Fri Mar 05 19:16:07 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.010424	94.916051	0.000000
-0.400651	89.835767	0.005005
-1.226379	70.031540	0.010010
-2.844654	21.549186	0.015014
-6.129638	-2.489446	0.020019
-11.180748	0.754118	0.025024
-16.148309	-1.460828	0.030029
-21.072834	7.844846	0.035034
-25.373621	-0.416795	0.040038
-29.030011	-4.619655	0.045043
-32.436703	8.772642	0.050048
-36.352866	-1.004276	0.055053
-40.076224	4.249466	0.060058
-43.589054	1.351514	0.065062
-47.431788	2.861718	0.070067
-50.910105	8.369699	0.075072
-55.225938	2.170005	0.080077
-58.718600	6.297304	0.085082
-62.359069	11.402240	0.090086
-66.216264	4.823472	0.095091
-69.867376	2.942671	0.100096
-73.711988	-3.884091	0.105101
-77.623517	5.802555	0.110106
-81.371952	-2.208056	0.115110
-84.838155	-2.628120	0.120115
-88.800762	2.370551	0.125120
-92.720800	-2.728432	0.130125
-96.638489	7.273038	0.135130
-100.298058	-1.483422	0.140134
-103.868439	2.651608	0.145139
-107.491055	2.283339	0.150144
-110.955776	-6.748614	0.155149
-115.229681	-6.998767	0.160154
-118.885246	1.128503	0.165158
-122.673767	-1.066182	0.170163
-126.722255	3.922597	0.175168
-130.134542	-0.017858	0.180173
-133.778465	-3.984427	0.185178
-137.541308	-7.484162	0.190182
-141.318611	-4.929277	0.195187
-145.525781	-3.805468	0.200192
-149.185645	-11.312857	0.205197
-153.245163	1.751670	0.210202
-157.166738	6.778595	0.215206
-160.899757	-5.189318	0.220211
-164.259474	3.693474	0.225216
-167.634306	-2.578895	0.230221
-171.614389	0.596595	0.235226
-175.399099	-1.406227	0.240230
-178.970988	0.666509	0.245235
-182.955997	1.966242	0.250240
-186.641749	-9.092964	0.255245
-190.562157	-1.882111	0.260250
-194.263712	-5.916658	0.265254
-197.856793	3.173727	0.270259
-201.979468	-1.575769	0.275264
-205.411458	-8.450811	0.280269
-208.949409	0.063091	0.285274
-212.982478	-4.492529	0.290278
-216.782881	6.751958	0.295283
-220.907143	0.372189	0.300288
-224.294303	-8.433849	0.305293
-228.199540	0.862512	0.310298
-231.853027	-0.547732	0.315302
-235.544236	-2.511765	0.320307
-239.558116	-1.680414	0.325312
-242.746359	-5.866195	0.330317
-246.999947	0.281448	0.335322
-250.969597	1.091565	0.340326
-254.446864	-1.728171	0.345331
-258.137300	-2.681472	0.350336
-261.679846	-9.698055	0.355341
-265.338892	-3.750931	0.360346
-269.527557	-5.031543	0.365350
-273.190194	0.531393	0.370355
-277.406810	5.055247	0.375360
-280.851976	2.642007	0.380365
-284.595151	5.183781	0.385370
-288.267787	3.144326	0.390374
-292.118451	2.741774	0.395379
-295.871736	-7.219960	0.400384
-299.525186	-10.784205	0.405389
-303.421249	0.265940	0.410394
-307.199275	2.439577	0.415398
-310.583085	0.514900	0.420403
-314.493190	1.342424	0.425408
-318.119845	-2.672346	0.430413
-322.078565	5.719651	0.435418
-326.051126	-0.416067	0.440422
-329.647535	1.891037	0.445427
-333.530367	-0.846493	0.450432
-336.823362	-6.496168	0.455437
-340.875708	-3.010828	0.460442
-344.938142	-11.112797	0.465446
-348.301600	-12.890857	0.470451
-352.360481	-10.039962	0.475456
-355.885940	-7.144911	0.480461
-359.813128	-4.231449	0.485466
-363.885584	2.504059	0.490470
-367.445960	0.967194	0.495475
-371.112971	-6.109773	0.500480
-374.703478	-12.118743	0.505485
-378.396144	-3.382791	0.510490
-382.186722	-8.459375	0.515494
-386.023359	1.080161	0.520499
-390.334164	0.057380	0.525504
-393.437573	-5.430098	0.530509
-397.307541	1.005055	0.535514
-401.387000	-6.947442	0.540518
-404.871076	-11.902617	0.545523
-408.861088	-5.033548	0.550528
-412.411678	-9.722628	0.555533
-416.411223	0.872706	0.560538
-420.029970	-1.047417	0.565542
-423.655865	-12.883753	0.570547
-427.558767	0.540961	0.575552
-431.118627	-5.319854	0.580557
-434.950404	-9.594996	0.585562
-438.599083	-13.328516	0.590566
-442.266031	-11.352179	0.595571
-446.069247	-4.328377	0.600576
-449.920539	-5.414965	0.605581
-454.164456	-3.835325	0.610586
-457.840204	-6.304522	0.615590
-461.410785	-9.426013	0.620595
-464.939303	-1.168729	0.625600
-468.323594	-14.669395	0.630605
-472.652852	-5.771724	0.635610
-476.643843	-1.684105	0.640614
-480.252900	-5.944280	0.645619
-484.131159	-2.745122	0.650624
-487.636399	-6.717515	0.655629
-491.711426	-3.624114	0.660634
-495.267893	-5.848954	0.665638
-498.718525	-14.707514	0.670643
-503.043139	-11.331386	0.675648
-506.379546	-9.895015	0.680653
-510.441682	-8.254424	0.685658
-514.373566	-13.361837	0.690662
-517.703975	-9.521582	0.695667
-521.391711	-9.558705	0.700672
-524.736438	-2.180662	0.705677
-528.775003	-5.911695	0.710682
-532.870322	-3.302257	0.715686
-536.982183	-4.913205	0.720691
-540.584420	-3.483212	0.725696
-543.908152	-8.752368	0.730701
-548.013199	-1.740123	0.735706
-551.335054	-9.568934	0.740710
-555.163472	-3.791451	0.745715
-559.184796	-0.294934	0.750720
-563.273625	-9.764231	0.755725
-566.624465	-7.470772	0.760730
-570.399753	-10.297625	0.765734
-574.271345	-7.025274	0.770739
-578.129247	1.462978	0.775744
-581.867624	-15.040202	0.780749
-585.422841	-8.085768	0.785754
-589.436327	-6.463853	0.790758
-593.090414	-8.999375	0.795763
-597.007840	-5.243430	0.800768
-600.276964	-8.826022	0.805773
-604.133989	-7.872467	0.810778
-607.798504	-8.715825	0.815782
-611.671774	-8.590707	0.820787
-615.825826	3.464633	0.825792
-619.275182	-4.965024	0.830797
-623.109806	-3.961401	0.835802
-626.985760	-5.218800	0.840806
-630.091668	-5.804443	0.845811
-634.526707	-7.740475	0.850816
-638.151518	-9.766523	0.855821
-641.972589	-3.912809	0.860826
-645.875174	-6.924204	0.865830
-649.500421	-10.266904	0.870835
-653.199075	-10.224809	0.875840
-656.623172	-18.612703	0.880845
-660.631225	-13.318862	0.885850
-664.248090	-11.559922	0.890854
-668.164754	-9.407726	0.895859
-671.983870	-3.957973	0.900864
-675.502499	-16.828150	0.905869
-679.433161	-5.223141	0.910874
-683.626295	-9.211477	0.915878
-687.284854	-7.109953	0.920883
-691.016018	-4.031739	0.925888
-694.552550	-9.850137	0.930893
-698.403748	-3.690327	0.935898
-702.022630	-5.874917	0.940902
-705.273674	-16.917561	0.945907
-709.598791	-4.891511	0.950912
-713.654105	-7.704923	0.955917
-717.221936	-1.964098	0.960922
-720.954226	-5.691699	0.965926
-724.784902	-6.140899	0.970931
-728.714134	-3.037282	0.975936
-731.760702	-17.499813	0.980941
-735.749037	-4.242338	0.985946
-739.940370	2.828169	0.990950
-743.500156	-4.982836	0.995955
-747.258906	4.319297	1.000960
-750.992188	-7.634955	1.005965
-754.751062	-1.494542	1.010970
-758.459533	-1.666754	1.015974
-762.242124	-10.763586	1.020979
-766.017194	3.243592	1.025984
-769.474789	-5.059936	1.030989
-773.760472	4.394260	1.035994
-777.557911	6.210617	1.040998
-781.139101	-14.190282	1.046003
-784.951988	5.230266	1.051008
-788.372013	10.644804	1.056013
-792.226637	-4.443853	1.061018
-796.084634	-0.763316	1.066022
-799.789159	-10.027102	1.071027
-804.067063	-1.039295	1.076032
-807.561633	-8.162039	1.081037
-811.126312	-5.744176	1.086042
-814.870626	-3.095747	1.091046
-818.424642	-4.273404	1.096051
-822.428191	0.520100	1.101056
-826.142608	-8.546522	1.106061
-830.031852	-9.913423	1.111066
-833.866670	-6.559803	1.116070
-837.343288	-12.704516	1.121075
-841.209556	-4.260257	1.126080
-844.937977	-4.768184	1.131085
-848.931165	-2.179265	1.136090
-852.880337	-10.956005	1.141094
-856.377680	-3.302393	1.146099
-860.190657	6.122118	1.151104
-863.743257	-10.017613	1.156109
-867.286085	0.841302	1.161114
-871.264312	6.308919	1.166118
-875.001984	3.979587	1.171123
-878.934724	-3.986042	1.176128
-882.377138	-12.340702	1.181133
-886.665404	-0.671894	1.186138
-890.405406	-3.694677	1.191142
-893.636815	-3.020440	1.196147
-897.935621	0.686579	1.201152
-901.537961	2.697443	1.206157
-905.292583	0.432370	1.211162
-909.079097	0.113604	1.216166
-912.703593	-7.923322	1.221171
-916.645365	-1.685612	1.226176
-920.097631	-0.936605	1.231181
-923.949974	-9.843816	1.236186
-927.690225	2.618947	1.241190
-931.398154	-12.910790	1.246195
-935.455244	3.609619	1.251200
-939.288761	4.831192	1.256205
-943.020388	0.003147	1.261210
-946.532047	11.002273	1.266214
-950.181471	-12.763629	1.271219
-954.123611	8.008754	1.276224
-957.773000	-11.810085	1.281229
-961.463164	-0.298287	1.286234
-965.251558	-2.613054	1.291238
-968.999237	-10.135033	1.296243
-973.061236	-2.748928	1.301248
-976.502085	-14.558739	1.306253
-980.180348	-14.145660	1.311258
-984.185165	-4.734445	1.316262
-987.652609	-6.397188	1.321267
-991.785472	2.766443	1.326272
-995.504237	-10.675174	1.331277
-999.570318	7.833705	1.336282
-1003.396870	-3.499659	1.341286
-1006.703440	-2.138323	1.346291
-1010.749033	-8.016739	1.351296
-1014.232515	-12.439653	1.356301
-1017.788249	-1.471236	1.361306
-1022.202415	-0.251283	1.366310
-1025.911230	-12.746702	1.371315
-1029.627770	1.306689	1.376320
-1033.019545	-4.248907	1.381325
-1036.447401	-2.719900	1.386330
-1040.415000	-0.552639	1.391334
-1044.359180	-11.662111	1.396339
-1048.403779	-1.342426	1.401344
-1052.242751	-0.211259	1.406349
-1055.813789	-6.056688	1.411354
-1059.306822	-5.163763	1.416358
-1062.964143	-10.869224	1.421363
-1066.898273	-10.463968	1.426368
-1070.589620	-8.321920	1.431373
-1074.610157	10.826332	1.436378
-1078.560971	-0.865488	1.441382
-1082.046143	-7.273380	1.446387
-1086.067604	-8.197664	1.451392
-1088.786821	-8.065550	1.456397
-1092.925666	-0.810453	1.461402
-1097.236540	4.363820	1.466406
-1100.594479	-4.499171	1.471411
-1104.810167	2.367700	1.476416
-1108.412179	-4.461423	1.481421
-1112.301196	-5.485695	1.486426
-1115.793271	-3.708184	1.491430
-1119.488507	-6.988484	1.496435
-1123.147754	7.503728	1.501440
-1126.982790	2.397643	1.506445
-1130.686441	-5.982649	1.511450
-1134.900958	1.833396	1.516454
-1138.353659	6.015762	1.521459
-1142.370351	-1.896547	1.526464
-1146.018446	-4.534654	1.531469
-1149.725044	0.946733	1.536474
-1153.769103	-4.075402	1.541478
-1157.011972	-10.231785	1.546483
-1160.858098	3.006758	1.551488
-1164.788502	2.328234	1.556493
-1168.446431	-11.327813	1.561498
-1172.415991	-6.103939	1.566502
-1175.911186	-12.998923	1.571507
-1179.762248	-8.530419	1.576512
-1183.429805	-15.500313	1.581517
-1187.498895	-1.751407	1.586522
-1191.183032	2.072256	1.591526
-1194.373405	-8.859516	1.596531
-1198.436005	-1.971248	1.601536
-1202.307286	-7.383632	1.606541
-1206.039446	-7.130304	1.611546
-1210.075689	-9.067546	1.616550
-1213.548613	-6.597532	1.621555
-1217.789403	6.070326	1.626560
-1221.326176	-5.580250	1.631565
-1224.630651	-9.859598	1.636570
-1228.733496	-13.836149	1.641574
-1232.391386	-5.216471	1.646579
-1236.316775	10.616300	1.651584
-1239.955206	-0.144366	1.656589
-1243.675459	-7.708117	1.661594
-1247.685650	-7.000231	1.666598
-1251.230893	-9.441742	1.671603
-1255.098171	-1.383020	1.676608
-1258.858405	-8.766884	1.681613
-1262.546728	-1.580443	1.686618
-1266.217788	2.816820	1.691622
-1269.847824	-7.151940	1.696627
-1273.957295	2.345880	1.701632
-1277.642277	1.469002	1.706637
-1281.622285	4.474425	1.711642
-1285.251428	3.590200	1.716646
-1288.728081	-1.055732	1.721651
-1292.820498	1.843122	1.726656
-1296.338628	-3.138351	1.731661
-1300.009579	1.351984	1.736666
-1303.904299	-0.486321	1.741670
-1307.302711	-0.809785	1.746675
-1311.514257	-2.081715	1.751680
-1314.727464	-4.353926	1.756685
-1319.175105	-7.674321	1.761690
-1322.896245	0.615003	1.766694
-1326.255658	-5.535095	1.771699
-1330.194666	3.577574	1.776704
-1334.208388	-4.533552	1.781709
-1338.117022	-6.889955	1.786714
-1341.530027	-2.021383	1.791718
-1344.886334	-4.803644	1.796723
-1349.136578	8.069373	1.801728
-1352.683707	0.577437	1.806733
-1356.541677	-3.229928	1.811738
-1360.698113	-6.194741	1.816742
-1364.137913	-2.520308	1.821747
-1367.622659	-5.045438	1.826752
-1371.411060	2.360613	1.831757
-1375.276368	-1.666315	1.836762
-1379.335132	6.946799	1.841766
-1382.989968	-0.795922	1.846771
-1386.928732	-2.803650	1.851776
-1390.735377	0.175780	1.856781
-1394.098203	-1.731751	1.861786
-1398.050872	-0.446199	1.866790
-1401.556453	-7.807511	1.871795
-1405.436922	-0.884975	1.876800
-1409.260715	2.083038	1.881805
-1412.858592	-0.375027	1.886810
-1416.928539	-9.587149	1.891814
-1420.632379	-7.302206	1.896819
-1424.362692	-1.337217	1.901824
-1427.756460	-3.796397	1.906829
-1431.475662	-0.930247	1.911834
-1434.957252	0.677330	1.916838
-1439.161612	-6.262966	1.921843
-1443.406693	-1.295720	1.926848
-1447.101004	1.143856	1.931853
-1450.413695	-4.934688	1.936858
-1454.408285	-2.095370	1.941862
-1457.922960	-10.374477	1.946867
-1461.903811	-6.040851	1.951872
-1465.981569	-4.675232	1.956877
-1469.389722	-3.150324	1.961882
-1473.337614	-1.871716	1.966886
-1476.994122	-4.170483	1.971891
-1480.772388	-4.715135	1.976896
-1484.275010	-3.317001	1.981901
-1487.818441	0.320591	1.986906
-1492.046293	-0.047974	1.991910
-1495.883481	-8.160262	1.996915
-1499.608585	-1.534445	2.006912
-1500.736810	-7.229150	2.016909
-1497.890260	-4.138828	2.026906
-1494.851272	0.442781	2.036902
-1493.271629	-6.643958	2.046899
-1491.549038	-6.896257	2.056896
-1489.430093	-0.943638	2.066893
-1487.303388	-4.254312	2.076890
-1485.295173	-1.329730	2.086886
-1483.566540	1.636466	2.096883
-1481.792354	3.985898	2.106880
-1479.965158	-4.359414	2.116877
-1477.915773	-3.814562	2.126874
-1475.824794	-8.859494	2.136870
-1474.200001	-5.856140	2.146867
-1472.310526	-0.956228	2.156864
-1470.334971	-1.904276	2.166861
-1468.333314	0.378744	2.176858
-1466.694828	-6.229508	2.186854
-1464.590648	1.972330	2.196851
-1462.757903	-3.413348	2.206848
-1461.113372	-4.418910	2.216845
-1458.806517	-5.225786	2.226842
-1457.059830	-13.187136	2.236838
-1455.128288	-2.035034	2.246835
-1453.577819	-4.459208	2.256832
-1451.872441	-4.672406	2.266829
-1449.570904	-5.712103	2.276826
-1447.566313	-15.922095	2.286822
-1445.621839	-16.814619	2.296819
-1443.731853	-5.932170	2.306816
-1442.165303	-5.643135	2.316813
-1440.229194	-12.052706	2.326810
-1438.338072	-1.547796	2.336806
-1436.293420	-1.352674	2.346803
-1434.357035	-5.602297	2.356800
-1432.588944	-8.842874	2.366797
-1430.859013	-11.630499	2.376794
-1428.977085	-12.628258	2.386790
-1427.201614	-6.175328	2.396787
-1425.330115	-5.944579	2.406784
-1422.872452	-2.193481	2.416781
-1421.507301	-5.374276	2.426778
-1419.410627	-4.194314	2.436774
-1417.559655	-8.109725	2.446771
-1415.674806	-2.239554	2.456768
-1414.054965	0.894112	2.466765
-1411.844124	-8.260988	2.476762
-1410.061128	-0.626620	2.486758
-1408.410858	-0.734648	2.496755
-1406.298078	-0.417774	2.506752
-1404.288982	-1.754818	2.516749
-1402.406207	-3.434794	2.526746
-1400.666113	-3.890352	2.536742
-1398.678888	-1.271803	2.546739
-1396.990473	0.909849	2.556736
-1395.209626	1.123557	2.566733
-1393.167501	-4.786639	2.576730
-1391.040049	-5.545779	2.586726
-1389.601376	0.125843	2.596723
-1387.500594	-1.671125	2.606720
-1385.674232	1.866868	2.616717
-1383.843443	-1.263712	2.626714
-1382.009874	-0.011596	2.636710
-1379.771429	1.172550	2.646707
-1378.137248	-2.059183	2.656704
-1376.145968	1.062419	2.666701
-1374.334785	-1.476070	2.676698
-1372.628455	-1.506205	2.686694
-1370.655979	0.912626	2.696691
-1368.832402	-0.735741	2.706688
-1366.788424	-1.476760	2.716685
-1365.005925	-3.120128	2.726682
-1362.988466	-0.247440	2.736678
-1361.065563	-3.140117	2.746675
-1359.484349	2.150290	2.756672
-1357.658935	-8.147799	2.766669
-1355.624042	-0.961073	2.776666
-1353.743333	-5.743297	2.786662
-1351.985421	-4.073260	2.796659
-1349.811336	-2.334048	2.806656
-1348.153400	-5.530089	2.816653
-1346.278842	-3.270826	2.826650
-1344.323622	-4.635510	2.836646
-1342.160887	-3.832365	2.846643
-1340.516837	5.606931	2.856640
-1338.758257	-0.789940	2.866637
-1337.047722	-8.908057	2.876634
-1335.112170	-4.700661	2.886630
-1332.968627	-6.359162	2.896627
-1331.160994	-6.249166	2.906624
-1329.456652	-3.605803	2.916621
-1327.397775	-7.623896	2.926618
-1325.370733	-4.913761	2.936614
-1323.758646	-6.608769	2.946611
-1321.575661	-1.728862	2.956608
-1320.151158	-2.724372	2.966605
-1318.089835	-5.328117	2.976602
-1315.850852	-8.132400	2.986598
-1314.208419	-5.502801	2.996595
-1312.670953	-6.385335	3.006592
-1310.790185	-4.180720	3.016589
-1308.566173	-4.888924	3.026586
-1306.705523	-8.783694	3.036582
-1304.885338	-10.008312	3.046579
-1303.176636	-4.877217	3.056576
-1301.226980	-1.695202	3.066573
-1299.184991	-2.658474	3.076570
-1297.228791	-4.406959	3.086566
-1295.827189	-0.853016	3.096563
-1293.506991	-3.851855	3.106560
-1291.583608	1.462788	3.116557
-1289.862277	-6.154923	3.126554
-1287.814089	-1.561303	3.136550
-1286.092022	-7.772291	3.146547
-1284.595735	-5.659279	3.156544
-1282.542507	-9.796429	3.166541
-1280.452283	-2.684802	3.176538
-1278.706346	-8.228555	3.186534
-1276.455723	-1.936801	3.196531
-1274.940994	-6.805657	3.206528
-1273.071226	-6.648717	3.216525
-1271.073114	-8.924938	3.226522
-1269.242440	-4.478070	3.236518
-1267.272391	-3.276124	3.246515
-1265.435255	-7.313942	3.256512
-1263.699393	-8.285034	3.266509
-1262.036449	-11.249713	3.276506
-1260.057609	-6.074972	3.286502
-1257.966326	-8.566617	3.296499
-1255.993763	-4.792968	3.306496
-1254.068305	-7.873861	3.316493
-1252.339058	-5.926002	3.326490
-1250.531115	-9.434928	3.336486
-1248.530257	-6.772638	3.346483
-1246.880311	-4.418928	3.356480
-1244.873764	-4.173327	3.366477
-1242.764155	-9.590514	3.376474
-1241.238548	-2.202182	3.386470
-1239.124355	-4.688004	3.396467
-1237.251460	-2.354173	3.406464
-1235.534526	-4.643792	3.416461
-1233.563092	-4.746246	3.426458
-1231.888690	1.214606	3.436454
-1229.724267	-1.301352	3.446451
-1227.965030	-3.921417	3.456448
-1226.060882	0.238996	3.466445
-1223.987061	-7.976652	3.476442
-1222.322422	-7.827900	3.486438
-1220.454171	-5.422260	3.496435
-1218.470791	-2.474516	3.506432
-1216.730330	0.346312	3.516429
-1214.748215	2.852159	3.526426
-1212.847263	-2.525302	3.536422
-1210.986811	-6.443653	3.546419
-1209.444498	-6.657422	3.556416
-1207.350666	-4.409445	3.566413
-1205.536274	-3.263065	3.576410
-1203.470892	-3.080527	3.586406
-1201.443761	-2.396077	3.596403
-1199.976974	-5.461959	3.606400
-1197.899051	-4.566161	3.616397
-1196.019681	-5.004377	3.626394
-1194.216222	-2.954663	3.636390
-1192.128478	-9.456202	3.646387
-1190.550949	-2.725085	3.656384
-1188.595476	-0.837056	3.666381
-1186.771111	-4.605931	3.676378
-1184.785201	-1.023825	3.686374
-1182.980971	-4.794212	3.696371
-1180.982618	-1.619883	3.706368
-1179.114550	1.984240	3.716365
-1177.231082	9.217476	3.726362
-1175.307722	1.330671	3.736358
-1173.578156	1.972754	3.746355
-1171.672942	5.754099	3.756352
-1169.722804	-4.639611	3.766349
-1167.962493	-1.512448	3.776346
-1166.061219	3.471108	3.786342
-1163.935582	2.671412	3.796339
-1162.219305	5.324048	3.806336
-1160.473604	7.490399	3.816333
-1158.551212	0.229024	3.826330
-1156.834679	-2.292579	3.836326
-1154.940763	-5.493084	3.846323
-1152.856640	-0.638244	3.856320
-1150.728782	-3.246175	3.866317
-1149.007656	-0.325885	3.876314
-1147.442084	3.299817	3.886310
-1145.203908	-2.294174	3.896307
-1143.399042	3.611140	3.906304
-1141.635719	-2.170565	3.916301
-1139.761787	3.216862	3.926298
-1137.995077	2.171452	3.936294
-1136.100870	1.402490	3.946291
-1134.236216	-3.512790	3.956288
-1132.295617	-1.038124	3.966285
-1130.274580	-1.645793	3.976282
-1128.485819	-7.745766	3.986278
-1126.579302	-4.916696	3.996275
-1124.603084	-3.589299	4.006272
-1123.155335	-4.629461	4.016269
-1120.910689	-5.915524	4.026266
-1118.956107	-4.729923	4.036262
-1117.392758	-5.745943	4.046259
-1115.424333	-3.416240	4.056256
-1113.487787	-1.711435	4.066253
-1111.570190	-4.312538	4.076250
-1109.562868	5.337256	4.086246
-1107.921493	-1.078602	4.096243
-1106.192098	-1.241703	4.106240
-1103.937969	-0.527164	4.116237
-1102.117118	-4.484887	4.126234
-1100.343107	-2.334071	4.136230
-1098.558694	-1.209654	4.146227
-1096.461123	-3.089534	4.156224
-1094.719175	0.004308	4.166221
-1092.919987	0.902157	4.176218
-1091.038527	-7.705773	4.186214
-1088.901911	-7.327685	4.196211
-1087.080505	-0.782341	4.206208
-1085.213621	-0.646893	4.216205
-1083.551366	-2.711341	4.226202
-1081.531425	-6.614052	4.236198
-1079.957731	-4.240127	4.246195
-1077.722503	-2.354119	4.256192
-1075.959105	-1.979480	4.266189
-1074.092300	2.194934	4.276186
-1072.432811	-0.358538	4.286182
-1070.039991	-5.566670	4.296179
-1068.243333	-1.534190	4.306176
-1066.773284	1.350533	4.316173
-1064.712053	-2.246138	4.326170
-1062.934080	4.487755	4.336166
-1060.735528	-0.073508	4.346163
-1059.194731	1.086748	4.356160
-1057.372863	0.226788	4.366157
-1055.260001	-7.874971	4.376154
-1053.350961	-8.436239	4.386150
-1051.640390	-7.134186	4.396147
-1049.826682	0.855579	4.406144
-1047.689761	0.591025	4.416141
-1045.717932	-5.509749	4.426138
-1044.225491	-5.533854	4.436134
-1042.228992	-2.381210	4.446131
-1040.301561	-4.788040	4.456128
-1038.406813	-6.633851	4.466125
-1036.562110	0.007284	4.476122
-1034.684592	-8.726290	4.486118
-1032.968020	-5.112027	4.496115
-1030.824259	-0.613977	4.506112
-1028.902187	-4.442572	4.516109
-1027.361180	-7.919694	4.526106
-1025.295202	-11.622878	4.536102
-1023.244680	-6.560438	4.546099
-1021.556940	-6.813131	4.556096
-1019.779366	0.211386	4.566093
-1017.547192	-5.162056	4.576090
-1015.828373	-2.152874	4.586086
-1013.870178	-2.783551	4.596083
-1012.383746	-10.297196	4.606080
-1010.194289	-7.118541	4.616077
-1008.515501	-5.801899	4.626074
-1006.582635	-7.097992	4.636070
-1004.765354	-4.777180	4.646067
-1002.839937	-3.280500	4.656064
-1000.992143	-5.447195	4.666061
-998.983918	-4.333229	4.676058
-997.014994	-1.221923	4.686054
-995.240002	-3.250655	4.696051
-993.480680	0.118383	4.706048
-991.378256	-2.831129	4.716045
-989.413779	1.067210	4.726042
-987.743806	-2.229986	4.736038
-986.018913	-6.593857	4.746035
-983.782611	-2.625297	4.756032
-982.270246	1.345346	4.766029
-980.363451	-3.974452	4.776026
-978.535903	-5.616839	4.786022
-976.430493	-6.591552	4.796019
-974.555732	-8.593590	4.806016
-972.670363	-7.016272	4.816013
-971.122263	-3.059230	4.826010
-968.912972	-0.673179	4.836006
-967.009767	-6.380813	4.846003
-965.402221	-1.683273	4.856000
-963.429759	1.751181	4.865997
-961.660041	1.062265	4.875994
-959.637101	-4.476616	4.885990
-957.516873	1.986321	4.895987
-955.798672	-0.205407	4.905984
-954.049295	-1.789486	4.915981
-952.119766	-1.690791	4.925978
-950.344902	-6.263154	4.935974
-948.299887	1.604451	4.945971
-946.461232	-2.690742	4.955968
-944.601829	3.300755	4.965965
-942.733213	-0.948700	4.975962
-940.885887	2.581572	4.985958
-939.078831	0.961439	4.995955
-937.006869	-2.302103	5.005952
-934.982756	-6.581150	5.015949
-933.339490	-1.448771	5.025946
-931.467694	1.993912	5.035942
-929.529437	-2.037720	5.045939
-927.814508	7.425317	5.055936
-926.015581	7.364916	5.065933
-924.014744	3.054860	5.075930
-922.039001	-1.197497	5.085926
-920.197961	-3.634629	5.095923
-918.185575	7.801912	5.105920
-916.329529	4.786066	5.115917
-914.733417	0.791779	5.125914
-912.526653	1.117762	5.135910
-910.578447	-6.518606	5.145907
-909.065580	-2.001677	5.155904
-907.502768	0.448320	5.165901
-905.358930	6.779641	5.175898
-903.125036	3.033921	5.185894
-901.547906	4.747422	5.195891
-899.581896	8.404019	5.205888
-897.691516	2.827957	5.215885
-895.647144	-0.549561	5.225882
-894.105226	-0.535691	5.235878
-892.003512	-1.178158	5.245875
-890.047109	-1.142129	5.255872
-888.388259	-1.579582	5.265869
-886.602512	-0.461528	5.275866
-884.517541	-6.212371	5.285862
-882.546382	2.301842	5.295859
-880.751000	6.116785	5.305856
-878.999130	3.526570	5.315853
-877.133014	3.278623	5.325850
-875.006626	-4.888311	5.335846
-873.034492	1.142067	5.345843
-871.630061	-2.335231	5.355840
-869.623030	1.194832	5.365837
-867.620778	0.972497	5.375834
-865.775489	0.634730	5.385830
-863.977586	0.983488	5.395827
-862.029304	4.155054	5.405824
-860.261401	5.872824	5.415821
-858.323784	-6.609189	5.425818
-856.268830	-2.993619	5.435814
-854.473714	0.551387	5.445811
-852.522462	1.892483	5.455808
-851.164074	2.264142	5.465805
-849.086726	6.474564	5.475802
-846.910826	7.416597	5.485798
-844.936766	2.592989	5.495795
-843.582592	5.788489	5.505792
-841.314842	6.351106	5.515789
-839.105142	2.904576	5.525786
-837.697764	-2.025810	5.535782
-835.839625	-0.327183	5.545779
-833.995661	2.032134	5.555776
-831.862020	2.354092	5.565773
-830.186398	-3.958117	5.575770
-828.158956	2.755042	5.585766
-826.382251	1.656162	5.595763
-824.537188	0.099513	5.605760
-822.924912	6.465356	5.615757
-821.005762	-0.507882	5.625754
-818.717206	-5.099104	5.635750
-816.734592	-0.142457	5.645747
-815.173624	0.661053	5.655744
-813.312799	0.008211	5.665741
-811.368710	-6.490581	5.675738
-809.537985	-1.953335	5.685734
-807.609331	-5.844389	5.695731
-805.555807	2.388310	5.705728
-804.090121	-6.879280	5.715725
-802.052249	-5.529881	5.725722
-799.934593	-4.736391	5.735718
-798.236740	-7.284755	5.745715
-796.601270	0.029504	5.755712
-794.464336	-6.157465	5.765709
-792.588106	-2.696429	5.775706
-790.817244	-2.794873	5.785702
-788.791573	-1.053511	5.795699
-787.155778	-3.869844	5.805696
-785.054725	-2.101053	5.815693
-783.358916	3.653045	5.825690
-781.287083	-5.450885	5.835686
-779.141715	-4.394963	5.845683
-777.560158	-4.638405	5.855680
-775.930045	-1.085913	5.865677
-773.890456	-1.666242	5.875674
-771.835318	-4.887481	5.885670
-770.492313	-3.250156	5.895667
-768.138437	-4.793344	5.905664
-766.217769	-3.017812	5.915661
-764.574927	-5.029991	5.925658
-762.317184	-5.623070	5.935654
-760.697675	-0.445710	5.945651
-759.009551	-2.207754	5.955648
-757.249394	-2.579199	5.965645
-754.959640	-1.142118	5.975642
-753.159314	4.007930	5.985638
-751.210293	-3.686872	5.995635
-749.383928	-2.303625	6.005632
-747.398811	0.470573	6.015629
-745.859273	-0.598240	6.025626
-744.186623	-0.723585	6.035622
-742.071244	1.268746	6.045619
-739.980651	-0.881288	6.055616
-738.215820	-3.032946	6.065613
-736.166508	-2.711635	6.075610
-734.502655	-0.370824	6.085606
-732.508791	1.776725	6.095603
-730.771707	0.068456	6.105600
-728.954366	-6.544230	6.115597
-726.854013	-2.285268	6.125594
-725.048995	-2.425437	6.135590
-723.250374	-5.114589	6.145587
-721.407327	-1.392400	6.155584
-719.364250	-4.731668	6.165581
-717.642388	-5.215386	6.175578
-715.603389	-7.199259	6.185574
-713.713785	-7.532936	6.195571
-712.086903	-1.551454	6.205568
-710.226994	2.654369	6.215565
-708.059091	0.825167	6.225562
-706.103777	3.040478	6.235558
-704.430972	-8.825953	6.245555
-702.631268	-0.442072	6.255552
-700.700589	-2.538098	6.265549
-698.877482	-4.967460	6.275546
-696.549245	-5.004897	6.285542
-695.005161	-5.905456	6.295539
-693.277505	-1.168486	6.305536
-691.555254	-9.089113	6.315533
-689.469146	-4.440997	6.325530
-687.403541	-6.759098	6.335526
-685.532316	-1.964536	6.345523
-683.865926	2.428546	6.355520
-682.103104	-1.666441	6.365517
-680.011219	-1.855570	6.375514
-678.358109	-0.575637	6.385510
-676.301505	-0.043859	6.395507
-674.221453	3.094183	6.405504
-672.182173	-0.741811	6.415501
-670.631910	2.946676	6.425498
-668.779375	2.025270	6.435494
-666.995420	1.849037	6.445491
-665.036741	2.360155	6.455488
-663.414563	1.649244	6.465485
-661.203764	3.583772	6.475482
-659.339968	0.547935	6.485478
-657.595449	-1.115680	6.495475
-655.716223	2.035518	6.505472
-653.675179	-1.576531	6.515469
-651.998324	-1.361429	6.525466
-649.926051	3.093147	6.535462
-648.097228	-2.005523	6.545459
-646.244466	-0.327990	6.555456
-644.430474	-0.081108	6.565453
-642.523896	-3.676401	6.575450
-640.667183	-0.493173	6.585446
-638.819985	-6.201089	6.595443
-636.989398	2.239495	6.605440
-635.023877	2.897966	6.615437
-633.048089	2.793743	6.625434
-631.035393	0.885196	6.635430
-629.278608	-2.812472	6.645427
-627.464730	-5.721888	6.655424
-625.741638	1.145873	6.665421
-623.892870	-4.162809	6.675418
-621.965042	-5.088312	6.685414
-619.822424	-5.710231	6.695411
-618.129072	-1.562988	6.705408
-616.397782	-0.783397	6.715405
-614.250906	-7.718649	6.725402
-612.332192	-8.139002	6.735398
-610.847828	-11.687345	6.745395
-608.800179	-8.264594	6.755392
-606.993946	-4.076955	6.765389
-605.080523	-11.069641	6.775386
-602.980789	-5.299406	6.785382
-601.139906	-4.319416	6.795379
-599.576055	-5.185177	6.805376
-597.518849	0.004488	6.815373
-595.381984	6.248805	6.825370
-593.651031	-0.608938	6.835366
-591.898884	1.023133	6.845363
-589.986832	2.588609	6.855360
-588.268993	3.414580	6.865357
-585.974329	-0.537929	6.875354
-584.536836	-1.462443	6.885350
-582.802161	-2.677588	6.895347
-580.417664	1.245595	6.905344
-578.531886	-3.843176	6.915341
-576.941275	-1.814235	6.925338
-575.046113	2.313436	6.935334
-572.989182	-5.016365	6.945331
-571.195560	3.046495	6.955328
-569.138468	0.481957	6.965325
-567.597909	3.518378	6.975322
-565.692894	0.300763	6.985318
-563.408828	-1.750549	6.995315
-561.822880	1.475995	7.005312
-559.900532	0.404574	7.015309
-558.301817	-2.123053	7.025306
-556.329848	4.086061	7.035302
-554.268606	0.505603	7.045299
-552.526204	-1.970760	7.055296
-550.944423	1.619617	7.065293
-548.738499	5.220829	7.075290
-546.441016	2.965283	7.085286
-544.763991	1.320423	7.095283
-543.042058	1.763667	7.105280
-541.029284	0.608344	7.115277
-539.455536	9.202146	7.125274
-537.375328	1.884441	7.135270
-535.693220	-1.136494	7.145267
-533.705195	5.861134	7.155264
-531.798462	-0.442010	7.165261
-530.088833	0.453210	7.175258
-528.038217	2.528713	7.185254
-526.219449	4.177036	7.195251
-524.330457	5.239404	7.205248
-522.448085	4.074923	7.215245
-520.686887	2.048740	7.225242
-518.485964	-0.759782	7.235238
-516.916126	0.640936	7.245235
-514.722877	3.404200	7.255232
-513.070127	3.484302	7.265229
-511.011771	-4.532524	7.275226
-509.398833	-0.645514	7.285222
-507.380067	-0.255968	7.295219
-505.501164	0.512761	7.305216
-503.867598	4.001742	7.315213
-501.810994	3.777352	7.325210
-499.869787	1.300853	7.335206
-497.974464	-6.653608	7.345203
-496.089244	0.740998	7.355200
-494.405758	3.816222	7.365197
-492.323465	4.261951	7.375194
-490.310653	-1.922313	7.385190
-488.591469	-3.611761	7.395187
-486.879121	5.090998	7.405184
-485.028431	3.530551	7.415181
-483.022183	4.998965	7.425178
-481.062272	-8.171619	7.435174
-479.009180	2.388843	7.445171
-477.572613	-1.503898	7.455168
-475.679850	3.519509	7.465165
-473.801210	6.604636	7.475162
-471.674937	2.432805	7.485158
-469.852943	-5.773613	7.495155
-468.168127	1.948287	7.505152
-465.779793	-2.928550	7.515149
-464.434924	-4.253466	7.525146
-462.337462	-1.460646	7.535142
-460.477518	-2.983077	7.545139
-458.686925	-7.677609	7.555136
-456.852626	-1.029579	7.565133
-454.910487	1.009627	7.575130
-452.713195	-0.779829	7.585126
-451.178957	0.373984	7.595123
-449.170929	-0.069974	7.605120
-447.472690	8.639809	7.615117
-445.478067	5.210605	7.625114
-443.686741	-0.286145	7.635110
-441.679775	3.514310	7.645107
-439.765801	1.800107	7.655104
-437.860222	-0.691180	7.665101
-436.315596	0.986777	7.675098
-434.248656	3.936078	7.685094
-432.246714	5.721016	7.695091
-430.538521	-0.319824	7.705088
-428.782983	3.174999	7.715085
-426.695331	0.769912	7.725082
-424.672742	-0.243197	7.735078
-423.164024	-1.777413	7.745075
-421.189768	10.207287	7.755072
-419.174975	5.131188	7.765069
-417.495905	2.852928	7.775066
-415.516993	4.219975	7.785062
-413.360088	-0.623018	7.795059
-411.654114	8.148717	7.805056
-410.071899	12.429131	7.815053
-407.860030	8.152105	7.825050
-406.010235	5.939751	7.835046
-404.096465	1.626643	7.845043
-402.306175	8.401751	7.855040
-400.317098	-1.593418	7.865037
-398.653426	5.047170	7.875034
-397.126806	3.926957	7.885030
-394.829763	3.893217	7.895027
-392.926871	10.152984	7.905024
-390.949081	1.467000	7.915021
-389.409291	0.226266	7.925018
-387.229171	2.717009	7.935014
-385.247485	3.033632	7.945011
-383.821364	4.204751	7.955008
-381.929642	5.465747	7.965005
-379.838452	0.056954	7.975002
-377.897902	8.690211	7.984998
-375.980718	2.284458	7.994995
-374.013542	3.909205	8.004992
-372.236182	8.730072	8.014989
-370.428318	0.615974	8.024986
-368.908401	0.295802	8.034982
-366.868144	9.566839	8.044979
-364.573102	2.281288	8.054976
-362.816995	5.016593	8.064973
-361.173398	7.081434	8.074970
-359.115923	7.687560	8.084966
-357.179535	3.386665	8.094963
-355.421494	2.107952	8.104960
-353.491545	7.645005	8.114957
-351.935915	6.466504	8.124954
-349.997986	9.842270	8.134950
-347.807969	2.020865	8.144947
-346.089442	-0.778387	8.154944
-344.042889	5.647960	8.164941
-342.600851	4.315492	8.174938
-340.585229	5.959376	8.184934
-338.630193	8.301360	8.194931
-336.465743	6.247248	8.204928
-334.788974	9.048925	8.214925
-332.971821	9.808702	8.224922
-330.704238	1.907033	8.234918
-329.284088	-1.761950	8.244915
-327.425774	6.958690	8.254912
-325.393381	-0.444372	8.264909
-323.571246	2.817268	8.274906
-321.412399	2.234076	8.284902
-319.860837	0.399397	8.294899
-317.670314	1.189584	8.304896
-316.076777	2.346652	8.314893
-314.612653	0.042773	8.324890
-312.240878	-3.866531	8.334886
-310.232254	-0.773599	8.344883
-308.398455	1.147232	8.354880
-306.855825	1.988745	8.364877
-304.741603	1.673220	8.374874
-302.880104	6.092287	8.384870
-300.972103	-0.768264	8.394867
-299.040868	2.796509	8.404864
-297.213679	0.182052	8.414861
-295.370716	2.044589	8.424858
-293.689462	2.538717	8.434854
-291.462610	-1.772175	8.444851
-289.830151	-1.200781	8.454848
-288.236538	0.349455	8.464845
-286.035617	3.429082	8.474842
-284.086476	1.140962	8.484838
-282.113043	2.752155	8.494835
-280.349685	3.556875	8.504832
-278.448530	6.327513	8.514829
-276.544556	1.171321	8.524826
-274.827920	1.407181	8.534822
-272.953586	6.733705	8.544819
-270.952115	3.085652	8.554816
-269.172614	3.069901	8.564813
-267.213930	-2.210280	8.574810
-265.453983	-0.866580	8.584807
-263.561127	-1.219368	8.594803
-261.498435	-0.053461	8.604800
-260.126183	4.656889	8.614797
-257.556135	1.293889	8.624794
-255.911778	-1.970309	8.634791
-254.213060	-7.456883	8.644787
-252.190307	3.910755	8.654784
-250.459925	-2.645092	8.664781
-248.694999	-1.112699	8.674778
-246.395338	2.495949	8.684775
-244.587422	-0.631714	8.694771
-242.931780	1.436026	8.704768
-240.804860	4.380664	8.714765
-239.143536	-3.321533	8.724762
-237.385545	6.480996	8.734759
-235.027183	-5.827746	8.744755
-233.364260	-5.982761	8.754752
-231.805025	-8.019136	8.764749
-229.695124	-6.135993	8.774746
-227.614805	-3.758648	8.784743
-225.843975	-3.315084	8.794739
-224.106016	-1.107310	8.804736
-222.312601	-2.761050	8.814733
-220.209082	-2.073732	8.824730
-218.438510	-4.788043	8.834727
-216.632493	-5.693783	8.844723
-214.773266	-3.350617	8.854720
-212.877841	-1.567442	8.864717
-210.862294	-5.445063	8.874714
-208.893079	-11.817940	8.884711
-207.198185	-10.601185	8.894707
-205.663156	-7.552586	8.904704
-203.701349	-6.283686	8.914701
-201.436059	-7.363761	8.924698
-199.687674	-11.838216	8.934695
-197.743983	-12.579595	8.944691
-195.751329	-14.715113	8.954688
-194.100432	-11.932894	8.964685
-192.303261	-13.730896	8.974682
-190.438645	-12.871216	8.984679
-188.563569	-11.790571	8.994675
-186.491495	-10.741360	9.004672
-184.566033	-9.465066	9.014669
-182.845168	-6.435054	9.024666
-181.071455	-9.454578	9.034663
-179.135921	-14.686784	9.044659
-177.348813	-9.564163	9.054656
-175.225186	-6.202096	9.064653
-173.382519	-12.418962	9.074650
-171.484248	-1.721392	9.084647
-169.822395	-5.215696	9.094643
-167.884241	-10.471998	9.104640
-165.911869	-5.865249	9.114637
-164.082307	-4.365212	9.124634
-161.991455	-2.821603	9.134631
-160.308957	-9.050798	9.144627
-158.379607	-8.157211	9.154624
-156.475547	-10.837514	9.164621
-154.938816	-8.245472	9.174618
-152.778390	-7.060329	9.184615
-150.861640	-10.345816	9.194611
-149.195798	-8.394903	9.204608
-147.142095	-11.883820	9.214605
-145.238593	-7.308697	9.224602
-143.571084	-7.775437	9.234599
-141.526340	-13.596625	9.244595
-139.683888	-13.848115	9.254592
-137.687121	-7.329955	9.264589
-135.784354	-6.370529	9.274586
-133.969564	-6.532338	9.284583
-132.330327	-7.125613	9.294579
-130.408446	-0.469178	9.304576
-128.358442	-5.316977	9.314573
-126.554459	-1.288069	9.324570
-124.578086	-3.048298	9.334567
-122.871074	-8.694007	9.344563
-120.859026	-3.973549	9.354560
-118.942089	-4.379014	9.364557
-116.994490	-6.786758	9.374554
-115.462621	-6.006563	9.384551
-113.419169	-4.281662	9.394547
-111.569192	-6.710143	9.404544
-109.510697	-6.713445	9.414541
-108.191995	-4.850804	9.424538
-105.863648	-2.770294	9.434535
-103.725292	-7.657433	9.444531
-102.121067	-2.759785	9.454528
-100.381344	2.927836	9.464525
-98.390594	-1.520484	9.474522
-96.542378	-2.199182	9.484519
-94.832906	-6.094196	9.494515
-92.735649	-3.970489	9.504512
-91.057254	-10.064774	9.514509
-88.985051	-6.910742	9.524506
-87.288935	-7.699379	9.534503
-85.119610	-7.229285	9.544499
-83.267768	-10.655946	9.554496
-81.707138	-12.141392	9.564493
-79.690646	-5.807906	9.574490
-77.492064	-8.753033	9.584487
-75.755063	-3.390228	9.594483
-74.086667	-10.056071	9.604480
-72.063218	-6.682664	9.614477
-70.345265	-0.738915	9.624474
-68.435320	-7.964348	9.634471
-66.356276	-17.111506	9.644467
-64.680406	-9.005759	9.654464
-62.754314	-8.484211	9.664461
-61.108228	-8.254312	9.674458
-59.185875	-4.458973	9.684455
-56.867178	-11.146438	9.694451
-55.143227	-10.291055	9.704448
-52.630574	-5.865134	9.714445
-50.258677	-6.581545	9.724442
-49.595369	1.692061	9.734439
-47.696383	-6.996888	9.744435
-45.733058	-9.438664	9.754432
-44.212702	-7.257625	9.764429
-41.893013	-6.415158	9.774426
-39.894460	-6.552525	9.784423
-38.387255	-4.097802	9.794419
-36.879114	-7.971714	9.804416
-34.794439	-1.453271	9.814413
-32.570128	-0.290840	9.824410
-30.796684	-1.112299	9.834407
-29.015841	-9.403437	9.844403
-26.982272	-1.811034	9.854400
-25.272529	-2.301799	9.864397
-23.320718	-1.613793	9.874394
-21.571162	-6.798851	9.884391
-19.617409	-1.563734	9.894387
-17.587753	-5.110292	9.904384
-15.884166	-1.030544	9.914381
-13.987967	0.165293	9.924378
-11.912254	-0.188045	9.934375
-10.309378	-3.920737	9.944371
-8.551013	-6.141895	9.954368
-6.512124	3.740759	9.964365
-4.834793	5.833629	9.974362
-3.329792	33.219045	9.984359
-2.343705	71.406924	9.994355
-0.896794	126.346993	10.004352
0.000000	173.772024	10.009357
1.198878	195.387017	10.014362
1.855962	228.896813	10.019367
2.254480	255.832521	10.024371
3.008419	272.093809	10.029376
3.340863	293.085467	10.034381
3.597360	297.188783	10.039386
3.719409	318.775440	10.044391
4.193184	310.625663	10.049395
4.163493	308.066158	10.054400
4.047010	323.546957	10.059405
4.371995	305.279353	10.064410
4.156943	304.848373	10.069415
3.601127	296.580543	10.074419
3.913033	298.128202	10.079424
3.987623	296.660682	10.084429
4.016584	300.197885	10.089434
4.046823	325.230701	10.094439
4.199384	325.253606	10.099443
4.427347	330.660915	10.104448
4.202313	335.487608	10.109453
4.666892	332.639524	10.114458
4.337024	335.976920	10.119463
4.381729	339.092144	10.124467
4.821972	332.419028	10.129472
4.438535	342.922894	10.134477
4.838783	340.118186	10.139482
4.366197	335.235458	10.144487
4.798639	342.849473	10.149491
4.813737	334.091584	10.154496
4.822873	326.968405	10.159501
4.806420	320.383907	10.164506
4.731677	320.720615	10.169511
4.856104	339.939877	10.174515
4.825025	343.182308	10.179520
5.046810	349.319176	10.184525
5.169418	347.862917	10.189530
5.159266	355.164324	10.194535
5.121974	351.787569	10.199539
4.850952	339.960769	10.204544
4.759759	362.754779	10.209549
5.284017	359.517119	10.214554
5.385257	359.604980	10.219559
4.999140	372.933675	10.224563
4.948175	373.007966	10.229568
4.954571	374.970223	10.234573
5.362026	372.347290	10.239578
5.074742	374.058338	10.244583
5.125984	372.201865	10.249587
5.416600	375.180100	10.254592
5.213801	389.479381	10.259597
5.714012	396.781411	10.264602
5.684978	391.991924	10.269607
5.920109	393.942932	10.274611
5.701999	396.906117	10.279616
5.876823	402.667289	10.284621
5.886363	392.464153	10.289626
6.226825	398.853355	10.294631
6.114525	395.660445	10.299635
6.353469	396.768733	10.304640
6.134358	407.415173	10.309645
6.294790	405.382004	10.314650
6.032407	398.961279	10.319655
5.902849	404.651149	10.324659
5.878702	414.657780	10.329664
6.291295	406.721140	10.334669
6.258741	413.431624	10.339674
6.257568	419.462154	10.344679
6.282062	421.134518	10.349683
6.629300	407.390780	10.354688
6.120956	425.845314	10.359693
6.335926	418.876922	10.364698
6.310414	413.686310	10.369703
6.135641	421.285250	10.374707
6.758623	421.405016	10.379712
6.498071	427.006976	10.384717
6.485516	440.416502	10.389722
6.470270	451.735374	10.394727
6.682066	455.744938	10.399731
6.884412	448.172978	10.404736
7.096664	455.192952	10.409741
7.205538	451.114752	10.414746
7.314719	450.272498	10.419751
6.909586	445.539827	10.424755
7.247117	458.839914	10.429760
6.837964	452.797398	10.434765
7.168354	453.484241	10.439770
7.136277	464.405251	10.444775
7.146371	460.763861	10.449779
7.274142	447.788394	10.454784
6.785348	462.516572	10.459789
6.992089	455.685096	10.464794
7.328303	462.347824	10.469799
7.300188	456.165682	10.474803
7.691546	473.010169	10.479808
7.513639	476.722339	10.484813
7.822696	470.267210	10.489818
7.785755	472.524982	10.494823
7.355570	471.215229	10.499827
7.630306	477.294819	10.504832
7.712550	488.900954	10.509837
7.959045	490.905358	10.514842
8.053723	493.537968	10.519847
8.175488	495.829568	10.524851
8.008393	490.558217	10.529856
7.737381	481.172495	10.534861
7.901754	471.939694	10.539866
8.007640	473.622736	10.544871
7.648208	481.041419	10.549875
7.811024	470.466841	10.554880
7.722474	473.221715	10.559885
7.811909	473.931220	10.564890
7.845989	489.446530	10.569895
7.969375	507.782273	10.574899
8.226841	506.730278	10.579904
8.175854	513.003765	10.584909
8.614118	509.349267	10.589914
8.432241	505.506666	10.594919
8.340154	511.152754	10.599923
8.473828	512.667361	10.604928
8.349257	508.331480	10.609933
8.454914	516.530735	10.614938
8.522946	523.769293	10.619943
8.985819	523.529809	10.624947
9.159365	521.366796	10.629952
8.832119	533.047741	10.634957
9.005825	525.708975	10.639962
8.690154	528.485891	10.644967
8.656910	537.473736	10.649971
8.918136	528.261722	10.654976
8.357578	529.614237	10.659981
8.602788	513.834991	10.664986
8.697502	528.747720	10.669991
8.779967	549.885281	10.674995
9.005831	544.919466	10.680000
8.941956	553.451721	10.685005
9.187362	550.942916	10.690010
9.376861	552.975344	10.695015
9.423224	554.814551	10.700019
9.355008	545.257666	10.705024
9.192066	555.892101	10.710029
9.630481	566.813842	10.715034
9.704045	578.006681	10.720039
9.834632	580.499533	10.725043
10.001749	574.513291	10.730048
9.592741	578.104646	10.735053
9.561784	576.228140	10.740058
9.838897	573.780509	10.745063
9.735047	579.982029	10.750067
10.197037	581.086297	10.755072
9.453806	584.174277	10.760077
10.074931	576.032392	10.765082
10.056947	585.333234	10.770087
9.957217	587.757163	10.775091
10.171808	583.840267	10.780096
10.204517	584.167728	10.785101
10.269068	583.116534	10.790106
10.330892	588.663984	10.795111
10.041897	588.017698	10.800115
10.350686	584.443759	10.805120
10.146128	590.297057	10.810125
10.274465	587.567213	10.815130
10.425687	600.731561	10.820135
10.473034	607.246458	10.825139
10.845277	614.833948	10.830144
10.642049	621.138072	10.835149
10.455190	608.807177	10.840154
10.794382	610.970284	10.845159
10.868219	620.516711	10.850163
10.988796	612.279593	10.855168
10.904880	624.043231	10.860173
10.856105	623.262432	10.865178
10.964573	630.904618	10.870183
10.750579	630.087089	10.875187
11.227253	623.748667	10.880192
11.094067	628.761087	10.885197
11.101597	631.472280	10.890202
11.121226	629.417381	10.895207
11.030779	632.574725	10.900211
11.234924	625.988022	10.905216
11.082164	629.825535	10.910221
10.975281	633.218899	10.915226
10.894366	631.801381	10.920231
10.867371	632.554697	10.925235
11.374103	637.409860	10.930240
11.272590	652.401324	10.935245
11.558576	652.549612	10.940250
11.516842	652.199791	10.945255
11.706166	659.436418	10.950259
11.613431	664.827191	10.955264
11.403428	665.360529	10.960269
11.590432	661.312389	10.965274
11.613526	670.040584	10.970279
11.725250	669.051250	10.975283
11.763199	667.606884	10.980288
11.692952	674.690946	10.985293
12.026711	666.591691	10.990298
11.892724	671.583753	10.995303
11.655327	688.956148	11.000307
12.048012	690.243374	11.005312
12.355916	701.585020	11.010317
12.336658	702.948990	11.015322
12.634708	699.622752	11.020327
12.512724	699.993812	11.025331
12.609031	701.397700	11.030336
12.349478	686.968277	11.035341
12.372238	686.336921	11.040346
12.653647	698.356178	11.045351
12.581182	694.000892	11.050355
12.610061	689.031751	11.055360
12.392458	688.744674	11.060365
12.590244	691.794555	11.065370
12.698629	700.799338	11.070375
12.603713	708.259528	11.075379
12.900905	700.066734	11.080384
12.914073	701.635277	11.085389
12.908918	696.431855	11.090394
12.816291	702.890268	11.095399
12.847719	701.459556	11.100403
12.624190	702.748869	11.105408
12.412851	705.304164	11.110413
12.861471	699.547374	11.115418
13.000412	700.488702	11.120423
12.582462	715.149062	11.125427
13.166790	722.081434	11.130432
13.107043	737.924226	11.135437
13.106257	737.200425	11.140442
13.541374	735.872487	11.145447
13.396519	736.360742	11.150451
13.861481	731.749408	11.155456
13.612130	735.160788	11.160461
13.533758	731.120260	11.165466
13.649863	732.129891	11.170471
13.367937	736.795470	11.175475
13.780980	735.612986	11.180480
13.700567	735.898565	11.185485
13.904817	737.791465	11.190490
13.902000	736.446640	11.195495
13.903401	743.509846	11.200499
14.031031	738.155914	11.205504
13.919710	738.403843	11.210509
13.663598	742.191635	11.215514
13.700977	737.910283	11.220519
13.714610	743.708341	11.225523
13.776955	742.302657	11.230528
14.006978	747.080560	11.235533
13.795462	747.434361	11.240538
14.054011	760.793058	11.245543
14.079562	770.733657	11.250547
14.430677	769.647784	11.255552
14.296789	775.720131	11.260557
14.628067	777.556505	11.265562
14.851663	767.407277	11.270567
14.660963	774.453827	11.275571
14.741955	762.062733	11.280576
14.859564	771.894029	11.285581
14.519670	762.016038	11.290586
14.929210	755.046416	11.295591
14.726613	759.150544	11.300595
14.685914	746.130715	11.305600
14.763048	761.786113	11.310605
14.908522	767.634118	11.315610
15.242543	762.849684	11.320615
14.572373	767.433687	11.325619
14.918090	753.560550	11.330624
14.814651	764.065793	11.335629
14.678521	768.600891	11.340634
15.239880	770.879984	11.345639
14.842768	773.690436	11.350643
14.909878	768.765636	11.355648
15.036838	777.996173	11.360653
14.868790	772.922788	11.365658
15.165901	775.959999	11.370663
15.087964	793.461635	11.375667
15.613998	788.829504	11.380672
15.598929	798.647284	11.385677
15.491242	799.553834	11.390682
15.494542	801.272202	11.395687
15.174132	801.339004	11.400691
15.507555	802.395985	11.405696
15.504629	809.847864	11.410701
15.521793	810.296086	11.415706
15.708561	809.080296	11.420711
15.551095	810.172992	11.425715
15.898738	804.485885	11.430720
15.664820	801.774353	11.435725
16.044337	800.830612	11.440730
15.773621	808.238464	11.445735
15.747807	824.468620	11.450739
16.316685	823.996173	11.455744
16.243640	836.551497	11.460749
16.364679	832.554834	11.465754
16.182823	817.564080	11.470759
16.097121	819.694058	11.475763
16.281430	825.906496	11.480768
16.719272	829.099479	11.485773
16.512251	825.101522	11.490778
16.227703	822.629885	11.495783
16.235138	832.885670	11.500787
16.374017	827.760158	11.505792
16.303445	843.967510	11.510797
16.677737	839.842139	11.515802
17.000906	837.940659	11.520807
16.531577	842.855370	11.525811
16.910106	836.012088	11.530816
16.589518	846.209807	11.535821
16.876581	839.810066	11.540826
16.828716	845.048662	11.545831
16.762987	837.883553	11.550835
16.788132	837.340125	11.555840
16.501878	844.852981	11.560845
16.776036	837.037542	11.565850
17.180309	842.992543	11.570855
16.793274	842.860225	11.575859
16.981219	846.029987	11.580864
17.375592	857.118255	11.585869
17.301278	860.495438	11.590874
17.722341	866.914574	11.595879
17.281726	854.221797	11.600883
17.003955	839.012917	11.605888
17.750633	851.606256	11.610893
17.433937	855.903661	11.615898
17.654043	853.517119	11.620903
17.513062	864.164047	11.625907
17.831738	861.671891	11.630912
17.629078	867.099196	11.635917
17.738859	864.127819	11.640922
17.807708	861.503611	11.645927
17.943916	866.594578	11.650931
18.072908	853.016125	11.655936
17.750995	840.548869	11.660941
17.749456	849.599663	11.665946
18.147596	858.684493	11.670951
17.880609	864.136249	11.675955
18.237382	860.660253	11.680960
18.151613	861.656356	11.685965
17.851601	860.407808	11.690970
18.090084	865.947690	11.695975
18.146627	865.935446	11.700979
18.054558	859.209791	11.705984
18.235994	866.077176	11.710989
18.124322	866.851894	11.715994
18.506318	867.096843	11.720999
18.315816	872.601062	11.726003
18.384229	866.937966	11.731008
18.214945	869.896612	11.736013
18.240611	859.930285	11.741018
18.424673	868.987761	11.746023
18.370882	894.304635	11.751027
18.471791	889.975257	11.756032
18.614929	894.434312	11.761037
18.538216	902.677066	11.766042
18.938722	887.213289	11.771047
18.760512	898.761940	11.776051
18.701856	901.846459	11.781056
18.584366	902.801890	11.786061
18.632288	899.816716	11.791066
19.028038	896.492199	11.796071
19.139997	907.489923	11.801075
19.412747	909.217371	11.806080
19.391521	897.526902	11.811085
19.201909	899.214545	11.816090
19.213704	896.697208	11.821095
18.999013	899.380811	11.826099
19.320033	904.443893	11.831104
19.161848	923.887209	11.836109
19.342389	916.080352	11.841114
19.673827	909.060033	11.846119
19.508678	924.252749	11.851123
19.864147	910.423643	11.856128
19.764929	919.461672	11.861133
19.616985	913.520810	11.866138
20.036936	911.767898	11.871143
19.954949	914.433493	11.876147
20.224149	906.740241	11.881152
19.761174	908.179731	11.886157
19.581980	915.049461	11.891162
19.798617	905.590417	11.896167
19.664312	912.285819	11.901171
19.677790	904.751632	11.906176
19.971836	911.216280	11.911181
19.888306	903.885234	11.916186
20.246258	912.199024	11.921191
20.003238	918.332993	11.926195
20.149436	907.057387	11.931200
19.965725	914.604389	11.936205
20.066527	917.838531	11.941210
20.653076	918.990775	11.946215
20.428575	935.301632	11.951219
20.817057	935.596013	11.956224
20.503765	919.924330	11.961229
20.395145	912.370187	11.966234
20.638705	922.558410	11.971239
20.925271	929.259239	11.976243
20.640505	916.003777	11.981248
20.352205	920.435451	11.986253
20.747147	930.678389	11.991258
20.957699	939.075632	11.996263
20.779536	941.914276	12.001267
21.015857	940.870356	12.006272
20.793002	942.351981	12.011277
20.903489	940.780895	12.016282
21.151604	935.434485	12.021287
21.181285	937.886720	12.026291
21.133055	931.341708	12.031296
20.801288	912.824831	12.036301
20.570342	925.331295	12.041306
21.135499	929.295673	12.046311
20.727346	945.107521	12.051315
21.044806	938.302319	12.056320
21.082358	941.163331	12.061325
21.251840	941.483180	12.066330
20.941841	920.819613	12.071335
20.631564	911.678006	12.076339
21.084025	922.347028	12.081344
20.935664	935.535807	12.086349
20.851165	935.839389	12.091354
21.038871	928.280556	12.096359
21.110225	937.898555	12.101363
20.668248	926.018111	12.106368
20.904658	933.472884	12.111373
21.215815	943.618801	12.116378
21.234758	927.804228	12.121383
20.842958	932.406964	12.126387
21.116338	929.483602	12.131392
21.013892	921.209336	12.136397
20.955620	926.178369	12.141402
20.983131	922.051510	12.146407
20.835312	931.952058	12.151411
20.864696	918.819964	12.156416
20.937221	925.430343	12.161421
20.742876	936.752925	12.166426
20.880205	925.347824	12.171431
20.643237	930.944637	12.176435
20.758939	925.173045	12.181440
21.034710	945.763081	12.186445
21.043371	947.994730	12.191450
21.296979	935.560187	12.196455
20.934389	936.608331	12.201459
20.840251	928.080408	12.206464
21.062081	931.724207	12.211469
20.853392	930.243455	12.216474
20.965445	926.300242	12.221479
20.895159	930.969977	12.226483
20.862929	918.683545	12.231488
21.024990	925.312761	12.236493
20.791305	929.634796	12.241498
20.959162	923.780765	12.246503
20.706644	935.669322	12.251507
21.058097	927.931400	12.256512
20.911444	937.300301	12.261517
20.629433	927.269452	12.266522
21.191834	946.511134	12.271527
20.981764	950.823101	12.276531
21.251488	936.171810	12.281536
21.320998	931.315962	12.286541
20.952013	933.418594	12.291546
21.149065	925.266879	12.296551
20.968952	938.460724	12.301555
21.340009	934.323227	12.306560
21.109296	932.909068	12.311565
20.946863	932.882861	12.316570
21.225392	919.692105	12.321575
20.759648	935.188256	12.326579
21.073318	925.491360	12.331584
20.906746	931.737728	12.336589
21.101233	934.873348	12.341594
21.244052	927.485688	12.346599
21.179285	933.660623	12.351603
21.047334	933.087050	12.356608
21.097939	918.637891	12.361613
20.815050	912.404720	12.366618
21.033804	910.841602	12.371623
20.713208	909.935397	12.376627
20.894357	912.309850	12.381632
21.177224	918.449835	12.386637
20.730254	912.900462	12.391642
20.932176	912.171131	12.396647
20.769550	926.005611	12.401651
21.225038	943.188946	12.406656
21.013435	935.021974	12.411661
20.926459	923.043909	12.416666
20.937522	916.702348	12.421671
20.889602	918.320083	12.426675
20.729318	913.805261	12.431680
20.925563	921.678043	12.436685
20.871223	940.425113	12.441690
21.019795	936.654279	12.446695
21.051505	944.666863	12.451699
21.141470	934.720194	12.456704
21.055091	934.170893	12.461709
20.945323	925.889907	12.466714
21.176761	913.742787	12.471719
20.912048	921.906720	12.476723
21.147235	922.580386	12.481728
21.208781	924.857215	12.486733
20.796398	923.642354	12.491738
21.032384	910.770647	12.496743
21.016459	916.950401	12.501747
21.021974	916.547303	12.506752
21.207012	917.965448	12.511757
21.133870	919.561972	12.516762
21.186047	910.132310	12.521767
21.007221	922.609957	12.526771
21.224199	921.271062	12.531776
20.878958	924.401294	12.536781
20.771255	931.493032	12.541786
21.043785	924.923674	12.546791
21.046580	931.109911	12.551795
21.277138	927.696610	12.556800
21.003102	922.849823	12.561805
20.709789	921.310024	12.566810
21.141291	921.796252	12.571815
20.890613	930.897871	12.576819
20.879682	915.942836	12.581824
20.900645	916.802064	12.586829
20.917270	923.001863	12.591834
21.236646	923.162178	12.596839
20.897911	905.334014	12.601843
20.783483	894.246650	12.606848
20.870038	904.267503	12.611853
21.007376	919.986015	12.616858
21.152514	915.252159	12.621863
20.805727	904.690731	12.626867
20.704320	897.308920	12.631872
20.942738	906.654234	12.636877
20.546208	922.125139	12.641882
20.859466	921.685575	12.646887
20.875268	929.132951	12.651891
20.592790	927.209778	12.656896
20.840355	928.863970	12.661901
20.955355	932.789751	12.666906
21.540752	913.491043	12.671911
21.137596	925.430428	12.676915
21.007044	928.904910	12.681920
21.288090	923.001286	12.686925
21.176032	919.423422	12.691930
21.181631	904.092002	12.696935
20.903911	898.659150	12.701939
20.941368	896.730688	12.706944
20.897134	891.531852	12.711949
20.720131	891.380228	12.716954
21.148771	893.735707	12.721959
21.010100	899.644855	12.726963
21.206233	897.818826	12.731968
21.143487	891.064824	12.736973
20.715350	896.452403	12.741978
20.973274	889.811269	12.746983
20.897467	897.913520	12.751987
20.826111	900.504872	12.756992
20.818957	894.628300	12.761997
20.703418	904.958945	12.767002
20.853881	902.023653	12.772007
21.062940	899.115287	12.777011
21.115413	901.571766	12.782016
20.818929	893.733763	12.787021
20.895438	899.241141	12.792026
20.992278	896.145658	12.797031
20.758673	901.581065	12.802035
21.058034	895.062637	12.807040
20.779543	895.733069	12.812045
20.689370	903.400773	12.817050
21.024533	901.842745	12.822055
20.930722	903.920409	12.827059
20.828979	892.113469	12.832064
21.083559	904.107213	12.837069
21.196456	917.388356	12.842074
21.187480	906.870825	12.847079
21.079545	906.913200	12.852083
21.402069	891.203222	12.857088
21.333019	903.868360	12.862093
20.748621	907.959303	12.867098
21.369692	898.746437	12.872103
21.299213	908.642520	12.877107
21.192387	905.771917	12.882112
21.111412	892.100752	12.887117
21.039789	883.995066	12.892122
21.128629	870.818838	12.897127
20.645877	882.482284	12.902131
20.711710	875.796095	12.907136
20.985971	887.573787	12.912141
20.911947	896.674020	12.917146
21.377706	901.997884	12.922151
20.885915	887.884437	12.927155
20.840564	876.976891	12.932160
20.837884	875.422284	12.937165
20.777723	874.619631	12.942170
21.052443	878.300716	12.947175
20.972590	892.533570	12.952179
20.960102	883.637816	12.957184
21.321162	877.379230	12.962189
20.983133	881.916601	12.967194
20.924188	873.103961	12.972199
21.221798	876.641037	12.977203
20.965861	878.908568	12.982208
20.821425	872.582365	12.987213
20.901200	876.841774	12.992218
20.876825	871.155626	12.997223
20.795877	883.346378	13.002227
21.026075	876.779062	13.007232
21.093784	872.183733	13.012237
20.776696	880.762873	13.017242
21.098368	874.977375	13.022247
20.870681	882.547145	13.027251
21.063928	877.693659	13.032256
21.050499	876.389938	13.037261
20.941788	880.075404	13.042266
21.087656	877.935677	13.047271
20.704553	881.694870	13.052275
20.945863	886.660266	13.057280
21.125103	879.593269	13.062285
20.750641	877.661117	13.067290
21.117592	873.577911	13.072295
20.851189	881.835137	13.077299
21.251307	878.069933	13.082304
21.244094	884.617312	13.087309
21.261086	884.094107	13.092314
21.129568	872.996868	13.097319
21.325005	885.793282	13.102323
20.890488	881.110885	13.107328
21.089507	883.547142	13.112333
20.677752	882.614474	13.117338
20.933169	885.940651	13.122343
20.952455	889.340761	13.127347
20.724463	878.870798	13.132352
20.950199	881.529887	13.137357
20.755604	889.531223	13.142362
20.916708	887.740746	13.147367
20.670748	892.160928	13.152371
20.519478	888.789609	13.157376
21.032177	890.828889	13.162381
20.665096	892.514872	13.167386
20.943136	884.998427	13.172391
20.841705	888.753700	13.177395
20.807332	885.881008	13.182400
21.014916	880.274562	13.187405
20.963043	891.582272	13.192410
21.029091	890.737411	13.197415
20.699682	890.849805	13.202419
20.809923	888.419275	13.207424
20.815362	889.364562	13.212429
20.640043	892.828828	13.217434
20.535208	891.874018	13.222439
20.946878	902.674118	13.227443
21.146906	915.916130	13.232448
21.151240	904.969098	13.237453
20.723547	908.448388	13.242458
20.986199	889.710572	13.247463
20.905433	889.291272	13.252467
21.105705	892.296643	13.257472
21.097913	893.554717	13.262477
21.093025	894.112121	13.267482
21.206745	891.343549	13.272487
21.117700	893.600235	13.277491
21.045694	895.944095	13.282496
21.287756	888.668366	13.287501
20.697756	892.611956	13.292506
21.016627	886.136155	13.297511
21.106037	898.000111	13.302515
21.027585	887.906859	13.307520
21.222085	889.790296	13.312525
20.950544	888.564014	13.317530
20.956263	884.150465	13.322535
21.064568	889.588110	13.327539
21.058329	889.724659	13.332544
21.071765	881.021902	13.337549
20.952929	897.580807	13.342554
21.138753	886.705774	13.347559
21.053859	886.373870	13.352563
20.743003	883.043776	13.357568
21.007980	882.985672	13.362573
20.914567	889.393828	13.367578
20.975371	880.459577	13.372583
20.765404	888.316700	13.377587
20.779270	893.761522	13.382592
20.897440	892.884692	13.387597
20.632412	897.826764	13.392602
20.632527	888.337606	13.397607
20.784499	899.150736	13.402611
20.704223	894.288827	13.407616
21.053671	889.588629	13.412621
20.880262	897.558204	13.417626
21.053641	893.206227	13.422631
20.869374	897.892553	13.427635
20.786660	899.190965	13.432640
21.027266	889.188759	13.437645
21.047281	902.585633	13.442650
21.041211	888.899370	13.447655
21.084579	902.683626	13.452659
20.931420	900.940115	13.457664
21.111623	896.115513	13.462669
21.010942	892.567381	13.467674
21.131267	893.360296	13.472679
20.747040	901.289376	13.477683
20.985406	898.379490	13.482688
21.160814	898.353019	13.487693
20.968370	900.627774	13.492698
20.781445	898.241484	13.497703
20.840124	908.561693	13.502707
20.898997	903.786403	13.507712
21.415878	897.025112	13.512717
21.223872	903.568855	13.517722
21.082149	893.132434	13.522727
20.880691	880.694819	13.527731
20.861756	872.933993	13.532736
20.876850	876.519282	13.537741
20.957345	890.788065	13.542746
20.938631	886.392606	13.547751
20.863249	891.383281	13.552755
21.097431	893.580529	13.557760
20.946189	881.532319	13.562765
20.796401	880.848046	13.567770
21.057585	885.304041	13.572775
20.956347	873.965416	13.577779
20.719452	868.351014	13.582784
20.976272	883.118398	13.587789
20.998515	898.073030	13.592794
21.141429	880.674308	13.597799
20.872886	871.205932	13.602803
20.858346	869.120177	13.607808
20.904373	864.074121	13.612813
20.926888	878.617082	13.617818
21.359985	874.222111	13.622823
20.901917	870.685251	13.627827
20.732556	865.121583	13.632832
20.889467	863.519445	13.637837
20.606493	870.981326	13.642842
21.135677	872.713604	13.647847
20.956507	875.844149	13.652851
21.015999	882.466048	13.657856
21.261732	864.694535	13.662861
20.888896	868.933085	13.667866
20.627997	865.150302	13.672871
20.909961	865.256655	13.677875
21.010699	861.189101	13.682880
20.692343	861.823309	13.687885
20.586325	879.928803	13.692890
21.184349	889.601551	13.697895
20.885220	900.571789	13.702899
21.148417	900.744218	13.707904
21.363000	891.933675	13.712909
20.961740	880.032581	13.717914
21.156865	871.100568	13.722919
21.082939	876.351217	13.727923
20.951118	871.880757	13.732928
21.175188	868.430655	13.737933
20.994789	868.490897	13.742938
21.192481	870.470021	13.747943
21.230229	870.568014	13.752947
21.221558	871.924003	13.757952
21.415656	865.781943	13.762957
21.174568	864.050884	13.767962
21.181579	855.215119	13.772967
20.797814	851.343120	13.777971
21.073758	842.068634	13.782976
21.106590	838.513414	13.787981
20.892845	843.459905	13.792986
20.571723	844.583435	13.797991
20.937547	847.139746	13.802995
20.602612	856.858764	13.808000
21.144145	855.914413	13.813005
21.167071	866.134632	13.818010
21.028567	850.821521	13.823015
20.703930	846.168921	13.828019
20.769993	856.402755	13.833024
21.374500	864.886942	13.838029
21.077714	866.140641	13.843034
20.875106	850.511306	13.848039
20.703276	852.390083	13.853043
20.823984	846.433210	13.858048
