Fri Mar 05 19:23:09 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.377279	96.660420	0.000000
-0.681594	88.710846	0.005005
-1.769363	72.998316	0.010010
-3.544826	33.928883	0.015014
-7.282519	7.553159	0.020019
-11.998167	4.511431	0.025024
-16.673368	3.316174	0.030029
-21.536074	14.006324	0.035034
-25.854809	4.557251	0.040038
-29.656336	6.813360	0.045043
-33.415283	6.353488	0.050048
-36.734590	5.597987	0.055053
-40.678584	14.626173	0.060058
-44.024272	4.809022	0.065062
-47.974015	10.547048	0.070067
-51.766432	4.882313	0.075072
-55.368213	7.581258	0.080077
-59.243028	2.596729	0.085082
-63.214522	1.300338	0.090086
-66.815822	8.666982	0.095091
-70.238316	6.532391	0.100096
-73.983426	7.789246	0.105101
-78.118803	10.229579	0.110106
-81.747409	7.820383	0.115110
-86.054021	6.369337	0.120115
-89.814415	6.810220	0.125120
-92.888488	5.037964	0.130125
-96.776747	10.985452	0.135130
-100.465748	-1.411912	0.140134
-104.497385	10.189734	0.145139
-108.369277	1.707155	0.150144
-112.088051	2.874711	0.155149
-115.773219	7.487267	0.160154
-119.281332	3.931388	0.165158
-123.232387	7.637058	0.170163
-126.977440	4.901161	0.175168
-130.303259	0.291199	0.180173
-134.809911	2.514901	0.185178
-138.280277	0.419587	0.190182
-142.629765	11.272499	0.195187
-146.334560	1.329879	0.200192
-149.797923	2.628624	0.205197
-153.581639	7.876700	0.210202
-157.231876	3.176618	0.215206
-160.869375	-0.965675	0.220211
-165.006441	9.348754	0.225216
-168.218601	0.221687	0.230221
-171.858317	8.513967	0.235226
-175.552196	-4.417075	0.240230
-179.654281	6.536764	0.245235
-183.825613	-4.228621	0.250240
-187.515333	0.438381	0.255245
-191.266675	9.975365	0.260250
-194.647757	-5.733674	0.265254
-198.517583	5.101126	0.270259
-202.221527	8.545137	0.275264
-205.951211	4.360855	0.280269
-210.101620	9.930888	0.285274
-213.497148	2.064741	0.290278
-217.567119	7.989376	0.295283
-220.978180	3.022565	0.300288
-224.545904	1.669886	0.305293
-228.719259	7.189994	0.310298
-232.268155	-0.217985	0.315302
-236.460664	2.689045	0.320307
-240.024782	5.120475	0.325312
-243.474160	0.005274	0.330317
-247.443830	7.967127	0.335322
-250.736836	0.057866	0.340326
-255.016112	12.244893	0.345331
-258.888881	8.050416	0.350336
-262.347766	-0.374819	0.355341
-266.567606	12.157552	0.360346
-270.075667	5.944740	0.365350
-273.446097	11.604844	0.370355
-277.529267	14.473994	0.375360
-281.188996	4.715211	0.380365
-285.184939	2.516349	0.385370
-289.067287	3.100010	0.390374
-292.856713	7.016692	0.395379
-296.451018	7.041879	0.400384
-299.990735	4.473750	0.405389
-304.150930	7.184929	0.410394
-307.639485	7.374600	0.415398
-311.308079	4.932716	0.420403
-315.374545	6.405245	0.425408
-318.785754	6.711894	0.430413
-322.830568	8.939487	0.435418
-326.420233	5.628747	0.440422
-330.120725	9.256902	0.445427
-333.696188	3.179528	0.450432
-337.229243	3.098805	0.455437
-341.686754	-0.683638	0.460442
-345.231228	-4.044138	0.465446
-349.124708	8.701186	0.470451
-353.110870	7.093807	0.475456
-356.412732	5.528569	0.480461
-360.300669	0.535599	0.485466
-363.947680	-5.337914	0.490470
-368.259247	4.752388	0.495475
-372.044508	9.486960	0.500480
-375.119550	1.877391	0.505485
-379.069190	8.831742	0.510490
-382.792053	5.559702	0.515494
-386.547781	1.834027	0.520499
-390.686589	3.319809	0.525504
-394.285387	11.730452	0.530509
-397.847836	10.700462	0.535514
-401.826609	6.278724	0.540518
-405.560052	16.322517	0.545523
-409.230505	10.990549	0.550528
-412.531700	6.858025	0.555533
-417.020768	9.270252	0.560538
-420.811162	0.549692	0.565542
-424.378277	11.366458	0.570547
-428.201929	1.736594	0.575552
-431.735544	3.887469	0.580557
-435.552597	10.393387	0.585562
-439.153318	1.451759	0.590566
-443.157685	10.666820	0.595571
-446.839981	8.892803	0.600576
-450.329118	-1.518986	0.605581
-454.250190	8.576914	0.610586
-458.135756	-2.999990	0.615590
-461.944622	5.780181	0.620595
-465.812132	6.511567	0.625600
-469.592274	0.366170	0.630605
-473.352083	15.182934	0.635610
-476.774443	5.410217	0.640614
-480.469018	12.614151	0.645619
-484.432121	9.125175	0.650624
-487.887724	3.476751	0.655629
-492.173229	13.394374	0.660634
-495.821920	9.468853	0.665638
-499.278480	9.410845	0.670643
-503.597890	11.072321	0.675648
-506.961588	6.970415	0.680653
-511.050162	8.101454	0.685658
-514.428375	4.173764	0.690662
-518.364579	3.246230	0.695667
-522.533151	11.904177	0.700672
-525.725350	0.467376	0.705677
-529.660567	10.840039	0.710682
-533.240374	1.149330	0.715686
-537.027362	5.870237	0.720691
-540.727946	-2.268382	0.725696
-544.290412	-2.162753	0.730701
-548.541623	6.475319	0.735706
-552.403848	0.614403	0.740710
-555.918101	10.419974	0.745715
-560.145717	13.348940	0.750720
-563.386898	3.851766	0.755725
-567.010309	10.060450	0.760730
-570.850094	4.177056	0.765734
-574.887176	7.659077	0.770739
-578.842315	17.306457	0.775744
-582.189116	4.039955	0.780749
-586.250902	9.883462	0.785754
-589.323506	-1.170230	0.790758
-593.352375	6.691238	0.795763
-597.324270	10.658041	0.800768
-601.218323	7.336428	0.805773
-605.240801	15.889174	0.810778
-608.837919	15.929473	0.815782
-612.001251	16.731522	0.820787
-616.009696	8.206970	0.825792
-619.835348	6.413551	0.830797
-623.793145	17.239397	0.835802
-627.431089	7.507663	0.840806
-631.035974	14.107716	0.845811
-635.156660	13.323389	0.850816
-638.729444	7.195602	0.855821
-642.619002	9.982391	0.860826
-646.220391	4.559347	0.865830
-649.940648	8.837687	0.870835
-654.001840	13.293508	0.875840
-657.413885	6.110329	0.880845
-661.034552	4.752575	0.885850
-664.917826	0.254532	0.890854
-668.748285	9.147274	0.895859
-672.707410	10.738872	0.900864
-676.222743	8.679920	0.905869
-680.447221	13.983460	0.910874
-683.991266	2.997346	0.915878
-687.538596	13.081194	0.920883
-691.096499	13.572664	0.925888
-695.024445	4.524465	0.930893
-698.826564	13.521535	0.935898
-702.274009	0.433731	0.940902
-706.365203	1.308483	0.945907
-710.369328	2.910488	0.950912
-714.029203	8.005589	0.955917
-718.078276	10.619297	0.960922
-721.267318	-2.014611	0.965926
-725.149148	6.290344	0.970931
-729.451468	-1.717108	0.975936
-732.814904	-1.067422	0.980941
-736.726168	5.761514	0.985946
-740.172187	-5.505093	0.990950
-744.023402	0.182018	0.995955
-747.415353	6.599975	1.000960
-751.210564	2.546891	1.005965
-755.266384	9.783733	1.010970
-759.147615	5.233483	1.015974
-762.675651	-1.002180	1.020979
-766.852510	8.736117	1.025984
-770.378363	-0.489749	1.030989
-774.139291	9.502202	1.035994
-777.829402	-1.834144	1.040998
-781.481476	2.901847	1.046003
-785.642073	13.433931	1.051008
-789.294992	-1.052747	1.056013
-792.983388	11.408155	1.061018
-796.696247	3.486381	1.066022
-800.364068	7.151026	1.071027
-804.588348	9.693539	1.076032
-807.998202	10.098442	1.081037
-811.705799	2.210545	1.086042
-815.357807	2.168471	1.091046
-818.861228	0.172487	1.096051
-822.987605	7.237793	1.101056
-826.797762	4.682155	1.106061
-830.464344	0.409948	1.111066
-834.320015	5.886607	1.116070
-838.438116	-1.292234	1.121075
-841.871285	3.935549	1.126080
-845.393080	0.241032	1.131085
-849.375865	10.320599	1.136090
-853.001183	0.852148	1.141094
-856.696623	-1.442661	1.146099
-860.753838	19.036078	1.151104
-864.177092	2.789222	1.156109
-868.335116	7.322381	1.161114
-871.973753	7.819144	1.166118
-875.844687	2.777022	1.171123
-879.794882	13.892204	1.176128
-883.082354	-5.225836	1.181133
-886.683840	9.424274	1.186138
-890.804409	3.621006	1.191142
-894.283394	13.017712	1.196147
-897.989612	8.024983	1.201152
-901.701729	2.336202	1.206157
-905.859453	11.920288	1.211162
-909.364494	7.530916	1.216166
-913.569660	12.229385	1.221171
-917.420191	12.452597	1.226176
-920.863258	4.022698	1.231181
-924.854497	10.847376	1.236186
-928.276496	6.305986	1.241190
-932.192421	8.331071	1.246195
-935.979152	8.227149	1.251200
-939.330392	4.658467	1.256205
-943.347021	10.419652	1.261210
-946.904507	9.917974	1.266214
-950.826095	1.794872	1.271219
-954.577840	3.374278	1.276224
-958.471733	-3.512192	1.281229
-962.625586	6.656408	1.286234
-965.955905	-1.852946	1.291238
-969.639829	-0.774787	1.296243
-973.810632	6.245838	1.301248
-977.060506	-0.095471	1.306253
-980.926919	2.595126	1.311258
-984.263428	2.961748	1.316262
-988.272342	-4.511816	1.321267
-992.354090	10.450206	1.326272
-995.928289	1.837974	1.331277
-999.721076	5.188598	1.336282
-1003.706986	0.303852	1.341286
-1007.414860	3.826987	1.346291
-1011.632374	7.617711	1.351296
-1014.853183	-4.600671	1.356301
-1018.681557	3.353997	1.361306
-1022.177949	6.431754	1.366310
-1026.224225	3.534170	1.371315
-1029.973858	11.367458	1.376320
-1033.685522	5.879091	1.381325
-1037.535597	14.535845	1.386330
-1041.365037	4.335540	1.391334
-1044.660548	4.905422	1.396339
-1048.365408	9.325411	1.401344
-1052.331730	3.966114	1.406349
-1056.416375	8.052629	1.411354
-1060.084216	4.599419	1.416358
-1063.708417	4.900209	1.421363
-1067.992567	10.950392	1.426368
-1071.157119	-1.190175	1.431373
-1074.958760	17.726269	1.436378
-1078.954414	9.140581	1.441382
-1082.482509	17.498325	1.446387
-1086.424377	15.822033	1.451392
-1089.943671	1.374420	1.456397
-1094.026983	11.374265	1.461402
-1098.030048	10.031054	1.466406
-1101.336616	13.671487	1.471411
-1104.981795	15.738702	1.476416
-1108.796794	7.507364	1.481421
-1112.517733	-0.019931	1.486426
-1116.340962	4.561021	1.491430
-1120.043100	4.333480	1.496435
-1124.300062	14.835812	1.501440
-1127.819212	4.201249	1.506445
-1131.425598	6.090413	1.511450
-1135.006658	14.991283	1.516454
-1138.769379	-2.634233	1.521459
-1142.755026	9.650801	1.526464
-1146.434495	5.573551	1.531469
-1150.664854	16.212019	1.536474
-1154.260524	-0.822041	1.541478
-1157.360792	-6.895286	1.546483
-1161.396173	-2.704515	1.551488
-1165.057957	-7.096792	1.556493
-1169.381131	4.570513	1.561498
-1173.070238	6.485592	1.566502
-1176.669080	2.550030	1.571507
-1180.330016	4.870613	1.576512
-1184.023356	0.238990	1.581517
-1187.862849	3.382925	1.586522
-1191.637923	6.847714	1.591526
-1195.349800	12.472248	1.596531
-1199.660431	9.133153	1.601536
-1202.963866	-1.422261	1.606541
-1206.681329	7.058995	1.611546
-1210.420476	0.913011	1.616550
-1214.130264	2.982848	1.621555
-1217.931576	10.733230	1.626560
-1221.640174	2.779950	1.631565
-1225.318921	9.616614	1.636570
-1229.329380	4.961695	1.641574
-1232.832146	0.780618	1.646579
-1236.794731	9.447799	1.651584
-1240.705862	8.739817	1.656589
-1244.279145	12.949823	1.661594
-1248.027485	13.862113	1.666598
-1251.494522	-0.926321	1.671603
-1255.785423	7.807624	1.676608
-1259.450082	2.122879	1.681613
-1263.261685	5.538435	1.686618
-1267.042279	7.326380	1.691622
-1270.297773	1.281286	1.696627
-1274.337558	6.583111	1.701632
-1278.306973	1.918557	1.706637
-1281.898808	11.422168	1.711642
-1285.577952	3.189897	1.716646
-1289.125603	-0.220677	1.721651
-1293.087209	12.067058	1.726656
-1297.262584	6.599729	1.731661
-1300.779009	8.867409	1.736666
-1304.484881	-1.982974	1.741670
-1307.904348	1.391967	1.746675
-1312.253851	12.696317	1.751680
-1315.755160	-3.646099	1.756685
-1319.911204	12.775953	1.761690
-1323.648734	4.360706	1.766694
-1326.998892	-0.071728	1.771699
-1330.456491	8.297159	1.776704
-1334.157919	-0.644231	1.781709
-1338.262275	1.839037	1.786714
-1342.165628	7.514945	1.791718
-1345.664225	-0.694084	1.796723
-1349.881223	8.282081	1.801728
-1353.472530	1.753134	1.806733
-1356.957586	8.890146	1.811738
-1360.972710	1.757286	1.816742
-1364.579475	3.266831	1.821747
-1368.544184	3.084875	1.826752
-1372.260053	-0.585639	1.831757
-1375.913303	5.960171	1.836762
-1379.662751	5.914081	1.841766
-1383.264385	0.457567	1.846771
-1387.537342	8.282141	1.851776
-1390.828194	4.396962	1.856781
-1394.323696	-0.355871	1.861786
-1398.418637	0.583766	1.866790
-1402.361119	0.051387	1.871795
-1406.324244	7.807467	1.876800
-1410.008627	10.567394	1.881805
-1413.597274	2.604697	1.886810
-1417.280838	4.445157	1.891814
-1420.922544	1.571810	1.896819
-1424.735178	4.161485	1.901824
-1428.269756	-5.815684	1.906829
-1432.285704	12.476424	1.911834
-1436.303721	10.924889	1.916838
-1439.917235	6.411790	1.921843
-1443.963446	5.268476	1.926848
-1447.267924	8.412324	1.931853
-1451.046560	10.690676	1.936858
-1454.823216	10.142873	1.941862
-1458.503513	8.860572	1.946867
-1462.715949	6.879754	1.951872
-1466.283463	0.875451	1.956877
-1470.091883	6.476444	1.961882
-1473.448997	8.729912	1.966886
-1477.278890	2.087988	1.971891
-1481.325455	13.055550	1.976896
-1484.985069	-0.102658	1.981901
-1488.522592	4.265986	1.986906
-1492.496879	6.222505	1.991910
-1496.539515	7.103478	1.996915
-1500.363428	6.180788	2.006912
-1501.331750	5.482069	2.016909
-1498.566754	7.378113	2.026906
-1495.811329	1.898887	2.036902
-1493.509349	2.511195	2.046899
-1491.935403	6.585863	2.056896
-1489.748495	10.781849	2.066893
-1487.951590	4.218235	2.076890
-1486.120704	2.352844	2.086886
-1484.522593	2.908928	2.096883
-1482.273987	5.364522	2.106880
-1480.285333	5.044917	2.116877
-1478.389729	2.941801	2.126874
-1476.464792	6.485015	2.136870
-1474.725557	3.358525	2.146867
-1472.884064	5.244586	2.156864
-1470.938483	5.711882	2.166861
-1468.942668	8.241127	2.176858
-1466.888555	7.939472	2.186854
-1465.260687	5.285556	2.196851
-1463.374210	10.028620	2.206848
-1461.427602	9.163134	2.216845
-1459.649546	3.690449	2.226842
-1457.653049	-0.648795	2.236838
-1456.033520	3.409126	2.246835
-1453.668031	0.461848	2.256832
-1452.126126	3.780625	2.266829
-1450.218260	5.716077	2.276826
-1448.129756	-1.055249	2.286822
-1446.259737	-0.290045	2.296819
-1444.523330	1.499181	2.306816
-1442.837234	5.072772	2.316813
-1440.890272	2.929884	2.326810
-1438.852883	-0.645369	2.336806
-1436.835382	1.542537	2.346803
-1434.901869	-2.061869	2.356800
-1433.141319	-2.425438	2.366797
-1431.324465	4.741420	2.376794
-1429.656108	6.153134	2.386790
-1427.326008	2.624181	2.396787
-1425.486467	8.514788	2.406784
-1423.969545	6.248135	2.416781
-1422.000169	1.114318	2.426778
-1420.362498	5.243572	2.436774
-1417.989395	-4.563807	2.446771
-1416.203850	3.964386	2.456768
-1414.437883	11.663617	2.466765
-1412.701845	-1.201225	2.476762
-1410.368459	0.533502	2.486758
-1408.625326	5.092720	2.496755
-1406.943824	5.362350	2.506752
-1405.028307	8.952925	2.516749
-1403.114579	3.085929	2.526746
-1401.408559	0.515861	2.536742
-1399.270785	10.696095	2.546739
-1397.314286	4.891729	2.556736
-1395.854677	6.914780	2.566733
-1393.930481	4.939785	2.576730
-1391.681902	4.997063	2.586726
-1389.745662	1.970147	2.596723
-1387.933251	-2.727988	2.606720
-1386.149394	0.452628	2.616717
-1384.702281	2.060846	2.626714
-1382.460662	8.024488	2.636710
-1380.314180	-0.609741	2.646707
-1378.912272	2.403080	2.656704
-1376.711884	-1.081373	2.666701
-1374.906669	-3.146251	2.676698
-1373.189095	0.566037	2.686694
-1370.989154	1.575328	2.696691
-1369.120122	4.342851	2.706688
-1367.788624	5.492747	2.716685
-1365.574251	5.546052	2.726682
-1363.526834	3.275042	2.736678
-1361.719342	2.932434	2.746675
-1359.965739	7.306859	2.756672
-1358.299808	10.155851	2.766669
-1355.966476	7.384342	2.776666
-1354.133151	3.497617	2.786662
-1352.491679	4.422640	2.796659
-1350.457176	6.154747	2.806656
-1348.937988	14.034065	2.816653
-1346.862623	5.259666	2.826650
-1344.855782	2.606747	2.836646
-1342.906611	5.509885	2.846643
-1341.274621	2.692762	2.856640
-1339.303068	3.538116	2.866637
-1337.369825	3.819607	2.876634
-1335.400197	5.230534	2.886630
-1333.529010	4.307754	2.896627
-1331.685550	1.442578	2.906624
-1329.734581	0.705977	2.916621
-1327.935870	0.955325	2.926618
-1325.963505	2.106876	2.936614
-1324.425664	2.945875	2.946611
-1322.544871	6.046291	2.956608
-1320.539085	3.129878	2.966605
-1318.432846	0.833702	2.976602
-1316.840054	-2.005550	2.986598
-1314.852255	6.578779	2.996595
-1312.684432	8.895896	3.006592
-1311.224237	5.397345	3.016589
-1309.112925	7.871930	3.026586
-1307.303021	7.494242	3.036582
-1305.419406	5.480024	3.046579
-1303.623984	10.012012	3.056576
-1301.793263	3.882063	3.066573
-1300.044304	9.215699	3.076570
-1298.126355	3.016529	3.086566
-1295.882621	3.210464	3.096563
-1294.386489	4.231423	3.106560
-1292.285020	9.818118	3.116557
-1290.670126	3.326406	3.126554
-1288.217743	9.098519	3.136550
-1286.659781	-0.297228	3.146547
-1284.840085	6.978250	3.156544
-1282.907036	7.588238	3.166541
-1281.113015	0.055762	3.176538
-1279.249272	3.064206	3.186534
-1277.056915	0.916914	3.196531
-1275.585878	6.062944	3.206528
-1273.585513	8.814265	3.216525
-1271.809459	9.141494	3.226522
-1269.728053	6.568282	3.236518
-1267.843395	5.040242	3.246515
-1266.070465	5.330080	3.256512
-1264.352883	13.709814	3.266509
-1262.221546	9.033358	3.276506
-1260.169604	4.876453	3.286502
-1258.372355	5.163984	3.296499
-1256.785846	8.093657	3.306496
-1254.744145	12.248379	3.316493
-1252.822772	11.677631	3.326490
-1251.072625	7.673240	3.336486
-1249.407952	6.035156	3.346483
-1247.284740	9.155263	3.356480
-1245.382006	8.870135	3.366477
-1243.731792	13.354358	3.376474
-1241.615651	11.434031	3.386470
-1239.636193	9.984000	3.396467
-1237.859646	10.281176	3.406464
-1236.107701	7.533348	3.416461
-1233.973104	10.861645	3.426458
-1232.271447	4.892926	3.436454
-1230.271738	7.224392	3.446451
-1228.444588	5.653481	3.456448
-1226.547885	12.485637	3.466445
-1224.958088	1.248517	3.476442
-1223.115276	5.417724	3.486438
-1220.728973	4.428394	3.496435
-1219.075624	7.093188	3.506432
-1217.446351	4.682372	3.516429
-1215.539282	9.510777	3.526426
-1213.362506	4.498673	3.536422
-1211.574125	9.437652	3.546419
-1209.756243	13.752967	3.556416
-1207.828198	6.548039	3.566413
-1206.008346	10.405147	3.576410
-1203.840330	5.456032	3.586406
-1202.131524	5.165654	3.596403
-1200.584941	10.931227	3.606400
-1198.784053	13.095588	3.616397
-1196.380037	9.201347	3.626394
-1194.731756	10.235920	3.636390
-1192.998010	4.151567	3.646387
-1190.863999	7.015788	3.656384
-1189.051175	8.431406	3.666381
-1187.180603	4.360424	3.676378
-1185.261014	-5.423124	3.686374
-1183.654844	5.800808	3.696371
-1181.814750	7.652594	3.706368
-1179.638017	13.364725	3.716365
-1177.700187	16.490877	3.726362
-1175.848848	5.106144	3.736358
-1174.253258	4.398113	3.746355
-1172.523047	5.312225	3.756352
-1170.157228	6.202011	3.766349
-1168.384877	3.310442	3.776346
-1166.605903	3.880441	3.786342
-1164.515643	-2.163037	3.796339
-1162.812720	8.480172	3.806336
-1161.164175	6.101047	3.816333
-1159.160114	7.200302	3.826330
-1157.207913	3.708388	3.836326
-1155.056232	8.854551	3.846323
-1153.367321	7.878971	3.856320
-1151.579181	7.114886	3.866317
-1149.830947	5.664029	3.876314
-1147.986590	4.242005	3.886310
-1145.928804	5.027940	3.896307
-1144.233032	4.853374	3.906304
-1142.186474	11.726367	3.916301
-1140.114204	13.961042	3.926298
-1138.410081	6.146202	3.936294
-1136.622489	4.082742	3.946291
-1134.676688	2.241869	3.956288
-1132.868245	12.727699	3.966285
-1130.669550	8.460581	3.976282
-1128.975627	8.946322	3.986278
-1127.330909	6.905726	3.996275
-1125.339420	4.599656	4.006272
-1123.528606	5.573542	4.016269
-1121.773930	2.286940	4.026266
-1119.637066	1.408670	4.036262
-1117.432720	-1.283550	4.046259
-1116.008044	-1.443148	4.056256
-1114.142644	3.938325	4.066253
-1112.127511	2.844272	4.076250
-1110.452179	7.386155	4.086246
-1108.392158	8.148082	4.096243
-1106.335621	6.892674	4.106240
-1104.613379	4.135483	4.116237
-1102.651312	5.318873	4.126234
-1100.813473	5.007928	4.136230
-1099.072164	2.855585	4.146227
-1097.407677	8.172897	4.156224
-1095.402707	8.184168	4.166221
-1093.228152	4.735683	4.176218
-1091.335829	9.009187	4.186214
-1089.553575	5.009248	4.196211
-1087.858839	8.760151	4.206208
-1086.095189	6.083191	4.216205
-1083.976349	6.477309	4.226202
-1082.198673	7.120213	4.236198
-1080.007102	5.167438	4.246195
-1078.465323	6.984920	4.256192
-1076.822151	5.819344	4.266189
-1074.368224	8.143029	4.276186
-1072.381327	-0.653314	4.286182
-1070.905890	-4.716264	4.296179
-1069.255940	1.138655	4.306176
-1067.227273	7.548791	4.316173
-1065.463307	3.597584	4.326170
-1063.374095	2.864356	4.336166
-1061.268143	1.310557	4.346163
-1059.582269	8.034477	4.356160
-1057.742968	8.893332	4.366157
-1055.745350	7.511602	4.376154
-1054.174117	1.884390	4.386150
-1051.998168	3.507297	4.396147
-1050.192333	-3.551645	4.406144
-1048.383324	-0.684255	4.416141
-1046.699784	0.033732	4.426138
-1045.018025	-1.415889	4.436134
-1042.834169	-1.741080	4.446131
-1040.513382	4.868673	4.456128
-1038.761243	3.469378	4.466125
-1037.183752	-5.199875	4.476122
-1035.382948	1.802521	4.486118
-1033.379612	3.309370	4.496115
-1031.255908	7.452760	4.506112
-1029.444069	5.211818	4.516109
-1027.878259	-2.737142	4.526106
-1025.762341	1.091707	4.536102
-1023.836276	1.074606	4.546099
-1022.372176	0.332444	4.556096
-1020.332996	1.738834	4.566093
-1018.317414	4.645844	4.576090
-1016.391526	-3.509119	4.586086
-1014.513323	-1.849609	4.596083
-1012.614613	-3.043379	4.606080
-1011.006012	0.441883	4.616077
-1009.047618	-4.118271	4.626074
-1006.865470	-3.378944	4.636070
-1005.202819	-3.267060	4.646067
-1003.586175	-5.702554	4.656064
-1001.290681	-1.352928	4.666061
-999.642665	-8.362910	4.676058
-997.626827	-7.802241	4.686054
-996.078791	-0.489389	4.696051
-994.081321	-6.322095	4.706048
-991.981019	-0.044928	4.716045
-989.939641	-1.239390	4.726042
-988.292046	-8.617192	4.736038
-986.840054	-1.431079	4.746035
-984.441812	-2.808921	4.756032
-982.348213	-4.518569	4.766029
-981.090852	-3.787644	4.776026
-978.993270	-1.646873	4.786022
-977.007136	-2.158278	4.796019
-975.030212	5.204428	4.806016
-973.137191	2.484757	4.816013
-971.336566	-1.134349	4.826010
-969.631742	-0.498657	4.836006
-967.839266	3.400917	4.846003
-965.950548	-1.219115	4.856000
-963.840542	0.854948	4.865997
-961.939491	-5.203895	4.875994
-960.064070	-1.803896	4.885990
-958.412278	-2.707085	4.895987
-956.439864	2.115831	4.905984
-954.571304	1.326403	4.915981
-952.737370	4.013043	4.925978
-950.707514	4.058353	4.935974
-948.787484	-1.046673	4.945971
-946.804473	1.428239	4.955968
-945.190158	-0.046844	4.965965
-943.464302	-5.011868	4.975962
-941.925545	1.413561	4.985958
-939.626337	0.578968	4.995955
-937.678930	-0.401475	5.005952
-935.769306	5.648870	5.015949
-933.757760	-0.482885	5.025946
-931.913931	-2.533079	5.035942
-929.875963	-2.023258	5.045939
-928.403646	-0.114042	5.055936
-926.499247	-0.648651	5.065933
-924.748861	0.505579	5.075930
-922.546094	-0.861473	5.085926
-920.737409	0.313439	5.095923
-918.632844	3.171572	5.105920
-917.363664	-5.708843	5.115917
-915.333638	-3.850896	5.125914
-913.119381	-3.992932	5.135910
-911.285308	-7.980499	5.145907
-909.238194	-7.347385	5.155904
-908.098409	-0.275510	5.165901
-905.929761	-3.465514	5.175898
-903.844378	-6.736939	5.185894
-901.857813	1.208502	5.195891
-899.836960	-2.286288	5.205888
-898.188869	-6.225163	5.215885
-896.358181	-1.084272	5.225882
-894.545049	-4.864795	5.235878
-892.846296	-0.850703	5.245875
-890.952048	0.073710	5.255872
-888.746348	2.492542	5.265869
-886.789772	4.723838	5.275866
-885.190677	0.465961	5.285862
-883.172685	0.475332	5.295859
-881.514110	0.594271	5.305856
-879.695557	-6.180796	5.315853
-877.578917	0.243870	5.325850
-875.606783	-7.349959	5.335846
-873.683610	-2.039099	5.345843
-871.871355	-4.009988	5.355840
-869.848517	-4.896645	5.365837
-868.240197	-0.738603	5.375834
-866.484766	-6.031988	5.385830
-864.503975	-5.637707	5.395827
-862.585598	-6.300816	5.405824
-860.897840	3.970860	5.415821
-858.946454	-3.695432	5.425818
-856.803751	-0.672812	5.435814
-855.191410	-4.814365	5.445811
-852.974128	-3.071562	5.455808
-851.533801	-4.111398	5.465805
-849.433502	-4.121473	5.475802
-847.682368	-2.518882	5.485798
-845.607632	-0.505389	5.495795
-843.868764	2.586537	5.505792
-842.071493	-3.037206	5.515789
-840.044008	2.007537	5.525786
-838.299677	-0.612471	5.535782
-836.466969	8.887634	5.545779
-834.479070	0.435520	5.555776
-832.482661	2.445757	5.565773
-830.576483	3.808839	5.575770
-828.971233	2.316336	5.585766
-826.771041	3.641896	5.595763
-825.205770	3.903685	5.605760
-823.171358	2.535216	5.615757
-821.327282	-2.410730	5.625754
-819.366059	0.459355	5.635750
-817.494954	-3.639853	5.645747
-815.862619	-5.433519	5.655744
-813.757142	3.538263	5.665741
-812.024062	-1.132565	5.675738
-809.734981	-1.531201	5.685734
-808.319819	1.928285	5.695731
-806.427268	2.388826	5.705728
-804.540171	0.110759	5.715725
-802.528250	3.858548	5.725722
-800.581658	2.330450	5.735718
-798.043678	0.628879	5.745715
-797.208590	-4.062613	5.755712
-795.411223	2.190534	5.765709
-793.367305	3.078471	5.775706
-791.328304	0.420870	5.785702
-788.918533	3.026656	5.795699
-786.470022	4.683618	5.805696
-785.428775	5.607087	5.815693
-783.885012	4.849180	5.825690
-782.135573	-0.684771	5.835686
-780.023063	-0.311471	5.845683
-778.195433	-0.276321	5.855680
-776.209004	3.439249	5.865677
-774.261196	3.122034	5.875674
-772.545190	3.025029	5.885670
-770.759343	-0.979992	5.895667
-768.834729	-0.399808	5.905664
-767.036145	0.922101	5.915661
-764.848861	2.529257	5.925658
-763.294245	2.881212	5.935654
-761.219104	2.646289	5.945651
-759.066266	-3.556857	5.955648
-757.717532	0.729596	5.965645
-755.828082	0.868567	5.975642
-753.677612	-0.384181	5.985638
-751.934839	-9.935476	5.995635
-750.072341	-8.116926	6.005632
-748.011420	-2.445864	6.015629
-746.306936	-6.657337	6.025626
-744.522957	0.077992	6.035622
-742.552379	-3.328108	6.045619
-740.515061	3.908319	6.055616
-738.742286	3.186474	6.065613
-736.699733	1.355723	6.075610
-735.083651	-4.970044	6.085606
-733.125990	-2.094579	6.095603
-731.102052	1.084508	6.105600
-729.676920	1.785600	6.115597
-727.691788	-2.459659	6.125594
-725.854187	3.228167	6.135590
-723.554147	-1.651627	6.145587
-721.845618	1.999454	6.155584
-719.893597	7.582159	6.165581
-718.136307	2.504892	6.175578
-716.513816	8.920265	6.185574
-714.166419	8.668717	6.195571
-712.550092	4.850301	6.205568
-710.544985	0.207124	6.215565
-708.598184	9.043317	6.225562
-706.908700	2.551098	6.235558
-704.886578	2.959436	6.245555
-703.115120	2.510986	6.255552
-701.340206	3.003042	6.265549
-699.417241	-0.959102	6.275546
-697.399498	-1.109007	6.285542
-695.691273	-1.389452	6.295539
-693.726874	-2.913993	6.305536
-691.999221	-0.625424	6.315533
-690.070074	-2.693805	6.325530
-688.002125	-0.088557	6.335526
-686.401063	-1.166610	6.345523
-684.049611	-3.056151	6.355520
-682.596834	4.441105	6.365517
-680.488517	-9.720679	6.375514
-678.770294	0.980489	6.385510
-677.904979	2.003171	6.395507
-675.323284	5.249502	6.405504
-673.187706	6.463953	6.415501
-671.183515	2.894641	6.425498
-669.248395	0.842691	6.435494
-667.172327	-0.983883	6.445491
-665.514552	-4.073098	6.455488
-664.185860	-2.344448	6.465485
-661.859572	-1.124144	6.475482
-659.504134	-2.240610	6.485478
-657.808394	-2.507980	6.495475
-656.304354	3.927941	6.505472
-654.371656	-0.264672	6.515469
-652.408138	-4.425892	6.525466
-650.582140	-5.347229	6.535462
-648.918478	-4.750516	6.545459
-646.920388	-2.197228	6.555456
-644.892588	3.302382	6.565453
-642.956929	7.165130	6.575450
-641.194765	-0.042872	6.585446
-639.244297	-1.333037	6.595443
-637.391767	-5.315458	6.605440
-635.733349	-1.435253	6.615437
-633.639528	-2.322000	6.625434
-631.712694	-8.179453	6.635430
-629.935280	-1.403507	6.645427
-628.016748	2.941991	6.655424
-626.148568	-2.394508	6.665421
-624.652176	-4.706330	6.675418
-622.618616	-2.493425	6.685414
-620.573097	-6.064560	6.695411
-618.530582	-5.037298	6.705408
-616.708398	-5.607473	6.715405
-615.168935	1.947032	6.725402
-613.139351	-1.882079	6.735398
-611.090810	-1.204722	6.745395
-609.271901	3.343025	6.755392
-607.186506	-0.111312	6.765389
-605.717459	-4.905607	6.775386
-603.672936	0.806105	6.785382
-601.504928	-2.326686	6.795379
-599.720054	-2.541938	6.805376
-598.380510	3.419774	6.815373
-596.278754	-1.208752	6.825370
-594.339171	-4.657152	6.835366
-592.669243	-0.180329	6.845363
-590.540774	-2.127315	6.855360
-588.215108	-1.664737	6.865357
-587.054675	1.756635	6.875354
-584.877853	-6.938629	6.885350
-583.136890	-6.655799	6.895347
-581.244067	-6.567754	6.905344
-579.272912	-5.889060	6.915341
-577.214966	-6.367393	6.925338
-575.557772	-5.621174	6.935334
-573.322095	-12.235291	6.945331
-571.890648	-8.658258	6.955328
-569.989032	-6.894759	6.965325
-568.399362	-4.506688	6.975322
-566.082817	-10.527398	6.985318
-564.097983	-10.559828	6.995315
-562.396124	-10.850213	7.005312
-560.431519	-12.110993	7.015309
-558.843312	-12.247430	7.025306
-556.666226	-5.881060	7.035302
-554.703690	-8.796250	7.045299
-552.998204	-5.790349	7.055296
-551.225431	-8.801540	7.065293
-549.280836	-6.541203	7.075290
-547.522748	-5.668975	7.085286
-545.532425	-9.903865	7.095283
-543.764970	-5.933641	7.105280
-541.701339	-3.115992	7.115277
-539.726139	-2.745808	7.125274
-537.987418	-4.306807	7.135270
-535.959510	-2.557137	7.145267
-534.235225	-7.992163	7.155264
-532.512733	-4.527908	7.165261
-530.655385	-7.377330	7.175258
-528.696150	-2.242456	7.185254
-526.517254	-2.777959	7.195251
-524.781487	-10.665352	7.205248
-523.075732	-7.477892	7.215245
-521.182248	-4.618838	7.225242
-519.295387	-10.130347	7.235238
-517.651097	-2.253041	7.245235
-515.475966	-6.645322	7.255232
-513.411129	-7.438913	7.265229
-511.934571	-2.348511	7.275226
-509.799436	-0.112256	7.285222
-507.807562	-5.831585	7.295219
