Fri Mar 05 19:19:39 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.593353	96.118378	0.000000
-0.464309	80.695824	0.005005
-1.407987	62.225854	0.010010
-3.009818	27.709796	0.015014
-6.626906	-2.922376	0.020019
-12.694390	7.422213	0.025024
-17.308330	2.356839	0.030029
-21.790102	0.640320	0.035034
-26.172129	3.310725	0.040038
-29.593204	4.470082	0.045043
-33.308652	10.583860	0.050048
-37.008271	10.123989	0.055053
-40.350510	3.162135	0.060058
-44.433422	13.194915	0.065062
-47.988203	5.699280	0.070067
-51.852268	11.035708	0.075072
-55.784665	0.553678	0.080077
-59.632554	8.831691	0.085082
-63.543234	6.453278	0.090086
-66.854503	2.859605	0.095091
-70.730276	5.819898	0.100096
-74.476121	5.514116	0.105101
-77.987802	6.617036	0.110106
-81.915444	7.346362	0.115110
-85.547303	-2.576444	0.120115
-89.610167	-2.347497	0.125120
-93.724974	-3.300847	0.130125
-97.330766	1.969207	0.135130
-101.399417	6.582999	0.140134
-105.312796	6.455384	0.145139
-109.001757	10.117631	0.150144
-112.213889	4.596947	0.155149
-115.714034	2.044303	0.160154
-119.678726	18.722502	0.165158
-123.203697	3.588242	0.170163
-127.420918	15.293646	0.175168
-131.057692	6.081317	0.180173
-134.852888	11.697041	0.185178
-138.655989	12.214198	0.190182
-142.231368	-2.126663	0.195187
-146.255068	4.183126	0.200192
-149.936537	4.368655	0.205197
-153.343560	8.749214	0.210202
-157.784822	10.453181	0.215206
-160.920791	2.130799	0.220211
-164.634248	12.002306	0.225216
-168.337352	5.112421	0.230221
-172.258193	6.965169	0.235226
-176.570841	10.496819	0.240230
-180.075114	0.763535	0.245235
-183.798562	10.579893	0.250240
-187.130923	11.476156	0.255245
-190.566970	2.192465	0.260250
-195.272060	9.174054	0.265254
-198.692686	3.923309	0.270259
-202.785340	12.677417	0.275264
-206.253772	7.538390	0.280269
-209.911013	4.306066	0.285274
-213.535974	11.391255	0.290278
-217.562051	1.189385	0.295283
-221.772835	12.597448	0.300288
-225.417413	10.517447	0.305293
-228.830494	6.090282	0.310298
-232.838592	5.038136	0.315302
-235.904833	8.199053	0.320307
-239.821646	8.206245	0.325312
-243.590375	3.037940	0.330317
-247.551420	8.886886	0.335322
-251.778823	12.466562	0.340326
-254.887123	4.966211	0.345331
-259.151328	15.449315	0.350336
-263.043848	9.217441	0.355341
-266.585273	7.576773	0.360346
-270.310947	10.910809	0.365350
-273.926260	-5.189630	0.370355
-278.035109	8.247538	0.375360
-281.716529	4.063560	0.380365
-284.943148	2.235471	0.385370
-288.615373	13.931402	0.390374
-292.303400	1.754985	0.395379
-296.632470	17.638488	0.400384
-300.550954	6.913388	0.405389
-304.465056	9.403933	0.410394
-308.020383	15.751173	0.415398
-311.549826	10.081153	0.420403
-315.066004	11.511560	0.425408
-319.236637	6.130001	0.430413
-323.002371	7.235989	0.435418
-327.178767	14.656962	0.440422
-330.388849	5.441485	0.445427
-334.373325	11.384196	0.450432
-337.645529	4.340633	0.455437
-341.488864	2.097006	0.460442
-345.630828	2.496708	0.465446
-349.304574	-1.849234	0.470451
-353.226503	8.544679	0.475456
-356.797272	4.627001	0.480461
-360.270964	8.668408	0.485466
-364.290023	11.827084	0.490470
-368.218902	6.381781	0.495475
-371.576706	4.927991	0.500480
-375.573801	9.750003	0.505485
-379.231878	5.054677	0.510490
-383.441728	6.862452	0.515494
-386.599071	4.630782	0.520499
-390.667414	6.248817	0.525504
-394.435806	8.329889	0.530509
-398.032421	3.482855	0.535514
-401.795379	3.795323	0.540518
-405.711617	1.787369	0.545523
-409.780038	11.793182	0.550528
-413.304385	2.538127	0.555533
-416.772988	2.357339	0.560538
-420.486769	2.699830	0.565542
-424.272099	-7.579532	0.570547
-428.540574	2.913989	0.575552
-432.377780	7.696365	0.580557
-435.656795	-3.759812	0.585562
-439.609583	10.598850	0.590566
-443.034780	3.445834	0.595571
-446.913454	15.185998	0.600576
-451.146236	14.482337	0.605581
-454.821319	4.347836	0.610586
-458.188918	18.631994	0.615590
-461.911415	-1.667745	0.620595
-465.959845	15.077948	0.625600
-469.597952	8.509327	0.630605
-473.122954	5.139600	0.635610
-477.406938	13.287628	0.640614
-480.832221	5.306791	0.645619
-484.814380	6.042328	0.650624
-488.665346	10.830144	0.655629
-492.129060	3.803202	0.660634
-496.116725	8.489863	0.665638
-499.394454	-6.177064	0.670643
-503.257741	13.016475	0.675648
-507.536110	8.007276	0.680653
-510.886439	11.679111	0.685658
-514.953795	5.360478	0.690662
-518.340940	3.708160	0.695667
-522.120672	10.108894	0.700672
-526.084631	14.638855	0.705677
-529.631950	8.101559	0.710682
-533.726085	11.319816	0.715686
-537.555940	2.258840	0.720691
-540.940156	10.561281	0.725696
-545.055012	13.793907	0.730701
-548.481364	5.209377	0.735706
-552.527790	10.689254	0.740710
-556.123229	4.498730	0.745715
-559.922829	3.377559	0.750720
-563.990291	8.125963	0.755725
-567.436758	6.226153	0.760730
-570.901530	13.787730	0.765734
-574.755905	7.939796	0.770739
-578.816676	4.477633	0.775744
-583.083741	4.501923	0.780749
-586.455798	3.530105	0.785754
-590.300191	4.117653	0.790758
-593.632693	2.401521	0.795763
-597.358053	2.118517	0.800768
-601.164471	11.920352	0.805773
-604.831538	9.535453	0.810778
-608.738000	14.188825	0.815782
-612.529662	8.269434	0.820787
-616.305133	11.113643	0.825792
-620.318805	9.413347	0.830797
-623.679067	0.618105	0.835802
-627.644838	16.243830	0.840806
-631.641190	7.231693	0.845811
-635.065914	6.995327	0.850816
-638.981527	8.486878	0.855821
-642.667380	1.831551	0.860826
-646.969015	10.790079	0.865830
-650.149491	0.496447	0.870835
-653.601427	0.524651	0.875840
-657.660087	8.629095	0.880845
-661.314697	0.820799	0.885850
-665.590799	8.821233	0.890854
-668.875712	5.375592	0.895859
-672.528663	5.344484	0.900864
-676.171584	13.573333	0.905869
-680.194379	-0.937984	0.910874
-684.202301	13.710553	0.915878
-687.766871	4.276283	0.920883
-691.891849	2.888784	0.925888
-695.471894	17.222961	0.930893
-699.233605	6.544474	0.935898
-702.696191	8.744311	0.940902
-706.727933	-0.771379	0.945907
-710.358951	12.943341	0.950912
-714.040425	6.404122	0.955917
-717.755414	-3.140094	0.960922
-721.818218	10.599496	0.965926
-725.573602	7.430975	0.970931
-729.420724	6.125289	0.975936
-733.182334	10.271588	0.980941
-736.574036	5.736105	0.985946
-740.547390	6.189969	0.990950
-744.193126	10.541690	0.995955
-747.912979	9.679309	1.000960
-751.931537	21.543219	1.005965
-755.531001	8.973381	1.010970
-759.491278	16.231227	1.015974
-762.875960	8.231716	1.020979
-766.935644	10.804627	1.025984
-770.350830	3.975359	1.030989
-774.204608	0.064143	1.035994
-778.280186	11.326929	1.040998
-781.776543	1.724216	1.046003
-785.672433	6.994336	1.051008
-789.230753	4.579731	1.056013
-793.146003	2.764653	1.061018
-797.087195	12.255594	1.066022
-800.626984	3.068278	1.071027
-804.328888	11.775090	1.076032
-808.214410	9.715590	1.081037
-811.854815	6.427907	1.086042
-815.592373	10.836991	1.091046
-819.042075	-0.545590	1.096051
-823.185657	5.640960	1.101056
-827.295922	15.447558	1.106061
-830.923738	6.149784	1.111066
-834.825402	17.512592	1.116070
-838.450195	3.956635	1.121075
-841.672964	17.109540	1.126080
-845.680812	4.906341	1.131085
-849.341821	6.269225	1.136090
-853.691042	13.201479	1.141094
-857.002538	2.157977	1.146099
-860.868413	7.024455	1.151104
-864.983797	14.157459	1.156109
-868.147505	7.403247	1.161114
-872.297840	12.740998	1.166118
-876.109336	-1.641312	1.171123
-879.553063	-1.251396	1.176128
-883.420586	3.463995	1.181133
-886.918491	-4.368983	1.186138
-890.925656	5.345535	1.191142
-894.552156	4.116807	1.196147
-898.230065	-3.539141	1.201152
-902.138540	0.414864	1.206157
-905.877457	-3.844073	1.211162
-909.779565	3.056205	1.216166
-913.486217	10.231163	1.221171
-917.399220	5.832925	1.226176
-921.305056	5.445255	1.231181
-924.648437	4.959765	1.236186
-928.570200	9.453672	1.241190
-932.197834	6.656139	1.246195
-936.007952	3.898833	1.251200
-940.045351	9.106676	1.256205
-943.609332	-0.300462	1.261210
-947.643323	16.016311	1.266214
-951.118596	5.915339	1.271219
-954.863206	7.548795	1.276224
-958.730268	11.322809	1.281229
-962.149734	0.331430	1.286234
-966.230553	16.286720	1.291238
-970.267956	5.808907	1.296243
-973.644872	1.782340	1.301248
-977.172818	13.828329	1.306253
-981.070468	2.568108	1.311258
-984.933657	10.236556	1.316262
-988.653114	14.403320	1.321267
-992.613403	14.167979	1.326272
-996.867996	12.287672	1.331277
-1000.053478	6.751366	1.336282
-1003.694281	3.728976	1.341286
-1007.204665	2.649007	1.346291
-1011.582822	13.802874	1.351296
-1015.425088	11.954420	1.356301
-1018.304828	6.219429	1.361306
-1022.737133	11.927385	1.366310
-1026.674413	2.887592	1.371315
-1029.998628	6.877659	1.376320
-1033.704267	14.104676	1.381325
-1037.208345	1.046982	1.386330
-1041.379786	12.393335	1.391334
-1045.115053	6.311113	1.396339
-1048.959581	4.526155	1.401344
-1053.015785	11.820316	1.406349
-1056.783994	8.477774	1.411354
-1060.229621	11.754036	1.416358
-1063.791284	6.352114	1.421363
-1067.427502	4.024516	1.426368
-1071.488286	8.141933	1.431373
-1075.355029	9.430849	1.436378
-1079.446676	20.346620	1.441382
-1082.994157	17.498655	1.446387
-1086.307680	8.728178	1.451392
-1090.353191	10.173449	1.456397
-1093.777400	-2.961579	1.461402
-1097.640102	-0.660888	1.466406
-1101.502806	1.821156	1.471411
-1105.398163	9.950671	1.476416
-1109.501170	16.314145	1.481421
-1112.663104	6.243723	1.486426
-1116.563419	8.957311	1.491430
-1120.388997	11.053408	1.496435
-1123.961667	5.322189	1.501440
-1128.110161	14.294898	1.506445
-1131.652762	4.883066	1.511450
-1135.572189	9.328053	1.516454
-1139.290667	1.541802	1.521459
-1142.857494	-2.462009	1.526464
-1146.609195	4.975968	1.531469
-1150.413283	2.758940	1.536474
-1154.408890	8.649571	1.541478
-1157.841137	20.082846	1.546483
-1161.557254	4.818472	1.551488
-1165.856508	5.831397	1.556493
-1169.272962	-1.310860	1.561498
-1173.186352	5.514376	1.566502
-1176.960636	8.209473	1.571507
-1180.202854	13.604284	1.576512
-1184.636818	9.572141	1.581517
-1187.836200	0.442944	1.586522
-1191.966398	9.274061	1.591526
-1195.747297	-0.370760	1.596531
-1199.356988	5.565419	1.601536
-1203.458355	16.470331	1.606541
-1206.681741	0.463304	1.611546
-1210.661656	8.459863	1.616550
-1214.250994	11.068654	1.621555
-1218.115705	8.516093	1.626560
-1222.225027	11.630727	1.631565
-1225.857144	3.840262	1.636570
-1229.655556	6.387920	1.641574
-1233.256968	8.565017	1.646579
-1236.841884	2.999940	1.651584
-1240.635986	11.725312	1.656589
-1244.527834	5.111831	1.661594
-1248.306944	9.785276	1.666598
-1252.192595	17.336321	1.671603
-1255.509773	-1.183425	1.676608
-1259.556467	11.425363	1.681613
-1262.971572	15.830842	1.686618
-1267.320734	10.990518	1.691622
-1270.816846	7.835012	1.696627
-1274.097551	8.035417	1.701632
-1278.668950	18.247727	1.706637
-1282.055302	5.501169	1.711642
-1285.957308	11.328152	1.716646
-1289.593679	5.430781	1.721651
-1293.308874	14.159374	1.726656
-1297.293694	5.632290	1.731661
-1300.963729	10.961706	1.736666
-1304.761687	16.232759	1.741670
-1308.754185	5.242195	1.746675
-1312.163502	6.549741	1.751680
-1316.226886	10.578108	1.756685
-1319.289519	0.635601	1.761690
-1323.260496	7.765183	1.766694
-1327.316780	6.456129	1.771699
-1330.949618	5.550795	1.776704
-1334.914675	11.585067	1.781709
-1338.581741	7.969764	1.786714
-1342.577696	9.940537	1.791718
-1345.928666	16.945674	1.796723
-1349.733876	14.511541	1.801728
-1353.648676	11.167730	1.806733
-1357.540986	8.088402	1.811738
-1361.212273	16.745417	1.816742
-1365.177094	16.541400	1.821747
-1368.592650	6.434693	1.826752
-1371.971808	5.965040	1.831757
-1375.404641	7.678558	1.836762
-1379.439488	11.800234	1.841766
-1383.626755	5.568604	1.846771
-1387.403568	-0.359734	1.851776
-1391.419989	13.012382	1.856781
-1395.096859	1.132524	1.861786
-1398.864480	14.725009	1.866790
-1402.612825	12.695014	1.871795
-1406.108310	6.950313	1.876800
-1410.581119	14.021625	1.881805
-1413.869160	1.576503	1.886810
-1417.782718	16.441305	1.891814
-1421.142469	6.855592	1.896819
-1424.472169	0.645994	1.901824
-1428.806423	13.351564	1.906829
-1432.182367	8.022993	1.911834
-1436.491131	17.862389	1.916838
-1440.178309	17.505235	1.921843
-1443.908802	12.235032	1.926848
-1447.927515	14.741053	1.931853
-1451.274730	12.982788	1.936858
-1455.036038	11.021186	1.941862
-1459.061106	11.505056	1.946867
-1462.665719	6.501727	1.951872
-1466.823120	16.506167	1.956877
-1470.112981	2.957580	1.961882
-1473.683216	13.378919	1.966886
-1477.662323	8.503396	1.971891
-1481.487308	5.508117	1.976896
-1485.315561	10.076271	1.981901
-1488.682480	11.656401	1.986906
-1492.601456	10.226305	1.991910
-1496.597040	16.604773	1.996915
-1500.753269	11.015853	2.006912
-1501.418149	10.922101	2.016909
-1498.722893	8.573890	2.026906
-1495.756962	6.152333	2.036902
-1494.132194	8.057127	2.046899
-1492.038545	7.246845	2.056896
-1490.028382	3.645743	2.066893
-1488.207849	5.550767	2.076890
-1486.257342	8.237079	2.086886
-1484.517328	10.202371	2.096883
-1482.251195	13.084453	2.106880
-1480.647337	10.328422	2.116877
-1478.587362	3.526739	2.126874
-1476.881048	6.681636	2.136870
-1475.101286	4.753224	2.146867
-1473.185549	3.074615	2.156864
-1470.775537	11.591002	2.166861
-1469.189208	5.106755	2.176858
-1467.284198	6.393536	2.186854
-1465.394456	4.008573	2.196851
-1463.537928	9.275730	2.206848
-1461.583040	2.242996	2.216845
-1459.814870	7.222727	2.226842
-1457.964011	12.661323	2.236838
-1456.169174	11.486822	2.246835
-1454.249610	9.327617	2.256832
-1452.129635	11.132615	2.266829
-1450.392679	9.904230	2.276826
-1448.458002	15.493622	2.286822
-1446.522851	5.764073	2.296819
-1444.742833	8.981403	2.306816
-1442.858600	10.573109	2.316813
-1440.823959	12.574939	2.326810
-1439.087945	11.788817	2.336806
-1437.057932	3.806181	2.346803
-1435.129336	6.713939	2.356800
-1433.598623	7.048584	2.366797
-1431.342445	6.873907	2.376794
-1429.819688	4.683526	2.386790
-1427.902541	8.016280	2.396787
-1425.797735	10.281624	2.406784
-1423.649613	5.569017	2.416781
-1422.130688	-4.101754	2.426778
-1420.252704	3.808302	2.436774
-1418.339722	2.682807	2.446771
-1416.568916	7.032155	2.456768
-1414.430639	4.043756	2.466765
-1412.766882	9.510770	2.476762
-1411.147475	7.732818	2.486758
-1409.094631	4.908102	2.496755
-1406.951470	8.141527	2.506752
-1405.060693	4.338560	2.516749
-1403.390098	6.957658	2.526746
-1401.322536	12.549498	2.536742
-1399.398417	5.976472	2.546739
-1397.629199	13.133447	2.556736
-1395.851624	6.446519	2.566733
-1393.899014	11.778879	2.576730
-1392.136912	10.298617	2.586726
-1390.132601	13.093241	2.596723
-1388.185536	7.424439	2.606720
-1386.580358	9.365607	2.616717
-1384.618288	6.688076	2.626714
-1382.778587	13.612727	2.636710
-1380.937547	11.221418	2.646707
-1378.680385	10.983477	2.656704
-1376.824673	12.098228	2.666701
-1374.963034	17.708855	2.676698
-1373.330300	16.014057	2.686694
-1371.655227	12.485647	2.696691
-1369.357687	11.164413	2.706688
-1367.526287	6.576773	2.716685
-1365.885713	9.025444	2.726682
-1364.072011	9.344829	2.736678
-1362.099426	8.364573	2.746675
-1359.976873	8.612410	2.756672
-1358.116694	10.705404	2.766669
-1356.258073	4.206055	2.776666
-1354.445928	5.872532	2.786662
-1352.729924	9.109659	2.796659
-1350.806479	8.340964	2.806656
-1348.814162	-0.235562	2.816653
-1346.633362	3.713470	2.826650
-1345.076380	1.298192	2.836646
-1343.431603	2.705684	2.846643
-1341.146583	5.251728	2.856640
-1339.543079	-1.582552	2.866637
-1337.675722	4.750341	2.876634
-1335.611536	-1.235586	2.886630
-1333.869442	-0.491032	2.896627
-1331.853563	3.282312	2.906624
-1329.937479	0.708505	2.916621
-1328.300854	8.657285	2.926618
-1326.365655	7.746202	2.936614
-1324.693954	9.048346	2.946611
-1322.411020	11.601061	2.956608
-1320.550686	6.966192	2.966605
-1318.703333	3.711820	2.976602
-1316.810592	7.482786	2.986598
-1315.296350	6.845940	2.996595
-1313.547266	7.197813	3.006592
-1311.316169	6.730427	3.016589
-1309.281983	8.970869	3.026586
-1307.330441	6.955085	3.036582
-1305.817697	8.757949	3.046579
-1303.699900	11.532906	3.056576
-1301.802930	3.126413	3.066573
-1300.199087	9.973626	3.076570
-1298.244708	7.537396	3.086566
-1296.132320	6.479555	3.096563
-1294.432175	1.949297	3.106560
-1292.579812	-2.209011	3.116557
-1290.644716	-0.914267	3.126554
-1288.880528	1.511515	3.136550
-1286.954735	7.208260	3.146547
-1284.844915	0.548757	3.156544
-1283.167683	0.410052	3.166541
-1281.180682	3.941750	3.176538
-1279.401798	7.522552	3.186534
-1277.326632	10.781197	3.196531
-1275.597421	4.149463	3.206528
-1273.895055	4.005162	3.216525
-1271.936868	6.189908	3.226522
-1270.041238	9.087297	3.236518
-1268.081560	9.103920	3.246515
-1266.077459	9.086593	3.256512
-1264.583511	7.112506	3.266509
-1262.553006	6.287274	3.276506
-1260.541143	9.309751	3.286502
-1258.858615	10.191791	3.296499
-1256.803846	6.969004	3.306496
-1254.718516	8.834995	3.316493
-1253.103091	12.486192	3.326490
-1251.485707	8.310259	3.336486
-1249.335281	9.477417	3.346483
-1247.597148	11.908983	3.356480
-1245.628347	8.407860	3.366477
-1243.580864	7.992031	3.376474
-1241.632072	-0.552184	3.386470
-1240.228628	11.555026	3.396467
-1237.953241	7.065370	3.406464
-1236.205910	10.468101	3.416461
-1234.356048	8.940753	3.426458
-1232.494300	9.006237	3.436454
-1230.710401	7.246293	3.446451
-1228.612464	4.109779	3.456448
-1226.951063	2.184707	3.466445
-1224.876692	1.834064	3.476442
-1222.998900	4.702769	3.486438
-1221.174587	9.162135	3.496435
-1219.289485	1.037075	3.506432
-1217.379853	8.367517	3.516429
-1215.442844	1.164150	3.526426
-1213.033335	4.457768	3.536422
-1211.400657	3.560457	3.546419
-1209.776492	9.479227	3.556416
-1208.055774	9.767826	3.566413
-1206.340224	14.252506	3.576410
-1204.298313	14.677602	3.586406
-1202.445543	10.669293	3.596403
-1200.486254	9.186040	3.606400
-1198.568044	10.063566	3.616397
-1196.654203	12.713368	3.626394
-1195.050175	9.068555	3.636390
-1193.340560	11.806304	3.646387
-1191.117771	12.450360	3.656384
-1189.064804	12.393700	3.666381
-1187.609785	10.841153	3.676378
-1185.792129	12.702674	3.686374
-1183.799630	10.214648	3.696371
-1181.609512	5.572901	3.706368
-1179.620754	10.073882	3.716365
-1177.961979	9.426628	3.726362
-1176.205966	4.593826	3.736358
-1174.390293	8.483036	3.746355
-1172.410776	8.809196	3.756352
-1170.447918	7.511712	3.766349
-1168.916451	6.660626	3.776346
-1166.560963	3.839795	3.786342
-1164.734242	2.208838	3.796339
-1162.887325	6.716740	3.806336
-1161.401390	2.814531	3.816333
-1159.508021	3.073960	3.826330
-1157.295633	2.022349	3.836326
-1155.626144	2.709182	3.846323
-1153.636096	7.094717	3.856320
-1151.804672	-1.381703	3.866317
-1149.808690	-3.450257	3.876314
-1147.933705	1.680005	3.886310
-1146.160950	3.916634	3.896307
-1144.213127	0.317899	3.906304
-1142.395741	1.078973	3.916301
-1140.557962	-0.875840	3.926298
-1138.589086	4.132040	3.936294
-1136.894042	5.624798	3.946291
-1134.942010	-5.362480	3.956288
-1132.927573	-1.955040	3.966285
-1130.973359	-0.247957	3.976282
-1129.187148	3.982317	3.986278
-1127.693297	3.364645	3.996275
-1125.335642	2.084558	4.006272
-1123.523284	-0.140911	4.016269
-1121.754871	-1.824085	4.026266
-1120.037529	-6.857499	4.036262
-1118.109597	-9.085664	4.046259
-1116.051856	-7.251449	4.056256
-1114.025919	2.435206	4.066253
-1112.214432	-1.899584	4.076250
-1110.878336	4.278505	4.086246
-1108.610167	4.432223	4.096243
-1106.894656	3.665416	4.106240
-1104.733230	1.658851	4.116237
-1102.692595	4.035815	4.126234
-1101.112576	5.510685	4.136230
-1099.417514	1.608214	4.146227
-1097.225149	-0.573820	4.156224
-1095.509356	-0.312771	4.166221
-1093.548033	2.506363	4.176218
-1091.795927	-1.994175	4.186214
-1089.921915	-2.664748	4.196211
-1087.349859	-3.368045	4.206208
-1085.395438	1.530089	4.216205
-1084.131323	-2.761322	4.226202
-1082.607880	3.991549	4.236198
-1080.453134	1.711339	4.246195
-1078.447652	-0.821307	4.256192
-1076.784854	0.547180	4.266189
-1074.926838	-4.933444	4.276186
-1072.809459	-4.266097	4.286182
-1071.241399	-6.147708	4.296179
-1069.235353	0.477442	4.306176
-1067.307954	-1.006915	4.316173
-1065.347922	-1.697545	4.326170
-1063.710477	0.390268	4.336166
-1061.911483	1.372242	4.346163
-1059.620938	1.994532	4.356160
-1057.828718	4.757064	4.366157
-1056.047535	3.465053	4.376154
-1054.360735	6.863398	4.386150
-1052.255015	6.122632	4.396147
-1050.432957	3.011457	4.406144
-1048.684701	6.463134	4.416141
-1046.838309	4.516488	4.426138
-1044.948361	3.961823	4.436134
-1042.759405	7.133009	4.446131
-1041.045112	2.201186	4.456128
-1039.032694	-1.333587	4.466125
-1037.169605	1.021309	4.476122
-1035.431446	7.799871	4.486118
-1033.410616	7.571648	4.496115
-1031.825159	5.777278	4.506112
-1029.851628	8.723989	4.516109
-1027.912772	-3.099526	4.526106
-1026.838872	1.232137	4.536102
-1024.330334	3.166434	4.546099
-1022.208744	4.845259	4.556096
-1020.445771	7.400921	4.566093
-1018.712577	9.798716	4.576090
-1016.546316	6.395668	4.586086
-1014.744379	11.270891	4.596083
-1012.969263	10.279882	4.606080
-1010.846758	5.958575	4.616077
-1009.181004	0.504012	4.626074
-1007.558424	2.932138	4.636070
-1005.660062	6.427735	4.646067
-1003.481778	9.638562	4.656064
-1001.308799	3.794981	4.666061
-999.734704	2.667186	4.676058
-998.044407	4.340805	4.686054
-996.022310	7.985567	4.696051
-994.324284	2.922167	4.706048
-992.207981	7.238707	4.716045
-990.005327	5.721440	4.726042
-988.440445	-0.836449	4.736038
-986.794758	3.727469	4.746035
-984.657521	-1.436169	4.756032
-983.117298	-1.158009	4.766029
-981.218472	3.408058	4.776026
-979.253511	-1.532233	4.786022
-977.127210	2.713247	4.796019
-975.194180	5.819640	4.806016
-973.454311	5.156403	4.816013
-971.725215	9.825416	4.826010
-969.577518	7.570115	4.836006
-967.908007	5.809713	4.846003
-966.043030	0.743317	4.856000
-964.038590	4.949878	4.865997
-962.257523	0.905851	4.875994
-960.316576	2.157307	4.885990
-958.779610	6.585476	4.895987
-956.467743	0.975513	4.905984
-955.005543	6.026694	4.915981
-953.018698	7.746080	4.925978
-950.837230	8.711185	4.935974
-948.948277	8.128335	4.945971
-947.314075	6.354646	4.955968
-945.358582	-3.061998	4.965965
-943.448707	1.540229	4.975962
-941.671367	-0.101608	4.985958
-939.794054	4.902147	4.995955
-937.690120	-3.766125	5.005952
-935.740808	-2.372302	5.015949
-934.320376	2.595571	5.025946
-932.172356	0.796569	5.035942
-930.292320	0.658844	5.045939
-928.716442	1.825022	5.055936
-926.594819	8.297615	5.065933
-924.477761	7.034097	5.075930
-922.812384	1.391756	5.085926
-921.126740	3.069333	5.095923
-919.165861	0.799742	5.105920
-916.805147	-0.527995	5.115917
-915.478824	-3.412955	5.125914
-913.631887	-0.834322	5.135910
-911.662208	-1.554788	5.145907
-909.702663	2.092158	5.155904
-907.771112	0.395687	5.165901
-905.867468	0.576312	5.175898
-904.420856	6.828441	5.185894
-902.390689	5.381468	5.195891
-900.330876	-0.481824	5.205888
-898.155577	-2.300947	5.215885
-896.414937	-0.103197	5.225882
-894.942604	0.436929	5.235878
-892.727708	3.733586	5.245875
-890.985583	-4.789953	5.255872
-888.950206	0.902254	5.265869
-887.249573	5.057988	5.275866
-885.528838	3.311558	5.285862
-883.470861	0.636470	5.295859
-881.352572	-2.645102	5.305856
-879.632433	5.211731	5.315853
-877.728769	-0.140259	5.325850
-876.128643	2.042078	5.335846
-874.304396	-0.606684	5.345843
-872.248772	-1.896648	5.355840
-870.184915	-0.898453	5.365837
-868.090304	-1.081489	5.375834
-866.731894	3.351609	5.385830
-864.937978	2.719284	5.395827
-862.588180	-1.410866	5.405824
-860.799312	-5.343961	5.415821
-859.043156	-3.819718	5.425818
-857.181701	-7.297046	5.435814
-855.186324	-2.728941	5.445811
-853.083393	-0.434345	5.455808
-851.754644	-3.550185	5.465805
-849.982485	5.796777	5.475802
-847.940104	0.631052	5.485798
-845.883305	-0.578551	5.495795
-843.941490	-4.116087	5.505792
-842.212054	-3.455980	5.515789
-840.196866	-2.800503	5.525786
-838.357896	-1.232641	5.535782
-836.521335	1.571925	5.545779
-834.598837	-6.825677	5.555776
-832.693428	-2.778431	5.565773
-830.784969	-3.310621	5.575770
-829.335529	1.161631	5.585766
-826.993967	4.357576	5.595763
-825.072419	-6.067238	5.605760
-823.573023	-6.047710	5.615757
-821.726533	-3.249457	5.625754
-819.625130	-2.719851	5.635750
-817.923333	-2.622150	5.645747
-815.616267	-0.818049	5.655744
-813.904609	0.365975	5.665741
-812.103319	-0.515384	5.675738
-810.451731	-1.473863	5.685734
-808.485499	-1.947376	5.695731
-806.473361	-4.461913	5.705728
-804.295899	-3.483399	5.715725
-802.630867	-2.579282	5.725722
-801.033067	-1.598101	5.735718
-799.186940	-3.895040	5.745715
-797.316701	-5.883200	5.755712
-795.263474	-2.914290	5.765709
-793.217293	-2.716886	5.775706
-791.611467	-1.451191	5.785702
-789.727992	2.436968	5.795699
-787.618551	1.389526	5.805696
-785.897150	-4.264839	5.815693
-783.942384	-0.298072	5.825690
-782.067778	0.019926	5.835686
-780.140689	0.612169	5.845683
-778.413372	-1.588395	5.855680
-776.405902	-2.456895	5.865677
-774.437654	-8.883341	5.875674
-772.991839	-5.323106	5.885670
-771.322778	-6.232245	5.895667
-768.947822	-4.186318	5.905664
-766.873906	1.248789	5.915661
-765.144102	-4.451116	5.925658
-763.566142	-0.932523	5.935654
-761.421395	-2.061375	5.945651
-759.439917	-3.645707	5.955648
-757.741311	-2.423240	5.965645
-755.863853	-2.171993	5.975642
-753.874423	-2.177062	5.985638
-752.200449	-0.339600	5.995635
-750.229051	1.289271	6.005632
-748.382153	-3.535653	6.015629
-746.473167	0.697412	6.025626
-744.800377	0.791908	6.035622
-742.714750	3.796741	6.045619
-740.579311	0.109917	6.055616
-739.063425	-1.281560	6.065613
-737.033266	-0.011018	6.075610
-735.275502	-3.286946	6.085606
-733.047254	-2.573852	6.095603
-731.499453	1.818008	6.105600
-729.760802	-4.298551	6.115597
-727.842995	-1.967937	6.125594
-725.530817	3.114918	6.135590
-723.873318	9.600310	6.145587
-722.160828	2.767933	6.155584
-720.144522	2.104910	6.165581
-718.371392	6.580767	6.175578
-716.651629	1.114604	6.185574
-714.757386	1.386886	6.195571
-712.473243	-3.488946	6.205568
-710.767558	1.444538	6.215565
-708.583078	2.818337	6.225562
-707.261464	4.159513	6.235558
-705.341131	3.166051	6.245555
-703.204867	-0.839821	6.255552
-701.534241	-0.306000	6.265549
-699.834594	6.625832	6.275546
-697.682200	9.012141	6.285542
-695.522503	4.069369	6.295539
-693.798686	-4.627960	6.305536
-692.325547	5.550084	6.315533
-690.493837	0.426049	6.325530
-688.390286	7.062815	6.335526
-686.317818	10.505595	6.345523
-684.639133	7.752340	6.355520
-682.426429	5.092168	6.365517
-680.388654	2.305216	6.375514
-679.052388	7.665658	6.385510
-677.407272	4.344613	6.395507
-675.136350	2.074619	6.405504
-673.070058	2.914705	6.415501
-671.400961	0.211940	6.425498
-669.575085	3.143086	6.435494
-667.853606	9.559877	6.445491
-665.888518	3.040855	6.455488
-663.776359	0.922558	6.465485
-662.051369	5.819838	6.475482
-660.181846	2.996631	6.485478
-658.046870	2.063644	6.495475
-656.277816	6.631782	6.505472
-654.768285	5.302951	6.515469
-652.658765	-1.139664	6.525466
-650.752839	3.722395	6.535462
-648.976836	13.878923	6.545459
-647.112550	11.904460	6.555456
-645.009783	12.195583	6.565453
-643.225267	4.660165	6.575450
-641.209670	4.467850	6.585446
-639.739685	9.276422	6.595443
-637.898201	10.114567	6.605440
-635.761323	9.309191	6.615437
-633.706582	11.400111	6.625434
-632.044974	3.611181	6.635430
-630.117283	10.347158	6.645427
-628.222415	9.124141	6.655424
-626.414671	6.050302	6.665421
-624.337832	5.594005	6.675418
-622.814552	8.562487	6.685414
-620.776091	9.831806	6.695411
-618.793459	6.058974	6.705408
-616.930455	2.993682	6.715405
-615.167053	3.459056	6.725402
-612.973374	4.383052	6.735398
-611.659675	8.130294	6.745395
-609.644845	1.238630	6.755392
-607.729118	-2.880344	6.765389
-605.590459	0.507721	6.775386
-603.686630	3.446991	6.785382
-601.933052	-0.590809	6.795379
-600.244296	-5.900359	6.805376
-598.276748	1.366118	6.815373
-596.420564	-1.980700	6.825370
-594.617993	0.993703	6.835366
-592.530055	-1.996981	6.845363
-590.700700	-0.203174	6.855360
-588.608850	-4.111851	6.865357
-587.121568	-4.950767	6.875354
-585.298116	-2.701274	6.885350
-583.324707	4.629018	6.895347
-581.381194	6.917755	6.905344
-579.263638	3.611295	6.915341
-577.632653	5.169963	6.925338
-575.821094	8.436632	6.935334
-573.955740	0.282029	6.945331
-572.076394	1.690494	6.955328
-569.733517	3.781225	6.965325
-567.901285	2.928264	6.975322
-566.494572	0.392226	6.985318
-564.626191	2.599821	6.995315
-562.428320	-0.313664	7.005312
-560.546394	-0.104027	7.015309
-559.076979	4.486793	7.025306
-557.335582	6.291521	7.035302
-555.031934	4.306938	7.045299
-553.129719	0.976482	7.055296
-551.497922	-3.116038	7.065293
-549.474110	1.138325	7.075290
-547.171917	0.339777	7.085286
-545.801577	4.084325	7.095283
-543.966583	-1.674870	7.105280
-541.814522	1.426903	7.115277
-540.095410	-3.219561	7.125274
-538.334041	0.666209	7.135270
-536.291947	-4.030268	7.145267
-534.271914	-2.296877	7.155264
-532.479273	-3.877700	7.165261
-530.809219	-4.081039	7.175258
-528.885378	0.921947	7.185254
-526.942634	-1.773907	7.195251
-525.400443	1.310040	7.205248
-523.116455	-4.459283	7.215245
-520.890890	-0.328702	7.225242
-519.393576	-4.139191	7.235238
-517.781908	-6.603730	7.245235
-515.622212	-4.581579	7.255232
-513.647323	-7.734138	7.265229
-511.690652	-5.370078	7.275226
-510.453376	-3.549526	7.285222
-508.312628	1.545146	7.295219
-506.110791	-1.027867	7.305216
-504.545005	-0.125053	7.315213
-502.442905	-6.413200	7.325210
-500.581691	-0.568078	7.335206
-498.829994	2.793477	7.345203
-496.741258	-2.782003	7.355200
-495.142988	-6.659129	7.365197
-492.958173	-7.699404	7.375194
-491.290026	-0.561851	7.385190
-489.477313	-3.380591	7.395187
-487.651786	2.705508	7.405184
-485.673744	0.332470	7.415181
-483.602760	-0.163823	7.425178
-481.847270	7.632426	7.435174
-480.173830	0.815916	7.445171
-478.230558	-6.506322	7.455168
-476.467527	-1.417606	7.465165
-474.372461	-2.517740	7.475162
-472.525942	4.059232	7.485158
-470.598386	-1.417851	7.495155
-468.702106	1.178525	7.505152
-466.848773	-2.447217	7.515149
-465.113213	0.219043	7.525146
-463.207255	7.950221	7.535142
-461.310368	3.640154	7.545139
-459.220951	6.545167	7.555136
-457.260359	-0.719824	7.565133
-455.621556	2.366109	7.575130
-453.651907	-3.780845	7.585126
-451.943440	-0.393403	7.595123
-450.360234	-3.994937	7.605120
-448.251023	-1.293604	7.615117
-446.223528	-2.660819	7.625114
-444.362452	0.913836	7.635110
-442.536948	-0.623222	7.645107
-440.551907	-3.962082	7.655104
-438.638491	-3.297903	7.665101
-436.815909	-0.287097	7.675098
-435.205168	-3.504596	7.685094
-432.965928	3.080743	7.695091
-431.065975	-1.525055	7.705088
-429.305971	-5.653762	7.715085
-427.594331	-4.131555	7.725082
-425.597560	-7.677541	7.735078
-424.110195	-5.841619	7.745075
-421.952723	-5.495877	7.755072
-419.786102	-6.654760	7.765069
-418.049644	-1.947019	7.775066
-415.936025	-2.677432	7.785062
-414.332320	-9.612234	7.795059
-412.566259	-7.814496	7.805056
-410.819082	-8.127962	7.815053
-408.657635	-4.861775	7.825050
-407.038804	1.102661	7.835046
-404.935186	-0.204043	7.845043
-402.865815	-8.635842	7.855040
-401.161290	-8.118275	7.865037
-399.254931	-0.816585	7.875034
-397.481727	-4.611059	7.885030
-395.939441	-1.828621	7.895027
-393.536556	-5.898909	7.905024
-391.636444	-6.194151	7.915021
-390.219703	-5.066934	7.925018
-388.034897	-3.451308	7.935014
-386.302036	-6.195642	7.945011
-384.109954	-1.969581	7.955008
-382.530733	-4.450956	7.965005
-380.605438	-8.200230	7.975002
-378.914634	-1.227262	7.984998
-376.609578	0.628122	7.994995
-375.101112	-0.360889	8.004992
-372.805501	-0.094003	8.014989
-371.280226	7.977520	8.024986
-369.603744	3.600082	8.034982
-367.447893	1.601381	8.044979
-365.470704	0.794902	8.054976
-363.847625	-2.563471	8.064973
-361.854234	0.473805	8.074970
-359.948374	-2.913928	8.084966
-357.971801	3.538164	8.094963
-356.181001	-1.459100	8.104960
-354.310271	1.727243	8.114957
-352.006255	-1.575637	8.124954
-350.401381	1.972108	8.134950
-349.075688	0.153343	8.144947
-346.710261	-3.729340	8.154944
-344.908556	-5.320946	8.164941
-343.069392	-4.539044	8.174938
-341.342828	4.382996	8.184934
-339.508154	-0.269154	8.194931
-337.421289	-1.645757	8.204928
-335.509052	-3.081319	8.214925
-333.658632	-1.919099	8.224922
-331.754795	-4.089111	8.234918
-329.859067	-0.085682	8.244915
-327.945050	-7.747352	8.254912
-326.193324	-3.405138	8.264909
-324.365789	3.078674	8.274906
-322.456789	1.907324	8.284902
-320.546347	-2.636908	8.294899
-318.565645	-2.777590	8.304896
-316.871537	-5.758848	8.314893
-314.956295	-3.909063	8.324890
-313.224736	-1.998372	8.334886
-311.225368	0.531148	8.344883
-308.911237	-0.952767	8.354880
-307.598616	-6.961555	8.364877
-305.489162	0.067792	8.374874
-303.639828	2.280217	8.384870
-301.790273	5.428931	8.394867
-299.993102	4.245452	8.404864
-297.857139	7.007390	8.414861
-296.089697	5.383394	8.424858
-294.250497	-1.481568	8.434854
-292.515778	3.442867	8.444851
-290.485863	-0.427254	8.454848
-288.592261	0.304947	8.464845
-286.964747	-2.187236	8.474842
-285.180486	6.641956	8.484838
-283.061585	3.596062	8.494835
-281.100884	5.050194	8.504832
-279.105670	3.524060	8.514829
-277.223628	-5.078266	8.524826
-275.557427	4.230835	8.534822
-273.628952	4.180633	8.544819
-271.793503	8.399001	8.554816
-270.033111	4.432972	8.564813
-268.017028	6.029855	8.574810
-266.082328	4.106020	8.584807
-264.231684	3.935618	8.594803
-262.364650	4.841031	8.604800
-260.546701	2.550571	8.614797
-258.911245	-1.597611	8.624794
-256.980262	6.006595	8.634791
-254.747169	-4.301768	8.644787
-252.895208	1.164512	8.654784
-250.808378	0.678522	8.664781
-249.145366	3.005996	8.674778
-247.527002	6.486924	8.684775
-245.341088	0.144550	8.694771
-243.632584	0.176854	8.704768
-241.706485	4.429722	8.714765
-240.217065	2.597512	8.724762
-237.763165	-0.560239	8.734759
-235.910683	0.781731	8.744755
-234.287023	2.643388	8.754752
-232.470351	1.638426	8.764749
-230.828495	6.797209	8.774746
-228.480838	8.394884	8.784743
-226.457636	1.396387	8.794739
-224.999224	-4.948268	8.804736
-223.048915	9.857678	8.814733
-220.989016	5.294398	8.824730
-219.366603	4.394664	8.834727
-217.264538	6.268395	8.844723
-215.249953	6.422393	8.854720
-213.574910	2.286867	8.864717
-212.046851	7.699092	8.874714
-209.647446	0.403717	8.884711
-207.769957	2.652777	8.894707
-206.241511	-1.045657	8.904704
-204.481609	-4.185764	8.914701
-202.116036	7.945480	8.924698
-200.410302	-4.236580	8.934695
-198.840954	-3.229921	8.944691
-196.801195	2.339065	8.954688
-194.694514	1.458372	8.964685
-192.811187	-3.585125	8.974682
-191.314273	2.544194	8.984679
-189.212169	2.567401	8.994675
-187.200554	2.935056	9.004672
-185.368732	-5.258136	9.014669
-183.682580	-1.004820	9.024666
-181.633041	3.657875	9.034663
-179.746330	-2.535637	9.044659
-177.678057	-7.676535	9.054656
-175.960837	-5.971877	9.064653
-174.221129	-3.793960	9.074650
-172.276564	-3.802437	9.084647
-170.364037	-4.533701	9.094643
-168.709693	-7.270091	9.104640
-166.832625	-1.040373	9.114637
-165.047986	-8.820227	9.124634
-162.533465	1.826747	9.134631
-161.205170	-1.088132	9.144627
-159.227934	-5.930274	9.154624
-157.393753	-2.322673	9.164621
-155.284868	1.800043	9.174618
-153.466222	-0.559923	9.184615
-151.679008	-2.106444	9.194611
-149.853512	-6.141199	9.204608
-148.007369	-6.899746	9.214605
-146.266220	-1.418852	9.224602
-143.964944	-7.422704	9.234599
-142.290571	-1.787465	9.244595
-140.407586	-10.123002	9.254592
-138.293292	-13.788567	9.264589
-136.871113	-10.626786	9.274586
-134.893013	-6.367919	9.284583
-132.843891	-4.866195	9.294579
-131.094253	0.384407	9.304576
-129.243847	-3.973259	9.314573
-127.056991	-8.801457	9.324570
-125.461102	-12.169547	9.334567
-123.739768	-3.347553	9.344563
-121.813064	-3.539457	9.354560
-119.738604	-6.829175	9.364557
-117.975766	-2.820155	9.374554
-116.014081	-0.393402	9.384551
-114.049618	-8.299814	9.394547
-112.311697	-3.419964	9.404544
-110.355775	0.465094	9.414541
-108.527866	-3.903178	9.424538
-106.697015	0.876586	9.434535
-104.629107	0.471109	9.444531
-102.942538	-5.455146	9.454528
-101.005803	-0.657537	9.464525
-99.289723	-4.362162	9.474522
-97.348771	-7.106343	9.484519
-95.559575	-4.350470	9.494515
-93.657233	-2.782659	9.504512
-91.408066	-4.931799	9.514509
-89.718422	-10.331161	9.524506
-88.032968	-1.948679	9.534503
-85.950810	-11.171755	9.544499
-84.038522	-9.665525	9.554496
-82.384390	-9.223375	9.564493
-80.242777	-2.314209	9.574490
-78.386704	-1.856909	9.584487
-76.868540	4.867526	9.594483
-74.607004	9.076490	9.604480
-72.956987	8.529294	9.614477
-71.099392	6.834231	9.624474
-69.186387	3.876632	9.634471
-67.450217	1.193568	9.644467
-65.310995	-1.481170	9.654464
-63.340716	6.367993	9.664461
-61.621758	6.438232	9.674458
-59.913045	6.026945	9.684455
-57.964903	9.292759	9.694451
-55.778950	13.768014	9.704448
-54.196153	8.084134	9.714445
-52.294329	13.796842	9.724442
-50.264603	8.362187	9.734439
-48.541659	10.050238	9.744435
-46.566189	6.708475	9.754432
-44.858940	8.806405	9.764429
-42.653569	-1.006308	9.774426
-41.192530	4.047249	9.784423
-39.448253	3.203982	9.794419
-37.163641	6.725609	9.804416
-35.181778	6.291286	9.814413
-33.517277	4.278107	9.824410
-31.639232	4.510884	9.834407
-29.826206	13.217282	9.844403
-27.513715	6.832788	9.854400
-26.181986	4.449540	9.864397
-24.126602	5.162457	9.874394
-22.077601	6.957984	9.884391
-20.408861	11.108413	9.894387
-18.571113	6.035993	9.904384
-16.445042	4.724461	9.914381
-14.652421	6.401420	9.924378
-12.906330	7.035792	9.934375
-11.170103	5.371189	9.944371
-9.368743	9.959947	9.954368
-7.331112	10.809923	9.964365
-6.043932	30.562995	9.974362
-4.507501	60.227000	9.984359
-2.753896	99.046050	9.994355
-1.270948	139.451044	10.004352
0.000000	184.364033	10.009357
1.056467	210.929947	10.014362
1.458136	228.674718	10.019367
2.346230	245.337383	10.024371
2.255460	260.956144	10.029376
2.756001	264.498746	10.034381
2.914034	276.652648	10.039386
2.806714	287.762354	10.044391
3.279558	279.034204	10.049395
2.859539	275.773934	10.054400
3.125417	269.986746	10.059405
3.245411	280.607594	10.064410
3.001986	288.373748	10.069415
3.523789	278.196433	10.074419
3.427593	284.776868	10.079424
3.595386	288.307901	10.084429
3.454795	291.889707	10.089434
3.235953	299.390168	10.094439
3.721653	297.071946	10.099443
3.568713	295.942140	10.104448
3.666190	295.067280	10.109453
3.920589	296.813555	10.114458
3.779893	304.251089	10.119463
4.234491	300.985334	10.124467
4.144883	301.280474	10.129472
4.037421	289.181849	10.134477
4.097780	281.678575	10.139482
3.601953	279.867021	10.144487
3.842219	275.906900	10.149491
3.840702	277.097901	10.154496
3.976578	278.448337	10.159501
3.847181	282.324825	10.164506
3.927490	286.508489	10.169511
4.260769	290.779534	10.174515
4.343971	304.139167	10.179520
4.158929	297.406751	10.184525
4.256684	289.949548	10.189530
4.175891	294.147874	10.194535
4.574645	294.134870	10.199539
4.469536	290.795975	10.204544
3.934807	287.520884	10.209549
4.160377	300.897228	10.214554
4.277045	315.325455	10.219559
4.998353	312.289968	10.224563
4.661762	320.681293	10.229568
4.824204	313.831935	10.234573
4.956775	316.493370	10.239578
4.810750	311.046269	10.244583
5.162089	315.077894	10.249587
4.689453	304.008929	10.254592
4.466228	297.191138	10.259597
4.451120	301.716461	10.264602
4.786539	315.075295	10.269607
5.081045	321.389992	10.274611
4.775850	320.426399	10.279616
5.094489	329.624699	10.284621
5.017416	326.953116	10.289626
4.771992	336.511065	10.294631
5.211790	319.925337	10.299635
4.827069	328.508850	10.304640
5.149449	319.711637	10.309645
5.261630	331.078102	10.314650
5.232818	332.945255	10.319655
5.474818	334.991562	10.324659
5.300691	345.003352	10.329664
5.720878	348.270206	10.334669
5.729121	344.536317	10.339674
5.433785	344.657691	10.344679
5.706205	336.362033	10.349683
5.577876	353.412475	10.354688
5.714994	352.882957	10.359693
5.929105	352.807943	10.364698
5.585670	364.169842	10.369703
6.147883	356.881369	10.374707
6.025301	360.293159	10.379712
6.095354	360.293165	10.384717
6.105270	357.721243	10.389722
5.619043	358.611097	10.394727
6.014854	353.202126	10.399731
5.939756	359.864388	10.404736
5.995430	354.530177	10.409741
6.038884	370.178107	10.414746
5.888204	368.084396	10.419751
6.130730	364.404594	10.424755
5.712280	376.011863	10.429760
5.869482	377.103435	10.434765
6.439219	391.702319	10.439770
6.641239	398.854990	10.444775
6.955207	386.783675	10.449779
6.565795	382.744197	10.454784
6.674969	375.245704	10.459789
6.658665	375.418762	10.464794
6.740069	376.713240	10.469799
6.560773	373.597477	10.474803
6.525335	385.503207	10.479808
6.754376	393.627720	10.484813
7.088101	408.328927	10.489818
6.959828	404.334519	10.494823
7.373616	400.047056	10.499827
7.171420	400.808022	10.504832
6.966693	379.516807	10.509837
6.734463	378.940548	10.514842
6.900110	407.919793	10.519847
7.488563	395.400976	10.524851
7.295774	405.330627	10.529856
7.182498	408.200035	10.534861
7.348909	408.902201	10.539866
7.356583	413.425502	10.544871
7.517570	408.785694	10.549875
7.466222	417.677209	10.554880
7.534322	410.775044	10.559885
7.277719	412.609158	10.564890
7.324618	424.269968	10.569895
7.604018	411.568620	10.574899
7.515135	423.090237	10.579904
7.210881	424.391045	10.584909
7.386987	422.730910	10.589914
7.053137	426.960181	10.594919
7.529344	429.185188	10.599923
7.490984	445.518049	10.604928
7.570925	444.098762	10.609933
7.845010	446.848037	10.614938
7.823847	456.848118	10.619943
8.218057	453.875823	10.624947
8.057152	458.640500	10.629952
7.968639	457.274893	10.634957
8.090089	455.833214	10.639962
8.057201	465.108177	10.644967
8.315210	453.999815	10.649971
8.240902	463.161533	10.654976
7.916639	460.259692	10.659981
8.521933	462.910402	10.664986
8.376537	482.393868	10.669991
8.769338	467.998033	10.674995
8.473845	470.812940	10.680000
8.468551	465.398526	10.685005
8.652950	475.831042	10.690010
8.510203	493.765490	10.695015
8.797961	489.360908	10.700019
8.971928	494.643051	10.705024
8.987212	492.568581	10.710029
8.704175	480.207636	10.715034
8.651092	488.028690	10.720039
9.406195	490.532503	10.725043
9.238618	478.284032	10.730048
8.885027	468.038066	10.735053
9.021449	467.335185	10.740058
8.758060	474.516403	10.745063
9.001090	481.175282	10.750067
9.068704	493.503067	10.755072
9.302959	499.898418	10.760077
9.541419	503.620087	10.765082
9.221728	507.345636	10.770087
9.466557	502.651422	10.775091
9.524830	514.338088	10.780096
9.314392	509.092004	10.785101
9.533699	498.686027	10.790106
9.378549	507.057976	10.795111
9.797871	499.328590	10.800115
9.468648	500.235984	10.805120
9.694620	499.458891	10.810125
9.877214	507.696536	10.815130
9.244022	511.807208	10.820135
9.558850	503.373011	10.825139
9.876674	505.194353	10.830144
9.681890	513.210707	10.835149
9.746007	513.577525	10.840154
9.511849	508.518945	10.845159
9.745401	507.351123	10.850163
9.822738	529.602238	10.855168
9.713278	536.549191	10.860173
10.318952	531.240723	10.865178
10.146878	538.133008	10.870183
10.263633	532.713292	10.875187
10.210849	540.080150	10.880192
10.213150	542.883838	10.885197
10.402859	539.109913	10.890202
10.574495	541.763582	10.895207
10.411603	534.742083	10.900211
10.483548	542.973744	10.905216
10.378379	542.184815	10.910221
10.537344	538.149281	10.915226
10.203411	546.190215	10.920231
10.911903	537.966811	10.925235
10.841171	545.405923	10.930240
10.939684	538.039939	10.935245
10.682924	542.567614	10.940250
10.616740	541.882856	10.945255
10.877354	545.328181	10.950259
10.758334	549.499562	10.955264
10.565630	544.499802	10.960269
10.990610	545.461936	10.965274
10.938174	567.095912	10.970279
11.105565	570.016777	10.975283
11.218009	580.992299	10.980288
10.864102	586.010164	10.985293
11.146150	584.101292	10.990298
10.951460	583.343988	10.995303
11.392667	578.213132	11.000307
11.250969	585.923791	11.005312
11.245813	588.930535	11.010317
11.554478	589.841838	11.015322
11.321789	587.483623	11.020327
11.626716	586.660813	11.025331
11.600466	587.109860	11.030336
11.604210	588.960814	11.035341
11.638210	580.718820	11.040346
11.590573	583.984660	11.045351
11.678899	579.726986	11.050355
11.518782	589.456001	11.055360
11.607025	603.814930	11.060365
11.963306	611.480860	11.065370
11.878634	617.849865	11.070375
12.001903	617.357241	11.075379
11.909425	624.459228	11.080384
12.149278	622.378878	11.085389
12.087409	618.854807	11.090394
11.872712	626.219151	11.095399
12.199905	620.016753	11.100403
12.312205	621.348904	11.105408
12.221169	625.033276	11.110413
12.471471	624.381610	11.115418
12.331897	630.106496	11.120423
12.781774	616.776933	11.125427
12.758876	626.941417	11.130432
12.669010	626.386594	11.135437
12.887909	627.703318	11.140442
12.492228	623.273672	11.145447
12.671218	617.254194	11.150451
12.444063	629.930326	11.155456
12.298915	633.005143	11.160461
12.578289	622.823683	11.165466
12.350455	630.365173	11.170471
12.242518	623.905743	11.175475
12.369891	643.084128	11.180480
13.000132	646.185074	11.185485
13.138110	646.828707	11.190490
12.598306	657.354801	11.195495
12.466762	653.376616	11.200499
12.952526	659.642028	11.205504
12.917853	671.620414	11.210509
13.280202	660.235043	11.215514
13.232223	664.019794	11.220519
13.026611	657.615356	11.225523
13.062242	672.790178	11.230528
13.373730	684.224479	11.235533
13.644626	685.659076	11.240538
13.441022	693.471134	11.245543
14.043452	679.543144	11.250547
13.422020	675.666755	11.255552
13.469730	687.335532	11.260557
13.400309	687.854549	11.265562
13.518736	691.000879	11.270567
13.566139	698.203595	11.275571
13.591884	695.073978	11.280576
13.669697	695.649936	11.285581
13.936287	694.981476	11.290586
13.571699	703.842706	11.295591
13.907112	693.822576	11.300595
13.789337	696.102953	11.305600
13.878607	695.347656	11.310605
14.264004	694.658667	11.315610
13.995736	698.120583	11.320615
13.975055	691.364918	11.325619
13.890084	708.047722	11.330624
14.180076	718.767935	11.335629
14.392224	716.756650	11.340634
14.234397	734.107147	11.345639
14.301198	719.316771	11.350643
14.635384	725.951759	11.355648
14.226604	733.963733	11.360653
14.493176	725.925842	11.365658
14.619561	737.974789	11.370663
14.523509	733.229218	11.375667
14.638181	733.436583	11.380672
14.392677	731.995063	11.385677
14.763645	727.280655	11.390682
14.400327	731.749690	11.395687
14.502934	735.444203	11.400691
14.591394	740.847315	11.405696
14.712243	762.517021	11.410701
15.222144	759.346429	11.415706
15.308050	766.153511	11.420711
15.300027	758.711365	11.425715
14.970113	747.084679	11.430720
14.907781	763.984720	11.435725
15.311006	758.479797	11.440730
15.069405	765.914738	11.445735
15.145671	763.906198	11.450739
15.348821	768.133487	11.455744
15.249536	767.053433	11.460749
15.434005	772.463320	11.465754
15.258051	779.059856	11.470759
15.015021	765.236687	11.475763
15.356280	769.787314	11.480768
15.362008	772.330290	11.485773
15.730832	764.705019	11.490778
15.278759	774.200018	11.495783
15.549255	772.548443	11.500787
15.839369	788.021853	11.505792
15.694792	797.622365	11.510797
15.930726	802.724418	11.515802
15.576331	805.996661	11.520807
15.603889	809.982300	11.525811
15.934305	812.471912	11.530816
15.969844	816.694411	11.535821
16.199101	808.488954	11.540826
16.046821	816.199846	11.545831
16.128956	806.530716	11.550835
16.331414	811.808431	11.555840
16.160487	815.718495	11.560845
16.338870	805.694951	11.565850
16.241463	810.397572	11.570855
16.238046	805.837483	11.575859
16.097687	813.978579	11.580864
15.976706	812.484069	11.585869
16.399182	816.032956	11.590874
16.252095	828.202876	11.595879
16.466510	836.322086	11.600883
16.621022	835.345052	11.605888
16.399939	849.908118	11.610893
16.606004	846.022689	11.615898
16.467178	845.675951	11.620903
16.541633	845.178490	11.625907
16.605829	839.267124	11.630912
16.492809	844.202494	11.635917
16.895788	835.377921	11.640922
16.969501	866.826615	11.645927
16.777431	878.112725	11.650931
17.233469	878.896455	11.655936
17.238489	883.743619	11.660941
17.432412	872.367603	11.665946
17.228380	877.120372	11.670951
17.379194	870.651098	11.675955
16.958628	863.222664	11.680960
17.174459	872.896628	11.685965
17.592664	863.197508	11.690970
17.504782	879.357396	11.695975
17.360289	880.197495	11.700979
17.489013	885.007578	11.705984
17.420397	883.072599	11.710989
17.534092	884.764118	11.715994
17.484196	884.053089	11.720999
17.708117	871.609364	11.726003
17.793887	873.694864	11.731008
17.695168	876.685051	11.736013
17.735146	877.880521	11.741018
17.518035	882.723693	11.746023
17.618941	877.902498	11.751027
17.633610	879.226592	11.756032
17.555520	886.714363	11.761037
17.913051	892.509873	11.766042
17.861062	912.229763	11.771047
18.013225	906.184482	11.776051
18.250343	910.731265	11.781056
17.727121	913.360220	11.786061
18.037325	913.195756	11.791066
18.109752	920.703691	11.796071
17.699711	923.213662	11.801075
18.267045	920.573224	11.806080
18.723662	941.445272	11.811085
18.842562	929.087640	11.816090
18.710078	925.292467	11.821095
18.683227	909.389249	11.826099
18.598511	914.586648	11.831104
18.397145	912.832122	11.836109
18.594494	915.992721	11.841114
18.563801	915.773820	11.846119
18.580310	924.173822	11.851123
18.983434	943.494708	11.856128
18.815325	938.197557	11.861133
19.225086	936.369199	11.866138
18.870830	944.348934	11.871143
19.125564	945.631585	11.876147
19.071145	949.307044	11.881152
18.660902	954.584771	11.886157
19.034043	950.295749	11.891162
18.953716	948.842051	11.896167
19.111804	944.916939	11.901171
19.339371	945.445364	11.906176
19.083738	950.706311	11.911181
19.104892	938.506198	11.916186
18.911455	951.858514	11.921191
19.048941	949.559469	11.926195
19.291673	951.768186	11.931200
19.533031	968.386617	11.936205
19.402581	968.905916	11.941210
19.795426	980.381094	11.946215
19.738040	966.360953	11.951219
20.016748	974.471562	11.956224
19.552549	969.030809	11.961229
19.885683	971.116291	11.966234
19.709655	971.650746	11.971239
19.570371	981.856123	11.976243
19.943746	971.052261	11.981248
19.675913	983.700493	11.986253
19.700309	971.518760	11.991258
19.917556	980.288921	11.996263
19.953352	974.259021	12.001267
20.240851	971.518124	12.006272
19.590648	980.368307	12.011277
19.958666	982.612240	12.016282
20.191761	1003.122615	12.021287
20.158303	1005.859551	12.026291
20.570444	1001.663648	12.031296
20.090603	996.495055	12.036301
20.088721	988.376834	12.041306
20.328909	996.908365	12.046311
20.275972	994.638111	12.051315
20.309861	982.869619	12.056320
20.334441	982.738100	12.061325
20.495629	979.049041	12.066330
20.126501	982.435644	12.071335
20.253368	991.295927	12.076339
20.448427	979.438646	12.081344
19.963154	988.664673	12.086349
20.061984	984.526638	12.091354
20.225393	984.869744	12.096359
19.984697	989.688326	12.101363
20.217241	981.444398	12.106368
20.260393	990.160330	12.111373
20.686716	973.107628	12.116378
20.404963	990.817264	12.121383
20.123328	981.226548	12.126387
20.484742	979.916861	12.131392
20.274408	984.347374	12.136397
20.531522	983.260918	12.141402
20.630402	987.678380	12.146407
20.352050	970.646618	12.151411
20.328660	964.293406	12.156416
19.952859	962.995656	12.161421
20.380103	959.339860	12.166426
19.944851	964.284091	12.171431
19.909346	967.658476	12.176435
20.474517	975.706043	12.181440
20.126220	977.118008	12.186445
20.029323	968.715314	12.191450
19.882351	973.309192	12.196455
20.334856	978.226941	12.201459
20.442177	974.786188	12.206464
20.156139	985.426586	12.211469
20.176564	966.934132	12.216474
20.324132	975.251752	12.221479
20.038110	973.540686	12.226483
20.389674	974.826819	12.231488
20.395139	976.534036	12.236493
20.133408	976.238440	12.241498
20.261778	969.260161	12.246503
20.180617	971.534740	12.251507
20.028256	968.266307	12.256512
20.150978	969.844425	12.261517
20.378898	957.511959	12.266522
20.320421	972.266841	12.271527
20.083922	978.124026	12.276531
20.434703	973.198282	12.281536
20.006032	965.704851	12.286541
20.287872	967.839518	12.291546
20.124531	966.411677	12.296551
20.060555	969.771679	12.301555
20.069428	972.481355	12.306560
20.031377	971.082417	12.311565
20.130909	967.113019	12.316570
20.397315	967.974315	12.321575
20.174575	980.107541	12.326579
20.149293	979.086634	12.331584
20.075011	974.638727	12.336589
20.029461	975.970859	12.341594
19.835211	974.525869	12.346599
20.132666	978.891150	12.351603
20.276492	975.618049	12.356608
20.043463	984.846417	12.361613
20.239910	973.351641	12.366618
20.238204	972.363246	12.371623
20.106935	974.122238	12.376627
20.325355	970.018750	12.381632
19.994479	974.624617	12.386637
20.264239	970.404123	12.391642
20.190226	971.712407	12.396647
19.914531	981.477468	12.401651
20.779570	982.713234	12.406656
20.363855	992.574759	12.411661
20.335053	978.395495	12.416666
20.222992	970.775859	12.421671
20.059326	977.238052	12.426675
20.430099	980.241683	12.431680
20.308312	979.961613	12.436685
20.435385	982.346489	12.441690
20.440193	987.515440	12.446695
20.201412	983.267246	12.451699
20.504179	970.954370	12.456704
20.305034	988.021583	12.461709
20.376526	979.688223	12.466714
20.512119	976.561524	12.471719
20.225103	966.492252	12.476723
20.493620	955.525344	12.481728
20.050089	952.055765	12.486733
20.382146	942.212630	12.491738
20.142294	954.381682	12.496743
19.962497	949.531119	12.501747
20.213845	943.618244	12.506752
19.836599	955.607352	12.511757
20.005896	963.055700	12.516762
20.353824	977.247411	12.521767
20.210134	974.401821	12.526771
20.424789	952.577635	12.531776
19.780026	959.349966	12.536781
20.372488	963.032633	12.541786
20.124118	960.984382	12.546791
19.758908	962.134100	12.551795
20.194015	968.754680	12.556800
20.201680	983.156802	12.561805
20.499936	977.679582	12.566810
20.456707	960.700218	12.571815
20.137075	949.503840	12.576819
20.344857	951.655049	12.581824
19.937806	965.651771	12.586829
20.150181	948.514946	12.591834
20.130673	951.076172	12.596839
19.933431	951.699172	12.601843
20.318170	948.334028	12.606848
20.162992	964.127830	12.611853
20.333415	966.171454	12.616858
20.245133	959.510031	12.621863
20.043542	959.326275	12.626867
20.112158	954.117521	12.631872
20.147158	957.923807	12.636877
20.159473	961.582316	12.641882
20.206355	960.947315	12.646887
19.776338	975.222115	12.651891
20.631135	973.480467	12.656896
20.047941	974.497790	12.661901
20.115515	975.799260	12.666906
20.361598	984.028627	12.671911
20.069070	972.449415	12.676915
20.135852	968.786458	12.681920
20.237733	982.217858	12.686925
20.308777	961.001654	12.691930
20.256374	962.855303	12.696935
20.149260	969.932983	12.701939
20.396422	961.732469	12.706944
20.086077	966.052766	12.711949
20.388815	962.413677	12.716954
20.261237	953.648433	12.721959
20.206508	960.258831	12.726963
20.627249	960.292790	12.731968
20.333218	963.318881	12.736973
20.364580	952.911810	12.741978
20.258619	961.941687	12.746983
20.522079	958.636890	12.751987
20.695347	965.001173	12.756992
20.266858	959.698238	12.761997
20.403738	957.085456	12.767002
20.268734	932.448426	12.772007
20.194080	932.261770	12.777011
20.159270	928.417897	12.782016
19.842098	933.220273	12.787021
20.375036	943.256887	12.792026
20.173502	941.751558	12.797031
19.756087	945.562195	12.802035
20.391792	945.367886	12.807040
20.280442	957.631568	12.812045
20.380863	952.315233	12.817050
20.372802	948.626370	12.822055
20.225574	942.512131	12.827059
20.424078	929.132491	12.832064
20.110776	940.398562	12.837069
19.998796	932.657500	12.842074
20.065262	936.871947	12.847079
20.071292	940.189234	12.852083
19.971661	938.394820	12.857088
20.275479	940.516516	12.862093
20.342290	942.974079	12.867098
20.116670	936.045975	12.872103
20.001218	942.196091	12.877107
20.047934	936.882021	12.882112
20.181479	951.650408	12.887117
20.158149	945.207303	12.892122
20.167399	944.879521	12.897127
20.068711	970.013058	12.902131
20.414373	960.514691	12.907136
20.207262	950.199281	12.912141
19.966884	948.372121	12.917146
20.404844	953.136053	12.922151
20.420176	955.921971	12.927155
20.367412	937.363953	12.932160
20.177465	936.796696	12.937165
20.188940	941.726432	12.942170
20.310093	939.519886	12.947175
20.061774	946.025532	12.952179
20.192308	944.397842	12.957184
20.063440	948.682877	12.962189
20.088534	940.375864	12.967194
20.238586	944.930239	12.972199
19.923851	944.807112	12.977203
19.910682	950.090887	12.982208
19.674290	958.252114	12.987213
20.240864	965.405264	12.992218
20.416015	967.683114	12.997223
20.344179	976.787987	13.002227
20.691463	969.765325	13.007232
20.148005	959.891515	13.012237
20.231997	957.276130	13.017242
20.035549	956.695715	13.022247
20.011593	958.598446	13.027251
19.892765	948.904505	13.032256
19.736900	955.876407	13.037261
20.142723	967.414163	13.042266
20.402581	975.731219	13.047271
20.190320	984.315992	13.052275
20.660443	981.033420	13.057280
20.298957	971.608421	13.062285
20.310154	953.535374	13.067290
20.519738	955.422929	13.072295
20.158227	955.898657	13.077299
20.370159	945.596835	13.082304
20.400795	948.620023	13.087309
20.210882	959.096826	13.092314
20.001368	951.189952	13.097319
19.881277	954.506859	13.102323
20.401680	952.712892	13.107328
20.176649	953.521685	13.112333
20.346517	944.078180	13.117338
20.490441	943.121753	13.122343
20.645416	946.382165	13.127347
20.390680	944.115722	13.132352
20.396029	945.999583	13.137357
20.296774	938.704370	13.142362
20.704777	942.011155	13.147367
20.290029	933.148221	13.152371
20.178934	919.135116	13.157376
19.936710	918.872682	13.162381
19.832811	914.915247	13.167386
20.121725	917.425692	13.172391
20.048849	944.133688	13.177395
20.510157	943.112439	13.182400
20.222076	933.425006	13.187405
19.976623	930.657161	13.192410
20.077385	930.988181	13.197415
20.095790	943.912436	13.202419
20.334871	939.326239	13.207424
19.879531	948.817141	13.212429
20.156152	952.693699	13.217434
20.383572	947.282987	13.222439
20.196377	962.271292	13.227443
20.310009	948.034643	13.232448
19.989755	935.314947	13.237453
19.993660	955.413933	13.242458
20.346059	946.802378	13.247463
20.214461	955.224447	13.252467
20.272088	953.105307	13.257472
19.948375	944.393434	13.262477
20.112975	949.095309	13.267482
20.261457	954.794873	13.272487
19.888356	962.968447	13.277491
20.305563	958.491033	13.282496
20.425377	954.614604	13.287501
20.278069	952.318407	13.292506
20.636008	945.177355	13.297511
20.019713	931.006692	13.302515
20.114062	925.027399	13.307520
20.397033	927.914131	13.312525
20.291468	928.946731	13.317530
20.504343	922.148970	13.322535
20.167827	927.903811	13.327539
20.326119	923.669570	13.332544
20.061587	927.618251	13.337549
20.055352	927.327635	13.342554
20.050780	930.681306	13.347559
20.339727	928.211438	13.352563
20.355075	932.205367	13.357568
20.372651	927.892641	13.362573
20.120729	923.829498	13.367578
20.209780	927.111460	13.372583
20.069782	928.534351	13.377587
19.852545	924.934058	13.382592
20.042916	927.573771	13.387597
19.750435	935.650886	13.392602
20.134396	930.999001	13.397607
20.115730	923.653091	13.402611
20.025636	919.737610	13.407616
20.256009	927.111538	13.412621
20.160361	929.145556	13.417626
20.469927	918.859721	13.422631
20.192735	925.961355	13.427635
20.315421	923.896500	13.432640
19.898220	932.313649	13.437645
20.178190	932.349561	13.442650
20.122140	926.167165	13.447655
20.071789	928.608720	13.452659
20.267051	925.073522	13.457664
20.063639	939.976077	13.462669
20.209963	936.615848	13.467674
20.447368	928.404293	13.472679
20.165289	937.979520	13.477683
20.473759	931.819404	13.482688
20.307301	933.882066	13.487693
20.414435	930.723644	13.492698
20.265455	933.426953	13.497703
20.384633	934.210801	13.502707
20.289794	930.087905	13.507712
20.128054	936.097160	13.512717
20.182587	933.734074	13.517722
20.151650	942.515415	13.522727
20.049531	942.025616	13.527731
20.205295	940.389170	13.532736
20.090927	937.499483	13.537741
19.867404	940.957473	13.542746
20.132336	934.187675	13.547751
20.289897	935.993635	13.552755
20.320775	934.949579	13.557760
20.165049	935.547031	13.562765
20.089157	927.372836	13.567770
20.542276	933.826513	13.572775
20.391608	939.088061	13.577779
20.490059	933.057645	13.582784
20.192010	933.542174	13.587789
20.241187	934.362421	13.592794
20.313767	934.243747	13.597799
20.504966	936.864406	13.602803
20.410867	925.455440	13.607808
20.121140	928.126003	13.612813
20.011971	917.358151	13.617818
20.128361	918.669176	13.622823
20.350330	936.311012	13.627827
20.375674	931.323647	13.632832
20.065738	915.298412	13.637837
19.984695	908.766752	13.642842
19.982026	914.168695	13.647847
20.004063	926.521466	13.652851
20.319102	931.364927	13.657856
20.404501	937.714828	13.662861
20.046029	938.516519	13.667866
20.298992	932.622315	13.672871
20.041598	940.550325	13.677875
20.189509	940.949522	13.682880
20.212807	937.829705	13.687885
20.096019	931.210691	13.692890
20.266271	932.279723	13.697895
20.083200	936.089248	13.702899
20.344873	945.353802	13.707904
20.383112	936.857026	13.712909
19.964010	925.963555	13.717914
20.002217	922.445525	13.722919
20.232906	930.573231	13.727923
20.086842	937.488365	13.732928
20.275481	936.589464	13.737933
20.293789	933.632880	13.742938
20.144596	926.796673	13.747943
20.029147	937.873477	13.752947
20.266854	931.671029	13.757952
20.303284	938.241643	13.762957
20.228801	939.029574	13.767962
20.159388	917.340646	13.772967
20.010877	919.334207	13.777971
20.028531	934.628872	13.782976
19.992197	939.258711	13.787981
19.968779	945.277446	13.792986
20.238293	942.660856	13.797991
20.249041	943.761641	13.802995
20.425073	945.938416	13.808000
20.437308	944.785362	13.813005
19.916897	943.144807	13.818010
20.323627	939.747770	13.823015
20.056744	934.930029	13.828019
20.358167	939.446062	13.833024
20.031950	922.199629	13.838029
19.928772	939.341368	13.843034
20.268064	938.260732	13.848039
19.998269	951.417058	13.853043
20.337332	942.052228	13.858048
20.088209	947.312136	13.863053
20.002075	946.026531	13.868058
20.225311	945.721390	13.873063
20.201471	947.447471	13.878067
20.160256	960.704547	13.883072
20.168575	956.856941	13.888077
20.307921	954.205917	13.893082
20.586424	942.903092	13.898087
19.825818	942.731233	13.903091
20.126616	944.495421	13.908096
20.309640	944.706080	13.913101