20.959084	851.975382	13.863053
20.856634	872.075251	13.868058
21.026012	862.683700	13.873063
21.086353	856.919387	13.878067
21.079068	850.006739	13.883072
21.198291	847.535358	13.888077
20.875062	851.851151	13.893082
20.943482	849.879908	13.898087
20.626252	840.173298	13.903091
20.784219	846.836249	13.908096
20.838309	839.440706	13.913101
20.763695	851.903249	13.918106
21.057779	854.614514	13.923111
21.011166	871.521436	13.928115
20.654988	864.087230	13.933120
21.026708	862.644808	13.938125
20.842489	870.959887	13.943130
20.856031	870.728985	13.948135
21.021004	872.945153	13.953139
20.977886	875.921527	13.958144
21.053054	877.294109	13.963149
20.957030	885.191407	13.968154
21.073293	874.869979	13.973159
20.918872	868.871818	13.978163
21.017954	866.080352	13.983168
21.149273	847.748334	13.988173
20.869012	844.932215	13.993178
21.205005	842.117162	13.998183
20.808428	850.256353	14.003187
20.919914	850.872470	14.008192
20.756619	833.618988	14.013210
20.790281	844.678129	14.018227
21.008919	847.366075	14.023245
20.975856	848.798002	14.028263
20.694493	856.121148	14.033280
21.234175	863.269304	14.038298
21.194261	871.390794	14.043315
21.418736	868.927754	14.048333
20.983819	855.464385	14.053351
21.023413	857.535953	14.058368
21.026724	850.606218	14.063386
20.727104	854.835009	14.068403
21.159327	859.939651	14.073421
21.246183	872.832332	14.078439
21.260431	873.937392	14.083456
21.240951	874.473680	14.088474
20.908659	883.912808	14.093491
21.009773	872.742336	14.098509
21.234177	875.306672	14.103527
21.557522	880.519921	14.108544
21.178562	867.164021	14.113562
21.227978	876.499792	14.118579
21.553678	868.302688	14.123597
21.481340	876.338117	14.128615
21.140133	880.829950	14.133632
21.330439	883.385569	14.138650
20.982418	882.209330	14.143667
21.465586	877.792238	14.148685
21.338726	886.006254	14.153703
21.030290	878.984656	14.158720
21.468345	882.636480	14.163738
21.316777	885.226176	14.168755
21.334786	879.403062	14.173773
21.415894	872.707873	14.178791
21.097041	875.317956	14.183808
21.525793	900.447700	14.188826
21.784783	908.435022	14.193843
21.442130	917.576949	14.198861
21.867250	917.454018	14.203879
21.266839	919.750366	14.208896
21.394483	911.443254	14.213914
21.203821	911.752016	14.218931
21.415283	922.853645	14.223949
21.551790	918.342394	14.228967
21.464393	931.970779	14.233984
21.801620	929.684801	14.239002
21.914572	921.493284	14.244019
21.787564	916.397999	14.249037
21.995038	923.701415	14.254055
21.935918	921.551012	14.259072
21.841656	917.282633	14.264090
21.721873	918.465702	14.269107
21.527187	926.100675	14.274125
21.875784	917.659218	14.279143
21.620092	925.454931	14.284160
21.737546	923.974788	14.289178
21.921646	932.246200	14.294195
22.100303	936.460081	14.299213
21.982219	923.993751	14.304231
21.620396	933.884359	14.309248
22.464691	933.488507	14.314266
22.116238	945.264620	14.319283
21.812393	931.283200	14.324301
22.157050	933.735558	14.329319
22.089573	945.477869	14.334336
22.348705	944.640517	14.339354
22.167528	940.417454	14.344371
22.026814	931.483023	14.349389
22.266429	928.227900	14.354407
21.830310	932.576011	14.359424
21.990127	943.190390	14.364442
22.148962	950.371016	14.369459
22.018126	955.996505	14.374477
22.317557	945.772769	14.379495
22.201351	956.297474	14.384512
22.177205	960.211798	14.389530
22.168324	953.301263	14.394547
22.429865	951.274318	14.399565
22.565823	950.057062	14.404583
22.283357	959.046271	14.409600
22.778456	953.784111	14.414618
22.568129	949.436707	14.419635
22.216171	961.600356	14.424653
22.383005	946.820259	14.429671
22.146171	955.567807	14.434688
22.244106	955.366498	14.439706
22.131964	962.195519	14.444723
22.203640	953.798208	14.449741
22.398938	953.715078	14.454759
22.035663	969.493782	14.459776
22.386207	976.560475	14.464794
22.506035	988.708676	14.469811
22.710558	993.104065	14.474829
22.887162	980.744843	14.479847
22.464888	986.259523	14.484864
22.663357	992.444413	14.489882
22.777969	990.351234	14.494899
22.743027	990.938756	14.499917
23.065217	975.761044	14.504935
22.872747	993.568480	14.509952
23.389407	981.479066	14.514970
23.005700	975.307850	14.519987
22.448766	964.624506	14.525005
22.981704	974.620974	14.530023
22.711923	986.535583	14.535040
23.112625	991.426648	14.540058
23.227628	988.741948	14.545075
23.117902	967.301685	14.550093
23.330409	954.680355	14.555111
22.727834	965.166234	14.560128
23.000588	955.994383	14.565146
22.842063	956.818692	14.570163
22.749987	962.771483	14.575181
23.022166	958.161503	14.580199
22.893746	962.584816	14.585216
23.270627	970.352022	14.590234
22.972147	967.923609	14.595251
22.749660	977.077868	14.600269
23.373720	984.347908	14.605287
23.015744	1000.704674	14.610304
23.188975	997.148664	14.615322
23.536754	988.724601	14.620339
23.292225	993.134981	14.625357
23.212297	980.679820	14.630375
23.202840	988.175171	14.635392
23.422785	988.890355	14.640410
23.397123	986.487640	14.645427
23.106455	985.756850	14.650445
23.358800	975.520154	14.655463
23.446228	985.089034	14.660480
23.437308	983.157131	14.665498
23.460834	981.278256	14.670515
23.128340	984.862665	14.675533
23.429044	985.017555	14.680551
23.304736	993.053472	14.685568
23.443293	989.130185	14.690586
23.706295	988.584797	14.695603
23.338453	987.902496	14.700621
23.716939	989.547224	14.705639
23.468737	993.369877	14.710656
23.432801	990.540935	14.715674
23.541978	985.610877	14.720691
23.354791	999.104230	14.725709
23.714889	980.628112	14.730727
23.794085	987.904829	14.735744
23.519394	990.031260	14.740762
23.607904	991.808754	14.745779
23.584627	995.636432	14.750797
23.810208	987.812307	14.755815
23.769030	990.466213	14.760832
23.513276	997.118381	14.765850
23.518126	982.935092	14.770867
23.224245	995.684113	14.775885
23.342674	989.037974	14.780903
23.581949	1004.758367	14.785920
23.714812	1004.540475	14.790938
23.877775	1012.853058	14.795955
23.928161	1021.951240	14.800973
23.996949	1014.240198	14.805991
23.825464	1011.322759	14.811008
23.928980	1026.043929	14.816026
23.888007	1012.391741	14.821043
23.902404	1013.271844	14.826061
23.910885	1005.889751	14.831079
24.115458	1015.133225	14.836096
23.849827	1015.834620	14.841114
24.106365	1020.163520	14.846131
23.766636	1019.945497	14.851149
23.982177	1008.879367	14.856167
23.871825	1024.065656	14.861184
24.205321	1028.673295	14.866202
24.657505	1041.691905	14.871219
24.063977	1034.770756	14.876237
24.008712	1032.929609	14.881255
24.200700	1042.787019	14.886272
24.378107	1040.287412	14.891290
24.369603	1045.108480	14.896307
24.314691	1046.422786	14.901325
24.308666	1046.256933	14.906343
24.590030	1046.191537	14.911360
24.343752	1054.478177	14.916378
24.655866	1034.888068	14.921395
24.637140	1035.510759	14.926413
24.358102	1025.766195	14.931431
24.239946	1024.479349	14.936448
24.495579	1037.562337	14.941466
24.579753	1045.911100	14.946483
24.602888	1048.315657	14.951501
24.993669	1041.180888	14.956519
24.471873	1038.761337	14.961536
24.563051	1030.345142	14.966554
24.614474	1023.108775	14.971571
24.655923	1037.135136	14.976589
24.617322	1034.652679	14.981607
24.859160	1047.722145	14.986624
24.632128	1040.382315	14.991642
24.740946	1035.998141	14.996659
24.442207	1047.489553	15.001677
24.880902	1039.117028	15.006695
25.144761	1039.738694	15.011712
24.944609	1051.956859	15.016730
25.003733	1039.202615	15.021747
24.667432	1043.629220	15.026765
24.916440	1034.763130	15.031783
25.038103	1042.904564	15.036800
25.251874	1040.676012	15.041818
25.100622	1010.791961	15.046835
24.654933	1019.783644	15.051853
24.896942	1025.212840	15.056871
24.868499	1034.405401	15.061888
24.501784	1045.544282	15.066906
24.950358	1036.967261	15.071923
24.911961	1045.247482	15.076941
24.858710	1037.894094	15.081959
24.979877	1043.097177	15.086976
24.931970	1042.411037	15.091994
25.300362	1037.211529	15.097011
25.022232	1045.773806	15.102029
25.066441	1039.625550	15.107047
25.243181	1043.059542	15.112064
24.839233	1045.401653	15.117082
25.235684	1059.204674	15.122099
25.162461	1069.809122	15.127117
25.335838	1079.568851	15.132135
25.353097	1081.035246	15.137152
25.057634	1072.797097	15.142170
24.962949	1059.323319	15.147187
25.062011	1059.878461	15.152205
25.130664	1073.288606	15.157223
25.408711	1063.486628	15.162240
25.502537	1074.437247	15.167258
25.695233	1072.152276	15.172275
25.493167	1065.123060	15.177293
25.673590	1069.129057	15.182311
25.732389	1075.323674	15.187328
25.473702	1066.728875	15.192346
25.684845	1058.641172	15.197363
25.634577	1067.683077	15.202381
25.633311	1065.227693	15.207399
25.735484	1057.379169	15.212416
25.632444	1072.558050	15.217434
25.536826	1065.419046	15.222451
25.624766	1058.219310	15.227469
25.716991	1070.364117	15.232487
25.695954	1058.494106	15.237504
25.800076	1072.298145	15.242522
26.112667	1066.755165	15.247539
25.927910	1065.488376	15.252557
25.830928	1071.489186	15.257575
25.973491	1068.881873	15.262592
25.768506	1069.965284	15.267610
26.034779	1062.010360	15.272627
25.816279	1078.650138	15.277645
25.620260	1080.913473	15.282663
25.951739	1084.892237	15.287680
26.109707	1100.776713	15.292698
26.544868	1096.537103	15.297715
25.872326	1088.744480	15.302733
26.264011	1090.088237	15.307751
26.228389	1075.709964	15.312768
26.029435	1086.109532	15.317786
26.306358	1086.626869	15.322803
26.261794	1073.492727	15.327821
26.154238	1075.828469	15.332839
26.390826	1074.709986	15.337856
26.223932	1070.984833	15.342874
26.517796	1079.053204	15.347891
26.480641	1071.917458	15.352909
26.176418	1073.258945	15.357927
26.602015	1058.901511	15.362944
26.623219	1067.924152	15.367962
26.728355	1059.277623	15.372979
26.404371	1068.411947	15.377997
26.240236	1059.275104	15.383015
26.518133	1063.238812	15.388032
26.151189	1075.946071	15.393050
26.323993	1066.892339	15.398067
26.413262	1069.983209	15.403085
26.837335	1088.696028	15.408103
26.683164	1074.303630	15.413120
26.231363	1074.092469	15.418138
26.647631	1087.404714	15.423155
27.002029	1089.882289	15.428173
26.843000	1086.541272	15.433191
26.726404	1071.814118	15.438208
26.451541	1076.652509	15.443226
26.713592	1082.479655	15.448243
26.557191	1096.073582	15.453261
26.834791	1101.718929	15.458279
27.141696	1091.259517	15.463296
27.017647	1098.899045	15.468314
26.754348	1091.135533	15.473331
26.963282	1083.936936	15.478349
26.738416	1088.072072	15.483367
27.088660	1096.844050	15.488384
26.922931	1098.732892	15.493402
27.233978	1094.303862	15.498419
27.106854	1078.302643	15.503437
26.894148	1080.008638	15.508455
27.299017	1089.679543	15.513472
26.690104	1082.672733	15.518490
27.244871	1094.072102	15.523507
27.120208	1095.257536	15.528525
27.030307	1097.909794	15.533543
27.037810	1094.471429	15.538560
27.031251	1101.266372	15.543578
27.310478	1092.143741	15.548595
27.310615	1094.943661	15.553613
26.824341	1091.595060	15.558631
27.215794	1099.446530	15.563648
27.143805	1105.718649	15.568666
27.187368	1101.779022	15.573683
27.274373	1094.768182	15.578701
27.232228	1098.883618	15.583719
27.280776	1096.005002	15.588736
27.226786	1111.915430	15.593754
27.131277	1099.687597	15.598771
27.251148	1106.857213	15.603789
27.192534	1126.084370	15.608807
27.517265	1125.529132	15.613824
27.856674	1127.343706	15.618842
27.704470	1127.194874	15.623859
27.811055	1128.658039	15.628877
27.933126	1130.035363	15.633895
27.830795	1126.911813	15.638912
27.826990	1119.690498	15.643930
27.650700	1104.360917	15.648947
27.846272	1106.335283	15.653965
27.681443	1098.247746	15.658983
27.859977	1103.891591	15.664000
27.983343	1109.457720	15.669018
27.714333	1099.272628	15.674035
27.935180	1090.019308	15.679053
27.667028	1092.067631	15.684071
27.890689	1106.849947	15.689088
27.772183	1114.700959	15.694106
27.950554	1118.131563	15.699123
28.082861	1119.993324	15.704141
27.969959	1127.966148	15.709159
28.232388	1109.848367	15.714176
28.165190	1117.472545	15.719194
27.928944	1113.009673	15.724211
28.041399	1109.271418	15.729229
27.901147	1116.850617	15.734247
28.344731	1117.081823	15.739264
28.144702	1120.494126	15.744282
28.443403	1112.628385	15.749299
28.352857	1102.721570	15.754317
28.074124	1119.570778	15.759335
28.491049	1109.749766	15.764352
28.352639	1108.385917	15.769370
28.405155	1101.956308	15.774387
28.468871	1088.399038	15.779405
28.123690	1100.114977	15.784423
28.581723	1096.911500	15.789440
28.259025	1096.708062	15.794458
28.514863	1097.187864	15.799475
28.475332	1101.033893	15.804493
28.076074	1111.020254	15.809511
28.426436	1112.235323	15.814528
28.251440	1119.551074	15.819546
27.798923	1116.725626	15.824563
28.048303	1119.606924	15.829581
28.528994	1122.674704	15.834599
28.933519	1124.261812	15.839616
28.837423	1121.535249	15.844634
28.447964	1104.367743	15.849651
28.729808	1113.430641	15.854669
28.605215	1134.194185	15.859687
28.759316	1141.179031	15.864704
28.844233	1142.253964	15.869722
29.001990	1147.389900	15.874739
28.813467	1140.748602	15.879757
29.083361	1153.154583	15.884775
29.254958	1126.248494	15.889792
28.880014	1128.919477	15.894810
28.425402	1121.883320	15.899827
28.318026	1130.094365	15.904845
28.707943	1140.280502	15.909863
28.872176	1138.064556	15.914880
28.734614	1144.027822	15.919898
29.098780	1139.096370	15.924915
28.909601	1142.061776	15.929933
28.617964	1145.240154	15.934951
29.102153	1149.163119	15.939968
28.847447	1170.207018	15.944986
29.112452	1170.334570	15.950003
29.526605	1167.180549	15.955021
29.398714	1168.331897	15.960039
29.538165	1166.755411	15.965056
29.518626	1169.840060	15.970074
29.446667	1162.530492	15.975091
29.475861	1154.525238	15.980109
29.317756	1142.398589	15.985127
29.647553	1136.635759	15.990144
29.278708	1137.446430	15.995162
29.035578	1137.260189	16.000179
29.406760	1136.463159	16.005197
29.608208	1162.759059	16.010215
29.518389	1172.667795	16.015232
29.935325	1171.449754	16.020250
29.668373	1174.134983	16.025267
29.779725	1181.911618	16.030285
29.783124	1172.387755	16.035303
29.900168	1150.624759	16.040320
29.778182	1142.829242	16.045338
29.553232	1143.395164	16.050355
29.764993	1135.609345	16.055373
29.770544	1151.124925	16.060391
29.610583	1159.034483	16.065408
30.001544	1165.182455	16.070426
29.752342	1170.502856	16.075443
29.851245	1171.304997	16.080461
29.939474	1172.283448	16.085479
30.153802	1166.762395	16.090496
30.141159	1169.240320	16.095514
29.811283	1170.063654	16.100531
30.098626	1165.879060	16.105549
29.493776	1169.920664	16.110567
29.666036	1170.309977	16.115584
30.152205	1171.237546	16.120602
29.902756	1163.397852	16.125619
29.985207	1168.210746	16.130637
29.825445	1175.818257	16.135655
30.022458	1167.001278	16.140672
30.200771	1169.293016	16.145690
29.819437	1175.490232	16.150707
30.531750	1183.208775	16.155725
30.569018	1198.651706	16.160743
30.495104	1193.072793	16.165760
30.363932	1175.818389	16.170778
30.365218	1179.338600	16.175795
30.284845	1183.546674	16.180813
30.548752	1197.646252	16.185831
30.452505	1196.374773	16.190848
30.730609	1198.807905	16.195866
30.695188	1197.655715	16.200883
30.696940	1190.628538	16.205901
30.589108	1178.611820	16.210919
30.360299	1173.947965	16.215936
30.582002	1185.551538	16.220954
30.365396	1194.388812	16.225971
30.766106	1188.230827	16.230989
30.501136	1203.906014	16.236007
30.724192	1199.926723	16.241024
30.996813	1189.751139	16.246042
30.701241	1192.731949	16.251059
31.012227	1197.020758	16.256077
30.878546	1194.639955	16.261095
30.956154	1206.790354	16.266112
31.345136	1198.719829	16.271130
30.870434	1199.961099	16.276147
30.963064	1194.273825	16.281165
30.928056	1208.490300	16.286183
31.256417	1228.288243	16.291200
31.429401	1228.814298	16.296218
31.161611	1238.916634	16.301235
31.020493	1213.351739	16.306253
31.295190	1197.571026	16.311271
31.210230	1186.581003	16.316288
31.130374	1171.547434	16.321306
31.138069	1188.736437	16.326323
31.316046	1187.847521	16.331341
31.121175	1189.590009	16.336359
31.090579	1189.739538	16.341376
31.297553	1191.672771	16.346394
31.081214	1200.104159	16.351411
31.395243	1186.248894	16.356429
31.463604	1196.415568	16.361447
31.056007	1194.415085	16.366464
31.286924	1203.133798	16.371482
31.211505	1198.604350	16.376499
31.550795	1196.922056	16.381517
31.352772	1197.287053	16.386535
31.487908	1194.868096	16.391552
31.438783	1198.484442	16.396570
31.366702	1214.736076	16.401587
31.609051	1215.977819	16.406605
31.677670	1224.524225	16.411623
31.491217	1224.583778	16.416640
32.039360	1215.290764	16.421658
31.749532	1225.560203	16.426675
31.759489	1217.174157	16.431693
31.805932	1228.560321	16.436711
31.654950	1227.783643	16.441728
31.865298	1225.835614	16.446746
31.343008	1225.352541	16.451763
31.759495	1222.364880	16.456781
31.856337	1225.061311	16.461799
31.637876	1223.170661	16.466816
31.917740	1236.474911	16.471834
32.002736	1253.428288	16.476851
32.300830	1256.339598	16.481869
32.344077	1254.111469	16.486887
32.005589	1256.900932	16.491904
32.812397	1254.348100	16.496922
32.015007	1237.575838	16.501939
31.797235	1240.792793	16.506957
32.116733	1245.723640	16.511975
32.022399	1251.395331	16.516992
32.352715	1246.088563	16.522010
32.313318	1265.724981	16.527027
32.640994	1254.574712	16.532045
32.557617	1259.640605	16.537063
32.374710	1260.478257	16.542080
32.552887	1253.138188	16.547098
32.613714	1259.957066	16.552115
32.062186	1249.632877	16.557133
32.553310	1245.527448	16.562151
32.521378	1248.931848	16.567168
32.600535	1246.433719	16.572186
32.548527	1255.649055	16.577203
32.672956	1247.307657	16.582221
32.663127	1247.982422	16.587239
32.278209	1257.139166	16.592256
32.481437	1246.293476	16.597274
32.544447	1252.265696	16.602291
32.904836	1270.296762	16.607309
33.025753	1267.277579	16.612327
32.634529	1277.374459	16.617344
32.750621	1275.512244	16.622362
32.730856	1283.860417	16.627379
32.941442	1276.633148	16.632397
33.178898	1270.527908	16.637415
33.094480	1278.400313	16.642432
33.262423	1270.572646	16.647450
33.169821	1273.620205	16.652467
33.082632	1274.617202	16.657485
33.262010	1280.223228	16.662503
33.021441	1278.606663	16.667520
33.357912	1270.129185	16.672538
33.178217	1279.632320	16.677555
33.267627	1272.674496	16.682573
33.425426	1275.293573	16.687591
33.218578	1276.721796	16.692608
33.330533	1268.825979	16.697626
33.229153	1270.407271	16.702643
32.982263	1275.906670	16.707661
33.395300	1273.231016	16.712679
33.303751	1280.835567	16.717696
33.828995	1271.796286	16.722714
33.480769	1274.570002	16.727731
33.566535	1274.362765	16.732749
33.558857	1271.779378	16.737767
33.426776	1280.504120	16.742784
33.501123	1272.990261	16.747802
33.777300	1285.735135	16.752819
33.825069	1291.423505	16.757837
33.748849	1284.413437	16.762855
33.747231	1296.025974	16.767872
33.862850	1297.342994	16.772890
33.506380	1300.303650	16.777907
33.865737	1301.446514	16.782925
33.921670	1303.377109	16.787943
33.698746	1299.630945	16.792960
34.218296	1299.222387	16.797978
33.998259	1308.327698	16.802995
33.622965	1304.126048	16.808013
33.922256	1297.845763	16.813031
33.939284	1305.815265	16.818048
34.335458	1294.241899	16.823066
33.720618	1297.396349	16.828083
33.919471	1307.948139	16.833101
34.280050	1301.090202	16.838119
33.848922	1307.658792	16.843136
33.881603	1307.906771	16.848154
34.495151	1312.729395	16.853171
34.489723	1325.192018	16.858189
34.505482	1316.628806	16.863207
34.254146	1309.173162	16.868224
34.555453	1308.453337	16.873242
34.558293	1308.389890	16.878259
34.592653	1303.632109	16.883277
34.820450	1285.098054	16.888295
34.629773	1295.241614	16.893312
34.484846	1291.437393	16.898330
34.564691	1289.129488	16.903347
34.596430	1294.496365	16.908365
34.719482	1298.088422	16.913383
34.721372	1304.385025	16.918400
34.923570	1311.102727	16.923418
34.765371	1311.411037	16.928435
34.814187	1315.512027	16.933453
34.776202	1318.244137	16.938471
34.558568	1328.627979	16.943488
34.757041	1321.301943	16.948506
34.838354	1317.999622	16.953523
35.029714	1322.681937	16.958541
34.953430	1329.302485	16.963559
34.747150	1328.635298	16.968576
34.917111	1318.984098	16.973594
34.890841	1328.572910	16.978611
34.921919	1321.407282	16.983629
35.286381	1308.670174	16.988647
35.305075	1320.266907	16.993664
35.192972	1313.485923	16.998682
35.357890	1318.858311	17.003699
34.885780	1330.915584	17.008717
35.037135	1316.231965	17.013735
35.093811	1333.034218	17.018752
35.301919	1341.871487	17.023770
35.165316	1353.754143	17.028787
35.181324	1348.503758	17.033805
35.534078	1351.046138	17.038823
35.062203	1352.902038	17.043840
35.501129	1344.233567	17.048858
35.765063	1354.617706	17.053875
35.646692	1348.718624	17.058893
35.943375	1346.396577	17.063911
35.724932	1346.930007	17.068928
35.600093	1345.910047	17.073946
35.728546	1353.624271	17.078963
35.603251	1353.294960	17.083981
35.762987	1346.832412	17.088999
35.863357	1347.878155	17.094016
36.006762	1348.934337	17.099034
36.187315	1345.384941	17.104051
36.073997	1350.285749	17.109069
36.064294	1347.078163	17.114087
36.056612	1346.961336	17.119104
35.919804	1340.697100	17.124122
36.113702	1336.613881	17.129139
36.098653	1339.045026	17.134157
36.135910	1333.591478	17.139175
36.268203	1349.022559	17.144192
36.048853	1348.469143	17.149210
36.135248	1344.851391	17.154227
36.078262	1346.840901	17.159245
36.387670	1338.775125	17.164263
35.998811	1355.115190	17.169280
35.848129	1356.337829	17.174298
36.240886	1353.641799	17.179315
36.377600	1379.602342	17.184333
36.678046	1372.810592	17.189351
36.631274	1385.163453	17.194368
36.471991	1380.959578	17.199386
36.814609	1374.256273	17.204403
36.803727	1378.987378	17.209421
37.060599	1361.931209	17.214439
36.489934	1351.043693	17.219456
36.443444	1349.433921	17.224474
36.666619	1358.824090	17.229491
36.673571	1378.369110	17.234509
36.856635	1372.246547	17.239527
36.822457	1377.821388	17.244544
36.671908	1380.072010	17.249562
36.789269	1375.062649	17.254579
36.857624	1370.477969	17.259597
36.930514	1372.558457	17.264615
36.891465	1369.517573	17.269632
37.182411	1380.813737	17.274650
36.999027	1373.750715	17.279667
36.665000	1372.224551	17.284685
36.722891	1367.499178	17.289703
37.016054	1372.975406	17.294720
36.871929	1374.104189	17.299738
37.053371	1375.361167	17.304755
37.159082	1395.385976	17.309773
37.429997	1397.659836	17.314791
37.392388	1399.820874	17.319808
37.434298	1409.464149	17.324826
37.446591	1396.308849	17.329843
37.435717	1394.875867	17.334861
37.676568	1392.252036	17.339879
37.756841	1390.528444	17.344896
37.242582	1386.455114	17.349914
37.417644	1378.923565	17.354931
37.620242	1394.884619	17.359949
37.651062	1379.496546	17.364967
37.690718	1387.633949	17.369984
37.658030	1394.643202	17.375002
37.995567	1389.490179	17.380019
37.570971	1394.756833	17.385037
38.102967	1386.588676	17.390055
38.060292	1386.580466	17.395072
38.036555	1389.871904	17.400090
38.048329	1384.884884	17.405107
37.933254	1392.445267	17.410125
37.805281	1388.787758	17.415143
38.007998	1392.264884	17.420160
38.016910	1396.535073	17.425178
38.040123	1386.521830	17.430195
37.985799	1391.859996	17.435213
38.137763	1393.485056	17.440231
38.015950	1390.337814	17.445248
37.782252	1394.291967	17.450266
37.998061	1385.316126	17.455283
38.121512	1398.151526	17.460301
38.361804	1390.224164	17.465319
38.483595	1395.732451	17.470336
38.443540	1395.445389	17.475354
38.493741	1388.837478	17.480371
38.174388	1406.907909	17.485389
38.470095	1396.229048	17.490407
38.261269	1401.872652	17.495424
38.231837	1401.487152	17.500442
38.516918	1413.061137	17.505459
38.549050	1406.760491	17.510477
38.284370	1418.280582	17.515495
38.483761	1419.415934	17.520512
38.202204	1417.132612	17.525530
38.647210	1407.880309	17.530547
38.539185	1417.062994	17.535565
38.490906	1432.929604	17.540583
39.035544	1443.755906	17.545600
38.837933	1442.249665	17.550618
38.797742	1442.168697	17.555635
38.814855	1438.937151	17.560653
38.972748	1443.885188	17.565671
39.079052	1444.557957	17.570688
39.298860	1439.369422	17.575706
39.643763	1434.137341	17.580723
39.033621	1444.900053	17.585741
39.080034	1441.570235	17.590759
39.515132	1438.721928	17.595776
39.300204	1437.610932	17.600794
39.724595	1438.681299	17.605811
39.503842	1436.552664	17.610829
39.727061	1432.349907	17.615847
39.618747	1440.739035	17.620864
39.207370	1449.347967	17.625882
39.623057	1438.995232	17.630899
39.801407	1432.638220	17.635917
39.467610	1433.213646	17.640935
39.573230	1434.923183	17.645952
39.556289	1438.989862	17.650970
39.803178	1427.224689	17.655987
39.681630	1437.207880	17.661005
39.852060	1436.698479	17.666023
40.160536	1433.750026	17.671040
39.663185	1443.419550	17.676058
39.874589	1431.276988	17.681075
39.818810	1441.280368	17.686093
39.334469	1434.930727	17.691111
39.648465	1438.381464	17.696128
39.734332	1433.106536	17.701146
39.849176	1433.145566	17.706163
39.529489	1438.181565	17.711181
39.969083	1448.209769	17.716199
40.095278	1464.274324	17.721216
39.820453	1470.243097	17.726234
40.177554	1457.604565	17.731251
40.258644	1465.720459	17.736269
40.135142	1466.359878	17.741287
40.450741	1460.002202	17.746304
40.326311	1465.738554	17.751322
40.322492	1463.458909	17.756339
40.059469	1467.542033	17.761357
40.237871	1468.488820	17.766375
40.424439	1454.603291	17.771392
40.395974	1465.056952	17.776410
40.589232	1487.793291	17.781427
40.312263	1495.779896	17.786445
40.691121	1498.167123	17.791463
40.893923	1491.677980	17.796480
40.820517	1496.394712	17.801498
40.940882	1497.913922	17.806515
40.590287	1505.478103	17.811533
40.752700	1499.890483	17.816551
40.899858	1496.498966	17.821568
40.755973	1491.106497	17.826586
41.083034	1489.532304	17.831603
41.170883	1487.408716	17.836621
40.914243	1494.122599	17.841639
41.169494	1490.608447	17.846656
41.055857	1482.451967	17.851674
41.121622	1490.408291	17.856691
41.024342	1493.151463	17.861709
41.328188	1492.299873	17.866727
41.466558	1480.076106	17.871744
40.782068	1489.038516	17.876762
41.514307	1485.115586	17.881779
41.426167	1486.314890	17.886797
41.479047	1480.571708	17.891815
41.590494	1485.759983	17.896832
41.214805	1489.505564	17.901850
41.616649	1490.294016	17.906867
41.722916	1494.717029	17.911885
41.552293	1491.689237	17.916903
41.434470	1483.722194	17.921920
41.323000	1504.273378	17.926938
41.742335	1516.705391	17.931955
41.578881	1518.811796	17.936973
41.561516	1523.521173	17.941991
41.741479	1520.876354	17.947008
41.716357	1520.111835	17.952026
41.992320	1517.212598	17.957043
41.957720	1518.503257	17.962061
42.109317	1519.462974	17.967079
42.424829	1512.013567	17.972096
42.101560	1516.313959	17.977114
41.988793	1515.451730	17.982131
41.980553	1517.409106	17.987149
42.113341	1516.104217	17.992167
42.068998	1511.238580	17.997184
41.823083	1515.235615	18.002202
42.183905	1525.269357	18.007219
42.148944	1539.412213	18.012237
42.227142	1554.372348	18.017255
42.129369	1543.097009	18.022272
42.157684	1545.039907	18.027290
42.225574	1551.009113	18.032307
42.497482	1545.640763	18.037325
42.326129	1551.100689	18.042343
42.442331	1540.472375	18.047360
42.612227	1545.699329	18.052378
42.867475	1563.113574	18.057395
42.541732	1555.165493	18.062413
42.866386	1579.394334	18.067431
43.318797	1568.791035	18.072448
43.021612	1554.485464	18.077466
42.859313	1552.378164	18.082483
42.945581	1544.037964	18.087501
42.849340	1567.353875	18.092519
43.143359	1569.093159	18.097536
43.060654	1575.592929	18.102554
43.010494	1575.849405	18.107571
43.299247	1567.109581	18.112589
43.352900	1579.884698	18.117607
43.483143	1563.979544	18.122624
43.539201	1571.880043	18.127642
43.264217	1559.621454	18.132659
43.384748	1551.048474	18.137677
43.729422	1562.174969	18.142695
43.358253	1541.836604	18.147712
43.494954	1545.679814	18.152730
43.406535	1541.148398	18.157747
43.447190	1545.313678	18.162765
43.201078	1568.063584	18.167783
43.477561	1559.457861	18.172800
43.335224	1566.480751	18.177818
43.247769	1577.716290	18.182835
43.310350	1569.579635	18.187853
43.251161	1569.980703	18.192871
43.495419	1579.438444	18.197888
43.645816	1590.831909	18.202906
43.520806	1590.058147	18.207923
44.038194	1594.216627	18.212941
44.082778	1604.735033	18.217959
44.302595	1602.006762	18.222976
44.351948	1599.147582	18.227994
44.200941	1600.846941	18.233011
44.363504	1603.651731	18.238029
44.215646	1601.811906	18.243047
44.245001	1600.949815	18.248064
44.013045	1599.788037	18.253082
44.319270	1597.802646	18.258099
44.472926	1585.802878	18.263117
44.149291	1601.724597	18.268135
44.587260	1592.091039	18.273152
44.465005	1598.216437	18.278170
44.542888	1591.507275	18.283187
44.258111	1591.621836	18.288205
44.032569	1599.198370	18.293223
44.414096	1601.250906	18.298240
44.720805	1608.379175	18.303258
44.553916	1611.992381	18.308275
45.066319	1616.325490	18.313293
44.520119	1621.226995	18.318311
45.034753	1624.640274	18.323328
44.936557	1617.693328	18.328346
44.884797	1626.525022	18.333363
45.316356	1617.992853	18.338381
44.841472	1621.895079	18.343399
44.951117	1618.743121	18.348416
44.942153	1621.797864	18.353434
44.756479	1616.957090	18.358451
45.114280	1626.658674	18.363469
44.999471	1626.425216	18.368487
45.202541	1619.539553	18.373504
45.241150	1623.115270	18.378522
44.856772	1621.553061	18.383539
45.443295	1646.482754	18.388557
45.426582	1648.973994	18.393575
45.560615	1648.248583	18.398592
45.336887	1648.151265	18.403610
45.288872	1642.695470	18.408627
45.741887	1658.259783	18.413645
45.406158	1664.199806	18.418663
45.746847	1656.763615	18.423680
45.600908	1650.782286	18.428698
45.618466	1657.950401	18.433715
45.916659	1652.145218	18.438733
45.637310	1658.798301	18.443751
45.658966	1648.682873	18.448768
45.479948	1654.675768	18.453786
45.517044	1669.157274	18.458803
46.250182	1671.295325	18.463821
46.145952	1677.179555	18.468839
46.198705	1681.475086	18.473856
46.607195	1679.600796	18.478874
46.138189	1680.741301	18.483891
46.309240	1676.843325	18.488909
46.508294	1680.967651	18.493927
46.740766	1671.377039	18.498944
46.417923	1652.865837	18.503962
46.405847	1652.022935	18.508979
46.687411	1636.959561	18.513997
46.205544	1647.742077	18.519015
46.357551	1654.239844	18.524032
46.395347	1675.045117	18.529050
46.399039	1679.843999	18.534067
46.720899	1676.327833	18.539085
46.709019	1677.647918	18.544103
46.424669	1669.726207	18.549120
46.804101	1670.040808	18.554138
46.615769	1671.683990	18.559155
46.729223	1668.916038	18.564173
47.014586	1673.938998	18.569191
46.667998	1670.486964	18.574208
47.001691	1679.807019	18.579226
46.392354	1690.529667	18.584243
46.890820	1702.453691	18.589261
47.033682	1696.967434	18.594279
47.248007	1701.336309	18.599296
47.615677	1697.325955	18.604314
47.569373	1696.659192	18.609331
47.700164	1697.158960	18.614349
47.658674	1695.350139	18.619367
47.813565	1695.020969	18.624384
47.863991	1683.153995	18.629402
47.432269	1675.789066	18.634419
47.903129	1672.942091	18.639437
47.552560	1657.057670	18.644455
47.794303	1665.417056	18.649472
48.075598	1655.687313	18.654490
47.686172	1659.301414	18.659507
47.569083	1650.211752	18.664525
47.880002	1659.585765	18.669543
47.725060	1669.703435	18.674560
48.026728	1675.867443	18.679578
48.017435	1675.728846	18.684595
48.162612	1685.195379	18.689613
48.180638	1689.195200	18.694631
47.991592	1695.609730	18.699648
48.089935	1696.049389	18.704666
48.063588	1700.831832	18.709683
48.085892	1689.735440	18.714701
48.053517	1691.344314	18.719719
48.071611	1696.471257	18.724736
48.455677	1695.925417	18.729754
47.926165	1700.131333	18.734771
47.990733	1690.218256	18.739789
48.375590	1693.395833	18.744807
48.271458	1695.437743	18.749824
48.586428	1707.290358	18.754842
48.640049	1718.886557	18.759859
48.640630	1725.938644	18.764877
48.743464	1730.649368	18.769895
48.579053	1730.501688	18.774912
48.626982	1728.570845	18.779930
48.487560	1728.707845	18.784947
48.636696	1726.024646	18.789965
48.730433	1729.752841	18.794983
48.270163	1726.259146	18.800000
48.734762	1727.980685	18.805018
49.062254	1747.935215	18.810035
49.452336	1741.969830	18.815053
49.739055	1740.026073	18.820071
49.365007	1742.480717	18.825088
49.275056	1719.344307	18.830106
49.255382	1722.628880	18.835123
49.536088	1738.408747	18.840141
49.611211	1742.038448	18.845159
49.660044	1728.894324	18.850176
49.783512	1713.418759	18.855194
49.451668	1720.840053	18.860211
49.420843	1709.026130	18.865229
49.571159	1725.475685	18.870247
49.446733	1733.652821	18.875264
49.871725	1737.553931	18.880282
49.546447	1742.410804	18.885299
49.528015	1740.122434	18.890317
49.884761	1732.983322	18.895335
49.789555	1747.341279	18.900352
49.811755	1742.556192	18.905370
49.558794	1748.592380	18.910387
49.768720	1741.174640	18.915405
50.037763	1754.938083	18.920423
50.159861	1768.611710	18.925440
50.526008	1768.152101	18.930458
50.357072	1772.395706	18.935475
50.160266	1774.564884	18.940493
50.253061	1776.030315	18.945511
50.538367	1772.538047	18.950528
50.452374	1763.091764	18.955546
50.184842	1775.207228	18.960563
50.195812	1765.286917	18.965581
50.472249	1772.770113	18.970599
50.532512	1777.995759	18.975616
50.708307	1770.610191	18.980634
50.621154	1771.535638	18.985651
50.560673	1765.273990	18.990669
50.389103	1761.202531	18.995687
50.634575	1773.764746	19.000704
50.848714	1783.346194	19.005722
50.695448	1795.842236	19.010739
50.856320	1801.220955	19.015757
51.166195	1797.422724	19.020775
51.129109	1796.324238	19.025792
51.213005	1792.815319	19.030810
51.396060	1799.043130	19.035827
51.007245	1788.178192	19.040845
51.633879	1792.985524	19.045863
51.465375	1792.880183	19.050880
51.650561	1790.956545	19.055898
51.439548	1798.651208	19.060915
51.375122	1797.136273	19.065933
51.670427	1789.573537	19.070951
51.163993	1799.403627	19.075968
51.576226	1786.958165	19.080986
51.563894	1790.192815	19.086003
51.406245	1793.330298	19.091021
51.681472	1802.650317	19.096039
51.484124	1797.024786	19.101056
52.047992	1791.104815	19.106074
51.778051	1798.249632	19.111091
51.883675	1809.814015	19.116109
52.165298	1806.984609	19.121127
51.797787	1819.214373	19.126144
52.044747	1815.988562	19.131162
52.139465	1826.849153	19.136179
52.152346	1818.956254	19.141197
52.620239	1813.246647	19.146215
52.092228	1822.536681	19.151232
52.513086	1817.947557	19.156250
52.347924	1820.159675	19.161267
51.953943	1819.580602	19.166285
52.231086	1818.616056	19.171303
52.020106	1825.029421	19.176320
52.055435	1837.270466	19.181338
52.219818	1842.255360	19.186355
52.324663	1851.307622	19.191373
52.756126	1845.419758	19.196391
52.425995	1856.386666	19.201408
53.015224	1845.273681	19.206426
52.534149	1857.282473	19.211443
52.583129	1863.607990	19.216461
53.298130	1871.134561	19.221479
53.092792	1887.455389	19.226496
53.041146	1878.882145	19.231514
53.029946	1876.709799	19.236531
53.039291	1880.327214	19.241549
53.351119	1873.578254	19.246567
53.422618	1874.086698	19.251584
53.454171	1872.360594	19.256602
53.376767	1880.662456	19.261619
53.239608	1878.593572	19.266637
53.380945	1869.275358	19.271655
53.320091	1872.192128	19.276672
53.607317	1871.952755	19.281690
53.489640	1871.131401	19.286707
53.341886	1872.808248	19.291725
53.305417	1874.465774	19.296743
53.366465	1895.732513	19.301760
53.762232	1907.016305	19.306778
53.955767	1908.445233	19.311795
53.937678	1920.402264	19.316813
54.546398	1909.302640	19.321831
54.312520	1906.102366	19.326848
54.413532	1902.504955	19.331866
54.131184	1903.829653	19.336883
54.208115	1903.494034	19.341901
54.228497	1901.464521	19.346919
53.972720	1908.062830	19.351936
54.182792	1907.817670	19.356954
54.256182	1905.463505	19.361971
54.205524	1905.237115	19.366989
54.574082	1904.832965	19.372007
54.340348	1911.258648	19.377024
54.390588	1900.907237	19.382042
54.972118	1905.164913	19.387059
54.805002	1900.487836	19.392077
54.464219	1901.744769	19.397095
54.453889	1915.483701	19.402112
54.412932	1920.248881	19.407130
54.731815	1928.657469	19.412147
54.469011	1937.287039	19.417165
54.796788	1927.297217	19.422183
54.913285	1931.005316	19.427200
55.252585	1944.168596	19.432218
55.260282	1953.975789	19.437235
55.263287	1972.122144	19.442253
55.300201	1959.811116	19.447271
55.310511	1964.427339	19.452288
55.309655	1967.502885	19.457306
55.519839	1956.016080	19.462323
55.213562	1965.289719	19.467341
55.502689	1957.254369	19.472359
55.655533	1958.809349	19.477376
55.457770	1956.263234	19.482394
55.292929	1960.445674	19.487411
55.401248	1956.854165	19.492429
55.452796	1961.751694	19.497447
55.294685	1979.119094	19.502464
55.501612	1982.412422	19.507482
55.949251	1977.872464	19.512499
55.672663	1990.155515	19.517517
55.959811	1988.812597	19.522535
55.908032	1993.975172	19.527552
56.451610	1994.213265	19.532570
56.341491	1990.550396	19.537587
56.431220	1990.515564	19.542605
56.381831	1982.211693	19.547623
56.282952	1988.592307	19.552640
56.418580	1980.545242	19.557658
56.521322	1990.328649	19.562675
56.526111	2004.540341	19.567693
56.705567	2013.771942	19.572711
56.659571	2022.477892	19.577728
56.690061	2018.670674	19.582746
56.825664	2010.661352	19.587763
56.850024	2017.373135	19.592781
57.013503	2020.045717	19.597799
56.714458	2017.125604	19.602816
56.823219	2019.020341	19.607834
57.107873	2015.306307	19.612851
56.668849	2023.880654	19.617869
57.230830	2014.699773	19.622887
56.919358	2014.609364	19.627904
57.118609	2012.307474	19.632922
57.199297	2008.741595	19.637939
57.079911	2020.349108	19.642957
57.236866	2015.677731	19.647975
57.350193	2037.729203	19.652992
57.727873	2037.054588	19.658010
58.160721	2046.324457	19.663027
57.378474	2038.366321	19.668045
57.480903	2035.088000	19.673063
57.506612	2039.755279	19.678080
57.587429	2045.839826	19.683098
57.561050	2044.513867	19.688115
57.561929	2051.114571	19.693133
57.645585	2033.208215	19.698151
57.720462	2048.293666	19.703168
57.761842	2061.214319	19.708186
58.386311	2064.429278	19.713203
58.046572	2077.627033	19.718221
58.186831	2081.024617	19.723239
58.163939	2081.799825	19.728256
57.688316	2081.827623	19.733274
58.133304	2080.086689	19.738291
57.877543	2082.957499	19.743309
58.528216	2090.772892	19.748327
58.107392	2106.222982	19.753344
58.143344	2111.369247	19.758362
58.829546	2103.506467	19.763379
58.428888	2113.013131	19.768397
58.676706	2109.736779	19.773415
58.887757	2109.250768	19.778432
58.659474	2104.945205	19.783450
59.058058	2100.909363	19.788467
58.960021	2102.317950	19.793485
59.103682	2112.870477	19.798503
59.380561	2120.945289	19.803520
59.513748	2112.908766	19.808538
59.667518	2098.299488	19.813555
59.283443	2093.752124	19.818573
59.443041	2091.233944	19.823591
59.676492	2092.499997	19.828608
59.385865	2096.505891	19.833626
59.747061	2092.510623	19.838643
59.377584	2095.379906	19.843661
59.656748	2081.533290	19.848679
59.348532	2093.729442	19.853696
59.266955	2097.274101	19.858714
59.664483	2109.607848	19.863731
59.630285	2118.897973	19.868749
59.910983	2119.957490	19.873767
60.129485	2130.336846	19.878784
60.056697	2132.870935	19.883802
60.184127	2124.943871	19.888819
59.671267	2132.154333	19.893837
60.041452	2118.232600	19.898855
60.025182	2120.048968	19.903872
59.727514	2127.338377	19.908890
60.202828	2127.654219	19.913907
60.315818	2145.297932	19.918925
60.409758	2156.115631	19.923943
60.428720	2151.317555	19.928960
60.431943	2151.904543	19.933978
60.620340	2158.672035	19.938995
60.263760	2150.612129	19.944013
60.428813	2155.829065	19.949031
60.696064	2155.113062	19.954048
60.726041	2160.698422	19.959066
60.956651	2162.580825	19.964083
60.870425	2184.244309	19.969101
61.099197	2179.065096	19.974119
61.093382	2182.271264	19.979136
61.136119	2180.831228	19.984154
61.087896	2176.910669	19.989171
60.978412	2185.816406	19.994189
61.158980	2176.142500	19.999207
61.501594	2179.387490	20.004224
61.193750	2178.707352	20.009242
61.515025	2177.363695	20.014259
61.318374	2180.503546	20.019277
61.380137	2189.617164	20.024295
61.664877	2195.634644	20.029312
61.759540	2205.358130	20.034330
61.719194	2207.964143	20.039347
61.606961	2217.341500	20.044365
61.729704	2202.981693	20.049383
62.069792	2202.671747	20.054400
61.608106	2216.021218	20.059418
62.056992	2205.932449	20.064435
61.677762	2211.262161	20.069453
62.067011	2233.691534	20.074471
62.418431	2235.904710	20.079488
62.086436	2242.276202	20.084506
62.434553	2238.418273	20.089523
62.390090	2239.876537	20.094541
62.211775	2238.615693	20.099559
62.431732	2239.413535	20.104576
62.293854	2237.188184	20.109594
62.549498	2241.757505	20.114611
62.520004	2237.765510	20.119629
62.388747	2245.199127	20.124647
62.803554	2257.213251	20.129664
62.563782	2255.535878	20.134682
62.523121	2257.386829	20.139699
62.948859	2263.915155	20.144717
62.658955	2259.430592	20.149735
62.957846	2251.394312	20.154752
62.940605	2266.989440	20.159770
63.331682	2275.577857	20.164787
63.424264	2287.225716	20.169805
63.594982	2287.557889	20.174823
63.580010	2284.946382	20.179840
63.723501	2288.380469	20.184858
63.683638	2284.099078	20.189875
63.956395	2277.511122	20.194893
63.913487	2277.845112	20.199911
64.092607	2269.138874	20.204928
63.620924	2274.241872	20.209946
63.869196	2266.599869	20.214963
63.989889	2282.423937	20.219981
64.061416	2279.207125	20.224999
64.469550	2277.955796	20.230016
64.368682	2284.880386	20.235034
64.301807	2278.451994	20.240051
64.448980	2282.461273	20.245069
64.231132	2284.482070	20.250087
64.594566	2278.346097	20.255104
64.271274	2291.214988	20.260122
64.360384	2284.742053	20.265139
64.435479	2284.735511	20.270157
64.083661	2280.520388	20.275175
64.326362	2285.013915	20.280192
64.276020	2284.302933	20.285210
64.722946	2288.274636	20.290227
64.652903	2307.567314	20.295245
64.352118	2317.101445	20.300263
64.907436	2315.604824	20.305280
64.602140	2314.743358	20.310298
64.525463	2314.551788	20.315315
64.767640	2327.224343	20.320333
65.037125	2337.905633	20.325351
65.414160	2344.395354	20.330368
65.013146	2349.487893	20.335386
65.192276	2346.923293	20.340403
65.234216	2347.924153	20.345421
65.295932	2347.266877	20.350439
65.655018	2351.416216	20.355456
65.922883	2368.245766	20.360474
65.952739	2356.787405	20.365491
66.046595	2348.047523	20.370509
65.591786	2337.418447	20.375527
65.839249	2342.085068	20.380544
65.728592	2362.609013	20.385562
65.991771	2359.463090	20.390579
66.233138	2368.444348	20.395597
66.082787	2364.189206	20.400615
66.319384	2366.860417	20.405632
66.603672	2360.040115	20.410650
66.443701	2366.668185	20.415667
66.135675	2360.091793	20.420685
66.066444	2370.770489	20.425703
66.243441	2362.824380	20.430720
66.177125	2370.316137	20.435738
66.493392	2356.886529	20.440755
66.425549	2383.921355	20.445773
66.125805	2390.642520	20.450791
66.726559	2394.158670	20.455808
66.499847	2405.911818	20.460826
66.495696	2402.903695	20.465843
67.194209	2407.223100	20.470861
66.857095	2425.024669	20.475879
66.850251	2428.558277	20.480896
67.169162	2435.740858	20.485914
67.375716	2423.628138	20.490931
67.392954	2431.288305	20.495949
67.119345	2437.789796	20.500967
67.496384	2428.283400	20.505984
67.126510	2432.953321	20.511002
67.179152	2441.123066	20.516019
67.639297	2455.848592	20.521037
67.658567	2457.968466	20.526055
67.951560	2458.886035	20.531072
68.007902	2462.680950	20.536090
67.743885	2462.032351	20.541107
68.237161	2463.485902	20.546125
67.986247	2466.367811	20.551143
67.835560	2468.772006	20.556160
67.803433	2458.921811	20.561178
68.292109	2467.344539	20.566195
68.405603	2469.468266	20.571213
68.529477	2484.171148	20.576231
68.670860	2487.113996	20.581248
68.603762	2492.097486	20.586266
68.349097	2493.276231	20.591283
68.812283	2492.324452	20.596301
68.634134	2493.261309	20.601319
68.676909	2486.844443	20.606336
68.911153	2490.625940	20.611354
68.678072	2481.255350	20.616371
69.200307	2481.912183	20.621389
68.844168	2487.917931	20.626407
69.178333	2480.611368	20.631424
68.987528	2485.952819	20.636442
68.917218	2493.340659	20.641459
68.954558	2497.620010	20.646477
69.130713	2518.031574	20.651495
69.466428	2516.993145	20.656512
69.342502	2513.308748	20.661530
69.253053	2514.002561	20.666547
69.304818	2507.503233	20.671565
69.303094	2510.663984	20.676583
69.555241	2525.474666	20.681600
69.610681	2540.483492	20.686618
69.632081	2555.376626	20.691635
70.069046	2540.007514	20.696653
69.865470	2542.543651	20.701671
70.309798	2529.557558	20.706688
70.060375	2541.250721	20.711706
69.872511	2537.212319	20.716723
69.958494	2536.713204	20.721741
70.385156	2549.262140	20.726759
70.307364	2554.447153	20.731776
70.455861	2565.075537	20.736794
70.470297	2569.597688	20.741811
70.767578	2561.567002	20.746829
70.272352	2572.764501	20.751847
70.483421	2571.049804	20.756864
70.586196	2572.184926	20.761882
70.693513	2577.517412	20.766899
70.750618	2586.311873	20.771917
71.133944	2604.219019	20.776935
71.384648	2597.836593	20.781952
71.384899	2599.235847	20.786970
71.161544	2598.506816	20.791987
71.317132	2587.316121	20.797005
71.420464	2602.377941	20.802023
71.537785	2599.937999	20.807040
71.851414	2590.525777	20.812058
71.787839	2592.629777	20.817075
71.720238	2590.987049	20.822093
71.801655	2597.408396	20.827111
71.685749	2591.416383	20.832128
71.946271	2600.930406	20.837146
71.608405	2597.699363	20.842163
72.044736	2588.221953	20.847181
72.086169	2598.610216	20.852199
72.005853	2616.232623	20.857216
72.112583	2627.378218	20.862234
72.309428	2631.218419	20.867251
72.627122	2626.725733	20.872269
72.246806	2631.194438	20.877287
72.545278	2627.518952	20.882304
72.318565	2629.413779	20.887322
72.335508	2630.137040	20.892339
72.583917	2622.313126	20.897357
72.474460	2633.625351	20.902375
72.844667	2641.878288	20.907392
72.861889	2639.717814	20.912410
72.954063	2654.456600	20.917427
73.220222	2648.049664	20.922445
72.795762	2649.244485	20.927463
73.145210	2654.490404	20.932480
73.206486	2656.967806	20.937498
72.881853	2659.527987	20.942515
73.479171	2644.913507	20.947533
73.185262	2652.614756	20.952551
73.574960	2644.877636	20.957568
73.514305	2656.093996	20.962586
73.565047	2675.762774	20.967603
73.783224	2674.363934	20.972621
73.706544	2687.705924	20.977639
73.904952	2680.566434	20.982656
73.722488	2684.337347	20.987674
73.512945	2689.751868	20.992691
73.767425	2685.041130	20.997709
73.699045	2682.116347	21.002727
73.798990	2690.005735	21.007744
74.182607	2700.101160	21.012762
74.124203	2714.060106	21.017779
74.222519	2696.109699	21.022797
74.115609	2707.254813	21.027815
74.605397	2721.414245	21.032832
74.728661	2729.666495	21.037850
74.745335	2734.490399	21.042867
74.877821	2728.770216	21.047885
74.859178	2734.179482	21.052903
75.237713	2732.286245	21.057920
75.090709	2724.175292	21.062938
75.208483	2733.361338	21.067955
75.118634	2733.423578	21.072973
74.837386	2736.706041	21.077991
75.098960	2731.097422	21.083008
75.339182	2727.070934	21.088026
74.989681	2731.607908	21.093043
75.466131	2746.288653	21.098061
75.386747	2758.804412	21.103079
75.635014	2762.281686	21.108096
75.698347	2755.490144	21.113114
75.969833	2758.251045	21.118131
76.081496	2750.850041	21.123149
75.935363	2756.187613	21.128167
75.809058	2756.099130	21.133184
75.841171	2751.069857	21.138202
75.766554	2767.439253	21.143219
75.945989	2781.665541	21.148237
76.316685	2785.501657	21.153255
75.995337	2787.996048	21.158272
76.629996	2779.596798	21.163290
76.465195	2783.677991	21.168307
76.642034	2783.377551	21.173325
76.549627	2791.008194	21.178343
76.732219	2802.914279	21.183360
76.903818	2804.399500	21.188378
76.761419	2812.694949	21.193395
76.765607	2808.127131	21.198413
77.060702	2818.200571	21.203431
77.167288	2816.031327	21.208448
77.450759	2817.869991	21.213466
77.121210	2818.016078	21.218483
77.389599	2809.473060	21.223501
77.267873	2808.598807	21.228519
77.504587	2808.661673	21.233536
77.963003	2811.293662	21.238554
77.456691	2808.478021	21.243571
77.483222	2810.676235	21.248589
77.416691	2817.254997	21.253607
77.569883	2835.553103	21.258624
77.969289	2837.743776	21.263642
77.888199	2845.456811	21.268659
78.070712	2848.869863	21.273677
78.071963	2847.523693	21.278695
78.320990	2849.857128	21.283712
78.334432	2833.730876	21.288730
78.010581	2843.703236	21.293747
78.092830	2852.563070	21.298765
78.420014	2864.483906	21.303783
78.089993	2867.804853	21.308800
78.615096	2860.481814	21.313818
78.852363	2868.326588	21.318835
78.585377	2875.835658	21.323853
78.458554	2881.451804	21.328871
78.593368	2894.364587	21.333888
78.963776	2896.184677	21.338906
78.964701	2897.793092	21.343923
78.795269	2897.809813	21.348941
79.120295	2909.310975	21.353959
79.198974	2928.503666	21.358976
79.209917	2923.549292	21.363994
79.113599	2928.487245	21.369011
79.565462	2927.516796	21.374029
79.392470	2931.694517	21.379047
79.232144	2944.992656	21.384064
79.578431	2953.822246	21.389082
79.862898	2964.006822	21.394099
79.950209	2965.197932	21.399117
80.126186	2961.287033	21.404135
80.197864	2960.317426	21.409152
80.393361	2956.371164	21.414170
80.455984	2956.812626	21.419187
80.420790	2955.296841	21.424205
80.604657	2949.279689	21.429223
80.260481	2960.499017	21.434240
80.933986	2965.893961	21.439258
80.877575	2980.523832	21.444275
81.155984	2969.118964	21.449293
81.059898	2968.777875	21.454311
80.778218	2977.619518	21.459328
81.301927	2978.579780	21.464346
81.082111	2983.540592	21.469363
81.521396	2980.712569	21.474381
81.396948	2975.341619	21.479399
81.263301	2985.138218	21.484416
81.502030	2973.543806	21.489434
81.074497	2983.047448	21.494451
81.072227	2987.034342	21.499469
81.342817	2981.323503	21.504487
81.000989	2984.057965	21.509504
81.538648	2986.039399	21.514522
81.558950	3005.060576	21.519539
81.686880	3006.253865	21.524557
81.839258	3003.639141	21.529575
81.627322	3013.890326	21.534592
81.962193	3016.641170	21.539610
81.853250	3037.011607	21.544627
82.210931	3037.203858	21.549645
82.675803	3037.464757	21.554663
82.397245	3046.493946	21.559680
82.524601	3044.866489	21.564698
82.866123	3047.389729	21.569715
82.577341	3043.599333	21.574733
82.647579	3039.889346	21.579751
82.660539	3047.880900	21.584768
83.018410	3055.174784	21.589786
82.924501	3068.766082	21.594803
83.013925	3072.913009	21.599821
82.979691	3071.172083	21.604839
83.135984	3076.166558	21.609856
83.110145	3071.553103	21.614874
83.175665	3071.300302	21.619891
83.467950	3095.499071	21.624909
83.821330	3094.830650	21.629927
83.691947	3100.625066	21.634944
84.055045	3095.081143	21.639962
83.782205	3100.365101	21.644979
83.499863	3106.508003	21.649997
83.943007	3096.616201	21.655015
83.898433	3104.386479	21.660032
84.088945	3098.155816	21.665050
83.927462	3110.736098	21.670067
84.246470	3119.066696	21.675085
84.775328	3114.707742	21.680103
84.816111	3116.239028	21.685120
85.288822	3119.408424	21.690138
85.355548	3124.714545	21.695155
84.934406	3109.745987	21.700173
85.009486	3086.391517	21.705191
84.927832	3088.798962	21.710208
84.672018	3089.209399	21.715226
84.964897	3101.435605	21.720243
85.065397	3113.421898	21.725261
85.282549	3109.911869	21.730279
85.078407	3116.962660	21.735296
85.450177	3120.439993	21.740314
85.350552	3113.148803	21.745331
85.300680	3110.482143	21.750349
85.692441	3111.982632	21.755367
85.487455	3121.542123	21.760384
85.831528	3126.368224	21.765402
85.611510	3130.391454	21.770419
85.586426	3130.787911	21.775437
86.059587	3122.201046	21.780455
85.706982	3133.860001	21.785472
85.991431	3125.628106	21.790490
86.190677	3146.788885	21.795507
86.230188	3160.096257	21.800525
86.273026	3165.900207	21.805543
86.598548	3165.601223	21.810560
86.431885	3165.099898	21.815578
86.383924	3168.154102	21.820595
86.313719	3171.676754	21.825613
86.671055	3181.027831	21.830631
86.449231	3197.633573	21.835648
86.816475	3205.512867	21.840666
87.110222	3196.737458	21.845683
87.166724	3205.226387	21.850701
87.186818	3196.255479	21.855719
87.283709	3219.866532	21.860736
87.247323	3223.846345	21.865754
87.210995	3232.662388	21.870771
87.253691	3232.528073	21.875789
87.646990	3230.475881	21.880807
87.757219	3236.340697	21.885824
87.663595	3251.957707	21.890842
87.815123	3253.103202	21.895859
87.793254	3265.859585	21.900877
88.215210	3264.704306	21.905895
87.901996	3262.217274	21.910912
88.091293	3256.604249	21.915930
88.198240	3263.750245	21.920947
88.068285	3290.099686	21.925965
88.948759	3283.548889	21.930983
88.952546	3293.129478	21.936000
88.754132	3291.494157	21.941018
88.705177	3283.743271	21.946035
88.769609	3292.529123	21.951053
88.867224	3286.733260	21.956071
89.178157	3283.929583	21.961088
89.529553	3298.600150	21.966106
89.463751	3290.524704	21.971123
89.297814	3303.689547	21.976141
89.486749	3304.783456	21.981159
89.695127	3308.422978	21.986176
89.863036	3314.294360	21.991194
90.013696	3315.526528	21.996211
90.153627	3307.165755	22.001229
90.000634	3310.563979	22.006247
90.009199	3317.831100	22.011264
90.001165	3305.932014	22.016282
90.659971	3305.363556	22.021299
90.144874	3309.628975	22.026317
90.380027	3307.169340	22.031335
90.332079	3301.584691	22.036352
90.520921	3307.744575	22.041370
90.386627	3298.813956	22.046387
90.553235	3296.809705	22.051405
90.683711	3297.851577	22.056423
90.627461	3302.384440	22.061440
90.702293	3296.643338	22.066458
90.769321	3315.037595	22.071475
90.596878	3325.746817	22.076493
90.907242	3321.350276	22.081511
90.987615	3328.141046	22.086528
90.898909	3330.148468	22.091546
91.302677	3343.025839	22.096563
91.391762	3351.388515	22.101581
91.532165	3352.162136	22.106599
91.648967	3359.150852	22.111616
91.614709	3356.211839	22.116634
91.961635	3355.507465	22.121651
91.419525	3360.072197	22.126669
91.851910	3367.752398	22.131687
91.920307	3381.610735	22.136704
91.952226	3381.804594	22.141722
91.833701	3380.984860	22.146739
92.175265	3399.483333	22.151757
92.614932	3409.674939	22.156775
92.282673	3418.794730	22.161792
92.523369	3420.250904	22.166810
92.683490	3419.463826	22.171827
92.085107	3428.041581	22.176845
92.726551	3434.099454	22.181863
92.961813	3435.173398	22.186880
92.761297	3449.023548	22.191898
93.150611	3444.416933	22.196915
92.974122	3451.405262	22.201933
93.312665	3449.867588	22.206951
93.556968	3465.558376	22.211968
93.711502	3469.544784	22.216986
93.929757	3465.614424	22.222003
94.015259	3473.254811	22.227021
94.178913	3467.116381	22.232039
94.403713	3470.506318	22.237056
93.993848	3477.796188	22.242074
94.268649	3466.976779	22.247091
94.649212	3467.019073	22.252109
94.593484	3464.603437	22.257127
94.623031	3464.699344	22.262144
94.609382	3467.462586	22.267162
94.342414	3465.048381	22.272179
94.425747	3473.513522	22.277197
94.690345	3467.074228	22.282215
94.681032	3469.423788	22.287232
94.727659	3485.493818	22.292250
94.890714	3483.958951	22.297267
94.726984	3502.386306	22.302285
94.746975	3493.571776	22.307303
94.953012	3500.772099	22.312320
94.844267	3520.827729	22.317338
95.334223	3517.617869	22.322355
95.011046	3526.507362	22.327373
95.368633	3529.360095	22.332391
95.758956	3534.316622	22.337408
95.989866	3551.841752	22.342426
96.194207	3556.689493	22.347443
96.052187	3556.992116	22.352461
96.099025	3560.434838	22.357479
96.207314	3563.096055	22.362496
96.448585	3551.381998	22.367514
96.753606	3544.022135	22.372531
96.251004	3557.632643	22.377549
96.571179	3547.007323	22.382567
96.686934	3548.204171	22.387584
96.348404	3550.806051	22.392602
96.949545	3555.178312	22.397619
97.138118	3569.148247	22.402637
96.768543	3567.083928	22.407655
96.874408	3573.416848	22.412672
97.093432	3579.410771	22.417690
97.387763	3567.321660	22.422707
97.224979	3584.310963	22.427725
97.629174	3597.802870	22.432743
97.784260	3598.497858	22.437760
97.657012	3608.423649	22.442778
97.703868	3606.915165	22.447795
97.760874	3603.569795	22.452813
97.659852	3599.610860	22.457831
97.943191	3602.947440	22.462848
98.302853	3623.596390	22.467866
98.397434	3628.563136	22.472883
98.485003	3636.769672	22.477901
98.449262	3631.149124	22.482919
98.588259	3626.679914	22.487936
98.479737	3626.697147	22.492954
98.735250	3630.341820	22.497971
98.978338	3630.654622	22.502989
98.994085	3628.271614	22.508007
99.087996	3641.640760	22.513024
99.181915	3668.540455	22.518042
99.331341	3654.424345	22.523059
98.873130	3658.618644	22.528077
99.063609	3661.088201	22.533095
99.546583	3656.171589	22.538112
99.523142	3681.156413	22.543130
99.182242	3678.721708	22.548147
99.287435	3684.845532	22.553165
99.142001	3689.085151	22.558183
99.809371	3702.694881	22.563200
99.670697	3718.849780	22.568218
100.394257	3708.878244	22.573235
100.787542	3703.214429	22.578253
100.299946	3705.144696	22.583271
100.865980	3706.110065	22.588288
100.918962	3702.707888	22.593306
100.882783	3697.750540	22.598323
101.103270	3706.461409	22.603341
101.261771	3692.140071	22.608359
101.093198	3687.118091	22.613376
100.896048	3702.005547	22.618394
101.136934	3688.424697	22.623411
101.333245	3699.297227	22.628429
101.595278	3711.538304	22.633447
101.847500	3717.716576	22.638464
101.214596	3729.293257	22.643482
101.768661	3733.625880	22.648499
102.244203	3732.598117	22.653517
102.044543	3731.589128	22.658535
102.077195	3728.212999	22.663552
101.671081	3739.633952	22.668570
102.190977	3734.187510	22.673587
102.115992	3725.242453	22.678605
102.085888	3729.546292	22.683623
102.391536	3742.184785	22.688640
102.288548	3751.047168	22.693658
102.466023	3758.453559	22.698675
102.661552	3768.050295	22.703693
102.653793	3763.120647	22.708711
102.833083	3776.394489	22.713728
102.681689	3787.197449	22.718746
102.745192	3782.629310	22.723763
102.833098	3786.635083	22.728781
102.730878	3809.105916	22.733799
102.839341	3815.205673	22.738816
102.869763	3821.365076	22.743834
103.370280	3836.669274	22.748851
103.856630	3850.052340	22.753869
104.030468	3856.817438	22.758887
103.812892	3850.941027	22.763904
103.674294	3862.050376	22.768922
104.282638	3856.792746	22.773939
104.535196	3873.550166	22.778957
104.717866	3882.938988	22.783975
104.693146	3886.470291	22.788992
104.716095	3886.719081	22.794010
104.425609	3886.666995	22.799027
104.743451	3893.147973	22.804045
104.881036	3892.057662	22.809063
104.980394	3884.871239	22.814080
104.822886	3887.697619	22.819098
105.072663	3896.359878	22.824115
105.197849	3909.132704	22.829133
105.290101	3907.787659	22.834151
105.508413	3906.263606	22.839168
105.338672	3916.544089	22.844186
105.606345	3907.940765	22.849203
105.944279	3923.379539	22.854221
106.027049	3938.864524	22.859239
106.086081	3933.686592	22.864256
105.926582	3944.452413	22.869274
106.343921	3940.532664	22.874291
106.215838	3943.093186	22.879309
106.059001	3946.132659	22.884327
106.294188	3937.508537	22.889344
105.893958	3953.536266	22.894362
106.286526	3969.912747	22.899379
106.737603	3962.888898	22.904397
106.950121	3968.916272	22.909415
106.870221	3964.951510	22.914432
106.839737	3989.528123	22.919450
107.149706	3996.867881	22.924467
107.304428	4005.517828	22.929485
107.310978	4012.146831	22.934503
107.247326	4004.493095	22.939520
107.334151	4007.679383	22.944538
107.690787	4018.179660	22.949555
107.735962	4025.380719	22.954573
107.526006	4035.032847	22.959591
108.120326	4025.196564	22.964608
107.854839	4030.345157	22.969626
107.939164	4045.939355	22.974643
108.258882	4042.204282	22.979661
108.333022	4047.376607	22.984679
108.497074	4062.822015	22.989696
108.402429	4066.423511	22.994714
108.541120	4082.131014	22.999731
108.975515	4078.234471	23.004749
108.760006	4086.448678	23.009767
109.133982	4080.532129	23.014784
108.989923	4088.828560	23.019802
109.177828	4111.223698	23.024819
109.405961	4102.215917	23.029837
109.235400	4114.963706	23.034855
109.340952	4111.938527	23.039872
109.876947	4121.541781	23.044890
109.772908	4134.450477	23.049907
110.330970	4141.400673	23.054925
109.978311	4140.734658	23.059943
110.489820	4139.427369	23.064960
110.367250	4134.860470	23.069978
110.496127	4143.278614	23.074995
110.855897	4136.732601	23.080013
110.365684	4131.491136	23.085031
110.665248	4145.989882	23.090048
111.007013	4166.725840	23.095066
111.140852	4163.933719	23.100083
111.619581	4163.053319	23.105101
111.291998	4171.172161	23.110119
111.652013	4164.257927	23.115136
111.736461	4168.589257	23.120154
111.749924	4169.668732	23.125171
111.867526	4152.082427	23.130189
111.666255	4155.952687	23.135207
111.475284	4162.685628	23.140224
111.302956	4165.794484	23.145242
111.649956	4167.520926	23.150259
112.059640	4170.301759	23.155277
111.550895	4186.976392	23.160295
111.950770	4189.844542	23.165312
112.108519	4202.536910	23.170330
112.316747	4224.926621	23.175347
112.512929	4220.015434	23.180365
112.534965	4221.648949	23.185383
112.626825	4228.293554	23.190400
112.612176	4242.419259	23.195418
112.759784	4249.547453	23.200435
113.188150	4252.344203	23.205453
112.968840	4267.538638	23.210471
113.601977	4281.414765	23.215488
113.818335	4289.027632	23.220506
113.676934	4289.596071	23.225523
113.918277	4291.363763	23.230541
113.849860	4298.310872	23.235559
113.867422	4284.562904	23.240576
114.236186	4284.102032	23.245594
114.466309	4284.403544	23.250611
114.502349	4278.362223	23.255629
114.319883	4289.438766	23.260647
114.521464	4297.282921	23.265664
115.093889	4298.506926	23.270682
114.578636	4310.250169	23.275699
115.371509	4303.728640	23.280717
115.231551	4300.875520	23.285735
114.994432	4295.031940	23.290752
115.481893	4301.873894	23.295770
115.257381	4302.782851	23.300787
115.464595	4298.400111	23.305805
115.349224	4316.159950	23.310823
115.798660	4331.368968	23.315840
115.838330	4330.909435	23.320858
115.681170	4329.495558	23.325875
116.064964	4323.507332	23.330893
116.373901	4331.211662	23.335911
116.355515	4327.606740	23.340928
116.478048	4341.953755	23.345946
116.442398	4350.963100	23.350963
116.704437	4352.161079	23.355981
116.746037	4357.396917	23.360999
116.821079	4347.665250	23.366016
117.224458	4348.943749	23.371034
116.632988	4349.340865	23.376051
116.875404	4363.035496	23.381069
116.978354	4378.735642	23.386087
117.275155	4381.440113	23.391104
117.467938	4385.383698	23.396122
117.385597	4383.876069	23.401139
117.826723	4394.450469	23.406157
117.567359	4407.529710	23.411175
117.756746	4416.619644	23.416192
118.076688	4415.043933	23.421210
118.064769	4413.952250	23.426227
118.014706	4417.711930	23.431245
117.925423	4434.109908	23.436263