-505.941140	0.237086	7.305216
-504.380676	-6.062288	7.315213
-502.404648	0.052039	7.325210
-500.500034	0.027737	7.335206
-498.346163	-4.931137	7.345203
-496.770892	-5.240732	7.355200
-495.028131	-3.451800	7.365197
-492.899965	-6.229183	7.375194
-491.054056	-6.891473	7.385190
-488.980114	-3.679106	7.395187
-487.367877	-5.703029	7.405184
-485.567205	-1.671746	7.415181
-483.623966	-4.493798	7.425178
-481.542534	-3.840530	7.435174
-479.935292	0.610072	7.445171
-478.182324	-1.655795	7.455168
-475.982422	-3.225666	7.465165
-474.297877	1.073647	7.475162
-472.250706	-0.269723	7.485158
-470.467181	-1.930988	7.495155
-468.510214	5.541161	7.505152
-466.747173	-1.914763	7.515149
-464.857089	3.635426	7.525146
-462.918163	-2.031203	7.535142
-461.216900	-0.663516	7.545139
-459.127403	-1.851001	7.555136
-457.215860	-1.581109	7.565133
-455.547879	-1.351268	7.575130
-453.428913	-5.218208	7.585126
-451.444741	0.792232	7.595123
-449.791885	-6.710820	7.605120
-448.023077	-0.378615	7.615117
-446.147361	0.279115	7.625114
-444.321190	-0.245776	7.635110
-442.079223	-3.169185	7.645107
-440.272997	-10.305139	7.655104
-438.575859	-4.705172	7.665101
-436.948734	-4.972481	7.675098
-435.000105	-8.722203	7.685094
-432.428908	-5.693402	7.695091
-431.255457	-8.834596	7.705088
-429.419721	-6.310457	7.715085
-427.170505	1.088216	7.725082
-425.439390	0.998521	7.735078
-423.314156	-0.557801	7.745075
-421.526108	-3.146601	7.755072
-419.889139	-0.780189	7.765069
-417.890566	-5.977883	7.775066
-415.895560	-3.262849	7.785062
-414.113977	0.405221	7.795059
-412.437132	0.338412	7.805056
-410.354736	0.003161	7.815053
-408.571964	-1.710045	7.825050
-406.885976	5.402794	7.835046
-404.800224	-2.346199	7.845043
-402.831637	-6.075399	7.855040
-400.821038	-6.947076	7.865037
-399.162427	-0.055654	7.875034
-397.195912	-2.980830	7.885030
-395.679730	3.135965	7.895027
-393.349564	0.773258	7.905024
-391.649179	-0.091512	7.915021
-389.889995	6.003857	7.925018
-387.699669	1.478203	7.935014
-385.718132	-3.022005	7.945011
-384.224321	1.490989	7.955008
-382.612941	-4.682232	7.965005
-380.448174	0.153112	7.975002
-378.384892	3.690969	7.984998
-376.672819	-4.743606	7.994995
-374.718334	-3.708394	8.004992
-372.735402	-7.564598	8.014989
-370.802242	-4.910704	8.024986
-369.387449	-5.999862	8.034982
-367.175596	-8.154178	8.044979
-365.305492	-8.333916	8.054976
-363.360512	-3.723994	8.064973
-361.438298	0.947987	8.074970
-359.937804	-1.785913	8.084966
-357.878681	-8.701660	8.094963
-355.921364	-4.147386	8.104960
-354.352789	2.109494	8.114957
-352.294352	2.521808	8.124954
-350.201878	-0.563968	8.134950
-348.512390	-0.086431	8.144947
-346.601299	-0.399015	8.154944
-344.623361	2.718284	8.164941
-342.825718	-1.713059	8.174938
-341.165257	-5.140386	8.184934
-339.008174	6.211013	8.194931
-337.308165	-0.415283	8.204928
-335.310037	-5.513368	8.214925
-333.360350	-8.596860	8.224922
-331.576802	-2.524286	8.234918
-329.719364	-6.152000	8.244915
-328.101070	1.601710	8.254912
-326.050109	-6.975355	8.264909
-323.926608	0.208227	8.274906
-322.220304	-2.114819	8.284902
-320.497566	-4.674173	8.294899
-318.436651	-2.291683	8.304896
-316.268496	-2.226856	8.314893
-314.896740	3.652523	8.324890
-312.925051	-5.215039	8.334886
-310.884059	4.129114	8.344883
-308.865772	-1.346383	8.354880
-307.216573	-0.614489	8.364877
-305.339564	-5.047421	8.374874
-303.563730	-2.728359	8.384870
-301.658342	-10.663213	8.394867
-299.865711	-1.691515	8.404864
-297.906920	-7.924879	8.414861
-296.009902	1.871747	8.424858
-294.032341	-0.685634	8.434854
-292.053711	-4.818987	8.444851
-290.110177	-3.777220	8.454848
-288.674193	-1.174947	8.464845
-286.738801	2.422881	8.474842
-284.716586	-2.289008	8.484838
-282.567455	-2.132692	8.494835
-280.908243	-3.756607	8.504832
-278.974955	-1.726346	8.514829
-277.302233	2.120262	8.524826
-275.197878	-1.158402	8.534822
-273.634467	-1.642801	8.544819
-271.844470	-0.426510	8.554816
-269.665361	-2.250248	8.564813
-267.968902	-0.924286	8.574810
-265.706674	2.018228	8.584807
-263.940395	-8.720737	8.594803
-262.096510	-5.166706	8.604800
-260.402007	-6.889399	8.614797
-258.482960	-0.082070	8.624794
-256.676983	-0.587807	8.634791
-254.612598	-0.727416	8.644787
-252.757121	-0.983680	8.654784
-251.013911	-4.853633	8.664781
-248.840681	-3.414280	8.674778
-247.378742	-4.956160	8.684775
-245.308309	-5.414097	8.694771
-243.188439	-8.019414	8.704768
-241.481410	-1.244548	8.714765
-239.877826	-4.073779	8.724762
-237.778271	-7.809543	8.734759
-236.075020	-6.296747	8.744755
-233.980108	-4.139085	8.754752
-232.239914	-1.834806	8.764749
-230.201065	-2.147162	8.774746
-228.455593	3.328412	8.784743
-226.531316	-0.785163	8.794739
-224.548606	1.515153	8.804736
-222.738865	0.934630	8.814733
-220.812864	1.729776	8.824730
-218.774610	-6.044647	8.834727
-217.112444	-4.776334	8.844723
-215.316768	-2.381423	8.854720
-213.202479	-4.434767	8.864717
-211.635395	-0.752833	8.874714
-209.553908	0.142245	8.884711
-207.836674	0.738612	8.894707
-205.681734	-3.557023	8.904704
-204.138184	-4.762951	8.914701
-202.115962	-6.351589	8.924698
-200.309145	-3.271596	8.934695
-198.301655	-3.408393	8.944691
-196.351977	-7.132836	8.954688
-194.561125	-15.496180	8.964685
-192.845008	-7.983776	8.974682
-191.156868	-8.593817	8.984679
-189.295630	-2.677212	8.994675
-186.976880	-13.071657	9.004672
-185.429410	-7.559719	9.014669
-183.568006	-6.705287	9.024666
-181.427622	-13.011753	9.034663
-179.425265	-6.173442	9.044659
-177.728561	-10.871194	9.054656
-175.774017	-5.482631	9.064653
-174.109132	-2.588391	9.074650
-172.211049	-6.516163	9.084647
-170.147330	-11.059317	9.094643
-168.323672	-10.645696	9.104640
-166.565184	-1.464751	9.114637
-164.744718	-7.236991	9.124634
-162.472458	-2.036485	9.134631
-161.062571	-3.429480	9.144627
-158.970925	-9.331832	9.154624
-156.999682	-11.564408	9.164621
-155.374314	-8.865957	9.174618
-153.413046	1.629497	9.184615
-151.348235	-7.829128	9.194611
-149.539811	-4.907249	9.204608
-147.881052	-0.868843	9.214605
-145.960956	-3.052198	9.224602
-143.916506	-11.084921	9.234599
-141.996601	-12.894027	9.244595
-140.196181	-12.452992	9.254592
-138.465718	-10.813414	9.264589
-136.539171	-2.834009	9.274586
-134.802638	-10.318641	9.284583
-132.740414	-11.722550	9.294579
-130.668359	-13.172236	9.304576
-129.120052	-12.869388	9.314573
-127.168216	-4.766115	9.324570
-125.234755	-9.481083	9.334567
-122.942628	-4.992663	9.344563
-121.596974	-7.109604	9.354560
-119.707258	-0.930639	9.364557
-117.775613	-1.497377	9.374554
-115.772179	0.226561	9.384551
-113.931463	0.591712	9.394547
-111.986094	6.496541	9.404544
-110.028971	3.269926	9.414541
-108.427893	5.395967	9.424538
-106.822475	9.610286	9.434535
-104.631467	6.182146	9.444531
-102.598523	-3.200309	9.454528
-100.965003	-0.746279	9.464525
-98.783803	3.428284	9.474522
-96.822735	-1.782128	9.484519
-95.349501	-3.109402	9.494515
-93.527562	1.457225	9.504512
-91.318615	4.488936	9.514509
-89.466224	-2.453624	9.524506
-87.766248	1.957202	9.534503
-85.734792	5.086710	9.544499
-83.974601	-1.465343	9.554496
-82.141230	-4.114817	9.564493
-80.495904	3.039499	9.574490
-78.454854	1.672171	9.584487
-76.398508	4.320869	9.594483
-74.502905	1.315678	9.604480
-72.780679	-0.550260	9.614477
-70.686031	0.960215	9.624474
-68.885277	-2.587214	9.634471
-66.987634	-6.053781	9.644467
-65.083523	-2.003931	9.654464
-63.301837	3.710734	9.664461
-61.496209	2.800983	9.674458
-59.619171	-0.138077	9.684455
-57.705012	-6.217300	9.694451
-55.649080	-4.926428	9.704448
-53.989905	0.250413	9.714445
-52.169439	-4.438581	9.724442
-50.339792	1.682131	9.734439
-48.286775	-6.013992	9.744435
-46.407700	-1.887500	9.754432
-44.563597	-2.740218	9.764429
-42.612224	-5.637438	9.774426
-40.827219	-6.967046	9.784423
-38.775251	0.722437	9.794419
-37.123286	-3.841771	9.804416
-35.029518	-5.091156	9.814413
-33.394046	-1.877909	9.824410
-31.376485	-7.302547	9.834407
-29.569290	2.409171	9.844403
-27.863038	-4.004765	9.854400
-25.946826	-5.102659	9.864397
-23.779570	-7.573243	9.874394
-21.999104	-4.114693	9.884391
-19.899406	-1.646548	9.894387
-18.453083	-2.890536	9.904384
-16.546836	-3.500512	9.914381
-14.473890	-3.576545	9.924378
-12.522092	-3.986939	9.934375
-10.558549	0.072424	9.944371
-9.026352	-5.210039	9.954368
-7.398373	8.602441	9.964365
-5.781126	35.002606	9.974362
-4.020826	59.501025	9.984359
-2.547042	88.515268	9.994355
-0.788739	122.277967	10.004352
0.000000	161.845273	10.009357
1.077631	177.162541	10.014362
1.548917	212.307571	10.019367
2.158933	225.914350	10.024371
2.722048	242.770879	10.029376
3.121361	251.338171	10.034381
3.449547	254.234974	10.039386
3.367441	253.623798	10.044391
3.545928	263.852180	10.049395
3.304511	261.709941	10.054400
3.249893	256.442306	10.059405
3.322309	247.357057	10.064410
3.622816	269.997267	10.069415
3.396801	255.615245	10.074419
3.521260	256.458208	10.079424
3.464477	264.335002	10.084429
3.993296	262.878893	10.089434
3.625917	260.460275	10.094439
3.553131	254.359741	10.099443
3.494663	256.159143	10.104448
3.438506	264.321269	10.109453
3.853041	274.489930	10.114458
3.991665	280.998289	10.119463
4.227101	276.460253	10.124467
4.084072	269.511465	10.129472
3.501282	272.876859	10.134477
3.953370	271.772038	10.139482
4.074003	288.276570	10.144487
4.089829	284.785981	10.149491
4.521333	291.441596	10.154496
4.318101	285.694599	10.159501
4.339851	276.928078	10.164506
3.726872	285.341461	10.169511
4.141688	282.755496	10.174515
4.783154	296.819380	10.179520
4.512127	296.378688	10.184525
4.557986	294.239508	10.189530
4.350725	299.528847	10.194535
4.529495	301.932243	10.199539
4.530954	296.781807	10.204544
4.295576	300.282607	10.209549
4.627502	298.749089	10.214554
4.534634	309.511227	10.219559
4.603988	312.465097	10.224563
5.027350	304.333102	10.229568
4.794450	310.243134	10.234573
5.166301	308.641745	10.239578
4.943024	308.601873	10.244583
4.679811	313.584746	10.249587
4.959227	315.163100	10.254592
4.725604	324.635653	10.259597
5.021578	314.689942	10.264602
4.816291	324.386637	10.269607
4.863096	318.347427	10.274611
5.167111	314.716244	10.279616
4.826809	323.056192	10.284621
5.376755	324.123033	10.289626
5.837771	337.860920	10.294631
5.822062	338.991178	10.299635
5.830930	331.246988	10.304640
5.641056	328.684924	10.309645
5.661524	323.093046	10.314650
5.442135	335.658950	10.319655
5.376136	329.137825	10.324659
5.564840	321.424880	10.329664
5.389434	337.634483	10.334669
5.603440	327.343863	10.339674
5.738164	336.065374	10.344679
5.937279	338.473417	10.349683
5.966220	348.404008	10.354688
6.105707	352.374893	10.359693
6.042605	350.096964	10.364698
5.725852	346.181582	10.369703
5.970467	357.334634	10.374707
6.172159	354.604451	10.379712
6.179667	358.785628	10.384717
6.367642	357.109482	10.389722
6.477798	354.966345	10.394727
6.147056	361.147475	10.399731
6.178680	357.149713	10.404736
6.389697	366.187087	10.409741
6.661969	358.864501	10.414746
6.322971	370.156385	10.419751
6.302035	374.275870	10.424755
6.679873	366.073830	10.429760
6.445917	373.579966	10.434765
6.915656	371.639674	10.439770
6.918513	373.001945	10.444775
6.802298	366.113490	10.449779
6.956291	362.903625	10.454784
6.565508	366.340917	10.459789
6.790045	364.758289	10.464794
6.611834	377.817566	10.469799
6.801187	380.220865	10.474803
7.069030	383.310250	10.479808
6.731411	383.879987	10.484813
6.768090	375.921597	10.489818
6.785538	384.770656	10.494823
7.297776	377.628986	10.499827
6.965575	388.484552	10.504832
6.961234	387.187592	10.509837
7.216403	389.752287	10.514842
6.856352	389.781540	10.519847
7.247117	405.154996	10.524851
7.533648	408.291869	10.529856
7.499719	413.599335	10.534861
7.720485	407.868240	10.539866
7.651307	412.328175	10.544871
7.634237	403.190869	10.549875
7.311261	406.234146	10.554880
7.510031	414.100222	10.559885
7.921564	402.940659	10.564890
7.828257	415.598488	10.569895
7.578126	413.082292	10.574899
8.018120	410.591639	10.579904
7.883285	419.581706	10.584909
8.186174	418.899653	10.589914
7.794158	427.897630	10.594919
7.783889	426.951705	10.599923
7.959854	421.281368	10.604928
7.925182	420.317258	10.609933
8.044924	418.448557	10.614938
7.902120	416.083979	10.619943
8.010967	425.790561	10.624947
8.410555	416.701908	10.629952
8.198110	428.604448	10.634957
8.512855	421.057432	10.639962
8.487604	425.548213	10.644967
8.065209	418.918310	10.649971
8.118296	434.191112	10.654976
8.137538	451.420072	10.659981
8.764835	454.920506	10.664986
8.729462	462.415513	10.669991
8.817307	459.552079	10.674995
9.252830	452.744316	10.680000
8.720751	460.626064	10.685005
8.592563	459.545976	10.690010
8.996089	458.057794	10.695015
8.889020	468.136321	10.700019
9.268613	462.219017	10.705024
8.992683	460.561660	10.710029
9.228205	455.905281	10.715034
8.725001	460.730935	10.720039
8.633898	467.581958	10.725043
8.738598	477.405933	10.730048
8.848133	474.972711	10.735053
9.185510	467.664918	10.740058
9.082034	473.532294	10.745063
9.174806	469.368625	10.750067
9.503773	464.938619	10.755072
9.105113	476.599657	10.760077
9.388463	483.329457	10.765082
9.481237	493.961981	10.770087
9.789077	495.647789	10.775091
9.803506	494.273707	10.780096
9.371335	493.817709	10.785101
9.779703	491.163348	10.790106
9.733193	505.668343	10.795111
9.553408	506.309106	10.800115
10.053793	508.509846	10.805120
9.637405	516.201277	10.810125
9.898365	511.231730	10.815130
10.027811	503.293168	10.820135
10.004043	509.236156	10.825139
9.987269	509.515017	10.830144
9.685220	520.301214	10.835149
10.084145	506.058966	10.840154
9.708262	512.800887	10.845159
9.868670	527.006386	10.850163
10.058152	510.723781	10.855168
9.936321	523.438295	10.860173
10.305359	531.051765	10.865178
10.427395	531.876206	10.870183
10.191191	546.477733	10.875187
10.369489	534.809628	10.880192
10.590000	547.969468	10.885197
10.787115	539.854507	10.890202
10.643772	544.468243	10.895207
10.688205	553.123860	10.900211
10.532190	537.478249	10.905216
10.377501	544.486111	10.910221
10.422652	537.256435	10.915226
10.179658	544.883953	10.920231
10.314932	541.680189	10.925235
10.818082	561.893062	10.930240
10.694219	572.751805	10.935245
11.230885	569.313695	10.940250
11.267351	577.710391	10.945255
11.066043	575.197417	10.950259
11.428245	575.909434	10.955264
11.201606	578.483202	10.960269
11.541501	571.066142	10.965274
11.529111	561.002286	10.970279
10.981039	554.876508	10.975283
11.523352	558.914090	10.980288
11.263112	577.870445	10.985293
11.476253	578.768670	10.990298
11.614522	575.961827	10.995303
11.269027	589.680357	11.000307
11.622943	583.216724	11.005312
11.112940	585.999699	11.010317
11.434616	588.922842	11.015322
11.516363	581.737771	11.020327
11.342032	590.142864	11.025331
11.954708	583.756233	11.030336
11.536114	586.149300	11.035341
11.730796	584.188197	11.040346
11.247092	591.515075	11.045351
11.341188	598.913806	11.050355
12.012455	601.170887	11.055360
12.178006	619.919027	11.060365
12.160913	613.281160	11.065370
12.118060	614.846294	11.070375
11.909362	617.363588	11.075379
12.069789	613.045578	11.080384
12.081826	621.461966	11.085389
12.599706	618.134078	11.090394
11.944141	619.494155	11.095399
12.049462	633.314291	11.100403
12.552077	625.984795	11.105408
12.456650	634.451449	11.110413
12.370911	638.103509	11.115418
12.843044	647.364348	11.120423
13.206775	640.834466	11.125427
12.875220	628.492219	11.130432
12.675700	633.132290	11.135437
12.687369	626.076651	11.140442
12.768766	624.354394	11.145447
12.683402	626.205442	11.150451
12.731593	632.868737	11.155456
12.879278	646.625356	11.160461
13.005305	654.971540	11.165466
12.968205	660.150286	11.170471
13.201212	659.315359	11.175475
13.117559	664.738085	11.180480
13.253426	666.807750	11.185485
13.468084	658.013384	11.190490
13.278207	651.740540	11.195495
13.204316	662.104081	11.200499
13.222671	653.549195	11.205504
13.035952	660.989593	11.210509
13.540164	662.344467	11.215514
13.502617	662.033684	11.220519
13.373990	665.310954	11.225523
13.706441	667.948531	11.230528
13.313117	670.272922	11.235533
13.258934	666.806024	11.240538
13.310507	670.811521	11.245543
13.285612	666.128801	11.250547
13.280658	666.995584	11.255552
13.353209	679.909475	11.260557
13.768015	676.150141	11.265562
13.711775	685.665600	11.270567
13.586483	681.421530	11.275571
14.108148	685.930817	11.280576
13.822795	687.438440	11.285581
14.011642	684.457922	11.290586
13.975199	682.473744	11.295591
14.206653	692.627747	11.300595
14.022465	680.200446	11.305600
14.139066	689.264120	11.310605
14.113363	688.271752	11.315610
14.020286	703.041426	11.320615
14.253210	719.599504	11.325619
14.832286	716.048936	11.330624
14.330310	721.448515	11.335629
14.442942	716.795885	11.340634
14.601089	718.404667	11.345639
14.663817	714.141637	11.350643
14.623078	707.569002	11.355648
14.701833	722.183548	11.360653
14.898873	720.356099	11.365658
14.507390	722.352183	11.370663
14.570755	717.123911	11.375667
14.949031	711.992076	11.380672
14.736191	720.778719	11.385677
14.755603	716.787537	11.390682
14.878427	721.357297	11.395687
14.768421	721.081727	11.400691
15.092604	723.919338	11.405696
14.745145	720.869806	11.410701
14.967697	716.149178	11.415706
15.079818	728.302983	11.420711
15.149963	742.398505	11.425715
15.451895	741.957876	11.430720
15.055742	747.327970	11.435725
15.268049	749.499001	11.440730
15.620795	743.590598	11.445735
15.684881	740.970606	11.450739
16.161626	738.328951	11.455744
15.527754	735.157935	11.460749
15.533685	721.996920	11.465754
15.538276	735.530431	11.470759
15.554482	747.496114	11.475763
15.879426	751.650427	11.480768
15.277455	755.638758	11.485773
15.699207	754.928270	11.490778
15.999516	748.315412	11.495783
15.736395	754.359759	11.500787
16.027933	752.405264	11.505792
15.706115	761.061072	11.510797
16.097079	750.275128	11.515802
16.118458	756.870215	11.520807
15.916702	752.559468	11.525811
16.203521	746.655271	11.530816
15.965143	760.836293	11.535821
16.048110	754.272292	11.540826
16.425090	759.743012	11.545831
15.957084	765.457326	11.550835
16.453081	774.343840	11.555840
16.425403	793.607174	11.560845
16.718743	786.457642	11.565850
16.317308	796.126009	11.570855
16.408206	802.208530	11.575859
16.657104	783.471742	11.580864
16.493529	786.667876	11.585869
16.697451	789.215585	11.590874
16.715066	785.481727	11.595879
16.816118	789.745884	11.600883
17.024415	784.431390	11.605888
16.728524	790.796384	11.610893
16.956554	776.548014	11.615898
16.944514	774.585164	11.620903
17.037928	787.954739	11.625907
17.197433	778.878923	11.630912
16.973590	790.766230	11.635917
16.625453	787.502315	11.640922
16.630114	791.064297	11.645927
17.089825	793.273148	11.650931
17.241561	787.335284	11.655936
16.677177	800.956455	11.660941
17.255664	814.344883	11.665946
17.457928	813.240448	11.670951
17.231271	826.924475	11.675955
17.802240	812.246036	11.680960
17.669978	821.024618	11.685965
17.286948	811.432890	11.690970
17.293774	824.046716	11.695975
17.354282	819.449677	11.700979
18.107210	807.778014	11.705984
17.529881	821.276682	11.710989
17.834187	813.546616	11.715994
17.867582	816.733418	11.720999
17.760139	818.736253	11.726003
17.838180	811.004428	11.731008
18.242662	815.508793	11.736013
18.384618	815.759188	11.741018
18.010076	814.268911	11.746023
18.214347	821.224383	11.751027
18.328892	814.910798	11.756032
17.860810	818.264323	11.761037
18.268732	808.923350	11.766042
18.424203	812.126951	11.771047
18.169817	819.728042	11.776051
17.970429	813.057655	11.781056
17.984485	828.281901	11.786061
18.200090	837.795104	11.791066
18.569343	843.883710	11.796071
18.490484	853.137944	11.801075
18.877794	841.734317	11.806080
18.713943	856.442891	11.811085
18.628038	844.310450	11.816090
18.592011	854.026233	11.821095
18.503789	854.035783	11.826099
18.755740	854.109353	11.831104
18.602784	854.777391	11.836109
18.500303	851.726606	11.841114
18.786047	858.560285	11.846119
18.605894	853.574243	11.851123
19.006067	852.278958	11.856128
19.009317	880.176496	11.861133
19.417528	872.869821	11.866138
19.359000	858.717542	11.871143
18.951762	852.501358	11.876147
19.633531	850.003612	11.881152
19.323339	857.064813	11.886157
19.108965	845.966898	11.891162
19.164605	853.679415	11.896167
19.562324	873.368617	11.901171
19.762839	872.453702	11.906176
19.397736	882.553170	11.911181
19.710295	875.890990	11.916186
19.595152	871.060163	11.921191
19.688154	880.124567	11.926195
19.822188	872.648722	11.931200
20.006126	870.952661	11.936205
19.950576	853.521244	11.941210
19.444798	852.319993	11.946215
19.747856	861.286223	11.951219
20.150006	873.031170	11.956224
19.969629	878.248617	11.961229
19.962245	869.229327	11.966234
20.188455	865.146770	11.971239
19.824858	872.962437	11.976243
20.109711	876.216384	11.981248
19.880704	876.188461	11.986253
20.179791	877.607615	11.991258
20.179336	880.288869	11.996263
20.313245	876.702029	12.001267
20.583168	871.748279	12.006272
20.189710	876.711112	12.011277
19.908902	879.944890	12.016282
20.283406	875.617891	12.021287
20.137708	880.085443	12.026291
20.812616	876.893311	12.031296
20.580683	877.597603	12.036301
20.307062	876.106993	12.041306
20.297501	875.320207	12.046311
20.155017	883.550069	12.051315
20.213391	877.254879	12.056320
20.207567	880.671890	12.061325
20.314398	879.882310	12.066330
20.424613	883.832778	12.071335
20.222807	889.452638	12.076339
20.476594	881.817332	12.081344
20.353289	886.885322	12.086349
20.600768	883.873333	12.091354
20.565645	882.354145	12.096359
20.290601	885.484496	12.101363
20.531013	874.683048	12.106368
20.366904	883.613412	12.111373
20.102041	876.253232	12.116378
20.502029	877.709912	12.121383
20.436302	883.098319	12.126387
20.413117	884.455329	12.131392
20.273024	889.062346	12.136397
20.567055	882.111366	12.141402
20.581241	890.972293	12.146407
20.308336	898.262546	12.151411
20.763056	892.019256	12.156416
20.264149	896.435911	12.161421
20.526805	893.859918	12.166426
20.379149	891.428222	12.171431
20.534625	894.627110	12.176435
20.548992	897.048945	12.181440
20.553712	889.421819	12.186445
20.605598	885.557883	12.191450
20.840462	880.696460	12.196455
20.072624	880.689822	12.201459
20.362950	858.386946	12.206464
20.200112	866.626354	12.211469
20.529333	876.649769	12.216474
20.399801	870.187421	12.221479
20.327894	868.907504	12.226483
20.812214	860.978380	12.231488
20.445042	866.810698	12.236493
20.515785	868.904974	12.241498
20.539634	864.359503	12.246503
20.218975	870.010929	12.251507
20.345303	856.945712	12.256512
20.303539	872.888577	12.261517
20.215099	870.759693	12.266522
20.399868	864.105285	12.271527
20.367184	861.357195	12.276531
20.394937	860.761588	12.281536
20.265689	858.803228	12.286541
20.599516	869.246973	12.291546
20.571750	863.979564	12.296551
20.473818	870.067001	12.301555
20.514770	867.971099	12.306560
20.409793	869.934121	12.311565
20.324189	874.608141	12.316570
20.756553	868.940893	12.321575
20.395583	872.775691	12.326579
20.595215	874.431493	12.331584
20.423809	873.454467	12.336589
20.464872	867.491643	12.341594
20.361184	861.335855	12.346599
20.073988	877.947110	12.351603
20.459763	870.107820	12.356608
20.512684	868.375884	12.361613
20.646359	871.310147	12.366618
20.278283	867.413846	12.371623
20.290604	871.701642	12.376627
20.414895	864.189506	12.381632
20.408752	871.790455	12.386637
20.252572	871.173720	12.391642
20.577739	862.675436	12.396647
20.304632	873.971392	12.401651
20.677886	869.073706	12.406656
20.652049	876.915932	12.411661
20.325856	881.085825	12.416666
20.630888	879.663779	12.421671
20.578900	877.800332	12.426675
20.611447	853.909495	12.431680
20.199247	855.205541	12.436685
20.212259	851.048177	12.441690
20.242899	841.146007	12.446695
20.087000	857.368847	12.451699
20.521149	860.095901	12.456704
20.672292	872.327186	12.461709
20.232649	857.243737	12.466714
20.279722	854.505006	12.471719
20.409523	862.076382	12.476723
20.694376	859.165676	12.481728
20.418632	858.424501	12.486733
20.098063	854.074324	12.491738
20.339641	853.837295	12.496743
20.030907	866.085151	12.501747
20.718234	881.071172	12.506752
20.877261	867.790984	12.511757
20.512168	859.374411	12.516762
20.611583	850.090504	12.521767
20.432204	858.726805	12.526771
20.740096	841.872980	12.531776
20.325192	852.199579	12.536781
20.551439	860.392695	12.541786
20.397137	850.766034	12.546791
20.398194	858.555073	12.551795
20.467711	850.174847	12.556800
20.084003	861.332307	12.561805
20.318784	859.060404	12.566810
20.279240	853.140407	12.571815
20.260569	863.690836	12.576819
20.471535	856.806735	12.581824
20.166544	858.449978	12.586829
20.351052	854.657942	12.591834
20.642706	851.307736	12.596839
20.623163	859.478550	12.601843
20.605575	854.822990	12.606848
20.445222	854.363048	12.611853
20.436875	861.603201	12.616858
20.894334	856.143278	12.621863
20.459300	859.972538	12.626867
20.528393	855.935545	12.631872
20.385623	865.832374	12.636877
20.182380	863.764383	12.641882
20.460994	850.573952	12.646887
20.154887	871.174971	12.651891
20.430812	862.058456	12.656896
20.305915	857.207110	12.661901
20.630113	861.274838	12.666906
20.646106	855.066846	12.671911
20.387880	848.748044	12.676915
20.359405	830.990620	12.681920
20.248938	844.971539	12.686925
19.980520	850.396994	12.691930
20.446664	858.906679	12.696935
20.467454	861.461531	12.701939
20.413478	855.211080	12.706944
20.615723	860.307564	12.711949
20.386367	854.641781	12.716954
20.307515	840.453335	12.721959
20.269503	859.343070	12.726963
20.355448	850.736284	12.731968
20.357060	855.218182	12.736973
20.129144	863.404886	12.741978
20.667817	855.746232	12.746983
20.358694	857.484756	12.751987
20.403207	861.092441	12.756992
20.516714	858.820957	12.761997
20.371609	848.823803	12.767002
20.397817	841.937638	12.772007
20.082999	842.439093	12.777011
20.471351	850.428142	12.782016
20.600919	858.351233	12.787021
20.324115	857.983985	12.792026
20.605996	841.077537	12.797031
20.294004	844.696346	12.802035
20.285113	839.194111	12.807040
20.185868	843.572237	12.812045
20.311945	855.552026	12.817050
20.475914	855.748445	12.822055
20.362718	852.899652	12.827059
20.116302	858.285328	12.832064
20.299310	864.163940	12.837069
20.453640	867.866081	12.842074
20.495417	855.888316	12.847079
20.262482	872.910403	12.852083
20.569452	866.085107	12.857088
20.616674	870.521885	12.862093
20.394847	857.149480	12.867098
20.472196	849.234809	12.872103
20.437631	850.569976	12.877107
20.353652	836.749801	12.882112
20.605058	846.285686	12.887117
20.382116	843.233614	12.892122
20.619587	844.287257	12.897127
20.474454	855.297845	12.902131
20.188411	841.798494	12.907136
20.314664	851.043666	12.912141
20.044628	847.822477	12.917146
20.543893	844.379231	12.922151
20.337496	849.556660	12.927155
20.641503	841.053879	12.932160
20.234181	841.126941	12.937165
20.257787	848.048161	12.942170
20.444497	842.152008	12.947175
20.411175	844.070479	12.952179
20.559012	839.112557	12.957184
20.674339	840.250341	12.962189
20.241201	849.840216	12.967194
20.521573	841.385361	12.972199
20.415037	853.110497	12.977203
20.531498	845.129663	12.982208
20.485254	845.662402	12.987213
20.400256	849.416904	12.992218
20.631998	844.350976	12.997223
20.163367	844.826500	13.002227
20.395517	847.773438	13.007232
20.164306	853.552524	13.012237
20.319157	847.833348	13.017242
20.599998	847.299882	13.022247
20.520203	850.570980	13.027251
20.689007	849.609082	13.032256
20.262778	851.197540	13.037261
20.137778	851.435319	13.042266
20.130120	844.065672	13.047271
20.289044	844.505759	13.052275
20.591531	844.473493	13.057280
20.262721	852.610048	13.062285
20.517663	849.388707	13.067290
20.441245	842.610378	13.072295
20.323521	858.954871	13.077299
20.556128	852.578281	13.082304
20.766848	847.301227	13.087309
20.618325	851.114750	13.092314
20.920800	857.267634	13.097319
20.458960	844.985407	13.102323
20.351975	830.258957	13.107328
20.247849	823.533945	13.112333
20.147292	832.365827	13.117338
20.563638	832.468372	13.122343
20.283079	829.158974	13.127347
20.067863	825.501669	13.132352
20.349909	837.940715	13.137357
20.224852	846.896369	13.142362
20.542471	854.767385	13.147367
20.292063	858.802176	13.152371
20.281566	852.033829	13.157376
20.629850	855.370699	13.162381
20.281230	858.992200	13.167386
20.623360	854.389658	13.172391
20.324450	856.684825	13.177395
20.235079	848.568076	13.182400
20.733958	848.176461	13.187405
20.437152	831.251931	13.192410
20.470973	822.696055	13.197415
20.076701	828.895399	13.202419
20.343226	830.321319	13.207424
20.350732	844.371735	13.212429
20.284161	837.471983	13.217434
20.631351	840.000004	13.222439
20.190461	830.507382	13.227443
20.079766	837.434247	13.232448
20.212770	848.783686	13.237453
20.226881	861.459465	13.242458
20.528452	860.347072	13.247463
20.017871	861.490067	13.252467
20.614007	854.323747	13.257472
20.730984	854.193329	13.262477
20.556290	864.364923	13.267482
20.717228	851.888735	13.272487
20.425842	847.718419	13.277491
20.196804	832.938890	13.282496
20.326075	830.213863	13.287501
20.256699	827.564677	13.292506
20.638046	819.035379	13.297511
19.975994	840.033767	13.302515
20.301889	845.228802	13.307520
20.405698	860.117050	13.312525
20.107221	869.157151	13.317530
20.692051	860.623761	13.322535
20.450675	871.938310	13.327539
20.146166	859.287181	13.332544
