
3048.293239	305433.308268	54.029095
3047.758734	305209.627043	54.034100
3047.089295	304987.214610	54.039105
3046.451603	304775.390475	54.044109
3045.797856	304546.251920	54.049114
3045.023550	304328.158698	54.054119
3044.621355	304110.362772	54.059124
3043.870027	303890.278901	54.064129
3043.201427	303674.205191	54.069133
3042.440330	303445.591130	54.074138
3041.672050	303224.082820	54.079143
3040.946118	303009.086741	54.084148
3040.458863	302780.122701	54.089153
3039.734955	302565.227511	54.094157
3038.832074	302349.570880	54.099162
3038.440106	302133.985888	54.104167
3037.739858	301920.486654	54.109172
3037.241540	301697.583626	54.114177
3036.446229	301476.076974	54.119181
3035.686078	301253.673120	54.124186
3035.196707	301032.372081	54.129191
3034.475242	300816.353508	54.134196
3034.133771	300591.794225	54.139201
3033.269794	300374.677080	54.144205
3032.491478	300160.270989	54.149210
3031.822338	299941.339781	54.154215
3030.949036	299718.187685	54.159220
3030.544472	299489.562218	54.164225
3029.587340	299277.984580	54.169229
3029.165756	299052.442654	54.174234
3028.827132	298837.481403	54.179239
3027.721125	298624.373040	54.184244
3027.270871	298392.442653	54.189249
3026.746591	298186.245029	54.194253
3025.953995	297961.371579	54.199258
3025.473582	297729.725220	54.204263
3024.513177	297516.235934	54.209268
3024.032479	297288.816536	54.214273
3023.294569	297083.950250	54.219277
3022.656678	296855.612914	54.224282
3022.109791	296631.972275	54.229287
3020.994636	296419.575811	54.234292
3020.884210	296192.631283	54.239297
3020.255901	295974.401748	54.244301
3019.146354	295752.275263	54.249306
3019.071317	295524.076465	54.254311
3018.062559	295300.660168	54.259316
3017.607537	295082.962496	54.264321
3016.948355	294856.026858	54.269325
3016.044162	294633.179019	54.274330
3015.562603	294403.973662	54.279335
3014.769166	294189.333724	54.284340
3014.094315	293956.516653	54.289345
3013.555748	293736.742475	54.294349
3012.665782	293520.767374	54.299354
3012.155353	293295.589229	54.304359
3011.362251	293079.216356	54.309364
3010.809834	292847.015413	54.314369
3010.077652	292632.975470	54.319373
3009.502845	292405.692829	54.324378
3009.039547	292181.040934	54.329383
3008.344554	291952.936446	54.334388
3007.568215	291726.347196	54.339393
3006.389314	291506.672201	54.344397
3005.760793	291288.896382	54.349402
3005.502200	291066.350330	54.354407
3004.709281	290847.250360	54.359412
3004.157358	290625.081419	54.364417
3003.229330	290412.012815	54.369421
3002.400138	290190.498604	54.374426
3002.072992	289959.558122	54.379431
3001.548031	289750.805644	54.384436
3000.668704	289518.857059	54.389441
3000.069731	289314.394540	54.394445
2999.494786	289089.299187	54.399450
2998.443910	288873.829391	54.404455
2997.960377	288660.994706	54.409460
2997.666312	288439.878312	54.414465
2996.980528	288216.226027	54.419469
2996.214182	287981.558748	54.424474
2995.558835	287762.893015	54.429479
2994.692989	287548.437177	54.434484
2993.788023	287321.992004	54.439489
2993.275424	287116.648423	54.444493
2992.735660	286898.855193	54.449498
2991.961412	286689.452419	54.454503
2991.138347	286471.398135	54.459508
2990.869383	286242.559472	54.464513
2989.948766	286031.676859	54.469517
2989.296694	285815.046790	54.474522
2988.906972	285591.957133	54.479527
2988.109235	285380.341599	54.484532
2987.539324	285149.614319	54.489537
2987.147634	284938.978477	54.494541
2986.146459	284716.494448	54.499546
2985.582069	284488.771152	54.504551
2984.435833	284280.495579	54.509556
2984.028126	284044.954007	54.514561
2983.483236	283837.525377	54.519565
2982.348302	283614.679928	54.524570
2982.079584	283399.388672	54.529575
2981.447839	283188.611700	54.534580
2980.864325	282969.091418	54.539585
2980.042804	282760.178007	54.544589
2979.385757	282542.350078	54.549594
2978.752151	282325.588015	54.554599
2977.832507	282116.537070	54.559604
2977.560176	281892.866709	54.564609
2976.831404	281679.048304	54.569613
2976.132994	281470.318668	54.574618
2975.474048	281248.466560	54.579623
2974.405528	281041.781879	54.584628
2974.047756	280810.738848	54.589633
2973.225673	280606.536392	54.594637
2972.956441	280387.653048	54.599642
2972.345085	280173.815571	54.604647
2971.685422	279961.284564	54.609652
2971.341330	279730.340900	54.614657
2970.598027	279509.596746	54.619661
2969.847724	279285.593697	54.624666
2969.366630	279059.816141	54.629671
2968.473644	278849.588471	54.634676
2967.886367	278613.181851	54.639681
2967.008011	278400.354004	54.644685
2966.472418	278180.238857	54.649690
2965.768502	277942.118710	54.654695
2964.780258	277711.684029	54.659700
2964.496812	277486.002223	54.664705
2963.860106	277263.356093	54.669709
2962.923456	277046.207637	54.674714
2962.071061	276823.111689	54.679719
2961.831505	276603.458828	54.684724
2961.169152	276376.818119	54.689729
2960.628494	276151.813576	54.694733
2959.462009	275929.200219	54.699738
2959.145878	275709.559408	54.704743
2957.991922	275498.252010	54.709748
2957.647023	275274.286108	54.714753
2956.859192	275062.513256	54.719757
2956.227838	274838.134252	54.724762
2955.828911	274613.438308	54.729767
2955.152384	274393.829044	54.734772
2954.810205	274173.326411	54.739777
2953.698379	273961.935940	54.744781
2953.216286	273725.181168	54.749786
2952.449639	273504.058101	54.754791
2951.517493	273292.842977	54.759796
2950.898585	273064.157919	54.764801
2950.319023	272852.785155	54.769805
2949.333438	272636.815961	54.774810
2948.943899	272414.334424	54.779815
2948.008184	272208.570207	54.784820
2947.615851	271989.068970	54.789825
2946.948377	271767.803060	54.794829
2945.952796	271555.044613	54.799834
2945.395627	271324.287091	54.804839
2944.633429	271136.858259	54.809844
2944.220934	270925.230119	54.814849
2943.594672	270705.231303	54.819853
2942.852774	270487.695799	54.824858
2941.998519	270275.220856	54.829863
2941.339178	270070.686699	54.834868
2940.822708	269846.392033	54.839873
2939.885333	269640.093737	54.844877
2939.438138	269430.636246	54.849882
2938.993280	269215.116989	54.854887
2937.849389	269007.781883	54.859892
2937.390840	268794.735343	54.864897
2937.147124	268570.779915	54.869901
2936.431173	268365.694886	54.874906
2935.571235	268154.342054	54.879911
2934.926342	267940.586712	54.884916
2934.523689	267719.152634	54.889921
2933.596006	267515.272946	54.894925
2933.187453	267293.330603	54.899930
2932.376907	267074.635504	54.904935
2931.751919	266866.684173	54.909940
2930.928282	266645.775594	54.914945
2930.311699	266423.841081	54.919949
2929.929125	266217.405208	54.924954
2929.125945	265990.737884	54.929959
2928.242031	265781.758337	54.934964
2927.961543	265554.932091	54.939969
2927.107820	265342.458838	54.944973
2926.341847	265133.206249	54.949978
2925.931391	264906.630129	54.954983
2925.177674	264705.296390	54.959988
2924.421741	264472.026155	54.964993
2923.818773	264253.477843	54.969997
2923.382602	264041.295729	54.975002
2922.746517	263820.613592	54.980007
2921.849384	263607.154882	54.985012
2921.422994	263382.059320	54.990017
2920.626921	263172.456005	54.995021
2920.007903	262953.045095	55.000026
2919.406557	262724.514007	55.005031
2918.588102	262506.612092	55.010036
2917.914305	262290.164563	55.015041
2917.160251	262074.926871	55.020045
2916.130328	261860.395155	55.025050
2915.698293	261636.957070	55.030055
2914.791134	261433.102713	55.035060
2914.417131	261213.144844	55.040065
2913.728843	261007.346043	55.045069
2913.100766	260787.224962	55.050074
2912.780281	260563.719083	55.055079
2911.813088	260361.988792	55.060084
2911.183051	260137.921020	55.065089
2910.369641	259923.814858	55.070093
2909.951613	259707.557928	55.075098
2909.275562	259487.674670	55.080103
2908.622528	259280.827382	55.085108
2908.229541	259056.264566	55.090113
2907.544630	258839.108289	55.095117
2906.740441	258623.677404	55.100122
2906.220504	258399.237129	55.105127
2905.272307	258184.567977	55.110132
2904.644024	257955.382827	55.115137
2903.668537	257749.937615	55.120141
2902.986314	257530.642793	55.125146
2902.457750	257319.931845	55.130151
2901.826108	257115.400519	55.135156
2901.320042	256898.345007	55.140161
2900.622265	256678.060224	55.145165
2899.474271	256466.811428	55.150170
2899.285793	256240.639902	55.155175
2898.611010	256035.326899	55.160180
2897.851298	255820.044364	55.165185
2897.003007	255605.998494	55.170189
2896.288504	255392.823014	55.175194
2895.815256	255179.023815	55.180199
2895.093931	254971.783700	55.185204
2894.747330	254753.915613	55.190209
2893.995892	254549.456611	55.195213
2893.241557	254338.682437	55.200218
2892.821378	254108.780762	55.205223
2892.067054	253904.934087	55.210228
2891.302661	253679.798803	55.215233
2890.918818	253471.742815	55.220237
2890.101368	253254.536658	55.225242
2889.531751	253029.243972	55.230247
2888.706162	252821.233159	55.235252
2888.383565	252590.350119	55.240257
2887.574540	252372.379650	55.245261
2886.641176	252149.972435	55.250266
2886.144375	251939.160164	55.255271
2885.460591	251713.581571	55.260276
2884.955124	251503.305990	55.265281
2884.076251	251286.595772	55.270285
2883.446926	251077.460845	55.275290
2882.591125	250840.934490	55.280295
2881.477985	250629.457372	55.285300
2881.112768	250415.926664	55.290305
2880.479956	250205.800169	55.295309
2880.062147	250002.643184	55.300314
2879.475492	249788.129679	55.305319
2878.395713	249570.893213	55.310324
2878.014074	249363.987736	55.315329
2877.514340	249152.644609	55.320333
2876.945413	248931.457256	55.325338
2876.343633	248709.638757	55.330343
2875.228195	248504.887866	55.335348
2874.786903	248291.346549	55.340353
2874.127409	248071.295267	55.345357
2873.606095	247855.500736	55.350362
2872.886711	247631.053931	55.355367
2872.146508	247425.557501	55.360372
2871.495885	247212.254572	55.365377
2870.829341	246987.163720	55.370381
2870.102260	246771.887185	55.375386
2869.612307	246553.975907	55.380391
2868.774579	246346.943007	55.385396
2867.874531	246125.964996	55.390401
2867.480255	245911.808489	55.395405
2866.734051	245700.967637	55.400410
2866.541878	245476.746291	55.405415
2865.582339	245265.914401	55.410420
2865.005630	245048.426629	55.415425
2864.215824	244834.996501	55.420429
2863.585624	244614.767602	55.425434
2863.062981	244394.140052	55.430439
2862.167229	244179.327128	55.435444
2861.665912	243957.270856	55.440449
2861.130048	243742.197941	55.445453
2860.053695	243528.229557	55.450458
2859.399243	243325.883307	55.455463
2858.485108	243105.574542	55.460468
2858.176473	242886.469022	55.465473
2857.257715	242682.001083	55.470477
2856.924274	242466.465336	55.475482
2856.276193	242254.493951	55.480487
2855.185742	242033.603796	55.485492
2854.565026	241823.029388	55.490497
2854.422698	241609.018228	55.495501
2853.641052	241397.833400	55.500506
2852.995839	241182.807606	55.505511
2852.233106	240970.703788	55.510516
2851.594311	240754.786469	55.515521
2851.007645	240542.426349	55.520525
2850.234549	240329.663223	55.525530
2849.597575	240102.185830	55.530535
2848.693273	239895.453913	55.535540
2848.237268	239684.857172	55.540545
2847.661479	239482.504810	55.545549
2847.166199	239260.863462	55.550554
2846.463510	239040.375811	55.555559
2845.820298	238818.605952	55.560564
2845.110225	238594.198824	55.565569
2844.364746	238391.315047	55.570573
2843.501925	238169.046483	55.575578
2843.141993	237935.138019	55.580583
2842.110194	237733.930475	55.585588
2841.867050	237516.479687	55.590593
2841.198461	237300.446280	55.595597
2840.318768	237087.400543	55.600602
2839.771213	236865.644912	55.605607
2838.667546	236649.274264	55.610612
2838.154747	236439.125532	55.615617
2837.506165	236231.239521	55.620621
2836.696354	236023.226663	55.625626
2836.712510	235797.819090	55.630631
2835.695453	235592.004309	55.635636
2835.157015	235382.931214	55.640641
2834.393662	235166.917152	55.645645
2833.844330	234946.642727	55.650650
2833.323924	234721.602543	55.655655
2832.316494	234510.695722	55.660660
2831.927964	234286.170353	55.665665
2831.370331	234072.825148	55.670669
2830.839014	233856.777134	55.675674
2830.195627	233622.821302	55.680679
2829.302371	233415.972806	55.685684
2828.358054	233200.831891	55.690689
2827.904750	232970.539646	55.695693
2827.036688	232754.521899	55.700698
2826.276669	232537.952807	55.705703
2825.496423	232344.482138	55.710708
2824.937291	232126.532638	55.715713
2824.796274	231918.193247	55.720717
2823.725448	231696.379032	55.725722
2823.001318	231473.339168	55.730727
2822.215980	231276.281259	55.735732
2821.690659	231055.629846	55.740737
2821.308168	230833.988770	55.745741
2820.453860	230624.924919	55.750746
2819.627555	230404.933801	55.755751
2819.415837	230206.106834	55.760756
2818.686527	229985.923128	55.765761
2817.890719	229765.725022	55.770765
2817.123093	229549.444138	55.775770
2816.655562	229322.524087	55.780775
2815.888050	229117.422019	55.785780
2815.335113	228900.243003	55.790785
2814.747032	228682.153458	55.795789
2813.982468	228463.786852	55.800794
2813.258931	228248.138688	55.805799
2812.168782	228031.836176	55.810804
2811.892435	227815.074349	55.815809
2811.247911	227600.026352	55.820813
2810.259205	227392.544494	55.825818
2810.244987	227170.370426	55.830823
2809.233082	226957.113573	55.835828
2808.609032	226741.300645	55.840833
2807.856403	226529.480561	55.845837
2807.094155	226314.607203	55.850842
2806.499478	226095.875980	55.855847
2805.836340	225882.630269	55.860852
2805.113609	225669.623686	55.865857
2804.789862	225453.550101	55.870861
2803.610262	225251.985179	55.875866
2803.368475	225035.174080	55.880871
2802.659849	224819.086717	55.885876
2801.781059	224608.920984	55.890881
2801.331870	224394.626827	55.895885
2800.839746	224178.634188	55.900890
2800.389220	223948.110418	55.905895
2799.596654	223737.691426	55.910900
2798.698142	223521.548488	55.915905
2798.260255	223292.043016	55.920909
2797.519205	223081.681252	55.925914
2796.834379	222856.671654	55.930919
2795.985658	222644.469528	55.935924
2795.415950	222425.158691	55.940929
2794.636803	222214.614336	55.945933
2793.900813	221997.253248	55.950938
2793.398576	221775.858597	55.955943
2792.461294	221563.749828	55.960948
2792.048291	221353.888174	55.965953
2791.962251	221134.147990	55.970957
2790.462228	220921.429976	55.975962
2790.326134	220703.226525	55.980967
2789.403357	220479.254464	55.985972
2788.799691	220261.075411	55.990977
2788.013163	220046.044683	55.995981
2787.176453	219835.897915	56.000986
2787.014353	219613.030035	56.005991
2786.147584	219407.510032	56.010996
2785.699210	219185.796230	56.016001
2784.816849	218963.617185	56.021005
2784.523980	218746.208065	56.026010
2783.481529	218524.806734	56.031015
2782.572265	218320.747653	56.036020
2781.957222	218106.013686	56.041025
2781.558280	217889.400415	56.046029
2780.729647	217672.130278	56.051034
2780.522591	217439.322014	56.056039
2779.614003	217240.573923	56.061044
2778.933628	217024.109675	56.066049
2778.429081	216795.627573	56.071053
2777.659004	216579.713510	56.076058
2776.954296	216361.727683	56.081063
2776.340138	216150.741787	56.086068
2775.906140	215919.909267	56.091073
2775.530689	215697.965643	56.096077
2774.558147	215474.029771	56.101082
2774.138856	215246.112048	56.106087
2773.340010	215036.686241	56.111092
2772.467399	214808.701744	56.116097
2771.941464	214586.861917	56.121101
2771.015092	214368.573836	56.126106
2770.524225	214146.500786	56.131111
2769.412069	213923.877702	56.136116
2768.999958	213705.892190	56.141121
2768.553778	213480.975840	56.146125
2767.520814	213269.352410	56.151130
2766.896766	213048.882408	56.156135
2766.045839	212834.711348	56.161140
2765.330646	212613.213521	56.166145
2764.968380	212397.171834	56.171149
2764.432251	212180.763822	56.176154
2763.377017	211968.944457	56.181159
2762.766888	211751.976827	56.186164
2762.089896	211529.292931	56.191169
2761.411858	211327.089187	56.196173
2760.543156	211122.917995	56.201178
2760.144116	210901.554141	56.206183
2759.302027	210696.107314	56.211188
2758.785115	210480.847471	56.216193
2758.276538	210264.925197	56.221197
2757.738468	210054.659414	56.226202
2757.105067	209832.712745	56.231207
2756.135049	209620.938589	56.236212
2755.586364	209397.185458	56.241217
2755.015891	209179.380315	56.246221
2754.215543	208973.703409	56.251226
2753.890670	208745.768032	56.256231
2752.959058	208543.206102	56.261236
2752.187117	208331.023159	56.266241
2751.583740	208106.443352	56.271245
2750.866967	207897.562263	56.276250
2750.379216	207674.696635	56.281255
2749.591562	207459.910136	56.286260
2748.939198	207249.773814	56.291265
2748.541304	207027.379966	56.296269
2747.505995	206821.480249	56.301274
2746.983264	206604.427619	56.306279
2746.289767	206393.689910	56.311284
2745.810772	206175.219227	56.316289
2745.525768	205953.651465	56.321293
2744.317290	205748.304677	56.326298
2743.657174	205522.267204	56.331303
2743.052648	205307.688525	56.336308
2742.403354	205090.445129	56.341313
2741.814725	204881.376122	56.346317
2740.860712	204660.033717	56.351322
2740.623937	204449.765150	56.356327
2740.010969	204236.044423	56.361332
2739.237914	204020.657228	56.366337
2738.546109	203796.731322	56.371341
2738.054828	203578.679533	56.376346
2737.560728	203355.462164	56.381351
2736.758968	203135.755916	56.386356
2736.016801	202917.033717	56.391361
2735.405316	202691.037791	56.396365
2734.678063	202476.170939	56.401370
2733.993910	202252.657128	56.406375
2733.169771	202042.350455	56.411380
2732.608470	201827.205282	56.416385
2732.161102	201601.200471	56.421389
2731.121711	201385.980003	56.426394
2730.693062	201159.948568	56.431399
2729.524866	200954.230855	56.436404
2728.880186	200737.677827	56.441409
2728.726676	200524.038380	56.446413
2727.578275	200313.535102	56.451418
2727.288287	200090.171187	56.456423
2726.474171	199883.637882	56.461428
2725.956616	199667.094405	56.466433
2725.455757	199449.174810	56.471437
2724.808433	199233.518940	56.476442
2724.088566	199005.684634	56.481447
2723.293635	198792.777107	56.486452
2722.599534	198570.603277	56.491457
2722.014386	198353.286824	56.496461
2721.046429	198138.856840	56.501466
2720.399935	197923.244286	56.506471
2719.801455	197718.593900	56.511476
2719.289320	197489.486126	56.516481
2718.480013	197271.980554	56.521485
2717.670844	197074.415591	56.526490
2717.128997	196844.399146	56.531495
2716.305002	196648.543250	56.536500
2715.765247	196433.619753	56.541505
2715.489342	196209.748155	56.546509
2714.681809	195995.263341	56.551514
2714.014042	195772.295512	56.556519
2712.996251	195564.882414	56.561524
2712.283770	195360.590165	56.566529
2712.040537	195148.907933	56.571533
2711.096775	194936.968518	56.576538
2710.842694	194710.262473	56.581543
2710.052052	194506.736743	56.586548
2709.284588	194292.647156	56.591553
2708.784194	194072.892150	56.596557
2707.884361	193864.920154	56.601562
2707.840916	193641.913657	56.606567
2706.811771	193429.765042	56.611572
2706.263558	193206.967660	56.616577
2705.640227	192979.055491	56.621581
2705.017598	192768.333982	56.626586
2704.770358	192545.135626	56.631591
2703.475762	192319.902971	56.636596
2702.764615	192097.327222	56.641601
2702.303390	191876.799545	56.646605