118.249942	4437.912137	23.441280
118.584296	4441.588500	23.446298
118.415386	4450.586113	23.451315
118.546478	4455.662177	23.456333
118.484931	4464.509726	23.461351
118.685078	4469.609399	23.466368
118.961759	4474.486033	23.471386
118.828561	4495.859896	23.476403
119.508991	4499.684061	23.481421
119.549688	4502.594599	23.486439
119.401092	4504.205789	23.491456
119.481854	4507.972954	23.496474
119.605771	4520.228076	23.501491
119.972304	4520.710027	23.506509
120.055233	4528.581091	23.511527
120.189082	4529.482483	23.516544
120.455406	4535.280448	23.521562
120.265674	4561.047731	23.526579
120.575296	4562.805357	23.531597
120.901353	4564.288161	23.536615
120.939120	4565.481796	23.541632
120.961999	4567.072732	23.546650
121.039849	4570.327444	23.551667
121.326698	4575.812190	23.556685
121.294373	4589.631083	23.561703
121.289081	4595.735142	23.566720
121.424265	4583.534478	23.571738
121.348193	4584.837525	23.576755
121.523387	4605.590436	23.581773
121.668616	4611.414821	23.586791
121.662946	4615.628485	23.591808
122.006869	4624.520044	23.596826
122.096516	4644.378786	23.601843
122.855148	4640.555487	23.606861
122.672931	4651.237332	23.611879
122.658700	4653.647655	23.616896
122.786202	4645.700344	23.621914
122.623807	4657.131916	23.626931
122.861261	4672.204373	23.631949
123.247231	4680.189263	23.636967
123.200603	4678.740419	23.641984
123.720959	4672.726345	23.647002
123.526792	4681.812304	23.652019
123.631420	4666.661547	23.657037
124.090014	4663.113443	23.662055
123.986501	4673.979434	23.667072
124.256649	4662.913653	23.672090
124.149990	4663.770010	23.677107
124.293090	4681.443446	23.682125
124.690726	4695.151400	23.687143
124.692892	4694.880353	23.692160
124.789158	4691.168161	23.697178
124.546799	4688.312412	23.702195
124.790538	4688.944544	23.707213
125.115173	4696.290970	23.712231
124.889815	4698.457254	23.717248
125.002847	4687.810650	23.722266
124.843673	4702.977062	23.727283
125.106320	4715.592571	23.732301
125.019699	4716.868202	23.737319
125.294596	4724.468028	23.742336
125.370150	4732.437930	23.747354
125.633073	4752.025308	23.752371
125.711378	4748.439480	23.757389
125.724443	4766.131391	23.762407
125.827839	4781.169479	23.767424
126.144687	4791.699472	23.772442
126.200995	4800.511123	23.777459
126.654909	4811.455119	23.782477
127.158521	4797.585904	23.787495
127.028209	4803.493635	23.792512
127.138394	4802.089794	23.797530
127.202024	4812.121274	23.802547
127.204447	4800.379803	23.807565
127.338058	4800.421365	23.812583
127.259126	4814.671943	23.817600
127.681110	4833.367887	23.822618
127.680336	4837.551725	23.827635
127.677754	4834.624673	23.832653
127.958883	4843.872536	23.837671
127.910297	4860.164584	23.842688
128.336362	4860.367210	23.847706
128.203423	4870.253846	23.852723
128.459851	4870.139722	23.857741
128.600031	4868.848314	23.862759
128.471985	4892.253249	23.867776
128.830627	4897.341174	23.872794
128.719525	4908.617644	23.877811
128.711873	4897.365472	23.882829
128.912500	4912.845278	23.887847
129.166343	4927.731290	23.892864
129.587015	4923.798169	23.897882
129.343234	4937.859587	23.902899
129.773869	4953.308268	23.907917
129.997888	4954.281063	23.912935
129.796899	4957.683381	23.917952
130.314859	4947.950717	23.922970
130.005956	4964.636053	23.927987
130.186093	4987.768570	23.933005
130.569504	4988.581421	23.938023
130.430691	4996.282756	23.943040
131.018089	4992.164114	23.948058
130.822015	4995.505079	23.953075
130.764178	5007.342724	23.958093
130.977600	5015.754969	23.963111
131.420070	5021.900313	23.968128
131.563789	5016.484281	23.973146
131.559711	5019.517709	23.978163
131.234421	5025.318152	23.983181
131.575100	5030.545093	23.988199
131.718002	5042.374361	23.993216
132.137949	5033.396011	23.998234
131.941555	5049.531673	24.003251
132.160012	5044.161932	24.008269
132.906511	5060.041057	24.013287
132.298223	5080.887305	24.018304
132.594374	5077.239915	24.023322
132.840958	5076.045600	24.028339
133.026104	5078.050503	24.033357
133.210374	5075.227356	24.038375
132.994393	5093.948252	24.043392
133.375731	5104.070886	24.048410
133.430668	5112.502162	24.053427
133.312300	5111.386490	24.058445
133.836088	5116.240462	24.063463
133.927259	5133.803923	24.068480
133.745558	5136.292951	24.073498
134.155119	5138.135416	24.078515
134.099764	5132.666115	24.083533
134.319581	5142.478593	24.088551
134.581440	5155.086737	24.093568
134.839164	5156.721327	24.098586
134.986118	5158.722890	24.103603
135.167766	5169.727087	24.108621
135.121106	5154.776183	24.113639
135.176835	5163.240405	24.118656
135.516912	5160.773967	24.123674
135.616439	5180.455627	24.128691
135.731676	5181.258538	24.133709
136.023174	5182.210362	24.138727
135.566587	5194.833963	24.143744
135.742397	5182.668812	24.148762
135.926851	5193.117928	24.153779
135.782118	5218.399269	24.158797
136.351434	5214.624897	24.163815
135.934758	5214.799831	24.168832
136.478074	5235.642843	24.173850
136.580783	5248.041206	24.178867
136.604939	5256.320124	24.183885
137.049637	5266.506722	24.188903
137.163820	5281.224181	24.193920
137.272556	5278.334364	24.198938
137.591022	5288.917956	24.203955
137.202694	5292.928479	24.208973
137.700508	5302.680217	24.213991
137.848554	5310.420945	24.219008
138.091920	5317.811325	24.224026
137.908341	5325.601789	24.229043
137.772389	5331.420154	24.234061
138.304593	5340.788795	24.239079
138.269162	5354.384675	24.244096
138.626615	5347.770055	24.249114
138.950787	5350.944755	24.254131
138.630645	5358.769599	24.259149
139.187750	5359.968610	24.264167
138.916741	5379.547543	24.269184
139.149728	5384.196212	24.274202
139.315989	5369.266214	24.279219
139.474628	5384.356688	24.284237
139.600425	5391.329990	24.289255
139.487102	5407.190021	24.294272
139.773486	5401.127208	24.299290
139.944764	5419.233682	24.304307
140.161060	5440.553972	24.309325
140.364210	5441.157207	24.314343
140.311462	5442.814582	24.319360
140.198215	5458.559789	24.324378
140.532180	5462.910724	24.329395
140.582610	5467.094444	24.334413
140.798736	5484.979851	24.339431
140.840041	5499.293740	24.344448
141.060579	5495.717311	24.349466
141.504938	5505.210997	24.354483
141.465052	5521.861934	24.359501
141.851452	5525.583776	24.364519
141.708071	5527.874003	24.369536
141.917426	5541.245351	24.374554
142.087400	5553.944016	24.379571
142.488486	5561.277114	24.384589
142.726475	5554.661781	24.389607
142.389926	5568.859748	24.394624
142.828976	5583.941121	24.399642
143.263016	5583.218047	24.404659
142.852207	5592.940976	24.409677
143.103889	5581.588715	24.414695
143.357396	5592.102633	24.419712
143.801850	5611.315247	24.424730
143.817588	5615.109585	24.429747
143.872301	5614.037086	24.434765
144.199785	5614.676365	24.439783
143.921388	5625.730649	24.444800
144.345863	5621.034368	24.449818
144.528086	5632.418040	24.454835
144.592459	5642.569554	24.459853
144.627572	5639.176075	24.464871
144.978483	5646.193856	24.469888
144.898759	5644.389068	24.474906
145.037408	5647.908906	24.479923
145.179717	5664.354719	24.484941
145.400051	5673.413747	24.489959
145.494039	5667.018015	24.494976
145.442950	5673.548381	24.499994
145.663976	5672.940303	24.505011
145.381080	5698.194924	24.510029
145.739945	5699.320934	24.515047
146.038757	5705.235347	24.520064
146.189017	5720.719311	24.525082
146.263499	5734.027366	24.530099
146.253172	5742.834469	24.535117
146.721043	5733.970794	24.540135
146.728807	5748.617568	24.545152
146.919040	5763.881202	24.550170
147.178410	5758.132540	24.555187
147.041582	5768.959012	24.560205
147.234704	5774.918628	24.565223
147.608711	5791.286728	24.570240
147.589871	5792.056763	24.575258
147.732277	5793.582355	24.580275
147.629944	5801.401813	24.585293
148.017082	5812.653819	24.590311
148.283515	5825.764557	24.595328
148.331539	5826.207650	24.600346
148.493745	5829.752886	24.605363
148.737474	5852.635078	24.610381
148.968908	5858.431264	24.615399
149.162188	5853.073116	24.620416
149.528964	5858.238759	24.625434
149.580360	5857.269052	24.630451
149.574498	5876.552236	24.635469
150.005856	5877.463714	24.640487
149.832005	5881.573161	24.645504
149.678672	5881.687229	24.650522
150.078774	5873.306344	24.655539
150.073717	5899.991431	24.660557
150.044774	5906.216245	24.665575
150.261941	5907.770841	24.670592
150.292333	5925.078215	24.675610
150.676933	5934.030961	24.680627
150.804931	5945.077336	24.685645
151.006151	5946.165558	24.690663
151.480466	5974.362072	24.695680
151.131970	5975.840853	24.700698
151.446982	5978.163492	24.705715
151.638794	5982.423951	24.710733
151.808557	5999.156868	24.715751
152.015882	6004.545468	24.720768
152.065864	6006.950494	24.725786
152.353098	6016.882625	24.730803
152.645499	6032.533082	24.735821
152.647662	6029.804880	24.740839
152.984992	6032.802179	24.745856
152.807514	6025.159248	24.750874
153.247323	6030.523380	24.755891
153.404049	6047.307211	24.760909
153.539448	6042.217076	24.765927
153.587551	6045.007932	24.770944
154.023675	6048.570918	24.775962
154.363937	6038.508678	24.780979
154.234361	6042.031249	24.785997
154.502827	6042.228344	24.791015
154.618020	6038.197299	24.796032
154.638589	6042.064934	24.801050
154.794721	6036.352294	24.806067
154.737832	6056.591139	24.811085
154.929224	6068.886358	24.816103
154.999151	6071.861782	24.821120
155.106444	6077.338742	24.826138
155.317988	6070.184515	24.831155
155.372611	6082.802104	24.836173
155.437745	6101.662772	24.841191
155.679344	6095.770471	24.846208
155.403929	6115.817642	24.851226
155.634816	6121.230853	24.856243
155.616682	6136.938798	24.861261
155.674014	6156.537216	24.866279
156.168533	6170.158715	24.871296
156.014827	6184.375323	24.876314
156.696439	6201.483203	24.881331
156.932947	6211.928676	24.886349
157.066577	6216.915249	24.891367
157.249279	6228.833538	24.896384
157.309665	6240.110429	24.901402
157.459103	6233.460134	24.906419
157.605408	6251.263185	24.911437
157.549877	6268.212503	24.916455
157.838080	6275.462460	24.921472
157.951021	6295.786279	24.926490
158.264179	6298.480635	24.931507
158.244711	6310.052772	24.936525
158.287889	6310.454165	24.941543
158.775119	6331.441427	24.946560
158.651962	6338.778244	24.951578
159.021363	6354.785776	24.956595
158.967945	6363.606411	24.961613
159.004854	6367.350358	24.966631
159.614900	6378.376064	24.971648
159.787350	6394.750218	24.976666
160.144559	6399.676816	24.981683
160.100324	6404.436886	24.986701
160.324251	6421.639236	24.991719
160.580905	6421.277228	24.996736
160.788000	6422.108838	25.001754
160.808275	6419.033843	25.006771
161.147461	6425.408687	25.011789
160.974547	6445.318790	25.016807
161.528212	6450.643680	25.021824
161.791762	6463.238512	25.026842
161.896767	6454.948413	25.031859
162.126880	6464.014235	25.036877
161.999652	6452.882231	25.041895
162.277934	6462.863299	25.046912
162.279515	6485.648959	25.051930
162.639968	6488.135174	25.056947
162.754829	6489.544062	25.061965
162.616798	6478.768613	25.066983
162.703114	6485.247529	25.072000
162.552978	6489.117319	25.077018
162.763113	6500.127408	25.082035
162.827109	6512.096323	25.087053
162.690206	6519.316612	25.092071
163.163371	6534.543801	25.097088
163.510610	6541.042514	25.102106
163.518174	6562.154574	25.107123
163.737391	6572.953977	25.112141
163.685711	6587.759764	25.117159
164.220007	6607.670634	25.122176
163.858314	6616.776612	25.127194
164.317282	6621.496652	25.132211
164.656880	6650.663262	25.137229
164.866930	6650.722546	25.142247
165.324142	6663.035676	25.147264
165.255803	6668.595147	25.152282
166.125056	6653.966436	25.157299
166.800528	6643.507295	25.162317
166.705339	6642.945662	25.167335
167.239378	6639.861885	25.172352
167.004184	6643.273185	25.177370
166.939669	6643.037125	25.182387
167.106584	6650.568615	25.187405
166.770842	6648.671548	25.192423
167.325170	6648.103141	25.197440
167.141073	6651.691198	25.202458
167.337304	6650.522889	25.207475
167.150445	6650.905889	25.212493
167.237048	6671.734838	25.217511
167.617129	6671.599422	25.222528
167.772190	6683.543729	25.227546
167.972030	6694.152752	25.232563
167.748860	6710.137120	25.237581
167.722695	6718.306067	25.242599
167.969671	6725.239435	25.247616
168.345512	6736.458542	25.252634
168.357003	6756.548170	25.257651
168.842481	6776.552814	25.262669
168.980504	6777.363985	25.267687
169.128286	6794.181561	25.272704
169.241652	6816.341689	25.277722
169.399954	6825.842496	25.282739
169.781823	6829.164901	25.287757
169.730002	6845.414795	25.292775
170.174895	6834.540644	25.297792
170.080332	6858.890680	25.302810
170.271555	6865.319204	25.307827
170.686774	6861.225942	25.312845
170.667087	6884.213097	25.317863
171.075371	6894.324802	25.322880
170.776998	6898.609385	25.327898
171.285669	6905.658483	25.332915
171.435662	6921.593812	25.337933
171.373345	6927.879453	25.342951
171.717197	6930.921535	25.347968
171.821334	6938.737785	25.352986
171.720593	6956.435505	25.358003
171.943493	6957.981434	25.363021
172.639215	6973.545767	25.368039
173.567917	6966.222485	25.373056
173.478140	6971.001799	25.378074
173.716685	6975.945937	25.383091
174.194607	6970.477490	25.388109
173.860001	6975.453204	25.393127
174.280690	6966.785169	25.398144
174.099281	6971.211639	25.403162
174.086255	6976.716770	25.408179
174.278835	6965.084112	25.413197
174.142615	6976.178887	25.418215
174.453530	6968.781780	25.423232
174.404306	6983.557669	25.428250
174.455438	6997.782525	25.433267
174.850702	6998.078234	25.438285
174.548745	7020.097155	25.443303
174.899268	7026.594773	25.448320
175.227939	7044.029788	25.453338
174.935746	7059.876821	25.458355
175.272194	7075.383662	25.463373
175.166413	7084.701701	25.468391
175.629879	7093.754312	25.473408
175.684268	7117.826482	25.478426
175.711282	7130.410807	25.483443
176.189341	7150.613852	25.488461
175.930206	7176.724850	25.493479
176.489379	7183.656659	25.498496
177.137403	7196.389105	25.503514
177.049631	7215.372346	25.508531
177.059253	7229.673283	25.513549
177.445072	7235.668077	25.518567
177.775670	7256.354294	25.523584
177.810904	7268.802875	25.528602
178.239915	7273.410662	25.533619
178.479658	7287.639560	25.538637
178.566192	7302.427955	25.543655
178.738908	7303.656952	25.548672
179.125924	7302.918487	25.553690
178.943036	7325.590847	25.558707
179.394174	7321.314693	25.563725
179.812771	7319.538053	25.568743
179.918501	7320.023925	25.573760
179.982694	7330.477200	25.578778
180.216281	7344.183875	25.583795
180.427269	7347.787797	25.588813
180.290248	7360.087660	25.593831
180.330373	7360.199220	25.598848
180.683940	7370.730714	25.603866
180.679223	7382.121928	25.608883
180.825416	7376.732974	25.613901
181.128351	7391.305195	25.618919
181.529264	7410.172219	25.623936
181.341560	7414.266982	25.628954
181.251243	7422.319858	25.633971
181.723849	7426.178736	25.638989
181.896965	7448.981800	25.644007
182.279831	7445.921965	25.649024
182.516330	7458.919321	25.654042
182.462742	7482.766548	25.659059
183.003654	7489.075858	25.664077
182.836780	7497.329826	25.669095
183.101826	7507.726026	25.674112
183.403347	7515.825070	25.679130
183.288630	7518.963989	25.684148
183.769626	7521.208484	25.689165
183.509418	7545.230386	25.694183
183.510617	7552.584956	25.699200
183.943489	7567.386071	25.704218
184.231052	7580.624042	25.709236
184.126491	7590.545728	25.714253
184.265346	7615.991303	25.719271
184.523796	7617.906972	25.724288
184.855954	7643.648329	25.729306
184.970609	7649.094795	25.734324
185.609905	7651.713805	25.739341
186.040199	7670.430904	25.744359
186.260173	7667.824266	25.749376
186.619092	7661.649834	25.754394
186.405033	7678.563866	25.759412
186.856858	7668.359210	25.764429
187.010946	7689.206365	25.769447
187.217783	7686.796962	25.774464
187.302961	7696.258050	25.779482
187.046280	7697.679862	25.784500
187.309401	7701.149659	25.789517
187.772626	7724.183874	25.794535
187.958437	7726.532903	25.799552
188.114753	7723.063760	25.804570
188.048496	7729.148138	25.809588
188.590397	7757.400222	25.814605
188.478201	7764.103341	25.819623
188.533902	7759.097722	25.824640
189.312698	7773.348950	25.829658
188.828210	7792.245088	25.834676
189.545443	7783.979403	25.839693
189.321146	7797.921590	25.844711
189.200419	7813.853034	25.849728
189.605131	7818.379098	25.854746
189.690960	7834.247734	25.859764
189.792965	7837.925805	25.864781
189.645553	7856.101798	25.869799
189.974146	7873.713274	25.874816
189.949372	7893.320773	25.879834
190.381775	7918.721641	25.884852
190.838200	7916.350315	25.889869
190.972655	7949.705357	25.894887
190.985144	7955.970061	25.899904
191.362831	7964.494718	25.904922
191.537671	7983.474445	25.909940
191.780617	7985.496897	25.914957
192.049973	7999.244900	25.919975
192.031211	8019.598364	25.924992
192.292334	8016.256446	25.930010
192.330178	8043.235978	25.935028
193.245791	8052.260770	25.940045
193.150166	8049.865299	25.945063
193.198652	8066.881521	25.950080
193.724349	8074.137781	25.955098
193.983784	8080.748748	25.960116
194.465452	8072.180522	25.965133
194.541434	8080.799771	25.970151
194.788596	8087.530337	25.975168
195.136131	8091.246445	25.980186
194.916250	8108.338940	25.985204
195.318148	8103.604184	25.990221
195.205526	8101.089052	25.995239
195.143040	8115.005737	26.000256
195.602342	8120.619732	26.005274
195.217700	8131.104990	26.010292
195.439147	8131.217552	26.015309
195.756639	8160.745538	26.020327
195.887292	8176.463782	26.025344
196.177169	8188.699024	26.030362
196.377322	8203.830207	26.035380
196.681804	8212.419006	26.040397
196.762294	8233.920765	26.045415
196.745786	8238.539290	26.050432
197.111014	8259.806838	26.055450
197.295578	8271.457349	26.060468
197.659918	8297.767964	26.065485
197.666880	8305.016934	26.070503
197.801221	8316.381971	26.075520
198.035305	8325.689880	26.080538
197.968916	8344.285953	26.085556
198.210372	8354.745131	26.090573
198.760757	8373.904707	26.095591
198.959272	8391.523761	26.100608
199.160998	8394.423950	26.105626
199.080375	8414.874767	26.110644
199.545607	8423.845288	26.115661
199.792574	8439.510249	26.120679
200.057352	8454.061659	26.125696
200.437511	8456.416414	26.130714
200.875065	8485.155906	26.135732
201.169607	8491.573387	26.140749
201.107881	8483.389796	26.145767
201.151982	8489.807854	26.150784
201.486231	8498.895700	26.155802
201.510860	8517.568760	26.160820
201.985122	8525.192277	26.165837
202.093608	8512.905700	26.170855
202.031916	8519.454346	26.175872
202.683919	8530.051224	26.180890
202.674632	8539.742734	26.185908
202.752833	8540.079194	26.190925
203.613621	8543.577853	26.195943
203.505852	8541.090595	26.200960
203.691173	8555.304199	26.205978
203.647208	8568.257918	26.210996
203.963719	8563.574797	26.216013
204.120642	8571.536546	26.221031
203.863294	8576.381643	26.226048
204.373599	8591.008149	26.231066
204.312184	8604.529297	26.236084
204.060980	8612.385761	26.241101
204.553958	8626.160860	26.246119
204.860988	8645.702285	26.251136
205.259652	8670.555426	26.256154
205.199182	8675.250344	26.261172
205.284293	8684.832862	26.266189
205.201285	8705.196712	26.271207
205.542499	8733.317385	26.276224
205.936451	8740.670521	26.281242
205.943347	8766.501472	26.286260
206.203161	8783.665421	26.291277
206.412795	8799.240311	26.296295
206.797518	8819.349546	26.301312
207.242758	8834.013420	26.306330
207.353858	8844.878139	26.311348
207.705096	8861.515703	26.316365
208.020836	8870.336807	26.321383
207.686231	8880.109514	26.326400
208.539347	8889.121179	26.331418
208.615191	8911.515069	26.336436
209.021619	8920.926509	26.341453
209.496836	8929.606939	26.346471
209.341306	8934.177410	26.351488
209.582634	8937.469978	26.356506
210.051970	8951.369550	26.361524
210.333281	8956.919379	26.366541
210.310859	8965.567809	26.371559
210.129905	8974.159674	26.376576
210.370901	8985.349649	26.381594
210.686654	8994.161382	26.386612
210.454431	8999.114747	26.391629
210.840587	9017.070947	26.396647
210.895324	9029.557232	26.401664
211.292706	9042.827787	26.406682
211.333133	9065.906293	26.411700
211.796038	9087.095706	26.416717
212.142277	9091.612992	26.421735
211.824078	9113.475854	26.426752
212.582154	9123.603754	26.431770
212.722372	9131.017206	26.436788
212.640970	9152.638164	26.441805
213.195095	9155.136069	26.446823
213.114778	9164.024025	26.451840
213.321473	9182.838872	26.456858
213.725494	9189.758197	26.461876
214.049191	9207.490858	26.466893
214.064471	9203.370621	26.471911
214.459909	9225.762824	26.476928
214.894359	9223.547474	26.481946
215.139935	9238.902255	26.486964
215.034010	9254.551531	26.491981
215.239689	9255.196241	26.496999
215.537704	9267.490092	26.502016
215.585185	9286.045571	26.507034
216.004797	9290.298609	26.512052
216.202536	9301.743608	26.517069
216.252173	9312.103401	26.522087
216.031851	9333.509889	26.527104
216.888457	9334.853930	26.532122
216.931274	9359.242793	26.537140
216.749666	9368.812785	26.542157
217.172388	9376.984813	26.547175
217.376137	9391.648383	26.552192
217.628947	9403.441568	26.557210
217.784906	9422.746819	26.562228
218.249273	9440.523043	26.567245
218.347221	9451.615371	26.572263
218.495695	9465.013334	26.577280
218.874783	9476.464971	26.582298
218.953114	9490.173972	26.587316
219.106083	9507.850392	26.592333
219.575761	9513.891770	26.597351
219.310715	9532.819242	26.602368
219.807057	9547.749144	26.607386
220.065396	9569.656120	26.612404
220.513269	9591.489239	26.617421
220.632271	9591.630739	26.622439
220.558689	9613.718968	26.627456
221.045084	9626.476518	26.632474
221.238407	9626.141463	26.637492
221.142467	9659.924623	26.642509
221.727951	9667.950064	26.647527
221.844290	9681.986465	26.652544
222.312729	9686.223572	26.657562
222.614005	9704.691498	26.662580
222.638142	9719.190816	26.667597
223.115766	9716.907917	26.672615
223.444716	9730.415069	26.677632
223.441062	9737.734496	26.682650
223.911276	9740.521717	26.687668
223.851947	9750.870457	26.692685
224.300663	9764.052412	26.697703
224.464784	9772.235581	26.702720
224.776789	9776.920653	26.707738
224.652219	9788.773119	26.712756
224.750045	9801.290558	26.717773
225.209762	9807.668505	26.722791
225.507012	9806.369745	26.727808
225.508596	9823.003518	26.732826
225.916037	9829.728211	26.737844
225.908565	9846.527540	26.742861
226.032605	9846.438047	26.747879
226.050475	9855.645622	26.752896
226.126869	9864.902897	26.757914
226.528763	9886.197212	26.762932
226.311097	9908.483158	26.767949
226.871808	9917.110796	26.772967
226.939968	9947.470613	26.777984
227.191665	9969.604312	26.783002
227.779482	9969.207940	26.788020
227.765759	9991.781806	26.793037
228.162216	10005.301661	26.798055
228.261865	10029.847426	26.803072
228.432034	10038.732958	26.808090
228.730219	10058.211921	26.813108
229.176980	10069.454116	26.818125
229.435471	10083.765718	26.823143
229.832194	10107.981330	26.828160
229.753445	10116.943575	26.833178
230.192070	10130.659868	26.838196
230.122624	10155.100969	26.843213
230.478773	10168.090661	26.848231
230.489673	10181.699679	26.853248
230.601530	10203.772198	26.858266
231.025140	10224.223796	26.863284
231.156805	10249.556544	26.868301
231.524180	10257.864587	26.873319
231.702982	10278.323408	26.878336
231.763272	10294.732703	26.883354
232.556623	10314.440001	26.888372
232.577324	10334.148108	26.893389
232.784439	10348.678677	26.898407
233.267578	10354.116582	26.903424
233.466976	10375.412782	26.908442
233.600698	10381.613132	26.913460
233.738115	10409.326146	26.918477
234.207652	10414.429792	26.923495
234.103769	10426.964950	26.928512
234.305367	10443.695808	26.933530
234.815395	10458.927046	26.938548
234.625949	10480.335352	26.943565
235.078402	10492.842878	26.948583
235.579247	10507.205185	26.953600
235.800409	10514.014579	26.958618
236.077906	10532.824552	26.963636
236.214513	10540.819312	26.968653
236.579597	10552.621083	26.973671
237.002411	10569.379780	26.978688
237.065188	10577.097491	26.983706
237.451807	10574.758143	26.988724
237.775333	10580.520643	26.993741
238.026038	10598.029689	26.998759
238.223181	10603.036336	27.003776
238.169759	10611.820510	27.008794
238.377127	10607.496519	27.013812
238.274379	10639.257151	27.018829
238.684061	10638.950551	27.023847
238.872259	10657.511261	27.028864
238.480426	10667.609837	27.033882
239.160248	10685.630623	27.038900
239.477228	10697.619619	27.043917
239.397865	10721.060539	27.048935
239.857154	10742.953721	27.053952
240.065091	10763.651357	27.058970
240.446954	10774.694682	27.063988
240.391144	10804.347583	27.069005
240.792066	10807.466379	27.074023
241.091809	10829.557479	27.079040
241.480736	10843.457855	27.084058
241.978183	10861.772762	27.089076
242.206439	10876.337856	27.094093
242.281281	10885.497625	27.099111
242.519061	10912.745181	27.104128
242.787235	10916.124420	27.109146
243.229953	10931.102028	27.114164
243.078652	10937.831678	27.119181
243.720376	10956.923339	27.124199
243.903002	10966.685381	27.129216
243.768298	10979.076764	27.134234
244.043425	10999.038357	27.139252
244.198891	11015.445463	27.144269
244.678782	11029.565658	27.149287
244.923410	11034.120592	27.154304
245.081190	11064.276723	27.159322
245.498771	11075.451523	27.164340
245.552559	11101.724078	27.169357
245.735591	11109.642873	27.174375
246.209793	11131.160000	27.179392
246.208426	11148.568982	27.184410
246.513837	11157.162476	27.189428
246.654502	11184.908468	27.194445
246.747289	11200.157381	27.199463
247.068258	11220.921054	27.204480
247.162140	11251.766778	27.209498
247.760201	11258.169143	27.214516
247.925860	11281.323164	27.219533
248.631796	11283.268733	27.224551
249.176733	11299.922595	27.229568
249.300260	11311.735919	27.234586
250.042014	11313.651778	27.239604
250.091527	11322.989594	27.244621
249.970029	11335.081259	27.249639
249.698311	11335.683116	27.254656
250.026272	11355.723730	27.259674
250.382891	11365.621612	27.264692
250.475122	11381.718860	27.269709
250.933661	11401.112019	27.274727
251.003134	11408.554991	27.279744
250.992702	11426.143811	27.284762
251.335091	11437.886339	27.289780
251.706411	11452.629494	27.294797
251.929794	11464.744997	27.299815
252.529914	11485.315193	27.304832
252.433075	11500.714859	27.309850
252.761339	11500.587692	27.314868
252.960455	11528.520781	27.319885
252.906653	11544.034250	27.324903
253.528885	11559.455918	27.329920
253.452415	11584.665483	27.334938
253.705606	11599.688527	27.339956
253.918293	11625.549814	27.344973
254.392814	11644.166057	27.349991
254.651047	11656.483160	27.355008
255.229083	11660.000504	27.360026
256.308328	11648.556633	27.365044
256.495703	11663.474530	27.370061
256.276921	11660.266952	27.375079
257.106619	11662.106859	27.380096
257.141939	11686.790912	27.385114
257.464612	11690.223427	27.390132
257.806518	11689.165329	27.395149
258.025572	11693.064965	27.400167
258.271686	11691.709269	27.405184
258.097527	11688.675601	27.410202
258.631565	11696.019874	27.415220
258.863351	11706.515007	27.420237
258.881602	11711.457269	27.425255
259.113113	11710.043491	27.430272
259.052879	11732.834961	27.435290
259.060626	11740.134649	27.440308
259.322938	11753.681396	27.445325
259.559128	11774.760799	27.450343
260.051761	11789.383807	27.455360
259.664315	11822.322356	27.460378
260.486839	11830.136256	27.465396
260.351179	11843.951357	27.470413
260.415952	11869.616843	27.475431
260.799631	11886.628031	27.480448
260.857852	11924.686443	27.485466
261.236304	11938.525156	27.490484
261.501313	11962.783829	27.495501
261.724296	11986.623617	27.500519
262.369639	12009.002170	27.505536
262.142228	12029.944878	27.510554
262.705287	12043.880199	27.515572
263.016660	12078.011354	27.520589
263.168087	12090.714396	27.525607
263.341673	12116.680158	27.530624
263.769316	12129.955707	27.535642
264.332754	12147.023543	27.540660
264.668412	12156.693879	27.545677
264.687561	12175.068712	27.550695
265.217681	12182.227303	27.555712
265.218147	12207.955757	27.560730
265.519134	12218.391218	27.565748
266.137173	12229.164000	27.570765
265.913136	12253.615021	27.575783
266.623244	12253.085581	27.580800
267.074623	12276.020055	27.585818
267.238355	12278.714541	27.590836
267.329754	12293.627498	27.595853
267.415408	12307.382359	27.600871
268.163769	12309.305372	27.605888
268.068622	12328.906042	27.610906
268.401994	12335.273728	27.615924
268.601083	12353.427057	27.620941
268.626543	12370.868978	27.625959
269.119261	12374.323744	27.630976
269.309364	12396.231926	27.635994
269.493050	12415.537371	27.641012
270.064267	12438.731829	27.646029
270.130737	12445.193068	27.651047
271.048985	12459.071964	27.656064
271.040125	12461.335886	27.661082
271.203459	12468.953918	27.666100
271.936970	12486.630831	27.671117
271.670156	12496.373993	27.676135
272.096942	12512.837867	27.681152
272.197672	12520.397817	27.686170
272.275809	12531.372577	27.691188
272.691551	12559.026666	27.696205
272.828214	12565.764464	27.701223
272.956356	12590.960599	27.706240
273.188657	12611.192866	27.711258
273.554644	12629.182175	27.716276
273.614143	12643.127076	27.721293
273.919639	12666.483485	27.726311
274.604445	12688.947080	27.731328
274.604034	12705.529039	27.736346
274.869812	12729.281704	27.741364
275.186658	12745.307799	27.746381
275.311269	12765.996068	27.751399
275.584920	12780.903281	27.756416
275.888355	12804.308837	27.761434
276.077756	12830.994515	27.766452
276.479381	12848.007269	27.771469
276.662247	12884.596332	27.776487
276.934340	12892.007934	27.781504
277.213515	12914.577938	27.786522
277.416700	12932.093620	27.791540
277.835310	12948.647824	27.796557
278.095324	12979.911677	27.801575
278.436447	13006.010177	27.806592
278.695022	13017.883004	27.811610
279.024574	13039.327115	27.816628
279.224843	13053.869935	27.821645
279.105613	13072.349081	27.826663
279.117246	13092.872394	27.831680
279.402622	13128.243226	27.836698
280.087811	13149.555734	27.841716
280.431586	13171.027872	27.846733
280.679607	13194.583958	27.851751
281.115085	13209.020070	27.856768
281.332477	13233.372882	27.861786
281.622233	13259.650621	27.866804
282.092037	13262.146645	27.871821
282.328408	13284.250761	27.876839
282.273264	13301.166698	27.881856
282.784533	13322.820067	27.886874
283.172788	13341.631327	27.891892
283.490297	13360.998705	27.896909
283.419770	13393.824499	27.901927
283.884801	13411.575295	27.906944
284.106446	13441.205153	27.911962
284.605666	13452.771245	27.916980
285.079840	13465.922179	27.921997
285.148998	13479.419288	27.927015
285.493975	13502.789974	27.932032
285.904416	13520.051217	27.937050
286.270760	13540.638051	27.942068
286.529851	13553.603227	27.947085
286.845559	13586.190564	27.952103
286.939853	13584.412082	27.957120
287.256670	13597.446222	27.962138
287.359411	13616.771897	27.967156
287.839747	13631.697383	27.972173
288.153665	13660.837305	27.977191
288.342226	13669.718891	27.982208
288.904205	13695.326806	27.987226
289.267355	13702.889699	27.992244
289.814595	13728.028495	27.997261
289.698100	13739.269037	28.002279
290.031686	13739.850272	28.007296
290.229364	13757.111845	28.012314
290.748175	13772.319547	28.017332
291.152939	13785.877975	28.022349
291.311799	13796.001044	28.027367
291.742351	13806.858859	28.032384
292.220927	13828.174846	28.037402
292.329945	13833.680244	28.042420
292.678116	13850.392289	28.047437
292.947709	13859.177235	28.052455
293.054370	13865.790406	28.057472
293.259200	13891.949439	28.062490
293.230877	13908.290071	28.067508
293.757415	13924.752765	28.072525
293.868221	13941.730831	28.077543
294.186380	13958.304213	28.082560
294.093213	13972.413993	28.087578
294.139126	14002.645637	28.092596
294.725854	14020.383455	28.097613
295.020709	14051.311750	28.102631
295.395216	14075.597472	28.107648
296.169663	14078.310075	28.112666
296.440466	14094.519394	28.117684
296.959930	14100.144540	28.122701
297.327431	14108.546007	28.127719
297.685097	14114.592247	28.132736
297.833973	14114.578386	28.137754
297.925807	14125.170118	28.142772
298.386015	14129.964597	28.147789
298.167279	14146.923481	28.152807
298.736939	14161.574194	28.157824
299.181765	14170.570114	28.162842
298.755721	14203.878415	28.167860
299.656326	14207.808335	28.172877
299.814017	14235.130801	28.177895
299.922732	14240.489087	28.182912
300.291428	14263.738093	28.187930
300.214415	14294.052880	28.192948
300.895194	14312.969078	28.197965
300.568133	14342.397651	28.202983
300.874230	14358.162062	28.208000
301.406915	14382.003768	28.213018
301.223308	14425.253217	28.218036
302.015650	14442.208535	28.223053
302.524705	14475.351566	28.228071
302.627944	14491.477309	28.233088
303.269530	14515.545613	28.238106
303.495205	14549.602280	28.243124
303.807840	14566.568948	28.248141
303.859491	14597.361948	28.253159
304.048616	14622.067861	28.258176
304.286098	14641.321102	28.263194
304.619161	14674.808393	28.268212
305.051592	14693.368761	28.273229
305.232551	14737.232991	28.278247
306.025002	14748.511952	28.283264
305.947742	14774.881196	28.288282
306.437934	14803.337464	28.293300
306.856401	14821.486616	28.298317
306.947336	14848.246912	28.303335
307.191148	14873.945496	28.308352
307.517973	14887.920987	28.313370
307.684996	14931.328633	28.318388
308.306069	14953.841651	28.323405
308.783178	14986.722428	28.328423
308.825135	15005.697996	28.333440
309.391373	15019.441590	28.338458
309.455091	15054.766984	28.343476
309.879860	15068.315787	28.348493
310.167358	15092.567589	28.353511
310.553353	15131.575955	28.358528
311.155073	15132.261146	28.363546
310.976440	15177.204916	28.368564
311.559366	15183.557649	28.373581
312.558747	15188.395845	28.378599
312.294585	15201.397001	28.383616
312.882846	15208.306769	28.388634
312.975237	15226.086690	28.393652
313.274225	15224.923710	28.398669
313.592300	15258.346565	28.403687
313.385723	15267.942138	28.408704
314.379675	15288.426780	28.413722
314.180444	15304.152739	28.418740
314.293373	15329.657430	28.423757
314.785813	15347.358581	28.428775
315.035324	15361.980284	28.433792
315.559958	15380.231368	28.438810
315.683742	15421.966957	28.443828
316.108571	15429.907729	28.448845
316.139964	15463.659644	28.453863
316.326747	15493.793536	28.458880
317.265422	15507.432456	28.463898
316.639429	15556.296843	28.468916
317.330410	15577.152154	28.473933
317.338455	15604.972387	28.478951
317.641488	15628.524436	28.483968
318.189218	15661.123002	28.488986
318.530661	15698.002128	28.494004
319.311464	15717.189026	28.499021
319.460190	15745.186277	28.504039
319.950265	15775.750075	28.509056
320.394162	15785.033279	28.514074
320.514600	15810.883880	28.519092
320.941104	15834.807656	28.524109
321.067879	15855.374572	28.529127
321.333016	15882.099750	28.534144
321.498011	15903.332008	28.539162
321.766009	15940.522593	28.544180
322.187383	15959.895209	28.549197
322.678535	15991.926598	28.554215
322.840966	16024.444441	28.559232
323.555690	16046.988527	28.564250
323.819739	16074.138373	28.569268
324.222561	16098.815652	28.574285
324.510615	16114.260964	28.579303
324.859377	16144.393146	28.584320
324.970216	16158.898745	28.589338
325.255709	16188.092385	28.594356
325.990642	16202.233636	28.599373
326.239523	16226.475665	28.604391
326.401258	16254.507787	28.609408
326.856897	16266.996940	28.614426
327.161850	16301.241089	28.619444
327.434942	16325.801232	28.624461
327.862009	16341.507266	28.629479
328.787206	16355.964367	28.634496
329.097321	16359.579464	28.639514
329.196018	16366.590907	28.644532
329.708782	16375.167108	28.649549
329.879779	16392.872075	28.654567
329.962757	16399.654171	28.659584
330.565912	16406.317157	28.664602
330.543166	16420.365991	28.669620
330.485016	16433.796524	28.674637
331.041877	16450.177391	28.679655
331.355143	16469.376165	28.684672
331.668410	16481.790553	28.689690
331.944019	16511.183212	28.694708
331.970918	16544.354991	28.699725
332.582299	16558.918786	28.704743
332.230464	16586.306645	28.709760
332.979185	16615.998288	28.714778
333.053360	16643.519326	28.719796
333.317647	16671.573260	28.724813
333.901059	16702.623786	28.729831
334.120294	16731.729217	28.734848
334.691042	16751.758895	28.739866
334.714937	16781.468538	28.744884
335.257143	16812.683320	28.749901
335.752481	16832.899912	28.754919
335.947161	16868.999968	28.759936
335.913616	16897.559420	28.764954
336.368067	16921.767419	28.769972
336.868367	16956.672002	28.774989
337.431295	16983.636260	28.780007
337.548904	17018.118139	28.785024
338.111815	17044.495729	28.790042
338.499774	17076.347007	28.795060
338.805045	17094.736262	28.800077
339.113043	17115.163187	28.805095
339.218525	17153.838025	28.810112
339.446184	17177.594992	28.815130
340.203419	17215.417340	28.820148
340.365951	17243.503879	28.825165
340.868792	17260.401282	28.830183
341.176460	17294.285402	28.835200
341.874317	17313.557199	28.840218
342.046502	17339.971575	28.845236
342.169710	17359.193670	28.850253
342.539572	17382.100761	28.855271
342.749840	17416.181765	28.860288
343.292543	17445.463164	28.865306
343.604908	17467.306349	28.870324
344.118560	17491.275694	28.875341
344.302957	17519.542315	28.880359
344.501014	17540.680216	28.885376
344.836430	17566.452446	28.890394
345.152900	17596.882362	28.895412
345.225264	17626.545348	28.900429
346.179525	17646.488893	28.905447
346.354834	17679.281186	28.910464
346.596077	17700.974619	28.915482
347.005414	17728.842789	28.920500
347.498523	17757.442139	28.925517
348.555048	17764.924016	28.930535
348.913528	17778.584790	28.935552
349.065235	17776.839300	28.940570
349.355412	17792.237331	28.945588
349.549484	17815.723859	28.950605
350.127864	17822.445745	28.955623
350.194169	17851.425484	28.960640
350.273130	17861.231287	28.965658
350.302538	17879.510711	28.970676
350.774122	17897.572450	28.975693
351.328218	17918.277752	28.980711
351.450599	17954.802288	28.985728
351.816424	17970.299859	28.990746
352.192716	18005.708065	28.995764
352.152856	18038.899974	29.000781
352.942671	18055.845038	29.005799
352.606488	18093.357546	29.010816
353.184364	18123.682665	29.015834
353.566106	18151.455991	29.020852
353.821018	18177.747190	29.025869
354.310630	18217.852071	29.030887
354.507544	18261.098644	29.035904
354.999683	18285.661243	29.040922
355.443194	18315.447505	29.045940
355.867864	18353.431929	29.050957
356.652963	18377.556247	29.055975
357.114600	18407.641382	29.060992
357.110155	18435.279109	29.066010
357.422164	18455.865040	29.071028
357.572748	18489.139768	29.076045
357.861275	18511.384692	29.081063
358.404740	18550.712135	29.086080
358.635186	18572.766000	29.091098
359.240844	18604.829042	29.096116
359.584808	18631.896616	29.101133
360.379301	18646.139493	29.106151
360.797840	18677.403725	29.111168
361.076540	18706.530352	29.116186
361.525686	18719.177851	29.121204
361.271636	18751.250229	29.126221
361.872908	18772.090501	29.131239
362.233165	18797.919086	29.136256
362.429863	18834.729527	29.141274
362.851779	18859.036490	29.146292
363.125657	18903.494700	29.151309
363.573127	18921.159481	29.156327
363.635558	18962.807673	29.161344
363.971042	18991.024148	29.166362
364.265766	19023.022236	29.171380
364.758591	19065.106091	29.176397
365.194474	19094.785210	29.181415
364.954568	19133.787738	29.186432
365.212672	19165.147414	29.191450
365.860759	19201.435574	29.196468
365.821734	19240.144525	29.201485
366.283989	19265.644613	29.206503
366.940598	19305.065389	29.211520
367.405298	19341.670130	29.216538
368.256635	19377.181756	29.221556
368.365291	19403.691653	29.226573
369.004712	19433.397256	29.231591
369.055197	19474.030110	29.236608
369.084508	19502.334882	29.241626
369.841636	19525.172397	29.246644
370.070591	19563.705574	29.251661
370.885452	19594.064307	29.256679
370.796458	19624.599017	29.261696
371.206380	19657.252561	29.266714
372.040121	19687.390727	29.271732
372.296142	19716.379134	29.276749
373.212952	19722.439590	29.281767
373.539459	19755.044025	29.286784
374.021310	19775.570379	29.291802
374.338856	19797.699507	29.296820
374.619016	19812.942454	29.301837
375.301400	19830.030611	29.306855
375.768810	19853.941277	29.311872
375.503979	19870.850055	29.316890
375.996214	19892.924313	29.321908
376.190823	19923.066733	29.326925
376.630711	19939.951888	29.331943
376.950096	19974.108901	29.336960
377.027322	19997.672456	29.341978
377.775831	20030.556332	29.346996
377.779493	20058.866983	29.352013
378.386995	20084.575218	29.357031
378.678041	20115.413763	29.362048
378.717388	20153.809682	29.367066
379.260077	20183.349029	29.372084
379.574510	20220.701923	29.377101
380.194915	20252.780178	29.382119
380.573809	20287.463510	29.387136
380.745710	20316.244350	29.392154
381.427965	20350.849558	29.397172
381.375868	20398.258890	29.402189
381.987214	20413.850501	29.407207
383.031269	20421.531774	29.412224
383.407353	20449.999965	29.417242
384.196646	20461.858738	29.422260
384.013339	20494.018300	29.427277
384.659212	20514.067447	29.432295
384.852046	20535.199210	29.437312
385.083969	20563.727592	29.442330
385.840103	20578.344170	29.447348
385.727331	20611.581893	29.452365
386.237789	20633.248319	29.457383
386.722270	20670.218433	29.462400
386.743986	20690.918537	29.467418
387.206084	20708.136869	29.472436
387.510517	20738.465359	29.477453
387.883413	20776.101650	29.482471
388.038857	20797.138918	29.487488
388.243306	20824.122260	29.492506
388.886739	20845.433084	29.497524
388.729029	20892.470108	29.502541
389.268701	20919.860130	29.507559
389.684559	20954.100379	29.512576
390.100613	20997.916558	29.517594
390.397275	21015.352963	29.522612
390.832112	21047.370269	29.527629
390.990678	21094.527613	29.532647
391.384950	21136.190519	29.537664
391.842767	21170.409589	29.542682
392.673099	21203.449460	29.547700
392.697905	21245.997683	29.552717
392.957616	21286.117528	29.557735
393.256334	21326.360422	29.562752
393.806018	21363.286335	29.567770
394.376654	21410.422283	29.572788
394.879185	21450.322714	29.577805
394.847637	21484.484975	29.582823
395.383927	21533.079847	29.587840
395.667081	21569.769120	29.592858
396.610053	21604.921516	29.597876
397.335279	21630.689925	29.602893
397.513971	21660.940991	29.607911
398.085109	21696.237109	29.612928
398.357494	21731.978641	29.617946
398.659460	21753.748353	29.622964
398.984320	21794.504937	29.627981
399.445165	21820.476452	29.632999
400.042610	21849.241908	29.638016
400.033288	21894.147505	29.643034
400.885044	21910.850627	29.648052
401.248731	21952.631615	29.653069
401.643030	21987.517866	29.658087
402.067761	22012.079337	29.663104
402.223519	22049.944654	29.668122
403.238896	22079.732417	29.673140
403.850807	22102.648031	29.678157
404.533207	22123.032089	29.683175
404.856353	22150.985667	29.688192
405.098051	22165.380103	29.693210
405.402736	22173.799913	29.698228
405.652618	22212.813930	29.703245
405.829744	22233.733880	29.708263
406.904512	22257.487246	29.713280
407.031708	22281.258517	29.718298
407.375850	22299.004615	29.723316
407.505355	22338.404365	29.728333
407.692735	22363.537421	29.733351
408.023933	22389.792022	29.738368
408.087125	22433.418731	29.743386
408.845442	22456.655726	29.748404
409.469893	22482.824377	29.753421
409.398114	22515.008082	29.758439
409.652617	22535.926342	29.763456
410.245621	22583.216604	29.768474
410.401878	22616.641726	29.773492
410.697675	22652.120900	29.778509
411.173776	22685.276244	29.783527
411.893891	22710.276925	29.788544
412.120453	22743.305168	29.793562
412.841141	22772.382695	29.798580
413.138432	22805.607737	29.803597
413.555455	22840.056680	29.808615
414.317167	22861.285232	29.813632
414.477843	22912.084231	29.818650
415.134867	22936.452599	29.823668
415.260423	22962.106065	29.828685
415.384515	23009.721209	29.833703
415.721898	23036.508352	29.838720
415.849562	23085.500766	29.843738
416.406545	23123.243284	29.848756
417.448595	23157.831996	29.853773
418.382283	23175.827783	29.858791
418.675028	23204.237820	29.863808
418.718525	23232.057486	29.868826
419.118070	23263.398850	29.873844
419.970414	23305.934181	29.878861
420.081669	23339.072618	29.883879
420.685954	23366.877214	29.888896
420.826155	23395.033060	29.893914
421.253290	23426.540488	29.898932
421.692402	23461.500827	29.903949
422.001682	23498.189617	29.908967
422.635502	23526.921614	29.913984
422.626265	23569.235738	29.919002
423.010090	23599.731935	29.924020
423.423545	23647.660495	29.929037
423.514747	23687.738440	29.934055
424.056123	23723.263588	29.939072
424.236293	23772.318280	29.944090
424.746105	23816.179313	29.949108
425.215251	23870.444560	29.954125
425.678929	23920.655779	29.959143
426.327542	23951.683910	29.964160
426.565601	23999.423279	29.969178
427.019282	24043.808253	29.974196
427.699333	24083.985578	29.979213
427.623129	24125.331148	29.984231
428.294020	24164.583000	29.989248
428.794792	24215.996803	29.994266
428.902734	24254.168808	29.999284
429.552713	24291.176159	30.004301
429.900958	24342.291705	30.009319
430.347979	24385.679860	30.014336
430.952174	24434.678484	30.019354
431.457416	24466.378760	30.024372
432.013367	24507.641933	30.029389
432.068276	24547.183496	30.034407
432.972552	24575.965677	30.039424
433.188472	24617.158057	30.044442
433.340568	24653.232543	30.049460
434.000320	24692.129050	30.054477
434.478798	24727.989432	30.059495
434.859108	24766.954273	30.064512
435.100054	24810.963283	30.069530
435.494814	24849.018540	30.074548
436.048576	24886.222208	30.079565
436.208479	24934.540061	30.084583
437.162225	24969.873100	30.089600
437.299142	25025.867601	30.094618
437.682744	25067.264450	30.099636
438.616801	25100.971834	30.104653
438.868429	25147.938103	30.109671
439.003781	25187.176958	30.114688
439.528920	25214.699618	30.119706
440.227713	25251.268937	30.124724
440.927435	25298.162683	30.129741
441.219770	25341.471727	30.134759
441.855776	25370.740812	30.139776
442.201958	25416.399282	30.144794
442.963097	25446.162199	30.149812
443.562802	25466.262807	30.154829
444.041617	25502.286367	30.159847
444.526675	25532.555854	30.164864
444.718134	25558.385758	30.169882
445.317085	25591.367662	30.174900
445.750327	25627.945486	30.179917
445.675149	25664.641418	30.184935
446.541681	25686.573152	30.189952
447.007750	25732.667189	30.194970
447.391911	25772.646174	30.199988
447.565516	25803.314783	30.205005
447.750584	25836.983123	30.210023
448.138642	25875.998270	30.215040
448.658129	25925.719247	30.220058
448.884029	25962.945350	30.225076
449.563175	26008.995206	30.230093
449.940458	26041.509156	30.235111
450.744458	26082.933039	30.240128
450.849354	26133.160302	30.245146
451.359144	26172.286765	30.250164
452.009202	26208.733683	30.255181
452.757412	26240.895878	30.260199
453.201512	26271.554588	30.265216
453.890016	26308.398182	30.270234
454.241718	26344.510848	30.275252
454.601737	26372.961495	30.280269
455.045757	26413.625821	30.285287
455.621608	26437.862009	30.290304
455.853677	26475.635066	30.295322
455.976999	26514.616732	30.300340
456.341983	26542.958956	30.305357
456.727767	26581.140290	30.310375
457.361035	26613.442870	30.315392
457.496567	26648.740584	30.320410
458.110272	26695.258989	30.325428
458.552704	26725.389403	30.330445
458.437473	26776.470727	30.335463
459.200974	26807.125270	30.340480
459.797084	26858.095894	30.345498
459.899396	26893.735846	30.350516
460.495244	26938.937368	30.355533
460.856369	26997.216924	30.360551
461.432620	27030.145524	30.365568
461.561327	27086.902480	30.370586
462.082149	27128.515984	30.375604
463.241963	27171.652367	30.380621
463.576487	27215.315847	30.385639
463.987994	27249.741291	30.390656
464.424609	27296.122613	30.395674
464.725924	27347.517558	30.400692
465.552374	27380.378652	30.405709
465.695923	27430.703854	30.410727
466.282442	27473.415530	30.415744
466.746812	27517.880108	30.420762
467.356274	27574.601583	30.425780
468.091032	27603.826705	30.430797
468.158114	27652.735563	30.435815
468.724865	27690.849723	30.440832
469.250897	27728.318090	30.445850
469.775085	27779.696237	30.450868
470.467945	27815.017230	30.455885
470.800868	27853.730003	30.460903
471.359829	27894.406538	30.465920
471.853960	27940.102955	30.470938
472.088462	27976.091392	30.475956
472.816536	28019.190092	30.480973
473.176763	28071.480884	30.485991
473.478209	28109.130884	30.491008
474.425852	28150.433200	30.496026
474.558158	28191.268269	30.501044
474.940081	28227.979143	30.506061
475.157916	28275.649327	30.511079
475.702183	28322.569557	30.516096
476.210579	28363.346723	30.521114
476.605268	28412.824986	30.526132
477.404073	28457.442151	30.531149
477.742525	28500.769663	30.536167
478.413337	28544.871669	30.541184
478.923141	28581.063426	30.546202
478.874310	28631.527004	30.551220
479.498384	28671.139289	30.556237
480.152924	28727.562932	30.561255
480.544786	28768.380166	30.566272
480.719513	28806.067726	30.571290
481.414804	28859.404492	30.576308
481.896331	28894.011383	30.581325
482.183372	28946.729533	30.586343
482.624561	28998.011295	30.591360
483.173269	29023.436039	30.596378
483.655552	29074.194599	30.601396
484.334732	29111.838756	30.606413
484.685229	29160.406002	30.611431
485.075772	29202.009339	30.616448
485.674009	29249.331811	30.621466
485.821794	29306.862536	30.626484
486.269181	29346.920658	30.631501
486.863855	29398.415620	30.636519
487.601465	29444.482499	30.641536
488.310672	29486.054711	30.646554
488.825096	29532.595505	30.651572
489.185353	29575.654493	30.656589
489.571121	29619.574731	30.661607
490.130141	29653.501112	30.666624
490.714501	29702.746631	30.671642
490.906240	29753.577228	30.676660
491.648812	29795.866711	30.681677
492.146694	29847.118473	30.686695
492.710366	29897.474213	30.691712
493.963290	29905.535871	30.696730
494.644739	29947.236609	30.701748
495.117302	29978.832368	30.706765
495.493462	30010.174049	30.711783
496.025661	30039.706904	30.716800
496.636911	30083.444330	30.721818
496.786654	30126.919698	30.726836
497.542687	30144.543462	30.731853
498.206949	30188.234901	30.736871
498.626847	30218.766249	30.741888
499.022217	30246.332343	30.746906
499.331210	30277.585948	30.751924
499.820272	30307.055238	30.756941
499.811544	30351.084412	30.761959
500.463999	30389.222771	30.766976
501.152314	30431.686453	30.771994
501.459295	30482.050211	30.777012
501.929688	30525.617405	30.782029
502.395151	30571.100400	30.787047
502.220465	30609.731943	30.792064
502.910808	30662.104546	30.797082
502.957647	30719.497136	30.802100
503.484021	30769.636126	30.807117
504.545937	30815.962553	30.812135
505.112460	30881.224216	30.817152
505.548683	30917.929346	30.822170
505.837187	30972.225149	30.827188
506.942543	31020.683988	30.832205
507.281553	31063.911039	30.837223
507.544743	31120.137353	30.842240
508.147289	31162.331317	30.847258
508.653020	31214.142474	30.852276
509.134834	31250.327274	30.857293
509.578548	31291.757237	30.862311
509.733163	31340.226610	30.867328
510.766188	31369.278605	30.872346
510.985388	31428.569088	30.877364
511.453671	31469.215401	30.882381
512.083786	31506.715282	30.887399
512.305786	31563.619531	30.892416
513.059986	31616.270292	30.897434
513.368986	31664.240030	30.902452
513.828380	31715.897805	30.907469
514.471465	31769.580225	30.912487
514.967298	31822.225513	30.917504
515.847201	31867.220519	30.922522
516.049071	31914.500348	30.927540
516.212622	31964.882037	30.932557
516.887878	32024.795544	30.937575
517.083680	32080.654433	30.942592
517.813821	32126.577161	30.947610
518.358680	32182.150670	30.952628
519.026182	32247.655438	30.957645
519.477591	32305.269676	30.962663
519.751539	32365.000874	30.967680
520.665306	32421.109087	30.972698
520.935124	32479.690711	30.977716
521.629806	32531.207956	30.982733
522.104364	32591.431329	30.987751
522.187486	32662.415266	30.992768
523.093655	32712.770797	30.997786
523.551014	32768.186827	31.002804
524.330494	32819.691465	31.007821
524.798476	32866.430379	31.012839
525.228814	32926.360947	31.017856
526.291172	32974.151445	31.022874
526.521791	33030.391031	31.027892
527.152236	33078.624205	31.032909
527.998970	33137.570239	31.037927
528.336877	33193.675069	31.042944
529.109798	33239.724913	31.047962
529.466905	33293.300207	31.052980
529.445362	33343.784933	31.057997
530.532706	33390.207568	31.063015
530.875528	33444.435068	31.068032
531.372763	33485.795809	31.073050
531.910013	33551.138903	31.078068
532.598449	33596.772858	31.083085
532.989219	33641.971989	31.088103
533.432435	33699.111598	31.093120
534.598119	33747.318217	31.098138
534.812960	33791.670902	31.103156
535.443440	33848.560509	31.108173
536.152911	33890.763337	31.113191
536.323017	33945.464517	31.118208
537.450072	33975.040534	31.123226
538.274478	34013.574488	31.128244
538.464544	34053.478553	31.133261
538.852320	34085.332156	31.138279
539.244916	34123.471685	31.143296
540.142651	34167.029299	31.148314
540.472998	34204.379698	31.153332
540.750498	34254.482209	31.158349
541.064372	34298.883529	31.163367
541.119003	34354.391070	31.168384
541.698684	34393.184005	31.173402
542.336827	34452.104877	31.178420
542.467952	34510.914387	31.183437
544.263510	34540.604066	31.188455
544.937109	34584.116499	31.193472
545.638395	34620.890107	31.198490
545.857006	34669.444151	31.203508
545.929435	34709.724799	31.208525
546.948992	34748.511561	31.213543
547.798300	34803.143639	31.218560
547.797303	34842.266574	31.223578
548.290768	34896.854740	31.228596
548.773938	34950.366423	31.233613
549.187243	34993.620278	31.238631
549.487940	35060.490431	31.243648
550.176463	35103.669208	31.248666
550.355943	35162.113872	31.253684
550.930454	35228.572190	31.258701
551.613902	35278.835407	31.263719
551.885836	35344.205721	31.268736
552.460300	35403.951996	31.273754
552.876160	35468.060736	31.278772
553.406961	35527.259472	31.283789
554.448474	35589.080820	31.288807
554.673368	35648.525773	31.293824
555.198263	35718.539557	31.298842
555.728679	35786.367665	31.303860
556.536474	35853.341523	31.308877
557.049900	35909.859514	31.313895
557.479773	35966.350012	31.318912
558.221075	36032.784957	31.323930
558.642240	36091.356755	31.328948
559.052999	36160.756781	31.333965
559.973480	36216.395884	31.338983
560.434890	36285.654350	31.344000
560.944755	36344.504574	31.349018
561.587281	36400.644193	31.354036
562.404330	36463.538769	31.359053
563.085036	36530.409443	31.364071
563.475289	36577.160104	31.369088
564.183960	36632.553683	31.374106
564.404550	36694.842522	31.379124
565.128307	36757.656883	31.384141
566.041022	36810.923205	31.389159
566.263627	36875.723980	31.394176
566.939256	36923.139644	31.399194
567.751108	36975.429262	31.404212
568.219064	37025.549144	31.409229
569.630943	37053.959543	31.414247
570.220880	37087.300265	31.419264
570.787176	37124.342107	31.424282
571.538502	37160.884715	31.429300
571.682210	37208.100519	31.434317
572.340574	37239.092432	31.439335
572.576691	37274.173768	31.444352
573.163256	37318.821887	31.449370
573.742522	37362.796462	31.454388
573.797477	37414.140566	31.459405
574.440216	37462.028113	31.464423
574.766489	37527.934341	31.469440
575.391937	37574.227756	31.474458
575.769704	37630.689568	31.479476
576.325590	37701.458765	31.484493
576.776766	37751.723806	31.489511
577.312803	37817.359669	31.494528
577.591914	37881.835229	31.499546
578.217262	37943.130783	31.504564
578.570691	38017.331430	31.509581
579.466048	38081.600814	31.514599
579.871742	38159.402961	31.519616
580.439404	38219.155587	31.524634
581.897290	38277.530458	31.529652
582.206334	38347.330952	31.534669
583.042914	38407.407231	31.539687
583.869516	38454.806311	31.544704
584.910258	38499.646969	31.549722
585.748727	38540.207408	31.554740
585.929612	38595.377702	31.559757
586.809957	38645.402025	31.564775
586.900992	38697.081708	31.569792
587.475688	38749.313674	31.574810
588.210512	38796.800863	31.579828
588.474327	38860.397981	31.584845
589.170374	38911.042173	31.589863
589.692513	38967.543792	31.594880
589.944304	39033.918713	31.599898
590.468819	39086.208590	31.604916
590.762080	39158.952608	31.609933
591.370143	39219.353566	31.614951
591.830359	39283.811918	31.619968
592.499463	39358.624133	31.624986
593.083751	39416.134430	31.630004
593.844804	39482.630265	31.635021
594.123992	39548.906640	31.640039
594.969914	39620.900746	31.645056
595.533218	39691.686522	31.650074
596.188798	39764.160965	31.655092
596.309285	39831.782012	31.660109
597.412419	39890.994784	31.665127
598.343139	39946.997779	31.670144
599.341857	40006.262274	31.675162
599.883035	40051.904098	31.680180
599.926054	40116.417842	31.685197
600.710027	40165.550513	31.690215
601.489012	40233.989228	31.695232
601.556880	40281.246149	31.700250
602.200170	40342.112258	31.705268
602.552094	40406.349242	31.710285
603.222453	40470.081588	31.715303
603.822560	40535.834439	31.720320
604.461540	40596.452976	31.725338
605.256925	40653.057019	31.730356
605.557449	40729.685982	31.735373
606.307036	40790.808005	31.740391
607.044892	40853.644753	31.745408
607.501131	40922.986054	31.750426
608.344166	40983.428381	31.755444
608.530635	41056.150169	31.760461
608.998579	41113.943344	31.765479
609.337267	41187.761147	31.770496
610.104674	41262.085043	31.775514
610.908738	41323.515701	31.780532
611.500553	41411.159655	31.785549
611.808016	41488.424880	31.790567
612.493498	41558.984441	31.795584
612.931685	41637.169456	31.800602
613.819639	41714.888932	31.805620
614.577315	41799.675993	31.810637
615.791778	41847.420176	31.815655
616.800241	41916.851034	31.820672
617.469475	41974.993558	31.825690
618.296750	42029.136763	31.830708
619.179190	42086.841971	31.835725
619.837778	42125.288383	31.840743
620.368517	42185.649041	31.845760
620.962791	42233.177629	31.850778
621.836775	42280.239133	31.855796
622.186191	42346.511981	31.860813
622.645429	42391.621079	31.865831
623.550933	42455.834353	31.870848
623.552150	42512.637231	31.875866
624.787075	42558.553776	31.880884
625.198063	42605.711977	31.885901
625.892430	42664.777053	31.890919
626.469249	42720.252448	31.895936
626.546323	42786.961494	31.900954
627.064636	42851.979177	31.905972
627.777339	42915.417337	31.910989
628.122833	42977.154037	31.916007
628.504768	43048.572410	31.921024
629.017129	43133.745772	31.926042
629.617225	43191.676286	31.931060
630.495290	43270.965809	31.936077
630.550459	43343.058858	31.941095
631.455826	43420.546662	31.946112
631.978411	43497.048466	31.951130
632.686922	43561.319298	31.956148
633.047617	43642.692872	31.961165
633.248593	43718.224791	31.966183
634.214728	43789.581582	31.971200
634.749018	43866.291351	31.976218
635.436412	43933.532229	31.981236
635.858681	43998.884966	31.986253
636.791056	44083.721660	31.991271
637.566417	44163.564747	31.996288
637.938019	44233.999087	32.001306
638.567691	44312.701993	32.006324
639.500829	44408.158739	32.011341
640.350582	44497.076986	32.016359
641.175992	44564.168984	32.021376
641.634162	44654.273460	32.026394
642.537717	44726.596791	32.031412
643.234294	44802.862112	32.036429
643.615542	44866.126728	32.041447
644.520962	44931.320854	32.046464
645.207358	44999.540834	32.051482
646.122668	45072.636652	32.056500
646.590437	45151.318647	32.061517
647.306126	45213.496491	32.066535
648.890153	45250.057870	32.071552
649.584105	45313.665516	32.076570
650.743102	45364.365410	32.081588
650.877101	45412.856204	32.086605
651.540957	45471.393049	32.091623
652.218544	45526.438607	32.096640
652.388070	45571.791389	32.101658
652.913076	45624.984394	32.106676
653.513908	45689.396959	32.111693
653.765411	45748.394751	32.116711
654.829916	45828.581168	32.121728
655.368945	45897.014258	32.126746
656.121442	45967.789311	32.131764
656.763891	46035.931996	32.136781
657.412532	46099.025987	32.141799
658.261060	46160.318427	32.146816
658.746180	46236.891848	32.151834
659.581451	46288.611403	32.156852
659.861208	46368.493004	32.161869
660.293652	46440.816409	32.166887
661.017604	46504.196440	32.171904
661.405913	46585.285903	32.176922
662.063283	46653.119411	32.181940
662.797160	46724.970054	32.186957
663.549746	46808.662291	32.191975
664.176121	46874.636919	32.196992
664.586739	46960.271087	32.202010
665.432331	47043.397482	32.207028
665.902792	47123.681245	32.212045
666.218833	47202.396593	32.217063
666.967757	47274.979087	32.222080
667.540931	47361.621070	32.227098
668.404340	47434.476272	32.232116
669.051654	47514.512789	32.237133
669.417266	47590.467454	32.242151
670.149600	47667.197046	32.247168
670.824699	47758.317841	32.252186
671.649635	47830.767463	32.257204
672.436930	47902.759546	32.262221
672.871304	47972.848660	32.267239
673.492681	48042.141532	32.272256
673.970253	48117.266558	32.277274
674.623883	48179.742450	32.282292
675.700439	48266.674742	32.287309
676.296242	48341.352764	32.292327
677.235623	48416.664275	32.297344
677.862809	48501.921179	32.302362
678.251631	48581.703915	32.307380
678.991206	48655.580979	32.312397
679.643897	48742.396921	32.317415
680.147613	48826.791516	32.322432
680.758162	48911.311500	32.327450
682.057966	48987.767136	32.332468
683.304426	49052.941180	32.337485
683.912840	49134.537409	32.342503
685.045190	49211.254179	32.347520
685.719681	49295.387145	32.352538
686.723899	49354.804118	32.357556
687.308342	49414.007275	32.362573
687.879493	49486.551403	32.367591
688.997212	49543.445401	32.372608
689.430224	49607.034345	32.377626
689.830812	49677.088230	32.382644
690.297055	49737.942738	32.387661
690.985028	49819.005603	32.392679
691.462292	49889.758135	32.397696
692.075450	49979.069905	32.402714
692.896006	50031.165660	32.407732
693.723933	50109.203352	32.412749
693.984949	50184.841786	32.417767
694.616613	50266.540478	32.422784
695.764628	50331.419309	32.427802
696.482884	50418.589579	32.432820
697.118035	50480.801946	32.437837
697.744055	50560.565242	32.442855
698.398790	50623.415609	32.447872
698.753598	50691.767167	32.452890
699.568338	50768.818916	32.457908
700.049592	50844.709098	32.462925
700.592548	50928.529869	32.467943
701.424594	51015.246264	32.472960
702.327396	51103.602335	32.477978
703.149737	51159.898405	32.482996
704.116494	51241.658653	32.488013
704.762897	51319.657936	32.493031
705.687320	51379.621391	32.498048
706.205203	51466.219561	32.503066
706.937349	51528.110840	32.508084
707.533981	51598.058972	32.513101
708.107425	51672.842859	32.518119
708.970102	51733.634723	32.523136
709.304501	51814.406280	32.528154
709.898132	51898.813680	32.533172
710.185849	51982.910390	32.538189
710.632625	52061.014100	32.543207