20.209096	957.857492	13.918106
20.402365	946.244966	13.923111
19.833214	928.453770	13.928115
20.009793	943.361950	13.933120
20.515586	943.978465	13.938125
20.448303	943.719666	13.943130
20.247927	921.968039	13.948135
19.775322	924.331862	13.953139
20.069440	931.285592	13.958144
20.333300	943.401095	13.963149
19.831724	950.208931	13.968154
20.280340	944.990030	13.973159
20.324432	954.748219	13.978163
20.314342	951.668419	13.983168
20.372443	946.363569	13.988173
20.092376	934.399177	13.993178
20.174413	928.581129	13.998183
19.731642	938.756034	14.003187
20.221521	942.524450	14.008192
20.288057	953.850113	14.013210
20.135322	957.899991	14.018227
20.545754	951.026612	14.023245
20.577480	943.669379	14.028263
20.270188	928.573474	14.033280
20.117783	930.894541	14.038298
20.002925	934.123546	14.043315
20.196782	927.058209	14.048333
20.334612	942.165701	14.053351
20.673718	943.755561	14.058368
20.483902	931.434605	14.063386
20.010161	928.738652	14.068403
20.377631	925.472786	14.073421
20.362719	946.969095	14.078439
20.450089	954.911661	14.083456
20.609539	949.560107	14.088474
20.194611	951.212047	14.093491
20.560844	946.131103	14.098509
20.368412	957.449968	14.103527
20.239774	959.422756	14.108544
20.564994	963.605607	14.113562
20.630971	962.149615	14.118579
20.121421	962.061154	14.123597
20.342125	959.819136	14.128615
20.179435	965.424754	14.133632
20.560341	952.869595	14.138650
20.373387	962.037265	14.143667
20.728173	962.004409	14.148685
20.259083	959.639617	14.153703
20.284675	961.576792	14.158720
20.836893	980.903145	14.163738
20.667659	990.275646	14.168755
20.891299	997.112680	14.173773
20.876755	998.375140	14.178791
20.848057	991.570217	14.183808
20.671022	970.951035	14.188826
20.670777	984.982624	14.193843
21.039037	980.522691	14.198861
20.840867	999.303377	14.203879
21.057109	1000.134193	14.208896
21.044685	979.738853	14.213914
20.674558	973.765477	14.218931
20.934149	980.239691	14.223949
20.828355	983.259621	14.228967
21.000807	986.493143	14.233984
20.993040	994.704164	14.239002
20.920344	991.846698	14.244019
21.153711	1001.162849	14.249037
20.805798	1000.881862	14.254055
20.801336	999.166542	14.259072
21.278031	1000.114687	14.264090
20.972363	1002.230551	14.269107
21.150789	995.183373	14.274125
21.060972	1003.509734	14.279143
21.016330	998.727122	14.284160
20.978578	1001.951707	14.289178
20.916960	1008.132678	14.294195
21.101148	997.273127	14.299213
20.863417	1002.212753	14.304231
20.590574	1005.013942	14.309248
21.203904	1011.681855	14.314266
21.206627	1023.674359	14.319283
21.222025	1027.530695	14.324301
21.067161	1027.426553	14.329319
21.286990	1035.119943	14.334336
21.280023	1028.591536	14.339354
21.143254	1044.111026	14.344371
21.216518	1031.615885	14.349389
21.353609	1036.778879	14.354407
21.122795	1031.236291	14.359424
21.464429	1026.539917	14.364442
21.302849	1036.611226	14.369459
21.323314	1030.330128	14.374477
21.326079	1029.961741	14.379495
21.271022	1026.203253	14.384512
21.553508	1033.650692	14.389530
21.457385	1028.166844	14.394547
21.832072	1028.728567	14.399565
21.635027	1033.507557	14.404583
21.273843	1036.116776	14.409600
21.754948	1035.303995	14.414618
21.468930	1044.537856	14.419635
21.874463	1047.553313	14.424653
21.673643	1050.673359	14.429671
21.736927	1054.528356	14.434688
21.984839	1051.646478	14.439706
21.864409	1039.949867	14.444723
21.584602	1034.853969	14.449741
21.663015	1031.774189	14.454759
21.722808	1049.527499	14.459776
22.073473	1065.582742	14.464794
22.168498	1049.629725	14.469811
21.921203	1044.462569	14.474829
22.209074	1040.064206	14.479847
22.104864	1040.683445	14.484864
22.078352	1026.876582	14.489882
22.064685	1034.190364	14.494899
22.062744	1024.964978	14.499917
21.989605	1030.156785	14.504935
21.944139	1034.000810	14.509952
22.275477	1033.839560	14.514970
22.114083	1033.789943	14.519987
22.306021	1034.555424	14.525005
22.001840	1040.564315	14.530023
21.888634	1033.908134	14.535040
22.112105	1032.395551	14.540058
22.062445	1040.135078	14.545075
21.727478	1032.532698	14.550093
22.406770	1035.185157	14.555111
21.844675	1039.685751	14.560128
21.959904	1046.000551	14.565146
21.754931	1043.115411	14.570163
22.182425	1059.587831	14.575181
22.361153	1059.461936	14.580199
22.222962	1073.446401	14.585216
22.530802	1065.846859	14.590234
22.165664	1069.524807	14.595251
22.236160	1068.602916	14.600269
22.499985	1068.664796	14.605287
22.224522	1074.201927	14.610304
22.233664	1075.240391	14.615322
22.201222	1074.106829	14.620339
22.195472	1074.343846	14.625357
22.354514	1073.302437	14.630375
22.255693	1075.594530	14.635392
22.407561	1066.976943	14.640410
22.446617	1071.880306	14.645427
22.164261	1078.022585	14.650445
22.329545	1073.672081	14.655463
22.309954	1082.581893	14.660480
22.467946	1086.821344	14.665498
22.724587	1090.392248	14.670515
22.507906	1096.635744	14.675533
22.860767	1097.068816	14.680551
22.840530	1095.889261	14.685568
23.120851	1098.015485	14.690586
22.944008	1094.317305	14.695603
22.573779	1082.341180	14.700621
22.713603	1072.297192	14.705639
22.836353	1078.283615	14.710656
23.004614	1090.329993	14.715674
22.963348	1087.810417	14.720691
22.667420	1073.933227	14.725709
22.805936	1070.790368	14.730727
22.748035	1084.865857	14.735744
22.767189	1092.869716	14.740762
22.593801	1097.464053	14.745779
22.859466	1108.267937	14.750797
22.861202	1094.701899	14.755815
23.043295	1100.548302	14.760832
23.030065	1105.968109	14.765850
22.999316	1097.351320	14.770867
22.735011	1110.575709	14.775885
22.985080	1100.739061	14.780903
23.284546	1105.830561	14.785920
23.126540	1101.876114	14.790938
23.187659	1105.324053	14.795955
22.980045	1100.288975	14.800973
23.124365	1099.419802	14.805991
22.963496	1101.031231	14.811008
23.368043	1099.398521	14.816026
23.319506	1099.286856	14.821043
23.154289	1100.109313	14.826061
23.221712	1097.695095	14.831079
23.144446	1105.448498	14.836096
23.473504	1091.529798	14.841114
23.293052	1101.907760	14.846131
22.929136	1108.648233	14.851149
23.412917	1105.020851	14.856167
23.555662	1118.836275	14.861184
23.437021	1120.412656	14.866202
23.556082	1104.937096	14.871219
23.420061	1099.643631	14.876237
23.390111	1094.734373	14.881255
23.587349	1110.837736	14.886272
23.657254	1114.501355	14.891290
23.279017	1114.656216	14.896307
23.642540	1125.991922	14.901325
24.000343	1111.562098	14.906343
23.732640	1105.337946	14.911360
23.486852	1108.949674	14.916378
23.679461	1092.715199	14.921395
23.376676	1102.752449	14.926413
23.736323	1111.353244	14.931431
24.111109	1122.842882	14.936448
23.807595	1120.456370	14.941466
23.881647	1104.310008	14.946483
23.725621	1103.501327	14.951501
24.253384	1102.105369	14.956519
24.018026	1096.061680	14.961536
23.736217	1093.992610	14.966554
24.006706	1092.571623	14.971571
23.940656	1094.399164	14.976589
23.940183	1095.247251	14.981607
23.767481	1098.801700	14.986624
24.053592	1093.385844	14.991642
24.009626	1093.726485	14.996659
23.615754	1107.731319	15.001677
23.913810	1094.055091	15.006695
23.639473	1101.570938	15.011712
24.022142	1122.022509	15.016730
24.197910	1126.386552	15.021747
24.126733	1131.062124	15.026765
24.356750	1129.476128	15.031783
23.931264	1137.269363	15.036800
23.878528	1133.680366	15.041818
24.483842	1135.300144	15.046835
24.076953	1135.821375	15.051853
24.382843	1133.642822	15.056871
24.612766	1129.739747	15.061888
24.191467	1127.499439	15.066906
24.305980	1125.063547	15.071923
24.200224	1125.563485	15.076941
24.402540	1121.675826	15.081959
24.086159	1135.095737	15.086976
24.000793	1134.216008	15.091994
24.289810	1128.088660	15.097011
24.258976	1141.735165	15.102029
24.158506	1140.374920	15.107047
24.645086	1137.431359	15.112064
24.114832	1137.945527	15.117082
24.332406	1126.926395	15.122099
24.394578	1127.550558	15.127117
24.436313	1135.774211	15.132135
24.468551	1142.399597	15.137152
24.405575	1151.866938	15.142170
24.740683	1158.299298	15.147187
24.602824	1163.167991	15.152205
24.705536	1165.086599	15.157223
24.787449	1159.165310	15.162240
24.700815	1157.746227	15.167258
24.865988	1158.487669	15.172275
24.484636	1154.748163	15.177293
25.030681	1152.710626	15.182311
24.974736	1162.592137	15.187328
24.656183	1152.245253	15.192346
24.987203	1148.886051	15.197363
24.578508	1159.520688	15.202381
24.849547	1158.497588	15.207399
24.941728	1161.614964	15.212416
24.625891	1160.679187	15.217434
24.899376	1154.722622	15.222451
24.772094	1157.091628	15.227469
25.065251	1154.532853	15.232487
25.035700	1161.315969	15.237504
24.647387	1161.974239	15.242522
25.100151	1154.930416	15.247539
24.716793	1168.985540	15.252557
25.029834	1159.664206	15.257575
24.842456	1168.235888	15.262592
24.848453	1167.889004	15.267610
25.017660	1187.114705	15.272627
25.073559	1197.242670	15.277645
25.394845	1195.107271	15.282663
25.590120	1199.432045	15.287680
25.133848	1197.294833	15.292698
25.661366	1186.440151	15.297715
25.157127	1189.342780	15.302733
25.140532	1193.713932	15.307751
25.273672	1195.029931	15.312768
25.474929	1187.831153	15.317786
25.545517	1190.461188	15.322803
25.450363	1195.801287	15.327821
25.321931	1201.143550	15.332839
25.545584	1187.066965	15.337856
25.406972	1204.142665	15.342874
25.655359	1193.173626	15.347891
25.499987	1199.979977	15.352909
25.677759	1204.999687	15.357927
25.742837	1193.842807	15.362944
25.679765	1199.764537	15.367962
25.853995	1194.163568	15.372979
25.550388	1195.601145	15.377997
25.973912	1197.201164	15.383015
26.118368	1193.671934	15.388032
25.810067	1185.003410	15.393050
25.628337	1170.258464	15.398067
25.544157	1170.039224	15.403085
25.596370	1182.064864	15.408103
25.692495	1182.895975	15.413120
25.729667	1199.262500	15.418138
25.922075	1189.485327	15.423155
26.096842	1194.138992	15.428173
25.757710	1196.522920	15.433191
25.769992	1195.262664	15.438208
25.225250	1198.044338	15.443226
25.439079	1198.851955	15.448243
25.623062	1199.379611	15.453261
25.503663	1210.712191	15.458279
25.989790	1218.300278	15.463296
25.686086	1221.114295	15.468314
26.066966	1222.148528	15.473331
25.728795	1230.453285	15.478349
25.741135	1216.808361	15.483367
26.326824	1219.889501	15.488384
26.215924	1225.721342	15.493402
26.646504	1220.323295	15.498419
26.372354	1225.087904	15.503437
26.131232	1220.393190	15.508455
26.775560	1223.173962	15.513472
26.459782	1217.224850	15.518490
26.328820	1219.020288	15.523507
26.503337	1224.053108	15.528525
26.582295	1222.610750	15.533543
26.760367	1216.109372	15.538560
26.624311	1219.473957	15.543578
27.023922	1214.268046	15.548595
26.482450	1202.249922	15.553613
26.519582	1202.692463	15.558631
26.605497	1196.857037	15.563648
26.376237	1196.325879	15.568666
26.480129	1181.700531	15.573683
26.535417	1202.592981	15.578701
26.529983	1212.188037	15.583719
26.704767	1215.587983	15.588736
26.375830	1225.887469	15.593754
26.792438	1219.524223	15.598771
26.768029	1213.596275	15.603789
26.645202	1226.431680	15.608807
27.057335	1217.009558	15.613824
26.675558	1221.284811	15.618842
26.782581	1219.131675	15.623859
26.871403	1221.190935	15.628877
27.017726	1222.212246	15.633895
27.116021	1217.296647	15.638912
26.831889	1227.346737	15.643930
26.873867	1217.985232	15.648947
26.787114	1221.664429	15.653965
26.838501	1223.872809	15.658983
26.952970	1217.817312	15.664000
26.872147	1228.498801	15.669018
26.930088	1223.237273	15.674035
26.822480	1216.701239	15.679053
26.968663	1227.772814	15.684071
26.868918	1224.081179	15.689088
26.869439	1225.883960	15.694106
26.998192	1228.931022	15.699123
27.222112	1239.047945	15.704141
27.164179	1254.400924	15.709159
27.462845	1241.042220	15.714176
27.384274	1247.081276	15.719194
27.341557	1246.756318	15.724211
27.479058	1241.469509	15.729229
27.332874	1235.581427	15.734247
27.527397	1233.670740	15.739264
27.219631	1224.187264	15.744282
27.761499	1226.035829	15.749299
27.815423	1225.630961	15.754317
26.970293	1214.987350	15.759335
27.223366	1221.516196	15.764352
27.408369	1238.949311	15.769370
27.542300	1237.841109	15.774387
27.632950	1245.739265	15.779405
27.639645	1251.714384	15.784423
27.535122	1241.734425	15.789440
27.708074	1252.830064	15.794458
27.799594	1248.343407	15.799475
27.654134	1251.196683	15.804493
27.674363	1250.193135	15.809511
27.747891	1247.140831	15.814528
27.818440	1242.453024	15.819546
27.731953	1246.958040	15.824563
28.066695	1244.118904	15.829581
28.063024	1247.353837	15.834599
28.057962	1239.168603	15.839616
27.961333	1255.350464	15.844634
27.768734	1248.459878	15.849651
28.130030	1247.200574	15.854669
27.848766	1245.523086	15.859687
28.072520	1244.826854	15.864704
27.880345	1247.132292	15.869722
28.131150	1247.262318	15.874739
28.066717	1251.556174	15.879757
27.938040	1242.508171	15.884775
28.439272	1240.749910	15.889792
28.253377	1247.067213	15.894810
28.077015	1250.008789	15.899827
28.636145	1249.073439	15.904845
28.201030	1254.219245	15.909863
28.424400	1247.956025	15.914880
28.374402	1246.365918	15.919898
28.271490	1256.080374	15.924915
28.236248	1250.578865	15.929933
28.066995	1261.195831	15.934951
28.467892	1256.507235	15.939968
28.137195	1252.249952	15.944986
28.455670	1247.005060	15.950003
28.647234	1250.809759	15.955021
27.911392	1256.579274	15.960039
28.198466	1248.489011	15.965056
28.094698	1253.350722	15.970074
28.194025	1267.780415	15.975091
28.531724	1271.530348	15.980109
28.524936	1285.637204	15.985127
28.532935	1277.339751	15.990144
28.479968	1283.936319	15.995162
28.369076	1284.835066	16.000179
28.622606	1278.378254	16.005197
28.617123	1288.047303	16.010215
28.580746	1286.725585	16.015232
28.574376	1287.900248	16.020250
28.487798	1290.081880	16.025267
28.695526	1300.141653	16.030285
28.726251	1315.209987	16.035303
29.066982	1315.599384	16.040320
29.125677	1316.574903	16.045338
29.087798	1322.448619	16.050355
29.542077	1303.291889	16.055373
29.263088	1290.783499	16.060391
29.000182	1283.424327	16.065408
29.311375	1283.066511	16.070426
29.074506	1274.378674	16.075443
29.150225	1275.387655	16.080461
28.888720	1281.891643	16.085479
28.977366	1276.840707	16.090496
29.055365	1278.083711	16.095514
28.907625	1306.524778	16.100531
29.459803	1302.600141	16.105549
29.535922	1316.530204	16.110567
29.289379	1310.203485	16.115584
29.634776	1310.903603	16.120602
29.687039	1299.489131	16.125619
29.656246	1286.016194	16.130637
29.382999	1279.564756	16.135655
29.339486	1279.216329	16.140672
29.827135	1277.140900	16.145690
29.081830	1284.939610	16.150707
29.728100	1272.502300	16.155725
29.384612	1270.402143	16.160743
29.244648	1279.683642	16.165760
29.630192	1289.653695	16.170778
29.468251	1300.258511	16.175795
29.710281	1305.079238	16.180813
29.616384	1310.971323	16.185831
29.393742	1306.553639	16.190848
29.611735	1305.981022	16.195866
29.603560	1308.661396	16.200883
29.725385	1309.911569	16.205901
29.706188	1314.533289	16.210919
29.705918	1306.465233	16.215936
29.588606	1314.629412	16.220954
29.517045	1317.423721	16.225971
30.005906	1311.053629	16.230989
29.987686	1330.183572	16.236007
30.029346	1318.846282	16.241024
30.128712	1306.162693	16.246042
29.594844	1317.039212	16.251059
29.782209	1324.748946	16.256077
30.009264	1336.273331	16.261095
30.086942	1333.083490	16.266112
30.423053	1338.018213	16.271130
30.413963	1338.395769	16.276147
30.107285	1330.942879	16.281165
30.187600	1344.664655	16.286183
30.650693	1334.296781	16.291200
30.433994	1335.629270	16.296218
30.494017	1334.594200	16.301235
30.397870	1336.514663	16.306253
30.179806	1330.077996	16.311271
30.505656	1333.343759	16.316288
30.451982	1325.023082	16.321306
30.641824	1340.050330	16.326323
30.727349	1331.120691	16.331341
30.366099	1327.643780	16.336359
30.241619	1330.680919	16.341376
30.390644	1334.992661	16.346394
30.437494	1344.077657	16.351411
30.423561	1343.183374	16.356429
30.360736	1346.268886	16.361447
30.579879	1346.416549	16.366464
30.395009	1341.336859	16.371482
30.299359	1346.194161	16.376499
30.296539	1337.070966	16.381517
30.580464	1358.356616	16.386535
30.586294	1374.251697	16.391552
31.223631	1366.750456	16.396570
30.981146	1385.014875	16.401587
30.943688	1369.342197	16.406605
31.019483	1375.155329	16.411623
30.912426	1377.618674	16.416640
31.097213	1373.249240	16.421658
30.794818	1382.671548	16.426675
30.756595	1373.077338	16.431693
30.822500	1380.347139	16.436711
30.579089	1380.338918	16.441728
31.273084	1369.389905	16.446746
31.326840	1369.241470	16.451763
31.241976	1366.365421	16.456781
30.888792	1362.962722	16.461799
30.749224	1371.641731	16.466816
31.235615	1378.858617	16.471834
31.285389	1400.731467	16.476851
31.684071	1400.643633	16.481869
31.512116	1389.522840	16.486887
31.405804	1377.328188	16.491904
31.285264	1373.163191	16.496922
31.204011	1389.411176	16.501939
31.646156	1394.800140	16.506957
31.823285	1397.115907	16.511975
31.802686	1386.644248	16.516992
31.714454	1360.584824	16.522010
31.504985	1365.718271	16.527027
31.912808	1359.159732	16.532045
31.669821	1357.276345	16.537063
31.290420	1366.539461	16.542080
32.004301	1357.441934	16.547098
31.568655	1368.294958	16.552115
31.504373	1360.059326	16.557133
31.714790	1362.361912	16.562151
31.529527	1387.390844	16.567168
31.820532	1377.045671	16.572186
31.866547	1397.235930	16.577203
31.974569	1387.425680	16.582221
32.007537	1397.868912	16.587239
31.723563	1408.893620	16.592256
31.790059	1395.591472	16.597274
31.781848	1397.095210	16.602291
31.731334	1390.135486	16.607309
31.699902	1392.389350	16.612327
32.013990	1397.492779	16.617344
31.983441	1394.718175	16.622362
31.768207	1413.505262	16.627379
31.825094	1420.911020	16.632397
32.160578	1420.653937	16.637415
32.052477	1424.697611	16.642432
32.437646	1415.571468	16.647450
32.154631	1420.221147	16.652467
32.393409	1431.208105	16.657485
32.462842	1430.673339	16.662503
32.029991	1432.371448	16.667520
32.285241	1427.008372	16.672538
32.270907	1432.870511	16.677555
32.220964	1436.112867	16.682573
32.569583	1435.633458	16.687591
32.470952	1453.613885	16.692608
32.844707	1447.025347	16.697626
33.159364	1457.420543	16.702643
32.968776	1445.010394	16.707661
32.664050	1440.741046	16.712679
32.452248	1427.270896	16.717696
32.448663	1425.455495	16.722714
32.522157	1435.986674	16.727731
32.774244	1444.026719	16.732749
33.178305	1440.714004	16.737767
32.784007	1456.553447	16.742784
32.978774	1454.285604	16.747802
32.934338	1449.185049	16.752819
32.753474	1456.479307	16.757837
33.179816	1451.383883	16.762855
32.700086	1458.924023	16.767872
32.939547	1445.510080	16.772890
32.700112	1454.229450	16.777907
32.864167	1454.219942	16.782925
33.052101	1457.385819	16.787943
32.930955	1451.676919	16.792960
33.047961	1459.003105	16.797978
33.023464	1456.896870	16.802995
33.110927	1474.550327	16.808013
33.602778	1479.656105	16.813031
33.320247	1483.570310	16.818048
33.798652	1477.073609	16.823066
33.622322	1460.279354	16.828083
33.266691	1455.654740	16.833101
33.422684	1443.265604	16.838119
32.923684	1457.865646	16.843136
33.258211	1468.900283	16.848154
33.330617	1481.079470	16.853171
33.572360	1482.657395	16.858189
33.740823	1482.120988	16.863207
33.330203	1494.401617	16.868224
33.791881	1478.815164	16.873242
33.817751	1484.023588	16.878259
33.904703	1485.234507	16.883277
33.857052	1485.003929	16.888295
33.624739	1486.619717	16.893312
33.861371	1483.642810	16.898330
33.929993	1483.109744	16.903347
33.598479	1483.758180	16.908365
33.921022	1478.518850	16.913383
34.026790	1485.654926	16.918400
34.091656	1479.744091	16.923418
34.028403	1479.784999	16.928435
33.888759	1478.735362	16.933453
34.375619	1476.650594	16.938471
34.312409	1482.776176	16.943488
34.120237	1483.833409	16.948506
34.129607	1483.297210	16.953523
33.924958	1482.352326	16.958541
34.101482	1479.440066	16.963559
34.177376	1477.726816	16.968576
34.126183	1477.944345	16.973594
34.118168	1481.611834	16.978611
33.890113	1501.371670	16.983629
34.388744	1497.439794	16.988647
34.345720	1511.105893	16.993664
34.346884	1504.554738	16.998682
34.721743	1512.289724	17.003699
34.811457	1516.694354	17.008717
34.630283	1509.695637	17.013735
34.593393	1521.446323	17.018752
34.767353	1512.582695	17.023770
34.928948	1510.154961	17.028787
34.415852	1511.668456	17.033805
35.008948	1502.354144	17.038823
34.419170	1513.054102	17.043840
34.425629	1508.319015	17.048858
34.753365	1501.363399	17.053875
34.480418	1507.969989	17.058893
34.569919	1509.007464	17.063911
34.917018	1510.839943	17.068928
34.939799	1505.970901	17.073946
34.894283	1507.425543	17.078963
34.884204	1506.839746	17.083981
34.903024	1505.513924	17.088999
34.797081	1506.284474	17.094016
34.861175	1522.450432	17.099034
35.182913	1527.043793	17.104051
35.233823	1538.589358	17.109069
35.483874	1544.801856	17.114087
35.305412	1538.612047	17.119104
35.382309	1519.393317	17.124122
35.364728	1516.645723	17.129139
35.046090	1522.377893	17.134157
35.427870	1524.547776	17.139175
35.209263	1534.910107	17.144192
35.453893	1535.808003	17.149210
35.552263	1532.017831	17.154227
35.678007	1531.027322	17.159245
35.885102	1528.534123	17.164263
35.600819	1535.095341	17.169280
35.622318	1530.940677	17.174298
35.791038	1530.017248	17.179315
35.293372	1526.595083	17.184333
35.632260	1524.881563	17.189351
35.596760	1533.296307	17.194368
35.466276	1536.813451	17.199386
35.573046	1527.675802	17.204403
35.686236	1537.097989	17.209421
35.482921	1532.898170	17.214439
35.624300	1537.734244	17.219456
35.878782	1531.085253	17.224474
35.662164	1528.592785	17.229491
35.655912	1533.278580	17.234509
35.863657	1544.559236	17.239527
35.945463	1552.337842	17.244544
35.811887	1556.850463	17.249562
36.071761	1549.410913	17.254579
35.972642	1557.059499	17.259597
35.964875	1551.741477	17.264615
36.038061	1551.672529	17.269632
36.295360	1551.825907	17.274650
36.252853	1553.639525	17.279667
35.974165	1552.951848	17.284685
36.248982	1558.538245	17.289703
36.474951	1570.495589	17.294720
36.733670	1583.256290	17.299738
36.490030	1570.050646	17.304755
36.409376	1571.857765	17.309773
36.718721	1573.096141	17.314791
36.621132	1574.734495	17.319808
36.593479	1577.410160	17.324826
36.637222	1570.298456	17.329843
36.708121	1577.385867	17.334861
36.822238	1573.105515	17.339879
36.985833	1557.812714	17.344896
36.316535	1556.159329	17.349914
36.575758	1568.155414	17.354931
36.729479	1576.432243	17.359949
36.895397	1577.297078	17.364967
36.834347	1585.067026	17.369984
36.739129	1592.954118	17.375002
36.970666	1589.095497	17.380019
36.631337	1585.585924	17.385037
37.325389	1584.436331	17.390055
37.118827	1577.773554	17.395072
36.998653	1575.506376	17.400090
37.180094	1573.760548	17.405107
37.321913	1585.312886	17.410125
37.052595	1582.722630	17.415143
36.796772	1579.366486	17.420160
37.042251	1582.671081	17.425178
36.961200	1574.010908	17.430195
36.986835	1591.876512	17.435213
37.444067	1601.492411	17.440231
37.517920	1602.874536	17.445248
37.559452	1613.871860	17.450266
37.380183	1613.821157	17.455283
37.468271	1610.852975	17.460301
37.290091	1614.071778	17.465319
37.390732	1616.681367	17.470336
37.248431	1613.502170	17.475354
37.364015	1608.231310	17.480371
37.364260	1611.680427	17.485389
37.030234	1622.272811	17.490407
37.759053	1631.173697	17.495424
37.782108	1639.419492	17.500442
38.162419	1645.056738	17.505459
37.666596	1637.599251	17.510477
37.773290	1634.727202	17.515495
37.870760	1633.533547	17.520512
37.536772	1639.147082	17.525530
38.069033	1637.165954	17.530547
37.800035	1650.076959	17.535565
37.811070	1642.098940	17.540583
37.997782	1639.747407	17.545600
37.976186	1656.612267	17.550618
37.980359	1663.949476	17.555635
38.158075	1666.619928	17.560653
38.568965	1667.744583	17.565671
38.788319	1672.511632	17.570688
38.490984	1677.930563	17.575706
38.599231	1673.937422	17.580723
38.738793	1670.463130	17.585741
38.446245	1645.261666	17.590759
38.628970	1644.033961	17.595776
38.627185	1633.340462	17.600794
38.712812	1642.712842	17.605811
38.649211	1640.818107	17.610829
38.510522	1639.544139	17.615847
38.552655	1638.562240	17.620864
38.546376	1639.600057	17.625882
38.403836	1635.550971	17.630899
38.717336	1651.408290	17.635917
38.915576	1670.948554	17.640935
39.023240	1661.689550	17.645952
38.924130	1674.240767	17.650970
39.026565	1669.214239	17.655987
39.143038	1671.207802	17.661005
39.290006	1667.581312	17.666023
39.005125	1647.980437	17.671040
38.517779	1652.271079	17.676058
38.877190	1663.750230	17.681075
39.124951	1669.753924	17.686093
39.109940	1676.641933	17.691111
39.138460	1669.228213	17.696128
39.013661	1672.735831	17.701146
39.223877	1669.210942	17.706163
39.231626	1671.130608	17.711181
39.015311	1671.861353	17.716199
39.002477	1671.760505	17.721216
39.185232	1682.785694	17.726234
39.371228	1685.211784	17.731251
39.821453	1700.537663	17.736269
39.758984	1699.387605	17.741287
39.663643	1681.628448	17.746304
39.581413	1673.521349	17.751322
39.671459	1689.728187	17.756339
39.746629	1694.036086	17.761357
39.550647	1692.245048	17.766375
39.513256	1693.685827	17.771392
39.755113	1704.946223	17.776410
40.195800	1694.137268	17.781427
40.263703	1699.617504	17.786445
39.872923	1705.177985	17.791463
40.230120	1699.109528	17.796480
40.359092	1693.234002	17.801498
39.878285	1676.539977	17.806515
39.937292	1674.591859	17.811533
39.961988	1687.730556	17.816551
40.382953	1684.666789	17.821568
40.131604	1691.739588	17.826586
40.293860	1693.240548	17.831603
40.285028	1688.304911	17.836621
39.821204	1699.996419	17.841639
40.131297	1691.503458	17.846656
39.987709	1701.338748	17.851674
39.875601	1697.915606	17.856691
40.067194	1701.701542	17.861709
40.296382	1719.861254	17.866727
40.669702	1723.803050	17.871744
40.668092	1727.604080	17.876762
40.743501	1725.401642	17.881779
41.012726	1714.877224	17.886797
40.746257	1706.731064	17.891815
40.887264	1704.760424	17.896832
40.819161	1692.466599	17.901850
40.781003	1697.528789	17.906867
40.637853	1688.251570	17.911885
40.517127	1699.114382	17.916903
40.982106	1706.849256	17.921920
41.147056	1719.028039	17.926938
41.003726	1721.092939	17.931955
41.296236	1706.036623	17.936973
41.046554	1706.892248	17.941991
40.937769	1697.202894	17.947008
41.000271	1705.947402	17.952026
41.185507	1721.826044	17.957043
41.254292	1723.511813	17.962061
41.246692	1727.778652	17.967079
41.613331	1725.858539	17.972096
41.205269	1731.769444	17.977114
41.003999	1726.918762	17.982131
41.035812	1719.435275	17.987149
40.906296	1735.007042	17.992167
40.911567	1725.922427	17.997184
40.869890	1730.166386	18.002202
41.034758	1751.077539	18.007219
41.291364	1755.984974	18.012237
41.187427	1761.088353	18.017255
41.807783	1752.332711	18.022272
41.725479	1759.095418	18.027290
41.445298	1759.422626	18.032307
41.612299	1757.426595	18.037325
41.370747	1764.411345	18.042343
41.734902	1769.944246	18.047360
41.847772	1782.319376	18.052378
42.031415	1785.856478	18.057395
42.697916	1779.755957	18.062413
42.367574	1789.665142	18.067431
42.467301	1760.457894	18.072448
42.086059	1754.016391	18.077466
41.970714	1755.495567	18.082483
42.049623	1743.071278	18.087501
41.930025	1757.143099	18.092519
42.192874	1759.973032	18.097536
42.484227	1773.732340	18.102554
42.548765	1774.474138	18.107571
42.784121	1770.994768	18.112589
42.588641	1770.896310	18.117607
42.424180	1755.776759	18.122624
42.395258	1757.913082	18.127642
42.484157	1768.479800	18.132659
42.877735	1766.335936	18.137677
42.498835	1777.253359	18.142695
42.541888	1765.040062	18.147712
42.468154	1771.116317	18.152730
42.561826	1769.533125	18.157747
42.720290	1770.632769	18.162765
42.385183	1777.923473	18.167783
42.401277	1770.890018	18.172800
42.665610	1776.391651	18.177818
42.452656	1781.860871	18.182835
42.755406	1784.503536	18.187853
42.873331	1802.748743	18.192871
43.124730	1799.561767	18.197888
43.122501	1801.840925	18.202906
43.360627	1804.005449	18.207923
43.505029	1805.504550	18.212941
43.192083	1806.273525	18.217959
43.454914	1804.215009	18.222976
43.541161	1797.893198	18.227994
43.510666	1795.031201	18.233011
43.862722	1800.456713	18.238029
43.161957	1791.081957	18.243047
43.330213	1785.956796	18.248064
43.611102	1802.046011	18.253082
43.229760	1803.129507	18.258099
43.691707	1805.633519	18.263117
43.565074	1795.924135	18.268135
43.707343	1799.425366	18.273152
43.740025	1789.397976	18.278170
43.452431	1803.410116	18.283187
43.677397	1799.686991	18.288205
43.712154	1800.043407	18.293223
43.458513	1793.360510	18.298240
43.752276	1798.553845	18.303258
43.590751	1799.893305	18.308275
44.162301	1808.525215	18.313293
43.657133	1821.341900	18.318311
44.073365	1823.007655	18.323328
44.382963	1823.888915	18.328346
44.044833	1832.063435	18.333363
44.228013	1827.696483	18.338381
44.271693	1835.442780	18.343399
44.042728	1834.418375	18.348416
44.202615	1823.525906	18.353434
44.312228	1828.539400	18.358451
44.616542	1825.127675	18.363469
44.350695	1832.016438	18.368487
44.308135	1827.757070	18.373504
44.192944	1825.308936	18.378522
44.149087	1834.083857	18.383539
44.424811	1844.472170	18.388557
44.726248	1865.099779	18.393575
44.840015	1856.439038	18.398592
45.074959	1860.970841	18.403610
44.682657	1860.204524	18.408627
44.704062	1853.734146	18.413645
44.663415	1862.565204	18.418663
45.009423	1864.858830	18.423680
45.220575	1859.930521	18.428698
44.688835	1863.803561	18.433715
44.966382	1864.051248	18.438733
44.901547	1864.021618	18.443751
44.715971	1862.442057	18.448768
45.166560	1860.024016	18.453786
44.813210	1869.118114	18.458803
45.135547	1866.689066	18.463821
45.045173	1889.366061	18.468839
44.998824	1887.157063	18.473856
45.353302	1882.769064	18.478874
45.340207	1895.362596	18.483891
45.458142	1890.228121	18.488909
45.664768	1894.618151	18.493927
45.458319	1884.073525	18.498944
45.793683	1882.819881	18.503962
45.655040	1890.074584	18.508979
45.795451	1882.863933	18.513997
45.648102	1892.240599	18.519015
45.672868	1886.826812	18.524032
45.722453	1884.397219	18.529050
45.753103	1887.288598	18.534067
45.767898	1885.912256	18.539085
45.775906	1880.061456	18.544103
45.770888	1886.565700	18.549120
46.243369	1907.561728	18.554138
46.158047	1915.203580	18.559155
46.258274	1911.070859	18.564173
46.271375	1920.872652	18.569191
46.095770	1918.940686	18.574208
46.315768	1909.221558	18.579226
46.195294	1920.926119	18.584243
46.464561	1918.964095	18.589261
46.587545	1913.561374	18.594279
46.461474	1922.675886	18.599296
46.740062	1915.201704	18.604314
46.490538	1919.492242	18.609331
46.545145	1906.993034	18.614349
46.871949	1913.792811	18.619367
46.441441	1925.399740	18.624384
46.427330	1913.701985	18.629402
46.464016	1924.666493	18.634419
46.828023	1918.146160	18.639437
46.860610	1914.412790	18.644455
47.005872	1918.304494	18.649472
47.036102	1916.912316	18.654490
46.702842	1914.008134	18.659507
46.857688	1915.677838	18.664525
46.688787	1909.738832	18.669543
46.727249	1925.392554	18.674560
47.477093	1930.805792	18.679578
47.513318	1932.630495	18.684595
47.661055	1914.323373	18.689613
47.348008	1909.080658	18.694631
47.251787	1906.176424	18.699648
47.406520	1888.338584	18.704666
47.914521	1893.654308	18.709683
47.941056	1894.170924	18.714701
48.104969	1887.024953	18.719719
47.669921	1900.584049	18.724736
47.987932	1889.961270	18.729754
47.575333	1901.486667	18.734771
47.495623	1893.243754	18.739789
47.989785	1892.468181	18.744807
47.849805	1891.905449	18.749824
47.835462	1883.019719	18.754842
47.359533	1883.493776	18.759859
47.767152	1882.236473	18.764877
47.919951	1882.089541	18.769895
47.907968	1894.227475	18.774912
48.153222	1880.684787	18.779930
47.879315	1886.246357	18.784947
47.876862	1891.324943	18.789965
48.005675	1891.851201	18.794983
47.852634	1896.318265	18.800000
48.040080	1912.555437	18.805018
48.417776	1930.809710	18.810035
48.193779	1923.477040	18.815053
48.599298	1922.945282	18.820071
48.166382	1930.811697	18.825088
48.301866	1918.771518	18.830106
48.237470	1925.455148	18.835123
48.286334	1925.349177	18.840141
48.718463	1925.088472	18.845159
48.590591	1928.319770	18.850176
48.655759	1935.489287	18.855194
48.829288	1943.294373	18.860211
48.928594	1956.550410	18.865229
49.410854	1949.218341	18.870247
48.950785	1941.642513	18.875264
49.047203	1917.453769	18.880282
48.908016	1923.068588	18.885299
49.062720	1942.176472	18.890317
49.275404	1955.846248	18.895335
49.125283	1952.197071	18.900352
49.320350	1949.509079	18.905370
48.990292	1947.895921	18.910387
48.989669	1948.971400	18.915405
49.076243	1944.619035	18.920423
48.986957	1948.423882	18.925440
49.084118	1941.560684	18.930458
49.412755	1948.051851	18.935475
49.253226	1947.587409	18.940493
49.625326	1953.415650	18.945511
49.581544	1969.454584	18.950528
49.505528	1964.222022	18.955546
49.587205	1977.130080	18.960563
49.613356	1969.619838	18.965581
49.798504	1962.281668	18.970599
49.479351	1968.743240	18.975616
49.894169	1972.577019	18.980634
49.962736	1969.679523	18.985651
49.812715	1972.027116	18.990669
49.804112	1966.743685	18.995687
49.629732	1977.710437	19.000704
49.841010	1984.901508	19.005722
49.853227	2002.192414	19.010739
49.646460	2010.569465	19.015757
50.141595	2002.182887	19.020775
49.995610	2008.254247	19.025792
50.060216	2003.978520	19.030810
50.317530	2006.608810	19.035827
50.751541	2021.958067	19.040845
50.768901	2015.467026	19.045863
50.410302	2010.351098	19.050880
50.521927	2018.473647	19.055898
50.439822	2021.237522	19.060915
50.609953	2024.354450	19.065933
51.195245	2023.281171	19.070951
50.875625	2030.445251	19.075968
50.809488	2027.464616	19.080986
50.814641	2033.319169	19.086003
50.901688	2030.710531	19.091021
51.071058	2020.222274	19.096039
50.812579	2024.537868	19.101056
51.238405	2025.230704	19.106074
51.315004	2016.313869	19.111091
51.197866	2025.416795	19.116109
51.011264	2019.228865	19.121127
50.862793	2025.376139	19.126144
50.933643	2021.479324	19.131162
51.595364	2027.607490	19.136179
51.111917	2032.071449	19.141197
51.487113	2041.826580	19.146215
51.631539	2059.293896	19.151232
51.791033	2063.770153	19.156250
51.987505	2055.269149	19.161267
51.755219	2054.335713	19.166285
51.777447	2036.779182	19.171303
51.643700	2046.447168	19.176320
51.901139	2052.583197	19.181338
52.192145	2055.831087	19.186355
52.107576	2054.945667	19.191373
52.407508	2054.510977	19.196391
51.952678	2048.821242	19.201408
52.372958	2051.773212	19.206426
52.391317	2036.387450	19.211443
52.192652	2031.253084	19.216461
52.186621	2013.463545	19.221479
52.412411	2030.653561	19.226496
52.560793	2037.207342	19.231514
52.476800	2029.299328	19.236531
52.540102	2017.159675	19.241549
52.303633	2013.952935	19.246567
52.301552	2035.688709	19.251584
52.410453	2043.020416	19.256602
52.448011	2041.597954	19.261619
52.362197	2054.898553	19.266637
52.418895	2049.076100	19.271655
52.335529	2051.288009	19.276672
52.207618	2049.652821	19.281690
52.673051	2065.372307	19.286707
52.566042	2080.036293	19.291725
52.954916	2073.994094	19.296743
52.846099	2074.177561	19.301760
52.888932	2078.292516	19.306778
53.167001	2074.084188	19.311795
53.234057	2080.858616	19.316813
53.382722	2069.764031	19.321831
53.272724	2075.426167	19.326848
53.263492	2082.166356	19.331866
53.204053	2072.725303	19.336883
53.474777	2079.647370	19.341901
53.377567	2077.004401	19.346919
53.356500	2084.455968	19.351936
53.151736	2100.860523	19.356954
53.459343	2108.479918	19.361971
53.532874	2122.664443	19.366989
53.926574	2109.313388	19.372007
53.924810	2112.118739	19.377024
53.715982	2111.308196	19.382042
54.059071	2108.220582	19.387059
53.829302	2109.618936	19.392077
53.820252	2107.473173	19.397095
54.075284	2112.341652	19.402112
53.816535	2107.217629	19.407130
54.189953	2106.149036	19.412147
53.908438	2115.838278	19.417165
54.242739	2121.146397	19.422183
54.394906	2129.349065	19.427200
54.382772	2139.255712	19.432218
54.633044	2131.657725	19.437235
54.430087	2139.172154	19.442253
54.451282	2134.250455	19.447271
54.700172	2131.207752	19.452288
54.423600	2138.325689	19.457306
54.867811	2119.789323	19.462323
54.489769	2136.735190	19.467341
54.639839	2130.895452	19.472359
54.888558	2129.341766	19.477376
54.691224	2140.634797	19.482394
55.148724	2130.257032	19.487411
54.677758	2133.011373	19.492429
54.948151	2140.440077	19.497447
54.766228	2136.994143	19.502464
54.986991	2154.426586	19.507482
55.335453	2162.883491	19.512499
55.000353	2168.885973	19.517517
55.292595	2166.582024	19.522535
55.502345	2167.492606	19.527552
54.988792	2167.117660	19.532570
55.563750	2163.280412	19.537587
55.560986	2165.140467	19.542605
55.419878	2163.814136	19.547623
55.536811	2166.361445	19.552640
55.618925	2166.313095	19.557658
55.691484	2162.290118	19.562675
55.566124	2165.395215	19.567693
55.680124	2166.236118	19.572711
55.698495	2166.823265	19.577728
55.802017	2182.310357	19.582746
55.917238	2191.142710	19.587763
55.848469	2192.145699	19.592781
55.913102	2196.442055	19.597799
56.131670	2190.143018	19.602816
56.011218	2196.882122	19.607834
56.307423	2188.575937	19.612851
56.260378	2187.414727	19.617869
56.340665	2187.675008	19.622887
56.331998	2184.947104	19.627904
56.155892	2192.366034	19.632922
56.339874	2178.198862	19.637939
56.249814	2193.008921	19.642957
56.596633	2212.571049	19.647975
56.601058	2219.528579	19.652992
56.450059	2220.886848	19.658010
56.863234	2211.254696	19.663027
56.775008	2220.826653	19.668045
56.449402	2219.818420	19.673063
56.898239	2211.504395	19.678080
56.524645	2222.932578	19.683098
56.833534	2231.081989	19.688115
56.996825	2232.274502	19.693133
57.307807	2244.634945	19.698151
57.567730	2242.103311	19.703168
57.698817	2250.269294	19.708186
57.979650	2244.348875	19.713203
57.763975	2232.993713	19.718221
57.329144	2217.885343	19.723239
57.599240	2218.391439	19.728256
57.620561	2236.651025	19.733274
57.853322	2235.913985	19.738291
57.654843	2241.555688	19.743309
57.741759	2230.543196	19.748327
57.876191	2233.640693	19.753344
57.734212	2238.551301	19.758362
58.074104	2235.402032	19.763379
57.513381	2232.678795	19.768397
57.834229	2235.013465	19.773415
57.976118	2232.963170	19.778432
57.986571	2245.549316	19.783450
58.038492	2234.666682	19.788467
57.778946	2238.118055	19.793485
58.026767	2245.315226	19.798503
58.229065	2267.362482	19.803520
58.203304	2275.774527	19.808538
58.803373	2267.123288	19.813555
58.756110	2271.211765	19.818573
58.585207	2264.590965	19.823591
58.528495	2262.084661	19.828608
58.491058	2268.506935	19.833626
58.826526	2258.533184	19.838643
58.740115	2269.044063	19.843661
58.552485	2265.626538	19.848679
59.226121	2258.679896	19.853696
58.883824	2271.880802	19.858714
58.882682	2261.442380	19.863731
58.630854	2259.348690	19.868749
58.891366	2262.079201	19.873767
59.085597	2259.449494	19.878784
59.076471	2278.329883	19.883802
59.337734	2279.923663	19.888819
59.386410	2285.029627	19.893837
59.097435	2288.784607	19.898855
59.297322	2287.425114	19.903872
59.164971	2286.356948	19.908890
59.232932	2284.383723	19.913907
59.332941	2286.745760	19.918925
59.027809	2301.450221	19.923943
59.805723	2311.182203	19.928960
59.807576	2317.117628	19.933978
60.015955	2322.574907	19.938995
59.940719	2325.993757	19.944013
60.013458	2326.621793	19.949031
60.043327	2320.860933	19.954048
59.843507	2322.379595	19.959066
59.953285	2322.242668	19.964083
59.885511	2316.815164	19.969101
60.020619	2316.431928	19.974119
60.484168	2331.357553	19.979136
60.625580	2342.334775	19.984154
60.758386	2347.901655	19.989171
60.629314	2335.711402	19.994189
60.742645	2322.810751	19.999207
60.816831	2312.637156	20.004224
60.672550	2319.801727	20.009242
60.959657	2319.144899	20.014259
61.047512	2312.862725	20.019277
60.652428	2308.861596	20.024295
60.801023	2313.876907	20.029312
60.777396	2332.585844	20.034330
61.080698	2338.143617	20.039347
61.466548	2329.340089	20.044365
61.096439	2333.009699	20.049383
61.236355	2326.572910	20.054400
61.245623	2332.344336	20.059418
61.288772	2329.833104	20.064435
61.554933	2335.082952	20.069453
61.269306	2332.528196	20.074471
61.484292	2324.289163	20.079488
61.469925	2324.046970	20.084506
61.442024	2316.019731	20.089523
61.581875	2323.212924	20.094541
61.477351	2323.032305	20.099559
61.805997	2325.866016	20.104576
61.571879	2336.293526	20.109594
61.635830	2351.469329	20.114611
61.814944	2360.680168	20.119629
61.901188	2369.140476	20.124647
61.933278	2353.863885	20.129664
62.225583	2360.096740	20.134682
62.274756	2366.911910	20.139699
62.346965	2364.654038	20.144717
62.342143	2365.941810	20.149735
62.499826	2355.960166	20.154752
62.377130	2361.169790	20.159770
62.586123	2363.243083	20.164787
62.766501	2354.548612	20.169805
62.410681	2359.933857	20.174823
62.537616	2351.026095	20.179840
62.572661	2355.873897	20.184858
62.782286	2364.371943	20.189875
62.810210	2365.247825	20.194893
62.471295	2373.311860	20.199911
63.040529	2360.974810	20.204928
62.984676	2368.235423	20.209946
62.802097	2373.147832	20.214963
63.207437	2369.263648	20.219981
63.075542	2381.028606	20.224999
63.015988	2375.444811	20.230016
63.300877	2373.237181	20.235034
63.286331	2395.407316	20.240051
63.800899	2393.325874	20.245069
63.667129	2406.700514	20.250087
63.912830	2398.674427	20.255104
63.581948	2398.253818	20.260122
63.743260	2399.997274	20.265139
64.027630	2394.887205	20.270157
63.674999	2402.815791	20.275175
63.756025	2401.962932	20.280192
63.930516	2405.879996	20.285210
63.613042	2408.517088	20.290227
64.044647	2407.896204	20.295245
63.456748	2398.336288	20.300263
64.087833	2401.771499	20.305280
64.203551	2414.781492	20.310298
63.954763	2440.049683	20.315315
64.263051	2431.915271	20.320333
64.280531	2438.774859	20.325351
64.381484	2426.182076	20.330368
64.635556	2426.385539	20.335386
64.398809	2430.948707	20.340403
64.756581	2427.797333	20.345421
64.425622	2448.402356	20.350439
64.781358	2456.947158	20.355456
64.643011	2463.723849	20.360474
64.695356	2475.575126	20.365491
64.973639	2463.698932	20.370509
64.882615	2462.741363	20.375527
64.737479	2465.042632	20.380544
64.834563	2466.922982	20.385562
64.970691	2482.224276	20.390579
65.301669	2479.077951	20.395597
65.317694	2494.293796	20.400615
65.492055	2495.951017	20.405632
65.541418	2486.488410	20.410650
65.207519	2486.942186	20.415667
65.614890	2488.603145	20.420685
65.371234	2495.020654	20.425703
65.471835	2489.112364	20.430720
65.799194	2495.141464	20.435738
65.840287	2510.510647	20.440755
65.829848	2505.545886	20.445773
66.072610	2522.890310	20.450791
66.318477	2524.459829	20.455808
66.584477	2515.208069	20.460826
66.297989	2523.781404	20.465843
66.585966	2510.754408	20.470861
66.558806	2501.601329	20.475879
66.538785	2497.624491	20.480896
66.348227	2492.476082	20.485914
66.625260	2512.022214	20.490931
66.796274	2513.834144	20.495949
66.585660	2521.850265	20.500967
66.672482	2510.987030	20.505984
66.923896	2517.685848	20.511002
66.641504	2516.363140	20.516019
66.942385	2513.308134	20.521037
66.881874	2507.941542	20.526055
66.878997	2509.972350	20.531072
66.661857	2510.653708	20.536090
66.937681	2518.502570	20.541107
67.298210	2523.485724	20.546125
67.040205	2541.797323	20.551143
67.324946	2548.437351	20.556160
67.483780	2541.641909	20.561178
66.971114	2548.464969	20.566195
67.367414	2542.304979	20.571213
67.394595	2543.078733	20.576231
67.414818	2548.243602	20.581248
67.582935	2559.366183	20.586266
67.636657	2575.283253	20.591283
67.756395	2571.136222	20.596301
67.753183	2577.364389	20.601319
67.886672	2585.597039	20.606336
68.053254	2575.672822	20.611354
68.021844	2572.959485	20.616371
68.431919	2569.306542	20.621389
68.260322	2573.559668	20.626407
68.226721	2568.014136	20.631424
68.591916	2583.155504	20.636442
68.401645	2591.099197	20.641459
68.487947	2593.328962	20.646477
68.932217	2596.915154	20.651495
68.786502	2590.246924	20.656512
68.918592	2591.988772	20.661530
68.713843	2602.186032	20.666547
68.651601	2590.829716	20.671565
68.989867	2597.567421	20.676583
69.019929	2596.436356	20.681600
69.139307	2592.836851	20.686618
68.976072	2591.799546	20.691635
69.039685	2596.421836	20.696653
69.020022	2594.362648	20.701671
69.026889	2606.232297	20.706688
69.218510	2594.048100	20.711706
69.233345	2615.987342	20.716723
69.576822	2617.293524	20.721741
69.567235	2620.879743	20.726759
69.586924	2621.933153	20.731776
69.725684	2622.182543	20.736794
69.739035	2621.768377	20.741811
69.798594	2617.771734	20.746829
70.081099	2622.886930	20.751847
69.873980	2623.141144	20.756864
70.038395	2622.654901	20.761882
69.884225	2623.872910	20.766899
69.817663	2641.204669	20.771917
70.115860	2644.689102	20.776935
70.024674	2656.272374	20.781952
70.637296	2650.825112	20.786970
70.370423	2649.349675	20.791987
70.402501	2653.774856	20.797005
70.659639	2657.962772	20.802023
70.560013	2660.190737	20.807040
70.750229	2652.598914	20.812058
70.319989	2673.525289	20.817075
71.000181	2677.647308	20.822093
71.085958	2679.444537	20.827111
70.903699	2671.552634	20.832128
71.015795	2675.298018	20.837146
71.030422	2686.482147	20.842163
70.927442	2674.109677	20.847181
71.220314	2678.283246	20.852199
71.241284	2687.238698	20.857216
71.306202	2698.496623	20.862234
71.529497	2699.836140	20.867251
71.714800	2702.149243	20.872269
71.941545	2698.261209	20.877287
71.804069	2697.558028	20.882304
72.103582	2692.903246	20.887322
71.844658	2694.141115	20.892339
72.379228	2695.018017	20.897357
72.468270	2693.100371	20.902375
72.136605	2701.213770	20.907392
72.233849	2691.788230	20.912410
72.170524	2691.910958	20.917427
72.112715	2684.906942	20.922445
72.395192	2696.225345	20.927463
72.070249	2696.615556	20.932480
72.169301	2696.751716	20.937498
72.253752	2703.018657	20.942515
72.371209	2696.183334	20.947533
72.430244	2710.203981	20.952551
72.437108	2720.850550	20.957568
72.625204	2716.473112	20.962586
72.601450	2720.610667	20.967603
72.601925	2727.403881	20.972621
72.975634	2719.822875	20.977639
72.954495	2740.910639	20.982656
73.331532	2744.280262	20.987674
73.373061	2747.920502	20.992691
73.433960	2734.514983	20.997709
73.519710	2738.815998	21.002727
73.547372	2749.934382	21.007744
73.644746	2747.694463	21.012762
73.861251	2755.635509	21.017779
73.489860	2755.044361	21.022797
73.712189	2751.701351	21.027815
73.699036	2750.848547	21.032832
73.533174	2750.092468	21.037850
73.716010	2762.299951	21.042867
73.643829	2753.695083	21.047885
73.969951	2770.242257	21.052903
73.791779	2789.366586	21.057920
74.312740	2782.581710	21.062938
74.417122	2783.255850	21.067955
74.184211	2785.671067	21.072973
74.265965	2778.804429	21.077991
74.119029	2791.199043	21.083008
74.517725	2793.742427	21.088026
74.581118	2804.854367	21.093043
74.722483	2806.084251	21.098061
75.134469	2802.028201	21.103079
74.906356	2810.704091	21.108096
74.935490	2810.980408	21.113114
75.204226	2813.601947	21.118131
74.881410	2813.219367	21.123149
75.130539	2808.641021	21.128167
74.886668	2807.976042	21.133184
75.037394	2825.779942	21.138202
75.030929	2843.088196	21.143219
75.058882	2845.155037	21.148237
75.592546	2846.194923	21.153255
75.178345	2842.796092	21.158272
75.630022	2851.187382	21.163290
76.512363	2855.394419	21.168307
76.055809	2849.729810	21.173325
76.269348	2831.416553	21.178343
76.213347	2831.511369	21.183360
76.214261	2831.489342	21.188378
76.423401	2825.990737	21.193395
75.941521	2830.405911	21.198413
76.374794	2819.935561	21.203431
76.519417	2840.838136	21.208448
76.471227	2840.171050	21.213466
76.752467	2850.916329	21.218483
76.388989	2855.545464	21.223501
76.858811	2853.674046	21.228519
76.574836	2855.947961	21.233536
76.909981	2850.220798	21.238554
76.786353	2858.052532	21.243571
76.649653	2848.783769	21.248589
77.053952	2847.770772	21.253607
76.820433	2856.021993	21.258624
76.692519	2854.354462	21.263642
77.222379	2858.706606	21.268659
76.863494	2880.980379	21.273677
77.482420	2885.712421	21.278695
77.079364	2891.253275	21.283712
77.227186	2882.706063	21.288730
77.208876	2883.513835	21.293747
77.280340	2904.542229	21.298765
77.778033	2902.274623	21.303783
77.695656	2915.267887	21.308800
77.592828	2916.187469	21.313818
78.398008	2910.607928	21.318835
78.005386	2908.948785	21.323853
78.126164	2905.700599	21.328871
78.108203	2905.979709	21.333888
78.368377	2904.359615	21.338906
78.359005	2916.230532	21.343923
78.375927	2937.472980	21.348941
78.640454	2936.638807	21.353959
78.553663	2939.095247	21.358976
78.767874	2939.452962	21.363994
79.050032	2935.282284	21.369011
78.671698	2934.115642	21.374029
78.935804	2937.611877	21.379047
79.003914	2939.119333	21.384064
78.804677	2937.250780	21.389082
78.876934	2939.854909	21.394099
78.619650	2948.430126	21.399117
79.108629	2954.452520	21.404135
79.097829	2970.948251	21.409152
79.115433	2970.242348	21.414170
79.324139	2965.410029	21.419187
79.515615	2986.682917	21.424205
79.565850	2986.977111	21.429223
79.937730	3004.340846	21.434240
79.815108	2994.651262	21.439258
79.690974	2993.403168	21.444275
79.650264	3009.696832	21.449293
80.113628	2996.713016	21.454311
79.988426	2997.081602	21.459328
80.092124	3003.721608	21.464346
80.338801	3021.326374	21.469363
80.473985	3023.320287	21.474381
80.229587	3027.130486	21.479399
80.418558	3028.826344	21.484416
80.550100	3031.416314	21.489434
80.776043	3026.305907	21.494451
80.500440	3029.415482	21.499469
80.744309	3022.979902	21.504487
80.765268	3030.724165	21.509504
80.566329	3035.781782	21.514522
80.941419	3045.825513	21.519539
81.319482	3058.748615	21.524557
81.176126	3053.405261	21.529575
81.167056	3064.819220	21.534592
81.097213	3072.350652	21.539610
81.739595	3052.646404	21.544627
81.389266	3065.628260	21.549645
81.757337	3049.402964	21.554663
81.583629	3049.446544	21.559680
81.730380	3069.594733	21.564698
82.078616	3079.732446	21.569715
82.107803	3083.622526	21.574733
82.259071	3087.084876	21.579751
82.262295	3086.022558	21.584768
82.375958	3083.717060	21.589786
82.159010	3085.301461	21.594803
82.226317	3083.105619	21.599821
82.491335	3077.848943	21.604839
82.515637	3074.376972	21.609856
82.869343	3087.302411	21.614874
82.906596	3074.050598	21.619891
82.849277	3074.907867	21.624909
82.699381	3062.246778	21.629927
82.954646	3068.077588	21.634944
82.677219	3073.944589	21.639962
82.968907	3083.642160	21.644979
82.731185	3108.087710	21.649997
82.887211	3109.263364	21.655015
82.943038	3103.547614	21.660032
83.009077	3118.037939	21.665050
83.254699	3120.026838	21.670067
83.328227	3130.552157	21.675085
83.810087	3130.162370	21.680103
83.766706	3128.356250	21.685120
83.955158	3128.386121	21.690138
84.127578	3121.948521	21.695155
84.096103	3126.708860	21.700173
84.034711	3123.894794	21.705191
83.762117	3131.045613	21.710208
84.207669	3142.610528	21.715226
84.203564	3147.730718	21.720243
84.442447	3155.011576	21.725261
84.786819	3159.942465	21.730279
84.866144	3153.072892	21.735296
84.924285	3158.616592	21.740314
84.691544	3157.054634	21.745331
84.361872	3158.412378	21.750349
84.669428	3162.530256	21.755367
85.021447	3154.643341	21.760384
84.669054	3162.128634	21.765402
84.941929	3153.587278	21.770419
84.893591	3176.516005	21.775437
85.046034	3178.201974	21.780455
85.255725	3186.654866	21.785472
85.035815	3195.179427	21.790490
85.503954	3184.831480	21.795507
85.391632	3192.744972	21.800525
85.180141	3204.507552	21.805543
85.822567	3210.601550	21.810560
85.649815	3220.263157	21.815578
85.884118	3223.414162	21.820595
85.697514	3229.456318	21.825613
85.601932	3214.465861	21.830631
85.871340	3229.634979	21.835648
85.799284	3240.517130	21.840666
86.217047	3240.062046	21.845683
85.941070	3247.411693	21.850701
86.224181	3259.044300	21.855719
86.552510	3252.609310	21.860736
87.018516	3263.954735	21.865754
87.240904	3254.405038	21.870771
87.434780	3260.988302	21.875789
87.482273	3245.756309	21.880807
87.594672	3226.918272	21.885824
87.268946	3230.898034	21.890842
87.994948	3213.726573	21.895859
87.834298	3224.732971	21.900877
87.614103	3211.537040	21.905895
87.734812	3212.096894	21.910912
87.782610	3216.088663	21.915930
87.984506	3214.211949	21.920947
88.153582	3214.078144	21.925965
88.087452	3219.670006	21.930983
88.336797	3208.649753	21.936000
88.125626	3210.078278	21.941018
88.178782	3208.412506	21.946035
88.155908	3212.442290	21.951053
88.111074	3211.605526	21.956071
88.272983	3211.258900	21.961088
88.096905	3217.341063	21.966106
88.352148	3226.912388	21.971123
88.185754	3235.548006	21.976141
88.455092	3243.449427	21.981159
88.806912	3243.262091	21.986176
88.398809	3247.786761	21.991194
88.489911	3247.683485	21.996211
88.827178	3265.854635	22.001229
88.746707	3278.411333	22.006247
88.944650	3276.373981	22.011264
89.081523	3286.894816	22.016282
89.164789	3278.980687	22.021299
88.999161	3291.374771	22.026317
89.035384	3309.213255	22.031335
89.056240	3304.812758	22.036352
89.312408	3321.597481	22.041370
89.798367	3318.722828	22.046387
89.809154	3336.959509	22.051405
89.565659	3347.988651	22.056423
89.982236	3340.735600	22.061440
89.842233	3347.521614	22.066458
89.702785	3349.777273	22.071475
89.892871	3358.416679	22.076493
90.290041	3369.497055	22.081511
90.175714	3371.830521	22.086528
89.898218	3381.468820	22.091546
90.543242	3373.819036	22.096563
90.640281	3385.639537	22.101581
90.697205	3390.569937	22.106599
91.111018	3383.819971	22.111616
91.019698	3398.046186	22.116634
91.195705	3388.649329	22.121651
91.397137	3396.096757	22.126669
91.388602	3383.321594	22.131687
91.406421	3390.904499	22.136704
91.604262	3395.180752	22.141722
91.503604	3392.796898	22.146739
91.501723	3383.474828	22.151757
92.128949	3396.650336	22.156775
92.852735	3389.028889	22.161792
92.575596	3375.971687	22.166810
92.649260	3376.455667	22.171827
92.800609	3373.661903	22.176845
92.429762	3373.396308	22.181863
92.851643	3364.271763	22.186880
92.629999	3368.022569	22.191898
92.515677	3362.963954	22.196915
92.579932	3365.400308	22.201933
92.190388	3371.317559	22.206951
92.691155	3366.936475	22.211968
92.794021	3361.317745	22.216986
92.564679	3352.125582	22.222003
92.905932	3365.504000	22.227021
92.894651	3388.880255	22.232039
92.895886	3389.601554	22.237056
92.979904	3392.853656	22.242074
93.013708	3398.364356	22.247091
93.474264	3404.468565	22.252109
93.047368	3421.452020	22.257127
93.093305	3425.804427	22.262144
93.173325	3430.193878	22.267162
93.225786	3435.736229	22.272179
93.503402	3449.566182	22.277197
93.906024	3459.785165	22.282215
93.805291	3451.360649	22.287232
93.982306	3463.817441	22.292250
94.141067	3474.404146	22.297267
94.307162	3487.412567	22.302285
93.932666	3487.747764	22.307303
94.485875	3493.740477	22.312320
94.688853	3487.777700	22.317338
94.477410	3493.294510	22.322355
94.716913	3497.203076	22.327373
94.687920	3495.737595	22.332391
94.942492	3512.498406	22.337408
94.972343	3522.769805	22.342426
95.091818	3526.438713	22.347443
95.385987	3520.117614	22.352461
95.170049	3528.751078	22.357479
95.401218	3513.298358	22.362496
95.401556	3516.608672	22.367514
95.677426	3530.631710	22.372531
95.843912	3544.280453	22.377549
95.694810	3551.310301	22.382567
95.855477	3540.556459	22.387584
95.898416	3545.761323	22.392602
95.897460	3546.110893	22.397619
96.160615	3540.026793	22.402637
96.094303	3550.809926	22.407655
96.233416	3566.561844	22.412672
96.442394	3578.583338	22.417690
96.228749	3583.738671	22.422707
96.870411	3575.078472	22.427725
96.664628	3580.625091	22.432743
96.930745	3574.977097	22.437760
96.835732	3568.954828	22.442778
97.090433	3590.447428	22.447795
97.316498	3592.577178	22.452813
97.047354	3607.995418	22.457831
97.475842	3603.647819	22.462848
97.680198	3600.526963	22.467866
97.798399	3602.440280	22.472883
97.712835	3590.714032	22.477901
97.310631	3609.637589	22.482919
97.633397	3604.290492	22.487936
97.913274	3613.478974	22.492954
97.895773	3625.361202	22.497971
98.381516	3626.551967	22.502989
97.926226	3641.004808	22.508007
98.027152	3627.258547	22.513024
98.325665	3624.206842	22.518042
98.416465	3620.880681	22.523059
98.737218	3630.891791	22.528077
99.398949	3632.444671	22.533095
99.950501	3623.755549	22.538112
99.680813	3603.077404	22.543130
99.507026	3608.126485	22.548147
99.580739	3592.546969	22.553165
99.368951	3599.805527	22.558183
99.743348	3590.063026	22.563200
99.899563	3603.286310	22.568218
99.498428	3603.354361	22.573235
100.034072	3591.699745	22.578253
99.755639	3600.265338	22.583271
100.032659	3602.716572	22.588288
99.827197	3597.927288	22.593306
99.417272	3606.391924	22.598323
99.894246	3588.883725	22.603341
99.741625	3596.316923	22.608359
99.679491	3604.458628	22.613376
99.840993	3610.903256	22.618394
99.852465	3614.570532	22.623411
100.433350	3622.962119	22.628429
100.150100	3636.365652	22.633447
99.900214	3641.053218	22.638464
100.372058	3648.548114	22.643482
100.416635	3658.657569	22.648499
100.596887	3672.378183	22.653517
100.676529	3692.111562	22.658535
100.657004	3695.987547	22.663552
100.876842	3695.255649	22.668570
101.170120	3724.755216	22.673587
101.319618	3721.090061	22.678605
101.465169	3732.017323	22.683623
101.209287	3728.559990	22.688640
101.578524	3737.717779	22.693658
101.377853	3758.887560	22.698675
101.750115	3754.850177	22.703693
101.878425	3761.138898	22.708711
101.992985	3780.880201	22.713728
102.515358	3778.272628	22.718746
102.647696	3767.385473	22.723763
102.876687	3763.865748	22.728781
102.788734	3768.057890	22.733799
103.141359	3770.400335	22.738816
103.179243	3757.428644	22.743834
102.757896	3762.266313	22.748851
103.245540	3766.754482	22.753869
103.162891	3766.603394	22.758887
103.290888	3762.293446	22.763904
103.026412	3765.700330	22.768922
102.884669	3772.641789	22.773939
103.529302	3780.445103	22.778957
103.636448	3794.193223	22.783975
103.834889	3793.896613	22.788992
104.141806	3791.667959	22.794010
104.115529	3798.388842	22.799027
103.894267	3795.380664	22.804045
104.038709	3796.918516	22.809063
103.955668	3805.973053	22.814080
104.345504	3814.694153	22.819098
104.288072	3823.091683	22.824115
104.295008	3827.481109	22.829133
104.466325	3826.445424	22.834151
104.737617	3832.667319	22.839168
104.872290	3849.008677	22.844186
104.894800	3850.717808	22.849203
105.253611	3848.616963	22.854221
105.454309	3853.517510	22.859239
105.569999	3854.324418	22.864256
105.589477	3845.861623	22.869274
105.625947	3862.104590	22.874291
105.734340	3850.587923	22.879309
105.797603	3852.076581	22.884327
105.602452	3859.952508	22.889344
105.513647	3850.666816	22.894362
105.545563	3857.814261	22.899379
105.709819	3860.096295	22.904397
106.063230	3876.024411	22.909415
106.023463	3881.035690	22.914432
106.339786	3881.790150	22.919450
105.947130	3883.748003	22.924467
106.401059	3893.809642	22.929485
106.354379	3921.600107	22.934503
106.320150	3919.451014	22.939520
106.593385	3910.428509	22.944538
106.556503	3931.987779	22.949555
106.716212	3953.466955	22.954573
107.108069	3946.832732	22.959591
106.891726	3953.591078	22.964608
107.295336	3958.683502	22.969626
107.283818	3971.343862	22.974643
107.796346	3971.380269	22.979661
107.803905	3979.747857	22.984679
107.645098	3980.541908	22.989696
108.141458	3974.314238	22.994714
107.683952	3983.460858	22.999731
108.171655	3996.502616	23.004749
108.055389	4002.981488	23.009767
108.154810	4003.830333	23.014784
108.435025	4005.157752	23.019802
108.278146	4014.105404	23.024819
108.744204	4010.724030	23.029837
108.970893	4018.089866	23.034855
108.720918	4030.270673	23.039872
109.486581	4022.093128	23.044890
109.571502	4025.224865	23.049907
109.475801	4031.306344	23.054925
109.651537	4018.662510	23.059943
109.426136	4020.681028	23.064960
109.817393	4029.735582	23.069978
109.748836	4019.299579	23.074995
109.937150	4010.979685	23.080013
110.037367	4010.625575	23.085031
109.679943	4028.094252	23.090048
110.008862	4041.771836	23.095066
110.014884	4053.697859	23.100083
110.029020	4054.560308	23.105101
110.552478	4054.049804	23.110119
110.390952	4046.654177	23.115136
110.645632	4059.604925	23.120154
110.802333	4068.421573	23.125171
110.894628	4071.456956	23.130189
110.977122	4064.731202	23.135207
110.780501	4069.899723	23.140224
111.166915	4066.610493	23.145242
111.085493	4071.973833	23.150259
110.594521	4077.668388	23.155277
111.148649	4083.603773	23.160295
111.095377	4105.383822	23.165312
111.515718	4099.912425	23.170330
111.607046	4104.414345	23.175347
111.761840	4119.813497	23.180365
112.046546	4132.805936	23.185383
111.491267	4136.254560	23.190400
112.136030	4130.389421	23.195418
112.045964	4148.849305	23.200435
112.393671	4156.219512	23.205453
112.538091	4159.034982	23.210471
112.314865	4157.749095	23.215488
112.665048	4161.369570	23.220506
112.401149	4171.255593	23.225523
112.739434	4184.289094	23.230541
113.356299	4188.707228	23.235559
113.110628	4200.506731	23.240576
113.351235	4186.798247	23.245594
113.346633	4201.284388	23.250611
113.784637	4215.825041	23.255629
114.037024	4222.415928	23.260647
113.861887	4229.484078	23.265664
113.966384	4215.264685	23.270682
113.667781	4221.122141	23.275699
114.098461	4225.840599	23.280717
114.437700	4228.821686	23.285735
114.107709	4225.628578	23.290752
114.278819	4239.692604	23.295770
114.587635	4255.542496	23.300787
114.551623	4258.551965	23.305805
114.555896	4255.901068	23.310823
114.554296	4264.609342	23.315840
115.041749	4271.916414	23.320858
115.261438	4292.366181	23.325875
115.148827	4290.836860	23.330893
115.359106	4288.626692	23.335911
114.898979	4294.325063	23.340928
115.245829	4311.618824	23.345946
115.646665	4322.184844	23.350963
115.849457	4323.936868	23.355981
116.163907	4321.411138	23.360999
116.085389	4318.679030	23.366016
116.008895	4338.722961	23.371034
116.309350	4343.866587	23.376051
116.460967	4353.013055	23.381069
116.695531	4344.776855	23.386087
116.356401	4346.807259	23.391104
116.726143	4354.035594	23.396122
116.841550	4351.593524	23.401139
116.872780	4368.398013	23.406157
116.807932	4369.564942	23.411175
116.903662	4377.247642	23.416192
116.975348	4374.596200	23.421210
116.927819	4383.978987	23.426227
117.269690	4397.750028	23.431245
117.500986	4403.080925	23.436263
117.445287	4403.923851	23.441280
117.413538	4410.317833	23.446298
117.806409	4426.809038	23.451315
117.778254	4432.680089	23.456333
118.251033	4436.395154	23.461351