2701.467894	191666.447256	56.651610
2701.057858	191441.994609	56.656615
2700.479899	191228.448017	56.661620
2699.778841	191000.684535	56.666625
2699.181083	190775.615798	56.671629
2698.020107	190559.454442	56.676634
2697.705207	190333.719523	56.681639
2696.651601	190117.873937	56.686644
2696.366770	189897.556305	56.691649
2695.597888	189684.504790	56.696653
2694.911749	189470.054327	56.701658
2694.570932	189239.557586	56.706663
2693.863308	189021.804616	56.711668
2693.025839	188798.182612	56.716673
2692.322392	188567.822899	56.721677
2691.766085	188359.298342	56.726682
2691.319426	188124.332724	56.731687
2690.551498	187905.487589	56.736692
2689.913249	187693.403960	56.741697
2689.392023	187458.173596	56.746701
2688.548250	187241.010204	56.751706
2687.860231	187016.266176	56.756711
2687.184533	186796.139416	56.761716
2686.245890	186566.704631	56.766721
2685.972341	186349.480542	56.771725
2685.183433	186138.572855	56.776730
2684.620062	185906.206760	56.781735
2683.436856	185681.802101	56.786740
2682.724977	185467.463131	56.791745
2682.393472	185248.726822	56.796749
2681.562372	185033.836299	56.801754
2680.794003	184805.070339	56.806759
2680.240783	184593.852587	56.811764
2679.676734	184382.688423	56.816769
2679.248747	184158.527876	56.821773
2678.474682	183953.517979	56.826778
2677.890429	183723.278114	56.831783
2676.905016	183503.801507	56.836788
2676.363295	183292.180976	56.841793
2675.508650	183060.817009	56.846797
2674.936918	182848.122052	56.851802
2674.313842	182628.923117	56.856807
2673.750211	182423.467140	56.861812
2673.133234	182198.812110	56.866817
2672.631177	181972.422719	56.871821
2671.826084	181761.652635	56.876826
2671.193205	181540.349037	56.881831
2670.468731	181322.571947	56.886836
2669.878264	181096.786237	56.891841
2669.492602	180867.700104	56.896845
2668.265052	180652.219412	56.901850
2667.510417	180432.988716	56.906855
2667.108774	180216.806961	56.911860
2666.496936	179991.348407	56.916865
2665.832627	179775.566639	56.921869
2664.804174	179564.219336	56.926874
2664.378413	179343.708256	56.931879
2663.850369	179124.677308	56.936884
2662.953686	178908.720485	56.941889
2662.627627	178684.991615	56.946893
2661.865515	178477.779611	56.951898
2661.297150	178252.552318	56.956903
2660.544517	178039.171925	56.961908
2659.724187	177817.026855	56.966913
2659.287320	177595.763460	56.971917
2658.192424	177375.724771	56.976922
2657.661804	177153.728118	56.981927
2657.074233	176941.281118	56.986932
2656.070829	176721.040601	56.991937
2655.952927	176515.351593	56.996941
2655.055268	176294.053623	57.001946
2654.476654	176076.865415	57.006951
2653.920222	175863.185264	57.011956
2653.187157	175647.282959	57.016961
2652.581423	175419.622163	57.021965
2651.622643	175202.282572	57.026970
2651.085140	174993.284445	57.031975
2650.522936	174786.491619	57.036980
2649.545299	174568.814986	57.041985
2648.802743	174347.210431	57.046989
2648.611767	174134.638807	57.051994
2647.955980	173915.553829	57.056999
2647.292650	173707.904956	57.062004
2646.664884	173489.148530	57.067009
2646.328648	173261.431708	57.072013
2645.403565	173045.955197	57.077018
2644.852184	172825.956635	57.082023
2644.166372	172601.453001	57.087028
2643.666427	172375.865608	57.092033
2643.093555	172152.592963	57.097037
2642.212364	171931.036433	57.102042
2641.458723	171714.357225	57.107047
2640.285592	171488.589013	57.112052
2639.852007	171269.407060	57.117057
2639.502713	171043.905137	57.122061
2638.472749	170838.364109	57.127066
2637.817030	170616.130675	57.132071
2637.480575	170401.376515	57.137076
2636.566896	170183.828184	57.142081
2635.935640	169957.881221	57.147085
2635.358858	169747.517972	57.152090
2634.760687	169517.994853	57.157095
2633.867461	169309.744251	57.162100
2633.364804	169092.747342	57.167105
2632.575160	168865.305836	57.172109
2631.836679	168657.835397	57.177114
2631.431556	168434.582885	57.182119
2630.685288	168223.199332	57.187124
2629.845334	168010.382118	57.192129
2629.620591	167785.527986	57.197133
2628.524286	167569.956246	57.202138
2628.072400	167352.172757	57.207143
2627.239220	167136.040437	57.212148
2626.685445	166921.708919	57.217153
2626.420251	166690.865709	57.222157
2625.265239	166480.650190	57.227162
2624.742382	166261.625360	57.232167
2624.020377	166042.480767	57.237172
2623.332896	165825.747968	57.242177
2622.683201	165607.738878	57.247181
2621.561525	165407.442284	57.252186
2621.380699	165184.631213	57.257191
2620.925457	164975.127102	57.262196
2619.704311	164765.211463	57.267201
2619.348984	164537.650962	57.272205
2618.701324	164324.773330	57.277210
2617.670832	164112.148301	57.282215
2617.011381	163893.883829	57.287220
2616.499400	163681.713181	57.292225
2615.661786	163483.123976	57.297229
2615.272361	163200.979505	57.302234
2615.148404	162984.466551	57.307239
2614.284372	162773.730135	57.312244
2613.485837	162542.997287	57.317249
2613.208891	162322.481999	57.322253
2612.042922	162112.725414	57.327258
2611.716596	161889.690422	57.332263
2610.868975	161679.911350	57.337268
2610.232056	161452.096857	57.342273
2609.701168	161225.868986	57.347277
2608.716491	161017.526760	57.352282
2608.091822	160801.983482	57.357287
2607.498383	160583.143668	57.362292
2606.779701	160367.948466	57.367297
2606.085104	160151.479380	57.372301
2605.650332	159936.852068	57.377306
2604.980117	159717.406779	57.382311
2604.171529	159500.756310	57.387316
2603.616131	159284.677303	57.392321
2603.408475	159061.717480	57.397325
2602.143037	158853.178182	57.402330
2601.913266	158621.605082	57.407335
2601.403322	158402.066322	57.412340
2600.597040	158187.622947	57.417345
2599.942810	157962.872052	57.422349
2599.022221	157748.729169	57.427354
2598.791824	157512.459774	57.432359
2598.019114	157278.617033	57.437364
2597.254068	157067.123375	57.442369
2596.547798	156840.773493	57.447373
2595.570136	156631.413750	57.452378
2595.082759	156400.366623	57.457383
2594.581649	156181.959206	57.462388
2593.423120	155970.026134	57.467393
2593.086152	155741.845276	57.472397
2592.397504	155529.077769	57.477402
2591.683684	155306.044333	57.482407
2590.814421	155092.202229	57.487412
2590.065002	154872.825575	57.492417
2589.627309	154658.333088	57.497421
2588.757025	154436.003874	57.502426
2588.334214	154219.719473	57.507431
2587.579703	154003.056820	57.512436
2586.933455	153795.886508	57.517441
2586.239176	153574.107105	57.522445
2585.672156	153361.956806	57.527450
2585.128883	153144.007817	57.532455
2584.369383	152932.424603	57.537460
2583.511637	152710.651396	57.542465
2583.173366	152487.017843	57.547469
2582.461059	152280.019917	57.552474
2581.829061	152058.850830	57.557479
2581.083777	151830.163770	57.562484
2580.358344	151625.472634	57.567489
2580.203760	151394.496077	57.572493
2579.210707	151181.016337	57.577498
2578.566549	150960.072610	57.582503
2577.633364	150742.658754	57.587508
2577.195994	150531.535554	57.592513
2576.535841	150306.556948	57.597517
2575.582749	150088.527801	57.602522
2574.971043	149871.882238	57.607527
2574.268221	149653.740090	57.612532
2573.445648	149446.688519	57.617537
2572.769227	149235.077783	57.622541
2572.247709	149015.703786	57.627546
2571.953170	148803.196540	57.632551
2571.245454	148588.099899	57.637556
2570.182404	148386.507404	57.642561
2569.858425	148151.983946	57.647565
2569.115117	147945.577615	57.652570
2568.426476	147726.124498	57.657575
2567.650868	147508.326117	57.662580
2567.089810	147290.444392	57.667585
2566.686127	147074.242194	57.672589
2565.973072	146857.861724	57.677594
2565.444821	146627.372340	57.682599
2564.516786	146415.527782	57.687604
2563.944044	146195.888930	57.692609
2563.536846	145969.947466	57.697613
2562.746297	145761.643834	57.702618
2561.762872	145535.072415	57.707623
2561.412116	145314.769118	57.712628
2560.232151	145105.667383	57.717633
2559.815215	144880.675673	57.722637
2559.027969	144673.064964	57.727642
2558.336221	144452.135540	57.732647
2557.842198	144244.646421	57.737652
2557.004802	144035.103639	57.742657
2556.869594	143808.168893	57.747661
2555.652267	143592.894702	57.752666
2555.344512	143375.355778	57.757671
2554.550411	143153.041304	57.762676
2553.384107	142941.575714	57.767681
2553.137803	142725.848739	57.772685
2552.343828	142520.337455	57.777690
2551.914639	142302.024806	57.782695
2551.547314	142086.143599	57.787700
2550.516845	141879.466940	57.792705
2550.023825	141649.148576	57.797709
2549.283200	141435.745351	57.802714
2548.486348	141214.525408	57.807719
2547.871972	141010.342689	57.812724
2547.210944	140794.517156	57.817729
2546.638980	140583.278655	57.822733
2545.806203	140360.584013	57.827738
2545.315308	140138.395901	57.832743
2544.838411	139931.454195	57.837748
2543.932275	139714.976384	57.842753
2543.779568	139496.373258	57.847757
2542.559668	139284.585823	57.852762
2541.739407	139054.288233	57.857767
2541.422659	138847.938475	57.862772
2540.818047	138637.824169	57.867777
2539.968755	138416.340854	57.872781
2539.202201	138198.339975	57.877786
2538.916097	137970.710407	57.882791
2538.403739	137757.843413	57.887796
2537.202770	137535.685500	57.892801
2537.099451	137310.776271	57.897805
2535.980947	137101.948499	57.902810
2535.307168	136887.334699	57.907815
2534.661479	136669.757877	57.912820
2533.857457	136456.425594	57.917825
2533.352096	136237.394146	57.922829
2532.864747	136032.552022	57.927834
2532.020592	135804.011265	57.932839
2531.488125	135585.217662	57.937844
2530.837981	135380.710795	57.942849
2530.136988	135160.879953	57.947853
2529.186719	134947.988373	57.952858
2528.688937	134721.281368	57.957863
2528.148298	134506.727463	57.962868
2527.507691	134297.856706	57.967873
2526.789930	134080.844157	57.972877
2526.105768	133855.659752	57.977882
2525.512338	133638.795969	57.982887
2524.967333	133423.971333	57.987892
2523.929520	133215.603260	57.992897
2523.595116	132988.972896	57.997901
2523.009912	132782.289243	58.002906
2522.352904	132559.359083	58.007911
2521.639246	132343.095769	58.012916
2520.719530	132129.267510	58.017921
2520.336135	131896.454783	58.022925
2519.456563	131692.823424	58.027930
2518.665669	131469.198986	58.032935
2518.219656	131259.646346	58.037940
2517.241750	131049.201490	58.042945
2516.972634	130836.791413	58.047949
2516.272102	130614.518515	58.052954
2515.421540	130395.256037	58.057959
2514.754644	130181.097598	58.062964
2513.977679	129967.212263	58.067969
2513.541933	129750.302367	58.072973
2512.873513	129538.473428	58.077978
2512.324279	129324.506110	58.082983
2511.870577	129112.824189	58.087988
2511.056269	128888.322219	58.092993
2510.399176	128663.124000	58.097997
2509.670271	128452.494080	58.103002
2509.275367	128230.280609	58.108007
2508.243937	128006.810826	58.113012
2507.428063	127792.262528	58.118017
2507.028067	127570.867990	58.123021
2506.133725	127362.761858	58.128026
2505.768944	127144.565634	58.133031
2505.439755	126933.388648	58.138036
2504.542626	126711.305097	58.143041
2504.072835	126494.527675	58.148045
2503.149297	126259.701292	58.153050
2502.503448	126054.613650	58.158055
2501.712602	125831.110739	58.163060
2501.327143	125612.231524	58.168065
2500.361269	125380.645085	58.173069
2499.732780	125170.011732	58.178074
2499.097074	124956.498446	58.183079
2498.577741	124722.472118	58.188084
2497.692047	124523.986749	58.193089
2497.052299	124299.024831	58.198093
2496.277683	124076.752900	58.203098
2495.702936	123865.143393	58.208103
2495.194180	123642.134493	58.213108
2494.060075	123427.429740	58.218113
2493.831734	123202.983222	58.223117
2492.994089	122991.434963	58.228122
2492.446373	122787.270845	58.233127
2492.028234	122566.453320	58.238132
2491.381066	122349.648370	58.243137
2490.695388	122131.518016	58.248141
2489.909882	121911.995825	58.253146
2489.161090	121685.854172	58.258151
2488.196918	121471.328710	58.263156
2487.693237	121255.767008	58.268161
2487.181640	121028.958507	58.273165
2486.375867	120816.940018	58.278170
2485.780512	120605.232711	58.283175
2485.179086	120383.256201	58.288180
2484.520448	120166.305901	58.293185
2483.956106	119941.546630	58.298189
2483.081196	119731.300012	58.303194
2482.709176	119500.343464	58.308199
2481.969270	119295.367075	58.313204
2480.780864	119083.994577	58.318209
2480.742745	118856.577531	58.323213
2479.768381	118650.697500	58.328218
2478.910131	118432.847372	58.333223
2478.252638	118213.596097	58.338228
2477.619284	117991.695771	58.343233
2476.993261	117783.818610	58.348237
2476.397503	117565.267657	58.353242
2475.824316	117360.889517	58.358247
2475.058736	117145.892037	58.363252
2474.084061	116928.625294	58.368257
2474.220382	116705.757120	58.373261
2473.170417	116495.170953	58.378266
2472.429376	116289.501299	58.383271
2472.123275	116064.258683	58.388276
2471.217648	115851.077883	58.393281
2470.864778	115631.381416	58.398285
2469.673598	115418.738231	58.403290
2469.349813	115193.925022	58.408295
2469.001042	114975.566481	58.413300
2467.983455	114764.361109	58.418305
2467.686004	114542.995973	58.423309
2466.655341	114330.266653	58.428314
2466.224178	114114.283331	58.433319
2465.779693	113880.177239	58.438324
2464.946502	113670.379837	58.443329
2464.383861	113441.957923	58.448333
2463.268639	113225.500384	58.453338
2462.545463	112995.381664	58.458343
2462.181594	112774.816882	58.463348
2461.548880	112566.545508	58.468353
2460.860655	112330.594872	58.473357
2460.337085	112119.003405	58.478362
2459.268729	111904.453807	58.483367
2458.608417	111675.847721	58.488372
2458.187351	111460.323573	58.493377
2457.141679	111242.209489	58.498381
2456.868655	111030.365460	58.503386
2456.036580	110812.703615	58.508391
2455.348140	110600.370647	58.513396
2454.350926	110388.005945	58.518401
2454.202042	110158.279375	58.523405
2453.327896	109944.103092	58.528410
2452.502771	109742.955251	58.533415
2452.035604	109510.029764	58.538420
2451.488745	109306.791709	58.543425
2450.940829	109081.923121	58.548429
2450.164055	108863.438481	58.553434
2449.654296	108640.427169	58.558439
2449.253475	108416.271131	58.563444
2448.188224	108202.832032	58.568449
2447.803788	107972.071886	58.573453
2447.134690	107756.264202	58.578458
2446.016693	107536.113281	58.583463
2445.559314	107319.178201	58.588468
2445.033072	107105.479314	58.593473
2444.344798	106872.284150	58.598477
2443.711597	106658.009736	58.603482
2442.822183	106428.162852	58.608487
2442.431730	106214.088676	58.613492
2441.676367	105996.540155	58.618497
2441.170130	105763.238052	58.623501
2440.449540	105550.789279	58.628506
2439.732254	105324.548526	58.633511
2439.309986	105106.580955	58.638516
2438.347155	104881.906020	58.643521
2438.017438	104656.841009	58.648525
2437.264739	104443.468189	58.653530
2436.558904	104214.983868	58.658535
2435.860852	103977.853197	58.663540
2434.810229	103766.310091	58.668545
2434.028334	103545.089430	58.673549
2433.602424	103333.933332	58.678554
2433.033559	103115.842309	58.683559
2432.688303	102893.004242	58.688564
2431.819809	102673.670615	58.693569
2431.445359	102446.724159	58.698573
2430.579238	102227.578289	58.703578
2429.781057	101995.920084	58.708583
2429.295957	101761.455023	58.713588
2428.451489	101543.434957	58.718593
2428.057758	101327.514995	58.723597
2427.310852	101101.078313	58.728602
2426.505902	100877.203110	58.733607
2426.281817	100659.803437	58.738612
2425.372120	100431.400887	58.743617
2424.767088	100197.230636	58.748621
2424.029538	99981.142954	58.753626
2423.465832	99755.318323	58.758631
2422.534268	99523.667789	58.763636
2421.905958	99309.725722	58.768641
2421.092696	99079.672028	58.773645
2420.652111	98856.938389	58.778650
2419.963613	98634.379400	58.783655
2419.421070	98414.197013	58.788660
2418.631506	98187.820969	58.793665
2418.317031	97963.008268	58.798669
2417.320952	97732.489626	58.803674
2416.449547	97505.828850	58.808679
2415.880256	97280.999816	58.813684
2415.207544	97069.102591	58.818689
2414.688475	96844.783634	58.823693
2414.190307	96632.120751	58.828698
2413.600149	96398.120068	58.833703
2413.190759	96166.471463	58.838708
2412.032386	95948.382905	58.843713
2411.564876	95713.145820	58.848717
2410.904920	95492.636091	58.853722
2410.132895	95261.130340	58.858727
2409.577502	95033.505559	58.863732
2408.722953	94812.792331	58.868737
2408.294291	94578.359991	58.873741
2407.599533	94351.601311	58.878746
2406.973462	94116.203102	58.883751
2406.179415	93888.602383	58.888756
2405.663317	93673.040447	58.893761
2405.015183	93431.539747	58.898765
2404.411237	93212.863517	58.903770
2403.390298	92984.426530	58.908775
2402.986821	92753.306794	58.913780
2401.891098	92532.736737	58.918785
2401.518072	92302.568035	58.923789
2400.905247	92079.801667	58.928794
2400.128619	91852.244370	58.933799
2399.642792	91631.041287	58.938804
2398.659296	91406.831318	58.943809
2398.209928	91186.267335	58.948813
2397.426367	90956.063589	58.953818
2396.942774	90730.240469	58.958823
2396.360937	90500.738684	58.963828
2395.780927	90291.072134	58.968833
2394.819565	90057.234831	58.973837
2394.279906	89829.755984	58.978842
2393.667046	89607.737439	58.983847
2393.036233	89376.517948	58.988852
2392.346823	89153.114964	58.993857
2391.730441	88914.480067	58.998861
2391.104596	88697.094796	59.003866
2390.152150	88469.898447	59.008871
2389.706937	88234.312436	59.013876
2388.780929	88010.388107	59.018881
2388.298072	87794.815086	59.023885
2387.339752	87566.513337	59.028890
2386.915451	87341.318197	59.033895
2386.315744	87117.643014	59.038900
2385.218130	86900.192083	59.043905
2384.893639	86671.285835	59.048909
2384.535711	86440.320681	59.053914
2383.648483	86214.196409	59.058919
2382.899172	85992.521837	59.063924
2382.208321	85765.128677	59.068929
2381.566531	85531.194521	59.073933
2381.190055	85315.173074	59.078938
2380.257962	85086.145531	59.083943
2379.347480	84856.394386	59.088948
2378.712960	84647.247634	59.093953
2377.959024	84416.943954	59.098957
2377.792481	84193.541268	59.103962
2376.606927	83976.406599	59.108967
2376.352491	83748.103737	59.113972
2375.428758	83532.833691	59.118977
2374.858882	83304.230666	59.123981
2374.488194	83088.896486	59.128986
2373.406326	82865.342342	59.133991
2373.063073	82638.574073	59.138996
2372.282452	82423.032800	59.144001
2371.756209	82190.479908	59.149005
2371.025213	81969.427594	59.154010
2370.040470	81744.367861	59.159015
2369.717363	81526.633705	59.164020
2368.844750	81307.423475	59.169025
2368.340222	81076.514677	59.174029
2367.896751	80860.416340	59.179034
2366.818001	80636.631975	59.184039
2366.116338	80409.469344	59.189044
2365.400967	80202.458337	59.194049
2364.634143	79981.160250	59.199053
2364.465526	79748.400423	59.204058
2363.625809	79524.596486	59.209063
2362.983282	79315.808335	59.214068
2362.056155	79090.166142	59.219073
2361.895005	78871.204705	59.224077
2360.988943	78646.920161	59.229082
2360.337451	78433.541661	59.234087
2359.499798	78199.130997	59.239092
2358.768237	77978.438113	59.244097
2358.043130	77768.683847	59.249101
2357.588281	77542.286710	59.254106
2356.698945	77322.836204	59.259111
2356.382573	77105.641748	59.264116
2355.488964	76889.542278	59.269121
2355.083957	76666.087074	59.274125
2354.376729	76446.224256	59.279130
2353.544751	76219.603753	59.284135
2353.045825	75999.782433	59.289140