711.346239	52136.800154	32.548224
711.840448	52230.241775	32.553242
712.517001	52323.231936	32.558260
713.240243	52417.225095	32.563277
713.419571	52521.464877	32.568295
714.300969	52617.030893	32.573312
714.909826	52727.266419	32.578330
715.942820	52835.591888	32.583348
716.335336	52922.346407	32.588365
717.153792	53030.438920	32.593383
718.082919	53135.367703	32.598400
718.859669	53231.215589	32.603418
719.575189	53337.587232	32.608436
720.424194	53432.206361	32.613453
721.070858	53534.067172	32.618471
722.148913	53635.430621	32.623488
723.043809	53742.186400	32.628506
723.632150	53837.190020	32.633524
724.656203	53925.161836	32.638541
725.150296	54025.051709	32.643559
725.838892	54106.714544	32.648576
726.399865	54216.610064	32.653594
726.987111	54317.010674	32.658612
727.611689	54417.753102	32.663629
728.454925	54511.924240	32.668647
729.370524	54605.939146	32.673664
730.334190	54710.637943	32.678682
731.076840	54813.740606	32.683700
732.278856	54904.321357	32.688717
733.113873	54988.108117	32.693735
734.037395	55066.461357	32.698752
734.734034	55177.458487	32.703770
735.290673	55264.914583	32.708788
735.806651	55357.077763	32.713805
736.531324	55450.357195	32.718823
737.569021	55536.377504	32.723840
738.764968	55623.878751	32.728858
739.191673	55706.581620	32.733876
740.057628	55792.431600	32.738893
740.697728	55867.288430	32.743911
741.504361	55946.538451	32.748928
742.398108	56028.657038	32.753946
743.081161	56106.497426	32.758964
744.016794	56188.265975	32.763981
744.572420	56305.160781	32.768999
745.662235	56385.930224	32.774016
745.963583	56467.460050	32.779034
746.798936	56545.312777	32.784052
747.598849	56618.104768	32.789069
747.888623	56704.186472	32.794087
748.429906	56783.457086	32.799104
749.049187	56872.606097	32.804122
749.633053	56954.175182	32.809140
750.836932	57023.030972	32.814157
751.139116	57107.025871	32.819175
751.741593	57181.445755	32.824192
752.269845	57271.207840	32.829210
752.910776	57362.846597	32.834228
753.832468	57459.665901	32.839245
754.450824	57568.199067	32.844263
755.211641	57678.651753	32.849280
756.060694	57780.387132	32.854298
756.854041	57889.203713	32.859316
757.584422	57981.453231	32.864333
758.409408	58088.128615	32.869351
758.987984	58198.199829	32.874368
760.282643	58290.503133	32.879386
761.149610	58378.761240	32.884404
762.264035	58468.249547	32.889421
762.757840	58575.012018	32.894439
763.646511	58652.066369	32.899456
764.364316	58746.730615	32.904474
764.992029	58851.070734	32.909492
765.755845	58932.335735	32.914509
766.543389	59027.770143	32.919527
767.476493	59129.730014	32.924544
768.113285	59224.052813	32.929562
769.206942	59318.499119	32.934580
770.059308	59411.036256	32.939597
770.616717	59505.625698	32.944615
771.428908	59595.319086	32.949632
772.228328	59697.565399	32.954650
772.655703	59796.148956	32.959668
773.729277	59888.293307	32.964685
774.656633	59978.011247	32.969703
775.114306	60075.871569	32.974720
775.801227	60176.597589	32.979738
776.832715	60266.344541	32.984756
777.522232	60356.345274	32.989773
778.156880	60455.856021	32.994791
779.037851	60552.792621	32.999808
780.251434	60646.980266	33.004826
780.744841	60749.514686	33.009844
781.891588	60831.140627	33.014861
782.228094	60926.378650	33.019879
783.098494	61013.388799	33.024896
784.051484	61111.403024	33.029914
784.664535	61200.993702	33.034932
785.727726	61298.511407	33.039949
786.378509	61392.823948	33.044967
787.049553	61484.910752	33.049984
787.533746	61573.604836	33.055002
788.132715	61670.326838	33.060020
788.865266	61759.582226	33.065037
789.926730	61857.295716	33.070055
790.098763	61961.675148	33.075072
791.226619	62044.828229	33.080090
791.793328	62150.235304	33.085108
792.571027	62238.570018	33.090125
793.170656	62336.188974	33.095143
794.275679	62440.365706	33.100160
795.152348	62537.193202	33.105178
795.712745	62647.242895	33.110196
797.074254	62725.482914	33.115213
797.834609	62803.016839	33.120231
798.320178	62886.601111	33.125248
799.000511	62982.044240	33.130266
799.782040	63096.826615	33.135284
800.346619	63193.148181	33.140301
801.305625	63307.628842	33.145319
801.805671	63415.096750	33.150336
802.424952	63529.427548	33.155354
803.121996	63649.096322	33.160372
803.987737	63757.010079	33.165389
804.999379	63864.193823	33.170407
805.772441	63981.964077	33.175424
807.004057	64082.652639	33.180442
807.504038	64198.304405	33.185460
808.885490	64302.845271	33.190477
809.730427	64414.492638	33.195495
810.608272	64527.657650	33.200512
811.393912	64623.332257	33.205530
812.014335	64730.441011	33.210548
813.063228	64834.513457	33.215565
813.672174	64947.265806	33.220583
814.454206	65054.628574	33.225600
815.741323	65156.769911	33.230618
816.372546	65261.785989	33.235636
817.271636	65376.879183	33.240653
818.318072	65471.126865	33.245671
818.576367	65586.007465	33.250688
819.404098	65685.454875	33.255706
820.012596	65807.602107	33.260724
820.844567	65914.876458	33.265741
821.799312	66020.590567	33.270759
822.456011	66142.144785	33.275776
822.984882	66256.218820	33.280794
823.903559	66375.755633	33.285812
825.067793	66490.920674	33.290829
825.604102	66605.504103	33.295847
826.341492	66724.298093	33.300864
827.420293	66829.671563	33.305882
828.088379	66965.591001	33.310900
828.868005	67089.743738	33.315917
829.938685	67187.647263	33.320935
830.752743	67322.787913	33.325952
831.794345	67420.204498	33.330970
833.015296	67512.690814	33.335988
834.384314	67606.796510	33.341005
835.259823	67703.350210	33.346023
835.694417	67788.268457	33.351040
836.924045	67870.761014	33.356058
837.606178	67966.910898	33.361076
838.164748	68051.570502	33.366093
839.175723	68141.010308	33.371111
839.653809	68241.767887	33.376128
840.301521	68332.523572	33.381146
840.849472	68451.244560	33.386164
841.623849	68554.382555	33.391181
842.577702	68656.127919	33.396199
843.386597	68771.985337	33.401216
844.202328	68881.827874	33.406234
844.765925	68991.730107	33.411252
845.454270	69105.776536	33.416269
846.869384	69215.064358	33.421287
847.390842	69351.068002	33.426304
848.181864	69457.531318	33.431322
849.430691	69581.081917	33.436340
850.178038	69680.685779	33.441357
851.129685	69800.734347	33.446375
852.125720	69927.214694	33.451392
853.290912	70032.673876	33.456410
854.221437	70138.948100	33.461428
855.572030	70234.705801	33.466445
856.447906	70339.606128	33.471463
857.508963	70442.550485	33.476480
858.091945	70520.702783	33.481498
858.783550	70622.500086	33.486516
859.730484	70720.074554	33.491533
860.625388	70816.621575	33.496551
861.221290	70928.469232	33.501568
862.413418	71025.443855	33.506586
862.982757	71113.160441	33.511604
863.584122	71207.462490	33.516621
864.351539	71334.992893	33.521639
865.292040	71467.147033	33.526656
866.460493	71558.567709	33.531674
866.979233	71666.634347	33.536692
867.695450	71765.274306	33.541709
868.589297	71877.756011	33.546727
869.076811	72002.807776	33.551744
869.593617	72120.014074	33.556762
870.655512	72254.681650	33.561780
871.520085	72381.211264	33.566797
872.373345	72503.838409	33.571815
872.857416	72627.321243	33.576832
873.923177	72736.981166	33.581850
874.713366	72868.505056	33.586868
875.689834	72989.636937	33.591885
876.687193	73111.328627	33.596903
877.288642	73252.673341	33.601920
878.849167	73362.030482	33.606938
879.413695	73476.974903	33.611956
880.054222	73599.383544	33.616973
880.883198	73711.216080	33.621991
881.469085	73835.922437	33.627008
882.556820	73955.134030	33.632026
883.241538	74076.255724	33.637044
883.980742	74193.476713	33.642061
885.203018	74320.043834	33.647079
885.943972	74445.159023	33.652096
886.474465	74575.187166	33.657114
887.798938	74693.720881	33.662132
888.604718	74819.725464	33.667149
889.988627	74944.229558	33.672167
890.788081	75077.984664	33.677184
891.714252	75192.540088	33.682202
892.715666	75316.961995	33.687220
893.725618	75448.278227	33.692237
894.651726	75559.865432	33.697255
895.270422	75687.611563	33.702272
896.098931	75802.792696	33.707290
897.314049	75928.625306	33.712308
897.656403	76072.527432	33.717325
898.573597	76189.617937	33.722343
899.360453	76328.925999	33.727360
901.075592	76453.424607	33.732378
902.207305	76570.066045	33.737396
903.123279	76695.868853	33.742413
904.039832	76806.560653	33.747431
904.818759	76930.067188	33.752448
905.912551	77054.668350	33.757466
907.032947	77166.846550	33.762484
907.518133	77286.394883	33.767501
908.771332	77410.448264	33.772519
909.442129	77531.219941	33.777536
910.038350	77652.882747	33.782554
911.250431	77781.053248	33.787572
911.980382	77911.943268	33.792589
912.970834	78027.218674	33.797607
913.510654	78164.992111	33.802624
914.233492	78299.867755	33.807642
915.377171	78421.485943	33.812660
916.300926	78558.575182	33.817677
917.411730	78685.433771	33.822695
918.279610	78823.582924	33.827712
919.259026	78940.793081	33.832730
920.414561	79065.579967	33.837748
921.016812	79208.546274	33.842765
921.911328	79329.918717	33.847783
922.825926	79467.950981	33.852800
923.443484	79600.753312	33.857818
924.631139	79728.971460	33.862836
925.160436	79864.811034	33.867853
926.332903	79998.722334	33.872871
926.779314	80138.123094	33.877888
927.952605	80278.863040	33.882906
928.682833	80410.116560	33.887924
929.037207	80545.880967	33.892941
930.292343	80676.015946	33.897959
931.276921	80807.237830	33.902976
932.027960	80949.117832	33.907994
933.287014	81080.797172	33.913012
933.993071	81212.792908	33.918029
935.092368	81353.001927	33.923047
936.144469	81489.154563	33.928064
937.072790	81628.248414	33.933082
937.906313	81765.398531	33.938100
938.745316	81894.874015	33.943117
939.880499	82031.579610	33.948135
940.663307	82171.256549	33.953152
941.399492	82313.432674	33.958170
942.791142	82451.908281	33.963188
943.534270	82591.019033	33.968205
944.588324	82732.382463	33.973223
945.533111	82880.086321	33.978240
946.578818	83024.209476	33.983258
947.862417	83159.204481	33.988276
948.491103	83312.531505	33.993293
949.263548	83444.454874	33.998311
950.132456	83582.648090	34.003328
951.017304	83734.495942	34.008346
951.979655	83886.029081	34.013364
952.987927	84036.772018	34.018381
954.115856	84186.535977	34.023399
954.676815	84346.494599	34.028416
956.897772	84458.619305	34.033434
959.160170	84566.874909	34.038452
960.193147	84682.755752	34.043469
961.626846	84795.026462	34.048487
962.515843	84908.497219	34.053504
963.638020	85016.297933	34.058522
964.606559	85117.712357	34.063540
965.252436	85230.882086	34.068557
966.013978	85337.357111	34.073575
966.764397	85455.114418	34.078592
967.500338	85581.802609	34.083610
968.431168	85695.163419	34.088628
968.926422	85825.274116	34.093645
969.833430	85942.522334	34.098663
970.577628	86076.559481	34.103680
971.473646	86212.957118	34.108698
972.812395	86341.634213	34.113716
973.150665	86476.004012	34.118733
974.322073	86609.135550	34.123751
975.079846	86749.295609	34.128768
975.610560	86890.175620	34.133786
976.694311	87028.496153	34.138804
977.546120	87186.709853	34.143821
978.689861	87316.587322	34.148839
979.987112	87461.781844	34.153856
980.614386	87604.510266	34.158874
981.839660	87731.746697	34.163892
982.811433	87865.050569	34.168909
983.858967	87990.792823	34.173927
984.850340	88114.255586	34.178944
985.979649	88239.455095	34.183962
987.148863	88359.988402	34.188980
987.695327	88498.163539	34.193997
988.860904	88623.612452	34.199015
989.603574	88760.771538	34.204032
990.448954	88896.024316	34.209050
991.582262	89022.062464	34.214068
992.339709	89156.072392	34.219085
993.454584	89299.531238	34.224103
994.448229	89442.605579	34.229120
995.255686	89587.025885	34.234138
996.661246	89713.423149	34.239156
997.151995	89864.188161	34.244173
998.245809	90006.156188	34.249191
999.511340	90152.006200	34.254208
1000.333758	90302.942826	34.259226
1001.207786	90443.873533	34.264244
1001.750706	90600.542236	34.269261
1002.958881	90749.675052	34.274279
1003.972657	90899.560795	34.279296
1004.988668	91061.571264	34.284314
1006.416570	91216.275805	34.289332
1006.986633	91367.190327	34.294349
1007.883500	91526.282241	34.299367
1009.210811	91683.441052	34.304384
1009.679996	91845.272313	34.309402
1011.022603	92004.081730	34.314420
1012.294818	92165.427087	34.319437
1013.200754	92328.198056	34.324455
1013.940392	92485.690080	34.329472
1014.889662	92642.953803	34.334490
1016.294056	92804.940593	34.339508
1017.299686	92963.627075	34.344525
1018.034359	93130.542455	34.349543
1019.160585	93285.688981	34.354560
1020.069147	93460.681674	34.359578
1021.158204	93620.719490	34.364596
1021.962468	93788.862155	34.369613
1023.094324	93945.454544	34.374631
1024.101174	94119.121103	34.379648
1025.141871	94286.774482	34.384666
1026.567821	94446.663424	34.389684
1027.740448	94608.504107	34.394701
1028.546028	94770.385366	34.399719
1030.275962	94928.534149	34.404736
1030.856457	95089.871561	34.409754
1032.193839	95240.842125	34.414772
1033.432530	95392.569513	34.419789
1034.636744	95546.333980	34.424807
1035.846293	95697.612604	34.429824
1036.787247	95849.769979	34.434842
1037.958086	95963.012878	34.439860
1038.529337	96119.817147	34.444877
1039.025379	96251.697485	34.449895
1040.332824	96395.462618	34.454912
1041.007195	96551.051531	34.459930
1042.023725	96694.168967	34.464948
1043.214733	96852.575124	34.469965
1044.227329	96996.099964	34.474983
1045.332092	97146.943137	34.480000
1046.020030	97308.684167	34.485018
1047.259395	97454.649403	34.490036
1048.284484	97619.603389	34.495053
1049.347611	97775.303332	34.500071
1050.461469	97925.460638	34.505088
1051.681751	98094.208176	34.510106
1052.518005	98243.975203	34.515124
1053.748371	98404.916504	34.520141
1054.755879	98563.730682	34.525159
1056.031466	98713.861116	34.530176
1056.727274	98884.241597	34.535194
1057.811163	99042.085280	34.540212
1058.837241	99211.884215	34.545229
1059.714622	99370.730998	34.550247
1061.392821	99529.185777	34.555264
1062.442848	99693.752131	34.560282
1063.436743	99854.703237	34.565300
1064.409651	100010.875584	34.570317
1065.414042	100177.034392	34.575335
1066.886120	100326.675888	34.580352
1067.700711	100497.650468	34.585370
1068.863712	100657.953879	34.590388
1069.955722	100817.928019	34.595405
1070.893640	100983.786821	34.600423
1072.254436	101133.451225	34.605440
1073.242272	101295.027045	34.610458
1074.174997	101458.251548	34.615476
1075.202103	101632.294772	34.620493
1076.200477	101801.509657	34.625511
1077.750187	101962.108561	34.630528
1078.561891	102130.754403	34.635546
1079.839673	102281.046823	34.640564
1080.930266	102445.803384	34.645581
1081.844318	102615.088185	34.650599
1083.321161	102757.815699	34.655616
1084.441872	102931.568947	34.660634
1085.573076	103085.098025	34.665652
1086.828700	103243.025179	34.670669
1087.738240	103401.850047	34.675687
1088.994157	103556.267257	34.680704
1089.838992	103719.496163	34.685722
1091.222531	103876.584577	34.690740
1092.127987	104034.205690	34.695757
1093.402029	104189.763215	34.700775
1094.395904	104344.322170	34.705792
1095.243561	104498.373817	34.710810
1096.344330	104651.031961	34.715828
1097.364661	104800.280270	34.720845
1098.233834	104954.021363	34.725863
1099.193658	105106.268190	34.730880
1100.014078	105263.803407	34.735898
1100.907104	105416.790610	34.740916
1102.190465	105573.260679	34.745933
1103.210086	105745.373584	34.750951
1104.820634	105891.864217	34.755968
1105.809996	106056.510113	34.760986
1106.566172	106214.061810	34.766004
1107.781394	106383.293963	34.771021
1108.652065	106551.012571	34.776039
1109.952407	106711.037810	34.781056
1110.640274	106893.964355	34.786074
1111.866190	107063.807169	34.791092
1113.483841	107230.107966	34.796109
1114.294809	107407.082284	34.801127
1115.261215	107577.476302	34.806144
1116.409998	107750.728577	34.811162
1117.816883	107912.618253	34.816180
1119.036517	108084.026202	34.821197
1120.061177	108258.036027	34.826215
1121.432764	108428.801986	34.831232
1121.981206	108622.694390	34.836250
1123.240796	108818.627228	34.841268
1124.360177	108981.329272	34.846285
1125.049758	109158.696437	34.851303
1126.155146	109337.043132	34.856320
1127.333713	109521.791311	34.861338
1128.695496	109715.607362	34.866356
1129.961454	109899.521649	34.871373
1131.860794	110071.854558	34.876391
1133.043595	110239.726234	34.881408
1134.013900	110419.963231	34.886426
1134.858279	110613.552162	34.891444
1136.353243	110787.511530	34.896461
1136.994753	110961.506561	34.901479
1138.156508	111137.768502	34.906496
1139.411255	111320.207650	34.911514
1140.458071	111502.497636	34.916532
1141.724616	111688.817942	34.921549
1142.319385	111878.455851	34.926567
1143.237673	112060.061397	34.931584
1144.270917	112267.933128	34.936602
1144.862049	112458.759793	34.941620
1146.766454	112655.424562	34.946637
1147.798574	112865.048624	34.951655
1148.608986	113056.275455	34.956672
1149.954292	113267.366064	34.961690
1151.367729	113455.303157	34.966708
1152.911361	113645.202431	34.971725
1154.294058	113846.257993	34.976743
1155.582059	114030.705838	34.981760
1156.598231	114220.554057	34.986778
1157.433983	114400.790620	34.991796
1158.972973	114580.467161	34.996813
1159.879031	114755.364524	35.001831
1160.914469	114917.321142	35.006848
1162.172854	115093.380355	35.011866
1163.134870	115276.622947	35.016884
1164.393800	115451.893189	35.021901
1165.131417	115635.060091	35.026919
1166.152674	115823.539349	35.031936
1167.374822	116015.489201	35.036954
1168.436381	116214.930552	35.041972
1169.753911	116398.941428	35.046989
1170.596152	116603.010856	35.052007
1172.124116	116805.238083	35.057024
1173.344771	116996.442111	35.062042
1174.666159	117188.967488	35.067060
1176.051188	117385.017176	35.072077
1177.184868	117580.202911	35.077095
1178.681537	117763.561944	35.082112
1179.883747	117951.781160	35.087130
1180.660845	118146.666976	35.092148
1182.315052	118334.095299	35.097165
1183.505189	118515.836833	35.102183
1184.910320	118710.139491	35.107200
1185.796466	118890.070421	35.112218
1187.093868	119078.801914	35.117236
1188.531593	119273.445532	35.122253
1189.444223	119475.987817	35.127271
1190.811246	119657.994160	35.132288
1192.256269	119842.268935	35.137306
1192.908085	120046.465472	35.142324
1194.371815	120234.716642	35.147341
1195.271013	120427.263541	35.152359
1196.585528	120622.506707	35.157376
1198.026975	120820.378068	35.162394
1199.139963	121009.995031	35.167412
1200.494849	121195.661451	35.172429
1201.879701	121396.788357	35.177447
1203.084939	121582.645939	35.182464
1204.312669	121774.175247	35.187482
1205.240277	121981.534571	35.192500
1206.674837	122169.512912	35.197517
1207.722891	122374.449743	35.202535
1208.857635	122566.632833	35.207552
1209.800394	122761.646939	35.212570
1210.849197	122979.152622	35.217588
1212.284323	123166.998602	35.222605
1213.146703	123366.500947	35.227623
1214.608356	123569.455990	35.232640
1216.122448	123772.454900	35.237658
1217.619016	123956.091506	35.242676
1219.174292	124148.282448	35.247693
1220.568322	124341.425046	35.252711
1221.531208	124525.961042	35.257728
1223.146659	124707.151919	35.262746
1224.110265	124881.316328	35.267764
1225.521331	125051.838709	35.272781
1226.830596	125230.092430	35.277799
1227.664303	125394.350026	35.282816
1228.764591	125556.450856	35.287834
1229.500920	125744.083918	35.292852
1230.626718	125930.896331	35.297869
1232.009857	126116.529066	35.302887
1232.685535	126300.464113	35.307904
1234.179671	126510.453776	35.312922
1235.287538	126710.841167	35.317940
1236.814531	126894.074836	35.322957
1237.715790	127104.505338	35.327975
1238.742385	127293.952385	35.332992
1240.089201	127485.706051	35.338010
1241.173970	127699.443581	35.343028
1242.286655	127914.369127	35.348045
1243.599716	128116.342994	35.353063
1244.691800	128324.016166	35.358080
1246.137619	128539.755061	35.363098
1247.392405	128748.114976	35.368116
1248.676399	128954.470189	35.373133
1250.315943	129171.133339	35.378151
1251.634619	129375.915259	35.383168
1252.697531	129571.389770	35.388186
1254.019797	129780.088748	35.393204
1255.246620	129994.923579	35.398221
1256.619328	130202.388800	35.403239
1257.802252	130410.493847	35.408256
1259.170099	130609.221121	35.413274
1260.352124	130836.738793	35.418292
1261.987206	131038.049178	35.423309
1263.051437	131237.259914	35.428327
1264.704822	131450.023606	35.433344
1266.205462	131653.260201	35.438362
1267.249995	131863.121059	35.443380
1268.813884	132054.428173	35.448397
1270.169626	132251.192425	35.453415
1271.533293	132457.712751	35.458432
1272.875134	132657.573527	35.463450
1274.242762	132859.382829	35.468468
1275.723163	133052.471095	35.473485
1277.198300	133243.002074	35.478503
1277.975509	133449.318706	35.483520
1279.231547	133642.636676	35.488538
1280.257701	133842.011074	35.493556
1281.322695	134053.988123	35.498573
1282.470541	134264.065600	35.503591
1283.785083	134480.010117	35.508608
1285.233323	134681.629352	35.513626
1286.082970	134892.582419	35.518644
1287.640858	135107.023083	35.523661
1289.018938	135325.561418	35.528679
1289.927712	135543.884551	35.533696
1291.329443	135740.918806	35.538714
1292.101552	135945.175924	35.543732
1293.229587	136151.886895	35.548749
1294.572727	136360.098425	35.553767
1295.435785	136566.372913	35.558784
1296.678443	136788.327121	35.563802
1297.965014	137000.303097	35.568820
1299.406090	137207.453291	35.573837
1300.684574	137428.620962	35.578855
1301.839646	137660.974256	35.583872
1303.630402	137861.509180	35.588890
1305.134514	138088.817413	35.593908
1306.482755	138301.933462	35.598925
1307.560508	138523.534071	35.603943
1309.059452	138746.944963	35.608960
1310.232884	138966.518682	35.613978
1311.859665	139182.067980	35.618996
1313.616355	139380.388117	35.624013
1314.746954	139586.641107	35.629031
1315.927515	139810.414712	35.634048
1317.476741	140020.558211	35.639066
1319.036601	140232.640527	35.644084
1320.394211	140451.067908	35.649101
1322.433913	140653.875932	35.654119
1323.586135	140852.973564	35.659136
1325.271249	141050.631712	35.664154
1326.143405	141259.015725	35.669172
1327.649844	141459.619931	35.674189
1328.710022	141670.245520	35.679207
1330.192736	141873.289644	35.684224
1331.404927	142075.478246	35.689242
1332.670848	142297.570990	35.694260
1333.715202	142519.814629	35.699277
1335.237741	142726.001342	35.704295
1336.317382	142941.423550	35.709312
1337.757630	143156.751932	35.714330
1338.955775	143384.693660	35.719348
1340.405111	143598.730860	35.724365
1342.082662	143808.208320	35.729383
1343.220826	144025.796212	35.734400
1344.586852	144242.462160	35.739418
1346.081743	144464.648203	35.744436
1347.337186	144678.622272	35.749453
1348.926168	144890.060428	35.754471
1350.007353	145107.690293	35.759488
1351.497836	145326.093211	35.764506
1352.480979	145548.735892	35.769524
1353.843067	145774.019860	35.774541
1355.383875	145995.182749	35.779559
1356.183855	146221.915569	35.784576
1358.275616	146433.778590	35.789594
1359.450807	146660.150703	35.794612
1360.527595	146890.811947	35.799629
1361.812403	147115.230435	35.804647
1363.006100	147344.697504	35.809664
1364.568093	147555.701491	35.814682
1365.705043	147779.818576	35.819700
1367.264425	147993.589361	35.824717
1368.807468	148198.579216	35.829735
1369.788463	148421.597355	35.834752
1371.133332	148630.386471	35.839770
1372.382076	148856.166666	35.844788
1373.248497	149083.124780	35.849805
1374.781088	149304.071079	35.854823
1376.063903	149534.858076	35.859840
1377.747150	149765.063314	35.864858
1378.683785	150006.925276	35.869876
1379.658438	150232.847373	35.874893
1381.299973	150466.651941	35.879911
1382.275857	150716.233583	35.884928
1384.062722	150943.755696	35.889946
1385.846806	151184.857828	35.894964
1387.323131	151423.538435	35.899981
1389.159626	151658.664399	35.904999
1390.197108	151900.194693	35.910016
1391.905303	152132.073461	35.915034
1393.223813	152359.426228	35.920052
1395.326603	152592.234427	35.925069
1396.751699	152814.831656	35.930087
1397.655450	153046.451617	35.935104
1399.185956	153273.523380	35.940122
1400.765342	153510.503708	35.945140
1401.918881	153745.474052	35.950157
1403.553416	153969.212152	35.955175
1404.656335	154209.417508	35.960192
1406.305272	154436.262789	35.965210
1407.507866	154677.203709	35.970228
1408.500646	154927.651114	35.975245
1410.188915	155162.140633	35.980263
1411.433007	155411.778240	35.985280
1412.651475	155653.002523	35.990298
1414.157545	155904.960518	35.995316
1415.704246	156148.240971	36.000333
1417.068123	156396.814336	36.005351
1418.520771	156639.631392	36.010368
1419.945564	156891.723683	36.015386
1421.481722	157146.120586	36.020404
1422.940554	157402.661925	36.025421
1424.550287	157647.008106	36.030439
1425.466760	157906.340259	36.035456
1427.214506	158158.048099	36.040474
1429.045370	158403.886130	36.045492
1429.985852	158659.859731	36.050509
1431.612886	158907.990858	36.055527
1432.744778	159163.176880	36.060544
1434.591524	159409.957843	36.065562
1435.578782	159666.654171	36.070580
1437.229489	159925.060352	36.075597
1438.140848	160171.158312	36.080615
1439.717895	160445.444192	36.085632
1441.263295	160695.566473	36.090650
1443.098024	160936.501195	36.095668
1444.608845	161172.530519	36.100685
1445.998380	161397.674458	36.105703
1447.200323	161635.265028	36.110720
1449.019411	161873.913162	36.115738
1450.357661	162104.687731	36.120756
1451.165987	162344.095625	36.125773
1452.853570	162578.064306	36.130791
1453.845597	162839.601859	36.135808
1455.272910	163078.586529	36.140826
1457.096819	163321.935890	36.145844
1457.937458	163584.618898	36.150861
1459.667424	163844.714776	36.155879
1460.768020	164114.158107	36.160896
1462.391968	164367.616181	36.165914
1463.891978	164639.067181	36.170932
1465.187192	164907.318587	36.175949
1466.653951	165163.889048	36.180967
1467.713283	165439.347655	36.185984
1469.546143	165722.307980	36.191002
1470.890246	165986.881313	36.196020
1472.209276	166267.073680	36.201037
1473.945231	166548.901486	36.206055
1475.190877	166836.440789	36.211072
1476.925902	167118.501320	36.216090
1478.008983	167404.789742	36.221108
1479.359787	167686.116480	36.226125
1481.457617	167957.357080	36.231143
1482.969092	168241.681177	36.236160
1484.155251	168532.401121	36.241178
1486.088708	168809.546636	36.246196
1487.903909	169097.925842	36.251213
1489.153361	169373.712724	36.256231
1490.888232	169657.567884	36.261248
1492.037945	169940.795073	36.266266
1493.644281	170223.469774	36.271284
1495.143044	170512.988010	36.276301
1496.700250	170793.010861	36.281319
1498.629824	171074.486070	36.286336
1500.314339	171363.917682	36.291354
1502.190572	171641.676045	36.296372
1503.625033	171924.250811	36.301389
1505.260856	172191.738180	36.306407
1506.988498	172448.328728	36.311424
1508.607468	172719.019045	36.316442
1510.186745	172982.677039	36.321460
1511.760459	173257.285348	36.326477
1513.533964	173503.650803	36.331495
1515.176498	173769.891821	36.336512
1516.600814	174038.833299	36.341530
1518.139197	174288.691473	36.346548
1519.476523	174550.710970	36.351565
1521.403040	174801.284501	36.356583
1523.022696	175063.148285	36.361600
1524.082544	175329.936146	36.366618
1525.513321	175557.516765	36.371636
1526.949274	175800.308835	36.376653
1528.253331	176045.051640	36.381671
1529.660665	176285.199646	36.386688
1531.010607	176543.246331	36.391706
1532.237981	176784.745239	36.396724
1533.663822	177054.188412	36.401741
1535.261197	177308.990799	36.406759
1536.473241	177576.898144	36.411776
1537.754283	177841.117004	36.416794
1539.305281	178112.120319	36.421812
1540.285450	178388.455870	36.426829
1541.764478	178666.477523	36.431847
1543.303461	178957.635599	36.436864
1544.650248	179243.116847	36.441882
1546.536634	179526.484293	36.446900
1548.101365	179821.057141	36.451917
1549.817178	180105.242155	36.456935
1551.312208	180399.665112	36.461952
1552.777217	180690.428052	36.466970
1554.747204	180979.920071	36.471988
1555.976784	181274.492661	36.477005
1557.304835	181569.292680	36.482023
1558.962669	181861.225525	36.487040
1560.250419	182168.584651	36.492058
1561.865452	182464.423629	36.497076
1563.375104	182776.154634	36.502093
1564.734429	183092.809509	36.507111
1566.474319	183405.637664	36.512128
1568.110711	183710.960023	36.517146
1569.984848	184017.198375	36.522164
1571.240934	184329.145496	36.527181
1573.081496	184635.279202	36.532199
1575.007251	184945.614240	36.537216
1576.596330	185251.830138	36.542234
1578.651731	185552.606472	36.547252
1580.213111	185857.904535	36.552269
1582.087291	186156.277277	36.557287
1583.781926	186450.277213	36.562304
1585.605016	186744.575866	36.567322
1587.487611	187037.179218	36.572340
1589.227157	187344.197337	36.577357
1591.018290	187634.116061	36.582375
1593.110113	187911.844573	36.587392
1594.540745	188190.123897	36.592410
1595.983660	188471.613509	36.597428
1597.637051	188743.718736	36.602445
1598.907832	189029.515597	36.607463
1600.449288	189316.222966	36.612480
1601.838911	189603.844504	36.617498
1603.444329	189883.996897	36.622516
1604.773628	190180.870138	36.627533
1606.588241	190459.241377	36.632551
1608.429009	190751.582509	36.637568
1609.977423	191037.905657	36.642586
1611.745797	191311.098626	36.647604
1613.170229	191578.573393	36.652621
1614.662587	191842.180783	36.657639
1616.291520	192101.922519	36.662656
1617.627483	192393.909486	36.667674
1619.086023	192654.036547	36.672692
1620.324355	192934.556701	36.677709
1621.692077	193225.832821	36.682727
1623.534084	193506.069960	36.687744
1624.975076	193799.749158	36.692762
1626.339933	194092.338001	36.697780
1627.679573	194390.148801	36.702797
1629.401741	194683.928109	36.707815
1631.282065	194977.925146	36.712832
1633.007149	195275.464172	36.717850
1635.118907	195568.958266	36.722868
1636.658468	195874.221531	36.727885
1637.991798	196174.302920	36.732903
1640.199070	196470.845775	36.737920
1641.933715	196763.441952	36.742938
1644.232334	197046.278705	36.747956
1645.681764	197340.649561	36.752973
1647.114977	197630.963072	36.757991
1649.250153	197915.518559	36.763008
1650.433073	198210.101597	36.768026
1652.421339	198489.327242	36.773044
1654.468392	198777.962988	36.778061
1656.255556	199055.471941	36.783079
1658.412323	199333.101339	36.788096
1660.106003	199619.639951	36.793114
1661.819669	199889.016042	36.798132
1663.183215	200174.911903	36.803149
1664.794702	200453.382521	36.808167
1666.840018	200733.131143	36.813184
1667.709505	201025.634178	36.818202
1669.495476	201302.761306	36.823220
1671.074262	201587.919526	36.828237
1672.738052	201888.247024	36.833255
1674.230372	202169.893189	36.838272
1675.253194	202466.936419	36.843290
1676.912797	202776.192904	36.848308
1678.785698	203083.830505	36.853325
1680.451668	203384.762256	36.858343
1682.202705	203689.566397	36.863360
1683.450317	204016.272880	36.868378
1685.029549	204311.015970	36.873396
1686.985489	204622.025255	36.878413
1688.833240	204940.593676	36.883431
1690.579355	205239.339018	36.888448
1692.242660	205562.014943	36.893466
1693.817854	205865.550951	36.898484
1695.794152	206171.487538	36.903501
1697.538553	206484.203263	36.908519
1699.690310	206783.640995	36.913536
1701.021502	207093.696211	36.918554
1702.846286	207365.133823	36.923572
1704.391163	207651.254048	36.928589
1706.029218	207945.802823	36.933607
1708.039326	208222.635506	36.938624
1709.550325	208495.994135	36.943642
1711.340325	208779.821061	36.948660
1713.004525	209072.923895	36.953677
1714.428598	209375.244743	36.958695
1716.372166	209657.121671	36.963712
1717.481209	209946.292428	36.968730
1719.437099	210238.872025	36.973748
1721.321446	210536.428186	36.978765
1722.839027	210842.460974	36.983783
1724.426546	211135.433283	36.988800
1725.964456	211449.374977	36.993818
1727.806607	211751.805869	36.998836
1729.595712	212051.123496	37.003853
1731.297033	212374.400376	37.008871
1733.397152	212675.080716	37.013888
1735.303190	212987.486025	37.018906
1736.787349	213280.852623	37.023924
1738.660226	213592.466229	37.028941
1740.553472	213897.577758	37.033959
1742.720611	214192.338072	37.038976
1744.325709	214510.206807	37.043994
1746.312636	214806.928224	37.049012
1747.906725	215121.602169	37.054029
1749.764793	215434.724812	37.059047
1751.593007	215735.766790	37.064064
1753.181343	216048.046314	37.069082
1754.357503	216354.539656	37.074100
1756.200174	216673.688445	37.079117
1757.619370	217004.167702	37.084135
1759.540643	217326.506499	37.089152
1760.966707	217668.465455	37.094170
1762.499042	217984.114391	37.099188
1764.153533	218324.834046	37.104205
1765.727768	218666.228287	37.109223
1767.970009	219006.273803	37.114240
1769.635720	219350.691285	37.119258
1771.301823	219700.163713	37.124276
1773.087776	220028.960719	37.129293
1774.720478	220377.362401	37.134311
1776.269207	220735.174920	37.139328
1778.040697	221076.650578	37.144346
1779.623092	221486.418255	37.149364
1781.397986	221857.113291	37.154381
1783.016191	222213.321877	37.159399
1785.210522	222562.228504	37.164416
1787.180373	222922.041389	37.169434
1789.188079	223277.558144	37.174452
1790.860637	223628.914094	37.179469
1792.454214	223996.448270	37.184487
1793.812829	224347.069963	37.189504
1796.179930	224696.453788	37.194522
1797.695389	225038.393696	37.199540
1799.730388	225374.665497	37.204557
1801.084109	225721.611501	37.209575
1803.129036	226052.284697	37.214592
1805.397298	226378.314367	37.219610
1806.701897	226723.697780	37.224628
1809.140116	227043.684156	37.229645
1811.231865	227386.583472	37.234663
1812.897262	227716.218682	37.239680
1814.800399	228045.588847	37.244698
1816.559222	228372.849847	37.249716
1818.549168	228707.389654	37.254733
1820.055576	229042.286846	37.259751
1822.323091	229377.420053	37.264768
1824.034055	229712.490472	37.269786
1825.569032	230049.748827	37.274804
1827.534246	230385.187737	37.279821
1829.184486	230735.027366	37.284839
1831.362505	231070.028645	37.289856
1833.110496	231417.823546	37.294874
1835.097522	231762.203916	37.299892
1837.069800	232092.796929	37.304909
1838.542577	232437.845523	37.309927
1840.603865	232789.633984	37.314944
1842.421891	233136.966892	37.319962
1843.825498	233485.230346	37.324980
1846.158682	233832.610950	37.329997
1847.945238	234192.194495	37.335015
1850.009758	234536.216830	37.340032
1851.933754	234887.932967	37.345050
1853.500232	235241.053183	37.350068
1855.673085	235582.064839	37.355085
1857.537691	235940.296049	37.360103
1859.654048	236286.525712	37.365120
1861.653250	236631.860748	37.370138
1863.051691	236983.946771	37.375156
1864.908661	237327.096919	37.380173
1866.757220	237683.660213	37.385191
1868.892615	238036.242274	37.390208
1870.739897	238382.978558	37.395226
1872.546870	238735.919756	37.400244
1875.090240	239084.579690	37.405261
1876.985866	239432.479909	37.410279
1878.806139	239776.024416	37.415296
1880.840119	240116.589668	37.420314
1882.472039	240475.380517	37.425332
1884.354172	240823.312433	37.430349
1886.063822	241172.999926	37.435367
1887.963724	241515.317658	37.440384
1890.066842	241873.072709	37.445402
1891.724567	242222.923854	37.450420
1893.660461	242578.878675	37.455437
1895.675687	242930.148272	37.460455
1897.230162	243281.771359	37.465472
1899.389458	243639.547917	37.470490
1901.338774	243967.868877	37.475508
1902.926450	244293.022183	37.480525
1904.720300	244619.794602	37.485543
1906.454204	244949.422198	37.490560
1908.683552	245283.086884	37.495578
1910.570178	245618.610219	37.500596
1912.321762	245945.925934	37.505613
1913.643125	246292.158120	37.510631
1915.629878	246630.284271	37.515648
1917.788538	246975.801024	37.520666
1919.612566	247331.481314	37.525684
1921.397114	247670.861217	37.530701
1923.763283	248020.513272	37.535719
1925.468446	248371.642691	37.540736
1927.496505	248727.395512	37.545754
1929.278464	249074.627949	37.550772
1931.345902	249428.877439	37.555789
1932.582868	249797.814522	37.560807
1934.463379	250152.552493	37.565824
1936.587735	250513.729935	37.570842
1938.442419	250894.586399	37.575860
1940.460872	251263.986981	37.580877
1942.204662	251644.380082	37.585895
1944.452060	252011.027943	37.590912
1946.465324	252395.317183	37.595930
1948.640051	252784.153961	37.600948
1950.707733	253149.791173	37.605965
1952.303769	253526.375988	37.610983
1954.591879	253887.204083	37.616000
1957.014046	254262.287554	37.621018
1958.659272	254647.528857	37.626036
1961.341840	255012.233759	37.631053
1963.271729	255380.284820	37.636071
1965.155533	255743.898447	37.641088
1967.317455	256115.190874	37.646106
1969.412443	256478.670633	37.651124
1971.446791	256836.038636	37.656141
1973.309851	257202.553859	37.661159
1975.508236	257561.294111	37.666176
1977.591128	257925.209949	37.671194
1979.467154	258294.087256	37.676212
1981.358306	258656.332645	37.681229
1983.153497	259024.741219	37.686247
1984.903055	259393.005148	37.691264
1987.290143	259757.840694	37.696282
1989.189219	260130.756024	37.701300
1991.552428	260495.672561	37.706317
1993.499305	260860.604818	37.711335
1995.414283	261233.315864	37.716352
1997.521559	261595.175250	37.721370
1999.180127	261972.957658	37.726388
2001.268948	262341.019152	37.731405
2003.274279	262718.823641	37.736423
2005.099223	263089.518941	37.741440
2007.402410	263444.033265	37.746458
2009.557157	263791.763483	37.751476
2011.666241	264126.901364	37.756493
2013.629481	264458.176011	37.761511
2015.242008	264793.621882	37.766528
2017.299005	265134.738626	37.771546
2019.025712	265485.307211	37.776564
2020.996869	265831.010701	37.781581
2022.722952	266186.355740	37.786599
2024.513105	266544.002577	37.791616
2027.068502	266898.683123	37.796634
2028.856751	267259.938038	37.801652
2031.090871	267607.328506	37.806669
2033.273674	267964.431380	37.811687
2034.971725	268332.534782	37.816704
2037.395728	268677.939717	37.821722
2039.410503	269042.995704	37.826740
2041.246789	269412.983041	37.831757
2043.466303	269780.979119	37.836775
2045.366245	270143.970799	37.841792
2047.542943	270516.343379	37.846810
2049.453286	270897.420910	37.851828
2051.921122	271258.087454	37.856845
2053.921550	271633.384399	37.861863
2055.947357	272017.771848	37.866880
2058.148079	272370.910886	37.871898
2060.113507	272755.028670	37.876916
2062.270607	273124.382155	37.881933
2064.768303	273499.575269	37.886951
2066.625301	273869.408330	37.891968
2069.026549	274235.878059	37.896986
2070.950868	274612.559427	37.902004
2073.300037	274969.943033	37.907021
2075.662147	275329.661702	37.912039
2077.722242	275696.414206	37.917056
2079.840184	276048.702969	37.922074
2081.777060	276426.627057	37.927092
2084.388473	276790.141987	37.932109
2086.633783	277139.641444	37.937127
2088.715327	277496.686219	37.942144
2091.514745	277857.478368	37.947162
2093.092881	278222.909727	37.952180
2095.061680	278572.173278	37.957197
2097.137026	278925.077907	37.962215
2098.971261	279292.043312	37.967232
2101.091901	279649.563912	37.972250
2103.312922	280023.834646	37.977268
2105.293450	280383.714264	37.982285
2107.678577	280745.765031	37.987303
2109.378387	281112.852548	37.992320
2111.499235	281466.587168	37.997338
2113.665017	281834.819730	38.002356
2115.747267	282196.511274	38.007373
2117.995699	282565.924217	38.012391
2119.874292	282935.573387	38.017408
2122.232343	283285.941431	38.022426
2123.900115	283629.991699	38.027444
2125.905800	283975.410701	38.032461
2128.226422	284323.269001	38.037479
2130.010448	284670.754870	38.042496
2132.205347	285011.011617	38.047514
2134.019560	285368.500936	38.052532
2135.999856	285712.626987	38.057549
2137.913402	286066.645092	38.062567
2139.674228	286435.751060	38.067584
2141.986705	286811.983605	38.072602
2144.184388	287169.613583	38.077620
2145.979532	287548.772489	38.082637
2147.988725	287915.703618	38.087655
2149.994240	288310.146203	38.092672
2152.372356	288691.040290	38.097690
2154.634701	289077.312241	38.102708
2156.865753	289456.653685	38.107725
2159.244959	289846.106814	38.112743
2161.137614	290239.853395	38.117760
2163.650985	290631.290933	38.122778
2165.915543	291025.790252	38.127796
2167.979091	291424.080417	38.132813
2170.066558	291813.703887	38.137831
2171.998921	292214.477619	38.142848
2174.492382	292600.148850	38.147866
2176.695045	293005.552416	38.152884
2178.692334	293410.073339	38.157901
2181.361695	293801.531773	38.162919
2182.821075	294223.664087	38.167936
2185.182824	294629.090228	38.172954
2187.533419	295041.477540	38.177972
2189.829793	295448.512770	38.182989
2191.992953	295857.905284	38.188007
2194.136513	296275.784316	38.193024
2196.652163	296681.080278	38.198042
2198.434862	297092.207015	38.203060
2201.030993	297507.699978	38.208077
2203.262068	297910.218764	38.213095
2205.758050	298326.208349	38.218112
2207.929962	298739.047723	38.223130
2210.254737	299142.437875	38.228148
2212.605083	299559.082610	38.233165
2214.644365	299967.850365	38.238183
2216.755991	300381.558901	38.243200
2219.433661	300782.348945	38.248218
2221.600570	301195.640182	38.253236
2223.581577	301604.717798	38.258253
2226.365887	302002.465053	38.263271
2228.573937	302428.701026	38.268288
2230.712367	302837.216922	38.273306
2232.952365	303250.211538	38.278324
2234.797562	303657.603181	38.283341
2237.088010	304064.364246	38.288359
2239.066087	304486.414081	38.293376
2241.345752	304890.862980	38.298394
2243.889798	305274.033900	38.303412
2245.732028	305669.913642	38.308429
2248.148072	306053.788439	38.313447
2249.909040	306439.594797	38.318464
2252.099300	306825.865353	38.323482
2254.594912	307217.674373	38.328500
2256.702617	307616.503307	38.333517
2258.669534	308007.149086	38.338535
2260.662880	308421.639978	38.343552
2262.818973	308826.807318	38.348570
2265.167009	309244.769745	38.353588
2266.935653	309661.273182	38.358605
2269.660885	310074.931135	38.363623
2271.832433	310495.736455	38.368640
2274.367294	310923.213474	38.373658
2276.401259	311349.803122	38.378676
2278.360806	311774.650401	38.383693
2280.984565	312203.480009	38.388711
2282.887798	312646.163025	38.393728
2285.302505	313070.755332	38.398746
2287.887278	313517.568339	38.403764
2290.109393	313960.550955	38.408781
2292.942699	314389.668777	38.413799
2295.519188	314819.231910	38.418816
2297.693688	315238.164256	38.423834
2300.431413	315678.390921	38.428852
2303.322951	316098.526734	38.433869
2305.837177	316519.457125	38.438887
2308.011983	316947.601735	38.443904
2310.528250	317348.057501	38.448922
2313.092180	317766.536427	38.453940
2315.420469	318180.225326	38.458957
2317.849648	318595.775835	38.463975
2320.078595	319019.864361	38.468992
2322.241201	319435.580366	38.474010
2324.717909	319848.831970	38.479028
2327.151058	320281.822093	38.484045
2329.298520	320697.509333	38.489063
2331.151350	321121.952438	38.494080
2333.723906	321548.692106	38.499098
2336.478903	321966.486591	38.504116
2338.568628	322392.257408	38.509133
2341.102637	322804.368679	38.514151
2343.408479	323237.237400	38.519168
2345.476729	323663.792556	38.524186
2347.859781	324081.889599	38.529204
2350.372804	324509.182605	38.534221
2353.200854	324918.951256	38.539239
2355.660247	325338.731330	38.544256
2358.238344	325756.611156	38.549274
2361.004681	326147.413021	38.554292
2363.336948	326565.251405	38.559309
2365.681146	326966.959866	38.564327
2368.054835	327367.899751	38.569344
2370.120082	327763.325010	38.574362
2372.270932	328146.240530	38.579380
2374.604972	328536.667267	38.584397
2377.074221	328909.599255	38.589415
2379.152396	329297.573985	38.594432
2380.865815	329685.122033	38.599450
2383.276384	330072.608364	38.604468
2385.130074	330481.384775	38.609485
2387.407347	330889.914023	38.614503
2389.513810	331299.204469	38.619520
2391.902419	331708.320918	38.624538
2394.200310	332135.300872	38.629556
2396.076049	332551.654683	38.634573
2398.697360	332973.652085	38.639591
2401.001599	333418.779251	38.644608
2403.286741	333854.689083	38.649626
2405.812806	334296.550613	38.654644
2407.419926	334748.635679	38.659661
2410.147000	335190.586548	38.664679
2412.518269	335644.144263	38.669696
2414.968470	336093.471374	38.674714
2417.897320	336557.675266	38.679732
2420.349893	337023.627217	38.684749
2422.752400	337480.290601	38.689767
2425.112985	337948.535764	38.694784
2427.558628	338405.160425	38.699802
2430.518975	338875.995248	38.704820
2432.553187	339330.114055	38.709837
2435.077437	339806.368500	38.714855
2437.625678	340267.660742	38.719872
2440.072742	340728.787881	38.724890
2442.943499	341192.307259	38.729908
2444.891475	341674.630713	38.734925
2447.367541	342141.556889	38.739943
2449.920265	342612.123368	38.744960
2452.524754	343093.341342	38.749978
2455.368381	343560.807618	38.754996
2457.290059	344046.315252	38.760013
2459.652619	344515.119655	38.765031
2462.519540	344997.067622	38.770048
2464.743324	345485.739763	38.775066
2467.387241	345965.379334	38.780084
2469.838311	346456.469839	38.785101
2472.691773	346929.086565	38.790119
2475.449833	347394.022178	38.795136
2478.236192	347877.608823	38.800154
2481.090361	348335.032282	38.805172
2484.141213	348789.831394	38.810189
2487.097808	349238.345907	38.815207
2489.778086	349683.067243	38.820224
2491.903858	350131.680690	38.825242
2494.651155	350582.857440	38.830260
2496.733682	351037.562773	38.835277
2499.411706	351481.635041	38.840295
2501.777900	351926.133790	38.845312
2503.861189	352376.740592	38.850330
2506.690637	352781.609261	38.855348
2508.748863	353216.398241	38.860365
2510.929865	353647.686512	38.865383
2513.394978	354089.384361	38.870400
2515.399269	354507.620725	38.875418
2517.787698	354943.992795	38.880436
2520.022682	355371.501286	38.885453
2522.458586	355791.892460	38.890471
2524.944667	356249.838819	38.895488
2527.289271	356700.848572	38.900506
2529.764383	357149.853742	38.905524
2531.994284	357614.249904	38.910541
2534.599259	358081.755012	38.915559
2537.201981	358543.976630	38.920576
2539.690252	359015.374697	38.925594
2542.362752	359486.815138	38.930612
2544.938285	359961.007473	38.935629
2547.164804	360444.133648	38.940647
2549.612121	360927.093046	38.945664
2551.864680	361415.433592	38.950682
2554.709085	361907.203124	38.955700
2556.970252	362412.130397	38.960717
2559.789585	362909.451490	38.965735
2562.813258	363400.872308	38.970752
2565.159308	363890.339547	38.975770
2568.055329	364380.907224	38.980788
2570.510589	364883.847898	38.985805
2573.118014	365387.799381	38.990823
2576.070667	365891.969695	38.995840
2578.598146	366394.273004	39.000858
2581.202276	366889.681311	39.005876
2584.120630	367396.555385	39.010893
2586.369674	367902.514592	39.015911
2589.566924	368402.354340	39.020928
2591.838194	368906.166806	39.025946
2594.429445	369408.349441	39.030964
2597.075168	369914.044776	39.035981
2599.692509	370419.535645	39.040999
2602.702511	370918.741512	39.046016
2604.692025	371439.468444	39.051034
2607.633547	371953.517004	39.056052
2610.047534	372454.346944	39.061069
2612.829578	372968.002332	39.066087
2615.564210	373476.406626	39.071104
2618.010219	373997.993544	39.076122
2620.390157	374500.529508	39.081140
2622.844521	375025.298984	39.086157
2625.587261	375546.869899	39.091175
2628.543162	376056.221962	39.096192
2630.857478	376582.566475	39.101210
2633.701306	377100.625393	39.106228
2636.475089	377623.864277	39.111245
2638.839297	378158.958307	39.116263
2641.763193	378680.890920	39.121280
2644.503562	379180.977062	39.126298
2647.477680	379669.705077	39.131316
2649.861890	380152.228873	39.136333
2652.336786	380616.060951	39.141351
2655.198625	381096.924437	39.146368
2657.302060	381587.034500	39.151386
2660.030571	382062.934828	39.156404
2662.699562	382556.291387	39.161421
2665.076810	383046.060228	39.166439
2667.903048	383537.375061	39.171456
2670.395899	384040.480890	39.176474
2673.289594	384540.269600	39.181492
2675.742809	385042.074502	39.186509
2678.025395	385558.890536	39.191527
2680.642713	386060.199021	39.196544
2683.076869	386581.694543	39.201562
2685.918448	387098.121321	39.206580
2688.532055	387632.940321	39.211597
2691.247393	388158.122513	39.216615
2693.802517	388691.311798	39.221632
2696.533977	389233.063192	39.226650
2699.384810	389761.066387	39.231668
2701.909438	390309.960942	39.236685
2704.367192	390859.161884	39.241703
2707.330390	391403.075147	39.246720
2709.837072	391966.859022	39.251738
2712.800641	392517.323281	39.256756
2715.771025	393080.178738	39.261773
2718.125964	393637.391189	39.266791
2721.445693	394188.000579	39.271808
2724.085194	394751.971420	39.276826
2726.753549	395304.973529	39.281844
2730.020725	395851.405497	39.286861
2732.852556	396408.775892	39.291879
2735.990092	396949.631856	39.296896
2738.837248	397507.235069	39.301914
2741.589770	398058.834468	39.306932
2744.654810	398596.809806	39.311949
2747.229089	399140.406885	39.316967
2750.096094	399694.724456	39.321984
2752.823430	400239.648178	39.327002
2755.876572	400788.542467	39.332020
2758.513161	401336.098933	39.337037
2761.277365	401897.696930	39.342055
2764.216676	402420.239364	39.347072
2767.013823	402977.984881	39.352090
2769.575267	403527.315722	39.357108
2772.505735	404067.959076	39.362125
2774.993692	404620.121894	39.367143
2778.523783	405151.525272	39.372160
2781.204299	405696.743223	39.377178
2784.141181	406233.748399	39.382196
2787.064504	406770.670358	39.387213
2789.897874	407315.810242	39.392231
2792.609654	407832.265272	39.397248
2795.070795	408364.745854	39.402266
2797.792056	408882.094145	39.407284
2800.756123	409379.776483	39.412301
2803.365761	409879.179621	39.417319
2806.200187	410380.566594	39.422336
2808.657577	410887.733046	39.427354
2811.726727	411379.307966	39.432372
2814.462005	411892.952461	39.437389
2817.212335	412397.081457	39.442407
2820.581489	412889.445569	39.447424
2823.207200	413395.934230	39.452442
2826.105370	413899.481877	39.457460
2829.211508	414394.117923	39.462477
2831.777771	414908.623470	39.467495
2834.736515	415415.607222	39.472512
2837.463705	415926.572017	39.477530
2840.251013	416436.428564	39.482548
2843.135868	416957.613211	39.487565
2845.311496	417477.329539	39.492583
2848.797054	417997.513197	39.497600
2851.253561	418540.022033	39.502618
2853.732688	419074.737892	39.507636
2856.838993	419603.491184	39.512653
2859.565421	420147.167917	39.517671
2862.345236	420693.663399	39.522688
2865.096532	421241.343502	39.527706
2867.727315	421796.936784	39.532724
2870.984587	422352.749095	39.537741
2873.401055	422908.835287	39.542759
2876.918551	423455.387413	39.547776
2880.022837	424009.467605	39.552794
2882.777350	424567.974614	39.557812
2885.682187	425124.546339	39.562829
2888.406282	425689.722976	39.567847
2891.345444	426266.177156	39.572864
2894.273816	426830.790812	39.577882
2896.923691	427394.271387	39.582900
2900.309697	427963.728165	39.587917
2902.847158	428546.807873	39.592935
2905.803380	429116.814459	39.597952
2908.848517	429693.709392	39.602970
2911.397980	430279.636287	39.607988
2914.562169	430856.233459	39.613005
2917.309300	431433.415728	39.618023
2920.132071	432023.135149	39.623040
2923.207261	432613.535603	39.628058
2925.717059	433206.569852	39.633076
2928.873536	433792.903578	39.638093
2931.557360	434399.203479	39.643111
2934.979353	434987.924126	39.648128
2937.936253	435581.997210	39.653146
2940.916667	436180.813205	39.658164
2944.238812	436774.015375	39.663181
2946.959333	437369.273765	39.668199
2949.825369	437953.632377	39.673216
2952.954746	438530.390207	39.678234
2955.730466	439078.174462	39.683252
2958.693936	439630.980636	39.688269
2961.214841	440183.793792	39.693287
2964.343473	440725.004038	39.698304
2967.150923	441279.215544	39.703322
2970.088639	441840.634384	39.708340
2973.100068	442404.357650	39.713357
2976.026182	442957.145003	39.718375
2978.871048	443524.918946	39.723392
2982.064449	444089.485349	39.728410
2985.044798	444659.843672	39.733428
2987.812126	445220.198098	39.738445
2990.581195	445810.104003	39.743463
2993.792431	446388.383067	39.748480
2996.754448	446967.446746	39.753498
2999.160786	447562.276666	39.758516
3002.118564	448147.335854	39.763533
3004.947978	448756.444534	39.768551
3008.017754	449362.715306	39.773568
3011.227526	449970.972727	39.778586
3013.415352	450603.417763	39.783604
3016.940518	451213.617119	39.788621
3019.532783	451847.735417	39.793639
3022.634806	452469.912656	39.798656
3026.325021	453092.283501	39.803674
3029.428692	453717.260479	39.808692
3032.723462	454347.402405	39.813709
3035.746935	454981.466220	39.818727
3038.795791	455610.549003	39.823744
3041.797299	456245.390226	39.828762
3044.555148	456885.666192	39.833780
3048.061711	457510.929148	39.838797
3051.116929	458150.362598	39.843815
3054.306564	458788.339572	39.848832
3057.695302	459420.043401	39.853850
3060.670339	460061.710746	39.858868
3064.277800	460678.975159	39.863885
3068.207455	461287.368376	39.868903
3071.780830	461897.419743	39.873920
3075.573988	462492.596988	39.878938
3079.076017	463093.317742	39.883956
3082.672176	463668.056842	39.888973
3085.681981	464263.005462	39.893991
3088.832527	464833.737059	39.899008
3092.285090	465409.210731	39.904026
3094.997584	465980.790112	39.909044
3097.509977	466564.069197	39.914061
3100.817727	467150.240915	39.919079
3103.705593	467725.943100	39.924096
3106.770302	468320.364323	39.929114
3109.475396	468917.505850	39.934132
3113.144263	469489.849831	39.939149
3115.712577	470073.376259	39.944167
3118.590911	470675.395627	39.949184
3121.883508	471238.142884	39.954202
3124.607032	471802.835678	39.959220
3127.104295	472361.481072	39.964237
3130.195537	472913.444143	39.969255
3132.843407	473477.142003	39.974272
3135.680434	474049.136650	39.979290
3138.607171	474627.673531	39.984308
3141.541112	475212.411188	39.989325
3144.882351	475793.730814	39.994343
3147.386347	476393.213735	39.999360
3150.553539	476994.039834	40.004378
3153.117729	477593.224521	40.009396
3156.265150	478211.002102	40.014413
3159.490620	478836.026956	40.019431
3162.734268	479452.537483	40.024448
3165.936708	480078.689230	40.029466
3168.823365	480712.755652	40.034484
3172.236141	481339.288819	40.039501
3175.405832	481983.933463	40.044519
3178.451108	482628.172155	40.049536
3181.864461	483273.139838	40.054554
3185.208519	483912.336075	40.059572
3188.865566	484550.703646	40.064589
3191.973606	485211.269441	40.069607
3195.608587	485848.081452	40.074624
3199.037401	486489.250227	40.079642
3202.264457	487147.608134	40.084660
3205.874573	487770.869417	40.089677
3208.948390	488419.658338	40.094695
3212.134573	489059.667110	40.099712
3215.466072	489709.684422	40.104730
3218.608153	490349.959345	40.109748
3221.951856	491014.528939	40.114765
3225.606477	491642.453749	40.119783
3228.694927	492293.783443	40.124800
3232.161580	492927.553898	40.129818
3234.986565	493600.093586	40.134836
3238.603899	494240.967289	40.139853
3242.012128	494882.356744	40.144871
3245.272477	495538.645536	40.149888
3248.533774	496179.760197	40.154906
3251.830670	496830.744551	40.159924
3254.996753	497473.899094	40.164941
3258.302330	498121.452356	40.169959
3261.472241	498764.105898	40.174976
3264.847829	499431.950084	40.179994
3268.208923	500079.020142	40.185012
3271.431639	500732.854128	40.190029
3274.845321	501378.707518	40.195047
3277.679183	502046.892943	40.200064
3281.036445	502694.625782	40.205082
3284.222864	503358.566318	40.210100
3287.339890	504011.740732	40.215117
3290.625492	504686.468481	40.220135
3293.570825	505345.879528	40.225152
3296.879333	505994.356447	40.230170
3300.142806	506627.321539	40.235188
3303.516485	507254.896320	40.240205
3307.142243	507867.116680	40.245223
3310.174357	508491.521079	40.250240
3313.487653	509095.571679	40.255258
3316.640625	509730.105792	40.260276
3320.162823	510344.323256	40.265293
3323.374953	510966.439239	40.270311
3326.606919	511603.414184	40.275328
3330.065146	512231.398900	40.280346
3333.145669	512872.891064	40.285364
3336.513334	513502.104236	40.290381
3339.858476	514161.163523	40.295399
3342.686980	514812.661065	40.300416
3346.211934	515449.999309	40.305434
3349.332103	516122.889468	40.310452
3352.412685	516781.433322	40.315469
3355.691969	517451.974676	40.320487
3359.256722	518119.165313	40.325504
3362.804375	518796.015278	40.330522
3366.050430	519480.097048	40.335540
3369.417409	520165.341542	40.340557
3373.183069	520828.456824	40.345575
3376.253948	521532.904263	40.350592
3379.630793	522216.245721	40.355610
3383.374044	522904.946125	40.360628
3386.275206	523608.826058	40.365645
3390.094890	524309.504988	40.370663
3393.333751	525002.430721	40.375680
3397.293008	525705.597903	40.380698
3400.563876	526397.651594	40.385716
3403.935643	527103.269865	40.390733
3407.692449	527799.369807	40.395751
3410.991619	528505.138887	40.400768
3414.993359	529200.332032	40.405786
3418.495787	529883.426903	40.410804
3421.906897	530581.626044	40.415821
3425.790265	531279.316272	40.420839
3429.076780	531965.227139	40.425856
3432.812533	532654.916977	40.430874
3436.206742	533351.231216	40.435892
3440.094996	534027.986637	40.440909
3444.038891	534707.424425	40.445927
3447.391495	535388.638740	40.450944
3450.773009	536060.598667	40.455962
3453.960031	536743.895017	40.460980
3457.250039	537427.547572	40.465997
3461.005489	538105.403679	40.471015
3464.266189	538792.072424	40.476032
3467.834135	539471.458721	40.481050
3471.252797	540159.652332	40.486068
3474.748858	540843.118404	40.491085
3478.421171	541509.754880	40.496103
3481.936314	542188.926279	40.501120
3485.270256	542864.688936	40.506125
3488.561970	543484.284122	40.511130
3491.817989	544059.636419	40.516135
3495.035351	544566.419575	40.521140
3497.642840	545021.944337	40.526144
3500.733980	545414.987898	40.531149
3503.492643	545759.413913	40.536154
3505.625619	546046.691213	40.541159
3508.062052	546260.827098	40.546164
3509.882417	546445.933454	40.551168
3511.621293	546572.803369	40.556173
3513.324887	546665.456583	40.561178
3514.622975	546699.068758	40.566183
3516.216517	546715.977885	40.571188
3517.423075	546693.578734	40.576192
3518.635351	546616.616417	40.581197
3519.853299	546524.106741	40.586202
3520.348283	546398.498434	40.591207
3521.232633	546246.883293	40.596212
3521.910719	546072.787004	40.601216
3522.328117	545885.202182	40.606221
3522.997638	545676.273794	40.611226
3523.193846	545444.803154	40.616231
3523.523389	545196.548876	40.621236
3523.745171	544948.812266	40.626240
3524.189422	544672.413904	40.631245
3524.368927	544405.138906	40.636250
3524.239300	544125.893143	40.641255
3524.543224	543838.243862	40.646260
3524.472697	543538.481463	40.651264
3524.619583	543227.218480	40.656269
3524.274542	542928.900809	40.661274
3524.310005	542618.955409	40.666279
3524.647249	542303.301177	40.671284
3524.241647	541999.218839	40.676288
3524.524004	541679.016072	40.681293
3524.254647	541361.973667	40.686298
3523.832493	541039.596484	40.691303
3523.792787	540715.940101	40.696308
3523.524713	540403.926708	40.701312
3523.322904	540079.221886	40.706317
3523.044057	539779.417331	40.711322
3522.900779	539458.174218	40.716327
3522.885529	539151.296325	40.721332
3522.450443	538852.962598	40.726336
3522.314477	538534.577274	40.731341
3522.030997	538237.369027	40.736346
3521.688315	537939.305777	40.741351
3521.476574	537629.347521	40.746356
3520.681411	537338.010576	40.751360
3520.394818	537060.729409	40.756365
3520.898703	536782.611190	40.761370
3520.374300	536498.993542	40.766375
3520.001084	536203.830724	40.771380
3519.672386	535945.072771	40.776384
3519.574380	535664.806976	40.781389
3519.436086	535402.524559	40.786394
3518.865801	535137.780324	40.791399
3519.011453	534879.687171	40.796404
3518.644948	534620.912929	40.801408
3518.236792	534366.990367	40.806413
3518.075717	534112.317363	40.811418
3517.756263	533861.100325	40.816423
3517.579400	533617.686872	40.821428
3517.302013	533390.754399	40.826432
3517.027853	533152.602907	40.831437
3516.887329	532922.206669	40.836442
3516.365520	532695.807865	40.841447
3516.319123	532465.592069	40.846452
3516.206801	532252.308106	40.851456
3516.324437	532030.648668	40.856461
3515.695968	531814.206842	40.861466
3515.649093	531611.311556	40.866471
3515.326427	531394.108245	40.871476
3515.268602	531198.939599	40.876480
3515.030367	530983.940361	40.881485
3515.000995	530789.671585	40.886490
3514.767569	530598.413753	40.891495
3514.560488	530397.953370	40.896500
3514.260943	530215.695271	40.901504
3514.145091	530024.866629	40.906509
3514.036246	529829.436368	40.911514
3513.653142	529668.357032	40.916519
3513.758295	529470.361987	40.921524
3513.314070	529308.176951	40.926528
3512.904104	529129.865173	40.931533
3512.602500	528976.699390	40.936538
3512.631703	528807.663050	40.941543
3512.715823	528646.600506	40.946548
3512.451946	528481.548606	40.951552
3512.427456	528329.596108	40.956557
3512.494580	528170.855994	40.961562
3511.739262	528019.066553	40.966567
3512.328001	527867.518064	40.971572
3511.781036	527725.193628	40.976576
3511.467627	527572.824712	40.981581
3511.422936	527439.767649	40.986586
3511.416161	527300.234656	40.991591
3511.545099	527168.461863	40.996596
3510.920126	527035.745819	41.001600
3510.810914	526891.222112	41.006605
3510.796840	526770.031272	41.011610
3510.483516	526639.385326	41.016615
3510.487819	526509.345132	41.021620
3510.432927	526391.746224	41.026624
3510.372585	526262.775591	41.031629
3510.350408	526143.097501	41.036634
3509.841097	526034.917934	41.041639
3510.066351	525906.960670	41.046644
3509.962705	525795.480674	41.051648
3510.016620	525674.169691	41.056653
3509.730812	525575.605376	41.061658
3509.519007	525465.909190	41.066663
3509.796760	525357.499566	41.071668
3509.550340	525246.745931	41.076672
3509.211384	525132.468035	41.081677
3509.312179	525029.088071	41.086682
3509.418654	524928.183258	41.091687
3509.366903	524826.089726	41.096692
3508.680205	524723.287161	41.101696
3508.700498	524631.391264	41.106701
3508.945761	524533.899179	41.111706
3508.729297	524453.109350	41.116711
3508.776936	524345.740203	41.121716
3508.842682	524251.459242	41.126720
3508.575163	524169.513470	41.131725
3508.715528	524068.547363	41.136730
3508.221599	523977.285029	41.141735
3508.434073	523892.431289	41.146740
3508.407676	523811.759849	41.151744
3508.307932	523726.347995	41.156749