20.285137	860.362845	13.337549
20.428523	859.682559	13.342554
20.722508	860.198881	13.347559
20.445866	858.352345	13.352563
20.533144	846.493493	13.357568
20.216380	832.678911	13.362573
20.127701	839.545492	13.367578
20.543504	846.637557	13.372583
20.116906	847.552679	13.377587
20.314473	853.570898	13.382592
20.477993	863.079808	13.387597
20.387609	871.296622	13.392602
20.603977	861.161377	13.397607
19.997027	850.465137	13.402611
20.270968	869.018107	13.407616
20.783854	867.135531	13.412621
20.314126	865.572117	13.417626
20.340970	849.089558	13.422631
20.531594	850.828801	13.427635
20.416752	845.540593	13.432640
20.272337	851.764753	13.437645
20.475670	852.744990	13.442650
20.350667	838.188572	13.447655
20.202587	849.966066	13.452659
20.705431	849.731522	13.457664
20.441427	841.068589	13.462669
20.330232	840.121387	13.467674
20.693310	842.008174	13.472679
20.393558	844.347630	13.477683
20.428151	844.487410	13.482688
20.159464	844.153563	13.487693
20.141588	847.332779	13.492698
20.286502	835.704453	13.497703
20.346594	849.003702	13.502707
20.126811	835.001752	13.507712
20.409587	853.733075	13.512717
20.336704	862.563716	13.517722
20.844229	862.637525	13.522727
20.333497	852.908433	13.527731
20.583213	844.040551	13.532736
20.409435	841.725000	13.537741
19.965487	841.799173	13.542746
20.164683	842.881000	13.547751
20.445911	855.326500	13.552755
20.132429	866.136854	13.557760
20.556838	871.287798	13.562765
20.542423	869.222806	13.567770
20.513180	855.095824	13.572775
20.436063	850.609041	13.577779
20.645070	845.460001	13.582784
20.643654	842.199122	13.587789
20.544548	837.733197	13.592794
20.617883	840.833205	13.597799
20.620414	845.155673	13.602803
20.508816	847.285337	13.607808
20.607795	846.061748	13.612813
20.392632	846.022155	13.617818
20.586622	842.662296	13.622823
20.586407	852.378674	13.627827
20.572718	846.747885	13.632832
20.622875	838.104234	13.637837
20.262527	838.530946	13.642842
20.455665	813.029639	13.647847
20.261749	817.796615	13.652851
20.412611	811.953502	13.657856
20.424382	823.241830	13.662861
19.997003	824.108187	13.667866
20.296188	835.243443	13.672871
20.429824	845.635519	13.677875
20.451386	847.020083	13.682880
20.657440	850.045305	13.687885
20.196815	838.390551	13.692890
20.423001	842.975405	13.697895
20.259767	839.483279	13.702899
20.304022	844.713773	13.707904
20.400007	845.559736	13.712909
20.374900	849.829840	13.717914
20.456398	850.427364	13.722919
20.324402	847.699849	13.727923
20.473490	848.245590	13.732928
20.637688	845.628536	13.737933
19.743279	840.087759	13.742938
20.073586	836.130539	13.747943
20.634817	851.019941	13.752947
20.354359	853.723771	13.757952
20.543444	841.761948	13.762957
20.435512	845.736162	13.767962
20.409746	846.071659	13.772967
20.322354	848.522332	13.777971
20.638037	850.692661	13.782976
20.681612	840.922476	13.787981
20.109172	833.434748	13.792986
20.387425	818.323573	13.797991
20.230259	826.601479	13.802995
20.023410	836.166291	13.808000
20.628737	844.669538	13.813005
20.572602	847.856434	13.818010
20.547471	841.063617	13.823015
20.305274	832.657422	13.828019
20.325816	826.954945	13.833024
20.240590	826.123456	13.838029
20.084384	831.715520	13.843034
20.392656	845.113960	13.848039
20.498400	854.603693	13.853043
20.575975	853.746236	13.858048
20.485995	846.552153	13.863053
20.036577	843.815340	13.868058
20.311364	842.588943	13.873063
20.452202	855.634031	13.878067
20.455247	849.311405	13.883072
20.560578	858.195624	13.888077
20.333283	851.875042	13.893082
20.547519	837.568885	13.898087
20.151895	831.018103	13.903091
20.395571	837.465800	13.908096
20.295086	846.188863	13.913101
20.192520	850.665297	13.918106
20.776117	848.933880	13.923111
20.343885	842.352660	13.928115
20.357828	833.085551	13.933120
20.330785	837.821185	13.938125
19.887282	844.621354	13.943130
20.751656	839.225852	13.948135
20.297644	848.380639	13.953139
20.490996	857.085229	13.958144
20.588070	845.182236	13.963149
20.502001	830.829361	13.968154
20.261319	823.828070	13.973159
20.247910	822.705992	13.978163
20.367590	830.812003	13.983168
20.378996	820.453997	13.988173
20.167070	826.611639	13.993178
20.391734	839.666999	13.998183
20.483381	847.086749	14.003187
20.508154	839.907484	14.008192
20.577661	834.082608	14.013210
20.153344	831.970299	14.018227
20.229176	827.314878	14.023245
20.422113	838.348895	14.028263
20.473178	855.230426	14.033280
20.664692	851.199910	14.038298
20.294314	851.004367	14.043315
20.690468	846.889302	14.048333
20.502432	839.803184	14.053351
20.495195	839.235118	14.058368
20.600004	841.109374	14.063386
20.523626	850.583454	14.068403
20.680554	843.604333	14.073421
20.253193	852.253507	14.078439
20.384164	856.308512	14.083456
20.599670	857.749839	14.088474
20.442527	865.358628	14.093491
20.594174	861.460309	14.098509
20.690682	857.459102	14.103527
20.467636	856.676919	14.108544
20.780209	859.883419	14.113562
20.852508	859.353002	14.118579
21.136194	852.205795	14.123597
20.794898	865.760071	14.128615
20.732767	869.638242	14.133632
20.890829	859.711097	14.138650
20.440930	866.834902	14.143667
20.716771	862.963965	14.148685
20.985011	864.458228	14.153703
20.671582	869.000968	14.158720
20.710256	864.063600	14.163738
20.339688	873.998322	14.168755
20.644017	865.093901	14.173773
20.976976	878.005819	14.178791
21.139794	881.783620	14.183808
21.191442	874.410718	14.188826
20.555372	879.465817	14.193843
20.873634	883.893650	14.198861
20.988108	896.955264	14.203879
21.297507	902.513946	14.208896
21.301822	894.281849	14.213914
21.077261	897.023472	14.218931
21.134275	892.589682	14.223949
20.996549	905.221196	14.228967
20.786510	903.180091	14.233984
21.174568	899.033270	14.239002
21.018095	903.167169	14.244019
20.928278	908.402565	14.249037
21.331117	897.851188	14.254055
21.024360	903.355563	14.259072
21.249977	899.318022	14.264090
21.308348	902.668895	14.269107
21.113633	897.090769	14.274125
21.399162	894.533323	14.279143
21.313651	899.393649	14.284160
21.394106	898.806875	14.289178
21.230247	901.829825	14.294195
21.386186	897.578456	14.299213
21.173169	888.978333	14.304231
21.510432	906.441911	14.309248
21.463215	896.335125	14.314266
21.376360	894.622012	14.319283
21.568196	893.795676	14.324301
21.466617	899.630692	14.329319
21.452012	897.924931	14.334336
21.683213	891.578879	14.339354
21.652129	906.230446	14.344371
21.478868	895.206244	14.349389
21.951916	901.289380	14.354407
21.334055	907.041579	14.359424
21.703067	898.542098	14.364442
21.561820	901.747059	14.369459
21.462712	905.067995	14.374477
22.022499	917.495459	14.379495
21.707359	927.087895	14.384512
21.708517	908.878605	14.389530
21.962854	914.221131	14.394547
21.691289	914.374767	14.399565
21.945066	913.184621	14.404583
21.548917	912.669144	14.409600
21.678752	909.837655	14.414618
21.908582	927.710076	14.419635
21.810378	928.432238	14.424653
21.888827	932.113397	14.429671
21.869393	936.494435	14.434688
22.314204	933.699219	14.439706
22.323952	928.307119	14.444723
21.939822	920.649770	14.449741
22.044176	904.763111	14.454759
22.165742	909.541649	14.459776
22.115340	912.870548	14.464794
21.856530	914.607757	14.469811
21.826855	912.363278	14.474829
21.966172	919.767508	14.479847
21.860605	939.025790	14.484864
22.531192	925.037100	14.489882
22.369086	936.473885	14.494899
21.775740	930.910564	14.499917
22.185832	935.205789	14.504935
22.100144	940.335144	14.509952
22.375013	933.019418	14.514970
22.527305	944.137076	14.519987
22.271294	940.402858	14.525005
22.478732	936.851125	14.530023
22.312052	947.837190	14.535040
22.642300	923.039470	14.540058
22.292763	922.011618	14.545075
22.261407	918.623818	14.550093
22.402682	910.761550	14.555111
22.262059	921.630182	14.560128
22.240054	933.596751	14.565146
22.474238	937.492171	14.570163
22.673530	943.823483	14.575181
22.593444	929.392950	14.580199
22.202612	929.428756	14.585216
22.346316	935.106687	14.590234
22.240946	931.924171	14.595251
22.073351	950.448321	14.600269
22.807785	939.359533	14.605287
22.389619	946.368203	14.610304
22.569562	941.422434	14.615322
22.568438	941.432261	14.620339
22.497423	937.858873	14.625357
22.954811	936.922540	14.630375
22.433350	949.137097	14.635392
22.409491	945.461805	14.640410
22.516932	943.349608	14.645427
22.500974	949.844242	14.650445
22.521001	946.097455	14.655463
22.383636	952.029436	14.660480
22.585160	967.279466	14.665498
22.659148	965.419567	14.670515
22.582455	974.140296	14.675533
22.746990	967.938552	14.680551
22.619695	983.214304	14.685568
22.986531	971.866371	14.690586
23.588810	971.586474	14.695603
22.983077	971.253862	14.700621
23.207350	966.796517	14.705639
23.104253	977.390218	14.710656
23.363106	969.743545	14.715674
23.274982	974.871728	14.720691
22.935402	975.976885	14.725709
23.399836	968.055177	14.730727
23.173193	971.486132	14.735744
23.142109	956.615174	14.740762
22.923204	956.931871	14.745779
23.214535	970.190285	14.750797
23.145677	970.730016	14.755815
23.253779	976.228024	14.760832
23.230157	970.962354	14.765850
23.364468	979.803589	14.770867
23.324472	979.665460	14.775885
23.578269	973.529701	14.780903
23.362870	957.462750	14.785920
23.129817	950.923306	14.790938
23.151480	952.080955	14.795955
23.068775	964.990035	14.800973
23.331078	959.496294	14.805991
23.581952	965.169727	14.811008
23.538853	970.962411	14.816026
23.491392	973.524790	14.821043
23.237517	972.701900	14.826061
23.762249	973.060437	14.831079
23.379765	976.434453	14.836096
23.454451	974.749047	14.841114
23.453254	972.408781	14.846131
23.522452	971.657058	14.851149
23.421046	966.158404	14.856167
23.644372	966.827710	14.861184
23.508116	972.306490	14.866202
23.504758	969.551289	14.871219
23.185473	976.806898	14.876237
23.237407	973.921754	14.881255
23.331807	976.809147	14.886272
23.223049	987.369151	14.891290
23.575871	998.487900	14.896307
23.700211	1000.294568	14.901325
23.593138	1004.610953	14.906343
23.601819	1004.526408	14.911360
23.951575	995.688595	14.916378
24.200208	996.149373	14.921395
23.872388	999.113552	14.926413
24.270236	998.597273	14.931431
24.536165	994.993724	14.936448
23.887239	994.903954	14.941466
24.037992	984.984182	14.946483
23.674087	990.958603	14.951501
24.286507	985.158897	14.956519
24.413676	993.751168	14.961536
24.204902	975.024718	14.966554
24.149945	966.803607	14.971571
23.867791	963.311079	14.976589
24.211996	961.656620	14.981607
23.944660	970.156070	14.986624
23.903083	961.342942	14.991642
24.555053	976.805856	14.996659
23.986905	973.643660	15.001677
24.287183	990.572117	15.006695
24.290150	989.302417	15.011712
24.324777	986.808570	15.016730
24.053168	988.250526	15.021747
24.375978	995.641259	15.026765
24.602439	992.792768	15.031783
24.205056	986.756147	15.036800
24.313987	1000.839635	15.041818
24.719428	998.662597	15.046835
24.125523	996.391694	15.051853
24.158194	985.789183	15.056871
24.402683	1002.369474	15.061888
24.423294	1005.120776	15.066906
24.669244	999.805808	15.071923
24.302959	998.313430	15.076941
24.323655	999.705619	15.081959
24.468355	997.727471	15.086976
24.571752	1000.514332	15.091994
24.674471	999.409621	15.097011
24.453311	994.529382	15.102029
24.405331	999.106902	15.107047
24.248109	994.529498	15.112064
24.215740	1002.516435	15.117082
24.792976	1004.515137	15.122099
24.629434	1023.043451	15.127117
24.581210	1021.840116	15.132135
24.716053	1026.187136	15.137152
24.906867	1036.756024	15.142170
24.939498	1029.906752	15.147187
24.954077	1023.345082	15.152205
24.960910	1030.979714	15.157223
24.746169	1021.292819	15.162240
25.005132	1028.245438	15.167258
25.248216	1022.355187	15.172275
24.994439	1023.838347	15.177293
24.924167	1006.837407	15.182311
24.922223	1005.628265	15.187328
25.118151	1014.601266	15.192346
25.244678	1010.636128	15.197363
24.937163	1007.433927	15.202381
25.373481	1008.910837	15.207399
25.200854	1005.529819	15.212416
25.198597	1004.795783	15.217434
25.230436	996.685080	15.222451
25.198131	998.425497	15.227469
25.153938	997.263993	15.232487
25.451005	995.689408	15.237504
25.052178	1005.367603	15.242522
25.113217	999.758082	15.247539
25.170397	1007.376806	15.252557
25.434473	1009.043211	15.257575
25.198357	1007.139958	15.262592
24.984773	1027.681877	15.267610
25.508542	1031.968439	15.272627
25.241236	1031.808362	15.277645
25.597707	1034.946551	15.282663
25.514899	1035.708734	15.287680
25.464819	1034.856482	15.292698
25.454814	1040.941218	15.297715
25.492076	1034.454577	15.302733
25.698643	1040.839827	15.307751
25.941339	1033.079294	15.312768
25.477509	1039.145178	15.317786
25.831055	1028.263367	15.322803
25.531065	1030.878618	15.327821
25.300037	1031.107587	15.332839
25.601613	1033.771610	15.337856
25.564092	1039.723881	15.342874
25.537880	1031.001069	15.347891
25.438627	1038.227905	15.352909
25.514845	1040.372592	15.357927
25.531403	1028.352168	15.362944
25.305526	1035.537851	15.367962
25.664962	1037.873320	15.372979
25.827488	1056.862480	15.377997
25.863057	1055.401957	15.383015
25.943222	1065.098174	15.388032
25.964341	1058.467804	15.393050
26.081105	1056.995904	15.398067
25.916771	1058.271317	15.403085
26.115596	1059.164762	15.408103
26.253551	1048.957548	15.413120
25.852949	1053.940542	15.418138
26.158220	1048.548454	15.423155
26.371221	1052.566835	15.428173
25.848546	1053.071985	15.433191
26.305672	1047.627362	15.438208
26.307939	1049.879800	15.443226
26.283931	1047.657992	15.448243
26.213069	1040.159827	15.453261
25.924457	1042.757535	15.458279
26.231655	1049.206964	15.463296
25.971457	1056.726896	15.468314
26.497885	1053.300437	15.473331
26.422923	1063.085890	15.478349
26.302558	1059.245061	15.483367
26.617252	1058.027884	15.488384
26.215157	1066.501692	15.493402
26.295017	1061.900611	15.498419
26.438947	1062.321461	15.503437
26.441745	1060.079645	15.508455
26.196382	1053.732455	15.513472
26.150981	1058.092503	15.518490
26.402916	1051.094984	15.523507
26.442405	1055.995200	15.528525
26.338799	1068.586807	15.533543
26.920077	1059.554725	15.538560
26.665545	1062.176888	15.543578
26.311656	1060.347470	15.548595
26.564119	1063.621805	15.553613
26.479969	1063.956337	15.558631
26.744657	1084.381154	15.563648
26.544344	1087.273102	15.568666
26.996949	1092.371711	15.573683
27.101762	1089.327098	15.578701
26.651482	1078.546717	15.583719
27.018247	1072.243460	15.588736
27.002351	1087.254586	15.593754
26.595312	1084.765098	15.598771
26.796570	1078.285314	15.603789
26.766749	1092.251021	15.608807
27.083950	1084.777456	15.613824
27.012752	1090.090172	15.618842
26.935773	1086.939273	15.623859
27.390040	1087.062086	15.628877
27.281575	1082.412383	15.633895
27.538438	1080.252739	15.638912
27.156514	1074.152266	15.643930
26.733743	1062.285257	15.648947
27.208595	1064.430860	15.653965
27.230486	1089.846338	15.658983
27.254445	1083.833708	15.664000
27.425735	1084.627726	15.669018
27.132417	1080.819196	15.674035
27.201826	1088.362079	15.679053
27.260528	1091.215863	15.684071
27.225730	1086.891039	15.689088
27.425059	1088.254745	15.694106
27.033930	1080.109211	15.699123
27.288588	1083.749719	15.704141
26.975872	1092.111758	15.709159
27.633972	1083.548759	15.714176
27.092712	1086.372390	15.719194
27.415661	1084.950972	15.724211
27.501892	1079.307515	15.729229
27.295779	1088.525587	15.734247
27.629225	1085.963612	15.739264
27.619481	1079.350739	15.744282
27.775858	1085.519070	15.749299
27.700795	1075.773681	15.754317
27.495380	1082.702864	15.759335
27.716242	1078.505582	15.764352
27.454005	1089.110589	15.769370
27.753324	1096.431187	15.774387
28.070060	1105.657113	15.779405
27.861740	1097.304658	15.784423
27.999702	1082.169079	15.789440
27.799486	1084.911572	15.794458
27.832781	1081.975897	15.799475
27.752943	1083.156037	15.804493
27.934867	1105.972523	15.809511
27.910872	1108.650735	15.814528
28.120780	1113.670082	15.819546
28.164203	1111.380880	15.824563
28.522342	1100.930870	15.829581
28.090672	1101.311392	15.834599
27.693018	1082.138298	15.839616
27.684028	1092.835051	15.844634
27.990445	1099.243727	15.849651
28.147718	1102.824267	15.854669
28.087492	1113.653478	15.859687
28.352895	1104.707929	15.864704
28.315128	1113.491747	15.869722
28.490208	1118.384516	15.874739
28.456431	1112.511646	15.879757
28.001403	1117.530084	15.884775
28.482376	1107.949247	15.889792
28.696463	1101.715948	15.894810
28.201979	1095.167798	15.899827
28.212852	1107.753764	15.904845
28.117913	1112.131167	15.909863
28.432564	1110.986353	15.914880
28.238037	1105.107664	15.919898
28.439326	1110.885020	15.924915
28.387249	1110.597804	15.929933
28.042467	1115.875512	15.934951
28.221505	1113.541084	15.939968
28.261595	1129.833220	15.944986
28.553601	1138.396140	15.950003
28.616159	1126.797740	15.955021
28.484257	1147.816017	15.960039
28.640929	1144.926719	15.965056
28.896173	1145.222850	15.970074
28.553366	1147.506746	15.975091
29.080242	1129.883447	15.980109
28.697383	1133.804978	15.985127
29.200806	1138.186054	15.990144
29.051628	1134.944413	15.995162
29.266315	1140.104582	16.000179
29.528763	1128.258791	16.005197
29.028755	1126.385028	16.010215
29.239331	1097.179550	16.015232
28.731645	1103.250881	16.020250
28.860268	1102.266301	16.025267
29.174545	1107.840015	16.030285
29.227865	1124.999930	16.035303
28.992803	1119.030172	16.040320
29.375260	1120.943553	16.045338
28.737550	1122.275597	16.050355
29.330899	1119.571488	16.055373
29.174034	1141.507677	16.060391
29.112691	1128.195540	16.065408
29.490462	1132.289912	16.070426
28.967359	1134.654472	16.075443
29.499979	1121.862667	16.080461
29.263047	1132.256027	16.085479
29.436476	1131.042499	16.090496
29.301789	1129.215862	16.095514
29.442113	1132.646528	16.100531
29.592811	1122.817908	16.105549
29.495200	1126.322701	16.110567
29.733897	1128.320361	16.115584
29.572159	1130.575374	16.120602
29.448631	1136.445447	16.125619
29.552702	1134.525671	16.130637
29.572393	1138.672438	16.135655
29.466351	1137.728430	16.140672
29.415748	1145.048235	16.145690
29.227551	1135.728270	16.150707
29.697165	1131.061856	16.155725
29.292280	1138.828279	16.160743
29.419029	1144.373715	16.165760
29.912236	1154.397376	16.170778
29.889157	1167.989268	16.175795
30.299500	1158.410226	16.180813
30.199341	1163.313875	16.185831
29.806839	1148.626209	16.190848
30.057006	1136.936529	16.195866
29.673953	1141.147533	16.200883
30.164372	1145.554281	16.205901
29.934991	1158.037036	16.210919
30.219560	1160.651885	16.215936
30.492447	1160.054857	16.220954
29.881974	1155.785651	16.225971
30.097255	1146.517731	16.230989
29.900339	1152.866710	16.236007
30.100839	1158.612750	16.241024
30.446669	1154.518212	16.246042
30.320574	1166.735959	16.251059
30.531076	1165.939665	16.256077
30.417997	1164.586212	16.261095
30.070588	1151.694065	16.266112
30.113915	1147.090918	16.271130
30.145484	1160.302848	16.276147
30.368322	1158.036932	16.281165
30.431203	1163.172558	16.286183
30.513019	1169.142028	16.291200
30.700396	1167.709191	16.296218
30.333620	1157.096333	16.301235
30.301421	1154.982781	16.306253
30.241849	1168.509707	16.311271
30.585369	1167.917144	16.316288
30.486750	1156.956344	16.321306
30.420127	1165.175352	16.326323
30.861954	1173.091469	16.331341
30.595841	1167.417658	16.336359
30.540961	1163.995800	16.341376
30.805163	1159.335397	16.346394
30.800665	1161.996351	16.351411
30.858803	1164.477426	16.356429
30.920992	1165.740315	16.361447
31.139506	1156.497042	16.366464
31.132467	1163.007653	16.371482
30.801276	1161.213926	16.376499
31.056252	1160.692116	16.381517
30.972613	1160.247909	16.386535
30.932200	1166.889688	16.391552
30.748951	1153.758995	16.396570
30.893158	1182.062119	16.401587
31.360730	1191.569214	16.406605
31.433162	1198.226044	16.411623
31.108496	1191.465144	16.416640
31.617457	1194.849613	16.421658
31.408851	1177.082437	16.426675
31.166547	1164.856219	16.431693
31.104002	1161.975139	16.436711
31.070604	1157.988277	16.441728
31.254761	1173.736806	16.446746
31.483529	1172.330402	16.451763
31.674192	1179.452865	16.456781
31.320890	1179.174365	16.461799
31.321727	1193.435733	16.466816
31.725170	1196.775683	16.471834
31.354335	1186.157158	16.476851
31.529277	1192.497182	16.481869
31.641067	1193.646767	16.486887
31.466498	1191.966485	16.491904
31.675183	1189.005960	16.496922
31.782015	1196.437536	16.501939
31.489260	1184.381373	16.506957
31.822430	1188.402649	16.511975
31.428009	1193.837742	16.516992
31.735985	1184.364675	16.522010
31.734891	1183.098752	16.527027
31.572661	1191.016841	16.532045
31.921284	1188.847265	16.537063
31.756527	1191.982105	16.542080
31.989672	1188.866665	16.547098
31.727925	1187.645462	16.552115
31.913930	1185.833737	16.557133
32.018424	1194.349518	16.562151
31.805403	1196.801487	16.567168
31.902901	1181.470908	16.572186
31.937430	1192.659450	16.577203
31.737767	1188.404938	16.582221
32.041442	1198.981113	16.587239
32.219643	1208.993705	16.592256
32.310960	1207.950573	16.597274
32.326133	1218.942445	16.602291
32.354531	1219.737238	16.607309
32.454346	1216.890028	16.612327
32.327638	1222.652101	16.617344
32.571536	1214.317115	16.622362
32.460216	1205.374961	16.627379
32.483521	1199.124857	16.632397
32.390428	1197.011574	16.637415
32.479251	1204.667827	16.642432
32.707429	1202.928027	16.647450
32.404568	1201.260340	16.652467
32.463059	1210.588871	16.657485
32.373118	1211.080062	16.662503
32.226474	1215.064614	16.667520
32.679476	1207.289323	16.672538
32.761696	1218.799048	16.677555
32.675333	1208.948404	16.682573
32.623106	1218.727189	16.687591
32.386207	1215.530982	16.692608
32.576789	1217.857232	16.697626
32.536484	1216.953072	16.702643
32.481164	1211.734843	16.707661
32.894051	1224.145103	16.712679
32.856829	1245.634495	16.717696
32.968284	1236.222626	16.722714
33.253983	1237.133688	16.727731
33.130749	1242.552288	16.732749
33.198060	1229.905391	16.737767
32.805179	1217.009427	16.742784
33.296359	1223.970721	16.747802
33.273538	1238.402650	16.752819
33.209896	1232.260783	16.757837
33.484014	1211.355405	16.762855
33.175826	1214.064805	16.767872
32.914779	1203.169203	16.772890
33.195724	1216.204553	16.777907
33.432089	1227.895770	16.782925
33.606219	1225.628175	16.787943
33.252903	1231.514486	16.792960
32.926382	1227.557052	16.797978
33.343369	1241.138601	16.802995
33.152633	1233.195403	16.808013
33.363795	1238.787188	16.813031
33.208134	1244.130735	16.818048
33.481380	1233.156185	16.823066
33.352383	1236.234993	16.828083
33.330294	1244.635710	16.833101
33.233334	1237.308349	16.838119
33.418208	1258.126821	16.843136
34.018692	1256.944273	16.848154
33.759766	1257.594555	16.853171
33.630728	1269.345658	16.858189
34.170396	1259.434458	16.863207
33.709571	1265.827151	16.868224
33.869563	1264.066757	16.873242
33.759710	1261.512534	16.878259
33.647017	1254.648581	16.883277
34.163612	1262.474170	16.888295
33.920780	1267.034087	16.893312
34.043538	1263.870169	16.898330
34.031759	1264.031137	16.903347
34.000113	1265.999575	16.908365
34.385804	1256.882161	16.913383
33.932157	1267.160741	16.918400
34.294048	1257.199244	16.923418
34.193227	1256.951260	16.928435
34.252362	1253.001524	16.933453
34.440059	1262.164760	16.938471
34.260502	1258.194890	16.943488
34.428759	1250.063861	16.948506
34.383210	1254.644220	16.953523
34.294255	1261.021645	16.958541
34.464299	1251.413227	16.963559
34.044033	1261.551196	16.968576
34.193972	1255.340647	16.973594
34.336160	1259.644094	16.978611
34.018769	1268.914634	16.983629
34.397371	1284.070687	16.988647
34.499483	1291.278117	16.993664
34.865091	1283.066829	16.998682
34.819121	1290.746199	17.003699
34.717986	1289.743195	17.008717
34.953394	1284.436098	17.013735
35.106099	1288.797652	17.018752
34.634716	1291.500061	17.023770
34.966251	1285.707285	17.028787
35.175603	1290.355541	17.033805
35.222736	1286.138717	17.038823
34.912239	1292.342273	17.043840
35.255091	1281.705805	17.048858
34.911149	1274.612878	17.053875
34.780427	1274.152581	17.058893
35.016195	1284.292900	17.063911
34.720449	1289.059469	17.068928
34.764142	1288.824616	17.073946
34.933069	1287.061222	17.078963
34.629046	1285.915967	17.083981
35.483517	1284.963474	17.088999
35.085112	1290.268674	17.094016
35.259444	1284.007030	17.099034
34.861958	1285.459652	17.104051
34.809909	1294.967893	17.109069
35.257715	1303.688538	17.114087
35.459100	1310.567104	17.119104
35.389823	1310.501283	17.124122
35.477362	1313.954568	17.129139
35.335988	1318.561242	17.134157
35.778595	1306.867475	17.139175
35.703597	1315.470159	17.144192
35.529630	1314.099660	17.149210
35.734962	1311.306390	17.154227
35.649771	1311.979303	17.159245
35.852995	1307.460717	17.164263
35.918846	1309.330238	17.169280
35.530616	1317.668268	17.174298
35.742649	1308.413348	17.179315
35.619933	1313.043786	17.184333
35.673587	1307.559597	17.189351
35.790616	1316.768746	17.194368
35.709635	1312.293915	17.199386
35.938508	1319.350576	17.204403
36.029423	1343.523777	17.209421
36.141406	1343.156906	17.214439
35.989012	1349.697076	17.219456
36.123969	1348.966306	17.224474
36.146519	1343.861456	17.229491
35.951421	1349.901908	17.234509
36.408043	1345.272108	17.239527
36.363293	1342.488830	17.244544
36.319115	1341.300554	17.249562
36.336544	1346.415179	17.254579
36.392284	1345.151189	17.259597
36.708726	1332.708294	17.264615
36.580976	1331.432672	17.269632
36.569919	1337.881079	17.274650
36.709404	1333.981429	17.279667
36.351062	1341.318953	17.284685
36.681653	1336.964094	17.289703
36.440603	1335.126079	17.294720
36.480598	1333.114249	17.299738
36.810855	1331.726250	17.304755
36.321561	1343.103851	17.309773
36.627112	1341.011911	17.314791
37.023024	1332.411933	17.319808
36.596522	1338.454681	17.324826
36.722772	1333.695100	17.329843
36.593975	1336.465576	17.334861
37.008988	1335.831717	17.339879
37.019753	1338.740387	17.344896
36.960610	1335.621196	17.349914
36.916973	1331.152988	17.354931
37.087069	1327.621274	17.359949
37.113950	1330.717713	17.364967
37.102343	1334.307943	17.369984
37.199813	1336.247931	17.375002
37.169513	1330.025198	17.380019
36.876234	1334.737903	17.385037
36.980175	1331.794056	17.390055
37.216239	1342.720903	17.395072
37.257806	1350.630169	17.400090
37.591079	1354.516192	17.405107
37.431208	1357.620400	17.410125
37.341170	1341.031219	17.415143
37.626911	1351.734639	17.420160
37.421231	1346.741696	17.425178
37.455128	1350.277479	17.430195
37.527431	1357.135756	17.435213
37.773790	1357.386118	17.440231
37.855525	1351.183261	17.445248
37.653804	1356.183400	17.450266
37.862644	1348.080452	17.455283
37.678901	1347.985695	17.460301
37.643989	1352.441689	17.465319
38.097191	1355.460699	17.470336
37.555918	1358.241909	17.475354
37.860941	1345.882623	17.480371
37.850815	1359.530832	17.485389
37.796294	1353.099587	17.490407
38.018374	1355.691405	17.495424
37.863669	1363.268603	17.500442
38.114693	1353.991704	17.505459
38.039169	1360.930190	17.510477
37.868624	1351.909299	17.515495
38.190896	1355.243357	17.520512
37.996026	1354.783849	17.525530
38.029570	1353.935544	17.530547
38.120025	1362.815469	17.535565
38.187537	1354.788543	17.540583
38.337733	1362.957351	17.545600
38.050347	1358.737228	17.550618
38.374532	1364.093952	17.555635
38.469943	1377.767032	17.560653
38.622861	1384.273466	17.565671
38.584040	1386.039351	17.570688
38.516116	1382.691882	17.575706
38.669766	1384.398754	17.580723
38.585021	1393.003824	17.585741
38.786094	1384.369609	17.590759
38.919160	1391.429789	17.595776
38.561298	1395.571564	17.600794
38.875473	1387.801016	17.605811
38.650595	1389.749951	17.610829
38.625104	1391.001674	17.615847
38.857888	1387.219268	17.620864
38.718175	1390.534205	17.625882
38.785216	1375.838296	17.630899
38.728401	1386.414687	17.635917
38.729576	1389.091295	17.640935
39.017080	1395.898749	17.645952
38.616379	1389.904172	17.650970
39.006382	1385.345548	17.655987
39.047055	1379.846885	17.661005
38.445046	1389.760664	17.666023
39.311490	1398.999781	17.671040
39.482488	1415.019667	17.676058
39.671071	1415.469588	17.681075
39.561682	1417.125604	17.686093
39.465541	1411.010081	17.691111
39.631789	1402.242193	17.696128
39.252978	1402.446757	17.701146
39.776324	1403.765895	17.706163
39.496849	1408.468557	17.711181
39.461297	1401.590657	17.716199
39.777113	1404.869125	17.721216
39.492814	1410.731128	17.726234
39.683479	1401.874399	17.731251
39.674442	1412.642183	17.736269
39.864738	1411.727187	17.741287
40.147678	1416.841176	17.746304
39.848210	1421.079827	17.751322
40.236938	1407.386541	17.756339
40.053933	1388.944892	17.761357
39.551277	1386.103287	17.766375
39.911535	1381.098722	17.771392
39.772699	1401.535648	17.776410
39.698378	1405.419838	17.781427
39.973172	1411.803023	17.786445
39.722237	1404.017988	17.791463
40.075726	1398.198858	17.796480
40.046403	1405.255842	17.801498
39.726324	1405.046759	17.806515
39.897523	1407.230622	17.811533
40.101414	1434.927738	17.816551
40.631936	1440.141465	17.821568
40.443483	1441.027488	17.826586
40.596023	1440.728080	17.831603
40.655861	1434.486993	17.836621
40.575162	1445.572194	17.841639
40.370859	1438.486803	17.846656
40.221210	1440.859489	17.851674
40.308834	1438.038563	17.856691
40.490751	1442.437192	17.861709
40.506225	1440.673085	17.866727
40.826494	1439.670502	17.871744
40.320139	1449.809745	17.876762
40.333158	1444.383111	17.881779
40.440776	1444.484138	17.886797