2352.017986	75790.071145	59.294145
2351.618507	75563.908952	59.299149
2350.836406	75340.813214	59.304154
2350.169059	75130.848840	59.309159
2349.831634	74909.195318	59.314164
2348.849093	74698.037239	59.319169
2348.618690	74472.988208	59.324173
2347.865579	74245.534634	59.329178
2347.136839	74027.595846	59.334183
2346.630739	73801.755384	59.339188
2346.014686	73586.901585	59.344193
2345.084792	73363.794132	59.349197
2344.644407	73135.657330	59.354202
2344.044145	72918.229714	59.359207
2343.376872	72694.416545	59.364212
2342.665862	72463.466806	59.369217
2342.010951	72233.486443	59.374221
2341.222895	72022.034290	59.379226
2340.754872	71797.528086	59.384231
2340.165587	71560.994795	59.389236
2339.386795	71341.173772	59.394241
2338.671795	71111.291925	59.399245
2338.021068	70884.424163	59.404250
2337.159261	70675.588896	59.409255
2336.538567	70449.031756	59.414260
2335.846637	70228.772232	59.419265
2335.388564	69995.505385	59.424269
2334.269675	69774.051765	59.429274
2333.838920	69560.263583	59.434279
2333.566927	69332.422488	59.439284
2332.496071	69113.508670	59.444289
2331.941431	68881.651161	59.449293
2331.251098	68660.902222	59.454298
2330.652638	68446.513033	59.459303
2330.087358	68215.108468	59.464308
2329.263932	68000.291142	59.469313
2328.718106	67767.026699	59.474317
2328.031486	67548.842177	59.479322
2327.188537	67335.396983	59.484327
2326.722055	67101.133581	59.489332
2325.887605	66888.629286	59.494337
2325.311256	66667.137515	59.499341
2324.892014	66440.987480	59.504346
2323.893008	66218.735032	59.509351
2323.289185	65984.307402	59.514356
2322.732792	65778.398715	59.519361
2321.790569	65551.696034	59.524365
2321.275469	65317.737397	59.529370
2320.327051	65110.479448	59.534375
2320.170316	64879.964982	59.539380
2319.473534	64666.598898	59.544385
2318.953962	64438.810105	59.549389
2317.998022	64229.805578	59.554394
2317.529391	63996.359090	59.559399
2316.999063	63766.689780	59.564404
2315.840854	63554.286266	59.569409
2315.313000	63329.665433	59.574413
2314.687388	63107.003525	59.579418
2314.225713	62895.035143	59.584423
2313.391894	62667.925154	59.589428
2312.667284	62449.744309	59.594433
2312.134213	62220.508801	59.599437
2311.901892	62004.183049	59.604442
2311.162695	61782.403115	59.609447
2310.061054	61554.639773	59.614452
2309.097687	61326.271589	59.619457
2308.992149	61097.266806	59.624461
2308.341830	60878.854855	59.629466
2307.287098	60659.724479	59.634471
2307.008899	60431.388283	59.639476
2306.206216	60209.880645	59.644481
2305.801049	59980.101241	59.649485
2304.688405	59762.820171	59.654490
2304.006639	59540.661831	59.659495
2303.452480	59312.715364	59.664500
2302.805665	59102.847938	59.669505
2302.113050	58873.311276	59.674509
2301.371915	58664.609577	59.679514
2300.643125	58442.228019	59.684519
2300.464830	58206.822426	59.689524
2299.315802	57987.671812	59.694529
2298.732484	57767.566837	59.699533
2298.053925	57548.137912	59.704538
2297.177049	57342.555377	59.709543
2296.931514	57108.687258	59.714548
2295.859127	56902.048677	59.719553
2295.473183	56675.829593	59.724557
2294.935277	56469.744087	59.729562
2293.762197	56250.747601	59.734567
2293.163046	56030.219546	59.739572
2292.881231	55808.691206	59.744577
2291.971059	55602.820001	59.749581
2291.169777	55378.736623	59.754586
2290.520014	55168.436348	59.759591
2289.981043	54948.952901	59.764596
2289.187901	54735.765673	59.769601
2288.728093	54508.613405	59.774605
2288.106570	54286.280715	59.779610
2287.332350	54093.363714	59.784615
2286.807304	53870.368900	59.789620
2285.927844	53653.790353	59.794625
2285.563249	53427.902203	59.799629
2284.852373	53213.669126	59.804634
2284.064122	53003.792289	59.809639
2283.658448	52786.848326	59.814644
2282.474048	52573.897144	59.819649
2282.172863	52347.907945	59.824653
2281.460490	52135.978713	59.829658
2280.547258	51927.365018	59.834663
2280.037176	51709.346233	59.839668
2279.497635	51494.577909	59.844673
2278.640914	51276.875603	59.849677
2278.090505	51055.381204	59.854682
2277.254954	50851.399703	59.859687
2276.936084	50627.776157	59.864692
2275.612981	50418.770337	59.869697
2275.395953	50204.526271	59.874701
2274.878974	49984.457166	59.879706
2274.324054	49774.220232	59.884711
2273.622622	49558.966036	59.889716
2272.951332	49355.741122	59.894721
2272.307961	49127.154344	59.899725
2271.379807	48912.421601	59.904730
2270.496284	48697.801421	59.909735
2270.120905	48484.586944	59.914740
2269.035928	48276.729442	59.919745
2268.464571	48058.837549	59.924750
2267.895622	47857.995574	59.929754
2266.989164	47642.426934	59.934759
2266.810892	47439.730948	59.939764
2265.919961	47237.646927	59.944769
2265.008035	47025.999666	59.949774
2264.971549	46810.394940	59.954778
2263.998633	46588.333440	59.959783
2263.374396	46372.852565	59.964788
2262.378089	46174.340153	59.969793
2262.020841	45964.430134	59.974798
2261.230592	45755.957715	59.979802
2260.514048	45542.415284	59.984807
2260.163515	45327.359284	59.989812
2259.144960	45140.653598	59.994817
2258.291940	44932.640562	59.999822
2257.982941	44716.114732	60.004826
2256.952137	44516.019827	60.009831
2256.202890	44300.656962	60.014836
2255.730532	44103.425934	60.019841
2255.253379	43903.430530	60.024846
2254.399002	43702.535790	60.029850
2253.670116	43495.225470	60.034855
2253.097763	43277.095716	60.039860
2252.403490	43085.695781	60.044865
2252.117349	42882.848169	60.049870
2251.042249	42684.745262	60.054874
2250.108905	42478.153116	60.059879
2249.529176	42265.587338	60.064884
2249.037633	42062.361303	60.069889
2248.722110	41862.667364	60.074894
2247.813486	41666.927788	60.079898
2247.118568	41463.393200	60.084903
2246.483608	41251.778359	60.089908
2245.828728	41060.318699	60.094913
2245.456502	40856.901374	60.099918
2244.550088	40653.466819	60.104922
2243.949684	40447.197198	60.109927
2243.401573	40240.697259	60.114932
2242.874390	40033.213107	60.119937
2241.872977	39825.164796	60.124942
2241.080075	39626.581189	60.129946
2240.558705	39422.847227	60.134951
2240.137308	39225.001422	60.139956
2239.208296	39024.527159	60.144961
2238.574498	38825.644653	60.149966
2238.035225	38620.844940	60.154970
2236.696884	38423.082718	60.159975
2236.502534	38217.275166	60.164980
2235.490975	38010.894663	60.169985
2234.790382	37822.350850	60.174990
2234.232779	37619.023605	60.179994
2233.676571	37431.768536	60.184999
2233.150149	37245.149431	60.190004
2232.256165	37043.096453	60.195009
2231.667939	36844.814793	60.200014
2230.844668	36642.208472	60.205018
2229.921045	36460.015809	60.210023
2229.781631	36258.763012	60.215028
2228.910232	36075.816993	60.220033
2228.245193	35877.348665	60.225038
2227.677068	35678.736119	60.230042
2226.968631	35490.870783	60.235047
2226.496127	35300.969148	60.240052
2225.493938	35117.515334	60.245057
2224.828943	34920.894887	60.250062
2224.326330	34725.226165	60.255066
2222.994944	34542.869245	60.260071
2222.622017	34345.667128	60.265076
2222.039408	34163.404219	60.270081
2221.530054	33967.313972	60.275086
2220.482244	33784.724386	60.280090
2219.426455	33601.076041	60.285095
2219.186533	33421.761738	60.290100
2218.358000	33239.181287	60.295105
2217.544685	33056.116843	60.300110
2217.159197	32872.966019	60.305114
2216.297788	32709.507503	60.310119
2215.646318	32528.836339	60.315124
2215.029400	32351.605087	60.320129
2214.134577	32173.609132	60.325134
2213.283614	31998.119141	60.330138
2212.221581	31837.818868	60.335143
2211.889030	31666.003225	60.340148
2210.610955	31505.250578	60.345153
2209.649269	31342.120134	60.350158
2209.212672	31189.444568	60.355162
2208.058053	31045.380769	60.360167
2207.284022	30891.908195	60.365172
2206.729652	30754.731209	60.370177
2205.494354	30605.085684	60.375182
2204.767763	30476.907037	60.380186
2203.764335	30344.500747	60.385191
2203.239453	30204.662814	60.390196
2202.174537	30095.244123	60.395201
2201.542827	29964.979806	60.400206
2200.733816	29840.129408	60.405210
2200.182432	29722.919601	60.410215
2199.534588	29602.701786	60.415220
2198.649258	29479.441517	60.420225
2198.030784	29356.727609	60.425230
2197.609109	29244.186909	60.430234
2196.660039	29132.289938	60.435239
2196.225586	29009.032805	60.440244
2195.304958	28905.449770	60.445249
2194.695676	28789.515056	60.450254
2194.205606	28669.694605	60.455258
2193.658000	28557.459838	60.460263
2193.037770	28442.459896	60.465268
2192.378730	28329.865195	60.470273
2191.846044	28216.345962	60.475278
2191.241512	28090.108341	60.480282
2190.392333	27979.848086	60.485287
2190.192355	27867.348081	60.490292
2189.184251	27752.234436	60.495297
2188.780618	27637.472825	60.500302
2188.286830	27513.296429	60.505306
2187.505541	27397.337304	60.510311
2187.016117	27277.211050	60.515316
2185.912513	27162.072509	60.520321
2185.482436	27028.490051	60.525326
2184.806398	26908.498814	60.530330
2184.076466	26798.733200	60.535335
2183.590534	26677.097451	60.540340
2182.675325	26559.805421	60.545345
2182.312474	26448.459535	60.550350
2181.841292	26332.685543	60.555354
2180.962881	26216.682361	60.560359
2180.376351	26089.574429	60.565364
2179.815926	25976.809045	60.570369
2179.113015	25857.479910	60.575374
2178.358136	25730.419678	60.580378
2177.472615	25620.842350	60.585383
2177.260506	25496.057840	60.590388
2176.500387	25387.609009	60.595393
2175.831952	25275.600183	60.600398
2175.239341	25157.118835	60.605402
2174.347385	25038.525515	60.610407
2174.104466	24914.065531	60.615412
2173.283254	24794.194411	60.620417
2172.478153	24673.104602	60.625422
2172.279640	24552.175377	60.630426
2171.369289	24438.302705	60.635431
2170.977450	24300.129374	60.640436
2170.196580	24193.103981	60.645441
2169.421760	24076.918971	60.650446
2168.733271	23945.228958	60.655450
2168.073751	23821.660119	60.660455
2167.621420	23703.102515	60.665460
2166.705604	23591.923363	60.670465
2165.884707	23467.891658	60.675470
2165.466353	23339.219171	60.680474
2164.460037	23223.581709	60.685479
2164.303651	23099.625937	60.690484
2163.389007	22984.827742	60.695489
2162.154935	22869.695682	60.700494
2161.708752	22754.388152	60.705498
2161.307194	22634.127124	60.710503
2160.534205	22526.531265	60.715508
2159.885245	22413.345445	60.720513
2159.051466	22294.491642	60.725518
2158.788966	22177.198465	60.730522
2157.555424	22071.355158	60.735527
2157.554484	21954.988651	60.740532
2156.475243	21845.310036	60.745537
2155.813003	21725.338077	60.750542
2155.376201	21618.410449	60.755546
2154.645064	21503.220378	60.760551
2154.276809	21383.911863	60.765556
2153.511093	21265.989870	60.770561
2152.843893	21144.160443	60.775566
2152.446267	21034.278266	60.780570
2151.417993	20915.107198	60.785575
2151.162759	20795.606751	60.790580
2150.477932	20684.842444	60.795585
2149.401696	20564.438063	60.800590
2149.177920	20446.148040	60.805594
2148.420243	20331.131801	60.810599
2147.753536	20208.598925	60.815604
2146.958893	20086.957369	60.820609
2146.507631	19969.412858	60.825614
2145.724868	19847.951279	60.830618
2144.975423	19737.408771	60.835623
2144.344661	19616.824923	60.840628
2143.838242	19497.040997	60.845633
2143.071047	19383.341419	60.850638
2142.596693	19264.473559	60.855642
2141.598287	19140.264343	60.860647
2140.881285	19016.939514	60.865652
2140.396776	18900.942247	60.870657
2139.514092	18788.106894	60.875662
2139.243432	18671.350300	60.880666
2138.417096	18562.731681	60.885671
2137.902075	18440.986301	60.890676
2137.228818	18324.708648	60.895681
2136.315841	18199.547197	60.900686
2135.769286	18079.863766	60.905690
2134.894776	17972.859847	60.910695
2134.428535	17832.353390	60.915700
2133.809674	17733.915293	60.920705
2132.995530	17619.406708	60.925710
2132.665654	17500.941808	60.930714
2131.589930	17387.513311	60.935719
2131.008403	17265.728450	60.940724
2130.313376	17152.426786	60.945729
2129.653813	17030.497873	60.950734
2129.046451	16921.563887	60.955738
2128.689070	16802.821726	60.960743
2128.078706	16678.398287	60.965748
2127.140696	16561.202318	60.970753
2126.456827	16447.314773	60.975758
2126.341999	16336.285225	60.980762
2125.137672	16217.978689	60.985767
2124.634342	16098.026794	60.990772
2123.839335	15980.298481	60.995777
2123.334322	15854.762641	61.000782
2122.880914	15739.358827	61.005786
2122.079755	15620.947320	61.010791
2121.926190	15492.829709	61.015796
2120.757728	15379.751083	61.020801
2119.902854	15257.562638	61.025806
2119.792400	15137.414390	61.030810
2118.957462	15025.117367	61.035815
2118.240607	14889.875145	61.040820
2117.523276	14774.151132	61.045825
2116.429790	14646.496087	61.050830
2116.183235	14529.010212	61.055834
2115.127143	14418.622447	61.060839
2114.796185	14302.504368	61.065844
2113.665955	14184.836926	61.070849
2112.997780	14072.964446	61.075854
2112.433559	13957.668305	61.080858
2111.615101	13843.024023	61.085863
2111.108510	13732.487061	61.090868
2110.511926	13628.659428	61.095873
2109.823330	13509.550527	61.100878
2109.357716	13394.559052	61.105882
2108.287068	13276.876405	61.110887
2107.806951	13158.816478	61.115892
2107.413681	13043.200206	61.120897
2106.418455	12946.546694	61.125902
2105.850974	12828.721875	61.130906
2105.078317	12719.276808	61.135911
2104.428952	12595.887190	61.140916
2103.794702	12490.935883	61.145921
2103.120076	12372.638262	61.150926
2102.590293	12264.729904	61.155930
2101.526865	12162.500160	61.160935
2101.371571	12043.946132	61.165940
2100.438966	11942.667344	61.170945
2099.708493	11828.226830	61.175950
2099.460357	11714.450251	61.180954
2098.449610	11611.975170	61.185959
2097.715481	11498.708750	61.190964
2096.941433	11388.317866	61.195969
2096.695984	11279.873069	61.200974
2095.901381	11163.688063	61.205978
2094.920129	11067.917016	61.210983
2094.242540	10951.679167	61.215988
2093.860026	10842.382580	61.220993
2093.048956	10735.519980	61.225998
2092.510121	10625.112722	61.231002
2091.634962	10525.191260	61.236007
2091.274836	10408.915495	61.241012
2090.354833	10301.180045	61.246017
2089.659632	10191.000782	61.251022
2089.151371	10085.643012	61.256026
2088.406170	9985.479626	61.261031
2087.751802	9878.575339	61.266036
2087.018748	9775.675110	61.271041
2086.413247	9666.754170	61.276046
2085.909162	9558.220317	61.281050
2085.324418	9454.803255	61.286055
2084.583014	9339.529589	61.291060
2084.008413	9232.023910	61.296065
2083.249065	9125.792525	61.301070
2082.774883	9013.925208	61.306074
2081.872799	8914.827379	61.311079
2081.217891	8806.290129	61.316084
2080.706769	8696.554914	61.321089
2080.073796	8592.362080	61.326094
2079.502530	8472.950141	61.331098
2078.321816	8362.750824	61.336103
2077.770670	8259.201743	61.341108
2077.091111	8156.739589	61.346113
2076.556014	8052.050576	61.351118
2076.004079	7937.812389	61.356122
2074.887115	7838.769565	61.361127
2074.594924	7734.852073	61.366132
2073.722409	7634.245685	61.371137
2072.857150	7536.429929	61.376142
2072.656747	7434.955387	61.381146
2071.969442	7326.115674	61.386151
2071.241692	7220.956970	61.391156
2070.516885	7120.112878	61.396161
2069.802979	7007.766071	61.401166
2069.125178	6898.325273	61.406170
2068.279235	6806.352743	61.411175
2067.752020	6703.554127	61.416180
2066.848625	6597.216013	61.421185
2066.170917	6495.797546	61.426190
2065.280546	6398.542265	61.431194
2064.535943	6303.952819	61.436199
2064.318985	6206.298507	61.441204
2063.112043	6114.766160	61.446209
2062.481733	6024.833318	61.451214
2062.240287	5921.089598	61.456218
2061.153702	5835.050496	61.461223
2060.472487	5738.368206	61.466228
2059.959998	5648.370043	61.471233
2059.173694	5566.925327	61.476238
2058.640025	5476.470124	61.481242
2057.640378	5397.739690	61.486247
2057.129245	5300.070169	61.491252
2056.237725	5215.921223	61.496257
2055.533921	5135.349214	61.501262
2055.059555	5046.467914	61.506266
2054.185214	4962.606370	61.511271
2053.472306	4878.941327	61.516276
2052.856874	4803.475321	61.521281
2051.999751	4721.094475	61.526286
2051.593249	4643.975263	61.531290
2050.519114	4563.623662	61.536295
2050.210466	4482.234537	61.541300
2049.356023	4412.722361	61.546305
2048.514963	4336.086210	61.551310
2048.080679	4252.875034	61.556314
2046.943826	4180.578047	61.561319
2046.779764	4109.881162	61.566324
2045.878104	4048.089435	61.571329
2044.891629	3970.833092	61.576334
2044.367191	3896.534031	61.581338
2043.575407	3826.665283	61.586343
2042.975546	3751.467187	61.591348
2042.049996	3691.482124	61.596353
2040.926324	3626.209053	61.601358
2040.438403	3561.708470	61.606362
2039.951576	3501.811517	61.611367
2039.056674	3451.759934	61.616372
2038.641823	3394.866319	61.621377
2037.749341	3335.527330	61.626382
2037.092721	3269.373351	61.631386
2036.149011	3220.063764	61.636391
2035.984554	3157.502642	61.641396
2035.199550	3109.988472	61.646401
2034.636448	3046.756044	61.651406
2034.249834	2992.797246	61.656410
2033.399440	2941.717461	61.661415
2032.883187	2880.750414	61.666420
2032.145552	2824.088461	61.671425
2031.417474	2763.591631	61.676430
2031.044055	2707.806875	61.681434
2030.295922	2648.912268	61.686439
2029.760987	2584.347727	61.691444
2029.063194	2528.686887	61.696449
2028.066392	2469.770945	61.701454
2027.711090	2409.709318	61.706458
2026.914914	2351.654736	61.711463
2026.163232	2286.280504	61.716468
2025.134088	2228.203444	61.721473
2024.356259	2184.310079	61.726478
2024.105930	2125.448995	61.731482
2023.004051	2084.340657	61.736487
2022.685597	2027.931503	61.741492
2021.992021	1972.195618	61.746497
2021.378507	1930.978676	61.751502
2020.981012	1874.788478	61.756506
2020.507788	1823.808103	61.761511
2019.302966	1769.727349	61.766516
2018.510640	1723.439580	61.771521
2017.886801	1669.726754	61.776526
2017.395314	1612.010805	61.781530
2016.539478	1563.704610	61.786535
2016.038214	1510.171643	61.791540
2015.310348	1477.650792	61.796545
2014.651840	1424.542107	61.801550
2014.081088	1364.273717	61.806554
2013.287545	1319.250706	61.811559
2012.953326	1275.498655	61.816564
2011.799624	1226.050910	61.821569
2011.104971	1177.038320	61.826574
2010.502027	1124.888679	61.831578
2009.759718	1089.263308	61.836583
2009.248817	1034.722696	61.841588
2008.743081	993.639551	61.846593
2007.864129	952.277460	61.851598
2007.374439	899.405699	61.856602
2006.572213	853.830376	61.861607
2005.898618	802.366512	61.866612
2005.207888	761.850370	61.871617
2004.582223	719.757995	61.876622
2004.575548	672.287542	61.881626
2003.412200	626.295544	61.886631
2002.711358	586.100060	61.891636
2002.027750	542.328380	61.896641
2001.152912	497.300317	61.901646
2000.398650	452.325803	61.906650
1999.846473	416.573350	61.911655
1999.368062	379.200717	61.916660
1998.527947	329.774080	61.921665
1997.814705	302.771528	61.926670
1997.445054	254.566797	61.931674
1996.048735	218.094049	61.936679
1995.558528	174.208421	61.941684
1995.037749	140.350376	61.946689
1994.222396	100.379422	61.951694
1993.786736	72.103199	61.956698
1992.412921	27.871731	61.961703
1991.985970	-2.328072	61.966708
1991.531052	-23.316975	61.971713
1990.589613	-51.184684	61.976718
1990.146628	-88.995399	61.981722
1988.971268	-97.205203	61.986727
1988.553455	-123.712936	61.991732
1987.537837	-157.425525	61.996737
1986.085435	-163.840895	62.001742
1984.478348	-151.117335	62.006746
1982.186180	-90.895559	62.011751