3508.365991	523632.317375	41.161754
3508.034361	523554.119253	41.166759
3508.012053	523455.854147	41.171764
3507.852799	523383.997234	41.176768
3507.793915	523310.759282	41.181773
3508.032770	523244.500461	41.186778
3507.895051	523162.175206	41.191783
3507.951407	523068.192125	41.196788
3507.652153	523001.410742	41.201792
3507.644306	522914.160227	41.206797
3507.874309	522846.435183	41.211802
3507.545948	522771.518621	41.216807
3507.805306	522703.636685	41.221812
3507.602157	522627.688626	41.226816
3507.591316	522556.057345	41.231821
3507.374985	522491.535622	41.236826
3507.144811	522419.180108	41.241831
3506.911304	522341.112275	41.246836
3507.114191	522279.961080	41.251840
3507.144557	522213.326569	41.256845
3507.449429	522133.150501	41.261850
3507.146432	522083.756479	41.266855
3507.183207	522008.677578	41.271860
3507.271091	521949.868817	41.276864
3507.011556	521877.363866	41.281869
3506.955538	521818.779592	41.286874
3506.713100	521761.842334	41.291879
3507.044883	521704.207461	41.296884
3507.045697	521646.574136	41.301888
3506.608592	521592.700380	41.306893
3506.875921	521528.250059	41.311898
3506.591164	521471.166805	41.316903
3506.891436	521421.068754	41.321908
3506.726905	521353.096507	41.326912
3506.651844	521298.355655	41.331917
3506.678281	521235.458945	41.336922
3506.553554	521180.624434	41.341927
3506.940691	521125.860513	41.346932
3506.375337	521067.809051	41.351936
3506.519956	521018.644396	41.356941
3506.925312	520954.321667	41.361946
3506.509950	520906.761906	41.366951
3506.316651	520845.971292	41.371956
3505.938230	520800.377141	41.376960
3506.291991	520746.476711	41.381965
3506.480665	520700.843215	41.386970
3506.207137	520642.895795	41.391975
3506.035133	520592.263141	41.396980
3506.000716	520545.906090	41.401984
3505.886696	520515.689806	41.406989
3506.222785	520452.791703	41.411994
3506.055462	520415.960408	41.416999
3506.182864	520360.274348	41.422004
3505.734157	520327.784878	41.427008
3506.156921	520275.388778	41.432013
3506.115865	520240.357282	41.437018
3505.878377	520200.300762	41.442023
3506.080638	520151.174951	41.447028
3506.107106	520105.009269	41.452032
3506.153141	520051.357428	41.457037
3506.119753	520004.391957	41.462042
3505.920065	519958.666090	41.467047
3506.125545	519924.606169	41.472052
3506.267010	519871.039777	41.477056
3506.633330	519819.005068	41.482061
3506.091951	519778.136006	41.487066
3506.053208	519726.620074	41.492071
3506.062298	519671.961603	41.497076
3506.038096	519624.690224	41.502080
3506.004113	519596.987682	41.507085
3506.060636	519548.338156	41.512090
3505.862210	519494.369196	41.517095
3506.272792	519453.146623	41.522100
3505.974641	519413.198892	41.527104
3505.793687	519361.249228	41.532109
3506.121344	519319.988865	41.537114
3505.905349	519279.977263	41.542119
3506.042399	519238.797384	41.547124
3506.134692	519185.337655	41.552128
3505.942268	519145.069184	41.557133
3506.285156	519105.423898	41.562138
3505.962312	519048.439339	41.567143
3505.953347	519013.855226	41.572148
3506.365676	518958.271072	41.577152
3505.729498	518916.049624	41.582157
3505.936169	518870.054248	41.587162
3506.208739	518846.094295	41.592167
3506.050217	518783.267974	41.597172
3506.226144	518750.929481	41.602176
3506.093850	518701.548828	41.607181
3505.983674	518653.479214	41.612186
3505.755920	518612.608249	41.617191
3506.007084	518567.262340	41.622196
3506.112793	518521.332514	41.627200
3506.017347	518481.653876	41.632205
3506.196617	518426.205895	41.637210
3505.605670	518377.503545	41.642215
3505.625098	518340.739214	41.647220
3505.698614	518290.718016	41.652224
3505.551717	518261.564664	41.657229
3506.186258	518207.712671	41.662234
3505.627538	518184.894462	41.667239
3506.043907	518131.734062	41.672244
3505.827327	518104.007302	41.677248
3505.750205	518065.690060	41.682253
3505.911814	518017.373374	41.687258
3505.522751	517984.111340	41.692263
3505.778610	517943.364552	41.697268
3505.750799	517901.246620	41.702272
3505.657696	517871.628976	41.707277
3505.715928	517822.923523	41.712282
3505.567495	517787.549806	41.717287
3505.542984	517743.913932	41.722292
3505.509292	517712.921292	41.727296
3505.681886	517673.602891	41.732301
3505.713471	517632.031132	41.737306
3505.309943	517599.478560	41.742311
3505.369538	517559.469797	41.747316
3505.559231	517526.216508	41.752320
3505.322035	517492.373234	41.757325
3505.464306	517454.677291	41.762330
3505.377669	517428.243637	41.767335
3505.647873	517381.273280	41.772340
3505.593121	517360.346455	41.777344
3505.475296	517315.004865	41.782349
3505.597125	517279.789625	41.787354
3505.336078	517249.792860	41.792359
3505.527710	517223.416039	41.797364
3505.656645	517180.917520	41.802368
3505.395691	517151.729670	41.807373
3505.462805	517107.925933	41.812378
3505.306434	517072.551944	41.817383
3505.365265	517036.233615	41.822388
3505.512360	517006.424753	41.827392
3505.250774	516972.179713	41.832397
3505.299607	516926.001603	41.837402
3505.198707	516902.502425	41.842407
3505.240319	516865.680744	41.847412
3505.744320	516831.061564	41.852416
3505.320559	516798.460046	41.857421
3505.741942	516759.858717	41.862426
3505.710868	516729.015537	41.867431
3505.392600	516690.429804	41.872436
3505.375290	516648.863310	41.877440
3505.310343	516620.907819	41.882445
3505.653805	516586.718072	41.887450
3505.290063	516559.416552	41.892455
3505.310174	516525.732924	41.897460
3505.095093	516496.688386	41.902464
3505.074279	516453.149677	41.907469
3505.199543	516424.759222	41.912474
3505.039802	516403.038640	41.917479
3505.469388	516368.784262	41.922484
3505.393480	516344.774629	41.927488
3505.217826	516308.542343	41.932493
3505.471796	516267.488312	41.937498
3505.248454	516243.046685	41.942503
3505.148951	516203.818384	41.947508
3505.374457	516183.098643	41.952512
3505.019423	516144.820889	41.957517
3505.174442	516107.119877	41.962522
3505.392269	516096.768594	41.967527
3505.464186	516056.450831	41.972532
3505.462706	516021.606426	41.977536
3505.304370	515991.742875	41.982541
3505.218157	515943.459325	41.987546
3505.245008	515937.234535	41.992551
3505.316830	515893.578577	41.997556
3505.574258	515874.825760	42.002560
3505.372352	515830.252008	42.007565
3505.218528	515790.070426	42.012570
3505.758530	515773.396919	42.017575
3505.851620	515725.691283	42.022580
3505.592584	515696.450002	42.027584
3505.600884	515654.067800	42.032589
3505.547354	515607.548197	42.037594
3505.600040	515584.022884	42.042599
3505.233371	515535.833054	42.047604
3505.473546	515506.815988	42.052608
3505.113565	515484.266092	42.057613
3505.017178	515441.899897	42.062618
3505.238417	515416.881050	42.067623
3505.111104	515383.066691	42.072628
3505.172710	515352.358040	42.077632
3504.975460	515331.754635	42.082637
3505.218529	515279.674588	42.087642
3505.110095	515267.907683	42.092647
3505.090506	515218.397708	42.097652
3505.525687	515195.924050	42.102656
3505.217170	515174.225381	42.107661
3505.121008	515139.748128	42.112666
3504.939751	515113.275179	42.117671
3505.345877	515081.955252	42.122676
3505.166127	515049.716349	42.127680
3505.141440	515025.342693	42.132685
3505.419666	514983.624192	42.137690
3505.129719	514968.294877	42.142695
3505.167281	514923.680860	42.147700
3504.950347	514901.562754	42.152704
3505.153515	514876.697685	42.157709
3505.242744	514836.424821	42.162714
3504.939864	514816.950154	42.167719
3505.181114	514785.352274	42.172724
3505.527797	514754.192859	42.177728
3505.202794	514728.348939	42.182733
3505.408896	514685.427256	42.187738
3505.118014	514653.154577	42.192743
3504.980244	514625.055524	42.197748
3505.137375	514600.298475	42.202752
3505.100860	514575.167379	42.207757
3505.115834	514543.250766	42.212762
3504.754576	514518.524949	42.217767
3504.940928	514486.530565	42.222772
3504.989152	514454.254486	42.227776
3504.744058	514439.979724	42.232781
3504.976211	514421.532742	42.237786
3505.166400	514406.835115	42.242791
3504.928268	514365.550730	42.247796
3505.146429	514330.314046	42.252800
3504.882736	514313.513225	42.257805
3504.980985	514273.187007	42.262810
3505.008678	514256.188341	42.267815
3505.170659	514224.399622	42.272820
3504.973350	514201.670553	42.277824
3504.766236	514185.568756	42.282829
3505.178906	514137.049415	42.287834
3504.922978	514118.932133	42.292839
3504.799234	514090.475919	42.297844
3504.796841	514077.275219	42.302848
3504.994790	514040.372029	42.307853
3504.883300	514021.523712	42.312858
3504.757853	513994.382652	42.317863
3504.858919	513972.263639	42.322868
3504.912099	513948.938271	42.327872
3504.933218	513926.073149	42.332877
3505.191501	513893.358161	42.337882
3504.654700	513864.258738	42.342887
3504.853364	513850.014499	42.347892
3505.032987	513816.502526	42.352896
3505.006497	513793.594169	42.357901
3505.040059	513758.840680	42.362906
3504.806909	513743.248369	42.367911
3504.798850	513712.041933	42.372916
3505.232244	513684.356832	42.377920
3504.753899	513671.787414	42.382925
3505.302874	513637.710913	42.387930
3505.345295	513612.009522	42.392935
3504.803270	513573.097900	42.397940
3504.949003	513551.679398	42.402944
3504.627863	513531.700323	42.407949
3505.167714	513502.581852	42.412954
3504.934969	513490.175803	42.417959
3504.868903	513448.406749	42.422964
3504.996828	513421.679945	42.427968
3504.732345	513397.847633	42.432973
3504.892308	513380.827180	42.437978
3504.830705	513347.807627	42.442983
3504.679312	513318.191119	42.447988
3504.749371	513306.647533	42.452992
3504.942133	513282.034658	42.457997
3504.871599	513253.366295	42.463002
3504.541914	513239.053301	42.468007
3504.853721	513213.561634	42.473012
3504.915748	513184.113485	42.478016
3504.522572	513157.418040	42.483021
3504.925992	513138.740261	42.488026
3504.891901	513120.384517	42.493031
3504.851227	513087.310565	42.498036
3504.916851	513061.908159	42.503040
3504.716076	513048.232190	42.508045
3505.133278	513009.622898	42.513050
3505.087500	512989.346750	42.518055
3504.976346	512961.443039	42.523060
3504.978623	512934.836488	42.528064
3504.827636	512919.483339	42.533069
3504.732396	512891.526415	42.538074
3504.669498	512876.614545	42.543079
3504.583243	512848.656130	42.548084
3504.769234	512832.086251	42.553088
3504.673217	512795.176217	42.558093
3504.804541	512774.062501	42.563098
3504.696711	512761.383260	42.568103
3504.460605	512736.028052	42.573108
3504.718952	512719.041966	42.578112
3504.849104	512695.905032	42.583117
3504.860127	512673.140973	42.588122
3504.553367	512655.434812	42.593127
3504.913345	512631.350975	42.598132
3504.644191	512607.315952	42.603136
3504.650740	512591.330611	42.608141
3504.971950	512556.023354	42.613146
3504.881330	512543.543562	42.618151
3504.413477	512510.333663	42.623156
3504.655149	512492.338320	42.628160
3504.864614	512470.908376	42.633165
3504.869215	512453.759795	42.638170
3504.699407	512429.253567	42.643175
3504.371821	512394.352015	42.648180
3504.509758	512375.563605	42.653184
3504.238482	512369.941034	42.658189
3504.834102	512337.675558	42.663194
3504.665015	512334.869518	42.668199
3504.584181	512301.547457	42.673204
3505.052494	512283.313737	42.678208
3504.696084	512262.327053	42.683213
3504.864918	512229.015974	42.688218
3504.796836	512221.641379	42.693223
3504.958918	512199.510404	42.698228
3504.927843	512169.619946	42.703232
3504.422586	512142.434768	42.708237
3504.725813	512131.207619	42.713242
3504.590542	512107.555403	42.718247
3504.349399	512083.818717	42.723252
3504.450638	512067.767332	42.728256
3504.450548	512048.545113	42.733261
3504.555498	512031.936676	42.738266
3504.611638	512008.557577	42.743271
3504.787292	511994.669508	42.748276
3504.732064	511966.552979	42.753280
3504.313846	511964.190930	42.758285
3504.524813	511920.856771	42.763290
3504.734590	511922.695192	42.768295
3504.436747	511881.667092	42.773300
3504.397751	511873.276045	42.778304
3504.595913	511858.524358	42.783309
3504.638298	511837.625875	42.788314
3504.526361	511829.903943	42.793319
3504.505992	511798.038311	42.798324
3504.532979	511774.511742	42.803329
3504.461718	511772.904198	42.808333
3504.675924	511744.289448	42.813338
3504.672102	511729.771916	42.818343
3504.744976	511695.918516	42.823348
3504.735348	511674.370438	42.828353
3504.135780	511658.075327	42.833357
3504.774659	511633.389552	42.838362
3504.451696	511627.572558	42.843367
3504.464509	511595.448373	42.848372
3504.541596	511582.435507	42.853377
3504.195978	511579.606655	42.858381
3504.585176	511548.282857	42.863386
3504.754281	511539.251721	42.868391
3504.505336	511510.558019	42.873396
3504.460306	511482.186145	42.878401
3504.240836	511478.477370	42.883405
3504.573240	511455.964403	42.888410
3504.223365	511450.404534	42.893415
3504.128906	511433.928202	42.898420
3504.650553	511418.770904	42.903425
3504.351666	511407.183163	42.908429
3504.665042	511389.124733	42.913434
3504.333455	511364.086082	42.918439
3504.294150	511355.846588	42.923444
3504.494092	511331.432097	42.928449
3504.260962	511312.650571	42.933453
3504.576782	511299.751519	42.938458
3504.271787	511279.059012	42.943463
3504.337440	511266.907691	42.948468
3504.609595	511250.525000	42.953473
3504.139662	511232.185508	42.958477
3504.215916	511202.074037	42.963482
3504.687105	511209.233461	42.968487
3504.448148	511179.020006	42.973492
3504.508301	511165.705975	42.978497
3504.103499	511172.143880	42.983501
3504.357005	511165.021523	42.988506
3504.100027	511163.696210	42.993511
3504.283096	511161.997824	42.998516
3504.096861	511130.410093	43.003521
3503.983158	511119.349348	43.008525
3503.835629	511116.489110	43.013530
3504.022792	511114.284199	43.018535
3504.268039	511104.481987	43.023540
3504.274458	511081.412997	43.028545
3504.142082	511068.888133	43.033549
3504.238581	511062.549361	43.038554
3504.408957	511054.124819	43.043559
3504.094929	511025.592348	43.048564
3504.567488	511020.863520	43.053569
3504.288174	511006.844201	43.058573
3504.508625	510979.845989	43.063578
3504.352656	510969.196530	43.068583
3504.352555	510955.689506	43.073588
3504.678132	510935.605152	43.078593
3504.309749	510925.798645	43.083597
3504.409734	510898.667579	43.088602
3504.274595	510900.459449	43.093607
3504.055946	510876.515168	43.098612
3504.592117	510850.428027	43.103617
3504.688644	510846.264465	43.108621
3504.726903	510828.451277	43.113626
3504.652389	510802.966464	43.118631
3504.544445	510792.359892	43.123636
3504.828452	510765.300707	43.128641
3504.446781	510757.266799	43.133645
3504.713564	510723.380820	43.138650
3504.445725	510707.487663	43.143655
3504.451049	510693.676043	43.148660
3504.772168	510660.084883	43.153665
3504.735257	510645.369300	43.158669
3504.696985	510621.952631	43.163674
3504.496747	510606.200461	43.168679
3504.373574	510582.898334	43.173684
3504.451874	510572.161012	43.178689
3504.340886	510558.570021	43.183693
3504.725018	510514.344903	43.188698
3504.646449	510509.247738	43.193703
3504.300518	510479.353484	43.198708
3504.681738	510473.728335	43.203713
3504.418754	510466.940265	43.208717
3504.557024	510424.220863	43.213722
3504.867763	510421.237490	43.218727
3504.701596	510388.684012	43.223732
3504.652221	510371.643042	43.228737
3504.897425	510349.243579	43.233741
3504.745007	510327.514006	43.238746
3504.572836	510300.576774	43.243751
3504.414456	510274.902067	43.248756
3504.727031	510258.056729	43.253761
3504.537822	510248.069742	43.258765
3504.686570	510222.397006	43.263770
3504.529701	510204.563417	43.268775
3504.501971	510194.297927	43.273780
3504.840667	510159.084120	43.278785
3504.371388	510151.468494	43.283789
3504.496186	510131.060797	43.288794
3504.358648	510101.031763	43.293799
3504.442016	510093.379357	43.298804
3504.469860	510061.907584	43.303809
3504.167727	510053.658410	43.308813
3504.383158	510042.494358	43.313818
3504.023685	510039.768616	43.318823
3504.050863	510022.917562	43.323828
3504.214590	510010.952210	43.328833
3504.088942	510017.042882	43.333837
3504.582787	509991.770575	43.338842
3504.376987	509968.935986	43.343847
3504.170141	509966.995564	43.348852
3504.603414	509929.034431	43.353857
3504.195745	509922.724330	43.358861
3504.629517	509913.448142	43.363866
3504.452362	509893.745568	43.368871
3504.118537	509876.850244	43.373876
3504.363706	509864.315416	43.378881
3504.221275	509839.801131	43.383885
3504.414300	509830.613540	43.388890
3504.368091	509820.806068	43.393895
3504.056277	509797.785641	43.398900
3504.225594	509782.733174	43.403905
3504.573104	509787.029039	43.408909
3504.395798	509755.842084	43.413914
3504.172225	509738.726832	43.418919
3504.421801	509729.327882	43.423924
3504.486857	509700.986240	43.428929
3504.100237	509697.607043	43.433933
3504.353737	509673.080536	43.438938
3504.434496	509651.970944	43.443943
3504.504887	509637.389311	43.448948
3504.611229	509626.899923	43.453953
3504.516098	509602.580192	43.458957
3504.550809	509588.560667	43.463962
3504.325601	509565.374464	43.468967
3504.181925	509550.978366	43.473972
3504.625952	509542.307463	43.478977
3504.540246	509524.917248	43.483981
3504.226816	509497.697524	43.488986
3504.268595	509491.012674	43.493991
3504.449901	509470.139929	43.498996
3504.260225	509459.596040	43.504001
3504.450534	509450.408675	43.509005
3504.527884	509420.850410	43.514010
3504.471671	509410.690137	43.519015
3504.703505	509382.271017	43.524020
3504.669156	509338.665525	43.529025
3504.428710	509313.558867	43.534029
3504.339231	509280.991162	43.539034
3504.670833	509270.769513	43.544039
3504.652186	509256.555779	43.549044
3504.556241	509240.431716	43.554049
3504.466778	509228.101092	43.559053
3504.289473	509196.913120	43.564058
3504.344896	509194.880564	43.569063
3504.161929	509180.186806	43.574068
3504.514530	509141.629566	43.579073
3504.404094	509137.650080	43.584077
3504.176666	509128.275599	43.589082
3504.131046	509101.114105	43.594087
3504.606457	509081.611021	43.599092
3504.655071	509071.535166	43.604097
3504.368913	509054.277341	43.609101
3504.750171	509034.030181	43.614106
3504.554708	509008.511218	43.619111
3504.027045	509002.624489	43.624116
3504.687614	508985.267561	43.629121
3504.445031	508962.133882	43.634125
3504.360335	508954.608718	43.639130
3504.672236	508932.449835	43.644135
3504.497544	508918.513453	43.649140
3504.445539	508903.242226	43.654145
3504.470635	508885.429099	43.659149
3504.497198	508860.330172	43.664154
3504.669375	508846.642475	43.669159
3504.293905	508821.303466	43.674164
3504.240664	508806.639479	43.679169
3504.116424	508796.034246	43.684173
3504.226112	508776.993373	43.689178
3504.637737	508760.434480	43.694183
3504.413981	508742.964102	43.699188
3504.307487	508724.463283	43.704193
3504.125264	508720.039695	43.709197
3504.307388	508697.293886	43.714202
3504.271803	508687.534682	43.719207
3503.983549	508682.318328	43.724212
3504.169526	508671.461610	43.729217
3504.426080	508650.221815	43.734221
3504.481165	508631.290601	43.739226
3504.332072	508626.052236	43.744231
3504.365727	508595.588753	43.749236
3504.486624	508578.873254	43.754241
3504.328769	508580.264195	43.759245
3504.218412	508547.040666	43.764250
3504.493005	508528.226431	43.769255
3504.260005	508522.545940	43.774260
3504.210909	508494.321541	43.779265
3504.276970	508502.760422	43.784269
3503.910012	508490.169554	43.789274
3504.349388	508490.757778	43.794279
3504.132613	508463.976496	43.799284
3504.526828	508447.521245	43.804289
3504.217946	508441.903315	43.809293
3504.274376	508411.435907	43.814298
3504.587509	508394.689848	43.819303
3504.266375	508401.621514	43.824308
3504.353911	508355.363302	43.829313
3504.323218	508349.903758	43.834317
3504.369940	508335.729527	43.839322
3504.589988	508316.620109	43.844327
3504.138416	508309.405625	43.849332
3504.483118	508294.526521	43.854337
3504.469862	508266.447872	43.859341
3504.159785	508249.344807	43.864346
3504.145809	508245.147484	43.869351
3504.193105	508226.621824	43.874356
3504.271251	508210.418686	43.879361
3504.149809	508207.604431	43.884365
3504.112599	508192.077256	43.889370
3504.428546	508172.648945	43.894375
3504.236218	508156.943869	43.899380
3504.213736	508142.527437	43.904385
3504.062052	508136.783370	43.909389
3504.199847	508116.624209	43.914394
3504.519247	508109.692561	43.919399
3504.043140	508095.651362	43.924404
3504.040043	508073.389372	43.929409
3504.500355	508061.881755	43.934413
3504.270765	508054.834466	43.939418
3504.477698	508035.018459	43.944423
3504.463815	508019.285055	43.949428
3504.593792	507993.561362	43.954433
3504.314553	507983.233108	43.959437
3504.231903	507984.005050	43.964442
3504.658678	507963.800039	43.969447
3504.309385	507946.601677	43.974452
3504.332254	507933.746403	43.979457
3504.398139	507916.178812	43.984461
3504.178838	507897.340756	43.989466
3504.191498	507890.457500	43.994471
3504.242837	507869.603358	43.999476
3504.398559	507834.312522	44.004481
3504.329779	507841.609305	44.009485
3504.193653	507828.121319	44.014490
3504.335084	507796.121477	44.019495
3504.167181	507794.377040	44.024500
3504.333778	507774.263525	44.029505
3504.315104	507756.607942	44.034509
3503.957403	507748.670023	44.039514
3504.250585	507745.688967	44.044519
3504.142186	507737.357459	44.049524
3504.308644	507708.591733	44.054529
3504.058502	507701.345158	44.059533
3503.910925	507699.192718	44.064538
3504.404259	507686.718282	44.069543
3504.478645	507671.780171	44.074548
3504.138355	507653.922326	44.079553
3504.130299	507652.152610	44.084557
3503.961866	507620.505003	44.089562
3504.200547	507607.665975	44.094567
3504.162390	507612.883505	44.099572
3504.353644	507595.295774	44.104577
3504.190943	507573.007767	44.109581
3504.066004	507565.994335	44.114586
3504.442668	507552.070903	44.119591
3503.897718	507538.191923	44.124596
3503.966860	507517.587533	44.129601
3504.200402	507518.866100	44.134605
3504.304063	507510.855154	44.139610
3504.289047	507487.025753	44.144615
3504.085820	507468.842464	44.149620
3504.404820	507452.701746	44.154625
3504.347279	507455.949055	44.159629
3504.126224	507425.523765	44.164634
3504.391946	507415.716220	44.169639
3504.330086	507409.046944	44.174644
3504.340574	507379.495748	44.179649
3503.962515	507374.546182	44.184653
3504.396612	507369.518853	44.189658
3504.505037	507336.562007	44.194663
3504.270210	507332.702960	44.199668
3504.469819	507322.399825	44.204673
3504.248936	507298.046116	44.209677
3504.149551	507282.072561	44.214682
3504.030739	507274.956846	44.219687
3504.020720	507273.946383	44.224692
3504.214222	507243.455253	44.229697
3504.306498	507233.067832	44.234701
3504.187037	507230.101308	44.239706
3504.274415	507218.905070	44.244711
3504.132593	507186.189885	44.249716
3504.308496	507183.632062	44.254721
3504.192349	507174.694320	44.259725
3504.033575	507149.622199	44.264730
3504.374944	507126.494962	44.269735
3504.150859	507125.670121	44.274740
3504.173906	507116.659750	44.279745
3504.136920	507096.678824	44.284749
3504.297770	507081.473543	44.289754
3504.342847	507083.085525	44.294759
3504.042161	507069.167562	44.299764
3504.089602	507042.190517	44.304769
3504.156649	507037.423502	44.309773
3504.042977	507028.535893	44.314778
3504.252852	507009.325441	44.319783
3504.352718	507001.365459	44.324788
3503.771324	507004.088453	44.329793
3503.784448	507005.047699	44.334797
3503.921378	506989.997917	44.339802
3503.782256	506969.020994	44.344807
3504.003779	506957.803387	44.349812
3503.953172	506942.631405	44.354817
3504.241412	506950.934729	44.359821
3503.998934	506939.992844	44.364826
3504.220945	506921.387574	44.369831
3504.101680	506910.527396	44.374836
3504.152201	506902.625768	44.379841
3504.041937	506904.717717	44.384845
3504.353438	506885.693466	44.389850
3504.337453	506863.330757	44.394855
3504.057854	506861.148479	44.399860
3504.279735	506835.459142	44.404865
3504.421135	506830.730919	44.409869
3503.910815	506817.250685	44.414874
3504.168478	506806.988671	44.419879
3503.609599	506793.010092	44.424884
3503.942102	506774.134200	44.429889
3503.900882	506773.229840	44.434893
3503.966782	506767.349728	44.439898
3504.443539	506764.794895	44.444903
3503.980631	506746.904891	44.449908
3504.338347	506721.801122	44.454913
3504.301522	506719.934657	44.459917
3504.259582	506704.609296	44.464922
3504.357942	506680.254863	44.469927
3504.229320	506675.974078	44.474932
3504.052476	506663.402429	44.479937
3504.049092	506648.222726	44.484941
3503.977037	506630.726234	44.489946
3504.467305	506623.210382	44.494951
3504.162992	506621.436784	44.499956
3504.281041	506593.840676	44.504961
3504.479474	506587.534750	44.509965
3503.999524	506581.538443	44.514970
3504.338017	506557.702494	44.519975
3503.974154	506543.591689	44.524980
3504.385239	506524.045296	44.529985
3504.011106	506527.393417	44.534989
3503.946177	506503.216346	44.539994
3504.191336	506491.640496	44.544999
3504.002299	506493.744944	44.550004
3503.956781	506477.509130	44.555009
3504.148648	506476.719718	44.560013
3503.835041	506461.487680	44.565018
3504.250390	506443.711562	44.570023
3504.085910	506436.147309	44.575028
3504.219814	506433.596014	44.580033
3504.188189	506406.124467	44.585037
3504.236321	506401.208463	44.590042
3504.466412	506377.642407	44.595047
3503.849549	506369.846016	44.600052
3504.224545	506352.430392	44.605057
3504.398980	506342.282461	44.610061
3504.218335	506333.253275	44.615066
3504.621026	506307.433379	44.620071
3504.525063	506296.720939	44.625076
3504.321305	506283.141235	44.630081
3504.067245	506273.921216	44.635085
3504.011016	506263.151873	44.640090
3504.414755	506244.921972	44.645095
3504.073195	506237.537425	44.650100
3503.967859	506219.185549	44.655105
3504.022345	506203.692700	44.660109
3504.076787	506210.110461	44.665114
3504.258781	506206.235885	44.670119
3504.202592	506179.577491	44.675124
3504.211305	506154.932880	44.680129
3504.283441	506162.714117	44.685133
3504.237597	506144.757575	44.690138
3504.443818	506121.903375	44.695143
3504.223964	506124.164544	44.700148
3504.193924	506089.860961	44.705153
3504.212132	506080.901420	44.710157
3504.201391	506075.286198	44.715162
3504.325351	506063.425606	44.720167
3504.089999	506047.067586	44.725172
3504.594242	506027.556516	44.730177
3504.273995	506032.515490	44.735181
3504.100773	505996.412667	44.740186
3504.339714	505986.659154	44.745191
3504.341486	505983.926268	44.750196
3504.202529	505956.369769	44.755201
3504.336755	505949.213517	44.760205
3504.319003	505932.061958	44.765210
3504.307628	505915.061182	44.770215
3504.437982	505890.346369	44.775220
3504.355535	505894.609962	44.780225
3504.606730	505871.039886	44.785229
3503.999121	505850.489877	44.790234
3504.561012	505836.383991	44.795239
3504.525080	505817.970120	44.800244
3504.421690	505798.251211	44.805249
3504.500262	505792.166355	44.810253
3504.115948	505764.091697	44.815258
3504.556938	505744.185482	44.820263
3504.299851	505735.117464	44.825268
3504.419758	505709.138965	44.830273
3504.564656	505698.792915	44.835277
3504.226255	505689.788328	44.840282
3504.624193	505655.972887	44.845287
3504.104868	505646.642648	44.850292
3504.206328	505634.684114	44.855297
3504.403404	505623.469513	44.860301
3504.280371	505613.570587	44.865306
3504.645340	505599.951068	44.870311
3504.391771	505573.525357	44.875316
3504.212643	505556.500142	44.880321
3504.212923	505545.265990	44.885325
3504.073385	505524.287391	44.890330
3504.351453	505518.879363	44.895335
3504.373341	505514.473296	44.900340
3504.349027	505495.551210	44.905345
3504.628957	505472.127866	44.910349
3504.227395	505462.272876	44.915354
3504.544488	505431.607228	44.920359
3504.065059	505427.988829	44.925364
3504.341395	505419.190568	44.930369
3504.523257	505390.823408	44.935373
3504.468603	505384.000403	44.940378
3504.241078	505358.632940	44.945383
3504.344718	505343.688207	44.950388
3504.364933	505335.487032	44.955393
3504.158910	505316.795888	44.960397
3504.015701	505292.831928	44.965402
3504.211298	505282.275201	44.970407
3503.954776	505279.633632	44.975412
3503.936274	505279.130440	44.980417
3504.150254	505248.632581	44.985421
3503.986189	505247.089697	44.990426
3503.962027	505229.837251	44.995431
3504.088528	505232.802864	45.000436
3504.195949	505224.790273	45.005441
3504.102979	505197.832564	45.010445
3504.092652	505185.891391	45.015450
3504.346376	505186.660896	45.020455
3504.024330	505185.800837	45.025460
3503.848831	505155.364373	45.030465
3504.444682	505146.464872	45.035469
3504.134572	505149.044060	45.040474
3504.327026	505123.306248	45.045479
3503.929045	505102.013753	45.050484
3504.253980	505091.436469	45.055489
3504.428817	505084.475866	45.060493
3504.013538	505067.234471	45.065498
3504.285220	505049.024196	45.070503
3504.297127	505054.993658	45.075508
3504.202267	505026.467223	45.080513
3504.406224	505006.091580	45.085517
3503.995269	505008.889148	45.090522
3504.150527	504992.974457	45.095527
3503.964117	504984.451536	45.100532
3503.892187	504962.651890	45.105537
3504.127255	504962.564061	45.110541
3503.719196	504958.124596	45.115546
3504.203251	504950.204169	45.120551
3504.016037	504939.100472	45.125556
3503.771779	504924.210366	45.130561
3503.907348	504896.659411	45.135565
3503.641519	504897.359228	45.140570
3503.953940	504898.777343	45.145575
3503.854139	504897.679721	45.150580
3503.855202	504882.092933	45.155585
3503.952962	504858.646955	45.160589
3503.730751	504857.518071	45.165594
3504.184263	504844.592452	45.170599
3504.086255	504851.540866	45.175604
3503.967917	504850.041324	45.180609
3504.296698	504827.621514	45.185613
3503.508438	504807.604884	45.190618
3503.717838	504806.205357	45.195623
3504.016337	504811.623547	45.200628
3504.041539	504797.449834	45.205633
3504.034303	504797.602724	45.210637
3503.932057	504788.813376	45.215642
3503.983543	504771.852159	45.220647
3503.928241	504772.974161	45.225652
3503.878482	504760.634082	45.230657
3504.083625	504755.237346	45.235661
3503.930577	504754.097524	45.240666
3503.803882	504725.373205	45.245671
3504.101124	504724.465851	45.250676
3504.181542	504718.430936	45.255681
3503.692007	504721.898849	45.260685
3503.496843	504720.310226	45.265690
3503.979518	504712.895972	45.270695
3504.161129	504683.009520	45.275700
3503.964618	504664.467994	45.280705
3504.233893	504662.249292	45.285709
3503.969888	504665.883996	45.290714
3503.896885	504639.377728	45.295719
3503.766696	504622.596900	45.300724
3503.829573	504605.785541	45.305729
3503.897028	504614.327305	45.310733
3504.003026	504617.650508	45.315738
3504.049498	504601.955081	45.320743
3503.872535	504596.213836	45.325748
3503.861484	504573.341346	45.330753
3503.928104	504568.270086	45.335757
3503.808834	504575.778641	45.340762
3504.295179	504570.084372	45.345767
3503.962773	504559.914301	45.350772
3503.984667	504534.607435	45.355777
3504.087481	504521.230939	45.360781
3503.790631	504528.413334	45.365786
3504.147377	504519.652521	45.370791
3503.820158	504518.084751	45.375796
3503.753493	504495.271556	45.380801
3504.117984	504483.321271	45.385805
3504.013137	504483.540198	45.390810
3504.203713	504479.005996	45.395815
3503.952183	504476.717764	45.400820
3503.950929	504443.114895	45.405825
3504.070028	504437.984696	45.410829
3503.711207	504433.334886	45.415834
3504.170631	504428.859394	45.420839
3504.125727	504429.423098	45.425844
3504.108275	504409.284184	45.430849
3504.222242	504387.555656	45.435853
3504.060193	504389.605481	45.440858
3504.087604	504379.682079	45.445863
3503.976828	504359.760287	45.450868
3504.036878	504339.001757	45.455873
3504.109469	504340.710860	45.460877
3503.887659	504337.709410	45.465882
3504.097394	504322.190358	45.470887
3504.253693	504298.683773	45.475892
3503.921126	504298.888086	45.480897
3504.073426	504284.289011	45.485901
3504.180116	504283.715396	45.490906
3504.328616	504257.780832	45.495911
3504.032902	504248.363893	45.500916
3503.942539	504234.865888	45.505921
3504.049584	504240.719375	45.510925
3503.749847	504224.420431	45.515930
3504.281346	504197.160054	45.520935
3504.071827	504189.146475	45.525940
3503.699858	504197.454247	45.530945
3503.732630	504196.183804	45.535949
3504.004682	504182.476656	45.540954
3504.085376	504158.931226	45.545959
3504.021743	504148.617220	45.550964
3503.977564	504145.233408	45.555969
3504.520369	504128.699995	45.560973
3504.012280	504117.545275	45.565978
3504.395574	504099.265769	45.570983
3504.291733	504106.822694	45.575988
3503.944075	504083.041215	45.580993
3504.079914	504058.879639	45.585997
3504.199079	504052.382899	45.591002
3504.120913	504044.146061	45.596007
3503.932590	504049.287173	45.601012
3503.958276	504033.746348	45.606017
3504.289227	504021.649227	45.611021
3503.758698	504009.991903	45.616026
3504.225124	504003.136611	45.621031
3504.153278	503995.455442	45.626036
3503.925707	503972.059699	45.631041
3504.020813	503971.943380	45.636045
3504.311540	503963.496375	45.641050
3504.394569	503947.490936	45.646055
3504.171743	503934.317286	45.651060
3504.054326	503919.709929	45.656065
3504.350335	503912.122409	45.661069
3504.243282	503898.272524	45.666074
3503.878300	503876.366018	45.671079
3504.256539	503861.629666	45.676084
3503.983155	503863.646540	45.681089
3504.121796	503845.051177	45.686093
3503.993155	503831.305868	45.691098
3504.094948	503831.188492	45.696103
3503.905317	503830.712304	45.701108
3503.766279	503816.260105	45.706113
3503.936848	503785.058042	45.711117
3503.604859	503783.440350	45.716122
3503.671018	503778.115890	45.721127
3504.068579	503778.103594	45.726132
3503.825909	503776.319957	45.731137
3504.175096	503778.693923	45.736141
3503.672577	503753.721861	45.741146
3504.276710	503736.064991	45.746151
3504.308934	503741.323162	45.751156
3504.007356	503736.360465	45.756161
3504.261777	503713.596725	45.761165
3503.962244	503703.319742	45.766170
3504.118830	503686.340866	45.771175
3504.260713	503681.510501	45.776180
3504.042181	503664.995765	45.781185
3504.051735	503645.408409	45.786189
3503.861916	503635.721358	45.791194
3503.904523	503629.995701	45.796199
3503.632051	503630.949662	45.801204
3503.561509	503639.969194	45.806209
3504.137501	503622.215440	45.811213
3504.115617	503612.906708	45.816218
3504.435814	503589.879366	45.821223
3503.995908	503574.816598	45.826228
3504.285887	503575.732276	45.831233
3504.287668	503541.013795	45.836237
3503.640339	503545.519066	45.841242
3504.107941	503533.400013	45.846247
3504.083608	503539.831204	45.851252
3503.729269	503521.110976	45.856257
3504.169503	503485.563945	45.861261
3503.721370	503496.262740	45.866266
3503.804432	503478.941018	45.871271
3503.682924	503489.841242	45.876276
3504.029334	503488.824837	45.881281
3504.141840	503469.625892	45.886285
3504.002389	503466.560665	45.891290
3504.123041	503442.299424	45.896295
3503.845258	503435.156656	45.901300
3503.443524	503452.478036	45.906305
3504.108108	503434.710092	45.911309
3503.603827	503427.603119	45.916314
3504.056555	503407.945456	45.921319
3503.641886	503398.648080	45.926324
3503.938514	503393.287079	45.931329
3504.340090	503384.974109	45.936333
3503.714847	503397.168646	45.941338
3504.067331	503376.818252	45.946343
3504.121152	503364.865702	45.951348
3503.945268	503342.928645	45.956353
3504.195571	503342.231082	45.961357
3503.923665	503338.528835	45.966362
3504.205315	503333.068963	45.971367
3504.158809	503306.303446	45.976372
3504.218646	503307.711004	45.981377
3504.323277	503285.881372	45.986381
3503.791414	503277.513439	45.991386
3504.187262	503244.958948	45.996391
3503.762115	503242.040057	46.001396
3503.688334	503243.620570	46.006401
3503.840277	503233.676839	46.011405
3503.499648	503235.653801	46.016410
3504.269931	503229.306902	46.021415
3503.849930	503204.978953	46.026420
3503.718419	503199.381898	46.031425
3504.096481	503184.594399	46.036429
3503.705366	503195.638638	46.041434
3503.573139	503179.413469	46.046439
3503.651464	503184.462078	46.051444
3503.760716	503193.301591	46.056449
3503.846885	503172.537558	46.061453
3503.752788	503158.685043	46.066458
3504.185054	503134.576571	46.071463
3503.874425	503144.595906	46.076468
3504.098981	503134.792476	46.081473
3503.840591	503134.985075	46.086477
3503.823986	503117.678750	46.091482
3503.866982	503102.184978	46.096487
3503.894498	503086.086309	46.101492
3503.669380	503100.444688	46.106497
3503.992957	503086.222438	46.111501
3503.972911	503091.539676	46.116506
3504.046248	503080.089957	46.121511
3503.829874	503064.738367	46.126516
3504.153229	503056.235162	46.131521
3504.080840	503049.059775	46.136525
3503.949066	503053.989795	46.141530
3504.029599	503027.203776	46.146535
3504.245880	503014.111869	46.151540
3503.853879	503008.454701	46.156545
3503.985147	503003.878884	46.161549
3503.997982	502994.513727	46.166554
3503.957411	502986.928396	46.171559
3504.155015	502963.514725	46.176564
3503.861956	502961.789579	46.181569
3504.037770	502954.929204	46.186573
3504.241946	502953.530359	46.191578
3504.146967	502933.098342	46.196583
3504.271902	502915.010279	46.201588
3503.777408	502906.686874	46.206593
3504.128732	502907.086779	46.211597
3503.934056	502891.782221	46.216602
3504.154545	502872.312503	46.221607
3504.093989	502861.136861	46.226612
3503.924594	502860.708059	46.231617
3504.044370	502839.988935	46.236621
3503.830068	502837.643990	46.241626
3503.778656	502809.765041	46.246631
3503.946232	502809.687873	46.251636
3503.735357	502809.113791	46.256641
3503.906386	502809.187912	46.261645
3503.905930	502796.534992	46.266650
3503.895600	502791.880277	46.271655
3503.653028	502782.352928	46.276660
3503.514457	502765.925934	46.281665
3504.011552	502752.485781	46.286669
3503.690456	502758.103759	46.291674
3503.775906	502751.409422	46.296679
3503.810242	502752.517384	46.301684
3503.568963	502755.592157	46.306689
3504.127538	502742.699009	46.311693
3503.793796	502745.636561	46.316698
3503.770296	502728.330944	46.321703
3503.838782	502710.302205	46.326708
3504.083578	502713.198937	46.331713
3504.383570	502698.625820	46.336717
3504.000158	502704.962231	46.341722
3503.476340	502684.091585	46.346727
3503.980246	502671.409473	46.351732
3503.878661	502658.772439	46.356737
3503.974178	502662.148281	46.361741
3503.786508	502669.466010	46.366746
3503.791886	502654.939421	46.371751
3503.883268	502663.630187	46.376756
3503.632094	502632.948254	46.381761
3504.104319	502625.534782	46.386765
3503.890057	502620.912253	46.391770
3503.970331	502629.655404	46.396775
3503.950484	502612.197260	46.401780
3504.237076	502611.595158	46.406785
3504.148631	502585.695585	46.411789
3504.121183	502580.385560	46.416794
3504.209509	502575.664583	46.421799
3504.168665	502573.241575	46.426804
3503.962351	502551.510792	46.431809
3504.308094	502519.215948	46.436813
3504.303390	502517.748858	46.441818
3504.174048	502522.476191	46.446823
3504.134580	502497.074872	46.451828
3504.026531	502494.864926	46.456833
3503.837951	502485.835009	46.461837
3504.044658	502482.816125	46.466842
3504.334212	502453.668022	46.471847
3504.383887	502441.664891	46.476852
3503.964466	502439.251086	46.481857
3504.379927	502419.395766	46.486861
3504.169879	502399.841736	46.491866
3504.113310	502389.272520	46.496871
3504.174174	502388.807314	46.501876
3503.998396	502356.898277	46.506881
3504.293867	502345.058684	46.511885
3504.014951	502344.697792	46.516890
3504.054908	502337.605585	46.521895
3504.195323	502321.387150	46.526900
3504.039581	502313.566668	46.531905
3504.221133	502297.696001	46.536909
3504.078792	502297.111069	46.541914
3504.087883	502285.822830	46.546919
3504.191224	502256.450769	46.551924
3503.994369	502245.397507	46.556929
3504.369647	502246.856521	46.561933
3504.120018	502231.560076	46.566938
3503.859906	502208.723882	46.571943
3503.947551	502198.384826	46.576948
3503.881170	502204.266401	46.581953
3504.387400	502192.494623	46.586957
3504.076528	502183.888787	46.591962
3503.934906	502162.906504	46.596967
3504.039574	502147.351536	46.601972
3504.079535	502146.585945	46.606977
3504.333645	502138.852450	46.611981
3503.999464	502113.649002	46.616986
3504.032155	502116.933651	46.621991
3503.688169	502105.954169	46.626996
3503.855066	502100.258988	46.632001
3504.012502	502096.235552	46.637005
3503.898971	502077.323890	46.642010
3504.079797	502065.401002	46.647015
3504.069750	502058.417815	46.652020
3504.320252	502057.416490	46.657025
3504.292671	502033.632270	46.662029
3504.216639	502026.912568	46.667034
3503.982108	502017.231694	46.672039
3504.139648	502003.237274	46.677044
3503.941671	501985.654824	46.682049
3504.082414	501976.218298	46.687053
3504.049716	501966.201812	46.692058
3504.104234	501961.739085	46.697063
3504.121539	501949.082753	46.702068
3504.008058	501929.462328	46.707073
3504.271485	501918.690413	46.712077
3503.909252	501921.430146	46.717082
3504.143918	501905.803805	46.722087
3504.384338	501879.243852	46.727092
3503.991270	501875.206144	46.732097
3504.016609	501867.154388	46.737101
3503.848491	501861.309622	46.742106
3503.872444	501837.314536	46.747111
3504.135573	501832.059590	46.752116
3503.789795	501831.709253	46.757121
3503.830357	501812.621111	46.762125
3503.860335	501822.233056	46.767130
3503.754782	501813.392131	46.772135
3504.002981	501802.268251	46.777140
3503.623739	501783.297042	46.782145
3503.931129	501774.289602	46.787149
3504.070764	501773.811930	46.792154
3503.989763	501774.938183	46.797159
3503.927923	501770.139497	46.802164
3503.678297	501757.373372	46.807169
3503.951217	501743.613586	46.812173
3504.095540	501740.148904	46.817178
3504.066461	501730.030483	46.822183
3504.276996	501730.705743	46.827188
3503.881091	501716.089963	46.832193
3504.079279	501691.156076	46.837197
3504.125838	501682.291044	46.842202
3503.946430	501679.940429	46.847207
3504.086765	501672.072869	46.852212
3504.017172	501654.014264	46.857217
3503.907057	501627.711797	46.862221
3503.783284	501638.562903	46.867226
3504.001227	501626.431395	46.872231
3504.289817	501627.549858	46.877236
3503.732332	501618.122268	46.882241
3503.812050	501597.003103	46.887245
3503.645320	501590.955567	46.892250
3503.606574	501588.835784	46.897255
3503.995796	501582.143611	46.902260
3504.057042	501579.198180	46.907265
3504.179920	501578.470076	46.912269
3504.039349	501551.463696	46.917274
3503.834424	501545.675258	46.922279
3503.972745	501540.541183	46.927284
3503.575812	501543.944455	46.932289
3503.959651	501539.075267	46.937293
3504.060734	501543.513364	46.942298
3504.068922	501512.383576	46.947303
3504.237093	501496.210617	46.952308
3504.087505	501492.994801	46.957313
3504.191241	501483.918172	46.962317
3503.743195	501459.035482	46.967322
3503.745550	501448.456392	46.972327
3503.935337	501440.682145	46.977332
3503.766557	501448.503546	46.982337
3503.712575	501446.993540	46.987341
3503.684074	501440.114257	46.992346
3503.844881	501443.328167	46.997351
3503.778770	501436.454827	47.002356
3503.809735	501411.648209	47.007361
3504.083426	501401.785442	47.012365
3503.933503	501396.545035	47.017370
3503.606153	501390.117891	47.022375
3503.541143	501396.455058	47.027380
3503.741538	501394.449302	47.032385
3503.725969	501394.249229	47.037389
3503.790249	501390.189742	47.042394
3503.787921	501372.778225	47.047399
3503.602212	501350.536555	47.052404
3503.801754	501347.923539	47.057409
3503.797842	501339.876167	47.062413
3503.927382	501343.297500	47.067418
3503.601567	501349.422825	47.072423
3504.000894	501346.727617	47.077428
3503.701581	501351.633972	47.082433
3503.832184	501338.250677	47.087437
3503.910745	501308.121726	47.092442
3503.612742	501307.561363	47.097447
3504.001444	501298.490216	47.102452
3503.521417	501300.540036	47.107457
3503.925264	501293.845444	47.112461
3504.087641	501292.149382	47.117466
3503.739819	501298.379434	47.122471
3504.073983	501280.459100	47.127476
3503.522391	501267.487269	47.132481
3503.769066	501252.972011	47.137485
3503.671621	501243.876440	47.142490
3503.552325	501245.413707	47.147495
3503.922619	501248.088382	47.152500
3503.520253	501248.961763	47.157505
3503.952810	501245.299582	47.162509
3503.941473	501250.717227	47.167514
3503.869154	501227.293311	47.172519
3503.729212	501204.082518	47.177524
3503.580414	501210.432993	47.182529
3503.650063	501194.123482	47.187533
3503.653480	501206.625086	47.192538
3503.748572	501193.550992	47.197543
3503.898612	501191.553173	47.202548
3503.458861	501191.774453	47.207553
3504.034027	501189.506977	47.212557
3504.049193	501176.293654	47.217562
3503.854238	501167.112222	47.222567
3504.180237	501151.116470	47.227572
3503.914169	501153.132490	47.232577
3504.410400	501136.249342	47.237581
3504.239379	501122.458008	47.242586
3503.768903	501099.906717	47.247591
3504.283930	501102.659772	47.252596
3504.034368	501100.876949	47.257601
3504.103533	501088.464891	47.262605
3504.091747	501057.843630	47.267610
3503.811722	501060.114950	47.272615
3504.501771	501046.491166	47.277620
3504.231661	501035.954894	47.282625
3504.093257	501012.946075	47.287629
3504.145750	501021.998110	47.292634
3504.192272	501003.060008	47.297639
3504.147068	500985.401804	47.302644
3503.919475	500977.237770	47.307649
3504.144104	500983.782391	47.312653
3504.290661	500965.537074	47.317658
3503.760647	500949.625818	47.322663
3504.320329	500930.302832	47.327668
3503.974979	500931.521535	47.332673
3504.060677	500920.017852	47.337677
3503.880676	500916.351185	47.342682
3503.793312	500890.398351	47.347687
3504.212571	500884.409811	47.352692
3503.713496	500882.717018	47.357697
3504.167100	500883.252661	47.362701
3504.153260	500881.381942	47.367706
3504.034166	500845.260006	47.372711
3504.250355	500835.152928	47.377716
3503.930645	500832.976226	47.382721
3504.337645	500828.153802	47.387725
3504.319911	500806.542929	47.392730
3504.167077	500793.052170	47.397735
3504.236646	500785.094169	47.402740
3503.907967	500758.521256	47.407745
3503.895377	500743.995944	47.412749
3503.960829	500745.757142	47.417754
3504.057109	500736.580076	47.422759
3503.856456	500734.131457	47.427764
3503.818023	500738.186866	47.432769
3504.130060	500711.057060	47.437773
3504.039258	500700.441631	47.442778
3503.808802	500698.200189	47.447783
3503.901921	500684.316151	47.452788
3503.641455	500688.609134	47.457793
3503.656997	500697.616556	47.462797
3503.719317	500683.231208	47.467802
3503.673052	500664.965442	47.472807
3503.697048	500639.956381	47.477812
3503.676227	500652.462204	47.482817
3503.477150	500639.079873	47.487821
3503.820644	500651.021938	47.492826
3503.672182	500639.453848	47.497831
3504.277112	500639.256933	47.502836
3504.069340	500642.529242	47.507841
3503.701566	500620.112963	47.512845
3503.777837	500610.230344	47.517850
3503.533638	500599.689719	47.522855
3503.642097	500595.167507	47.527860
3503.585743	500597.251679	47.532865
3503.694685	500587.566356	47.537869
3503.492040	500596.051516	47.542874
3503.746533	500590.898807	47.547879
3503.950195	500584.893624	47.552884
3503.802908	500584.208179	47.557889
3503.843729	500585.618961	47.562893
3503.877964	500561.873622	47.567898
3503.935864	500550.070386	47.572903
3503.729096	500533.145923	47.577908
3503.437127	500551.616994	47.582913
3503.720126	500537.146032	47.587917
3503.568172	500528.969838	47.592922
3503.675661	500545.859235	47.597927
3504.095302	500533.593871	47.602932
3504.218955	500528.208732	47.607937
3504.117260	500509.091059	47.612941
3504.161121	500500.833285	47.617946
3504.203226	500493.335058	47.622951
3504.255466	500477.128880	47.627956
3503.925206	500466.247449	47.632961
3503.922342	500445.848629	47.637965
3504.284087	500449.132198	47.642970
3503.754980	500440.711862	47.647975
3504.149453	500422.578663	47.652980
3503.599661	500414.161583	47.657985
3503.748404	500408.114403	47.662989
3503.927605	500409.098379	47.667994
3503.910096	500405.507161	47.672999
3503.992545	500398.609941	47.678004
3503.835720	500394.332080	47.683009
3503.754866	500365.795909	47.688013
3503.960229	500350.881499	47.693018
3503.585999	500357.875331	47.698023
3503.592216	500350.939521	47.703028
3503.725222	500347.526978	47.708033
3503.624923	500348.453895	47.713037
3503.787894	500353.135602	47.718042
3503.658250	500350.726326	47.723047
3503.892015	500342.792795	47.728052
3503.802225	500330.962139	47.733057
3503.686580	500306.075918	47.738061
3504.102285	500296.291334	47.743066
3503.720791	500302.577672	47.748071
3503.894746	500290.300353	47.753076
3503.790589	500298.972563	47.758081
3503.818794	500288.793650	47.763085
3503.753408	500296.649832	47.768090
3503.544450	500274.815444	47.773095
3503.753271	500254.028617	47.778100
3503.515487	500254.977268	47.783105
3503.858514	500250.215420	47.788109
3503.632477	500241.595232	47.793114
3503.774750	500257.062074	47.798119
3504.011775	500247.356323	47.803124
3503.821714	500250.069095	47.808129
3503.795813	500245.264317	47.813133
3503.795094	500239.341940	47.818138
3503.946945	500231.117592	47.823143
3504.156279	500217.467919	47.828148
3503.932100	500215.529137	47.833153
3503.740130	500209.738215	47.838157
3504.208760	500210.929554	47.843162
3503.953301	500194.974228	47.848167
3503.920635	500178.578723	47.853172
3503.982715	500169.305533	47.858177
3503.996061	500160.748709	47.863181
3504.140068	500163.459315	47.868186
3504.110499	500136.990059	47.873191
3504.230017	500115.710992	47.878196
3503.719565	500128.092091	47.883201
3504.025774	500115.490034	47.888205
3504.197539	500100.833824	47.893210
3503.601302	500086.501461	47.898215
3504.131347	500070.928070	47.903220
3504.012262	500078.792834	47.908225
3503.817868	500070.977473	47.913229
3503.939899	500064.883779	47.918234
3503.516361	500057.003389	47.923239
3503.457016	500036.714269	47.928244
3503.499764	500028.557691	47.933249
3503.532126	500025.059755	47.938253
3503.556592	500028.143611	47.943258
3503.482854	500027.446520	47.948263
3503.573654	500027.837055	47.953268
3503.496854	500021.015478	47.958273
3503.671766	500019.317315	47.963277
3503.907873	500015.432837	47.968282
3503.573270	500031.076484	47.973287
3503.740253	500013.535642	47.978292
3503.895419	500019.281683	47.983297
3503.835775	500007.041090	47.988301
3504.073892	500014.039513	47.993306
3503.747126	500001.031222	47.998311
3503.761861	499973.592948	48.003316
3503.688475	499978.059012	48.008321
3503.510220	499967.001392	48.013325
3503.764073	499973.896104	48.018330
3503.552233	499977.321036	48.023335
3503.892360	499972.205235	48.028340
3503.969940	499978.064791	48.033345
3503.967207	499971.079629	48.038349
3504.065411	499943.476259	48.043354
3503.627923	499934.889342	48.048359
3503.658309	499920.457808	48.053364
3503.625793	499928.207716	48.058369
3503.607063	499920.769485	48.063373
3503.794193	499916.386527	48.068378
3503.538403	499929.739911	48.073383
3503.963114	499914.537371	48.078388
3503.722599	499919.941022	48.083393
3503.814684	499912.687752	48.088397
3504.054065	499880.101220	48.093402
3503.654860	499880.619823	48.098407
3503.841922	499873.807106	48.103412
3503.818237	499871.026678	48.108417
3503.937982	499875.361002	48.113421
3504.123856	499863.385228	48.118426
3504.060990	499861.724631	48.123431
3504.307210	499834.603899	48.128436
3504.045622	499833.632770	48.133441
3504.051933	499830.037672	48.138445
3504.121691	499813.878745	48.143450
3504.214530	499787.440246	48.148455
3504.057496	499781.896765	48.153460
3503.924492	499780.146006	48.158465
3504.133117	499771.051929	48.163469
3504.240048	499747.952085	48.168474
3503.792458	499744.226227	48.173479
3503.908979	499732.868771	48.178484
3504.298747	499739.590231	48.183489
3504.139072	499710.508648	48.188493
3504.289151	499701.170687	48.193498
3504.169377	499699.316588	48.198503
3504.002018	499684.409912	48.203508
3503.893219	499658.964884	48.208513
3504.130604	499653.460266	48.213517
3504.217372	499642.866765	48.218522
3504.000525	499646.596275	48.223527
3504.270591	499622.913659	48.228532
3503.872675	499605.967908	48.233537
3504.058118	499604.774250	48.238541
3504.262056	499601.198492	48.243546
3503.902969	499581.766163	48.248551
3503.799091	499554.244753	48.253556
3504.227388	499560.200877	48.258561
3503.956572	499556.750766	48.263565
3504.121561	499546.347330	48.268570
3503.780999	499538.099249	48.273575
3504.007736	499509.158750	48.278580
3503.770767	499496.844593	48.283585
3503.772309	499505.854828	48.288589
3504.107271	499500.334742	48.293594
3504.110711	499508.686601	48.298599
3504.130260	499481.550540	48.303604
3503.977131	499479.904174	48.308609
3504.096779	499469.507859	48.313613
3504.029423	499460.406624	48.318618
3503.797070	499457.557869	48.323623
3504.067092	499429.825309	48.328628
3503.877540	499427.020406	48.333633
3503.857531	499421.202050	48.338637
3503.876419	499414.061390	48.343642
3503.942347	499412.886609	48.348647
3504.050088	499411.350870	48.353652
3503.814579	499392.708745	48.358657
3503.661246	499379.976318	48.363661
3504.098957	499373.883119	48.368666
3503.530808	499372.707308	48.373671
3503.732171	499369.233154	48.378676
3503.802578	499367.602069	48.383681
3503.788406	499368.768531	48.388685
3504.227444	499356.549921	48.393690
3504.015400	499328.944018	48.398695
3504.059388	499326.507160	48.403700
3504.238922	499324.453851	48.408705
3503.932797	499299.798823	48.413709
3503.955387	499290.531421	48.418714
3503.693445	499278.069195	48.423719
3503.735270	499280.492355	48.428724
3503.988458	499273.517095	48.433729
3503.859022	499268.576553	48.438733
3503.946274	499280.357549	48.443738
3503.589849	499267.657142	48.448743
3503.853101	499240.684686	48.453748
3503.757644	499222.880820	48.458753
3503.320799	499229.783741	48.463757
3503.814612	499218.771304	48.468762
3503.479413	499222.975203	48.473767
3503.740416	499217.770451	48.478772
3503.990562	499210.340051	48.483777
3503.720401	499212.863151	48.488781
3503.790441	499213.054498	48.493786
3503.827310	499217.604568	48.498791
3504.006975	499206.489909	48.503796
3503.980728	499190.497460	48.508801
3503.536223	499186.214156	48.513805
3503.831174	499175.789964	48.518810
3503.442258	499176.863801	48.523815
3503.755254	499170.435891	48.528820
3503.829488	499167.437389	48.533825
3503.659814	499173.133799	48.538829
3503.804435	499165.416326	48.543834
3503.679340	499168.777079	48.548839
3503.859216	499141.513920	48.553844
3503.704798	499133.590587	48.558849
3503.622959	499128.389373	48.563853
3503.857058	499121.214583	48.568858
3503.777791	499132.060174	48.573863
3503.710895	499123.211806	48.578868
3503.795851	499117.579250	48.583873
3503.562747	499113.971226	48.588877
3503.978170	499117.904647	48.593882
3503.598651	499099.993689	48.598887
3503.713529	499074.664345	48.603892
3503.444004	499074.959984	48.608897
3503.524182	499077.832710	48.613901
3503.875707	499071.904897	48.618906
3503.720490	499074.055494	48.623911
3503.781027	499073.134654	48.628916
3503.898229	499071.192413	48.633921
3503.941182	499074.121645	48.638925
3504.074052	499064.583585	48.643930
3503.633445	499043.948621	48.648935
3503.584683	499028.516432	48.653940
3503.573834	499021.481561	48.658945
3503.855342	499027.309197	48.663949
3503.841040	499013.795201	48.668954
3503.678465	499033.107963	48.673959
3503.636656	499016.004126	48.678964
3503.611418	499017.476095	48.683969
3503.591010	499013.530699	48.688973
3504.058176	499019.784596	48.693978
3503.835171	499001.190711	48.698983
3503.988563	498978.285023	48.703988
3504.244060	498976.675272	48.708993
3503.769764	498984.292921	48.713997
3503.855914	498972.737295	48.719002
3503.892405	498972.478344	48.724007
3503.695825	498946.134972	48.729012
3503.429305	498935.546270	48.734017
3503.247460	498935.625562	48.739021
3503.733750	498922.083000	48.744026
3503.547372	498935.679264	48.749031
3503.389337	498931.654357	48.754036
3503.662466	498925.485774	48.759041
3503.667766	498924.371166	48.764045
3504.021097	498918.240527	48.769050
3503.742223	498931.750167	48.774055
3503.974432	498921.740727	48.779060
3503.660769	498921.486494	48.784065
3503.736818	498921.120045	48.789069
3504.261735	498896.535607	48.794074
3503.700983	498893.333683	48.799079
3503.861197	498876.552143	48.804084
3503.698343	498884.576216	48.809089
3503.649194	498886.507579	48.814093
3503.777565	498869.224837	48.819098
3503.730650	498880.116089	48.824103
3504.011412	498852.887172	48.829108
3503.632751	498850.770164	48.834113
3503.962142	498836.594239	48.839117
3503.856056	498827.296312	48.844122
3503.453144	498832.169102	48.849127
3503.772066	498831.004920	48.854132
3503.994330	498820.237651	48.859137
3503.883936	498825.064211	48.864141
3503.978936	498812.444001	48.869146
3503.248773	498800.662923	48.874151
3503.413152	498795.928928	48.879156
3503.641014	498784.907638	48.884161
3503.476989	498785.844707	48.889165
3503.830395	498782.447656	48.894170
3503.805383	498787.058238	48.899175
3503.887463	498776.920577	48.904180
3503.899693	498778.285396	48.909185
3503.514824	498782.092263	48.914189
3503.886818	498780.919690	48.919194
3503.796288	498776.225979	48.924199
3503.815418	498769.034402	48.929204
3503.564992	498747.356577	48.934209
3503.932821	498736.667497	48.939213
3504.170019	498724.480361	48.944218
3503.552842	498735.866816	48.949223
3503.531947	498728.225940	48.954228
3503.972047	498721.676535	48.959233
3503.695177	498730.883031	48.964237
3504.191499	498719.869894	48.969242
3503.949633	498709.277161	48.974247
3503.867492	498696.937985	48.979252
3503.809897	498685.708634	48.984257
3503.737172	498692.655456	48.989261
3503.895533	498684.378749	48.994266
3503.949617	498681.838962	48.999271
3503.542985	498659.426368	49.004276
3503.765422	498644.912832	49.009281
3503.860796	498651.984973	49.014285
3504.172871	498639.988439	49.019290
3503.960714	498643.261802	49.024295
3503.759938	498642.584735	49.029300
3504.264827	498634.101366	49.034305
3503.610363	498612.082248	49.039309
3504.099779	498595.704028	49.044314
3503.574251	498603.076816	49.049319
3503.774560	498598.033349	49.054324
3504.107609	498601.423045	49.059329
3503.849839	498591.187121	49.064333
3503.960030	498565.047824	49.069338
3503.931461	498553.206319	49.074343
3503.702962	498548.635602	49.079348
3503.965581	498551.428953	49.084353
3503.530738	498543.904047	49.089357
3504.006917	498534.918932	49.094362
3504.001084	498531.679860	49.099367
3503.281192	498518.580753	49.104372
3503.656216	498506.169190	49.109377
3503.800738	498503.665708	49.114381
3503.828774	498508.622345	49.119386
3503.790524	498513.032594	49.124391
3504.021334	498494.062715	49.129396
3503.915254	498501.217379	49.134401
3503.617514	498505.010532	49.139405
3504.017978	498486.975685	49.144410
3503.997098	498472.348596	49.149415
3503.726993	498461.810804	49.154420
3503.837881	498449.491573	49.159425
3503.563684	498450.851064	49.164429
3503.928742	498453.223248	49.169434
3503.904039	498455.150794	49.174439
3503.708281	498434.527055	49.179444
3503.905477	498417.739243	49.184449
3503.397045	498408.707187	49.189453
3503.921881	498395.006267	49.194458
3503.874623	498404.834753	49.199463
3503.904369	498402.450645	49.204468
3504.030872	498400.658735	49.209473
3503.563755	498402.149968	49.214477
3503.794600	498385.660553	49.219482
3503.769551	498377.665815	49.224487
3503.931488	498363.971604	49.229492
3503.893633	498350.055838	49.234497
3504.037365	498357.930439	49.239501
3503.853511	498348.391435	49.244506
3503.655974	498358.952438	49.249511
3503.969962	498344.373567	49.254516
3504.018038	498321.179944	49.259521
3503.764074	498318.790041	49.264525
3503.879976	498303.938699	49.269530
3503.934270	498306.461268	49.274535
3504.114232	498312.305187	49.279540
3504.248294	498290.515418	49.284545
3503.823823	498284.051877	49.289549
3503.890988	498261.057658	49.294554
3504.058446	498263.056102	49.299559
3503.790767	498262.136471	49.304564
3503.985024	498252.335157	49.309569
3503.638302	498234.114404	49.314573
3503.684803	498223.121435	49.319578
3503.282633	498223.387426	49.324583
3503.729901	498212.938606	49.329588
3503.898610	498206.077536	49.334593
3503.535412	498209.020477	49.339597
3503.921806	498207.238096	49.344602
3503.897391	498220.758675	49.349607
3503.683995	498217.046106	49.354612
3503.882503	498198.587268	49.359617
3503.626629	498180.098978	49.364621
3503.747028	498166.664306	49.369626
3503.536987	498174.645527	49.374631
3503.518490	498161.789677	49.379636
3503.890025	498166.692117	49.384641
3503.606778	498169.419929	49.389645
3503.766325	498161.244045	49.394650
3503.726528	498161.351513	49.399655
3503.445385	498158.358387	49.404660
3503.705912	498156.089646	49.409665
3503.580000	498167.651937	49.414669
3503.876798	498159.808734	49.419674
3503.842194	498141.285432	49.424679
3503.809505	498130.304923	49.429684
3504.015571	498116.856675	49.434689
3503.638309	498123.699973	49.439693
3503.718014	498110.828566	49.444698
3504.139989	498116.229298	49.449703
3504.051781	498108.649422	49.454708
3504.076415	498085.206077	49.459713
3504.040727	498077.820388	49.464717
3504.059707	498070.223555	49.469722
3503.796919	498072.340647	49.474727
3503.852345	498059.219914	49.479732
3504.034373	498041.674774	49.484737
3503.744618	498027.039194	49.489741
3504.141909	498020.141926	49.494746
3504.002064	498027.808366	49.499751
3503.745466	498022.128201	49.504756
3504.061335	498008.814393	49.509761
3503.987314	497984.171503	49.514765
3504.176456	497974.522723	49.519770
3503.818032	497983.843738	49.524775
3503.960724	497979.366085	49.529780
3504.277647	497970.152735	49.534785
3503.820371	497957.366088	49.539789
3503.788945	497947.954656	49.544794
3503.921290	497944.592390	49.549799
3504.030741	497933.184292	49.554804
3503.983069	497929.394845	49.559809
3503.838237	497914.230013	49.564813
3504.037127	497885.696314	49.569818
3503.811374	497897.223932	49.574823
3503.830004	497893.322747	49.579828
3504.205115	497889.010840	49.584833
3503.672830	497881.298554	49.589837
3503.682013	497867.020601	49.594842
3503.728303	497848.433588	49.599847
3503.771052	497841.541663	49.604852
3503.671449	497847.429918	49.609857
3503.992577	497844.189672	49.614861
3503.850035	497831.251940	49.619866
3503.971209	497839.434089	49.624871
3503.898496	497828.004090	49.629876
3503.835313	497796.119744	49.634881
3503.741710	497797.349488	49.639885
3503.619547	497797.216847	49.644890