40.587910	1460.988457	17.891815
41.025102	1462.446401	17.896832
40.686370	1473.271533	17.901850
40.607692	1470.223072	17.906867
40.733776	1459.569137	17.911885
40.871639	1472.896537	17.916903
40.878212	1462.473240	17.921920
41.400443	1464.262126	17.926938
41.197961	1458.105340	17.931955
41.170811	1456.948946	17.936973
41.108421	1471.049204	17.941991
41.254913	1468.842611	17.947008
41.498035	1459.246785	17.952026
41.240754	1452.461643	17.957043
41.604764	1463.921899	17.962061
41.428726	1463.217916	17.967079
41.707196	1464.037335	17.972096
41.705241	1466.535125	17.977114
41.520100	1456.249379	17.982131
41.656581	1464.290653	17.987149
41.624739	1464.092227	17.992167
41.715674	1457.484361	17.997184
41.465827	1460.350461	18.002202
41.477106	1471.092239	18.007219
41.558388	1477.880711	18.012237
41.667460	1497.925862	18.017255
42.010587	1489.358594	18.022272
41.925808	1485.710185	18.027290
42.129320	1488.150826	18.032307
42.158231	1486.940655	18.037325
41.739387	1491.198366	18.042343
42.092653	1483.262652	18.047360
41.680426	1493.487590	18.052378
42.109539	1493.658470	18.057395
42.098359	1487.989491	18.062413
42.401880	1488.992900	18.067431
42.268707	1484.851968	18.072448
42.201984	1489.524656	18.077466
42.294098	1486.051748	18.082483
42.382698	1481.753532	18.087501
41.715010	1493.969053	18.092519
42.602059	1501.546919	18.097536
42.564848	1510.713148	18.102554
42.738282	1515.668452	18.107571
42.635832	1510.497746	18.112589
42.960977	1516.876880	18.117607
42.953011	1508.798984	18.122624
42.790738	1492.155867	18.127642
42.774831	1488.727716	18.132659
42.742668	1484.094816	18.137677
42.695925	1488.020249	18.142695
43.167344	1488.069545	18.147712
42.845334	1487.084450	18.152730
42.695934	1487.844692	18.157747
43.097588	1500.098888	18.162765
42.857063	1507.289497	18.167783
42.931889	1510.327989	18.172800
43.246732	1510.174161	18.177818
42.967580	1509.455159	18.182835
43.411503	1498.265206	18.187853
43.127168	1506.629246	18.192871
43.165258	1498.895594	18.197888
43.294745	1506.462934	18.202906
43.171752	1517.654041	18.207923
43.608590	1506.127784	18.212941
43.466352	1510.799939	18.217959
43.593432	1506.022079	18.222976
43.443237	1500.605725	18.227994
43.590639	1511.786736	18.233011
43.542104	1511.044324	18.238029
43.348502	1509.882226	18.243047
43.645442	1502.407747	18.248064
43.779238	1505.907973	18.253082
43.474637	1510.529728	18.258099
43.945858	1507.192200	18.263117
43.756860	1503.975703	18.268135
43.879249	1496.463784	18.273152
43.842351	1502.694580	18.278170
44.129007	1499.729423	18.283187
44.015288	1509.172133	18.288205
43.899025	1523.697902	18.293223
43.781781	1516.335095	18.298240
44.086694	1529.998501	18.303258
43.991125	1543.927149	18.308275
44.314918	1558.510975	18.313293
44.412685	1556.318433	18.318311
44.320850	1530.142115	18.323328
44.607339	1531.123074	18.328346
44.271528	1532.587904	18.333363
44.578575	1522.105630	18.338381
44.235803	1535.348502	18.343399
44.216404	1519.987445	18.348416
44.531748	1523.999076	18.353434
44.207803	1529.630699	18.358451
44.480666	1525.420277	18.363469
44.489115	1520.768303	18.368487
44.304090	1525.061879	18.373504
44.516078	1525.736956	18.378522
44.660824	1548.326464	18.383539
44.907118	1551.157499	18.388557
44.975175	1557.071118	18.393575
44.801642	1557.485986	18.398592
44.737982	1551.363650	18.403610
44.808868	1565.294873	18.408627
45.142569	1550.107140	18.413645
44.944584	1560.504030	18.418663
44.865014	1555.111786	18.423680
45.110436	1549.420735	18.428698
45.076257	1557.683556	18.433715
45.285148	1551.980240	18.438733
44.987177	1551.473459	18.443751
45.054086	1557.897730	18.448768
45.489210	1571.121179	18.453786
45.446617	1584.751181	18.458803
45.504377	1581.661272	18.463821
45.817022	1588.537171	18.468839
45.844450	1569.890261	18.473856
45.559145	1563.724616	18.478874
45.263333	1555.024038	18.483891
45.604853	1564.898353	18.488909
45.424706	1576.564255	18.493927
45.671883	1587.900093	18.498944
45.910272	1576.874214	18.503962
45.772073	1586.494704	18.508979
45.835409	1584.800815	18.513997
46.008656	1582.663086	18.519015
45.992429	1585.870280	18.524032
46.156674	1586.299705	18.529050
45.951054	1591.038626	18.534067
46.238869	1603.549389	18.539085
46.105008	1605.367426	18.544103
45.977619	1603.530912	18.549120
46.367690	1593.979991	18.554138
46.135488	1600.854699	18.559155
46.064054	1588.055006	18.564173
46.210595	1590.702961	18.569191
46.393561	1588.603796	18.574208
46.490060	1595.717100	18.579226
46.390108	1611.363546	18.584243
46.466193	1608.805563	18.589261
46.637070	1612.722277	18.594279
46.282094	1619.841528	18.599296
46.204270	1609.341920	18.604314
46.538224	1613.461511	18.609331
46.776082	1615.544322	18.614349
46.554280	1612.812827	18.619367
46.598725	1601.601560	18.624384
46.976311	1609.738961	18.629402
47.130486	1632.810038	18.634419
47.508517	1623.051795	18.639437
47.178741	1621.514197	18.644455
46.885922	1616.885072	18.649472
46.901676	1609.775512	18.654490
46.952910	1617.806083	18.659507
46.864950	1626.355172	18.664525
47.160005	1637.740045	18.669543
47.447324	1644.855188	18.674560
47.267794	1640.818350	18.679578
46.948255	1644.685081	18.684595
47.102724	1643.934669	18.689613
47.092776	1637.629903	18.694631
47.043763	1642.530275	18.699648
47.755358	1656.405018	18.704666
47.381888	1666.934583	18.709683
47.648125	1658.010589	18.714701
47.645792	1664.772370	18.719719
47.613576	1668.830034	18.724736
47.908738	1667.753573	18.729754
47.879736	1663.249106	18.734771
48.046464	1658.689827	18.739789
48.214312	1661.047306	18.744807
47.762446	1664.865930	18.749824
48.073413	1655.837270	18.754842
47.965617	1655.069694	18.759859
47.924706	1658.767715	18.764877
48.110737	1660.639351	18.769895
48.103918	1660.665032	18.774912
48.472666	1653.903439	18.779930
47.937608	1669.351127	18.784947
48.266839	1658.486100	18.789965
48.230783	1662.210091	18.794983
47.962450	1668.459778	18.800000
48.402996	1673.483439	18.805018
48.635017	1689.337372	18.810035
48.888011	1688.178753	18.815053
48.859305	1678.305224	18.820071
48.747529	1670.032211	18.825088
48.933873	1652.978575	18.830106
48.572824	1656.988003	18.835123
48.734166	1658.129723	18.840141
48.846111	1673.831322	18.845159
48.713667	1688.260730	18.850176
48.903786	1682.711375	18.855194
48.789547	1683.093193	18.860211
49.096873	1686.965355	18.865229
48.975518	1685.824754	18.870247
49.002546	1689.931967	18.875264
49.020972	1682.464849	18.880282
48.955595	1682.632011	18.885299
49.243849	1680.952577	18.890317
49.394823	1676.888974	18.895335
48.765053	1680.815418	18.900352
49.390612	1679.882113	18.905370
49.297597	1701.007462	18.910387
49.538464	1708.382530	18.915405
49.736328	1698.481503	18.920423
49.608784	1711.639082	18.925440
49.923330	1703.344464	18.930458
49.905000	1712.198693	18.935475
49.715938	1709.065534	18.940493
50.097468	1702.628300	18.945511
50.096562	1707.228423	18.950528
49.624028	1686.988888	18.955546
49.749077	1693.908915	18.960563
49.806721	1708.222291	18.965581
50.078916	1707.503440	18.970599
49.601608	1701.878044	18.975616
50.100121	1702.743399	18.980634
49.903067	1709.258603	18.985651
49.839498	1706.685121	18.990669
50.293705	1697.171096	18.995687
50.107417	1703.367600	19.000704
50.196366	1702.238290	19.005722
50.185041	1710.321364	19.010739
50.272970	1732.884039	19.015757
50.657835	1731.239532	19.020775
50.429427	1745.888020	19.025792
50.846785	1730.692263	19.030810
50.997420	1735.756678	19.035827
50.885807	1739.539145	19.040845
50.805193	1709.885710	19.045863
50.476957	1718.306425	19.050880
51.058944	1721.886240	19.055898
50.977814	1736.076264	19.060915
51.157993	1734.519460	19.065933
50.808231	1721.417955	19.070951
50.760615	1731.583334	19.075968
50.883691	1729.190878	19.080986
50.978304	1733.015176	19.086003
50.775022	1737.890631	19.091021
51.266007	1725.561145	19.096039
50.953403	1733.671832	19.101056
50.827598	1734.350454	19.106074
50.660747	1739.392355	19.111091
51.188449	1748.942930	19.116109
51.622190	1755.680826	19.121127
51.351670	1767.694794	19.126144
51.923698	1766.684287	19.131162
51.655093	1764.723189	19.136179
51.408462	1761.456833	19.141197
51.720333	1759.682384	19.146215
51.822930	1766.174206	19.151232
51.780350	1761.326575	19.156250
51.813763	1758.220062	19.161267
51.616579	1768.619332	19.166285
51.563986	1759.257673	19.171303
51.830739	1771.708230	19.176320
52.006112	1765.130806	19.181338
52.038132	1780.130286	19.186355
52.138930	1793.039149	19.191373
52.524686	1785.131127	19.196391
52.209855	1795.381643	19.201408
52.311210	1791.451771	19.206426
52.718128	1785.930726	19.211443
52.233430	1790.258015	19.216461
52.406594	1787.028528	19.221479
52.322879	1798.983626	19.226496
52.323892	1792.062742	19.231514
52.546525	1796.314191	19.236531
52.572046	1794.093021	19.241549
52.785765	1788.473792	19.246567
52.487756	1794.150146	19.251584
52.497927	1793.041259	19.256602
52.671229	1787.142169	19.261619
52.545792	1789.720273	19.266637
52.818324	1793.418678	19.271655
52.894499	1815.338378	19.276672
53.164812	1815.017821	19.281690
52.908485	1817.826817	19.286707
52.950904	1818.300850	19.291725
53.380815	1817.316152	19.296743
53.088911	1818.662315	19.301760
53.417771	1814.530189	19.306778
53.246854	1822.037059	19.311795
53.194509	1823.370972	19.316813
53.321595	1818.597729	19.321831
53.107806	1825.854234	19.326848
53.331767	1814.561474	19.331866
53.514370	1811.797692	19.336883
53.551585	1818.926067	19.341901
53.871392	1817.438227	19.346919
53.555657	1814.288279	19.351936
53.676628	1832.314468	19.356954
53.857922	1836.456111	19.361971
53.674292	1845.999068	19.366989
54.128934	1844.458259	19.372007
54.499497	1850.965587	19.377024
54.126113	1844.113042	19.382042
54.436127	1832.859243	19.387059
54.231460	1841.056601	19.392077
54.463943	1831.617967	19.397095
54.222587	1826.503910	19.402112
54.192061	1832.920246	19.407130
54.396543	1842.531086	19.412147
54.566488	1845.412897	19.417165
54.609840	1834.630301	19.422183
54.193612	1843.478852	19.427200
54.045988	1850.142761	19.432218
54.381101	1842.691912	19.437235
53.996521	1838.038808	19.442253
54.475506	1834.066789	19.447271
54.556480	1852.406926	19.452288
54.621600	1857.858639	19.457306
54.790266	1857.756439	19.462323
54.642208	1866.308961	19.467341
54.671324	1869.713491	19.472359
54.448817	1868.028975	19.477376
54.689054	1873.911331	19.482394
55.158199	1882.391383	19.487411
54.770498	1897.228246	19.492429
55.250951	1889.806107	19.497447
55.264041	1897.807521	19.502464
55.237793	1895.279180	19.507482
55.363678	1886.177644	19.512499
55.396416	1885.325503	19.517517
55.505337	1884.699541	19.522535
55.509216	1886.971516	19.527552
55.624546	1886.479035	19.532570
55.747147	1876.201329	19.537587
55.706219	1888.533520	19.542605
55.832581	1878.708273	19.547623
55.759708	1884.075031	19.552640
55.625605	1881.324778	19.557658
55.891018	1892.128588	19.562675
55.755286	1900.456566	19.567693
56.227157	1904.812239	19.572711
56.040821	1915.990943	19.577728
56.071654	1910.643097	19.582746
56.494920	1898.825309	19.587763
55.860671	1913.177657	19.592781
56.135322	1912.445820	19.597799
56.415695	1914.118387	19.602816
56.212517	1916.363609	19.607834
56.483988	1906.917136	19.612851
56.220966	1910.015886	19.617869
56.345571	1904.084401	19.622887
56.464674	1906.489023	19.627904
56.279912	1923.894717	19.632922
56.863785	1928.347374	19.637939
56.798599	1934.369707	19.642957
56.888179	1940.904584	19.647975
57.095416	1931.582392	19.652992
56.923186	1939.843062	19.658010
56.979487	1935.280072	19.663027
57.211150	1939.395621	19.668045
57.125476	1938.317740	19.673063
57.361966	1926.508481	19.678080
57.055909	1938.211270	19.683098
57.627337	1929.533400	19.688115
57.329221	1924.282846	19.693133
57.511673	1930.368723	19.698151
57.498348	1934.098597	19.703168
57.008397	1930.364459	19.708186
57.385586	1925.614219	19.713203
57.330337	1930.115320	19.718221
57.837156	1925.821066	19.723239
57.711806	1930.721124	19.728256
57.297485	1936.666210	19.733274
57.887470	1941.707034	19.738291
57.777892	1949.778381	19.743309
57.651204	1965.318564	19.748327
58.031673	1958.062571	19.753344
57.838121	1961.714222	19.758362
57.896040	1959.622363	19.763379
57.926533	1958.481120	19.768397
58.028680	1957.050004	19.773415
58.051434	1954.100102	19.778432
57.935661	1982.632665	19.783450
58.599978	1985.790403	19.788467
58.621560	1989.537533	19.793485
58.577534	1993.030055	19.798503
58.776333	1990.343887	19.803520
58.920227	1985.950183	19.808538
58.803987	1988.119412	19.813555
59.038209	1992.054443	19.818573
58.971848	1971.556235	19.823591
58.952776	1959.385771	19.828608
58.678161	1959.126950	19.833626
58.951873	1958.595048	19.838643
58.844104	1968.846484	19.843661
58.774744	1979.962532	19.848679
59.175646	1994.659565	19.853696
59.022360	1988.977660	19.858714
59.389244	1980.162482	19.863731
58.963103	1988.012971	19.868749
59.004175	1995.451512	19.873767
59.570721	1986.801130	19.878784
59.177074	1990.941697	19.883802
59.248935	1978.800763	19.888819
59.478329	1983.899111	19.893837
59.264318	1995.168811	19.898855
59.476558	2001.648758	19.903872
59.516951	2005.196250	19.908890
59.658601	2015.276582	19.913907
59.741397	2017.327550	19.918925
59.864162	2009.266281	19.923943
60.101991	2008.968993	19.928960
59.779501	2016.031340	19.933978
59.821348	2013.684042	19.938995
59.988336	2009.983548	19.944013
60.092168	2018.304849	19.949031
60.322334	2022.235817	19.954048
60.410885	2038.945205	19.959066
60.780257	2037.440787	19.964083
60.757891	2021.647059	19.969101
60.766748	2011.455044	19.974119
60.659211	2013.969767	19.979136
60.312281	2012.536328	19.984154
60.762442	2006.744017	19.989171
60.580240	2012.879433	19.994189
60.681083	2044.187200	19.999207
61.080476	2045.184014	20.004224
60.617272	2043.968905	20.009242
60.698171	2040.282134	20.014259
60.938309	2034.027767	20.019277
60.895284	2040.922064	20.024295
61.249591	2036.405904	20.029312
60.937970	2046.683612	20.034330
61.005301	2035.255201	20.039347
61.378110	2026.083521	20.044365
61.021534	2036.800220	20.049383
61.480171	2040.316413	20.054400
61.474050	2042.975428	20.059418
61.782907	2054.415847	20.064435
61.758016	2053.521761	20.069453
61.749531	2058.530648	20.074471
62.161853	2054.707640	20.079488
61.718100	2048.625263	20.084506
61.862503	2037.312770	20.089523
61.587548	2037.559766	20.094541
61.334805	2052.140077	20.099559
61.735558	2049.848013	20.104576
61.823370	2056.605038	20.109594
61.990286	2048.095439	20.114611
61.939836	2055.166333	20.119629
61.759073	2066.502363	20.124647
62.019688	2075.981700	20.129664
62.344901	2092.172023	20.134682
62.175267	2079.262493	20.139699
62.433917	2085.567536	20.144717
62.062039	2083.783324	20.149735
62.657508	2085.467798	20.154752
62.273249	2085.215448	20.159770
62.471391	2087.225219	20.164787
62.878310	2100.205094	20.169805
62.811415	2108.813245	20.174823
62.811460	2105.819741	20.179840
62.725398	2118.860949	20.184858
63.044189	2115.254206	20.189875
63.015800	2111.046042	20.194893
62.907307	2118.698064	20.199911
63.116151	2116.798421	20.204928
62.842679	2123.408586	20.209946
63.057602	2119.680756	20.214963
63.311643	2115.744538	20.219981
63.454526	2133.808508	20.224999
63.376780	2141.630258	20.230016
63.275966	2147.491606	20.235034
63.468052	2153.757740	20.240051
63.505990	2146.259743	20.245069
63.353139	2152.215129	20.250087
63.699050	2148.125813	20.255104
63.625546	2151.980967	20.260122
63.911770	2154.655517	20.265139
64.255867	2153.317154	20.270157
63.922154	2160.142240	20.275175
64.576877	2163.115916	20.280192
64.353154	2158.327719	20.285210
64.023102	2154.684434	20.290227
64.768523	2151.896903	20.295245
64.385139	2146.616604	20.300263
64.799995	2148.811277	20.305280
64.500214	2143.597877	20.310298
64.401602	2144.890430	20.315315
64.903007	2143.917123	20.320333
64.694890	2153.626221	20.325351
64.923991	2153.030636	20.330368
64.729690	2159.033537	20.335386
64.811390	2160.287896	20.340403
64.942133	2157.372646	20.345421
65.016875	2158.096387	20.350439
65.128144	2160.078335	20.355456
65.329565	2154.664651	20.360474
65.215067	2159.108413	20.365491
65.240580	2158.132343	20.370509
64.910830	2161.411688	20.375527
65.152782	2154.880105	20.380544
65.115461	2155.591828	20.385562
65.056306	2161.084712	20.390579
65.509606	2149.329579	20.395597
65.535507	2161.301315	20.400615
65.598562	2168.659354	20.405632
65.755382	2184.066459	20.410650
65.950444	2189.519597	20.415667
65.784810	2185.308129	20.420685
65.514645	2200.434105	20.425703
66.124388	2185.436879	20.430720
65.820300	2196.588167	20.435738
65.975406	2189.983109	20.440755
66.125815	2194.186415	20.445773
65.881597	2179.841382	20.450791
66.076664	2180.365808	20.455808
66.056576	2191.880822	20.460826
66.218493	2202.027270	20.465843
66.621652	2205.956656	20.470861
66.411295	2219.055533	20.475879
66.537538	2211.886369	20.480896
66.505241	2213.597825	20.485914
66.455104	2225.113724	20.490931
66.672574	2217.536717	20.495949
66.619055	2215.719020	20.500967
66.641122	2227.347685	20.505984
67.041878	2234.919339	20.511002
67.079414	2245.258702	20.516019
67.133954	2253.215158	20.521037
67.105269	2256.837442	20.526055
67.393213	2253.226146	20.531072
67.563170	2241.348586	20.536090
67.510815	2243.919834	20.541107
67.403757	2234.626336	20.546125
67.630027	2239.557731	20.551143
67.660508	2238.437705	20.556160
67.746947	2236.206753	20.561178
67.693932	2234.856989	20.566195
68.017323	2232.911534	20.571213
67.522774	2236.086605	20.576231
67.995520	2229.334121	20.581248
67.971140	2235.046449	20.586266
67.630791	2233.455408	20.591283
67.686985	2238.906327	20.596301
68.190706	2254.129969	20.601319
68.364303	2261.350078	20.606336
68.380508	2254.789167	20.611354
68.307736	2259.993223	20.616371
68.243461	2253.554483	20.621389
68.390876	2256.145787	20.626407
68.482702	2253.136042	20.631424
68.797950	2253.688500	20.636442
68.316455	2254.306668	20.641459
68.588330	2254.126654	20.646477
68.282648	2267.685983	20.651495
68.535551	2279.025383	20.656512
68.646096	2283.337328	20.661530
68.755585	2286.790491	20.666547
69.343452	2282.811216	20.671565
69.116500	2282.902682	20.676583
69.026144	2291.369950	20.681600
69.399589	2281.267480	20.686618
69.230942	2290.228624	20.691635
69.319848	2281.800550	20.696653
69.480865	2290.854638	20.701671
69.484264	2303.697683	20.706688
69.493557	2311.302704	20.711706
69.452216	2318.104046	20.716723
69.783412	2308.031106	20.721741
69.441723	2317.077283	20.726759
69.664471	2312.584381	20.731776
69.941506	2304.591165	20.736794
69.811766	2309.973440	20.741811
69.996547	2306.402968	20.746829
70.180730	2316.044103	20.751847
69.909167	2333.274560	20.756864
70.130355	2337.299077	20.761882
70.384910	2346.140061	20.766899
70.497019	2339.471786	20.771917
70.435236	2346.481700	20.776935
70.224444	2344.235994	20.781952
70.564729	2346.235718	20.786970
70.335686	2345.799716	20.791987
70.369140	2345.098460	20.797005
70.786240	2362.378801	20.802023
71.077319	2363.873519	20.807040
71.307532	2355.456691	20.812058
71.155559	2360.068527	20.817075
71.485038	2353.833600	20.822093
71.635438	2354.368303	20.827111
71.518048	2359.494559	20.832128
71.706645	2351.375408	20.837146
71.453723	2337.897642	20.842163
71.179590	2336.868664	20.847181
71.462113	2342.714578	20.852199
71.483605	2350.294076	20.857216
71.627597	2350.692934	20.862234
71.533167	2355.485946	20.867251
71.866859	2355.174938	20.872269
71.922261	2355.674450	20.877287
71.783553	2361.106156	20.882304
71.923029	2352.352195	20.887322
71.561577	2354.418998	20.892339
71.826648	2371.940694	20.897357
71.828892	2379.151220	20.902375
71.918674	2387.857256	20.907392
72.252187	2390.278893	20.912410
71.978746	2388.198916	20.917427
71.894074	2392.973079	20.922445
72.303589	2402.063118	20.927463
72.466221	2420.982465	20.932480
72.670373	2412.678311	20.937498
72.657553	2414.411068	20.942515
72.540648	2412.647504	20.947533
72.708574	2416.162173	20.952551
72.830244	2423.313558	20.957568
73.169287	2419.822287	20.962586
73.203656	2444.807873	20.967603
73.614399	2443.429753	20.972621
73.497759	2430.189744	20.977639
73.125600	2426.321846	20.982656
73.441049	2433.969350	20.987674
73.456194	2441.321009	20.992691
73.491582	2442.613455	20.997709
73.573323	2437.661607	21.002727
74.108312	2442.461245	21.007744
74.032847	2441.896917	21.012762
73.626481	2451.709408	21.017779
73.850058	2444.738562	21.022797
74.238699	2443.628262	21.027815
74.023453	2450.581682	21.032832
74.100734	2448.695900	21.037850
74.104353	2448.901620	21.042867
73.781495	2447.857594	21.047885
73.899315	2447.306490	21.052903
74.062417	2453.212396	21.057920
74.483781	2457.894866	21.062938
74.269357	2463.602981	21.067955
74.458810	2466.499112	21.072973
74.767060	2470.291894	21.077991
74.602006	2463.954085	21.083008
74.864245	2468.548666	21.088026
74.838844	2462.271178	21.093043
74.817437	2469.631040	21.098061
74.968553	2474.008152	21.103079
75.037143	2495.137195	21.108096
75.394195	2492.669545	21.113114
75.382841	2498.334276	21.118131
75.408408	2503.431490	21.123149
75.660086	2494.497512	21.128167
75.069223	2499.583695	21.133184
75.283822	2491.454028	21.138202
75.340276	2491.592328	21.143219
75.514720	2490.159071	21.148237
75.999318	2486.411740	21.153255
75.842776	2507.782793	21.158272
76.214520	2515.053235	21.163290
75.979712	2515.955363	21.168307
76.296200	2522.038205	21.173325
76.286514	2517.790757	21.178343
76.163449	2526.587456	21.183360
76.460650	2515.132237	21.188378
76.393853	2523.582510	21.193395
76.222404	2530.621800	21.198413
76.464118	2524.481032	21.203431
76.250800	2529.738275	21.208448
76.656908	2524.323278	21.213466
76.407392	2525.358327	21.218483
76.138465	2525.039589	21.223501
76.574727	2535.465025	21.228519
76.434649	2547.885951	21.233536
76.535925	2544.103772	21.238554
76.860732	2554.812079	21.243571
76.857148	2547.471525	21.248589
77.207782	2569.504336	21.253607
76.985817	2585.400183	21.258624
77.250711	2574.905004	21.263642
77.271812	2576.925774	21.268659
77.537247	2577.917247	21.273677
77.950207	2573.200428	21.278695
77.434947	2573.243480	21.283712
77.592051	2573.475067	21.288730
77.401231	2579.098443	21.293747
77.686582	2601.598728	21.298765
78.045653	2602.237818	21.303783
77.944926	2612.871656	21.308800
78.156761	2604.014759	21.313818
78.048293	2609.149905	21.318835
78.105861	2607.602339	21.323853
78.478896	2599.389924	21.328871
78.360244	2610.110785	21.333888
78.437505	2604.567283	21.338906
78.621185	2612.527725	21.343923
78.684093	2629.962409	21.348941
79.183948	2621.574795	21.353959
79.072764	2635.746101	21.358976
78.902695	2628.384074	21.363994
78.990357	2624.310642	21.369011
79.025218	2635.018052	21.374029
79.056852	2621.080103	21.379047
79.137516	2627.608845	21.384064
79.384501	2629.488981	21.389082
79.223273	2632.111483	21.394099
79.101935	2637.055973	21.399117
79.190432	2624.333695	21.404135
79.135508	2649.250491	21.409152
79.479680	2656.469552	21.414170
79.748760	2659.329425	21.419187
79.363376	2668.089381	21.424205
79.879478	2663.393055	21.429223
79.813367	2663.417181	21.434240
79.837113	2676.198313	21.439258
80.218611	2687.166697	21.444275
80.159110	2689.481941	21.449293
80.399543	2684.061843	21.454311
80.222038	2687.963614	21.459328
80.368418	2684.759441	21.464346
80.242409	2684.474543	21.469363
80.150346	2684.440666	21.474381
80.552300	2692.719529	21.479399
80.764279	2709.492596	21.484416
80.943606	2716.670328	21.489434
81.169409	2717.421136	21.494451
81.059578	2717.233557	21.499469
81.173521	2713.954317	21.504487
81.079804	2715.195009	21.509504
81.227328	2712.719047	21.514522
81.499694	2714.297808	21.519539
81.126918	2718.714492	21.524557
81.416695	2719.754010	21.529575
81.470170	2717.027173	21.534592
81.569959	2714.272498	21.539610
81.549052	2713.487861	21.544627
81.405194	2710.710687	21.549645
81.703437	2721.074886	21.554663
81.793523	2739.173983	21.559680
81.963639	2733.236479	21.564698
82.239985	2737.399407	21.569715
82.102932	2735.384941	21.574733
82.311091	2730.876934	21.579751
82.377130	2732.494894	21.584768
82.349963	2733.813075	21.589786
82.487362	2733.143993	21.594803
82.258186	2737.801296	21.599821
82.683899	2748.241153	21.604839
82.925069	2762.633276	21.609856
82.820622	2764.131332	21.614874
83.065501	2764.289143	21.619891
82.982945	2763.384544	21.624909
83.342304	2766.068785	21.629927
83.517212	2762.716883	21.634944
83.261337	2768.445885	21.639962
83.659002	2763.547378	21.644979
83.410250	2758.482939	21.649997
83.666118	2767.834482	21.655015
83.472942	2769.631441	21.660032
83.350843	2760.954349	21.665050
83.507352	2754.715374	21.670067
83.400830	2767.972022	21.675085
83.501777	2757.310139	21.680103
83.921213	2779.727961	21.685120
83.953924	2785.081357	21.690138
84.061941	2784.630131	21.695155
83.841534	2785.841476	21.700173
84.042258	2783.987095	21.705191
84.003663	2794.005464	21.710208
84.074689	2810.220605	21.715226
84.425207	2817.690452	21.720243
84.150542	2822.350316	21.725261
84.456933	2816.686026	21.730279
84.842867	2822.183692	21.735296
84.632015	2819.992983	21.740314
84.914916	2825.309641	21.745331
84.850274	2848.948504	21.750349
85.137461	2847.772549	21.755367
85.245342	2847.528223	21.760384
84.940071	2856.716020	21.765402
85.315491	2846.148745	21.770419
84.739819	2857.689168	21.775437
85.137555	2855.151255	21.780455
85.464946	2865.669019	21.785472
85.246906	2887.905486	21.790490
85.364590	2883.883831	21.795507
85.471566	2889.934164	21.800525
85.414486	2888.578695	21.805543
85.843420	2891.692371	21.810560
85.754095	2902.271897	21.815578
86.414627	2892.913778	21.820595
86.067586	2912.468034	21.825613
86.053724	2905.930505	21.830631
86.300986	2893.871753	21.835648
86.318035	2899.573014	21.840666
86.156212	2896.932394	21.845683
86.313805	2921.051168	21.850701
86.384767	2933.674751	21.855719
86.700343	2931.330851	21.860736
86.478535	2937.121348	21.865754
86.892834	2931.648260	21.870771
86.981794	2953.921610	21.875789
86.908703	2957.132666	21.880807
87.323429	2955.936363	21.885824
87.293369	2961.636508	21.890842
87.534398	2956.563115	21.895859
87.424080	2964.490400	21.900877
87.491381	2951.893145	21.905895
87.540081	2960.096344	21.910912
87.640725	2968.359700	21.915930
87.852112	2984.816956	21.920947
88.057814	2988.966050	21.925965
88.220011	2987.654266	21.930983
88.420285	2985.260308	21.936000
88.609020	2988.044172	21.941018
88.887143	2980.922782	21.946035
88.723008	2984.240397	21.951053
88.711134	2980.845076	21.956071
88.460762	2981.913330	21.961088
88.335222	2975.981186	21.966106
88.792994	2968.643937	21.971123
88.735166	2978.264322	21.976141
88.836013	2976.376288	21.981159
88.800480	2975.599475	21.986176
88.840057	2981.625983	21.991194
89.135855	2980.953657	21.996211
89.130136	2995.306719	22.001229
89.407366	2998.154348	22.006247
89.489467	2997.593975	22.011264
89.193472	3009.943402	22.016282
89.320031	3003.555706	22.021299
89.340746	3006.164992	22.026317
89.343317	3000.573468	22.031335
89.772390	3007.188411	22.036352
89.746257	3015.551461	22.041370
89.911726	3014.207687	22.046387
89.872389	3025.347273	22.051405
89.918101	3020.849350	22.056423
90.078786	3026.754303	22.061440
89.985503	3031.020313	22.066458
90.314889	3029.917850	22.071475
90.467091	3049.906340	22.076493
90.571313	3056.444104	22.081511
90.651262	3054.222716	22.086528
90.664816	3056.605031	22.091546
90.727417	3048.670781	22.096563
90.436785	3052.888819	22.101581
90.746336	3067.073682	22.106599
91.173064	3078.478807	22.111616
91.141384	3089.093325	22.116634
91.346011	3077.649286	22.121651
91.287327	3088.564670	22.126669
91.038481	3095.927291	22.131687
91.582329	3087.410473	22.136704
91.650289	3100.894464	22.141722
91.666085	3104.803277	22.146739
91.887806	3108.073546	22.151757
92.004610	3107.856899	22.156775
92.145898	3117.308748	22.161792
91.967632	3123.572218	22.166810
91.979959	3117.967295	22.171827
92.098862	3110.878313	22.176845
91.934880	3129.957646	22.181863
92.438595	3142.870316	22.186880
92.501823	3148.756247	22.191898
92.581455	3148.246607	22.196915
92.510902	3151.299974	22.201933
92.908862	3145.996967	22.206951
93.023775	3138.800053	22.211968
92.579274	3155.845874	22.216986
93.553380	3160.025087	22.222003
93.580575	3162.662473	22.227021
93.498784	3171.665366	22.232039
93.524181	3168.411945	22.237056
93.336041	3168.710400	22.242074
93.642406	3171.733556	22.247091
93.549757	3175.034307	22.252109
93.252943	3173.841330	22.257127
93.371492	3170.981316	22.262144
93.018258	3204.815131	22.267162
93.159711	3212.788929	22.272179
93.859642	3212.710560	22.277197
93.921913	3234.815533	22.282215
94.004098	3237.824108	22.287232
94.164815	3241.226851	22.292250
94.418891	3234.865132	22.297267
94.467930	3236.404836	22.302285
94.265185	3245.290975	22.307303
95.016170	3246.635357	22.312320
95.011395	3271.866948	22.317338
95.153790	3261.186290	22.322355
95.549978	3259.810422	22.327373
95.177106	3263.082723	22.332391
95.283404	3268.942169	22.337408
95.452600	3261.960730	22.342426
95.612027	3266.090538	22.347443
95.530618	3254.820198	22.352461
95.431277	3267.028350	22.357479
95.870081	3255.237680	22.362496
95.457821	3259.111746	22.367514
95.651849	3260.043859	22.372531
95.931308	3254.611823	22.377549
95.774140	3260.899519	22.382567
95.944714	3273.985787	22.387584
95.804116	3282.242953	22.392602