1980.309269	-40.336917	62.016756
1980.014932	-7.983175	62.021761
1980.170499	14.096162	62.026766
1980.485628	17.797271	62.031770
1980.613529	36.116773	62.036775
1980.550999	30.108397	62.041780
1980.691613	27.915627	62.046785
1980.275647	20.545634	62.051790
1980.134187	2.727155	62.056794
1979.098866	-22.944737	62.061799
1978.275190	-39.528938	62.066804
1976.927326	-35.256428	62.071809
1975.386061	-25.757082	62.076814
1974.574802	-16.072374	62.081818
1974.154242	0.438591	62.086823
1973.612683	0.061952	62.091828
1973.462810	2.509031	62.096833
1972.750281	9.654919	62.101838
1972.291505	-6.022113	62.106842
1971.876223	6.255406	62.111847
1971.461289	-3.264162	62.116852
1970.475085	-5.656582	62.121857
1969.473197	2.585492	62.126862
1968.755005	-1.054274	62.131866
1967.313604	3.045434	62.136871
1967.116290	7.931748	62.141876
1966.533591	19.874718	62.146881
1966.225656	29.074297	62.151886
1965.601179	14.226227	62.156890
1965.043228	23.717797	62.161895
1964.534786	19.513297	62.166900
1964.017938	16.784610	62.171905
1963.191989	21.291289	62.176910
1962.436824	16.157678	62.181914
1961.368855	23.875655	62.186919
1960.726065	25.546239	62.191924
1960.446183	16.658098	62.196929
1959.861576	32.781964	62.201934
1959.162037	25.349741	62.206938
1958.678731	34.392648	62.211943
1958.008761	22.205858	62.216948
1957.340148	22.358751	62.221953
1956.146518	25.961825	62.226958
1955.835578	29.109419	62.231962
1954.948890	29.369463	62.236967
1954.746337	35.336851	62.241972
1954.291802	31.462847	62.246977
1953.428219	44.275177	62.251982
1952.931036	21.195543	62.256986
1952.122038	28.263711	62.261991
1951.179390	42.652956	62.266996
1950.527999	39.280134	62.272001
1949.476576	38.949722	62.277006
1949.400992	28.341780	62.282010
1948.367563	29.538189	62.287015
1947.976045	30.306287	62.292020
1947.686775	36.306363	62.297025
1946.976831	35.343005	62.302030
1946.673278	26.701474	62.307034
1945.173701	29.815356	62.312039
1944.471929	23.995171	62.317044
1944.169192	36.021461	62.322049
1943.572468	33.691814	62.327054
1943.187333	26.059885	62.332058
1942.459994	32.093212	62.337063
1941.704355	25.961448	62.342068
1941.159565	27.532903	62.347073
1940.174006	34.479285	62.352078
1939.707234	31.698499	62.357082
1938.535780	38.824199	62.362087
1938.039120	33.796222	62.367092
1937.232223	32.174883	62.372097
1936.602139	34.769146	62.377102
1936.048247	31.393471	62.382106
1935.512938	37.396325	62.387111
1934.625629	29.399386	62.392116
1934.309984	32.863126	62.397121
1933.640005	34.621612	62.402126
1933.715120	39.649207	62.407130
1932.238747	42.833535	62.412135
1931.052034	36.263974	62.417140
1931.176695	36.901266	62.422145
1930.726288	41.271085	62.427150
1929.466129	30.907920	62.432154
1928.822814	37.334779	62.437159
1928.748012	41.197121	62.442164
1928.162537	27.547679	62.447169
1926.713203	36.761257	62.452174
1926.085111	41.408440	62.457178
1926.120965	43.367147	62.462183
1925.126772	42.906235	62.467188
1924.488110	37.307851	62.472193
1923.548057	41.775885	62.477198
1923.571112	31.850893	62.482202
1922.515650	40.434247	62.487207
1921.300171	37.537323	62.492212
1921.222043	37.061910	62.497217
1920.772065	40.200036	62.502222
1920.248129	46.568529	62.507226
1918.947727	44.151870	62.512231
1918.270789	51.555496	62.517236
1917.587277	40.154618	62.522241
1917.297455	46.452836	62.527246
1916.965620	37.601323	62.532250
1915.872272	47.993190	62.537255
1915.049254	40.960626	62.542260
1914.638627	42.670068	62.547265
1913.847341	42.607472	62.552270
1913.679486	39.865980	62.557274
1912.777727	45.832384	62.562279
1912.209518	43.644877	62.567284
1911.646678	50.213516	62.572289
1910.834858	50.015405	62.577294
1910.220876	41.516185	62.582298
1909.645674	45.562032	62.587303
1908.923611	37.595643	62.592308
1907.832042	38.503245	62.597313
1906.393576	50.313984	62.602318
1906.589442	33.091665	62.607322
1906.531824	44.705310	62.612327
1905.637906	41.358377	62.617332
1904.658079	36.225743	62.622337
1903.531764	47.925434	62.627342
1903.691469	46.087605	62.632346
1902.584828	50.503239	62.637351
1902.272607	47.004053	62.642356
1901.516437	43.867075	62.647361
1900.846325	43.550279	62.652366
1900.276142	38.795759	62.657370
1899.381441	47.949708	62.662375
1898.572658	50.758429	62.667380
1898.518095	44.613169	62.672385
1897.646657	43.550876	62.677390
1897.335321	49.984978	62.682394
1896.769284	55.229461	62.687399
1895.674242	47.151958	62.692404
1894.799686	48.337363	62.697409
1893.461231	57.642181	62.702414
1893.250468	43.029648	62.707418
1893.168055	53.445573	62.712423
1892.072471	47.481318	62.717428
1891.797739	45.371815	62.722433
1890.812088	60.460211	62.727438
1890.207966	54.033162	62.732442
1889.632233	52.122826	62.737447
1889.023724	51.725291	62.742452
1888.454420	51.961788	62.747457
1887.943127	57.479865	62.752462
1887.440262	50.855392	62.757466
1886.362569	49.114620	62.762471
1885.122680	49.888075	62.767476
1884.887211	56.469414	62.772481
1884.587191	58.929298	62.777486
1884.026097	49.253141	62.782490
1882.909012	54.709675	62.787495
1882.184185	48.629803	62.792500
1881.794629	47.942044	62.797505
1880.911700	65.065799	62.802510
1880.429641	56.342208	62.807514
1879.739550	48.925848	62.812519
1879.213103	51.812764	62.817524
1878.583344	43.658263	62.822529
1878.169157	58.419404	62.827534
1877.032943	50.406792	62.832538
1876.001770	49.578022	62.837543
1875.462611	47.360681	62.842548
1874.837144	43.982186	62.847553
1874.262037	47.466619	62.852558
1874.056042	46.932654	62.857562
1873.023208	43.648785	62.862567
1872.748197	53.272093	62.867572
1872.492777	42.591771	62.872577
1871.227242	58.014760	62.877582
1870.993520	41.973976	62.882586
1869.775544	39.129513	62.887591
1868.777087	45.704223	62.892596
1868.296936	44.157198	62.897601
1867.357408	52.121342	62.902606
1867.163010	49.035552	62.907610
1866.883369	53.810370	62.912615
1866.132012	44.281120	62.917620
1865.500987	45.632885	62.922625
1864.625592	45.235141	62.927630
1864.354458	42.754480	62.932634
1863.498199	47.761177	62.937639
1862.799204	50.205544	62.942644
1861.814358	54.986646	62.947649
1861.257105	50.876643	62.952654
1860.970315	47.117955	62.957658
1859.989360	46.022595	62.962663
1859.408265	52.414364	62.967668
1858.815694	44.938377	62.972673
1857.556884	50.349605	62.977678
1857.279805	43.142090	62.982682
1856.577894	45.672077	62.987687
1855.591441	52.325315	62.992692
1855.187761	37.508450	62.997697
1854.305547	48.160139	63.002702
1854.332167	40.322510	63.007706
1853.951010	48.901355	63.012711
1852.731214	52.155386	63.017716
1852.767343	49.914539	63.022721
1851.818846	56.613795	63.027726
1850.442198	44.354699	63.032730
1849.803640	42.843861	63.037735
1849.040344	47.786919	63.042740
1848.753828	45.524748	63.047745
1848.085718	54.417235	63.052750
1847.565345	47.645741	63.057754
1847.162537	43.419762	63.062759
1846.379702	52.981755	63.067764
1845.780485	44.401361	63.072769
1844.290544	51.350573	63.077774
1843.558832	40.364237	63.082778
1843.650921	48.353861	63.087783
1842.642839	56.652179	63.092788
1842.182127	51.410350	63.097793
1841.580463	54.692421	63.102798
1841.341046	51.728900	63.107802
1840.925032	55.035117	63.112807
1839.479491	57.296797	63.117812
1838.502220	49.586987	63.122817
1837.629319	56.906617	63.127822
1837.408908	52.661145	63.132826
1836.958054	55.636996	63.137831
1836.266177	58.113357	63.142836
1835.886057	56.438491	63.147841
1835.421181	52.537762	63.152846
1834.784193	54.371462	63.157850
1833.814948	57.052707	63.162855
1832.473753	52.592488	63.167860
1832.127936	41.466046	63.172865
1831.307440	50.076789	63.177870
1830.890277	48.915594	63.182874
1830.535296	58.553178	63.187879
1829.470125	55.974639	63.192884
1829.595880	51.070230	63.197889
1828.743225	55.297336	63.202894
1827.495890	45.586634	63.207898
1826.709764	45.289851	63.212903
1826.026813	53.692679	63.217908
1825.706943	48.278683	63.222913
1825.185339	57.870177	63.227918
1824.834969	49.917347	63.232922
1824.192697	52.951972	63.237927
1823.014889	56.092116	63.242932
1822.253789	47.915903	63.247937
1821.403713	50.799011	63.252942
1820.768965	47.456698	63.257946
1820.569893	44.671283	63.262951
1820.020536	51.337144	63.267956
1819.685201	48.123921	63.272961
1818.321829	53.086555	63.277966
1817.477008	48.668972	63.282970
1816.922329	45.290294	63.287975
1816.286761	55.095425	63.292980
1815.762183	47.367377	63.297985
1815.198003	55.268795	63.302990
1815.315167	44.611338	63.307994
1814.294411	52.407039	63.312999
1812.801578	47.970904	63.318004
1812.342439	51.112079	63.323009
1811.867614	50.523025	63.328014
1811.481329	52.660712	63.333018
1811.059187	53.503080	63.338023
1809.751995	54.090131	63.343028
1809.091797	48.135645	63.348033
1807.885658	50.635306	63.353038
1807.642192	48.265378	63.358042
1806.990454	50.131388	63.363047
1806.261365	56.702783	63.368052
1806.116626	51.622115	63.373057
1805.603370	58.044126	63.378062
1805.238931	42.104537	63.383066
1804.277942	60.070183	63.388071
1803.192126	46.561705	63.393076
1802.723452	42.322537	63.398081
1801.853315	53.275105	63.403086
1801.497158	49.174193	63.408090
1801.114103	61.457684	63.413095
1799.558764	60.064020	63.418100
1798.739881	44.631825	63.423105
1798.074393	51.142659	63.428110
1797.770357	51.827503	63.433114
1797.425195	53.581764	63.438119
1796.887984	48.850419	63.443124
1796.387751	49.337750	63.448129
1795.932509	57.901556	63.453134
1795.078571	51.867442	63.458138
1794.144366	51.848072	63.463143
1793.220323	60.812744	63.468148
1792.998989	58.067135	63.473153
1792.365517	49.853323	63.478158
1791.263727	50.059260	63.483162
1790.456596	52.512927	63.488167
1789.691466	57.574567	63.493172
1789.460768	52.777212	63.498177
1788.794622	57.848368	63.503182
1788.635011	61.579096	63.508186
1787.822847	54.806631	63.513191
1786.515667	59.438656	63.518196
1785.834064	59.204140	63.523201
1784.896877	65.666653	63.528206
1784.563436	58.455476	63.533210
1784.076040	63.927195	63.538215
1783.769203	58.902226	63.543220
1783.323540	54.260429	63.548225
1782.646736	68.024041	63.553230
1781.743327	67.078827	63.558234
1781.190926	64.202850	63.563239
1780.689727	63.734684	63.568244
1779.734410	62.723594	63.573249
1778.328323	59.858574	63.578254
1777.752281	54.706035	63.583258
1777.299187	58.227886	63.588263
1776.862295	54.071986	63.593268
1776.327032	51.502381	63.598273
1775.887172	71.843823	63.603278
1775.267747	56.206492	63.608282
1774.211087	53.213457	63.613287
1773.517701	64.044933	63.618292
1772.906655	55.721905	63.623297
1772.226137	60.188209	63.628302
1772.109049	53.876261	63.633306
1771.222209	59.166968	63.638311
1770.122350	49.191603	63.643316
1769.772686	57.240322	63.648321
1768.731315	59.882577	63.653326
1768.051688	57.405281	63.658330
1767.894633	57.295647	63.663335
1767.410316	66.931696	63.668340
1766.103009	60.160579	63.673345
1765.301390	61.968393	63.678350
1764.645950	60.356175	63.683354
1764.300694	61.120110	63.688359
1763.618694	64.768197	63.693364
1763.463201	63.548119	63.698369
1762.509679	59.362281	63.703374
1761.511161	65.257362	63.708378
1760.747347	67.303609	63.713383
1760.444043	66.371933	63.718388
1759.918907	60.419667	63.723393
1759.117901	67.597018	63.728398
1758.646691	61.166249	63.733402
1758.307009	62.254158	63.738407
1757.292315	67.710254	63.743412
1756.481087	57.909840	63.748417
1756.060216	69.560664	63.753422
1755.090991	59.876801	63.758426
1754.048763	65.226881	63.763431
1753.146913	60.312160	63.768436
1752.995665	55.175760	63.773441
1752.065913	60.686179	63.778446
1751.842535	58.007132	63.783450
1751.262301	48.119587	63.788455
1750.656169	59.356686	63.793460
1750.513141	45.518769	63.798465
1749.509866	58.744421	63.803470
1748.875384	58.595474	63.808474
1748.365163	55.096209	63.813479
1747.276385	52.332216	63.818484
1746.419883	59.362256	63.823489
1745.144397	62.760798	63.828494
1744.601068	58.844158	63.833498
1744.383597	50.356147	63.838503
1744.064448	55.991969	63.843508
1743.547037	48.418925	63.848513
1742.910384	64.716681	63.853518
1742.122293	52.468278	63.858522
1741.185078	64.391900	63.863527
1740.443614	55.223827	63.868532
1740.029077	61.718483	63.873537
1739.113967	71.404015	63.878542
1738.989061	60.111616	63.883546
1737.970069	51.042807	63.888551
1737.151951	59.342533	63.893556
1736.707477	64.982489	63.898561
1735.889481	65.611752	63.903566
1735.733440	55.272068	63.908570
1734.745242	48.929708	63.913575
1733.915568	57.273847	63.918580
1733.173730	51.852750	63.923585
1732.516459	65.100744	63.928590
1732.171965	56.703865	63.933594
1731.784172	60.191699	63.938599
1730.534225	65.691466	63.943604
1729.955440	51.862813	63.948609
1729.078108	63.745388	63.953614
1728.771000	60.556080	63.958618
1728.568513	60.008954	63.963623
1727.588685	59.798152	63.968628
1726.374344	55.127033	63.973633
1725.578130	57.195779	63.978638
1725.297560	55.033606	63.983642
1724.754784	59.135842	63.988647
1724.162640	64.334037	63.993652
1724.079362	60.571436	63.998657
1723.171949	65.616262	64.003662
1722.248235	49.770228	64.008666
1721.681261	55.574716	64.013671
1720.877900	57.267699	64.018676
1720.611448	53.715540	64.023681
1719.536449	57.870748	64.028686
1718.841611	60.672466	64.033690
1718.445421	63.819431	64.038695
1717.304679	55.807618	64.043700
1716.777276	49.776879	64.048705
1715.688850	51.209194	64.053710
1715.180463	57.598903	64.058714
1715.035407	60.005809	64.063719
1714.592913	52.753617	64.068724
1713.989302	54.777590	64.073729
1712.922283	57.532750	64.078734
1711.951467	61.313443	64.083738
1711.585127	54.862882	64.088743
1710.488283	57.865635	64.093748
1710.611381	58.705017	64.098753
1709.875145	59.964714	64.103758
1708.696185	53.124366	64.108762
1708.207654	58.820204	64.113767
1707.314950	65.461760	64.118772
1707.338336	51.244175	64.123777
1706.411903	62.779730	64.128782
1705.544513	61.060833	64.133786
1704.763213	63.187143	64.138791
1703.627281	68.659355	64.143796
1703.984482	57.036513	64.148801
1703.093885	59.274797	64.153806
1702.759996	63.019009	64.158810
1701.637900	60.041126	64.163815
1700.568953	60.235577	64.168820
1700.096915	56.594639	64.173825
1699.668186	59.783043	64.178830
1699.140025	62.492064	64.183834
1698.795656	54.027364	64.188839
1697.754269	61.831112	64.193844
1696.977713	60.578773	64.198849
1696.120946	67.829649	64.203854
1696.038876	56.640846	64.208858
1695.605687	53.488913	64.213863
1694.547070	58.081507	64.218868
1693.728415	54.445150	64.223873
1692.917182	58.306165	64.228878
1692.449791	57.029964	64.233882
1692.376942	56.227284	64.238887
1690.903489	57.414818	64.243892
1690.404633	50.742451	64.248897
1689.433473	61.515545	64.253902
1688.773318	53.823252	64.258906
1688.647583	53.845847	64.263911
1687.831606	59.940624	64.268916
1687.104531	57.486655	64.273921
1686.057364	57.311794	64.278926
1685.719636	53.193783	64.283930
1685.253333	56.549007	64.288935
1684.737086	66.264250	64.293940
1684.535307	51.623523	64.298945
1683.141600	57.617654	64.303950
1681.952923	55.213337	64.308954
1681.348940	63.624154	64.313959
1680.952034	67.384684	64.318964
1680.940896	56.140464	64.323969
1680.105498	56.132252	64.328974
1679.377315	50.418841	64.333978
1678.700151	47.961682	64.338983
1678.013917	53.630570	64.343988
1677.807540	54.088603	64.348993
1676.472577	57.345230	64.353998
1675.695447	52.763981	64.359002
1675.277736	54.351578	64.364007
1674.456584	54.662809	64.369012
1674.487864	57.825473	64.374017
1673.400261	62.859503	64.379022
1672.215534	54.589766	64.384026
1671.876653	50.394669	64.389031
1671.094741	53.096682	64.394036
1671.249160	50.135294	64.399041
1670.065769	55.479430	64.404046
1669.305030	59.207851	64.409050
1668.492963	50.175603	64.414055
1667.790153	58.554805	64.419060
1667.736398	52.567131	64.424065
1667.091050	60.677007	64.429070
1666.205285	55.934813	64.434074
1665.535318	58.275269	64.439079
1664.729368	62.483966	64.444084
1664.072161	49.246547	64.449089
1662.792390	60.850840	64.454094
1662.031974	64.771605	64.459098
1661.812028	57.725359	64.464103
1661.163354	63.422983	64.469108
1661.096619	54.004281	64.474113
1660.358884	53.542164	64.479118
1660.167363	49.634333	64.484122
1659.027006	53.593357	64.489127
1657.918590	63.489378	64.494132
1657.498405	55.790524	64.499137
1656.893151	60.659645	64.504142
1655.628100	64.416122	64.509146
1655.252766	53.701265	64.514151
1654.432619	65.771898	64.519156
1654.201642	54.854338	64.524161
1653.769904	63.427041	64.529166
1653.124847	66.818546	64.534170
1652.305224	56.887043	64.539175
1651.367996	63.453680	64.544180
1651.103678	56.860769	64.549185
1650.569636	56.259071	64.554190
1649.462011	63.180783	64.559194
1648.841592	65.480257	64.564199
1647.887643	62.453615	64.569204
1647.571365	62.804524	64.574209
1647.176232	59.644978	64.579214
1646.418176	63.858690	64.584218
1645.288858	61.869170	64.589223
1644.296339	64.252973	64.594228
1644.067099	62.590445	64.599233
1643.415363	59.935286	64.604238
1643.128478	60.712042	64.609242
1642.863789	55.328738	64.614247
1641.540789	67.163841	64.619252
1640.894589	63.629423	64.624257
1640.309346	65.749845	64.629262
1639.647646	61.986073	64.634266
1639.095437	57.137297	64.639271
1638.227314	67.122899	64.644276
1637.712528	53.023913	64.649281
1636.864681	59.145841	64.654286
1636.108299	64.024776	64.659290
1636.045510	58.633060	64.664295
1634.759558	61.246399	64.669300
1634.340648	57.959743	64.674305
1633.991738	59.105903	64.679310
1633.187863	56.064895	64.684314
1632.116622	56.124119	64.689319
1630.875561	67.553543	64.694324
1630.833622	53.046717	64.699329
1629.976158	57.569538	64.704334
1629.515065	57.042992	64.709338
1629.672838	53.303618	64.714343
1629.170402	61.113253	64.719348
1627.947669	53.548180	64.724353
1627.196808	61.993370	64.729358
1626.760702	57.329588	64.734362
1625.486813	58.018675	64.739367
1624.221244	62.972177	64.744372
1624.115102	51.492317	64.749377
1623.659768	51.007436	64.754382
1623.006986	57.566749	64.759386
1622.881856	52.386791	64.764391
1621.990134	66.441601	64.769396
1621.792507	60.625015	64.774401
1620.490004	56.672863	64.779406
1620.338730	62.395574	64.784410
1619.391837	57.700955	64.789415
1618.246729	58.730720	64.794420
1617.501808	58.250833	64.799425
1617.015428	59.272170	64.804430
1616.459099	54.554945	64.809434
1616.311620	51.412843	64.814439
1614.606668	59.363010	64.819444
1614.287265	53.321338	64.824449
1613.362306	57.895886	64.829454
1613.215454	61.298155	64.834458
1613.008208	57.593101	64.839463
1612.582088	59.707177	64.844468
1611.539763	61.122751	64.849473
1610.810767	62.780300	64.854478
1609.899601	70.829907	64.859482
1609.138728	69.619259	64.864487
1607.818716	66.154025	64.869492
1607.555316	57.667021	64.874497
1607.116804	63.602515	64.879502
1606.509860	60.736821	64.884506
1606.280210	62.904850	64.889511
1605.993537	67.215592	64.894516
1604.852668	60.735105	64.899521
1604.132578	67.048068	64.904526
1603.547390	65.563508	64.909530
1602.701200	54.494512	64.914535
1601.147943	68.130845	64.919540
1601.243132	59.935397	64.924545
1600.690671	65.674522	64.929550
1600.205312	68.354685	64.934554
1599.733003	61.875244	64.939559
1598.306724	66.649276	64.944564
1597.861369	56.782931	64.949569
1597.339649	68.388275	64.954574
1596.571206	64.392307	64.959578
1596.444442	56.730441	64.964583