118.156015	4446.354338	23.466368
118.543357	4436.767346	23.471386
118.290058	4451.497936	23.476403
118.282397	4471.850471	23.481421
118.708862	4465.750177	23.486439
118.387017	4468.657373	23.491456
118.671878	4481.436900	23.496474
119.008292	4496.099451	23.501491
119.128527	4501.112959	23.506509
119.549320	4492.533870	23.511527
119.417360	4504.317055	23.516544
119.696133	4510.327211	23.521562
120.183213	4519.458833	23.526579
120.626005	4518.164250	23.531597
120.959059	4502.236387	23.536615
120.828571	4484.712294	23.541632
120.840461	4479.135970	23.546650
120.831609	4472.987876	23.551667
120.765657	4479.517936	23.556685
120.643355	4470.511753	23.561703
120.932850	4466.433885	23.566720
121.019727	4464.152113	23.571738
121.201497	4464.540221	23.576755
120.844941	4473.265889	23.581773
121.172839	4477.457211	23.586791
121.360087	4501.542287	23.591808
121.170112	4504.002853	23.596826
121.472118	4500.661694	23.601843
121.459974	4501.963408	23.606861
121.528649	4510.031257	23.611879
121.591903	4523.851570	23.616896
121.596960	4529.858183	23.621914
122.170125	4532.864177	23.626931
122.003910	4544.857401	23.631949
122.531323	4555.655150	23.636967
122.307946	4568.109864	23.641984
122.336677	4561.629257	23.647002
122.574746	4562.865112	23.652019
122.661104	4572.446946	23.657037
122.596728	4591.354069	23.662055
122.904036	4592.290950	23.667072
123.069126	4594.573754	23.672090
123.070647	4593.630392	23.677107
123.051621	4623.819591	23.682125
123.437836	4620.884293	23.687143
123.669559	4620.663392	23.692160
123.410467	4635.540630	23.697178
123.750542	4629.905618	23.702195
123.982358	4648.004044	23.707213
123.967578	4652.069121	23.712231
124.233083	4643.738923	23.717248
124.137322	4648.664200	23.722266
124.592999	4651.250759	23.727283
124.471683	4681.358836	23.732301
124.723507	4678.988577	23.737319
124.896121	4684.642833	23.742336
124.503711	4679.989999	23.747354
125.276160	4687.513020	23.752371
125.286098	4704.584050	23.757389
125.225967	4705.982333	23.762407
125.488416	4705.977598	23.767424
125.738903	4710.559742	23.772442
125.802373	4704.365403	23.777459
125.633963	4706.138908	23.782477
126.120715	4719.492218	23.787495
126.124665	4732.100415	23.792512
126.052796	4737.744117	23.797530
126.152341	4735.964569	23.802547
126.480431	4746.038999	23.807565
126.608676	4751.233834	23.812583
126.851224	4767.847735	23.817600
126.840859	4768.914747	23.822618
127.003438	4770.085561	23.827635
126.803504	4777.777859	23.832653
126.720061	4772.652468	23.837671
127.353655	4787.513375	23.842688
127.095872	4795.473738	23.847706
127.350466	4802.453174	23.852723
127.501288	4816.517054	23.857741
127.582131	4825.845035	23.862759
127.593043	4834.056016	23.867776
127.826435	4843.624805	23.872794
128.135666	4851.511296	23.877811
128.025184	4867.660799	23.882829
128.391061	4863.565135	23.887847
128.568966	4874.746920	23.892864
128.602281	4887.168047	23.897882
128.777133	4898.054530	23.902899
128.981716	4900.815706	23.907917
129.112179	4892.806646	23.912935
128.958230	4907.124550	23.917952
129.093526	4918.870165	23.922970
129.424422	4919.781278	23.927987
129.568102	4927.439312	23.933005
129.718185	4931.548980	23.938023
130.350324	4933.868285	23.943040
130.310451	4943.953540	23.948058
130.399369	4939.818630	23.953075
130.588864	4940.828606	23.958093
130.696050	4937.322525	23.963111
131.003423	4940.651068	23.968128
130.724246	4942.862377	23.973146
131.063968	4939.021829	23.978163
130.891395	4936.018236	23.983181
131.002851	4934.656877	23.988199
131.522092	4943.122000	23.993216
131.121109	4945.276422	23.998234
131.397629	4942.429361	24.003251
131.337485	4959.843861	24.008269
131.551301	4967.081632	24.013287
131.663215	4971.183237	24.018304
131.733405	4974.502408	24.023322
132.233703	4972.289161	24.028339
131.823039	4992.798729	24.033357
131.844799	4998.113694	24.038375
132.441555	4992.521793	24.043392
132.274711	4996.833859	24.048410
132.577026	5015.214945	24.053427
132.457144	5029.602273	24.058445
132.700663	5025.069774	24.063463
132.913356	5038.937544	24.068480
133.303799	5045.638959	24.073498
134.083953	5039.104399	24.078515
134.173032	5031.037352	24.083533
133.669876	5041.524620	24.088551
134.325789	5031.235923	24.093568
134.420808	5038.783765	24.098586
134.356488	5040.368416	24.103603
134.405346	5031.704359	24.108621
134.457446	5032.895173	24.113639
134.678374	5031.827893	24.118656
134.560224	5031.281218	24.123674
134.908265	5035.773955	24.128691
135.138985	5055.563744	24.133709
135.048369	5053.913612	24.138727
135.339244	5051.483570	24.143744
135.253796	5060.464519	24.148762
135.214197	5060.285309	24.153779
135.177844	5060.112661	24.158797
135.515579	5082.684617	24.163815
135.690106	5091.615474	24.168832
135.344820	5100.438840	24.173850
135.492189	5106.209001	24.178867
135.988603	5118.517924	24.183885
136.323110	5132.445817	24.188903
136.362950	5121.444964	24.193920
136.577942	5142.914701	24.198938
136.577793	5156.811017	24.203955
136.795635	5150.577713	24.208973
136.779854	5154.926313	24.213991
137.100613	5158.918353	24.219008
137.124009	5177.756372	24.224026
137.723520	5176.640511	24.229043
137.922703	5186.373902	24.234061
137.667692	5187.642025	24.239079
137.609035	5183.105740	24.244096
137.687613	5181.106049	24.249114
137.815308	5184.689096	24.254131
137.887680	5199.476278	24.259149
138.373225	5214.729424	24.264167
138.139241	5214.907707	24.269184
138.112021	5219.356493	24.274202
138.440034	5235.747235	24.279219
138.865662	5238.396912	24.284237
138.505889	5255.617225	24.289255
138.783534	5259.705857	24.294272
139.026952	5276.269056	24.299290
139.068195	5272.989765	24.304307
139.190076	5293.999376	24.309325
139.493510	5315.633065	24.314343
139.953165	5309.811939	24.319360
139.821603	5311.115459	24.324378
139.920764	5312.394774	24.329395
140.130682	5318.175499	24.334413
140.409604	5335.105234	24.339431
140.414086	5328.444845	24.344448
140.514101	5328.430613	24.349466
140.620267	5331.405040	24.354483
141.071651	5350.429148	24.359501
140.998365	5364.363285	24.364519
141.171710	5359.096037	24.369536
140.850045	5369.032192	24.374554
141.070190	5377.783649	24.379571
141.364736	5394.429304	24.384589
141.389500	5397.656684	24.389607
141.908392	5414.097434	24.394624
141.910443	5427.122719	24.399642
141.818463	5429.992655	24.404659
142.067517	5438.024381	24.409677
142.337910	5442.034758	24.414695
142.579734	5445.022192	24.419712
142.463736	5459.665800	24.424730
142.265693	5457.072126	24.429747
142.660100	5473.812092	24.434765
142.612709	5495.282484	24.439783
143.079738	5499.229263	24.444800
143.229789	5512.028039	24.449818
143.465519	5508.248775	24.454835
143.845357	5518.759216	24.459853
143.932354	5531.088141	24.464871
144.035909	5538.021993	24.469888
144.134359	5545.307557	24.474906
144.323456	5545.719704	24.479923
144.750104	5535.774845	24.484941
144.673762	5543.258221	24.489959
144.655603	5558.595195	24.494976
144.708375	5567.390764	24.499994
144.741299	5566.872690	24.505011
145.115475	5572.427485	24.510029
144.958502	5571.606106	24.515047
145.160075	5592.505875	24.520064
145.281941	5609.854350	24.525082
145.358624	5610.733667	24.530099
145.787099	5611.565540	24.535117
145.689397	5630.487174	24.540135
146.026562	5640.426235	24.545152
146.147387	5635.967404	24.550170
146.100275	5649.628561	24.555187
146.592182	5662.672711	24.560205
146.379693	5669.648368	24.565223
146.602933	5663.877394	24.570240
146.823363	5688.214029	24.575258
146.855568	5699.863411	24.580275
147.095563	5701.941687	24.585293
146.990654	5717.010209	24.590311
147.695552	5726.149553	24.595328
147.754638	5733.998519	24.600346
147.481715	5741.451187	24.605363
147.730427	5742.632736	24.610381
147.821497	5764.795825	24.615399
148.188261	5763.130898	24.620416
148.452340	5764.417785	24.625434
150.071311	5732.773950	24.630451
150.497985	5725.278960	24.635469
150.459645	5725.647130	24.640487
150.484772	5706.170762	24.645504
150.462764	5692.871758	24.650522
150.211136	5684.055397	24.655539
150.550167	5676.412333	24.660557
150.300505	5674.462558	24.665575
150.563827	5665.824512	24.670592
150.541730	5650.199883	24.675610
149.904875	5656.372256	24.680627
150.594413	5664.188313	24.685645
150.610356	5675.859940	24.690663
150.560574	5680.025293	24.695680
150.555507	5686.602822	24.700698
150.492590	5686.049674	24.705715
150.727726	5700.423527	24.710733
150.672778	5705.029513	24.715751
151.222865	5708.727863	24.720768
151.294275	5732.372376	24.725786
151.361276	5738.076924	24.730803
151.574164	5736.925908	24.735821
151.644190	5757.742248	24.740839
151.905912	5776.152000	24.745856
151.731209	5780.024953	24.750874
152.087981	5794.746924	24.755891
152.129722	5803.027483	24.760909
151.918686	5813.944707	24.765927
152.358491	5829.646379	24.770944
152.542625	5846.213378	24.775962
152.745678	5855.041015	24.780979
153.021616	5861.761065	24.785997
153.066583	5886.081947	24.791015
152.860606	5885.637362	24.796032
153.337940	5894.951574	24.801050
153.377568	5908.897327	24.806067
153.559141	5909.652148	24.811085
153.379019	5929.117594	24.816103
153.717597	5936.945703	24.821120
154.336596	5940.884106	24.826138
154.173836	5963.586788	24.831155
154.416119	5964.679688	24.836173
154.542322	5975.471656	24.841191
155.087989	5988.354101	24.846208
155.368365	6008.053850	24.851226
155.224649	6011.748043	24.856243
155.527530	6002.273438	24.861261
155.706637	6015.385090	24.866279
155.726143	6008.119324	24.871296
155.982038	6023.059025	24.876314
156.121520	6032.199031	24.881331
156.383140	6026.156651	24.886349
156.260774	6045.509184	24.891367
156.532440	6053.789411	24.896384
156.811269	6064.758524	24.901402
156.888979	6067.784845	24.906419
156.849225	6065.368025	24.911437
157.019203	6083.698376	24.916455
157.081702	6091.304656	24.921472
157.168595	6102.575058	24.926490
157.025756	6117.246412	24.931507
157.468074	6118.087912	24.936525
157.466041	6136.071244	24.941543
157.374970	6157.243498	24.946560
157.915151	6172.301670	24.951578
157.973403	6193.731050	24.956595
158.016415	6192.703864	24.961613
158.266556	6213.908337	24.966631
158.628447	6223.363906	24.971648
158.976778	6236.131691	24.976666
159.164643	6248.290918	24.981683
159.100559	6261.811361	24.986701
159.369818	6273.747555	24.991719
159.393077	6274.337235	24.996736
159.587702	6287.334928	25.001754
159.685510	6301.765096	25.006771
160.028751	6298.860721	25.011789
160.038030	6328.018176	25.016807
160.518597	6331.243103	25.021824
160.937616	6323.086550	25.026842
160.736409	6336.324435	25.031859
161.107169	6344.661411	25.036877
161.151353	6354.170872	25.041895
161.332377	6357.004534	25.046912
161.466539	6358.210696	25.051930
161.473075	6369.365865	25.056947
161.824717	6380.821648	25.061965
161.877944	6386.479074	25.066983
162.150629	6392.002371	25.072000
162.268231	6387.524159	25.077018
161.913571	6398.135828	25.082035
162.169894	6407.523374	25.087053
162.293681	6415.832893	25.092071
162.640843	6426.693815	25.097088
163.029947	6438.022501	25.102106
162.974514	6447.048284	25.107123
163.273405	6449.801799	25.112141
163.288389	6459.236516	25.117159
163.584387	6481.145333	25.122176
163.833769	6475.202288	25.127194
163.535439	6478.015633	25.132211
164.036597	6495.609947	25.137229
164.153656	6509.192214	25.142247
164.212985	6524.070135	25.147264
164.363065	6524.553053	25.152282
164.788771	6540.753422	25.157299
164.802603	6542.085792	25.162317
165.148118	6552.991131	25.167335
165.131907	6570.297443	25.172352
165.191348	6573.926333	25.177370
165.496034	6583.911339	25.182387
166.042339	6594.665095	25.187405
166.309763	6598.325345	25.192423
166.297589	6608.283785	25.197440
166.598430	6608.093544	25.202458
166.565242	6606.803882	25.207475
166.475609	6607.324240	25.212493
166.717474	6625.089879	25.217511
166.768293	6647.938942	25.222528
167.053928	6632.626932	25.227546
167.204101	6652.670109	25.232563
167.237843	6671.848282	25.237581
167.242638	6678.256299	25.242599
167.358163	6680.624443	25.247616
167.759173	6702.250110	25.252634
167.594932	6719.786347	25.257651
167.958846	6724.986002	25.262669
168.306711	6729.880570	25.267687
168.209614	6741.707179	25.272704
168.865039	6761.962636	25.277722
169.120324	6764.325818	25.282739
168.910198	6773.822595	25.287757
169.336715	6783.893744	25.292775
169.383658	6795.383485	25.297792
169.856462	6794.417552	25.302810
169.697760	6799.864226	25.307827
169.934112	6791.520170	25.312845
170.105809	6813.428841	25.317863
170.494914	6817.402571	25.322880
170.853875	6815.345364	25.327898
171.115340	6810.812613	25.332915
171.270308	6816.211638	25.337933
171.595018	6808.189458	25.342951
171.402148	6810.002516	25.347968
171.697694	6808.002632	25.352986
171.794696	6815.051431	25.358003
171.748408	6807.755637	25.363021
171.733168	6808.816491	25.368039
171.641567	6834.472340	25.373056
172.359733	6840.947648	25.378074
172.225834	6851.898966	25.383091
172.072920	6854.726174	25.388109
172.216640	6858.702848	25.393127
172.375788	6884.856992	25.398144
172.743122	6881.199604	25.403162
172.469785	6891.664893	25.408179
172.786262	6901.045522	25.413197
173.267485	6916.889672	25.418215
173.115970	6932.370500	25.423232
173.328878	6939.858813	25.428250
174.009241	6953.147090	25.433267
173.792148	6962.109263	25.438285
174.044674	6973.592327	25.443303
174.369329	6990.285337	25.448320
174.754082	6984.868930	25.453338
174.865048	7006.467328	25.458355
174.859590	7021.023244	25.463373
175.288383	7026.443204	25.468391
175.096306	7029.508806	25.473408
175.556083	7044.617673	25.478426
175.342168	7063.533694	25.483443
175.427142	7061.726294	25.488461
175.743493	7081.158144	25.493479
175.632792	7095.122687	25.498496
176.024809	7109.483909	25.503514
176.327896	7129.316472	25.508531
176.142513	7149.321763	25.513549
176.932943	7150.993809	25.518567
176.655288	7169.219049	25.523584
177.056516	7183.172075	25.528602
177.292352	7203.947479	25.533619
177.556549	7205.143993	25.538637
177.384573	7223.302877	25.543655
177.953481	7230.666903	25.548672
178.127744	7227.773560	25.553690
178.219935	7256.892861	25.558707
178.152662	7269.077083	25.563725
178.548806	7263.653252	25.568743
178.691462	7291.414340	25.573760
178.748778	7289.654600	25.578778
179.002391	7303.199296	25.583795
179.256208	7326.285348	25.588813
179.781306	7332.324269	25.593831
179.960845	7336.215889	25.598848
179.894081	7340.238058	25.603866
180.044236	7354.177773	25.608883
180.101183	7359.133889	25.613901
180.287806	7355.985970	25.618919
180.344643	7375.884486	25.623936
180.580208	7394.617523	25.628954
180.987003	7396.460930	25.633971
180.739292	7402.546780	25.638989
181.235300	7413.271386	25.644007
181.254410	7415.228545	25.649024
181.518051	7423.435283	25.654042
181.565780	7444.823292	25.659059
181.469476	7456.666078	25.664077
182.189193	7467.028507	25.669095
182.404179	7484.935587	25.674112
182.305838	7491.244730	25.679130
182.656712	7500.257511	25.684148
182.556293	7515.870858	25.689165
182.930871	7520.981753	25.694183
183.058572	7530.779231	25.699200
183.060597	7540.154537	25.704218
183.667316	7551.829435	25.709236
183.586864	7574.126438	25.714253
184.393841	7572.956887	25.719271
184.479830	7575.776037	25.724288
184.613536	7581.402201	25.729306
184.568377	7597.012329	25.734324
184.736583	7600.847598	25.739341
184.711030	7603.988270	25.744359
185.079550	7623.211859	25.749376
185.420662	7626.095781	25.754394
185.549282	7644.354391	25.759412
185.469708	7654.239294	25.764429
186.083100	7660.744264	25.769447
186.067413	7672.330436	25.774464
186.161383	7674.139564	25.779482
186.310772	7690.482822	25.784500
187.113803	7683.003965	25.789517
188.189634	7663.597500	25.794535
188.228292	7670.413651	25.799552
188.093513	7662.974173	25.804570
188.374744	7659.327181	25.809588
188.140581	7673.185263	25.814605
188.405028	7662.954834	25.819623
188.753697	7670.407707	25.824640
188.627795	7666.755597	25.829658
188.831562	7656.119380	25.834676
188.793585	7667.002494	25.839693
188.933431	7652.250120	25.844711
189.036011	7670.568783	25.849728
189.037958	7664.054897	25.854746
189.198465	7688.183256	25.859764
189.199539	7696.537453	25.864781
189.432075	7700.183870	25.869799
189.790559	7730.939251	25.874816
189.395251	7729.150122	25.879834
190.582202	7715.019965	25.884852
190.627239	7734.335408	25.889869
191.184462	7736.095860	25.894887
191.278534	7730.369868	25.899904
191.408277	7728.467121	25.904922
191.378866	7726.369426	25.909940
191.503036	7731.680058	25.914957
191.695910	7727.703273	25.919975
192.027914	7727.174421	25.924992
191.813069	7732.686253	25.930010
192.075022	7745.945175	25.935028
191.915625	7761.025238	25.940045
192.118481	7757.932876	25.945063
191.872365	7783.735386	25.950080
192.176391	7803.434537	25.955098
192.523710	7815.410675	25.960116
192.554216	7837.041991	25.965133
192.685137	7848.132010	25.970151
192.769656	7863.037940	25.975168
192.775162	7884.377444	25.980186
193.203124	7907.152567	25.985204
193.141805	7937.393802	25.990221
193.676601	7960.837350	25.995239
193.791215	7984.323537	26.000256
193.881379	7995.601935	26.005274
194.415078	8015.788421	26.010292
194.616884	8037.688584	26.015309
195.197818	8046.647313	26.020327
195.804008	8062.901620	26.025344
195.042005	8073.658895	26.030362
195.601039	8078.860969	26.035380
195.695771	8104.153679	26.040397
196.226199	8113.299913	26.045415
196.500163	8129.308245	26.050432
196.546240	8145.820738	26.055450
196.733240	8140.905621	26.060468
196.896661	8165.559541	26.065485
197.135135	8173.775429	26.070503
197.308003	8185.346886	26.075520
197.200940	8196.235891	26.080538
197.542482	8209.599390	26.085556
197.617848	8232.220733	26.090573
197.742613	8226.786714	26.095591
198.112057	8253.287441	26.100608
198.504108	8268.932825	26.105626
198.927286	8279.284091	26.110644
199.253794	8298.193014	26.115661
199.322604	8298.733413	26.120679
199.781585	8295.478922	26.125696
199.842146	8313.444277	26.130714
199.577540	8329.067337	26.135732
200.180494	8339.175550	26.140749
200.480581	8336.549548	26.145767
200.870905	8362.211052	26.150784
200.771451	8368.956294	26.155802
201.160873	8362.737974	26.160820
200.715621	8382.386991	26.165837
200.790029	8378.140128	26.170855
200.982753	8390.421518	26.175872
201.254154	8395.551530	26.180890
201.914958	8411.607080	26.185908
201.861911	8434.235039	26.190925
201.902099	8432.582163	26.195943
202.454010	8438.771108	26.200960
202.477739	8453.435508	26.205978
203.000448	8453.384180	26.210996
202.724980	8458.365727	26.216013
203.149719	8481.149717	26.221031
203.379608	8486.381990	26.226048
203.222430	8493.154590	26.231066
203.421898	8505.072625	26.236084
203.592019	8519.589023	26.241101
203.760581	8542.626026	26.246119
203.953866	8554.063099	26.251136
204.255305	8574.031232	26.256154
204.547989	8577.711557	26.261172
204.729351	8591.207566	26.266189
205.193448	8606.089129	26.271207
205.471071	8609.194264	26.276224
205.853478	8625.939709	26.281242
206.188633	8629.312278	26.286260
206.262838	8645.080738	26.291277
206.454394	8650.524174	26.296295
206.720338	8644.236504	26.301312
206.455853	8670.739500	26.306330
206.669000	8673.023543	26.311348
206.953114	8683.540485	26.316365
206.997281	8700.490244	26.321383
207.356972	8718.410753	26.326400
207.141361	8722.582539	26.331418
207.368045	8741.301372	26.336436
207.871237	8753.610678	26.341453
208.404694	8766.863419	26.346471
208.540678	8777.695995	26.351488
208.228807	8794.713645	26.356506
208.538951	8803.971367	26.361524
208.783499	8820.256621	26.366541
208.913600	8842.467250	26.371559
209.642516	8846.512084	26.376576
209.479878	8871.396213	26.381594
209.753447	8883.122134	26.386612
209.974202	8897.284180	26.391629
209.955925	8905.404088	26.396647
210.289385	8916.284759	26.401664
210.102068	8945.311052	26.406682
210.543258	8957.985322	26.411700
210.840260	8976.080999	26.416717
210.709686	8993.020783	26.421735
211.124082	9014.276636	26.426752
211.431761	9024.816029	26.431770
211.631319	9048.934062	26.436788
211.690427	9064.184020	26.441805
211.933111	9079.609329	26.446823
212.568296	9082.840521	26.451840
212.535740	9100.279460	26.456858
213.101904	9100.951100	26.461876
213.158291	9110.472177	26.466893
213.326785	9125.011062	26.471911
213.739691	9151.000444	26.476928
213.700373	9144.200930	26.481946
214.020280	9158.391091	26.486964
214.172473	9174.231877	26.491981
214.344697	9183.121103	26.496999
214.734443	9190.018900	26.502016
214.870243	9217.151555	26.507034
215.062496	9215.398407	26.512052
215.419740	9233.367534	26.517069
215.323967	9245.603550	26.522087
215.702196	9255.176890	26.527104
215.521055	9278.528900	26.532122
215.930996	9279.464298	26.537140
216.166296	9301.164232	26.542157
216.355258	9319.179573	26.547175
216.996112	9331.097146	26.552192
216.817448	9348.230325	26.557210
217.151133	9348.945340	26.562228
217.342653	9365.550491	26.567245
217.528591	9379.530461	26.572263
217.997101	9397.648882	26.577280
217.820243	9409.580813	26.582298
218.471538	9418.004252	26.587316
218.669279	9431.346129	26.592333
218.519852	9444.819311	26.597351
218.730396	9456.003281	26.602368
218.897487	9471.447735	26.607386
219.254932	9481.739493	26.612404
219.497923	9499.184935	26.617421
219.579203	9526.415768	26.622439
219.937908	9532.338504	26.627456
219.935217	9552.556322	26.632474
220.522774	9560.272681	26.637492
220.605658	9586.307172	26.642509
220.790003	9601.475930	26.647527
221.366822	9600.836377	26.652544
222.033276	9602.328606	26.657562
222.271876	9607.960454	26.662580
222.885126	9607.555513	26.667597
222.643845	9607.475685	26.672615
222.792986	9616.871331	26.677632
222.842344	9622.270900	26.682650
223.396563	9628.792476	26.687668
223.521543	9637.848867	26.692685
223.271855	9645.578742	26.697703
224.075078	9640.612505	26.702720
224.144491	9645.186496	26.707738
223.928087	9657.906394	26.712756
224.387211	9668.113603	26.717773
224.405172	9679.210003	26.722791
224.708661	9683.830894	26.727808
224.478751	9694.844056	26.732826
224.787830	9708.238077	26.737844
224.869276	9713.054921	26.742861
224.748011	9740.502980	26.747879
225.104117	9733.141998	26.752896
225.193345	9781.590186	26.757914
225.517012	9787.663809	26.762932
226.182251	9802.113530	26.767949
225.882938	9822.212948	26.772967
226.184869	9836.588018	26.777984
226.593431	9863.065685	26.783002
226.854079	9882.106339	26.788020
227.096919	9899.802927	26.793037
227.009084	9925.864043	26.798055
227.494882	9932.621347	26.803072
227.668114	9947.399912	26.808090
227.910289	9958.715757	26.813108
227.972477	9979.166197	26.818125
228.339619	9998.204580	26.823143
228.424140	10010.683197	26.828160
228.895687	10040.272353	26.833178
229.414361	10052.653456	26.838196
229.474240	10067.981041	26.843213
229.655451	10086.687554	26.848231
229.905414	10109.610100	26.853248
230.282801	10119.293129	26.858266
230.595162	10143.748299	26.863284
230.917952	10145.012845	26.868301
230.915354	10158.932308	26.873319
231.227068	10180.674846	26.878336
231.616925	10185.017297	26.883354
231.590162	10194.905287	26.888372
232.438642	10206.434343	26.893389
232.291157	10221.870303	26.898407
232.712887	10237.047897	26.903424
232.972038	10249.754648	26.908442
232.807140	10253.389899	26.913460
233.091497	10264.857438	26.918477
233.370642	10279.296378	26.923495
233.484812	10292.428834	26.928512
233.806327	10307.953415	26.933530
234.162024	10322.187374	26.938548
234.508504	10334.375407	26.943565
234.465774	10358.601459	26.948583
234.843779	10355.050940	26.953600
234.855197	10384.687766	26.958618
234.830472	10389.022787	26.963636
235.509048	10407.972884	26.968653
235.483796	10422.960639	26.973671
235.831017	10438.958975	26.978688
235.918255	10454.717811	26.983706
236.070488	10459.452777	26.988724
236.254809	10474.693646	26.993741
236.630215	10497.259547	26.998759
236.664700	10512.885977	27.003776
236.892003	10529.517797	27.008794
237.044034	10546.877432	27.013812
237.485170	10561.005127	27.018829
237.364205	10583.058056	27.023847
237.600062	10597.816258	27.028864
238.078378	10618.433789	27.033882
238.183150	10639.653949	27.038900
238.794517	10656.995572	27.043917
238.654287	10683.599558	27.048935
238.982321	10686.803344	27.053952
239.101031	10711.542158	27.058970
239.427840	10727.687688	27.063988
239.932529	10744.078764	27.069005
239.978609	10766.773126	27.074023
240.772390	10786.124628	27.079040
241.725062	10766.751952	27.084058
242.266668	10759.246782	27.089076
242.766762	10750.588542	27.094093
242.764105	10746.122700	27.099111
243.286601	10739.245884	27.104128
243.474624	10740.271068	27.109146
243.272498	10749.788747	27.114164
243.639102	10738.915049	27.119181
243.755976	10739.342020	27.124199
244.012920	10736.949549	27.129216
244.279054	10741.575938	27.134234
244.274930	10744.257763	27.139252
244.235863	10734.600170	27.144269
244.111087	10748.867847	27.149287
244.233081	10763.710475	27.154304
244.699141	10774.602842	27.159322
244.500643	10798.329874	27.164340
245.034984	10816.632341	27.169357
244.905355	10827.165592	27.174375
245.222716	10841.635971	27.179392
245.437523	10868.600419	27.184410
245.772122	10886.518076	27.189428
245.975515	10898.751417	27.194445
246.080091	10916.584971	27.199463
246.319543	10943.166269	27.204480
246.622563	10959.660566	27.209498
246.496165	10975.150993	27.214516
246.725414	10993.789191	27.219533
247.106736	11022.220391	27.224551
247.504626	11030.478941	27.229568
247.582341	11055.752570	27.234586
248.023803	11084.223096	27.239604
248.206094	11096.406836	27.244621
248.627613	11119.374797	27.249639
248.368729	11145.893046	27.254656
248.922480	11166.839311	27.259674
249.114313	11190.435468	27.264692
249.462813	11203.321216	27.269709
249.627582	11233.432284	27.274727
250.019330	11246.081353	27.279744
250.255015	11268.527242	27.284762
250.389550	11279.161349	27.289780
250.867163	11299.684888	27.294797
251.092786	11315.205332	27.299815
251.016778	11335.644025	27.304832
251.810474	11345.372454	27.309850
251.773292	11367.345874	27.314868
252.101524	11376.458273	27.319885
252.762592	11404.827494	27.324903
252.693477	11408.661634	27.329920
252.853742	11429.589728	27.334938
253.139015	11443.434179	27.339956
253.436382	11458.663332	27.344973
253.499554	11475.181672	27.349991
253.707658	11502.469049	27.355008
254.215281	11514.498942	27.360026
254.453398	11533.272555	27.365044
254.478269	11542.532390	27.370061
254.919824	11558.579647	27.375079
254.853840	11581.075863	27.380096
255.521673	11595.520018	27.385114
255.552686	11616.417029	27.390132
255.978365	11631.886621	27.395149
256.456424	11651.765755	27.400167
256.539162	11675.598869	27.405184
257.139782	11681.021682	27.410202
257.217574	11695.100735	27.415220
257.484744	11710.517756	27.420237
257.801339	11731.123632	27.425255
257.445011	11742.643667	27.430272
258.115315	11760.756777	27.435290
258.395646	11785.801764	27.440308
258.689024	11799.703887	27.445325
258.914943	11813.564435	27.450343
258.950882	11839.318086	27.455360
259.899944	11829.309236	27.460378
260.157802	11851.450017	27.465396
260.518761	11857.823928	27.470413
260.922691	11850.833485	27.475431
261.069644	11857.452649	27.480448
261.705278	11877.613139	27.485466
261.500917	11890.476630	27.490484
261.739760	11889.690568	27.495501
262.133288	11893.538642	27.500519
261.981908	11903.739625	27.505536
262.508340	11910.727676	27.510554
262.509130	11923.213154	27.515572
262.617109	11943.302791	27.520589
263.023802	11960.471739	27.525607
262.837264	11974.662061	27.530624
263.127111	11986.536769	27.535642
263.357829	12006.690946	27.540660
263.699271	12021.704667	27.545677
264.089998	12037.197367	27.550695
264.208252	12052.809278	27.555712
264.474315	12062.532561	27.560730
264.664155	12080.562475	27.565748
264.776139	12092.125002	27.570765
265.223071	12117.327767	27.575783
265.653841	12109.116657	27.580800
266.379659	12125.727633	27.585818
266.755638	12140.169645	27.590836
267.121832	12141.101590	27.595853
267.117023	12138.662278	27.600871
267.203955	12170.935823	27.605888
267.881185	12163.847163	27.610906
267.719192	12167.943649	27.615924
268.043360	12194.362318	27.620941
268.158949	12211.554345	27.625959
268.398507	12219.560746	27.630976
268.768633	12239.184339	27.635994
268.716531	12255.422410	27.641012
268.993899	12275.135612	27.646029
269.414832	12288.007790	27.651047
269.256825	12319.327163	27.656064
269.582781	12335.650274	27.661082
269.587663	12354.256255	27.666100
270.171920	12380.865987	27.671117
270.079993	12411.858004	27.676135
270.012867	12432.378419	27.681152
270.630987	12455.734835	27.686170
270.911971	12487.225628	27.691188
271.308600	12514.753575	27.696205
271.586889	12530.617337	27.701223
271.903713	12562.019530	27.706240
272.460733	12586.790515	27.711258
272.309503	12601.675941	27.716276
272.678765	12621.393835	27.721293
272.929317	12641.093289	27.726311
273.397086	12668.035766	27.731328
273.925123	12697.303320	27.736346
273.952219	12708.126168	27.741364
274.723876	12726.817782	27.746381
274.842416	12746.941038	27.751399
275.247487	12766.625666	27.756416
275.401772	12785.571621	27.761434
275.965843	12800.914677	27.766452
275.904380	12817.780417	27.771469
276.225907	12829.752868	27.776487
276.488916	12855.230193	27.781504
277.213789	12851.186948	27.786522
277.357070	12859.703163	27.791540
277.583852	12876.003505	27.796557
278.296959	12886.100987	27.801575
278.240110	12904.597441	27.806592
278.643070	12907.783664	27.811610
279.102816	12924.734984	27.816628
279.117310	12930.012299	27.821645
279.586339	12931.668313	27.826663
279.364589	12937.569516	27.831680
279.768810	12954.867209	27.836698
279.680125	12966.154321	27.841716
279.845202	12976.149620	27.846733
280.478378	12984.158127	27.851751
280.424201	13010.927313	27.856768
280.545857	13028.801952	27.861786
281.035823	13038.173539	27.866804
281.204104	13060.567098	27.871821
281.354192	13079.722192	27.876839
281.483796	13105.271875	27.881856
282.209057	13122.861095	27.886874
282.085531	13138.879870	27.891892
282.401986	13172.114799	27.896909
282.817009	13185.382852	27.901927
282.860714	13206.777803	27.906944
283.165132	13228.680072	27.911962
283.615557	13244.993668	27.916980
283.523713	13282.009719	27.921997
283.790503	13296.852826	27.927015
284.077159	13340.742422	27.932032
284.465144	13359.252744	27.937050
285.283657	13380.976264	27.942068
284.986034	13418.032826	27.947085
285.453362	13439.550382	27.952103
285.601707	13472.444563	27.957120
285.833282	13490.131306	27.962138
286.270583	13522.645969	27.967156
286.683555	13542.738887	27.972173
287.134718	13569.042189	27.977191
287.292165	13599.238811	27.982208
287.689869	13614.127851	27.987226
287.929380	13644.439890	27.992244
287.972641	13664.045893	27.997261
288.412805	13683.609906	28.002279
288.972537	13700.686962	28.007296
289.037121	13724.951747	28.012314
289.338523	13751.448188	28.017332
289.834674	13782.305062	28.022349
289.944776	13796.752658	28.027367
290.276305	13823.197385	28.032384
290.489478	13837.974364	28.037402
291.228640	13869.083052	28.042420
290.946609	13897.282360	28.047437
291.517767	13910.617570	28.052455
291.721066	13942.822095	28.057472
291.916075	13964.174307	28.062490
292.119967	13986.853533	28.067508
292.475458	14007.809355	28.072525
292.918043	14026.192326	28.077543
293.207338	14059.956218	28.082560
293.290819	14081.472890	28.087578
293.863595	14100.999278	28.092596
293.554119	14128.875489	28.097613
294.115307	14146.245359	28.102631
294.361588	14167.552092	28.107648
294.705763	14192.106238	28.112666
295.028798	14220.350600	28.117684
295.319498	14240.902307	28.122701
295.896523	14257.701314	28.127719
296.329129	14267.810093	28.132736
296.471791	14288.385954	28.137754
296.998424	14298.979648	28.142772
297.145983	14328.158364	28.147789
297.713281	14337.525908	28.152807
298.337289	14349.700397	28.157824
298.143759	14364.553342	28.162842
298.578321	14377.869900	28.167860
298.318465	14404.488916	28.172877
298.973961	14420.716667	28.177895
299.280351	14444.619813	28.182912
299.837563	14463.122902	28.187930
299.954278	14466.331766	28.192948
299.682938	14488.164268	28.197965
300.126636	14507.364783	28.202983
300.435509	14541.067672	28.208000
300.804335	14571.429916	28.213018
301.397314	14591.204149	28.218036
301.413284	14617.663549	28.223053
301.906091	14647.498121	28.228071
302.279611	14658.431858	28.233088
302.755023	14680.121197	28.238106
303.151890	14691.421138	28.243124
303.286501	14715.582453	28.248141
303.539891	14727.378814	28.253159
304.028718	14746.003459	28.258176
303.826567	14770.207616	28.263194
304.460896	14785.274408	28.268212
304.864150	14805.393172	28.273229
305.320950	14813.395244	28.278247
305.581548	14838.924579	28.283264
305.936743	14850.526005	28.288282
306.705787	14856.214018	28.293300
306.925906	14874.062916	28.298317
307.406703	14864.203524	28.303335
307.842691	14874.175975	28.308352
308.007599	14899.271639	28.313370
307.925596	14899.174442	28.318388
308.358095	14905.808757	28.323405
308.651521	14921.044568	28.328423
308.896968	14927.637069	28.333440
308.911368	14937.990972	28.338458
309.438736	14945.083517	28.343476
309.279496	14974.507997	28.348493
309.654933	14999.823074	28.353511
309.893331	15018.331404	28.358528
309.776591	15049.913018	28.363546
310.501717	15066.717750	28.368564
310.071000	15088.443166	28.373581
310.413980	15101.316869	28.378599
310.746995	15129.290894	28.383616
311.028278	15165.398724	28.388634
311.883414	15187.349459	28.393652
311.916247	15211.680113	28.398669
312.264670	15232.336627	28.403687
312.495451	15257.462330	28.408704
312.880141	15286.027316	28.413722
313.198107	15308.465746	28.418740
313.289069	15338.388645	28.423757
313.930550	15350.084953	28.428775
314.101525	15383.256253	28.433792
314.878373	15398.144466	28.438810
315.119996	15410.550512	28.443828
315.503915	15436.597416	28.448845
315.839499	15457.001203	28.453863
316.219421	15465.691551	28.458880
316.363198	15492.009860	28.463898
316.822440	15514.860749	28.468916
317.058206	15528.750859	28.473933
317.128519	15550.524405	28.478951
317.739287	15581.669053	28.483968
317.527483	15601.983340	28.488986
318.365188	15618.366566	28.494004
318.412704	15650.032758	28.499021
318.560832	15675.925160	28.504039
319.195780	15691.397219	28.509056
319.763111	15719.348551	28.514074
320.346273	15725.782957	28.519092
320.555475	15746.652879	28.524109
320.845717	15755.662959	28.529127
321.669079	15770.391191	28.534144
321.698962	15791.800905	28.539162
322.144072	15799.118054	28.544180
322.130665	15819.561022	28.549197
322.363998	15823.594086	28.554215
322.396572	15845.855691	28.559232
322.621429	15878.754743	28.564250
323.175611	15894.606762	28.569268
323.236018	15919.070832	28.574285
323.702768	15946.607957	28.579303
323.759887	15966.192546	28.584320
323.860454	15995.134212	28.589338
324.550738	16020.477451	28.594356
324.562273	16051.199926	28.599373
325.270345	16068.087309	28.604391
325.775228	16092.090698	28.609408
325.851244	16111.395918	28.614426
326.520230	16129.582950	28.619444
326.944865	16165.481913	28.624461
327.424035	16175.454533	28.629479
327.982409	16188.684243	28.634496
327.602213	16215.128241	28.639514
327.928140	16221.863869	28.644532
328.203182	16237.906191	28.649549
328.464815	16264.404650	28.654567
328.888194	16287.425773	28.659584
328.969923	16317.799437	28.664602
329.358273	16326.103539	28.669620
329.104499	16363.142481	28.674637
329.345657	16396.014252	28.679655
329.877848	16414.415139	28.684672
330.076214	16460.354790	28.689690
330.530113	16487.064695	28.694708
330.649982	16522.515472	28.699725
330.647947	16548.531491	28.704743
331.237275	16588.224135	28.709760
331.322183	16622.413109	28.714778
331.996669	16654.497133	28.719796
332.355021	16705.185631	28.724813
332.679766	16734.686013	28.729831
333.539725	16771.121480	28.734848
333.342936	16795.150012	28.739866
333.820676	16825.815858	28.744884
334.458802	16864.938681	28.749901
334.705821	16884.632739	28.754919
335.298115	16927.256881	28.759936
335.589536	16948.707214	28.764954
336.037123	16976.381902	28.769972
336.038047	17005.311419	28.774989
336.588611	17032.896965	28.780007
337.489989	17043.596510	28.785024
337.395037	17073.568346	28.790042
337.610016	17101.754714	28.795060
338.094324	17121.261262	28.800077
338.438907	17150.928165	28.805095
339.046152	17169.076271	28.810112
339.502934	17202.560238	28.815130
339.656384	17226.593455	28.820148
339.447413	17253.657568	28.825165
339.850879	17282.868902	28.830183
340.757584	17298.477412	28.835200
340.783395	17340.857562	28.840218
340.868103	17368.582127	28.845236
341.274162	17385.241743	28.850253
341.300683	17421.616706	28.855271
341.778727	17442.622245	28.860288
342.407100	17487.338568	28.865306
342.641388	17514.635628	28.870324
343.003900	17547.359009	28.875341
343.090617	17569.574306	28.880359
343.802575	17601.069693	28.885376
343.741479	17637.061889	28.890394
344.029924	17653.190944	28.895412
344.838000	17693.156081	28.900429
344.812786	17719.159448	28.905447
345.326800	17749.789455	28.910464
345.522563	17775.060856	28.915482
345.821166	17807.855601	28.920500
346.257680	17836.953264	28.925517
346.167909	17868.930516	28.930535
346.840032	17897.319091	28.935552
346.958657	17929.753016	28.940570
347.284227	17962.992216	28.945588
347.917920	17986.745736	28.950605
348.282047	18023.825781	28.955623
348.795895	18044.866589	28.960640
349.324649	18081.543366	28.965658
349.898895	18111.551884	28.970676
349.875319	18135.074557	28.975693
350.022747	18170.717818	28.980711
350.865977	18203.709673	28.985728
351.017526	18226.329754	28.990746
351.065982	18252.899447	28.995764
351.441565	18268.938874	29.000781
351.637284	18304.770420	29.005799
352.172082	18340.319653	29.010816
352.423099	18372.503079	29.015834
352.746759	18395.097944	29.020852
353.122190	18424.936779	29.025869
353.110697	18468.368101	29.030887
353.932568	18490.604164	29.035904
354.760913	18527.694893	29.040922
354.871853	18553.290536	29.045940
355.611046	18575.060351	29.050957
355.640196	18608.692674	29.055975
356.139008	18639.615848	29.060992
356.510009	18669.400738	29.066010
356.832467	18680.887824	29.071028
356.934571	18716.793507	29.076045
357.252631	18750.357648	29.081063
357.951798	18774.847649	29.086080
358.116795	18802.380465	29.091098
358.308680	18828.011298	29.096116
358.809349	18853.053560	29.101133
358.791764	18891.539892	29.106151
358.983761	18920.083634	29.111168
359.581597	18947.090606	29.116186
360.256542	18974.394018	29.121204
360.897572	19011.787820	29.126221
361.298343	19048.271117	29.131239
361.645972	19066.023424	29.136256
361.942526	19093.354277	29.141274
361.714198	19119.490781	29.146292
362.447460	19154.621632	29.151309
362.817369	19189.171444	29.156327
363.312814	19212.294885	29.161344
363.503865	19248.448264	29.166362
363.755049	19279.798033	29.171380
364.139494	19306.508113	29.176397
364.190394	19344.180636	29.181415
364.866996	19370.244997	29.186432
365.359088	19402.157853	29.191450
365.534684	19433.992068	29.196468
366.085182	19455.708932	29.201485
366.129530	19498.995226	29.206503
366.528093	19512.340275	29.211520
368.829952	19491.327024	29.216538
369.124162	19500.656406	29.221556
369.449119	19502.856954	29.226573
369.294244	19512.005920	29.231591
369.733139	19522.209197	29.236608
369.918759	19526.533741	29.241626
370.416772	19526.078887	29.246644
371.082294	19534.456504	29.251661
371.075492	19549.205694	29.256679
371.491097	19558.331887	29.261696
372.008178	19573.382689	29.266714
372.039266	19588.675542	29.271732
372.387379	19594.025107	29.276749
372.517363	19626.551309	29.281767
372.503480	19643.399580	29.286784
372.899057	19659.449463	29.291802
372.857062	19699.163066	29.296820
373.186306	19717.693542	29.301837
373.290603	19758.931008	29.306855
373.790684	19789.886186	29.311872
373.926482	19833.950265	29.316890
374.379964	19863.381335	29.321908
375.072317	19905.737035	29.326925
374.776167	19949.520626	29.331943
375.393521	19984.057961	29.336960
375.558730	20010.074562	29.341978
375.893517	20060.291451	29.346996
376.493265	20107.949786	29.352013
376.843579	20146.358913	29.357031
377.035354	20190.081165	29.362048
377.309335	20235.020932	29.367066
377.936748	20283.315248	29.372084
378.836430	20315.519790	29.377101
379.117709	20354.342457	29.382119
379.420911	20387.693155	29.387136
380.261342	20422.755443	29.392154
380.190293	20455.932034	29.397172
380.996041	20487.445094	29.402189
381.134501	20514.542558	29.407207
382.042824	20557.735824	29.412224
382.111501	20577.120396	29.417242
382.467171	20616.072036	29.422260
383.008204	20638.059815	29.427277
383.336392	20668.712177	29.432295
383.313893	20706.629630	29.437312
383.942736	20730.604685	29.442330
384.242059	20769.235704	29.447348
384.740757	20794.954744	29.452365
385.126035	20829.134398	29.457383
385.988049	20841.416781	29.462400
386.586650	20862.525462	29.467418
386.937070	20893.418073	29.472436
387.506052	20900.835255	29.477453
387.463240	20922.051746	29.482471
387.659302	20955.606587	29.487488
388.453480	20965.260002	29.492506
388.116936	20991.899238	29.497524
388.284612	21013.587919	29.502541
388.749527	21050.440141	29.507559
389.179616	21091.966651	29.512576
389.776072	21112.646792	29.517594
389.601082	21152.855431	29.522612
390.302577	21174.704195	29.527629
390.529425	21212.798134	29.532647
390.771943	21230.233358	29.537664
391.808156	21270.906110	29.542682
391.675398	21304.466052	29.547700
391.846949	21341.872903	29.552717
392.248681	21381.368822	29.557735
392.508281	21426.571427	29.562752
393.171909	21457.723174	29.567770
393.483707	21510.167357	29.572788
394.033593	21543.477257	29.577805
394.328377	21589.022832	29.582823
394.496332	21621.401404	29.587840
395.405889	21644.373843	29.592858
395.692516	21693.650245	29.597876
396.170906	21721.227236	29.602893
396.732965	21758.927260	29.607911
396.898248	21792.892034	29.612928
397.442271	21832.026165	29.617946
397.774656	21875.493621	29.622964
398.260153	21898.480452	29.627981
398.677356	21936.149639	29.632999
398.826115	21966.174685	29.638016
399.286020	22003.893935	29.643034
399.924546	22044.768318	29.648052
400.099713	22072.398183	29.653069
400.592017	22116.533912	29.658087
401.003041	22155.560872	29.663104
401.450038	22178.935452	29.668122
401.282591	22226.810676	29.673140
401.909695	22260.957260	29.678157
402.565454	22302.258028	29.683175
402.850762	22347.393010	29.688192
403.577875	22372.471760	29.693210
403.973493	22408.956989	29.698228
404.858877	22430.423766	29.703245
405.316727	22466.974037	29.708263
405.595303	22498.887041	29.713280
405.975065	22522.405954	29.718298
406.148655	22560.454918	29.723316
406.495240	22578.743808	29.728333
406.752203	22608.874125	29.733351
407.177194	22650.204700	29.738368
407.809569	22681.343368	29.743386
408.250463	22710.300129	29.748404
408.771548	22741.095122	29.753421
408.738069	22770.982179	29.758439
409.281387	22797.696111	29.763456
409.858413	22812.192273	29.768474
409.755485	22864.050923	29.773492
410.244858	22889.869388	29.778509
410.851122	22922.357996	29.783527
410.794924	22958.914914	29.788544
410.838173	22988.486119	29.793562
411.470756	23036.604918	29.798580
411.886684	23070.107154	29.803597
412.207348	23112.894611	29.808615
412.431363	23162.745587	29.813632
412.999928	23193.166842	29.818650
413.094019	23248.695008	29.823668
413.971682	23292.440211	29.828685
414.729058	23338.984394	29.833703
414.765178	23383.060079	29.838720
415.607505	23415.606601	29.843738
415.736519	23458.929641	29.848756
416.122829	23492.309097	29.853773
416.733491	23539.763387	29.858791
417.142852	23577.076178	29.863808
417.665452	23600.083203	29.868826
417.952336	23653.370241	29.873844
418.015385	23661.580639	29.878861
418.507192	23691.160440	29.883879
418.899244	23743.607887	29.888896
419.216887	23782.366223	29.893914
419.680803	23820.908359	29.898932
420.403585	23864.413578	29.903949
420.814531	23907.978060	29.908967
421.131729	23954.819471	29.913984
421.667534	23980.663821	29.919002
421.894893	24037.193573	29.924020
422.502257	24079.819788	29.929037
423.020286	24125.204735	29.934055
423.359919	24165.201141	29.939072
424.178290	24186.640813	29.944090
424.527411	24225.833968	29.949108
425.410583	24260.121292	29.954125
425.763590	24296.515244	29.959143
426.129895	24335.583046	29.964160
426.873689	24353.475119	29.969178
427.325677	24391.632191	29.974196
427.425456	24426.845033	29.979213
428.116104	24450.026593	29.984231
428.277075	24486.893494	29.989248
428.592998	24514.727314	29.994266
428.944831	24554.763714	29.999284
429.131299	24585.691226	30.004301
429.894645	24628.262545	30.009319
429.910428	24671.706962	30.014336
430.407565	24708.701987	30.019354
430.897450	24740.035187	30.024372
430.969089	24783.967284	30.029389
431.592725	24808.174657	30.034407
431.577712	24852.637510	30.039424
431.773068	24895.393001	30.044442
432.396503	24930.395894	30.049460
433.826242	24952.665578	30.054477
434.879236	24967.215490	30.059495
435.489931	24998.721372	30.064512
435.770276	25008.938907	30.069530
436.145088	25037.629996	30.074548
436.366977	25070.418993	30.079565
436.817231	25091.515215	30.084583
437.288074	25116.578488	30.089600
437.354363	25151.970780	30.094618
437.758579	25170.659956	30.099636
438.142327	25207.408728	30.104653
438.370891	25235.640577	30.109671
438.527923	25280.965016	30.114688
439.197908	25310.255530	30.119706
439.729726	25340.405513	30.124724
439.570877	25389.996737	30.129741
440.273945	25420.984559	30.134759
440.311258	25467.588251	30.139776
440.841389	25513.873280	30.144794
441.307257	25571.170042	30.149812
441.786983	25619.811785	30.154829
442.149782	25655.012200	30.159847
442.363602	25711.146676	30.164864
443.019383	25760.755769	30.169882
443.365393	25811.530676	30.174900
443.102170	25864.428241	30.179917
443.764331	25914.247133	30.184935
444.357466	25968.725989	30.189952
445.160735	26013.870745	30.194970
445.579973	26065.354050	30.199988
445.988916	26118.251700	30.205005
446.558688	26159.412311	30.210023
446.768389	26216.866425	30.215040
448.307065	26238.412316	30.220058
449.781491	26261.716637	30.225076
450.539216	26288.937189	30.230093
451.404172	26307.299816	30.235111
451.224993	26330.921288	30.240128
451.286649	26345.587095	30.245146
451.949387	26371.772761	30.250164
452.264017	26395.487392	30.255181
452.927501	26415.614664	30.260199
452.801372	26444.603165	30.265216
453.252349	26467.779365	30.270234
453.569174	26494.958648	30.275252
453.524181	26532.413755	30.280269
454.029379	26573.378518	30.285287
453.999931	26608.871205	30.290304
454.467295	26644.238328	30.295322
455.356688	26692.240560	30.300340
455.336486	26733.465131	30.305357
455.776129	26768.892094	30.310375
455.783344	26812.376749	30.315392
456.273658	26853.082243	30.320410
456.507489	26906.699748	30.325428
456.564370	26963.768831	30.330445
457.382564	27014.795316	30.335463
458.018281	27061.612384	30.340480
458.244143	27123.607557	30.345498
458.975896	27163.730168	30.350516
459.255807	27222.187499	30.355533
459.844526	27265.579145	30.360551
460.417214	27326.478279	30.365568
460.784295	27370.082002	30.370586
461.770921	27404.090134	30.375604
462.082009	27467.757514	30.380621
462.579451	27505.104023	30.385639
463.397067	27546.580083	30.390656
463.452747	27596.221902	30.395674
463.854852	27639.830227	30.400692
464.253339	27687.687517	30.405709
465.277900	27727.805849	30.410727
465.517326	27776.059051	30.415744
465.816986	27823.125690	30.420762
466.650281	27870.491934	30.425780
466.789902	27918.813464	30.430797
467.573365	27956.550362	30.435815
468.121821	27986.354405	30.440832
468.621945	28038.183307	30.445850
469.249579	28083.761316	30.450868
469.566414	28120.244538	30.455885
470.228754	28170.623486	30.460903
470.584084	28203.695425	30.465920
470.791507	28251.714041	30.470938
471.741860	28287.737416	30.475956
472.128057	28331.428928	30.480973
472.802249	28347.830073	30.485991
473.597972	28373.833921	30.491008
473.753482	28420.307533	30.496026
474.328074	28451.890544	30.501044
476.074873	28458.460993	30.506061
476.859643	28454.815669	30.511079
477.449687	28477.815805	30.516096
477.393349	28483.092977	30.521114
478.368645	28499.908028	30.526132
478.568044	28520.616149	30.531149
478.716003	28527.327902	30.536167
479.140675	28544.840582	30.541184
479.390914	28561.946137	30.546202
479.413713	28596.636682	30.551220
479.695068	28629.532175	30.556237
480.111391	28661.552112	30.561255
480.050271	28690.115088	30.566272
480.226329	28741.873379	30.571290
480.899949	28769.076070	30.576308
481.258008	28817.187398	30.581325
481.433855	28856.310697	30.586343
481.778238	28896.146329	30.591360
481.994036	28948.783018	30.596378
482.596804	28988.944894	30.601396
482.889007	29040.587924	30.606413
483.580973	29084.443917	30.611431
483.814187	29136.613546	30.616448
484.528983	29194.632055	30.621466
485.205276	29230.778414	30.626484
485.507353	29281.046432	30.631501
486.102058	29326.664698	30.636519
486.467611	29377.020606	30.641536
487.343769	29423.823531	30.646554
488.049425	29472.273822	30.651572
488.228387	29521.501587	30.656589
488.615289	29569.757105	30.661607
489.013929	29611.336723	30.666624
489.579205	29674.419092	30.671642
490.431866	29708.724483	30.676660
490.822712	29758.418786	30.681677
491.106438	29803.808985	30.686695
491.915487	29854.224939	30.691712
492.148333	29905.126844	30.696730
492.630564	29944.722439	30.701748
492.979296	30010.105298	30.706765
493.485887	30059.695397	30.711783
494.263911	30104.689329	30.716800
494.304027	30169.305622	30.721818
495.073638	30200.520544	30.726836
495.665169	30254.102347	30.731853
495.930133	30303.252570	30.736871
496.943551	30350.151337	30.741888
497.364164	30402.911379	30.746906
498.173347	30448.867404	30.751924
498.218207	30493.339342	30.756941
498.831001	30543.733529	30.761959
499.237871	30589.557038	30.766976
499.753895	30644.641516	30.771994
500.296618	30697.537506	30.777012
500.765351	30739.119858	30.782029
501.192701	30796.504266	30.787047
501.573875	30850.416258	30.792064
502.156762	30890.608047	30.797082
503.393370	30924.028963	30.802100
503.832863	30969.816816	30.807117
504.463878	31011.159657	30.812135
504.983082	31049.117630	30.817152
505.195166	31100.660145	30.822170
505.387030	31138.407265	30.827188
505.777314	31185.942001	30.832205
506.131602	31245.435840	30.837223
506.836749	31287.413773	30.842240
507.260336	31346.829165	30.847258
507.654457	31389.794702	30.852276
507.948655	31445.916473	30.857293
508.415747	31485.092648	30.862311
509.348450	31526.686615	30.867328
509.366945	31585.193349	30.872346
510.247095	31620.637931	30.877364
511.040015	31670.994277	30.882381
511.379620	31725.602965	30.887399
511.985000	31758.322308	30.892416
512.336777	31802.515619	30.897434
512.819831	31846.539974	30.902452
513.160896	31901.412232	30.907469
513.871061	31942.637630	30.912487
514.476928	31988.214249	30.917504
514.737690	32054.907003	30.922522
515.328785	32097.567175	30.927540
515.814387	32145.154121	30.932557
516.001779	32190.320377	30.937575
516.588870	32235.353729	30.942592
517.157639	32299.512726	30.947610
518.041202	32347.766644	30.952628
518.357026	32405.726106	30.957645
518.967243	32459.559593	30.962663
519.579630	32505.789163	30.967680
519.910896	32557.022489	30.972698
520.118881	32609.881804	30.977716
520.870801	32668.757867	30.982733
521.430563	32727.458262	30.987751
521.808452	32775.336875	30.992768
522.091899	32829.904569	30.997786
523.011384	32876.866505	31.002804
523.521733	32934.532018	31.007821
523.980198	32999.212557	31.012839
524.951078	33041.158935	31.017856
525.427583	33110.611599	31.022874
526.176640	33152.888365	31.027892
527.051106	33197.739847	31.032909
527.695503	33241.824188	31.037927
528.049608	33278.238871	31.042944
528.323702	33329.100652	31.047962
528.591115	33374.036708	31.052980
529.161533	33428.374652	31.057997
529.522539	33479.648655	31.063015
530.030040	33532.411180	31.068032
530.316519	33589.205092	31.073050
530.573047	33648.789363	31.078068
531.338684	33709.200722	31.083085
531.564808	33776.583755	31.088103
532.135594	33825.448266	31.093120
532.776016	33893.497205	31.098138
533.546488	33954.011148	31.103156
534.141324	34016.449670	31.108173
534.617402	34080.433283	31.113191
535.412857	34124.098657	31.118208
535.728793	34175.788695	31.123226
536.125710	34227.622056	31.128244
536.767435	34273.974847	31.133261
537.112859	34330.374104	31.138279
538.017101	34377.760474	31.143296
538.159580	34436.091992	31.148314
538.759267	34485.660074	31.153332
539.397404	34542.409102	31.158349
539.547665	34614.880549	31.163367
540.251034	34657.371787	31.168384
540.603915	34719.156279	31.173402
541.197182	34780.937389	31.178420
541.635570	34840.955700	31.183437
541.959042	34901.006722	31.188455
542.600835	34958.415543	31.193472
543.161944	35022.020331	31.198490
544.650732	35059.175669	31.203508
545.307143	35126.558673	31.208525
546.024282	35172.310770	31.213543
547.173025	35192.581252	31.218560
547.708452	35239.568493	31.223578
548.568990	35284.144063	31.228596
548.956683	35323.471236	31.233613
549.640644	35350.380493	31.238631
550.582426	35372.509754	31.243648
550.863713	35405.760884	31.248666
551.545431	35431.146148	31.253684
551.838830	35466.422861	31.258701
551.935054	35507.201568	31.263719
552.548754	35542.428996	31.268736
553.070905	35583.636646	31.273754
553.326859	35631.203948	31.278772
554.244790	35669.753800	31.283789
554.521710	35714.574834	31.288807
554.957375	35751.628314	31.293824
555.251157	35812.885510	31.298842
555.797080	35853.899277	31.303860
556.157040	35905.029555	31.308877
556.543743	35973.676036	31.313895
557.277533	36020.227120	31.318912
558.015887	36080.862680	31.323930
558.333166	36138.634679	31.328948
558.727913	36179.052152	31.333965
558.911356	36255.006499	31.338983
559.217402	36307.574978	31.344000
559.826823	36390.090074	31.349018
560.371058	36451.598222	31.354036
560.965197	36514.675257	31.359053
561.317169	36590.897525	31.364071
561.975557	36659.126716	31.369088
562.683610	36727.434988	31.374106
563.228123	36799.039533	31.379124
563.544768	36862.734394	31.384141
564.547445	36923.031329	31.389159
567.272887	36933.605513	31.394176
567.876002	36970.165169	31.399194
568.646535	37012.396277	31.404212
568.868705	37034.021168	31.409229
569.476234	37062.671800	31.414247
570.110796	37091.117938	31.419264
570.670606	37126.010414	31.424282
570.734757	37153.664582	31.429300
570.834673	37181.467613	31.434317
571.327183	37228.185038	31.439335
571.728380	37279.886839	31.444352
572.107094	37316.875587	31.449370
572.438833	37366.999420	31.454388
573.026239	37411.345085	31.459405
572.908988	37476.746412	31.464423
573.597338	37532.397032	31.469440
573.959247	37595.475690	31.474458
574.520179	37661.420889	31.479476
574.839498	37736.546681	31.484493
574.955784	37811.796596	31.489511
575.741624	37890.180396	31.494528
576.176380	37958.363746	31.499546
576.724802	38037.722633	31.504564
577.471846	38113.155657	31.509581
577.824031	38198.394758	31.514599
578.761948	38278.566263	31.519616
580.343332	38324.253939	31.524634
581.085074	38378.113925	31.529652
582.159515	38437.337364	31.534669
582.580174	38500.980835	31.539687
582.998634	38558.694544	31.544704
583.328958	38611.627419	31.549722
583.573421	38679.793524	31.554740
584.679346	38730.870316	31.559757
584.946904	38798.629554	31.564775
585.536030	38871.337973	31.569792
586.119525	38921.087287	31.574810
586.661942	38989.853681	31.579828
587.545859	39045.110722	31.584845
588.160698	39110.373353	31.589863
589.275199	39161.484769	31.594880
589.744829	39213.957388	31.599898
589.806653	39268.623895	31.604916
590.436641	39316.507835	31.609933
590.954112	39380.489247	31.614951
591.737560	39451.537127	31.619968
592.450924	39505.268023	31.624986
592.854626	39571.810220	31.630004
593.432772	39626.629017	31.635021
593.908598	39696.295090	31.640039
594.555463	39741.490490	31.645056
595.461027	39802.940655	31.650074
595.791082	39874.860436	31.655092
596.472405	39920.356746	31.660109
597.162372	39983.023019	31.665127
597.300076	40048.098737	31.670144
598.291475	40102.425894	31.675162
598.459077	40166.669406	31.680180
599.104491	40215.953751	31.685197
599.254171	40288.208352	31.690215
600.211155	40334.797274	31.695232
600.345127	40402.443812	31.700250
600.710990	40480.039112	31.705268
601.415091	40539.237398	31.710285
602.075957	40615.777057	31.715303
602.374119	40682.316733	31.720320
603.144440	40752.985758	31.725338
603.160502	40839.945882	31.730356
603.775757	40913.964610	31.735373
604.427796	41006.369084	31.740391
605.012072	41089.041923	31.745408
605.868175	41166.259456	31.750426
606.362224	41251.625266	31.755444
606.994150	41327.586050	31.760461
607.416067	41407.986934	31.765479
608.697941	41477.527146	31.770496
610.243259	41534.576241	31.775514
611.577377	41580.591213	31.780532
612.142197	41647.089005	31.785549
612.908698	41699.550358	31.790567
613.424143	41755.013643	31.795584
614.094191	41804.768612	31.800602
613.957494	41868.713688	31.805620
614.892672	41923.189636	31.810637
615.146428	41990.971599	31.815655
615.398816	42056.505069	31.820672
616.001766	42119.614106	31.825690
616.354310	42198.316969	31.830708
616.886311	42270.102647	31.835725
617.396423	42346.027397	31.840743
617.986108	42420.602379	31.845760
618.560741	42506.251773	31.850778
618.932695	42587.678660	31.855796
619.639547	42668.812862	31.860813
620.685696	42749.174210	31.865831
621.042231	42816.911502	31.870848
621.924483	42892.978114	31.875866
622.475747	42972.678035	31.880884
623.300048	43046.997546	31.885901
623.765286	43126.711877	31.890919
624.177467	43208.986981	31.895936
625.316685	43284.292019	31.900954
624.982314	43351.841763	31.905972
625.965854	43433.241469	31.910989
626.684628	43513.052842	31.916007
627.479746	43597.656769	31.921024
628.504495	43677.186733	31.926042
628.924150	43751.251947	31.931060
630.004931	43812.619149	31.936077
631.149871	43885.512648	31.941095
631.778019	43941.450806	31.946112
632.604880	43987.893699	31.951130
633.149210	44042.962246	31.956148
634.269526	44079.696087	31.961165
634.945823	44118.302008	31.966183
635.392478	44173.733534	31.971200
635.943576	44221.656329	31.976218
636.510451	44256.797262	31.981236
637.313980	44301.572749	31.986253
637.589786	44370.619218	31.991271
637.807722	44412.443996	31.996288
638.796078	44457.663652	32.001306
639.153767	44526.827042	32.006324
639.409044	44591.155075	32.011341
639.776811	44647.521848	32.016359
640.200235	44721.499106	32.021376
640.841355	44789.359662	32.026394
641.184884	44870.719760	32.031412
641.821166	44953.333380	32.036429
642.243892	45025.908166	32.041447
642.771722	45112.221446	32.046464
643.494066	45196.043417	32.051482
643.556161	45294.224476	32.056500
644.247463	45370.102043	32.061517
645.146022	45460.639133	32.066535
645.626920	45551.356781	32.071552
646.888334	45635.195966	32.076570
647.314169	45732.744209	32.081588
648.029127	45817.914330	32.086605
648.604092	45892.781028	32.091623
649.179954	45998.421372	32.096640
650.081981	46091.172798	32.101658
650.856037	46167.763133	32.106676
651.854961	46245.939665	32.111693
652.764024	46323.118096	32.116711
653.298139	46391.333183	32.121728
655.685040	46433.296950	32.126746
658.865620	46429.449406	32.131764
659.590672	46464.206767	32.136781
660.435909	46491.117378	32.141799
660.231961	46523.441966	32.146816
660.947458	46527.584340	32.151834
661.081760	46545.427036	32.156852
661.609907	46586.898415	32.161869
661.965494	46620.427656	32.166887
662.213937	46654.406268	32.171904
662.613169	46686.070342	32.176922
662.599794	46745.388313	32.181940
663.155100	46787.120869	32.186957
663.665690	46853.972187	32.191975
664.153704	46908.689585	32.196992
664.843013	46980.349730	32.202010
665.270975	47040.791057	32.207028
665.318751	47118.062813	32.212045
665.836545	47186.990344	32.217063
665.941217	47271.980737	32.222080
666.696630	47344.218700	32.227098
667.470575	47416.810547	32.232116
668.194705	47497.532186	32.237133
668.852243	47573.490915	32.242151
669.274547	47659.211934	32.247168
669.850739	47730.520820	32.252186
670.245119	47815.300461	32.257204
670.879381	47889.468896	32.262221
672.005916	47965.483992	32.267239
672.671709	48049.360134	32.272256
673.421569	48123.896094	32.277274
674.857045	48193.467100	32.282292
675.589910	48257.931290	32.287309
676.594968	48328.350743	32.292327
677.311944	48392.186877	32.297344
678.332757	48443.081895	32.302362
678.955681	48501.739616	32.307380
679.787867	48564.068670	32.312397
680.263865	48617.316538	32.317415
680.479574	48680.558269	32.322432
681.235061	48749.113252	32.327450
682.092947	48805.898091	32.332468
683.069200	48859.477236	32.337485
683.819004	48924.307189	32.342503
684.242491	48993.487125	32.347520
684.794408	49055.332413	32.352538
685.530114	49122.380500	32.357556
685.861666	49194.901776	32.362573
686.488157	49266.136254	32.367591
686.959722	49343.444890	32.372608
687.690635	49421.482524	32.377626
688.127965	49503.082572	32.382644
688.507923	49585.089734	32.387661
689.336628	49665.769882	32.392679
689.526380	49760.951282	32.397696
690.344962	49850.182484	32.402714
690.779609	49942.662490	32.407732
691.006246	50038.820906	32.412749
692.032493	50130.478718	32.417767
692.505450	50234.144236	32.422784
693.463674	50341.740865	32.427802
694.427775	50435.502390	32.432820
694.817398	50535.654794	32.437837
695.016927	50632.107887	32.442855
695.939984	50744.193751	32.447872
696.557748	50838.003063	32.452890
697.092472	50940.820229	32.457908
697.672770	51052.467130	32.462925
699.106524	51152.885919	32.467943
700.925482	51229.050864	32.472960
701.996324	51310.132231	32.477978
702.858786	51392.345405	32.482996
703.311678	51465.288922	32.488013
704.125387	51547.213910	32.493031
704.646825	51625.711096	32.498048
705.096522	51696.090263	32.503066
706.096299	51774.259455	32.508084
706.470647	51846.932986	32.513101
707.403800	51920.366801	32.518119
707.898966	51992.952252	32.523136
708.440919	52072.533792	32.528154
708.921150	52140.558584	32.533172
709.445377	52230.934183	32.538189
710.394598	52299.219442	32.543207
711.064135	52384.548198	32.548224
711.701341	52473.745581	32.553242
712.663895	52550.289204	32.558260