96.182556	3290.529842	22.397619
96.080953	3288.935217	22.402637
96.010224	3292.252165	22.407655
96.934073	3300.000553	22.412672
96.510399	3311.318855	22.417690
97.051136	3317.394591	22.422707
97.147505	3306.300388	22.427725
96.977310	3318.784979	22.432743
97.030482	3320.217837	22.437760
97.177659	3325.679826	22.442778
97.141677	3313.271792	22.447795
97.100091	3315.508760	22.452813
96.976705	3324.763026	22.457831
97.699974	3325.045938	22.462848
97.759296	3334.392216	22.467866
97.718475	3330.546751	22.472883
98.161929	3330.182827	22.477901
97.856150	3335.171909	22.482919
97.880275	3331.385312	22.487936
98.109091	3330.077034	22.492954
98.239079	3346.814350	22.497971
98.357873	3348.513643	22.502989
98.507649	3359.885277	22.508007
98.665936	3353.439666	22.513024
98.647343	3362.684324	22.518042
98.606163	3367.997797	22.523059
98.900283	3360.053205	22.528077
98.715709	3363.551159	22.533095
98.771062	3365.373848	22.538112
98.915511	3376.201987	22.543130
99.297906	3378.509803	22.548147
99.348118	3388.121094	22.553165
99.431084	3391.182281	22.558183
99.344325	3390.476547	22.563200
99.664002	3386.889811	22.568218
99.266542	3390.476785	22.573235
99.857341	3382.256743	22.578253
99.520386	3392.631464	22.583271
99.764626	3406.110438	22.588288
100.028061	3415.123720	22.593306
100.038940	3411.713658	22.598323
100.356361	3414.009815	22.603341
100.199899	3429.065429	22.608359
100.300088	3413.416638	22.613376
100.412449	3415.020208	22.618394
100.497458	3419.910028	22.623411
100.811364	3428.762660	22.628429
101.029269	3441.530804	22.633447
100.914275	3444.218448	22.638464
100.866223	3442.712024	22.643482
101.094984	3439.032003	22.648499
101.207426	3433.128588	22.653517
100.815457	3449.312072	22.658535
100.805105	3452.223744	22.663552
101.483053	3459.667667	22.668570
101.408621	3471.052329	22.673587
101.574234	3470.742935	22.678605
101.354231	3483.606908	22.683623
101.847709	3489.930968	22.688640
102.052223	3495.913293	22.693658
102.009188	3504.037028	22.698675
102.328545	3496.019900	22.703693
102.180219	3498.745908	22.708711
102.127353	3509.456147	22.713728
102.406437	3507.073139	22.718746
102.645939	3524.048068	22.723763
102.753830	3527.503356	22.728781
102.562324	3532.880980	22.733799
102.743661	3525.980079	22.738816
102.879402	3531.547807	22.743834
102.878686	3529.705792	22.748851
103.577014	3541.979700	22.753869
103.605214	3556.637058	22.758887
103.495288	3570.105009	22.763904
104.037194	3559.683741	22.768922
103.624513	3555.541162	22.773939
103.757175	3553.467052	22.778957
103.920327	3555.659608	22.783975
103.564188	3550.774853	22.788992
103.800891	3554.761836	22.794010
103.698106	3559.871233	22.799027
104.327177	3570.004712	22.804045
104.170843	3583.631113	22.809063
104.313831	3586.834594	22.814080
104.513496	3580.477471	22.819098
104.636654	3580.495801	22.824115
104.852043	3583.546925	22.829133
104.903874	3589.478118	22.834151
104.669361	3602.165150	22.839168
105.426288	3606.903045	22.844186
105.152465	3611.452103	22.849203
105.602241	3606.470279	22.854221
105.504252	3614.157590	22.859239
105.290394	3614.009399	22.864256
105.692723	3609.528374	22.869274
105.558685	3609.061445	22.874291
105.847009	3611.153810	22.879309
105.822857	3611.587386	22.884327
105.534013	3613.048066	22.889344
105.962342	3623.330019	22.894362
105.974926	3640.723585	22.899379
105.893827	3643.744122	22.904397
106.186723	3647.526292	22.909415
106.212800	3639.551922	22.914432
106.355662	3647.874222	22.919450
106.238150	3666.678590	22.924467
106.534503	3660.298934	22.929485
106.499267	3671.373850	22.934503
106.751620	3679.966626	22.939520
107.050135	3678.928829	22.944538
107.059744	3699.599379	22.949555
107.448324	3692.571740	22.954573
107.536024	3690.930364	22.959591
107.459816	3690.231585	22.964608
107.714234	3687.081554	22.969626
107.302019	3693.293679	22.974643
107.860251	3708.624222	22.979661
108.162829	3717.436357	22.984679
108.082326	3713.397307	22.989696
108.405266	3703.666146	22.994714
108.662087	3712.879692	22.999731
108.819729	3701.275103	23.004749
108.747704	3706.545631	23.009767
108.587045	3713.175487	23.014784
108.735797	3707.654783	23.019802
108.797998	3710.185206	23.024819
109.300784	3703.679000	23.029837
109.077343	3704.500716	23.034855
109.285448	3703.828972	23.039872
109.721637	3692.375063	23.044890
109.270171	3707.583418	23.049907
109.531941	3717.916384	23.054925
109.752846	3723.700311	23.059943
109.477684	3733.957644	23.064960
109.599581	3734.662146	23.069978
109.525286	3738.448615	23.074995
109.750588	3736.340039	23.080013
110.282269	3750.064560	23.085031
110.031326	3754.396040	23.090048
110.125817	3751.083486	23.095066
110.172651	3763.359207	23.100083
110.263267	3754.838763	23.105101
110.582873	3771.093208	23.110119
110.346287	3783.213541	23.115136
110.517730	3780.241135	23.120154
110.457547	3789.723974	23.125171
110.435137	3789.979491	23.130189
110.827599	3802.934089	23.135207
111.113746	3813.264023	23.140224
111.107055	3813.089873	23.145242
111.237239	3823.396697	23.150259
111.074632	3825.590108	23.155277
111.440100	3838.825949	23.160295
111.235166	3852.222775	23.165312
111.629475	3847.610011	23.170330
111.852051	3860.715259	23.175347
112.043900	3874.832356	23.180365
112.315124	3869.620103	23.185383
112.304457	3877.931617	23.190400
112.386918	3879.308725	23.195418
112.693417	3885.888552	23.200435
112.509481	3879.774977	23.205453
112.887190	3890.472687	23.210471
112.601844	3905.073404	23.215488
113.101796	3907.805458	23.220506
112.893248	3911.902874	23.225523
113.080248	3901.366468	23.230541
113.231735	3902.786852	23.235559
113.458055	3922.531072	23.240576
113.759132	3931.175228	23.245594
113.667468	3939.117368	23.250611
113.790555	3936.795356	23.255629
113.979864	3936.302027	23.260647
113.925001	3943.875645	23.265664
114.099030	3936.993025	23.270682
113.824375	3940.314317	23.275699
114.226672	3958.077212	23.280717
114.466334	3955.148174	23.285735
114.414639	3961.614444	23.290752
114.395794	3970.007555	23.295770
114.556759	3976.765604	23.300787
115.095007	3997.802256	23.305805
115.147297	3993.196786	23.310823
115.342245	3987.855053	23.315840
115.893904	3978.730742	23.320858
115.772564	3978.705461	23.325875
115.898576	3975.645073	23.330893
115.810162	3978.661338	23.335911
115.792227	3979.521886	23.340928
116.222863	3972.819386	23.345946
116.118145	3977.150426	23.350963
116.363588	3972.852433	23.355981
116.299251	3970.162244	23.360999
116.144187	3974.456472	23.366016
116.256401	3975.071276	23.371034
116.675567	3979.595688	23.376051
116.774324	3994.445194	23.381069
116.855750	4002.318074	23.386087
116.566861	4014.887476	23.391104
116.877065	3997.404655	23.396122
116.792348	4009.589850	23.401139
116.606836	4012.010357	23.406157
117.202098	4025.455169	23.411175
117.010854	4027.944246	23.416192
117.150276	4030.417570	23.421210
117.541286	4033.292889	23.426227
117.768957	4038.692749	23.431245
117.694126	4053.131815	23.436263
117.859404	4065.669746	23.441280
117.992860	4064.874581	23.446298
118.087353	4075.108606	23.451315
117.760780	4077.068594	23.456333
118.212360	4081.726325	23.461351
117.973714	4095.716398	23.466368
118.261944	4097.991361	23.471386
118.826882	4106.924739	23.476403
118.501007	4122.596516	23.481421
118.977955	4126.981171	23.486439
118.529791	4133.447016	23.491456
118.721520	4158.839960	23.496474
119.193676	4181.566202	23.501491
119.515627	4200.456153	23.506509
120.173969	4190.973277	23.511527
119.702512	4169.945785	23.516544
119.950467	4153.235792	23.521562
119.919981	4147.260480	23.526579
119.987244	4144.590969	23.531597
120.099980	4162.882524	23.536615
119.887172	4175.880475	23.541632
120.088454	4176.953884	23.546650
120.141734	4177.006173	23.551667
120.376393	4193.982652	23.556685
120.250793	4191.788364	23.561703
120.482032	4204.099556	23.566720
120.343230	4218.215428	23.571738
120.837054	4232.738637	23.576755
120.911123	4232.067790	23.581773
121.082673	4240.033416	23.586791
121.264566	4265.563423	23.591808
121.082126	4265.781531	23.596826
121.394793	4276.587445	23.601843
121.366603	4292.982892	23.606861
122.018600	4290.666955	23.611879
121.794159	4302.819604	23.616896
121.905983	4301.570021	23.621914
122.365984	4320.572637	23.626931
122.511098	4324.279427	23.631949
122.654198	4322.420673	23.636967
122.635837	4333.771886	23.641984
122.510257	4325.389431	23.647002
123.148951	4327.234079	23.652019
123.022880	4354.061833	23.657037
123.378262	4358.012019	23.662055
123.281753	4358.513797	23.667072
123.125820	4361.651044	23.672090
123.538621	4354.925257	23.677107
123.487349	4361.977724	23.682125
123.677431	4361.564502	23.687143
123.770162	4378.167331	23.692160
123.700273	4372.804755	23.697178
123.950504	4387.124657	23.702195
123.843702	4393.373335	23.707213
124.281637	4394.115585	23.712231
124.292568	4409.095159	23.717248
124.455542	4410.365076	23.722266
124.379079	4413.730392	23.727283
124.441850	4415.408063	23.732301
124.671176	4431.860152	23.737319
124.834423	4448.719293	23.742336
125.154103	4445.220417	23.747354
125.627868	4435.998109	23.752371
125.552159	4440.683395	23.757389
125.749590	4441.450625	23.762407
125.568332	4459.564432	23.767424
125.873564	4465.647527	23.772442
126.093345	4468.252865	23.777459
125.814552	4482.730380	23.782477
125.878070	4478.352686	23.787495
126.127766	4486.103802	23.792512
126.557124	4506.009174	23.797530
126.553066	4500.612453	23.802547
126.423025	4508.831646	23.807565
126.638014	4502.694321	23.812583
126.868814	4513.226318	23.817600
126.802723	4525.494720	23.822618
127.118540	4529.085444	23.827635
127.047995	4529.638157	23.832653
127.547833	4540.012414	23.837671
127.462294	4564.512517	23.842688
127.580104	4565.280649	23.847706
128.089541	4554.959057	23.852723
127.648099	4567.196087	23.857741
128.202951	4566.852930	23.862759
128.630344	4582.358663	23.867776
128.521493	4592.937796	23.872794
128.698610	4596.176967	23.877811
128.301474	4597.909900	23.882829
128.666807	4586.803314	23.887847
129.047655	4587.892177	23.892864
128.773852	4586.182473	23.897882
129.418233	4594.229451	23.902899
129.609464	4614.248465	23.907917
129.532296	4611.291149	23.912935
129.628964	4610.855842	23.917952
129.633575	4619.407644	23.922970
129.823838	4617.503571	23.927987
129.719539	4615.028114	23.933005
129.807244	4622.018422	23.938023
130.050266	4634.968480	23.943040
129.956736	4650.646248	23.948058
130.197439	4643.720413	23.953075
130.515308	4658.987224	23.958093
130.601439	4651.127818	23.963111
130.877082	4644.201132	23.968128
130.754437	4660.903919	23.973146
130.921381	4663.557053	23.978163
130.864047	4673.634760	23.983181
131.106075	4664.702585	23.988199
131.458475	4663.354821	23.993216
131.022166	4667.799513	23.998234
131.499455	4679.123094	24.003251
131.659000	4701.605760	24.008269
131.423819	4699.230617	24.013287
131.820797	4705.437645	24.018304
131.669914	4724.299032	24.023322
132.251087	4721.032173	24.028339
132.137934	4727.044415	24.033357
132.092054	4732.078272	24.038375
132.248764	4741.621543	24.043392
132.189037	4760.248160	24.048410
132.862861	4763.105280	24.053427
132.967138	4772.073974	24.058445
133.122892	4780.604916	24.063463
133.326713	4782.788027	24.068480
133.477662	4786.289457	24.073498
133.736161	4788.110614	24.078515
133.744438	4808.344730	24.083533
133.852103	4818.336435	24.088551
134.400830	4806.382253	24.093568
134.128264	4806.474701	24.098586
134.426569	4809.541972	24.103603
134.631197	4808.043106	24.108621
134.331631	4809.648003	24.113639
134.923113	4825.249772	24.118656
134.569217	4832.844779	24.123674
134.995208	4833.271912	24.128691
134.922909	4836.473808	24.133709
135.228227	4837.536185	24.138727
135.454032	4845.810539	24.143744
135.388448	4873.310105	24.148762
135.502775	4870.747034	24.153779
135.795874	4865.700879	24.158797
135.570463	4870.672149	24.163815
135.742444	4870.626842	24.168832
136.080537	4883.587921	24.173850
136.153942	4880.242289	24.178867
136.335038	4900.859646	24.183885
136.581623	4893.655830	24.188903
136.980996	4896.258571	24.193920
136.930794	4916.454956	24.198938
137.198849	4905.040300	24.203955
137.567628	4915.833806	24.208973
137.519811	4913.949564	24.213991
138.037386	4909.821900	24.219008
137.970444	4915.986556	24.224026
138.128810	4910.721132	24.229043
137.648433	4910.494262	24.234061
138.028284	4914.364388	24.239079
138.011089	4914.097493	24.244096
138.064265	4920.474296	24.249114
138.112743	4895.802132	24.254131
137.957854	4912.105968	24.259149
137.871137	4930.995937	24.264167
138.413228	4938.970518	24.269184
138.294315	4946.314910	24.274202
138.500490	4958.485974	24.279219
138.696233	4967.995634	24.284237
138.544275	4983.550114	24.289255
139.060123	4985.738574	24.294272
138.797135	5007.007496	24.299290
139.404829	5003.002329	24.304307
139.392413	5032.429072	24.309325
139.638407	5037.210369	24.314343
140.119548	5040.282366	24.319360
140.143791	5044.944824	24.324378
140.540267	5040.872624	24.329395
141.105182	5045.061799	24.334413
140.988102	5065.630950	24.339431
141.198017	5054.904401	24.344448
140.937819	5062.092004	24.349466
141.392338	5058.722538	24.354483
141.768203	5050.180254	24.359501
141.451343	5054.572970	24.364519
141.851202	5034.299821	24.369536
141.667910	5062.851489	24.374554
141.793153	5048.682323	24.379571
142.065902	5048.635896	24.384589
141.580845	5056.710595	24.389607
141.890110	5069.051769	24.394624
141.827256	5076.405383	24.399642
142.226532	5080.410135	24.404659
142.277811	5088.432376	24.409677
142.233413	5107.219840	24.414695
142.478383	5104.941938	24.419712
142.883562	5124.628573	24.424730
142.814488	5131.557580	24.429747
143.085617	5138.894162	24.434765
142.757711	5150.167907	24.439783
143.357000	5157.692915	24.444800
143.249866	5180.426532	24.449818
143.192608	5187.920135	24.454835
143.751676	5199.754264	24.459853
143.781345	5209.739002	24.464871
143.865294	5213.815312	24.469888
143.677441	5235.731872	24.474906
143.915819	5240.983349	24.479923
144.011371	5261.953151	24.484941
144.165202	5269.725475	24.489959
144.529297	5288.878385	24.494976
144.795224	5299.177976	24.499994
144.876055	5305.517491	24.505011
145.182229	5309.010818	24.510029
145.518344	5338.550175	24.515047
145.923568	5334.789627	24.520064
145.904045	5336.818828	24.525082
146.105506	5322.906314	24.530099
146.360843	5335.712625	24.535117
146.226267	5334.768165	24.540135
146.304355	5321.871348	24.545152
146.271971	5333.536331	24.550170
145.986284	5349.778107	24.555187
146.760337	5351.088353	24.560205
146.700577	5362.370643	24.565223
146.919480	5367.588294	24.570240
146.936256	5381.103780	24.575258
147.375145	5390.367240	24.580275
147.297434	5390.678807	24.585293
147.337504	5405.838059	24.590311
147.944664	5412.549229	24.595328
148.031555	5415.867483	24.600346
148.065664	5420.357761	24.605363
148.146595	5427.780673	24.610381
148.178684	5441.487313	24.615399
148.463049	5447.256297	24.620416
148.604736	5456.198987	24.625434
148.576397	5451.883644	24.630451
149.138279	5458.258243	24.635469
149.169993	5467.609492	24.640487
149.634080	5464.560982	24.645504
149.781216	5467.712290	24.650522
150.029581	5476.317773	24.655539
150.380999	5455.602536	24.660557
150.320823	5465.049471	24.665575
150.240929	5460.047641	24.670592
150.371824	5465.645200	24.675610
150.285814	5471.139665	24.680627
150.416572	5470.787802	24.685645
150.508285	5491.427317	24.690663
150.729212	5494.819415	24.695680
150.921052	5490.570446	24.700698
150.809505	5497.821100	24.705715
151.138824	5513.054716	24.710733
151.025562	5525.364512	24.715751
151.432577	5526.305303	24.720768
151.411698	5537.773495	24.725786
151.828322	5557.400664	24.730803
151.915703	5556.284690	24.735821
151.969707	5560.184129	24.740839
151.938779	5562.253730	24.745856
151.997470	5573.825704	24.750874
151.774648	5592.070258	24.755891
152.286138	5602.171193	24.760909
152.465125	5623.556204	24.765927
152.544375	5623.679888	24.770944
152.894327	5643.365794	24.775962
153.103722	5658.081321	24.780979
153.578237	5645.409757	24.785997
153.346789	5652.094250	24.791015
153.723389	5675.733381	24.796032
153.759957	5676.501153	24.801050
153.694661	5683.853883	24.806067
154.062499	5681.369841	24.811085
154.279395	5687.185082	24.816103
154.185982	5701.430453	24.821120
154.255912	5703.363618	24.826138
154.530980	5714.618752	24.831155
154.792938	5727.269353	24.836173
154.871223	5748.558093	24.841191
155.004369	5737.206795	24.846208
155.274784	5750.588551	24.851226
155.091084	5776.039420	24.856243
155.430066	5771.724425	24.861261
155.460230	5788.351404	24.866279
155.611845	5801.964577	24.871296
155.789853	5814.990555	24.876314
156.276140	5817.743257	24.881331
156.535554	5835.484000	24.886349
156.686295	5840.573428	24.891367
156.705173	5843.517890	24.896384
157.122814	5845.623797	24.901402
156.886142	5847.900907	24.906419
157.155000	5853.796835	24.911437
157.368443	5866.083146	24.916455
157.636632	5871.764397	24.921472
157.969568	5871.693427	24.926490
157.982653	5888.342124	24.931507
158.079510	5890.112877	24.936525
158.382693	5892.027758	24.941543
158.232006	5892.079532	24.946560
158.559170	5894.599556	24.951578
158.413223	5909.633988	24.956595
158.987455	5919.522937	24.961613
158.758934	5929.146497	24.966631
159.102368	5925.488496	24.971648
159.451525	5940.248110	24.976666
159.633157	5949.021865	24.981683
159.873378	5950.294552	24.986701
159.645721	5951.218549	24.991719
159.725769	5951.371221	24.996736
160.143886	5962.620259	25.001754
160.370034	5982.753580	25.006771
160.503136	5980.096845	25.011789
160.619063	5976.373612	25.016807
160.346986	5981.798797	25.021824
160.766668	5998.067288	25.026842
160.658113	6015.548271	25.031859
161.017897	6017.908119	25.036877
161.164089	6038.516107	25.041895
160.911281	6050.454408	25.046912
161.576748	6055.113295	25.051930
161.570071	6067.227158	25.056947
161.795981	6070.485628	25.061965
161.507215	6076.566542	25.066983
161.815046	6084.996888	25.072000
162.359826	6107.517833	25.077018
162.360005	6114.168749	25.082035
162.519394	6101.239409	25.087053
162.729925	6127.802701	25.092071
162.709041	6136.813423	25.097088
163.208146	6131.265857	25.102106
163.083177	6150.216980	25.107123
163.361684	6163.678860	25.112141
163.878861	6164.001023	25.117159
164.100606	6167.419111	25.122176
164.454841	6157.266719	25.127194
164.423253	6167.719784	25.132211
164.588469	6175.519096	25.137229
164.805201	6185.303933	25.142247
164.969776	6186.685477	25.147264
165.204630	6182.559275	25.152282
164.918314	6184.916735	25.157299
165.156004	6181.417943	25.162317
165.406039	6190.000760	25.167335
165.256137	6207.321760	25.172352
165.843734	6208.089824	25.177370
165.648740	6216.152729	25.182387
165.862531	6225.470705	25.187405
166.231114	6244.074172	25.192423
166.140062	6241.185619	25.197440
166.709040	6234.459269	25.202458
166.651287	6250.075588	25.207475
167.219156	6262.272674	25.212493
166.952416	6264.517660	25.217511
167.166636	6271.957511	25.222528
167.308133	6260.285042	25.227546
167.443710	6288.368078	25.232563
167.342446	6288.636996	25.237581
167.649289	6292.427077	25.242599
167.570064	6314.716588	25.247616
167.557818	6330.342258	25.252634
167.792022	6345.679235	25.257651
168.088228	6356.967682	25.262669
168.256598	6368.614059	25.267687
168.620880	6390.050101	25.272704
169.105479	6395.431898	25.277722
169.144579	6403.452073	25.282739
169.051497	6402.404937	25.287757
169.305748	6413.231968	25.292775
169.147889	6431.519908	25.297792
169.965635	6437.026422	25.302810
170.110098	6447.955171	25.307827
170.104608	6455.807812	25.312845
170.370179	6469.189419	25.317863
170.263698	6469.969811	25.322880
170.911694	6474.079280	25.327898
170.805616	6491.489614	25.332915
170.899438	6491.717990	25.337933
171.175798	6485.060215	25.342951
171.072802	6491.641987	25.347968
171.462489	6514.004954	25.352986
171.621662	6524.814966	25.358003
171.529311	6526.352382	25.363021
171.828190	6528.677177	25.368039
171.946358	6540.045293	25.373056
172.114085	6542.822175	25.378074
172.254386	6545.284770	25.383091
172.778127	6556.648034	25.388109
173.195994	6567.107614	25.393127
173.137955	6568.376767	25.398144
173.460201	6566.090260	25.403162
173.636682	6567.920787	25.408179
173.726018	6570.022497	25.413197
173.725045	6566.105315	25.418215
173.734509	6595.631599	25.423232
174.233094	6594.629381	25.428250
173.908424	6600.885397	25.433267
174.627409	6597.212994	25.438285
174.895293	6616.955771	25.443303
174.708636	6627.144334	25.448320
174.859131	6625.249499	25.453338
174.853906	6633.930710	25.458355
175.267080	6634.270256	25.463373
175.378151	6644.081685	25.468391
175.331734	6659.758786	25.473408
175.566464	6665.698249	25.478426
175.682129	6679.631902	25.483443
175.747318	6696.155175	25.488461
175.962208	6691.519010	25.493479
175.999258	6718.657860	25.498496
176.451053	6718.365727	25.503514
176.748062	6738.320398	25.508531
176.637731	6746.158435	25.513549
177.125770	6757.456732	25.518567
176.851914	6779.072975	25.523584
177.289827	6775.189625	25.528602
177.172501	6798.552083	25.533619
177.533871	6809.659746	25.538637
178.269679	6807.622785	25.543655
178.716492	6822.279587	25.548672
179.219229	6824.866988	25.553690
179.529018	6802.067491	25.558707
179.529207	6801.315465	25.563725
179.739000	6792.095245	25.568743
179.663693	6807.207445	25.573760
179.523953	6789.405174	25.578778
179.832042	6806.127464	25.583795
179.862646	6819.637335	25.588813
180.189242	6824.330044	25.593831
179.842782	6831.560574	25.598848
180.268716	6843.378704	25.603866
180.368219	6832.544160	25.608883
180.301408	6850.793707	25.613901
180.570815	6867.016302	25.618919
180.431966	6878.649902	25.623936
180.626559	6872.757202	25.628954
180.708259	6887.665840	25.633971
180.769783	6893.736872	25.638989
181.263215	6906.739488	25.644007
181.305189	6928.884702	25.649024
181.397965	6943.022894	25.654042
181.488364	6959.532212	25.659059
181.492378	6970.224869	25.664077
181.838750	6992.992031	25.669095
181.899927	7013.136531	25.674112
182.297183	7016.691285	25.679130
182.411761	7037.207346	25.684148
182.627961	7063.853241	25.689165
183.148814	7058.719683	25.694183
183.160427	7076.373954	25.699200
183.137803	7102.796371	25.704218
183.639841	7112.626034	25.709236
183.866611	7122.029059	25.714253
184.239571	7127.921491	25.719271
184.042989	7146.971852	25.724288
184.504826	7148.748302	25.729306
184.755065	7162.004723	25.734324
184.520401	7184.565027	25.739341
184.917036	7193.998455	25.744359
185.295984	7201.906651	25.749376
184.875682	7216.312600	25.754394
185.628199	7223.504230	25.759412
185.847182	7247.174149	25.764429
186.331615	7256.599127	25.769447
186.176565	7263.212357	25.774464
186.346402	7265.284021	25.779482
186.656772	7283.503076	25.784500
186.392080	7297.364184	25.789517
186.943956	7303.132952	25.794535
187.166906	7325.723588	25.799552
187.488179	7326.194261	25.804570
187.597460	7328.879893	25.809588
187.617960	7345.385045	25.814605
188.030768	7350.034277	25.819623
188.109973	7352.722347	25.824640
188.316720	7357.989855	25.829658
188.582627	7388.160601	25.834676
188.723678	7389.513750	25.839693
188.882310	7391.323621	25.844711
189.431741	7402.045301	25.849728
189.478547	7411.947742	25.854746
189.765752	7416.012713	25.859764
189.599445	7412.580407	25.864781
190.158244	7428.817279	25.869799
189.897544	7435.388414	25.874816
190.056518	7437.915066	25.879834
190.438062	7439.448624	25.884852
190.526244	7460.559622	25.889869
190.789126	7465.761565	25.894887
190.820808	7473.947167	25.899904
190.985067	7480.784200	25.904922
191.280044	7479.235262	25.909940
191.347993	7505.138392	25.914957
191.291857	7509.670444	25.919975
191.407814	7521.951640	25.924992
191.789823	7535.103192	25.930010
192.037072	7534.436852	25.935028
191.948990	7560.276038	25.940045
192.376909	7562.988025	25.945063
192.542562	7571.411200	25.950080
192.597797	7585.786540	25.955098
193.215224	7589.577015	25.960116
193.065318	7622.870726	25.965133
193.224004	7628.301792	25.970151
193.262032	7641.653851	25.975168
193.114837	7659.755106	25.980186
193.797425	7664.584899	25.985204
193.702673	7693.136939	25.990221
194.297448	7704.160064	25.995239
194.600617	7728.392530	26.000256
194.755566	7733.330073	26.005274
195.158544	7745.517694	26.010292
195.099278	7770.801837	26.015309
195.383873	7770.216876	26.020327
195.466903	7774.504922	26.025344
195.552309	7801.059678	26.030362
195.951554	7799.199792	26.035380
196.154745	7823.422386	26.040397
196.337917	7831.173280	26.045415
196.706558	7839.968703	26.050432
196.902667	7860.143195	26.055450
196.925235	7862.434356	26.060468
197.161876	7866.770332	26.065485
197.549265	7877.954124	26.070503
197.391327	7893.850168	26.075520
197.301051	7910.692294	26.080538
197.832770	7923.669241	26.085556
198.025735	7928.902952	26.090573
198.238044	7950.401280	26.095591
198.671873	7944.191068	26.100608
198.803868	7959.281613	26.105626
199.447548	7976.303458	26.110644
199.078753	7982.808654	26.115661
199.657214	7987.794435	26.120679
199.635165	8007.186329	26.125696
199.591440	8023.700109	26.130714
200.320902	8019.147141	26.135732
200.436916	8031.355566	26.140749
200.295142	8041.231440	26.145767
200.786225	8048.052040	26.150784
200.946446	8052.403795	26.155802
201.026566	8057.411999	26.160820
200.919984	8064.466383	26.165837
201.424508	8068.171115	26.170855
201.417832	8085.209816	26.175872
201.140232	8105.036418	26.180890
201.656531	8109.376668	26.185908
201.707295	8123.143000	26.190925
202.098676	8134.457761	26.195943
202.436193	8146.093123	26.200960
202.148595	8160.125108	26.205978
202.733134	8176.861918	26.210996
202.494126	8209.651785	26.216013
202.844511	8216.571617	26.221031
203.091995	8231.594450	26.226048
203.104931	8249.711021	26.231066
203.452088	8261.525137	26.236084
203.692682	8278.366469	26.241101
204.428697	8289.784967	26.246119
204.888038	8291.758293	26.251136
205.023375	8299.330168	26.256154
205.323050	8305.493254	26.261172
205.402118	8317.025556	26.266189
205.443072	8330.877842	26.271207
205.586142	8334.124449	26.276224
205.721792	8337.528833	26.281242
206.248402	8350.910653	26.286260
206.378647	8364.967890	26.291277
206.145793	8373.644696	26.296295
206.867070	8388.937608	26.301312
206.712996	8396.500194	26.306330
207.031719	8400.905866	26.311348
207.181301	8420.157618	26.316365
207.335678	8435.839981	26.321383
207.242770	8441.877245	26.326400
207.493792	8461.405609	26.331418
207.766186	8476.885063	26.336436
207.941739	8487.582149	26.341453
208.155007	8508.885580	26.346471
208.658195	8525.742773	26.351488
208.598007	8536.402325	26.356506
208.966191	8554.564536	26.361524
208.893970	8567.442780	26.366541
209.025441	8575.953813	26.371559
209.759072	8597.189363	26.376576
209.729532	8608.221016	26.381594
210.113611	8610.927992	26.386612
210.109704	8631.162168	26.391629
210.216998	8645.510554	26.396647
210.954286	8653.825112	26.401664
211.153385	8660.881406	26.406682
211.169543	8664.263996	26.411700
211.559543	8672.788560	26.416717
212.047935	8682.519145	26.421735
212.347985	8675.819642	26.426752
212.616322	8682.678802	26.431770
212.384904	8681.771201	26.436788
212.745870	8682.555088	26.441805
212.836418	8707.497437	26.446823
212.992518	8715.652080	26.451840
213.025342	8720.884845	26.456858
213.137818	8717.530552	26.461876
213.223646	8729.915124	26.466893
213.667890	8746.185079	26.471911
214.012697	8744.355796	26.476928
213.559530	8771.465569	26.481946
213.686604	8776.789957	26.486964
214.449461	8793.203149	26.491981
214.503985	8820.992251	26.496999
214.587148	8828.792660	26.502016
214.768436	8843.134554	26.507034
214.887713	8861.505224	26.512052
215.141903	8877.489666	26.517069
215.236409	8891.509813	26.522087
215.823888	8908.810033	26.527104
215.734815	8931.201414	26.532122
215.682245	8945.097507	26.537140
216.117440	8961.540299	26.542157
216.357036	8988.553795	26.547175
217.071184	9001.184284	26.552192
217.105874	9015.909741	26.557210
217.104527	9027.339335	26.562228
217.580032	9041.845024	26.567245
217.904805	9056.835512	26.572263
218.892851	9062.239551	26.577280
218.907671	9072.578650	26.582298
218.919363	9069.179358	26.587316
219.124745	9072.893869	26.592333
219.561549	9079.526471	26.597351
219.353924	9072.115271	26.602368
219.481711	9097.310449	26.607386
219.585824	9107.867881	26.612404
219.871440	9119.366299	26.617421
220.115184	9126.554200	26.622439
220.413440	9126.295567	26.627456
220.386517	9151.838936	26.632474
220.363954	9168.311648	26.637492
220.581245	9171.231826	26.642509
220.650222	9202.996581	26.647527
221.190615	9215.297677	26.652544
221.272851	9233.132890	26.657562
221.327439	9252.205690	26.662580
221.839009	9269.992176	26.667597
221.551925	9290.574575	26.672615
222.384335	9307.620192	26.677632
222.538722	9334.402756	26.682650
222.601498	9342.303872	26.687668
223.191885	9362.639853	26.692685
223.030744	9378.415998	26.697703
223.429758	9386.889170	26.702720
223.834218	9401.895238	26.707738
224.007290	9408.993810	26.712756
224.385251	9419.802130	26.717773
224.558945	9445.670904	26.722791
224.846737	9440.338797	26.727808
225.038410	9447.590635	26.732826
225.384066	9456.840825	26.737844
225.230711	9463.280830	26.742861
225.047151	9473.600677	26.747879
225.401566	9497.912836	26.752896
226.277267	9508.539173	26.757914
226.084705	9523.871907	26.762932