1595.204930	65.645924	64.969588
1594.747358	66.192749	64.974593
1593.924320	68.177483	64.979598
1593.393605	61.604816	64.984602
1593.286010	54.857711	64.989607
1592.022337	64.850955	64.994612
1591.173756	60.003534	64.999617
1590.456202	65.696342	65.004622
1590.312955	63.047164	65.009626
1589.978031	59.386047	65.014631
1588.749131	66.035302	65.019636
1588.017710	60.931148	65.024641
1587.494476	66.145229	65.029646
1587.149063	59.041652	65.034650
1586.521955	48.786284	65.039655
1584.776643	64.126302	65.044660
1584.340014	50.462785	65.049665
1584.042303	63.450249	65.054670
1583.434452	65.225760	65.059674
1583.115673	55.222618	65.064679
1582.426388	66.192246	65.069684
1581.868977	55.203548	65.074689
1580.753850	58.056287	65.079694
1580.185240	60.300236	65.084698
1579.809172	55.989633	65.089703
1578.166510	62.559532	65.094708
1578.253669	55.901343	65.099713
1577.656118	56.457789	65.104718
1577.191277	63.733171	65.109722
1576.500060	60.201193	65.114727
1575.118597	66.056234	65.119732
1574.821594	63.645949	65.124737
1574.248064	63.395898	65.129742
1573.960772	64.371426	65.134746
1573.228584	62.413475	65.139751
1571.970545	70.997593	65.144756
1571.390230	63.573355	65.149761
1570.938985	59.638977	65.154766
1570.685721	56.486873	65.159770
1569.935213	52.986394	65.164775
1568.721151	59.248514	65.169780
1568.396406	59.581853	65.174785
1567.947842	59.710928	65.179790
1567.054442	57.471077	65.184794
1566.232119	62.975525	65.189799
1564.995484	64.179127	65.194804
1564.731935	55.411453	65.199809
1564.210305	57.073922	65.204814
1564.029701	61.150193	65.209818
1563.899073	53.148320	65.214823
1562.248387	67.781027	65.219828
1561.760768	50.992155	65.224833
1561.570194	55.205629	65.229838
1559.947227	61.570556	65.234842
1559.349752	54.639493	65.239847
1558.586509	65.530984	65.244852
1558.185666	57.040591	65.249857
1557.647053	60.762141	65.254862
1557.368302	63.195021	65.259866
1557.005870	54.534522	65.264871
1556.105691	67.034209	65.269876
1555.624116	51.726741	65.274881
1554.252308	55.107551	65.279886
1553.317888	58.996057	65.284890
1552.555801	56.952974	65.289895
1552.066714	65.523757	65.294900
1551.892610	58.525441	65.299905
1551.600881	60.674949	65.304910
1551.017067	66.788076	65.309914
1550.021165	59.674296	65.314919
1549.147550	55.698208	65.319924
1548.557524	57.511895	65.324929
1548.169815	55.989671	65.329934
1546.780478	52.970733	65.334938
1546.120172	45.246977	65.339943
1545.584276	53.651722	65.344948
1545.449428	60.179236	65.349953
1544.788239	57.544530	65.354958
1544.133011	53.992653	65.359962
1543.204716	53.065670	65.364967
1542.189511	59.061241	65.369972
1542.020973	55.501437	65.374977
1541.540380	56.870380	65.379982
1540.271694	56.421679	65.384986
1539.667293	44.513204	65.389991
1539.212350	55.688458	65.394996
1538.698307	55.351693	65.400001
1538.550964	57.736889	65.405006
1537.292603	52.290679	65.410010
1536.749753	49.447940	65.415015
1535.714699	56.889601	65.420020
1535.734614	56.009111	65.425025
1534.471644	56.335379	65.430030
1533.698086	56.229079	65.435034
1533.292100	51.268792	65.440039
1532.539980	56.117109	65.445044
1532.389318	50.441315	65.450049
1531.573120	52.577946	65.455054
1530.360630	44.467246	65.460058
1530.057906	50.863727	65.465063
1529.448574	54.601245	65.470068
1528.732734	51.293972	65.475073
1527.569486	53.444735	65.480078
1526.697316	51.228336	65.485082
1526.429563	47.066121	65.490087
1525.826629	57.350240	65.495092
1525.635582	52.368425	65.500097
1525.531967	49.648301	65.505102
1524.181426	59.286355	65.510106
1523.493532	46.736701	65.515111
1522.849345	53.423976	65.520116
1522.205168	47.624733	65.525121
1521.123073	51.024190	65.530126
1520.357946	47.606476	65.535130
1520.026587	45.026616	65.540135
1519.551895	51.286411	65.545140
1519.362788	47.119588	65.550145
1518.221424	59.266502	65.555150
1517.237287	56.500180	65.560154
1517.152744	52.961728	65.565159
1516.365738	57.153261	65.570164
1515.323745	54.121737	65.575169
1514.587561	62.408497	65.580174
1514.027446	60.281299	65.585178
1513.854506	54.708394	65.590183
1512.986784	61.470612	65.595188
1511.990809	50.497997	65.600193
1511.359511	52.080125	65.605198
1510.824469	55.641839	65.610202
1510.291345	53.805250	65.615207
1509.633911	55.703772	65.620212
1509.029329	54.242818	65.625217
1508.104030	59.096577	65.630222
1507.664996	58.788902	65.635226
1507.287275	45.417259	65.640231
1506.088322	53.280788	65.645236
1505.688989	40.852462	65.650241
1505.089541	53.466799	65.655246
1504.477571	60.734022	65.660250
1503.976247	51.914250	65.665255
1502.524857	56.868938	65.670260
1502.013335	54.155272	65.675265
1501.635536	49.655724	65.680270
1500.920365	56.146120	65.685274
1500.503896	50.370631	65.690279
1499.596472	57.536557	65.695284
1498.907134	55.459856	65.700289
1498.241070	49.932183	65.705294
1497.746702	56.174608	65.710298
1496.884359	41.836006	65.715303
1495.875496	54.925405	65.720308
1495.459544	47.765249	65.725313
1495.392833	49.656656	65.730318
1494.719010	57.156059	65.735322
1493.903425	49.953737	65.740327
1492.744693	56.287521	65.745332
1492.529676	52.766647	65.750337
1491.632610	58.656731	65.755342
1490.857513	55.614353	65.760346
1490.257264	53.944554	65.765351
1489.407959	66.065582	65.770356
1489.181355	62.647473	65.775361
1488.670492	49.028898	65.780366
1488.132614	52.649414	65.785370
1487.243566	53.291618	65.790375
1486.359662	65.479644	65.795380
1485.667350	54.285327	65.800385
1485.296003	51.923138	65.805390
1484.031523	56.452318	65.810394
1483.689059	48.996632	65.815399
1482.759625	59.113431	65.820404
1482.517334	54.535584	65.825409
1482.141396	56.648013	65.830414
1481.463243	54.586887	65.835418
1480.730693	56.380654	65.840423
1479.713612	56.525954	65.845428
1479.396104	53.052904	65.850433
1478.493816	56.378077	65.855438
1477.449285	55.111612	65.860442
1477.077884	56.603568	65.865447
1476.575426	59.623939	65.870452
1476.222952	46.786042	65.875457
1475.145668	57.757400	65.880462
1474.157852	58.516227	65.885466
1473.923756	52.144056	65.890471
1473.125492	65.017079	65.895476
1472.718974	59.873957	65.900481
1472.318247	57.183696	65.905486
1471.160582	55.925746	65.910490
1470.629889	48.757018	65.915495
1469.985510	61.077301	65.920500
1469.564589	52.205340	65.925505
1468.530395	57.197839	65.930510
1467.505777	56.421808	65.935514
1467.181294	44.853666	65.940519
1466.733534	59.200663	65.945524
1466.237444	56.367857	65.950529
1465.282561	61.566957	65.955534
1464.251104	56.846414	65.960538
1464.119939	49.797136	65.965543
1463.329644	53.170752	65.970548
1462.655634	49.956203	65.975553
1461.781115	55.008490	65.980558
1460.870838	61.873679	65.985562
1460.475007	56.801404	65.990567
1459.990862	54.606954	65.995572
1459.931234	58.260299	66.000577
1458.904158	55.690061	66.005582
1458.096476	53.654253	66.010586
1458.065911	44.445882	66.015591
1456.679654	52.413307	66.020596
1456.189365	63.288253	66.025601
1455.357128	46.732382	66.030606
1454.926114	54.466027	66.035610
1454.161195	47.523757	66.040615
1453.052470	55.879181	66.045620
1452.569073	55.707877	66.050625
1452.207064	47.430545	66.055630
1451.645720	49.400545	66.060634
1451.556006	39.414665	66.065639
1449.975504	46.897283	66.070644
1449.555493	43.593494	66.075649
1448.670987	43.947979	66.080654
1447.536253	50.005148	66.085658
1447.311104	41.363870	66.090663
1446.305445	43.262542	66.095668
1446.043305	42.043664	66.100673
1445.760909	47.826628	66.105678
1444.863166	50.192285	66.110682
1444.607760	45.009395	66.115687
1443.587201	48.315522	66.120692
1443.094635	46.497736	66.125697
1442.390946	41.013910	66.130702
1441.061345	43.785662	66.135706
1440.477250	46.629770	66.140711
1439.996427	49.477971	66.145716
1439.601076	49.999165	66.150721
1439.532181	52.119582	66.155726
1438.150420	47.932539	66.160730
1437.535298	37.959184	66.165735
1437.069315	49.506781	66.170740
1436.544941	46.046110	66.175745
1435.360902	43.417245	66.180750
1434.453697	46.503511	66.185754
1434.271821	41.523408	66.190759
1433.480237	47.097117	66.195764
1433.343564	44.071589	66.200769
1432.381330	43.282507	66.205774
1431.316350	53.556473	66.210778
1431.008029	38.819207	66.215783
1430.387590	45.051705	66.220788
1429.761261	52.732808	66.225793
1428.731643	42.495727	66.230798
1427.998240	52.218681	66.235802
1427.959345	41.929833	66.240807
1427.376463	52.988222	66.245812
1426.449880	56.213192	66.250817
1425.556467	52.823778	66.255822
1424.618984	52.010264	66.260826
1424.452999	45.412811	66.265831
1424.338194	54.146479	66.270836
1423.174106	47.620893	66.275841
1422.356029	44.809301	66.280846
1421.479190	55.614778	66.285850
1421.305565	43.768784	66.290855
1420.216866	54.574810	66.295860
1419.442626	55.802775	66.300865
1418.816837	52.139022	66.305870
1418.244563	58.400145	66.310874
1418.238393	50.891034	66.315879
1417.190393	53.047185	66.320884
1416.219219	46.021009	66.325889
1415.622375	49.633560	66.330894
1414.934006	52.929490	66.335898
1414.872791	40.936324	66.340903
1413.335324	45.526257	66.345908
1412.984872	45.444223	66.350913
1412.387371	36.360646	66.355918
1411.943862	39.532507	66.360922
1411.536685	41.258816	66.365927
1410.437844	58.817494	66.370932
1409.720535	50.527243	66.375937
1409.498159	38.398839	66.380942
1408.731576	44.941574	66.385946
1408.060140	38.211556	66.390951
1407.121074	44.956745	66.395956
1406.781316	48.638831	66.400961
1406.123480	43.130384	66.405966
1404.707164	46.289676	66.410970
1404.244313	37.044353	66.415975
1403.561205	49.279323	66.420980
1403.182848	39.161120	66.425985
1402.909125	45.015246	66.430990
1402.206149	43.111056	66.435994
1401.486744	41.176360	66.440999
1400.655960	45.338604	66.446004
1400.016594	43.675045	66.451009
1399.065331	39.686125	66.456014
1397.911456	49.158928	66.461018
1397.727550	34.237900	66.466023
1397.205555	44.215845	66.471028
1396.637401	40.623368	66.476033
1396.623249	31.497560	66.481038
1395.368826	48.137923	66.486042
1394.593470	47.519432	66.491047
1394.276467	42.942436	66.496052
1393.424048	43.178297	66.501057
1392.349900	46.589154	66.506062
1391.716050	44.099962	66.511066
1391.257688	44.944994	66.516071
1390.554789	52.982052	66.521076
1390.211239	44.394292	66.526081
1389.353695	43.708439	66.531086
1388.374783	42.459969	66.536090
1388.113436	45.183411	66.541095
1387.745291	42.711920	66.546100
1386.971466	42.328159	66.551105
1386.235493	40.684687	66.556110
1384.889176	50.872485	66.561114
1384.925277	47.866813	66.566119
1384.457307	50.837561	66.571124
1383.398960	43.494089	66.576129
1382.717372	39.239967	66.581134
1382.284436	41.484468	66.586138
1381.677397	40.815578	66.591143
1380.451819	43.233355	66.596148
1379.761921	47.229712	66.601153
1379.372686	39.980185	66.606158
1378.710299	53.397754	66.611162
1378.390974	38.682752	66.616167
1377.443768	50.574915	66.621172
1376.394330	50.998214	66.626177
1376.232445	51.357733	66.631182
1375.572073	51.151490	66.636186
1375.125745	43.187204	66.641191
1373.739685	44.581799	66.646196
1373.243606	42.840281	66.651201
1372.900360	45.072107	66.656206
1372.045451	46.781267	66.661210
1371.972959	45.672609	66.666215
1370.741343	49.887525	66.671220
1370.272960	44.207052	66.676225
1370.126321	45.155515	66.681230
1368.888698	48.524551	66.686234
1367.871702	47.865622	66.691239
1367.316992	43.395794	66.696244
1366.900053	45.771799	66.701249
1366.417917	41.009736	66.706254
1365.465608	39.566234	66.711258
1364.640283	40.133695	66.716263
1363.549068	46.049934	66.721268
1363.607024	44.190405	66.726273
1363.309758	42.835191	66.731278
1362.338221	45.635232	66.736282
1361.741155	38.081267	66.741287
1360.948754	41.131962	66.746292
1360.181094	51.563703	66.751297
1359.994619	44.972669	66.756302
1359.035856	53.995005	66.761306
1358.431220	44.849495	66.766311
1357.849489	53.960145	66.771316
1357.460890	53.313316	66.776321
1356.623490	52.307300	66.781326
1355.542323	48.700168	66.786330
1355.111936	47.205261	66.791335
1354.381849	44.989997	66.796340
1353.531357	51.386809	66.801345
1353.102154	49.352387	66.806350
1352.216202	50.924559	66.811354
1352.066613	49.515913	66.816359
1350.925198	43.169692	66.821364
1349.979243	54.060287	66.826369
1349.331542	44.183600	66.831374
1349.070349	48.025096	66.836378
1349.109624	42.688152	66.841383
1347.902731	52.103167	66.846388
1346.737924	60.066989	66.851393
1346.080206	54.175332	66.856398
1345.627825	52.406373	66.861402
1345.419330	40.581708	66.866407
1344.354673	60.678630	66.871412
1343.441809	55.138189	66.876417
1343.175265	46.544508	66.881422
1342.214647	58.547629	66.886426
1342.294452	57.211336	66.891431
1341.265107	61.841982	66.896436
1340.401825	57.208307	66.901441
1339.669712	45.716023	66.906446
1339.222343	55.073407	66.911450
1338.801609	52.108803	66.916455
1337.484691	55.176639	66.921460
1337.008774	54.846470	66.926465
1336.776179	44.047515	66.931470
1336.218211	52.170358	66.936474
1335.361858	53.282085	66.941479
1334.555645	54.429999	66.946484
1334.289499	47.752281	66.951489
1333.444742	46.261734	66.956494
1331.909401	43.963148	66.961498
1331.463179	44.142355	66.966503
1331.009104	51.237845	66.971508
1330.618887	51.906475	66.976513
1330.328496	48.336099	66.981518
1329.154279	52.707493	66.986522
1328.729885	49.104799	66.991527
1327.957795	55.916518	66.996532
1327.622091	54.980584	67.001537
1326.857749	35.734717	67.006542
1325.641834	52.249134	67.011546
1325.461148	45.053204	67.016551
1324.817485	45.421490	67.021556
1323.785560	48.544961	67.026561
1323.321147	42.687248	67.031566
1322.450267	55.959765	67.036570
1321.992015	55.100081	67.041575
1321.542499	57.202147	67.046580
1320.374716	48.196618	67.051585
1319.720048	52.816603	67.056590
1319.015763	50.396973	67.061594
1318.849355	48.363367	67.066599
1318.169173	48.672804	67.071604
1317.446074	53.595406	67.076609
1316.895473	48.177175	67.081614
1316.115614	53.152954	67.086618
1315.749761	46.864831	67.091623
1314.630876	49.174215	67.096628
1313.798378	52.330648	67.101633
1313.427500	45.567078	67.106638
1312.711959	50.907955	67.111642
1312.247523	46.385944	67.116647
1311.403783	56.629514	67.121652
1310.759304	53.970141	67.126657
1310.309421	49.830598	67.131662
1309.823006	48.724655	67.136666
1308.945372	47.439618	67.141671
1308.113040	55.998742	67.146676
1307.592703	49.001881	67.151681
1306.701176	49.480533	67.156686
1305.672344	48.113872	67.161690
1304.996881	46.348841	67.166695
1304.619266	52.943319	67.171700
1304.178368	47.051909	67.176705
1304.138062	44.561439	67.181710
1302.626142	55.830592	67.186714
1301.951698	43.203198	67.191719
1301.626673	47.977372	67.196724
1300.964731	50.043817	67.201729
1300.700176	47.901232	67.206734
1299.207832	57.590302	67.211738
1299.067110	47.812822	67.216743
1298.378728	50.723998	67.221748
1297.341340	49.331892	67.226753
1296.566604	51.066179	67.231758
1295.927915	52.189053	67.236762
1295.587267	50.761894	67.241767
1295.103160	52.462601	67.246772
1294.651556	57.231667	67.251777
1293.405251	51.698517	67.256782
1292.639392	62.432770	67.261786
1292.248683	50.302753	67.266791
1291.755323	53.585061	67.271796
1290.789869	55.994648	67.276801
1289.988954	47.003363	67.281806
1289.303059	53.684692	67.286810
1288.998344	45.164900	67.291815
1288.641384	62.872194	67.296820
1288.044855	48.122423	67.301825
1287.409653	52.739320	67.306830
1286.612622	57.818764	67.311834
1286.022391	51.599428	67.316839
1284.865132	58.224797	67.321844
1283.889090	53.082360	67.326849
1283.937361	48.411047	67.331854
1283.104151	54.783053	67.336858
1282.225298	46.873349	67.341863
1280.985785	49.894213	67.346868
1280.546666	56.362851	67.351873
1280.247288	51.617487	67.356878
1279.766946	55.164237	67.361882
1279.674312	46.658043	67.366887
1278.886404	57.283834	67.371892
1277.797746	56.573253	67.376897
1277.485414	52.784018	67.381902
1276.144994	64.913766	67.386906
1275.376067	51.790453	67.391911
1274.978802	59.629139	67.396916
1274.311455	55.128350	67.401921
1274.196553	39.892020	67.406926
1273.021906	51.836132	67.411930
1271.986976	48.866671	67.416935
1271.517983	54.562610	67.421940
1271.141472	59.614637	67.426945
1270.725282	48.199894	67.431950
1270.046591	52.199226	67.436954
1269.228235	53.621906	67.441959
1268.729520	50.814794	67.446964
1267.969716	51.950619	67.451969
1267.155873	50.288021	67.456974
1266.128486	50.275767	67.461978
1265.734691	46.668221	67.466983
1265.067694	46.683836	67.471988
1264.542307	53.180381	67.476993
1264.239281	52.144643	67.481998
1262.988192	55.506406	67.487002
1262.685487	45.895033	67.492007
1262.167278	50.244174	67.497012
1261.495484	50.080777	67.502017
1260.507317	44.251143	67.507022
1259.370467	51.396830	67.512026
1259.371320	54.427112	67.517031
1258.809657	51.789283	67.522036
1257.782874	64.026876	67.527041
1257.623101	53.292049	67.532046
1256.674573	55.930773	67.537050
1256.128522	51.445402	67.542055
1254.805640	64.696752	67.547060
1254.149210	61.853210	67.552065
1253.780593	45.050274	67.557070
1253.058936	61.350531	67.562074
1252.732584	50.244790	67.567079
1252.414476	50.309026	67.572084
1251.393318	55.337374	67.577089
1250.886460	58.115625	67.582094
1250.162087	62.987986	67.587098
1249.663748	54.109464	67.592103
1248.465366	59.982860	67.597108
1247.803626	52.776677	67.602113
1247.600176	47.226006	67.607118
1246.807897	61.003294	67.612122
1245.716283	54.557741	67.617127
1245.218131	51.023559	67.622132
1244.547048	54.260009	67.627137
1244.567128	49.325093	67.632142
1243.482939	52.199855	67.637146
1242.689040	49.791340	67.642151
1242.176149	58.643479	67.647156
1241.301019	43.608433	67.652161
1240.537155	43.644184	67.657166
1239.580709	46.623220	67.662170
1239.374203	48.208841	67.667175
1238.744616	53.980777	67.672180
1238.692509	52.589758	67.677185
1237.984209	50.009939	67.682190
1236.642519	52.170270	67.687194
1235.858540	45.992790	67.692199
1235.695906	47.724404	67.697204
1234.900379	44.111343	67.702209
1234.163479	37.582604	67.707214
1233.134161	50.192761	67.712218
1232.539428	48.015941	67.717223
1232.539639	51.394835	67.722228
1231.526123	52.530004	67.727233
1230.878689	39.951964	67.732238
1229.987208	54.776360	67.737242
1229.728067	44.628206	67.742247
1229.159991	45.034962	67.747252
1227.740818	52.050500	67.752257
1227.264385	41.225678	67.757262
1226.935084	54.598196	67.762266
1226.891871	43.471108	67.767271
1225.748909	56.544045	67.772276
1224.623965	61.628329	67.777281
1224.031872	51.771227	67.782286
1223.485446	56.134324	67.787290
1223.208309	45.881797	67.792295
1221.713068	43.750371	67.797300
1220.967839	48.700167	67.802305
1220.753986	50.255418	67.807310
1220.137252	55.348793	67.812314
1220.184888	41.023355	67.817319
1219.283661	45.818176	67.822324
1218.401772	44.350918	67.827329
1218.191393	44.380684	67.832334
1217.053512	52.972635	67.837338
1216.139233	56.410184	67.842343
1215.697358	53.035797	67.847348
1215.355657	56.603093	67.852353
1214.638303	53.600514	67.857358
1213.536560	49.183000	67.862362
1212.840288	43.505679	67.867367
1212.744265	49.538147	67.872372
1211.968587	58.990317	67.877377
1210.963335	48.446691	67.882382
1210.012226	59.197792	67.887386
1209.760095	52.798567	67.892391
1209.438213	45.030583	67.897396
1208.307711	48.772171	67.902401
1207.737144	51.215201	67.907406
1206.693141	60.219593	67.912410
1206.366974	50.241371	67.917415