3503.569746	497798.237164	49.649895
3503.832420	497791.766093	49.654900
3503.918555	497788.461727	49.659905
3503.549709	497792.367518	49.664909
3503.968404	497788.808087	49.669914
3503.898681	497772.213741	49.674919
3503.718472	497760.952567	49.679924
3503.939086	497740.970991	49.684929
3503.738959	497754.823446	49.689933
3503.801283	497753.092241	49.694938
3503.932004	497741.427531	49.699943
3503.660482	497740.002220	49.704948
3503.942072	497743.805220	49.709953
3503.480760	497731.120303	49.714957
3504.002916	497702.484596	49.719962
3503.865351	497704.480686	49.724967
3503.449149	497701.002568	49.729972
3503.898942	497694.957523	49.734977
3503.834357	497700.334030	49.739981
3503.660627	497694.134403	49.744986
3503.780738	497699.177962	49.749991
3503.768368	497690.016514	49.754996
3504.095355	497658.272763	49.760001
3503.396710	497671.545931	49.765005
3503.720555	497644.561515	49.770010
3503.677157	497647.909638	49.775015
3503.392416	497658.282326	49.780020
3504.019240	497648.007308	49.785025
3503.688589	497654.185274	49.790029
3503.707962	497648.208242	49.795034
3503.460171	497657.360061	49.800039
3503.494390	497661.809691	49.805044
3504.178807	497650.057410	49.810049
3503.698046	497634.236670	49.815053
3503.500141	497615.283002	49.820058
3503.751345	497599.599675	49.825063
3503.720268	497610.236058	49.830068
3503.698740	497607.353686	49.835073
3503.383275	497611.099200	49.840077
3503.995698	497598.902627	49.845082
3503.961820	497606.501870	49.850087
3503.961343	497599.262300	49.855092
3504.041849	497578.847051	49.860097
3503.826085	497562.579353	49.865101
3503.709602	497548.776650	49.870106
3503.749915	497556.971706	49.875111
3503.905008	497547.631840	49.880116
3504.026673	497548.422564	49.885121
3504.163380	497545.413920	49.890125
3504.003386	497525.998528	49.895130
3503.718675	497522.398339	49.900135
3503.758272	497511.102270	49.905140
3503.890155	497498.627193	49.910145
3503.585539	497509.357495	49.915149
3503.544378	497502.984969	49.920154
3503.888097	497503.183707	49.925159
3503.577285	497498.929492	49.930164
3504.059558	497469.945336	49.935169
3503.984717	497468.387663	49.940173
3503.860853	497449.624627	49.945178
3503.756418	497453.336819	49.950183
3503.792677	497457.229282	49.955188
3503.834658	497452.767417	49.960193
3503.550132	497453.318583	49.965197
3503.680818	497434.110284	49.970202
3503.661683	497413.356209	49.975207
3503.725731	497415.978616	49.980212
3503.714112	497402.513615	49.985217
3503.948705	497403.134617	49.990221
3503.957047	497399.943729	49.995226
3504.006837	497405.808516	50.000231
3503.773768	497402.149514	50.005236
3503.835478	497384.572127	50.010241
3503.538863	497371.152147	50.015245
3503.482916	497359.010423	50.020250
3503.778895	497356.837235	50.025255
3503.801982	497359.162361	50.030260
3503.658476	497364.146424	50.035265
3503.698851	497357.052182	50.040269
3503.778595	497360.583403	50.045274
3503.828725	497358.651579	50.050279
3503.743104	497361.398903	50.055284
3503.907371	497343.855894	50.060289
3503.518923	497335.361232	50.065293
3503.468749	497314.156305	50.070298
3503.638069	497315.547035	50.075303
3503.379651	497309.461915	50.080308
3503.428928	497305.657013	50.085313
3503.382789	497310.625702	50.090317
3503.669482	497307.643941	50.095322
3503.569720	497311.557933	50.100327
3503.478475	497319.976398	50.105332
3503.950573	497308.308082	50.110337
3503.633321	497317.926695	50.115341
3503.624176	497307.043219	50.120346
3504.200873	497302.446178	50.125351
3503.866877	497302.296386	50.130356
3503.746249	497287.177830	50.135361
3503.606885	497278.289382	50.140365
3503.583364	497262.598558	50.145370
3503.400148	497255.894006	50.150375
3503.528284	497266.505427	50.155380
3503.489060	497255.930438	50.160385
3503.375802	497264.149899	50.165389
3503.766497	497258.063424	50.170394
3503.975173	497259.650447	50.175399
3503.656371	497254.840536	50.180404
3503.667171	497252.358017	50.185409
3503.477858	497264.386551	50.190413
3503.922669	497255.760154	50.195418
3503.654554	497245.373218	50.200423
3503.678520	497254.279779	50.205428
3504.049173	497245.006942	50.210433
3503.824669	497235.018127	50.215437
3503.658372	497208.059902	50.220442
3503.765402	497208.549190	50.225447
3503.575574	497196.985420	50.230452
3503.767401	497198.777622	50.235457
3503.484690	497205.758203	50.240461
3503.504866	497199.831524	50.245466
3503.393376	497196.507657	50.250471
3503.495677	497200.997267	50.255476
3503.700832	497193.674407	50.260481
3503.606443	497196.726906	50.265485
3503.446748	497199.334079	50.270490
3503.758916	497197.006431	50.275495
3503.939148	497187.561151	50.280500
3504.091668	497182.119825	50.285505
3503.634402	497167.105002	50.290509
3503.948708	497160.271153	50.295514
3504.045783	497155.901762	50.300519
3503.629065	497158.903957	50.305524
3503.714322	497154.080785	50.310529
3503.891824	497155.419606	50.315533
3503.963590	497145.080149	50.320538
3503.748149	497114.079337	50.325543
3503.536285	497116.593512	50.330548
3503.966070	497112.374036	50.335553
3503.782089	497122.022317	50.340557
3503.812068	497116.752222	50.345562
3503.498498	497109.713824	50.350567
3503.579167	497107.726520	50.355572
3503.829798	497106.522397	50.360577
3503.907169	497113.648614	50.365581
3503.413528	497087.906385	50.370586
3503.560563	497078.111900	50.375591
3503.423096	497067.299190	50.380596
3503.697310	497058.851547	50.385601
3503.365156	497064.776811	50.390605
3503.807854	497066.630631	50.395610
3503.906148	497057.248862	50.400615
3503.550667	497062.114627	50.405620
3503.949177	497056.533128	50.410625
3503.783397	497059.495678	50.415629
3504.026206	497058.748440	50.420634
3504.085772	497055.498767	50.425639
3503.843437	497029.159829	50.430644
3504.000767	497011.364456	50.435649
3503.637313	497017.547822	50.440653
3503.866294	497004.196383	50.445658
3503.984265	497006.152161	50.450663
3503.706743	497005.588416	50.455668
3503.810116	496988.510341	50.460673
3504.073809	496983.658921	50.465677
3503.732667	496978.194301	50.470682
3503.968788	496974.916710	50.475687
3503.653464	496973.700772	50.480692
3503.790071	496969.578230	50.485697
3503.538266	496970.883661	50.490701
3503.501768	496963.143248	50.495706
3503.867692	496962.933457	50.500711
3503.381986	496948.277345	50.505716
3503.523772	496932.509480	50.510721
3503.372875	496925.900954	50.515725
3503.354968	496930.510887	50.520730
3503.594506	496923.638138	50.525735
3503.685075	496905.701328	50.530740
3503.753191	496869.238047	50.535745
3503.451597	496825.694500	50.540749
3503.215324	496766.749396	50.545754
3503.596987	496703.757381	50.550759
3503.043874	496634.229851	50.555764
3503.229570	496546.865023	50.560769
3503.267462	496459.016841	50.565773
3502.840259	496356.356566	50.570778
3502.666500	496243.529621	50.575783
3502.359863	496124.697947	50.580788
3502.310545	495994.888562	50.585793
3501.867397	495865.748073	50.590797
3501.176307	495720.089318	50.595802
3501.457543	495569.313781	50.600807
3501.170715	495418.576151	50.605812
3500.793366	495252.104749	50.610817
3500.625199	495090.611475	50.615821
3500.651591	494916.680734	50.620826
3500.129261	494726.783975	50.625831
3499.628690	494547.920218	50.630836
3499.072200	494340.150732	50.635841
3499.029850	494151.995039	50.640845
3498.463505	493943.969452	50.645850
3498.574669	493724.846172	50.650855
3497.850948	493513.447906	50.655860
3497.818003	493286.037599	50.660865
3497.343174	493054.896410	50.665869
3496.585795	492815.694647	50.670874
3496.186841	492572.787038	50.675879
3495.495378	492339.442976	50.680884
3495.343667	492082.766166	50.685889
3494.954102	491840.201968	50.690893
3494.364693	491585.815735	50.695898
3494.009735	491331.338323	50.700903
3493.281520	491060.963445	50.705908
3492.892667	490813.220026	50.710913
3492.126508	490569.331388	50.715917
3491.984091	490296.371209	50.720922
3491.488579	490030.148295	50.725927
3490.825019	489753.312093	50.730932
3490.653266	489467.834440	50.735937
3490.022527	489183.691237	50.740941
3489.107345	488897.866593	50.745946
3488.943655	488601.130162	50.750951
3488.278576	488304.468315	50.755956
3487.774251	488006.054214	50.760961
3487.348473	487711.118082	50.765965
3486.812809	487399.428172	50.770970
3486.277928	487094.470150	50.775975
3485.502366	486787.367074	50.780980
3485.377898	486463.186123	50.785985
3484.565686	486148.328055	50.790989
3483.776156	485824.747958	50.795994
3483.405697	485504.895596	50.800999
3482.841655	485192.566194	50.806004
3482.080943	484876.615206	50.811009
3481.393077	484547.779408	50.816013
3480.768890	484222.474316	50.821018
3480.152959	483897.010439	50.826023
3479.469269	483573.578363	50.831028
3478.791225	483235.903050	50.836033
3478.200114	482922.223852	50.841037
3477.672375	482602.094868	50.846042
3477.320567	482256.244232	50.851047
3476.718630	481928.921066	50.856052
3476.045749	481590.101633	50.861057
3475.374053	481254.873736	50.866061
3475.015590	480903.933148	50.871066
3474.249823	480561.563592	50.876071
3473.555604	480222.825219	50.881076
3473.106400	479866.661105	50.886081
3472.099187	479530.646015	50.891085
3471.532227	479183.609650	50.896090
3471.013836	478836.407487	50.901095
3470.073371	478487.897659	50.906100
3469.279751	478142.855307	50.911105
3468.813843	477803.177846	50.916109
3467.889772	477453.278938	50.921114
3467.824683	477108.508941	50.926119
3466.672450	476766.996436	50.931124
3466.325176	476420.688045	50.936129
3465.943759	476065.357375	50.941133
3464.846646	475720.422516	50.946138
3464.349579	475366.922424	50.951143
3463.676666	475017.853639	50.956148
3462.802430	474656.442960	50.961153
3462.523534	474317.944118	50.966157
3461.662651	473969.545897	50.971162
3461.149754	473612.215968	50.976167
3460.132531	473269.406333	50.981172
3459.644415	472900.806660	50.986177
3459.030644	472527.049555	50.991181
3458.441605	472170.568174	50.996186
3457.812139	471804.150895	51.001191
3456.971906	471444.147990	51.006196
3456.479738	471094.375068	51.011201
3455.546483	470737.061391	51.016205
3454.812452	470379.760732	51.021210
3454.095083	470030.765852	51.026215
3453.477242	469683.168947	51.031220
3452.697741	469313.790598	51.036225
3452.205726	468969.203882	51.041229
3451.164989	468620.084314	51.046234
3450.856061	468270.843223	51.051239
3449.979144	467925.387465	51.056244
3449.273540	467571.279136	51.061249
3448.595881	467240.332824	51.066253
3447.819554	466889.621448	51.071258
3447.349357	466529.424307	51.076263
3446.374845	466184.766687	51.081268
3445.683351	465842.543440	51.086273
3445.004947	465486.823825	51.091277
3444.101662	465145.332738	51.096282
3443.653605	464795.599681	51.101287
3442.787286	464461.394201	51.106292
3442.180030	464112.435785	51.111297
3441.517164	463772.761082	51.116301
3440.438587	463419.453774	51.121306
3440.232684	463076.805076	51.126311
3439.172320	462757.615431	51.131316
3438.800379	462415.033159	51.136321
3438.058155	462073.518338	51.141325
3437.215432	461736.223648	51.146330
3436.813087	461396.064524	51.151335
3435.834530	461060.860289	51.156340
3435.274296	460722.034290	51.161345
3434.379919	460384.270276	51.166349
3433.755872	460044.074339	51.171354
3433.256020	459704.259261	51.176359
3432.270435	459373.747473	51.181364
3431.609732	459037.548893	51.186369
3431.332814	458697.835158	51.191373
3430.144503	458361.963287	51.196378
3429.756793	458023.727743	51.201383
3428.891283	457698.295262	51.206388
3428.504204	457359.745100	51.211393
3427.445451	457033.876853	51.216397
3426.594646	456702.644286	51.221402
3426.593005	456365.337030	51.226407
3425.807868	456036.164144	51.231412
3424.700207	455704.094916	51.236417
3423.934882	455377.192160	51.241421
3423.467218	455046.584741	51.246426
3422.381416	454724.136990	51.251431
3422.025169	454405.983263	51.256436
3421.365456	454066.817540	51.261441
3420.779773	453733.165344	51.266445
3420.035782	453404.353332	51.271450
3419.395825	453067.858615	51.276455
3418.588217	452746.251977	51.281460
3417.973299	452413.904233	51.286465
3417.428931	452088.542690	51.291469
3416.439087	451761.876928	51.296474
3415.754341	451430.337782	51.301479
3414.940189	451119.009902	51.306484
3414.294974	450789.586447	51.311489
3413.638386	450464.118121	51.316493
3412.782237	450153.189774	51.321498
3412.416685	449828.326159	51.326503
3411.312732	449513.317999	51.331508
3410.845232	449194.906392	51.336513
3410.381742	448879.280908	51.341517
3409.353121	448558.970150	51.346522
3408.869657	448231.869939	51.351527
3408.361224	447925.525723	51.356532
3407.554764	447596.945209	51.361537
3406.771003	447272.568843	51.366541
3405.885714	446961.602520	51.371546
3405.509047	446639.081627	51.376551
3404.683944	446331.193370	51.381556
3403.923803	446005.222482	51.386561
3403.373735	445697.485511	51.391565
3402.481581	445384.317077	51.396570
3401.926782	445069.213216	51.401575
3401.071319	444765.623683	51.406580
3400.720071	444439.414406	51.411585
3399.959384	444126.970024	51.416589
3398.982499	443815.723192	51.421594
3398.794828	443500.388333	51.426599
3397.963351	443190.227106	51.431604
3397.040401	442879.517981	51.436609
3396.735809	442564.240114	51.441613
3395.829161	442252.251313	51.446618
3394.938053	441940.763661	51.451623
3394.338492	441625.875552	51.456628
3393.707157	441303.475357	51.461633
3392.925213	441005.613907	51.466637
3391.992064	440707.265078	51.471642
3391.498952	440394.933256	51.476647
3390.740753	440094.011009	51.481652
3389.900659	439781.827769	51.486657
3389.044269	439488.655581	51.491661
3388.376274	439185.804174	51.496666
3388.088044	438879.944420	51.501671
3387.144996	438592.867541	51.506676
3386.722565	438281.005436	51.511681
3386.183552	437981.977424	51.516685
3385.177520	437689.797610	51.521690
3384.921386	437387.189130	51.526695
3383.978742	437079.938301	51.531700
3383.125149	436771.222585	51.536705
3382.471173	436470.595291	51.541709
3381.877312	436179.449680	51.546714
3381.254343	435878.023392	51.551719
3380.330978	435593.473055	51.556724
3379.837786	435290.851396	51.561729
3379.045713	434986.369246	51.566733
3378.405366	434694.858423	51.571738
3378.058569	434389.892493	51.576743
3376.939048	434092.077896	51.581748
3376.103808	433796.119083	51.586753
3375.424637	433510.973609	51.591757
3374.937622	433212.947189	51.596762
3374.623299	432912.554084	51.601767
3373.686167	432617.968842	51.606772
3372.779518	432322.740631	51.611777
3372.439372	432026.073730	51.616781
3371.507247	431735.946475	51.621786
3370.604929	431441.773950	51.626791
3370.023590	431162.757214	51.631796
3369.386181	430867.520607	51.636801
3368.804226	430585.653824	51.641805
3368.069754	430292.051171	51.646810
3367.667466	429995.980335	51.651815
3366.678932	429719.297921	51.656820
3365.704324	429420.263846	51.661825
3365.365543	429139.282601	51.666829
3364.519153	428842.659512	51.671834
3364.342092	428556.313663	51.676839
3363.468785	428272.665078	51.681844
3362.919130	427973.217261	51.686849
3362.352192	427686.364951	51.691853
3361.323763	427401.284028	51.696858
3361.254387	427097.229954	51.701863
3359.795072	426811.829912	51.706868
3359.410711	426529.126663	51.711873
3358.911076	426239.606905	51.716877
3357.946416	425954.068708	51.721882
3357.252075	425667.443440	51.726887
3356.525769	425381.201140	51.731892
3356.004790	425085.475306	51.736897
3355.332193	424803.231261	51.741901
3354.292094	424520.128038	51.746906
3353.899677	424231.331727	51.751911
3353.275937	423952.855522	51.756916
3352.199130	423666.599738	51.761921
3351.626173	423381.378859	51.766925
3351.059966	423108.066439	51.771930
3350.438672	422824.015786	51.776935
3349.431576	422545.357261	51.781940
3348.907192	422264.968548	51.786945
3348.301549	421984.412024	51.791949
3347.426773	421712.048950	51.796954
3346.919355	421429.998004	51.801959
3346.137947	421162.237798	51.806964
3345.448514	420875.256685	51.811969
3345.000225	420604.161592	51.816973
3344.020661	420329.388323	51.821978
3343.393469	420046.122974	51.826983
3342.380937	419777.700141	51.831988
3341.888638	419505.026370	51.836993
3341.545407	419222.088838	51.841997
3340.546907	418963.410882	51.847002
3340.191686	418679.682287	51.852007
3339.289983	418415.979452	51.857012
3338.516354	418140.313885	51.862017
3337.983246	417860.593685	51.867021
3337.348818	417593.411320	51.872026
3336.612146	417324.362642	51.877031
3335.647246	417057.202100	51.882036
3335.111875	416782.832189	51.887041
3334.520361	416513.244810	51.892045
3334.037642	416250.776777	51.897050
3333.238954	415978.371665	51.902055
3332.474109	415705.272649	51.907060
3331.671017	415437.029777	51.912065
3331.424712	415171.033810	51.917069
3330.626378	414906.342237	51.922074
3329.879424	414626.395679	51.927079
3328.737552	414362.591918	51.932084
3328.443900	414095.018311	51.937089
3327.917779	413828.190440	51.942093
3326.957821	413566.307139	51.947098
3326.524689	413285.662887	51.952103
3325.966144	413026.887366	51.957108
3324.943186	412759.975890	51.962113
3324.357035	412500.056698	51.967117
3323.763627	412235.333973	51.972122
3323.145008	411970.257130	51.977127
3322.303381	411704.882853	51.982132
3321.728627	411432.145873	51.987137
3321.026944	411176.629307	51.992141
3320.034064	410910.992354	51.997146
3319.829804	410638.875618	52.002151
3319.043258	410383.009933	52.007156
3318.029093	410126.263253	52.012161
3317.431771	409859.944558	52.017165
3316.616787	409595.360515	52.022170
3316.491012	409345.302444	52.027175
3315.669220	409078.402462	52.032180
3314.991298	408810.969128	52.037185
3314.385009	408549.417836	52.042189
3313.473342	408295.460196	52.047194
3312.764030	408028.202832	52.052199
3312.336191	407763.033331	52.057204
3311.478238	407517.472512	52.062209
3310.982683	407248.090625	52.067213
3310.352839	406988.766107	52.072218
3309.440234	406719.216812	52.077223
3308.423045	406471.614276	52.082228
3307.835769	406214.182585	52.087233
3307.678941	405954.952480	52.092237
3306.657258	405709.758961	52.097242
3306.105099	405440.853152	52.102247
3305.482006	405185.883872	52.107252
3304.665694	404925.351634	52.112257
3304.262037	404665.946510	52.117261
3303.479634	404409.039072	52.122266
3302.793340	404152.520991	52.127271
3301.963783	403898.183871	52.132276
3301.359753	403637.124458	52.137281
3300.844952	403386.240930	52.142285
3300.040227	403132.224133	52.147290
3299.258346	402866.357249	52.152295
3299.028114	402613.465476	52.157300
3298.223992	402359.188227	52.162305
3297.632884	402100.706736	52.167309
3296.810503	401851.359397	52.172314
3296.389500	401586.060223	52.177319
3295.606254	401324.832265	52.182324
3294.861930	401067.840949	52.187329
3294.405861	400803.862642	52.192333
3293.472804	400553.505988	52.197338
3292.814611	400288.640351	52.202343
3292.185399	400035.486358	52.207348
3291.352542	399777.431178	52.212353
3290.865569	399516.065505	52.217357
3290.215794	399264.383123	52.222362
3289.682827	399007.621694	52.227367
3288.566807	398745.103747	52.232372
3287.816238	398488.804819	52.237377
3287.318866	398221.736232	52.242381
3286.348493	397984.406707	52.247386
3285.935550	397724.031907	52.252391
3285.368770	397469.246695	52.257396
3284.656195	397224.930890	52.262401
3284.079315	396965.237028	52.267405
3283.209540	396718.349336	52.272410
3282.765481	396463.435329	52.277415
3281.959715	396213.737339	52.282420
3281.465663	395975.809710	52.287425
3280.808163	395701.170286	52.292429
3279.873962	395460.308728	52.297434
3279.246125	395202.668537	52.302439
3278.394916	394951.722638	52.307444
3277.590960	394697.436919	52.312449
3277.152710	394451.455876	52.317453
3276.051151	394212.086490	52.322458
3275.727188	393959.143081	52.327463
3274.860542	393713.936347	52.332468
3274.402495	393475.222753	52.337473
3273.955700	393218.199955	52.342477
3273.331882	392977.907368	52.347482
3272.342916	392725.339712	52.352487
3271.547641	392475.663476	52.357492
3270.699558	392229.553348	52.362497
3270.562116	391987.854833	52.367501
3269.474152	391743.152176	52.372506
3269.082608	391495.337394	52.377511
3268.465205	391245.369927	52.382516
3267.522229	391007.224543	52.387521
3266.697240	390765.346615	52.392525
3265.708115	390532.697426	52.397530
3265.456141	390285.106278	52.402535
3265.006202	390053.131449	52.407540
3264.048911	389815.870210	52.412545
3263.396246	389566.303227	52.417549
3262.763827	389327.766827	52.422554
3262.557788	389085.779510	52.427559
3261.665541	388846.670716	52.432564
3260.998747	388605.897271	52.437569
3260.506494	388350.244532	52.442573
3259.752826	388110.956337	52.447578
3259.119838	387872.054318	52.452583
3258.551848	387628.817554	52.457588
3258.027650	387385.572225	52.462593
3256.839405	387133.784408	52.467597
3255.966687	386892.955796	52.472602
3255.477664	386643.190040	52.477607
3254.957945	386415.296857	52.482612
3254.016708	386173.431712	52.487617
3253.565288	385929.885411	52.492621
3252.631933	385693.152685	52.497626
3252.235922	385452.849504	52.502631
3251.653477	385223.992487	52.507636
3250.845183	384982.276483	52.512641
3250.234375	384745.232347	52.517645
3249.160755	384512.583144	52.522650
3249.001092	384267.987925	52.527655
3248.217549	384033.026478	52.532660
3247.116185	383795.062055	52.537665
3246.747118	383556.929429	52.542669
3246.035247	383315.111052	52.547674
3245.157375	383075.275626	52.552679
3244.605861	382852.680818	52.557684
3244.463351	382614.964167	52.562689
3243.768125	382370.059798	52.567693
3242.635070	382136.591420	52.572698
3242.065301	381896.191129	52.577703
3241.534717	381655.808555	52.582708
3240.508371	381417.359486	52.587713
3240.237490	381185.274884	52.592717
3239.230808	380958.112145	52.597722
3238.660120	380708.395951	52.602727
3238.097823	380475.030610	52.607732
3237.783491	380250.043205	52.612737
3237.064039	380012.223586	52.617741
3236.253278	379774.416950	52.622746
3235.548746	379514.006473	52.627751
3234.832619	379290.755714	52.632756
3233.899383	379054.719022	52.637761
3233.363082	378814.853789	52.642765
3232.437120	378589.292224	52.647770
3232.284840	378353.789088	52.652775
3231.109150	378121.295154	52.657780
3230.617675	377883.019558	52.662785
3230.142808	377657.483048	52.667789
3229.320624	377429.482070	52.672794
3228.852910	377183.644146	52.677799
3228.395051	376950.037804	52.682804
3227.409968	376724.424090	52.687809
3227.158762	376484.703130	52.692813
3226.325562	376242.478290	52.697818
3225.569783	376008.023304	52.702823
3224.884380	375775.590751	52.707828
3224.102174	375546.453515	52.712833
3223.487881	375301.670157	52.717837
3222.340741	375070.273191	52.722842
3221.970214	374842.720269	52.727847
3221.518930	374617.519087	52.732852
3220.634607	374381.447040	52.737857
3220.144123	374137.959857	52.742861
3219.684317	373911.789510	52.747866
3218.806638	373670.726519	52.752871
3218.093062	373436.835135	52.757876
3216.862468	373205.644346	52.762881
3216.740211	372967.027017	52.767885
3215.881789	372747.349257	52.772890
3215.289687	372517.020299	52.777895
3214.821209	372290.130190	52.782900
3214.054226	372062.039560	52.787905
3213.276082	371821.815025	52.792909
3212.853943	371597.991965	52.797914
3212.263675	371357.964016	52.802919
3211.325800	371131.777886	52.807924
3210.464871	370905.858211	52.812929
3210.096989	370661.110243	52.817933
3209.245110	370442.335243	52.822938
3208.452322	370215.510726	52.827943
3207.841277	369978.581952	52.832948
3207.172029	369751.531911	52.837953
3206.421653	369522.992518	52.842957
3205.874698	369305.181093	52.847962
3205.297261	369070.404446	52.852967
3204.672474	368849.906324	52.857972
3203.928690	368624.668443	52.862977
3203.399282	368387.870667	52.867981
3202.383313	368163.920072	52.872986
3201.861736	367941.162190	52.877991
3201.179921	367704.791882	52.882996
3200.332813	367488.367243	52.888001
3199.942071	367265.687003	52.893005
3198.948006	367043.330055	52.898010
3198.493392	366810.709849	52.903015
3197.840732	366592.087487	52.908020
3197.029444	366363.108698	52.913025
3196.734758	366130.052554	52.918029
3196.184742	365913.802212	52.923034
3194.924705	365678.326726	52.928039
3194.853674	365454.365599	52.933044
3194.213954	365230.696861	52.938049
3193.414887	365001.556525	52.943053
3192.221375	364780.263035	52.948058
3191.776201	364544.754498	52.953063
3191.198999	364329.951131	52.958068
3190.467653	364106.851098	52.963073
3189.790702	363875.853833	52.968077
3189.289327	363653.529406	52.973082
3188.560057	363424.777199	52.978087
3187.924884	363204.380060	52.983092
3187.269507	362981.135318	52.988097
3186.679844	362756.835887	52.993101
3185.959881	362531.690874	52.998106
3185.290405	362303.305328	53.003111
3184.582355	362078.436129	53.008116
3183.958790	361856.275074	53.013121
3183.390047	361609.778962	53.018125
3182.707439	361398.159272	53.023130
3181.834355	361174.584099	53.028135
3181.437580	360940.957972	53.033140
3180.522887	360726.140436	53.038145
3179.929426	360503.866467	53.043149
3179.133950	360284.600557	53.048154
3178.685893	360054.184334	53.053159
3178.111791	359830.377422	53.058164
3177.047418	359603.084587	53.063169
3176.514640	359378.556545	53.068173
3175.949247	359163.040580	53.073178
3175.002111	358941.884067	53.078183
3174.634553	358717.072354	53.083188
3173.774901	358502.287058	53.088193
3173.165347	358270.361080	53.093197
3172.684827	358058.236647	53.098202
3171.696345	357834.104374	53.103207
3171.639789	357608.474955	53.108212
3170.358747	357390.087075	53.113217
3170.190167	357155.515913	53.118221
3169.200086	356929.420343	53.123226
3168.389079	356710.446159	53.128231
3167.882743	356489.488796	53.133236
3167.206052	356274.105008	53.138241
3166.747717	356046.089076	53.143245
3166.025842	355827.834915	53.148250
3165.033305	355601.097530	53.153255
3164.532099	355374.917601	53.158260
3163.541618	355166.551516	53.163265
3163.032067	354941.032627	53.168269
3162.722312	354729.096076	53.173274
3161.806037	354501.756402	53.178279
3161.407148	354282.197518	53.183284
3160.440899	354064.305281	53.188289
3159.752612	353835.628699	53.193293
3159.172624	353617.113587	53.198298
3158.635878	353401.899102	53.203303
3158.031367	353172.570108	53.208308
3156.937875	352966.959924	53.213313
3156.660729	352746.051900	53.218317
3156.087533	352523.586458	53.223322
3155.181843	352301.758018	53.228327
3154.693926	352086.454045	53.233332
3153.697892	351855.068899	53.238337
3153.240589	351632.530464	53.243341
3152.704035	351422.754137	53.248346
3151.977375	351196.744379	53.253351
3151.317794	350979.579762	53.258356
3150.426386	350766.472107	53.263361
3149.712511	350533.738619	53.268365
3149.075203	350325.144660	53.273370
3148.310498	350103.157518	53.278375
3147.852147	349889.188913	53.283380
3146.650231	349676.304241	53.288385
3146.208112	349454.797885	53.293389
3145.580229	349255.309797	53.298394
3145.208376	349035.292244	53.303399
3144.605705	348819.077125	53.308404
3143.572238	348606.670674	53.313409
3143.141819	348385.132708	53.318413
3142.252520	348171.454654	53.323418
3141.674253	347958.057444	53.328423
3141.142551	347739.129005	53.333428
3140.335222	347530.678603	53.338433
3139.843886	347313.091065	53.343437
3138.941949	347093.353315	53.348442
3138.451666	346883.017803	53.353447
3137.959071	346659.777557	53.358452
3137.174264	346448.799820	53.363457
3136.510706	346225.177679	53.368461
3136.049266	346009.031202	53.373466
3135.222100	345787.774876	53.378471
3134.805300	345586.687741	53.383476
3133.663758	345370.900995	53.388481
3133.343182	345146.482261	53.393485
3132.708687	344934.406160	53.398490
3132.072430	344716.169900	53.403495
3131.295114	344497.064279	53.408500
3130.209376	344286.406242	53.413505
3129.638074	344068.869987	53.418509
3129.052703	343865.080066	53.423514
3128.493930	343649.398391	53.428519
3128.064815	343439.244329	53.433524
3127.184496	343222.873821	53.438529
3126.814188	342995.578473	53.443533
3126.253471	342781.599377	53.448538
3124.997923	342568.900342	53.453543
3124.596205	342343.134739	53.458548
3124.150077	342127.226125	53.463553
3123.441871	341912.681836	53.468557
3122.536215	341693.102594	53.473562
3122.318438	341474.559180	53.478567
3121.514807	341255.038586	53.483572
3120.579607	341038.592592	53.488577
3120.250896	340813.318876	53.493581
3119.272832	340603.140023	53.498586
3118.618892	340384.050836	53.503591
3118.105845	340161.654880	53.508596
3117.586847	339949.542965	53.513601
3116.559556	339720.583007	53.518605
3115.735147	339512.412593	53.523610
3115.270828	339291.940454	53.528615
3114.715300	339077.769493	53.533620
3113.747064	338865.394092	53.538625
3113.234753	338650.756655	53.543629
3112.626340	338435.319119	53.548634
3111.489302	338231.979669	53.553639
3111.102881	338018.465712	53.558644
3110.609445	337801.124122	53.563649
3109.953528	337588.898734	53.568653
3109.179082	337382.724527	53.573658
3108.551049	337161.710949	53.578663
3108.042460	336948.416461	53.583668
3107.134394	336734.573533	53.588673
3106.613893	336510.307781	53.593677
3105.879193	336301.374587	53.598682
3104.953412	336091.681813	53.603687
3104.308624	335871.481183	53.608692
3103.709078	335666.037647	53.613697
3103.125649	335460.158164	53.618701
3102.464812	335249.147984	53.623706
3102.065508	335038.172134	53.628711
3101.394692	334816.419290	53.633716
3100.576981	334609.632375	53.638721
3099.969165	334394.665277	53.643725
3099.496100	334180.618107	53.648730
3098.715148	333966.746276	53.653735
3098.109664	333745.106916	53.658740
3097.357996	333531.050901	53.663745
3096.818847	333318.080739	53.668749
3095.972251	333108.417175	53.673754
3095.261420	332893.716299	53.678759
3095.056517	332675.345140	53.683764
3094.107985	332469.972739	53.688769
3093.623455	332238.635421	53.693773
3092.749982	332025.561506	53.698778
3091.977767	331816.824296	53.703783
3091.518730	331598.617335	53.708788
3090.599008	331383.079367	53.713793
3090.430223	331161.744687	53.718797
3089.554035	330953.454222	53.723802
3088.715615	330740.320043	53.728807
3088.372026	330513.792029	53.733812
3087.221849	330304.855684	53.738817
3086.930450	330094.535371	53.743821
3086.130406	329877.548326	53.748826
3085.294006	329665.810956	53.753831
3085.022601	329441.610463	53.758836
3084.034914	329230.074010	53.763841
3083.395973	329017.616162	53.768845
3082.534485	328801.017603	53.773850
3082.114159	328589.211358	53.778855
3081.578307	328366.322481	53.783860
3080.418956	328166.343350	53.788865
3080.139439	327948.148162	53.793869
3079.458831	327738.290215	53.798874
3078.558865	327527.040663	53.803879
3077.913450	327311.192949	53.808884
3077.563091	327105.711037	53.813889
3077.045597	326881.541973	53.818893
3076.220850	326672.442298	53.823898
3075.502486	326457.367575	53.828903
3075.130123	326239.182297	53.833908
3074.259534	326030.164559	53.838913
3073.939142	325810.213126	53.843917
3072.995798	325593.465830	53.848922
3072.317408	325380.316864	53.853927
3071.540971	325165.578840	53.858932
3070.602541	324949.618315	53.863937
3070.176241	324729.909845	53.868941
3069.471572	324510.550364	53.873946
3068.811032	324308.242025	53.878951
3068.339723	324096.177212	53.883956
3067.373886	323880.778352	53.888961
3066.814862	323659.051164	53.893965
3066.713466	323444.838356	53.898970
3065.587273	323235.853928	53.903975
3065.072061	323017.784510	53.908980
3064.346570	322802.268468	53.913985
3063.658769	322568.133717	53.918989
3063.045172	322368.563098	53.923994
3062.503443	322155.995325	53.928999
3061.817790	321929.980684	53.934004
3061.092474	321719.910655	53.939009
3060.330190	321500.883486	53.944013
3059.808145	321283.116296	53.949018
3059.009223	321067.887631	53.954023
3058.393670	320849.243006	53.959028
3057.717755	320637.533019	53.964033
3057.094377	320422.555089	53.969037
3056.330070	320207.267941	53.974042
3055.723687	319989.892861	53.979047
3055.168916	319762.451563	53.984052
3053.857809	319558.783731	53.989057
3053.473920	319346.209711	53.994061
3052.874960	319132.752592	53.999066
3052.237001	318921.618223	54.004071
3051.771848	318700.347457	54.009076
3050.938421	318495.226712	54.014081
3050.235690	318275.647595	54.019085
3049.471676	318061.883128	54.024090
3048.708209	317854.865686	54.029095
3048.041036	317643.249271	54.034100
3047.548925	317435.729646	54.039105
3046.822022	317226.948126	54.044109
3046.074979	317008.951792	54.049114
3045.401500	316799.346082	54.054119
3044.533513	316594.939682	54.059124
3043.967533	316389.619319	54.064129
3043.399494	316172.916864	54.069133
3042.811773	315972.793538	54.074138
3041.999983	315767.790877	54.079143
3041.481500	315553.600082	54.084148
3040.765875	315356.805980	54.089153
3040.181382	315146.138694	54.094157
3039.554371	314931.148925	54.099162
3038.874080	314726.250653	54.104167
3038.538489	314513.123642	54.109172
3037.501806	314313.373643	54.114177
3036.942340	314084.366468	54.119181
3036.365430	313879.271909	54.124186
3035.461556	313673.846736	54.129191
3034.889104	313462.639371	54.134196
3034.273521	313252.456962	54.139201
3033.232451	313044.276726	54.144205
3033.021064	312832.832721	54.149210
3032.271507	312631.404407	54.154215
3031.607116	312421.406340	54.159220
3031.028132	312209.408155	54.164225
3030.312270	311995.419560	54.169229
3029.496269	311784.323843	54.174234
3028.770209	311581.387490	54.179239
3028.104171	311361.303843	54.184244
3027.526645	311167.306638	54.189249
3026.690444	310954.684690	54.194253
3026.286886	310751.899512	54.199258
3025.537167	310538.804739	54.204263
3024.946943	310330.013285	54.209268
3024.136809	310130.270693	54.214273
3023.552512	309906.835444	54.219277
3023.071927	309698.432933	54.224282
3022.059031	309491.234741	54.229287
3021.892459	309289.504473	54.234292
3020.918598	309080.567785	54.239297
3020.414049	308866.870936	54.244301
3019.587403	308653.097358	54.249306
3018.830154	308445.805961	54.254311
3018.561984	308223.972736	54.259316
3017.551745	308024.793040	54.264321
3017.319617	307807.002284	54.269325
3016.487994	307597.021934	54.274330
3015.977633	307403.517225	54.279335
3015.199864	307172.493479	54.284340
3014.508345	306970.969795	54.289345
3013.793382	306757.047944	54.294349
3013.199023	306539.490582	54.299354
3012.371459	306337.911037	54.304359
3011.791513	306122.489776	54.309364
3011.010654	305911.327211	54.314369
3010.479417	305700.939693	54.319373
3010.038647	305491.581606	54.324378
3009.298812	305285.122659	54.329383
3008.622211	305066.098875	54.334388
3007.985959	304849.003735	54.339393
3007.120386	304630.034621	54.344397
3006.508299	304421.109440	54.349402
3005.780429	304214.214058	54.354407
3005.354676	303997.899161	54.359412
3004.262213	303796.739724	54.364417
3004.004643	303589.183271	54.369421
3003.374691	303378.349427	54.374426
3002.357060	303169.766696	54.379431
3001.970864	302942.722793	54.384436
3001.511066	302731.988403	54.389441
3000.621806	302523.766417	54.394445
3000.332263	302309.184573	54.399450
2999.610968	302091.130970	54.404455
2998.676345	301877.261791	54.409460
2997.853650	301658.383228	54.414465
2997.530949	301447.396130	54.419469
2997.133728	301224.476880	54.424474
2995.979104	301018.001056	54.429479
2995.372922	300797.075168	54.434484
2994.473642	300594.021786	54.439489
2993.874179	300373.017843	54.444493
2993.373381	300168.347400	54.449498
2992.566775	299954.786386	54.454503
2991.941851	299723.828211	54.459508
2991.111105	299530.465363	54.464513
2990.643886	299317.180866	54.469517
2990.051561	299108.092412	54.474522
2988.915592	298890.482040	54.479527
2988.427048	298684.305293	54.484532
2987.756399	298480.423653	54.489537
2987.079229	298263.733066	54.494541
2986.533397	298063.039981	54.499546
2985.720644	297858.237837	54.504551
2985.237029	297643.986124	54.509556
2984.590562	297436.279431	54.514561
2983.521351	297233.605442	54.519565
2982.855385	297015.740091	54.524570
2982.322745	296809.593613	54.529575
2981.782615	296619.212110	54.534580
2981.007800	296411.830179	54.539585
2980.490805	296197.123660	54.544589
2979.892202	295987.548684	54.549594
2979.055370	295789.675083	54.554599
2978.482390	295577.854510	54.559604
2977.740179	295382.257555	54.564609
2977.060307	295176.692905	54.569613
2976.661713	294966.703178	54.574618
2976.163515	294765.158626	54.579623
2975.359688	294548.840354	54.584628
2974.631990	294336.329888	54.589633
2974.130380	294123.579682	54.594637
2973.696788	293914.944191	54.599642
2972.640906	293713.665171	54.604647
2972.538307	293494.611699	54.609652
2971.530946	293279.088373	54.614657
2970.659676	293066.039097	54.619661
2970.096487	292850.801594	54.624666
2969.329176	292641.631971	54.629671
2968.575110	292436.356576	54.634676
2968.011862	292221.857047	54.639681
2967.434739	292009.473319	54.644685
2966.896791	291803.297268	54.649690
2966.000829	291594.936569	54.654695
2965.622941	291376.968829	54.659700
2965.046463	291172.453733	54.664705
2964.136895	290960.147181	54.669709
2963.771388	290748.645697	54.674714
2963.176617	290525.847238	54.679719
2962.399300	290312.373173	54.684724
2961.876110	290098.374824	54.689729
2960.977198	289892.025147	54.694733
2960.404617	289665.886188	54.699738
2959.345462	289457.778809	54.704743
2958.747275	289239.564017	54.709748
2958.322282	289037.544606	54.714753
2957.462869	288821.815750	54.719757
2956.971124	288600.552959	54.724762
2956.247183	288395.778968	54.729767
2955.667615	288188.460668	54.734772
2954.635867	287979.864009	54.739777
2953.998559	287762.978652	54.744781
2953.594209	287553.034470	54.749786
2952.582727	287342.753302	54.754791
2952.231766	287128.190704	54.759796
2951.581244	286921.264830	54.764801
2950.650407	286718.661818	54.769805
2949.934901	286508.104064	54.774810
2949.340220	286304.199667	54.779815
2948.763028	286093.339623	54.784820
2948.086654	285888.429202	54.789825
2947.269732	285676.511742	54.794829
2946.601843	285465.691165	54.799834
2945.834316	285264.665976	54.804839
2945.110366	285057.495983	54.809844
2944.530126	284855.702365	54.814849
2944.058197	284644.850331	54.819853
2943.348677	284444.197573	54.824858
2942.649304	284249.604525	54.829863
2942.162732	284027.548532	54.834868
2941.500338	283836.183899	54.839873
2940.660922	283616.195540	54.844877
2940.301768	283407.184234	54.849882
2939.473538	283210.599154	54.854887
2939.046283	282998.898825	54.859892
2938.191587	282790.118508	54.864897
2937.484455	282586.535728	54.869901
2936.616091	282370.753651	54.874906
2936.033564	282159.892543	54.879911
2935.502811	281960.713078	54.884916
2934.771482	281757.897869	54.889921
2934.139027	281550.227970	54.894925
2933.719066	281341.378291	54.899930
2932.654385	281141.391686	54.904935
2932.154518	280924.430143	54.909940
2931.764557	280716.772522	54.914945
2930.778207	280510.304386	54.919949
2930.275778	280292.196977	54.924954
2929.559007	280082.502508	54.929959
2929.009379	279867.229431	54.934964
2928.302238	279664.384303	54.939969
2927.447689	279453.616344	54.944973
2926.723476	279242.623956	54.949978
2925.895925	279036.970761	54.954983
2925.325727	278832.728478	54.959988
2924.726033	278633.482619	54.964993
2924.026819	278426.229947	54.969997
2923.534993	278222.357166	54.975002
2922.782593	278013.151777	54.980007
2922.341665	277807.156997	54.985012
2921.529226	277608.275736	54.990017
2920.881609	277401.014730	54.995021
2920.488329	277196.565892	55.000026
2919.534809	276982.094774	55.005031
2918.956577	276775.586761	55.010036
2918.206112	276565.387609	55.015041
2917.502847	276353.627395	55.020045
2916.766170	276155.319762	55.025050
2916.211078	275958.511472	55.030055
2915.924296	275741.438795	55.035060
2914.853903	275535.237822	55.040065
2914.144116	275331.501124	55.045069
2913.734657	275125.144569	55.050074
2912.956806	274923.099552	55.055079
2911.968321	274715.077340	55.060084
2911.817474	274514.486633	55.065089
2910.973229	274307.205642	55.070093
2910.514999	274089.701659	55.075098
2909.693656	273894.361730	55.080103
2909.254509	273680.089229	55.085108
2908.421342	273483.146685	55.090113
2907.613794	273270.078611	55.095117
2907.351801	273054.555626	55.100122
2906.248440	272849.913517	55.105127
2905.650359	272640.199634	55.110132
2904.952864	272443.133826	55.115137
2904.162222	272225.911838	55.120141
2903.606819	272033.458828	55.125146
2902.713962	271823.689844	55.130151
2902.217112	271606.166753	55.135156
2901.692853	271407.494622	55.140161
2900.858942	271206.095496	55.145165
2900.308489	270995.457457	55.150170
2899.780798	270789.400158	55.155175
2899.181032	270590.485445	55.160180
2898.269564	270383.139167	55.165185
2897.454818	270177.942431	55.170189
2896.977709	269967.089259	55.175194
2895.957904	269764.522854	55.180199
2895.487610	269560.366874	55.185204
2894.799622	269366.636477	55.190209
2893.925596	269178.844228	55.195213
2893.748150	268965.065968	55.200218
2893.002211	268760.877445	55.205223
2892.557855	268557.761840	55.210228
2891.827388	268359.123074	55.215233
2891.067027	268149.716031	55.220237
2890.410563	267940.394485	55.225242
2889.793907	267738.172347	55.230247
2889.316095	267530.961995	55.235252
2888.488383	267322.202618	55.240257
2887.459721	267117.422708	55.245261
2887.034829	266903.124054	55.250266
2886.619537	266707.670427	55.255271
2885.972469	266504.944205	55.260276
2885.248896	266297.187483	55.265281
2884.385100	266091.490503	55.270285
2884.163180	265878.357165	55.275290
2883.362538	265674.000184	55.280295
2882.871958	265465.391967	55.285300
2882.240869	265264.319187	55.290305
2881.347212	265041.538320	55.295309
2880.615211	264832.739422	55.300314
2879.973755	264624.715806	55.305319
2879.271180	264416.701974	55.310324
2878.347178	264210.327796	55.315329
2878.006167	264000.652456	55.320333
2877.471649	263783.698549	55.325338
2876.471458	263588.848317	55.330343
2876.003304	263374.660157	55.335348
2875.725550	263169.941532	55.340353
2874.666548	262963.436623	55.345357
2874.220174	262751.537511	55.350362
2873.122041	262532.534301	55.355367
2872.736932	262329.233914	55.360372
2872.065657	262116.071952	55.365377
2870.952075	261921.138754	55.370381
2870.584372	261712.895233	55.375386
2869.748449	261516.161043	55.380391
2869.398158	261299.179574	55.385396
2868.768791	261086.801184	55.390401
2867.661602	260886.010039	55.395405
2867.144899	260680.566808	55.400410
2866.577685	260481.116643	55.405415
2866.034350	260258.716410	55.410420
2865.466427	260059.088381	55.415425
2864.471970	259853.823266	55.420429
2864.299241	259643.716680	55.425434
2863.018080	259438.268065	55.430439
2862.789847	259227.864982	55.435444
2862.213494	259032.848691	55.440449
2861.397067	258816.121232	55.445453
2860.579763	258608.918968	55.450458
2860.161260	258405.906812	55.455463
2859.066891	258193.375108	55.460468
2858.485034	257987.205719	55.465473
2857.772214	257784.851897	55.470477
2857.435193	257581.216306	55.475482
2856.509648	257383.124107	55.480487
2855.798426	257170.812786	55.485492
2855.276193	256958.726410	55.490497
2854.745464	256760.775970	55.495501
2854.032450	256551.827201	55.500506
2853.330605	256344.226627	55.505511
2852.768665	256140.678865	55.510516
2852.283795	255935.616520	55.515521
2851.531088	255731.411730	55.520525
2850.646275	255520.173629	55.525530
2849.809450	255316.848442	55.530535
2849.311828	255113.495211	55.535540
2848.858941	254907.231840	55.540545
2847.847321	254708.671818	55.545549
2847.454513	254498.299140	55.550554
2846.690597	254296.644249	55.555559
2845.961511	254080.009421	55.560564
2845.528719	253872.292308	55.565569
2844.620031	253679.039625	55.570573
2844.405552	253468.028601	55.575578
2843.361081	253272.072861	55.580583
2843.106258	253055.440488	55.585588
2842.343228	252855.009374	55.590593
2841.534015	252642.692766	55.595597
2840.921009	252432.229880	55.600602
2840.302106	252223.780047	55.605607
2839.810021	252005.811269	55.610612
2839.095593	251803.565475	55.615617
2838.125307	251596.037881	55.620621
2837.337517	251375.238962	55.625626
2836.618540	251181.169409	55.630631
2836.210535	250972.483925	55.635636
2835.713295	250771.172670	55.640641
2834.966873	250566.437658	55.645645
2834.469193	250346.281725	55.650650
2833.493714	250147.313464	55.655655
2833.036510	249933.849357	55.660660
2832.482291	249732.624775	55.665665
2831.587506	249520.987680	55.670669
2831.185556	249303.160896	55.675674
2830.289912	249096.617769	55.680679
2829.393361	248890.202385	55.685684
2828.983914	248689.414584	55.690689
2828.239701	248482.033364	55.695693
2827.421754	248273.034260	55.700698
2826.580353	248071.246078	55.705703
2826.018358	247857.928696	55.710708
2825.476237	247662.358333	55.715713
2824.887989	247461.753250	55.720717
2824.540897	247245.856099	55.725722
2823.845965	247039.411293	55.730727
2822.943661	246835.495277	55.735732
2822.205726	246627.478972	55.740737
2821.826765	246415.178786	55.745741
2821.446354	246194.373552	55.750746
2820.738347	245996.437893	55.755751
2819.926898	245783.977938	55.760756
2819.313183	245573.524251	55.765761
2818.720453	245369.688638	55.770765
2817.892522	245141.927390	55.775770
2816.956193	244946.193957	55.780775
2815.882305	244739.787045	55.785780
2815.400479	244525.978084	55.790785
2814.900676	244329.336052	55.795789
2814.719159	244117.619288	55.800794
2813.855697	243915.407587	55.805799
2813.288170	243694.839727	55.810804
2812.829535	243482.429366	55.815809
2811.778308	243280.783148	55.820813
2811.324538	243061.013237	55.825818
2810.563348	242854.356033	55.830823
2810.064193	242647.326623	55.835828
2809.353788	242427.954951	55.840833
2808.721737	242218.935541	55.845837
2807.783188	242009.684901	55.850842
2807.158503	241797.074460	55.855847
2806.284019	241591.506805	55.860852
2806.033619	241377.793754	55.865857
2805.298817	241184.096775	55.870861
2804.825708	240969.121000	55.875866
2803.977989	240756.394901	55.880871
2803.502094	240543.763087	55.885876
2802.840389	240328.105314	55.890881
2801.950310	240111.592836	55.895885
2801.602531	239896.242645	55.900890
2801.001383	239683.912324	55.905895
2800.154948	239465.509755	55.910900
2799.711990	239251.474519	55.915905
2798.728799	239045.139091	55.920909
2798.117663	238816.489268	55.925914
2797.419015	238597.682986	55.930919
2796.696471	238392.427899	55.935924
2795.999049	238184.368145	55.940929
2794.907879	237976.753097	55.945933
2794.509058	237764.496184	55.950938
2793.679431	237567.917377	55.955943
2793.236244	237359.309634	55.960948
2792.588500	237140.854663	55.965953
2791.832986	236939.019676	55.970957
2791.329064	236734.318733	55.975962
2790.601505	236517.838383	55.980967
2789.704267	236309.177257	55.985972
2789.037452	236105.801970	55.990977
2788.563012	235898.627986	55.995981
2787.987947	235692.845382	56.000986
2787.346277	235484.119957	56.005991
2786.583543	235269.990394	56.010996
2785.993844	235059.958954	56.016001
2785.137514	234852.949388	56.021005
2784.552848	234646.635657	56.026010
2783.933106	234448.781721	56.031015
2783.284325	234233.872383	56.036020
2782.327723	234023.977579	56.041025
2781.823455	233824.909811	56.046029
2781.263716	233616.735434	56.051034
2780.548970	233418.083760	56.056039
2779.560128	233199.792997	56.061044
2779.508388	233000.553370	56.066049
2778.156418	232800.603401	56.071053
2777.488422	232595.351105	56.076058
2777.114280	232394.279529	56.081063
2776.707019	232191.151137	56.086068
2776.216716	231983.554895	56.091073
2775.392291	231779.933264	56.096077
2774.985095	231566.646606	56.101082
2773.929428	231371.006798	56.106087
2773.268091	231156.335416	56.111092
2773.163350	230934.192284	56.116097
2772.167295	230731.338517	56.121101
2771.602278	230519.912528	56.126106
2770.932686	230322.176800	56.131111
2770.226656	230095.318551	56.136116
2769.512389	229888.500844	56.141121
2768.761473	229685.610567	56.146125
2768.033156	229469.884323	56.151130
2767.521638	229262.399388	56.156135
2766.886202	229055.749338	56.161140
2766.010412	228845.725950	56.166145
2765.770471	228643.419114	56.171149
2765.054891	228424.790741	56.176154
2764.298849	228213.349497	56.181159
2763.729456	228003.585129	56.186164
2762.896170	227790.247525	56.191169
2762.074839	227583.350297	56.196173
2761.503947	227368.953717	56.201178
2760.789281	227162.829908	56.206183
2760.231491	226948.101306	56.211188
2760.016789	226743.452461	56.216193
2759.195462	226536.583222	56.221197
2758.211789	226315.787536	56.226202
2757.712941	226101.140859	56.231207
2757.088549	225889.175282	56.236212
2756.596148	225668.545374	56.241217
2755.533967	225471.710301	56.246221
2755.106483	225250.905728	56.251226
2754.422175	225036.609433	56.256231
2753.622638	224835.176824	56.261236
2753.255152	224619.762096	56.266241
2752.497245	224404.982634	56.271245
2751.776401	224188.173769	56.276250
2750.634826	223977.033397	56.281255
2750.430541	223768.596683	56.286260
2749.911318	223551.528462	56.291265
2749.215482	223350.974243	56.296269
2748.589251	223123.625512	56.301274
2747.667703	222904.496867	56.306279
2747.080864	222706.205693	56.311284
2746.554238	222480.243341	56.316289
2745.693810	222274.880563	56.321293
2745.031045	222064.535105	56.326298
2744.396672	221855.853328	56.331303
2743.695493	221648.977599	56.336308
2743.178302	221437.694249	56.341313
2742.469952	221225.334274	56.346317
2741.943840	221003.666085	56.351322
2741.075933	220806.544527	56.356327
2740.408858	220589.558930	56.361332
2739.840820	220374.798679	56.366337
2739.143692	220154.280276	56.371341
2738.308022	219942.325966	56.376346
2737.829315	219743.248863	56.381351
2737.268923	219532.028621	56.386356
2736.924910	219314.499118	56.391361
2736.037507	219103.561027	56.396365
2735.130869	218886.541974	56.401370
2734.628952	218668.542955	56.406375
2733.492968	218460.522915	56.411380
2733.397110	218237.623760	56.416385
2732.686799	218039.033502	56.421389
2732.095336	217816.417816	56.426394
2731.326227	217616.323274	56.431399
2730.657003	217398.914677	56.436404
2730.104828	217177.822247	56.441409
2729.178720	216970.244269	56.446413
2728.447122	216750.467222	56.451418
2727.951903	216543.764195	56.456423
2727.291314	216327.146724	56.461428
2726.596964	216110.726206	56.466433
2725.383772	215887.056760	56.471437
2725.055834	215682.990107	56.476442
2724.654805	215480.195777	56.481447
2723.291587	215274.359551	56.486452
2722.769702	215051.474328	56.491457
2722.127020	214853.073321	56.496461
2721.303131	214648.006374	56.501466
2721.019755	214450.682472	56.506471
2720.365854	214243.502347	56.511476
2719.535393	214037.089075	56.516481
2718.906593	213837.186895	56.521485
2718.691804	213625.293256	56.526490
2717.755887	213425.173659	56.531495
2717.200727	213215.002650	56.536500
2716.538229	212993.202966	56.541505
2715.922083	212794.918403	56.546509
2715.154477	212581.397359	56.551514
2714.526530	212370.807813	56.556519
2713.989005	212166.657760	56.561524
2713.202101	211953.460026	56.566529
2712.607668	211744.954594	56.571533
2712.182755	211528.098897	56.576538
2711.403574	211317.689457	56.581543
2710.353822	211110.849186	56.586548
2709.740849	210897.118280	56.591553
2708.989972	210692.917592	56.596557
2708.290673	210488.582112	56.601562
2707.708571	210275.904805	56.606567
2707.168678	210077.285598	56.611572
2706.644071	209866.204250	56.616577
2705.813413	209667.797852	56.621581
2705.366598	209451.461812	56.626586
2704.690060	209241.615752	56.631591
2704.206330	209028.379809	56.636596
2703.946606	208804.112635	56.641601
2702.983536	208595.001428	56.646605
2702.417085	208380.673542	56.651610
2701.524273	208172.698101	56.656615
2700.933624	207947.239196	56.661620
2700.147270	207732.095688	56.666625
2699.435062	207522.248415	56.671629
2698.823954	207312.080403	56.676634
2698.147023	207101.007200	56.681639
2697.441298	206895.195553	56.686644
2696.892021	206675.652888	56.691649
2696.340427	206475.978114	56.696653
2695.569551	206256.306641	56.701658
2694.856011	206038.459559	56.706663
2694.020569	205833.601178	56.711668
2693.724633	205603.866364	56.716673
2692.941563	205406.471761	56.721677
2692.383648	205194.393786	56.726682
2691.659506	204975.661445	56.731687
2690.693153	204763.509739	56.736692
2690.279917	204548.611348	56.741697
2689.478086	204339.425856	56.746701
2688.614731	204130.378130	56.751706
2687.858493	203916.287279	56.756711
2687.454687	203708.504555	56.761716
2686.713906	203493.649251	56.766721
2686.155436	203291.899338	56.771725
2685.404253	203077.721736	56.776730
2684.946547	202867.341743	56.781735
2684.109789	202648.241578	56.786740
2683.658729	202439.122005	56.791745
2682.802200	202235.526887	56.796749
2682.408359	202023.371009	56.801754
2681.728744	201802.060383	56.806759
2681.049249	201589.378735	56.811764
2680.277900	201379.397593	56.816769
2679.612266	201172.772820	56.821773
2679.208848	200955.023197	56.826778
2678.406496	200746.754608	56.831783
2677.428571	200526.527105	56.836788
2677.215593	200302.005328	56.841793
2675.934240	200100.661414	56.846797
2675.013293	199890.989608	56.851802
2674.652552	199678.417550	56.856807
2674.273588	199477.734690	56.861812
2673.959634	199264.087915	56.866817
2672.623662	199054.994100	56.871821
2672.071674	198849.199983	56.876826
2671.518345	198636.637085	56.881831
2670.887262	198433.720252	56.886836
2670.577200	198219.224434	56.891841
2669.783705	198012.097491	56.896845
2669.221049	197791.675384	56.901850
2668.514837	197578.721003	56.906855
2667.457611	197363.698038	56.911860
2666.793285	197146.412319	56.916865
2665.863846	196944.693689	56.921869
2665.499632	196728.634632	56.926874
2665.075077	196527.282993	56.931879
2664.265435	196318.269307	56.936884
2663.746486	196102.733617	56.941889
2662.970228	195902.267212	56.946893
2662.019902	195679.421418	56.951898
2661.488120	195471.397814	56.956903
2660.892351	195263.486983	56.961908
2660.360643	195054.103554	56.966913
2659.846168	194846.283332	56.971917
2659.021999	194638.589364	56.976922
2658.348709	194421.761867	56.981927
2657.807172	194212.828797	56.986932
2657.400493	193999.536334	56.991937
2656.497210	193784.720226	56.996941
2655.639172	193572.417202	57.001946
2654.986334	193364.879462	57.006951
2654.296337	193153.913042	57.011956
2653.856830	192940.706621	57.016961
2653.051393	192732.368641	57.021965
2652.479559	192524.109040	57.026970
2652.174612	192301.964767	57.031975
2651.043668	192093.235718	57.036980
2650.800772	191886.491685	57.041985
2649.974711	191671.710640	57.046989
2649.072355	191456.840836	57.051994
2648.532978	191239.051725	57.056999
2647.758444	191035.512720	57.062004
2647.142243	190819.697037	57.067009
2646.584264	190607.473739	57.072013
2645.911426	190398.259494	57.077018
2645.161497	190176.958762	57.082023
2644.231159	189978.767112	57.087028
2644.061724	189760.722472	57.092033
2643.316709	189546.459643	57.097037
2642.579792	189340.682605	57.102042
2641.643444	189120.192378	57.107047
2641.014700	188915.265188	57.112052
2640.593981	188698.206692	57.117057
2639.573002	188502.859963	57.122061
2639.328199	188279.566895	57.127066
2638.818477	188066.596611	57.132071
2637.597382	187855.088572	57.137076
2637.199515	187643.667342	57.142081
2636.530582	187437.429822	57.147085
2635.889898	187223.606281	57.152090
2635.366700	187015.362870	57.157095
2634.474203	186808.374781	57.162100
2633.787090	186592.615016	57.167105
2633.289400	186388.492332	57.172109
2632.380982	186168.558626	57.177114
2632.030375	185963.523985	57.182119
2630.908466	185762.161853	57.187124
2630.693708	185541.167118	57.192129
2629.741529	185338.533227	57.197133
2629.168877	185129.199400	57.202138
2628.790946	184920.319108	57.207143
2627.826404	184709.408218	57.212148
2627.508977	184494.363076	57.217153
2626.435625	184286.766264	57.222157
2625.620446	184075.898279	57.227162
2625.506390	183868.316790	57.232167
2624.510318	183659.960074	57.237172
2623.887318	183438.315188	57.242177
2623.378648	183232.045848	57.247181
2622.833180	183020.554935	57.252186
2622.061597	182808.426642	57.257191
2621.095924	182603.720985	57.262196
2620.685580	182380.508451	57.267201
2619.992678	182183.088755	57.272205
2619.028966	181970.409772	57.277210
2618.731933	181754.687709	57.282215
2618.198904	181551.419444	57.287220
2617.385498	181337.333171	57.292225
2616.856496	181124.831114	57.297229
2616.361085	180908.584959	57.302234
2615.284671	180693.220601	57.307239
2614.489019	180488.726872	57.312244
2614.337498	180268.168118	57.317249
2613.566204	180066.381947	57.322253
2612.625191	179853.340846	57.327258
2612.084774	179632.401763	57.332263
2611.096634	179428.554137	57.337268
2610.720891	179205.784924	57.342273
2610.081081	178998.424337	57.347277
2609.190588	178793.114212	57.352282
2608.582842	178579.301638	57.357287
2607.724436	178381.963714	57.362292
2607.451833	178160.086744	57.367297
2606.604270	177954.506776	57.372301
2605.771806	177754.343934	57.377306
2605.271897	177541.855083	57.382311
2604.537094	177337.048879	57.387316
2603.917678	177123.360028	57.392321
2603.474480	176924.271498	57.397325
2602.695710	176704.390325	57.402330
2601.885218	176498.010339	57.407335
2601.010233	176298.217359	57.412340
2600.589030	176087.822105	57.417345
2599.956208	175888.196242	57.422349
2599.340656	175680.008802	57.427354
2598.899145	175470.853649	57.432359
2598.147516	175262.066668	57.437364
2597.760248	175049.928880	57.442369
2596.608895	174849.703423	57.447373
2595.963742	174629.201676	57.452378
2595.539516	174435.362226	57.457383
2594.625514	174222.485508	57.462388
2594.421616	174010.336805	57.467393
2593.843328	173805.447090	57.472397
2592.698485	173583.478581	57.477402
2592.192116	173379.622531	57.482407
2591.333038	173165.903289	57.487412
2590.884401	172950.632144	57.492417
2590.087637	172749.356200	57.497421
2589.555591	172537.915882	57.502426
2589.005643	172326.581266	57.507431
2588.228891	172128.942584	57.512436
2587.924303	171908.490834	57.517441
2587.245287	171696.645881	57.522445
2586.263789	171478.046102	57.527450
2585.750210	171265.681265	57.532455
2585.011460	171051.979771	57.537460
2584.590106	170841.294029	57.542465
2583.617737	170634.664522	57.547469
2583.023487	170409.434500	57.552474
2582.276319	170198.460484	57.557479
2581.696308	169988.745548	57.562484
2581.157032	169778.274987	57.567489
2580.515373	169561.425174	57.572493
2579.734125	169351.211462	57.577498
2579.086307	169145.593947	57.582503
2578.560477	168929.225285	57.587508
2578.016576	168711.334705	57.592513
2577.402838	168499.344203	57.597517
2576.528549	168284.344199	57.602522
2576.019968	168062.598610	57.607527
2575.144782	167860.915240	57.612532
2574.456907	167636.224913	57.617537
2573.944403	167416.670909	57.622541
2573.072152	167203.024608	57.627546
2572.752056	166979.131877	57.632551
2571.653279	166776.930197	57.637556
2571.406039	166555.139293	57.642561
2570.493749	166344.377999	57.647565
2569.824576	166132.244207	57.652570
2569.690115	165916.161308	57.657575
2568.713780	165700.035042	57.662580
2567.951786	165470.206835	57.667585
2567.420303	165254.953609	57.672589
2566.923382	165040.751533	57.677594
2566.129278	164833.832813	57.682599
2565.032975	164617.299534	57.687604
2564.631191	164390.294588	57.692609
2563.854299	164183.084336	57.697613
2563.211668	163970.386507	57.702618
2562.909351	163750.401164	57.707623
2561.564736	163547.594837	57.712628
2561.256737	163324.917391	57.717633
2560.448063	163118.773523	57.722637
2560.143477	162873.338899	57.727642
2559.507457	162627.411724	57.732647
2558.730339	162414.947700	57.737652
2558.367641	162185.941356	57.742657
2557.234333	161975.329091	57.747661
2556.772553	161764.509928	57.752666
2556.225218	161539.440227	57.757671
2555.491749	161331.247637	57.762676
2554.784033	161109.804141	57.767681
2554.068707	160894.872770	57.772685
2553.223717	160682.264453	57.777690
2552.693175	160459.423810	57.782695
2552.249061	160259.570012	57.787700
2551.361622	160035.275649	57.792705
2550.577533	159823.412922	57.797709
2549.871770	159602.830299	57.802714
2549.755909	159387.533351	57.807719
2548.623517	159172.525940	57.812724
2547.928787	158950.954005	57.817729
2547.508725	158736.052506	57.822733
2546.946052	158529.273176	57.827738
2546.223301	158303.056775	57.832743
2544.981224	158094.086626	57.837748
2544.739241	157875.767832	57.842753
2544.162707	157673.051179	57.847757
2543.069409	157461.722095	57.852762
2542.765553	157239.781261	57.857767
2541.927876	157030.677149	57.862772
2541.517925	156810.548354	57.867777
2540.484473	156602.189763	57.872781
2540.013858	156389.802415	57.877786
2539.206357	156169.562746	57.882791
2538.471642	155964.694685	57.887796
2538.185774	155750.705705	57.892801
2537.316446	155545.009780	57.897805
2536.322130	155334.580636	57.902810
2535.950243	155120.266019	57.907815
2535.345027	154910.197328	57.912820
2534.797467	154698.214046	57.917825
2534.302142	154486.872104	57.922829
2533.183954	154270.685402	57.927834
2532.881561	154056.633440	57.932839
2531.950626	153848.860178	57.937844
2531.369101	153631.829844	57.942849
2530.508906	153424.314935	57.947853
2529.704768	153221.076082	57.952858
2529.567051	153013.830553	57.957863
2528.569482	152804.040559	57.962868
2528.174217	152581.852277	57.967873
2527.376752	152375.439792	57.972877
2526.200798	152159.568226	57.977882
2526.283590	151950.527575	57.982887
2525.213178	151744.365644	57.987892
2524.691924	151532.182166	57.992897
2524.204657	151321.901227	57.997901
2523.405498	151116.844168	58.002906
2522.746857	150896.755304	58.007911
2522.100845	150702.137102	58.012916
2521.772274	150478.185682	58.017921
2521.020891	150264.839399	58.022925
2520.111931	150050.934825	58.027930
2519.655391	149829.308631	58.032935
2518.608561	149612.009844	58.037940
2518.168997	149396.077882	58.042945
2517.447229	149196.943319	58.047949
2516.643340	148985.939602	58.052954
2516.326221	148767.908063	58.057959
2515.317453	148553.914797	58.062964
2514.772273	148344.145209	58.067969
2514.330782	148141.210802	58.072973
2513.585407	147921.981945	58.077978
2512.809212	147705.491907	58.082983
2511.890876	147503.386942	58.087988
2511.169219	147295.355183	58.092993
2510.938348	147089.877710	58.097997
2510.235237	146879.507314	58.103002
2509.303423	146669.593940	58.108007
2508.847225	146460.089500	58.113012
2508.268084	146235.254158	58.118017
2507.748145	146026.868318	58.123021
2506.707943	145815.401955	58.128026
2506.309768	145609.071020	58.133031