226.611383	9537.275246	26.767949
226.633008	9536.075027	26.772967
226.967033	9556.792898	26.777984
227.032886	9568.658797	26.783002
227.232610	9584.660941	26.788020
227.976896	9598.533701	26.793037
227.609694	9602.505280	26.798055
227.809772	9617.973441	26.803072
228.034042	9631.281449	26.808090
228.243618	9644.679166	26.813108
228.692855	9660.856066	26.818125
228.540053	9683.700614	26.823143
228.949040	9694.334986	26.828160
229.185157	9706.945484	26.833178
229.301839	9731.735054	26.838196
229.418860	9746.154558	26.843213
229.701389	9766.061286	26.848231
229.956535	9783.105427	26.853248
230.318007	9801.675126	26.858266
230.237622	9813.354799	26.863284
230.669335	9836.381056	26.868301
230.786967	9868.357849	26.873319
231.206448	9881.583412	26.878336
231.631799	9893.310805	26.883354
232.064451	9916.153273	26.888372
232.060347	9920.671067	26.893389
232.040493	9939.197448	26.898407
232.377464	9943.155235	26.903424
233.227055	9967.539533	26.908442
233.241918	9970.426424	26.913460
233.537783	9986.155929	26.918477
233.603589	10011.649772	26.923495
233.984567	10004.377623	26.928512
234.409037	10023.612009	26.933530
234.182429	10042.463058	26.938548
234.788644	10041.362423	26.943565
234.812309	10056.784786	26.948583
235.112420	10071.015261	26.953600
235.553683	10074.668810	26.958618
235.540312	10088.299213	26.963636
235.829058	10097.575005	26.968653
235.720890	10115.615543	26.973671
236.250060	10116.678058	26.978688
236.862484	10130.826142	26.983706
236.408669	10131.696321	26.988724
236.599932	10138.364604	26.993741
236.914793	10167.214527	26.998759
236.767618	10170.431464	27.003776
237.131869	10188.515224	27.008794
237.211880	10207.275495	27.013812
237.947878	10220.240772	27.018829
237.734424	10248.721755	27.023847
238.169126	10264.793804	27.028864
238.280560	10274.138896	27.033882
238.245380	10299.867719	27.038900
238.702777	10306.198524	27.043917
239.014694	10327.195649	27.048935
239.353887	10345.062049	27.053952
239.436263	10366.401967	27.058970
239.601658	10385.164195	27.063988
239.996782	10393.447906	27.069005
239.902307	10432.627840	27.074023
239.989611	10453.894691	27.079040
240.858027	10465.850185	27.084058
240.580248	10493.218412	27.089076
240.871445	10504.958226	27.094093
241.441007	10528.636473	27.099111
241.657869	10549.510151	27.104128
242.307849	10559.774599	27.109146
242.564231	10578.681149	27.114164
242.846221	10590.823487	27.119181
242.947675	10611.599956	27.124199
243.041376	10630.569887	27.129216
243.600608	10637.878221	27.134234
243.610502	10655.688086	27.139252
243.916976	10668.934327	27.144269
244.103721	10687.392489	27.149287
244.397404	10700.305521	27.154304
244.585039	10711.256872	27.159322
245.436401	10715.830572	27.164340
245.910224	10719.489717	27.169357
246.220641	10731.697290	27.174375
246.558297	10721.118300	27.179392
246.847203	10717.867270	27.184410
246.740802	10725.825200	27.189428
247.087152	10723.022277	27.194445
247.437723	10733.538415	27.199463
247.751465	10735.785568	27.204480
247.944054	10750.327782	27.209498
247.813509	10746.811481	27.214516
248.156576	10747.753781	27.219533
248.124131	10748.391151	27.224551
248.209797	10775.844801	27.229568
248.596732	10779.323808	27.234586
248.579912	10796.947241	27.239604
248.857040	10811.548840	27.244621
248.815313	10826.248108	27.249639
248.927332	10840.883138	27.254656
249.454266	10865.129082	27.259674
249.380933	10894.447210	27.264692
249.533102	10895.072078	27.269709
249.589649	10916.127654	27.274727
249.934949	10940.801309	27.279744
250.495237	10957.645060	27.284762
250.562350	10986.102776	27.289780
251.034810	11002.945230	27.294797
251.333441	11018.244073	27.299815
251.245711	11033.640329	27.304832
251.572276	11053.439031	27.309850
251.628009	11081.890870	27.314868
252.306788	11092.955069	27.319885
252.798889	11115.782406	27.324903
252.610209	11136.266231	27.329920
252.869615	11144.463182	27.334938
252.864636	11177.415021	27.339956
253.564512	11188.562897	27.344973
253.919854	11196.807155	27.349991
253.764986	11222.740405	27.355008
254.071046	11237.882054	27.360026
254.063521	11269.763707	27.365044
254.641239	11293.495574	27.370061
255.048568	11317.858317	27.375079
255.338420	11332.918824	27.380096
255.738529	11348.508387	27.385114
255.993641	11370.613582	27.390132
255.816387	11379.940246	27.395149
256.291369	11409.009437	27.400167
256.694068	11423.144360	27.405184
256.856843	11439.750174	27.410202
256.883577	11473.943533	27.415220
257.035103	11487.878104	27.420237
257.687390	11512.016364	27.425255
257.817366	11531.492847	27.430272
258.133753	11550.719654	27.435290
258.159034	11564.933957	27.440308
258.454181	11586.769809	27.445325
258.831119	11604.209615	27.450343
259.167180	11631.830920	27.455360
259.532672	11643.204217	27.460378
259.693910	11665.841721	27.465396
260.142296	11672.385088	27.470413
260.776216	11700.961192	27.475431
260.587534	11731.291048	27.480448
261.007807	11729.908261	27.485466
261.517791	11738.014629	27.490484
261.658984	11742.968087	27.495501
261.867298	11758.362359	27.500519
262.146166	11785.158946	27.505536
262.424308	11784.712619	27.510554
262.442463	11806.029583	27.515572
262.826040	11815.893640	27.520589
263.336033	11831.389839	27.525607
263.367529	11859.604970	27.530624
263.514156	11860.024153	27.535642
263.959587	11887.084414	27.540660
263.879375	11893.544092	27.545677
264.139317	11909.588101	27.550695
264.316037	11926.029888	27.555712
264.798368	11931.689954	27.560730
264.796175	11959.190842	27.565748
264.937719	11977.173719	27.570765
265.434458	11994.280828	27.575783
265.292687	12022.533916	27.580800
265.565732	12048.305913	27.585818
265.683930	12068.390046	27.590836
265.654302	12096.791474	27.595853
266.261228	12120.713417	27.600871
266.447019	12149.295289	27.605888
267.197755	12162.364194	27.610906
267.150619	12191.414214	27.615924
267.355402	12217.101941	27.620941
268.155640	12230.349953	27.625959
268.107398	12264.772120	27.630976
268.510301	12282.351234	27.635994
268.369123	12287.519305	27.641012
268.872665	12312.824263	27.646029
269.412611	12335.967550	27.651047
269.366767	12359.363047	27.656064
269.602026	12388.174995	27.661082
269.956832	12417.015957	27.666100
270.073176	12431.288380	27.671117
270.473766	12447.452024	27.676135
270.626872	12487.362487	27.681152
271.081438	12512.944191	27.686170
271.262958	12531.988300	27.691188
271.276068	12560.951299	27.696205
271.831211	12579.571081	27.701223
272.026696	12616.893741	27.706240
272.286457	12634.470497	27.711258
272.728388	12664.415964	27.716276
272.911713	12693.052776	27.721293
273.740475	12705.037245	27.726311
273.461813	12729.945510	27.731328
273.739097	12741.928966	27.736346
274.246431	12773.845643	27.741364
274.739988	12792.131720	27.746381
275.283296	12802.822843	27.751399
275.156151	12828.621578	27.756416
275.542947	12848.455336	27.761434
276.014184	12864.825416	27.766452
276.299984	12882.399686	27.771469
277.003710	12874.350367	27.776487
277.012525	12904.893419	27.781504
277.361193	12912.256307	27.786522
277.351345	12925.476724	27.791540
277.460311	12939.846241	27.796557
277.995811	12946.363783	27.801575
278.205461	12973.333094	27.806592
278.521543	12977.076487	27.811610
278.633570	12989.275198	27.816628
278.657372	13014.366646	27.821645
279.032243	13015.310426	27.826663
279.505456	13043.495718	27.831680
279.557673	13051.417674	27.836698
279.847331	13070.553061	27.841716
280.033775	13079.690648	27.846733
280.394266	13106.124993	27.851751
280.472348	13119.226378	27.856768
281.036829	13139.779305	27.861786
281.485434	13151.031763	27.866804
281.283598	13187.693687	27.871821
281.885720	13190.658794	27.876839
281.932271	13219.491965	27.881856
282.079133	13235.608336	27.886874
282.161402	13259.622295	27.891892
282.238306	13288.067728	27.896909
282.667753	13304.936233	27.901927
282.954128	13336.452532	27.906944
283.372248	13374.185720	27.911962
283.724974	13398.842709	27.916980
283.971595	13419.109474	27.921997
284.367458	13427.712265	27.927015
284.431307	13462.382281	27.932032
284.929398	13480.020818	27.937050
285.407774	13509.045178	27.942068
285.817679	13530.888657	27.947085
286.232418	13551.572769	27.952103
286.091038	13571.808890	27.957120
286.710744	13582.677411	27.962138
286.899086	13606.209588	27.967156
287.190323	13634.071828	27.972173
287.412757	13650.323008	27.977191
287.512242	13679.071856	27.982208
287.607473	13697.010716	27.987226
288.312043	13716.120929	27.992244
288.822530	13735.954727	27.997261
289.670898	13724.550931	28.002279
289.781433	13747.652147	28.007296
290.282954	13772.451039	28.012314
290.409675	13771.030641	28.017332
290.346293	13790.176168	28.022349
290.663336	13801.136285	28.027367
291.269820	13807.420113	28.032384
291.686226	13823.139316	28.037402
291.992959	13828.771608	28.042420
292.437151	13834.442606	28.047437
292.566246	13833.125340	28.052455
292.770195	13856.443956	28.057472
292.993835	13862.255012	28.062490
293.463691	13866.023810	28.067508
293.483188	13900.109524	28.072525
293.528636	13899.806701	28.077543
293.595523	13913.858633	28.082560
293.963108	13938.232901	28.087578
294.417925	13945.070942	28.092596
294.546677	13976.324193	28.097613
294.825660	13967.312844	28.102631
295.124238	13986.546065	28.107648
294.887785	14007.834559	28.112666
295.287475	14023.014448	28.117684
295.200316	14053.530614	28.122701
295.846143	14076.657809	28.127719
296.229499	14098.717970	28.132736
296.501072	14110.182185	28.137754
297.053742	14132.097056	28.142772
297.462576	14154.387161	28.147789
297.867931	14175.172411	28.152807
297.885238	14192.856227	28.157824
297.853345	14211.125916	28.162842
298.252310	14230.500788	28.167860
298.339813	14261.393567	28.172877
298.703935	14289.802932	28.177895
299.061765	14315.421781	28.182912
298.965182	14341.722701	28.187930
299.358849	14372.210984	28.192948
299.490766	14398.677800	28.197965
299.982129	14429.680918	28.202983
300.624395	14455.159215	28.208000
300.869951	14491.882547	28.213018
301.211281	14510.460742	28.218036
301.392979	14535.464571	28.223053
301.703538	14567.384779	28.228071
302.223176	14581.446935	28.233088
302.288505	14608.345009	28.238106
302.968455	14634.680308	28.243124
303.184160	14659.319842	28.248141
303.499937	14683.956947	28.253159
303.874487	14707.684616	28.258176
303.991819	14732.220089	28.263194
304.492837	14743.073034	28.268212
305.043482	14773.038674	28.273229
305.380512	14777.193070	28.278247
306.151852	14800.065973	28.283264
305.962806	14817.297472	28.288282
306.369122	14836.050805	28.293300
306.748482	14866.063608	28.298317
306.792388	14890.291906	28.303335
307.099062	14899.150548	28.308352
307.012678	14932.181427	28.313370
307.766528	14940.888521	28.318388
307.585657	14967.303237	28.323405
307.947619	14996.562028	28.328423
308.055107	15018.759420	28.333440
308.160830	15052.877544	28.338458
308.921351	15076.143358	28.343476
309.287461	15104.670431	28.348493
309.057565	15115.371089	28.353511
309.679308	15149.207909	28.358528
309.925907	15175.750486	28.363546
310.249762	15205.433194	28.368564
310.422111	15231.678996	28.373581
310.542673	15257.495180	28.378599
311.428705	15279.227387	28.383616
311.203432	15300.794184	28.388634
311.914382	15330.776401	28.393652
311.918355	15362.503565	28.398669
312.516839	15377.359857	28.403687
312.745527	15407.627124	28.408704
312.986828	15439.123541	28.413722
313.525908	15456.466933	28.418740
313.898463	15480.178992	28.423757
314.020272	15513.357336	28.428775
314.635067	15520.773549	28.433792
315.020662	15545.076649	28.438810
315.103381	15564.746094	28.443828
315.414977	15593.916427	28.448845
315.752467	15613.440621	28.453863
316.088863	15635.856713	28.458880
316.032525	15669.587329	28.463898
316.384613	15676.858311	28.468916
316.991872	15715.435894	28.473933
317.061389	15742.167885	28.478951
317.499525	15756.528325	28.483968
317.844046	15795.612878	28.488986
318.410550	15813.967716	28.494004
318.598702	15843.410720	28.499021
318.597441	15866.426558	28.504039
319.185659	15890.104287	28.509056
319.518120	15912.950094	28.514074
320.447098	15932.583154	28.519092
321.051439	15950.954367	28.524109
321.172072	15957.569153	28.529127
321.996836	15974.230674	28.534144
321.884854	15989.938101	28.539162
322.045530	16005.540483	28.544180
322.333838	16018.856874	28.549197
322.480523	16045.795175	28.554215
322.605584	16064.196064	28.559232
322.813191	16083.897836	28.564250
323.507569	16103.333888	28.569268
323.491596	16124.600496	28.574285
323.797331	16151.586263	28.579303
323.996005	16180.510970	28.584320
324.363174	16213.665100	28.589338
324.588710	16238.261310	28.594356
325.011853	16268.596707	28.599373
325.177552	16295.086988	28.604391
325.453814	16315.569763	28.609408
325.703984	16352.778246	28.614426
326.424368	16376.603361	28.619444
326.499539	16397.243084	28.624461
326.412023	16431.973346	28.629479
327.161517	16455.467006	28.634496
327.395071	16501.828812	28.639514
327.722469	16516.966008	28.644532
327.925036	16547.398518	28.649549
328.175744	16578.251135	28.654567
328.485899	16597.325658	28.659584
328.612628	16633.552213	28.664602
329.627222	16655.489687	28.669620
330.347363	16669.852688	28.674637
330.261087	16692.220758	28.679655
330.581741	16713.889412	28.684672
331.339058	16737.279313	28.689690
331.735376	16758.358850	28.694708
332.152687	16768.593158	28.699725
332.846724	16774.442946	28.704743
333.549981	16770.642966	28.709760
333.924601	16778.370690	28.714778
334.299055	16788.817537	28.719796
334.870302	16791.464302	28.724813
334.578466	16801.007181	28.729831
334.819257	16788.339229	28.734848
335.090882	16804.165664	28.739866
335.093441	16828.178906	28.744884
335.296152	16832.520517	28.749901
335.644604	16862.642034	28.754919
336.006900	16870.556598	28.759936
335.961388	16909.452016	28.764954
335.974173	16925.368445	28.769972
336.769326	16951.280826	28.774989
336.786045	16986.513796	28.780007
336.902089	17001.337141	28.785024
337.215884	17035.273148	28.790042
337.477849	17062.661555	28.795060
337.760455	17105.015212	28.800077
338.074482	17131.821065	28.805095
338.601325	17162.931810	28.810112
338.917593	17197.442554	28.815130
338.848918	17236.908204	28.820148
339.686066	17254.705710	28.825165
340.005935	17298.560585	28.830183
340.503517	17325.313111	28.835200
340.895952	17364.033578	28.840218
340.827750	17393.533773	28.845236
341.098546	17419.268310	28.850253
341.406571	17455.797018	28.855271
341.830157	17481.847849	28.860288
342.196371	17522.077964	28.865306
342.491859	17559.110868	28.870324
343.039330	17586.123605	28.875341
343.195172	17621.423046	28.880359
343.275327	17665.971872	28.885376
343.713184	17686.440159	28.890394
344.133258	17722.140626	28.895412
344.763753	17762.091847	28.900429
344.753525	17801.164185	28.905447
345.668797	17829.510059	28.910464
345.778135	17865.605256	28.915482
346.150391	17898.549193	28.920500
346.788940	17916.448011	28.925517
347.267541	17944.873135	28.930535
348.042648	17951.939987	28.935552
348.236310	17990.986215	28.940570
348.539045	18015.827277	28.945588
348.962033	18045.288225	28.950605
349.279096	18062.604977	28.955623
349.620142	18081.194316	28.960640
349.905320	18094.416144	28.965658
350.260926	18112.527605	28.970676
350.366577	18099.341142	28.975693
350.401325	18117.746265	28.980711
350.946556	18145.120574	28.985728
351.171335	18169.705797	28.990746
351.565762	18191.278147	28.995764
351.928365	18221.608910	29.000781
351.677997	18261.367534	29.005799
352.032483	18295.364774	29.010816
352.623423	18323.169130	29.015834
352.898379	18356.821295	29.020852
353.086461	18384.603346	29.025869
353.539183	18425.145249	29.030887
353.746630	18459.350144	29.035904
354.184462	18492.858925	29.040922
354.518746	18542.062055	29.045940
354.967280	18562.443574	29.050957
355.355350	18612.780528	29.055975
355.696640	18631.025983	29.060992
356.189987	18669.222572	29.066010
356.403779	18711.086428	29.071028
357.176824	18729.994334	29.076045
357.799921	18754.124070	29.081063
358.121588	18785.462114	29.086080
358.596967	18817.600970	29.091098
358.674984	18844.444238	29.096116
359.170639	18863.130354	29.101133
359.369161	18909.023006	29.106151
359.911803	18923.731379	29.111168
360.261194	18950.069742	29.116186
360.392676	18984.700126	29.121204
361.185020	19014.482421	29.126221
361.587392	19041.330248	29.131239
361.946896	19067.152201	29.136256
362.251724	19093.806593	29.141274
362.460315	19115.201161	29.146292
362.920433	19132.257706	29.151309
363.081927	19163.966156	29.156327
363.410658	19183.390731	29.161344
363.614384	19207.842746	29.166362
364.003519	19244.892298	29.171380
364.485872	19276.980591	29.176397
364.811509	19305.414466	29.181415
364.980147	19329.387574	29.186432
365.795123	19356.371786	29.191450
365.861799	19384.373012	29.196468
366.129955	19404.941086	29.201485
366.353223	19434.325455	29.206503
366.818506	19465.158860	29.211520
367.299696	19484.225623	29.216538
367.434735	19527.661458	29.221556
367.802241	19552.484804	29.226573
368.133533	19581.613234	29.231591
368.327463	19615.370797	29.236608
368.705438	19646.535830	29.241626
369.262393	19677.851164	29.246644
370.067520	19699.449536	29.251661
370.249655	19739.366638	29.256679
370.608790	19754.685816	29.261696
371.187663	19784.255148	29.266714
371.034982	19815.318837	29.271732
371.820730	19844.096563	29.276749
372.155651	19869.593798	29.281767
372.545738	19907.707498	29.286784
372.904928	19921.102572	29.291802
373.094851	19961.560406	29.296820
373.716360	19976.498579	29.301837
373.679266	20013.114261	29.306855
373.859769	20050.579726	29.311872
374.700350	20076.471981	29.316890
374.588024	20116.072741	29.321908
375.328432	20145.128363	29.326925
375.649498	20174.364265	29.331943
376.018338	20210.770031	29.336960
376.459268	20247.721958	29.341978
376.709455	20291.850719	29.346996
377.216820	20328.051191	29.352013
377.718283	20359.632284	29.357031
377.781309	20387.007831	29.362048
378.710726	20418.948474	29.367066
378.771606	20444.027247	29.372084
379.226834	20473.515599	29.377101
379.714771	20500.316465	29.382119
380.750292	20500.407612	29.387136
381.112108	20517.876678	29.392154
381.615607	20552.561499	29.397172
382.093267	20569.045859	29.402189
382.134281	20584.140512	29.407207
382.423739	20607.638766	29.412224
382.820012	20633.345614	29.417242
382.983270	20655.641004	29.422260
383.591225	20684.402932	29.427277
383.942959	20702.975580	29.432295
384.215779	20725.786776	29.437312
384.341054	20747.661500	29.442330
385.036072	20770.333817	29.447348
385.374610	20791.636727	29.452365
386.047488	20828.126999	29.457383
386.027088	20855.482790	29.462400
386.648318	20870.320665	29.467418
387.050951	20895.045643	29.472436
387.083554	20919.802846	29.477453
387.274664	20932.594741	29.482471
387.724809	20966.129701	29.487488
387.794002	20984.787082	29.492506
388.231082	21028.252180	29.497524
388.418137	21050.273417	29.502541
388.957843	21083.184785	29.507559
388.639102	21121.594733	29.512576
389.211458	21148.827440	29.517594
389.498629	21199.870420	29.522612
389.893598	21238.072417	29.527629
390.217490	21272.952050	29.532647
390.869251	21318.040785	29.537664
391.229138	21363.762901	29.542682
391.604392	21400.390134	29.547700
392.176189	21442.058923	29.552717
392.519818	21482.199258	29.557735
392.479791	21535.592045	29.562752
393.249166	21577.659730	29.567770
393.417479	21634.258201	29.572788
394.092246	21669.801868	29.577805
394.731834	21703.143604	29.582823
395.285851	21745.252353	29.587840
395.945117	21780.861750	29.592858
396.072135	21815.533736	29.597876
396.419008	21848.926361	29.602893
396.852135	21884.242021	29.607911
397.495902	21919.906970	29.612928
397.886997	21952.298813	29.617946
398.370511	21966.790285	29.622964
398.677800	22000.337607	29.627981
399.738792	22023.746541	29.632999
399.776060	22046.378227	29.638016
400.558323	22075.154307	29.643034
400.728446	22105.587448	29.648052
401.095073	22126.956999	29.653069
401.596626	22149.292747	29.658087
401.526747	22183.765356	29.663104
402.214134	22205.805359	29.668122
402.400354	22234.059212	29.673140
402.243864	22263.445186	29.678157
403.230726	22297.440126	29.683175
403.442782	22345.766522	29.688192
403.654258	22364.130343	29.693210
403.913484	22403.286973	29.698228
404.165807	22447.969221	29.703245
404.660813	22477.776342	29.708263
404.867073	22525.636358	29.713280
405.439358	22561.107787	29.718298
406.038911	22604.615134	29.723316
406.175348	22642.304863	29.728333
406.325013	22682.776880	29.733351
406.717982	22724.090815	29.738368
407.399845	22761.945965	29.743386
407.701930	22802.180549	29.748404
408.395620	22835.076549	29.753421
408.927461	22865.232973	29.758439
408.999702	22908.284060	29.763456
409.219580	22937.990171	29.768474
409.919408	22977.637247	29.773492
410.418227	23009.104349	29.778509
410.950827	23037.506083	29.783527
411.156225	23087.306354	29.788544
411.806523	23114.421339	29.793562
411.710198	23147.012229	29.798580
412.138836	23191.677929	29.803597
412.594465	23232.461770	29.808615
412.983495	23273.608415	29.813632
413.605155	23307.732248	29.818650
414.139416	23338.572885	29.823668
414.567840	23381.108499	29.828685
415.000218	23407.168567	29.833703
415.609092	23439.707556	29.838720
415.981276	23474.314960	29.843738
416.142564	23519.403054	29.848756
416.479318	23552.173099	29.853773
417.183975	23588.885242	29.858791
417.114716	23631.663087	29.863808
417.736421	23667.601729	29.868826
418.409713	23703.728369	29.873844
418.464977	23750.306989	29.878861
419.007480	23782.262547	29.883879
419.685027	23823.055868	29.888896
420.253235	23865.425569	29.893914
420.613067	23905.812859	29.898932
420.454078	23939.571696	29.903949
421.285758	23964.611212	29.908967
421.666478	24004.201419	29.913984
422.616604	24033.629381	29.919002
423.315178	24062.335765	29.924020
423.861448	24092.934128	29.929037
424.434203	24105.615793	29.934055
424.860293	24144.338940	29.939072
425.228018	24157.365249	29.944090
425.403539	24183.376141	29.949108
425.589153	24219.389453	29.954125
425.966081	24255.490521	29.959143
425.947865	24290.640836	29.964160
426.385521	24329.122335	29.969178
426.908322	24360.750564	29.974196
427.015316	24388.801095	29.979213
427.776098	24435.571791	29.984231
428.246432	24482.543296	29.989248
428.691406	24511.798983	29.994266
429.349991	24541.302697	29.999284
429.450142	24587.127474	30.004301
429.843617	24593.238462	30.009319
430.080827	24642.396520	30.014336
430.240871	24676.444807	30.019354
430.849503	24710.079814	30.024372
430.820904	24753.557635	30.029389
431.433664	24803.768644	30.034407
431.575745	24843.443069	30.039424
432.221931	24883.735219	30.044442
432.655129	24920.366856	30.049460
432.924550	24970.086392	30.054477
433.602554	25011.535730	30.059495
434.316835	25056.021712	30.064512
434.678367	25089.578725	30.069530
435.394436	25111.004539	30.074548
435.860109	25153.360125	30.079565
436.189794	25185.818760	30.084583
436.428091	25218.540955	30.089600
436.948533	25264.296767	30.094618
437.346811	25295.249514	30.099636
437.495673	25354.893281	30.104653
438.031433	25391.638064	30.109671
438.547346	25430.692698	30.114688
438.951839	25480.001559	30.119706
439.573251	25522.102488	30.124724
439.610331	25567.253171	30.129741
439.974197	25607.786708	30.134759
440.502234	25666.121006	30.139776
441.040934	25712.004383	30.144794
441.635397	25746.208672	30.149812
441.938125	25802.875373	30.154829
442.536275	25845.690660	30.159847
443.094182	25888.401393	30.164864
443.323736	25933.774534	30.169882
443.721248	25977.643915	30.174900
444.409942	26017.794282	30.179917
445.521723	26049.358799	30.184935
446.199378	26071.078784	30.189952
446.708734	26107.162142	30.194970
447.475303	26124.984928	30.199988
447.839384	26166.462061	30.205005
448.305119	26185.347545	30.210023
449.103122	26206.155162	30.215040
449.377350	26250.499499	30.220058
449.708245	26255.879766	30.225076
449.993914	26285.976315	30.230093
450.072505	26313.900809	30.235111
450.371973	26345.921488	30.240128
450.712250	26371.028899	30.245146
451.164033	26406.751039	30.250164
451.522075	26450.607517	30.255181
451.702620	26487.576847	30.260199
452.160720	26526.074547	30.265216
452.354122	26570.714685	30.270234
452.828502	26615.402358	30.275252
452.936440	26673.529925	30.280269
453.705719	26716.305299	30.285287
453.833537	26762.824382	30.290304
454.400779	26808.744947	30.295322
455.166437	26850.850014	30.300340
455.120631	26906.822948	30.305357
455.609630	26948.505941	30.310375
456.341493	26984.438428	30.315392
456.656726	27030.238265	30.320410
456.774885	27074.736577	30.325428
457.180814	27133.687328	30.330445
457.838546	27176.432848	30.335463
458.162090	27231.862741	30.340480
458.565596	27274.745143	30.345498
459.103130	27320.663232	30.350516
459.390271	27378.801814	30.355533
460.120549	27430.128964	30.360551
460.648266	27479.824556	30.365568
460.741118	27537.372239	30.370586
461.190113	27587.249309	30.375604
462.298859	27635.358991	30.380621
462.702548	27681.070941	30.385639
463.523013	27728.457853	30.390656
463.893261	27777.326952	30.395674
464.928073	27815.304086	30.400692
465.099632	27862.835742	30.405709
465.291629	27890.509311	30.410727
465.989721	27937.583840	30.415744
466.346486	27985.292778	30.420762
466.957421	28023.727154	30.425780
467.246942	28062.242767	30.430797
467.581187	28095.325831	30.435815
468.356517	28145.734106	30.440832
468.613610	28189.571989	30.445850
469.303663	28226.637462	30.450868
469.587902	28277.483671	30.455885
469.994287	28321.616444	30.460903
470.590624	28355.041211	30.465920
470.794794	28414.890750	30.470938
471.262458	28457.520232	30.475956
471.965233	28508.040471	30.480973
472.379214	28544.378485	30.485991
473.100552	28593.937916	30.491008
473.184528	28635.330483	30.496026
474.057165	28669.810258	30.501044
474.498505	28717.782076	30.506061
474.970550	28772.309514	30.511079
475.754737	28793.320455	30.516096
476.602297	28836.815453	30.521114
476.895748	28863.858348	30.526132
477.742247	28898.479877	30.531149
477.989306	28931.630539	30.536167
478.520407	28958.416684	30.541184
479.004328	28978.311116	30.546202
479.425785	29013.848435	30.551220
480.047753	29053.561550	30.556237
479.973947	29091.470878	30.561255
480.695179	29115.335204	30.566272
480.695517	29153.234439	30.571290
481.170398	29197.330312	30.576308
481.616991	29226.888217	30.581325
482.244721	29269.614100	30.586343
482.404771	29302.530383	30.591360
482.658671	29349.400833	30.596378
483.377335	29385.819842	30.601396
483.800639	29426.607209	30.606413
484.231762	29468.509200	30.611431
484.573695	29508.531219	30.616448
485.051802	29553.932428	30.621466
485.445514	29598.210943	30.626484
485.939304	29648.865730	30.631501
485.945937	29702.534304	30.636519
486.509077	29747.487538	30.641536
486.830268	29811.539284	30.646554
487.564028	29853.515402	30.651572
487.923988	29915.615044	30.656589
488.177730	29976.322905	30.661607
488.871590	30030.004427	30.666624
489.463770	30087.763681	30.671642
489.724651	30141.981042	30.676660
490.496909	30203.423516	30.681677
490.905671	30259.491589	30.686695
491.565621	30308.405665	30.691712
491.855103	30368.674305	30.696730
492.615995	30415.262161	30.701748
493.126440	30477.144532	30.706765
493.347966	30533.597979	30.711783
494.083160	30583.954006	30.716800
494.698265	30649.607605	30.721818
495.438117	30701.558222	30.726836
495.810358	30751.878021	30.731853
496.228955	30801.096797	30.736871
497.169221	30831.496238	30.741888
497.154023	30890.470940	30.746906
497.852019	30938.578614	30.751924
498.552512	30982.293472	30.756941
499.313786	31033.920208	30.761959
499.923275	31072.321032	30.766976
500.280762	31116.004202	30.771994
500.969541	31164.523794	30.777012
501.435636	31214.642505	30.782029
501.850560	31251.555372	30.787047
502.176025	31296.850185	30.792064
502.981311	31352.198433	30.797082
503.200153	31387.439051	30.802100
503.508669	31428.172461	30.807117
503.880310	31484.994569	30.812135
504.468738	31526.328272	30.817152
504.807420	31587.411564	30.822170
505.046315	31645.981253	30.827188
505.812459	31689.671776	30.832205
506.185400	31749.475101	30.837223
506.598006	31810.295257	30.842240
506.940500	31860.675202	30.847258
507.691237	31908.591328	30.852276
508.351353	31967.266863	30.857293
508.695330	32016.641444	30.862311
509.178449	32053.977123	30.867328
509.719723	32097.034668	30.872346
510.310441	32148.521846	30.877364
510.778001	32191.537789	30.882381
511.158088	32250.413407	30.887399
512.039771	32290.723491	30.892416
512.396314	32344.534093	30.897434
513.043471	32394.485693	30.902452
513.627486	32436.397706	30.907469
513.989232	32488.505623	30.912487
514.835637	32530.439128	30.917504
515.367598	32581.472027	30.922522
515.836812	32622.628866	30.927540
516.655553	32660.810918	30.932557
517.190882	32703.048190	30.937575
517.703650	32736.873531	30.942592
517.674020	32786.234265	30.947610
518.110023	32838.211660	30.952628
518.902389	32886.745048	30.957645
519.167343	32943.535577	30.962663
519.412820	32987.238395	30.967680
520.328390	33040.500364	30.972698
520.598396	33097.667350	30.977716
521.481425	33153.942430	30.982733
521.514181	33205.089874	30.987751
522.363685	33256.605488	30.992768
522.723905	33311.066510	30.997786
523.368717	33365.269574	31.002804
523.875213	33408.637154	31.007821