1206.032264	58.186811	67.922420
1204.676247	57.613387	67.927425
1204.236511	52.920313	67.932430
1203.773992	57.851976	67.937434
1203.420939	62.480806	67.942439
1202.843077	51.733612	67.947444
1201.386820	53.095303	67.952449
1200.823485	48.978553	67.957454
1200.251584	49.130454	67.962458
1200.010597	42.677423	67.967463
1199.320524	50.113225	67.972468
1198.211981	57.421595	67.977473
1197.886526	50.128848	67.982478
1197.213144	57.183527	67.987482
1196.739347	54.966987	67.992487
1195.723050	48.873767	67.997492
1194.770017	53.979613	68.002497
1194.674676	53.394995	68.007502
1194.132065	60.859398	68.012506
1193.668668	54.724003	68.017511
1192.469345	54.642919	68.022516
1191.907282	53.008124	68.027521
1191.552174	44.614638	68.032526
1190.181173	49.528314	68.037530
1189.622252	49.991971	68.042535
1189.154957	56.632258	68.047540
1188.692964	54.617272	68.052545
1188.571897	48.209830	68.057550
1187.256839	59.261656	68.062554
1186.273700	47.214826	68.067559
1185.938028	52.954233	68.072564
1185.138957	59.487997	68.077569
1184.859375	56.166661	68.082574
1183.594546	60.861611	68.087578
1183.372935	41.272471	68.092583
1182.806111	52.506530	68.097588
1182.121929	53.630356	68.102593
1181.053129	48.215704	68.107598
1180.112596	53.198140	68.112602
1180.171635	49.581690	68.117607
1179.574726	52.902556	68.122612
1178.716772	53.500495	68.127617
1178.096759	50.144978	68.132622
1177.241105	54.737024	68.137626
1176.933898	50.358780	68.142631
1176.053285	43.621093	68.147636
1174.797828	49.790599	68.152641
1174.598486	48.751003	68.157646
1173.906797	54.463438	68.162650
1173.519347	45.983633	68.167655
1173.177211	52.850027	68.172660
1172.019960	47.774299	68.177665
1171.484315	54.146330	68.182670
1171.038084	59.447574	68.187674
1170.195250	58.369943	68.192679
1169.404788	50.747432	68.197684
1168.644017	64.723156	68.202689
1168.535108	48.631166	68.207694
1166.973404	55.983214	68.212698
1165.838587	53.080143	68.217703
1164.907243	51.136637	68.222708
1164.752978	61.461427	68.227713
1164.714307	47.217523	68.232718
1163.932152	50.698735	68.237722
1163.584560	54.665946	68.242727
1162.851768	59.273155	68.247732
1162.086486	60.846703	68.252737
1161.837108	48.539709	68.257742
1160.412859	58.657993	68.262746
1159.660680	47.243089	68.267751
1159.326420	54.669634	68.272756
1158.818399	54.100172	68.277761
1158.604084	50.271718	68.282766
1157.682457	56.695662	68.287770
1156.841389	54.305714	68.292775
1156.225569	59.673349	68.297780
1155.301646	54.667762	68.302785
1155.242444	51.005457	68.307790
1154.152844	64.347485	68.312794
1153.444260	52.878338	68.317799
1152.958155	49.000060	68.322804
1152.323416	62.526807	68.327809
1152.134668	46.726642	68.332814
1150.733373	53.319899	68.337818
1149.906604	59.187862	68.342823
1149.566769	52.077186	68.347828
1149.301372	54.741365	68.352833
1148.337600	52.944948	68.357838
1147.548688	61.823642	68.362842
1147.221324	47.023243	68.367847
1146.601988	49.070333	68.372852
1145.221987	61.430352	68.377857
1144.796224	54.506806	68.382862
1144.399474	55.261657	68.387866
1144.036065	49.048876	68.392871
1142.832387	48.733539	68.397876
1142.016899	51.265989	68.402881
1141.758518	45.187898	68.407886
1141.049262	50.384308	68.412890
1140.535088	50.527043	68.417895
1139.650555	46.338381	68.422900
1138.927093	51.300504	68.427905
1138.619058	52.657846	68.432910
1137.899577	55.329575	68.437914
1137.042955	51.177476	68.442919
1136.265288	54.307894	68.447924
1135.447735	52.560773	68.452929
1135.170104	57.005723	68.457934
1134.917996	55.127687	68.462938
1133.641393	52.204600	68.467943
1133.105052	43.051461	68.472948
1132.124068	51.326751	68.477953
1131.822002	48.015308	68.482958
1131.044386	54.222392	68.487962
1130.326800	55.947638	68.492967
1129.636571	49.195464	68.497972
1129.210065	59.021062	68.502977
1128.883182	47.910708	68.507982
1127.607330	60.104358	68.512986
1126.797270	50.811813	68.517991
1126.434402	41.982756	68.522996
1126.089644	56.721811	68.528001
1125.676087	51.296031	68.533006
1124.219255	54.100785	68.538010
1123.768169	52.672289	68.543015
1123.568946	50.315907	68.548020
1122.585542	53.026454	68.553025
1121.663322	45.150525	68.558030
1121.050004	53.176540	68.563034
1120.528073	52.118860	68.568039
1119.984142	42.722501	68.573044
1119.153772	50.585910	68.578049
1119.066913	54.016493	68.583054
1118.259536	56.905634	68.588058
1116.976507	55.237270	68.593063
1116.251921	55.856599	68.598068
1115.202027	53.025204	68.603073
1114.793737	47.754711	68.608078
1114.306526	51.348307	68.613082
1114.294899	52.753135	68.618087
1113.884952	53.727711	68.623092
1112.995845	52.365719	68.628097
1112.361504	51.250222	68.633102
1111.866575	49.757737	68.638106
1110.445888	45.280605	68.643111
1110.155338	51.334542	68.648116
1109.492571	52.880764	68.653121
1108.555621	46.926356	68.658126
1107.517782	47.685389	68.663130
1107.085139	47.004602	68.668135
1106.547546	47.986863	68.673140
1105.941417	53.302501	68.678145
1105.652511	48.172298	68.683150
1104.818975	46.653237	68.688154
1103.784941	46.041278	68.693159
1103.480032	43.397352	68.698164
1102.688294	54.441680	68.703169
1102.428223	45.435428	68.708174
1101.088764	52.365808	68.713178
1100.422979	52.950559	68.718183
1100.368043	43.479596	68.723188
1099.577996	56.341905	68.728193
1098.790443	49.261439	68.733198
1097.905623	45.900748	68.738202
1097.607745	47.548218	68.743207
1096.945605	45.744856	68.748212
1095.834425	48.299111	68.753217
1095.060419	40.005383	68.758222
1094.737266	39.532693	68.763226
1094.283927	43.526186	68.768231
1093.996453	43.103016	68.773236
1092.672129	49.609941	68.778241
1092.232982	45.790442	68.783246
1091.625409	47.789942	68.788250
1091.023409	40.727284	68.793255
1090.302296	31.931559	68.798260
1089.253711	44.197879	68.803265
1088.961855	46.699109	68.808270
1088.083388	38.158644	68.813274
1087.234745	32.321096	68.818279
1086.622935	31.444877	68.823284
1085.797254	38.091698	68.828289
1085.763222	34.269279	68.833294
1085.273604	45.390138	68.838298
1084.274047	48.101689	68.843303
1083.535135	40.207666	68.848308
1082.889907	55.164816	68.853313
1082.710613	46.328649	68.858318
1082.585621	41.653361	68.863322
1081.852559	49.162253	68.868327
1079.730888	50.120473	68.873332
1078.784521	48.162043	68.878337
1078.163385	36.597029	68.883342
1077.857364	46.912822	68.888346
1078.285089	43.636714	68.893351
1078.058617	38.512360	68.898356
1076.336193	48.369008	68.903361
1075.292701	41.259872	68.908366
1074.383276	40.580800	68.913370
1074.047102	47.473057	68.918375
1073.795730	35.937549	68.923380
1072.677611	43.682723	68.928385
1072.360829	37.987676	68.933390
1071.464678	41.474425	68.938394
1071.088719	42.125054	68.943399
1071.032861	42.775238	68.948404
1069.550082	42.837064	68.953409
1068.800776	34.643501	68.958414
1068.579061	48.449913	68.963418
1067.584946	41.848596	68.968423
1066.667089	45.936471	68.973428
1065.849620	50.885176	68.978433
1065.721286	45.079732	68.983438
1065.325053	49.113034	68.988442
1064.799935	49.462530	68.993447
1063.996410	41.384822	68.998452
1062.862209	43.146382	69.003457
1062.671123	50.351460	69.008462
1062.923313	51.206544	69.013466
1061.906768	54.401783	69.018471
1061.284502	48.392616	69.023476
1059.990686	43.952107	69.028481
1059.617154	52.783674	69.033486
1058.299493	52.164803	69.038490
1057.501505	45.079707	69.043495
1057.264033	46.723881	69.048500
1056.544467	56.362700	69.053505
1055.939649	46.957118	69.058510
1055.095338	45.417710	69.063514
1054.552257	55.012689	69.068519
1054.208302	44.542167	69.073524
1052.569541	51.173237	69.078529
1051.920874	47.924817	69.083534
1051.661171	45.343094	69.088538
1051.170188	47.516450	69.093543
1051.158852	42.267994	69.098548
1049.916961	55.036592	69.103553
1049.350473	52.254500	69.108558
1048.211433	54.065722	69.113562
1047.935864	48.799365	69.118567
1047.736798	42.013259	69.123572
1046.603730	49.095342	69.128577
1045.983240	42.983396	69.133582
1045.549796	41.933737	69.138586
1044.426302	46.967390	69.143591
1043.178529	45.735009	69.148596
1042.822918	47.994069	69.153601
1042.621973	46.552613	69.158606
1042.334009	45.785748	69.163610
1041.645052	48.324910	69.168615
1040.688825	44.284887	69.173620
1039.921767	48.299899	69.178625
1039.481764	39.188240	69.183630
1039.098825	46.811765	69.188634
1038.024003	46.559562	69.193639
1037.236257	45.886381	69.198644
1036.574100	58.211115	69.203649
1036.187763	45.508039	69.208654
1035.224955	50.251209	69.213658
1034.496819	44.446550	69.218663
1034.136578	42.565225	69.223668
1033.508281	45.878495	69.228673
1032.827870	48.588190	69.233678
1031.938527	42.758710	69.238682
1031.270834	49.831434	69.243687
1031.138643	44.944404	69.248692
1029.901914	51.398001	69.253697
1029.076780	44.036533	69.258702
1028.879086	56.968642	69.263706
1028.434063	60.487733	69.268711
1027.907107	45.179793	69.273716
1026.532178	44.131650	69.278721
1026.292630	40.919092	69.283726
1025.466590	48.017003	69.288730
1024.509820	48.693787	69.293735
1023.663432	52.450185	69.298740
1022.956160	42.474281	69.303745
1022.976726	43.591708	69.308750
1022.417631	50.284458	69.313754
1021.629178	48.327741	69.318759
1020.848133	41.989026	69.323764
1020.007626	54.272739	69.328769
1019.638963	47.802196	69.333774
1019.004728	44.671341	69.338778
1017.976634	45.329510	69.343783
1017.536848	45.315356	69.348788
1016.756085	45.423248	69.353793
1016.725844	46.446253	69.358798
1015.497155	49.610596	69.363802
1014.477920	53.044402	69.368807
1014.243704	49.864111	69.373812
1013.676227	51.281656	69.378817
1013.111629	48.962903	69.383822
1012.123593	52.388593	69.388826
1011.348561	43.856936	69.393831
1011.054673	45.325582	69.398836
1010.370543	53.832814	69.403841
1009.408801	49.145545	69.408846
1008.825687	51.289407	69.413850
1008.182577	56.705565	69.418855
1008.255519	46.208164	69.423860
1006.833778	54.846917	69.428865
1006.161546	46.601688	69.433870
1005.484756	52.723375	69.438874
1005.107112	51.218565	69.443879
1004.482694	48.226501	69.448884
1003.119715	53.656238	69.453889
1002.777866	39.564675	69.458894
1002.375804	50.207986	69.463898
1002.013838	47.954776	69.468903
1001.131408	41.889241	69.473908
1000.091889	47.623921	69.478913
999.775075	44.710664	69.483918
999.213273	53.775610	69.488922
998.246486	52.498556	69.493927
997.577526	48.056459	69.498932
996.764824	57.569754	69.503937
996.607948	58.437860	69.508942
995.960110	47.485826	69.513946
995.244336	53.709913	69.518951
994.285287	44.475820	69.523956
993.846912	54.864712	69.528961
993.284719	53.993238	69.533966
991.978969	44.341205	69.538970
991.252295	50.953382	69.543975
990.943632	46.283663	69.548980
990.180999	46.484874	69.553985
990.152140	51.637742	69.558990
989.546469	60.734904	69.563994
988.483784	56.956263	69.568999
987.945135	41.572930	69.574004
987.278433	54.291054	69.579009
986.706679	57.382451	69.584014
986.103487	49.695530	69.589018
985.233454	49.852325	69.594023
984.369050	43.353416	69.599028
983.162842	51.407531	69.604033
983.058508	49.121226	69.609038
982.451652	50.116106	69.614042
982.007454	43.905173	69.619047
981.913499	44.536187	69.624052
980.622571	51.733293	69.629057
979.789367	54.552463	69.634062
979.455764	49.803133	69.639066
978.308191	49.858999	69.644071
977.724015	46.348026	69.649076
976.907770	47.108131	69.654081
976.789293	43.888935	69.659086
975.887517	48.109899	69.664090
975.063181	45.611698	69.669095
974.356211	46.111568	69.674100
973.539309	48.519711	69.679105
973.260107	49.601244	69.684110
972.740906	50.198979	69.689114
971.755725	55.317895	69.694119
971.194415	55.105459	69.699124
970.369374	56.822609	69.704129
970.123533	49.618170	69.709134
969.657998	49.076683	69.714138
968.506230	59.336211	69.719143
968.056583	42.806462	69.724148
967.482233	46.841300	69.729153
967.083757	52.819372	69.734158
965.674755	45.888282	69.739162
965.241124	57.296721	69.744167
964.834445	44.027617	69.749172
964.196804	50.777025	69.754177
963.912919	45.934634	69.759182
962.993045	52.227465	69.764186
961.766348	48.728822	69.769191
961.294275	51.921060	69.774196
960.282594	53.197968	69.779201
959.866261	52.090407	69.784206
959.170326	40.956807	69.789210
958.879137	54.651265	69.794215
958.690223	46.963106	69.799220
957.401698	56.432254	69.804225
956.646273	44.743561	69.809230
956.394359	53.612556	69.814234
955.294201	49.830432	69.819239
954.634244	44.481738	69.824244
953.806294	56.345571	69.829249
953.599157	50.806566	69.834254
953.401992	46.311505	69.839258
952.177594	50.638996	69.844263
951.265874	44.071934	69.849268
950.505925	56.683472	69.854273
950.389797	43.103220	69.859278
949.478934	44.573829	69.864282
948.403341	50.869359	69.869287
948.000177	55.955616	69.874292
947.496797	56.330064	69.879297
947.284189	45.427083	69.884302
946.333832	47.127906	69.889306
945.575640	58.980645	69.894311
945.260871	56.880786	69.899316
944.078675	66.328298	69.904321
943.061318	46.572501	69.909326
942.152506	54.325429	69.914330
941.837817	56.464450	69.919335
941.585010	48.086283	69.924340
941.126088	48.849478	69.929345
940.703068	47.399206	69.934350
940.039941	40.123968	69.939354
939.051681	52.114230	69.944359
938.838565	51.941025	69.949364
937.240962	52.275088	69.954369
936.864669	49.618886	69.959374
936.588081	53.680478	69.964378
935.502020	51.758520	69.969383
934.699837	45.248155	69.974388
934.087885	52.414533	69.979393
933.711761	53.241828	69.984398
933.009381	49.585668	69.989402
932.591732	49.973287	69.994407
931.585877	45.838701	69.999412
930.625607	54.022446	70.004417
930.095577	57.599229	70.009422
929.783829	55.322271	70.014426
929.120811	59.140988	70.019431
928.357636	42.654825	70.024436
927.587562	55.884572	70.029441
927.260907	55.702623	70.034446
926.511501	54.397320	70.039450
925.328170	51.514698	70.044455
925.157836	46.802482	70.049460
924.640371	55.597031	70.054465
923.986748	45.839711	70.059470
923.151282	55.072787	70.064474
921.878236	50.272654	70.069479
921.795571	45.658456	70.074484
920.983241	53.399193	70.079489
920.596085	49.875813	70.084494
919.404035	51.583558	70.089498
918.982663	55.810114	70.094503
918.657903	47.818718	70.099508
918.080552	51.111292	70.104513
916.978261	47.286947	70.109518
916.447161	45.109547	70.114522
915.497168	47.191948	70.119527
915.451941	44.864705	70.124532
914.544704	44.287846	70.129537
913.605178	42.333123	70.134542
913.267165	41.397616	70.139546
912.799062	52.481952	70.144551
912.228020	42.525418	70.149556
911.162760	54.087966	70.154561
910.524839	48.584389	70.159566
910.115390	51.553781	70.164570
909.044670	57.129455	70.169575
908.316968	47.306655	70.174580
907.518019	46.690491	70.179585
907.358385	46.294312	70.184590
906.990373	41.148346	70.189594
905.709018	49.780576	70.194599
905.216969	45.015469	70.199604
904.317695	54.829563	70.204609
904.096214	50.019829	70.209614
903.459311	46.126178	70.214618
902.232334	58.119742	70.219623
901.902991	44.089293	70.224628
901.160375	56.920434	70.229633
900.908506	56.549969	70.234638
899.724670	54.758701	70.239642
898.982088	51.408571	70.244647
898.960123	46.138160	70.249652
898.026513	54.628335	70.254657
897.455388	47.992910	70.259662
896.283877	52.412937	70.264666
895.928800	48.827687	70.269671
895.615988	47.656358	70.274676
894.697344	44.682754	70.279681
893.691842	42.908849	70.284686
893.184685	55.508559	70.289690
892.561260	52.382325	70.294695
892.549603	39.567641	70.299700
891.215141	54.964056	70.304705
890.657529	48.389562	70.309710
890.292165	55.444174	70.314714
889.742035	49.959751	70.319719
888.810828	46.828873	70.324724
887.558795	42.952675	70.329729
887.378727	44.363799	70.334734
886.609406	41.262359	70.339738
886.159562	45.927111	70.344743
885.307410	47.246474	70.349748
884.314773	52.782922	70.354753
884.016085	50.742015	70.359758
883.725044	45.187986	70.364762
883.144787	49.372015	70.369767
882.259179	46.145575	70.374772
881.251149	46.472596	70.379777
881.351965	43.324173	70.384782
879.939237	43.338693	70.389786
878.509932	54.208539	70.394791
878.494158	42.045798	70.399796
877.895741	48.940368	70.404801
877.734360	48.757360	70.409806
877.436217	45.912115	70.414810
876.402150	52.831850	70.419815
875.763414	39.487737	70.424820
875.073439	52.865594	70.429825
873.682109	52.220694	70.434830
873.308196	50.562346	70.439834
872.663552	47.431610	70.444839
872.349215	45.543007	70.449844
871.808120	45.724772	70.454849
871.347266	47.893364	70.459854
870.170496	50.674192	70.464858
869.503385	54.908314	70.469863
869.430392	46.241352	70.474868
868.113887	58.973002	70.479873
867.420536	49.583148	70.484878
867.139442	43.910844	70.489882
866.398969	49.422943	70.494887
865.522525	45.509070	70.499892
864.452121	50.494922	70.504897
864.168882	47.461224	70.509902
863.932135	43.525990	70.514906
863.028419	44.945028	70.519911
862.310555	37.963957	70.524916
861.815369	48.735633	70.529921
861.256753	55.037244	70.534926
860.402586	45.357591	70.539930
859.346057	43.659629	70.544935
858.817299	49.437665	70.549940
858.272539	49.661017	70.554945
857.901812	47.582691	70.559950
857.470877	45.465060	70.564954
855.944344	54.991043	70.569959
855.581779	39.313236	70.574964
855.047806	55.496929	70.579969
854.207311	50.613811	70.584974
853.790235	47.380637	70.589978
852.880407	48.226635	70.594983
852.862579	46.010154	70.599988
852.065877	47.431091	70.604993
851.011527	49.976402	70.609998
850.516659	44.185152	70.615002
849.906895	53.551064	70.620007
849.110250	42.495034	70.625012
848.068776	54.123202	70.630017
847.292042	46.437134	70.635022
847.155345	53.605173	70.640026
846.263849	53.434267	70.645031
846.069093	44.275747	70.650036
845.260794	57.738673	70.655041
844.516882	48.768462	70.660046
844.095895	50.884982	70.665050
843.130826	51.716120	70.670055
842.311994	47.020374	70.675060
841.336673	48.506008	70.680065
840.605008	56.396357	70.685070
840.924623	43.252994	70.690074
840.262708	61.549686	70.695079
839.256428	50.990641	70.700084
838.356316	60.224565	70.705089
838.036256	49.742406	70.710094
837.449711	48.218825	70.715098
836.031486	51.020744	70.720103
835.887746	46.528236	70.725108
835.441376	51.758574	70.730113
834.819974	58.991131	70.735118
834.078914	40.197548	70.740122
833.015863	53.027647	70.745127
832.805335	52.275292	70.750132
831.922179	51.399737	70.755137
830.523999	45.641850	70.760142
830.314930	43.927315	70.765146
829.557572	54.830604	70.770151
829.367823	45.570364	70.775156
828.729696	44.665280	70.780161
828.232303	50.266440	70.785166
827.397980	48.069503	70.790170
826.395258	47.777531	70.795175
826.213997	46.768205	70.800180
825.743217	53.027458	70.805185
824.707948	51.789755	70.810190
824.334537	45.222239	70.815194
823.468246	50.528864	70.820199
822.459841	52.683673	70.825204
821.197207	48.386569	70.830209
820.753112	49.618938	70.835214
821.114598	51.795447	70.840218
820.436586	59.861768	70.845223
819.777868	46.768434	70.850228
818.539592	53.394254	70.855233
817.698830	43.040700	70.860238
817.692042	50.792041	70.865242
816.989535	46.342724	70.870247
815.868499	43.571671	70.875252
815.147897	51.655805	70.880257
814.824879	50.080831	70.885262
814.489866	43.715367	70.890266
813.050748	56.802442	70.895271
812.452632	43.798819	70.900276
812.090267	54.058928	70.905281
811.824228	59.880322	70.910286
810.950970	48.551065	70.915290