713.417926	52632.481118	32.563277
714.377728	52702.088639	32.568295
714.829939	52776.751357	32.573312
715.772962	52856.345084	32.578330
716.447146	52929.114101	32.583348
717.005079	53008.653034	32.588365
718.065279	53086.906670	32.593383
718.849921	53171.605352	32.598400
719.281863	53256.603618	32.603418
720.097527	53337.583238	32.608436
720.527783	53414.016427	32.613453
721.480905	53498.156400	32.618471
722.269347	53569.094931	32.623488
722.928111	53657.246821	32.628506
723.375268	53740.234357	32.633524
723.605400	53834.300873	32.638541
724.759301	53926.456388	32.643559
725.434019	54025.077172	32.648576
725.582724	54122.592281	32.653594
726.494445	54213.266426	32.658612
726.945491	54317.583851	32.663629
727.913953	54412.561636	32.668647
728.301599	54509.706187	32.673664
728.863929	54616.052988	32.678682
729.792660	54727.357746	32.683700
730.650088	54842.228776	32.688717
731.666893	54927.681488	32.693735
732.304912	55014.580634	32.698752
733.111348	55118.331532	32.703770
734.536413	55207.811465	32.708788
734.916905	55302.230924	32.713805
736.093453	55387.439392	32.718823
737.291345	55460.728595	32.723840
738.477692	55541.633743	32.728858
739.147088	55614.433198	32.733876
739.772209	55694.348800	32.738893
740.851174	55776.619980	32.743911
741.142721	55846.320678	32.748928
741.711160	55923.102237	32.753946
742.342964	56004.659614	32.758964
742.730740	56100.448883	32.763981
743.420951	56181.934613	32.768999
744.182508	56269.091520	32.774016
744.516713	56366.298619	32.779034
745.235556	56448.317623	32.784052
745.843431	56536.482029	32.789069
746.718391	56628.057901	32.794087
747.107030	56707.721975	32.799104
747.813364	56793.261228	32.804122
749.525799	56863.096283	32.809140
750.401183	56955.305088	32.814157
750.983637	57038.125028	32.819175
751.770876	57106.229953	32.824192
752.109239	57199.027423	32.829210
753.260551	57280.675060	32.834228
753.812227	57365.629145	32.839245
754.625629	57440.496487	32.844263
755.126602	57536.739268	32.849280
755.626299	57620.076951	32.854298
756.238633	57711.460080	32.859316
757.035658	57808.073864	32.864333
757.694424	57905.793028	32.869351
758.366028	57997.670104	32.874368
759.144722	58103.529061	32.879386
760.192274	58189.134105	32.884404
761.544007	58270.848921	32.889421
762.785197	58359.296891	32.894439
763.658960	58441.738922	32.899456
763.895464	58523.196714	32.904474
764.993781	58614.810011	32.909492
765.463694	58706.855308	32.914509
765.885875	58790.832555	32.919527
766.564177	58885.617576	32.924544
767.200503	58988.972162	32.929562
767.983231	59074.582405	32.934580
768.809511	59182.646846	32.939597
769.854561	59259.180099	32.944615
771.863101	59345.262624	32.949632
772.897596	59410.615072	32.954650
774.362870	59468.930989	32.959668
774.821800	59541.804675	32.964685
775.134783	59608.229349	32.969703
775.930406	59679.326068	32.974720
776.106801	59755.421855	32.979738
777.151166	59824.427245	32.984756
777.795301	59901.809991	32.989773
778.454563	59977.924534	32.994791
779.386747	60058.605754	32.999808
779.945417	60137.477590	33.004826
780.837150	60220.710830	33.009844
781.328839	60308.927433	33.014861
781.825674	60394.917619	33.019879
782.405015	60482.069646	33.024896
782.685028	60583.017464	33.029914
783.340019	60678.633083	33.034932
783.991534	60785.705258	33.039949
784.733267	60885.971796	33.044967
785.511089	60983.517619	33.049984
785.990435	61100.982125	33.055002
786.656985	61210.037285	33.060020
787.415169	61306.432225	33.065037
788.322294	61412.816809	33.070055
788.849297	61507.572877	33.075072
789.458050	61605.881413	33.080090
790.524800	61709.798227	33.085108
791.156795	61826.715619	33.090125
791.901330	61930.227073	33.095143
792.784356	62039.157834	33.100160
793.312216	62153.059234	33.105178
794.230495	62256.219566	33.110196
795.122319	62366.691807	33.115213
795.418647	62488.125528	33.120231
796.647171	62605.562230	33.125248
797.402351	62730.729651	33.130266
798.586179	62827.465641	33.135284
799.892679	62930.722583	33.140301
800.788206	63033.173928	33.145319
801.798339	63128.385414	33.150336
802.278730	63249.939971	33.155354
803.067317	63348.052079	33.160372
803.911408	63460.429905	33.165389
804.699515	63561.761169	33.170407
805.203895	63661.833879	33.175424
805.723186	63786.951064	33.180442
806.716155	63902.664786	33.185460
807.324702	64016.892951	33.190477
807.849897	64139.263985	33.195495
809.148217	64262.491748	33.200512
809.803595	64377.542039	33.205530
810.919467	64487.106656	33.210548
812.373522	64587.844692	33.215565
813.175612	64699.623817	33.220583
813.797339	64806.306549	33.225600
814.452621	64921.543300	33.230618
815.265030	65015.235521	33.235636
816.409578	65125.970937	33.240653
817.327568	65237.880032	33.245671
818.179295	65343.174241	33.250688
818.578120	65454.175535	33.255706
819.577700	65565.602965	33.260724
820.320751	65678.442596	33.265741
820.992027	65785.587156	33.270759
822.035748	65890.174752	33.275776
822.768793	66005.206646	33.280794
823.922844	66111.549743	33.285812
824.593401	66220.433964	33.290829
825.388165	66326.118471	33.295847
826.808654	66414.866186	33.300864
827.635899	66533.227888	33.305882
828.369770	66632.831057	33.310900
829.270611	66726.937617	33.315917
829.992968	66829.152562	33.320935
831.259134	66924.736980	33.325952
831.623836	67029.972631	33.330970
832.465917	67110.439107	33.335988
833.558474	67197.486452	33.341005
833.869769	67293.938524	33.346023
834.899405	67384.149012	33.351040
835.712564	67478.153153	33.356058
836.237001	67580.220363	33.361076
836.825642	67676.585969	33.366093
837.668409	67785.148347	33.371111
838.351325	67882.851887	33.376128
838.809371	67985.910991	33.381146
839.340799	68094.114016	33.386164
840.188323	68221.485191	33.391181
840.682500	68335.400198	33.396199
841.893967	68456.485878	33.401216
842.872066	68587.761885	33.406234
843.680237	68704.257202	33.411252
844.876369	68807.165260	33.416269
845.871342	68924.049124	33.421287
846.863313	69042.399889	33.426304
847.565937	69166.015942	33.431322
848.260483	69276.505558	33.436340
849.229810	69391.450398	33.441357
849.809210	69505.011170	33.446375
851.420078	69608.331278	33.451392
852.326634	69724.362115	33.456410
853.266794	69841.468674	33.461428
854.103272	69941.173516	33.466445
854.990887	70055.610855	33.471463
856.153252	70154.772100	33.476480
858.033170	70242.288988	33.481498
859.455352	70319.757382	33.486516
860.438177	70411.910042	33.491533
860.353013	70498.988973	33.496551
861.295889	70586.700765	33.501568
862.171054	70689.758250	33.506586
862.564489	70779.466478	33.511604
863.478746	70876.528936	33.516621
863.980102	70979.723250	33.521639
865.014370	71060.826199	33.526656
865.981639	71166.095598	33.531674
866.721536	71273.638492	33.536692
867.795548	71365.730549	33.541709
868.198562	71470.042497	33.546727
869.249257	71568.394579	33.551744
870.292000	71673.237639	33.556762
870.633061	71777.358868	33.561780
871.587530	71879.809663	33.566797
871.956622	72001.499880	33.571815
872.989463	72117.670023	33.576832
873.649706	72234.563621	33.581850
874.408307	72352.213149	33.586868
875.504762	72477.866167	33.591885
876.104616	72599.011483	33.596903
877.565095	72696.754193	33.601920
878.434278	72809.055633	33.606938
879.048947	72903.445895	33.611956
880.087584	73011.544641	33.616973
880.807744	73120.655159	33.621991
881.797371	73213.287379	33.627008
882.361813	73328.098374	33.632026
882.997674	73449.830804	33.637044
883.779310	73558.668524	33.642061
884.425184	73688.761140	33.647079
885.359985	73799.515805	33.652096
886.008656	73931.574853	33.657114
886.645406	74052.609357	33.662132
887.328460	74179.628025	33.667149
888.248609	74322.522151	33.672167
889.060384	74451.980323	33.677184
890.004295	74589.222933	33.682202
890.993508	74724.070465	33.687220
892.219975	74849.812482	33.692237
893.066064	74990.460713	33.697255
894.133554	75114.453855	33.702272
894.950456	75247.967260	33.707290
895.951068	75387.892178	33.712308
897.097846	75514.358838	33.717325
897.779769	75639.471979	33.722343
898.789252	75762.896907	33.727360
899.661102	75904.204670	33.732378
900.461433	76038.743445	33.737396
902.121016	76163.969678	33.742413
902.473521	76293.620186	33.747431
903.406875	76430.308174	33.752448
904.575247	76563.167586	33.757466
905.638569	76697.965925	33.762484
906.363257	76810.363244	33.767501
907.328679	76949.274340	33.772519
909.022080	77040.737708	33.777536
909.939439	77170.784259	33.782554
911.034878	77287.328239	33.787572
912.267558	77391.583118	33.792589
912.960754	77518.324059	33.797607
914.085675	77624.291158	33.802624
915.094075	77732.849802	33.807642
915.803383	77846.968142	33.812660
916.999564	77945.302979	33.817677
917.503701	78065.693608	33.822695
918.459717	78176.892324	33.827712
919.634524	78283.505930	33.832730
920.097848	78407.552099	33.837748
921.547531	78500.773720	33.842765
923.195719	78589.830384	33.847783
924.501818	78674.662685	33.852800
925.467448	78777.570230	33.857818
925.699252	78880.323269	33.862836
926.723169	78977.280918	33.867853
927.489813	79077.693269	33.872871
928.306982	79180.816085	33.877888
928.727695	79283.414653	33.882906
929.157837	79391.543131	33.887924
930.313727	79488.583324	33.892941
931.163555	79597.360375	33.897959
931.661063	79706.219349	33.902976
932.107848	79811.439659	33.907994
933.145310	79931.301210	33.913012
933.948582	80046.870679	33.918029
934.787500	80181.506387	33.923047
935.193071	80307.083955	33.928064
936.196665	80436.815067	33.933082
936.826051	80580.576810	33.938100
937.754968	80713.254660	33.943117
938.533688	80852.449412	33.948135
941.890082	80921.021943	33.953152
944.802810	80997.478703	33.958170
946.042049	81076.205972	33.963188
947.102473	81147.831267	33.968205
947.842219	81223.553653	33.973223
948.761625	81299.551164	33.978240
949.561946	81388.786444	33.983258
950.043187	81470.392056	33.988276
950.638449	81550.785046	33.993293
951.224459	81642.723266	33.998311
951.713507	81742.238126	34.003328
952.402448	81838.623982	34.008346
953.702143	81931.145305	34.013364
955.171033	82027.439537	34.018381
955.560460	82129.905424	34.023399
956.352788	82241.227896	34.028416
957.274150	82345.942979	34.033434
957.587344	82462.975707	34.038452
958.763521	82579.846483	34.043469
959.269156	82709.399134	34.048487
959.832251	82829.928162	34.053504
960.945672	82949.636950	34.058522
961.474736	83087.678798	34.063540
962.606528	83216.736646	34.068557
962.974042	83361.115537	34.073575
963.835482	83499.720455	34.078592
964.746969	83644.261298	34.083610
965.412062	83804.768368	34.088628
966.232489	83951.658758	34.093645
967.219911	84103.189567	34.098663
967.857523	84261.384135	34.103680
968.700902	84420.596686	34.108698
969.445605	84580.060070	34.113716
971.075582	84731.733396	34.118733
971.921913	84886.510482	34.123751
973.025796	85054.911147	34.128768
974.337808	85204.052441	34.133786
975.176937	85369.159292	34.138804
976.200953	85514.295651	34.143821
977.565760	85668.976966	34.148839
978.561418	85826.759485	34.153856
980.013335	85960.993240	34.158874
980.845166	86096.338190	34.163892
981.719668	86224.645936	34.168909
982.924283	86357.018281	34.173927
983.850155	86485.566020	34.178944
984.993104	86611.670854	34.183962
986.200747	86736.406643	34.188980
987.455568	86864.012739	34.193997
988.298008	86985.222786	34.199015
989.055074	87120.573456	34.204032
990.506690	87237.489301	34.209050
990.941140	87369.807058	34.214068
992.801337	87492.755064	34.219085
993.878827	87606.039541	34.224103
994.737811	87730.128343	34.229120
995.716365	87844.043195	34.234138
996.631925	87967.922010	34.239156
997.562893	88095.106345	34.244173
998.919805	88211.315330	34.249191
999.533419	88329.325306	34.254208
1000.945439	88455.619469	34.259226
1001.637068	88592.975443	34.264244
1002.571231	88723.432358	34.269261
1003.551890	88854.698438	34.274279
1003.848176	88990.127811	34.279296
1005.319278	89116.195089	34.284314
1006.130380	89264.015058	34.289332
1006.691602	89393.314805	34.294349
1008.119619	89527.093970	34.299367
1008.932429	89676.073766	34.304384
1009.779610	89818.212721	34.309402
1010.708237	89968.308108	34.314420
1012.070738	90109.108460	34.319437
1013.085779	90257.174659	34.324455
1013.868614	90411.350135	34.329472
1015.013267	90547.077930	34.334490
1015.983439	90699.967090	34.339508
1017.215714	90849.811511	34.344525
1018.430110	90980.294265	34.349543
1019.462554	91129.337558	34.354560
1020.415336	91264.638631	34.359578
1021.877962	91403.850241	34.364596
1023.445788	91530.548529	34.369613
1024.471763	91658.478515	34.374631
1024.848999	91800.856881	34.379648
1025.969548	91921.215324	34.384666
1026.599726	92075.692401	34.389684
1027.682468	92221.136278	34.394701
1028.862699	92365.743371	34.399719
1029.479922	92511.990580	34.404736
1030.442994	92659.088201	34.409754
1031.091120	92800.664585	34.414772
1032.311966	92958.766623	34.419789
1033.687154	93102.405079	34.424807
1034.502298	93258.037434	34.429824
1035.867064	93393.956462	34.434842
1036.812255	93533.523132	34.439860
1037.405506	93673.399675	34.444877
1038.678404	93809.127120	34.449895
1039.377933	93952.834277	34.454912
1040.658478	94085.064285	34.459930
1041.265815	94240.192576	34.464948
1042.186076	94382.273379	34.469965
1043.335911	94537.829791	34.474983
1043.794626	94706.217869	34.480000
1044.862806	94846.696703	34.485018
1045.823672	95006.625771	34.490036
1046.679972	95175.023697	34.495053
1047.575529	95335.389314	34.500071
1048.900513	95518.175822	34.505088
1049.921344	95685.842911	34.510106
1050.804046	95849.611192	34.515124
1051.780063	96019.508264	34.520141
1052.708695	96189.939204	34.525159
1053.736171	96374.241268	34.530176
1055.343505	96539.012647	34.535194
1056.719837	96703.632190	34.540212
1058.508085	96853.428532	34.545229
1060.745236	96990.647613	34.550247
1063.147725	97098.070108	34.555264
1064.848149	97204.415464	34.560282
1066.273090	97324.678633	34.565300
1067.410831	97425.148867	34.570317
1068.914192	97516.514750	34.575335
1069.485205	97625.875930	34.580352
1070.054624	97719.061347	34.585370
1071.257983	97831.739168	34.590388
1071.987479	97945.840455	34.595405
1072.762854	98064.819047	34.600423
1073.411018	98185.007876	34.605440
1074.296032	98306.488234	34.610458
1074.840267	98439.727599	34.615476
1075.482657	98576.741765	34.620493
1076.522893	98711.017292	34.625511
1077.336995	98874.267847	34.630528
1078.305443	99015.674106	34.635546
1078.754280	99159.587041	34.640564
1079.807906	99315.153562	34.645581
1081.104922	99470.188925	34.650599
1081.912811	99636.084172	34.655616
1083.457577	99788.969087	34.660634
1084.217736	99944.757366	34.665652
1085.094921	100109.221419	34.670669
1086.401523	100264.697161	34.675687
1086.887915	100442.272169	34.680704
1088.018910	100608.433027	34.685722
1089.389759	100770.766923	34.690740
1090.497754	100951.973685	34.695757
1091.718405	101113.156997	34.700775
1092.571244	101279.259334	34.705792
1093.701980	101446.514530	34.710810
1094.601484	101613.852000	34.715828
1095.500055	101777.033659	34.720845
1096.966719	101927.002809	34.725863
1097.736119	102103.026860	34.730880
1098.653410	102256.483413	34.735898
1100.465568	102406.938535	34.740916
1102.100176	102542.483184	34.745933
1103.518093	102689.547913	34.750951
1104.782762	102843.142887	34.755968
1106.028310	102976.125903	34.760986
1106.715065	103113.773581	34.766004
1107.656788	103269.998144	34.771021
1109.144941	103418.631909	34.776039
1109.978804	103585.158599	34.781056
1110.880043	103730.217457	34.786074
1112.563287	103871.026937	34.791092
1113.334833	104030.321064	34.796109
1115.156481	104155.562118	34.801127
1115.869067	104307.482569	34.806144
1117.322271	104446.591823	34.811162
1118.072244	104604.513693	34.816180
1119.074062	104758.498334	34.821197
1120.140969	104904.411336	34.826215
1120.728863	105071.677381	34.831232
1121.893859	105232.081412	34.836250
1122.805310	105396.532759	34.841268
1123.824983	105563.214644	34.846285
1125.321590	105722.284545	34.851303
1126.453514	105890.697538	34.856320
1127.808477	106047.380941	34.861338
1130.919660	106160.789129	34.866356
1132.254158	106307.003568	34.871373
1133.585725	106440.315084	34.876391
1134.342059	106572.636610	34.881408
1135.325435	106717.561369	34.886426
1136.194550	106845.847673	34.891444
1137.083411	106993.839627	34.896461
1138.208804	107132.004044	34.901479
1139.432226	107269.261282	34.906496
1140.524514	107412.964076	34.911514
1141.521523	107557.777799	34.916532
1142.283251	107704.332326	34.921549
1143.404275	107857.874886	34.926567
1144.156477	108012.679614	34.931584
1144.964356	108175.546183	34.936602
1146.477287	108330.124355	34.941620
1147.256468	108499.902847	34.946637
1148.647033	108655.097501	34.951655
1149.861385	108817.422699	34.956672
1150.792465	108980.376335	34.961690
1151.970547	109148.070501	34.966708
1152.494883	109328.161640	34.971725
1153.693347	109491.671136	34.976743
1154.576039	109675.265032	34.981760
1155.320174	109848.609369	34.986778
1156.265975	110022.201364	34.991796
1157.299893	110195.653978	34.996813
1158.729142	110364.367261	35.001831
1159.889789	110533.168727	35.006848
1160.726730	110715.442088	35.011866
1162.324391	110881.511581	35.016884
1163.238596	111068.946781	35.021901
1165.035996	111238.867163	35.026919
1166.044534	111411.192975	35.031936
1167.387603	111586.574846	35.036954
1168.729570	111751.241265	35.041972
1169.658998	111931.818747	35.046989
1170.978699	112091.800326	35.052007
1172.358669	112270.289288	35.057024
1173.264770	112434.143318	35.062042
1174.701612	112609.631448	35.067060
1175.483486	112796.100544	35.072077
1176.571410	112977.318760	35.077095
1177.796837	113154.939712	35.082112
1178.588340	113338.018191	35.087130
1180.158217	113523.588746	35.092148
1181.102484	113712.843281	35.097165
1182.215997	113906.244227	35.102183
1183.321263	114104.712530	35.107200
1184.416388	114286.920320	35.112218
1185.854958	114481.711075	35.117236
1186.581616	114684.333842	35.122253
1188.059011	114882.381900	35.127271
1189.181942	115072.162685	35.132288
1190.057342	115280.875934	35.137306
1191.428111	115468.682993	35.142324
1192.512872	115686.565290	35.147341
1193.819494	115882.881942	35.152359
1195.349004	116091.453514	35.157376
1196.089488	116296.182570	35.162394
1197.547139	116497.646238	35.167412
1199.137242	116700.109780	35.172429
1200.433573	116896.619477	35.177447
1201.999151	117092.245784	35.182464
1202.853945	117290.759803	35.187482
1204.329554	117473.208494	35.192500
1205.791037	117678.327801	35.197517
1206.892232	117864.694743	35.202535
1208.030261	118069.108798	35.207552
1208.939297	118264.316554	35.212570
1210.414957	118461.075615	35.217588
1211.756841	118664.461540	35.222605
1212.794966	118856.493652	35.227623
1215.947802	118998.105469	35.232640
1217.507785	119163.418543	35.237658
1219.101151	119335.274640	35.242676
1220.478775	119490.861197	35.247693
1221.541194	119643.719025	35.252711
1222.927773	119804.397013	35.257728
1223.881787	119948.389921	35.262746
1225.192013	120093.226151	35.267764
1225.757952	120244.349104	35.272781
1226.824316	120393.164407	35.277799
1227.763403	120538.720670	35.282816
1228.332147	120698.027102	35.287834
1229.143024	120860.360862	35.292852
1230.291525	121037.447096	35.297869
1231.526400	121206.567237	35.302887
1232.544967	121388.159859	35.307904
1233.246040	121572.299230	35.312922
1234.503009	121755.781564	35.317940
1235.373557	121943.835438	35.322957
1236.668171	122140.448311	35.327975
1237.915150	122336.639592	35.332992
1238.869299	122533.372838	35.338010
1240.514068	122737.635098	35.343028
1241.453823	122945.038129	35.348045
1242.400491	123149.427210	35.353063
1243.587737	123356.768758	35.358080
1244.334511	123577.291272	35.363098
1245.832184	123787.297327	35.368116
1246.985574	124010.608632	35.373133
1248.223586	124237.936230	35.378151
1249.647297	124454.558423	35.383168
1250.700675	124682.970449	35.388186
1252.225041	124906.660867	35.393204
1253.284862	125126.588973	35.398221
1255.093065	125346.729217	35.403239
1256.763503	125565.208451	35.408256
1257.766074	125787.519744	35.413274
1259.185486	125997.175430	35.418292
1260.513030	126234.930641	35.423309
1261.270368	126450.180001	35.428327
1263.199567	126661.001144	35.433344
1264.208905	126887.424586	35.438362
1266.208469	127079.236430	35.443380
1267.847518	127297.088485	35.448397
1269.114747	127509.668218	35.453415
1270.502162	127699.719552	35.458432
1271.781352	127914.707421	35.463450
1273.803790	128099.365316	35.468468
1275.196402	128296.526758	35.473485
1276.305509	128487.425866	35.478503
1277.734989	128688.372061	35.483520
1278.807462	128887.628222	35.488538
1280.466392	129061.341426	35.493556
1282.070620	129249.671360	35.498573
1283.072345	129427.038556	35.503591
1284.609635	129604.461093	35.508608
1286.104664	129790.062913	35.513626
1287.685040	129958.143879	35.518644
1289.021110	130142.493747	35.523661
1289.966774	130319.824850	35.528679
1291.378691	130497.957126	35.533696
1292.309350	130673.215097	35.538714
1293.292402	130841.130268	35.543732
1294.113567	131015.901006	35.548749
1295.092008	131188.341972	35.553767
1296.270616	131366.124081	35.558784
1296.857524	131564.893686	35.563802
1298.384920	131746.398307	35.568820
1299.464456	131947.664248	35.573837
1300.520361	132149.974310	35.578855
1301.941190	132338.392118	35.583872
1302.894855	132558.408715	35.588890
1303.862353	132759.343450	35.593908
1304.824592	132986.888103	35.598925
1306.265559	133195.796298	35.603943
1308.582259	133382.596150	35.608960
1311.101314	133565.297801	35.613978
1313.252565	133740.215952	35.618996
1314.695638	133920.620139	35.624013
1316.796758	134084.638859	35.629031
1318.167108	134249.839038	35.634048
1319.024438	134429.085111	35.639066
1320.084927	134591.181434	35.644084
1321.905771	134753.322521	35.649101
1322.693944	134924.980003	35.654119
1324.346826	135090.748298	35.659136
1325.004040	135276.392397	35.664154
1326.514930	135446.176764	35.669172
1327.730513	135631.138814	35.674189
1328.227524	135828.495013	35.679207
1329.737571	136020.736896	35.684224
1330.732569	136211.401920	35.689242
1331.965851	136413.092809	35.694260
1333.056053	136616.062350	35.699277
1333.879388	136827.109764	35.704295
1335.438230	137040.563525	35.709312
1335.866660	137269.215066	35.714330
1337.035518	137484.748916	35.719348
1338.441621	137705.454975	35.724365
1339.668863	137944.997068	35.729383
1341.308569	138167.114101	35.734400
1342.535722	138403.111590	35.739418
1343.952451	138641.361918	35.744436
1345.268811	138862.128867	35.749453
1346.494976	139107.142506	35.754471
1348.254895	139331.137392	35.759488
1349.290245	139573.967400	35.764506
1350.734330	139803.820339	35.769524
1352.309822	140035.871990	35.774541
1353.541403	140274.659014	35.779559
1355.078111	140514.590745	35.784576
1356.180248	140750.132326	35.789594
1357.517531	140991.595036	35.794612
1359.992889	141200.395666	35.799629
1361.434134	141429.158811	35.804647
1362.938660	141635.379175	35.809664
1364.160962	141864.167718	35.814682
1365.725059	142072.751637	35.819700
1367.376689	142264.922523	35.824717
1368.259627	142473.034423	35.829735
1369.523167	142669.870338	35.834752
1370.491406	142881.102042	35.839770
1371.988398	143085.863137	35.844788
1373.283317	143302.318459	35.849805
1374.215362	143513.141985	35.854823
1375.752826	143721.893440	35.859840
1376.548425	143959.295615	35.864858
1377.693522	144183.499992	35.869876
1379.414541	144413.077452	35.874893
1380.133683	144670.055018	35.879911
1381.750090	144894.772674	35.884928
1383.180654	145146.342784	35.889946
1384.137631	145381.030268	35.894964
1385.278118	145629.734984	35.899981
1386.724833	145900.398147	35.904999
1387.998677	146139.097183	35.910016
1389.718232	146400.328455	35.915034
1391.512987	146650.813293	35.920052
1393.188303	146896.502149	35.925069
1394.151307	147143.941359	35.930087
1395.767352	147399.949349	35.935104
1397.140426	147654.375424	35.940122
1398.240494	147912.320301	35.945140
1399.928890	148173.140099	35.950157
1401.302038	148436.230563	35.955175
1402.677055	148683.464094	35.960192
1404.285128	148950.489298	35.965210
1405.552152	149209.140647	35.970228
1407.177799	149467.622977	35.975245
1408.431491	149727.256734	35.980263
1410.002750	149988.654966	35.985280
1411.256430	150251.462265	35.990298
1412.657692	150509.456095	35.995316
1414.317665	150765.179574	36.000333
1415.599380	151031.576487	36.005351
1417.037209	151281.482157	36.010368
1418.696972	151556.266732	36.015386
1420.082245	151824.948339	36.020404
1421.999426	152064.058094	36.025421
1423.714436	152321.750057	36.030439
1425.277090	152566.041816	36.035456
1426.914470	152809.030293	36.040474
1428.310263	153063.165375	36.045492
1430.114770	153298.523718	36.050509
1431.221824	153552.594307	36.055527
1432.639760	153794.394996	36.060544
1433.992241	154043.396796	36.065562
1435.092027	154294.862297	36.070580
1436.997178	154531.430493	36.075597
1438.358124	154785.089677	36.080615
1439.811027	155026.259695	36.085632
1441.276452	155272.108144	36.090650
1442.689901	155501.622754	36.095668
1444.807150	155702.979840	36.100685
1446.342685	155925.998651	36.105703
1447.980728	156132.988122	36.110720
1449.016770	156349.444892	36.115738
1451.299592	156550.019880	36.120756
1453.103440	156741.517224	36.125773
1454.443827	156956.978469	36.130791
1456.051024	157150.563509	36.135808
1458.281525	157330.508160	36.140826
1459.768044	157515.517268	36.145844
1460.933482	157708.922034	36.150861
1461.995702	157900.188616	36.155879
1462.897867	158110.147318	36.160896
1464.695370	158317.111893	36.165914
1465.517968	158523.306930	36.170932
1466.999733	158728.713684	36.175949
1467.865393	158962.332801	36.180967
1468.937798	159187.386408	36.185984
1470.460130	159416.580034	36.191002
1471.631150	159655.785576	36.196020
1473.346463	159874.312144	36.201037
1474.502184	160137.363853	36.206055
1475.754660	160373.847538	36.211072
1477.395784	160617.195068	36.216090
1478.430977	160870.785707	36.221108
1480.109195	161115.817387	36.226125
1481.340297	161382.290343	36.231143
1482.165352	161639.673593	36.236160
1484.055314	161903.496708	36.241178
1485.212028	162171.433070	36.246196
1486.896166	162426.922664	36.251213
1488.586265	162697.669679	36.256231
1489.991001	162972.966240	36.261248
1491.480610	163237.230494	36.266266
1492.617388	163521.185054	36.271284
1494.166886	163799.863747	36.276301
1495.786489	164076.212511	36.281319
1497.885225	164344.332273	36.286336
1499.097366	164614.953856	36.291354
1500.678402	164890.135372	36.296372
1502.478567	165157.991426	36.301389
1503.870384	165433.841200	36.306407
1505.093197	165716.378523	36.311424
1506.853173	165978.678987	36.316442
1507.936405	166258.173252	36.321460
1509.663019	166539.989914	36.326477
1511.271331	166817.603880	36.331495
1512.840383	167093.158707	36.336512
1514.492343	167374.993489	36.341530
1516.189480	167643.771574	36.346548
1517.652872	167912.195504	36.351565
1519.127366	168192.441026	36.356583
1520.676736	168470.609211	36.361600
1522.933208	168724.960398	36.366618
1523.900021	168995.715944	36.371636
1525.477473	169243.252860	36.376653
1527.646902	169472.863054	36.381671
1529.645168	169704.328376	36.386688
1531.403924	169936.061461	36.391706
1532.579547	170182.932544	36.396724
1534.150279	170403.497771	36.401741
1535.141986	170655.969662	36.406759
1536.420312	170904.680985	36.411776
1538.340333	171144.805718	36.416794
1539.157491	171409.842930	36.421812
1540.619214	171653.240212	36.426829
1542.189533	171922.499528	36.431847
1543.780770	172184.983420	36.436864
1545.441800	172451.250888	36.441882
1546.398118	172723.277123	36.446900
1548.051716	172989.041957	36.451917
1549.208070	173274.080899	36.456935
1550.555591	173540.760652	36.461952
1552.041500	173816.794992	36.466970
1553.329446	174115.304003	36.471988
1554.856487	174410.580372	36.477005
1556.316207	174703.357748	36.482023
1557.777666	175000.374138	36.487040
1559.418130	175301.220880	36.492058
1560.970595	175612.854531	36.497076
1562.630409	175904.987117	36.502093
1564.248165	176207.988137	36.507111
1565.851888	176515.484682	36.512128
1568.043242	176821.253577	36.517146
1569.434484	177125.324930	36.522164
1571.072707	177413.018534	36.527181
1572.961753	177715.238947	36.532199
1574.680146	178004.129152	36.537216
1576.553231	178298.261948	36.542234
1578.313950	178586.578510	36.547252
1580.712178	178857.426798	36.552269
1582.843226	179129.270821	36.557287
1583.980129	179400.767007	36.562304
1586.309726	179657.522806	36.567322
1587.714559	179938.850796	36.572340
1589.195903	180199.500146	36.577357
1591.405292	180461.164644	36.582375
1592.778133	180721.352257	36.587392
1595.063170	180962.478778	36.592410
1596.766934	181211.159544	36.597428
1598.472786	181452.977137	36.602445
1599.831237	181705.839221	36.607463
1601.209492	181970.423572	36.612480
1602.944789	182205.693521	36.617498
1604.357393	182465.593414	36.622516
1605.759606	182711.386912	36.627533
1607.682787	182956.502665	36.632551
1608.779274	183206.204795	36.637568
1610.582427	183452.116363	36.642586
1611.919226	183701.897306	36.647604
1613.315227	183935.453928	36.652621
1614.632553	184166.232712	36.657639
1615.615304	184435.855968	36.662656
1617.439289	184674.639758	36.667674
1618.461272	184932.167110	36.672692
1619.759594	185184.982419	36.677709
1621.368065	185463.420220	36.682727
1622.626237	185742.879755	36.687744
1624.387333	186016.106758	36.692762
1625.577984	186292.090790	36.697780
1627.524558	186565.748431	36.702797
1629.522428	186839.551828	36.707815
1630.928496	187129.769810	36.712832
1632.541995	187408.916548	36.717850
1634.039886	187705.747614	36.722868
1635.508561	188003.295846	36.727885
1636.994187	188311.299861	36.732903
1638.255203	188616.600504	36.737920
1639.725835	188915.626254	36.742938
1641.359935	189228.498401	36.747956
1642.687455	189550.164960	36.752973
1644.622998	189858.399461	36.757991
1646.185308	190189.246296	36.763008
1648.287582	190495.872099	36.768026
1649.744874	190824.024187	36.773044
1651.077812	191135.763687	36.778061
1653.345425	191447.927827	36.783079
1655.100455	191771.521081	36.788096
1657.064129	192091.618687	36.793114
1658.498154	192415.965182	36.798132
1660.663480	192717.683490	36.803149
1662.031789	193038.922478	36.808167
1663.479802	193357.117648	36.813184
1665.880516	193656.659437	36.818202
1667.707439	193976.232503	36.823220
1669.255971	194287.335757	36.828237
1670.855780	194598.001269	36.833255
1672.425119	194913.141017	36.838272
1674.450620	195221.585142	36.843290
1676.100362	195539.533578	36.848308
1677.792345	195851.435896	36.853325
1679.832629	196163.779780	36.858343
1681.450927	196475.926034	36.863360
1683.506532	196779.475556	36.868378
1684.882932	197093.237765	36.873396
1686.591637	197400.552135	36.878413
1688.292287	197700.177974	36.883431
1690.257658	198001.108881	36.888448
1692.339409	198301.401083	36.893466
1694.493825	198594.423254	36.898484
1696.287914	198885.321113	36.903501
1698.050711	199164.497397	36.908519
1699.711597	199465.446848	36.913536
1701.636352	199740.373684	36.918554
1703.559001	199994.866567	36.923572
1705.098020	200253.838739	36.928589
1706.608425	200510.722325	36.933607
1707.957573	200782.102916	36.938624
1709.883763	201031.383186	36.943642
1711.419384	201311.203147	36.948660
1712.355925	201583.008614	36.953677
1714.395396	201846.402256	36.958695
1715.495407	202140.931059	36.963712
1716.880340	202430.516465	36.968730
1719.037526	202709.419666	36.973748
1721.624242	202967.425762	36.978765
1723.211156	203240.164175	36.983783
1724.938280	203515.433082	36.988800
1726.646546	203798.754203	36.993818
1728.412162	204078.081737	36.998836
1729.900240	204361.148641	37.003853
1732.380633	204637.293452	37.008871
1733.629974	204924.526580	37.013888
1735.495867	205200.987451	37.018906
1737.437962	205473.565801	37.023924
1739.072644	205752.135146	37.028941
1740.657160	206035.715338	37.033959
1742.147639	206327.842447	37.038976
1743.949648	206615.935471	37.043994
1745.691150	206907.263901	37.049012
1746.942058	207209.792090	37.054029
1748.831987	207503.118283	37.059047
1749.929405	207817.670321	37.064064
1751.721986	208135.185744	37.069082
1753.144509	208442.631104	37.074100
1754.901133	208759.241450	37.079117
1756.668942	209078.885745	37.084135
1758.211177	209410.691258	37.089152
1759.998990	209723.785068	37.094170
1761.704064	210064.442075	37.099188
1763.026844	210402.927269	37.104205
1764.723828	210737.216197	37.109223
1766.395570	211082.365428	37.114240
1768.146800	211421.790961	37.119258
1770.376269	211757.105192	37.124276
1772.422843	212095.370186	37.129293
1774.416424	212433.581882	37.134311
1775.933767	212770.436332	37.139328
1778.253153	213116.826647	37.144346
1779.750618	213450.843891	37.149364
1781.298307	213788.574740	37.154381
1783.519262	214119.712775	37.159399
1785.727571	214457.608738	37.164416
1787.748889	214779.069270	37.169434
1789.313439	215108.246924	37.174452
1791.115518	215441.590899	37.179469
1792.592262	215769.236742	37.184487
1794.488698	216109.920117	37.189504
1796.770044	216437.200159	37.194522
1798.226215	216743.143066	37.199540
1799.547797	217056.675788	37.204557
1801.555272	217372.043586	37.209575
1803.248703	217680.784231	37.214592
1804.743037	218005.707981	37.219610
1806.626752	218330.431724	37.224628
1808.266553	218635.756890	37.229645
1810.548378	218958.350684	37.234663
1811.805144	219282.403725	37.239680
1813.746606	219613.320124	37.244698
1815.867411	219930.039686	37.249716
1817.690381	220258.539964	37.254733
1819.918974	220562.928973	37.259751
1821.868559	220892.960989	37.264768
1823.674186	221216.706787	37.269786
1825.933347	221525.449979	37.274804
1827.462907	221851.070710	37.279821
1829.505396	222213.243336	37.284839
1830.945351	222558.727294	37.289856
1832.654785	222886.266541	37.294874
1834.414361	223205.215658	37.299892
1835.761503	223545.512711	37.304909
1837.874244	223888.762522	37.309927
1839.346019	224232.966305	37.314944
1840.981924	224577.945466	37.319962
1842.849666	224926.508173	37.324980
1844.318371	225282.322710	37.329997
1846.165820	225647.995748	37.335015
1847.948138	226008.880905	37.340032
1849.857621	226377.937674	37.345050
1851.744030	226734.606390	37.350068
1852.894785	227107.113693	37.355085
1855.168659	227479.850685	37.360103
1857.202957	227855.801890	37.365120
1859.069735	228219.946493	37.370138
1861.192917	228589.182055	37.375156
1863.309050	228972.896486	37.380173
1865.088058	229341.072365	37.385191
1866.822289	229716.012484	37.390208
1868.711516	230090.040660	37.395226
1871.143126	230458.142913	37.400244
1873.331855	230811.351553	37.405261
1875.627963	231170.335121	37.410279
1877.811977	231525.198066	37.415296
1879.608564	231888.911434	37.420314
1882.079178	232242.537902	37.425332
1883.895009	232588.421681	37.430349
1886.244693	232917.687920	37.435367
1888.813528	233254.946266	37.440384
1890.458498	233596.619296	37.445402
1892.408832	233921.685427	37.450420
1894.167873	234255.291404	37.455437
1895.745975	234591.721028	37.460455
1897.917589	234917.898199	37.465472
1899.659784	235235.356688	37.470490
1901.654412	235545.943874	37.475508
1903.202428	235853.250255	37.480525
1905.562976	236146.662466	37.485543
1907.289092	236452.469215	37.490560
1909.075199	236753.517735	37.495578
1911.831198	237031.909705	37.500596
1913.154124	237347.917193	37.505613
1915.193949	237640.901843	37.510631
1916.984854	237942.968886	37.515648
1918.223044	238256.427135	37.520666
1920.614032	238566.553795	37.525684
1921.872142	238881.712392	37.530701
1923.755294	239197.661650	37.535719
1925.531109	239516.549762	37.540736
1926.962445	239851.368168	37.545754
1929.215061	240170.487210	37.550772
1930.838761	240516.554443	37.555789
1932.726246	240854.859284	37.560807
1934.495102	241193.234710	37.565824
1936.157227	241545.470992	37.570842
1938.337410	241888.482068	37.575860
1940.417304	242241.847851	37.580877
1942.325067	242593.971947	37.585895
1944.506667	242943.742148	37.590912
1946.001615	243305.484222	37.595930
1948.096292	243657.251392	37.600948
1950.207172	244013.233414	37.605965
1952.327434	244376.276251	37.610983
1954.597186	244719.458505	37.616000
1956.691681	245065.488918	37.621018
1959.124036	245410.831575	37.626036
1961.193831	245756.334238	37.631053
1962.875374	246107.817762	37.636071
1965.246662	246459.116501	37.641088
1966.645998	246803.229468	37.646106
1969.123949	247157.815113	37.651124
1971.004990	247504.317193	37.656141
1972.560634	247861.387788	37.661159
1974.333188	248213.801792	37.666176
1976.189552	248582.841131	37.671194
1978.351301	248938.039980	37.676212
1980.015295	249309.626299	37.681229
1981.940153	249672.408600	37.686247
1984.028341	250035.597625	37.691264
1986.041958	250411.322250	37.696282
1987.724633	250775.999742	37.701300
1989.934404	251158.019917	37.706317
1991.709544	251528.145706	37.711335
1993.971332	251896.391538	37.716352
1995.958785	252271.438551	37.721370
1998.080240	252640.165422	37.726388
2000.038755	253019.206670	37.731405
2002.315548	253384.938361	37.736423
2004.774270	253755.417473	37.741440
2006.585283	254104.001886	37.746458
2009.167883	254435.521286	37.751476
2011.173999	254770.816025	37.756493
2013.241298	255110.242171	37.761511
2015.164605	255436.863599	37.766528
2016.822097	255771.656442	37.771546
2018.703862	256103.238939	37.776564
2020.712045	256437.519938	37.781581
2022.547277	256772.260728	37.786599
2024.318808	257121.135875	37.791616
2026.344820	257475.381903	37.796634
2027.937328	257829.570238	37.801652
2029.605095	258186.541440	37.806669
2031.414385	258553.931172	37.811687
2033.676127	258920.894024	37.816704
2035.542082	259300.570724	37.821722
2037.359438	259674.616292	37.826740
2039.215888	260061.916405	37.831757
2041.064148	260452.927169	37.836775
2043.438310	260826.581139	37.841792
2045.447108	261224.273832	37.846810
2048.231454	261598.625797	37.851828
2050.366914	261975.037196	37.856845
2052.220004	262370.241203	37.861863
2054.710653	262743.243974	37.866880
2056.880564	263130.091868	37.871898
2058.872150	263510.490721	37.876916
2061.670335	263882.455223	37.881933
2063.454385	264255.114459	37.886951
2066.398061	264624.795749	37.891968
2068.408110	264996.200498	37.896986
2070.642057	265356.367285	37.902004
2073.047379	265713.052363	37.907021
2075.060222	266086.642298	37.912039
2076.929691	266447.629898	37.917056
2078.924151	266812.941890	37.922074
2081.254746	267175.025422	37.927092
2083.253091	267533.935703	37.932109
2085.888524	267888.452000	37.937127
2088.159065	268234.897357	37.942144
2090.127868	268607.505362	37.947162
2092.656257	268943.875912	37.952180
2094.830436	269295.316182	37.957197
2096.898835	269646.519372	37.962215
2099.467845	269989.031578	37.967232
2101.194378	270329.746920	37.972250
2103.268148	270668.603674	37.977268
2105.480451	271028.802806	37.982285
2107.110036	271377.205722	37.987303
2109.030679	271720.786739	37.992320
2110.940856	272083.396650	37.997338
2113.104468	272435.728885	38.002356
2115.602819	272778.964489	38.007373
2117.908078	273126.142912	38.012391
2120.057126	273469.484852	38.017408
2122.406031	273816.275402	38.022426
2124.356051	274146.337605	38.027444
2126.343903	274464.123980	38.032461
2127.891848	274783.555160	38.037479
2130.232480	275106.239262	38.042496
2131.915582	275436.572474	38.047514
2134.051320	275765.462094	38.052532
2136.169186	276099.613035	38.057549
2137.709734	276442.949940	38.062567
2139.628666	276781.120700	38.067584
2141.542742	277124.195037	38.072602
2144.155323	277465.862946	38.077620
2146.428919	277821.835856	38.082637
2148.204535	278177.354194	38.087655
2150.463550	278533.659476	38.092672
2152.154088	278901.918188	38.097690
2153.921347	279269.605727	38.102708
2156.009365	279646.387455	38.107725
2157.973666	280028.777377	38.112743
2159.999778	280418.829119	38.117760
2162.053373	280813.550509	38.122778
2164.200727	281208.790275	38.127796
2166.232062	281611.719996	38.132813
2167.924694	282023.416491	38.137831
2170.715638	282411.389692	38.142848
2173.013025	282818.975980	38.147866
2175.252806	283224.513427	38.152884
2177.445954	283631.378904	38.157901
2179.477879	284044.391763	38.162919
2181.601900	284463.588003	38.167936
2183.786934	284879.801994	38.172954
2185.981196	285290.222200	38.177972
2188.441918	285711.497633	38.182989
2190.146768	286145.822620	38.188007
2192.624089	286557.085674	38.193024
2194.637824	286996.187215	38.198042
2196.661977	287428.935804	38.203060
2199.100711	287852.600043	38.208077
2200.892825	288296.891780	38.213095
2203.371466	288732.132202	38.218112
2205.624491	289175.384243	38.223130
2207.844258	289609.064040	38.228148
2210.258977	290046.954499	38.233165
2212.280081	290493.492775	38.238183
2214.630136	290928.191310	38.243200
2216.920029	291367.191685	38.248218
2219.007386	291827.967973	38.253236
2221.703371	292260.297696	38.258253
2224.522939	292688.085397	38.263271
2227.178441	293107.515536	38.268288
2229.606610	293538.132574	38.273306
2231.705948	293959.833906	38.278324
2234.310478	294376.678678	38.283341
2236.083889	294803.866104	38.288359
2238.574106	295212.674838	38.293376
2240.650587	295631.099538	38.298394
2242.639649	296029.418805	38.303412
2245.046340	296426.756558	38.308429
2246.972105	296827.268780	38.313447
2249.017645	297215.238027	38.318464
2250.875814	297620.687216	38.323482
2252.949777	298025.745652	38.328500
2255.353815	298430.547608	38.333517
2257.146232	298855.081077	38.338535
2259.536408	299269.129462	38.343552
2261.626387	299693.943868	38.348570
2263.592980	300123.094993	38.353588
2266.232693	300547.743812	38.358605
2268.059872	300970.539040	38.363623
2270.184130	301407.459917	38.368640
2272.434998	301848.423670	38.373658
2274.755889	302290.340282	38.378676
2277.642230	302733.334378	38.383693
2279.463909	303173.498642	38.388711
2282.003827	303619.745496	38.393728
2284.304813	304067.705290	38.398746
2286.554397	304517.907067	38.403764
2288.678887	304961.243645	38.408781
2290.921894	305424.042196	38.413799
2293.098143	305869.171027	38.418816
2295.656004	306346.242302	38.423834
2297.839216	306801.603207	38.428852
2300.411149	307250.627021	38.433869
2302.341217	307734.244317	38.438887
2304.927537	308194.159109	38.443904
2307.615523	308650.931876	38.448922
2309.740777	309123.108214	38.453940
2312.481981	309574.509687	38.458957
2314.681427	310043.927436	38.463975
2317.105135	310512.190161	38.468992
2319.236780	310979.328911	38.474010
2321.614747	311447.569652	38.479028
2324.375528	311909.778939	38.484045
2326.847146	312376.476973	38.489063
2329.065138	312840.114551	38.494080
2331.976009	313306.129373	38.499098
2334.309621	313765.604606	38.504116
2337.086020	314210.225637	38.509133
2339.444395	314662.378204	38.514151
2341.982620	315111.884236	38.519168
2344.542443	315556.914759	38.524186
2347.782306	315989.491992	38.529204
2350.785624	316397.494113	38.534221
2353.148675	316827.946257	38.539239
2355.653933	317249.586302	38.544256
2358.233792	317656.558181	38.549274
2360.212569	318070.353990	38.554292
2362.691390	318482.189305	38.559309
2364.737648	318894.650128	38.564327
2366.806590	319314.115179	38.569344
2369.197154	319714.631830	38.574362
2371.320040	320120.725719	38.579380
2373.618628	320504.212032	38.584397
2375.874203	320899.716236	38.589415
2377.880265	321290.153487	38.594432
2380.466120	321687.506571	38.599450
2381.986786	322091.578998	38.604468
2384.019090	322496.889049	38.609485
2386.411774	322906.609806	38.614503
2388.360947	323330.290583	38.619520
2390.679972	323757.821594	38.624538
2392.726409	324193.291747	38.629556
2394.960389	324615.803451	38.634573
2397.267873	325067.277726	38.639591
2399.674391	325511.546884	38.644608
2402.278563	325960.759754	38.649626
2404.690089	326409.492734	38.654644
2407.334372	326843.812691	38.659661
2409.613039	327306.122590	38.664679
2412.080513	327757.987978	38.669696
2415.044407	328206.191402	38.674714
2417.535297	328665.336002	38.679732
2420.101476	329108.188152	38.684749
2422.357225	329569.269112	38.689767
2424.606784	330021.003222	38.694784
2427.066858	330478.287856	38.699802
2429.296716	330937.459872	38.704820
2431.981336	331406.688930	38.709837
2434.169745	331881.199223	38.714855
2436.656939	332349.056797	38.719872
2439.447444	332810.946650	38.724890
2441.360877	333285.110265	38.729908
2443.905367	333753.457300	38.734925
2446.527987	334241.950430	38.739943
2448.626508	334729.659819	38.744960
2452.450128	335172.122853	38.749978
2455.316140	335631.671210	38.754996
2457.941801	336092.752636	38.760013
2460.375273	336554.419952	38.765031
2462.871023	337012.646336	38.770048
2465.339605	337466.379580	38.775066
2467.679720	337943.794519	38.780084
2470.334503	338394.368676	38.785101
2473.448341	338835.573922	38.790119
2475.903052	339283.710635	38.795136
2479.259622	339710.119443	38.800154
2482.365511	340132.375709	38.805172
2485.042388	340554.341654	38.810189
2487.685087	340986.821554	38.815207
2489.807553	341408.031682	38.820224
2492.606245	341817.376415	38.825242
2494.559660	342242.314461	38.830260
2496.628483	342665.403221	38.835277
2499.059787	343105.848405	38.840295
2501.083972	343526.500832	38.845312
2503.591966	343953.039941	38.850330
2505.629076	344369.266724	38.855348
2507.578657	344781.543863	38.860365
2509.522426	345196.408597	38.865383
2511.960281	345630.461478	38.870400
2514.387644	346054.789271	38.875418
2515.968752	346499.101051	38.880436
2518.519836	346945.438973	38.885453
2520.770543	347392.557203	38.890471
2522.767911	347856.289667	38.895488
2525.441849	348324.176040	38.900506
2527.375481	348796.846891	38.905524
2529.756875	349281.272733	38.910541
2532.168935	349770.081219	38.915559
2534.612161	350263.145194	38.920576
2537.569917	350762.774165	38.925594
2539.641814	351266.981289	38.930612
2542.083984	351773.790418	38.935629
2544.839263	352285.215903	38.940647
2547.038710	352807.005250	38.945664
2550.144931	353310.978239	38.950682
2552.627878	353833.448553	38.955700
2555.097733	354362.667753	38.960717
2557.943739	354889.435847	38.965735
2560.086333	355418.746747	38.970752
2562.676244	355951.890229	38.975770
2565.040354	356488.668190	38.980788
2567.789167	357039.542850	38.985805
2570.555929	357579.621131	38.990823
2573.464501	358111.853406	38.995840
2576.495907	358646.192499	39.000858
2578.921224	359189.733660	39.005876
2581.487247	359723.956955	39.010893
2584.083837	360263.372533	39.015911
2586.634088	360810.378129	39.020928
2589.295854	361354.060331	39.025946
2591.991164	361912.857374	39.030964
2594.938515	362454.857290	39.035981
2597.897072	362994.412712	39.040999
2600.440074	363535.296631	39.046016
2603.185227	364075.406183	39.051034
2605.448186	364620.559915	39.056052
2608.661413	365150.964154	39.061069
2611.900178	365677.297671	39.066087
2614.418972	366218.940206	39.071104
2616.897292	366741.701945	39.076122
2619.523954	367282.527760	39.081140
2622.292120	367817.919318	39.086157
2624.811630	368351.288256	39.091175
2627.140380	368885.848188	39.096192
2629.966163	369425.169545	39.101210
2632.330564	369964.836375	39.106228
2635.087307	370496.035132	39.111245
2638.089054	371031.882780	39.116263
2640.455801	371576.400785	39.121280
2643.338545	372080.713637	39.126298
2645.615591	372603.207861	39.131316
2648.048449	373097.354100	39.136333
2650.998532	373591.514016	39.141351
2653.485548	374094.114407	39.146368
2656.481784	374591.325130	39.151386
2659.340400	375086.344220	39.156404
2661.853352	375578.773360	39.161421
2665.096243	376074.658283	39.166439
2667.351704	376572.139671	39.171456
2670.414686	377062.230875	39.176474
2672.692572	377571.696743	39.181492
2675.203977	378070.032248	39.186509
2677.918925	378571.297516	39.191527
2680.566145	379086.165268	39.196544
2683.206376	379595.395352	39.201562
2685.496281	380119.033121	39.206580
2687.947984	380636.067698	39.211597
2690.591090	381150.604292	39.216615
2693.229895	381692.455971	39.221632
2695.722472	382221.233427	39.226650
2698.236879	382767.224425	39.231668
2700.408947	383321.734287	39.236685
2703.398279	383875.726026	39.241703
2706.161884	384437.304408	39.246720
2709.072580	384980.105729	39.251738
2712.239322	385541.172328	39.256756
2715.040568	386090.595006	39.261773
2718.196069	386632.521505	39.266791
2720.446338	387185.870393	39.271808
2723.621495	387738.404899	39.276826
2726.538957	388291.681932	39.281844
2729.380709	388851.176377	39.286861
2732.095991	389404.645778	39.291879
2734.809157	389960.161242	39.296896
2737.108814	390505.715537	39.301914
2740.289480	391066.262650	39.306932
2742.801229	391630.279751	39.311949
2745.777286	392188.406611	39.316967
2748.543033	392763.929558	39.321984
2751.583338	393320.988214	39.327002
2754.011582	393883.181289	39.332020
2757.051256	394440.779758	39.337037
2759.803771	394994.052894	39.342055
2762.813177	395557.546367	39.347072
2765.467663	396117.637978	39.352090
2768.468232	396676.524361	39.357108
2771.319396	397230.810103	39.362125
2774.620416	397790.593790	39.367143
2776.964149	398352.193100	39.372160
2779.844913	398895.847459	39.377178
2782.661195	399456.922027	39.382196
2784.759587	400018.709148	39.387213
2787.891945	400580.246773	39.392231
2790.655595	401145.991070	39.397248
2792.903711	401696.569668	39.402266
2796.070126	402228.181491	39.407284
2798.841860	402749.934104	39.412301
2801.899810	403277.159610	39.417319
2804.407567	403800.229719	39.422336
2807.197551	404316.604421	39.427354
2809.740872	404848.144182	39.432372
2812.907926	405370.652787	39.437389
2816.162700	405882.238220	39.442407
2818.943446	406411.761765	39.447424
2821.666805	406935.987345	39.452442
2824.250603	407466.968866	39.457460
2826.785902	408006.187075	39.462477
2829.451510	408540.913908	39.467495
2832.084054	409096.928397	39.472512
2834.863755	409642.415750	39.477530
2837.403892	410197.892335	39.482548
2839.835019	410760.295367	39.487565
2843.114331	411330.030465	39.492583
2846.215509	411893.345230	39.497600
2849.334172	412454.162762	39.502618
2852.242729	413027.446850	39.507636
2855.020014	413593.010760	39.512653
2857.977642	414164.414796	39.517671
2860.266717	414753.551917	39.522688
2863.273725	415335.797103	39.527706
2866.040071	415906.386217	39.532724
2868.752577	416515.288202	39.537741
2871.684328	417100.651919	39.542759
2874.579381	417687.681889	39.547776
2877.394211	418285.760448	39.552794
2880.359115	418894.115556	39.557812
2882.963186	419491.213760	39.562829
2886.263931	420084.920403	39.567847
2889.005299	420701.709246	39.572864
2892.247496	421298.895877	39.577882
2895.285876	421901.447847	39.582900
2898.206511	422514.696943	39.587917
2901.096972	423111.545365	39.592935
2903.865484	423717.900527	39.597952
2907.184035	424332.008659	39.602970
2910.481790	424932.502186	39.607988
2913.304853	425545.799925	39.613005
2916.763052	426137.298782	39.618023
2920.023339	426736.491426	39.623040
2922.892619	427324.738833	39.628058
2926.191605	427901.379823	39.633076
2929.038822	428503.789732	39.638093
2931.988857	429086.944605	39.643111
2934.801398	429676.719152	39.648128
2937.624173	430259.260250	39.653146
2941.010092	430838.710544	39.658164
2944.099484	431426.198250	39.663181
2947.169531	432004.760743	39.668199
2950.291945	432582.694158	39.673216
2952.879871	433155.659424	39.678234
2956.185100	433676.278370	39.683252
2958.802339	434223.257014	39.688269
2961.613463	434756.391714	39.693287
2964.382049	435294.333376	39.698304
2967.094182	435837.413054	39.703322
2969.708070	436384.801358	39.708340
2972.475671	436937.724171	39.713357
2975.132283	437492.880591	39.718375
2977.850879	438060.497871	39.723392
2980.412147	438638.913387	39.728410
2982.908117	439218.237223	39.733428
2985.197632	439807.302536	39.738445
2987.974912	440411.518055	39.743463
2990.936038	441031.639592	39.748480
2993.784765	441648.573235	39.753498
2996.659129	442269.537755	39.758516
2999.579485	442921.566543	39.763533
3002.413861	443549.238438	39.768551
3005.640848	444195.463040	39.773568
3008.434087	444856.116895	39.778586
3011.697709	445504.325368	39.783604
3014.467549	446164.794718	39.788621
3017.496788	446814.826914	39.793639
3020.661547	447480.461729	39.798656
3023.618415	448147.274824	39.803674
3027.058074	448821.939595	39.808692
3030.183052	449493.496367	39.813709
3033.570137	450148.694023	39.818727
3036.912262	450812.383381	39.823744
3040.286568	451481.565286	39.828762
3043.586721	452141.173891	39.833780
3046.609100	452805.868373	39.838797
3050.053242	453461.519049	39.843815
3053.216018	454121.395646	39.848832
3055.862413	454775.312650	39.853850
3059.147192	455444.391980	39.858868
3062.284489	456115.549370	39.863885
3065.302444	456783.264626	39.868903
3068.808252	457446.986510	39.873920
3071.361013	458106.740910	39.878938
3074.347961	458770.808772	39.883956
3077.294028	459458.541353	39.888973
3080.448805	460129.118888	39.893991
3083.501727	460799.944910	39.899008
3086.782242	461477.898010	39.904026
3089.880955	462154.492789	39.909044
3093.092670	462826.799208	39.914061
3096.170131	463499.965814	39.919079
3099.588264	464177.660491	39.924096
3102.350350	464851.138003	39.929114
3105.837637	465526.300361	39.934132
3108.858884	466207.078624	39.939149
3111.981513	466882.306011	39.944167
3115.261501	467562.240946	39.949184
3118.156205	468218.546225	39.954202
3121.197071	468869.447112	39.959220
3124.190067	469509.260242	39.964237
3127.557566	470139.588530	39.969255
3131.056217	470762.746822	39.974272
3133.731444	471389.505628	39.979290
3137.035287	472007.752147	39.984308
3139.865296	472636.319294	39.989325
3143.077866	473285.435682	39.994343
3146.085712	473925.614662	39.999360
3148.870058	474567.022207	40.004378
3151.996464	475211.034806	40.009396
3154.898247	475865.527268	40.014413
3158.352584	476519.860447	40.019431
3161.586187	477173.752199	40.024448
3164.511851	477846.576972	40.029466
3167.820119	478495.914571	40.034484
3171.064238	479168.896912	40.039501
3173.948649	479829.630810	40.044519
3177.631876	480496.988978	40.049536
3180.837431	481165.815182	40.054554
3184.402311	481837.695150	40.059572
3187.817977	482512.203549	40.064589
3190.505892	483180.890909	40.069607
3194.095343	483856.285282	40.074624
3196.863106	484529.562561	40.079642
3199.990230	485217.211310	40.084660
3203.234723	485907.949648	40.089677
3206.460319	486592.804844	40.094695
3209.965869	487290.828822	40.099712
3212.811987	487992.114435	40.104730
3216.410984	488683.655838	40.109748
3219.411695	489384.056981	40.114765
3222.316546	490087.427754	40.119783
3225.894275	490785.159435	40.124800
3228.723284	491496.571792	40.129818
3231.991502	492198.542715	40.134836
3235.448699	492914.246507	40.139853
3238.865278	493622.958854	40.144871
3242.484004	494327.369421	40.149888
3245.685039	495039.697731	40.154906
3249.399309	495742.069144	40.159924
3252.255832	496452.982773	40.164941
3255.369603	497175.038612	40.169959
3258.988042	497884.412212	40.174976
3261.872439	498600.084881	40.179994
3265.551310	499313.987687	40.185012
3268.983103	500021.741308	40.190029
3271.694984	500737.608464	40.195047
3275.076859	501455.713785	40.200064
3278.212726	502184.279279	40.205082
3281.489775	502906.431692	40.210100
3284.638852	503630.997856	40.215117
3287.690337	504359.840270	40.220135
3291.100074	505077.390030	40.225152
3294.259952	505801.107688	40.230170
3297.447580	506495.517121	40.235188
3301.026941	507183.427145	40.240205
3304.149743	507860.329528	40.245223
3307.473851	508539.999641	40.250240
3310.582805	509224.269172	40.255258
3314.327968	509911.842233	40.260276
3317.541174	510598.563498	40.265293
3320.669599	511295.967619	40.270311
3324.281632	511971.974258	40.275328
3327.214094	512666.426635	40.280346
3330.190981	513367.452651	40.285364
3333.482867	514062.345732	40.290381
3336.562556	514768.644794	40.295399
3340.409557	515475.902545	40.300416
3343.476944	516198.588384	40.305434
3346.744180	516900.479950	40.310452
3350.149828	517638.736890	40.315469
3353.100992	518370.778608	40.320487
3356.861084	519100.138213	40.325504
3359.727057	519846.098168	40.330522
3362.969758	520588.989255	40.335540
3366.798371	521338.612079	40.340557
3369.856828	522080.909664	40.345575
3373.500553	522832.207337	40.350592
3377.045196	523600.074169	40.355610
3380.463313	524352.597348	40.360628
3383.766527	525107.473034	40.365645
3386.912997	525881.091757	40.370663
3390.673058	526653.719044	40.375680
3394.298627	527421.490912	40.380698
3397.921293	528183.731864	40.385716
3401.293908	528943.959508	40.390733
3404.630168	529710.204434	40.395751
3408.413688	530480.927623	40.400768
3411.312689	531259.513805	40.405786
3415.048372	532025.431302	40.410804
3418.554271	532807.170348	40.415821
3421.773499	533578.585703	40.420839
3425.647641	534346.584006	40.425856
3428.759194	535135.674669	40.430874
3432.134016	535917.226873	40.435892
3435.547149	536701.453663	40.440909
3438.947005	537480.705513	40.445927
3442.713403	538262.277528	40.450944
3446.016428	539048.768582	40.455962
3449.559466	539821.682222	40.460980
3453.396231	540617.678059	40.465997
3456.691540	541396.745132	40.471015
3460.520080	542187.874694	40.476032
3464.217350	542963.170905	40.481050
3467.275130	543749.757105	40.486068
3471.102184	544530.389614	40.491085
3474.589384	545316.120088	40.496103
3478.012700	546081.075943	40.501120
3481.186385	546862.700999	40.506125
3484.425996	547573.742580	40.511130
3488.078877	548251.122916	40.516135
3490.845634	548857.706963	40.521140
3494.975029	549376.040581	40.526144
3498.255849	549874.557080	40.531149
3500.545286	550276.176264	40.536154
3503.131767	550648.066878	40.541159
3505.106675	550935.828641	40.546164
3507.540367	551179.512651	40.551168
3509.494563	551377.856622	40.556173
3511.422961	551510.254692	40.561178
3512.866410	551597.619910	40.566183
3513.909194	551660.980171	40.571188
3515.801922	551689.895467	40.576192
3516.681063	551665.739364	40.581197
3517.728826	551609.869778	40.586202
3518.656296	551534.340777	40.591207
3519.338937	551419.897027	40.596212
3520.388914	551280.619518	40.601216
3520.556836	551127.250822	40.606221
3520.958191	550947.150801	40.611226
3521.710574	550746.355044	40.616231
3521.948783	550551.693031	40.621236
3522.355363	550309.871062	40.626240
3522.348470	550075.427425	40.631245
3522.810607	549835.203568	40.636250
3522.789069	549568.508251	40.641255
3522.574461	549308.853165	40.646260
3523.026447	549040.963130	40.651264
3522.905529	548769.121407	40.656269
3522.798142	548485.008874	40.661274
3523.070613	548189.374419	40.666279
3522.923744	547914.442333	40.671284
3522.733250	547613.822489	40.676288
3522.875521	547311.629744	40.681293
3522.646350	547009.792331	40.686298
3522.527973	546710.051108	40.691303
3521.951910	546418.855871	40.696308
3522.107937	546109.115540	40.701312
3521.645891	545823.998100	40.706317
3521.438482	545534.140487	40.711322
3521.683898	545218.410994	40.716327
3521.427486	544927.792073	40.721332
3521.395674	544639.958877	40.726336
3521.159989	544350.536911	40.731341
3520.821262	544047.596224	40.736346
3520.610282	543754.927864	40.741351
3520.030054	543478.618675	40.746356
3520.123373	543185.083274	40.751360
3519.495749	542912.860435	40.756365
3519.548487	542634.920985	40.761370
3519.240968	542360.668483	40.766375
3519.146426	542104.906886	40.771380
3519.038870	541824.554248	40.776384
3518.562218	541559.705011	40.781389
3518.407202	541302.525546	40.786394
3518.182644	541034.244239	40.791399
3517.643669	540786.609308	40.796404
3517.457930	540520.281965	40.801408
3517.197833	540284.965894	40.806413
3517.010073	540051.452584	40.811418
3517.115382	539799.255947	40.816423
3516.433379	539573.387928	40.821428
3516.662108	539337.373871	40.826432
3515.936328	539107.263938	40.831437
3515.418412	538891.358682	40.836442
3515.648428	538660.989906	40.841447
3515.224699	538454.608208	40.846452
3515.133456	538233.424505	40.851456
3515.302357	538028.559428	40.856461
3514.708244	537813.862985	40.861466
3514.720806	537607.249329	40.866471
3514.126803	537412.647929	40.871476
3514.200238	537208.746527	40.876480
3513.732630	537013.160450	40.881485
3513.291169	536825.749861	40.886490
3513.498999	536643.234592	40.891495
3513.018882	536471.988178	40.896500
3513.197463	536290.432985	40.901504
3512.741028	536107.359719	40.906509
3512.815222	535945.667081	40.911514
3512.212025	535758.370025	40.916519
3512.402755	535609.990182	40.921524
3512.239658	535427.114998	40.926528
3511.976081	535283.501385	40.931533
3511.741974	535111.695799	40.936538
3511.790679	534953.179051	40.941543
3511.558296	534808.192225	40.946548
3511.407208	534647.632861	40.951552
3511.238713	534506.169083	40.956557
3511.123415	534356.259596	40.961562
3511.322955	534199.277232	40.966567
3511.034239	534065.910911	40.971572
3510.772197	533917.131713	40.976576
3510.755357	533788.620125	40.981581
3510.219949	533645.792001	40.986586
3510.466274	533504.000907	40.991591
3510.267782	533382.991301	40.996596
3510.097851	533251.619922	41.001600
3510.243901	533125.047315	41.006605
3509.388599	533001.713640	41.011610
3509.772885	532877.475772	41.016615
3510.127061	532748.543290	41.021620
3509.681562	532616.654378	41.026624
3509.506853	532505.182583	41.031629
3509.362342	532382.135811	41.036634
3509.453016	532266.679688	41.041639
3509.097236	532158.669518	41.046644
3509.077126	532043.027162	41.051648
3508.865661	531922.058765	41.056653
3508.777529	531822.138149	41.061658
3508.772078	531725.740476	41.066663
3508.466946	531629.288529	41.071668
3508.611759	531515.030863	41.076672
3508.539611	531420.006001	41.081677
3508.435115	531327.158244	41.086682
3508.580265	531207.643694	41.091687
3508.047280	531125.725394	41.096692
3508.065978	531015.526057	41.101696
3508.075131	530938.775775	41.106701
3507.932520	530834.057478	41.111706
3508.054527	530749.608410	41.116711
3507.975067	530656.803249	41.121716
3507.698896	530562.361230	41.126720
3507.574353	530476.787536	41.131725
3507.302723	530390.023956	41.136730
3507.285691	530311.809438	41.141735
3506.934446	530232.384148	41.146740
3507.227146	530155.130460	41.151744
3507.066976	530067.842196	41.156749
3506.990443	530011.110361	41.161754