2505.520492	145409.970781	58.138036
2504.797100	145188.304664	58.143041
2504.479537	144976.665871	58.148045
2503.639974	144771.503274	58.153050
2503.014700	144553.180967	58.158055
2502.210316	144348.117238	58.163060
2501.541895	144125.471454	58.168065
2500.723953	143920.870160	58.173069
2500.122278	143708.268402	58.178074
2499.676770	143492.682548	58.183079
2498.668786	143294.062528	58.188084
2497.834898	143080.370943	58.193089
2497.489703	142876.095547	58.198093
2496.741104	142672.609739	58.203098
2496.208927	142462.762949	58.208103
2495.755865	142255.509945	58.213108
2495.255563	142041.963302	58.218113
2494.625352	141833.711984	58.223117
2493.820284	141624.130199	58.228122
2493.126514	141405.434401	58.233127
2492.210494	141196.305162	58.238132
2491.865962	140979.755268	58.243137
2491.514479	140763.690852	58.248141
2490.634930	140551.447261	58.253146
2490.030879	140331.232952	58.258151
2489.127068	140115.578353	58.263156
2488.534471	139895.606818	58.268161
2487.746160	139680.801017	58.273165
2487.035947	139474.522555	58.278170
2486.543166	139254.044370	58.283175
2485.873063	139053.568874	58.288180
2485.228344	138835.989279	58.293185
2484.619539	138614.238248	58.298189
2483.985923	138402.453652	58.303194
2483.249505	138195.730775	58.308199
2482.254061	137978.340078	58.313204
2481.872110	137762.657830	58.318209
2481.284241	137557.567487	58.323213
2480.336640	137344.950861	58.328218
2479.753852	137126.522745	58.333223
2479.255292	136926.161453	58.338228
2478.454382	136705.433392	58.343233
2478.082072	136492.121917	58.348237
2476.898815	136286.855284	58.353242
2476.380110	136066.176225	58.358247
2476.110803	135860.068988	58.363252
2475.496692	135638.277614	58.368257
2474.692192	135426.173059	58.373261
2473.696896	135218.724472	58.378266
2473.544346	135002.746634	58.383271
2472.388780	134790.130693	58.388276
2472.045051	134571.226423	58.393281
2471.635383	134348.002391	58.398285
2470.417208	134148.028291	58.403290
2470.040991	133935.663493	58.408295
2469.414802	133713.393317	58.413300
2468.645866	133506.492765	58.418305
2468.145852	133296.489663	58.423309
2466.984749	133077.281685	58.428314
2466.754665	132863.275675	58.433319
2465.890701	132654.097134	58.438324
2465.130005	132436.634376	58.443329
2464.532795	132221.357594	58.448333
2463.637528	132013.801924	58.453338
2463.179641	131806.559510	58.458343
2462.648598	131597.780534	58.463348
2461.974873	131384.821314	58.468353
2461.355979	131171.664473	58.473357
2460.582264	130959.537230	58.478362
2460.122922	130740.083608	58.483367
2459.289043	130535.628286	58.488372
2459.052839	130315.863160	58.493377
2458.317127	130105.197013	58.498381
2457.307622	129890.625700	58.503386
2456.783322	129671.051003	58.508391
2455.883828	129464.975410	58.513396
2455.493963	129246.386135	58.518401
2454.634569	129035.442820	58.523405
2453.840111	128815.269922	58.528410
2453.501007	128610.813741	58.533415
2452.831320	128401.242258	58.538420
2452.120149	128182.966283	58.543425
2451.593243	127973.032487	58.548429
2450.596634	127759.732913	58.553434
2450.360054	127534.299971	58.558439
2449.244434	127338.117209	58.563444
2448.973242	127108.006842	58.568449
2448.285271	126892.912434	58.573453
2447.127038	126689.133724	58.578458
2446.500456	126475.836252	58.583463
2446.370266	126258.093034	58.588468
2445.465840	126039.534503	58.593473
2444.939329	125827.800982	58.598477
2444.107661	125620.803583	58.603482
2443.667433	125404.525964	58.608487
2442.839868	125203.880774	58.613492
2442.432482	124979.283310	58.618497
2441.759044	124757.930046	58.623501
2440.751814	124550.816251	58.628506
2440.434959	124328.419459	58.633511
2439.540959	124120.503687	58.638516
2438.987636	123893.576409	58.643521
2438.344290	123686.297287	58.648525
2437.439694	123469.981776	58.653530
2436.772356	123255.128807	58.658535
2435.893079	123051.942764	58.663540
2435.563028	122835.757169	58.668545
2434.896948	122604.579397	58.673549
2433.705238	122412.190302	58.678554
2433.202002	122187.885323	58.683559
2432.680097	121986.847473	58.688564
2431.886281	121782.273508	58.693569
2431.722538	121565.830605	58.698573
2430.882400	121361.152956	58.703578
2430.237127	121141.805951	58.708583
2429.460725	120938.492786	58.713588
2428.915079	120725.126554	58.718593
2428.503704	120506.039792	58.723597
2427.612311	120289.303701	58.728602
2427.072044	120073.453302	58.733607
2426.206653	119865.667858	58.738612
2425.544400	119649.497477	58.743617
2425.013681	119439.910225	58.748621
2424.448549	119232.882092	58.753626
2423.715606	119014.626912	58.758631
2423.038119	118814.660023	58.763636
2422.247523	118595.903297	58.768641
2421.893311	118377.491856	58.773645
2421.011195	118173.144134	58.778650
2420.578294	117949.695798	58.783655
2419.707187	117732.450879	58.788660
2419.014733	117515.033468	58.793665
2418.324213	117295.948127	58.798669
2417.488657	117096.413130	58.803674
2417.129097	116876.091877	58.808679
2416.608731	116671.597142	58.813684
2415.906294	116461.178912	58.818689
2415.383201	116230.701335	58.823693
2414.654073	116025.591060	58.828698
2413.882076	115804.481154	58.833703
2413.066130	115585.328757	58.838708
2412.215537	115368.475101	58.843713
2411.804563	115153.286387	58.848717
2410.817718	114944.576028	58.853722
2410.444473	114729.968859	58.858727
2409.966927	114522.152343	58.863732
2409.218576	114301.039078	58.868737
2408.492418	114091.494703	58.873741
2407.609940	113874.684274	58.878746
2407.235938	113658.734432	58.883751
2406.879530	113450.018982	58.888756
2405.947786	113227.547917	58.893761
2405.153935	113006.389764	58.898765
2404.421664	112801.756733	58.903770
2404.179962	112579.911882	58.908775
2403.249309	112367.120448	58.913780
2402.278377	112145.712386	58.918785
2401.986120	111937.094573	58.923789
2400.808466	111724.569907	58.928794
2400.466084	111510.328066	58.933799
2399.904461	111302.589644	58.938804
2399.431314	111070.615568	58.943809
2398.864476	110858.236295	58.948813
2397.613793	110649.736826	58.953818
2397.131875	110435.462941	58.958823
2396.391079	110224.379554	58.963828
2395.878611	110014.987864	58.968833
2395.062918	109790.644441	58.973837
2394.514557	109577.917902	58.978842
2393.717873	109371.851180	58.983847
2393.301044	109168.169059	58.988852
2392.643626	108943.744834	58.993857
2392.233864	108732.501232	58.998861
2391.440347	108527.310467	59.003866
2390.648442	108303.998529	59.008871
2390.290579	108086.292618	59.013876
2389.490634	107865.137075	59.018881
2388.860237	107646.869154	59.023885
2387.914289	107434.865210	59.028890
2387.479483	107214.539699	59.033895
2386.608183	107001.138126	59.038900
2385.923522	106778.527542	59.043905
2385.875402	106548.324644	59.048909
2384.676722	106343.451374	59.053914
2384.605027	106115.090044	59.058919
2384.004883	105910.011366	59.063924
2382.775082	105688.950258	59.068929
2382.396844	105462.635995	59.073933
2381.648389	105236.966275	59.078938
2380.956279	105022.557757	59.083943
2380.374107	104802.201590	59.088948
2379.519323	104591.470849	59.093953
2379.048106	104363.005592	59.098957
2378.325437	104160.416652	59.103962
2377.586449	103929.231875	59.108967
2377.223908	103711.166669	59.113972
2376.455049	103492.000558	59.118977
2376.116396	103261.589914	59.123981
2374.935956	103041.789036	59.128986
2374.500267	102810.973122	59.133991
2373.627860	102599.412807	59.138996
2373.114562	102371.385813	59.144001
2372.502636	102148.502481	59.149005
2371.657693	101931.113852	59.154010
2371.219724	101707.541034	59.159015
2370.304432	101497.634130	59.164020
2369.791423	101272.960881	59.169025
2369.092922	101048.281142	59.174029
2368.397353	100836.734087	59.179034
2367.766382	100605.736154	59.184039
2366.788331	100386.822534	59.189044
2366.380561	100172.736609	59.194049
2365.787887	99961.523745	59.199053
2364.862101	99742.493743	59.204058
2364.402819	99519.268825	59.209063
2363.850706	99298.686805	59.214068
2362.983435	99080.104161	59.219073
2362.430603	98854.350624	59.224077
2361.667357	98649.430934	59.229082
2361.147303	98426.093037	59.234087
2360.343417	98203.722013	59.239092
2359.782441	97979.037606	59.244097
2359.185027	97760.012460	59.249101
2358.397179	97544.102093	59.254106
2357.547730	97324.302893	59.259111
2356.945912	97105.696982	59.264116
2356.375559	96882.705591	59.269121
2355.608687	96663.273875	59.274125
2355.261176	96453.938089	59.279130
2354.623088	96228.204973	59.284135
2354.061824	96011.537524	59.289140
2352.910656	95777.854757	59.294145
2352.716634	95557.404286	59.299149
2351.867170	95350.244812	59.304154
2351.087492	95123.923655	59.309159
2350.619671	94906.211920	59.314164
2349.945229	94684.171917	59.319169
2349.072740	94459.869811	59.324173
2348.349037	94240.974802	59.329178
2347.899233	94022.958029	59.334183
2347.166428	93810.340494	59.339188
2346.554871	93580.869185	59.344193
2346.087294	93369.723052	59.349197
2345.094563	93150.145775	59.354202
2344.753468	92917.353594	59.359207
2343.951534	92703.508339	59.364212
2343.007124	92477.233729	59.369217
2342.713134	92265.284247	59.374221
2341.906099	92033.475641	59.379226
2341.327456	91814.397579	59.384231
2340.671951	91597.629277	59.389236
2339.835736	91383.713423	59.394241
2339.147584	91155.585536	59.399245
2338.692053	90940.668845	59.404250
2337.780593	90729.142700	59.409255
2337.307526	90510.073537	59.414260
2336.588313	90278.231414	59.419265
2335.915104	90058.228398	59.424269
2335.281850	89846.685669	59.429274
2334.740170	89623.717885	59.434279
2333.888836	89409.576392	59.439284
2333.064882	89184.064691	59.444289
2332.807223	88965.414309	59.449293
2331.786716	88748.598901	59.454298
2331.195675	88528.325655	59.459303
2330.713692	88314.662586	59.464308
2329.923532	88086.278579	59.469313
2329.523489	87873.278892	59.474317
2328.719922	87658.322907	59.479322
2328.013056	87426.680363	59.484327
2327.196439	87212.073232	59.489332
2326.421845	86990.247163	59.494337
2326.040114	86774.611816	59.499341
2325.278275	86567.964814	59.504346
2324.544982	86347.552516	59.509351
2324.227221	86128.445877	59.514356
2323.376834	85902.338676	59.519361
2322.917665	85682.390546	59.524365
2322.062974	85474.107952	59.529370
2321.423108	85236.969723	59.534375
2320.853417	85018.934981	59.539380
2320.073555	84807.046501	59.544385
2319.665961	84576.705788	59.549389
2318.720845	84365.627587	59.554394
2318.205061	84133.667089	59.559399
2317.616135	83917.212356	59.564404
2316.671004	83694.268572	59.569409
2316.379282	83467.737346	59.574413
2315.273929	83258.685877	59.579418
2314.973394	83034.854528	59.584423
2314.098080	82815.274630	59.589428
2313.672062	82594.079243	59.594433
2313.216420	82371.369717	59.599437
2312.622289	82148.424649	59.604442
2311.904285	81913.763544	59.609447
2311.175102	81687.270141	59.614452
2310.313717	81467.328192	59.619457
2309.762693	81237.414292	59.624461
2308.734698	81009.701710	59.629466
2308.432255	80788.797322	59.634471
2307.617351	80571.829819	59.639476
2306.708498	80342.337441	59.644481
2306.592609	80122.836487	59.649485
2305.441333	79915.796653	59.654490
2304.751822	79680.680856	59.659495
2304.206129	79461.546575	59.664500
2303.634411	79238.584721	59.669505
2302.667788	79017.044047	59.674509
2301.861587	78798.243283	59.679514
2301.527253	78575.536114	59.684519
2300.866732	78368.643083	59.689524
2299.837023	78148.674306	59.694529
2299.561773	77929.880952	59.699533
2298.694838	77712.222987	59.704538
2298.171997	77488.613313	59.709543
2297.389027	77278.556999	59.714548
2296.696345	77053.971484	59.719553
2296.251068	76843.270454	59.724557
2295.517268	76636.482570	59.729562
2294.807192	76411.311261	59.734567
2294.407865	76189.939283	59.739572
2293.552121	75976.080810	59.744577
2293.037425	75755.219749	59.749581
2292.122173	75534.988524	59.754586
2291.513476	75316.751272	59.759591
2290.966822	75106.711577	59.764596
2290.341986	74887.233335	59.769601
2289.567992	74657.396747	59.774605
2288.734645	74441.637516	59.779610
2288.273282	74217.122733	59.784615
2287.657459	73991.538891	59.789620
2286.783556	73785.214154	59.794625
2286.457048	73567.039775	59.799629
2285.566791	73351.028843	59.804634
2284.983339	73126.577282	59.809639
2284.337228	72913.060147	59.814644
2283.602365	72696.727537	59.819649
2283.276037	72477.044556	59.824653
2281.996930	72271.597902	59.829658
2281.583697	72039.409133	59.834663
2281.095412	71820.633293	59.839668
2280.248387	71598.742999	59.844673
2279.946110	71384.015763	59.849677
2279.120943	71165.382914	59.854682
2278.293829	70942.812648	59.859687
2277.516913	70728.826580	59.864692
2276.865314	70505.517591	59.869697
2276.449549	70279.082529	59.874701
2275.252664	70074.551419	59.879706
2274.550199	69861.259722	59.884711
2274.139758	69644.326190	59.889716
2273.638101	69431.450697	59.894721
2273.225687	69220.020191	59.899725
2272.233877	69002.584204	59.904730
2271.707011	68785.292245	59.909735
2270.823661	68567.153489	59.914740
2270.313848	68350.991071	59.919745
2269.856685	68133.416606	59.924750
2268.754713	67929.988538	59.929754
2268.245597	67707.144795	59.934759
2267.726962	67481.803371	59.939764
2266.916899	67271.147354	59.944769
2266.436575	67052.334607	59.949774
2265.707789	66844.539341	59.954778
2265.205832	66623.410536	59.959783
2264.674183	66405.275045	59.964788
2263.490690	66193.185831	59.969793
2263.031048	65971.269291	59.974798
2262.229713	65761.860064	59.979802
2261.433782	65542.392474	59.984807
2261.193078	65326.616843	59.989812
2260.491760	65109.225840	59.994817
2259.616546	64902.722227	59.999822
2258.734579	64698.938588	60.004826
2258.518922	64483.459740	60.009831
2257.709841	64268.289565	60.014836
2257.061413	64052.909521	60.019841
2256.477869	63831.363435	60.024846
2255.722763	63627.200635	60.029850
2254.751641	63404.989587	60.034855
2254.420213	63188.188597	60.039860
2253.461578	62983.428590	60.044865
2253.089575	62765.435758	60.049870
2252.169517	62561.785428	60.054874
2251.790233	62347.939593	60.059879
2251.076225	62134.206240	60.064884
2250.133574	61919.061606	60.069889
2249.613613	61706.533810	60.074894
2249.127252	61495.747409	60.079898
2248.179133	61275.751503	60.084903
2247.638188	61066.830495	60.089908
2247.084435	60848.489662	60.094913
2246.680756	60640.301868	60.099918
2245.790501	60437.331301	60.104922
2245.106534	60215.121622	60.109927
2244.816841	59994.054933	60.114932
2243.950065	59784.364142	60.119937
2243.402752	59559.430898	60.124942
2242.378640	59348.741168	60.129946
2241.755257	59135.673202	60.134951
2241.090388	58926.558250	60.139956
2240.037087	58716.883685	60.144961
2239.832575	58498.388204	60.149966
2239.014340	58291.042430	60.154970
2238.619061	58082.713975	60.159975
2238.152312	57865.486109	60.164980
2237.222454	57658.079637	60.169985
2236.718868	57439.647187	60.174990
2236.129250	57225.608213	60.179994
2235.430832	57000.954540	60.184999
2234.513712	56784.310841	60.190004
2233.983744	56575.792795	60.195009
2233.650482	56357.507511	60.200014
2232.488076	56142.802852	60.205018
2232.030336	55919.491378	60.210023
2231.401441	55706.099711	60.215028
2230.574397	55497.786559	60.220033
2229.986129	55278.624071	60.225038
2229.295704	55061.977331	60.230042
2228.564096	54850.083474	60.235047
2227.721252	54635.038782	60.240052
2226.864563	54434.714040	60.245057
2226.470184	54218.837282	60.250062
2225.606487	54009.720923	60.255066
2225.144154	53800.312293	60.260071
2224.600881	53586.339990	60.265076
2223.688105	53378.922123	60.270081
2223.439897	53159.028616	60.275086
2222.481904	52959.356368	60.280090
2221.682571	52747.386930	60.285095
2221.103749	52536.549431	60.290100
2220.272484	52318.464111	60.295105
2219.923339	52112.417356	60.300110
2218.958083	51906.878845	60.305114
2218.639747	51699.901649	60.310119
2217.938432	51487.966219	60.315124
2216.733898	51292.230605	60.320129
2216.517003	51071.294376	60.325134
2215.913493	50861.568749	60.330138
2215.223133	50654.991612	60.335143
2214.558758	50441.006108	60.340148
2213.738430	50240.889662	60.345153
2213.432383	50020.961271	60.350158
2212.603613	49817.358062	60.355162
2211.858293	49605.742879	60.360167
2211.014214	49392.146416	60.365172
2210.220837	49193.840702	60.370177
2209.799634	48984.883218	60.375182
2208.916937	48770.300623	60.380186
2208.323716	48569.489862	60.385191
2207.821588	48365.370549	60.390196
2206.654200	48177.426352	60.395201
2206.334219	47963.612039	60.400206
2205.527803	47770.078894	60.405210
2204.673066	47569.573991	60.410215
2204.185691	47348.141483	60.415220
2203.253962	47159.054052	60.420225
2203.020288	46967.358946	60.425230
2202.095425	46767.883330	60.430234
2201.765438	46563.618284	60.435239
2200.924653	46362.068363	60.440244
2200.136812	46156.741926	60.445249
2199.918580	45960.459316	60.450254
2199.006297	45760.759041	60.455258
2198.146740	45555.106234	60.460263
2197.678281	45347.037390	60.465268
2196.749919	45160.450651	60.470273
2196.041849	44957.722342	60.475278
2195.524670	44756.455804	60.480282
2194.569362	44559.980008	60.485287
2194.013668	44368.215672	60.490292
2193.237276	44168.799807	60.495297
2193.247302	43978.771751	60.500302
2192.202928	43776.948611	60.505306
2191.463161	43576.562769	60.510311
2191.507868	43377.215470	60.515316
2190.209739	43179.016427	60.520321
2190.041209	42979.511434	60.525326
2188.895771	42783.022597	60.530330
2188.473618	42575.649914	60.535335
2187.472065	42383.560740	60.540340
2186.602968	42189.997988	60.545345
2186.382897	41981.525152	60.550350
2185.495975	41790.553342	60.555354
2184.772512	41600.613916	60.560359
2184.287626	41399.994620	60.565364
2183.665510	41206.852751	60.570369
2182.913609	41009.281298	60.575374
2182.068841	40814.617039	60.580378
2181.342106	40618.396318	60.585383
2180.870007	40422.858395	60.590388
2179.829548	40237.205667	60.595393
2179.636704	40033.861933	60.600398
2178.935072	39846.611892	60.605402
2178.327010	39651.641868	60.610407
2177.691746	39461.561916	60.615412
2176.710058	39266.457939	60.620417
2175.879964	39070.930595	60.625422
2175.110105	38896.266848	60.630426
2174.389414	38701.610102	60.635431
2173.974963	38512.104852	60.640436
2173.085827	38322.134788	60.645441
2172.495819	38142.454799	60.650446
2172.050177	37958.254839	60.655450
2170.986675	37776.949727	60.660455
2170.685435	37586.301836	60.665460
2169.907644	37395.527773	60.670465
2169.099293	37211.605285	60.675470
2168.225231	37027.040805	60.680474
2167.951244	36838.957768	60.685479
2167.558305	36661.998409	60.690484
2166.247227	36478.824378	60.695489
2165.896954	36286.082412	60.700494
2165.255272	36105.841085	60.705498
2164.201873	35931.872495	60.710503
2163.507679	35754.799746	60.715508
2162.601696	35586.100030	60.720513
2162.286807	35403.023085	60.725518
2162.007351	35232.022643	60.730522
2161.184282	35049.196133	60.735527
2160.463014	34858.060931	60.740532
2159.158072	34698.905454	60.745537
2158.428878	34511.657171	60.750542
2157.836540	34353.167951	60.755546
2157.157109	34184.476440	60.760551
2156.549469	34011.606059	60.765556
2155.803425	33848.663904	60.770561
2154.942980	33674.312023	60.775566
2154.206133	33520.621710	60.780570
2153.280093	33363.008740	60.785575
2153.062922	33196.003369	60.790580
2151.749918	33052.943443	60.795585
2150.776833	32894.621743	60.800590
2150.208000	32742.539707	60.805594
2149.017070	32606.820622	60.810599
2148.123349	32466.682844	60.815604
2147.264948	32331.278308	60.820609
2146.533281	32198.620231	60.825614
2145.748928	32074.405365	60.830618
2144.774869	31950.196245	60.835623
2144.247053	31823.057055	60.840628
2143.361725	31705.324107	60.845633
2142.810543	31587.922976	60.850638
2142.166560	31460.844509	60.855642
2141.361734	31342.017371	60.860647
2140.862223	31222.739709	60.865652
2139.997707	31111.707611	60.870657
2139.489007	30991.957450	60.875662
2138.738182	30886.521513	60.880666
2137.940051	30767.604231	60.885671
2137.517457	30652.660677	60.890676
2136.808921	30548.917239	60.895681
2136.058842	30429.225271	60.900686
2135.358344	30323.334638	60.905690
2134.670852	30210.894809	60.910695
2134.276877	30096.438849	60.915700
2133.359288	29988.873613	60.920705
2132.824682	29878.364750	60.925710
2132.158236	29760.982308	60.930714
2131.381748	29660.058243	60.935719
2130.993733	29547.861434	60.940724
2130.320996	29450.045878	60.945729
2129.660173	29334.183983	60.950734
2128.967384	29216.043337	60.955738
2128.283025	29104.547536	60.960743
2127.907066	28995.389297	60.965748
2127.272464	28899.302618	60.970753
2126.577925	28773.815550	60.975758
2125.973154	28669.482988	60.980762
2125.247762	28551.309670	60.985767
2124.738864	28445.734159	60.990772
2123.856645	28337.905605	60.995777
2123.139585	28230.293282	61.000782
2122.740172	28112.243639	61.005786
2121.906444	28007.351297	61.010791
2121.425938	27890.085523	61.015796
2120.630071	27780.434882	61.020801
2120.033554	27662.389761	61.025806
2119.705777	27564.169019	61.030810
2118.789610	27447.725973	61.035815
2118.409695	27329.584135	61.040820
2117.112955	27230.683440	61.045825
2116.416528	27108.147928	61.050830
2116.248835	27009.687137	61.055834
2115.508255	26903.344837	61.060839
2115.007934	26781.082418	61.065844
2114.385551	26682.236057	61.070849
2113.691612	26556.582783	61.075854
2112.905231	26448.287156	61.080858
2112.130427	26343.746146	61.085863
2111.679056	26224.971296	61.090868
2110.635340	26117.188679	61.095873
2110.078134	25998.507322	61.100878
2109.602045	25899.039116	61.105882
2108.906376	25796.708509	61.110887
2108.304785	25686.440982	61.115892
2107.152976	25579.707455	61.120897
2106.831738	25462.246039	61.125902
2106.074310	25357.729208	61.130906
2105.361504	25250.092607	61.135911
2105.037246	25135.336734	61.140916
2103.952290	25037.536613	61.145921
2103.257529	24932.000896	61.150926
2102.900019	24830.700043	61.155930
2102.159585	24723.008969	61.160935
2101.481578	24615.266065	61.165940
2100.586815	24520.437654	61.170945
2100.385091	24411.604920	61.175950
2099.562495	24305.101685	61.180954
2098.649133	24197.157276	61.185959
2098.296023	24082.326645	61.190964
2097.634749	23989.953582	61.195969
2097.196803	23870.330834	61.200974
2096.384571	23766.937115	61.205978
2095.816486	23670.476152	61.210983
2094.960197	23561.234219	61.215988
2094.150885	23460.322507	61.220993
2093.906892	23345.444321	61.225998
2093.046044	23235.618596	61.231002
2092.085846	23141.748494	61.236007
2092.089114	23025.944186	61.241012
2090.930303	22930.046560	61.246017
2090.446937	22810.423965	61.251022
2089.854420	22703.451911	61.256026
2088.960690	22607.810296	61.261031
2088.483167	22498.753244	61.266036
2087.349425	22401.851965	61.271041
2087.135360	22289.850197	61.276046
2086.276726	22189.261550	61.281050
2085.669322	22082.341842	61.286055
2085.542420	21981.621031	61.291060
2084.266985	21873.484518	61.296065
2083.765230	21771.127616	61.301070
2083.446028	21658.823240	61.306074
2082.459322	21557.658027	61.311079
2081.973465	21463.146966	61.316084
2080.637872	21351.697744	61.321089
2080.378028	21250.244660	61.326094
2079.787031	21146.051991	61.331098
2078.763036	21043.218899	61.336103
2078.241897	20941.474475	61.341108
2077.340286	20839.749232	61.346113
2076.463218	20744.034913	61.351118
2076.383482	20648.230975	61.356122
2075.690162	20552.643416	61.361127
2075.238304	20447.968226	61.366132
2074.180008	20348.968929	61.371137
2073.803553	20256.485566	61.376142
2073.017750	20148.331349	61.381146
2072.127961	20059.418793	61.386151
2071.959393	19954.264530	61.391156
2071.091974	19848.367991	61.396161
2070.191287	19757.839160	61.401166
2069.685810	19654.952994	61.406170
2068.737538	19563.936227	61.411175
2068.197069	19460.253957	61.416180
2066.978170	19364.978478	61.421185
2066.747364	19276.531468	61.426190
2065.848575	19195.690745	61.431194
2064.815002	19116.301987	61.436199
2064.688866	19023.229969	61.441204
2063.634309	18944.983058	61.446209
2063.127279	18845.743536	61.451214
2062.329228	18765.636684	61.456218
2061.351746	18677.656541	61.461223
2061.173375	18588.008266	61.466228
2060.040240	18510.583227	61.471233
2059.647446	18419.144324	61.476238
2059.040919	18341.138020	61.481242
2057.817138	18262.152462	61.486247
2057.450864	18193.124648	61.491252
2056.887592	18104.042709	61.496257
2056.380187	18023.561980	61.501262
2055.517147	17945.612966	61.506266
2054.700251	17873.479828	61.511271
2054.189132	17780.492880	61.516276
2053.417644	17706.530930	61.521281
2052.841317	17622.238087	61.526286
2052.276210	17550.362127	61.531290
2051.221240	17472.268719	61.536295
2050.725442	17392.385413	61.541300
2049.938762	17320.197947	61.546305
2049.353604	17246.806586	61.551310
2048.811423	17163.370463	61.556314
2047.881770	17098.819600	61.561319
2047.737262	17004.833820	61.566324
2046.790772	16946.406742	61.571329
2046.132507	16866.789129	61.576334
2045.478095	16792.601401	61.581338
2044.784017	16720.951432	61.586343
2044.113768	16638.857289	61.591348
2043.547531	16559.991936	61.596353
2042.982102	16487.414275	61.601358
2042.085255	16413.268612	61.606362
2041.780952	16338.645057	61.611367
2041.245618	16257.399217	61.616372
2040.230651	16182.030783	61.621377
2039.551705	16105.642059	61.626382
2039.419677	16022.175011	61.631386
2038.101015	15948.942509	61.636391
2037.773034	15880.175231	61.641396
2036.822089	15808.584459	61.646401
2036.199232	15742.975106	61.651406
2035.608216	15662.913366	61.656410
2034.996917	15593.565412	61.661415
2034.457334	15507.538993	61.666420
2033.552256	15444.076635	61.671425
2032.744108	15371.413486	61.676430
2032.486932	15295.499351	61.681434
2031.639776	15218.129443	61.686439
2031.076041	15141.189900	61.691444
2030.220517	15073.382296	61.696449
2029.742642	15002.135953	61.701454
2029.154821	14927.289342	61.706458
2028.035810	14861.420824	61.711463
2027.967609	14770.115795	61.716468
2027.056176	14708.840991	61.721473
2026.307043	14637.544376	61.726478
2025.814243	14566.409462	61.731482
2025.190538	14504.042172	61.736487
2024.597774	14421.077774	61.741492
2023.467519	14349.153868	61.746497
2023.373510	14274.434411	61.751502
2022.596519	14204.711862	61.756506
2021.496613	14130.627173	61.761511
2021.082288	14054.486315	61.766516
2020.308886	13988.105790	61.771521
2019.633003	13917.873160	61.776526
2019.242583	13837.428606	61.781530
2018.378917	13779.575082	61.786535
2017.912943	13699.748868	61.791540
2017.046060	13633.643281	61.796545
2016.433283	13570.422552	61.801550
2015.838397	13500.745434	61.806554
2014.726278	13441.496837	61.811559
2014.359705	13353.723120	61.816564
2013.432716	13285.508799	61.821569
2013.055116	13230.714464	61.826574
2012.434537	13151.191865	61.831578
2011.847429	13096.032922	61.836583
2011.238763	13019.740226	61.841588
2010.125826	12940.520276	61.846593
2009.779014	12874.125518	61.851598
2009.365785	12800.138455	61.856602
2008.576271	12748.892141	61.861607
2008.059470	12662.303743	61.866612
2007.168195	12603.853648	61.871617
2006.649901	12530.798114	61.876622
2006.011635	12468.112262	61.881626
2005.464698	12394.045700	61.886631
2004.616493	12319.158664	61.891636
2003.865863	12261.588764	61.896641
2003.059679	12183.102383	61.901646
2002.544110	12115.325950	61.906650
2001.621688	12051.577392	61.911655
2001.098431	11976.692750	61.916660
2000.484746	11916.840988	61.921665
1999.884576	11852.154361	61.926670
1999.214760	11782.901409	61.931674
1998.435781	11719.537479	61.936679
1998.126657	11646.760152	61.941684
1997.415562	11580.639145	61.946689
1996.779104	11502.773053	61.951694
1996.269510	11440.369494	61.956698
1995.184552	11384.629871	61.961703
1994.570543	11305.294501	61.966708
1994.145051	11228.071599	61.971713
1993.471882	11168.948125	61.976718
1992.485453	11098.441038	61.981722
1991.563327	11030.597658	61.986727
1991.117982	10960.952423	61.991732
1990.566974	10897.531286	61.996737
1989.448002	10830.221896	62.001742
1989.499315	10774.313255	62.006746
1988.372311	10707.928492	62.011751
1987.755926	10644.128013	62.016756
1987.373058	10571.162595	62.021761
1986.584956	10511.721428	62.026766
1985.767554	10451.647992	62.031770
1985.054542	10394.787777	62.036775
1984.641427	10323.881440	62.041780
1983.737592	10265.311380	62.046785
1983.225879	10207.447830	62.051790
1982.745585	10137.010672	62.056794
1981.481204	10083.716195	62.061799
1981.283354	10016.286331	62.066804
1980.562390	9955.876064	62.071809
1979.971497	9885.405953	62.076814
1979.492507	9818.014495	62.081818
1978.653507	9764.462890	62.086823
1978.377928	9684.093682	62.091828
1977.265583	9624.412390	62.096833
1976.598667	9561.575257	62.101838
1976.046042	9494.444284	62.106842
1975.308365	9433.131816	62.111847
1974.557295	9371.479698	62.116852
1973.654583	9308.811229	62.121857
1973.177664	9241.445297	62.126862
1972.308259	9173.356140	62.131866
1971.829806	9118.955896	62.136871
1971.286761	9051.099524	62.141876
1970.087289	9004.690053	62.146881
1969.641137	8935.758053	62.151886
1969.120711	8874.923053	62.156890
1968.514900	8817.755131	62.161895
1968.229088	8756.677848	62.166900
1967.181449	8691.019175	62.171905
1966.951449	8629.187596	62.176910
1966.414674	8567.498848	62.181914
1965.453746	8502.438673	62.186919
1964.796185	8430.523656	62.191924
1964.042434	8371.148219	62.196929
1963.227439	8307.640050	62.201934
1962.536467	8255.720388	62.206938
1961.776157	8196.922603	62.211943
1961.444924	8132.146719	62.216948
1961.005089	8069.325152	62.221953
1960.222897	8006.172409	62.226958
1959.756235	7942.104411	62.231962
1958.890823	7878.733080	62.236967
1958.528525	7809.132630	62.241972
1957.812598	7746.909658	62.246977
1956.965490	7685.214635	62.251982
1956.497249	7612.299996	62.256986
1955.385328	7552.254538	62.261991
1955.236947	7482.481624	62.266996
1954.506741	7418.782723	62.272001
1953.677356	7350.278184	62.277006
1952.803725	7288.788598	62.282010
1952.159898	7234.307456	62.287015
1951.661534	7163.914725	62.292020
1950.858913	7107.412127	62.297025
1949.998753	7045.551427	62.302030
1949.302311	6987.642447	62.307034
1948.792858	6933.443210	62.312039
1948.150814	6870.037160	62.317044
1947.398069	6803.656040	62.322049
1946.726551	6751.776782	62.327054
1946.368088	6691.427454	62.332058
1945.524572	6621.275085	62.337063
1944.945032	6558.861483	62.342068
1944.249143	6498.280937	62.347073
1943.427447	6445.111200	62.352078
1943.046234	6381.104180	62.357082
1942.200081	6318.732328	62.362087
1941.626967	6257.234801	62.367092
1940.819338	6208.413261	62.372097
1940.097104	6145.263620	62.377102
1939.518896	6083.994010	62.382106
1938.548066	6036.736343	62.387111
1938.598661	5975.653706	62.392116
1937.466349	5909.838512	62.397121
1936.872945	5846.601066	62.402126
1936.095427	5789.092195	62.407130
1935.677227	5734.890731	62.412135
1935.128958	5670.806801	62.417140
1934.457960	5621.986802	62.422145
1933.508343	5548.895222	62.427150
1933.164788	5487.274524	62.432154
1932.304155	5439.435714	62.437159
1931.989328	5376.183661	62.442164
1931.282302	5305.071682	62.447169
1930.550056	5244.041385	62.452174
1929.826408	5185.621587	62.457178
1928.939239	5131.754699	62.462183
1928.410755	5064.622462	62.467188
1927.586246	5010.238109	62.472193
1926.805355	4946.042010	62.477198
1926.443760	4886.774799	62.482202
1925.375492	4836.618055	62.487207
1925.218756	4768.939912	62.492212
1924.648552	4717.526912	62.497217
1923.825260	4661.959745	62.502222
1923.054380	4589.507077	62.507226
1922.412860	4534.879313	62.512231
1921.599167	4471.666148	62.517236
1921.055176	4424.323800	62.522241
1920.419152	4358.881576	62.527246
1919.889156	4293.468557	62.532250
1919.054625	4253.100215	62.537255
1918.244517	4189.487810	62.542260
1917.639782	4129.173809	62.547265
1917.022776	4072.452204	62.552270
1916.333252	4023.084394	62.557274
1915.580369	3960.940351	62.562279
1915.085979	3906.626759	62.567284
1914.505853	3849.684055	62.572289
1913.526606	3782.946259	62.577294
1913.306386	3737.713374	62.582298
1912.602416	3666.501543	62.587303
1911.962159	3616.288114	62.592308
1911.473255	3552.432668	62.597313
1910.632417	3494.818968	62.602318
1910.139021	3428.399205	62.607322
1909.154190	3376.423401	62.612327
1908.660257	3308.950599	62.617332
1907.705945	3252.008882	62.622337
1906.955449	3208.827945	62.627342
1906.537512	3138.746005	62.632346
1905.481418	3092.889895	62.637351
1905.043906	3027.468611	62.642356
1904.714083	2973.917050	62.647361
1903.797428	2921.223042	62.652366
1902.971499	2861.095257	62.657370
1902.358217	2817.590062	62.662375
1901.747491	2753.339451	62.667380
1901.266791	2694.614947	62.672385
1900.506097	2646.314316	62.677390
1899.918954	2577.599438	62.682394
1899.183550	2534.746951	62.687399
1898.521036	2475.225710	62.692404
1898.080627	2409.855745	62.697409
1897.259053	2354.435833	62.702414
1896.529774	2290.449755	62.707418
1895.435302	2244.728578	62.712423
1895.274713	2194.830289	62.717428
1894.490505	2137.828839	62.722433
1893.847897	2085.061218	62.727438
1893.318837	2023.396924	62.732442
1892.472294	1970.851354	62.737447
1891.715678	1915.822613	62.742452
1891.251664	1866.877339	62.747457
1890.362730	1814.199483	62.752462
1889.932426	1761.688738	62.757466
1889.225024	1710.871097	62.762471
1888.609793	1642.288880	62.767476
1888.273930	1596.079463	62.772481
1887.336614	1537.358758	62.777486
1886.566996	1486.448473	62.782490
1885.779740	1433.518492	62.787495
1884.775646	1372.873909	62.792500
1884.311226	1323.955755	62.797505
1883.658542	1279.655488	62.802510
1883.305211	1228.056269	62.807514
1882.385163	1181.351069	62.812519
1881.796174	1127.433421	62.817524
1880.955512	1072.338410	62.822529
1880.102790	1024.897561	62.827534
1879.640760	966.758985	62.832538
1878.918587	926.530240	62.837543
1878.212282	881.638831	62.842548
1877.689073	828.082461	62.847553
1877.073250	785.479505	62.852558
1876.617026	734.185397	62.857562
1875.870822	681.642745	62.862567
1875.213608	630.518115	62.867572
1874.658594	582.670303	62.872577
1873.595224	523.219093	62.877582
1873.394079	485.443148	62.882586
1872.578169	437.296597	62.887591
1871.574243	387.172507	62.892596
1870.841728	343.930179	62.897601
1869.830678	306.494602	62.902606
1869.483631	257.307503	62.907610
1868.700138	228.200449	62.912615
1868.238496	175.161066	62.917620
1867.491252	132.388499	62.922625
1866.753729	96.143250	62.927630
1865.999012	52.208289	62.932634
1865.141819	15.435028	62.937639
1864.562548	-19.343232	62.942644
1863.716299	-53.311035	62.947649
1862.601632	-88.027782	62.952654
1862.253483	-123.642008	62.957658
1861.209163	-148.693513	62.962663
1860.645033	-177.016132	62.967668
1860.246471	-209.354682	62.972673
1858.876260	-225.539123	62.977678
1858.063442	-234.493401	62.982682
1856.395358	-222.379402	62.987687
1847.665562	-12.345067	62.992692
1846.878890	49.780338	62.997697
1848.604713	86.754669	63.002702
1851.292155	103.351510	63.007706
1852.976553	123.187491	63.012711
1853.830691	112.500159	63.017716
1853.851883	100.330242	63.022721
1853.124494	76.333504	63.027726
1853.077417	50.749583	63.032730
1851.570150	37.366835	63.037735
1850.298776	26.520281	63.042740
1848.924471	17.929391	63.047745
1847.764359	16.000357	63.052750
1847.586421	20.606512	63.057754
1846.532583	15.136053	63.062759
1845.958995	16.854495	63.067764
1845.482898	10.202617	63.072769
1844.864785	23.777560	63.077774
1844.612371	11.886129	63.082778
1844.314610	9.343933	63.087783
1843.077831	11.161363	63.092788
1842.309097	11.776940	63.097793
1841.204058	17.709874	63.102798
1840.728857	13.473788	63.107802
1839.766243	29.192933	63.112807
1839.070400	26.239268	63.117812
1839.053975	27.325190	63.122817
1837.915300	29.275285	63.127822
1837.697226	23.481314	63.132826
1836.678311	28.938525	63.137831
1836.699188	34.113947	63.142836
1836.513834	28.732680	63.147841
1835.559943	29.401313	63.152846
1834.206933	20.622543	63.157850
1833.199809	36.367687	63.162855
1832.947989	31.105785	63.167860
1832.693076	28.033226	63.172865
1831.381544	37.047263	63.177870
1830.908996	38.211916	63.182874
1830.151033	41.973445	63.187879
1830.219984	46.158778	63.192884
1829.856547	33.833944	63.197889
1828.919608	40.121830	63.202894
1828.163898	31.738660	63.207898
1826.517245	41.260082	63.212903
1826.144720	42.717943	63.217908
1825.976669	39.879177	63.222913
1825.406398	46.690754	63.227918
1824.454894	39.478828	63.232922
1823.696593	43.803396	63.237927
1822.734711	41.089097	63.242932
1822.964234	38.759649	63.247937
1822.441297	51.963110	63.252942
1821.846700	38.799751	63.257946
1820.486582	45.358266	63.262951
1819.589540	53.137959	63.267956
1819.506709	48.013227	63.272961
1818.980067	64.350754	63.277966
1818.946399	43.460989	63.282970
1817.295609	43.164781	63.287975
1816.307232	42.550502	63.292980
1816.013482	47.761693	63.297985
1815.402583	56.839545	63.302990
1815.213602	40.752709	63.307994
1814.668674	52.333794	63.312999
1813.587560	53.569850	63.318004
1812.707492	40.693099	63.323009
1811.730223	57.029629	63.328014
1811.650007	54.820324	63.333018
1811.120000	54.434469	63.338023
1810.609327	47.245590	63.343028
1809.595381	44.834458	63.348033
1808.288245	63.120484	63.353038
1808.430767	42.026126	63.358042
1808.058423	54.524421	63.363047
1806.839740	51.879289	63.368052
1806.511624	48.595998	63.373057
1805.352570	54.323066	63.378062
1805.091466	44.460999	63.383066
1804.209455	53.348506	63.388071
1803.835243	54.950145	63.393076
1802.722714	48.311006	63.398081
1802.201002	52.896064	63.403086
1801.922251	44.795136	63.408090
1801.458981	51.411530	63.413095
1800.514154	57.435751	63.418100
1799.366226	51.999164	63.423105
1798.411684	59.021582	63.428110
1798.727028	55.905781	63.433114
1797.668108	58.049816	63.438119
1797.076407	53.146238	63.443124
1796.599057	43.641793	63.448129
1795.388677	62.916997	63.453134
1795.459675	62.101390	63.458138
1794.635507	50.895251	63.463143
1793.518481	58.672038	63.468148
1792.807050	60.309879	63.473153
1792.266258	67.623002	63.478158
1792.348478	57.920881	63.483162
1791.522222	62.398181	63.488167
1790.431870	57.280467	63.493172
1789.815320	43.226452	63.498177
1788.998949	58.980765	63.503182
1788.549479	49.123378	63.508186
1788.003320	53.349614	63.513191
1787.403832	58.431160	63.518196
1786.912185	49.402079	63.523201
1786.111833	59.647025	63.528206
1785.586223	48.992737	63.533210
1785.095099	51.046613	63.538215
1783.305565	53.565295	63.543220
1783.138817	47.578666	63.548225
1782.793317	62.597456	63.553230
1781.819790	52.954175	63.558234
1781.113218	59.806333	63.563239
1780.338276	55.335565	63.568244
1780.537901	50.736850	63.573249
1779.285714	62.357715	63.578254
1779.089030	58.015899	63.583258
1778.002253	58.240445	63.588263
1777.233820	57.671680	63.593268
1776.606877	63.823630	63.598273
1775.865416	63.619597	63.603278
1775.277612	64.189116	63.608282
1774.742798	61.919535	63.613287
1774.175804	58.445518	63.618292
1773.825308	66.699846	63.623297
1773.244890	63.585934	63.628302
1772.306497	62.012812	63.633306
1771.110693	63.254482	63.638311
1770.344421	63.838151	63.643316
1769.928943	53.778245	63.648321
1769.203624	60.393681	63.653326
1769.029479	59.396224	63.658330
1768.155348	56.048255	63.663335
1767.466130	66.059514	63.668340
1766.860829	58.844667	63.673345
1765.816821	65.599025	63.678350
1765.440169	61.055550	63.683354
1765.255523	61.611513	63.688359
1764.681307	67.263075	63.693364
1764.337804	59.960922	63.698369
1763.112773	64.991998	63.703374
1761.941438	62.996969	63.708378
1761.037456	68.098492	63.713383
1760.262804	64.599105	63.718388
1760.638754	60.081198	63.723393
1759.717198	61.222550	63.728398
1759.442278	61.180980	63.733402
1758.601555	53.514659	63.738407
1757.606027	58.720605	63.743412
1757.413543	53.056615	63.748417
1756.056637	54.412186	63.753422
1755.165927	58.817727	63.758426
1754.895436	57.075466	63.763431
1754.223131	57.167968	63.768436
1753.454679	52.447017	63.773441
1752.863797	59.692400	63.778446
1752.455125	57.505296	63.783450
1751.823061	67.206278	63.788455
1751.057937	69.951816	63.793460
1750.688767	55.379116	63.798465
1750.167755	62.307470	63.803470
1749.618007	57.827759	63.808474
1748.479760	54.570627	63.813479
1747.218758	67.474993	63.818484
1746.805508	56.637284	63.823489
1745.988713	64.654999	63.828494
1745.493730	65.266556	63.833498
1745.332469	68.517027	63.838503
1744.788226	71.959210	63.843508
1744.335877	57.932740	63.848513
1743.847426	66.762498	63.853518
1742.948385	62.049670	63.858522
1742.057818	65.736090	63.863527
1741.390730	64.258668	63.868532
1740.675167	60.054455	63.873537
1739.919463	63.602760	63.878542
1738.550678	65.720333	63.883546
1738.373158	61.151547	63.888551
1737.537106	61.579147	63.893556
1737.500163	60.676600	63.898561
1736.120613	70.400101	63.903566
1735.810917	57.557371	63.908570
1734.993376	68.047918	63.913575
1734.445392	59.109797	63.918580
1734.092460	54.964693	63.923585
1733.588738	62.633063	63.928590
1733.329740	52.280229	63.933594
1732.135355	58.102826	63.938599
1730.878169	64.815355	63.943604
1730.492379	64.889169	63.948609
1729.347623	62.981399	63.953614
1728.818459	59.900362	63.958618
1728.650541	60.780106	63.963623
1727.962246	60.309017	63.968628
1727.733135	60.878353	63.973633
1727.054950	63.203227	63.978638
1726.744348	59.880894	63.983642
1725.248448	63.116242	63.988647
1724.399592	61.831699	63.993652
1724.103863	57.209147	63.998657
1723.260009	60.217935	64.003662
1723.068414	55.151484	64.008666
1722.490836	59.281795	64.013671
1721.270985	64.491842	64.018676
1720.492278	61.217045	64.023681
1719.601497	62.314098	64.028686
1719.076288	61.411826	64.033690
1719.037360	65.396666	64.038695
1718.113389	66.227750	64.043700
1717.677893	61.132224	64.048705
1716.975901	65.261797	64.053710
1716.748588	63.757114	64.058714
1715.466649	54.487705	64.063719
1714.266622	61.590139	64.068724
1713.864193	58.850106	64.073729
1713.225938	65.073252	64.078734
1712.859230	57.531940	64.083738
1712.164760	66.533197	64.088743
1711.592112	68.253099	64.093748
1711.050257	57.030540	64.098753
1710.565497	60.436470	64.103758
1709.476049	59.243761	64.108762
1708.776845	59.834142	64.113767
1707.891222	58.221124	64.118772
1707.586083	55.423063	64.123777
1706.770754	61.552904	64.128782
1706.408872	62.955475	64.133786
1706.050733	68.053900	64.138791
1704.987033	62.233388	64.143796
1704.381082	57.026164	64.148801
1703.231126	65.808023	64.153806
1702.778782	63.209962	64.158810
1702.288278	63.499111	64.163815
1701.672225	58.009635	64.168820
1701.262519	58.232334	64.173825
1700.390699	69.483731	64.178830
1699.538999	58.371889	64.183834
1698.686495	60.970465	64.188839
1697.818373	63.521059	64.193844
1697.809454	60.124006	64.198849
1696.799098	65.330753	64.203854
1696.586804	56.724111	64.208858
1696.003901	59.719846	64.213863
1695.441476	62.275505	64.218868
1694.687760	59.424110	64.223873
1693.585367	63.044837	64.228878
1692.548078	57.297410	64.233882
1692.337170	61.580805	64.238887
1691.881764	65.546637	64.243892
1691.464947	60.982747	64.248897
1690.210955	59.019804	64.253902
1689.462860	61.423601	64.258906
1689.104653	56.700590	64.263911
1688.237679	57.596750	64.268916
1687.939536	54.873275	64.273921
1687.432676	68.787001	64.278926
1687.113041	56.810050	64.283930
1685.881538	57.656875	64.288935
1684.788470	65.352625	64.293940
1684.572141	58.517577	64.298945
1683.763864	60.399491	64.303950
1683.340647	57.453027	64.308954
1682.677738	65.033145	64.313959
1681.330255	74.393603	64.318964
1680.879400	57.160909	64.323969
1680.205373	71.618439	64.328974
1679.826269	54.901064	64.333978
1679.383854	62.337347	64.338983
1678.550834	64.928104	64.343988
1678.317785	66.589342	64.348993
1677.573303	63.613480	64.353998
1676.612821	59.000326	64.359002
1675.770702	62.295863	64.364007
1675.203867	65.412055	64.369012
1674.639364	61.879319	64.374017
1674.083697	62.435871	64.379022
1673.528676	70.754231	64.384026
1672.384654	57.809070	64.389031
1671.516029	73.216892	64.394036
1671.252954	56.731829	64.399041
1670.735944	64.891181	64.404046
1670.189213	64.413391	64.409050
1669.768326	60.493562	64.414055
1668.542441	59.292579	64.419060
1667.974729	58.788160	64.424065
1667.045400	70.728378	64.429070
1666.792440	56.403754	64.434074
1666.474818	60.793987	64.439079
1665.319591	65.536468	64.444084
1664.440587	59.913725	64.449089
1663.912455	68.111116	64.454094
1663.152184	56.718260	64.459098
1662.863202	60.788548	64.464103
1662.324904	64.426922	64.469108
1661.826061	57.591021	64.474113
1660.656412	62.397295	64.479118
1659.661985	61.336173	64.484122
1659.319002	57.996917	64.489127
1658.452722	67.474914	64.494132
1658.605081	60.603384	64.499137
1657.740878	65.067824	64.504142
1656.833717	58.495482	64.509146
1656.317915	66.150010	64.514151
1655.151808	67.530521	64.519156
1654.994983	52.354832	64.524161
1654.534596	56.556427	64.529166
1653.492523	57.235979	64.534170
1652.364347	56.093602	64.539175
1651.579479	59.596098	64.544180
1651.010109	51.721135	64.549185
1650.749988	60.147193	64.554190
1650.461814	58.037163	64.559194
1649.971288	55.509836	64.564199
1649.091216	60.385236	64.569204
1648.237243	48.187246	64.574209
1647.214319	57.985016	64.579214
1646.871537	64.993885	64.584218
1646.400589	63.397021	64.589223
1645.519804	70.633281	64.594228
1645.405963	59.609264	64.599233
1644.082925	61.159788	64.604238
1643.411210	64.882437	64.609242
1643.071852	57.981783	64.614247
1642.242388	68.605132	64.619252
1641.790174	63.605319	64.624257
1640.912448	63.752559	64.629262
1639.936773	58.820130	64.634266
1639.577939	63.346225	64.639271
1638.506946	61.833641	64.644276
1638.272979	58.119097	64.649281
1637.597319	62.244503	64.654286
1637.531651	65.594911	64.659290
1636.422897	61.420073	64.664295
1635.532214	61.906847	64.669300
1634.939745	59.802578	64.674305
1634.079892	67.872891	64.679310
1634.006245	57.110580	64.684314
1633.504922	66.035434	64.689319
1631.985360	66.650494	64.694324
1631.436559	51.437728	64.699329
1630.804347	66.524139	64.704334
1630.139664	63.428381	64.709338
1630.298823	58.064945	64.714343
1629.582388	65.377603	64.719348
1628.430428	50.017798	64.724353
1627.502344	57.958596	64.729358
1626.802756	51.621383	64.734362
1626.505785	56.049339	64.739367
1626.040298	63.125009	64.744372
1625.167603	62.658009	64.749377
1624.294925	53.438762	64.754382
1623.557011	58.403551	64.759386
1623.137820	55.240414	64.764391
1622.381539	62.463206	64.769396
1622.301209	55.597104	64.774401
1620.879682	50.722896	64.779406
1619.894810	55.564488	64.784410
1619.637769	52.544330	64.789415
1618.922596	62.392573	64.794420
1618.356622	59.550802	64.799425
1618.073340	60.108251	64.804430
1617.641510	54.909664	64.809434
1616.886515	60.850166	64.814439
1615.400230	60.597340	64.819444
1615.412804	58.956788	64.824449
1614.678031	66.717071	64.829454
1613.920316	66.820023	64.834458
1612.906019	55.803439	64.839463
1612.282057	65.373840	64.844468
1611.836983	55.936853	64.849473
1611.081865	63.358163	64.854478
1610.619588	68.138819	64.859482
1610.350297	69.356379	64.864487
1609.761292	65.903246	64.869492
1608.767445	65.742508	64.874497
1608.158331	69.685460	64.879502
1607.565814	62.832913	64.884506
1606.530153	58.678018	64.889511
1605.387286	69.746985	64.894516
1604.940473	56.739990	64.899521
1604.244556	60.602111	64.904526
1603.712898	65.116241	64.909530
1603.522936	55.947818	64.914535
1602.976188	66.486836	64.919540
1602.761985	55.996022	64.924545
1601.741138	60.013844	64.929550
1600.995417	70.743750	64.934554
1600.322961	61.544740	64.939559
1599.246779	61.475935	64.944564
1598.449186	62.864158	64.949569
1597.844443	62.121206	64.954574
1597.517608	60.738005	64.959578
1597.226468	65.155577	64.964583
1595.896124	72.830707	64.969588
1595.002678	57.298957	64.974593
1594.520877	61.175952	64.979598
1594.086383	66.357480	64.984602
1593.804013	63.735593	64.989607
1592.931005	61.543436	64.994612
1591.822992	55.520281	64.999617
1591.230791	68.252217	65.004622
1590.593370	57.811294	65.009626
1590.039766	61.969360	65.014631
1589.619530	61.786888	65.019636
1589.264265	61.092614	65.024641
1588.082173	65.058787	65.029646
1587.126837	67.279490	65.034650
1587.290430	60.116012	65.039655
1586.250806	67.800151	65.044660
1585.750732	65.102463	65.049665
1584.673141	64.213857	65.054670
1583.842237	56.318961	65.059674
1583.615998	58.496372	65.064679
1582.875469	60.252432	65.069684
1582.703327	57.807004	65.074689
1581.365262	63.663527	65.079694
1580.458933	62.175271	65.084698
1580.128901	58.835548	65.089703
1579.422565	61.201199	65.094708
1579.174024	54.768687	65.099713
1578.635250	58.976438	65.104718
1577.532298	54.808593	65.109722
1576.711890	59.138361	65.114727
1576.186560	60.454950	65.119732
1575.658764	58.026602	65.124737
1575.192888	55.959007	65.129742
1574.388336	55.618396	65.134746
1573.375168	61.404380	65.139751
1572.730259	59.934519	65.144756
1572.424119	56.594155	65.149761
1572.146031	60.645372	65.154766
1571.257807	53.019791	65.159770
1570.250189	57.912323	65.164775
1569.272766	60.098692	65.169780
1568.920616	54.761297	65.174785
1568.584176	61.171485	65.179790
1567.508699	59.770033	65.184794
1566.621080	56.883183	65.189799
1565.593428	59.750903	65.194804
1565.572270	60.567915	65.199809
1565.180936	55.992120	65.204814
1564.626445	59.771855	65.209818
1564.510804	57.191294	65.214823
1563.386055	57.526042	65.219828
1562.678132	49.949093	65.224833
1561.818408	56.603270	65.229838
1561.137283	58.947573	65.234842
1560.026504	56.241263	65.239847
1559.346370	60.838914	65.244852
1559.067630	57.186688	65.249857
1558.318491	52.845941	65.254862
1558.020775	55.498342	65.259866
1557.567991	56.754521	65.264871
1556.043080	64.195644	65.269876
1555.775048	64.282314	65.274881
1554.855004	65.735738	65.279886
1554.589756	63.480149	65.284890
1554.109535	60.176907	65.289895
1552.923311	63.358415	65.294900
1552.268511	65.791581	65.299905
1551.497714	61.894253	65.304910
1550.983021	62.822796	65.309914
1550.686377	55.765562	65.314919
1550.194912	67.025943	65.319924
1549.415539	66.162512	65.324929
1548.459762	63.202916	65.329934
1548.131039	56.120817	65.334938
1547.620690	56.722235	65.339943
1546.679057	61.657909	65.344948
1545.949554	54.477060	65.349953
1545.247672	60.327137	65.354958
1544.508618	67.629213	65.359962
1544.275704	50.705731	65.364967
1543.095678	55.220380	65.369972
1542.352595	59.914770	65.374977
1541.764008	58.745057	65.379982
1541.146745	60.497312	65.384986
1541.059451	55.526278	65.389991
1539.687163	57.079949	65.394996
1538.847029	54.836857	65.400001
1538.679063	58.615107	65.405006
1537.805117	62.716846	65.410010
1537.685711	49.662588	65.415015
1536.945141	57.450611	65.420020
1535.869002	53.671194	65.425025
1535.304984	53.973631	65.430030
1534.463944	60.000365	65.435034
1534.259475	57.367686	65.440039
1533.592313	62.447414	65.445044
1532.471503	51.569227	65.450049
1531.733206	65.305259	65.455054
1531.132137	63.785865	65.460058
1530.952807	54.869659	65.465063
1530.431941	59.650170	65.470068
1529.485510	58.933140	65.475073
1528.223854	63.239992	65.480078
1528.052007	58.577288	65.485082
1527.507077	58.062973	65.490087
1526.808275	61.873530	65.495092
1526.290928	58.229259	65.500097
1525.224694	57.643232	65.505102
1524.043545	55.990503	65.510106
1523.691132	61.196843	65.515111
1523.432909	60.853018	65.520116
1523.236643	61.401382	65.525121
1522.645921	59.221168	65.530126
1521.671410	66.838210	65.535130
1521.138746	52.761501	65.540135
1520.193050	67.856731	65.545140
1519.654104	66.425241	65.550145
1518.713382	67.763690	65.555150
1517.825889	65.767829	65.560154
1517.606704	58.035961	65.565159
1516.909102	65.090177	65.570164
1516.492009	61.092504	65.575169
1515.015812	63.960552	65.580174
1514.200399	67.496325	65.585178
1514.190792	64.539366	65.590183
1513.516905	64.364094	65.595188
1513.314132	54.842902	65.600193
1512.774870	59.539606	65.605198
1511.635723	60.483801	65.610202
1511.219205	60.625609	65.615207
1510.438700	61.175344	65.620212
1509.175222	46.054114	65.625217
1508.338782	55.940564	65.630222
1507.808380	62.826285	65.635226
1507.473067	57.766928	65.640231
1506.879126	54.328801	65.645236
1506.490641	55.032291	65.650241
1506.450118	55.279936	65.655246
1505.170391	64.208641	65.660250
1504.668339	59.950076	65.665255
1503.554373	63.358246	65.670260
1502.368804	49.349025	65.675265
1501.774559	59.495042	65.680270
1501.030499	62.874396	65.685274
1500.834267	60.301914	65.690279
1500.159437	70.377164	65.695284
1499.509810	62.218524	65.700289
1499.602305	70.998571	65.705294
1498.822697	61.558000	65.710298
1498.263676	65.108229	65.715303
1497.000516	68.991127	65.720308
1496.792866	64.403501	65.725313
1495.404465	62.337433	65.730318
1494.785510	64.462135	65.735322
1494.375668	53.939354	65.740327
1493.657874	64.954999	65.745332
1493.536366	60.131333	65.750337
1492.786405	61.297549	65.755342
1492.056784	65.311712	65.760346
1491.429966	61.918236	65.765351
1490.361880	55.805207	65.770356
1489.097437	52.390054	65.775361
1488.656097	58.451056	65.780366
1488.077501	64.294171	65.785370
1487.726905	62.515785	65.790375
1487.230394	67.407554	65.795380
1486.852236	65.631971	65.800385
1486.405608	62.263481	65.805390
1484.876041	68.552610	65.810394
1484.812969	62.461228	65.815399
1484.097407	63.934222	65.820404
1483.333645	57.414862	65.825409
1482.289905	57.511264	65.830414
1481.496830	65.503192	65.835418
1481.273205	65.209068	65.840423
1480.753723	62.555489	65.845428
1479.948963	57.100798	65.850433
1478.881905	61.403555	65.855438
1478.206938	67.478033	65.860442
1477.619808	57.644181	65.865447
1477.067236	64.635933	65.870452
1477.077148	61.401479	65.875457
1476.145182	57.999730	65.880462
1475.159778	70.754738	65.885466
1474.979051	62.193580	65.890471
1474.137668	68.027995	65.895476
1473.215359	63.110811	65.900481
1472.636617	63.660033	65.905486
1471.760987	55.964682	65.910490
1471.474755	62.053079	65.915495
1470.543935	70.057439	65.920500
1469.637989	54.092497	65.925505
1468.591476	54.181461	65.930510
1468.333048	62.400667	65.935514
1468.310094	53.495893	65.940519
1467.611807	62.571912	65.945524
1467.431484	58.399426	65.950529
1466.344359	60.216905	65.955534
1465.733060	61.526675	65.960538
1464.781380	56.322423	65.965543
1463.434554	52.808410	65.970548
1462.926185	57.720988	65.975553
1462.646612	59.354939	65.980558
1462.164239	66.636742	65.985562
1461.748621	58.153918	65.990567
1460.679461	60.238207	65.995572
1459.619730	53.032598	66.000577
1459.256971	54.832736	66.005582
1458.785338	61.437883	66.010586
1458.508060	53.999115	66.015591
1457.552206	62.669783	66.020596
1456.657200	53.315384	66.025601
1455.981503	51.306391	66.030606
1455.172115	61.177517	66.035610
1454.696754	55.380324	66.040615
1454.231416	61.817311	66.045620
1453.729998	62.478831	66.050625
1452.817221	58.897419	66.055630
1451.842521	53.807220	66.060634
1451.846987	55.706697	66.065639
1450.807869	56.627137	66.070644
1449.580212	54.087689	66.075649
1449.403934	56.283976	66.080654
1448.877750	57.105553	66.085658
1448.363854	55.515555	66.090663
1447.731321	52.348510	66.095668
1447.051558	57.810309	66.100673
1446.536135	61.035068	66.105678
1445.703296	61.030157	66.110682
1445.136378	58.164926	66.115687
1443.979527	63.070180	66.120692
1443.246884	50.228517	66.125697
1442.893007	51.719735	66.130702
1442.038639	56.327752	66.135706
1441.923968	56.790613	66.140711
1441.055772	56.187341	66.145716
1440.121783	61.814126	66.150721
1439.532105	65.427586	66.155726
1439.035866	56.449795	66.160730
1438.584380	58.800210	66.165735
1437.191416	60.765656	66.170740
1436.630949	55.030879	66.175745
1436.436674	51.496138	66.180750
1435.925329	62.307089	66.185754
1435.227191	55.818319	66.190759
1434.254994	64.564134	66.195764
1433.820298	63.928239	66.200769
1433.338815	61.907308	66.205774
1432.248921	59.588827	66.210778
1431.477767	54.100429	66.215783
1430.728091	60.311368	66.220788
1430.202214	58.903053	66.225793
1429.983834	63.244416	66.230798
1428.960267	62.650071	66.235802
1428.250320	61.021848	66.240807
1427.771794	58.287655	66.245812
1427.222653	55.384910	66.250817
1426.384008	60.608609	66.255822
1425.305176	69.647348	66.260826
1424.674743	58.470501	66.265831
1424.150614	67.531467	66.270836
1423.902160	70.726418	66.275841
1423.442385	60.162701	66.280846
1422.835563	68.672252	66.285850
1421.609646	62.615878	66.290855
1420.982496	67.670347	66.295860
1420.475170	60.015829	66.300865
1420.198398	50.678309	66.305870
1419.028076	63.215129	66.310874
1418.199993	63.723566	66.315879
1417.331749	62.166238	66.320884
1417.202156	55.364759	66.325889
1416.861520	59.941597	66.330894
1415.490769	64.705814	66.335898
1414.913201	58.846025	66.340903
1414.401870	68.504210	66.345908
1413.853234	62.423775	66.350913
1413.632459	59.839433	66.355918
1412.624088	60.072170	66.360922
1411.665362	56.113296	66.365927
1410.898200	58.450808	66.370932
1410.318602	61.923897	66.375937
1410.063326	56.178468	66.380942
1409.342162	65.458411	66.385946
1408.604194	62.204052	66.390951
1407.839344	61.685292	66.395956
1407.085864	66.371906	66.400961
1407.018894	60.013066	66.405966
1405.991164	65.974888	66.410970
1405.041428	63.413365	66.415975
1404.297269	61.475192	66.420980
1403.949072	61.358572	66.425985
1403.760409	56.864139	66.430990
1402.112710	69.055791	66.435994
1401.382914	65.311271	66.440999
1400.845843	63.586192	66.446004
1400.629822	58.813828	66.451009
1400.087453	59.514983	66.456014
1399.418057	55.216810	66.461018
1399.556975	55.224621	66.466023
1398.264334	63.981953	66.471028
1397.457899	63.018790	66.476033
1396.596676	56.620610	66.481038
1395.708841	67.504025	66.486042
1395.772071	60.096301	66.491047
1394.541119	61.397343	66.496052
1394.262001	60.675225	66.501057
1393.420373	57.631316	66.506062
1392.437856	59.394350	66.511066
1392.021936	52.926972	66.516071
1391.476345	61.049894	66.521076
1391.194860	64.544990	66.526081
1390.162282	54.979093	66.531086
1389.453862	61.918356	66.536090
1389.320538	60.185877	66.541095
1388.073561	60.314621	66.546100
1387.219528	50.583152	66.551105
1386.720720	52.005948	66.556110
1385.981079	57.070416	66.561114
1385.964358	51.203496	66.566119
1384.432431	63.315248	66.571124
1383.911568	62.666249	66.576129
1383.708211	56.808492	66.581134
1382.969424	59.355971	66.586138
1382.372737	54.636232	66.591143
1380.955089	51.857354	66.596148
1380.362538	50.849162	66.601153
1380.082205	47.649810	66.606158
1379.588635	59.858293	66.611162
1379.326493	57.750470	66.616167
1378.019550	56.690248	66.621172
1377.466540	64.301835	66.626177
1377.051074	63.440540	66.631182
1376.414959	68.673064	66.636186
1375.731162	55.847317	66.641191
1374.814092	68.247704	66.646196
1374.128691	67.828291	66.651201
1373.830250	64.680701	66.656206
1372.632573	55.089015	66.661210
1371.842761	48.465029	66.666215
1371.382715	56.631124	66.671220
1370.599929	66.775591	66.676225
1370.554893	56.481865	66.681230
1369.894990	54.828358	66.686234
1368.979490	56.809409	66.691239
1368.038296	58.496497	66.696244
1367.365381	58.513500	66.701249
1367.194935	52.648939	66.706254
1366.607626	54.372816	66.711258
1365.811964	56.662831	66.716263
1364.683438	51.384230	66.721268
1364.333618	60.723424	66.726273
1363.790778	57.363946	66.731278
1362.764120	56.568267	66.736282
1362.097842	55.909271	66.741287
1361.253658	58.892984	66.746292
1360.990478	62.768378	66.751297
1360.872176	54.507985	66.756302
1359.966986	63.996963	66.761306
1358.805672	56.157834	66.766311
1358.258015	60.128910	66.771316
1357.709394	64.940669	66.776321
1357.540686	51.477959	66.781326
1356.269227	57.986324	66.786330
1355.491030	45.110943	66.791335
1355.134406	56.075501	66.796340
1354.769401	56.698007	66.801345
1353.860246	42.985572	66.806350
1352.702495	67.808210	66.811354
1352.468091	54.261323	66.816359
1351.803390	61.871742	66.821364
1351.161978	55.372407	66.826369
1350.172081	57.549797	66.831374
1349.450007	62.436438	66.836378
1349.051150	50.856955	66.841383
1348.412591	48.772703	66.846388
1348.075072	54.478164	66.851393
1347.637960	51.672750	66.856398
1346.311443	58.918435	66.861402
1345.742638	50.171410	66.866407
1345.303050	59.846576	66.871412
1344.666766	53.717018	66.876417
1343.810962	51.426023	66.881422
1343.000488	59.539016	66.886426
1343.008088	53.570460	66.891431
1341.830358	59.605032	66.896436
1340.844056	62.037325	66.901441
1340.698250	55.003463	66.906446
1339.866121	63.575648	66.911450
1339.510883	54.439853	66.916455
1338.396323	54.468722	66.921460
1337.266970	50.150645	66.926465
1337.194210	59.466297	66.931470
1336.484670	56.046592	66.936474
1336.258084	57.468702	66.941479
1335.643386	57.298261	66.946484
1334.515417	61.501943	66.951489
1334.314931	54.514622	66.956494
1333.487188	68.950887	66.961498
1332.912090	59.231866	66.966503
1331.630406	54.168443	66.971508
1331.141011	54.075856	66.976513
1330.639361	49.516070	66.981518
1330.094254	57.881775	66.986522
1328.806448	51.548284	66.991527
1328.120451	54.856948	66.996532
1327.743914	63.719415	67.001537
1327.439823	53.714463	67.006542
1326.817022	55.918661	67.011546
1326.470873	56.721103	67.016551
1325.440031	63.916642	67.021556
1324.528203	61.390127	67.026561
1324.470536	55.939732	67.031566
1323.280205	57.018303	67.036570
1322.679695	52.247150	67.041575
1322.396668	57.660096	67.046580
1321.095641	62.126264	67.051585
1320.855767	58.193500	67.056590
1319.686629	60.203851	67.061594
1319.032978	51.924491	67.066599
1318.676266	53.196975	67.071604
1318.149044	60.679887	67.076609
1318.090607	50.173834	67.081614
1316.891583	52.676221	67.086618
1316.186137	53.168348	67.091623
1315.812494	50.843290	67.096628
1314.379435	52.498201	67.101633
1313.497231	48.773213	67.106638
1312.892406	56.826710	67.111642
1313.035286	53.815556	67.116647
1312.249110	60.861813	67.121652
1311.340139	57.869641	67.126657
1311.537025	54.580239	67.131662
1310.116700	57.549902	67.136666
1309.693699	51.596187	67.141671
1309.069966	49.104305	67.146676
1307.984825	53.477808	67.151681
1307.332273	50.463798	67.156686
1306.216121	57.021611	67.161690
1305.916938	55.214580	67.166695
1305.558802	58.070576	67.171700
1305.311190	51.584346	67.176705
1304.615839	58.034261	67.181710
1303.423186	56.657860	67.186714
1303.312811	57.003347	67.191719
1302.512002	52.688249	67.196724
1301.042405	71.935412	67.201729
1300.535331	58.949130	67.206734
1299.850288	65.375332	67.211738
1299.560048	73.694223	67.216743
1299.250264	63.694907	67.221748
1298.406923	65.342808	67.226753