524.376773	33473.686408	31.012839
524.674228	33526.941212	31.017856
525.482391	33578.768645	31.022874
526.009679	33639.421203	31.027892
526.492015	33680.515528	31.032909
526.741688	33744.433164	31.037927
527.366371	33806.324016	31.042944
527.916622	33864.303387	31.047962
528.006485	33927.717525	31.052980
528.889181	33972.845785	31.057997
529.040052	34035.203902	31.063015
529.554874	34101.185140	31.068032
530.383316	34151.354350	31.073050
530.727462	34219.094118	31.078068
531.731454	34273.726890	31.083085
531.831970	34347.556219	31.088103
532.725514	34392.961341	31.093120
533.493547	34447.014313	31.098138
534.072070	34511.595054	31.103156
534.969187	34562.106108	31.108173
535.120201	34616.852228	31.113191
535.381205	34667.335656	31.118208
536.262168	34717.022123	31.123226
537.058540	34759.043335	31.128244
537.634163	34804.580620	31.133261
538.259454	34843.405451	31.138279
538.781761	34875.876306	31.143296
539.505930	34922.968289	31.148314
539.650940	34955.329138	31.153332
540.391395	34991.954143	31.158349
540.700254	35047.751686	31.163367
541.004050	35095.166502	31.168384
541.594936	35136.746877	31.173402
541.969374	35191.366279	31.178420
542.590216	35240.670089	31.183437
542.974818	35286.068854	31.188455
543.766670	35331.298825	31.193472
544.494388	35375.525441	31.198490
544.725420	35441.814155	31.203508
545.223853	35487.652524	31.208525
545.473083	35539.955034	31.213543
545.902817	35597.262805	31.218560
547.087463	35652.535044	31.223578
547.344480	35704.160494	31.228596
548.266012	35759.813952	31.233613
548.738079	35819.069075	31.238631
549.131723	35862.530386	31.243648
549.723253	35911.839267	31.248666
550.888887	35950.276334	31.253684
551.527791	35993.276402	31.258701
552.011906	36039.236804	31.263719
552.365265	36091.879179	31.268736
553.142375	36137.920887	31.273754
553.154042	36191.404709	31.278772
553.771257	36230.850496	31.283789
554.240849	36287.094811	31.288807
554.996603	36333.399019	31.293824
555.620970	36389.194920	31.298842
555.835744	36451.127756	31.303860
556.405858	36500.202134	31.308877
556.947850	36558.543756	31.313895
557.437073	36601.119888	31.318912
558.020970	36665.142077	31.323930
558.492740	36715.024213	31.328948
559.652961	36754.990172	31.333965
559.758119	36823.686684	31.338983
560.171474	36878.097263	31.344000
560.813261	36930.388878	31.349018
561.143579	36987.720382	31.354036
561.998246	37045.408455	31.359053
562.349658	37103.517441	31.364071
562.822724	37167.518200	31.369088
563.946726	37216.102820	31.374106
564.555828	37267.921379	31.379124
564.944899	37323.948635	31.384141
565.185402	37376.568856	31.389159
565.642933	37432.628140	31.394176
566.538649	37488.075434	31.399194
566.642426	37545.906890	31.404212
567.454640	37591.391988	31.409229
568.183439	37639.132588	31.414247
568.633083	37700.364075	31.419264
568.871373	37749.556436	31.424282
569.210443	37810.339221	31.429300
570.022039	37861.726862	31.434317
570.479754	37920.622712	31.439335
570.697017	37975.739753	31.444352
571.507498	38038.714065	31.449370
571.812706	38106.344847	31.454388
572.538491	38157.455353	31.459405
573.294638	38225.568235	31.464423
573.588613	38303.431693	31.469440
574.343416	38362.474130	31.474458
574.840127	38431.485353	31.479476
575.607511	38483.829578	31.484493
576.191855	38551.632123	31.489511
576.747419	38621.661245	31.494528
577.458259	38673.225080	31.499546
577.763731	38744.185439	31.504564
578.098728	38806.855169	31.509581
579.136353	38877.194892	31.514599
579.650492	38948.244286	31.519616
580.382668	39000.242501	31.524634
580.783111	39076.178256	31.529652
581.465107	39139.978164	31.534669
581.943757	39204.282179	31.539687
582.185391	39265.744823	31.544704
583.184253	39328.159365	31.549722
583.719044	39405.623682	31.554740
583.988926	39476.796182	31.559757
585.032022	39538.304047	31.564775
585.440029	39608.980455	31.569792
586.316634	39678.158579	31.574810
586.691448	39746.013448	31.579828
587.639359	39802.909190	31.584845
588.038500	39861.089406	31.589863
588.683478	39930.387444	31.594880
589.392990	39993.951207	31.599898
590.185597	40056.398114	31.604916
590.862208	40116.081989	31.609933
591.948106	40171.509350	31.614951
592.205656	40227.422053	31.619968
592.921909	40273.390103	31.624986
593.239882	40334.122188	31.630004
593.825248	40396.180717	31.635021
594.597519	40451.800865	31.640039
594.829211	40503.659447	31.645056
595.588075	40566.012666	31.650074
595.648084	40632.139192	31.655092
596.097634	40702.938091	31.660109
597.207733	40765.627197	31.665127
597.576911	40829.718218	31.670144
598.107392	40882.924444	31.675162
598.626250	40952.508495	31.680180
599.227979	41005.259032	31.685197
600.358772	41058.874850	31.690215
600.889939	41113.529399	31.695232
601.651358	41157.240622	31.700250
601.984521	41209.820082	31.705268
602.568864	41270.405826	31.710285
603.080182	41330.438826	31.715303
603.579456	41393.277974	31.720320
603.985227	41451.378954	31.725338
604.594441	41510.744087	31.730356
605.143965	41572.828356	31.735373
605.978312	41633.347178	31.740391
606.169584	41703.238775	31.745408
606.595866	41767.961350	31.750426
607.441851	41840.515470	31.755444
607.938138	41899.259623	31.760461
608.658860	41975.045258	31.765479
609.053158	42051.791634	31.770496
609.525963	42121.412986	31.775514
610.162442	42192.024230	31.780532
610.752711	42268.402854	31.785549
611.647705	42337.175579	31.790567
612.026654	42413.099579	31.795584
613.195484	42485.251720	31.800602
613.491042	42547.903566	31.805620
613.765239	42631.800457	31.810637
614.866075	42701.967625	31.815655
615.300710	42778.177718	31.820672
615.934897	42840.568509	31.825690
616.535087	42916.169282	31.830708
617.670432	42982.896949	31.835725
618.479363	43053.632512	31.840743
618.679875	43129.947682	31.845760
619.395584	43182.532172	31.850778
620.162054	43244.714088	31.855796
620.912669	43313.624102	31.860813
621.478398	43378.453530	31.865831
622.274811	43447.804723	31.870848
622.875686	43504.496716	31.875866
623.390946	43572.899510	31.880884
623.791402	43645.336585	31.885901
624.727123	43707.537374	31.890919
625.465319	43773.063205	31.895936
626.024777	43839.393773	31.900954
626.907842	43897.370190	31.905972
626.833165	43971.732876	31.910989
627.608182	44037.099265	31.916007
628.102781	44114.592764	31.921024
628.582564	44178.700686	31.926042
628.951762	44250.328208	31.931060
629.268764	44327.513389	31.936077
630.293832	44404.554609	31.941095
631.207822	44477.512762	31.946112
631.698340	44550.709010	31.951130
632.632669	44598.426819	31.956148
633.134632	44670.356708	31.961165
634.014357	44729.762370	31.966183
634.623404	44798.877486	31.971200
635.099747	44853.407470	31.976218
635.516102	44924.061742	31.981236
635.791797	44997.123714	31.986253
636.811192	45061.215205	31.991271
637.280266	45143.455847	31.996288
637.898345	45199.529128	32.001306
638.975228	45263.056958	32.006324
639.278695	45334.838213	32.011341
640.063544	45402.728884	32.016359
640.822394	45468.617461	32.021376
641.510022	45541.698140	32.026394
642.295265	45611.485644	32.031412
642.995915	45672.882225	32.036429
643.733872	45732.140357	32.041447
644.174698	45807.785380	32.046464
644.759026	45872.409749	32.051482
645.639742	45921.168229	32.056500
646.069177	45995.544432	32.061517
646.679891	46053.574548	32.066535
647.529031	46132.894601	32.071552
647.583972	46200.582786	32.076570
648.423364	46265.016546	32.081588
649.200964	46353.867665	32.086605
650.591162	46396.438208	32.091623
651.816793	46449.822159	32.096640
652.318083	46511.770853	32.101658
653.073386	46547.302970	32.106676
654.467710	46589.245470	32.111693
655.363402	46613.561181	32.116711
655.965440	46670.591408	32.121728
656.249928	46713.720557	32.126746
656.694590	46753.341077	32.131764
657.244836	46814.071483	32.136781
657.713511	46849.451082	32.141799
658.133969	46912.155512	32.146816
658.846542	46968.601181	32.151834
659.399503	47017.815606	32.156852
659.909384	47082.863300	32.161869
660.533302	47142.623941	32.166887
660.774672	47209.071578	32.171904
661.086881	47266.459093	32.176922
662.109041	47330.381761	32.181940
662.145115	47409.366916	32.186957
662.690314	47466.039609	32.191975
663.254135	47556.306520	32.196992
664.037517	47634.687781	32.202010
664.891438	47712.505985	32.207028
665.093731	47794.293515	32.212045
665.916969	47863.604311	32.217063
666.442638	47944.331348	32.222080
666.839838	48024.397658	32.227098
668.048883	48103.151809	32.232116
668.200271	48188.524267	32.237133
668.714409	48255.216383	32.242151
669.495701	48342.379348	32.247168
670.032835	48435.428574	32.252186
670.999532	48510.562863	32.257204
671.349051	48585.016352	32.262221
672.203018	48667.789614	32.267239
672.843467	48755.137961	32.272256
672.919245	48833.315339	32.277274
674.025135	48914.544480	32.282292
674.288024	49020.136160	32.287309
674.819372	49101.587013	32.292327
675.656722	49199.066961	32.297344
675.995062	49291.716858	32.302362
677.306031	49389.873461	32.307380
677.613981	49482.216786	32.312397
678.583867	49571.772931	32.317415
679.387778	49659.380539	32.322432
679.960824	49746.921200	32.327450
680.850174	49837.990432	32.332468
681.552498	49933.037644	32.337485
682.732324	50009.302462	32.342503
683.726308	50085.281627	32.347520
684.143787	50171.186089	32.352538
684.979747	50257.270478	32.357556
685.524183	50338.746986	32.362573
686.231281	50424.748560	32.367591
687.022105	50502.589028	32.372608
687.566202	50585.830788	32.377626
688.650652	50663.271757	32.382644
689.095417	50757.316635	32.387661
689.679426	50827.081012	32.392679
690.572289	50904.282128	32.397696
691.233257	50996.548660	32.402714
692.421139	51071.257738	32.407732
693.039634	51164.216718	32.412749
693.518519	51244.918812	32.417767
694.544045	51314.040413	32.422784
694.861173	51396.261686	32.427802
695.681282	51468.146459	32.432820
696.304056	51547.848664	32.437837
696.789343	51617.634988	32.442855
697.462224	51701.177011	32.447872
697.970974	51787.970977	32.452890
698.947543	51868.883827	32.457908
699.505054	51963.415713	32.462925
700.338623	52053.283703	32.467943
700.889187	52133.621737	32.472960
701.575910	52228.374299	32.477978
702.226385	52306.339612	32.482996
702.740213	52398.453705	32.488013
703.632767	52479.360579	32.493031
704.447804	52560.254909	32.498048
705.070126	52649.985917	32.503066
705.966868	52725.808686	32.508084
706.755804	52796.195079	32.513101
707.315018	52863.471611	32.518119
708.365425	52936.493362	32.523136
708.930351	53009.346518	32.528154
709.684761	53081.374433	32.533172
709.952807	53152.085015	32.538189
710.423230	53238.295522	32.543207
711.301025	53311.352580	32.548224
711.901474	53404.600567	32.553242
712.623289	53488.944760	32.558260
713.086225	53575.385313	32.563277
713.776423	53660.653821	32.568295
714.485224	53757.932771	32.573312
715.262072	53847.954428	32.578330
716.024752	53927.297649	32.583348
716.664474	54024.147131	32.588365
717.472837	54112.814151	32.593383
718.273120	54189.617944	32.598400
719.270647	54277.977889	32.603418
719.952351	54352.055158	32.608436
720.673935	54447.334578	32.613453
721.802691	54534.143994	32.618471
722.575946	54617.314180	32.623488
723.209150	54699.976751	32.628506
723.857891	54775.800220	32.633524
724.562599	54868.240510	32.638541
724.849081	54953.740328	32.643559
725.791925	55027.952377	32.648576
726.404020	55130.257186	32.653594
727.531428	55216.716530	32.658612
728.023620	55303.444710	32.663629
728.564237	55387.299385	32.668647
729.550588	55482.207449	32.673664
729.985629	55574.533251	32.678682
730.803496	55657.593741	32.683700
731.349327	55750.884515	32.688717
731.797733	55849.560810	32.693735
732.372035	55940.534156	32.698752
733.245276	56046.085482	32.703770
734.022884	56141.942487	32.708788
734.909485	56238.401366	32.713805
735.468685	56330.016711	32.718823
736.493834	56442.292163	32.723840
736.893201	56541.709198	32.728858
737.742876	56636.635519	32.733876
738.913716	56737.225094	32.738893
739.782419	56837.355062	32.743911
740.785423	56921.395675	32.748928
741.412267	57018.790236	32.753946
742.464410	57087.149803	32.758964
743.913852	57155.926228	32.763981
744.570475	57224.923831	32.768999
745.850289	57297.797075	32.774016
746.458752	57376.696775	32.779034
747.158333	57435.671308	32.784052
748.028050	57504.667603	32.789069
748.338956	57569.955257	32.794087
749.224655	57621.551285	32.799104
749.348792	57695.222532	32.804122
749.853190	57766.071142	32.809140
750.385235	57839.564374	32.814157
750.985444	57921.110148	32.819175
751.590193	58005.058084	32.824192
751.962438	58097.409670	32.829210
752.663634	58183.672984	32.834228
753.473608	58273.976268	32.839245
754.181230	58373.401435	32.844263
755.045402	58455.823105	32.849280
755.427915	58557.994054	32.854298
756.118116	58655.999628	32.859316
757.110836	58749.638523	32.864333
757.586481	58851.114302	32.869351
758.393183	58948.281996	32.874368
758.894653	59065.067369	32.879386
759.713986	59161.665860	32.884404
760.782324	59262.629614	32.889421
761.342554	59365.243975	32.894439
762.191373	59472.861501	32.899456
763.225198	59585.943953	32.904474
764.197650	59683.783707	32.909492
764.807030	59789.890917	32.914509
765.422193	59895.899930	32.919527
766.427540	59987.225512	32.924544
767.337363	60072.365586	32.929562
768.375912	60175.883895	32.934580
769.564946	60275.949834	32.939597
770.155037	60375.448583	32.944615
771.274247	60465.040712	32.949632
771.898951	60554.172055	32.954650
772.317007	60647.735127	32.959668
773.289381	60737.143535	32.964685
773.652433	60831.780364	32.969703
774.713186	60922.151264	32.974720
774.958959	61024.376395	32.979738
775.839663	61123.422361	32.984756
777.055269	61214.887806	32.989773
777.652305	61321.242460	32.994791
778.460092	61413.260061	32.999808
779.222896	61515.291878	33.004826
779.714306	61615.292858	33.009844
780.650312	61720.920067	33.014861
781.189467	61830.867629	33.019879
782.153930	61924.327960	33.024896
782.641804	62037.129993	33.029914
782.977422	62138.118492	33.034932
784.384897	62246.449263	33.039949
784.754774	62365.445491	33.044967
785.514781	62472.396455	33.049984
786.308014	62585.929974	33.055002
786.901494	62695.889701	33.060020
787.992754	62785.996256	33.065037
788.730571	62875.250030	33.070055
789.648925	62971.230229	33.075072
790.816527	63075.624976	33.080090
791.294370	63172.131050	33.085108
792.361742	63260.749962	33.090125
792.974555	63363.737735	33.095143
794.101306	63455.215534	33.100160
794.650184	63550.527978	33.105178
795.565206	63653.478690	33.110196
796.697913	63727.925707	33.115213
797.558903	63837.903146	33.120231
798.502102	63927.893416	33.125248
799.025152	64014.110773	33.130266
799.274397	64104.976590	33.135284
800.522853	64202.707410	33.140301
801.236107	64311.353109	33.145319
802.088478	64405.977263	33.150336
802.924224	64496.720006	33.155354
803.662450	64598.488070	33.160372
804.285849	64694.189133	33.165389
805.254797	64805.263479	33.170407
806.026285	64899.969273	33.175424
806.892626	65006.273261	33.180442
807.260270	65108.971535	33.185460
808.682953	65218.194801	33.190477
809.010712	65327.501376	33.195495
810.241184	65424.786509	33.200512
810.681648	65526.692166	33.205530
811.794673	65629.931515	33.210548
812.635324	65726.958075	33.215565
813.031645	65834.500573	33.220583
813.704737	65935.427015	33.225600
814.839587	66047.101182	33.230618
815.695865	66163.178960	33.235636
816.758619	66263.451316	33.240653
817.409159	66371.351150	33.245671
818.290454	66473.687527	33.250688
819.038161	66578.563027	33.255706
819.969148	66680.504097	33.260724
820.938824	66782.622741	33.265741
821.824620	66893.649731	33.270759
822.145571	66997.862646	33.275776
823.342549	67107.110441	33.280794
823.965795	67217.435650	33.285812
825.112608	67313.603378	33.290829
825.690760	67418.005034	33.295847
826.543706	67531.207724	33.300864
827.218120	67640.769121	33.305882
827.919765	67748.065185	33.310900
828.651954	67859.836016	33.315917
829.528296	67984.655326	33.320935
830.288064	68080.648392	33.325952
831.074730	68192.210302	33.330970
831.648247	68308.014260	33.335988
832.504138	68403.823047	33.341005
833.120859	68516.683695	33.346023
833.843387	68638.808784	33.351040
835.067357	68736.424330	33.356058
835.501759	68836.522537	33.361076
836.791263	68941.937380	33.366093
837.107529	69065.077454	33.371111
838.601926	69177.574791	33.376128
839.837112	69278.072189	33.381146
840.357238	69394.996709	33.386164
841.475603	69487.464777	33.391181
842.164895	69599.991592	33.396199
842.803308	69710.391667	33.401216
843.678520	69811.088086	33.406234
844.343893	69930.166080	33.411252
845.088588	70039.236929	33.416269
845.860103	70162.147161	33.421287
846.979858	70271.772468	33.426304
847.637521	70387.088822	33.431322
847.875150	70515.538847	33.436340
848.825571	70634.177683	33.441357
849.905256	70759.374046	33.446375
850.685323	70889.180754	33.451392
851.731116	71002.619242	33.456410
852.677536	71133.557350	33.461428
853.646317	71248.576484	33.466445
854.524245	71372.513552	33.471463
855.377518	71483.679177	33.476480
856.298862	71614.896160	33.481498
856.789737	71736.641362	33.486516
857.969769	71857.847963	33.491533
858.773574	71979.626997	33.496551
859.444448	72112.169830	33.501568
860.338665	72233.158822	33.506586
861.097475	72361.853811	33.511604
862.511465	72487.677694	33.516621
863.153865	72602.112091	33.521639
863.425529	72730.432027	33.526656
864.704293	72851.951244	33.531674
865.388096	72994.052219	33.536692
866.337036	73107.720361	33.541709
867.469393	73234.446856	33.546727
868.400592	73360.782784	33.551744
869.443506	73482.532951	33.556762
869.939357	73620.352276	33.561780
870.756622	73741.672305	33.566797
871.476366	73873.328038	33.571815
872.261501	74011.154566	33.576832
873.671905	74132.085556	33.581850
874.167195	74261.498250	33.586868
875.517622	74397.809280	33.591885
876.963801	74501.737393	33.596903
878.964061	74581.531990	33.601920
880.362387	74684.350107	33.606938
881.222301	74760.351876	33.611956
882.522687	74834.533301	33.616973
883.272524	74919.463859	33.621991
884.039342	74987.341593	33.627008
884.917612	75062.191401	33.632026
885.130390	75150.425123	33.637044
885.728484	75231.260684	33.642061
886.588697	75321.724112	33.647079
887.114329	75420.728688	33.652096
887.824719	75520.273133	33.657114
888.182305	75621.289862	33.662132
889.246424	75722.934090	33.667149
889.775988	75836.431614	33.672167
890.462814	75958.082793	33.677184
891.678986	76056.607713	33.682202
892.378417	76174.655784	33.687220
893.004178	76294.738690	33.692237
893.623970	76416.441205	33.697255
894.260053	76547.520969	33.702272
895.002597	76678.287586	33.707290
896.065747	76822.978080	33.712308
896.794497	76955.467780	33.717325
897.699448	77082.292573	33.722343
898.575825	77230.750995	33.727360
899.457057	77367.529601	33.732378
900.137600	77508.695852	33.737396
900.789059	77657.401742	33.742413
902.015885	77783.288480	33.747431
902.777671	77939.468706	33.752448
903.743358	78068.464239	33.757466
904.694161	78221.260282	33.762484
905.963537	78364.475123	33.767501
906.874420	78504.094609	33.772519
907.405930	78640.779351	33.777536
909.329766	78768.368981	33.782554
909.538266	78909.607349	33.787572
910.806387	79046.133326	33.792589
911.786494	79179.387529	33.797607
912.849785	79320.998378	33.802624
914.039742	79449.056666	33.807642
914.982333	79571.693690	33.812660
916.019316	79704.904313	33.817677
917.095021	79832.098201	33.822695
917.952415	79966.192443	33.827712
919.122100	80082.930284	33.832730
919.875480	80217.959289	33.837748
920.707778	80350.473370	33.842765
921.465122	80461.551836	33.847783
922.618079	80601.829704	33.852800
923.506525	80728.572147	33.857818
924.249774	80867.229175	33.862836
925.474030	80978.792405	33.867853
926.447952	81111.073874	33.872871
926.815578	81240.424609	33.877888
927.913874	81356.453991	33.882906
928.953913	81485.206166	33.887924
929.971645	81605.036433	33.892941
931.149618	81713.108738	33.897959
931.795921	81834.598824	33.902976
932.707888	81940.053161	33.907994
933.643158	82064.716407	33.913012
934.561912	82180.349053	33.918029
935.700959	82292.963342	33.923047
936.366221	82409.301387	33.928064
937.275533	82526.884610	33.933082
938.507830	82646.901657	33.938100
939.162285	82768.490694	33.943117
940.006471	82893.110141	33.948135
940.566142	83022.675250	33.953152
941.628698	83162.074314	33.958170
942.210254	83291.321486	33.963188
943.277059	83431.119955	33.968205
944.592963	83562.066434	33.973223
944.726809	83704.423953	33.978240
945.587157	83838.068400	33.983258
946.822055	83980.910122	33.988276
947.248849	84132.840321	33.993293
948.385621	84279.436251	33.998311
949.134923	84443.235299	34.003328
950.303088	84586.275081	34.008346
951.411379	84732.088350	34.013364
952.841278	84868.234644	34.018381
954.248575	85006.440294	34.023399
954.730521	85147.329503	34.028416
955.808776	85291.014293	34.033434
956.879511	85426.285532	34.038452
957.753087	85562.322455	34.043469
960.134585	85667.352963	34.048487
960.980674	85802.946869	34.053504
962.094979	85921.211877	34.058522
962.762964	86057.196145	34.063540
963.447579	86181.620046	34.068557
964.687988	86300.284413	34.073575
965.096904	86426.751707	34.078592
966.003561	86562.321823	34.083610
967.041303	86701.254868	34.088628
968.236137	86827.074655	34.093645
969.592010	86939.381960	34.098663
970.919898	87074.907270	34.103680
971.919066	87196.144316	34.108698
972.680360	87312.892330	34.113716
973.655734	87441.703668	34.118733
974.777178	87551.806649	34.123751
975.461727	87689.449052	34.128768
976.221470	87825.309774	34.133786
976.994603	87943.988009	34.138804
977.716226	88071.945532	34.143821
978.701416	88208.873111	34.148839
979.264551	88345.255303	34.153856
980.314646	88481.137190	34.158874
981.286310	88615.046738	34.163892
981.944390	88748.861554	34.168909
983.309029	88877.240092	34.173927
983.922498	89014.845318	34.178944
984.842833	89140.444017	34.183962
985.868098	89272.508828	34.188980
986.612983	89414.876608	34.193997
987.296801	89559.930113	34.199015
988.321784	89700.509757	34.204032
989.337255	89841.882339	34.209050
990.450552	89993.055415	34.214068
991.031930	90148.981444	34.219085
991.968839	90288.592307	34.224103
992.742287	90452.186585	34.229120
993.487136	90606.451867	34.234138
994.588272	90770.533961	34.239156
995.325495	90943.807700	34.244173
996.205495	91105.252228	34.249191
997.326258	91276.816880	34.254208
998.655782	91435.738393	34.259226
1000.591377	91591.054457	34.264244
1001.661172	91751.910643	34.269261
1003.060326	91900.837746	34.274279
1003.866549	92040.297113	34.279296
1004.955586	92188.775836	34.284314
1006.292470	92337.292027	34.289332
1006.938761	92494.767622	34.294349
1008.088392	92633.904131	34.299367
1009.186815	92782.473895	34.304384
1010.171614	92934.029169	34.309402
1010.988296	93081.266896	34.314420
1011.735464	93247.694419	34.319437
1013.186487	93391.341821	34.324455
1013.633883	93547.793894	34.329472
1014.862865	93698.189645	34.334490
1015.972821	93854.171605	34.339508
1016.654547	94019.400845	34.344525
1018.161698	94160.526792	34.349543
1019.641347	94309.881057	34.354560
1020.560828	94470.666991	34.359578
1021.650741	94608.756339	34.364596
1022.791082	94754.125546	34.369613
1024.541850	94893.794121	34.374631
1025.744124	95031.520293	34.379648
1026.449953	95167.137601	34.384666
1027.577916	95295.382392	34.389684
1028.467002	95436.614700	34.394701
1029.358729	95572.616054	34.399719
1030.093772	95719.169315	34.404736
1031.250914	95864.618943	34.409754
1032.254802	96007.367423	34.414772
1032.966741	96157.343190	34.419789
1034.052818	96294.595820	34.424807
1034.840054	96449.514790	34.429824
1035.669785	96593.983724	34.434842
1036.776668	96744.381337	34.439860
1037.368295	96893.210784	34.444877
1038.329116	97030.626972	34.449895
1039.371579	97180.107769	34.454912
1040.224483	97327.329593	34.459930
1041.349956	97480.620227	34.464948
1042.201581	97642.818676	34.469965
1043.413638	97793.269761	34.474983
1043.933660	97944.641702	34.480000
1045.029617	98109.233952	34.485018
1046.453662	98263.988061	34.490036
1047.620147	98425.281575	34.495053
1048.869789	98569.082563	34.500071
1049.994160	98746.486270	34.505088
1050.625669	98908.766667	34.510106
1051.989959	99061.789500	34.515124
1052.727183	99223.859177	34.520141
1053.725357	99389.804799	34.525159
1055.211813	99548.107000	34.530176
1055.796139	99714.348555	34.535194
1056.834804	99874.160432	34.540212
1057.796425	100051.524159	34.545229
1058.857225	100223.704257	34.550247
1059.689713	100400.838118	34.555264
1060.468300	100579.051196	34.560282
1061.499407	100755.339969	34.565300
1062.644957	100939.280515	34.570317
1064.028016	101119.875556	34.575335
1064.994486	101304.866175	34.580352
1065.959990	101491.952789	34.585370
1067.527592	101665.803003	34.590388
1068.202031	101845.655847	34.595405
1069.588905	102027.389936	34.600423
1070.429348	102211.192891	34.605440
1071.294282	102399.441735	34.610458
1072.699975	102575.039257	34.615476
1073.782182	102762.117466	34.620493
1075.290018	102936.151146	34.625511
1076.791707	103114.565963	34.630528
1077.345248	103297.246070	34.635546
1078.321682	103466.691879	34.640564
1079.749910	103651.678197	34.645581
1080.693623	103822.365722	34.650599
1081.821527	104004.808077	34.655616
1083.176087	104187.380321	34.660634
1084.640949	104351.673298	34.665652
1085.130235	104526.355316	34.670669
1086.235438	104694.270660	34.675687
1087.659650	104871.844090	34.680704
1088.512194	105047.440394	34.685722
1089.997347	105213.957365	34.690740
1091.156586	105389.368185	34.695757
1092.269431	105558.813569	34.700775
1093.577982	105723.837020	34.705792
1094.398205	105880.256458	34.710810
1095.404449	106038.242146	34.715828
1096.509638	106192.681743	34.720845
1097.201386	106355.883736	34.725863
1098.710413	106514.919112	34.730880
1099.437641	106678.339159	34.735898
1100.098807	106843.251771	34.740916
1101.123639	107011.601216	34.745933
1102.191843	107191.773706	34.750951
1103.161536	107358.109082	34.755968
1104.386061	107538.993463	34.760986
1106.088074	107698.499627	34.766004
1107.473965	107865.652045	34.771021
1108.530698	108024.838937	34.776039
1110.048745	108185.307953	34.781056
1111.160529	108353.532660	34.786074
1112.194747	108504.707145	34.791092
1113.210073	108673.354480	34.796109
1114.302467	108840.610926	34.801127
1115.383730	109005.522082	34.806144
1116.407099	109176.291969	34.811162
1117.639244	109336.535554	34.816180
1118.420352	109514.023940	34.821197
1119.345373	109691.186906	34.826215
1120.637159	109848.569720	34.831232
1121.620075	110037.283869	34.836250
1122.838459	110211.017564	34.841268
1123.661492	110391.410969	34.846285
1125.056170	110579.057363	34.851303
1125.851952	110758.584279	34.856320
1127.153410	110944.222726	34.861338
1128.331429	111122.754679	34.866356
1129.059547	111309.309941	34.871373
1130.367326	111501.553756	34.876391
1131.846878	111678.585857	34.881408
1132.661121	111870.537546	34.886426
1133.959441	112049.879969	34.891444
1135.362456	112233.144440	34.896461
1136.260467	112429.106816	34.901479
1137.456454	112612.812143	34.906496
1138.555005	112802.105048	34.911514
1139.842103	112988.001619	34.916532
1141.213724	113158.142261	34.921549
1142.306095	113341.343996	34.926567
1144.212103	113510.832311	34.931584
1145.101040	113678.464051	34.936602
1146.749335	113836.473869	34.941620
1148.597389	114006.398904	34.946637
1149.779269	114172.581947	34.951655
1151.129744	114331.503217	34.956672
1151.900975	114489.567981	34.961690
1153.299600	114645.679031	34.966708
1153.958216	114809.980593	34.971725
1154.820519	114977.751831	34.976743
1156.162213	115132.070626	34.981760
1156.988308	115295.164814	34.986778
1157.687124	115455.671901	34.991796
1158.642168	115613.885392	34.996813
1159.703017	115786.150795	35.001831
1160.818658	115946.145186	35.006848
1161.818070	116122.177011	35.011866
1162.791559	116289.103507	35.016884
1164.144841	116465.714558	35.021901
1165.007523	116646.058022	35.026919
1166.382991	116823.218841	35.031936
1167.362324	116997.480771	35.036954
1168.129649	117185.833455	35.041972
1169.134520	117366.722880	35.046989
1170.485700	117549.730234	35.052007
1171.830643	117742.832461	35.057024
1172.757534	117943.879189	35.062042
1173.807886	118130.382924	35.067060
1175.441840	118313.819286	35.072077
1176.540895	118513.443755	35.077095
1177.689709	118694.161303	35.082112
1179.067209	118879.636984	35.087130
1180.238576	119075.246197	35.092148
1181.605692	119260.365330	35.097165
1182.888240	119444.562087	35.102183
1184.661048	119627.555085	35.107200
1185.214837	119820.026075	35.112218
1186.364868	120018.267257	35.117236
1187.882246	120202.343374	35.122253
1188.656862	120399.722636	35.127271
1190.042060	120589.242899	35.132288
1191.426053	120778.131488	35.137306
1192.571702	120971.314698	35.142324
1193.992116	121161.542718	35.147341
1194.671487	121360.552775	35.152359
1196.037723	121547.258667	35.157376
1196.674976	121752.382931	35.162394
1198.059144	121952.919190	35.167412
1199.455851	122151.859140	35.172429
1200.186571	122369.942639	35.177447
1201.421126	122573.787733	35.182464
1202.745591	122780.457197	35.187482
1203.399869	122998.330017	35.192500
1205.127927	123202.418100	35.197517
1206.496403	123415.709727	35.202535