3507.145662	529925.388385	41.166759
3506.600960	529855.541819	41.171764
3506.651986	529779.587728	41.176768
3506.598431	529716.838147	41.181773
3506.808937	529643.233102	41.186778
3507.190520	529578.140327	41.191783
3506.804265	529500.182258	41.196788
3506.924498	529430.127639	41.201792
3506.745271	529372.348585	41.206797
3506.542063	529286.982979	41.211802
3506.564078	529221.440254	41.216807
3506.528971	529150.044591	41.221812
3506.317777	529084.689755	41.226816
3506.431886	529026.762005	41.231821
3506.350187	528965.833047	41.236826
3506.465272	528893.452367	41.241831
3506.183843	528832.301801	41.246836
3506.528608	528770.142423	41.251840
3506.325303	528711.505694	41.256845
3506.368089	528650.252642	41.261850
3506.550591	528577.303992	41.266855
3506.330432	528516.041450	41.271860
3506.207668	528454.359004	41.276864
3506.245092	528394.268093	41.281869
3506.110199	528334.507399	41.286874
3506.246044	528272.126417	41.291879
3506.033763	528216.016004	41.296884
3506.179755	528143.323800	41.301888
3506.246236	528087.623685	41.306893
3505.734827	528039.493961	41.311898
3505.725730	527979.004546	41.316903
3505.485617	527934.369111	41.321908
3505.745565	527875.403382	41.326912
3505.921280	527825.395638	41.331917
3506.117412	527779.579018	41.336922
3506.103126	527717.775486	41.341927
3505.820442	527664.858046	41.346932
3505.827416	527600.271183	41.351936
3506.040743	527554.350122	41.356941
3506.170869	527493.988464	41.361946
3505.929686	527427.873474	41.366951
3505.825679	527382.709601	41.371956
3505.551541	527326.656357	41.376960
3505.894909	527269.140787	41.381965
3505.687065	527224.346641	41.386970
3505.856826	527162.158092	41.391975
3505.545246	527110.304673	41.396980
3505.508927	527060.681810	41.401984
3505.818718	527018.281650	41.406989
3505.700231	526964.678922	41.411994
3505.993566	526911.769002	41.416999
3505.474557	526860.604565	41.422004
3505.669100	526799.472004	41.427008
3505.518147	526753.606215	41.432013
3505.500735	526702.867380	41.437018
3505.810069	526655.462903	41.442023
3505.439600	526613.725133	41.447028
3505.277795	526554.871719	41.452032
3505.362628	526513.769280	41.457037
3505.547135	526471.640174	41.462042
3505.332234	526419.819766	41.467047
3505.307317	526380.452711	41.472052
3505.452780	526330.394515	41.477056
3505.732989	526283.448406	41.482061
3505.238532	526240.971143	41.487066
3505.559388	526187.498522	41.492071
3505.130808	526141.725399	41.497076
3505.088504	526087.248475	41.502080
3505.160711	526045.338162	41.507085
3505.244352	526006.357360	41.512090
3505.361954	525965.602125	41.517095
3505.005700	525930.178067	41.522100
3505.428418	525881.540362	41.527104
3505.001014	525840.314991	41.532109
3504.884805	525802.881554	41.537114
3505.108841	525754.022155	41.542119
3505.138396	525719.143157	41.547124
3504.963761	525674.036152	41.552128
3504.965811	525630.518470	41.557133
3504.739215	525591.990041	41.562138
3504.991395	525554.598879	41.567143
3504.827604	525523.439676	41.572148
3504.642684	525485.056032	41.577152
3504.728960	525440.816912	41.582157
3504.805146	525421.042436	41.587162
3504.895493	525379.178056	41.592167
3504.940815	525336.865788	41.597172
3504.706146	525302.027647	41.602176
3504.963684	525266.959996	41.607181
3504.879820	525230.834258	41.612186
3505.010592	525191.641847	41.617191
3504.595284	525160.572239	41.622196
3504.588954	525123.423113	41.627200
3504.665658	525088.939649	41.632205
3504.455672	525071.130676	41.637210
3504.783515	525034.282336	41.642215
3504.800709	524994.399767	41.647220
3504.966985	524950.146650	41.652224
3504.690967	524922.895997	41.657229
3504.748444	524885.584600	41.662234
3505.026165	524847.783393	41.667239
3504.445703	524821.389418	41.672244
3504.753331	524765.487959	41.677248
3504.783320	524735.964605	41.682253
3504.670896	524711.467757	41.687258
3505.099455	524671.064450	41.692263
3504.978069	524633.881833	41.697268
3504.812190	524594.178848	41.702272
3504.913841	524557.971727	41.707277
3504.789520	524517.958706	41.712282
3504.921506	524481.038965	41.717287
3504.710830	524450.036728	41.722292
3504.813373	524412.161095	41.727296
3504.860397	524373.283209	41.732301
3504.557212	524339.414202	41.737306
3504.323926	524306.595567	41.742311
3504.730897	524275.798648	41.747316
3504.790134	524235.503174	41.752320
3504.648389	524207.016944	41.757325
3504.532989	524172.157500	41.762330
3504.737440	524128.603756	41.767335
3504.427436	524108.231589	41.772340
3504.502131	524076.475855	41.777344
3504.796863	524039.478830	41.782349
3504.598465	524011.708883	41.787354
3505.022241	523968.423327	41.792359
3504.804252	523942.172805	41.797364
3504.552674	523897.831200	41.802368
3504.807227	523867.916920	41.807373
3504.624227	523832.005905	41.812378
3504.672175	523797.423123	41.817383
3504.500524	523771.215546	41.822388
3504.539344	523748.563635	41.827392
3504.775964	523707.531118	41.832397
3504.635098	523679.296562	41.837402
3504.570397	523644.832358	41.842407
3504.517919	523617.796906	41.847412
3504.632037	523582.950458	41.852416
3504.708207	523546.745095	41.857421
3504.453500	523520.752438	41.862426
3504.845168	523478.329990	41.867431
3504.707891	523453.835158	41.872436
3504.363549	523415.876175	41.877440
3504.472152	523371.981692	41.882445
3504.578409	523344.617392	41.887450
3504.866104	523313.534193	41.892455
3504.690292	523286.669333	41.897460
3504.602959	523253.269429	41.902464
3504.813733	523215.323330	41.907469
3504.355283	523187.289766	41.912474
3504.591910	523145.295359	41.917479
3504.526560	523112.447748	41.922484
3504.389028	523091.187667	41.927488
3504.714033	523064.647683	41.932493
3504.379098	523025.725826	41.937498
3504.595010	522995.816042	41.942503
3504.736346	522965.614683	41.947508
3504.647521	522918.969851	41.952512
3504.452621	522885.586191	41.957517
3504.170607	522871.223682	41.962522
3504.675460	522830.399302	41.967527
3504.587732	522801.396536	41.972532
3504.485560	522773.710354	41.977536
3504.443052	522739.796785	41.982541
3503.867770	522711.578654	41.987546
3504.503294	522681.298650	41.992551
3504.297999	522645.944600	41.997556
3504.416591	522621.408062	42.002560
3504.738130	522605.180578	42.007565
3504.633447	522565.159614	42.012570
3504.551332	522525.438302	42.017575
3504.458787	522499.620582	42.022580
3504.367516	522469.657279	42.027584
3504.641235	522440.445075	42.032589
3504.173071	522412.260044	42.037594
3504.136505	522370.610133	42.042599
3504.006964	522352.431567	42.047604
3504.087193	522338.870733	42.052608
3504.293923	522317.807986	42.057613
3503.695800	522296.670220	42.062618
3504.114612	522262.480520	42.067623
3504.147113	522244.023451	42.072628
3503.969448	522216.803234	42.077632
3504.140276	522194.128282	42.082637
3504.206128	522174.503125	42.087642
3504.373277	522148.542690	42.092647
3504.263180	522123.687672	42.097652
3504.217083	522092.048248	42.102656
3504.252465	522063.530245	42.107661
3504.049600	522042.531886	42.112666
3504.230288	522012.828077	42.117671
3504.181630	521993.928564	42.122676
3504.230924	521957.622792	42.127680
3504.113525	521933.071963	42.132685
3503.949041	521918.791141	42.137690
3504.189800	521888.572063	42.142695
3504.262871	521869.400390	42.147700
3504.620017	521834.663436	42.152704
3504.472692	521801.977795	42.157709
3503.937883	521781.739339	42.162714
3504.372969	521745.675443	42.167719
3504.510561	521730.638934	42.172724
3504.277422	521705.196062	42.177728
3504.103112	521663.717780	42.182733
3504.172678	521657.134714	42.187738
3504.221923	521621.535977	42.192743
3504.307025	521601.856531	42.197748
3504.034624	521571.667425	42.202752
3504.289940	521545.338202	42.207757
3504.073772	521528.992417	42.212762
3504.269564	521489.376312	42.217767
3504.269779	521475.220734	42.222772
3504.115781	521444.102667	42.227776
3504.442593	521421.149203	42.232781
3504.243565	521384.527512	42.237786
3504.543590	521351.214134	42.242791
3504.180505	521336.913637	42.247796
3504.366945	521302.606985	42.252800
3504.889408	521277.499017	42.257805
3504.020877	521249.324695	42.262810
3504.322043	521212.067427	42.267815
3504.356275	521185.924242	42.272820
3504.542513	521157.936934	42.277824
3504.456762	521122.459560	42.282829
3504.152261	521099.453764	42.287834
3504.404562	521065.035088	42.292839
3504.239671	521035.232452	42.297844
3504.189090	521022.095658	42.302848
3504.110989	520983.886671	42.307853
3504.066803	520965.490834	42.312858
3504.287597	520929.762355	42.317863
3504.395937	520904.618159	42.322868
3504.298924	520886.837277	42.327872
3504.351191	520865.645398	42.332877
3503.940426	520841.948225	42.337882
3504.218690	520803.631928	42.342887
3504.134213	520789.640817	42.347892
3504.135545	520754.806135	42.352896
3504.443969	520724.270858	42.357901
3503.960073	520708.219361	42.362906
3504.157167	520683.718056	42.367911
3504.368369	520664.422016	42.372916
3504.060661	520624.125022	42.377920
3504.109979	520603.287180	42.382925
3504.084347	520573.866159	42.387930
3504.050651	520542.424003	42.392935
3503.803781	520534.626531	42.397940
3504.038846	520509.866170	42.402944
3504.382819	520469.769139	42.407949
3504.114215	520459.143754	42.412954
3504.195503	520425.306915	42.417959
3504.107830	520396.856010	42.422964
3504.035531	520378.969550	42.427968
3503.861451	520357.711672	42.432973
3503.849788	520345.731051	42.437978
3504.463467	520312.467100	42.442983
3504.379864	520294.936252	42.447988
3504.249799	520266.795179	42.452992
3504.352167	520233.611890	42.457997
3503.619477	520206.577168	42.463002
3504.094878	520195.176727	42.468007
3503.750544	520180.316090	42.473012
3503.824169	520163.468089	42.478016
3504.156941	520126.102234	42.483021
3503.896701	520115.778664	42.488026
3504.267732	520082.148119	42.493031
3504.277006	520070.720152	42.498036
3503.939404	520035.533031	42.503040
3504.135441	520015.480218	42.508045
3504.192668	519991.202229	42.513050
3504.341867	519960.791820	42.518055
3504.185960	519939.530527	42.523060
3503.796364	519910.974819	42.528064
3503.997000	519886.168398	42.533069
3503.591182	519868.586904	42.538074
3504.166729	519827.592162	42.543079
3504.165080	519829.867816	42.548084
3503.888050	519794.670603	42.553088
3504.179905	519772.782143	42.558093
3503.858727	519753.215255	42.563098
3503.927199	519727.721626	42.568103
3503.383021	519721.689850	42.573108
3503.819115	519704.025661	42.578112
3504.199551	519677.977028	42.583117
3503.877033	519655.376539	42.588122
3503.992703	519622.291035	42.593127
3503.917521	519611.937895	42.598132
3504.043844	519589.923671	42.603136
3504.329751	519558.378547	42.608141
3504.145208	519542.531395	42.613146
3504.066772	519518.122464	42.618151
3503.754520	519483.132399	42.623156
3504.016380	519469.034853	42.628160
3504.321283	519453.009124	42.633165
3504.001196	519430.205691	42.638170
3503.961541	519403.363467	42.643175
3504.113216	519395.148516	42.648180
3503.740800	519367.145333	42.653184
3504.103474	519340.795599	42.658189
3504.033025	519316.941296	42.663194
3503.976910	519298.899412	42.668199
3503.965444	519271.749140	42.673204
3503.983107	519251.723591	42.678208
3504.237784	519229.840286	42.683213
3503.969361	519213.247630	42.688218
3503.872568	519177.413848	42.693223
3503.666951	519154.895318	42.698228
3503.840559	519139.395669	42.703232
3503.893121	519119.971203	42.708237
3503.874658	519108.799767	42.713242
3503.670781	519088.707911	42.718247
3503.641872	519073.745847	42.723252
3503.662570	519045.326032	42.728256
3504.094858	519022.352542	42.733261
3503.657322	519018.022810	42.738266
3504.150086	518981.893157	42.743271
3504.005664	518965.381777	42.748276
3503.824598	518939.521861	42.753280
3503.839468	518925.311200	42.758285
3503.739889	518902.876691	42.763290
3504.006579	518879.878615	42.768295
3503.947663	518858.802847	42.773300
3504.177574	518833.939649	42.778304
3504.031278	518815.203591	42.783309
3503.903219	518803.644758	42.788314
3503.812114	518764.573063	42.793319
3504.071313	518746.278474	42.798324
3503.809574	518738.229674	42.803329
3504.299673	518711.201454	42.808333
3504.006527	518691.881693	42.813338
3504.016320	518670.491436	42.818343
3503.505237	518644.379834	42.823348
3503.587321	518621.360014	42.828353
3503.571285	518613.474573	42.833357
3503.266630	518597.038717	42.838362
3503.419567	518570.771471	42.843367
3503.476494	518565.301594	42.848372
3503.366998	518572.448709	42.853377
3503.525282	518535.865301	42.858381
3503.604363	518527.206308	42.863386
3503.520589	518512.151276	42.868391
3503.252875	518502.080697	42.873396
3503.189685	518483.685081	42.878401
3503.406308	518465.346346	42.883405
3503.137626	518476.361628	42.888410
3503.285463	518475.225965	42.893415
3503.174552	518447.179879	42.898420
3503.169278	518432.162931	42.903425
3503.307945	518424.354077	42.908429
3503.299940	518429.614290	42.913434
3503.383796	518417.516034	42.918439
3503.415882	518399.054698	42.923444
3503.151362	518381.297579	42.928449
3503.592888	518378.497388	42.933453
3503.689870	518366.447586	42.938458
3503.369564	518346.828319	42.943463
3503.668029	518337.072669	42.948468
3503.485779	518331.994481	42.953473
3503.293194	518306.185957	42.958477
3503.055438	518293.127131	42.963482
3503.579690	518288.392346	42.968487
3503.468787	518280.268913	42.973492
3503.384106	518258.994188	42.978497
3503.832721	518241.023060	42.983501
3503.263099	518244.753994	42.988506
3503.632667	518211.119863	42.993511
3503.786510	518198.353026	42.998516
3503.706530	518184.510682	43.003521
3503.494371	518159.564648	43.008525
3503.676446	518149.271056	43.013530
3503.760649	518140.762750	43.018535
3503.620634	518118.839229	43.023540
3503.386635	518111.797064	43.028545
3503.502241	518092.411989	43.033549
3503.377000	518072.154764	43.038554
3503.573592	518058.218030	43.043559
3503.602616	518054.522225	43.048564
3503.513176	518037.293292	43.053569
3503.960617	518012.242773	43.058573
3503.621197	518014.622635	43.063578
3503.626592	517987.872119	43.068583
3503.899513	517984.542279	43.073588
3503.708003	517975.774069	43.078593
3504.066015	517929.904019	43.083597
3503.732482	517927.479101	43.088602
3503.847177	517896.817504	43.093607
3504.200962	517882.350105	43.098612
3503.957043	517852.048513	43.103617
3504.141604	517836.090807	43.108621
3503.657902	517820.390419	43.113626
3503.857080	517790.827752	43.118631
3503.972074	517766.992462	43.123636
3503.700516	517766.226449	43.128641
3503.930877	517740.046781	43.133645
3503.648746	517722.392872	43.138650
3503.364808	517710.959048	43.143655
3503.531367	517677.659330	43.148660
3503.830231	517667.296410	43.153665
3503.936033	517652.008357	43.158669
3503.621863	517646.192293	43.163674
3503.708029	517627.114734	43.168679
3503.740399	517597.780361	43.173684
3503.623140	517581.566710	43.178689
3503.878977	517558.871923	43.183693
3504.098789	517547.408926	43.188698
3503.633642	517519.417260	43.193703
3503.367712	517502.215668	43.198708
3503.370531	517492.657959	43.203713
3503.859151	517478.624011	43.208717
3503.651984	517468.897207	43.213722
3503.577713	517446.406151	43.218727
3503.762048	517440.915763	43.223732
3503.212605	517413.442926	43.228737
3503.408333	517394.802898	43.233741
3503.707294	517391.569962	43.238746
3503.630914	517374.489981	43.243751
3503.709771	517357.941699	43.248756
3503.641008	517349.254891	43.253761
3503.944183	517316.539678	43.258765
3503.661798	517304.650208	43.263770
3503.712320	517291.797867	43.268775
3503.642258	517266.726887	43.273780
3503.433828	517265.242905	43.278785
3503.338030	517244.676600	43.283789
3503.639894	517225.969036	43.288794
3503.380589	517206.642187	43.293799
3503.469687	517210.016379	43.298804
3503.523037	517192.561720	43.303809
3503.552679	517167.677107	43.308813
3503.449484	517164.962819	43.313818
3503.289048	517147.086782	43.318823
3503.590290	517123.625682	43.323828
3503.531216	517121.460677	43.328833
3503.859477	517108.008027	43.333837
3503.733727	517086.940566	43.338842
3503.728682	517075.057661	43.343847
3503.865015	517052.431641	43.348852
3503.680892	517032.789288	43.353857
3503.827435	517011.779829	43.358861
3503.644340	516992.794672	43.363866
3503.965718	516980.910673	43.368871
3503.971640	516953.045866	43.373876
3503.685161	516940.398232	43.378881
3503.788593	516917.625520	43.383885
3503.793159	516897.194629	43.388890
3503.769008	516886.730573	43.393895
3503.908968	516854.495381	43.398900
3503.681552	516846.339090	43.403905
3504.019676	516816.044740	43.408909
3503.908949	516809.235385	43.413914
3504.047728	516784.484658	43.418919
3503.971544	516749.704336	43.423924
3503.801490	516740.072380	43.428929
3503.917090	516711.835838	43.433933
3503.661173	516708.892762	43.438938
3503.772388	516681.921130	43.443943
3503.706600	516662.714770	43.448948
3503.867305	516653.789042	43.453953
3504.069867	516623.212345	43.458957
3503.457724	516605.305984	43.463962
3503.605636	516583.486632	43.468967
3503.930502	516565.684970	43.473972
3503.766236	516553.928003	43.478977
3503.846970	516533.585768	43.483981
3503.952490	516531.698095	43.488986
3504.013801	516501.548072	43.493991
3503.822808	516477.759299	43.498996
3503.540116	516464.756704	43.504001
3503.900030	516436.885649	43.509005
3503.783851	516421.884411	43.514010
3503.925752	516405.375788	43.519015
3503.816766	516378.843045	43.524020
3503.640084	516365.014468	43.529025
3503.979129	516348.828629	43.534029
3503.698099	516325.711304	43.539034
3503.568856	516301.710232	43.544039
3503.990854	516286.724946	43.549044
3503.669745	516271.806538	43.554049
3504.138186	516244.676587	43.559053
3503.875310	516230.760379	43.564058
3503.713970	516210.456014	43.569063
3503.749761	516183.849503	43.574068
3503.700365	516174.299290	43.579073
3503.762507	516148.902293	43.584077
3503.771155	516125.132031	43.589082
3503.723629	516125.089113	43.594087
3503.860491	516095.330992	43.599092
3503.538512	516076.670177	43.604097
3503.851347	516059.375604	43.609101
3503.537034	516036.060847	43.614106
3503.355830	516029.717468	43.619111
3503.689958	516020.662843	43.624116
3503.543092	515992.668862	43.629121
3503.906357	515977.439719	43.634125
3503.786324	515959.100861	43.639130
3503.700680	515941.818581	43.644135
3503.755713	515928.458744	43.649140
3503.402756	515909.903785	43.654145
3503.706589	515888.210596	43.659149
3503.454451	515887.137984	43.664154
3503.346350	515858.631918	43.669159
3503.209555	515834.681940	43.674164
3503.582110	515843.979256	43.679169
3503.740141	515835.306380	43.684173
3503.607728	515805.033999	43.689178
3503.772198	515793.881986	43.694183
3503.776835	515778.405910	43.699188
3503.630123	515754.609105	43.704193
3503.927154	515741.008572	43.709197
3503.577694	515729.179148	43.714202
3503.403316	515711.860082	43.719207
3503.708775	515695.931789	43.724212
3503.713420	515669.683397	43.729217
3503.714113	515652.589465	43.734221
3503.725072	515646.519007	43.739226
3504.053677	515611.975769	43.744231
3504.015599	515600.147607	43.749236
3503.847044	515581.917153	43.754241
3503.721655	515561.252296	43.759245
3504.108426	515541.416792	43.764250
3503.990813	515528.589668	43.769255
3503.843919	515495.891451	43.774260
3503.650915	515484.644014	43.779265
3504.175601	515460.892387	43.784269
3503.706362	515450.497783	43.789274
3503.737310	515426.166683	43.794279
3503.684627	515400.078653	43.799284
3503.544056	515387.861946	43.804289
3503.519997	515375.677387	43.809293
3503.521747	515352.868036	43.814298
3503.805284	515338.510687	43.819303
3503.619012	515311.685014	43.824308
3503.475411	515303.110117	43.829313
3503.708714	515278.797391	43.834317
3503.486247	515272.005069	43.839322
3503.420181	515257.652337	43.844327
3503.520079	515246.560742	43.849332
3503.149840	515242.168797	43.854337
3503.321795	515206.385105	43.859341
3503.610924	515207.603925	43.864346
3503.500133	515189.819089	43.869351
3503.821571	515182.586729	43.874356
3503.756196	515165.603893	43.879361
3503.449028	515153.615649	43.884365
3503.389737	515127.730542	43.889370
3503.053285	515111.700859	43.894375
3503.415846	515108.609159	43.899380
3503.399164	515108.662513	43.904385
3503.487184	515087.407005	43.909389
3503.266834	515084.053413	43.914394
3503.094781	515079.984126	43.919399
3503.279664	515073.026183	43.924404
3502.975312	515071.961769	43.929409
3503.739139	515043.114184	43.934413
3503.494950	515035.060807	43.939418
3503.467683	515021.409800	43.944423
3503.717360	514996.335439	43.949428
3503.394716	514979.949416	43.954433
3503.342370	514980.564743	43.959437
3503.662359	514968.881839	43.964442
3503.242457	514946.391465	43.969447
3503.328161	514935.605364	43.974452
3503.504484	514932.441919	43.979457
3503.674433	514906.975418	43.984461
3503.621310	514896.110084	43.989466
3503.134648	514898.513656	43.994471
3503.502755	514868.666224	43.999476
3503.299607	514853.171560	44.004481
3503.265496	514837.549009	44.009485
3503.376581	514825.646146	44.014490
3503.258799	514821.618794	44.019495
3503.604034	514796.680759	44.024500
3503.353050	514795.759621	44.029505
3503.461644	514781.935214	44.034509
3503.226439	514776.409117	44.039514
3503.433238	514760.293225	44.044519
3503.322629	514739.068673	44.049524
3503.206445	514738.631990	44.054529
3503.404650	514738.701955	44.059533
3503.640537	514718.383563	44.064538
3503.690767	514706.287927	44.069543
3503.614335	514694.667495	44.074548
3503.187872	514678.955086	44.079553
3503.193428	514651.642841	44.084557
3503.339541	514661.027189	44.089562
3503.527022	514653.613469	44.094567
3503.620934	514624.061829	44.099572
3503.242301	514609.606219	44.104577
3503.200972	514605.870192	44.109581
3503.337208	514600.791094	44.114586
3503.489880	514587.263022	44.119591
3503.275056	514563.829329	44.124596
3503.460512	514563.597847	44.129601
3503.521271	514543.458657	44.134605
3503.265422	514524.279881	44.139610
3503.393312	514519.505541	44.144615
3503.476225	514508.517297	44.149620
3503.431052	514503.011648	44.154625
3503.618839	514479.311887	44.159629
3503.523170	514471.841690	44.164634
3503.461243	514449.951570	44.169639
3503.308129	514432.374930	44.174644
3503.219791	514431.832682	44.179649
3503.315632	514412.648764	44.184653
3503.236269	514415.594953	44.189658
3503.467452	514395.125180	44.194663
3503.486994	514379.847766	44.199668
3503.220111	514376.754275	44.204673
3503.224390	514375.742186	44.209677
3503.329964	514343.709899	44.214682
3503.326540	514341.080535	44.219687
3503.368227	514334.650700	44.224692
3503.372143	514340.517253	44.229697
3503.808731	514320.824168	44.234701
3503.814942	514298.214989	44.239706
3503.412668	514286.038844	44.244711
3503.772565	514258.821684	44.249716
3503.710194	514248.362017	44.254721
3503.714883	514234.705318	44.259725
3503.309363	514216.055630	44.264730
3503.456674	514192.614754	44.269735
3503.548214	514188.807053	44.274740
3503.401308	514170.369326	44.279745
3503.726005	514140.476885	44.284749
3503.715477	514147.660829	44.289754
3503.253202	514122.293075	44.294759
3503.402991	514109.017967	44.299764
3503.531530	514100.095965	44.304769
3503.514803	514079.968468	44.309773
3503.268133	514070.296501	44.314778
3503.681981	514067.651714	44.319783
3503.758147	514046.953129	44.324788
3503.349533	514035.839957	44.329793
3503.622717	514019.763442	44.334797
3503.681342	514017.731164	44.339802
3503.390896	513983.889375	44.344807
3503.600564	513973.234798	44.349812
3503.555184	513957.916684	44.354817
3503.712748	513926.532913	44.359821
3503.562248	513931.260699	44.364826
3503.557771	513915.986660	44.369831
3503.809885	513873.612171	44.374836
3503.394811	513885.260568	44.379841
3503.416882	513865.834791	44.384845
3503.732472	513847.525920	44.389850
3503.636739	513831.608699	44.394855
3503.530305	513830.007124	44.399860
3503.491592	513803.003974	44.404865
3503.450443	513793.299361	44.409869
3503.649065	513779.763377	44.414874
3503.256826	513754.282837	44.419879
3504.008367	513734.235805	44.424884
3503.627428	513729.288774	44.429889
3503.446128	513713.283807	44.434893
3503.340026	513695.041427	44.439898
3503.384285	513685.980789	44.444903
3503.651926	513678.301071	44.449908
3503.297937	513656.253765	44.454913
3503.418655	513632.917473	44.459917
3503.559866	513648.777397	44.464922
3503.304795	513630.002116	44.469927
3503.500825	513613.431609	44.474932
3503.366979	513610.013465	44.479937
3503.275607	513594.449390	44.484941
3503.302805	513569.155170	44.489946
3503.331617	513561.664891	44.494951
3503.275680	513564.556945	44.499956
3503.204711	513563.961343	44.504961
3503.330560	513541.079335	44.509965
3503.359732	513535.258136	44.514970
3503.033685	513520.236890	44.519975
3503.268426	513512.410557	44.524980
3503.382975	513509.812994	44.529985
3503.238692	513489.300311	44.534989
3503.171622	513471.405583	44.539994
3503.096817	513468.079238	44.544999
3503.137878	513461.649169	44.550004
3503.255109	513472.707903	44.555009
3503.401434	513436.519852	44.560013
3503.171176	513431.093689	44.565018
3503.022924	513422.923209	44.570023
3503.416237	513422.911760	44.575028
3503.395885	513417.452413	44.580033
3503.385259	513401.369590	44.585037
3503.472352	513379.302780	44.590042
3503.273555	513369.875746	44.595047
3503.379800	513369.100382	44.600052
3503.233412	513347.980890	44.605057
3503.505648	513326.694039	44.610061
3503.323849	513326.318270	44.615066
3503.244008	513325.875805	44.620071
3503.650243	513293.945739	44.625076
3503.299986	513295.670419	44.630081
3503.424990	513284.826467	44.635085
3503.377881	513283.518949	44.640090
3503.347723	513254.945557	44.645095
3503.743601	513239.658202	44.650100
3503.321678	513252.825551	44.655105
3503.471896	513215.169558	44.660109
3503.496883	513209.045421	44.665114
3503.276135	513207.563019	44.670119
3503.737003	513181.137460	44.675124
3503.229021	513165.537680	44.680129
3503.234232	513143.180016	44.685133
3503.526107	513146.877047	44.690138
3503.600733	513135.788056	44.695143
3503.370468	513117.716422	44.700148
3503.156777	513110.921836	44.705153
3503.337049	513107.150448	44.710157
3503.238062	513095.532476	44.715162
3502.914379	513077.880219	44.720167
3503.272314	513057.742860	44.725172
3503.271413	513055.719876	44.730177
3503.527187	513055.578424	44.735181
3503.457994	513048.811554	44.740186
3503.212916	513028.820061	44.745191
3503.542050	513002.010391	44.750196
3503.305321	513001.643298	44.755201
3503.303703	512987.733677	44.760205
3503.218960	512962.759734	44.765210
3503.291757	512979.440414	44.770215
3503.314159	512953.184972	44.775220
3503.239743	512972.367448	44.780225
3503.431162	512942.848028	44.785229
3503.358745	512924.194833	44.790234
3503.227190	512908.130655	44.795239
3503.172053	512908.544170	44.800244
3502.968815	512918.187042	44.805249
3503.286068	512888.495890	44.810253
3503.342220	512872.806666	44.815258
3503.034015	512879.481799	44.820263
3502.925252	512865.589014	44.825268
3503.069505	512870.826909	44.830273
3503.206805	512872.676891	44.835277
3503.284930	512844.895005	44.840282
3503.034568	512831.328068	44.845287
3503.302235	512827.087562	44.850292
3502.892546	512827.101881	44.855297
3503.290646	512816.669702	44.860301
3503.549438	512806.259538	44.865306
3503.235311	512786.784497	44.870311
3503.596846	512777.015647	44.875316
3503.465064	512773.951084	44.880321
3503.237754	512750.769752	44.885325
3503.327494	512741.145009	44.890330
3503.249470	512747.126235	44.895335
3503.400250	512726.970646	44.900340
3503.084636	512735.063322	44.905345
3503.720836	512705.928426	44.910349
3503.610301	512692.187527	44.915354
3503.222598	512689.264568	44.920359
3503.300901	512665.326652	44.925364
3503.299456	512646.409017	44.930369
3503.340093	512629.862110	44.935373
3503.607602	512639.784810	44.940378
3503.455083	512619.727619	44.945383
3503.585133	512596.489587	44.950388
3503.251849	512603.826373	44.955393
3503.386872	512582.863774	44.960397
3503.467737	512554.726897	44.965402
3503.504558	512554.721218	44.970407
3503.458950	512548.608001	44.975412
3503.436551	512527.265551	44.980417
3503.310728	512514.538590	44.985421
3503.484973	512504.394521	44.990426
3503.218090	512511.113850	44.995431
3503.478824	512480.672168	45.000436
3503.445203	512471.269105	45.005441
3503.318604	512458.137556	45.010445
3503.566894	512448.133500	45.015450
3503.381812	512432.482000	45.020455
3503.597997	512408.471342	45.025460
3503.362696	512405.625410	45.030465
3503.409007	512391.555972	45.035469
3503.548000	512373.121670	45.040474
3503.372041	512357.569826	45.045479
3503.989375	512353.223346	45.050484
3503.678996	512341.992358	45.055489
3503.405478	512333.132977	45.060493
3503.561036	512312.065630	45.065498
3503.266734	512290.715278	45.070503
3503.321340	512274.519904	45.075508
3503.072464	512271.676095	45.080513
3503.338503	512270.217831	45.085517
3503.584008	512253.992261	45.090522
3503.179947	512235.036641	45.095527
3503.613031	512214.633482	45.100532
3503.488824	512222.240888	45.105537
3503.457383	512196.245705	45.110541
3503.876303	512185.911017	45.115546
3503.519466	512175.142520	45.120551
3503.636188	512145.835857	45.125556
3503.463957	512146.470236	45.130561
3503.261453	512138.864139	45.135565
3503.447872	512117.235243	45.140570
3503.307169	512101.424667	45.145575
3503.576473	512095.969692	45.150580
3503.543002	512085.706453	45.155585
3503.238299	512063.345767	45.160589
3503.454827	512041.661430	45.165594
3503.293839	512039.815384	45.170599
3503.357199	512034.089434	45.175604
3503.301623	512010.171755	45.180609
3503.594349	511999.603978	45.185613
3503.751261	511993.256209	45.190618
3503.452512	511982.124312	45.195623
3503.426274	511952.991669	45.200628
3503.072299	511963.518855	45.205633
3503.113942	511951.776698	45.210637
3503.283472	511937.383896	45.215642
3502.964172	511910.877341	45.220647
3503.199748	511904.314763	45.225652
3503.222542	511905.626515	45.230657
3503.219232	511898.393504	45.235661
3503.656682	511888.460389	45.240666
3503.231381	511875.426189	45.245671
3503.670134	511851.177221	45.250676
3503.325344	511852.850593	45.255681
3503.344253	511839.796735	45.260685
3503.517822	511815.488463	45.265690
3503.800835	511809.828888	45.270695
3503.761243	511788.589397	45.275700
3503.315854	511769.285690	45.280705
3503.328739	511769.789650	45.285709
3503.551128	511755.995365	45.290714
3502.979668	511743.237095	45.295719
3503.313758	511720.623225	45.300724
3503.108854	511724.247340	45.305729
3503.385735	511718.386361	45.310733
3503.304136	511711.115059	45.315738
3503.361034	511683.536969	45.320743
3503.526416	511661.506132	45.325748
3503.141337	511670.116152	45.330753
3503.425166	511661.320076	45.335757
3503.373083	511637.806007	45.340762
3503.450702	511629.143683	45.345767
3503.500070	511613.606124	45.350772
3503.628815	511614.496463	45.355777
3503.402002	511579.172803	45.360781
3503.765270	511579.115523	45.365786
3503.594641	511561.184558	45.370791
3503.373410	511542.401607	45.375796
3503.428458	511540.723702	45.380801
3503.672313	511532.692672	45.385805
3503.586144	511494.058497	45.390810
3503.180872	511486.433572	45.395815
3503.634199	511485.350328	45.400820
3503.230899	511462.397397	45.405825
3503.248192	511441.350827	45.410829
3503.561238	511434.168784	45.415834
3503.216365	511437.865671	45.420839
3503.297118	511415.594960	45.425844
3503.520594	511404.582482	45.430849
3503.479730	511395.078794	45.435853
3503.603082	511388.634931	45.440858
3503.282291	511368.501685	45.445863
3503.216435	511350.351588	45.450868
3503.312440	511354.332911	45.455873
3503.103794	511341.162879	45.460877
3503.212480	511329.409695	45.465882
3503.145822	511309.944424	45.470887
3503.408456	511302.567947	45.475892
3503.103132	511302.666939	45.480897
3503.085616	511302.720436	45.485901
3503.338933	511290.792603	45.490906
3503.239340	511268.701969	45.495911
3503.179390	511248.881458	45.500916
3503.213276	511246.043366	45.505921
3503.303856	511245.270383	45.510925
3503.634331	511242.688931	45.515930
3503.365832	511225.278953	45.520935
3503.537597	511202.437119	45.525940
3503.269764	511212.495866	45.530945
3503.084061	511187.029394	45.535949
3503.621150	511173.893115	45.540954
3503.349938	511176.414906	45.545959
3503.469229	511153.024840	45.550964
3503.403795	511143.727245	45.555969
3503.137696	511129.959082	45.560973
3503.170421	511110.528462	45.565978
3503.005224	511108.733566	45.570983
3503.439300	511105.174554	45.575988
3503.274915	511090.125594	45.580993
3503.194263	511070.662261	45.585997
3503.354663	511059.659531	45.591002
3502.819016	511068.900706	45.596007
3503.127591	511063.742720	45.601012
3503.424630	511058.030092	45.606017
3503.402096	511033.094062	45.611021
3502.952808	511027.297045	45.616026
3503.005326	511028.502991	45.621031
3503.131663	511011.839786	45.626036
3503.033724	511020.151805	45.631041
3502.908115	511012.482459	45.636045
3503.213333	510993.109807	45.641050
3502.982383	510982.725355	45.646055
3503.168382	510973.438510	45.651060
3503.163180	510973.186535	45.656065
3503.340650	510966.379842	45.661069
3503.133469	510974.405625	45.666074
3503.118850	510953.616435	45.671079
3503.224255	510929.115321	45.676084
3503.136929	510928.623386	45.681089
3503.059411	510926.561671	45.686093
3503.085665	510914.720056	45.691098
3503.163558	510919.564340	45.696103
3503.238982	510900.936140	45.701108
3503.257406	510884.188692	45.706113
3503.052010	510870.208371	45.711117
3502.953941	510868.908721	45.716122
3502.842386	510882.028840	45.721127
3503.391807	510871.723318	45.726132
3503.416268	510866.711360	45.731137
3502.992737	510844.671381	45.736141
3503.613162	510836.580499	45.741146
3503.118558	510827.299983	45.746151
3503.518372	510823.442799	45.751156
3503.263250	510807.598518	45.756161
3503.169779	510780.346265	45.761165
3503.177142	510781.306424	45.766170
3503.386007	510788.001816	45.771175
3503.406183	510766.701014	45.776180
3503.076784	510753.600204	45.781185
3502.954842	510743.856026	45.786189
3503.391034	510728.863577	45.791194
3503.133960	510735.278522	45.796199
3503.231270	510727.472633	45.801204
3503.292796	510714.714708	45.806209
3503.352797	510694.773415	45.811213
3503.529447	510683.514930	45.816218
3502.965445	510693.317265	45.821223
3503.252527	510676.425969	45.826228
3503.472979	510665.565259	45.831233
3503.009890	510660.427952	45.836237
3503.288295	510649.406305	45.841242
3503.435535	510650.749072	45.846247
3503.491583	510625.091780	45.851252
3503.450311	510617.155979	45.856257
3503.199173	510598.123768	45.861261
3503.396989	510596.878504	45.866266
3503.045954	510586.816327	45.871271
3503.294820	510562.646133	45.876276
3503.202496	510556.438405	45.881281
3502.835968	510552.449352	45.886285
3503.223127	510554.158916	45.891290
3503.049719	510554.995894	45.896295
3503.085412	510539.611286	45.901300
3502.814009	510522.808118	45.906305
3502.901693	510513.131851	45.911309
3503.127208	510504.091452	45.916314
3503.001188	510507.804533	45.921319
3503.194359	510508.532979	45.926324
3503.285045	510502.852784	45.931329
3503.104378	510505.512128	45.936333
3503.358958	510480.278540	45.941338
3503.147076	510475.809719	45.946343
3503.426733	510460.993549	45.951348
3503.097477	510465.396427	45.956353
3503.076950	510459.885566	45.961357
3503.323376	510434.349662	45.966362
3503.001675	510425.092184	45.971367
3503.129410	510414.853046	45.976372
3502.989310	510413.003519	45.981377
3503.079149	510418.099006	45.986381
3503.272034	510413.566187	45.991386
3502.880910	510408.872734	45.996391
3503.044210	510382.085153	46.001396
3503.205165	510379.732727	46.006401
3503.271771	510366.872560	46.011405
3503.357298	510353.503494	46.016410
3503.100113	510370.845974	46.021415
3503.613661	510344.964175	46.026420
3503.524087	510326.361430	46.031425
3503.030207	510325.478433	46.036429
3503.233217	510320.792220	46.041434
3503.806321	510308.459024	46.046439
3503.547237	510286.594687	46.051444
3503.430068	510283.223823	46.056449
3503.367974	510267.601478	46.061453
3503.385433	510242.506201	46.066458
3503.390153	510234.815904	46.071463
3503.436434	510225.854280	46.076468
3503.409102	510209.771075	46.081473
3503.447544	510194.335131	46.086477
3503.354433	510186.154374	46.091482
3503.372129	510183.166894	46.096487
3503.762352	510162.515108	46.101492
3503.394116	510152.253031	46.106497
3503.384256	510142.288431	46.111501
3503.665074	510127.927103	46.116506
3503.377580	510110.822530	46.121511
3503.128892	510095.988380	46.126516
3503.317659	510092.316166	46.131521
3503.192733	510079.182515	46.136525
3503.352049	510054.317491	46.141530
3502.999172	510049.263759	46.146535
3503.413627	510039.990887	46.151540
3503.036260	510045.463881	46.156545
3502.723709	510038.481325	46.161549
3503.034190	510038.027663	46.166554
3502.952999	510024.128196	46.171559
3503.316188	510005.200579	46.176564
3503.195349	509995.051073	46.181569
3503.275577	509993.824353	46.186573
3503.561805	509989.934349	46.191578
3503.434381	509975.839788	46.196583
3503.502235	509951.596163	46.201588
3503.067135	509948.983762	46.206593
3502.918925	509949.614423	46.211597
3503.058694	509947.720606	46.216602
3503.028564	509933.661222	46.221607
3503.297865	509928.205558	46.226612
3502.972674	509922.337955	46.231617
3503.015418	509923.798480	46.236621
3503.358959	509908.061095	46.241626
3502.944784	509916.777775	46.246631
3502.896688	509910.006319	46.251636
3502.976098	509891.983483	46.256641
3503.038566	509874.317443	46.261645
3503.276729	509864.465250	46.266650
3503.065930	509870.063743	46.271655
3503.298805	509862.843125	46.276660
3503.054237	509864.551436	46.281665
3502.782581	509859.838946	46.286669
3502.784861	509853.312460	46.291674
3503.065732	509848.360855	46.296679
3503.560959	509824.605999	46.301684
3503.283463	509820.197969	46.306689
3503.398577	509815.474921	46.311693
3503.475242	509803.826933	46.316698
3503.141189	509784.806921	46.321703
3503.301872	509771.476113	46.326708
3503.133049	509768.214495	46.331713
3503.050109	509765.192259	46.336717
3503.124992	509765.737070	46.341722
3502.837533	509751.111114	46.346727
3503.282016	509730.197274	46.351732
3503.242551	509724.587987	46.356737
3503.183346	509723.889205	46.361741
3503.283347	509717.701362	46.366746
3503.209579	509712.805776	46.371751
3503.105616	509683.732134	46.376756
3503.257671	509676.827764	46.381761
3503.277551	509682.238079	46.386765
3503.246551	509664.434823	46.391770
3503.104187	509679.938547	46.396775
3503.254597	509654.011924	46.401780
3503.389965	509636.637667	46.406785
3503.041032	509633.202127	46.411789
3502.949263	509614.447179	46.416794
3503.168868	509618.156409	46.421799
3503.269793	509606.453860	46.426804
3503.340902	509592.782929	46.431809
3503.264232	509582.474420	46.436813
3503.374881	509568.696036	46.441818
3503.127151	509579.309075	46.446823
3503.097307	509567.981315	46.451828
3503.376263	509539.352820	46.456833
3503.112755	509540.962971	46.461837
3502.907076	509542.918126	46.466842
3503.164989	509536.047559	46.471847
3502.991245	509529.801736	46.476852
3503.277074	509532.842818	46.481857
3503.337111	509514.114357	46.486861
3503.265944	509497.683267	46.491866
3503.293298	509496.515462	46.496871
3503.323266	509494.234214	46.501876
3503.197446	509477.710560	46.506881
3503.159165	509449.739169	46.511885
3503.404488	509442.010484	46.516890
3503.403947	509440.391753	46.521895
3503.150728	509434.006680	46.526900
3503.371344	509417.832946	46.531905
3503.100744	509402.343954	46.536909
3503.402774	509390.963617	46.541914
3502.717486	509395.321861	46.546919
3503.408517	509386.561437	46.551924
3503.354329	509377.311696	46.556929
3503.089430	509366.476292	46.561933
3503.044390	509355.707313	46.566938
3502.931316	509353.094508	46.571943
3502.935254	509354.814179	46.576948
3503.372041	509349.989563	46.581953
3503.214290	509349.255750	46.586957
3503.497315	509320.474470	46.591962
3503.102099	509315.022468	46.596967
3503.299843	509306.289386	46.601972
3503.292050	509304.267046	46.606977
3503.078558	509280.724653	46.611981
3503.172255	509264.469651	46.616986
3503.138958	509266.599960	46.621991
3503.320310	509255.491575	46.626996
3503.242771	509261.372759	46.632001
3503.099168	509252.491235	46.637005
3503.241698	509222.365987	46.642010
3503.043780	509221.739704	46.647015
3503.128825	509213.530321	46.652020
3503.144991	509208.114443	46.657025
3503.037609	509209.851725	46.662029
3503.124668	509202.704474	46.667034
3503.009214	509200.850919	46.672039
3503.160667	509173.658578	46.677044
3503.087695	509173.569068	46.682049
3503.264551	509175.919135	46.687053
3503.488160	509167.232488	46.692058
3503.170071	509160.098668	46.697063
3503.429205	509138.403915	46.702068
3503.170054	509128.984065	46.707073
3503.235915	509133.071858	46.712077
3503.538616	509127.003542	46.717082
3503.253768	509102.409723	46.722087
3503.314573	509082.517020	46.727092
3503.412330	509083.210018	46.732097
3503.416690	509076.379348	46.737101
3503.460667	509049.709735	46.742106
3503.264040	509041.747168	46.747111
3503.178958	509030.579566	46.752116
3503.110063	509030.641191	46.757121
3503.357784	509025.289841	46.762125
3503.319505	509001.112245	46.767130
3502.894622	508990.301892	46.772135
3503.135125	508985.761171	46.777140
3503.059723	508987.139264	46.782145
3502.757249	508981.976058	46.787149
3502.915563	508977.296545	46.792154
3502.910175	508991.564986	46.797159
3503.130561	508968.459519	46.802164
3503.335468	508946.975472	46.807169
3502.979909	508938.076696	46.812173
3503.258918	508934.997098	46.817178
3503.327715	508946.977123	46.822183
3503.304776	508927.401041	46.827188
3503.191183	508901.211451	46.832193
3502.873072	508898.226235	46.837197
3503.180034	508877.788445	46.842202
3503.130862	508893.531117	46.847207
3503.195794	508894.279906	46.852212
3503.215700	508883.196800	46.857217
3503.079361	508862.677283	46.862221
3503.295696	508859.000450	46.867226
3503.109004	508855.286134	46.872231
3503.275009	508841.801982	46.877236
3503.428545	508839.298738	46.882241
3503.025633	508827.472924	46.887245
3503.270382	508806.690724	46.892250
3503.056527	508813.757278	46.897255
3503.117303	508804.033707	46.902260
3503.275257	508798.949448	46.907265
3503.251729	508788.176713	46.912269
3503.192270	508755.907020	46.917274
3503.092655	508752.836646	46.922279
3503.008653	508745.412678	46.927284
3503.093801	508744.640442	46.932289
3502.892630	508755.904357	46.937293
3503.157924	508741.645514	46.942298
3503.189393	508730.762861	46.947303
3503.085736	508711.351077	46.952308
3502.883942	508710.270036	46.957313
3502.923705	508697.261077	46.962317
3502.941301	508694.425138	46.967322
3502.691041	508706.658142	46.972327
3502.976169	508695.887154	46.977332
3503.121862	508697.989240	46.982337
3502.922653	508705.964226	46.987341
3503.167806	508695.958476	46.992346
3503.019389	508679.184652	46.997351
3503.319122	508650.399610	47.002356
3503.150560	508648.959148	47.007361
3503.074147	508651.551702	47.012365
3503.325295	508651.765118	47.017370
3503.232700	508651.982275	47.022375
3503.288914	508621.009509	47.027380
3503.250668	508615.450261	47.032385
3503.248898	508612.212610	47.037389
3503.384882	508609.408538	47.042394
3503.511584	508585.862013	47.047399
3503.417629	508572.317553	47.052404
3503.519927	508566.128933	47.057409
3503.421254	508556.885782	47.062413
3503.386046	508522.992778	47.067418
3503.331698	508527.909238	47.072423
3503.371595	508514.697740	47.077428
3503.311300	508502.362188	47.082433
3503.287370	508488.401831	47.087437
3503.326471	508467.854111	47.092442
3503.108303	508468.799454	47.097447
3503.468055	508467.730823	47.102452
3503.365203	508452.163862	47.107457
3503.128976	508440.918578	47.112461
3503.505471	508421.126996	47.117466
3503.214386	508438.577973	47.122471
3503.230845	508414.998045	47.127476
3503.358246	508384.064195	47.132481
3503.124808	508390.425679	47.137485
3503.190151	508393.400628	47.142490
3503.186733	508384.749474	47.147495
3503.032922	508375.514941	47.152500
3503.032372	508352.392977	47.157505
3502.945204	508343.755040	47.162509
3503.346798	508332.763033	47.167514
3503.219975	508332.631435	47.172519
3503.040624	508339.945707	47.177524
3503.175315	508324.543464	47.182529
3503.020329	508321.835936	47.187533
3503.266612	508293.665897	47.192538
3502.955433	508285.872874	47.197543
3503.093691	508289.747040	47.202548
3503.176692	508286.850099	47.207553
3502.962969	508287.389983	47.212557
3503.168768	508284.170056	47.217562
3503.165188	508267.221148	47.222567
3502.665630	508257.231670	47.227572
3503.231023	508240.749353	47.232577
3503.112365	508248.813008	47.237581
3503.415157	508244.818803	47.242586
3503.152035	508246.479607	47.247591
3502.927215	508218.586298	47.252596
3503.420957	508210.362429	47.257601
3502.841632	508199.727779	47.262605
3502.936846	508195.412201	47.267610
3503.116980	508190.577238	47.272615
3503.318179	508192.114056	47.277620
3503.500908	508179.233896	47.282625
3502.948908	508164.850788	47.287629
3502.887401	508148.973441	47.292634
3502.952266	508149.823465	47.297639
3502.973307	508134.489614	47.302644
3503.089117	508137.254245	47.307649
3502.793184	508148.128765	47.312653
3503.006177	508146.982121	47.317658
3503.047064	508144.294198	47.322663
3503.342910	508133.419973	47.327668
3503.381550	508108.824195	47.332673
3503.233579	508099.285013	47.337677
3503.213988	508093.621456	47.342682
3502.962062	508096.039451	47.347687
3503.053658	508090.560702	47.352692
3502.808902	508075.471200	47.357697
3502.677994	508074.884877	47.362701
3503.001985	508064.714510	47.367706
3503.045226	508055.296868	47.372711
3502.837240	508050.624410	47.377716
3503.264402	508050.253450	47.382721
3503.247247	508055.771324	47.387725
3503.071774	508044.870353	47.392730
3503.252496	508048.636668	47.397735
3503.305375	508032.842326	47.402740
3503.264868	508012.357244	47.407745
3502.982288	508009.012078	47.412749
3503.050332	507999.033922	47.417754
3502.996392	507999.852137	47.422759
3502.962181	507992.925940	47.427764
3503.675559	507991.750786	47.432769
3503.474167	507971.392280	47.437773
3503.281240	507958.773724	47.442778
3503.351466	507950.869663	47.447783
3503.417828	507934.263550	47.452788
3503.542601	507911.424766	47.457793
3502.842927	507905.312083	47.462797
3503.333179	507904.273387	47.467802
3503.513808	507902.170501	47.472807
3503.039136	507892.126280	47.477812
3503.146433	507871.718861	47.482817
3502.963878	507867.750692	47.487821
3503.482836	507867.517010	47.492826
3503.290298	507866.333257	47.497831
3503.348861	507835.915278	47.502836
3503.592993	507819.230357	47.507841
3503.110579	507814.904797	47.512845
3503.422668	507808.530953	47.517850
3503.310072	507786.842665	47.522855
3503.220358	507783.011593	47.527860
3503.088953	507772.103484	47.532865
3503.107023	507766.332671	47.537869
3503.100902	507764.309886	47.542874
3503.104886	507755.201869	47.547879
3503.044883	507739.576895	47.552884
3503.043704	507730.064902	47.557889
3502.842570	507728.933095	47.562893
3503.172733	507712.892240	47.567898
3503.196681	507716.885799	47.572903
3503.175438	507714.359424	47.577908
3503.364909	507702.338001	47.582913
3503.088575	507689.530042	47.587917
3503.341800	507684.379799	47.592922
3503.176593	507693.361828	47.597927
3503.178756	507685.114221	47.602932
3503.306663	507664.804496	47.607937
3503.042843	507652.652301	47.612941
3503.100677	507639.791482	47.617946
3502.955667	507637.790637	47.622951
3502.892106	507646.857818	47.627956
3502.916957	507632.079494	47.632961
3502.709228	507642.839192	47.637965
3503.005441	507631.408020	47.642970
3502.883272	507630.870898	47.647975
3503.132293	507622.280653	47.652980
3503.453374	507602.598091	47.657985
3503.468097	507602.848894	47.662989
3503.175164	507592.725172	47.667994
3503.030872	507589.003880	47.672999
3503.036486	507582.172419	47.678004
3503.200312	507553.002251	47.683009
3502.890323	507551.634649	47.688013
3503.093882	507546.745207	47.693018
3503.065872	507543.713896	47.698023
3503.304155	507546.965242	47.703028
3503.216942	507530.484213	47.708033
3502.773655	507532.375956	47.713037
3502.820679	507521.338287	47.718042
3502.839940	507504.587413	47.723047
3502.944979	507501.838652	47.728052
3503.050594	507498.533220	47.733057
3502.925034	507501.234911	47.738061
3503.394942	507495.898566	47.743066
3503.210778	507501.645409	47.748071
3503.348296	507492.718539	47.753076
3503.228232	507469.057705	47.758081
3503.446676	507457.436318	47.763085
3503.332166	507451.939349	47.768090
3503.239491	507440.569524	47.773095
3503.339660	507416.722010	47.778100
3503.078499	507407.503928	47.783105
3502.967391	507409.191380	47.788109
3503.128302	507404.055647	47.793114
3502.985843	507409.897125	47.798119
3502.732772	507407.407350	47.803124
3503.352198	507390.055511	47.808129
3502.955806	507378.480662	47.813133
3503.001407	507358.841368	47.818138
3503.091240	507352.553089	47.823143
3503.087029	507344.154531	47.828148
3503.032022	507350.386994	47.833153
3502.859288	507357.801831	47.838157
3503.109269	507346.175385	47.843162
3503.123573	507343.896329	47.848167
3503.321298	507332.025140	47.853172
3503.298646	507312.649577	47.858177
3503.049073	507307.072714	47.863181
3502.946685	507300.612406	47.868186
3502.954959	507303.039978	47.873191
3502.834872	507307.258795	47.878196
3502.934094	507299.400452	47.883201
3503.001845	507288.915945	47.888205
3503.028154	507262.752351	47.893210
3502.950531	507266.863268	47.898215
3502.728063	507268.315343	47.903220
3502.914870	507258.115591	47.908225
3502.950721	507260.842403	47.913229
3503.233720	507256.142716	47.918234
3503.075202	507255.307735	47.923239
3503.381001	507255.613730	47.928244
3503.378076	507222.168461	47.933249
3503.199467	507224.878580	47.938253
3503.130778	507213.555412	47.943258
3503.247354	507211.361371	47.948263
3503.408808	507206.984478	47.953268
3503.425676	507178.039304	47.958273
3503.273914	507171.080761	47.963277
3503.302127	507165.763537	47.968282
3503.120735	507166.045347	47.973287
3502.920751	507152.415335	47.978292
3503.223274	507126.359672	47.983297
3502.823758	507136.289813	47.988301
3503.367714	507122.542181	47.993306
3503.126655	507120.202262	47.998311
3503.204352	507120.594916	48.003316
3503.320449	507108.685879	48.008321
3502.960790	507093.664281	48.013325
3503.021063	507078.373892	48.018330
3503.025936	507077.411876	48.023335
3503.265433	507068.063872	48.028340
3503.521847	507058.713190	48.033345
3502.783108	507062.119069	48.038349
3503.312767	507043.769086	48.043354
3503.221495	507027.743616	48.048359
3502.994413	507023.529293	48.053364
3503.190145	507023.852692	48.058369
3502.900684	507022.077006	48.063373
3502.965049	507027.481123	48.068378
3502.814049	507025.379954	48.073383
3503.089952	507012.130002	48.078388
3502.989962	506983.051176	48.083393
3503.129680	506985.660414	48.088397
3502.944105	506966.968013	48.093402
3503.296554	506967.469039	48.098407
3503.292850	506973.491128	48.103412
3503.445973	506964.966318	48.108417
3503.178653	506947.045813	48.113421
3503.118993	506931.217655	48.118426
3503.101415	506921.556011	48.123431
3503.001867	506915.854107	48.128436
3503.170532	506914.157793	48.133441
3502.844959	506923.114970	48.138445
3502.856627	506908.692312	48.143450
3502.972862	506886.764325	48.148455
3502.827542	506881.120244	48.153460
3502.893648	506870.281545	48.158465
3502.379100	506865.606624	48.163469
3502.646919	506863.338031	48.168474
3502.511117	506863.207840	48.173479
3502.815923	506870.395598	48.178484
3503.129696	506859.568343	48.183489
3502.763890	506869.999307	48.188493
3503.213337	506867.499604	48.193498
3503.072762	506860.994568	48.198503
3502.814238	506862.654775	48.203508
3503.085064	506859.626706	48.208513
3502.946316	506868.706179	48.213517
3502.792482	506859.825039	48.218522
3502.758909	506858.261887	48.223527
3502.952854	506861.925172	48.228532
3503.093710	506841.612436	48.233537
3502.868924	506833.602699	48.238541
3502.916240	506818.010529	48.243546
3503.059348	506814.850841	48.248551
3502.742097	506826.387359	48.253556
3503.031809	506814.045875	48.258561
3502.874356	506825.202933	48.263565
3503.290269	506818.458115	48.268570
3503.127121	506812.614430	48.273575
3502.827439	506798.797498	48.278580
3503.419549	506768.090904	48.283585
3503.061120	506778.419557	48.288589
3503.146484	506774.155784	48.293594
3503.513717	506766.811437	48.298599
3503.089333	506758.732016	48.303604
3503.230892	506744.946493	48.308609
3503.076181	506734.547417	48.313613
3503.367787	506715.222712	48.318618
3503.438312	506728.064209	48.323623
3502.713800	506728.583680	48.328628
3502.962712	506719.841206	48.333633
3502.927518	506692.573266	48.338637
3503.250113	506683.566124	48.343642
3503.257280	506672.483616	48.348647
3503.065839	506674.386239	48.353652
3503.119294	506681.765609	48.358657
3502.913861	506686.200470	48.363661
3503.067484	506671.856377	48.368666
3503.191095	506647.295693	48.373671
3503.314720	506639.483795	48.378676
3503.497817	506627.310834	48.383681
3503.066503	506630.364594	48.388685
3503.098474	506621.251558	48.393690
3503.474650	506600.041131	48.398695
3502.966398	506588.989442	48.403700
3503.265671	506586.209833	48.408705
3502.888073	506581.917993	48.413709
3503.136703	506581.828232	48.418714
3502.959044	506574.873543	48.423719
3502.686302	506579.723877	48.428724
3503.308674	506558.221477	48.433729
3503.168550	506552.930675	48.438733
3503.110006	506548.385989	48.443738
3503.065860	506533.415232	48.448743
3503.140450	506538.514279	48.453748
3503.260334	506536.370231	48.458753
3502.916962	506528.632102	48.463757
3503.084874	506499.914927	48.468762
3503.215916	506488.458512	48.473767
3502.919128	506486.076716	48.478772
3503.179719	506477.990089	48.483777
3503.132559	506491.002168	48.488781
3503.354772	506487.273305	48.493786
3503.182320	506462.303749	48.498791
3503.100264	506448.452137	48.503796
3503.206145	506442.211593	48.508801
3502.641309	506447.917754	48.513805
3502.968608	506440.326577	48.518810
3503.055240	506430.344580	48.523815
3502.694237	506435.714918	48.528820
3503.186850	506437.104627	48.533825
3503.281785	506422.769606	48.538829
3503.061154	506396.441336	48.543834
3503.266844	506394.334309	48.548839
3503.054843	506394.165556	48.553844
3503.078546	506393.149924	48.558849
3503.368864	506392.547559	48.563853
3503.085352	506366.887003	48.568858
3502.930305	506353.198657	48.573863
3502.874137	506361.506318	48.578868
3503.512829	506352.297236	48.583873
3502.924340	506353.655438	48.588877
3503.047530	506343.971222	48.593882
3503.285159	506347.577109	48.598887
3502.939512	506330.629776	48.603892
3503.162210	506301.802411	48.608897
3502.848716	506304.483392	48.613901
3502.804961	506307.273540	48.618906
3503.664341	506289.275457	48.623911
3503.379763	506301.616784	48.628916
3503.305220	506270.053262	48.633921
3503.199171	506257.116121	48.638925
3503.035322	506253.600039	48.643930
3502.982252	506254.367596	48.648935
3503.093793	506261.383751	48.653940
3503.374959	506249.650440	48.658945
3502.712555	506229.160352	48.663949
3502.807382	506218.468512	48.668954
3503.409897	506200.156729	48.673959
3503.078128	506217.869377	48.678964
3503.099030	506207.492827	48.683969
3503.493732	506205.355899	48.688973
3503.404610	506197.779840	48.693978
3503.316708	506191.519236	48.698983
3503.281602	506177.406977	48.703988
3503.547483	506173.013318	48.708993
3503.375711	506158.720239	48.713997
3503.038115	506134.636552	48.719002
3503.415252	506115.449468	48.724007
3503.422450	506124.253248	48.729012
3503.367677	506106.399480	48.734017
3503.343944	506099.420269	48.739021
3503.181960	506074.094285	48.744026
3503.422841	506084.480419	48.749031
3503.036521	506076.951287	48.754036
3503.421966	506047.389343	48.759041
3503.000768	506041.130767	48.764045
3503.214532	506027.738083	48.769050
3503.303364	506026.762736	48.774055
3503.061334	506038.237282	48.779060
3503.265741	506023.834026	48.784065
3503.154709	505998.196263	48.789069
3503.171752	505989.237064	48.794074
3503.003502	505990.174647	48.799079
3502.644345	505990.535177	48.804084
3502.938787	505985.580328	48.809089
3503.076709	505988.696026	48.814093
3503.023581	505996.193740	48.819098
3503.236685	505980.321601	48.824103
3503.115715	505964.046831	48.829108
3503.291923	505938.262370	48.834113
3503.154435	505942.585472	48.839117
3503.139298	505936.819301	48.844122
3503.041058	505943.059102	48.849127
3502.868621	505936.103331	48.854132
3503.296913	505902.688564	48.859137
3503.019772	505889.525181	48.864141
3502.782911	505890.321806	48.869146
3503.114372	505893.508133	48.874151
3503.008701	505886.642994	48.879156
3503.042763	505883.854596	48.884161
3503.014955	505883.049487	48.889165
3502.898575	505880.386074	48.894170
3502.835571	505879.434721	48.899175
3502.501767	505873.971916	48.904180
3502.951863	505872.382823	48.909185
3503.171846	505871.083120	48.914189
3502.841981	505853.323180	48.919194
3503.402899	505831.272969	48.924199
3502.904262	505839.195394	48.929204
3502.934260	505824.212307	48.934209
3503.131348	505835.769382	48.939213
3502.954201	505834.684260	48.944218
3503.182805	505830.448217	48.949223
3502.951487	505820.313718	48.954228
3503.314359	505790.147671	48.959233
3503.265040	505791.876114	48.964237
3503.156856	505789.768026	48.969242
3503.148972	505788.200717	48.974247
3502.940360	505777.202351	48.979252
3503.101790	505751.976585	48.984257
3503.243343	505742.946974	48.989261
3503.014297	505731.901206	48.994266
3503.345828	505741.311754	48.999271
3503.068958	505741.659280	49.004276
3503.446262	505727.279053	49.009281
3503.160924	505708.499861	49.014285
3503.130640	505696.258774	49.019290
3503.254540	505688.345200	49.024295
3503.281337	505698.461785	49.029300
3503.332221	505686.005447	49.034305
3503.448089	505662.102443	49.039309
3502.732273	505647.237096	49.044314
3503.353395	505643.444997	49.049319
3503.083670	505650.369856	49.054324
3503.278603	505637.030452	49.059329
3503.274082	505621.192387	49.064333
3503.403563	505612.417635	49.069338
3503.391991	505598.402394	49.074343
3503.331127	505604.332785	49.079348
3503.291591	505579.846990	49.084353
3503.146251	505560.944302	49.089357
3503.543030	505550.912775	49.094362
3503.569072	505548.884648	49.099367
3503.167711	505526.176502	49.104372
3503.272334	505503.489551	49.109377
3503.442571	505509.535256	49.114381
3503.050181	505511.520373	49.119386
3503.412422	505494.966367	49.124391
3503.173383	505478.811015	49.129396
3503.371608	505462.384113	49.134401
3503.087120	505462.884661	49.139405
3502.999318	505452.676657	49.144410
3503.579404	505449.042816	49.149415
3503.437343	505440.361506	49.154420
3503.580698	505426.068616	49.159425
3503.317267	505416.495603	49.164429
3503.116298	505396.134008	49.169434
3503.307061	505376.773158	49.174439
3503.061201	505370.638436	49.179444
3502.771007	505372.506205	49.184449
3503.336423	505367.052910	49.189453
3503.034473	505363.001830	49.194458
3503.256954	505363.928286	49.199463
3503.041322	505339.520594	49.204468
3503.226733	505329.218726	49.209473
3503.336115	505324.950803	49.214477
3503.001206	505312.302159	49.219482
3503.383787	505316.188976	49.224487
3502.779617	505304.291352	49.229492
3503.078240	505285.723024	49.234497
3503.028837	505288.210599	49.239501
3502.820979	505277.970866	49.244506
3503.226579	505269.759551	49.249511
3502.896196	505277.149586	49.254516
3503.120338	505273.976811	49.259521
3503.193053	505267.994113	49.264525
3503.174332	505258.483541	49.269530
3503.269342	505244.349959	49.274535
3503.086931	505239.217255	49.279540
3503.025236	505230.270113	49.284545
3502.878291	505232.469486	49.289549
3502.753767	505231.072379	49.294554
3503.087840	505224.289282	49.299559
3502.728452	505232.594806	49.304564
3502.813973	505225.243742	49.309569
3503.172951	505222.808715	49.314573
3503.112155	505201.109011	49.319578
3503.334513	505181.338111	49.324583
3502.889828	505182.825482	49.329588
3502.914829	505164.654512	49.334593
3502.929923	505178.264988	49.339597
3503.047539	505164.684422	49.344602
3503.286478	505167.885509	49.349607
3503.001335	505153.558921	49.354612
3502.813652	505141.544746	49.359617
3503.022204	505136.046580	49.364621
3502.731132	505130.070735	49.369626
3503.154971	505129.346014	49.374631
3502.982035	505128.209577	49.379636
3503.051883	505116.761936	49.384641
3502.971037	505123.859565	49.389645
3502.832387	505125.197355	49.394650
3503.174429	505115.832098	49.399655
3502.867558	505103.735527	49.404660
3502.865811	505090.021956	49.409665
3502.876730	505082.429598	49.414669
3502.934025	505081.459185	49.419674
3503.057684	505077.391365	49.424679
3503.188913	505078.939524	49.429684
3503.332731	505078.815721	49.434689
3503.066104	505078.200142	49.439693
3502.960449	505063.086030	49.444698
3502.944958	505045.832231	49.449703
3502.715639	505037.417539	49.454708
3502.966631	505033.430792	49.459713
3502.917769	505029.086600	49.464717
3502.692306	505036.662573	49.469722
3502.961126	505036.670827	49.474727
3502.608502	505034.095233	49.479732
3502.741644	505033.062223	49.484737
3502.795321	505032.193589	49.489741
3502.594852	505036.071423	49.494746
3502.810988	505024.145149	49.499751
3502.881701	505030.054936	49.504756
3503.022870	505024.769809	49.509761
3502.965771	505020.882366	49.514765
3502.959183	505023.363210	49.519770
3503.253549	505015.675413	49.524775
3503.058471	505003.156258	49.529780
3503.577066	504981.314090	49.534785
3503.332035	504982.466284	49.539789
3503.052779	504992.125603	49.544794
3503.267211	504978.985038	49.549799
3502.968056	504956.462415	49.554804
3503.137316	504937.408111	49.559809
3503.175570	504928.900465	49.564813
3503.093353	504935.542937	49.569818
3502.989440	504936.774039	49.574823
3503.027729	504935.806622	49.579828
3502.947405	504927.874381	49.584833
3503.005757	504912.329369	49.589837
3502.749002	504898.655957	49.594842
3503.128702	504885.387986	49.599847
3502.707618	504886.871651	49.604852
3503.156326	504885.485115	49.609857
3503.195400	504882.695764	49.614861
3502.997679	504885.257447	49.619866
3503.113695	504886.757422	49.624871
3503.172961	504884.066091	49.629876
3503.076617	504853.262539	49.634881
3502.869787	504843.680265	49.639885