809.455783	55.411742	70.920295
809.545195	46.499743	70.925300
809.102576	54.240018	70.930305
808.466045	46.711427	70.935310
807.506645	48.013189	70.940314
806.478886	51.115686	70.945319
806.090137	49.861836	70.950324
805.491131	55.628984	70.955329
804.943532	51.158171	70.960334
803.831329	56.869795	70.965338
803.191652	58.488110	70.970343
803.068692	49.247205	70.975348
802.374839	47.933101	70.980353
801.568159	47.527938	70.985358
800.958819	41.674493	70.990362
800.106302	49.912088	70.995367
799.994366	55.623800	71.000372
798.955758	54.146941	71.005377
798.481735	54.286508	71.010382
798.148912	57.694733	71.015386
796.559871	64.229732	71.020391
795.876418	42.862848	71.025396
795.203217	58.715463	71.030401
794.919860	51.728338	71.035406
794.645846	48.581218	71.040410
793.550439	54.411599	71.045415
793.026830	46.552803	71.050420
792.297268	52.875321	71.055425
791.915171	57.116142	71.060430
791.118259	52.550967	71.065434
790.003305	51.426886	71.070439
789.857307	41.738642	71.075444
789.402155	40.635714	71.080449
788.105487	43.057186	71.085454
787.600701	46.424968	71.090458
786.771744	47.633436	71.095463
786.509669	44.416608	71.100468
785.983945	43.525186	71.105473
784.623763	42.943189	71.110478
784.257701	40.916174	71.115482
783.372506	48.554995	71.120487
783.370565	43.377600	71.125492
782.543157	54.066540	71.130497
781.082240	49.793130	71.135502
780.870696	48.837513	71.140506
780.368219	50.605887	71.145511
780.298239	51.097472	71.150516
779.390739	56.580982	71.155521
778.311751	53.226084	71.160526
777.755793	44.207064	71.165530
777.108410	47.132338	71.170535
776.407482	49.287114	71.175540
775.572969	50.326158	71.180545
774.630010	46.292018	71.185550
774.412770	43.430759	71.190554
774.137526	55.859524	71.195559
773.457586	42.367464	71.200564
772.243471	44.026747	71.205569
771.724174	47.128757	71.210574
771.575162	50.723773	71.215578
770.328324	49.868275	71.220583
769.733694	44.890867	71.225588
769.094177	44.640461	71.230593
768.305191	49.978953	71.235598
768.107600	50.246419	71.240602
767.120043	51.816030	71.245607
766.424075	51.494183	71.250612
765.787480	56.146098	71.255617
765.536733	48.234420	71.260622
764.684542	50.097880	71.265626
763.632135	58.756813	71.270631
763.500819	49.200274	71.275636
762.777097	50.008799	71.280641
761.914919	55.240671	71.285646
760.948946	45.887942	71.290650
760.206936	55.191336	71.295655
759.947027	48.768195	71.300660
759.411185	54.671955	71.305665
758.789122	45.419033	71.310670
757.927867	41.844987	71.315674
757.179081	53.372978	71.320679
756.986618	46.514900	71.325684
755.765128	47.776393	71.330689
755.141923	49.584487	71.335694
754.548376	46.166530	71.340698
753.993255	45.948426	71.345703
753.504582	47.421292	71.350708
752.908419	52.319087	71.355713
752.026603	52.656034	71.360718
751.672147	49.302525	71.365722
750.651825	50.440538	71.370727
749.528122	47.550090	71.375732
749.189784	48.942258	71.380737
748.686898	42.816417	71.385742
748.471555	40.864767	71.390746
747.212537	52.573320	71.395751
746.725820	41.190460	71.400756
746.229552	41.180612	71.405761
745.696239	48.295077	71.410766
744.551078	37.654116	71.415770
743.630628	49.460167	71.420775
743.310914	45.609118	71.425780
743.186013	50.556486	71.430785
742.353878	52.014635	71.435790
741.312260	40.857295	71.440794
740.424802	49.852677	71.445799
740.191572	40.903731	71.450804
739.948589	48.593309	71.455809
738.756320	53.570220	71.460814
737.935978	47.744069	71.465818
737.113489	48.281314	71.470823
737.151123	40.211779	71.475828
736.039396	50.977521	71.480833
735.158266	44.851963	71.485838
734.841953	43.320089	71.490842
734.072987	47.150978	71.495847
733.868403	44.439097	71.500852
733.098341	48.697519	71.505857
732.251872	50.872318	71.510862
731.724883	46.623751	71.515866
730.814690	51.699269	71.520871
729.812446	43.664364	71.525876
729.072834	52.063780	71.530881
728.651966	56.380165	71.535886
728.796459	37.748460	71.540890
727.853125	50.887539	71.545895
726.760556	51.344773	71.550900
726.230800	48.217869	71.555905
725.675594	42.716956	71.560910
724.971374	50.866309	71.565914
723.924033	57.881251	71.570919
723.319447	46.578657	71.575924
723.142248	50.157660	71.580929
722.392957	58.388309	71.585934
722.156358	45.905920	71.590938
720.629135	48.775712	71.595943
720.027951	41.023906	71.600948
719.835768	49.944893	71.605953
718.755166	54.694301	71.610958
717.820865	53.008483	71.615962
717.329592	52.406484	71.620967
716.850379	47.182059	71.625972
716.673249	53.769900	71.630977
716.258278	47.965965	71.635982
715.452296	41.670759	71.640986
714.360905	52.893745	71.645991
714.109687	51.419320	71.650996
713.168473	55.913152	71.656001
711.843770	50.402262	71.661006
711.512782	46.376393	71.666010
711.120065	49.671154	71.671015
710.314008	46.637122	71.676020
709.421863	50.624823	71.681025
708.777435	47.688066	71.686030
708.570761	42.617383	71.691034
708.006146	48.377493	71.696039
707.502941	54.124677	71.701044
706.466167	44.086227	71.706049
705.678687	58.217650	71.711054
705.246837	47.029493	71.716058
703.799086	53.180923	71.721063
703.717367	43.605463	71.726068
703.054831	45.199054	71.731073
702.585859	48.717268	71.736078
702.344599	48.930189	71.741082
700.902088	52.768957	71.746087
700.461763	53.824125	71.751092
700.042073	52.143129	71.756097
699.306074	47.241862	71.761102
698.632444	41.490147	71.766106
697.532726	59.325100	71.771111
697.298728	50.409394	71.776116
696.608206	56.623217	71.781121
695.696712	55.332749	71.786126
694.940033	50.172998	71.791130
694.388175	53.430017	71.796135
693.984494	48.605161	71.801140
693.366761	53.079045	71.806145
692.579372	46.099637	71.811150
692.132183	43.330185	71.816154
691.125244	52.133289	71.821159
690.807661	46.474708	71.826164
689.551961	45.254806	71.831169
688.934041	48.801464	71.836174
688.379400	37.708560	71.841178
688.122658	44.053601	71.846183
687.509275	46.315889	71.851188
686.750271	45.365429	71.856193
686.033150	46.693322	71.861198
685.443569	41.429706	71.866202
684.739379	49.217936	71.871207
683.609326	44.970766	71.876212
683.027778	44.294835	71.881217
682.442802	53.776673	71.886222
682.669853	47.026866	71.891226
681.362191	55.819499	71.896231
680.832023	51.096783	71.901236
680.078898	46.255020	71.906241
679.071188	52.636034	71.911246
678.491200	39.083950	71.916250
677.458135	59.097121	71.921255
676.981160	52.547698	71.926260
676.846227	44.879377	71.931265
676.394920	46.565505	71.936270
675.884684	40.814595	71.941274
674.757682	45.694406	71.946279
673.945197	44.656270	71.951284
673.474683	44.456254	71.956289
672.507614	49.476188	71.961294
671.983738	38.370507	71.966298
671.325006	49.928329	71.971303
670.923644	47.271435	71.976308
670.518246	48.871408	71.981313
669.150216	56.300122	71.986318
668.758540	51.996912	71.991322
668.125152	56.176824	71.996327
667.699845	49.513522	72.001332
666.650871	40.429524	72.006337
665.815085	51.827876	72.011342
665.459540	36.194747	72.016346
664.892943	46.458984	72.021351
664.454186	43.450074	72.026356
663.366751	40.598051	72.031361
662.661557	46.355316	72.036366
662.555510	40.199440	72.041370
661.525433	52.760984	72.046375
661.142828	45.906383	72.051380
660.492817	48.666520	72.056385
659.518877	53.692284	72.061390
658.752960	44.847078	72.066394
657.626492	53.467370	72.071399
657.086109	48.240082	72.076404
656.900677	45.818475	72.081409
655.911373	55.561807	72.086414
655.948628	42.455516	72.091418
655.029931	48.141117	72.096423
654.244327	46.844816	72.101428
653.745103	41.890102	72.106433
653.126712	55.067356	72.111438
652.441047	47.431521	72.116442
651.408738	54.188625	72.121447
650.931539	54.934279	72.126452
650.759382	47.908980	72.131457
649.770478	49.672815	72.136462
649.353679	46.321365	72.141466
648.289384	46.403545	72.146471
647.257644	44.285411	72.151476
646.360557	55.130554	72.156481
645.801713	48.184164	72.161486
645.360678	45.617170	72.166490
644.889205	50.116662	72.171495
644.633133	49.365268	72.176500
644.542805	49.169386	72.181505
643.475753	51.625337	72.186510
642.806185	46.946903	72.191514
641.321065	48.086417	72.196519
640.817016	44.313618	72.201524
640.404103	48.132001	72.206529
639.676744	49.213954	72.211534
639.609412	47.655068	72.216538
638.005414	52.918346	72.221543
637.513630	44.836909	72.226548
637.497746	45.911245	72.231553
636.588819	54.334483	72.236558
635.803052	39.184597	72.241562
634.784765	47.817632	72.246567
634.579164	51.823786	72.251572
633.884262	46.545412	72.256577
632.836528	58.285028	72.261582
632.192489	40.417547	72.266586
631.420602	51.384684	72.271591
631.404637	49.483304	72.276596
630.661177	44.039197	72.281601
629.403465	51.647483	72.286606
628.945379	45.241726	72.291610
628.226833	50.416073	72.296615
627.812001	42.942135	72.301620
627.838805	45.041008	72.306625
626.817790	51.075648	72.311630
625.850539	45.701866	72.316634
625.182446	48.215730	72.321639
624.182179	45.775625	72.326644
623.356454	49.129877	72.331649
622.782717	49.394163	72.336654
622.744870	54.616255	72.341658
622.457529	46.139569	72.346663
621.613766	47.708418	72.351668
620.599669	56.965273	72.356673
619.861523	47.896461	72.361678
619.435997	37.450079	72.366682
618.300209	45.174573	72.371687
617.169258	45.584348	72.376692
617.111042	46.342147	72.381697
616.763165	45.315212	72.386702
616.535041	41.962115	72.391706
615.327053	53.134309	72.396711
614.879710	49.734112	72.401716
614.345776	46.142697	72.406721
613.069865	49.939215	72.411726
612.723888	42.949484	72.416730
611.928152	45.589330	72.421735
611.591890	47.435349	72.426740
611.011968	37.931344	72.431745
609.606757	44.318896	72.436750
609.208342	44.282456	72.441754
608.535127	50.338997	72.446759
608.256294	39.552291	72.451764
607.271606	36.624010	72.456769
606.448658	52.653443	72.461774
606.379428	39.739158	72.466778
605.642234	44.836053	72.471783
604.585407	42.165264	72.476788
604.109202	37.927570	72.481793
603.238616	44.979058	72.486798
602.842357	43.564011	72.491802
602.046786	57.193686	72.496807
601.144381	46.167217	72.501812
600.628592	48.008705	72.506817
599.929327	52.695862	72.511822
599.974878	44.972006	72.516826
598.415666	60.530473	72.521831
597.801767	45.578739	72.526836
597.540794	51.143864	72.531841
596.981234	46.820092	72.536846
596.123356	45.839671	72.541850
595.053817	45.187845	72.546855
594.412434	45.254749	72.551860
594.010148	39.374709	72.556865
593.807522	52.596153	72.561870
593.366383	39.901938	72.566874
591.995439	43.593747	72.571879
591.843378	40.933444	72.576884
591.185103	39.971706	72.581889
589.663239	47.424947	72.586894
589.188703	33.299444	72.591898
588.857095	48.004841	72.596903
588.407210	51.064291	72.601908
587.928160	43.166923	72.606913
586.648929	43.064156	72.611918
586.325081	37.964840	72.616922
585.322373	35.930421	72.621927
585.099271	38.677790	72.626932
584.209091	35.941053	72.631937
583.556271	42.877446	72.636942
583.527119	34.939986	72.641946
582.293016	39.020019	72.646951
581.175643	39.128026	72.651956
580.784241	35.403540	72.656961
580.100021	42.229815	72.661966
580.154257	42.405156	72.666970
578.995624	41.854256	72.671975
578.224763	36.217414	72.676980
577.548348	39.912179	72.681985
576.956860	44.432366	72.686990
576.659333	38.521456	72.691994
575.501669	37.166154	72.696999
574.566996	41.214282	72.702004
574.331551	34.188039	72.707009
573.731393	35.755958	72.712014
572.774983	33.103889	72.717018
571.849388	40.774427	72.722023
571.464195	37.596159	72.727028
571.408192	31.312478	72.732033
570.490213	41.087045	72.737038
570.199204	37.094261	72.742042
569.000057	38.574634	72.747047
568.742944	35.893215	72.752052
567.838082	46.266519	72.757057
566.750996	38.454943	72.762062
566.296858	33.814774	72.767066
565.858166	46.045623	72.772071
565.078161	45.082776	72.777076
564.220025	39.215406	72.782081
563.376714	41.870726	72.787086
563.467379	37.022377	72.792090
562.607630	35.472984	72.797095
561.779818	38.822853	72.802100
561.169992	31.577107	72.807105
560.458737	42.339053	72.812110
560.239128	34.897126	72.817114
559.092696	45.228475	72.822119
558.018488	40.931474	72.827124
557.810648	42.922629	72.832129
557.376783	39.826231	72.837134
556.664226	33.383748	72.842138
555.566558	36.782898	72.847143
554.973016	37.121316	72.852148
554.813665	39.371255	72.857153
553.823847	37.975042	72.862158
552.915372	25.471966	72.867162
551.885190	42.508958	72.872167
551.297985	45.659666	72.877172
551.514386	41.713815	72.882177
550.871235	44.143300	72.887182
550.349135	39.100791	72.892186
549.473588	37.451416	72.897191
548.613099	41.490893	72.902196
548.248116	38.142253	72.907201
546.938913	51.793801	72.912206
546.622490	41.779497	72.917210
545.952610	32.706160	72.922215
545.399055	38.183832	72.927220
544.657439	37.457731	72.932225
543.609794	41.400856	72.937230
543.270799	41.440120	72.942234
542.529041	42.185345	72.947239
541.952770	41.836615	72.952244
541.170812	29.788059	72.957249
540.366697	42.025059	72.962254
540.294517	35.493219	72.967258
539.837082	34.122619	72.972263
538.717418	38.219141	72.977268
538.170181	32.308583	72.982273
537.320516	46.068298	72.987278
536.920446	42.037692	72.992282
535.514544	44.410450	72.997287
534.986761	39.395659	73.002292
534.726645	32.067423	73.007297
534.310578	44.233167	73.012302
533.480979	41.253411	73.017306
532.408924	44.523913	73.022311
531.869672	44.516221	73.027316
531.719909	38.472977	73.032321
530.604150	44.803435	73.037326
530.206181	35.141172	73.042330
529.275459	30.567447	73.047335
528.878768	42.510908	73.052340
528.328197	28.085302	73.057345
527.164332	37.973153	73.062350
526.094645	34.632664	73.067354
525.797735	36.005644	73.072359
525.341803	39.244260	73.077364
525.459619	40.912318	73.082369
524.409205	43.075504	73.087374
523.621014	43.097996	73.092378
522.771747	45.241766	73.097383
522.184343	45.161320	73.102388
521.460951	36.211630	73.107393
520.537218	46.531181	73.112398
519.931809	39.682136	73.117402
519.703227	40.979579	73.122407
518.884719	39.907760	73.127412
518.289315	35.871998	73.132417
517.129307	46.856808	73.137422
516.691395	32.742844	73.142426
516.427688	40.817346	73.147431
515.592457	46.532274	73.152436
514.975244	37.783297	73.157441
513.968793	44.058505	73.162446
513.645030	38.468754	73.167450
513.117049	39.454332	73.172455
512.264897	43.587111	73.177460
511.554211	46.431062	73.182465
510.985939	46.543114	73.187470
510.296651	37.411377	73.192474
509.430503	40.481937	73.197479
508.872574	39.180964	73.202484
508.490752	37.971793	73.207489
507.767936	49.314337	73.212494
506.974220	38.034065	73.217498
506.104591	34.644378	73.222503
505.497780	44.878765	73.227508
505.091174	41.601416	73.232513
504.249267	49.484155	73.237518
503.142996	39.296032	73.242522
502.815899	39.415409	73.247527
502.398937	45.029032	73.252532
502.112962	39.818043	73.257537
500.874913	43.539196	73.262542
500.233098	35.628355	73.267546
499.672925	47.690897	73.272551
499.245314	44.683401	73.277556
498.812773	42.334282	73.282561
497.036007	47.405957	73.287566
496.830098	36.079384	73.292570
496.598788	44.043071	73.297575
495.985024	41.344345	73.302580
494.722949	38.822990	73.307585
494.252245	42.303662	73.312590
493.985552	37.625771	73.317594
493.386352	43.219533	73.322599
492.437013	43.696634	73.327604
491.910178	31.921281	73.332609
491.014829	42.256816	73.337614
490.706454	40.679558	73.342618
489.822680	41.537303	73.347623
488.983785	46.853851	73.352628
488.313217	39.866959	73.357633
487.785853	51.208341	73.362638
487.197240	44.515902	73.367642
486.286356	49.332982	73.372647
485.508299	51.667274	73.377652
485.433581	39.116584	73.382657
484.869383	46.839978	73.387662
483.679016	39.849143	73.392666
483.162697	40.673597	73.397671
482.264041	43.719381	73.402676
482.143837	31.980193	73.407681
480.934076	37.691700	73.412686
480.313010	36.872301	73.417690
479.863715	39.565816	73.422695
479.146274	39.892446	73.427700
478.982186	47.591538	73.432705
478.106177	54.134571	73.437710
477.526698	39.857079	73.442714
476.884726	33.587887	73.447719
475.688417	43.752165	73.452724
475.180495	42.424311	73.457729
474.128529	48.134347	73.462734
474.041625	31.149620	73.467738
473.797696	42.191962	73.472743
472.549680	42.822298	73.477748
471.925821	37.624130	73.482753
470.870626	50.740082	73.487758
470.932371	44.421881	73.492762
469.757714	41.670572	73.497767
469.144293	46.060232	73.502772
468.878013	41.450086	73.507777
468.022787	44.460572	73.512782
467.627267	40.650030	73.517786
466.791142	47.543102	73.522791
465.739381	47.467244	73.527796
465.436042	42.678497	73.532801
464.692591	52.190334	73.537806
463.648963	52.814928	73.542810
463.290069	42.438400	73.547815
462.753411	40.763464	73.552820
462.613252	40.092976	73.557825
461.391572	52.976829	73.562830
460.646811	34.171416	73.567834
459.915885	48.888373	73.572839
459.370793	49.487179	73.577844
458.541011	41.893295	73.582849
457.702966	49.303919	73.587854
457.413671	41.215515	73.592858
457.040212	48.597871	73.597863
456.349954	53.726752	73.602868
455.418546	47.230848	73.607873
454.744626	53.617118	73.612878
454.373694	36.133578	73.617882
453.757461	43.649219	73.622887
452.310730	46.637232	73.627892
452.122131	35.186485	73.632897
451.640444	48.095973	73.637902
451.079783	47.571312	73.642906
449.785408	42.612415	73.647911
448.926791	42.272410	73.652916
448.784402	40.670295	73.657921
448.129054	48.679450	73.662926
447.700359	43.841287	73.667930
446.686993	38.426047	73.672935
445.840843	41.510788	73.677940
445.631062	34.931489	73.682945
445.200686	41.936554	73.687950
444.413514	42.955547	73.692954
443.643859	43.437161	73.697959
442.782427	44.944225	73.702964
442.618028	36.463770	73.707969
441.456200	44.969916	73.712974
440.404741	43.488950	73.717978
440.136946	49.305904	73.722983
439.689063	47.578985	73.727988
439.465833	43.441381	73.732993
438.031680	51.737021	73.737998
437.700441	49.080039	73.743002
437.022932	39.369285	73.748007
436.404680	43.870106	73.753012
435.470293	31.569909	73.758017
434.398625	44.065591	73.763022
434.208237	32.269782	73.768026
433.939273	34.921962	73.773031
433.191449	50.695024	73.778036
432.491922	43.432064	73.783041
431.623267	49.798893	73.788046
431.318224	43.371962	73.793050
430.116641	36.744068	73.798055
429.019110	43.306626	73.803060
428.625131	45.376325	73.808065
428.221682	43.845758	73.813070
428.159020	39.693619	73.818074
427.746141	39.456084	73.823079
426.343287	45.076950	73.828084
426.006545	42.753586	73.833089
425.030364	44.990143	73.838094
423.989182	39.267106	73.843098
423.694670	37.954155	73.848103
422.833099	42.954210	73.853108
422.653526	40.790315	73.858113
421.696987	43.627719	73.863118
420.793723	48.071443	73.868122
420.250406	34.453696	73.873127
419.795789	46.742282	73.878132
419.547315	41.910111	73.883137
418.293693	47.444131	73.888142
417.673038	30.954450	73.893146
417.341502	42.436524	73.898151
416.572450	47.183724	73.903156
415.974750	38.012201	73.908161
414.838698	52.979784	73.913166
414.755580	41.460198	73.918170
414.434952	41.375127	73.923175
412.847209	48.842109	73.928180
412.080188	53.026013	73.933185
411.652836	51.273751	73.938190
411.303932	47.007936	73.943194
410.922549	41.208185	73.948199
409.703514	44.584151	73.953204
409.227355	35.722854	73.958209
408.759935	40.852513	73.963214