1297.570447	59.087391	67.231758
1296.662887	62.193166	67.236762
1296.524987	60.679043	67.241767
1295.962095	60.084054	67.246772
1294.768948	62.055655	67.251777
1294.318013	58.659505	67.256782
1293.615030	64.926132	67.261786
1293.474895	58.711401	67.266791
1292.623125	62.601525	67.271796
1291.986651	65.832940	67.276801
1291.239888	63.756441	67.281806
1290.029946	61.359337	67.286810
1289.375054	68.239649	67.291815
1288.704209	61.950017	67.296820
1287.915370	64.521249	67.301825
1288.098416	52.275249	67.306830
1287.411068	64.153422	67.311834
1286.551120	61.194466	67.316839
1285.627714	53.558832	67.321844
1284.990624	72.088586	67.326849
1284.961734	56.671861	67.331854
1283.561189	68.042098	67.336858
1282.730303	66.519879	67.341863
1282.551532	55.998264	67.346868
1281.856901	58.411014	67.351873
1281.475360	63.833319	67.356878
1280.061122	63.637042	67.361882
1279.503653	59.903014	67.366887
1279.098091	64.387684	67.371892
1278.589446	59.502586	67.376897
1278.193248	62.251095	67.381902
1276.881774	67.597320	67.386906
1276.407294	59.505530	67.391911
1276.353012	60.160648	67.396916
1275.348261	65.716733	67.401921
1274.523618	56.053178	67.406926
1273.434620	67.291883	67.411930
1273.370601	49.715565	67.416935
1272.680658	61.898507	67.421940
1271.472519	64.476483	67.426945
1271.225310	58.715600	67.431950
1270.769321	63.090016	67.436954
1270.009187	63.393729	67.441959
1269.273711	61.816921	67.446964
1268.075720	64.000618	67.451969
1267.803933	53.790268	67.456974
1267.464087	65.797700	67.461978
1266.925881	54.112659	67.466983
1265.447697	58.296354	67.471988
1264.401251	56.819453	67.476993
1264.075689	55.286285	67.481998
1263.747196	57.573015	67.487002
1263.385114	55.988882	67.492007
1263.156257	54.804620	67.497012
1262.128304	60.183043	67.502017
1261.660392	61.507909	67.507022
1260.620179	60.586691	67.512026
1260.344814	53.953491	67.517031
1259.271228	61.294619	67.522036
1258.349419	57.110739	67.527041
1258.062221	57.834430	67.532046
1257.445810	61.395403	67.537050
1256.949317	61.242457	67.542055
1255.706982	56.095547	67.547060
1255.236512	58.838520	67.552065
1254.983587	51.203529	67.557070
1254.112921	62.293980	67.562074
1252.670694	53.267957	67.567079
1252.030579	61.666126	67.572084
1251.629081	61.354573	67.577089
1251.620954	58.674936	67.582094
1251.274101	61.443988	67.587098
1250.320131	52.553226	67.592103
1249.518411	65.006261	67.597108
1248.691984	60.143313	67.602113
1248.229495	57.050212	67.607118
1247.445527	63.159411	67.612122
1246.538772	59.928789	67.617127
1245.863392	55.220024	67.622132
1245.341345	63.977896	67.627137
1245.291542	60.353970	67.632142
1244.331621	63.652593	67.637146
1243.308659	61.052315	67.642151
1242.862451	55.097573	67.647156
1242.620290	57.943020	67.652161
1241.634155	66.142318	67.657166
1240.639469	61.796565	67.662170
1240.427428	58.212629	67.667175
1239.937955	55.601645	67.672180
1238.153252	56.729030	67.677185
1238.042697	57.424636	67.682190
1237.246759	64.333690	67.687194
1237.093948	58.122559	67.692199
1236.539283	57.863747	67.697204
1235.345543	50.912950	67.702209
1234.767813	55.123796	67.707214
1234.135823	56.309173	67.712218
1233.886214	58.641711	67.717223
1232.967368	50.218466	67.722228
1231.833245	56.268224	67.727233
1231.373395	51.750702	67.732238
1231.123716	54.195216	67.737242
1230.608965	48.869552	67.742247
1229.468789	53.541997	67.747252
1228.348081	64.194390	67.752257
1228.133435	54.629407	67.757262
1227.662933	55.071584	67.762266
1227.227590	56.370776	67.767271
1226.077976	57.341991	67.772276
1225.221246	55.670935	67.777281
1224.823725	58.159459	67.782286
1224.327029	58.487529	67.787290
1224.246413	53.654236	67.792295
1223.488823	51.726141	67.797300
1222.458044	58.089057	67.802305
1222.281744	51.408574	67.807310
1220.888705	47.361145	67.812314
1219.975467	51.723115	67.817319
1219.610878	59.705310	67.822324
1218.953499	63.378463	67.827329
1218.490397	53.275817	67.832334
1217.602411	54.861454	67.837338
1216.650730	57.157396	67.842343
1216.369556	60.701340	67.847348
1215.796056	57.998065	67.852353
1215.372932	52.038083	67.857358
1213.984439	62.356164	67.862362
1213.336344	56.979164	67.867367
1213.263678	60.018438	67.872372
1212.610387	47.588464	67.877377
1212.292931	50.128913	67.882382
1211.423032	55.472757	67.887386
1210.461651	57.598354	67.892391
1209.978248	54.658401	67.897396
1208.599483	62.137962	67.902401
1208.274679	55.296587	67.907406
1207.407699	56.877310	67.912410
1207.134568	72.524834	67.917415
1206.731469	61.767661	67.922420
1205.944933	59.672283	67.927425
1205.099235	60.754453	67.932430
1204.580077	56.653226	67.937434
1204.171400	56.226126	67.942439
1202.980659	56.965767	67.947444
1202.094220	58.842904	67.952449
1201.883605	51.940795	67.957454
1201.122577	55.403348	67.962458
1200.831776	47.454266	67.967463
1200.142374	54.370038	67.972468
1198.870964	54.844962	67.977473
1198.451014	48.507584	67.982478
1197.882319	49.829562	67.987482
1197.499623	52.364618	67.992487
1196.742651	49.717333	67.997492
1195.940152	55.097773	68.002497
1195.858391	52.026144	68.007502
1194.648522	58.217273	68.012506
1193.770756	55.740587	68.017511
1193.198267	50.400459	68.022516
1192.750253	57.374042	68.027521
1191.773913	56.232959	68.032526
1190.739959	65.887538	68.037530
1190.111875	57.720850	68.042535
1189.743554	54.679020	68.047540
1189.024586	61.066482	68.052545
1189.136744	57.766893	68.057550
1188.662581	57.108932	68.062554
1187.343955	58.994877	68.067559
1187.066747	52.885539	68.072564
1185.876445	61.263977	68.077569
1184.961404	56.260602	68.082574
1184.610641	57.734009	68.087578
1184.047997	56.192822	68.092583
1183.711800	53.016574	68.097588
1182.802295	62.659248	68.102593
1182.015821	55.072847	68.107598
1181.188476	60.908258	68.112602
1180.676462	57.931859	68.117607
1180.554539	49.175322	68.122612
1179.064818	61.007640	68.127617
1178.706976	45.242708	68.132622
1177.725038	54.595695	68.137626
1177.452242	51.781531	68.142631
1177.284799	40.474390	68.147636
1176.051565	56.807595	68.152641
1175.475090	45.177563	68.157646
1174.839675	49.465402	68.162650
1173.799276	60.988143	68.167655
1173.080586	52.149889	68.172660
1172.474987	51.703648	68.177665
1172.057902	57.314541	68.182670
1171.425574	58.813805	68.187674
1171.154469	55.944178	68.192679
1170.418760	59.230823	68.197684
1169.228305	62.455745	68.202689
1168.911577	52.845506	68.207694
1168.433126	50.702723	68.212698
1167.677635	52.888633	68.217703
1166.684077	53.221613	68.222708
1165.724880	66.800435	68.227713
1165.592426	57.230276	68.232718
1165.101628	58.263903	68.237722
1164.475439	59.216559	68.242727
1163.703929	50.257398	68.247732
1162.925408	59.390382	68.252737
1162.469194	59.033928	68.257742
1161.081453	58.425067	68.262746
1160.482379	58.119718	68.267751
1160.191824	56.768657	68.272756
1159.567137	59.208160	68.277761
1159.248172	54.264543	68.282766
1158.228371	59.003031	68.287770
1157.318389	53.445346	68.292775
1156.829460	52.313494	68.297780
1156.207020	58.212519	68.302785
1155.913376	54.714113	68.307790
1154.722761	58.987752	68.312794
1154.110803	55.235614	68.317799
1153.459914	57.619361	68.322804
1153.024493	69.954237	68.327809
1152.795515	59.275047	68.332814
1151.535855	56.272478	68.337818
1151.062453	57.140913	68.342823
1150.460471	56.952725	68.347828
1149.784990	61.800461	68.352833
1149.161520	56.247675	68.357838
1148.601171	56.417147	68.362842
1148.260585	57.532545	68.367847
1147.237284	53.391661	68.372852
1145.961589	53.619708	68.377857
1145.796633	52.904695	68.382862
1145.098473	54.217312	68.387866
1144.486556	59.173213	68.392871
1143.788176	52.746085	68.397876
1142.760552	63.287505	68.402881
1142.477888	59.361571	68.407886
1142.029448	59.139503	68.412890
1140.720159	60.595050	68.417895
1140.251599	54.181834	68.422900
1139.367393	58.245897	68.427905
1139.093249	52.612326	68.432910
1138.739093	63.753121	68.437914
1138.040511	60.782749	68.442919
1136.981462	54.960194	68.447924
1136.136268	64.608422	68.452929
1136.177141	60.444949	68.457934
1135.392911	62.290083	68.462938
1134.460608	54.092951	68.467943
1133.904917	65.325725	68.472948
1133.396136	62.686294	68.477953
1132.227919	54.449412	68.482958
1131.342778	63.115233	68.487962
1130.731928	55.974010	68.492967
1130.279109	58.091291	68.497972
1129.771918	62.388712	68.502977
1129.789335	57.700685	68.507982
1128.974206	57.921721	68.512986
1127.695147	62.252018	68.517991
1127.459926	54.257838	68.522996
1126.589252	65.294702	68.528001
1125.532483	56.147531	68.533006
1124.907762	62.602020	68.538010
1123.971101	60.491121	68.543015
1124.234457	59.924031	68.548020
1123.658397	56.073151	68.553025
1123.169123	58.126844	68.558030
1121.929346	54.619651	68.563034
1121.299503	57.668694	68.568039
1120.655467	57.356313	68.573044
1119.641178	58.517366	68.578049
1119.006226	51.912999	68.583054
1118.906804	60.748745	68.588058
1118.344665	59.461386	68.593063
1117.551268	60.426455	68.598068
1116.482575	64.475714	68.603073
1116.127393	46.169874	68.608078
1115.443420	56.049505	68.613082
1114.328204	59.120555	68.618087
1113.927409	65.175150	68.623092
1112.999051	59.298702	68.628097
1112.624599	60.879967	68.633102
1112.296657	64.104924	68.638106
1111.732753	66.774472	68.643111
1111.172512	59.546356	68.648116
1110.282870	55.338497	68.653121
1109.419466	56.141236	68.658126
1108.680016	59.986739	68.663130
1107.805217	52.583153	68.668135
1107.592936	49.045006	68.673140
1106.622503	51.657786	68.678145
1105.926215	55.400229	68.683150
1104.883077	50.079791	68.688154
1104.294307	50.685883	68.693159
1104.277944	56.149467	68.698164
1104.022173	55.729602	68.703169
1102.823473	58.618391	68.708174
1102.294564	58.051157	68.713178
1101.701412	57.855268	68.718183
1101.324871	52.078716	68.723188
1099.702446	61.109399	68.728193
1099.233562	51.043980	68.733198
1098.913929	55.401457	68.738202
1097.926158	56.400603	68.743207
1097.892942	49.482911	68.748212
1096.826671	56.304105	68.753217
1096.019035	49.810793	68.758222
1095.734507	45.744816	68.763226
1094.846793	61.139988	68.768231
1094.063851	52.058092	68.773236
1093.106193	50.994502	68.778241
1093.137256	46.758477	68.783246
1092.698941	52.566721	68.788250
1091.498494	55.761725	68.793255
1090.948166	54.770541	68.798260
1089.925528	62.688680	68.803265
1089.353738	55.687917	68.808270
1089.168996	53.353351	68.813274
1088.125565	53.637523	68.818279
1087.218865	45.661852	68.823284
1086.463787	56.580983	68.828289
1086.467859	55.323417	68.833294
1085.926012	55.185604	68.838298
1084.977901	64.602630	68.843303
1084.200162	49.585765	68.848308
1083.324795	56.326135	68.853313
1083.076033	62.747637	68.858318
1082.793095	61.904736	68.863322
1081.710919	62.542008	68.868327
1080.973652	51.492676	68.873332
1080.265254	45.806766	68.878337
1079.943247	43.881972	68.883342
1078.959564	53.806127	68.888346
1078.216755	55.524837	68.893351
1078.055827	53.799926	68.898356
1076.699761	61.151356	68.903361
1076.051019	50.255104	68.908366
1075.254426	53.937814	68.913370
1074.412901	62.934183	68.918375
1074.475782	55.231642	68.923380
1074.293793	56.213009	68.928385
1073.524128	53.913140	68.933390
1072.665180	59.493405	68.938394
1071.762656	57.769763	68.943399
1071.273402	49.502188	68.948404
1070.024704	51.504801	68.953409
1069.558993	51.698660	68.958414
1068.890893	58.376101	68.963418
1068.564167	51.833110	68.968423
1068.506487	42.840868	68.973428
1067.213102	53.549158	68.978433
1066.345716	55.814397	68.983438
1065.981436	53.357004	68.988442
1064.559141	54.961452	68.993447
1064.132070	48.218380	68.998452
1062.926612	53.781226	69.003457
1062.920531	52.992059	69.008462
1062.779814	54.851543	69.013466
1062.088440	48.368137	69.018471
1062.115059	47.127486	69.023476
1060.650252	59.761724	69.028481
1060.143342	51.582116	69.033486
1059.240394	48.138072	69.038490
1057.999117	51.487820	69.043495
1057.606953	47.811136	69.048500
1056.848826	50.539972	69.053505
1056.596920	61.172486	69.058510
1056.361525	55.488609	69.063514
1055.190925	54.321711	69.068519
1054.817825	45.385953	69.073524
1054.109240	51.369660	69.078529
1053.238725	55.390568	69.083534
1052.444506	50.700771	69.088538
1051.538179	63.635687	69.093543
1051.557774	43.828902	69.098548
1050.934347	56.272526	69.103553
1049.838470	50.078978	69.108558
1049.005072	54.447224	69.113562
1048.327578	55.620959	69.118567
1048.190677	53.583142	69.123572
1047.731299	51.126688	69.128577
1046.234653	53.818467	69.133582
1045.699710	42.833166	69.138586
1045.102623	48.959988	69.143591
1045.163000	42.546238	69.148596
1044.130729	50.650423	69.153601
1043.190794	46.859029	69.158606
1042.807803	49.853048	69.163610
1042.295594	52.287298	69.168615
1041.783602	51.908200	69.173620
1040.705798	53.233929	69.178625
1040.005630	43.465526	69.183630
1039.816346	49.976912	69.188634
1038.520291	50.837462	69.193639
1037.770033	51.119172	69.198644
1037.043120	56.419818	69.203649
1036.651254	51.760636	69.208654
1036.578304	46.044616	69.213658
1035.539663	53.952697	69.218663
1034.808176	45.077112	69.223668
1034.059819	48.720619	69.228673
1033.381518	53.091004	69.233678
1032.560578	45.565344	69.238682
1031.856304	56.990494	69.243687
1031.481936	47.586582	69.248692
1031.002102	43.898619	69.253697
1030.437021	43.874902	69.258702
1029.285115	41.426121	69.263706
1028.216217	59.225042	69.268711
1027.980657	46.408562	69.273716
1027.643583	56.311869	69.278721
1027.181631	55.992622	69.283726
1026.324922	53.015903	69.288730
1025.645197	58.356355	69.293735
1025.277608	46.163283	69.298740
1023.989821	50.852984	69.303745
1023.143175	40.735727	69.308750
1022.621977	46.334810	69.313754
1022.205791	53.114109	69.318759
1021.895021	48.033595	69.323764
1020.245912	56.631742	69.328769
1019.858132	47.095924	69.333774
1019.301336	48.874944	69.338778
1018.724821	51.956525	69.343783
1019.136627	42.361314	69.348788
1017.971961	44.476740	69.353793
1016.742827	54.206570	69.358798
1016.311010	50.528316	69.363802
1015.704701	51.556692	69.368807
1015.087595	50.312796	69.373812
1014.090176	55.640713	69.378817
1013.476295	48.277662	69.383822
1013.135369	52.264791	69.388826
1012.371140	50.935491	69.393831
1011.824106	36.725649	69.398836
1010.626224	45.154236	69.403841
1010.571665	43.275213	69.408846
1010.140819	42.501585	69.413850
1009.214284	52.299971	69.418855
1008.646958	48.976019	69.423860
1007.767885	41.541621	69.428865
1006.740552	48.167411	69.433870
1006.177300	51.731014	69.438874
1005.499900	51.832406	69.443879
1005.579725	50.094430	69.448884
1004.287350	51.449581	69.453889
1003.403206	54.223712	69.458894
1003.007054	44.400647	69.463898
1002.246533	49.337635	69.468903
1002.177311	42.969738	69.473908
1000.966971	45.552912	69.478913
1000.312296	39.211928	69.483918
999.788598	43.136670	69.488922
999.012413	45.745391	69.493927
998.432967	40.970983	69.498932
997.373650	48.953327	69.503937
997.005727	47.318127	69.508942
996.468407	44.571307	69.513946
995.751737	54.552353	69.518951
995.661234	49.376874	69.523956
994.282161	53.655331	69.528961
993.767071	58.857632	69.533966
993.307799	54.647580	69.538970
992.453374	52.250835	69.543975
991.795672	46.209957	69.548980
990.998957	47.071511	69.553985
990.462774	53.194961	69.558990
990.346242	52.059089	69.563994
989.365079	47.928920	69.568999
988.314230	47.533063	69.574004
987.908105	42.325801	69.579009
987.321166	40.898916	69.584014
986.464809	45.212482	69.589018
985.738258	55.335453	69.594023
985.315761	45.753128	69.599028
984.924378	51.762077	69.604033
983.369167	47.934558	69.609038
982.638411	48.304645	69.614042
982.094790	53.945151	69.619047
982.065860	44.306518	69.624052
981.507708	43.397030	69.629057
980.899366	35.933765	69.634062
980.015438	39.226690	69.639066
978.953542	47.600537	69.644071
978.817595	41.115525	69.649076
978.080352	43.896252	69.654081
977.012945	39.525921	69.659086
976.184667	34.926732	69.664090
975.482690	47.023306	69.669095
975.582070	36.746092	69.674100
974.952118	43.433245	69.679105
974.182848	49.434508	69.684110
973.428483	47.143277	69.689114
972.772337	43.849237	69.694119
972.274838	37.423330	69.699124
971.332533	43.545164	69.704129
970.611743	42.571669	69.709134
970.578305	45.976861	69.714138
969.105722	55.064194	69.719143
968.673625	43.960051	69.724148
967.769002	50.779222	69.729153
967.353599	41.090120	69.734158
967.123134	39.966069	69.739162
965.714051	51.014508	69.744167
964.904877	43.654162	69.749172
964.505614	51.130946	69.754177
964.242209	44.653598	69.759182
963.913745	41.739513	69.764186
962.922990	51.802020	69.769191
962.427996	45.359944	69.774196
961.394615	53.577874	69.779201
960.995539	52.714043	69.784206
959.974112	44.077011	69.789210
959.009674	57.156806	69.794215
958.609754	47.645013	69.799220
958.181275	50.359271	69.804225
957.845585	48.477673	69.809230
956.986000	46.775629	69.814234
956.102457	49.712107	69.819239
955.654041	41.040675	69.824244
954.908272	44.505592	69.829249
953.849216	50.105111	69.834254
953.666514	44.952193	69.839258
952.703351	40.019655	69.844263
952.359400	48.812291	69.849268
951.329409	48.901990	69.854273
950.491326	54.422197	69.859278
950.129386	47.012771	69.864282
949.542662	51.089479	69.869287
949.370686	51.427435	69.874292
947.842641	54.228345	69.879297
947.094167	57.507616	69.884302
946.766974	49.624300	69.889306
945.923580	53.297146	69.894311
946.097884	44.960294	69.899316
945.439135	52.014740	69.904321
944.724950	46.203640	69.909326
944.091145	42.794089	69.914330
942.634283	49.592327	69.919335
942.165850	45.858416	69.924340
941.297356	49.107897	69.929345
941.170878	49.444922	69.934350
940.768528	43.073267	69.939354
939.153162	51.038453	69.944359
938.746577	43.640866	69.949364
938.355656	48.523789	69.954369
937.906519	53.449094	69.959374
937.208529	44.889917	69.964378
936.139247	46.938161	69.969383
936.067377	39.047343	69.974388
935.368019	49.339457	69.979393
933.928078	50.505233	69.984398
933.267542	49.798130	69.989402
932.180859	54.044285	69.994407
932.221463	45.235117	69.999412
932.110430	48.258414	70.004417
931.220151	47.980534	70.009422
931.066624	40.886462	70.014426
929.825641	55.439000	70.019431
929.620939	48.278950	70.024436
928.425041	49.174081	70.029441
927.001523	51.020074	70.034446
927.133666	46.928821	70.039450
926.560139	49.779707	70.044455
926.114213	45.551780	70.049460
925.087280	43.162011	70.054465
924.380617	42.875416	70.059470
924.190431	38.567373	70.064474
923.053849	45.888670	70.069479
922.157242	39.143081	70.074484
921.442087	48.021595	70.079489
921.355205	50.471764	70.084494
921.126846	44.408320	70.089498
919.671122	53.570265	70.094503
918.762980	44.470521	70.099508
918.197519	46.326634	70.104513
917.920415	47.703196	70.109518
917.644136	44.105871	70.114522
916.417707	54.168049	70.119527
916.013259	46.738586	70.124532
915.408645	53.927929	70.129537
914.665941	49.968005	70.134542
913.734751	47.283882	70.139546
912.951188	59.929626	70.144551
912.650694	45.857202	70.149556
912.268369	45.895893	70.154561
911.429542	54.759399	70.159566
910.428167	54.158580	70.164570
909.681439	60.061658	70.169575
909.433530	55.095739	70.174580
908.805689	56.548617	70.179585
907.811773	57.712817	70.184590
907.381958	53.993266	70.189594
906.643414	54.970170	70.194599
905.876029	46.887253	70.199604
904.843100	57.533661	70.204609
904.271126	60.653968	70.209614
904.139142	55.106624	70.214618
903.357351	57.698919	70.219623
903.017487	51.169090	70.224628
902.204875	48.948653	70.229633
901.178666	66.214110	70.234638
900.802844	55.205103	70.239642
900.141430	59.169128	70.244647
899.213001	54.309930	70.249652
898.770584	54.208374	70.254657
897.909314	57.472491	70.259662
897.583449	50.235531	70.264666
896.423551	54.105417	70.269671
895.595290	54.550971	70.274676
895.393736	56.355486	70.279681
894.698020	60.812255	70.284686
894.144258	56.264022	70.289690
893.894616	55.206109	70.294695
892.674304	50.729259	70.299700
892.095807	55.738235	70.304705
891.750023	54.496924	70.309710
890.751652	48.317901	70.314714
889.627958	57.004396	70.319719
889.532882	55.139709	70.324724
889.303682	49.811269	70.329729
888.189811	47.976250	70.334734
887.303139	52.587988	70.339738
886.381434	54.428262	70.344743
886.202584	47.918546	70.349748
885.620222	48.894255	70.354753
884.824068	59.132402	70.359758
884.186667	49.169561	70.364762
883.458007	49.011059	70.369767
882.954724	44.385412	70.374772
881.995737	55.589344	70.379777
881.154259	53.846597	70.384782
880.952896	47.944444	70.389786
880.239508	53.220895	70.394791
879.886860	44.425430	70.399796
878.905977	47.254420	70.404801
878.088699	54.799314	70.409806
877.583306	40.366848	70.414810
877.174188	47.633892	70.419815
876.438255	41.171837	70.424820
875.393244	42.525531	70.429825
874.507436	54.017440	70.434830
874.256178	49.876816	70.439834
873.935244	47.664872	70.444839
872.918450	46.632857	70.449844
871.983063	51.350124	70.454849
871.477352	50.467008	70.459854
871.426065	44.954139	70.464858
870.244904	47.237836	70.469863
869.530617	46.510919	70.474868
869.399468	52.159914	70.479873
868.528108	47.405191	70.484878
867.449904	50.114055	70.489882
866.599500	57.064978	70.494887
866.346809	43.946910	70.499892
866.129076	46.124588	70.504897
865.154910	49.472913	70.509902
864.269847	45.661822	70.514906
863.388692	57.036300	70.519911
862.941547	46.273629	70.524916
862.407045	43.141613	70.529921
861.558121	52.861453	70.534926
860.855721	50.946767	70.539930
860.368595	57.335246	70.544935
860.175153	48.785683	70.549940
858.902173	58.159851	70.554945
857.996612	54.438756	70.559950
857.982222	53.843304	70.564954
857.468786	62.878970	70.569959
856.757870	59.005468	70.574964
855.578998	57.388969	70.579969
854.923288	54.274666	70.584974
854.669075	55.906214	70.589978
853.708843	55.016593	70.594983
852.802742	54.026893	70.599988
852.559461	45.926816	70.604993
851.678802	57.282295	70.609998
851.400713	47.319051	70.615002
850.455121	53.444603	70.620007
849.601809	49.445535	70.625012
849.089789	53.901461	70.630017
848.497549	57.048657	70.635022
848.167515	54.443923	70.640026
846.920778	57.726828	70.645031
846.712681	53.416909	70.650036
846.202133	58.139110	70.655041
845.109313	54.093005	70.660046
844.014558	50.509262	70.665050
843.333857	54.320248	70.670055
843.078232	46.334103	70.675060
843.071208	47.609338	70.680065
842.503906	40.931220	70.685070
841.342955	49.571617	70.690074
840.376159	51.941059	70.695079
840.073626	52.370765	70.700084
839.326543	46.970217	70.705089
838.141207	54.128997	70.710094
837.930257	46.717642	70.715098
837.296339	44.214896	70.720103
836.835765	50.206484	70.725108
836.100883	50.542576	70.730113
835.111586	47.352064	70.735118
834.744604	39.976586	70.740122
833.877706	46.781903	70.745127
833.417904	47.897390	70.750132
832.282811	55.317837	70.755137
831.508826	59.720844	70.760142
831.713106	49.805408	70.765146
830.889953	56.742541	70.770151
830.067375	55.991870	70.775156
829.390956	52.175968	70.780161
828.692764	52.197137	70.785166
828.374742	53.178094	70.790170
827.199340	54.112588	70.795175
826.366341	44.988310	70.800180
826.107103	50.589882	70.805185
825.797054	50.665969	70.810190
824.914853	46.621046	70.815194
824.086726	51.849539	70.820199
823.729462	50.266288	70.825204
823.072308	51.428958	70.830209
821.834013	53.426878	70.835214
821.213340	55.783814	70.840218
820.620298	51.017926	70.845223
820.564927	49.243119	70.850228
819.187376	55.070003	70.855233
818.131167	54.807535	70.860238
817.867204	44.637047	70.865242
817.374378	50.583308	70.870247
816.955147	52.966528	70.875252
816.725134	50.293840	70.880257
815.587701	49.678446	70.885262
814.867431	45.415364	70.890266
814.351600	58.318132	70.895271
813.587757	47.504958	70.900276
812.377513	53.033976	70.905281
811.677958	52.766782	70.910286
811.708654	47.138364	70.915290
811.105798	60.406650	70.920295
810.125424	53.272310	70.925300
809.474057	63.132612	70.930305
808.731197	57.786593	70.935310
808.499796	55.377479	70.940314
807.170433	56.604573	70.945319
806.608227	52.973926	70.950324
806.038761	56.623712	70.955329
805.394654	60.476193	70.960334
805.237775	43.789983	70.965338
804.798163	53.536148	70.970343
803.392547	55.598558	70.975348
803.319891	47.767800	70.980353
802.251265	54.097456	70.985358
801.427120	50.394964	70.990362
800.257394	57.959710	70.995367
800.004123	49.009670	71.000372
800.026663	50.773789	71.005377
799.568801	54.080955	71.010382
798.581353	48.483714	71.015386
797.595389	48.093379	71.020391
797.026994	52.036310	71.025396
796.336950	54.224520	71.030401
794.903693	53.638877	71.035406
794.826306	43.060224	71.040410
794.342427	49.837701	71.045415
793.987923	48.531561	71.050420
793.221387	50.653098	71.055425
792.066289	50.423730	71.060430
791.558049	46.989504	71.065434
790.876642	52.877477	71.070439
790.692493	49.625053	71.075444
789.784418	51.009024	71.080449
788.735136	49.272581	71.085454
788.564476	48.534847	71.090458
787.933809	57.574985	71.095463
786.882467	46.577351	71.100468
786.249864	43.057267	71.105473
785.528357	52.682723	71.110478
785.099305	52.102816	71.115482
784.752695	54.376710	71.120487
783.954997	52.932960	71.125492
783.203192	54.525449	71.130497
782.711946	55.161822	71.135502
782.052918	47.673568	71.140506
780.984452	52.766865	71.145511
780.176807	47.202513	71.150516
779.935673	44.727144	71.155521
779.211629	53.285401	71.160526
778.650349	43.461874	71.165530
777.692093	45.334811	71.170535
777.030404	51.837818	71.175540
777.049659	50.510031	71.180545
775.531727	53.869254	71.185550
774.705662	35.952319	71.190554
774.214877	52.678390	71.195559
773.830327	42.400951	71.200564
773.834061	46.604473	71.205569
772.481049	56.259498	71.210574
771.883722	48.381377	71.215578
771.247922	49.188997	71.220583
770.650610	48.736803	71.225588
770.191755	40.051315	71.230593
769.243700	48.262029	71.235598
768.953895	44.523375	71.240602
767.903285	53.720251	71.245607
766.858594	53.962178	71.250612
766.529635	47.542608	71.255617
765.867543	51.636080	71.260622
765.794661	46.039923	71.265626
764.500518	44.132734	71.270631
763.639940	50.082351	71.275636
763.303451	47.022916	71.280641
762.713297	51.901304	71.285646
762.589948	47.740334	71.290650
761.190754	45.061388	71.295655
760.384392	46.408676	71.300660
760.070471	43.273111	71.305665
759.255222	41.974091	71.310670
758.425256	46.237791	71.315674
757.826498	48.061391	71.320679
757.342329	43.071609	71.325684
757.003096	37.992523	71.330689
756.261630	49.563980	71.335694
755.125436	48.440634	71.340698
754.728248	43.750822	71.345703
753.998802	44.568623	71.350708
753.878646	41.782261	71.355713
752.523291	44.740296	71.360718
751.910928	38.693858	71.365722
751.273379	49.108627	71.370727
750.913559	56.643806	71.375732
750.088078	49.847540	71.380737
749.173643	50.727909	71.385742
748.938129	45.400497	71.390746
748.205034	48.693139	71.395751
747.151144	51.935925	71.400756
746.838725	39.748347	71.405761
745.986406	41.412040	71.410766
745.774263	50.904374	71.415770
745.127004	48.793286	71.420775
744.082802	46.693352	71.425780
743.808827	46.951364	71.430785
743.001093	52.391100	71.435790
741.741402	45.725467	71.440794
740.836603	48.830978	71.445799
740.326890	47.292510	71.450804
739.757662	44.172361	71.455809
739.194299	50.148785	71.460814
739.091896	40.324760	71.465818
738.613035	41.651456	71.470823
737.881471	53.246573	71.475828
737.142744	47.800577	71.480833
736.608437	53.168399	71.485838
735.724440	41.544908	71.490842
734.742549	44.957586	71.495847
734.033697	44.491620	71.500852
734.092138	40.820535	71.505857
733.033714	45.514853	71.510862
732.604562	42.233633	71.515866
731.866426	47.094583	71.520871
730.781149	54.683756	71.525876
729.902178	41.081954	71.530881
729.008158	49.049109	71.535886
728.704732	37.560278	71.540890
728.335303	43.001197	71.545895
728.023651	37.777377	71.550900
727.277981	42.932841	71.555905
726.549293	49.640490	71.560910
725.946567	46.524100	71.565914
724.598572	49.282281	71.570919
723.697416	37.117478	71.575924
723.411446	42.592420	71.580929
722.603624	51.444724	71.585934
722.625221	45.317862	71.590938
721.989837	50.794819	71.595943
721.265855	50.413267	71.600948
720.777668	48.606447	71.605953
720.086548	49.277807	71.610958
719.036091	49.501747	71.615962
718.006008	56.681590	71.620967
717.496193	55.426996	71.625972
716.989777	47.785156	71.630977
716.570416	57.018745	71.635982
715.690903	48.095886	71.640986
715.187807	57.749664	71.645991
714.261869	52.230977	71.650996
714.064401	51.338243	71.656001
713.067144	58.429283	71.661006
712.230953	43.407716	71.666010
711.487980	47.083564	71.671015
711.334060	44.681051	71.676020
710.864964	43.136124	71.681025
709.441436	53.322800	71.686030
709.085944	43.923851	71.691034
708.789134	36.114606	71.696039
707.991212	41.871331	71.701044
706.846078	45.597017	71.706049
706.211756	53.913921	71.711054
706.052099	44.097437	71.716058
705.456002	49.669067	71.721063
704.387793	55.883574	71.726068
703.565870	48.457552	71.731073
702.711935	48.011540	71.736078
702.463750	38.450431	71.741082
702.577002	39.110422	71.746087
701.086642	49.653094	71.751092
700.761279	46.702287	71.756097
700.007530	51.923702	71.761102
699.472231	45.372996	71.766106
698.310164	45.729834	71.771111
697.585505	49.661392	71.776116
697.549430	42.897160	71.781121
696.819679	48.972622	71.786126
695.926642	45.235408	71.791130
694.997475	47.904841	71.796135
694.220877	48.124613	71.801140
694.039758	40.478299	71.806145
693.708799	52.848584	71.811150
692.780345	40.825336	71.816154
692.031770	37.032007	71.821159
691.440771	45.507592	71.826164
690.645998	37.347124	71.831169
689.533022	46.486141	71.836174
689.260886	35.444928	71.841178
688.522215	34.647830	71.846183
688.137314	45.719396	71.851188
687.690767	41.116306	71.856193
686.669508	44.574693	71.861198
686.018917	38.015542	71.866202
685.737078	38.587051	71.871207
684.417951	44.059338	71.876212
683.972927	36.546511	71.881217
683.046079	35.825109	71.886222
682.900890	44.412639	71.891226
682.151120	47.468253	71.896231
680.847105	38.152533	71.901236
680.696218	44.222561	71.906241
680.116760	43.959937	71.911246
679.806130	41.071443	71.916250
678.875926	36.181088	71.921255
677.874757	45.242381	71.926260
677.567098	38.480395	71.931265
676.794852	46.508599	71.936270
676.430792	50.220319	71.941274
675.386044	46.635003	71.946279
674.539083	48.280520	71.951284
674.402733	40.390536	71.956289
673.339724	46.523797	71.961294
672.343587	45.543770	71.966298
672.002654	38.400727	71.971303
671.069027	45.592030	71.976308
670.975181	37.135459	71.981313
670.801558	41.726762	71.986318
669.503355	44.218420	71.991322
668.850531	45.503441	71.996327
668.093918	51.606843	72.001332
667.936024	41.665506	72.006337
666.278443	47.734170	72.011342
666.000466	44.373698	72.016346
665.767724	47.455801	72.021351
665.005621	43.312972	72.026356
664.359108	35.687153	72.031361
663.212904	45.298250	72.036366
662.742236	37.086186	72.041370
662.588268	39.178028	72.046375
661.834165	48.346645	72.051380
660.778798	41.807799	72.056385
659.897318	48.178667	72.061390
659.746264	41.521057	72.066394
659.512267	40.944807	72.071399
658.286189	43.371369	72.076404
657.415982	43.839448	72.081409
656.825763	42.059928	72.086414
656.468862	42.439964	72.091418
655.415916	47.166556	72.096423
655.064405	41.863938	72.101428
654.466188	45.401632	72.106433
653.688450	48.313474	72.111438
652.855878	51.284510	72.116442
651.971298	45.079596	72.121447
651.721139	53.519841	72.126452
651.534596	44.264315	72.131457
650.356555	44.650528	72.136462
649.353526	46.308289	72.141466
648.702705	50.898311	72.146471
648.169531	45.148378	72.151476
648.190780	43.252568	72.156481
647.013367	52.023393	72.161486
645.955336	47.834651	72.166490
645.712547	42.647187	72.171495
644.950665	55.685339	72.176500
644.505253	42.140697	72.181505
644.123586	51.592213	72.186510
643.006445	36.626465	72.191514
642.576246	44.030925	72.196519
642.055772	46.955419	72.201524
641.415114	45.493019	72.206529
640.730379	47.622073	72.211534
639.957371	52.777184	72.216538
638.895470	41.522693	72.221543
637.917068	46.264229	72.226548
637.661067	40.672015	72.231553
637.029030	46.621542	72.236558
636.631974	44.726111	72.241562
636.351620	41.340791	72.246567
635.438356	51.498284	72.251572
634.688831	47.757163	72.256577
633.365836	55.489882	72.261582
632.362854	39.917750	72.266586
632.316159	49.273346	72.271591
631.649748	50.346074	72.276596
631.391746	42.227885	72.281601
630.868422	42.099837	72.286606
630.208143	40.708374	72.291610
629.159650	42.707698	72.296615
628.568440	38.275894	72.301620
628.350739	33.532298	72.306625
627.146060	42.983983	72.311630
626.222788	34.943354	72.316634
625.645608	38.389392	72.321639
624.942187	31.160584	72.326644
624.880808	43.563626	72.331649
624.022304	42.105959	72.336654
622.906236	40.630962	72.341658
622.641201	37.618522	72.346663
621.770696	45.692347	72.351668
621.954455	28.625524	72.356673
620.558591	40.402133	72.361678
620.032350	35.464820	72.366682
619.672307	37.650982	72.371687
618.806206	45.274672	72.376692
618.013916	33.989879	72.381697
617.462826	40.700805	72.386702
616.833389	27.985010	72.391706
615.455686	33.383075	72.396711
614.897616	32.721243	72.401716
614.620434	30.790958	72.406721
613.800993	37.762239	72.411726
613.512012	31.413612	72.416730
613.404293	35.986534	72.421735
612.106398	48.119714	72.426740
611.550046	37.440748	72.431745
610.639383	36.470790	72.436750
609.609170	30.818951	72.441754
608.946204	37.369497	72.446759
608.339201	37.797254	72.451764
608.092064	33.104080	72.456769
607.592525	31.759566	72.461774
607.206186	35.433837	72.466778
606.347655	25.512637	72.471783
605.397601	32.247674	72.476788
604.856248	32.332238	72.481793
604.156638	33.118521	72.486798
603.188343	30.350548	72.491802
602.784451	30.908386	72.496807
602.053788	36.022064	72.501812
602.045646	27.856212	72.506817
600.737675	36.835495	72.511822
600.022422	34.721087	72.516826
599.780511	37.616994	72.521831
598.948958	40.775540	72.526836
598.111605	29.192006	72.531841
597.596782	36.195202	72.536846
596.816475	36.671062	72.541850
596.519644	27.406314	72.546855
595.204604	42.219903	72.551860
594.778852	43.109233	72.556865
594.344609	47.574887	72.561870
593.874145	47.465236	72.566874
592.895217	41.098755	72.571879
591.905837	48.101841	72.576884
591.722807	38.604495	72.581889
591.019429	47.676737	72.586894
589.900715	36.991147	72.591898
589.232043	41.180319	72.596903
588.667191	44.141853	72.601908
588.338478	42.954641	72.606913
587.937575	42.766104	72.611918
587.152318	43.392567	72.616922
586.303959	43.641147	72.621927
585.448339	41.892874	72.626932
585.199813	36.271095	72.631937
583.906153	46.720993	72.636942
583.223389	43.199495	72.641946
582.954464	41.242667	72.646951
582.144231	48.169915	72.651956
582.100155	38.716674	72.656961
581.389916	44.014765	72.661966
580.203183	42.995744	72.666970
579.510682	38.772475	72.671975
579.080184	46.924469	72.676980
578.513813	46.677130	72.681985
577.510889	44.012451	72.686990
576.800711	48.015850	72.691994
576.613220	43.450374	72.696999
575.845416	43.120000	72.702004
575.302278	39.275068	72.707009
574.385670	40.862323	72.712014
573.976337	39.265328	72.717018
573.112751	39.175715	72.722023
572.105855	47.542513	72.727028
571.563333	37.831190	72.732033
570.925404	46.353690	72.737038
570.442071	41.713908	72.742042
569.991300	44.091147	72.747047
568.558361	52.148910	72.752052
568.222787	41.614567	72.757057
567.661454	46.805367	72.762062
567.420020	47.826196	72.767066
566.884653	52.071416	72.772071
565.326273	54.566718	72.777076
564.927574	43.708112	72.782081
564.323637	55.883755	72.787086
564.006767	47.366518	72.792090
563.488666	41.571632	72.797095
562.397509	43.964133	72.802100
562.067260	48.914702	72.807105
561.564913	53.935261	72.812110
560.213507	52.523006	72.817114
559.756878	45.251753	72.822119
559.122998	50.197066	72.827124
559.074634	45.396543	72.832129
557.618467	46.714925	72.837134
556.911712	50.020767	72.842138
556.530871	45.579129	72.847143
555.798269	55.237936	72.852148
555.655798	53.090656	72.857153
554.723990	53.759395	72.862158
553.634640	54.757580	72.867162
553.470438	53.343896	72.872167
552.763227	55.514400	72.877172
552.057183	48.492610	72.882177
551.349685	49.871525	72.887182
550.808269	50.992174	72.892186
550.152059	48.351132	72.897191
548.937349	51.122866	72.902196
548.511842	49.999962	72.907201
547.992014	46.909842	72.912206
547.436132	51.394877	72.917210
546.591981	48.115138	72.922215
545.762241	57.059287	72.927220
545.331401	47.314407	72.932225
544.865913	37.442588	72.937230
544.094720	49.326322	72.942234
543.245126	49.371686	72.947239
542.812362	46.889022	72.952244
542.188540	44.141898	72.957249
541.294230	43.234016	72.962254
540.251287	50.849627	72.967258
539.930552	48.894748	72.972263
539.383586	47.967811	72.977268
539.144676	48.953547	72.982273
538.155915	54.981993	72.987278
537.235957	50.257219	72.992282
536.768128	55.737488	72.997287
535.903210	59.259342	73.002292
535.972943	50.119133	73.007297
534.775151	49.734257	73.012302
534.086629	50.353213	73.017306
533.703167	45.027322	73.022311
532.369892	53.084999	73.027316
531.673563	49.455289	73.032321
531.315759	46.121744	73.037326
530.428423	57.041540	73.042330
530.322930	49.052040	73.047335
529.886186	43.993259	73.052340
528.812406	43.984450	73.057345
528.121366	50.321868	73.062350
527.753396	46.310273	73.067354
527.260746	39.923136	73.072359
526.065958	55.529744	73.077364
525.578030	46.949877	73.082369
524.854526	52.357330	73.087374
524.170311	45.289496	73.092378
523.512713	46.181074	73.097383
522.437066	50.315241	73.102388
522.222020	43.663111	73.107393
522.001748	47.405560	73.112398
520.561193	52.902000	73.117402
520.034637	42.215162	73.122407
519.221718	53.769658	73.127412
519.226598	51.266172	73.132417
518.735338	47.770960	73.137422
517.281706	43.421366	73.142426
516.954059	39.020151	73.147431
516.263661	50.045770	73.152436
515.705743	48.524492	73.157441
514.727214	50.446487	73.162446
514.052871	52.018828	73.167450
513.568463	48.074668	73.172455
512.947077	46.170838	73.177460
512.648510	49.720755	73.182465
511.518685	41.985891	73.187470
510.779605	48.822976	73.192474
510.428990	47.058942	73.197479
509.753960	48.465813	73.202484
509.246663	43.323658	73.207489
508.383257	48.529470	73.212494
507.835410	46.653351	73.217498
507.457180	44.652442	73.222503
506.231871	46.724137	73.227508
505.476824	44.371666	73.232513
505.153059	48.368722	73.237518
504.461852	49.566859	73.242522
503.784140	43.322748	73.247527
502.649159	44.749271	73.252532
502.021374	44.571658	73.257537
501.991400	42.266115	73.262542
501.507259	50.360429	73.267546
500.852902	43.412428	73.272551
499.883825	48.502612	73.277556
499.334864	40.938578	73.282561
498.261339	40.286343	73.287566
497.259559	44.203746	73.292570
497.124181	43.162369	73.297575
496.402995	47.758901	73.302580
496.181291	41.355419	73.307585
495.148637	43.800131	73.312590
494.044132	44.338706	73.317594
494.082586	46.046664	73.322599
493.098395	49.354139	73.327604
492.176464	50.552762	73.332609
491.666090	48.315861	73.337614
490.860269	48.131919	73.342618
491.034228	46.902492	73.347623
490.015071	54.329828	73.352628
489.232971	51.019725	73.357633
488.640959	51.812555	73.362638
488.079869	47.841193	73.367642
487.023319	48.832604	73.372647
485.868055	49.639467	73.377652
485.554937	51.807133	73.382657
485.198551	48.982729	73.387662
484.681548	45.690323	73.392666
484.688166	39.933295	73.397671
483.521642	52.260066	73.402676
482.855838	43.601316	73.407681
482.312503	42.470387	73.412686
480.977978	50.698596	73.417690
480.363320	45.633475	73.422695
479.908533	49.589905	73.427700
479.520696	45.554676	73.432705
478.465726	41.777114	73.437710
477.512411	46.120468	73.442714
477.184073	49.101117	73.447719
476.622763	47.389577	73.452724
476.129867	46.605429	73.457729
475.361262	38.439303	73.462734
474.363106	52.589029	73.467738
474.173409	46.629883	73.472743
473.624873	48.480238	73.477748
472.725832	47.992606	73.482753
471.947685	47.506216	73.487758
471.176098	35.229435	73.492762
471.152673	39.719542	73.497767
469.974463	51.981947	73.502772
469.058511	53.020354	73.507777
468.583704	48.383967	73.512782
467.969765	47.882457	73.517786
467.669453	46.178225	73.522791
466.518681	55.276037	73.527796
465.832849	50.482456	73.532801
465.576267	41.310664	73.537806
465.064406	58.183604	73.542810
464.324165	46.117868	73.547815
462.794414	57.734537	73.552820
462.691122	48.967253	73.557825
462.304645	41.706930	73.562830
461.146471	49.713087	73.567834
460.474809	47.621737	73.572839
460.010687	57.160520	73.577844
459.248095	44.350868	73.582849
458.876697	39.627049	73.587854
458.546176	45.362993	73.592858
457.735702	42.005384	73.597863
457.278993	47.748817	73.602868
456.767800	44.475993	73.607873
455.413510	42.190622	73.612878
454.525222	52.197525	73.617882
454.223926	43.985341	73.622887
453.640256	46.598237	73.627892
452.865615	58.905169	73.632897
452.100447	51.918064	73.637902
451.465807	50.719685	73.642906
451.408662	44.435073	73.647911
450.149070	57.755979	73.652916
449.338946	44.042422	73.657921
448.873197	40.016459	73.662926
448.181806	50.584930	73.667930
447.654205	40.052826	73.672935
446.542434	48.467912	73.677940
446.248247	43.741255	73.682945
445.530628	47.668600	73.687950
445.097910	47.439422	73.692954
444.353283	37.235213	73.697959
442.965752	56.423864	73.702964
442.650859	42.869533	73.707969
442.527713	45.647182	73.712974
441.882763	50.859211	73.717978
441.058841	46.991237	73.722983
440.169735	52.809872	73.727988
439.551508	48.480194	73.732993
439.555654	48.323343	73.737998
438.234498	53.627338	73.743002
437.920531	44.873124	73.748007
437.071494	46.925904	73.753012
436.179026	43.029431	73.758017
435.311263	41.920239	73.763022
434.239111	49.846468	73.768026
434.480336	39.384267	73.773031
433.951466	45.084006	73.778036
433.557676	50.265483	73.783041
432.600413	41.886578	73.788046
431.428331	46.599117	73.793050
431.582681	34.756730	73.798055
430.536820	42.483225	73.803060
429.642663	45.539834	73.808065
429.292899	42.802694	73.813070
428.472797	46.252783	73.818074
427.569622	39.487955	73.823079
426.487813	45.435065	73.828084
425.927775	47.061756	73.833089
425.395067	47.490336	73.838094
424.855186	50.130955	73.843098
424.960687	39.915883	73.848103
424.231694	45.779972	73.853108
423.135417	48.327890	73.858113
422.839201	44.896243	73.863118
421.815846	52.644392	73.868122
421.021774	47.652029	73.873127
420.201939	53.866488	73.878132
419.831305	38.868668	73.883137
419.353114	50.134883	73.888142
418.526424	53.141323	73.893146
418.117879	47.343211	73.898151
416.948259	56.554431	73.903156
416.611354	52.320286	73.908161
416.235828	47.223391	73.913166
415.108326	50.787118	73.918170
414.883844	43.228181	73.923175
414.092137	49.559584	73.928180
412.937362	59.214722	73.933185
412.178194	50.280708	73.938190
411.478704	54.224098	73.943194
411.267937	40.738343	73.948199
410.939535	52.713979	73.953204
410.299911	40.800973	73.958209
409.231565	43.256136	73.963214
408.512235	43.265021	73.968218
408.002533	42.340062	73.973223
406.965945	48.658445	73.978228
406.186306	39.864898	73.983233
405.930660	45.528991	73.988238
405.165673	47.943706	73.993242
404.863986	44.822017	73.998247
404.173409	47.068757	74.003252
403.353237	48.378932	74.008257
402.849976	46.382193	74.013262
402.177177	42.736162	74.018266
401.279334	45.473244	74.023271
400.329601	46.439787	74.028276
400.016454	48.946512	74.033281
399.805643	52.871965	74.038286
398.729523	49.913095	74.043290
397.564297	39.728611	74.048295
397.103957	53.750084	74.053300
397.037008	48.750682	74.058305
396.413386	46.708468	74.063310
395.144909	49.514071	74.068314
394.663351	43.128356	74.073319
394.032093	48.342943	74.078324
393.857180	45.513293	74.083329
392.863570	51.812218	74.088334
392.229460	44.662331	74.093338
391.680978	38.886526	74.098343
390.563396	45.042776	74.103348
389.567723	52.647753	74.108353
389.265916	47.903394	74.113358
388.637968	56.799656	74.118362
388.313045	46.266812	74.123367
387.772700	49.831609	74.128372
386.763159	48.795488	74.133377
386.227794	44.823209	74.138382
385.270440	47.599742	74.143386
385.172839	47.618376	74.148391
383.946583	51.543206	74.153396
383.069537	48.923208	74.158401
382.866798	40.040900	74.163406
382.313077	53.391276	74.168410
381.924097	42.233129	74.173415
380.546690	52.598687	74.178420
379.930150	46.743840	74.183425
379.721119	49.874222	74.188430
379.087169	54.942586	74.193434
378.620198	47.567373	74.198439
377.494989	57.400738	74.203444
377.033323	51.270475	74.208449
376.289179	45.229381	74.213454
375.266170	50.506397	74.218458
374.662242	45.983649	74.223463
374.003405	50.456735	74.228468
373.653188	44.911114	74.233473
373.479974	46.348444	74.238478
371.960397	52.120905	74.243482
371.499314	43.281340	74.248487
371.176748	46.554393	74.253492
370.814454	43.242093	74.258497
369.668682	37.954135	74.263502
368.906551	39.439575	74.268506
368.426246	47.992186	74.273511
367.357259	55.623046	74.278516
366.362631	47.679056	74.283521
366.467527	51.301889	74.288526
365.869282	47.502061	74.293530
365.508600	35.585629	74.298535
364.031588	49.959918	74.303540
363.189951	55.097651	74.308545
363.048999	41.061462	74.313550
362.523240	52.973930	74.318554
362.447754	42.387154	74.323559
360.873074	50.218446	74.328564
360.339034	48.103618	74.333569
360.088806	47.541023	74.338574
358.727657	47.827240	74.343578
358.194650	47.251360	74.348583
357.219076	39.597657	74.353588
357.012133	43.945117	74.358593
356.734079	42.891792	74.363598
356.177738	54.805982	74.368602
355.301646	44.211167	74.373607
354.681081	45.864865	74.378612
354.097867	47.190912	74.383617
353.034823	45.368545	74.388622
352.059939	54.655989	74.393626
351.531372	48.627858	74.398631
351.347301	45.537898	74.403636
350.630693	51.776925	74.408641
350.090131	50.948360	74.413646
349.236097	47.178260	74.418650
348.734339	40.114532	74.423655
347.663321	41.783243	74.428660
346.888110	44.726307	74.433665
346.798316	38.521027	74.438670
345.934353	43.025227	74.443674
344.793963	43.501777	74.448679
343.894959	49.186398	74.453684
343.475729	51.265332	74.458689
343.665797	41.418413	74.463694
342.752764	50.443687	74.468698
342.261390	41.284106	74.473703
341.091612	44.912946	74.478708
340.735053	45.397051	74.483713
339.971440	38.245745	74.488718
339.035847	49.343582	74.493722
338.492811	45.533388	74.498727
338.028533	51.598165	74.503732
337.102163	45.650781	74.508737
336.964438	40.369352	74.513742
335.931689	50.339380	74.518746
335.168018	44.553726	74.523751
334.687245	46.573083	74.528756
333.874461	44.739227	74.533761
333.240208	43.789979	74.538766
332.361460	41.771094	74.543770
331.853457	40.555721	74.548775
331.247477	48.707317	74.553780
330.894359	45.253213	74.558785
330.405721	45.613288	74.563790
329.185989	50.905901	74.568794
328.824137	48.948144	74.573799
328.343019	43.489627	74.578804
327.097901	45.239710	74.583809
326.937342	39.337446	74.588814
325.761825	40.734238	74.593818
325.416548	37.165346	74.598823
324.739451	39.995007	74.603828
323.759404	46.282330	74.608833
323.683670	41.052524	74.613838
322.985489	43.696312	74.618842
322.005529	40.600730	74.623847
321.213353	49.688751	74.628852
320.498527	43.576774	74.633857
320.637606	39.856575	74.638862
319.439982	47.634105	74.643866
318.371710	38.072884	74.648871
317.995663	40.977572	74.653876
317.818528	45.372322	74.658881
317.225324	39.821285	74.663886
315.963417	57.274234	74.668890
315.487086	45.250082	74.673895
315.064759	42.262752	74.678900
314.114994	49.748471	74.683905
313.062145	45.932800	74.688910
312.181734	50.340286	74.693914
312.091929	47.896051	74.698919
311.605942	46.814368	74.703924
311.108138	53.132075	74.708929
310.414651	46.907889	74.713934
309.699724	53.397395	74.718938
309.477606	50.559507	74.723943
308.016666	47.676203	74.728948
307.119168	55.155173	74.733953
306.821349	47.737251	74.738958
306.236436	53.803913	74.743962
305.812025	47.836467	74.748967
304.573178	47.814639	74.753972
303.865546	48.857750	74.758977
303.379314	42.628923	74.763982
302.942042	45.038745	74.768986
302.491974	40.881007	74.773991
302.036998	43.542809	74.778996
300.792529	45.292801	74.784001
300.467279	41.141978	74.789006
299.801532	51.681155	74.794010
298.765608	42.783417	74.799015
297.898023	42.729230	74.804020
297.602574	47.820929	74.809025
297.405885	36.149615	74.814030
296.163440	51.582535	74.819034
295.393244	40.571904	74.824039
294.931631	39.730770	74.829044
294.435847	45.551412	74.834049
294.463188	39.906211	74.839054
292.943574	50.773866	74.844058
292.448531	43.742197	74.849063
291.997077	45.444651	74.854068
290.608747	42.213895	74.859073
289.929205	39.739075	74.864078
289.024696	43.806631	74.869082
288.806816	38.925915	74.874087
288.377267	43.915984	74.879092
287.780165	41.997307	74.884097
287.697730	44.478310	74.889102
286.768682	45.580370	74.894106
286.015501	40.387577	74.899111
285.375037	44.241162	74.904116
284.029416	46.231212	74.909121
283.883913	38.604519	74.914126
283.013212	36.619064	74.919130
282.665597	39.229063	74.924135
281.769156	48.447251	74.929140
280.829726	44.949410	74.934145
280.717426	48.815011	74.939150
280.081581	46.943510	74.944154
279.312841	44.989113	74.949159
278.429511	48.588096	74.954164
278.089082	45.272329	74.959169
277.114226	52.235356	74.964174
276.134993	54.717371	74.969178
275.560690	46.758473	74.974183
275.414436	49.552424	74.979188
274.847746	39.332538	74.984193
273.915539	52.151889	74.989198
272.822677	57.529964	74.994202
272.256323	50.525434	74.999207
272.288872	51.195111	75.004212
270.979693	52.539116	75.009217
270.316774	44.799349	75.014222
269.557332	55.410237	75.019226
269.043833	49.903278	75.024231
269.051690	45.967448	75.029236
268.065894	48.595592	75.034241
266.999637	39.685360	75.039246
266.168526	47.697807	75.044250
265.967360	42.880660	75.049255
265.807082	45.930736	75.054260
264.981712	50.815166	75.059265
264.419617	44.822368	75.064270
263.331168	43.628565	75.069274
262.229618	46.235737	75.074279
261.518208	42.215858	75.079284
260.791482	52.140286	75.084289
260.347494	37.747146	75.089294
259.800198	42.722870	75.094298
259.707296	41.316770	75.099303
259.419608	43.423634	75.104308
258.118575	47.442441	75.109313
257.846876	43.861832	75.114318
256.639203	53.490760	75.119322
255.524242	44.990418	75.124327
254.936583	45.044593	75.129332
254.493084	47.239372	75.134337
254.565478	45.605073	75.139342
253.396957	41.673828	75.144346
252.707688	33.832617	75.149351
252.421648	40.260075	75.154356
251.565949	44.885989	75.159361
250.736453	39.471985	75.164366
250.004100	46.271785	75.169370
249.571400	41.393775	75.174375
248.999687	44.509433	75.179380
247.685990	47.480010	75.184385
247.519448	43.373285	75.189390
246.672266	52.440130	75.194394
246.003527	44.431640	75.199399
246.061783	45.680693	75.204404
244.655342	48.363280	75.209409
244.306098	44.323524	75.214414
243.582302	53.034810	75.219418
242.924329	44.800677	75.224423
241.943678	54.746663	75.229428
241.205174	51.167924	75.234433
241.135875	49.232935	75.239438
240.186172	55.548568	75.244442
239.269929	43.301251	75.249447
238.753272	47.078342	75.254452
238.071535	55.117451	75.259457
238.015292	48.228739	75.264462
236.646039	50.287237	75.269466
235.768946	49.179604	75.274471
235.472905	43.633261	75.279476
234.777332	55.366229	75.284481
234.957650	43.390398	75.289486
233.362537	54.140809	75.294490
232.795024	52.231621	75.299495
232.375167	45.276293	75.304500
231.708858	49.755331	75.309505
231.255419	49.210950	75.314510
230.195530	54.564861	75.319514
229.781873	51.815862	75.324519
229.283046	55.809310	75.329524
227.928100	46.208675	75.334529
227.501582	49.367426	75.339534
226.804895	57.907240	75.344538
226.515656	47.026548	75.349543
225.683775	51.636060	75.354548
224.572882	57.742427	75.359553
224.245387	51.713818	75.364558
223.547841	52.931963	75.369562
223.383001	56.175159	75.374567
222.553807	46.859726	75.379572
221.675780	51.011393	75.384577
221.474093	43.379470	75.389582
219.960042	52.607819	75.394586
219.151704	45.078909	75.399591
218.577098	45.359670	75.404596
218.016935	50.936697	75.409601
218.048728	39.143820	75.414606
217.422962	44.064252	75.419610
216.858784	53.262609	75.424615
216.053332	50.035174	75.429620
215.064062	53.567487	75.434625
214.478514	43.278085	75.439630
213.266243	47.484614	75.444634
213.070867	51.308265	75.449639
212.399805	40.898456	75.454644
211.669560	50.990611	75.459649
211.589245	48.475483	75.464654
210.438242	51.297142	75.469658
209.701830	46.044932	75.474663
209.142302	44.539755	75.479668
208.326329	51.146315	75.484673
207.544069	42.501500	75.489678
207.106553	51.304351	75.494682
206.329826	47.873644	75.499687
206.179972	46.970212	75.504692
205.604989	51.611317	75.509697
204.710940	51.794771	75.514702
203.643383	51.788265	75.519706
203.335608	49.306245	75.524711
202.249757	52.330410	75.529716
201.285335	52.950862	75.534721
201.209672	44.631799	75.539726
200.481993	47.221973	75.544730
200.033174	52.186743	75.549735
199.908570	47.619173	75.554740
198.399468	60.830138	75.559745
198.113742	43.484953	75.564750
197.058681	56.737073	75.569754
196.334103	57.131634	75.574759
196.035378	47.138710	75.579764
195.168199	49.934052	75.584769
194.872136	40.850612	75.589774
193.752833	52.671635	75.594778
192.997199	58.155253	75.599783
192.548403	47.066616	75.604788
191.929650	52.654566	75.609793
191.541283	40.171734	75.614798
190.694769	52.457049	75.619802
189.608414	52.693244	75.624807
189.049755	46.291488	75.629812
188.582096	48.983716	75.634817
188.655361	41.036730	75.639822
187.708618	48.364309	75.644826
186.904167	48.823646	75.649831
186.164368	50.132115	75.654836
185.287971	47.229816	75.659841
184.682078	45.733614	75.664846
184.199321	52.797991	75.669850
183.559303	47.438959	75.674855
182.690336	37.010253	75.679860
181.654320	46.285410	75.684865
181.432082	46.418540	75.689870
181.021067	57.182057	75.694874
180.156886	49.406596	75.699879
179.408607	45.094577	75.704884
178.857897	55.118695	75.709889
178.416684	46.197168	75.714894
177.338386	50.429663	75.719898
176.558294	48.652151	75.724903
175.774223	46.734925	75.729908
175.408883	51.300035	75.734913
175.324694	37.399920	75.739918
174.223017	47.455101	75.744922
173.274310	48.028904	75.749927
172.857727	43.804355	75.754932
171.926025	47.031037	75.759937
171.064793	45.988709	75.764942
170.407436	47.236731	75.769946
170.018044	43.812094	75.774951
169.609284	35.158215	75.779956
168.838233	48.150591	75.784961
168.366190	46.476935	75.789966
167.398808	45.773230	75.794970
166.719759	44.105769	75.799975
166.398456	38.787396	75.804980
165.497084	45.519543	75.809985
164.867221	49.604855	75.814990
164.216997	53.674490	75.819994
163.784646	43.747036	75.824999
163.396571	50.703279	75.830004
161.823817	51.073804	75.835009
161.331360	39.619982	75.840014
160.732161	49.134588	75.845018
160.360221	42.769305	75.850023
159.920965	44.558145	75.855028
158.776928	48.602432	75.860033
158.286186	44.444902	75.865038
157.965431	45.733879	75.870042
156.932008	52.600626	75.875047
156.184981	44.118948	75.880052
155.193053	52.339991	75.885057
155.066311	41.198447	75.890062
154.706002	44.398690	75.895066
153.660295	50.158797	75.900071
152.794867	43.302915	75.905076
152.487236	51.891097	75.910081
151.863280	48.352473	75.915086
150.650908	47.386637	75.920090
150.027329	43.289713	75.925095
149.742914	32.761519	75.930100
149.349971	45.919115	75.935105
148.470188	44.805636	75.940110
147.419649	49.317568	75.945114
146.746785	43.369275	75.950119
146.683816	40.559650	75.955124
145.876075	51.312301	75.960129
145.172749	42.145571	75.965134
144.282335	44.832669	75.970138
143.712448	45.852286	75.975143
143.569644	39.310127	75.980148
142.210503	50.951786	75.985153
141.482811	39.224816	75.990158
140.738121	47.086320	75.995162
140.554733	51.422149	76.000167
140.300640	45.601053	76.005172
138.994743	46.988757	76.010177
138.552125	39.161875	76.015182
138.129464	44.308559	76.020186
137.293346	43.811019	76.025191
136.323366	38.739581	76.030196
135.849723	47.070379	76.035201
135.280403	43.579820	76.040206
134.464739	42.982825	76.045210
133.466184	46.671189	76.050215
133.143806	33.225379	76.055220
132.656693	39.760595	76.060225
132.054039	47.293525	76.065230
131.041868	42.009619	76.070234
130.400317	39.356903	76.075239
130.160040	33.618766	76.080244
129.517997	52.702850	76.085249
128.394712	42.977036	76.090254
127.445380	37.579035	76.095258
127.149904	48.822443	76.100263
127.017051	42.043731	76.105268
126.012310	46.546792	76.110273
125.026366	37.393596	76.115278
124.352596	46.566858	76.120282
123.891753	49.144469	76.125287
123.961886	37.254028	76.130292
122.737478	48.730707	76.135297
122.248734	40.510638	76.140302
121.505374	40.343666	76.145306
120.089067	46.353687	76.150311
119.597353	43.883662	76.155316
118.834029	48.064380	76.160321
118.578297	43.555575	76.165326
118.352294	47.081337	76.170330
117.441552	46.275581	76.175335
116.646748	50.030811	76.180340
115.715004	56.376736	76.185345
115.573650	42.745940	76.190350
114.788851	46.171568	76.195354
113.562727	48.030690	76.200359
113.291959	36.694502	76.205364
112.532451	53.663702	76.210369
112.398563	43.538861	76.215374
111.337377	49.793461	76.220378
110.066552	45.370823	76.225383
110.118183	45.457136	76.230388
109.295458	48.382612	76.235393
109.116812	44.362987	76.240398
108.567607	43.893824	76.245402
107.466692	42.504961	76.250407
107.142329	44.505724	76.255412
105.863874	44.297924	76.260417
104.944653	57.700299	76.265422
104.042785	46.053153	76.270426
104.034618	45.404679	76.275431
103.842468	38.405193	76.280436
103.330647	44.272573	76.285441
102.243278	53.279982	76.290446
101.304148	53.685127	76.295450
100.833232	51.896187	76.300455
100.310442	46.013864	76.305460
99.375343	40.332908	76.310465
98.801212	46.834698	76.315470
98.369291	45.217738	76.320474
98.026514	43.063014	76.325479
96.917397	45.592614	76.330484
96.129861	39.754088	76.335489
95.612053	38.691719	76.340494
94.462380	50.866122	76.345498
93.595062	47.451477	76.350503
93.630188	52.788522	76.355508
92.932164	53.282957	76.360513
92.731247	48.483139	76.365518
92.214974	42.647089	76.370522
90.976860	45.705041	76.375527
90.340684	53.710104	76.380532
89.312926	45.367835	76.385537
88.173957	47.574194	76.390542
87.909829	39.832403	76.395546
87.420314	42.846676	76.400551
87.147783	35.497312	76.405556
86.633201	48.111337	76.410561
85.801967	38.230169	76.415566
84.878548	42.154149	76.420570
84.521699	50.266056	76.425575
84.144277	43.890626	76.430580
82.718187	45.571915	76.435585
82.295011	45.590440	76.440590
81.975553	50.124587	76.445594
80.950330	50.379466	76.450599
80.233566	38.642897	76.455604
79.514127	39.604374	76.460609
79.044356	46.067448	76.465614
78.785394	47.802320	76.470618
77.454042	50.405215	76.475623
77.151414	45.498617	76.480628
76.389123	48.477544	76.485633
75.742448	42.876759	76.490638
74.792684	43.632117	76.495642
73.894329	38.077777	76.500647
73.955492	39.741097	76.505652
73.092381	43.726428	76.510657
72.803361	33.023944	76.515662
71.991494	38.352548	76.520666
70.972890	42.266481	76.525671
70.832208	43.734909	76.530676
69.546928	51.920757	76.535681
68.712665	45.556681	76.540686
67.980327	47.646163	76.545690
67.690716	46.492215	76.550695
67.528714	40.784181	76.555700
66.645515	45.654233	76.560705
65.633055	46.490555	76.565710
65.044389	44.384511	76.570714
64.397931	52.110520	76.575719
64.232662	37.784962	76.580724
62.742143	44.863405	76.585729
62.096271	48.016158	76.590734
61.714807	46.627700	76.595738
61.371003	48.637877	76.600743
61.131335	40.931614	76.605748
59.783767	52.328613	76.610753
59.118876	43.603641	76.615758
58.698511	45.644951	76.620762
57.822243	47.503500	76.625767
57.214594	44.599393	76.630772
56.623673	47.199336	76.635777
56.165598	47.166660	76.640782
55.187982	47.147453	76.645786
54.142492	53.743348	76.650791
53.568167	44.791045	76.655796
53.164193	49.166785	76.660801
52.617247	44.385888	76.665806
52.596706	46.451745	76.670810
51.175850	48.110140	76.675815
50.648226	43.676245	76.680820
49.900946	50.046387	76.685825
49.386965	50.858413	76.690830
48.503283	51.705744	76.695834
47.840511	48.490309	76.700839
47.568193	39.707467	76.705844
46.847009	44.810307	76.710849
45.869332	47.454585	76.715854
45.463682	47.003544	76.720858
44.525632	37.735518	76.725863
44.192081	40.316494	76.730868
43.168312	41.271323	76.735873
42.241016	49.045276	76.740878
41.932990	38.867798	76.745882
41.632850	42.649813	76.750887
40.979281	37.878041	76.755892
39.985750	41.168244	76.760897
39.108199	37.753679	76.765902
39.030852	37.068931	76.770906
38.173658	47.230247	76.775911
37.479087	49.096095	76.780916
36.551074	45.678538	76.785921
36.409629	37.253296	76.790926
35.668458	43.122570	76.795930
34.741460	49.287988	76.800935
34.124625	39.489344	76.805940
33.530066	39.118895	76.810945
32.611646	43.412679	76.815950
32.045393	47.041596	76.820954
31.192893	47.691572	76.825959
30.618777	39.805266	76.830964
30.404487	48.009556	76.835969
29.441373	38.638302	76.840974
29.021414	38.970136	76.845978
27.988646	38.932928	76.850983
27.644964	35.955193	76.855988
26.783953	42.141625	76.860993
25.652848	34.465582	76.865998
25.530522	31.630740	76.871002
24.709256	38.059991	76.876007
24.792789	37.866824	76.881012
23.395425	43.848641	76.886017
22.662460	36.159563	76.891022
22.362984	35.298931	76.896026
21.516795	43.749079	76.901031
21.155992	29.732269	76.906036
20.080363	37.987196	76.911041
19.346080	39.722187	76.916046
19.412468	30.964183	76.921050
18.386540	31.775864	76.926055
17.538550	25.724666	76.931060
16.856623	33.262366	76.936065
16.407077	26.677689	76.941070
15.144096	36.399099	76.946074
14.051689	36.844493	76.951079
14.138934	34.717393	76.956084
13.713614	38.311218	76.961089
13.264089	37.879796	76.966094
13.092478	35.729326	76.971098
11.957329	44.223987	76.976103
11.165682	35.503485	76.981108
10.349782	45.035325	76.986113
9.198606	42.080727	76.991118
8.573568	37.488918	76.996122
7.904322	36.982154	77.001127
7.602699	34.491300	77.006132
7.216320	42.018138	77.011137
6.798915	29.951585	77.016142
5.782725	35.888382	77.021147
4.871516	30.776094	77.026151
4.970753	36.370982	77.031156
3.652402	37.647202	77.036161