3503.237286	504844.786250	49.644890
3503.091774	504834.688219	49.649895
3502.809787	504842.475634	49.654900
3503.217192	504837.856848	49.659905
3503.078750	504834.134038	49.664909
3502.809226	504839.490402	49.669914
3503.265700	504824.439043	49.674919
3503.008492	504804.490496	49.679924
3503.111623	504791.974656	49.684929
3503.358856	504791.783899	49.689933
3502.952258	504793.467705	49.694938
3503.356897	504785.762376	49.699943
3503.043290	504764.253911	49.704948
3502.979897	504745.539811	49.709953
3503.111677	504745.620334	49.714957
3503.290900	504746.907905	49.719962
3503.390032	504743.299341	49.724967
3503.071892	504736.568547	49.729972
3503.281475	504706.728502	49.734977
3503.189587	504693.534931	49.739981
3502.940497	504695.143243	49.744986
3502.802481	504690.458816	49.749991
3502.714908	504690.978863	49.754996
3503.068672	504691.378541	49.760001
3503.078282	504693.047171	49.765005
3503.052514	504698.010802	49.770010
3503.440936	504681.654316	49.775015
3503.093824	504674.523227	49.780020
3503.241239	504659.773614	49.785025
3503.295401	504657.538512	49.790029
3502.883424	504662.310171	49.795034
3503.213644	504653.452601	49.800039
3502.830749	504632.511597	49.805044
3503.060151	504616.939284	49.810049
3503.167195	504621.274664	49.815053
3502.889915	504608.009122	49.820058
3503.313410	504607.486862	49.825063
3503.233530	504601.730484	49.830068
3503.118139	504607.062554	49.835073
3503.126355	504578.569891	49.840077
3502.826745	504570.975791	49.845082
3503.064787	504563.195487	49.850087
3503.256860	504570.958692	49.855092
3503.136579	504565.664148	49.860097
3503.106080	504560.709658	49.865101
3503.301256	504548.583948	49.870106
3503.458001	504526.342953	49.875111
3503.020242	504527.778676	49.880116
3502.830588	504517.485013	49.885121
3503.268137	504525.411862	49.890125
3503.003722	504515.433656	49.895130
3503.129919	504506.254015	49.900135
3503.261546	504495.808340	49.905140
3503.407340	504479.085163	49.910145
3503.051366	504473.676028	49.915149
3502.974292	504466.198526	49.920154
3503.185443	504460.244277	49.925159
3502.926929	504460.943173	49.930164
3503.088669	504435.563642	49.935169
3503.171264	504419.356469	49.940173
3503.046341	504422.362175	49.945178
3503.384567	504424.788599	49.950183
3503.032330	504429.854519	49.955188
3503.022136	504411.536509	49.960193
3503.251304	504395.053109	49.965197
3502.725315	504383.041282	49.970202
3503.105102	504384.195962	49.975207
3502.912040	504375.269148	49.980212
3503.062272	504367.958102	49.985217
3503.183176	504375.024143	49.990221
3503.060180	504368.464789	49.995226
3503.151736	504371.588106	50.000231
3502.887555	504356.194799	50.005236
3502.968151	504331.941304	50.010241
3502.929057	504330.834264	50.015245
3502.893597	504334.028273	50.020250
3503.279230	504326.325748	50.025255
3503.230889	504333.216130	50.030260
3503.185639	504336.057435	50.035265
3503.137736	504324.880927	50.040269
3503.243815	504308.214473	50.045274
3503.030294	504297.064127	50.050279
3502.683696	504299.598821	50.055284
3502.711395	504278.288844	50.060289
3503.064147	504276.107710	50.065293
3502.908566	504283.166886	50.070298
3503.111913	504275.746191	50.075303
3503.153747	504287.126403	50.080308
3503.272550	504276.176549	50.085313
3503.001516	504250.915769	50.090317
3503.247885	504238.427500	50.095322
3503.390516	504231.876714	50.100327
3502.956309	504237.107469	50.105332
3503.207884	504230.337030	50.110337
3503.034325	504202.935252	50.115341
3503.194739	504191.270260	50.120346
3503.084256	504176.510400	50.125351
3503.172403	504177.205117	50.130356
3502.807928	504185.309507	50.135361
3503.229936	504185.141726	50.140365
3503.088653	504179.394915	50.145370
3503.376629	504143.417980	50.150375
3502.923073	504145.058660	50.155380
3502.836226	504139.100800	50.160385
3503.005013	504136.898122	50.165389
3503.012975	504128.091229	50.170394
3502.980297	504128.653223	50.175399
3502.832743	504130.194927	50.180404
3502.872301	504126.038966	50.185409
3502.851885	504119.412695	50.190413
3502.888564	504128.162212	50.195418
3503.318854	504109.116355	50.200423
3502.320030	504104.770274	50.205428
3502.849425	504093.451755	50.210433
3503.255533	504087.314739	50.215437
3502.829655	504087.837673	50.220442
3502.702568	504089.376144	50.225447
3502.712629	504090.994153	50.230452
3502.616068	504089.946790	50.235457
3502.838596	504086.369193	50.240461
3502.910612	504094.100980	50.245466
3502.917682	504093.290275	50.250471
3502.830820	504096.846709	50.255476
3502.955455	504089.084122	50.260481
3503.076943	504093.366742	50.265485
3502.873081	504086.567024	50.270490
3503.143711	504077.819801	50.275495
3502.747336	504065.281186	50.280500
3502.946236	504048.144340	50.285505
3503.085381	504036.432000	50.290509
3502.979738	504034.272689	50.295514
3503.223596	504034.133067	50.300519
3503.053827	504032.945448	50.305524
3502.862496	504029.939342	50.310529
3502.832542	504032.069763	50.315533
3502.732665	504036.994687	50.320538
3503.131220	504029.644248	50.325543
3502.670671	504017.520609	50.330548
3502.829272	504005.754564	50.335553
3502.758982	503996.858759	50.340557
3502.948853	503988.023041	50.345562
3503.332179	503978.751871	50.350567
3503.051370	503983.806627	50.355572
3503.046977	503978.847846	50.360577
3503.240311	503985.649553	50.365581
3503.042665	503985.883370	50.370586
3503.328972	503961.293197	50.375591
3503.152952	503949.326967	50.380596
3502.843053	503944.669511	50.385601
3503.127852	503939.766222	50.390605
3502.985025	503937.309126	50.395610
3502.926983	503935.800188	50.400615
3502.863706	503942.541258	50.405620
3502.842704	503932.372417	50.410625
3503.273013	503925.320566	50.415629
3502.850883	503911.621917	50.420634
3503.108038	503900.194483	50.425639
3502.919439	503897.795225	50.430644
3502.942365	503898.905132	50.435649
3503.137976	503891.181846	50.440653
3503.010055	503899.046541	50.445658
3503.129786	503891.436467	50.450663
3503.255869	503895.718410	50.455668
3503.098983	503859.507563	50.460673
3503.206275	503850.178742	50.465677
3503.091043	503857.484754	50.470682
3502.879945	503845.827651	50.475687
3502.782198	503848.474898	50.480692
3502.996574	503848.390543	50.485697
3502.910409	503833.171072	50.490701
3502.846623	503842.898178	50.495706
3503.192522	503833.379805	50.500711
3502.937507	503820.869279	50.505716
3502.702032	503810.076355	50.510721
3503.199540	503798.661471	50.515725
3502.924938	503801.589725	50.520730
3503.133821	503785.463223	50.525735
3503.067061	503758.246304	50.530740
3502.955846	503715.803036	50.535745
3503.014543	503668.727366	50.540749
3502.800045	503618.556974	50.545754
3502.940205	503545.505463	50.550759
3502.562091	503472.080087	50.555764
3502.114762	503384.241484	50.560769
3502.150810	503288.582654	50.565773
3502.169091	503194.849317	50.570778
3502.042718	503078.869550	50.575783
3501.519535	502965.482310	50.580788
3501.555796	502833.431445	50.585793
3501.343152	502692.814895	50.590797
3500.847764	502555.987241	50.595802
3501.099253	502401.579033	50.600807
3501.035310	502252.078219	50.605812
3500.430528	502077.557209	50.610817
3500.347261	501895.005595	50.615821
3499.595826	501714.886007	50.620826
3499.473399	501522.061934	50.625831
3499.067256	501329.128770	50.630836
3498.966795	501131.184777	50.635841
3498.616551	500930.443513	50.640845
3497.909257	500718.266221	50.645850
3497.724964	500491.678755	50.650855
3497.203288	500272.582730	50.655860
3496.501655	500042.983597	50.660865
3496.593448	499821.102229	50.665869
3496.176595	499584.618470	50.670874
3495.677248	499341.513210	50.675879
3495.331776	499098.127221	50.680884
3494.584266	498843.461949	50.685889
3494.420950	498577.512886	50.690893
3493.806112	498325.907366	50.695898
3493.531277	498059.664545	50.700903
3493.084068	497796.431977	50.705908
3492.548494	497531.994505	50.710913
3492.023470	497250.945713	50.715917
3491.616983	496974.430363	50.720922
3491.157702	496682.679820	50.725927
3490.630966	496403.288928	50.730932
3489.826800	496105.761220	50.735937
3489.596862	495813.909862	50.740941
3488.768696	495516.376329	50.745946
3488.740879	495216.939271	50.750951
3488.024475	494908.897133	50.755956
3487.475972	494607.152621	50.760961
3486.928963	494298.719009	50.765965
3486.241810	493990.353011	50.770970
3485.955987	493664.245971	50.775975
3485.289040	493345.839786	50.780980
3484.565670	493031.943907	50.785985
3484.186474	492709.075654	50.790989
3483.353327	492387.843400	50.795994
3483.147575	492044.831723	50.800999
3482.369255	491723.427373	50.806004
3481.836979	491392.406940	50.811009
3481.293106	491065.991105	50.816013
3480.258373	490736.101981	50.821018
3479.887483	490398.150627	50.826023
3479.312401	490064.631755	50.831028
3478.643134	489720.080556	50.836033
3478.142824	489377.674233	50.841037
3477.282396	489047.879788	50.846042
3476.894472	488705.392819	50.851047
3476.232716	488359.295998	50.856052
3475.177147	488014.875981	50.861057
3474.908764	487670.325251	50.866061
3474.166763	487328.477171	50.871066
3473.797126	486983.929989	50.876071
3473.005981	486648.865282	50.881076
3472.368941	486291.937051	50.886081
3472.008765	485943.823562	50.891085
3471.050348	485592.404151	50.896090
3470.528488	485236.856472	50.901095
3469.919220	484879.948176	50.906100
3469.071212	484527.022627	50.911105
3468.536511	484178.296756	50.916109
3467.768960	483832.539889	50.921114
3467.234508	483463.839543	50.926119
3466.373624	483119.705956	50.931124
3465.572206	482763.295557	50.936129
3465.182351	482404.533514	50.941133
3464.392142	482048.868256	50.946138
3463.892352	481689.046376	50.951143
3463.335706	481339.462248	50.956148
3462.412151	480974.576512	50.961153
3462.010427	480615.479448	50.966157
3461.227684	480279.542949	50.971162
3460.598532	479915.857811	50.976167
3459.650321	479549.784005	50.981172
3458.871820	479192.899572	50.986177
3458.678866	478841.389205	50.991181
3457.656554	478488.939490	50.996186
3457.113569	478118.720934	51.001191
3456.081915	477763.371138	51.006196
3455.491547	477413.722791	51.011201
3455.004517	477047.935347	51.016205
3454.383033	476701.168272	51.021210
3453.931199	476327.607726	51.026215
3452.940474	475982.407080	51.031220
3452.098464	475622.529073	51.036225
3451.556778	475260.519035	51.041229
3450.478575	474918.861979	51.046234
3450.254100	474555.065792	51.051239
3449.712542	474206.164907	51.056244
3448.619443	473848.525281	51.061249
3448.016150	473495.769555	51.066253
3447.173502	473145.782874	51.071258
3446.473725	472788.062422	51.076263
3445.794948	472445.337454	51.081268
3445.293814	472088.992761	51.086273
3445.027431	471735.595737	51.091277
3443.693255	471392.906096	51.096282
3443.112408	471035.288336	51.101287
3442.497824	470688.316103	51.106292
3442.038666	470343.037197	51.111297
3441.333623	469981.973368	51.116301
3440.344920	469635.803112	51.121306
3439.936767	469279.040281	51.126311
3439.305817	468939.190128	51.131316
3438.263632	468589.968835	51.136321
3437.820082	468222.343229	51.141325
3437.067437	467886.652837	51.146330
3436.535074	467537.231950	51.151335
3435.777442	467198.996100	51.156340
3434.923967	466840.284560	51.161345
3434.152552	466486.269718	51.166349
3433.197973	466153.017530	51.171354
3432.831307	465796.695984	51.176359
3432.408772	465465.580047	51.181364
3431.354150	465111.282726	51.186369
3430.884164	464766.065837	51.191373
3430.013928	464430.288401	51.196378
3429.572278	464083.889608	51.201383
3428.841345	463741.334481	51.206388
3428.049651	463383.974794	51.211393
3427.417619	463040.834978	51.216397
3426.382875	462710.888884	51.221402
3426.193353	462354.989092	51.226407
3425.276403	462017.964087	51.231412
3424.343403	461681.240678	51.236417
3423.940563	461346.913466	51.241421
3422.808923	460992.458937	51.246426
3422.438908	460657.101513	51.251431
3421.702368	460318.702844	51.256436
3420.955864	459992.879724	51.261441
3420.447500	459652.152134	51.266445
3419.423676	459316.522443	51.271450
3418.693318	458977.645542	51.276455
3418.237295	458650.589870	51.281460
3417.127103	458314.958544	51.286465
3417.068433	457980.271851	51.291469
3416.097069	457653.739435	51.296474
3415.361847	457318.794616	51.301479
3414.671662	456988.656928	51.306484
3413.630931	456660.396056	51.311489
3413.211407	456323.610765	51.316493
3412.464961	455997.170645	51.321498
3411.980177	455666.321385	51.326503
3411.036178	455332.546582	51.331508
3410.339317	455019.528696	51.336513
3409.758522	454683.048643	51.341517
3408.926065	454353.554122	51.346522
3408.133503	454031.912601	51.351527
3407.302675	453716.411726	51.356532
3406.625518	453388.755853	51.361537
3406.256584	453066.424784	51.366541
3405.107563	452765.167740	51.371546
3404.501226	452439.618027	51.376551
3403.995828	452122.369153	51.381556
3403.176589	451806.434030	51.386561
3402.786003	451483.424383	51.391565
3401.834653	451174.199365	51.396570
3401.544242	450842.944566	51.401575
3400.576086	450547.820426	51.406580
3399.694740	450224.870705	51.411585
3399.457895	449902.880213	51.416589
3398.490061	449595.920180	51.421594
3397.778364	449278.969218	51.426599
3397.521043	448969.046727	51.431604
3396.647904	448645.718482	51.436609
3396.078334	448322.084008	51.441613
3395.242156	448012.950827	51.446618
3394.564537	447702.570485	51.451623
3394.024205	447384.602446	51.456628
3393.203944	447075.403635	51.461633
3392.838919	446747.248946	51.466637
3391.794526	446433.103424	51.471642
3391.332304	446116.933030	51.476647
3390.426348	445800.422545	51.481652
3389.577874	445490.395380	51.486657
3388.927497	445177.998085	51.491661
3388.188965	444863.884916	51.496666
3387.484478	444556.360629	51.501671
3386.782755	444254.770584	51.506676
3386.201376	443942.803029	51.511681
3385.588120	443639.313191	51.516685
3384.563392	443331.519265	51.521690
3384.090345	443019.167269	51.526695
3383.440449	442712.422884	51.531700
3382.497309	442415.061085	51.536705
3382.246073	442101.697684	51.541709
3381.357647	441797.314476	51.546714
3380.973823	441486.349946	51.551719
3379.950423	441187.361364	51.556724
3379.261403	440885.574948	51.561729
3378.747290	440576.700771	51.566733
3377.986846	440282.634530	51.571738
3377.263387	439972.364391	51.576743
3376.737780	439668.912615	51.581748
3375.672760	439364.146282	51.586753
3375.204012	439061.160322	51.591757
3374.598529	438764.969935	51.596762
3373.935863	438459.341891	51.601767
3373.081352	438156.152006	51.606772
3372.161427	437852.841836	51.611777
3371.896203	437550.617569	51.616781
3370.962222	437261.036105	51.621786
3370.153391	436963.891748	51.626791
3369.643946	436670.149103	51.631796
3368.878156	436378.601444	51.636801
3368.261990	436081.593871	51.641805
3367.213187	435790.947318	51.646810
3367.048600	435487.971425	51.651815
3366.222019	435193.119238	51.656820
3365.868683	434899.280480	51.661825
3364.885916	434597.108797	51.666829
3364.573206	434304.932390	51.671834
3363.735250	434006.488361	51.676839
3362.988649	433709.956003	51.681844
3362.368686	433413.704856	51.686849
3361.588038	433118.212006	51.691853
3360.779885	432826.477893	51.696858
3360.220695	432527.286988	51.701863
3359.464661	432240.032148	51.706868
3358.763060	431944.894181	51.711873
3358.148144	431648.621900	51.716877
3357.343374	431360.654024	51.721882
3356.758419	431072.724366	51.726887
3355.783108	430789.093795	51.731892
3355.047778	430496.433140	51.736897
3354.444559	430207.125585	51.741901
3353.755465	429926.589109	51.746906
3353.309007	429628.565844	51.751911
3352.400501	429345.518483	51.756916
3351.772846	429061.026978	51.761921
3351.239178	428776.339775	51.766925
3350.419966	428488.850448	51.771930
3349.663596	428204.116109	51.776935
3348.925690	427924.277073	51.781940
3348.251796	427640.361677	51.786945
3347.857630	427352.894389	51.791949
3346.978253	427076.344856	51.796954
3346.057163	426796.649907	51.801959
3345.777891	426505.117296	51.806964
3344.802575	426224.180502	51.811969
3344.162026	425940.343342	51.816973
3343.472167	425670.555750	51.821978
3342.739265	425395.845116	51.826983
3342.046616	425105.023034	51.831988
3341.319105	424839.855512	51.836993
3340.945053	424550.399380	51.841997
3340.264878	424283.669625	51.847002
3339.831738	424004.122507	51.852007
3339.183284	423719.044142	51.857012
3338.209794	423445.545571	51.862017
3337.531119	423161.405945	51.867021
3337.027036	422878.150159	51.872026
3336.203967	422594.154489	51.877031
3335.567443	422319.473778	51.882036
3334.868360	422039.110447	51.887041
3334.120420	421762.638354	51.892045
3333.021596	421492.696317	51.897050
3332.714003	421210.027351	51.902055
3332.606917	420929.406745	51.907060
3331.330884	420653.743767	51.912065
3330.964965	420379.839296	51.917069
3330.435648	420105.805564	51.922074
3329.542547	419821.843380	51.927079
3328.898474	419543.503817	51.932084
3328.094921	419272.375853	51.937089
3327.550324	418984.869834	51.942093
3326.471442	418714.516747	51.947098
3326.221444	418438.771340	51.952103
3325.610025	418153.325153	51.957108
3324.358439	417890.663609	51.962113
3323.933468	417614.658411	51.967117
3323.283841	417346.053529	51.972122
3322.535260	417066.893172	51.977127
3321.837074	416805.531388	51.982132
3321.145818	416534.308691	51.987137
3320.963958	416252.027473	51.992141
3319.923393	415982.480793	51.997146
3319.300645	415704.151085	52.002151
3318.798832	415430.880911	52.007156
3317.678340	415164.946988	52.012161
3317.535066	414888.032601	52.017165
3316.601759	414618.405422	52.022170
3315.871520	414341.858146	52.027175
3315.137333	414070.669940	52.032180
3314.173628	413804.800410	52.037185
3314.071751	413534.675999	52.042189
3313.180050	413275.345636	52.047194
3312.430854	413010.502135	52.052199
3311.842286	412732.265675	52.057204
3311.131994	412465.352984	52.062209
3310.452594	412191.445372	52.067213
3309.728769	411924.834857	52.072218
3309.364071	411659.334005	52.077223
3308.711839	411387.244189	52.082228
3307.514663	411111.934717	52.087233
3307.289500	410845.413531	52.092237
3306.576261	410593.756315	52.097242
3305.782553	410307.982564	52.102247
3305.243195	410044.959867	52.107252
3304.260325	409769.731218	52.112257
3303.499485	409510.626859	52.117261
3303.366840	409247.354990	52.122266
3302.373578	408982.844691	52.127271
3301.781753	408711.534280	52.132276
3300.988748	408456.339510	52.137281
3300.555642	408180.831578	52.142285
3299.708742	407920.761563	52.147290
3298.644781	407652.235603	52.152295
3298.492061	407389.077907	52.157300
3297.674479	407126.938012	52.162305
3297.244968	406864.327877	52.167309
3296.322484	406598.794597	52.172314
3295.719126	406334.275963	52.177319
3295.209999	406059.650536	52.182324
3294.379073	405793.765472	52.187329
3293.741109	405524.213249	52.192333
3292.803465	405268.430373	52.197338
3292.412184	404996.572603	52.202343
3291.750195	404742.597153	52.207348
3291.174022	404484.310772	52.212353
3290.496299	404213.126908	52.217357
3289.590607	403954.456215	52.222362
3288.794312	403684.176122	52.227367
3288.068417	403424.100143	52.232372
3287.187055	403168.392929	52.237377
3286.711218	402910.357375	52.242381
3286.158856	402650.781367	52.247386
3285.535755	402403.008217	52.252391
3284.827675	402141.241353	52.257396
3284.083429	401879.325557	52.262401
3283.209069	401613.691715	52.267405
3282.223687	401350.793012	52.272410
3281.774923	401104.202325	52.277415
3281.001312	400848.281573	52.282420
3280.102293	400605.520286	52.287425
3279.814053	400356.382010	52.292429
3279.123120	400106.593773	52.297434
3278.348028	399856.105176	52.302439
3277.648848	399599.247683	52.307444
3276.998148	399351.684235	52.312449
3276.585343	399100.547870	52.317453
3275.553026	398845.694507	52.322458
3274.676724	398599.533761	52.327463
3274.344001	398355.293434	52.332468
3273.438927	398113.582247	52.337473
3273.453547	397855.937255	52.342477
3272.644390	397613.546287	52.347482
3271.571975	397347.502279	52.352487
3271.147862	397105.326330	52.357492
3270.089144	396862.130436	52.362497
3269.645581	396611.539307	52.367501
3268.923017	396374.413424	52.372506
3268.450376	396124.941833	52.377511
3268.027904	395873.985935	52.382516
3267.002471	395631.563942	52.387521
3266.235158	395382.057183	52.392525
3265.640686	395129.622988	52.397530
3264.709196	394890.155334	52.402535
3264.235322	394643.215325	52.407540
3263.516607	394393.998684	52.412545
3263.132491	394145.591707	52.417549
3262.304081	393909.126296	52.422554
3261.515195	393661.415430	52.427559
3261.212273	393414.414062	52.432564
3259.999109	393176.758655	52.437569
3259.849119	392917.195133	52.442573
3259.104670	392674.809358	52.447578
3258.414571	392423.972095	52.452583
3257.544693	392178.399098	52.457588
3257.068030	391940.161020	52.462593
3256.395759	391696.434852	52.467597
3255.559552	391457.970665	52.472602
3254.735106	391208.010364	52.477607
3254.433807	390952.905679	52.482612
3253.273196	390719.725604	52.487617
3252.772753	390473.344804	52.492621
3252.224471	390232.512906	52.497626
3251.487799	389992.319415	52.502631
3250.943035	389761.324013	52.507636
3250.274863	389510.818397	52.512641
3249.716749	389261.539556	52.517645
3248.501885	389029.806287	52.522650
3248.150221	388781.584822	52.527655
3247.781238	388540.662232	52.532660
3246.684950	388299.166512	52.537665
3246.406734	388048.283808	52.542669
3245.569391	387816.711824	52.547674
3244.621036	387573.382398	52.552679
3244.392882	387330.013691	52.557684
3243.453703	387095.528866	52.562689
3242.902941	386846.537256	52.567693
3242.413348	386609.689539	52.572698
3241.452864	386368.362875	52.577703
3240.848507	386117.874419	52.582708
3239.868519	385879.599186	52.587713
3239.313222	385636.245491	52.592717
3239.002206	385406.685611	52.597722
3238.156479	385171.487043	52.602727
3237.511603	384931.906569	52.607732
3236.690325	384690.623159	52.612737
3236.313568	384447.029935	52.617741
3235.299203	384212.284278	52.622746
3234.489276	383972.138805	52.627751
3234.548001	383730.455642	52.632756
3233.322070	383484.803366	52.637761
3232.737247	383255.934739	52.642765
3232.338199	383021.516608	52.647770
3231.689466	382778.998257	52.652775
3231.030880	382537.522628	52.657780
3229.728552	382307.922490	52.662785
3229.240461	382056.905112	52.667789
3228.639476	381818.467696	52.672794
3228.001879	381596.362478	52.677799
3227.493677	381353.100663	52.682804
3226.923023	381123.021566	52.687809
3225.898323	380877.549454	52.692813
3225.275399	380648.391382	52.697818
3224.388077	380413.246000	52.702823
3224.030310	380173.157555	52.707828
3223.424196	379952.640182	52.712833
3222.728138	379703.624160	52.717837
3222.065295	379468.056015	52.722842
3221.358057	379234.731696	52.727847
3220.868699	378995.801343	52.732852
3220.043943	378771.979945	52.737857
3219.607078	378527.391924	52.742861
3218.918537	378296.068410	52.747866
3217.937341	378051.716155	52.752871
3217.545885	377819.783274	52.757876
3216.784409	377590.400248	52.762881
3216.332311	377339.244923	52.767885
3215.366653	377114.317250	52.772890
3214.685932	376878.761882	52.777895
3214.117869	376634.767959	52.782900
3213.307411	376403.249217	52.787905
3212.409526	376170.369405	52.792909
3211.895883	375943.684841	52.797914
3211.493797	375710.851117	52.802919
3210.910872	375477.408740	52.807924
3209.932281	375246.266067	52.812929
3209.305673	375003.899500	52.817933
3208.579599	374775.257910	52.822938
3207.813784	374548.758065	52.827943
3207.492201	374310.765230	52.832948
3206.791491	374079.063227	52.837953
3205.961827	373845.167227	52.842957
3205.150875	373617.015920	52.847962
3204.250884	373391.217744	52.852967
3203.719943	373161.137199	52.857972
3202.946877	372939.997120	52.862977
3202.453451	372708.636212	52.867981
3201.993106	372475.131936	52.872986
3201.094679	372252.685231	52.877991
3200.542743	372015.936713	52.882996
3199.671133	371802.743153	52.888001
3198.927105	371570.474353	52.893005
3198.298321	371346.657347	52.898010
3197.190821	371120.370945	52.903015
3197.052927	370893.853611	52.908020
3196.307809	370684.094180	52.913025
3195.444020	370454.051462	52.918029
3195.154203	370231.752221	52.923034
3194.258508	370012.193457	52.928039
3193.950634	369782.542534	52.933044
3193.106382	369562.693487	52.938049
3192.570224	369324.197525	52.943053
3191.787482	369103.954798	52.948058
3191.025606	368877.983462	52.953063
3190.450979	368653.609544	52.958068
3189.433687	368434.672573	52.963073
3188.940024	368204.406638	52.968077
3188.206729	367986.287485	52.973082
3187.435355	367765.908978	52.978087
3187.065518	367536.764806	52.983092
3186.537849	367321.433833	52.988097
3185.671532	367098.497388	52.993101
3184.856521	366884.303744	52.998106
3184.004426	366659.403804	53.003111
3183.611967	366422.268611	53.008116
3183.168726	366222.947552	53.013121
3182.096624	365999.427532	53.018125
3181.841297	365779.847983	53.023130
3181.028128	365554.071264	53.028135
3180.341149	365317.612883	53.033140
3179.741486	365105.386625	53.038145
3179.243131	364875.994680	53.043149
3178.481482	364661.807406	53.048154
3177.840223	364443.198372	53.053159
3177.312778	364208.668098	53.058164
3176.237817	363986.410743	53.063169
3175.934143	363756.804250	53.068173
3175.250659	363528.986885	53.073178
3174.411295	363314.576597	53.078183
3174.086037	363094.333599	53.083188
3173.145328	362875.713584	53.088193
3172.525317	362641.368071	53.093197
3171.589957	362425.391300	53.098202
3171.162997	362206.534180	53.103207
3170.979570	361973.363014	53.108212
3169.724394	361756.670409	53.113217
3168.972440	361535.469758	53.118221
3168.695774	361306.635675	53.123226
3167.775735	361083.271219	53.128231
3167.005459	360851.357825	53.133236
3166.463153	360633.122326	53.138241
3166.080919	360405.852766	53.143245
3165.074372	360187.383331	53.148250
3164.760297	359962.238313	53.153255
3163.672306	359737.189244	53.158260
3163.043962	359525.654579	53.163265
3162.504822	359302.654102	53.168269
3162.157528	359072.955316	53.173274
3160.987863	358859.365897	53.178279
3160.422042	358640.208995	53.183284
3159.615612	358406.991750	53.188289
3159.073145	358184.012108	53.193293
3158.433269	357960.334351	53.198298
3157.663378	357751.918881	53.203303
3157.076216	357517.797513	53.208308
3156.304546	357307.675490	53.213313
3155.561551	357085.664146	53.218317
3155.038460	356873.745086	53.223322
3154.392429	356656.907755	53.228327
3153.985647	356430.310627	53.233332
3153.207202	356208.402772	53.238337
3152.631116	355992.874778	53.243341
3151.896451	355773.426515	53.248346
3151.097090	355552.944163	53.253351
3150.516523	355318.353374	53.258356
3149.751465	355112.165562	53.263361
3149.102329	354888.093784	53.268365
3148.573220	354665.783425	53.273370
3147.856916	354448.845935	53.278375
3147.316126	354231.625266	53.283380
3146.333718	354014.066377	53.288385
3145.854963	353796.248731	53.293389
3145.167333	353576.274599	53.298394
3144.392162	353362.752025	53.303399
3143.794640	353123.623934	53.308404
3143.124804	352912.042439	53.313409
3142.331731	352703.584426	53.318413
3141.745126	352475.064078	53.323418
3140.993004	352258.835689	53.328423
3140.992008	352048.442813	53.333428
3139.790395	351829.331611	53.338433
3139.532245	351600.984554	53.343437
3138.873123	351379.520601	53.348442
3137.735874	351159.454798	53.353447
3137.442869	350921.464705	53.358452
3136.740594	350710.515803	53.363457
3135.845416	350489.009168	53.368461
3135.637742	350275.053482	53.373466
3134.926920	350048.680244	53.378471
3134.112284	349814.941738	53.383476
3132.954486	349597.061586	53.388481
3132.491319	349375.914712	53.393485
3131.920229	349158.041774	53.398490
3131.097634	348937.026359	53.403495
3130.599020	348717.867645	53.408500
3129.951510	348513.595285	53.413505
3129.276546	348284.053103	53.418509
3128.522651	348071.905962	53.423514
3127.898741	347847.037007	53.428519
3127.264049	347620.845356	53.433524
3126.719980	347402.452211	53.438529
3126.030316	347175.656618	53.443533
3125.451564	346953.678478	53.448538
3124.619448	346747.163641	53.453543
3124.235982	346513.826611	53.458548
3123.456757	346293.430208	53.463553
3122.417513	346079.666318	53.468557
3121.752700	345861.311803	53.473562
3121.159972	345647.297474	53.478567
3120.783483	345420.445342	53.483572
3119.941739	345206.494238	53.488577
3119.251003	344989.591347	53.493581
3118.592613	344773.522482	53.498586
3117.684859	344560.572121	53.503591
3117.202155	344336.965135	53.508596
3116.296205	344113.729716	53.513601
3115.868028	343892.046871	53.518605
3115.331650	343686.696089	53.523610
3114.696899	343460.080860	53.528615
3114.018898	343236.551523	53.533620
3113.086446	343021.970483	53.538625
3112.512064	342810.513758	53.543629
3111.891662	342594.354566	53.548634
3110.858940	342381.594345	53.553639
3110.428072	342146.363829	53.558644
3109.612945	341952.760185	53.563649
3109.145550	341733.773728	53.568653
3108.421537	341525.136181	53.573658
3107.672538	341315.254601	53.578663
3107.359144	341098.226959	53.583668
3106.275632	340892.469627	53.588673
3105.775530	340676.386421	53.593677
3105.263917	340455.671480	53.598682
3104.166336	340252.968848	53.603687
3103.652199	340035.460154	53.608692
3103.232069	339821.855934	53.613697
3102.128117	339604.235442	53.618701
3101.564415	339403.812922	53.623706
3100.870397	339195.850112	53.628711
3100.497063	338978.850054	53.633716
3099.628016	338775.597392	53.638721
3099.243676	338565.190682	53.643725
3098.503476	338346.490088	53.648730
3097.825019	338143.994390	53.653735
3097.247640	337923.331943	53.658740
3096.617171	337711.841332	53.663745
3095.943309	337494.832914	53.668749
3095.184587	337278.371784	53.673754
3094.401786	337065.604915	53.678759
3093.843965	336855.703781	53.683764
3093.079275	336645.783804	53.688769
3092.360304	336427.149778	53.693773
3091.921533	336216.005856	53.698778
3091.168979	336009.162196	53.703783
3090.881353	335797.331153	53.708788
3089.737360	335583.802071	53.713793
3089.126837	335361.710712	53.718797
3088.786908	335154.086321	53.723802
3087.609774	334936.563677	53.728807
3087.617093	334716.816308	53.733812
3086.731193	334504.566751	53.738817
3085.976315	334294.994283	53.743821
3085.614574	334078.179954	53.748826
3084.897849	333863.788675	53.753831
3084.073947	333643.405696	53.758836
3083.334143	333428.049332	53.763841
3082.664668	333208.938879	53.768845
3082.155515	332986.569220	53.773850
3081.445696	332782.560325	53.778855
3080.915391	332565.131519	53.783860
3079.970313	332351.815523	53.788865
3079.112659	332132.807880	53.793869
3078.592231	331928.181015	53.798874
3077.768582	331713.163646	53.803879
3077.307045	331498.775701	53.808884
3076.944571	331288.801212	53.813889
3075.920079	331074.781146	53.818893
3075.488950	330864.154371	53.823898
3074.664661	330654.556640	53.828903
3074.244605	330428.422516	53.833908
3073.335425	330211.250242	53.838913
3072.913322	329997.055311	53.843917
3072.437569	329784.064823	53.848922
3071.429942	329566.626190	53.853927
3070.623565	329343.808654	53.858932
3069.824442	329136.493965	53.863937
3069.564626	328918.578668	53.868941
3068.815500	328707.410535	53.873946
3068.158537	328492.815665	53.878951
3067.507176	328274.782271	53.883956
3066.752654	328071.811184	53.888961
3066.019722	327848.748495	53.893965
3065.567277	327628.237657	53.898970
3064.917446	327416.108238	53.903975
3064.205432	327204.879177	53.908980
3063.327216	326994.516025	53.913985
3062.778104	326777.353325	53.918989
3062.435989	326556.796536	53.923994
3061.343428	326343.333980	53.928999
3060.947755	326132.051969	53.934004
3060.511059	325918.611769	53.939009
3059.351255	325697.978331	53.944013
3059.002537	325484.293907	53.949018
3058.238312	325267.110214	53.954023
3057.516191	325047.933353	53.959028
3056.492484	324829.211004	53.964033
3056.022433	324618.420551	53.969037
3055.536789	324409.821649	53.974042
3054.769981	324207.937448	53.979047
3054.075526	323987.862248	53.984052
3053.493769	323774.210244	53.989057
3053.217974	323557.886784	53.994061
3052.323506	323339.496497	53.999066
3051.791322	323120.106241	54.004071
3051.029293	322904.087211	54.009076
3050.160833	322692.973038	54.014081
3049.264060	322469.284932	54.019085
3048.681987	322263.089328	54.024090
3048.130903	322055.971714	54.029095
3047.611514	321838.663985	54.034100
3046.954192	321622.294161	54.039105
3046.362541	321416.760061	54.044109
3045.839775	321200.800745	54.049114
3045.166422	320975.953120	54.054119
3044.625496	320747.799388	54.059124
3043.443752	320546.787021	54.064129
3042.908187	320333.221036	54.069133
3042.193985	320116.703763	54.074138
3041.306800	319898.762013	54.079143
3040.867112	319689.991661	54.084148
3040.386677	319476.134843	54.089153
3039.730653	319259.759093	54.094157
3039.091023	319036.199870	54.099162
3038.372164	318823.626926	54.104167
3037.860911	318605.418903	54.109172
3037.095296	318396.875447	54.114177
3036.555737	318181.217162	54.119181
3036.124035	317955.967376	54.124186
3035.088812	317756.886339	54.129191
3034.701244	317520.883296	54.134196
3033.731780	317303.508675	54.139201
3033.019275	317076.951735	54.144205
3032.614727	316876.775996	54.149210
3031.608187	316663.912736	54.154215
3031.335492	316439.219878	54.159220
3030.878179	316220.030285	54.164225
3030.088966	316006.341845	54.169229
3029.324601	315778.338713	54.174234
3028.319492	315567.764547	54.179239
3028.002396	315339.129428	54.184244
3027.207951	315117.011571	54.189249
3026.389691	314905.769865	54.194253
3025.786798	314690.343091	54.199258
3024.822412	314483.045012	54.204263
3024.317878	314259.173348	54.209268
3023.540613	314061.495489	54.214273
3022.664394	313842.927263	54.219277
3022.522101	313630.608335	54.224282
3021.544001	313420.178276	54.229287
3021.124757	313200.110412	54.234292
3020.234293	312997.483031	54.239297
3019.520664	312784.743571	54.244301
3018.707818	312564.125569	54.249306
3018.237653	312360.717472	54.254311
3017.562433	312142.750549	54.259316
3016.886127	311944.085155	54.264321
3016.420479	311725.651343	54.269325
3015.498262	311511.312714	54.274330
3014.845479	311313.584641	54.279335
3014.110644	311099.622989	54.284340
3013.580990	310893.726113	54.289345
3012.926105	310683.443347	54.294349
3012.355517	310465.201945	54.299354
3011.489712	310259.357134	54.304359
3011.007783	310053.654906	54.309364
3009.955052	309837.958697	54.314369
3009.377246	309631.939862	54.319373
3008.954678	309415.099074	54.324378
3008.258288	309217.323371	54.329383
3007.482151	309015.587461	54.334388
3006.641305	308803.497283	54.339393
3006.263865	308591.409770	54.344397
3005.687564	308379.989987	54.349402
3005.076717	308179.321505	54.354407
3004.386249	307963.157131	54.359412
3003.858394	307755.242768	54.364417
3003.250336	307537.129264	54.369421
3002.717491	307329.851607	54.374426
3001.746901	307115.869174	54.379431
3000.969625	306907.738236	54.384436
3000.347541	306689.472696	54.389441
2999.658988	306483.058658	54.394445
2999.104594	306278.838535	54.399450
2998.112392	306071.809811	54.404455
2997.506546	305849.134779	54.409460
2997.446925	305643.358350	54.414465
2996.410686	305440.053557	54.419469
2996.169763	305214.034647	54.424474
2995.107279	305005.767575	54.429479
2994.710382	304784.789350	54.434484
2994.098923	304578.843993	54.439489
2993.459290	304366.434506	54.444493
2992.582191	304150.828138	54.449498
2991.947131	303942.848314	54.454503
2991.526311	303718.434298	54.459508
2990.535895	303511.324995	54.464513
2989.819809	303296.939658	54.469517
2989.724931	303078.432051	54.474522
2988.863906	302864.985788	54.479527
2988.072061	302638.107690	54.484532
2987.376980	302425.322099	54.489537
2986.651737	302210.350897	54.494541
2986.207116	301988.637379	54.499546
2985.454395	301773.720833	54.504551
2984.843426	301560.182181	54.509556
2983.847039	301344.565084	54.514561
2983.111013	301143.447689	54.519565
2982.647175	300916.846143	54.524570
2981.863770	300711.279094	54.529575
2981.283902	300497.912324	54.534580
2980.523418	300284.726658	54.539585
2979.631970	300074.006217	54.544589
2979.430214	299853.626405	54.549594
2978.350199	299658.928201	54.554599
2978.032881	299444.143290	54.559604
2977.184765	299230.180659	54.564609
2976.325552	299017.289108	54.569613
2976.024356	298813.375060	54.574618
2975.212440	298606.969490	54.579623
2974.427311	298394.014499	54.584628
2974.149183	298184.773522	54.589633
2973.237544	297968.807503	54.594637
2972.760833	297749.181555	54.599642
2971.408870	297550.754928	54.604647
2971.168962	297339.698762	54.609652
2970.533610	297128.577620	54.614657
2970.022335	296924.796517	54.619661
2969.379437	296716.299185	54.624666
2968.256316	296507.037235	54.629671
2967.809889	296295.121230	54.634676
2967.023095	296090.440562	54.639681
2966.314341	295879.049499	54.644685
2965.828731	295671.697604	54.649690
2965.094231	295475.386665	54.654695
2964.756277	295264.216374	54.659700
2964.315938	295050.031483	54.664705
2963.180449	294835.014131	54.669709
2962.751649	294617.847301	54.674714
2961.986691	294414.791355	54.679719
2961.428903	294200.904311	54.684724
2960.874137	293993.154179	54.689729
2959.747989	293774.747113	54.694733
2959.326029	293564.250542	54.699738
2958.391737	293361.373205	54.704743
2957.845257	293160.624477	54.709748
2957.182594	292946.905605	54.714753
2956.580121	292749.730805	54.719757
2956.012374	292534.595811	54.724762
2955.277972	292326.898026	54.729767
2954.674640	292118.440748	54.734772
2953.909531	291914.440242	54.739777
2953.466738	291694.598680	54.744781
2953.114312	291487.781986	54.749786
2952.108702	291277.121059	54.754791
2951.224396	291056.559332	54.759796
2950.837768	290849.289107	54.764801
2949.965514	290643.241639	54.769805
2949.855018	290420.162898	54.774810
2948.859196	290219.915811	54.779815
2947.954558	290011.300741	54.784820
2947.616235	289803.308946	54.789825
2946.632385	289584.951962	54.794829
2946.449054	289362.622441	54.799834
2945.593184	289157.004195	54.804839
2944.988894	288951.345971	54.809844
2944.209923	288736.954338	54.814849
2943.573450	288522.743730	54.819853
2943.118670	288302.239118	54.824858
2942.388064	288092.703720	54.829863
2941.871119	287883.872920	54.834868
2940.983067	287666.594464	54.839873
2940.368845	287450.826049	54.844877
2939.954175	287228.786258	54.849882
2939.107571	287016.135965	54.854887
2938.231278	286797.454334	54.859892
2937.340138	286583.639295	54.864897
2936.954867	286366.840685	54.869901
2936.163339	286163.375085	54.874906
2935.178917	285965.568340	54.879911
2934.606511	285749.486623	54.884916
2933.954570	285536.753686	54.889921
2933.408824	285340.761792	54.894925
2932.864460	285121.262561	54.899930
2932.229110	284911.124398	54.904935
2931.472688	284701.132636	54.909940
2930.762017	284489.860119	54.914945
2929.977448	284284.737011	54.919949
2929.740417	284075.808770	54.924954
2928.943212	283869.057509	54.929959
2928.561716	283659.820860	54.934964
2927.679769	283446.053616	54.939969
2926.667181	283239.387112	54.944973
2925.993312	283013.973246	54.949978
2925.118575	282801.910947	54.954983
2924.381243	282594.563890	54.959988
2923.785041	282389.435610	54.964993
2923.151876	282188.668170	54.969997
2922.864301	281992.735841	54.975002
2922.065098	281786.569814	54.980007
2921.535797	281567.015619	54.985012
2920.651026	281363.282478	54.990017
2920.097556	281162.094579	54.995021
2919.612221	280951.523504	55.000026
2918.908484	280746.870116	55.005031
2917.997364	280533.335603	55.010036
2917.309607	280337.236911	55.015041
2916.574531	280129.073685	55.020045
2916.197092	279910.615516	55.025050
2915.174372	279716.938256	55.030055
2914.731597	279501.750267	55.035060
2914.218494	279306.209443	55.040065
2913.384889	279099.360446	55.045069
2912.884773	278895.489335	55.050074
2912.031548	278691.928775	55.055079
2911.568359	278471.166221	55.060084
2911.099199	278276.458695	55.065089
2910.386031	278068.546226	55.070093
2909.625886	277849.944450	55.075098
2909.041025	277642.877522	55.080103
2908.629197	277426.818302	55.085108
2908.009923	277219.629424	55.090113
2907.145630	277004.558652	55.095117
2906.578705	276781.672915	55.100122
2905.912628	276584.958882	55.105127
2905.264054	276368.656874	55.110132
2904.562221	276160.003798	55.115137
2903.675514	275948.705799	55.120141
2903.209667	275733.291677	55.125146
2902.013185	275538.571691	55.130151
2901.475981	275325.486473	55.135156
2901.069815	275112.864401	55.140161
2900.311480	274908.626253	55.145165
2899.739641	274697.023677	55.150170
2898.910783	274488.186917	55.155175
2898.269212	274275.194627	55.160180
2897.529661	274062.676288	55.165185
2897.194707	273859.313450	55.170189
2896.434175	273640.813383	55.175194
2895.636223	273445.011585	55.180199
2895.040260	273227.809843	55.185204
2894.731927	273016.242025	55.190209
2894.075286	272807.861990	55.195213
2893.311345	272597.079471	55.200218
2892.651783	272386.840753	55.205223
2891.921242	272170.806512	55.210228
2891.320965	271957.655070	55.215233
2890.579188	271756.139637	55.220237
2890.115410	271534.536619	55.225242
2888.946742	271326.849103	55.230247
2888.261130	271120.231211	55.235252
2888.003177	270906.669187	55.240257
2886.949375	270692.469177	55.245261
2886.669276	270491.059144	55.250266
2885.744145	270279.640368	55.255271
2885.154697	270068.397702	55.260276
2884.558183	269855.271552	55.265281
2883.656968	269651.718853	55.270285
2883.279818	269444.364851	55.275290
2882.422571	269238.436747	55.280295
2881.863362	269034.295224	55.285300
2881.205588	268814.531845	55.290305
2880.478472	268609.169090	55.295309
2879.979376	268402.114856	55.300314
2879.274697	268198.658799	55.305319
2878.769485	267987.658092	55.310324
2878.250324	267772.610218	55.315329
2877.339161	267559.025251	55.320333
2877.049767	267344.043028	55.325338
2876.323901	267128.646110	55.330343
2875.395975	266909.002619	55.335348
2874.548891	266690.288744	55.340353
2873.861833	266491.669481	55.345357
2873.426628	266272.228396	55.350362
2872.772428	266059.723959	55.355367
2872.160602	265845.353735	55.360372
2871.664124	265629.360855	55.365377
2870.686560	265422.027016	55.370381
2869.993583	265202.194309	55.375386
2869.128973	264994.358896	55.380391
2868.324785	264778.720789	55.385396
2868.375734	264575.706880	55.390401
2867.603255	264361.770335	55.395405
2867.044962	264148.182011	55.400410
2865.817231	263937.170213	55.405415
2865.307521	263714.202209	55.410420
2865.065234	263504.715496	55.415425
2864.006039	263298.388955	55.420429
2863.735117	263077.522841	55.425434
2862.851414	262862.178577	55.430439
2862.074385	262650.790554	55.435444
2861.515484	262442.577079	55.440449
2860.826699	262230.334909	55.445453
2860.182371	262010.547345	55.450458
2859.421167	261801.653218	55.455463
2858.961727	261584.408926	55.460468
2858.292478	261375.958944	55.465473
2857.301463	261171.558507	55.470477
2856.957214	260941.587997	55.475482
2856.239315	260741.397726	55.480487
2855.426341	260531.035549	55.485492
2855.012268	260317.477825	55.490497
2854.344927	260110.581977	55.495501
2853.667039	259883.160991	55.500506
2853.113792	259678.412154	55.505511
2852.317730	259454.422910	55.510516
2851.915242	259240.329373	55.515521
2851.036329	259026.056781	55.520525
2850.581071	258799.390963	55.525530
2849.578945	258598.712468	55.530535
2848.901020	258375.800556	55.535540
2848.288303	258159.219932	55.540545
2847.696277	257947.806126	55.545549
2847.239627	257727.049969	55.550554
2846.148258	257520.630840	55.555559
2845.427876	257290.952309	55.560564
2845.057007	257081.872722	55.565569
2844.218845	256863.851874	55.570573
2843.681432	256655.333867	55.575578
2842.892251	256453.757574	55.580583
2842.338347	256231.210071	55.585588
2841.634008	256026.360916	55.590593
2840.771061	255808.166758	55.595597
2840.193187	255601.184196	55.600602
2839.361914	255397.960179	55.605607
2838.828608	255185.775654	55.610612
2838.390451	254971.055028	55.615617
2837.633316	254769.449783	55.620621
2836.766884	254559.101361	55.625626
2836.448519	254349.201171	55.630631
2835.325673	254125.803731	55.635636
2834.736560	253914.495257	55.640641
2834.068941	253708.216443	55.645645
2833.749877	253501.908116	55.650650
2832.532368	253296.098835	55.655655
2832.026036	253081.492930	55.660660
2831.800148	252876.265605	55.665665
2830.814882	252674.214793	55.670669
2830.297205	252449.119067	55.675674
2829.743755	252248.019010	55.680679
2828.886236	252031.814603	55.685684
2828.477534	251817.220183	55.690689
2827.484224	251610.409554	55.695693
2827.194702	251400.915573	55.700698
2826.406667	251190.864128	55.705703
2825.457938	250971.288406	55.710708
2825.190524	250752.852927	55.715713
2824.043509	250551.772425	55.720717
2823.567134	250336.528431	55.725722
2822.845609	250130.848007	55.730727
2822.393730	249922.553022	55.735732
2821.620482	249717.212371	55.740737
2821.117797	249506.608518	55.745741
2820.611368	249281.540641	55.750746
2819.799793	249068.210451	55.755751
2819.113551	248862.602450	55.760756
2818.903334	248655.085757	55.765761
2817.695704	248435.809114	55.770765
2817.202727	248216.190403	55.775770
2816.370193	248002.559397	55.780775
2815.902098	247784.898258	55.785780
2815.205897	247576.797872	55.790785
2814.543696	247368.794254	55.795789
2813.918354	247140.819743	55.800794
2813.226423	246938.856880	55.805799
2812.591458	246716.665325	55.810804
2812.082007	246505.684690	55.815809
2811.196359	246296.444691	55.820813
2810.807975	246076.354201	55.825818
2810.073031	245863.449358	55.830823
2809.515366	245640.585121	55.835828
2809.038619	245417.835752	55.840833
2808.022227	245209.764030	55.845837
2807.532029	244989.156597	55.850842
2806.754826	244773.611693	55.855847
2806.151855	244565.933854	55.860852
2805.901794	244338.923058	55.865857
2804.631207	244120.859861	55.870861
2803.654073	243894.270562	55.875866
2803.525518	243678.242707	55.880871
2802.422311	243470.900460	55.885876
2801.980646	243251.052172	55.890881
2801.093234	243043.982013	55.895885
2800.665087	242816.874730	55.900890
2799.896127	242611.569074	55.905895
2799.146764	242403.637739	55.910900
2798.858842	242181.169502	55.915905
2797.924038	241978.615907	55.920909
2797.422397	241752.769970	55.925914
2796.710283	241548.832164	55.930919
2795.976353	241326.359707	55.935924
2795.208293	241114.079003	55.940929
2794.450928	240909.512812	55.945933
2794.249129	240693.119720	55.950938
2793.392567	240480.930544	55.955943
2792.423303	240269.625396	55.960948
2791.979245	240049.070175	55.965953
2791.621407	239839.451480	55.970957
2790.916208	239618.174496	55.975962
2790.134845	239407.859724	55.980967
2789.385001	239193.211390	55.985972
2788.887996	238970.476665	55.990977
2788.190045	238755.235254	55.995981
2787.718416	238540.620476	56.000986
2787.068419	238326.976537	56.005991
2786.084248	238106.255961	56.010996
2785.661871	237882.467538	56.016001
2784.726637	237676.331020	56.021005
2784.226066	237451.486364	56.026010
2783.460208	237244.177951	56.031015
2782.711216	237028.311377	56.036020
2782.380873	236805.401819	56.041025
2781.528476	236594.594343	56.046029
2781.091925	236375.954962	56.051034
2780.384690	236160.389089	56.056039
2779.607236	235941.753674	56.061044
2779.274499	235726.893281	56.066049
2777.874852	235509.172157	56.071053
2777.375712	235285.986979	56.076058
2777.062323	235072.652686	56.081063
2776.304909	234849.483899	56.086068
2775.830952	234637.856530	56.091073
2774.820972	234424.939486	56.096077
2774.369642	234202.945876	56.101082
2773.800308	233986.115013	56.106087
2773.038753	233768.627562	56.111092
2772.301785	233549.125109	56.116097
2771.604741	233339.598326	56.121101
2771.154854	233111.037463	56.126106
2770.201760	232903.843836	56.131111
2769.394608	232681.247966	56.136116
2769.112497	232470.893437	56.141121
2768.152817	232260.493916	56.146125
2767.923434	232030.016432	56.151130
2767.266107	231821.377835	56.156135
2766.427456	231596.217748	56.161140
2765.751721	231380.886383	56.166145
2764.909993	231159.776366	56.171149
2764.444911	230941.077063	56.176154
2763.675974	230724.183305	56.181159
2762.939349	230511.180665	56.186164
2762.767386	230290.603184	56.191169
2761.757549	230078.281380	56.196173
2760.879211	229851.043918	56.201178
2760.263490	229641.079604	56.206183
2759.284871	229428.041439	56.211188
2758.998337	229204.938546	56.216193
2758.110517	229001.537075	56.221197
2757.728314	228781.862281	56.226202
2756.965474	228579.078524	56.231207
2756.008110	228361.558280	56.236212
2755.855530	228142.459783	56.241217
2754.952528	227931.908474	56.246221
2754.489171	227710.670597	56.251226
2754.143217	227493.335744	56.256231
2753.073327	227275.886961	56.261236
2752.874636	227048.039832	56.266241
2751.707180	226838.169616	56.271245
2750.875401	226615.363403	56.276250
2750.046828	226416.643456	56.281255
2749.624844	226193.136915	56.286260
2749.306921	225976.132490	56.291265
2748.320436	225765.727059	56.296269
2747.904096	225545.633115	56.301274
2747.120890	225332.930568	56.306279
2746.370578	225108.766048	56.311284
2745.691868	224889.962988	56.316289
2744.852460	224683.190622	56.321293
2744.211424	224469.589406	56.326298
2743.400943	224261.145870	56.331303
2742.993913	224055.910618	56.336308
2742.747332	223832.739158	56.341313
2741.581676	223622.189417	56.346317
2740.977196	223404.804397	56.351322
2740.543898	223197.245908	56.356327
2739.391615	222989.738208	56.361332
2739.180792	222770.268501	56.366337
2738.256791	222558.410317	56.371341
2737.909619	222343.648023	56.376346
2737.347508	222131.911890	56.381351
2736.330999	221909.300661	56.386356
2735.602940	221691.787218	56.391361
2734.988170	221486.273340	56.396365
2734.385244	221272.254679	56.401370
2733.676900	221058.851615	56.406375
2733.147066	220846.044625	56.411380
2732.784825	220630.245683	56.416385
2731.805429	220415.614410	56.421389
2731.172228	220195.926198	56.426394
2730.415899	219991.113475	56.431399
2729.711240	219780.972209	56.436404
2729.278659	219553.540050	56.441409
2728.611727	219344.106897	56.446413
2727.501226	219126.305041	56.451418
2727.016332	218917.149773	56.456423
2726.656261	218702.501736	56.461428
2725.626727	218488.456827	56.466433
2725.052522	218284.460144	56.471437
2724.909418	218066.839169	56.476442
2723.850111	217847.620103	56.481447
2723.291523	217631.924721	56.486452
2722.868842	217413.433525	56.491457
2722.157153	217196.414435	56.496461
2721.609571	216977.893450	56.501466
2721.143305	216753.135808	56.506471
2720.206576	216534.385082	56.511476
2719.603677	216309.141351	56.516481
2718.667828	216094.108692	56.521485
2718.007457	215871.064840	56.526490
2717.486433	215660.130121	56.531495
2716.822780	215435.153428	56.536500
2716.211440	215212.040296	56.541505
2715.441353	215004.341941	56.546509
2714.733774	214782.429219	56.551514
2714.043956	214563.798372	56.556519
2713.465978	214346.754303	56.561524
2713.067318	214127.149561	56.566529
2712.091782	213911.340895	56.571533
2711.787250	213686.834970	56.576538
2710.986520	213469.650829	56.581543
2709.971499	213249.561111	56.586548
2709.661422	213024.663722	56.591553
2708.891062	212811.791801	56.596557
2708.298731	212588.875302	56.601562
2707.688750	212367.553371	56.606567
2707.055105	212158.200329	56.611572
2706.503313	211932.352189	56.616577
2705.443710	211716.996780	56.621581
2704.775551	211491.423173	56.626586
2704.173385	211280.298797	56.631591
2703.287871	211067.170820	56.636596
2702.828217	210840.077308	56.641601
2702.024314	210627.803359	56.646605
2701.445386	210405.388658	56.651610
2700.749610	210187.117021	56.656615
2700.102153	209974.235003	56.661620
2699.253275	209750.287151	56.666625
2698.565207	209542.364067	56.671629
2698.170896	209330.729611	56.676634
2697.551598	209111.673222	56.681639
2696.922022	208906.937586	56.686644
2696.253378	208679.668625	56.691649
2695.282340	208461.675726	56.696653
2694.820988	208246.644673	56.701658
2694.047719	208035.201964	56.706663
2693.198450	207816.950250	56.711668
2693.027678	207604.268133	56.716673
2691.980358	207400.049165	56.721677
2691.166138	207170.212553	56.726682
2690.660042	206959.507615	56.731687
2689.929615	206753.611572	56.736692
2689.362959	206530.941650	56.741697
2688.746281	206330.628889	56.746701
2688.425331	206108.494325	56.751706
2687.296484	205890.815699	56.756711
2686.985355	205678.328099	56.761716
2686.414051	205456.439273	56.766721
2685.481342	205244.000812	56.771725
2685.128937	205017.993707	56.776730
2684.566646	204805.727229	56.781735
2683.855399	204590.952548	56.786740
2683.263583	204370.623728	56.791745
2682.245615	204150.363264	56.796749
2681.728849	203933.893047	56.801754
2681.225887	203715.372521	56.806759
2680.335799	203496.888709	56.811764
2679.899001	203268.025677	56.816769
2678.971237	203060.124993	56.821773
2678.507385	202833.915036	56.826778
2678.234349	202612.791628	56.831783
2677.202869	202396.103374	56.836788
2676.319560	202171.171500	56.841793
2676.025994	201961.049143	56.846797
2675.159770	201732.247643	56.851802
2674.553528	201516.882533	56.856807
2673.419568	201290.823140	56.861812
2673.292739	201067.582918	56.866817
2672.517194	200864.858352	56.871821
2671.836329	200633.092387	56.876826
2671.236179	200419.843036	56.881831
2670.179491	200193.674095	56.886836
2669.714485	199979.336104	56.891841
2668.821183	199769.011696	56.896845
2668.347623	199546.901534	56.901850
2667.647945	199338.024260	56.906855
2666.680107	199123.743868	56.911860
2666.188937	198901.931828	56.916865
2665.679916	198701.514531	56.921869
2664.768121	198477.773039	56.926874
2664.305258	198254.572156	56.931879
2663.413857	198047.091868	56.936884
2663.328843	197833.440267	56.941889
2662.560724	197617.060106	56.946893
2661.945169	197395.808490	56.951898
2661.387127	197176.673732	56.956903
2660.425956	196966.205692	56.961908
2659.946648	196737.783951	56.966913
2659.078289	196528.130074	56.971917
2658.450453	196306.032455	56.976922
2657.969136	196075.641624	56.981927
2657.508026	195871.206552	56.986932
2656.814858	195650.063709	56.991937
2655.662179	195438.817841	56.996941
2655.351069	195213.277328	57.001946
2654.634043	194993.108141	57.006951
2653.997432	194770.522287	57.011956
2653.405032	194551.976681	57.016961
2652.281797	194338.911144	57.021965
2651.561932	194116.163211	57.026970
2651.040703	193899.161477	57.031975
2650.202794	193694.387663	57.036980
2649.661059	193471.385324	57.041985
2648.955715	193258.716201	57.046989
2648.340626	193048.196723	57.051994
2647.380814	192836.473107	57.056999
2646.526046	192629.632361	57.062004
2646.248837	192414.366995	57.067009
2645.466480	192204.666460	57.072013
2645.069180	191994.765844	57.077018
2644.307596	191779.999870	57.082023
2643.868549	191573.657509	57.087028
2643.165380	191357.751746	57.092033
2642.680768	191151.952763	57.097037
2641.929589	190929.618520	57.102042
2641.345306	190708.938307	57.107047
2640.576069	190491.354675	57.112052
2640.438355	190279.689960	57.117057
2639.507851	190059.487432	57.122061
2638.590934	189839.449158	57.127066
2637.975351	189619.720387	57.132071
2637.302042	189405.765210	57.137076
2637.170786	189186.839558	57.142081
2636.285629	188972.754497	57.147085
2635.748096	188736.592413	57.152090
2634.967470	188516.220586	57.157095
2633.937060	188305.443987	57.162100
2633.678944	188072.625138	57.167105
2632.768629	187858.371001	57.172109
2632.123686	187637.307503	57.177114
2631.728093	187413.597469	57.182119
2631.034362	187204.884369	57.187124
2630.368952	186975.888576	57.192129
2629.613672	186757.391171	57.197133
2628.967880	186535.760546	57.202138
2628.460289	186311.475634	57.207143
2627.304989	186094.596836	57.212148
2626.952634	185863.216120	57.217153
2626.212249	185649.835798	57.222157
2625.653498	185429.570671	57.227162
2625.056804	185212.760195	57.232167
2624.560174	184978.811600	57.237172
2623.588180	184755.078613	57.242177
2622.904276	184539.099355	57.247181
2622.233424	184309.634348	57.252186
2621.815908	184097.215158	57.257191
2620.910187	183878.666337	57.262196
2620.128451	183648.204574	57.267201
2619.498582	183430.186687	57.272205
2618.716294	183211.888712	57.277210
2617.993510	182991.407078	57.282215
2617.466866	182782.255303	57.287220
2616.805561	182556.601367	57.292225
2615.911198	182348.553030	57.297229
2615.268195	182131.624883	57.302234
2614.681685	181913.302293	57.307239
2613.807553	181702.900469	57.312244
2613.502541	181474.638768	57.317249
2612.492076	181270.391967	57.322253
2612.042438	181052.675292	57.327258
2611.409197	180840.471307	57.332263
2610.845430	180628.562640	57.337268
2610.361180	180402.357511	57.342273
2609.676171	180187.557270	57.347277
2608.649081	179975.254584	57.352282
2608.336699	179749.394533	57.357287
2607.358215	179540.113683	57.362292
2606.833001	179318.830686	57.367297
2606.240219	179108.829388	57.372301
2605.518228	178883.509461	57.377306
2604.811707	178678.107461	57.382311
2604.269211	178469.207978	57.387316
2603.819736	178238.111700	57.392321
2602.672732	178020.991577	57.397325
2602.188667	177805.878959	57.402330
2601.812331	177580.205940	57.407335
2600.709754	177371.820401	57.412340
2600.231516	177146.636485	57.417345
2599.535412	176933.673359	57.422349
2598.724647	176718.541791	57.427354
2598.262590	176501.524523	57.432359
2597.311476	176288.605117	57.437364
2597.027558	176069.310610	57.442369
2595.887254	175868.531837	57.447373
2595.270994	175655.880604	57.452378
2595.170485	175439.511161	57.457383
2594.216165	175215.786835	57.462388
2593.403930	174999.176385	57.467393
2592.628665	174792.519887	57.472397
2591.970128	174581.763291	57.477402
2591.661717	174359.403935	57.482407
2590.917740	174144.936636	57.487412
2590.526401	173928.875672	57.492417
2589.839166	173717.021627	57.497421
2588.708595	173502.237462	57.502426
2588.647851	173277.148556	57.507431
2587.520050	173065.723871	57.512436
2586.972550	172845.076824	57.517441
2586.632926	172635.488075	57.522445
2585.741275	172418.687866	57.527450
2584.966686	172201.043631	57.532455
2583.959073	171984.709291	57.537460
2583.613791	171757.957161	57.542465
2582.754870	171550.020710	57.547469
2582.201752	171342.952552	57.552474
2581.938580	171121.824919	57.557479
2581.138129	170903.835846	57.562484
2580.778939	170679.330387	57.567489
2579.725153	170475.856123	57.572493
2579.289041	170255.472953	57.577498
2578.557647	170041.547234	57.582503
2578.075501	169824.340354	57.587508
2577.315772	169601.227156	57.592513
2576.424587	169383.210105	57.597517
2575.553583	169167.289359	57.602522
2575.244070	168938.525964	57.607527
2574.255659	168727.153445	57.612532
2573.964053	168511.462471	57.617537
2573.230648	168300.013742	57.622541
2572.726011	168075.470149	57.627546
2572.021624	167847.704147	57.632551
2570.909627	167639.599901	57.637556
2570.574077	167411.371135	57.642561
2569.585487	167202.219717	57.647565
2568.974840	166983.192752	57.652570
2568.394271	166766.959809	57.657575
2567.756634	166549.897900	57.662580
2567.511304	166342.006774	57.667585
2566.670755	166129.671600	57.672589
2566.117520	165901.562769	57.677594
2565.631808	165672.897857	57.682599
2564.795258	165462.689347	57.687604
2564.032365	165224.420014	57.692609
2563.398062	165019.306291	57.697613
2562.718358	164800.086886	57.702618
2562.263805	164570.711758	57.707623
2561.441550	164353.958918	57.712628
2560.959728	164128.227402	57.717633
2560.206464	163911.211932	57.722637
2559.274499	163688.631494	57.727642
2558.957236	163454.117448	57.732647
2558.310994	163247.044687	57.737652
2557.458229	163015.021427	57.742657
2557.000889	162794.303850	57.747661
2556.286869	162559.947440	57.752666
2555.665146	162286.862391	57.757671
2554.379861	162070.272783	57.762676
2553.866407	161842.284564	57.767681
2553.431476	161628.461694	57.772685
2552.695868	161404.872432	57.777690
2552.322435	161185.168519	57.782695
2551.134231	160971.634233	57.787700
2550.711606	160749.232714	57.792705
2550.224258	160528.190504	57.797709
2549.524154	160312.383311	57.802714
2549.016020	160087.049887	57.807719
2548.147013	159867.191082	57.812724
2547.565051	159638.185272	57.817729
2546.699434	159420.744271	57.822733
2546.080115	159206.278639	57.827738
2545.594926	158987.025575	57.832743
2544.970111	158770.224230	57.837748
2544.559233	158532.578947	57.842753
2543.788120	158308.252062	57.847757
2542.743802	158090.974754	57.852762
2542.459391	157867.692298	57.857767
2541.556331	157649.276624	57.862772
2540.897821	157426.424967	57.867777
2540.392214	157208.635557	57.872781
2539.822904	156983.764014	57.877786
2538.992192	156760.626125	57.882791
2538.122380	156543.368998	57.887796
2537.678874	156313.765591	57.892801
2536.974675	156094.247689	57.897805
2536.212416	155878.566748	57.902810
2535.810811	155655.190058	57.907815
2535.051793	155432.100294	57.912820
2534.252268	155200.069244	57.917825
2533.494749	154986.655907	57.922829
2532.890116	154767.016357	57.927834
2532.477606	154547.627434	57.932839
2531.700721	154329.670536	57.937844
2530.862811	154094.932864	57.942849
2530.219790	153881.368524	57.947853
2529.476324	153670.567104	57.952858
2529.152042	153440.582882	57.957863
2527.986543	153229.444369	57.962868
2527.477954	152994.929121	57.967873
2526.741212	152782.759430	57.972877
2526.281874	152553.997544	57.977882
2525.476631	152337.011415	57.982887
2524.706632	152122.512418	57.987892
2524.246645	151905.423543	57.992897
2523.491376	151690.594532	57.997901
2522.760644	151471.873625	58.002906
2522.948692	151247.326992	58.007911
2521.645431	151024.022387	58.012916
2521.033908	150789.818688	58.017921
2520.637841	150575.105252	58.022925
2519.620511	150353.691830	58.027930
2519.052914	150120.756957	58.032935
2518.551799	149912.660986	58.037940
2517.492521	149676.985632	58.042945
2517.197527	149465.479049	58.047949
2516.201910	149247.628420	58.052954
2515.718850	149027.893260	58.057959
2514.994910	148814.031404	58.062964
2514.238754	148587.466724	58.067969
2513.593811	148376.975932	58.072973
2513.086174	148156.831195	58.077978
2512.629297	147925.699271	58.082983
2511.439752	147712.337945	58.087988
2510.833669	147486.939179	58.092993
2510.447858	147268.052131	58.097997
2509.466138	147058.119034	58.103002
2508.959352	146832.950617	58.108007
2508.292281	146622.767180	58.113012
2507.518226	146392.637077	58.118017