407.893585	44.569690	73.968218
406.847706	44.303685	73.973223
406.169150	50.644970	73.978228
406.058075	40.030283	73.983233
405.475967	39.482241	73.988238
404.824110	35.084918	73.993242
403.813480	38.380377	73.998247
403.141192	43.910105	74.003252
402.993011	41.252354	74.008257
401.694543	43.179137	74.013262
400.967831	40.219308	74.018266
400.551733	38.793264	74.023271
399.871586	38.927895	74.028276
399.560197	35.417780	74.033281
398.106509	46.091445	74.038286
397.578337	43.699233	74.043290
397.101403	37.932054	74.048295
396.337148	44.862580	74.053300
396.472041	36.572574	74.058305
395.755007	38.793089	74.063310
394.832283	39.562454	74.068314
394.198370	35.278971	74.073319
393.168141	36.210543	74.078324
392.514035	34.071786	74.083329
391.609061	46.961975	74.088334
391.380315	36.448041	74.093338
391.111862	33.500369	74.098343
390.391814	43.423226	74.103348
389.623089	29.958098	74.108353
388.840828	32.058117	74.113358
388.016931	38.466709	74.118362
387.146661	32.852083	74.123367
386.410514	33.165950	74.128372
385.935480	40.666991	74.133377
385.620087	37.081822	74.138382
385.196017	36.667880	74.143386
384.524409	33.879053	74.148391
383.423801	40.080993	74.153396
383.110714	34.868038	74.158401
381.634384	40.511668	74.163406
380.889089	38.024740	74.168410
380.546891	41.659999	74.173415
379.989199	42.022709	74.178420
380.017407	31.392151	74.183425
378.986352	33.735236	74.188430
377.933369	26.621654	74.193434
377.595499	34.848318	74.198439
376.743202	41.078511	74.203444
376.491095	39.394533	74.208449
375.146639	43.320353	74.213454
374.789633	38.478671	74.218458
374.377814	33.163175	74.223463
373.670586	36.785625	74.228468
372.729695	30.037386	74.233473
371.821880	26.392061	74.238478
371.500503	22.024104	74.243482
371.038074	30.918739	74.248487
370.462521	35.512117	74.253492
369.631581	33.578157	74.258497
368.834002	35.549736	74.263502
368.347833	38.357952	74.268506
367.830804	34.721332	74.273511
366.705681	36.817634	74.278516
366.302886	27.146727	74.283521
365.501382	39.424342	74.288526
365.427461	31.339496	74.293530
364.472014	30.647516	74.298535
363.292505	36.002591	74.303540
363.272118	33.417526	74.308545
362.086193	28.712643	74.313550
360.891849	31.211060	74.318554
360.381260	33.942743	74.323559
360.060416	34.376532	74.328564
359.955403	30.100260	74.333569
359.568849	33.589621	74.338574
358.667684	31.753587	74.343578
357.678615	31.347664	74.348583
356.862006	43.697077	74.353588
356.432861	35.640439	74.358593
355.613509	33.600559	74.363598
354.841725	29.395826	74.368602
354.588407	28.369635	74.373607
354.046387	33.601070	74.378612
353.204782	34.986732	74.383617
352.219605	42.353012	74.388622
351.785240	34.803410	74.393626
351.566188	33.830107	74.398631
350.262390	34.048343	74.403636
349.481512	31.297437	74.408641
348.930228	32.657345	74.413646
348.511964	39.081746	74.418650
347.898009	25.913681	74.423655
346.748332	41.336030	74.428660
346.297601	27.063321	74.433665
345.735853	33.781816	74.438670
345.243818	30.136489	74.443674
344.726682	31.741694	74.448679
343.432135	32.887286	74.453684
342.823584	25.176210	74.458689
342.417641	27.186322	74.463694
341.951680	31.680241	74.468698
341.440804	31.860458	74.473703
340.546653	39.371509	74.478708
340.086816	30.266361	74.483713
339.321441	33.185299	74.488718
338.163417	36.620960	74.493722
337.861804	32.733982	74.498727
336.880421	38.847557	74.503732
336.751690	30.329900	74.508737
335.798502	36.413751	74.513742
334.512744	31.792597	74.518746
334.524314	34.605092	74.523751
333.777983	44.590495	74.528756
333.812489	43.576794	74.533761
332.879972	41.875074	74.538766
332.106577	47.108689	74.543770
331.654917	41.739623	74.548775
330.760202	45.869775	74.553780
329.920591	28.987666	74.558785
328.951220	40.487787	74.563790
328.550500	42.686307	74.568794
328.305761	39.865751	74.573799
326.838080	38.241418	74.578804
326.544389	37.850868	74.583809
325.592545	46.334640	74.588814
325.222501	38.558751	74.593818
325.489514	40.264525	74.598823
324.125763	41.399077	74.603828
323.468799	35.427213	74.608833
322.673605	37.281731	74.613838
321.721712	41.548728	74.618842
320.807893	37.615795	74.623847
320.233381	40.945875	74.628852
319.937466	34.670481	74.633857
319.244571	35.549910	74.638862
319.275731	35.889771	74.643866
318.359191	29.301681	74.648871
317.333238	47.493964	74.653876
316.992484	35.572324	74.658881
316.252238	32.769223	74.663886
315.267503	37.389961	74.668890
314.582364	33.974106	74.673895
313.892908	42.671537	74.678900
313.683785	36.019614	74.683905
312.749960	42.072004	74.688910
311.891988	50.703251	74.693914
311.494068	38.219860	74.698919
310.922353	43.555385	74.703924
310.519469	36.123780	74.708929
309.170425	40.554988	74.713934
308.365873	37.541361	74.718938
308.204559	36.383821	74.723943
307.694439	39.935456	74.728948
307.247613	42.205980	74.733953
305.909118	42.450268	74.738958
305.672300	40.058962	74.743962
305.231663	31.723473	74.748967
303.629115	39.408912	74.753972
303.279498	32.309445	74.758977
302.628806	35.538126	74.763982
302.438009	47.524483	74.768986
301.841361	38.132057	74.773991
300.605840	42.592490	74.778996
300.189094	37.041251	74.784001
299.841418	31.343390	74.789006
298.913175	32.170439	74.794010
298.301140	31.893697	74.799015
297.149725	45.624268	74.804020
297.181789	30.982905	74.809025
296.358570	36.571395	74.814030
295.620605	37.901137	74.819034
295.350774	29.904288	74.824039
294.226548	43.286750	74.829044
293.886090	22.966212	74.834049
292.779890	36.878806	74.839054
292.188862	33.875316	74.844058
291.881888	22.188008	74.849063
290.660158	33.094411	74.854068
289.929200	23.234545	74.859073
289.062504	29.222623	74.864078
288.913049	28.061618	74.869082
288.470888	36.957765	74.874087
287.813950	33.679350	74.879092
287.285075	35.466210	74.884097
286.314277	34.740436	74.889102
286.042630	26.431643	74.894106
285.264027	29.442589	74.899111
283.854424	33.260560	74.904116
283.614086	36.878019	74.909121
283.226613	31.568126	74.914126
282.400950	34.804192	74.919130
281.674107	39.180421	74.924135
280.711328	44.295993	74.929140
280.424731	48.762920	74.934145
279.960503	43.526756	74.939150
279.548418	56.358937	74.944154
278.522917	44.005519	74.949159
277.778795	44.297033	74.954164
277.289045	43.122445	74.959169
276.042737	46.949096	74.964174
275.508776	36.726674	74.969178
275.346816	42.786964	74.974183
274.603249	44.119183	74.979188
274.100200	42.710171	74.984193
272.647129	41.463588	74.989198
271.979277	39.998838	74.994202
271.862950	39.985309	74.999207
271.179187	40.377594	75.004212
270.915986	35.391675	75.009217
269.868065	50.923997	75.014222
268.927314	44.426512	75.019226
268.757694	49.738972	75.024231
267.924556	47.740742	75.029236
267.094981	41.586666	75.034241
266.190306	44.132007	75.039246
266.027371	48.594999	75.044250
265.709438	44.330585	75.049255
264.669524	47.790036	75.054260
263.792806	42.621186	75.059265
263.231533	41.705581	75.064270
262.502981	41.404838	75.069274
261.947319	36.323600	75.074279
260.927202	46.305339	75.079284
260.860894	44.700575	75.084289
260.428295	50.988501	75.089294
259.029913	43.136804	75.094298
258.151031	46.863909	75.099303
257.666486	50.272707	75.104308
257.577620	47.613401	75.109313
257.040451	47.923981	75.114318
256.014767	45.994286	75.119322
255.788103	48.128809	75.124327
254.463187	47.103088	75.129332
253.593256	50.912348	75.134337
252.836598	36.404563	75.139342
252.298191	46.654891	75.144346
252.009121	34.557875	75.149351
251.741713	45.892538	75.154356
251.152420	39.909913	75.159361
249.922666	52.393002	75.164366
249.247673	49.552712	75.169370
249.151012	38.314434	75.174375
248.269714	50.743568	75.179380
247.384195	47.941561	75.184385
246.957632	45.146837	75.189390
245.441901	47.795875	75.194394
244.958254	35.077010	75.199399
244.240176	49.959105	75.204404
243.638150	40.447706	75.209409
243.439678	42.546197	75.214414
243.155561	37.189877	75.219418
242.970868	35.719099	75.224423
241.632333	48.099675	75.229428
240.953285	41.576267	75.234433
239.931306	39.778454	75.239438
238.491257	51.492391	75.244442
238.239857	43.555687	75.249447
237.421382	46.197688	75.254452
237.457109	43.296176	75.259457
237.025646	34.993934	75.264462
236.634562	45.862605	75.269466
236.088050	33.257842	75.274471
235.123759	40.527788	75.279476
234.621142	48.572564	75.284481
233.170870	46.193304	75.289486
232.455362	43.058279	75.294490
232.406035	43.557623	75.299495
231.633644	48.740642	75.304500
230.913104	43.354526	75.309505
230.328216	45.047822	75.314510
229.644230	47.944360	75.319514
229.224835	48.589415	75.324519
228.006217	48.822524	75.329524
227.533155	50.442806	75.334529
226.965860	47.134350	75.339534
226.574463	46.160141	75.344538
225.478995	35.975185	75.349543
224.452589	52.185334	75.354548
223.951046	45.680949	75.359553
223.463418	42.818693	75.364558
223.052503	44.239836	75.369562
222.623814	25.622301	75.374567
221.664544	42.115053	75.379572
221.271072	48.633290	75.384577
220.368291	43.205260	75.389582
219.109237	47.967526	75.394586
218.794068	44.005454	75.399591
217.984721	50.296659	75.404596
217.776595	43.594125	75.409601
217.478030	44.142654	75.414606
216.165589	40.845728	75.419610
215.675009	41.879022	75.424615
215.073696	53.107634	75.429620
214.985081	39.603570	75.434625
213.859259	42.181021	75.439630
212.893756	38.546528	75.444634
212.061686	39.151701	75.449639
211.373324	44.490065	75.454644
210.879355	33.382929	75.459649
210.026337	33.611394	75.464654
209.403349	40.022705	75.469658
209.285259	34.106921	75.474663
208.799663	34.423484	75.479668
208.224708	34.804752	75.484673
207.266932	39.914819	75.489678
206.173817	36.906219	75.494682
206.185934	42.574488	75.499687
205.043478	38.949278	75.504692
204.375291	40.961785	75.509697
204.296788	34.394717	75.514702
203.047416	41.394719	75.519706
202.417669	38.939896	75.524711
201.711559	42.819254	75.529716
201.385346	46.999187	75.534721
200.440484	39.412715	75.539726
199.466244	39.272574	75.544730
199.157338	40.101874	75.549735
198.552990	41.206920	75.554740
197.843419	43.563493	75.559745
196.862809	43.835954	75.564750
196.248340	40.519257	75.569754
196.018530	31.500489	75.574759
195.164316	46.658175	75.579764
194.775911	37.579525	75.584769
193.980867	40.949511	75.589774
192.794627	43.266942	75.594778
192.853741	40.129892	75.599783
192.161333	40.006335	75.604788
191.206840	37.839819	75.609793
190.288229	46.811919	75.614798
189.897285	44.691198	75.619802
189.519831	36.344089	75.624807
188.755373	45.936593	75.629812
187.781558	40.335397	75.634817
187.053684	48.882859	75.639822
186.542544	47.243344	75.644826
186.404115	36.339742	75.649831
185.210780	48.269843	75.654836
184.644850	41.922390	75.659841
183.924984	37.125967	75.664846
183.129363	47.644382	75.669850
182.369705	38.896145	75.674855
181.170001	45.702162	75.679860
180.030270	38.883198	75.684865
179.655100	33.295398	75.689870
179.311563	42.797157	75.694874
179.738277	30.686998	75.699879
178.692414	39.203140	75.704884
177.983915	30.823647	75.709889
177.517274	33.478971	75.714894
176.749191	48.047345	75.719898
175.826022	28.237616	75.724903
175.002659	37.614002	75.729908
174.646975	34.030560	75.734913
174.399736	36.649336	75.739918
173.811076	41.333149	75.744922
173.193921	36.064619	75.749927
172.213366	43.934844	75.754932
171.294817	33.234441	75.759937
170.561429	36.060018	75.764942
169.495073	39.284021	75.769946
169.424138	30.547441	75.774951
168.832202	35.285392	75.779956
168.729042	40.778067	75.784961
167.303370	39.869379	75.789966
166.751842	47.642837	75.794970
166.290570	31.101052	75.799975
165.687803	44.857751	75.804980
164.982725	40.662950	75.809985
164.058152	32.988108	75.814990
163.174556	48.484799	75.819994
162.964007	32.606370	75.824999
161.607570	44.256546	75.830004
161.024729	47.621102	75.835009
160.718504	43.282300	75.840014
160.338045	43.935352	75.845018
159.937441	35.577749	75.850023
159.100537	45.847281	75.855028
158.343187	33.187844	75.860033
157.496676	29.613258	75.865038
157.044978	33.206066	75.870042
156.138463	37.784429	75.875047
155.162461	37.704511	75.880052
155.155728	37.947908	75.885057
154.840974	42.846684	75.890062
153.482198	45.808225	75.895066
152.977061	42.675962	75.900071
152.310032	41.465004	75.905076
151.546936	30.156361	75.910081
150.474485	35.428227	75.915086
149.520613	45.117164	75.920090
149.292257	34.016592	75.925095
148.876798	40.804842	75.930100
148.587850	33.801393	75.935105
148.390781	33.360770	75.940110
147.028020	37.516701	75.945114
146.447038	36.921233	75.950119
145.811285	45.195397	75.955124
144.659977	42.777997	75.960129
144.010190	42.682353	75.965134
143.220189	38.855911	75.970138
143.086899	35.675416	75.975143
142.371442	43.678434	75.980148
142.242438	50.064633	75.985153
141.468057	36.176315	75.990158
140.180633	52.287743	75.995162
139.863869	34.341516	76.000167
138.648113	45.649155	76.005172
138.072311	40.965400	76.010177
137.453382	42.337713	76.015182
136.660595	53.907518	76.020186
136.955070	46.172396	76.025191
136.242282	46.473151	76.030196
135.156575	47.306439	76.035201
134.845822	43.741070	76.040206
134.035540	57.138202	76.045210
133.002960	47.908360	76.050215
131.913996	46.304198	76.055220
131.543724	46.466775	76.060225
131.526311	35.718933	76.065230
130.386991	46.199106	76.070234
129.845747	43.555153	76.075239
129.129852	46.150872	76.080244
128.445668	45.169736	76.085249
128.262084	36.692389	76.090254
126.982244	48.910691	76.095258
126.727624	36.902830	76.100263
126.045073	44.583638	76.105268
125.266355	34.936448	76.110273
124.163737	39.292194	76.115278
123.319372	46.374326	76.120282
123.336785	40.913187	76.125287
122.671907	39.132615	76.130292
121.926784	40.370507	76.135297
121.284126	34.576203	76.140302
120.429693	45.823094	76.145306
119.971855	41.612548	76.150311
119.308355	45.179205	76.155316
118.472309	50.817102	76.160321
117.689247	41.643689	76.165326
117.152146	52.560878	76.170330
116.912597	43.682443	76.175335
115.690690	39.916979	76.180340
114.859336	47.124772	76.185345
114.517475	38.890278	76.190350
114.153666	47.855956	76.195354
113.847052	38.090929	76.200359
112.529774	44.250242	76.205364
111.925407	44.729262	76.210369
111.657042	44.944981	76.215374
110.267866	51.391728	76.220378
110.145630	45.096565	76.225383
109.194859	52.980989	76.230388
108.742125	44.797284	76.235393
108.382696	47.150101	76.240398
107.268474	55.708712	76.245402
106.528477	44.366433	76.250407
105.663533	50.683876	76.255412
105.272159	40.935516	76.260417
105.143950	48.636766	76.265422
103.785841	47.632188	76.270426
103.347253	46.446326	76.275431
102.640249	45.659648	76.280436
102.364645	38.348150	76.285441
101.495615	47.190945	76.290446
100.248475	44.820384	76.295450
100.335600	33.757837	76.300455
99.587103	43.995941	76.305460
98.867944	48.071371	76.310465
98.203511	43.327639	76.315470
97.208815	47.502190	76.320474
97.007580	36.195454	76.325479
95.561323	51.557936	76.330484
94.820156	44.555625	76.335489
94.599323	41.956793	76.340494
94.183994	43.856475	76.345498
93.911263	38.391133	76.350503
93.330450	42.821398	76.355508
92.176366	40.341389	76.360513
91.783150	40.852982	76.365518
90.690266	44.453407	76.370522
90.024894	36.253150	76.375527
89.135554	35.238502	76.380532
88.790105	47.356735	76.385537
88.594894	40.526008	76.390542
87.729751	48.551326	76.395546
86.764973	43.319318	76.400551
85.894535	44.566161	76.405556
85.298074	29.539335	76.410561
85.358967	40.922575	76.415566
84.139265	35.480477	76.420570
83.652776	29.178742	76.425575
82.919548	34.940599	76.430580
82.345016	39.803526	76.435585
81.269442	33.341819	76.440590
80.129209	38.430554	76.445594
80.461274	32.823060	76.450599
79.765581	34.833675	76.455604
79.195609	40.214692	76.460609
78.662615	34.022872	76.465614
77.406965	33.749451	76.470618
77.361213	31.381329	76.475623
76.495475	40.415989	76.480628
75.721782	38.403621	76.485633
74.851296	33.658059	76.490638
74.389331	38.400537	76.495642
74.212928	35.206422	76.500647
72.804855	36.291405	76.505652
72.142529	34.721752	76.510657
71.836191	30.857650	76.515662
70.854344	39.311581	76.520666
70.200403	36.165218	76.525671
69.388337	35.554572	76.530676
68.773820	35.650443	76.535681
68.757643	26.749029	76.540686
68.233202	34.820950	76.545690
67.070990	30.164482	76.550695
66.141404	39.737603	76.555700
65.888706	38.572573	76.560705
65.517559	36.626915	76.565710
64.162633	41.275225	76.570714
63.484964	30.916517	76.575719
63.191761	28.168380	76.580724
62.697990	35.481629	76.585729
61.831278	35.021625	76.590734
61.072237	40.565254	76.595738
60.300652	34.258516	76.600743
59.888505	38.900014	76.605748
58.828408	40.121912	76.610753
58.181276	41.560241	76.615758
57.293581	42.071832	76.620762
57.198459	44.147547	76.625767
57.330382	41.711671	76.630772
56.027217	44.596586	76.635777
55.550452	40.997777	76.640782
54.494243	51.193493	76.645786
53.655679	43.962299	76.650791
52.866280	41.255429	76.655796
52.046646	39.923752	76.660801
52.348802	37.556929	76.665806
51.390242	47.973617	76.670810
50.636855	38.866466	76.675815
49.915784	43.759072	76.680820
49.237386	40.786924	76.685825
48.967204	35.300683	76.690830
47.584297	46.794280	76.695834
46.938576	35.064841	76.700839
46.355382	38.467321	76.705844
45.862327	43.552230	76.710849
45.792264	44.704587	76.715854
44.566836	44.774869	76.720858
44.075052	36.835533	76.725863
43.556971	47.757577	76.730868
42.474494	50.987358	76.735873
41.649236	38.521722	76.740878
40.964262	49.277991	76.745882
40.986652	33.791382	76.750887
40.498023	43.309972	76.755892
39.280340	42.827089	76.760897
38.600208	37.623835	76.765902
37.830673	44.451206	76.770906
37.559467	33.144604	76.775911
36.432486	39.691500	76.780916
35.651275	37.071641	76.785921
35.522692	38.026748	76.790926
34.719569	46.398580	76.795930
34.185789	45.365105	76.800935
33.189511	44.001676	76.805940
32.247852	36.419504	76.810945
32.024981	33.358959	76.815950
31.809218	42.980697	76.820954
30.916033	47.132777	76.825959
30.273608	46.577096	76.830964
29.513474	47.871026	76.835969
28.575038	39.148204	76.840974
27.747457	46.375918	76.845978
27.077401	35.869350	76.850983
26.804577	46.794866	76.855988
26.156765	42.086354	76.860993
25.740723	34.272142	76.865998
24.704629	41.493679	76.871002
24.200428	37.665863	76.876007
23.583759	37.628048	76.881012
22.894933	38.312944	76.886017
22.293081	35.580911	76.891022
21.272606	45.094424	76.896026
20.788031	33.766655	76.901031
20.534369	44.063064	76.906036
19.501262	45.583449	76.911041
18.691326	47.142366	76.916046
18.117380	42.884125	76.921050
17.816943	46.307757	76.926055
17.034465	39.599071	76.931060
16.078124	49.498176	76.936065
15.937241	41.964938	76.941070
14.551957	43.992491	76.946074
13.713746	37.836742	76.951079
13.537692	41.636354	76.956084
12.558217	49.599499	76.961089
12.427170	40.743208	76.966094
12.119530	46.460876	76.971098
11.187742	35.251729	76.976103
10.469440	35.031428	76.981108
9.459059	40.490570	76.986113
8.782233	39.144020	76.991118
7.264122	47.552602	76.996122
7.385516	35.077958	77.001127
7.017236	45.072524	77.006132
6.255029	46.000937	77.011137
6.235880	41.616385	77.016142
4.637322	49.785485	77.021147
4.330521	41.916007	77.026151
3.857810	46.024701	77.031156
3.232054	40.148889	77.036161