2507.004971	146192.980142	58.123021
2505.966053	145979.987818	58.128026
2505.782902	145756.021170	58.133031
2504.928966	145541.490208	58.138036
2504.143444	145321.866648	58.143041
2503.514287	145108.268824	58.148045
2502.922248	144893.052673	58.153050
2502.236578	144682.859709	58.158055
2501.368350	144460.523126	58.163060
2500.929575	144240.343884	58.168065
2500.417229	144038.108165	58.173069
2499.391055	143818.457076	58.178074
2499.077861	143596.330957	58.183079
2498.413182	143387.642882	58.188084
2497.928552	143159.752563	58.193089
2497.033321	142950.138244	58.198093
2496.327367	142734.332459	58.203098
2495.965942	142518.765831	58.208103
2495.010931	142300.575553	58.213108
2494.533215	142076.046757	58.218113
2493.753327	141849.890234	58.223117
2492.893463	141642.604549	58.228122
2492.650712	141421.118295	58.233127
2491.528014	141199.696903	58.238132
2491.285186	140977.705632	58.243137
2490.475098	140773.492887	58.248141
2489.849456	140553.445916	58.253146
2489.280324	140327.496009	58.258151
2488.392518	140121.178088	58.263156
2487.669806	139895.077880	58.268161
2487.396752	139689.402396	58.273165
2486.331520	139476.395695	58.278170
2485.983058	139250.037718	58.283175
2485.100269	139041.807872	58.288180
2484.338773	138819.901997	58.293185
2483.711580	138604.773790	58.298189
2482.947356	138385.133114	58.303194
2482.760845	138166.977904	58.308199
2481.734185	137956.478823	58.313204
2481.256099	137736.378314	58.318209
2480.754573	137516.651592	58.323213
2479.588256	137300.627318	58.328218
2479.353333	137079.896020	58.333223
2478.377901	136866.512628	58.338228
2477.731213	136643.321677	58.343233
2477.387322	136437.705311	58.348237
2476.561228	136223.388201	58.353242
2476.253755	135999.627492	58.358247
2475.156153	135777.467420	58.363252
2474.717900	135560.451241	58.368257
2474.243233	135336.480738	58.373261
2473.140277	135126.229982	58.378266
2472.481009	134901.440940	58.383271
2471.939902	134691.548887	58.388276
2471.526637	134469.328423	58.393281
2470.745194	134250.813900	58.398285
2469.945555	134034.145889	58.403290
2469.504635	133802.382074	58.408295
2468.610267	133591.194774	58.413300
2468.401289	133370.741517	58.418305
2467.814263	133148.876348	58.423309
2466.964007	132924.844341	58.428314
2466.405944	132694.251288	58.433319
2465.398129	132480.536915	58.438324
2464.825182	132252.426793	58.443329
2464.328829	132035.662289	58.448333
2463.409311	131813.072659	58.453338
2463.033322	131587.146844	58.458343
2461.955043	131369.171356	58.463348
2461.341485	131150.539580	58.468353
2460.821663	130931.081713	58.473357
2459.917302	130719.460016	58.478362
2459.758307	130498.614620	58.483367
2459.134489	130272.332152	58.488372
2458.173576	130052.290577	58.493377
2457.817678	129832.980403	58.498381
2456.873966	129603.210357	58.503386
2456.496439	129375.892675	58.508391
2455.544610	129167.224190	58.513396
2454.809290	128944.894769	58.518401
2454.464694	128716.637366	58.523405
2453.545128	128494.251851	58.528410
2453.051299	128271.241792	58.533415
2452.639196	128053.669122	58.538420
2451.756663	127827.904728	58.543425
2450.963396	127599.295841	58.548429
2450.087823	127373.673763	58.553434
2449.745505	127145.759162	58.558439
2449.061766	126940.087601	58.563444
2448.365104	126710.708776	58.568449
2448.184609	126490.482839	58.573453
2446.713793	126265.764328	58.578458
2446.390714	126031.937844	58.583463
2445.511144	125814.939597	58.588468
2445.099199	125591.531914	58.593473
2444.686437	125373.129736	58.598477
2443.572410	125154.383321	58.603482
2443.452035	124916.495923	58.608487
2442.525732	124706.346076	58.613492
2441.658536	124483.197482	58.618497
2441.180684	124251.760167	58.623501
2440.221223	124029.137910	58.628506
2439.832870	123808.293644	58.633511
2439.170061	123594.224916	58.638516
2438.592406	123367.839638	58.643521
2438.037937	123143.344641	58.648525
2437.039443	122919.048908	58.653530
2436.691447	122689.153653	58.658535
2435.841617	122460.470062	58.663540
2435.077730	122241.488677	58.668545
2434.706046	122003.578040	58.673549
2433.983681	121785.063648	58.678554
2433.541374	121558.177065	58.683559
2432.679466	121340.932819	58.688564
2432.088026	121112.905533	58.693569
2431.281062	120888.342637	58.698573
2430.392286	120663.527986	58.703578
2430.086326	120432.718743	58.708583
2429.309032	120210.277327	58.713588
2428.438721	119987.624001	58.718593
2428.144785	119757.428233	58.723597
2427.262695	119534.444166	58.728602
2426.722018	119310.481030	58.733607
2425.580824	119094.283623	58.738612
2425.192856	118858.524292	58.743617
2424.701183	118641.884862	58.748621
2423.864436	118421.131305	58.753626
2423.590615	118189.340149	58.758631
2423.025044	117973.016373	58.763636
2422.194406	117733.617577	58.768641
2421.932319	117499.113866	58.773645
2421.261862	117277.366145	58.778650
2420.624807	117040.145755	58.783655
2419.683875	116807.926873	58.788660
2418.636335	116568.503476	58.793665
2418.306964	116338.730898	58.798669
2417.191912	116126.972055	58.803674
2417.128850	115893.295658	58.808679
2416.435659	115661.504908	58.813684
2415.632297	115424.770167	58.818689
2414.913384	115193.704994	58.823693
2414.084817	114963.814492	58.828698
2413.591879	114725.970719	58.833703
2412.657390	114505.412362	58.838708
2412.323473	114271.273359	58.843713
2411.574258	114048.518943	58.848717
2410.779099	113835.795492	58.853722
2410.130829	113598.107553	58.858727
2409.513347	113367.722094	58.863732
2408.829330	113141.557159	58.868737
2407.898701	112920.859744	58.873741
2407.194751	112695.431858	58.878746
2406.964384	112468.141191	58.883751
2406.099957	112246.893425	58.888756
2405.396002	112015.220404	58.893761
2404.990529	111787.931966	58.898765
2404.237466	111560.427827	58.903770
2404.011060	111324.014647	58.908775
2403.207954	111095.196344	58.913780
2402.409434	110875.746302	58.918785
2401.918033	110643.195656	58.923789
2401.086346	110408.784663	58.928794
2400.506106	110172.235521	58.933799
2399.515120	109944.003427	58.938804
2398.963229	109712.810131	58.943809
2398.658575	109479.574548	58.948813
2397.683030	109249.925006	58.953818
2397.059710	109014.707405	58.958823
2396.532168	108792.428214	58.963828
2395.831739	108561.161468	58.968833
2395.039574	108327.779385	58.973837
2394.554962	108098.798900	58.978842
2393.685757	107859.234069	58.983847
2392.956304	107640.614253	58.988852
2392.107234	107410.073660	58.993857
2391.830617	107175.789677	58.998861
2390.912868	106957.757913	59.003866
2390.457935	106718.335379	59.008871
2389.568791	106497.746184	59.013876
2388.822331	106272.326933	59.018881
2388.353011	106042.176993	59.023885
2387.749741	105816.180967	59.028890
2387.148741	105589.260377	59.033895
2386.486979	105366.608855	59.038900
2385.486212	105132.700696	59.043905
2385.223816	104891.330745	59.048909
2384.434085	104675.710350	59.053914
2383.807746	104437.670121	59.058919
2382.980312	104210.208515	59.063924
2382.284626	103980.050894	59.068929
2381.985718	103764.544921	59.073933
2381.329966	103530.959428	59.078938
2380.432713	103295.181403	59.083943
2380.104035	103066.471682	59.088948
2379.407356	102839.104022	59.093953
2378.936111	102596.267986	59.098957
2378.023405	102370.766161	59.103962
2377.502747	102128.811900	59.108967
2376.575230	101898.806504	59.113972
2376.106643	101661.371907	59.118977
2375.477407	101419.651528	59.123981
2374.524467	101198.094078	59.128986
2373.929635	100955.053590	59.133991
2373.358529	100733.135521	59.138996
2372.599739	100505.261181	59.144001
2372.146205	100263.861127	59.149005
2371.092711	100041.702647	59.154010
2370.461849	99800.614637	59.159015
2370.023835	99577.100720	59.164020
2369.148131	99341.428950	59.169025
2368.451641	99112.010732	59.174029
2367.612540	98889.873730	59.179034
2367.375007	98650.428922	59.184039
2366.520005	98428.571639	59.189044
2365.667133	98197.227415	59.194049
2365.672786	97959.901431	59.199053
2364.640335	97735.427755	59.204058
2364.251571	97506.934510	59.209063
2363.706700	97271.060279	59.214068
2362.714714	97033.584991	59.219073
2362.001739	96798.490714	59.224077
2361.221428	96566.986597	59.229082
2361.142606	96339.159906	59.234087
2360.217462	96105.780791	59.239092
2359.274739	95871.461897	59.244097
2359.026762	95642.242064	59.249101
2358.255485	95410.253654	59.254106
2357.343894	95178.949439	59.259111
2356.826829	94944.268253	59.264116
2356.286614	94710.182969	59.269121
2355.928467	94472.976498	59.274125
2354.708011	94254.502966	59.279130
2354.121753	94007.438291	59.284135
2353.540840	93777.985851	59.289140
2352.699366	93541.449307	59.294145
2352.606365	93303.781953	59.299149
2351.643998	93071.746568	59.304154
2351.102346	92822.328962	59.309159
2350.154482	92600.315348	59.314164
2349.778226	92366.761266	59.319169
2349.133144	92128.623315	59.324173
2348.591330	91893.267914	59.329178
2347.926297	91645.246415	59.334183
2346.749789	91409.223232	59.339188
2345.953449	91184.631751	59.344193
2345.529317	90947.162636	59.349197
2344.820972	90715.897908	59.354202
2344.065141	90481.358730	59.359207
2343.107094	90247.285282	59.364212
2342.559592	90016.211653	59.369217
2342.298296	89797.224190	59.374221
2341.443533	89570.933904	59.379226
2340.784097	89330.178276	59.384231
2340.516975	89103.102220	59.389236
2339.487678	88881.747711	59.394241
2338.919674	88639.767912	59.399245
2338.404903	88403.646828	59.404250
2337.903678	88170.201598	59.409255
2337.030299	87938.320440	59.414260
2336.323958	87702.858672	59.419265
2335.915662	87465.913092	59.424269
2334.976972	87235.222676	59.429274
2334.321185	86992.140421	59.434279
2333.705900	86760.414829	59.439284
2333.033931	86533.715197	59.444289
2332.557548	86299.658656	59.449293
2331.512537	86055.216032	59.454298
2331.051744	85827.013325	59.459303
2330.350862	85599.015945	59.464308
2329.569939	85366.932315	59.469313
2328.859438	85124.063745	59.474317
2328.266899	84906.192637	59.479322
2327.664777	84668.370539	59.484327
2327.277912	84434.744933	59.489332
2326.579536	84198.604118	59.494337
2326.032906	83968.862918	59.499341
2325.387899	83727.090169	59.504346
2324.844004	83488.200844	59.509351
2324.080958	83252.290009	59.514356
2323.208858	83007.994436	59.519361
2322.486030	82768.203560	59.524365
2321.419728	82533.610185	59.529370
2321.143322	82302.525911	59.534375
2320.312517	82074.048324	59.539380
2319.759085	81848.400355	59.544385
2319.019332	81607.966256	59.549389
2318.520668	81373.935957	59.554394
2317.781775	81137.227463	59.559399
2317.213869	80902.820481	59.564404
2316.079874	80668.708721	59.569409
2315.687004	80431.097782	59.574413
2314.528458	80210.392730	59.579418
2314.080294	79984.494723	59.584423
2313.624476	79750.767391	59.589428
2312.981557	79525.386914	59.594433
2312.541252	79293.861323	59.599437
2312.027720	79066.741593	59.604442
2311.134927	78830.140848	59.609447
2310.088603	78598.041107	59.614452
2310.055761	78363.368861	59.619457
2309.476399	78120.693780	59.624461
2308.439209	77902.985144	59.629466
2307.947762	77667.506426	59.634471
2307.405403	77427.697874	59.639476
2306.195341	77201.830806	59.644481
2305.806529	76968.168790	59.649485
2305.095509	76738.882008	59.654490
2304.382208	76499.897174	59.659495
2303.683468	76276.462118	59.664500
2302.779332	76045.876804	59.669505
2302.450481	75814.138388	59.674509
2301.852884	75595.402543	59.679514
2301.209917	75354.544536	59.684519
2300.574213	75123.996820	59.689524
2300.021949	74891.113232	59.694529
2299.441486	74654.587380	59.699533
2298.566664	74426.017972	59.704538
2298.268724	74187.577410	59.709543
2297.460231	73951.273376	59.714548
2296.489614	73723.113612	59.719553
2296.513064	73477.129260	59.724557
2295.533042	73251.953994	59.729562
2294.700658	73012.402094	59.734567
2294.082619	72775.207436	59.739572
2293.244652	72534.730868	59.744577
2292.576982	72314.470687	59.749581
2291.830700	72087.998115	59.754586
2291.611809	71838.233354	59.759591
2290.592594	71606.089135	59.764596
2289.652364	71384.621842	59.769601
2289.450562	71151.586776	59.774605
2288.461110	70917.615165	59.779610
2287.899394	70675.349911	59.784615
2287.348831	70446.894978	59.789620
2286.510201	70229.440540	59.794625
2285.887843	69984.456918	59.799629
2285.073191	69763.272907	59.804634
2284.579980	69523.766317	59.809639
2283.913352	69289.484104	59.814644
2282.980444	69065.786725	59.819649
2282.796586	68835.043750	59.824653
2282.065127	68609.406774	59.829658
2281.405191	68371.277142	59.834663
2280.670049	68146.849505	59.839668
2280.006222	67914.002052	59.844673
2279.591448	67669.103094	59.849677
2278.904256	67445.353614	59.854682
2278.269074	67203.586214	59.859687
2277.355507	66969.459650	59.864692
2276.689763	66748.324125	59.869697
2276.510985	66506.151017	59.874701
2275.752007	66274.034946	59.879706
2274.553417	66041.354922	59.884711
2274.016513	65803.601371	59.889716
2273.332708	65576.658946	59.894721
2273.124478	65337.772908	59.899725
2272.043821	65108.774285	59.904730
2271.674017	64868.475835	59.909735
2270.868242	64643.412891	59.914740
2269.996655	64412.818920	59.919745
2269.617026	64180.528587	59.924750
2268.858716	63949.358638	59.929754
2268.002597	63711.643601	59.934759
2267.243587	63482.806514	59.939764
2266.598012	63255.648017	59.944769
2266.412294	63028.419282	59.949774
2265.678138	62796.401472	59.954778
2264.734446	62559.221251	59.959783
2264.158236	62332.243228	59.964788
2263.236014	62104.528172	59.969793
2262.910231	61869.636116	59.974798
2261.913671	61637.420830	59.979802
2261.532786	61408.966617	59.984807
2260.713217	61174.228000	59.989812
2259.865436	60947.164039	59.994817
2259.620464	60708.879984	59.999822
2258.740054	60489.294446	60.004826
2258.064308	60258.444437	60.009831
2257.673717	60028.435210	60.014836
2256.757283	59799.556821	60.019841
2256.441212	59557.506391	60.024846
2255.363915	59336.832339	60.029850
2254.806145	59105.176964	60.034855
2254.348434	58879.788590	60.039860
2253.462595	58646.570297	60.044865
2253.065805	58410.324168	60.049870
2252.205168	58195.943899	60.054874
2251.374563	57958.623346	60.059879
2251.099819	57727.905562	60.064884
2250.093415	57503.886931	60.069889
2249.700505	57255.519903	60.074894
2249.144766	57038.379525	60.079898
2248.324481	56799.242791	60.084903
2247.785932	56567.970453	60.089908
2246.971183	56329.858023	60.094913
2246.298591	56089.969624	60.099918
2245.407819	55871.221910	60.104922
2244.637289	55646.318061	60.109927
2244.355066	55406.924143	60.114932
2243.188026	55188.364463	60.119937
2242.976182	54950.082472	60.124942
2242.465222	54724.661379	60.129946
2241.649328	54497.743957	60.134951
2241.208862	54265.744513	60.139956
2240.270803	54039.788859	60.144961
2239.879297	53800.012399	60.149966
2238.966492	53582.162576	60.154970
2238.323516	53351.978950	60.159975
2237.849342	53109.693190	60.164980
2237.088060	52887.150768	60.169985
2236.234358	52643.675206	60.174990
2235.238113	52421.390942	60.179994
2234.875821	52193.756307	60.184999
2234.161355	51971.717639	60.190004
2233.292984	51739.229792	60.195009
2233.153894	51508.511859	60.200014
2232.371960	51300.404500	60.205018
2231.601215	51061.572374	60.210023
2231.317772	50827.231667	60.215028
2230.409353	50595.334440	60.220033
2229.783427	50366.961056	60.225038
2228.945532	50147.229780	60.230042
2228.369090	49909.030733	60.235047
2227.877180	49686.807783	60.240052
2226.710036	49452.394274	60.245057
2226.606206	49218.381448	60.250062
2225.688036	48996.937030	60.255066
2224.819267	48770.172724	60.260071
2224.333326	48532.047280	60.265076
2223.805962	48315.351575	60.270081
2222.597205	48078.922286	60.275086
2222.058145	47863.053286	60.280090
2221.333484	47643.448781	60.285095
2220.987559	47413.651601	60.290100
2220.167340	47202.944023	60.295105
2219.404830	46963.675124	60.300110
2218.729718	46755.448827	60.305114
2217.703403	46526.372131	60.310119
2217.144272	46300.874547	60.315124
2216.468310	46080.180976	60.320129
2215.836203	45863.813434	60.325134
2215.123578	45648.584198	60.330138
2214.527356	45431.713363	60.335143
2213.976045	45219.446481	60.340148
2213.226906	45001.947330	60.345153
2212.750005	44779.024507	60.350158
2212.193809	44562.901346	60.355162
2211.406661	44338.512044	60.360167
2210.980612	44121.842344	60.365172
2209.849612	43908.715540	60.370177
2209.364596	43674.944230	60.375182
2208.483213	43461.865524	60.380186
2207.909159	43239.648257	60.385191
2207.748153	43023.443537	60.390196
2206.649551	42808.247295	60.395201
2206.111089	42589.729663	60.400206
2205.512028	42372.236374	60.405210
2204.843252	42167.700503	60.410215
2204.202622	41934.303052	60.415220
2203.335753	41714.327493	60.420225
2202.922286	41494.304940	60.425230
2202.183474	41273.808721	60.430234
2201.460477	41062.543215	60.435239
2200.867090	40827.104163	60.440244
2199.858008	40621.021618	60.445249
2199.378032	40400.356398	60.450254
2198.849473	40184.428940	60.455258
2197.887557	39973.910375	60.460263
2197.461667	39766.487106	60.465268
2196.560535	39552.176081	60.470273
2196.270203	39324.709190	60.475278
2195.338913	39120.417234	60.480282
2194.616610	38896.278101	60.485287
2194.385826	38686.293342	60.490292
2193.306998	38461.380215	60.495297
2192.830877	38245.570122	60.500302
2192.326628	38031.684753	60.505306
2191.092542	37824.154089	60.510311
2190.827655	37599.488399	60.515316
2190.150406	37392.285674	60.520321
2189.520997	37175.843269	60.525326
2188.213419	36958.872623	60.530330
2187.456394	36752.984989	60.535335
2186.923840	36547.592195	60.540340
2186.527692	36335.878200	60.545345
2185.953473	36129.762101	60.550350
2184.986505	35924.569111	60.555354
2184.294616	35715.190665	60.560359
2184.027900	35510.234616	60.565364
2183.435298	35299.438886	60.570369
2182.628636	35089.926807	60.575374
2181.775986	34888.747636	60.580378
2181.259052	34669.126971	60.585383
2180.716830	34462.158575	60.590388
2179.723756	34264.663246	60.595393
2179.109071	34041.662029	60.600398
2178.560244	33844.093287	60.605402
2177.748005	33639.332039	60.610407
2177.175444	33427.649576	60.615412
2176.304777	33227.542651	60.620417
2175.545527	33018.271875	60.625422
2174.471819	32824.074562	60.630426
2173.938577	32613.571984	60.635431
2173.776329	32421.289156	60.640436
2172.477735	32233.558285	60.645441
2172.172677	32031.666193	60.650446
2171.361767	31838.737692	60.655450
2170.746444	31640.570466	60.660455
2170.154584	31439.410600	60.665460
2169.351911	31242.790114	60.670465
2168.794224	31048.083007	60.675470
2167.887599	30866.253177	60.680474
2167.145660	30673.414269	60.685479
2166.760518	30474.576689	60.690484
2165.874772	30286.176766	60.695489
2164.994396	30086.520238	60.700494
2164.142474	29907.613864	60.705498
2163.389050	29725.954054	60.710503
2162.878009	29543.877018	60.715508
2162.076309	29350.870373	60.720513
2161.454376	29167.184577	60.725518
2160.401509	28992.944656	60.730522
2159.711124	28814.713461	60.735527
2159.349696	28638.206264	60.740532
2158.403074	28472.026852	60.745537
2157.801515	28286.922659	60.750542
2157.155372	28123.681944	60.755546
2156.424162	27940.362237	60.760551
2155.744687	27774.431933	60.765556
2154.646677	27606.703969	60.770561
2154.180441	27443.184032	60.775566
2153.285549	27281.311966	60.780570
2152.215752	27119.693598	60.785575
2151.609600	26966.012632	60.790580
2150.262072	26810.867864	60.795585
2149.380833	26665.909336	60.800590
2148.648489	26531.326940	60.805594
2147.674765	26387.565630	60.810599
2147.310294	26263.304140	60.815604
2146.123950	26142.535567	60.820609
2145.533425	26003.405352	60.825614
2144.839513	25880.103445	60.830618
2144.046013	25763.744205	60.835623
2143.460668	25631.804521	60.840628
2142.395109	25511.463812	60.845633
2142.063755	25390.250872	60.850638
2141.165450	25273.119642	60.855642
2140.167660	25150.893539	60.860647
2139.751005	25037.518865	60.865652
2139.060516	24935.367753	60.870657
2138.582385	24818.137629	60.875662
2137.539099	24712.929843	60.880666
2137.048400	24605.363707	60.885671
2136.439877	24490.445401	60.890676
2135.780151	24379.263669	60.895681
2135.211183	24277.021654	60.900686
2134.481402	24161.846168	60.905690
2133.799971	24051.649434	60.910695
2133.119687	23934.712939	60.915700
2132.423804	23838.915153	60.920705
2131.970467	23721.083410	60.925710
2131.417986	23612.038819	60.930714
2130.344069	23510.151920	60.935719
2130.378679	23400.244069	60.940724
2129.417513	23294.629055	60.945729
2129.007384	23182.691891	60.950734
2128.053127	23079.767686	60.955738
2127.647247	22967.657628	60.960743
2127.166171	22858.718205	60.965748
2126.336087	22746.650960	60.970753
2125.822370	22623.969382	60.975758
2124.967952	22514.994429	60.980762
2124.255872	22406.261382	60.985767
2123.554543	22291.257570	60.990772
2122.911391	22195.748736	60.995777
2122.473852	22086.580281	61.000782
2121.849656	21970.492647	61.005786
2120.948094	21862.902826	61.010791
2120.628682	21754.362247	61.015796
2119.787906	21653.557312	61.020801
2119.127319	21534.433890	61.025806
2118.476708	21423.354270	61.030810
2117.787886	21320.115106	61.035815
2117.283717	21212.435852	61.040820
2116.568363	21100.598130	61.045825
2116.045223	20997.892228	61.050830
2115.158834	20891.156205	61.055834
2114.703936	20782.679326	61.060839
2114.178024	20669.169919	61.065844
2113.158931	20572.045616	61.070849
2112.825745	20453.123160	61.075854
2112.027830	20343.148313	61.080858
2111.335792	20235.451852	61.085863
2110.967945	20119.622166	61.090868
2110.061024	20012.765869	61.095873
2109.186033	19901.341759	61.100878
2108.705376	19794.385747	61.105882
2108.166357	19678.876621	61.110887
2107.431089	19570.388243	61.115892
2106.564032	19462.614321	61.120897
2105.912783	19355.108087	61.125902
2105.172375	19251.926200	61.130906
2104.324533	19152.602519	61.135911
2104.056623	19039.309074	61.140916
2103.166724	18940.525920	61.145921
2102.897181	18829.084795	61.150926
2102.004836	18734.021363	61.155930
2101.370933	18619.666805	61.160935
2100.921134	18511.682029	61.165940
2099.827092	18418.790378	61.170945
2099.755192	18303.220817	61.175950
2098.843319	18197.736331	61.180954
2098.002530	18094.675112	61.185959
2097.346804	17988.392348	61.190964
2096.619609	17884.665578	61.195969
2096.104413	17783.197544	61.200974
2095.687487	17675.488450	61.205978
2094.795333	17575.208486	61.210983
2094.015973	17469.835389	61.215988
2092.802612	17373.256732	61.220993
2092.980382	17267.307622	61.225998
2092.448401	17164.393009	61.231002
2091.140571	17054.566024	61.236007
2090.741587	16964.743705	61.241012
2089.500819	16855.310467	61.246017
2089.404261	16755.221731	61.251022
2088.324326	16659.874924	61.256026
2087.515225	16558.960995	61.261031
2087.336009	16462.745652	61.266036
2086.368078	16373.519869	61.271041
2085.993600	16277.248456	61.276046
2085.377987	16173.474161	61.281050
2084.192350	16081.309001	61.286055
2083.828487	15982.102596	61.291060
2082.949047	15898.347211	61.296065
2082.501979	15796.341849	61.301070
2081.930171	15706.924835	61.306074
2080.939522	15608.391373	61.311079
2080.663774	15506.438876	61.316084
2079.224950	15417.607294	61.321089
2078.803230	15334.145802	61.326094
2078.402249	15245.537058	61.331098
2077.568371	15162.869633	61.336103
2077.164495	15066.143665	61.341108
2076.491413	14976.946052	61.346113
2075.847907	14887.356531	61.351118
2075.062560	14798.742888	61.356122
2074.249282	14711.795888	61.361127
2073.911030	14612.616519	61.366132
2072.948606	14528.963635	61.371137
2072.309922	14428.969685	61.376142
2071.296019	14357.653314	61.381146
2070.593928	14267.417584	61.386151
2069.916232	14182.137393	61.391156
2068.987230	14112.947423	61.396161
2068.709009	14027.298271	61.401166
2067.764358	13949.929575	61.406170
2066.782553	13871.942695	61.411175
2066.512876	13790.245861	61.416180
2065.975029	13718.916593	61.421185
2065.187301	13639.633702	61.426190
2064.407378	13560.417262	61.431194
2064.224420	13479.942710	61.436199
2063.237736	13392.501552	61.441204
2062.373395	13332.998067	61.446209
2061.896753	13246.523168	61.451214
2061.292857	13163.335984	61.456218
2060.249985	13094.759398	61.461223
2060.007888	13006.950818	61.466228
2059.416683	12939.576261	61.471233
2058.420901	12867.852112	61.476238
2057.793640	12790.069780	61.481242
2057.086274	12719.199810	61.486247
2056.581706	12643.796028	61.491252
2055.948497	12574.413771	61.496257
2055.237113	12496.513117	61.501262
2054.699582	12413.520721	61.506266
2053.789404	12344.746131	61.511271
2053.186094	12276.992629	61.516276
2052.654179	12204.269165	61.521281
2051.875841	12128.395291	61.526286
2051.560263	12053.754354	61.531290
2050.769213	11979.641023	61.536295
2050.230968	11898.385648	61.541300
2049.357299	11830.630487	61.546305
2048.805203	11751.607941	61.551310
2047.749281	11677.313426	61.556314
2046.751452	11618.832600	61.561319
2046.681792	11533.732088	61.566324
2046.053021	11473.335702	61.571329
2045.303880	11395.188056	61.576334
2044.693291	11327.267921	61.581338
2044.153024	11253.494333	61.586343
2043.609481	11174.056601	61.591348
2042.487725	11097.007869	61.596353
2041.941825	11032.409489	61.601358
2041.641804	10959.253343	61.606362
2040.612537	10886.562854	61.611367
2040.160022	10818.695857	61.616372
2039.338016	10742.811382	61.621377
2038.446976	10677.096954	61.626382
2037.857633	10610.180934	61.631386
2037.636200	10536.791447	61.636391
2036.959185	10452.000331	61.641396
2035.637854	10388.502052	61.646401
2035.212889	10320.194606	61.651406
2034.595550	10241.937113	61.656410
2033.792240	10180.303247	61.661415
2033.481233	10111.943739	61.666420
2032.565925	10049.291009	61.671425
2032.015029	9978.568196	61.676430
2031.428607	9913.525961	61.681434
2030.637305	9843.107051	61.686439
2029.998485	9774.293572	61.691444
2029.191278	9707.351436	61.696449
2028.936788	9636.548068	61.701454
2028.482473	9567.095955	61.706458
2027.286953	9498.203255	61.711463
2026.548019	9430.397033	61.716468
2025.800112	9368.062595	61.721473
2025.299339	9300.232570	61.726478
2024.890892	9244.472631	61.731482
2023.705813	9177.317084	61.736487
2023.399714	9095.933601	61.741492
2022.622932	9041.733904	61.746497
2022.411136	8982.553513	61.751502
2021.738537	8901.200460	61.756506
2020.861252	8831.711187	61.761511
2020.448440	8769.456222	61.766516
2019.697318	8703.917547	61.771521
2018.639349	8629.330088	61.776526
2018.182922	8562.510154	61.781530
2017.074198	8489.809138	61.786535
2016.901050	8419.608043	61.791540
2016.139467	8364.950006	61.796545
2015.530699	8301.359679	61.801550
2015.020105	8228.463612	61.806554
2014.248165	8167.005012	61.811559
2013.742763	8093.126962	61.816564
2012.957663	8036.612397	61.821569
2011.899553	7957.319256	61.826574
2011.661622	7893.998800	61.831578
2010.962513	7838.518219	61.836583
2010.431205	7765.146856	61.841588
2009.782668	7703.706468	61.846593
2008.870868	7635.990234	61.851598
2008.236310	7567.761697	61.856602
2007.370642	7499.566212	61.861607
2006.823826	7442.211799	61.866612
2006.130390	7386.928823	61.871617
2005.337714	7320.704247	61.876622
2004.712178	7258.214012	61.881626
2003.826759	7212.477602	61.886631
2003.251084	7142.602379	61.891636
2002.836864	7080.691509	61.896641
2002.156542	7029.954024	61.901646
2001.803470	6960.431652	61.906650
2000.759968	6892.904572	61.911655
2000.359913	6828.300917	61.916660
1999.532536	6769.066062	61.921665
1998.981708	6697.834521	61.926670
1998.343002	6636.590631	61.931674
1997.320162	6585.314243	61.936679
1997.009413	6502.328074	61.941684
1996.303814	6453.048030	61.946689
1995.417368	6390.198182	61.951694
1995.156562	6326.576415	61.956698
1994.077949	6279.193341	61.961703
1993.205385	6204.084519	61.966708
1992.977596	6152.962662	61.971713
1992.495546	6091.973811	61.976718
1991.772815	6021.175884	61.981722
1990.533171	5969.627617	61.986727
1990.516266	5893.445853	61.991732
1989.483733	5843.819806	61.996737
1988.985350	5786.967339	62.001742
1988.402186	5718.537976	62.006746
1987.688634	5655.746617	62.011751
1987.085103	5601.306328	62.016756
1986.194416	5544.976930	62.021761
1985.472484	5469.269736	62.026766
1985.069258	5412.672574	62.031770
1983.968481	5365.236787	62.036775
1983.455202	5290.977129	62.041780
1983.314351	5238.813692	62.046785
1982.526483	5182.392841	62.051790
1981.997202	5121.760958	62.056794
1981.161117	5060.268587	62.061799
1980.562408	4992.317513	62.066804
1979.847799	4941.195870	62.071809
1979.130716	4870.699905	62.076814
1978.383339	4816.103139	62.081818
1977.549571	4755.510053	62.086823
1977.009271	4692.227555	62.091828
1976.401309	4636.449872	62.096833
1975.490967	4578.128618	62.101838
1975.200219	4515.559714	62.106842
1974.401542	4453.712157	62.111847
1973.571482	4395.039728	62.116852
1972.839326	4336.807873	62.121857
1972.492036	4287.407176	62.126862
1971.872785	4221.262770	62.131866
1971.275013	4170.710476	62.136871
1970.578755	4100.613185	62.141876
1970.097677	4045.155163	62.146881
1969.117435	3980.297952	62.151886
1968.497030	3922.802415	62.156890
1967.640100	3869.270788	62.161895
1966.919426	3803.693292	62.166900
1966.487499	3757.543818	62.171905
1965.700142	3691.125622	62.176910
1965.336378	3622.962949	62.181914
1964.423913	3574.850009	62.186919
1964.116013	3515.182535	62.191924
1963.398709	3450.778841	62.196929
1962.652242	3394.315677	62.201934
1962.147561	3329.662664	62.206938
1961.251570	3272.874324	62.211943
1960.813824	3203.693763	62.216948
1960.103024	3154.464987	62.221953
1959.380876	3092.434345	62.226958
1958.885970	3023.617024	62.231962
1957.797393	2973.025315	62.236967
1957.140755	2909.883301	62.241972
1956.683344	2851.770652	62.246977
1955.808334	2801.998942	62.251982
1955.268072	2736.298201	62.256986
1954.490574	2678.171599	62.261991
1954.233966	2620.201488	62.266996
1953.361160	2562.115713	62.272001
1952.553090	2510.328100	62.277006
1952.147200	2439.176101	62.282010
1951.026023	2399.312070	62.287015
1950.786919	2333.582673	62.292020
1950.010048	2281.421057	62.297025
1949.305392	2220.470940	62.302030
1948.347284	2158.560574	62.307034
1947.753841	2107.861711	62.312039
1947.109083	2049.296998	62.317044
1946.634188	1998.980300	62.322049
1945.731700	1939.070592	62.327054
1945.422692	1873.654812	62.332058
1944.438970	1829.971088	62.337063
1943.679131	1776.433275	62.342068
1943.168956	1723.969499	62.347073
1942.255325	1667.854968	62.352078
1941.520225	1620.599566	62.357082
1940.846456	1570.416857	62.362087
1940.583971	1513.895940	62.367092
1939.891377	1469.744404	62.372097
1938.903328	1411.432317	62.377102
1938.572487	1355.373926	62.382106
1937.757856	1311.164967	62.387111
1937.107629	1257.211070	62.392116
1936.418941	1212.169414	62.397121
1935.932814	1153.308696	62.402126
1934.988367	1097.091649	62.407130
1934.355898	1064.371275	62.412135
1933.695393	1003.520168	62.417140
1933.277462	949.457986	62.422145
1932.254252	902.625215	62.427150
1931.872408	856.381525	62.432154
1931.108017	807.350536	62.437159
1930.392567	752.287574	62.442164
1929.968129	699.976311	62.447169
1929.171611	640.275912	62.452174
1928.427051	596.214920	62.457178
1927.888432	546.322598	62.462183
1927.208924	498.066119	62.467188
1926.394011	446.890143	62.472193
1925.326769	411.863691	62.477198
1924.857346	351.502240	62.482202
1923.944694	311.592699	62.487207
1923.483481	270.042472	62.492212
1922.975371	228.318454	62.497217
1922.380948	186.153296	62.502222
1922.112485	129.378497	62.507226
1920.989394	96.541079	62.512231
1920.608314	51.066248	62.517236
1919.646654	4.225034	62.522241
1918.823865	-40.572243	62.527246
1917.883541	-81.606994	62.532250
1917.296564	-118.774241	62.537255
1916.080864	-156.194808	62.542260
1915.520616	-176.989396	62.547265
1914.457627	-212.708869	62.552270
1913.818348	-228.091340	62.557274
1912.468170	-244.158861	62.562279
1910.688890	-231.736837	62.567284
1903.710477	-46.707508	62.572289
1901.313367	35.425321	62.577294
1903.046159	69.121716	62.582298
1904.564868	111.702247	62.587303
1906.116549	128.091698	62.592308
1907.077646	141.501377	62.597313
1907.923839	128.459481	62.602318
1907.994367	126.672732	62.607322
1907.414324	99.680163	62.612327
1906.767575	70.671809	62.617332
1906.086154	36.094386	62.622337
1904.838323	28.756260	62.627342
1903.736983	3.781597	62.632346
1902.161622	8.534144	62.637351
1901.486794	10.860243	62.642356
1900.824578	2.828321	62.647361
1900.612282	14.088683	62.652366
1900.027764	-0.452728	62.657370
1899.202822	8.793332	62.662375
1898.119850	1.660863	62.667380
1896.997166	5.980409	62.672385
1896.013009	20.334360	62.677390
1895.633594	16.176324	62.682394
1895.368609	17.317696	62.687399
1894.988137	10.390654	62.692404
1894.814603	21.659060	62.697409
1894.283464	19.360720	62.702414
1893.407250	9.508247	62.707418
1892.079481	24.747829	62.712423
1891.702250	26.667129	62.717428
1891.307612	24.976330	62.722433
1890.127092	33.293254	62.727438
1889.470893	19.971176	62.732442
1888.590545	35.792598	62.737447
1888.443091	40.042464	62.742452
1887.977023	34.769065	62.747457
1887.389402	42.498258	62.752462
1886.595661	36.437933	62.757466
1885.797192	41.921866	62.762471
1885.127749	38.702450	62.767476
1884.382020	29.881095	62.772481
1883.413864	42.608239	62.777486
1883.220356	40.432909	62.782490
1882.739032	47.055532	62.787495
1881.974759	45.111182	62.792500
1881.685264	39.699357	62.797505
1881.013156	47.418313	62.802510
1880.410328	41.999468	62.807514
1879.042003	47.654317	62.812519
1878.496010	49.835388	62.817524
1878.436584	42.534076	62.822529
1877.067620	43.563737	62.827534
1876.697078	40.405673	62.832538
1875.868158	54.004868	62.837543
1875.201305	50.677806	62.842548
1874.638788	57.303865	62.847553
1873.558796	58.429572	62.852558
1873.220485	48.925339	62.857562
1873.154128	59.626388	62.862567
1872.522126	57.858159	62.867572
1871.317072	56.106807	62.872577
1870.752899	64.639705	62.877582
1870.644971	54.002883	62.882586
1869.437572	62.073358	62.887591
1868.567852	58.224988	62.892596
1868.323525	57.499090	62.897601
1867.674593	60.177490	62.902606
1867.200732	56.819784	62.907610
1866.469872	58.091909	62.912615
1865.082371	56.147176	62.917620
1864.613460	62.167006	62.922625
1863.985548	68.000770	62.927630
1863.501797	62.782215	62.932634
1862.820531	62.642950	62.937639
1862.240225	62.564927	62.942644
1861.798069	64.912445	62.947649
1860.858591	65.019191	62.952654
1860.335867	63.902254	62.957658
1859.553649	73.712446	62.962663
1858.971276	66.167729	62.967668
1858.490407	63.478200	62.972673
1857.537000	64.112295	62.977678
1856.840846	63.462876	62.982682
1856.257329	68.912693	62.987687
1855.924467	66.204393	62.992692
1854.932598	71.425736	62.997697
1854.017409	67.901563	63.002702
1853.813355	61.779140	63.007706
1853.221713	70.813156	63.012711
1852.389202	69.444208	63.017716
1851.758095	64.584952	63.022721
1851.043250	73.561263	63.027726
1850.734097	70.549570	63.032730
1850.065699	68.490652	63.037735
1849.338145	79.249400	63.042740
1849.067247	66.369169	63.047745
1848.023558	76.482666	63.052750
1847.510023	70.256417	63.057754
1846.945956	78.142746	63.062759
1845.744067	65.673713	63.067764
1845.054423	68.987802	63.072769
1844.574192	81.639084	63.077774
1844.013587	66.811549	63.082778
1842.926616	71.362011	63.087783
1842.570406	65.356792	63.092788
1841.836616	69.382804	63.097793
1841.458951	69.660543	63.102798
1840.462806	64.649520	63.107802
1839.432867	67.760601	63.112807
1839.628665	76.587573	63.117812
1838.973323	64.818668	63.122817
1837.540015	72.103426	63.127822
1837.243186	70.445985	63.132826
1836.405567	68.213667	63.137831
1836.075032	74.539543	63.142836
1835.348382	64.674346	63.147841
1834.605312	73.450133	63.152846
1834.306048	67.997278	63.157850
1833.577339	74.380078	63.162855
1832.808312	71.914513	63.167860
1832.405711	65.047745	63.172865
1831.749962	77.674856	63.177870
1831.242422	73.070375	63.182874
1830.162185	66.938858	63.187879
1828.967733	70.889792	63.192884
1828.940165	68.432640	63.197889
1827.846939	73.266382	63.202894
1827.113131	66.192009	63.207898
1827.251163	70.100075	63.212903
1825.960389	70.163272	63.217908
1825.347121	65.927253	63.222913
1824.554393	75.710737	63.227918
1823.981974	68.287453	63.232922
1823.276771	68.481590	63.237927
1823.080278	75.322355	63.242932
1822.788974	71.583996	63.247937
1821.960358	75.819043	63.252942
1821.617796	72.319063	63.257946
1820.471835	79.709591	63.262951
1819.273847	71.031022	63.267956
1818.387858	71.061479	63.272961
1817.847629	72.349077	63.277966
1817.941562	70.003519	63.282970
1817.198971	66.324215	63.287975
1816.367457	67.506681	63.292980
1816.107805	70.153236	63.297985
1815.090068	75.643635	63.302990
1814.617048	68.152528	63.307994
1813.714635	75.004474	63.312999
1812.505200	71.892906	63.318004
1812.436202	62.282829	63.323009
1811.009626	77.248019	63.328014
1811.111723	61.277602	63.333018
1810.548345	70.830694	63.338023
1809.547558	76.299479	63.343028
1808.648387	67.672813	63.348033
1807.812038	84.372001	63.353038
1807.840938	75.033380	63.358042
1806.949394	75.471584	63.363047
1806.239525	74.121022	63.368052
1805.799688	71.964315	63.373057
1805.029474	80.887929	63.378062
1804.958662	72.782578	63.383066
1804.403485	76.814928	63.388071
1803.431831	76.292857	63.393076
1802.434102	71.581726	63.398081
1801.528463	77.817588	63.403086
1800.962344	70.978371	63.408090
1800.403658	68.488873	63.413095
1799.898951	80.361858	63.418100
1799.654178	70.498991	63.423105
1798.759863	80.205574	63.428110
1798.248812	73.606774	63.433114
1797.506120	76.476706	63.438119
1795.988434	71.133783	63.443124
1795.409288	68.456721	63.448129
1794.623499	78.587624	63.453134
1794.783740	70.024526	63.458138
1794.060511	74.023641	63.463143
1793.300142	76.864842	63.468148
1792.918693	69.333965	63.473153
1791.868935	78.639451	63.478158
1792.060253	75.425277	63.483162
1790.787364	81.329955	63.488167
1789.525813	75.067974	63.493172
1789.074698	61.984568	63.498177
1788.174530	83.155177	63.503182
1787.617272	77.328554	63.508186
1787.108530	81.023944	63.513191
1786.550574	72.514984	63.518196
1786.443903	76.931853	63.523201
1785.483215	83.698447	63.528206
1785.366105	72.094814	63.533210
1784.112634	73.014717	63.538215
1783.316518	77.659360	63.543220
1782.726005	71.683478	63.548225
1781.924026	84.598758	63.553230
1781.516398	63.718142	63.558234
1781.098355	78.594131	63.563239
1780.296446	71.442278	63.568244
1779.137150	72.066523	63.573249
1778.224408	80.545991	63.578254
1777.494634	68.993936	63.583258
1777.737929	76.263179	63.588263
1776.664102	74.762269	63.593268
1776.129653	73.145730	63.598273
1775.206724	75.241609	63.603278
1775.077860	75.842549	63.608282
1774.579815	77.754249	63.613287
1773.759267	77.674977	63.618292
1773.058011	73.509717	63.623297
1771.795026	77.771188	63.628302
1771.297890	73.953562	63.633306
1771.032739	78.811926	63.638311
1770.098916	79.985425	63.643316
1769.743043	75.618650	63.648321
1768.983510	81.755621	63.653326
1768.313679	71.834111	63.658330
1767.706643	77.877474	63.663335
1766.293854	76.364171	63.668340
1766.384409	72.845873	63.673345
1765.762927	70.828414	63.678350
1765.341304	72.472505	63.683354
1764.985625	68.454216	63.688359
1763.056902	74.101939	63.693364
1762.638237	69.402935	63.698369
1761.857984	74.535504	63.703374
1761.154522	73.800538	63.708378
1760.837062	78.050610	63.713383
1760.096125	79.177706	63.718388
1759.982231	70.848965	63.723393
1759.249908	72.662257	63.728398
1758.985644	70.594369	63.733402
1757.658350	71.991220	63.738407
1756.760552	76.757677	63.743412
1756.084876	67.665019	63.748417
1755.476494	80.819215	63.753422
1755.116478	74.046624	63.758426
1754.550137	75.311573	63.763431
1753.827118	76.800107	63.768436
1753.630182	72.595752	63.773441
1752.051613	73.449033	63.778446
1751.183525	75.067845	63.783450
1750.695870	74.468918	63.788455
1750.246021	83.371622	63.793460
1749.940593	71.924066	63.798465
1749.480870	78.939110	63.803470
1749.119196	74.702573	63.808474
1748.054666	71.921265	63.813479
1746.741164	80.659943	63.818484
1746.514814	75.476222	63.823489
1745.712637	81.506429	63.828494
1745.411576	81.555968	63.833498
1744.492464	79.413896	63.838503
1743.415582	82.917255	63.843508
1742.699930	70.208618	63.848513
1741.985908	88.112127	63.853518
1741.530235	75.300689	63.858522
1741.214237	70.534918	63.863527
1740.543205	77.608758	63.868532
1740.460928	72.574046	63.873537
1739.602137	82.055801	63.878542
1738.675860	71.479586	63.883546
1737.616703	75.651925	63.888551
1736.743934	88.863895	63.893556
1736.739810	73.381865	63.898561
1735.870663	79.865844	63.903566
1735.486789	78.115007	63.908570
1735.156392	71.473337	63.913575
1733.701284	84.016120	63.918580
1733.583078	74.765529	63.923585
1732.603851	79.576468	63.928590
1731.774025	77.068552	63.933594
1731.581450	72.543379	63.938599
1730.681447	83.391043	63.943604
1729.985797	71.675887	63.948609
1728.649432	77.239005	63.953614
1728.318615	78.745674	63.958618
1727.861011	72.669847	63.963623
1727.324156	82.463174	63.968628
1727.279622	82.654898	63.973633
1726.697801	84.452178	63.978638
1725.293779	81.497720	63.983642
1724.555420	70.260869	63.988647
1723.667444	77.929001	63.993652
1723.609761	68.717688	63.998657
1722.804268	80.587994	64.003662
1721.889487	76.470859	64.008666
1720.985155	72.131290	64.013671
1720.042959	79.618798	64.018676
1719.897291	73.307339	64.023681
1719.245682	76.684804	64.028686
1718.446776	76.114823	64.033690
1718.533003	79.733061	64.038695
1717.779346	83.615603	64.043700
1717.319779	66.214200	64.048705
1716.225928	75.769566	64.053710
1715.485481	72.758594	64.058714
1715.263455	71.084556	64.063719
1714.098631	79.004829	64.068724
1713.426588	75.320658	64.073729
1712.319636	86.675874	64.078734
1711.844299	76.349741	64.083738
1711.315836	73.516412	64.088743
1710.698781	86.992123	64.093748
1710.443222	74.366531	64.098753
1709.846009	78.374036	64.103758
1709.254868	73.185189	64.108762
1708.628148	75.735517	64.113767
1707.510655	80.032254	64.118772
1707.118241	83.849530	64.123777
1706.078590	78.783969	64.128782
1705.023608	78.242055	64.133786
1704.226712	80.362093	64.138791
1704.154303	80.998224	64.143796
1703.822800	71.152306	64.148801
1702.936962	72.031194	64.153806
1701.932755	70.708495	64.158810
1701.658846	66.568416	64.163815
1701.194687	73.049570	64.168820
1700.959907	70.144359	64.173825
1699.403103	76.329145	64.178830
1698.845167	70.805438	64.183834
1698.543747	67.182249	64.188839
1697.529287	70.834981	64.193844
1697.305486	61.285782	64.198849
1696.466606	70.933115	64.203854
1695.492452	77.173582	64.208858
1695.308682	80.593430	64.213863
1694.402901	75.583882	64.218868
1693.539845	73.849249	64.223873
1692.581695	77.707509	64.228878
1691.966611	71.472201	64.233882
1691.701871	64.074200	64.238887
1691.020401	77.328320	64.243892
1690.758124	70.568603	64.248897
1690.097403	75.474040	64.253902
1689.299120	77.950700	64.258906
1688.145234	75.855408	64.263911
1687.530240	73.255031	64.268916
1687.321346	72.335861	64.273921
1686.583212	81.019432	64.278926
1685.632308	74.591463	64.283930
1685.053063	64.631944	64.288935
1684.058387	79.624769	64.293940
1683.922883	68.577601	64.298945
1683.349465	71.631985	64.303950
1682.727148	72.674024	64.308954
1681.919046	78.236824	64.313959
1680.557576	80.093313	64.318964
1680.030185	77.059544	64.323969
1679.752569	79.847738	64.328974
1678.752987	76.753362	64.333978
1678.801791	77.151035	64.338983
1677.956176	79.699875	64.343988
1677.795316	77.760652	64.348993
1676.839324	74.765009	64.353998
1675.767349	75.966796	64.359002
1675.297450	73.180943	64.364007
1674.423493	76.910714	64.369012
1673.959579	75.043290	64.374017
1672.910266	81.240512	64.379022
1672.202044	82.764566	64.384026
1672.038698	74.620312	64.389031
1671.271658	71.703467	64.394036
1670.977463	78.428865	64.399041
1670.118026	72.049453	64.404046
1668.997703	81.709971	64.409050
1668.344159	79.636126	64.414055
1667.583006	82.174705	64.419060
1667.324909	69.771885	64.424065
1666.731643	67.445612	64.429070
1666.199954	74.743336	64.434074
1664.943803	80.049308	64.439079
1664.540771	86.407217	64.444084
1664.023172	77.983345	64.449089
1663.559873	80.849927	64.454094
1662.952088	77.467804	64.459098
1662.093402	73.764414	64.464103
1661.082974	79.807225	64.469108
1660.591899	78.617491	64.474113
1660.202541	73.629994	64.479118
1659.584922	75.190120	64.484122
1659.082455	73.180588	64.489127
1657.780770	74.597075	64.494132
1657.167794	70.386288	64.499137
1656.817391	77.494361	64.504142
1656.363191	75.341541	64.509146
1655.767495	71.153241	64.514151
1654.157761	75.947677	64.519156
1653.964597	76.216632	64.524161
1653.205562	73.792116	64.529166
1652.528160	81.155573	64.534170
1652.223839	75.214686	64.539175
1651.488094	75.560380	64.544180
1650.974581	74.738496	64.549185
1649.656239	84.040966	64.554190
1649.355486	79.564528	64.559194
1649.027227	76.849219	64.564199
1648.098862	81.554333	64.569204
1648.114282	81.378557	64.574209
1646.774301	78.603208	64.579214
1645.989304	85.635249	64.584218
1645.478581	78.121786	64.589223
1644.834871	83.138074	64.594228
1644.545823	75.285037	64.599233
1643.353762	82.932117	64.604238
1642.497279	80.436351	64.609242
1642.164822	66.020510	64.614247
1641.269953	89.265608	64.619252
1641.020880	78.231752	64.624257
1640.746161	89.841130	64.629262
1639.473655	85.963791	64.634266
1639.050385	76.944610	64.639271
1637.955914	80.854510	64.644276
1637.880341	79.475761	64.649281
1637.056662	79.710849	64.654286
1636.368782	76.872902	64.659290
1635.595496	69.366469	64.664295
1634.986442	87.418891	64.669300
1634.480935	78.299234	64.674305
1633.590817	75.709466	64.679310
1632.671615	81.026575	64.684314
1631.907790	79.793446	64.689319
1631.192517	81.082083	64.694324
1631.301139	79.374443	64.699329
1630.757767	82.745770	64.704334
1629.960116	84.140538	64.709338
1628.895003	77.970440	64.714343
1628.073586	78.597840	64.719348
1627.480622	71.073798	64.724353
1627.138971	88.725762	64.729358
1626.612678	80.585560	64.734362
1625.441191	72.251402	64.739367
1624.645821	73.975397	64.744372
1623.983810	71.317851	64.749377
1623.723501	76.732127	64.754382
1622.946359	76.418921	64.759386
1622.885753	79.186833	64.764391
1622.400150	80.505215	64.769396
1621.039039	76.438535	64.774401
1620.449516	77.462763	64.779406
1619.963428	77.658411	64.784410
1619.222610	69.728925	64.789415
1618.437675	80.014271	64.794420
1617.745223	70.522196	64.799425
1617.048495	83.102230	64.804430
1616.717905	77.173407	64.809434
1616.142425	73.158527	64.814439
1614.642039	75.688414	64.819444
1614.143761	76.923654	64.824449
1613.619828	72.764964	64.829454
1613.005955	77.058990	64.834458
1612.899857	72.691983	64.839463
1612.065406	75.125525	64.844468
1611.006197	70.812184	64.849473
1610.618422	76.727692	64.854478
1609.961222	77.478818	64.859482
1609.481268	71.551654	64.864487
1608.247873	81.163924	64.869492
1607.551547	81.358285	64.874497
1607.169363	73.827566	64.879502
1606.420734	77.835493	64.884506
1606.324067	72.904006	64.889511
1605.145807	82.565865	64.894516
1604.492080	76.223180	64.899521
1603.676646	75.479240	64.904526
1603.056446	78.202023	64.909530
1602.630105	75.869743	64.914535
1601.867321	77.668993	64.919540
1601.662839	75.866020	64.924545
1600.502294	76.824862	64.929550
1599.548154	70.559877	64.934554
1599.105056	69.318377	64.939559
1598.393105	80.162997	64.944564
1598.688459	68.563249	64.949569
1597.334049	72.142298	64.954574
1596.201572	69.904873	64.959578
1595.661470	74.758046	64.964583
1594.917087	80.526790	64.969588
1594.449157	72.044586	64.974593
1594.708473	78.877584	64.979598
1593.942811	86.346542	64.984602
1593.055103	82.359200	64.989607
1592.007940	89.309907	64.994612
1591.901777	83.820098	64.999617
1590.672420	79.437604	65.004622
1589.589979	79.395273	65.009626
1589.422892	75.821718	65.014631
1588.863460	80.077136	65.019636
1588.359768	77.183128	65.024641
1587.231708	70.854318	65.029646
1586.199044	80.838407	65.034650
1586.114573	78.021290	65.039655
1585.342743	88.049095	65.044660
1584.697819	76.609789	65.049665
1584.648488	86.008693	65.054670
1583.425461	87.092591	65.059674
1582.693375	76.195425	65.064679
1581.797404	84.210226	65.069684
1581.432253	79.031237	65.074689
1581.239545	84.993027	65.079694
1580.104242	77.880032	65.084698
1579.796178	74.729432	65.089703
1579.071970	77.484517	65.094708
1578.420635	78.296221	65.099713
1577.208564	80.938015	65.104718
1576.143056	87.808062	65.109722
1575.948871	76.070051	65.114727
1575.589630	81.906912	65.119732
1575.346601	76.853602	65.124737
1574.678403	78.931148	65.129742
1573.766389	85.149166	65.134746
1573.170115	73.632749	65.139751
1572.290317	89.648162	65.144756
1571.265608	80.883843	65.149761
1570.562794	76.845052	65.154766
1569.683145	82.061276	65.159770
1569.467501	72.307367	65.164775
1568.800920	86.935848	65.169780
1568.743035	75.642967	65.174785
1568.078042	74.780514	65.179790
1567.004270	87.418895	65.184794
1566.370375	71.863503	65.189799
1565.545727	79.800739	65.194804
1565.237522	75.043221	65.199809
1564.217630	79.627284	65.204814
1563.415557	83.919687	65.209818
1563.062249	72.711602	65.214823
1562.425044	77.780488	65.219828
1561.960625	76.607038	65.224833
1560.478116	82.206074	65.229838
1559.761824	83.709361	65.234842
1559.592843	78.073418	65.239847
1558.829787	78.760953	65.244852
1558.625479	82.398539	65.249857
1558.235328	75.299612	65.254862
1557.213040	78.601973	65.259866
1556.228153	75.111068	65.264871
1555.672753	75.322474	65.269876
1555.077421	79.324977	65.274881
1554.755932	77.900154	65.279886
1553.477937	81.008181	65.284890
1552.939019	78.078777	65.289895
1552.121036	84.759683	65.294900
1551.780439	75.525536	65.299905
1551.250843	70.322225	65.304910
1550.441783	77.832778	65.309914
1549.688593	69.255569	65.314919
1548.958299	72.737038	65.319924
1548.467814	74.977164	65.324929
1548.199773	74.237720	65.329934
1547.072301	78.096126	65.334938
1546.655783	64.874830	65.339943
1545.821057	75.789429	65.344948
1545.422857	68.474164	65.349953
1544.231870	71.377553	65.354958
1543.191087	71.071574	65.359962
1543.057954	74.718349	65.364967
1542.367943	74.550596	65.369972
1542.001708	71.792453	65.374977
1541.699141	73.526469	65.379982
1540.464476	78.466374	65.384986
1539.554396	70.866596	65.389991
1539.293588	77.266567	65.394996
1538.848147	71.758143	65.400001
1538.432739	73.095346	65.405006
1537.275196	79.633093	65.410010
1536.363069	72.049411	65.415015
1535.940411	73.788319	65.420020
1535.290759	74.218137	65.425025
1534.687251	77.026593	65.430030
1533.617803	80.374305	65.435034
1532.845193	78.923403	65.440039
1532.783636	82.566691	65.445044
1532.209077	80.787843	65.450049
1531.597996	76.395436	65.455054
1530.172988	83.835147	65.460058
1529.516623	80.143807	65.465063
1529.117702	74.613799	65.470068
1528.840608	81.415336	65.475073
1528.534055	74.899229	65.480078
1527.312187	78.070889	65.485082
1526.857557	75.325219	65.490087
1526.250170	74.094071	65.495092
1525.596313	70.369220	65.500097
1524.525382	76.066869	65.505102
1523.656616	78.308768	65.510106
1523.183148	67.359494	65.515111
1522.626298	75.571152	65.520116
1522.375641	69.752652	65.525121
1521.590783	71.374079	65.530126
1520.391921	74.048491	65.535130
1519.811924	76.222421	65.540135
1519.080305	75.088291	65.545140
1519.037135	76.429418	65.550145
1518.797481	72.020566	65.555150
1517.445037	73.766892	65.560154
1517.023154	64.447905	65.565159
1516.192052	64.523359	65.570164
1515.056289	63.256337	65.575169
1514.418552	70.077337	65.580174
1513.890917	80.807521	65.585178
1513.678926	73.129926	65.590183
1512.942673	75.948443	65.595188
1512.308586	78.499985	65.600193
1511.319007	67.634315	65.605198
1510.370358	71.402813	65.610202
1510.371921	76.624084	65.615207
1509.615178	75.621685	65.620212
1508.995879	71.366212	65.625217
1508.007716	72.098999	65.630222
1507.137719	73.864851	65.635226
1506.713761	65.243221	65.640231
1506.296663	66.792012	65.645236
1505.746483	73.097620	65.650241
1505.344835	72.423570	65.655246
1504.079485	81.342355	65.660250
1503.300192	70.321839	65.665255
1503.301961	70.868912	65.670260
1502.325210	71.814356	65.675265
1501.634732	71.408565	65.680270
1500.506228	82.994352	65.685274
1500.130862	71.803982	65.690279
1499.836708	75.880056	65.695284
1498.834570	79.191851	65.700289
1498.170433	78.772412	65.705294
1497.223510	81.927197	65.710298
1496.817917	69.199348	65.715303
1496.075255	83.731113	65.720308
1495.779964	77.080755	65.725313
1495.609518	73.159232	65.730318
1494.129474	80.426352	65.735322
1493.837311	75.273629	65.740327
1493.008690	84.878383	65.745332
1492.187567	76.275718	65.750337
1491.323437	69.299450	65.755342
1490.402873	79.931234	65.760346
1489.990319	74.666757	65.765351
1489.656144	73.997755	65.770356
1489.010826	74.411126	65.775361
1488.774626	75.435998	65.780366
1488.204543	80.850628	65.785370
1487.287945	74.289560	65.790375
1486.797554	80.446897	65.795380
1485.916890	78.013379	65.800385
1484.890695	71.824552	65.805390
1483.947529	78.763492	65.810394
1483.882526	61.495017	65.815399
1483.109441	72.387213	65.820404
1482.670450	64.226880	65.825409
1481.821514	67.955883	65.830414
1480.719313	77.301337	65.835418
1480.539461	72.085034	65.840423
1479.822747	72.968656	65.845428
1479.274133	76.432306	65.850433
1478.442672	76.140393	65.855438
1477.701130	80.396389	65.860442
1477.222130	78.687523	65.865447
1476.954668	81.634972	65.870452
1476.029466	78.877371	65.875457
1475.736109	70.607155	65.880462
1474.703520	87.922642	65.885466
1473.638086	80.886906	65.890471
1472.706656	83.861039	65.895476
1471.942868	81.378986	65.900481
1472.049250	74.787796	65.905486
1471.261054	81.262133	65.910490
1471.081505	79.966151	65.915495
1469.845392	86.156863	65.920500
1468.915975	83.004112	65.925505
1468.635325	72.943582	65.930510
1467.760025	84.977999	65.935514
1467.406696	71.677291	65.940519
1466.402412	82.945296	65.945524
1465.930865	79.967357	65.950529
1465.383682	77.607000	65.955534
1464.757597	78.943007	65.960538
1463.807000	74.919980	65.965543
1463.167869	80.462286	65.970548
1462.414811	86.716573	65.975553
1462.412527	61.636817	65.980558
1461.387542	78.787082	65.985562
1460.785243	72.139798	65.990567
1459.763897	78.810470	65.995572
1459.246783	73.903246	66.000577
1459.305257	69.503788	66.005582
1457.622656	80.922189	66.010586
1456.784616	67.745841	66.015591
1456.150750	77.814813	66.020596
1456.066631	72.715762	66.025601
1455.511548	73.663588	66.030606
1455.053115	80.766767	66.035610
1453.863088	77.131890	66.040615
1453.074207	75.454939	66.045620
1452.755079	78.901041	66.050625
1452.419894	65.570650	66.055630
1451.718831	79.077076	66.060634
1450.566589	75.532391	66.065639
1450.006734	77.513897	66.070644
1449.356018	77.660049	66.075649
1449.113832	63.564237	66.080654
1447.517707	78.042424	66.085658
1446.954446	78.352875	66.090663
1446.499433	72.842840	66.095668
1446.018485	82.341876	66.100673
1445.664084	71.993449	66.105678
1445.268917	80.442774	66.110682
1444.260842	66.550703	66.115687
1443.407226	80.832022	66.120692
1442.499632	80.996930	66.125697
1442.618679	58.920967	66.130702
1441.507465	76.775655	66.135706
1440.792481	74.090311	66.140711
1440.025901	79.835809	66.145716
1439.525309	71.801971	66.150721
1439.226855	70.125918	66.155726
1438.208130	80.532041	66.160730
1437.626253	79.211703	66.165735
1437.355176	76.539378	66.170740
1436.011455	79.318857	66.175745
1435.223546	68.846952	66.180750
1434.485225	71.053950	66.185754
1433.955543	73.497448	66.190759
1433.449480	77.522054	66.195764
1432.806657	70.182621	66.200769
1432.837935	68.985596	66.205774
1431.415322	79.272992	66.210778
1430.902211	75.308172	66.215783
1430.404515	76.634816	66.220788
1429.547494	82.498775	66.225793
1429.104694	66.665484	66.230798
1427.970644	75.066677	66.235802
1427.441948	76.052892	66.240807
1427.105568	68.984875	66.245812
1426.446741	75.351922	66.250817
1425.455182	70.889138	66.255822
1424.803570	81.279487	66.260826
1424.506452	72.022691	66.265831
1424.069100	81.584185	66.270836
1423.031353	71.782789	66.275841
1422.322603	70.378543	66.280846
1421.628117	81.616237	66.285850
1421.215994	77.249006	66.290855
1420.712119	74.913315	66.295860
1419.628695	80.184051	66.300865
1418.939302	73.139033	66.305870
1417.981315	85.760625	66.310874
1417.777170	75.755753	66.315879
1417.442265	78.319682	66.320884
1415.879871	84.567013	66.325889
1415.510262	79.943862	66.330894
1414.999921	79.963628	66.335898
1414.702676	80.892553	66.340903
1414.264317	78.327249	66.345908
1412.867058	80.366185	66.350913
1412.428372	78.926895	66.355918
1411.739768	83.814746	66.360922
1411.348914	80.888647	66.365927
1410.244227	75.522897	66.370932
1409.259123	86.357356	66.375937
1408.848715	80.070672	66.380942
1408.556975	85.130405	66.385946
1408.186838	73.242203	66.390951
1407.097487	70.206368	66.395956
1406.315007	82.260734	66.400961
1406.018746	74.878831	66.405966
1405.184299	81.005715	66.410970
1404.670232	66.803319	66.415975
1403.569617	72.781699	66.420980
1402.749230	75.060100	66.425985
1402.562199	75.892656	66.430990
1401.926380	78.078639	66.435994
1401.685282	66.821223	66.440999
1401.006216	66.675423	66.446004
1399.801275	81.343765	66.451009
1399.750801	68.280367	66.456014
1398.343567	88.140742	66.461018
1397.381452	72.360050	66.466023
1397.090323	74.663128	66.471028
1396.578164	76.914610	66.476033
1396.078048	70.885048	66.481038
1395.535097	76.841013	66.486042
1394.236509	72.225198	66.491047
1393.951861	67.206921	66.496052
1393.332205	81.692333	66.501057
1393.224008	65.820056	66.506062
1391.900291	76.899157	66.511066
1391.056361	76.976691	66.516071
1390.466159	67.395908	66.521076
1389.909134	76.654722	66.526081
1389.312201	74.168250	66.531086
1388.280661	74.026448	66.536090
1387.509614	68.293853	66.541095
1387.354065	69.392645	66.546100
1386.481302	77.712891	66.551105
1386.491484	74.849201	66.556110
1385.770262	80.168025	66.561114
1384.679603	75.640587	66.566119
1384.343752	73.530510	66.571124
1383.310412	68.700644	66.576129
1382.565704	67.298973	66.581134
1381.415472	71.520612	66.586138
1381.154299	72.060600	66.591143
1380.835067	71.550090	66.596148
1380.274807	70.204252	66.601153
1380.058402	67.655712	66.606158
1378.645571	75.747999	66.611162
1377.774997	71.494664	66.616167
1377.588885	72.853786	66.621172
1377.213411	79.759277	66.626177
1376.638192	71.221651	66.631182
1375.730851	76.631567	66.636186
1374.860296	74.866699	66.641191
1373.770747	77.498565	66.646196
1372.670786	77.244642	66.651201
1372.808862	62.984315	66.656206
1372.056418	76.500494	66.661210
1371.675637	75.285399	66.666215
1371.253123	71.944867	66.671220
1369.878214	78.733280	66.676225
1369.353242	75.027408	66.681230
1369.127381	76.872251	66.686234
1368.506852	85.373182	66.691239
1367.231749	74.805289	66.696244
1366.121208	79.454295	66.701249
1366.327516	70.108015	66.706254
1365.770510	72.633140	66.711258
1365.087830	76.356248	66.716263
1364.162862	75.596684	66.721268
1363.304221	73.938737	66.726273
1362.935298	76.579043	66.731278
1362.573322	80.519252	66.736282
1361.898998	77.207715	66.741287
1360.985079	74.054123	66.746292
1360.047320	75.909644	66.751297
1359.960730	67.177643	66.756302
1358.848295	77.895156	66.761306
1357.571677	75.978807	66.766311
1357.450440	74.309283	66.771316
1356.772475	77.796673	66.776321
1356.641082	69.109643	66.781326
1355.973447	75.621608	66.786330
1355.039655	77.741432	66.791335
1354.333156	74.687330	66.796340
1353.484652	79.545420	66.801345
1353.203319	71.497248	66.806350
1352.025984	76.691473	66.811354
1351.169509	71.240559	66.816359
1350.856562	71.268379	66.821364
1350.116290	83.943681	66.826369
1350.269349	79.314716	66.831374
1349.701901	77.840716	66.836378
1348.232304	75.932976	66.841383
1348.004915	70.809405	66.846388
1347.068363	76.567755	66.851393
1346.191185	67.056268	66.856398
1345.283023	68.404033	66.861402
1344.290546	74.909298	66.866407
1344.571819	68.310809	66.871412
1343.736507	71.938338	66.876417
1343.739864	66.965742	66.881422
1342.370537	80.013874	66.886426
1341.707540	75.243417	66.891431
1341.508191	71.837447	66.896436
1340.468223	78.769742	66.901441
1339.691453	72.147082	66.906446
1339.006979	76.911285	66.911450
1338.362533	83.886355	66.916455
1338.162825	71.073777	66.921460
1337.060227	75.235822	66.926465
1336.421949	70.388897	66.931470
1335.454260	78.635938	66.936474
1334.835909	84.056692	66.941479
1335.055700	69.151003	66.946484
1333.991661	72.177803	66.951489
1333.101502	69.391033	66.956494
1332.292074	72.484586	66.961498
1331.798628	74.740988	66.966503
1331.468929	70.346480	66.971508
1330.286421	76.184942	66.976513
1329.922435	72.718417	66.981518
1329.142338	71.847521	66.986522
1328.690845	78.383474	66.991527
1328.359025	74.724174	66.996532
1327.299279	78.166616	67.001537
1326.827035	72.594694	67.006542
1326.148754	74.915180	67.011546
1324.868640	73.142908	67.016551
1324.582552	68.033406	67.021556
1323.572531	72.715330	67.026561
1323.633538	68.130967	67.031566
1322.993714	73.809027	67.036570
1321.725109	73.310700	67.041575
1321.292264	67.806635	67.046580
1320.656497	69.842813	67.051585
1320.417702	70.246783	67.056590
1318.631331	67.775985	67.061594
1318.063595	70.665530	67.066599
1317.743159	70.951592	67.071604
1317.027030	84.638633	67.076609
1317.029321	68.837113	67.081614
1316.623073	71.589015	67.086618
1315.650687	74.090310	67.091623
1315.036512	62.116365	67.096628
1313.942394	72.990250	67.101633
1312.932186	69.358394	67.106638
1312.482899	82.586684	67.111642
1311.635030	81.882690	67.116647
1311.161817	72.881002	67.121652
1310.765501	79.275718	67.126657
1310.575236	66.527882	67.131662
1309.492229	69.330623	67.136666
1308.724620	72.106868	67.141671
1308.392893	65.889705	67.146676
1307.649989	74.796456	67.151681
1307.117445	62.383750	67.156686
1306.296469	70.757280	67.161690
1305.433520	69.316085	67.166695
1304.595360	72.008931	67.171700
1303.627286	68.723622	67.176705
1303.148796	77.712913	67.181710
1302.746187	68.168563	67.186714
1302.258002	74.431227	67.191719
1302.001202	66.699293	67.196724
1300.559896	72.451182	67.201729
1300.091087	64.921697	67.206734
1299.557825	66.705034	67.211738
1299.018187	66.332085	67.216743
1298.594917	72.557618	67.221748
1296.994957	71.135846	67.226753
1296.589170	73.277389	67.231758
1296.234901	70.774433	67.236762
1295.469949	75.234470	67.241767
1295.086002	67.931191	67.246772
1293.909633	73.637801	67.251777
1293.448461	73.233452	67.256782
1292.741470	76.993558	67.261786
1292.439110	69.885467	67.266791
1291.949786	74.817347	67.271796
1290.759849	76.236745	67.276801
1290.566050	64.531858	67.281806
1290.107421	72.111327	67.286810
1288.704595	76.354247	67.291815
1287.980371	65.823394	67.296820
1287.532809	80.909084	67.301825
1287.108790	73.391400	67.306830
1286.299097	73.551835	67.311834
1284.892654	74.001130	67.316839
1284.665979	81.638339	67.321844
1283.957702	80.569953	67.326849
1283.559305	73.436131	67.331854
1283.534730	74.704916	67.336858
1283.034706	69.768213	67.341863
1282.269693	66.964717	67.346868
1281.449436	73.220263	67.351873
1280.333033	75.329726	67.356878
1279.646225	74.734175	67.361882
1279.123144	79.871702	67.366887
1278.544004	77.885485	67.371892
1277.233414	86.242268	67.376897
1276.434922	71.384965	67.381902
1276.072928	80.663244	67.386906
1275.484135	79.637363	67.391911
1275.457335	67.484869	67.396916
1274.714128	84.576178	67.401921
1273.874661	70.242641	67.406926
1273.181210	73.538544	67.411930
1272.642656	74.786558	67.416935
1272.208852	70.343959	67.421940
1270.582361	67.278485	67.426945
1270.039649	67.998874	67.431950
1269.872239	77.933770	67.436954
1269.346112	79.654478	67.441959
1268.872250	71.854562	67.446964
1267.415415	81.119285	67.451969
1267.188798	74.404434	67.456974
1266.682597	70.829647	67.461978
1265.816210	71.855400	67.466983
1265.109580	70.922379	67.471988
1264.028404	73.966124	67.476993
1263.470203	72.069622	67.481998
1263.102398	79.628347	67.487002
1262.739232	75.806883	67.492007
1262.132064	72.229229	67.497012
1261.085963	70.055496	67.502017
1260.516629	65.140862	67.507022
1260.035329	71.143811	67.512026
1259.394880	66.385567	67.517031
1258.544051	63.187290	67.522036
1257.879261	74.174272	67.527041
1257.771280	66.857079	67.532046
1256.370270	65.723821	67.537050
1255.364011	76.638949	67.542055
1255.267441	69.449253	67.547060
1254.326446	78.515253	67.552065
1254.107343	69.777529	67.557070
1253.254915	72.781747	67.562074
1252.242979	75.540092	67.567079
1252.031864	61.545048	67.572084
1251.430338	71.878563	67.577089
1250.916297	77.159738	67.582094
1250.027072	73.131772	67.587098
1249.231052	76.532303	67.592103
1248.795827	69.377540	67.597108
1248.052227	71.725778	67.602113
1246.963372	70.432495	67.607118
1246.426345	76.359153	67.612122
1245.682022	74.847074	67.617127
1245.673414	57.530263	67.622132
1244.976753	72.119388	67.627137
1243.984850	76.953002	67.632142
1243.153137	69.186349	67.637146
1242.800712	75.288657	67.642151
1242.378076	64.637321	67.647156
1241.253386	71.685622	67.652161
1240.218466	71.462415	67.657166
1239.889754	73.984374	67.662170
1238.902807	71.984173	67.667175
1239.130167	65.916234	67.672180
1238.548793	75.650452	67.677185
1237.393994	74.262003	67.682190
1236.916635	59.486126	67.687194
1236.316502	75.269442	67.692199
1235.857969	65.555807	67.697204
1234.520786	79.360547	67.702209
1234.087618	70.401401	67.707214
1233.839520	67.711258	67.712218
1232.649705	77.772480	67.717223
1232.074840	74.574478	67.722228
1231.250376	75.208795	67.727233
1230.717196	77.263373	67.732238
1230.553915	75.414461	67.737242
1229.463620	78.995842	67.742247
1228.702512	67.606695	67.747252
1227.858550	78.537023	67.752257
1227.558532	70.583313	67.757262
1227.298060	73.600629	67.762266
1225.899400	78.696062	67.767271
1225.365219	72.347105	67.772276
1224.906821	68.703224	67.777281
1224.386478	70.620141	67.782286
1223.644945	69.410404	67.787290
1222.846459	73.664478	67.792295
1222.434829	68.191754	67.797300
1221.777704	80.256176	67.802305
1220.736262	73.344489	67.807310
1220.173433	75.611945	67.812314
1219.374729	78.360045	67.817319
1219.283174	75.425807	67.822324
1218.160213	68.318928	67.827329
1217.410418	62.888951	67.832334
1216.743680	62.816934	67.837338
1216.064620	67.119823	67.842343
1215.884547	66.489430	67.847348
1215.014165	70.311810	67.852353
1214.298297	65.109829	67.857358
1213.508322	70.226731	67.862362
1212.851613	71.152922	67.867367
1212.933315	63.747221	67.872372
1211.666585	73.100004	67.877377
1210.914324	76.433661	67.882382
1210.223793	70.800290	67.887386
1209.883175	77.788560	67.892391
1209.254170	69.718441	67.897396
1207.818484	70.874183	67.902401
1207.551460	67.087903	67.907406
1207.129084	64.288286	67.912410
1206.629883	69.087704	67.917415
1205.826474	61.051638	67.922420
1204.707054	67.394205	67.927425
1204.325492	61.833127	67.932430
1203.681046	66.004355	67.937434
1203.278382	63.819777	67.942439
1202.215060	60.425081	67.947444
1201.838677	69.407597	67.952449
1201.186511	64.156065	67.957454
1200.896315	58.194099	67.962458
1199.778894	69.029145	67.967463
1199.326720	62.921049	67.972468
1198.866027	66.613616	67.977473
1197.641166	64.943013	67.982478
1196.991328	65.518026	67.987482
1196.094549	74.696857	67.992487
1195.975529	65.530061	67.997492
1195.278586	69.723835	68.002497
1194.351439	58.411582	68.007502
1193.521238	58.748775	68.012506
1192.805210	75.093005	68.017511
1192.613448	66.109669	68.022516
1191.982419	63.710677	68.027521
1191.423121	68.262609	68.032526
1190.352951	58.594234	68.037530
1189.766032	67.706431	68.042535
1189.617551	70.858904	68.047540
1188.586604	75.138921	68.052545
1187.750691	64.911306	68.057550
1187.203136	64.750954	68.062554
1186.724719	67.383463	68.067559
1186.116631	60.726152	68.072564
1185.039108	67.855280	68.077569
1184.331642	64.454453	68.082574
1184.205117	67.917251	68.087578
1183.536075	69.088264	68.092583
1182.693183	67.615538	68.097588
1181.487787	72.098348	68.102593
1180.944924	70.459627	68.107598
1180.561322	71.817055	68.112602
1180.240334	75.279246	68.117607
1179.576441	62.461694	68.122612
1178.354756	65.557782	68.127617
1177.800056	71.927235	68.132622
1177.942606	69.890910	68.137626
1176.311343	79.437312	68.142631
1175.590782	70.457660	68.147636
1175.200292	63.625390	68.152641
1174.812910	71.977293	68.157646
1174.841061	64.248947	68.162650
1173.497770	68.911390	68.167655
1172.976644	64.220927	68.172660
1172.203553	65.862661	68.177665
1171.052376	66.649889	68.182670
1170.291228	68.859011	68.187674
1169.467830	69.671375	68.192679
1169.467711	60.022045	68.197684
1169.112881	74.395958	68.202689
1168.170252	68.779046	68.207694
1167.437211	58.882015	68.212698
1166.551972	68.885347	68.217703
1166.500389	65.112115	68.222708
1165.502838	68.771808	68.227713
1164.327002	67.847215	68.232718
1163.770117	57.721892	68.237722
1162.938917	70.413251	68.242727
1162.766747	71.587238	68.247732
1162.362623	66.821395	68.252737
1161.728071	72.452914	68.257742
1160.912960	54.568963	68.262746
1160.371735	65.485834	68.267751
1159.874418	58.981225	68.272756
1158.530255	62.694475	68.277761
1157.976995	68.243675	68.282766
1157.532884	60.689802	68.287770
1157.048748	69.654767	68.292775
1156.420655	66.779071	68.297780
1155.286682	62.206596	68.302785
1154.494764	61.446448	68.307790
1154.236464	60.755963	68.312794
1153.713673	68.642120	68.317799
1153.066909	59.895176	68.322804
1152.136634	59.341542	68.327809
1151.376028	63.993310	68.332814
1151.290172	58.708486	68.337818
1150.123808	69.094012	68.342823
1149.311504	63.841161	68.347828
1148.751823	62.392783	68.352833
1148.110048	64.767428	68.357838
1148.020385	56.553198	68.362842
1146.748538	64.597929	68.367847
1146.079061	61.727242	68.372852
1145.374867	62.366109	68.377857
1144.894553	64.360252	68.382862
1144.978994	60.827163	68.387866
1143.834091	61.148199	68.392871
1143.086187	65.264933	68.397876
1142.494591	68.088919	68.402881
1141.652568	70.645232	68.407886
1140.912943	59.749458	68.412890
1139.942770	70.054893	68.417895
1139.802051	65.255041	68.422900
1139.357923	65.272214	68.427905
1138.539985	64.923069	68.432910
1138.258952	59.569943	68.437914
1136.730753	74.605175	68.442919
1135.855512	68.509197	68.447924
1135.255827	68.719852	68.452929
1134.668618	68.674631	68.457934
1134.246933	70.754069	68.462938
1133.800966	69.235565	68.467943
1133.664293	68.257649	68.472948
1132.572868	69.095314	68.477953
1131.678330	73.013026	68.482958
1131.389760	65.431261	68.487962
1130.441957	69.904654	68.492967
1129.600255	61.519892	68.497972
1129.092518	65.377649	68.502977
1128.465516	69.738510	68.507982
1128.065317	68.496582	68.512986
1126.846897	72.295504	68.517991
1126.174878	72.178620	68.522996
1125.787301	68.600766	68.528001
1125.114904	70.926671	68.533006
1124.953435	67.763863	68.538010
1123.858306	72.453086	68.543015
1123.195840	60.367047	68.548020
1122.845151	66.776593	68.553025
1121.768657	68.108633	68.558030
1120.822454	69.013089	68.563034
1119.954080	80.625422	68.568039
1119.736702	75.192782	68.573044
1119.778514	70.985219	68.578049
1118.814707	74.349399	68.583054
1117.471422	65.524030	68.588058
1116.776723	70.013935	68.593063
1116.446135	70.844115	68.598068
1116.207872	65.375377	68.603073
1115.460401	70.301037	68.608078
1114.774963	60.774926	68.613082
1113.676315	72.157378	68.618087
1113.481171	60.391243	68.623092
1112.732517	73.966779	68.628097
1111.881630	67.855898	68.633102
1111.241774	65.092474	68.638106
1110.697472	67.912097	68.643111
1110.081518	63.113732	68.648116
1109.156556	63.641071	68.653121
1108.020637	69.431207	68.658126
1107.783309	61.325626	68.663130
1107.458176	65.728355	68.668135
1107.069088	62.655377	68.673140
1106.142254	62.941738	68.678145
1105.035665	68.441777	68.683150
1104.894186	62.363126	68.688154
1104.055754	67.897777	68.693159
1103.061894	65.394101	68.698164
1102.385444	74.026965	68.703169
1101.867702	72.690199	68.708174
1101.761166	63.374774	68.713178
1100.930266	69.950606	68.718183
1099.814425	75.240806	68.723188
1099.293169	77.378669	68.728193
1098.618887	75.298821	68.733198
1098.467652	67.859217	68.738202
1097.488252	75.813295	68.743207
1096.839051	73.019821	68.748212
1096.575328	66.419716	68.753217
1095.340826	67.664940	68.758222
1094.659213	61.810994	68.763226
1094.035415	78.323493	68.768231
1093.182047	59.373316	68.773236
1093.319687	67.132334	68.778241
1091.954570	76.847753	68.783246
1091.250150	64.574429	68.788250
1090.733834	69.837063	68.793255
1090.740667	67.054341	68.798260
1089.589284	62.956183	68.803265
1088.478506	71.271788	68.808270
1088.068760	65.412438	68.813274
1087.487700	66.290354	68.818279
1087.064785	66.722060	68.823284
1085.895636	63.497218	68.828289
1085.190167	65.284338	68.833294
1085.123589	61.914048	68.838298
1084.355627	67.700847	68.843303
1083.829874	68.041680	68.848308
1082.936832	65.815290	68.853313
1082.344465	70.812477	68.858318
1081.755075	60.741236	68.863322
1080.692528	72.479081	68.868327
1080.029120	65.862141	68.873332
1079.774514	68.481138	68.878337
1078.876619	68.056422	68.883342
1078.550241	60.778731	68.888346
1077.129268	62.788498	68.893351
1076.705334	59.221172	68.898356
1076.557217	60.139021	68.903361
1075.701294	73.796284	68.908366
1074.776809	63.385690	68.913370
1073.798614	71.628167	68.918375
1073.313726	67.879723	68.923380
1072.883572	74.995785	68.928385
1072.186516	72.211509	68.933390
1072.024157	59.311056	68.938394
1071.040040	67.237502	68.943399
1070.458376	69.135818	68.948404
1070.238217	64.309188	68.953409
1068.962809	65.772246	68.958414
1068.189847	58.149291	68.963418
1067.476934	65.761350	68.968423
1067.308972	62.601159	68.973428
1066.450508	60.317234	68.978433
1065.328615	61.528786	68.983438
1064.834299	60.309729	68.988442
1064.460393	61.121575	68.993447
1063.878627	59.490650	68.998452
1062.999857	63.782768	69.003457
1062.177536	66.402202	69.008462
1061.420619	56.885910	69.013466
1061.177265	67.971444	69.018471
1060.593571	69.281876	69.023476
1059.830246	62.654033	69.028481
1058.934928	65.972641	69.033486
1058.593978	62.213917	69.038490
1058.119742	67.871986	69.043495
1057.268387	66.701851	69.048500
1056.604198	62.680739	69.053505
1055.629076	65.215675	69.058510
1055.270941	52.106682	69.063514
1054.309608	62.953206	69.068519
1053.536129	64.311181	69.073524
1053.067314	61.780760	69.078529
1052.259129	66.670362	69.083534
1052.122747	60.406402	69.088538
1050.961684	68.351546	69.093543
1050.236920	65.483376	69.098548
1049.683583	64.341522	69.103553
1049.090692	69.102253	69.108558
1048.961713	55.351241	69.113562
1048.040265	66.692899	69.118567
1047.187384	64.824413	69.123572
1046.739055	64.821771	69.128577
1045.837520	75.203048	69.133582
1045.343185	66.042373	69.138586
1044.677477	64.409038	69.143591
1043.968676	71.559975	69.148596
1043.271273	67.036366	69.153601
1042.196442	76.092177	69.158606
1041.881442	64.127502	69.163610
1041.196749	66.444344	69.168615
1040.627034	70.299362	69.173620
1040.490871	66.203701	69.178625
1039.168330	76.150490	69.183630
1038.613824	57.594345	69.188634
1037.984752	75.640498	69.193639
1036.947311	65.985915	69.198644
1036.736796	63.395476	69.203649
1035.687346	75.055557	69.208654
1035.545220	63.856594	69.213658
1034.868178	69.531167	69.218663
1034.122715	75.175627	69.223668
1033.478994	61.422936	69.228673
1032.400012	66.945417	69.233678
1032.296944	65.501685	69.238682
1030.973009	73.330827	69.243687
1030.169991	71.205251	69.248692
1029.414978	69.625554	69.253697
1029.041687	70.270148	69.258702
1028.959876	54.628734	69.263706
1028.405095	79.398305	69.268711
1027.716312	68.141241	69.273716
1026.834895	68.095548	69.278721
1026.211457	69.611009	69.283726
1025.732481	63.366870	69.288730
1024.650641	66.480200	69.293735
1024.108962	68.318546	69.298740
1023.776487	63.025665	69.303745
1022.733063	65.702370	69.308750
1021.958925	69.564687	69.313754
1020.955445	63.897599	69.318759
1020.539607	63.225887	69.323764
1020.356698	60.446552	69.328769
1019.739956	61.795367	69.333774
1019.185676	57.297880	69.338778
1017.895314	64.740055	69.343783
1017.350482	67.670167	69.348788
1017.013587	58.542802	69.353793
1015.850358	62.140599	69.358798
1015.453157	59.330707	69.363802
1014.660749	67.963110	69.368807
1014.089007	63.257088	69.373812
1014.233231	59.056891	69.378817
1012.585437	64.863856	69.383822
1012.200630	61.295047	69.388826
1011.635401	62.878519	69.393831
1010.791881	64.548853	69.398836
1010.006851	62.043527	69.403841
1009.070886	70.932168	69.408846
1008.559003	60.001786	69.413850
1008.692086	66.465249	69.418855
1008.288564	68.295807	69.423860
1006.898195	62.890564	69.428865
1006.232958	66.409123	69.433870
1006.076845	64.655286	69.438874
1004.732867	69.702700	69.443879
1003.973972	61.796828	69.448884
1003.427026	71.117159	69.453889
1003.254100	70.629150	69.458894
1002.608617	69.077764	69.463898
1001.326871	61.833840	69.468903
1000.539079	70.422935	69.473908
1000.584139	61.244255	69.478913
999.764298	71.216721	69.483918
999.020520	61.554856	69.488922
998.312974	69.016264	69.493927
997.434061	67.940423	69.498932
997.266101	68.631196	69.503937
996.535573	73.059021	69.508942
995.398692	67.411595	69.513946
994.808300	73.080273	69.518951
994.586614	74.475040	69.523956
994.100124	72.953550	69.528961
992.828167	67.758132	69.533966
992.182876	69.092572	69.538970
991.745871	68.961980	69.543975
991.320505	70.442776	69.548980
990.651228	57.225612	69.553985
989.511697	63.117291	69.558990
989.170557	59.284493	69.563994
988.911288	70.459293	69.568999
987.443017	75.988548	69.574004
986.871059	77.366515	69.579009
986.154455	75.055312	69.584014
986.008259	70.726283	69.589018
985.366260	70.224610	69.594023
984.426514	71.435597	69.599028
983.815031	70.643636	69.604033
983.193325	68.583842	69.609038
982.533321	65.587115	69.614042
981.490758	73.011954	69.619047
980.655184	61.677347	69.624052
980.442575	61.148345	69.629057
980.141478	75.512128	69.634062
979.694644	69.226613	69.639066
978.522663	66.691411	69.644071
977.773950	73.370892	69.649076
977.434080	62.072521	69.654081
976.274098	70.559999	69.659086
975.333266	69.162855	69.664090
975.121512	62.385768	69.669095
974.320870	69.563949	69.674100
974.387953	62.386093	69.679105
973.307822	73.445518	69.684110
972.780149	61.193006	69.689114
971.768801	73.570870	69.694119
971.061412	67.968649	69.699124
970.873516	62.914546	69.704129
969.500701	73.064906	69.709134
968.906149	60.373603	69.714138
968.457450	68.762083	69.719143
968.028423	63.484577	69.724148
967.643437	62.856851	69.729153
966.557237	69.534847	69.734158
965.923445	66.045093	69.739162
965.510148	78.529641	69.744167
964.950854	71.407308	69.749172
964.458219	64.457300	69.754177
963.038788	71.475336	69.759182
962.834743	74.769123	69.764186
962.059082	73.374084	69.769191
960.660809	63.887354	69.774196
960.302902	70.673380	69.779201
959.752418	75.059946	69.784206
959.726036	71.705343	69.789210
959.412172	68.860120	69.794215
957.877389	70.127965	69.799220
957.617057	70.587435	69.804225
956.671431	77.888047	69.809230
955.843371	74.635794	69.814234
955.152884	72.716264	69.819239
954.429275	70.097101	69.824244
954.206103	67.015093	69.829249
953.531848	64.717664	69.834254
953.169635	65.021458	69.839258
951.930760	66.125519	69.844263
951.557205	68.725607	69.849268
951.368014	70.019011	69.854273
950.143352	67.608901	69.859278
949.372689	67.436799	69.864282
948.751503	65.444742	69.869287
948.351197	75.079215	69.874292
947.580935	69.969560	69.879297
946.522947	77.579796	69.884302
945.714783	67.855654	69.889306
945.164288	71.105229	69.894311
944.919942	71.581080	69.899316
944.735214	63.022452	69.904321
943.059566	75.663744	69.909326
942.718363	72.100622	69.914330
942.390237	59.896790	69.919335
941.740105	61.473288	69.924340
940.845036	61.836657	69.929345
939.962165	68.550111	69.934350
939.588176	71.237004	69.939354
939.196292	66.907658	69.944359
937.820776	72.934690	69.949364
937.329802	64.235567	69.954369
936.406221	68.749323	69.959374
935.997135	68.158554	69.964378
935.910902	67.379206	69.969383
935.141868	72.926514	69.974388
934.406109	61.569734	69.979393
933.659275	68.862364	69.984398
933.224919	72.443545	69.989402
932.499497	67.159601	69.994407
931.162059	72.059352	69.999412
931.043885	67.557134	70.004417
930.353578	78.582919	70.009422
929.835375	74.570148	70.014426
928.763375	71.968593	70.019431
928.193049	71.859231	70.024436
928.199562	59.006050	70.029441
927.155342	65.212171	70.034446
925.937185	72.505701	70.039450
925.572323	69.487248	70.044455
924.949347	73.470614	70.049460
924.787280	67.847851	70.054465
923.619574	71.326551	70.059470
922.983931	67.215779	70.064474
922.405887	70.149618	70.069479
921.836500	74.241152	70.074484
921.416654	57.754686	70.079489
920.119631	66.109450	70.084494
919.555038	64.813298	70.089498
919.242355	62.179208	70.094503
918.332551	79.505223	70.099508
917.549833	68.704704	70.104513
916.766217	73.541548	70.109518
916.326289	69.513169	70.114522
916.125376	71.887087	70.119527
915.249618	73.643007	70.124532
914.456511	66.822837	70.129537
913.906269	68.014434	70.134542
913.270928	62.271456	70.139546
912.245997	66.101178	70.144551
911.574968	76.597189	70.149556
911.063979	64.242691	70.154561
910.432518	70.014114	70.159566
910.284220	69.613656	70.164570
909.191050	66.435157	70.169575
908.080486	73.492371	70.174580
907.903173	59.980892	70.179585
907.428584	64.462618	70.184590
906.693287	63.799194	70.189594
905.974041	71.082709	70.194599
905.215695	67.510295	70.199604
905.123201	57.634422	70.204609
903.624179	66.425048	70.209614
902.837847	66.810547	70.214618
902.509664	67.865876	70.219623
901.830007	66.690545	70.224628
901.624346	59.540337	70.229633
900.382178	70.051556	70.234638
899.517089	66.959762	70.239642
899.337658	63.498635	70.244647
898.694600	68.309956	70.249652
898.105602	56.975568	70.254657
897.204229	63.595782	70.259662
896.804305	58.603824	70.264666
896.656759	63.288965	70.269671
894.998328	69.949256	70.274676
894.691518	57.880819	70.279681
893.830270	63.291421	70.284686
893.426205	62.108498	70.289690
892.299453	67.209699	70.294695
891.440465	66.737857	70.299700
891.237367	56.348154	70.304705
890.624919	63.843330	70.309710
890.376615	60.536671	70.314714
889.811028	61.550941	70.319719
888.540470	66.230329	70.324724
888.240239	61.585206	70.329729
887.533117	69.253151	70.334734
886.572372	62.962729	70.339738
885.907902	59.364342	70.344743
885.095246	70.012207	70.349748
884.928671	69.431731	70.354753
884.380923	81.909299	70.359758
883.435808	76.781764	70.364762
882.886969	67.970438	70.369767
882.157629	68.402066	70.374772
881.417641	62.644216	70.379777
880.266361	69.700035	70.384782
879.718164	71.101050	70.389786
879.509056	64.881802	70.394791
878.846241	67.512172	70.399796
878.560401	59.083195	70.404801
877.517558	63.767341	70.409806
876.412500	69.688272	70.414810
876.384793	64.646531	70.419815
875.604127	69.706844	70.424820
874.727856	68.286847	70.429825
874.207899	74.070492	70.434830
873.493788	68.245445	70.439834
873.357983	68.204126	70.444839
871.873015	73.586286	70.449844
871.346171	61.291100	70.454849
870.558363	67.290845	70.459854
870.369109	70.087113	70.464858
869.703779	65.430721	70.469863
868.527440	70.905682	70.474868
867.975897	63.801073	70.479873
867.658347	69.959356	70.484878
867.141071	70.481812	70.489882
866.353788	72.001313	70.494887
865.329923	72.878800	70.499892
865.107754	65.395329	70.504897
864.458347	69.523264	70.509902
863.491090	69.620604	70.514906
862.685958	64.724692	70.519911
862.059532	73.122551	70.524916
861.787259	64.656720	70.529921
861.653149	68.887135	70.534926
860.449581	72.308493	70.539930
860.048131	64.829906	70.544935
858.622095	74.165610	70.549940
857.711478	71.610939	70.554945
857.079743	69.480235	70.559950
856.845058	70.438685	70.564954
856.600757	58.678853	70.569959
856.196529	74.032034	70.574964
855.626691	62.472254	70.579969
854.468598	69.011922	70.584974
853.856693	64.766505	70.589978
852.880247	53.471734	70.594983
851.765747	71.516315	70.599988
851.348455	57.071640	70.604993
850.705273	69.848246	70.609998
850.140863	63.122585	70.615002
850.101515	60.224220	70.620007
849.020164	75.825542	70.625012
848.614682	62.104388	70.630017
848.058978	65.766397	70.635022
847.287482	66.475983	70.640026
846.320546	57.587727	70.645031
845.391579	73.037054	70.650036
845.259962	61.730798	70.655041
844.654809	56.618556	70.660046
843.777434	67.710396	70.665050
842.937064	59.328699	70.670055
842.462115	64.072267	70.675060
841.852640	60.566065	70.680065
841.411615	62.282766	70.685070
840.041691	69.363944	70.690074
839.918721	55.506362	70.695079
838.882552	62.919187	70.700084
839.014584	61.422271	70.705089
837.817044	67.790028	70.710094
837.224940	64.659532	70.715098
836.721616	55.995525	70.720103
835.521467	65.106039	70.725108
834.659859	61.696746	70.730113
834.086529	66.105892	70.735118
833.441162	64.951930	70.740122
833.306056	57.090329	70.745127
832.651055	63.097326	70.750132
832.423581	61.873685	70.755137
831.212444	66.606718	70.760142
830.165602	61.146897	70.765146
830.104433	61.557326	70.770151
829.837957	74.789637	70.775156
828.651898	61.400913	70.780161
827.781735	66.677336	70.785166
827.360348	71.571656	70.790170
826.696546	69.875000	70.795175
825.670006	65.947913	70.800180
825.034522	63.519769	70.805185
824.835175	70.542338	70.810190
824.171075	66.215351	70.815194
823.335260	61.653925	70.820199
822.246844	74.014135	70.825204
822.004461	59.443851	70.830209
821.523925	59.119944	70.835214
820.821151	68.152862	70.840218
819.996094	65.303886	70.845223
819.172211	67.502592	70.850228
818.769947	63.920829	70.855233
818.294757	55.514125	70.860238
817.336892	67.910319	70.865242
816.916744	64.774531	70.870247
816.087990	61.982917	70.875252
815.368039	67.322163	70.880257
814.696709	61.619640	70.885262
814.368335	63.901889	70.890266
813.831503	55.296841	70.895271
812.192594	56.814740	70.900276
811.770624	60.803973	70.905281
811.138962	58.261684	70.910286
810.609964	71.285047	70.915290
810.680159	56.803778	70.920295
809.247513	62.661767	70.925300
808.603016	59.744626	70.930305
808.023000	57.088459	70.935310
807.686205	60.374999	70.940314
807.251283	47.429695	70.945319
805.904736	59.898803	70.950324
805.212729	63.896335	70.955329
804.988796	61.095168	70.960334
804.143575	62.283286	70.965338
803.314033	53.362141	70.970343
802.496529	69.604288	70.975348
802.148501	61.413885	70.980353
801.794131	57.873388	70.985358
800.771641	69.169692	70.990362
800.302679	64.439482	70.995367
799.173334	69.034927	71.000372
798.977491	63.363942	71.005377
798.589234	64.687470	71.010382
797.605118	60.029816	71.015386
796.916150	57.006218	71.020391
795.905628	66.961774	71.025396
795.712952	65.177505	71.030401
794.908497	67.294277	71.035406
794.147469	66.231280	71.040410
793.782086	60.191470	71.045415
792.753038	65.397004	71.050420
792.575379	62.561663	71.055425
791.719304	51.175221	71.060430
790.866359	63.570483	71.065434
790.721851	57.621667	71.070439
789.298352	61.092261	71.075444
788.713334	64.277973	71.080449
788.121990	57.215998	71.085454
787.692335	56.842996	71.090458
787.340492	55.109302	71.095463
786.278359	63.406224	71.100468
785.468493	58.309245	71.105473
784.931910	56.937703	71.110478
784.547466	59.981094	71.115482
783.582363	55.801395	71.120487
782.848323	59.190607	71.125492
781.951174	59.921795	71.130497
781.785573	54.955635	71.135502
781.127675	60.761250	71.140506
780.537347	55.309197	71.145511
779.472013	62.956922	71.150516
778.887273	62.685884	71.155521
778.887792	60.158070	71.160526
777.867482	67.166266	71.165530
777.098080	54.140178	71.170535
776.394142	62.796391	71.175540
775.986107	51.414316	71.180545
775.227364	58.823990	71.185550
774.178381	66.549540	71.190554
774.093741	57.934008	71.195559
773.085775	59.928645	71.200564
772.361604	57.125127	71.205569
771.470423	59.454411	71.210574
770.879323	56.475164	71.215578
770.982690	53.686546	71.220583
769.851656	61.824131	71.225588
769.194957	62.799316	71.230593
768.500659	63.728449	71.235598
767.926098	64.838792	71.240602
767.194426	56.088159	71.245607
766.059630	62.535840	71.250612
765.686565	47.177407	71.255617
765.184648	53.516432	71.260622
764.815990	63.711998	71.265626
764.240866	58.262259	71.270631
762.898707	57.276031	71.275636
762.450450	53.599103	71.280641
762.239407	56.165452	71.285646
760.993040	58.809914	71.290650
759.995703	48.564049	71.295655
759.256867	62.507072	71.300660
758.797352	59.172560	71.305665
758.709951	54.135603	71.310670
758.225376	58.406048	71.315674
757.878094	57.313456	71.320679
756.683605	52.683011	71.325684
756.298312	52.173641	71.330689
755.372128	51.920705	71.335694
754.278791	52.711526	71.340698
753.675174	55.174802	71.345703
753.041617	55.288438	71.350708
752.718794	66.113802	71.355713
752.402584	58.864525	71.360718
751.208569	57.307509	71.365722
750.606081	56.842184	71.370727
750.206328	68.971332	71.375732
749.458346	51.613080	71.380737
748.458524	61.371398	71.385742
747.817064	61.721262	71.390746
747.541458	48.741147	71.395751
746.889525	58.768926	71.400756
745.898431	54.091907	71.405761
745.526835	59.520779	71.410766
744.815110	65.965760	71.415770
744.097463	57.222365	71.420775
743.248678	60.036920	71.425780
742.346531	60.675877	71.430785
742.060280	58.882859	71.435790
741.528496	65.368575	71.440794
741.296480	51.425878	71.445799
739.613081	55.975523	71.450804
739.330996	59.652330	71.455809
739.236342	47.654239	71.460814
737.922861	58.115365	71.465818
736.806300	45.970910	71.470823
736.079880	54.920867	71.475828
735.956588	46.040263	71.480833
735.969803	57.118043	71.485838
735.326656	51.437871	71.490842
734.531567	50.430781	71.495847
733.545206	64.742809	71.500852
732.714330	62.207031	71.505857
731.855762	53.927632	71.510862
730.832565	65.216181	71.515866
730.791762	45.988600	71.520871
730.394586	63.592548	71.525876
730.013454	48.216486	71.530881
728.934234	48.989300	71.535886
728.059863	62.211160	71.540890
727.703048	44.077852	71.545895
727.224195	57.812319	71.550900
726.043229	57.260917	71.555905
725.508960	56.451997	71.560910
724.798703	58.970107	71.565914
724.536770	52.606334	71.570919
723.760551	58.418185	71.575924
723.141651	46.446806	71.580929
722.895642	45.700796	71.585934
721.178884	54.045204	71.590938
720.724586	49.195988	71.595943
719.878986	61.653171	71.600948
719.286804	61.268215	71.605953
719.255519	57.365624	71.610958
718.202599	58.689346	71.615962
717.349951	60.164105	71.620967
716.921782	55.395883	71.625972
716.432894	60.846590	71.630977
716.184370	55.254972	71.635982
715.193514	62.944475	71.640986
714.234280	54.947619	71.645991
713.812992	56.495617	71.650996
712.756201	61.270353	71.656001
712.040751	58.744588	71.661006
711.354843	65.363661	71.666010
710.888227	54.446674	71.671015
710.564876	64.360636	71.676020
709.993825	60.518767	71.681025
708.931921	55.116599	71.686030
707.957330	61.783219	71.691034
707.705997	64.807000	71.696039
707.539936	61.916204	71.701044
706.354248	64.439065	71.706049
705.517852	57.507603	71.711054
705.004426	61.788959	71.716058
704.742422	56.830274	71.721063
703.685951	58.126182	71.726068
702.682825	64.718501	71.731073
702.571820	58.332272	71.736078
701.677159	65.997001	71.741082
701.517915	55.266036	71.746087
700.361349	61.442816	71.751092
699.902707	58.324222	71.756097
699.540144	64.500719	71.761102
698.238585	60.567025	71.766106
697.396038	58.693866	71.771111
696.605611	59.009118	71.776116
696.332457	61.057080	71.781121
696.098543	58.782645	71.786126
695.513269	69.149908	71.791130
694.367609	53.302664	71.796135
693.774447	63.242246	71.801140
692.817135	56.278005	71.806145
692.853640	50.022833	71.811150
692.038676	62.158174	71.816154
691.163391	61.010903	71.821159
690.535990	59.046715	71.826164
690.017276	57.798506	71.831169
689.345444	55.024527	71.836174
688.195063	68.090081	71.841178
687.672066	62.813412	71.846183
687.447351	62.729492	71.851188
686.813920	59.397460	71.856193
686.063533	54.265818	71.861198
685.264837	60.393497	71.866202
684.775571	59.774539	71.871207
683.979683	61.039995	71.876212
683.109892	64.034535	71.881217
682.364343	56.558755	71.886222
681.764004	58.868559	71.891226
681.443975	58.894436	71.896231
680.923768	61.199364	71.901236
679.766219	56.119950	71.906241
679.183849	56.616540	71.911246
678.883404	66.000150	71.916250
678.198295	54.935041	71.921255
677.182196	61.024805	71.926260
676.347354	62.537743	71.931265
676.157481	58.001240	71.936270
675.607920	63.314958	71.941274
674.486752	62.019193	71.946279
673.652647	69.874562	71.951284
673.189345	68.377832	71.956289
672.792105	57.214839	71.961294
672.177742	61.636855	71.966298
671.391425	54.705317	71.971303
670.406339	59.711501	71.976308
670.265451	62.102679	71.981313
670.184425	58.023508	71.986318
668.906350	62.902889	71.991322
668.122214	58.888385	71.996327
667.617113	60.676820	72.001332
666.397550	67.358815	72.006337
665.799001	57.771730	72.011342
664.975526	68.798257	72.016346
664.506644	62.795457	72.021351
664.300694	66.540571	72.026356
663.801863	58.230715	72.031361
662.955535	57.454161	72.036366
661.687349	66.029948	72.041370
661.677391	71.328697	72.046375
661.094663	63.193051	72.051380
660.264154	63.863206	72.056385
659.462488	61.713890	72.061390
658.509621	68.195718	72.066394
658.136622	64.339666	72.071399
657.810633	64.809622	72.076404
656.438075	55.721130	72.081409
655.870529	61.154410	72.086414
655.148757	65.561998	72.091418
655.154104	60.677435	72.096423
654.762771	60.462358	72.101428
653.856888	70.737186	72.106433
653.314519	62.809582	72.111438
651.852262	66.464620	72.116442
651.111231	53.020908	72.121447
650.562303	58.765038	72.126452
649.698265	69.462135	72.131457
649.734237	59.045441	72.136462
649.045312	65.751740	72.141466
649.092591	54.303492	72.146471
647.887236	63.856455	72.151476
646.758967	63.755594	72.156481
646.366042	61.654724	72.161486
645.177558	69.211724	72.166490
644.623319	56.411625	72.171495
644.263365	62.570363	72.176500
643.867465	61.272642	72.181505
643.463532	60.381479	72.186510
642.127356	62.642907	72.191514
641.453074	49.696353	72.196519
640.961599	58.851763	72.201524
640.657998	65.092992	72.206529
639.949530	61.228873	72.211534
638.663051	58.831926	72.216538
638.104294	49.821994	72.221543
637.926172	60.379879	72.226548
637.197262	63.361456	72.231553
636.455363	56.927485	72.236558
635.495961	62.407411	72.241562
635.008863	59.389558	72.246567
635.061893	61.513307	72.251572
633.720183	65.472433	72.256577
633.541963	61.326741	72.261582
632.238638	59.779310	72.266586
631.417191	48.221849	72.271591
630.775542	50.304853	72.276596
630.056008	58.950959	72.281601
630.050415	55.162554	72.286606
629.627807	62.816771	72.291610
628.586533	63.632470	72.296615
627.876270	59.486365	72.301620
627.202546	55.088436	72.306625
626.780790	61.465178	72.311630
625.529402	58.714140	72.316634
625.073716	50.260233	72.321639
624.560221	55.719601	72.326644
623.860692	49.581665	72.331649
622.864636	47.580020	72.336654
622.194097	61.300871	72.341658
621.864717	58.371441	72.346663
621.397924	56.857933	72.351668
620.495687	60.702911	72.356673
619.693659	55.120622	72.361678
619.042396	65.660830	72.366682
618.520139	56.570970	72.371687
618.537243	61.111614	72.376692
616.850001	66.945599	72.381697
616.211099	59.397662	72.386702
615.606873	64.939296	72.391706
615.354624	54.130120	72.396711
615.014984	56.865195	72.401716
614.303132	53.996688	72.406721
613.593650	50.019201	72.411726
612.960472	66.012814	72.416730
611.771209	56.616033	72.421735
610.978309	58.328893	72.426740
610.154583	61.563701	72.431745
610.302240	57.112217	72.436750
609.572805	61.730771	72.441754
608.656881	57.333578	72.446759
607.796421	51.864681	72.451764
607.198538	58.993302	72.456769
607.070923	59.324433	72.461774
605.999258	62.494656	72.466778
604.898999	48.333899	72.471783
604.639250	58.204612	72.476788
604.044547	56.203700	72.481793
603.647180	52.971289	72.486798
602.474506	63.752247	72.491802
601.979113	59.863663	72.496807
601.497622	51.628339	72.501812
600.761718	53.737402	72.506817
600.040326	52.436341	72.511822
599.298773	55.069855	72.516826
598.664473	53.054752	72.521831
598.189264	52.033025	72.526836
597.156093	56.408223	72.531841
596.777626	50.569241	72.536846
595.995496	62.093818	72.541850
595.671762	56.277655	72.546855
595.280896	56.849416	72.551860
594.018182	59.316788	72.556865
593.129539	52.740628	72.561870
592.954985	64.168427	72.566874
592.100938	57.178322	72.571879
591.277895	61.406512	72.576884
590.583916	61.974517	72.581889
590.355281	53.836113	72.586894
589.661341	62.399305	72.591898
588.828354	53.242257	72.596903
588.072265	56.947269	72.601908
587.565963	54.812431	72.606913
587.109109	52.652371	72.611918
586.486879	62.145585	72.616922
585.669980	60.829780	72.621927
585.521395	53.350411	72.626932
584.299803	55.543153	72.631937
583.218929	48.176024	72.636942
582.576824	53.767848	72.641946
582.248273	52.822110	72.646951
581.850151	54.544634	72.651956
580.272015	59.768321	72.656961
579.719153	45.285418	72.661966
579.311057	55.321686	72.666970
578.821419	58.933795	72.671975
579.118974	53.223673	72.676980
577.898361	52.162993	72.681985
577.306098	53.449662	72.686990
576.263106	56.851871	72.691994
575.175544	56.003388	72.696999
574.718252	51.476382	72.702004
573.898497	58.925782	72.707009
573.996706	66.210034	72.712014
573.349030	56.170336	72.717018
572.164546	66.049589	72.722023
571.908806	53.227200	72.727028
571.168657	62.009069	72.732033
570.150796	57.112464	72.737038
569.047205	60.199476	72.742042
568.375112	67.387239	72.747047
567.951954	53.260565	72.752052
567.520385	63.019879	72.757057
567.275222	59.559800	72.762062
567.237406	57.564804	72.767066
566.074115	57.693488	72.772071
565.116246	56.024829	72.777076
564.625169	60.036140	72.782081
563.854918	54.458272	72.787086
563.045906	61.819232	72.792090
562.360516	49.590421	72.797095
561.830310	53.494423	72.802100
560.363491	59.350096	72.807105
559.889973	54.729483	72.812110
559.388970	59.576588	72.817114
558.863980	61.164784	72.822119
558.719185	57.270822	72.827124
558.176321	62.427373	72.832129
557.335126	50.529314	72.837134
556.474643	64.770868	72.842138
555.999975	59.437652	72.847143
555.701823	47.803172	72.852148
554.218007	59.091028	72.857153
553.739791	51.719370	72.862158
553.421184	60.566552	72.867162
552.363719	59.563472	72.872167
551.393380	50.325821	72.877172
550.700068	50.808575	72.882177
550.393956	50.635132	72.887182
549.746867	57.202319	72.892186
549.508926	45.943028	72.897191
548.795229	46.388029	72.902196
547.901866	54.836336	72.907201
547.213702	53.115258	72.912206
546.904603	54.383632	72.917210
545.876838	57.960047	72.922215
545.151845	51.416186	72.927220
544.671446	53.590216	72.932225
544.304588	47.709973	72.937230
542.953478	49.311507	72.942234
542.360862	50.125152	72.947239
541.981979	45.767015	72.952244
541.473831	63.394942	72.957249
540.618105	48.302708	72.962254
540.116085	58.508486	72.967258
539.247501	66.623270	72.972263
539.498815	54.122235	72.977268
537.679635	65.193870	72.982273
537.257059	54.664160	72.987278
536.478118	53.824875	72.992282
536.087489	53.675937	72.997287
535.381772	51.416762	73.002292
534.475722	55.707076	73.007297
533.952121	52.860644	73.012302
533.597222	47.465778	73.017306
532.526742	45.999579	73.022311
531.819082	43.617713	73.027316
531.025838	54.596863	73.032321
530.767213	46.885876	73.037326
530.205817	52.447505	73.042330
529.390898	58.541538	73.047335
528.922926	47.538096	73.052340
527.953678	53.606251	73.057345
527.728898	49.687190	73.062350
526.533219	52.377303	73.067354
525.539776	49.347106	73.072359
525.364100	49.608627	73.077364
524.934112	55.936225	73.082369
524.437462	40.149710	73.087374
523.019985	58.466553	73.092378
522.565041	58.072396	73.097383
522.309179	54.861611	73.102388
521.655637	54.084354	73.107393
520.935070	52.166595	73.112398
519.855419	54.227943	73.117402
519.159181	53.200445	73.122407
518.905036	51.727197	73.127412
518.328846	58.125398	73.132417
517.293526	51.821800	73.137422
516.977549	59.283993	73.142426
516.023109	51.704365	73.147431
516.129147	52.009313	73.152436
514.823244	56.063716	73.157441
514.097187	52.620337	73.162446
513.399963	53.132110	73.167450
512.614099	51.852387	73.172455
512.733854	51.786141	73.177460
511.211756	53.730326	73.182465
510.936394	47.928553	73.187470
510.641775	55.839930	73.192474
509.901342	54.415774	73.197479
509.005541	52.093850	73.202484
508.331426	48.561774	73.207489
507.480006	50.151524	73.212494
506.444031	49.294852	73.217498
505.518824	53.209757	73.222503
505.244569	48.841265	73.227508
504.671120	57.978209	73.232513
504.673924	43.334266	73.237518
504.338672	44.166840	73.242522
503.052966	56.142247	73.247527
502.541634	42.931674	73.252532
501.569478	53.688597	73.257537
500.877635	49.235250	73.262542
500.133893	47.340114	73.267546
499.548524	44.877273	73.272551
499.117004	49.319073	73.277556
498.480687	56.013863	73.282561
497.637858	49.629143	73.287566
497.028228	45.591632	73.292570
496.262055	46.166435	73.297575
496.049754	48.781883	73.302580
494.686309	53.714368	73.307585
494.040390	55.815431	73.312590
493.607072	52.490998	73.317594
493.255078	57.082557	73.322599
492.949664	54.190333	73.327604
491.874738	52.521432	73.332609
491.039201	48.138292	73.337614
490.810561	47.687583	73.342618
489.657031	58.135943	73.347623
488.750762	45.898203	73.352628
488.109574	49.532893	73.357633
487.943987	47.569298	73.362638
487.244769	42.645621	73.367642
486.100873	55.240261	73.372647
485.586394	51.225438	73.377652
484.785654	58.503096	73.382657
484.756777	58.463685	73.387662
484.418328	52.463808	73.392666
483.253708	63.715036	73.397671
482.617046	50.634819	73.402676
481.685991	51.283206	73.407681
480.541220	53.523680	73.412686
479.988028	57.481822	73.417690
479.731696	53.249249	73.422695
479.427473	49.836442	73.427700
479.091119	53.050402	73.432705
478.084340	48.486393	73.437710
477.279625	48.247324	73.442714
476.254416	59.257140	73.447719
476.135820	62.188823	73.452724
475.085489	54.378486	73.457729
474.438593	54.388662	73.462734
473.850647	52.287360	73.467738
473.421317	57.862650	73.472743
472.682795	48.903494	73.477748
471.626844	63.253479	73.482753
471.124565	50.114009	73.487758
470.928541	51.007982	73.492762
469.890673	60.244163	73.497767
469.168992	53.007515	73.502772
468.392919	59.544808	73.507777
467.666008	58.389747	73.512782
467.619954	62.118851	73.517786
466.766811	61.756614	73.522791
465.841874	53.300249	73.527796
465.104865	61.282120	73.532801
464.561395	53.695379	73.537806
464.330704	48.380084	73.542810
463.047351	56.122578	73.547815
462.568314	46.156982	73.552820
462.111246	64.130010	73.557825
461.654916	49.447263	73.562830
460.550277	57.304785	73.567834
459.563926	62.811140	73.572839
459.232413	51.962592	73.577844
458.855331	56.359455	73.582849
458.370833	55.927442	73.587854
457.597618	58.226994	73.592858
456.650430	53.897926	73.597863
456.162794	45.245732	73.602868
455.495820	57.881084	73.607873
454.284792	55.104785	73.612878
453.987335	47.092494	73.617882
453.152845	53.844101	73.622887
453.226055	56.201169	73.627892
452.296111	53.616626	73.632897
451.252070	51.395617	73.637902
450.839954	49.547003	73.642906
450.328496	54.761642	73.647911
449.764675	53.366133	73.652916
448.675227	61.848870	73.657921
448.215037	61.124402	73.662926
447.626122	50.151294	73.667930
446.360474	57.894128	73.672935
445.843660	47.751629	73.677940
445.567344	59.056859	73.682945
445.062377	63.740610	73.687950
444.775001	50.379246	73.692954
443.513493	61.163375	73.697959
442.984728	49.359089	73.702964
442.160487	57.996685	73.707969
441.290968	54.246606	73.712974
440.730798	52.323814	73.717978
440.026485	58.580018	73.722983
439.511886	45.119250	73.727988
439.228548	62.135763	73.732993
438.353004	57.032038	73.737998
437.460002	56.748703	73.743002
436.714951	62.308078	73.748007
436.412763	49.157236	73.753012
435.167350	61.020596	73.758017
434.171727	58.594759	73.763022
434.388300	49.606423	73.768026
434.010082	58.300680	73.773031
433.689052	50.214878	73.778036
432.387826	54.558735	73.783041
431.470138	51.551199	73.788046
431.117090	49.943912	73.793050
430.053745	61.142747	73.798055
429.168665	50.794007	73.803060
428.579461	63.260855	73.808065
428.022724	56.833725	73.813070
427.771450	57.452653	73.818074
427.251101	57.103630	73.823079
426.923334	52.448785	73.828084
426.105033	55.323235	73.833089
425.138100	51.569764	73.838094
424.140557	56.491284	73.843098
423.251142	64.516376	73.848103
422.717608	48.313144	73.853108
422.395338	53.891878	73.858113
421.940263	57.916397	73.863118
421.425821	51.122984	73.868122
420.369706	58.901826	73.873127
420.016701	48.618112	73.878132
419.205299	49.140221	73.883137
417.887032	52.931712	73.888142
417.293127	46.630361	73.893146
416.725742	48.370419	73.898151
416.617524	44.929541	73.903156
416.070722	51.341996	73.908161
415.278574	50.545856	73.913166
414.635655	48.670951	73.918170
413.542024	54.025680	73.923175
413.581419	48.858164	73.928180
412.423079	48.415272	73.933185
411.560657	45.947720	73.938190
410.978081	47.250229	73.943194
410.495512	55.281447	73.948199
410.415720	45.867256	73.953204
409.132616	45.963068	73.958209
408.392657	44.042128	73.963214
408.197628	42.329238	73.968218
406.817104	50.979796	73.973223
406.349829	50.696436	73.978228
405.896689	49.396841	73.983233
405.153360	47.662519	73.988238
405.049064	50.655001	73.993242
403.917508	53.011675	73.998247
403.595317	52.356687	74.003252
402.708234	57.049299	74.008257
401.522653	54.753097	74.013262
401.132155	45.104572	74.018266
400.101170	57.077273	74.023271
399.552925	44.760445	74.028276
399.449796	51.554782	74.033281
398.659496	48.722502	74.038286
397.872119	56.303980	74.043290
397.156593	63.814087	74.048295
396.988445	45.502591	74.053300
396.201503	66.656874	74.058305
394.997405	52.944875	74.063310
394.478672	49.101065	74.068314
393.921425	56.021394	74.073319
393.524678	49.693359	74.078324
392.479206	55.888825	74.083329
391.567717	56.258159	74.088334
391.367060	50.130687	74.093338
390.673937	52.797540	74.098343
390.555862	46.398287	74.103348
389.284336	58.904491	74.108353
388.472078	64.091388	74.113358
387.882133	63.729811	74.118362
387.703693	63.504502	74.123367
386.619540	67.187737	74.128372
386.102469	65.199740	74.133377
385.051623	62.937266	74.138382
384.968596	54.741001	74.143386
383.922862	64.522515	74.148391
383.364673	46.359917	74.153396
382.719477	57.435352	74.158401
382.295701	61.827051	74.163406
381.563554	47.054251	74.168410
380.356849	61.593866	74.173415
380.167423	53.925493	74.178420
379.958726	54.443023	74.183425
379.016779	57.209460	74.188430
377.885964	51.354813	74.193434
377.182887	60.556590	74.198439
376.868286	48.497420	74.203444
376.305669	51.920917	74.208449
375.550330	55.652674	74.213454
374.721677	42.544760	74.218458
373.955549	57.690669	74.223463
373.950062	48.204715	74.228468
372.667320	51.982681	74.233473
371.821917	50.067519	74.238478
371.526968	54.601111	74.243482
370.766047	56.942884	74.248487
370.674774	46.423505	74.253492
369.532995	54.813680	74.258497
368.835514	53.747000	74.263502
368.266281	55.504711	74.268506
367.500236	59.457374	74.273511
366.582207	52.687299	74.278516
365.816300	52.118806	74.283521
365.418467	55.596466	74.288526
365.228551	54.882555	74.293530
364.827097	53.961084	74.298535
363.365952	44.536826	74.303540
362.736112	53.498270	74.308545
362.033681	63.073687	74.313550
362.066041	55.568664	74.318554
360.828419	61.597649	74.323559
360.114094	56.458798	74.328564
359.625814	50.550638	74.333569
359.167650	57.101942	74.338574
358.731714	47.277742	74.343578
357.770562	49.086880	74.348583
357.282396	52.905368	74.353588
356.305184	50.022469	74.358593
355.302069	54.883399	74.363598
355.233956	49.453899	74.368602
354.531896	61.615465	74.373607
353.832580	52.941842	74.378612
352.775480	51.265433	74.383617
351.675326	55.515780	74.388622
351.909793	55.677248	74.393626
351.211498	55.981078	74.398631
350.359901	48.823532	74.403636
349.551970	52.133169	74.408641
348.757932	52.316641	74.413646
348.375642	58.270803	74.418650
347.962214	62.591471	74.423655
347.173373	49.972383	74.428660
346.487113	51.233085	74.433665
345.455675	63.279995	74.438670
345.246760	58.648798	74.443674
344.364919	59.682054	74.448679
343.597411	56.169644	74.453684
342.976469	55.494473	74.458689
342.368196	55.399180	74.463694
342.289877	47.527026	74.468698
341.195326	56.392234	74.473703
340.261599	55.762188	74.478708
339.877964	55.139080	74.483713
339.257587	54.869097	74.488718
338.503159	56.295209	74.493722
337.281461	58.294119	74.498727
336.972793	50.982229	74.503732
336.740255	47.564327	74.508737
336.111163	54.961317	74.513742
335.547669	50.083866	74.518746
334.767313	62.407726	74.523751
334.213931	57.662701	74.528756
333.344564	55.350825	74.533761
332.323073	55.567404	74.538766
331.591472	47.178061	74.543770
331.117466	55.015533	74.548775
330.664218	57.350854	74.553780
329.674797	50.398211	74.558785
328.980660	43.341734	74.563790
329.115692	51.391211	74.568794
328.183837	57.317854	74.573799
326.868077	50.617503	74.578804
326.258859	49.593537	74.583809
325.796254	55.010144	74.588814
325.581642	47.937156	74.593818
324.975304	61.091143	74.598823
323.762094	51.031299	74.603828
323.246853	53.431695	74.608833
322.752454	58.851794	74.613838
322.473661	51.423182	74.618842
321.202320	57.813949	74.623847
320.321076	61.270900	74.628852
320.168347	50.639896	74.633857
319.485923	62.974958	74.638862
318.747954	49.515141	74.643866
317.683436	60.110223	74.648871
317.356813	48.568650	74.653876
317.264252	53.032139	74.658881
315.960749	58.808292	74.663886
315.162678	52.429128	74.668890
314.639118	63.778501	74.673895
314.150826	57.521845	74.678900
313.369746	53.830260	74.683905
312.372288	59.248547	74.688910
312.189170	53.906767	74.693914
311.936404	51.553383	74.698919
310.625144	56.805649	74.703924
310.150725	54.260515	74.708929
309.097335	65.393148	74.713934
309.072711	58.349798	74.718938
308.085103	63.716056	74.723943
307.028592	56.130717	74.728948
306.448809	57.587347	74.733953
305.851478	57.222236	74.738958
305.444789	58.323267	74.743962
304.974044	60.120485	74.748967
304.506030	56.547732	74.753972
303.539008	59.187306	74.758977
302.533335	61.101335	74.763982
302.468031	58.872610	74.768986
301.561068	63.185224	74.773991
300.702419	62.246756	74.778996
300.053640	60.811210	74.784001
299.506844	66.687523	74.789006
299.022126	63.746639	74.794010
297.947473	61.519539	74.799015
297.218330	54.632652	74.804020
296.878186	56.240318	74.809025
296.157774	60.838586	74.814030
296.153490	61.276229	74.819034
294.703291	62.335449	74.824039
294.010606	59.528643	74.829044
293.736837	53.225181	74.834049
292.951402	60.017898	74.839054
292.220578	54.482733	74.844058
291.440264	63.411410	74.849063
291.043754	62.743054	74.854068
290.404923	56.187125	74.859073
289.427977	64.133167	74.864078
288.927661	60.176058	74.869082
288.508338	54.556544	74.874087
287.588346	61.459023	74.879092
286.973859	55.097912	74.884097
285.893310	63.186626	74.889102
285.390355	60.776932	74.894106
284.939723	63.086613	74.899111
284.658141	64.945143	74.904116
283.934856	56.701144	74.909121
283.056264	56.505455	74.914126
282.366688	56.489370	74.919130
281.796995	56.405288	74.924135
281.096523	58.086167	74.929140
280.236398	52.171072	74.934145
279.385442	57.075583	74.939150
279.267594	50.485494	74.944154
278.091024	50.996476	74.949159
277.185956	57.625341	74.954164
277.153189	51.816474	74.959169
276.375254	62.211343	74.964174
276.527749	54.836986	74.969178
275.223239	56.557390	74.974183
274.523673	56.916638	74.979188
274.067910	53.468096	74.984193
272.539072	54.235513	74.989198
272.107312	56.422337	74.994202
271.636296	56.336719	74.999207
271.325423	63.094790	75.004212
271.034924	56.275179	75.009217
269.805387	58.105059	75.014222
269.346943	56.273325	75.019226
268.589146	60.924869	75.024231
267.967436	53.290736	75.029236
267.121415	48.363728	75.034241
266.273925	58.022208	75.039246
266.013713	51.025884	75.044250
265.467650	65.878114	75.049255
264.250453	61.437631	75.054260
263.760683	57.699621	75.059265
263.269446	62.360711	75.064270
262.852829	51.527358	75.069274
261.598736	59.803018	75.074279
260.916585	61.052050	75.079284
260.580732	58.767111	75.084289
260.081174	59.999649	75.089294
259.757814	52.373149	75.094298
258.611615	60.227909	75.099303
258.045883	58.000119	75.104308
257.532805	58.736496	75.109313
256.010044	64.162857	75.114318
255.749837	57.190186	75.119322
255.029521	47.154309	75.124327
254.649724	49.728666	75.129332
254.326882	48.747373	75.134337
253.026448	65.610638	75.139342
252.457250	57.554974	75.144346
251.870483	58.834533	75.149351
251.366039	62.578365	75.154356
250.638711	54.558953	75.159361
249.684948	61.154590	75.164366
249.241433	59.035050	75.169370
248.894071	56.944337	75.174375
248.518969	61.074402	75.179380
247.271131	47.724292	75.184385
246.475679	62.691973	75.189390
246.328157	55.420641	75.194394
245.447041	64.359092	75.199399
244.081032	64.633788	75.204404
243.973473	56.086635	75.209409
243.358781	58.983873	75.214414
242.926515	54.670575	75.219418
242.377950	57.401152	75.224423
241.092465	61.665323	75.229428
240.693157	54.347403	75.234433
240.460587	54.936559	75.239438
239.460222	53.224346	75.244442
238.383521	54.820139	75.249447
237.624141	62.132266	75.254452
237.243078	59.289989	75.259457
237.113010	61.395603	75.264462
236.388046	53.617094	75.269466
235.605120	58.345191	75.274471
234.767858	65.150919	75.279476
234.300620	58.302722	75.284481
233.126739	57.804047	75.289486
232.568555	52.944700	75.294490
231.826680	53.539364	75.299495
231.615486	57.569181	75.304500
231.372722	55.108556	75.309505
230.327018	62.928383	75.314510
229.527679	60.476070	75.319514
229.077090	56.829594	75.324519
228.230627	56.647726	75.329524
227.172619	52.279656	75.334529
226.569755	58.360460	75.339534
226.374671	51.576110	75.344538
225.765043	58.034884	75.349543
224.740902	54.238581	75.354548
224.121261	51.185187	75.359553
223.270515	55.070968	75.364558
223.249946	57.963370	75.369562
222.589397	55.171965	75.374567
221.119913	63.191826	75.379572
221.030671	52.847183	75.384577
220.646770	64.253146	75.389582
219.803961	62.318701	75.394586
218.773716	57.961977	75.399591
218.039281	59.744482	75.404596
217.870224	64.161822	75.409601
217.148070	65.863523	75.414606
216.524165	59.448741	75.419610
215.555096	57.499736	75.424615
215.029577	58.813693	75.429620
214.722236	65.355162	75.434625
213.243236	57.058218	75.439630
212.733245	66.956219	75.444634
212.347164	61.948009	75.449639
211.823360	66.853997	75.454644
211.034239	57.729543	75.459649
210.347923	60.739134	75.464654
209.671366	60.077596	75.469658
209.392465	51.937816	75.474663
207.937347	61.863506	75.479668
207.604000	58.452231	75.484673
206.877444	60.733377	75.489678
206.229535	58.663783	75.494682
206.096322	53.235213	75.499687
204.910723	58.517956	75.504692
204.431000	55.932690	75.509697
203.680040	60.652546	75.514702
203.581675	61.680778	75.519706
202.313701	53.550469	75.524711
201.411538	52.842905	75.529716
201.210688	54.850995	75.534721
200.743179	58.469097	75.539726
199.738109	60.629074	75.544730
199.273178	52.941582	75.549735
198.395262	57.495601	75.554740
198.287265	53.373460	75.559745
197.036186	64.159179	75.564750
196.075651	59.368726	75.569754
195.705412	51.415401	75.574759
195.268460	56.903629	75.579764
194.915834	51.891669	75.584769
193.367073	50.875622	75.589774
192.701445	57.237675	75.594778
192.435541	55.381564	75.599783
191.996370	55.607852	75.604788
191.967112	49.453080	75.609793
190.693394	60.068944	75.614798
189.854572	56.080680	75.619802
189.366939	53.219136	75.624807
188.011593	62.884500	75.629812
187.474547	58.375032	75.634817
186.682510	55.120479	75.639822
186.644052	51.799382	75.644826
186.175947	53.927359	75.649831
185.391616	55.053932	75.654836
184.746170	49.410576	75.659841
183.832823	62.123099	75.664846
183.511944	53.490123	75.669850
183.106645	57.979825	75.674855
181.543412	60.583625	75.679860
181.168945	54.160622	75.684865
180.510595	60.693406	75.689870
180.233965	54.144416	75.694874
179.115622	54.138382	75.699879
178.133819	59.551066	75.704884
178.152563	51.021633	75.709889
177.626936	57.657832	75.714894
177.107791	55.709640	75.719898
176.417024	53.381961	75.724903
175.547880	60.915031	75.729908
174.671700	51.965327	75.734913
173.656294	57.739762	75.739918
173.024423	62.467445	75.744922
172.890684	52.949921	75.749927
171.943760	56.184004	75.754932
171.779262	50.079184	75.759937
170.675661	62.397848	75.764942
170.145877	58.098538	75.769946
169.485942	49.836601	75.774951
168.134980	59.332539	75.779956
167.910319	49.362738	75.784961
167.305922	55.699262	75.789966
166.711888	63.614244	75.794970
166.506095	53.444313	75.799975
165.267965	66.035169	75.804980
164.908090	67.191836	75.809985
163.752021	66.535812	75.814990
163.658861	65.893220	75.819994
163.508520	58.098800	75.824999
162.353560	54.547313	75.830004
161.540445	66.176265	75.835009
160.850264	64.316850	75.840014
159.698238	55.120980	75.845018
159.228012	54.434439	75.850023
158.364714	60.681365	75.855028
158.590211	49.863921	75.860033
157.889716	62.421082	75.865038
156.720066	55.285949	75.870042
156.405451	53.303570	75.875047
155.537379	58.173000	75.880052
154.985778	58.637996	75.885057
154.380853	55.989128	75.890062
153.325999	55.129312	75.895066
153.012411	52.836110	75.900071
152.175421	60.004513	75.905076
151.599097	59.696015	75.910081
150.464334	55.314990	75.915086
150.008048	59.469051	75.920090
149.947260	51.745510	75.925095
148.982047	64.426891	75.930100
148.374925	55.276596	75.935105
147.098939	56.375929	75.940110
147.116112	53.925902	75.945114
146.584688	54.720420	75.950119
145.466031	60.549178	75.955124
145.170146	59.841145	75.960129
144.510764	58.331639	75.965134
143.775294	59.828902	75.970138
143.001570	61.299150	75.975143
142.079806	53.876913	75.980148
141.634036	55.712754	75.985153
141.140233	56.296269	75.990158
140.140877	54.175508	75.995162
139.416114	55.525984	76.000167
139.013996	51.695181	76.005172
138.872261	48.177669	76.010177
137.934075	47.173099	76.015182
136.731567	48.137716	76.020186
136.510002	50.831934	76.025191
135.712598	51.230478	76.030196
135.212107	49.643598	76.035201
134.169528	61.258682	76.040206
133.267304	44.062539	76.045210
133.084610	52.028616	76.050215
132.249824	56.044343	76.055220
132.265659	54.384584	76.060225
131.186913	57.909362	76.065230
130.682035	49.422438	76.070234
129.905018	49.827194	76.075239
128.462903	53.685888	76.080244
128.210053	63.088724	76.085249
127.586610	54.136582	76.090254
126.987229	56.846901	76.095258
127.035600	55.238722	76.100263
125.706218	62.291694	76.105268
124.963943	59.450273	76.110273
124.421826	53.137598	76.115278
123.602085	57.879481	76.120282
123.652707	52.859996	76.125287
122.457531	62.648079	76.130292
121.738511	46.805710	76.135297
120.967725	53.887867	76.140302
120.848977	53.815484	76.145306
120.014429	57.585174	76.150311
118.913946	63.352698	76.155316
118.774144	50.770554	76.160321
118.065342	56.486649	76.165326
117.072553	55.779376	76.170330
116.544889	53.525052	76.175335
115.594986	63.106864	76.180340
115.385602	57.267828	76.185345
114.922739	51.828764	76.190350
113.969219	61.974125	76.195354
113.300183	48.186442	76.200359
112.675801	54.332196	76.205364
112.103506	54.344763	76.210369
111.177461	63.601074	76.215374
110.628468	50.521220	76.220378
110.218528	50.039540	76.225383
109.009038	63.191972	76.230388
108.137620	58.791046	76.235393
107.655125	58.466017	76.240398
106.998392	55.689808	76.245402
106.914594	60.659677	76.250407
106.490403	60.815782	76.255412
105.745318	61.160260	76.260417
105.013987	55.473855	76.265422
104.269032	63.034448	76.270426
103.106303	55.992857	76.275431
101.932413	58.476264	76.280436
101.694388	52.892534	76.285441
101.245994	57.674547	76.290446
101.128413	58.328954	76.295450
100.646902	47.914432	76.300455
99.335389	59.126140	76.305460
98.643532	54.124147	76.310465
98.284895	56.141640	76.315470
96.952944	60.115247	76.320474
96.499004	44.954435	76.325479
95.858009	44.320375	76.330484
95.561498	50.894809	76.335489
95.239454	55.451666	76.340494
94.150637	61.119567	76.345498
93.659104	47.428162	76.350503
93.158624	62.096509	76.355508
91.983576	49.196938	76.360513
91.060252	48.372942	76.365518
90.509445	51.736262	76.370522
90.324528	50.822881	76.375527
89.553309	53.898081	76.380532
88.819934	44.044130	76.385537
88.136675	54.464932	76.390542
87.406962	56.339761	76.395546
87.184109	47.542943	76.400551
86.109084	59.546414	76.405556
85.719646	55.246821	76.410561
84.839481	48.297372	76.415566
84.468101	53.644266	76.420570
83.252963	49.804376	76.425575
82.360098	47.319726	76.430580
82.065252	48.950155	76.435585
81.930893	55.317380	76.440590
81.060377	63.383706	76.445594
80.272079	45.551254	76.450599
79.515964	56.661768	76.455604
78.984100	49.896465	76.460609
78.696381	51.837994	76.465614
77.640658	54.430296	76.470618
76.897705	51.787697	76.475623
76.468012	53.024896	76.480628
75.399164	60.731771	76.485633
74.557014	57.948875	76.490638
74.109218	65.660775	76.495642
73.702522	54.266075	76.500647
72.820879	59.541394	76.505652
72.683725	59.057212	76.510657
71.537966	61.250717	76.515662
70.561214	65.131414	76.520666
70.742501	54.489755	76.525671
69.846567	59.248538	76.530676
69.099248	46.022141	76.535681
68.501188	55.757577	76.540686
67.650989	64.003592	76.545690
67.051048	49.468469	76.550695
65.863922	55.219868	76.555700
65.386691	57.015008	76.560705
65.392029	58.917681	76.565710
64.723724	57.959978	76.570714
63.919101	56.377468	76.575719
62.528493	54.790655	76.580724
62.255455	56.739306	76.585729
61.999798	52.084066	76.590734
61.067330	56.795062	76.595738
60.425801	57.227115	76.600743
59.274504	59.337931	76.605748
58.857529	56.189179	76.610753
58.566198	52.570956	76.615758
58.066172	63.047698	76.620762
57.222599	50.254548	76.625767
56.248647	57.449552	76.630772
55.972275	55.837980	76.635777
55.910071	58.962524	76.640782
54.650920	56.850122	76.645786
54.144739	56.945197	76.650791
52.819358	60.260190	76.655796
51.976764	54.667246	76.660801
51.626860	63.369627	76.665806
51.024436	60.106954	76.670810
50.683910	58.303765	76.675815
50.081909	59.338219	76.680820
49.308758	47.196162	76.685825
48.518375	50.072580	76.690830
47.645965	61.337272	76.695834
47.485106	57.352886	76.700839
46.409086	60.246483	76.705844
45.869042	63.608098	76.710849
45.538568	53.992666	76.715854
44.825152	62.352485	76.720858
43.814471	51.355337	76.725863
42.842577	54.345866	76.730868
42.254678	53.794813	76.735873
41.709315	52.912123	76.740878
41.428113	56.197756	76.745882
41.004343	53.565755	76.750887
39.810887	56.927518	76.755892
39.786046	58.935929	76.760897
39.192878	56.524915	76.765902
37.700787	61.139107	76.770906
37.162351	51.022265	76.775911
36.759637	53.496227	76.780916
35.951329	50.354712	76.785921
34.962558	55.579321	76.790926
33.937706	60.000712	76.795930
34.066468	49.965101	76.800935
33.268153	56.367274	76.805940
32.781633	57.616700	76.810945
31.946329	55.964979	76.815950
30.738715	55.009736	76.820954
30.431484	55.852094	76.825959
30.107781	55.761948	76.830964
29.945817	53.484002	76.835969
29.186362	55.289474	76.840974
28.098814	59.845448	76.845978
27.980316	57.054366	76.850983
26.536315	64.196632	76.855988
25.341620	56.070511	76.860993
25.232525	53.829863	76.865998
24.888889	55.606853	76.871002
24.269006	59.254019	76.876007
23.659614	56.873982	76.881012
22.854494	56.420663	76.886017
22.309061	54.531894	76.891022
21.341879	58.016843	76.896026
20.484676	50.204320	76.901031
19.771096	52.849299	76.906036
19.442280	56.847426	76.911041
19.445971	53.846043	76.916046
18.570153	54.533100	76.921050
17.716196	50.459011	76.926055
16.713777	55.610110	76.931060
16.101387	59.057387	76.936065
15.165910	54.018593	76.941070
14.436108	54.165118	76.946074
14.164655	52.628460	76.951079
13.668094	51.939842	76.956084
13.230647	56.603425	76.961089
12.012192	60.005459	76.966094
10.946101	53.218164	76.971098
10.742928	46.849879	76.976103
10.534493	54.618212	76.981108
10.025746	52.692055	76.986113
9.180438	50.387505	76.991118
8.031810	56.519140	76.996122
7.725567	44.849822	77.001127
6.737386	50.727203	77.006132
5.715015	59.114238	77.011137
5.738199	47.532714	77.016142
5.066724	61.690603	77.021147
4.913753	56.929104	77.026151
3.507045	56.015098	77.031156
2.862695	56.207919	77.036161