1207.358193	123622.725262	35.207552
1208.315601	123832.602408	35.212570
1209.519802	124049.674381	35.217588
1211.067060	124252.861915	35.222605
1212.397958	124484.711548	35.227623
1213.736243	124688.632253	35.232640
1215.438120	124895.372020	35.237658
1216.262244	125104.317605	35.242676
1217.331343	125312.060505	35.247693
1218.801810	125530.571414	35.252711
1220.016280	125735.355715	35.257728
1220.815323	125938.902893	35.262746
1221.874660	126135.430570	35.267764
1223.696520	126334.992592	35.272781
1224.232381	126533.835815	35.277799
1225.673425	126730.015738	35.282816
1227.149006	126931.005261	35.287834
1228.374452	127122.395925	35.292852
1230.289943	127311.854058	35.297869
1231.424282	127509.722469	35.302887
1232.386908	127693.380836	35.307904
1233.641995	127898.301556	35.312922
1234.862362	128093.766228	35.317940
1236.258733	128283.326252	35.322957
1237.447824	128492.075004	35.327975
1238.351219	128695.398001	35.332992
1239.859791	128894.445674	35.338010
1240.652390	129104.870972	35.343028
1242.148720	129302.023224	35.348045
1243.228748	129522.135525	35.353063
1244.534210	129730.380996	35.358080
1245.628091	129934.506238	35.363098
1246.535186	130150.330866	35.368116
1247.953161	130366.354659	35.373133
1249.057445	130590.779025	35.378151
1250.131578	130808.748604	35.383168
1251.473188	131031.884495	35.388186
1252.583601	131253.285170	35.393204
1253.945413	131484.352571	35.398221
1254.989210	131708.618078	35.403239
1256.609567	131928.004494	35.408256
1257.706988	132163.579260	35.413274
1259.000451	132401.430765	35.418292
1260.093030	132616.433868	35.423309
1261.186777	132866.319652	35.428327
1262.224931	133093.650512	35.433344
1263.781083	133333.469946	35.438362
1265.045509	133576.923541	35.443380
1266.168334	133814.497168	35.448397
1267.625125	134065.843511	35.453415
1269.249647	134298.437777	35.458432
1270.321789	134519.096948	35.463450
1271.787052	134758.309161	35.468468
1273.336061	134988.652862	35.473485
1274.743510	135226.712383	35.478503
1275.724724	135457.910350	35.483520
1277.093902	135700.592231	35.488538
1278.359491	135930.088771	35.493556
1279.648542	136158.835755	35.498573
1281.019051	136398.329953	35.503591
1282.578114	136627.912037	35.508608
1283.961472	136855.445639	35.513626
1284.931320	137076.659990	35.518644
1286.750537	137307.777375	35.523661
1288.030355	137540.718425	35.528679
1289.670594	137762.971867	35.533696
1291.046723	137976.740370	35.538714
1292.367779	138176.465272	35.543732
1293.240592	138371.523192	35.548749
1294.411763	138585.341334	35.553767
1295.497123	138793.167721	35.558784
1297.087271	139000.167615	35.563802
1298.219579	139214.541383	35.568820
1299.406149	139423.737432	35.573837
1300.402317	139641.925163	35.578855
1301.871972	139862.016252	35.583872
1303.275616	140081.523797	35.588890
1304.117141	140302.997970	35.593908
1305.475358	140529.258292	35.598925
1306.650578	140748.312732	35.603943
1307.578802	140983.199530	35.608960
1309.222221	141218.443399	35.613978
1310.089389	141463.254584	35.618996
1311.043889	141696.266973	35.624013
1312.571665	141935.349664	35.629031
1313.794314	142188.880695	35.634048
1315.554305	142439.590754	35.639066
1316.897696	142679.202870	35.644084
1318.167182	142917.751266	35.649101
1319.535801	143168.884379	35.654119
1320.990161	143403.199160	35.659136
1322.518938	143642.827337	35.664154
1323.547815	143908.064222	35.669172
1324.929430	144147.060594	35.674189
1326.260405	144401.302416	35.679207
1327.312067	144651.331817	35.684224
1328.698278	144898.344009	35.689242
1329.624707	145153.632272	35.694260
1331.396575	145415.290816	35.699277
1332.428949	145675.357863	35.704295
1333.916777	145937.496882	35.709312
1335.964358	146184.122543	35.714330
1336.934819	146447.970555	35.719348
1338.529781	146693.265099	35.724365
1339.950402	146942.404790	35.729383
1341.130043	147197.555278	35.734400
1342.757393	147446.057600	35.739418
1343.991432	147692.152457	35.744436
1345.757273	147938.418219	35.749453
1347.266091	148181.443466	35.754471
1348.372410	148441.546786	35.759488
1350.151025	148674.150592	35.764506
1351.436801	148920.272012	35.769524
1352.645203	149165.583599	35.774541
1354.173636	149416.310050	35.779559
1355.183799	149663.748658	35.784576
1356.772105	149903.351394	35.789594
1358.291716	150153.856758	35.794612
1359.195966	150396.525696	35.799629
1360.515983	150640.639002	35.804647
1361.808696	150908.744784	35.809664
1363.406211	151145.096996	35.814682
1364.594873	151390.060824	35.819700
1365.610499	151612.588498	35.824717
1367.008700	151851.462360	35.829735
1368.278853	152089.851173	35.834752
1369.827627	152328.095998	35.839770
1371.015874	152573.791340	35.844788
1372.265102	152802.933378	35.849805
1373.786444	153054.855191	35.854823
1375.132972	153296.346782	35.859840
1376.701773	153528.625370	35.864858
1377.911515	153784.126902	35.869876
1379.537957	154026.707698	35.874893
1380.915587	154274.008355	35.879911
1382.160631	154511.518249	35.884928
1383.642749	154757.182917	35.889946
1384.869020	155010.751207	35.894964
1386.226406	155261.473049	35.899981
1387.996451	155519.117572	35.904999
1388.981635	155773.173651	35.910016
1390.311541	156016.500535	35.915034
1391.957353	156282.830805	35.920052
1393.364448	156535.443404	35.925069
1394.905320	156797.356389	35.930087
1396.009299	157054.268766	35.935104
1397.683746	157311.523527	35.940122
1398.953266	157565.065834	35.945140
1400.645757	157819.290923	35.950157
1402.348268	158070.802668	35.955175
1403.449203	158341.140993	35.960192
1405.037806	158593.105751	35.965210
1406.501143	158853.372751	35.970228
1407.521121	159103.453353	35.975245
1409.425669	159354.866156	35.980263
1410.712104	159617.170518	35.985280
1411.914057	159866.377999	35.990298
1413.316780	160139.040900	35.995316
1414.611740	160400.931246	36.000333
1416.446836	160657.652460	36.005351
1417.603836	160924.704550	36.010368
1418.963401	161176.445161	36.015386
1420.378957	161440.365720	36.020404
1421.882030	161712.225776	36.025421
1423.393719	161976.033548	36.030439
1424.493693	162253.123261	36.035456
1425.842909	162511.964088	36.040474
1427.464062	162784.092474	36.045492
1428.754139	163048.032065	36.050509
1430.402506	163308.834840	36.055527
1431.741973	163594.368533	36.060544
1433.502735	163852.202333	36.065562
1435.030643	164121.514650	36.070580
1436.503563	164390.228912	36.075597
1437.846068	164647.640139	36.080615
1438.982791	164914.661426	36.085632
1440.682164	165172.400094	36.090650
1441.995206	165432.243913	36.095668
1443.211505	165680.119362	36.100685
1445.113247	165921.736192	36.105703
1445.925495	166175.551466	36.110720
1447.738642	166417.147531	36.115738
1449.412104	166666.453527	36.120756
1450.259768	166924.491839	36.125773
1451.871890	167168.534555	36.130791
1453.253133	167445.263430	36.135808
1454.961304	167698.071446	36.140826
1456.344720	167960.369567	36.145844
1457.586150	168220.155261	36.150861
1459.421236	168470.449506	36.155879
1460.585097	168738.977697	36.160896
1462.119288	169001.182913	36.165914
1463.408978	169267.551174	36.170932
1465.134545	169533.408071	36.175949
1466.487666	169800.746640	36.180967
1467.825947	170066.338941	36.185984
1470.065402	170316.213097	36.191002
1471.541456	170580.861048	36.196020
1472.744223	170842.256156	36.201037
1474.456527	171098.561510	36.206055
1475.852656	171378.030873	36.211072
1477.295061	171638.416474	36.216090
1479.055249	171898.157104	36.221108
1480.612605	172162.333458	36.226125
1482.194219	172422.131275	36.231143
1483.403867	172692.556861	36.236160
1485.000249	172954.918275	36.241178
1486.383431	173224.343115	36.246196
1487.962150	173494.246131	36.251213
1489.900345	173743.923469	36.256231
1491.316917	174013.855741	36.261248
1492.583300	174276.227488	36.266266
1494.309441	174538.756244	36.271284
1495.592412	174813.370852	36.276301
1496.921357	175079.315342	36.281319
1498.094652	175357.782277	36.286336
1499.518821	175630.045681	36.291354
1500.845407	175915.812091	36.296372
1502.193086	176204.482354	36.301389
1503.864950	176474.809024	36.306407
1505.050912	176775.256784	36.311424
1506.219456	177064.164496	36.316442
1507.904316	177349.731659	36.321460
1509.297860	177655.519355	36.326477
1510.599671	177943.536585	36.331495
1512.185994	178242.243928	36.336512
1513.596920	178546.665143	36.341530
1515.198098	178840.971893	36.346548
1516.970135	179146.469232	36.351565
1518.554713	179443.599412	36.356583
1519.868852	179745.456352	36.361600
1521.759739	180025.921163	36.366618
1523.942704	180298.208548	36.371636
1525.362879	180574.526695	36.376653
1526.898160	180840.119712	36.381671
1528.242969	181114.321713	36.386688
1529.829506	181385.695666	36.391706
1531.292896	181650.784857	36.396724
1532.431560	181937.471887	36.401741
1533.698740	182209.295031	36.406759
1535.462025	182485.545434	36.411776
1536.580767	182768.878629	36.416794
1538.350564	183056.487775	36.421812
1539.558864	183354.148580	36.426829
1540.886723	183631.236629	36.431847
1542.330047	183929.434939	36.436864
1544.222435	184233.692644	36.441882
1545.551525	184533.892592	36.446900
1547.193602	184844.703649	36.451917
1548.824483	185129.569286	36.456935
1550.211217	185449.561253	36.461952
1551.382323	185751.494731	36.466970
1553.552916	186060.783575	36.471988
1554.566841	186379.356616	36.477005
1556.224119	186695.964299	36.482023
1557.697297	187018.313754	36.487040
1559.181450	187338.379551	36.492058
1560.942653	187648.873464	36.497076
1562.989914	187961.684335	36.502093
1565.230255	188258.984804	36.507111
1567.071810	188578.583559	36.512128
1568.564384	188892.922724	36.517146
1570.474171	189190.141984	36.522164
1572.323089	189493.108811	36.527181
1573.588614	189783.061019	36.532199
1575.339007	190082.252800	36.537216
1576.827847	190378.137677	36.542234
1578.474601	190679.430893	36.547252
1579.933641	190983.801582	36.552269
1581.442521	191268.089389	36.557287
1583.337273	191579.069971	36.562304
1584.467312	191890.224759	36.567322
1586.401680	192182.344095	36.572340
1587.871818	192485.618257	36.577357
1589.208933	192786.275639	36.582375
1591.165086	193086.595386	36.587392
1592.868680	193392.350891	36.592410
1594.171612	193697.575408	36.597428
1595.447771	194002.920258	36.602445
1597.185848	194311.315727	36.607463
1598.824679	194627.546913	36.612480
1599.978600	194935.137855	36.617498
1601.850562	195248.734072	36.622516
1603.279122	195563.633752	36.627533
1605.009564	195874.438676	36.632551
1606.706615	196186.063070	36.637568
1608.345332	196490.222941	36.642586
1610.046882	196777.671672	36.647604
1611.739080	197078.704210	36.652621
1613.085777	197352.200192	36.657639
1614.942270	197640.987143	36.662656
1615.995422	197935.881424	36.667674
1618.108254	198229.885574	36.672692
1619.472945	198520.443546	36.677709
1621.095050	198823.896074	36.682727
1622.520775	199113.571784	36.687744
1623.897061	199416.533611	36.692762
1625.613362	199718.719644	36.697780
1627.379002	200038.974329	36.702797
1628.797909	200340.969892	36.707815
1630.166645	200648.014261	36.712832
1631.650549	200968.661857	36.717850
1633.440647	201287.498328	36.722868
1635.161226	201607.083891	36.727885
1636.434104	201933.685692	36.732903
1638.053405	202260.437484	36.737920
1639.492907	202598.694718	36.742938
1641.430690	202918.786413	36.747956
1643.132179	203266.856310	36.752973
1644.200134	203589.565203	36.757991
1646.338199	203915.241361	36.763008
1647.989006	204261.738638	36.768026
1649.990559	204603.764782	36.773044
1651.610911	204933.578302	36.778061
1653.298241	205274.058841	36.783079
1654.970956	205607.447609	36.788096
1656.491035	205950.395928	36.793114
1658.294453	206272.063554	36.798132
1659.540897	206622.929734	36.803149
1661.467884	206969.856161	36.808167
1663.041157	207315.812504	36.813184
1664.567189	207659.874135	36.818202
1667.093865	207994.080041	36.823220
1668.787071	208334.107411	36.828237
1670.325792	208680.864098	36.833255
1672.040614	209007.524064	36.838272
1674.138104	209353.091342	36.843290
1676.374098	209674.505196	36.848308
1677.675919	210005.323809	36.853325
1679.403584	210338.856798	36.858343
1681.080501	210664.592010	36.863360
1682.307686	211007.031215	36.868378
1683.903097	211343.561201	36.873396
1685.790341	211680.922602	36.878413
1687.303224	212026.064110	36.883431
1689.112449	212361.473645	36.888448
1690.635976	212716.100754	36.893466
1692.458090	213048.261676	36.898484
1693.871209	213397.031862	36.903501
1695.669318	213737.604694	36.908519
1697.526839	214071.694903	36.913536
1699.217805	214423.905039	36.918554
1700.810659	214745.357312	36.923572
1702.845208	215064.950824	36.928589
1704.349583	215380.338708	36.933607
1706.254768	215694.762970	36.938624
1707.502915	216008.366166	36.943642
1709.466809	216330.503360	36.948660
1711.181378	216655.944616	36.953677
1712.590209	216974.808369	36.958695
1714.486954	217304.718266	36.963712
1715.753014	217643.668248	36.968730
1717.359466	217976.027018	36.973748
1719.652988	218296.279843	36.978765
1721.564536	218625.749118	36.983783
1723.230151	218951.475286	36.988800
1724.951975	219296.150443	36.993818
1727.018686	219613.143904	36.998836
1728.548230	219953.205593	37.003853
1729.869678	220292.616239	37.008871
1732.151745	220631.215661	37.013888
1733.942976	220973.145020	37.018906
1735.317939	221303.244710	37.023924
1736.586893	221689.903705	37.028941
1738.239676	222046.626830	37.033959
1740.258663	222390.164339	37.038976
1741.850316	222755.445798	37.043994
1743.690125	223104.411334	37.049012
1745.268624	223454.791246	37.054029
1746.854412	223815.977242	37.059047
1749.137838	224158.007570	37.064064
1750.704468	224513.396911	37.069082
1752.572697	224870.009713	37.074100
1754.575615	225223.936143	37.079117
1756.627440	225586.097287	37.084135
1758.034391	225931.740752	37.089152
1760.040330	226291.207595	37.094170
1761.562684	226640.975233	37.099188
1763.539297	227005.071884	37.104205
1765.105471	227365.197232	37.109223
1767.156759	227716.612276	37.114240
1769.088865	228075.971406	37.119258
1770.759271	228439.132277	37.124276
1772.592862	228789.494161	37.129293
1774.124177	229141.530823	37.134311
1776.013100	229505.397898	37.139328
1777.641058	229875.047622	37.144346
1779.236811	230223.700486	37.149364
1781.374699	230587.684778	37.154381
1783.145350	230947.004895	37.159399
1785.221879	231313.033581	37.164416
1786.885776	231667.090748	37.169434
1788.698387	232019.703368	37.174452
1790.791184	232386.800350	37.179469
1792.436454	232741.143854	37.184487
1794.233054	233097.572666	37.189504
1796.043005	233449.403615	37.194522
1797.788753	233790.680387	37.199540
1799.567150	234113.082266	37.204557
1801.216931	234457.043373	37.209575
1803.082213	234779.459002	37.214592
1804.754309	235120.244025	37.219610
1806.615012	235462.778143	37.224628
1808.432541	235799.681751	37.229645
1810.113864	236136.582672	37.234663
1812.273145	236470.259351	37.239680
1813.925494	236811.230837	37.244698
1815.731583	237147.556393	37.249716
1817.982235	237492.625902	37.254733
1819.718330	237837.803583	37.259751
1821.625751	238167.918822	37.264768
1823.086838	238504.506512	37.269786
1824.790310	238860.563450	37.274804
1826.688964	239206.583149	37.279821
1828.296890	239561.539878	37.284839
1830.039817	239922.800771	37.289856
1831.524549	240284.230767	37.294874
1833.437941	240646.762223	37.299892
1835.685124	241011.324589	37.304909
1837.142702	241381.575974	37.309927
1838.896191	241743.882123	37.314944
1840.626542	242118.207243	37.319962
1842.248733	242492.398258	37.324980
1844.494914	242861.233502	37.329997
1845.938724	243248.155175	37.335015
1848.236966	243623.055025	37.340032
1850.011343	244010.739323	37.345050
1851.918126	244382.503026	37.350068
1853.867351	244768.612358	37.355085
1855.545497	245159.998354	37.360103
1857.422707	245543.022436	37.365120
1859.278775	245929.429238	37.370138
1861.187685	246316.920953	37.375156
1863.258801	246699.511000	37.380173
1865.375137	247087.886313	37.385191
1867.461311	247465.243382	37.390208
1869.177242	247841.491722	37.395226
1871.108990	248229.569109	37.400244
1873.452538	248607.701036	37.405261
1875.089227	248986.225489	37.410279
1877.157232	249362.675692	37.415296
1879.445945	249730.480670	37.420314
1881.338395	250110.973920	37.425332
1882.998411	250479.286793	37.430349
1885.023105	250850.438388	37.435367
1887.398475	251220.087249	37.440384
1889.269345	251588.546888	37.445402
1891.086479	251951.732264	37.450420
1893.514895	252307.962883	37.455437
1894.931583	252672.051537	37.460455
1896.844225	253034.817514	37.465472
1899.468422	253374.787317	37.470490
1901.725133	253703.740777	37.475508
1904.270110	254017.865061	37.480525
1906.116242	254330.602035	37.485543
1908.485244	254628.777312	37.490560
1910.544174	254922.506058	37.495578
1912.012868	255228.090117	37.500596
1913.943055	255521.001880	37.505613
1915.320048	255834.526881	37.510631
1917.370688	256151.603374	37.515648
1918.861066	256465.035095	37.520666
1920.708321	256781.408111	37.525684
1922.717177	257100.143757	37.530701
1924.479788	257429.384740	37.535719
1926.235230	257746.434129	37.540736
1928.056933	258069.239802	37.545754
1929.411102	258411.984903	37.550772
1931.400045	258741.140972	37.555789
1933.099575	259094.374288	37.560807
1934.782189	259435.823937	37.565824
1936.836023	259787.274592	37.570842
1938.282945	260145.706156	37.575860
1940.379450	260493.772392	37.580877
1941.974755	260872.782988	37.585895
1943.986994	261231.888312	37.590912
1945.667167	261606.618716	37.595930
1947.670482	261983.711579	37.600948
1949.640137	262358.168333	37.605965
1951.371342	262746.228534	37.610983
1953.386444	263134.955422	37.616000
1955.246725	263515.451337	37.621018
1957.232837	263908.248166	37.626036
1959.181782	264291.855403	37.631053
1961.236418	264690.815124	37.636071
1963.715294	265073.272118	37.641088
1965.332459	265460.870614	37.646106
1967.320512	265854.735999	37.651124
1969.744700	266232.833365	37.656141
1971.918857	266623.316665	37.661159
1973.861544	267010.534588	37.666176
1976.110548	267397.627991	37.671194
1978.307403	267770.758158	37.676212
1980.627362	268155.376722	37.681229
1982.320049	268541.314418	37.686247
1984.549646	268908.724364	37.691264
1986.342432	269289.210315	37.696282
1988.409334	269667.188853	37.701300
1990.747314	270042.914479	37.706317
1992.681314	270419.415665	37.711335
1994.577687	270797.396376	37.716352
1996.803913	271168.389780	37.721370
1998.836100	271548.660929	37.726388
2000.851527	271920.653355	37.731405
2002.672290	272294.734446	37.736423
2005.030418	272661.592018	37.741440
2007.014459	273018.220641	37.746458
2009.078117	273371.686671	37.751476
2011.121061	273713.495873	37.756493
2013.191107	274051.769738	37.761511
2014.704642	274396.330353	37.766528
2016.852890	274737.386231	37.771546
2018.650855	275089.548175	37.776564
2020.668936	275436.797740	37.781581
2022.324078	275789.947656	37.786599
2024.440386	276147.749420	37.791616
2026.757948	276494.265511	37.796634
2028.196189	276869.474485	37.801652
2030.352892	277230.572140	37.806669
2032.540957	277592.934920	37.811687
2034.189414	277971.463564	37.816704
2036.056215	278337.179567	37.821722
2038.067569	278719.435525	37.826740
2039.980925	279100.919393	37.831757
2041.993668	279486.172448	37.836775
2044.047596	279873.425669	37.841792
2046.219248	280244.173277	37.846810
2048.135753	280642.955637	37.851828
2050.223250	281029.491664	37.856845
2052.121697	281423.246591	37.861863
2054.381809	281822.634233	37.866880
2056.207708	282216.450968	37.871898
2058.508057	282619.972410	37.876916
2060.511360	283012.515675	37.881933
2062.535701	283421.973826	37.886951
2064.476057	283834.391722	37.891968
2067.016679	284228.398361	37.896986
2068.896946	284651.367349	37.902004
2070.545523	285059.257823	37.907021
2072.959741	285474.393326	37.912039
2075.182165	285888.999944	37.917056
2077.363586	286293.934060	37.922074
2079.389753	286705.446319	37.927092
2081.545842	287118.258437	37.932109
2083.588738	287537.032289	37.937127
2085.506057	287952.396131	37.942144
2088.187578	288361.084271	37.947162
2090.002956	288782.280425	37.952180
2091.980890	289194.711638	37.957197
2094.437101	289601.884237	37.962215
2096.274680	290025.843948	37.967232
2098.608761	290433.822173	37.972250
2100.635670	290849.774111	37.977268
2102.748719	291267.769325	37.982285
2104.877276	291683.576764	37.987303
2106.946679	292113.440461	37.992320
2109.365317	292515.508510	37.997338
2111.305689	292942.850916	38.002356
2113.396898	293351.726479	38.007373
2115.958615	293765.988163	38.012391
2118.025699	294174.662805	38.017408
2120.342505	294576.336847	38.022426
2122.337267	294968.433772	38.027444
2125.237879	295337.727580	38.032461
2127.516724	295695.231152	38.037479
2129.320210	296061.623974	38.042496
2132.105920	296423.338769	38.047514
2134.148497	296790.174920	38.052532
2135.984823	297154.477474	38.057549
2138.321146	297518.979430	38.062567
2140.293144	297884.757719	38.067584
2142.175867	298247.679022	38.072602
2144.202290	298628.002333	38.077620
2146.123432	299004.709073	38.082637
2148.036117	299386.776048	38.087655
2149.684098	299787.935257	38.092672
2152.142198	300163.411162	38.097690
2154.318541	300558.820163	38.102708
2155.740343	300971.417531	38.107725
2158.018876	301364.039573	38.112743
2160.252632	301772.670464	38.117760
2162.576823	302181.285919	38.122778
2164.531741	302587.317115	38.127796
2166.988912	303005.307607	38.132813
2169.154355	303418.898007	38.137831
2170.709124	303832.304651	38.142848
2172.704053	304248.586772	38.147866
2174.910466	304689.066351	38.152884
2177.313540	305104.925563	38.157901
2179.676419	305526.098581	38.162919
2181.707462	305962.944159	38.167936
2183.943640	306391.729250	38.172954
2185.852823	306837.582954	38.177972
2188.092542	307280.512472	38.182989
2190.434307	307718.369641	38.188007
2192.501892	308160.180350	38.193024
2194.704449	308605.193856	38.198042
2196.853377	309052.093821	38.203060
2199.095505	309500.450524	38.208077
2201.259557	309949.579896	38.213095
2203.173795	310398.848752	38.218112
2205.810928	310853.766893	38.223130
2207.918549	311319.155497	38.228148
2210.339007	311765.366969	38.233165
2212.660875	312214.030595	38.238183
2214.773740	312669.786446	38.243200
2217.622441	313122.325037	38.248218
2219.621740	313571.999345	38.253236
2221.588157	314028.382204	38.258253
2224.148099	314479.513053	38.263271
2226.837673	314917.617373	38.268288
2229.368008	315362.475625	38.273306
2231.508170	315791.723078	38.278324
2233.814731	316227.926789	38.283341
2236.078264	316666.827588	38.288359
2238.195848	317124.213827	38.293376
2240.806237	317540.121402	38.298394
2242.909590	317962.888743	38.303412
2244.721483	318370.563473	38.308429
2247.137940	318768.921309	38.313447
2249.279895	319184.057809	38.318464
2250.910486	319592.517861	38.323482
2253.307349	320009.489611	38.328500
2255.339303	320438.784045	38.333517
2257.342366	320850.582567	38.338535
2259.655889	321290.774314	38.343552
2261.526662	321710.386611	38.348570
2264.173101	322145.035621	38.353588
2266.179993	322600.075536	38.358605
2268.825254	323036.040847	38.363623
2270.868098	323486.168865	38.368640
2273.124137	323916.858162	38.373658
2275.266239	324373.797188	38.378676
2277.322579	324824.931672	38.383693
2279.581723	325281.770910	38.388711
2281.498986	325740.337874	38.393728
2283.999898	326198.377973	38.398746
2286.147519	326669.169000	38.403764
2288.146144	327153.592532	38.408781
2290.848847	327620.937724	38.413799
2293.145986	328100.102111	38.418816
2295.426655	328583.633970	38.423834
2297.597523	329057.708087	38.428852
2299.638139	329545.792051	38.433869
2302.423045	330034.211930	38.438887
2304.669448	330521.114148	38.443904
2307.185866	330991.464463	38.448922
2309.900392	331478.489248	38.453940
2311.932737	331958.153260	38.458957
2314.565998	332437.007790	38.463975
2317.249883	332919.380689	38.468992
2319.228571	333399.779865	38.474010
2321.458128	333884.528892	38.479028
2323.849388	334369.756741	38.484045
2326.595913	334848.322859	38.489063
2329.301622	335330.599331	38.494080
2331.689767	335811.399188	38.499098
2334.418492	336279.014091	38.504116
2336.619614	336755.317075	38.509133
2339.422840	337216.667236	38.514151
2341.890461	337681.926808	38.519168
2344.326594	338152.393199	38.524186
2346.614445	338604.649062	38.529204
2349.051222	339079.298058	38.534221
2351.698850	339528.240353	38.539239
2353.532368	339999.677324	38.544256
2356.289906	340450.068259	38.549274
2359.454739	340894.018517	38.554292
2362.634469	341324.912915	38.559309
2365.059426	341762.855271	38.564327
2367.647894	342186.728256	38.569344
2369.597785	342604.352200	38.574362
2372.156734	343007.963539	38.579380
2373.650730	343409.354405	38.584397
2376.526526	343807.146860	38.589415
2378.684296	344210.661308	38.594432
2380.732934	344600.455205	38.599450
2383.031910	345000.590587	38.604468
2385.170162	345416.946225	38.609485
2387.214322	345825.595892	38.614503
2389.145734	346251.041739	38.619520
2391.095374	346683.996210	38.624538
2393.253458	347120.011588	38.629556
2395.193917	347573.245108	38.634573
2397.567796	348015.667656	38.639591
2399.615047	348476.340663	38.644608
2401.891640	348933.495562	38.649626
2404.713057	349402.161808	38.654644
2406.417242	349875.392881	38.659661
2408.829410	350344.090518	38.664679
2411.077990	350838.322461	38.669696
2413.453054	351325.168085	38.674714
2415.904291	351808.189441	38.679732
2418.118926	352310.206351	38.684749
2420.681073	352798.252665	38.689767
2423.342029	353300.823993	38.694784
2425.726699	353807.952620	38.699802
2428.217429	354312.977992	38.704820
2430.589303	354825.860762	38.709837
2432.975101	355337.771607	38.714855
2435.056143	355848.456429	38.719872
2437.742770	356361.502241	38.724890
2440.324987	356878.062134	38.729908
2442.694358	357395.741834	38.734925
2445.457268	357913.785245	38.739943
2448.101536	358435.598494	38.744960
2450.484602	358970.366726	38.749978
2453.337352	359472.262138	38.754996
2455.819391	359987.586823	38.760013
2458.415534	360508.090920	38.765031
2461.030481	361018.992571	38.770048
2463.582280	361529.771817	38.775066
2466.373828	362034.619410	38.780084
2469.111423	362546.728660	38.785101
2471.528800	363055.862883	38.790119
2474.254265	363558.953240	38.795136
2476.418547	364077.531898	38.800154
2479.090947	364575.949827	38.805172
2481.448257	365084.893396	38.810189
2484.141376	365590.326638	38.815207
2486.762515	366106.500317	38.820224
2489.194220	366613.283082	38.825242
2491.671600	367119.266147	38.830260
2494.081987	367635.937626	38.835277
2496.505205	368135.751071	38.840295
2498.865098	368640.060409	38.845312
2501.064349	369138.958928	38.850330
2503.763413	369620.390260	38.855348
2505.923914	370106.672087	38.860365
2508.409806	370590.892213	38.865383
2511.002814	371071.512034	38.870400
2513.218495	371552.135441	38.875418
2515.791763	372048.403279	38.880436
2517.979479	372529.527432	38.885453
2520.311188	373018.260650	38.890471
2523.281438	373518.964591	38.895488
2525.413821	374025.199639	38.900506
2528.397594	374520.028141	38.905524
2530.549329	375020.285285	38.910541
2533.256499	375519.915470	38.915559
2535.407730	376034.241633	38.920576
2537.992447	376552.146020	38.925594
2540.493981	377069.498733	38.930612
2543.087347	377602.686837	38.935629
2545.441360	378126.112761	38.940647
2548.016709	378642.240870	38.945664
2550.220994	379179.452401	38.950682
2552.816688	379709.440403	38.955700
2555.320051	380261.506768	38.960717
2557.724937	380803.560273	38.965735
2560.114874	381352.660867	38.970752
2562.668094	381910.961604	38.975770
2565.655273	382456.603147	38.980788
2568.334970	383018.520475	38.985805
2570.908038	383575.246140	38.990823
2573.835571	384132.541540	38.995840
2575.758274	384696.329278	39.000858
2578.761535	385256.994868	39.005876
2581.399835	385817.481467	39.010893
2584.046458	386376.740682	39.015911
2586.522842	386946.240153	39.020928
2588.909903	387519.422630	39.025946
2591.769352	388078.926306	39.030964
2594.555337	388651.976863	39.035981
2596.780018	389223.636120	39.040999
2599.998188	389786.353443	39.046016
2602.749714	390369.247792	39.051034
2605.538418	390930.417126	39.056052
2608.042365	391497.125962	39.061069
2610.799376	392073.879085	39.066087
2613.675216	392634.449290	39.071104
2616.256773	393188.615603	39.076122
2618.919469	393750.444068	39.081140
2621.428353	394320.148993	39.086157
2624.362709	394878.416326	39.091175
2627.409062	395438.406448	39.096192
2629.895861	396001.062408	39.101210
2632.674411	396565.412397	39.106228
2635.315040	397126.097949	39.111245
2637.860985	397677.838197	39.116263
2640.739167	398228.324900	39.121280
2643.244404	398774.145327	39.126298
2645.824818	399294.006316	39.131316
2648.215797	399821.064481	39.136333
2650.885523	400331.919160	39.141351
2653.875084	400850.321361	39.146368
2655.862988	401373.893914	39.151386
2658.495448	401890.003413	39.156404
2661.426909	402417.009671	39.161421
2664.038261	402937.669107	39.166439
2667.061568	403456.277306	39.171456
2669.244091	403991.007021	39.176474
2671.648875	404517.960356	39.181492
2674.581945	405058.079606	39.186509
2677.008078	405598.675409	39.191527
2679.850092	406137.598914	39.196544
2682.255151	406688.319019	39.201562
2684.786995	407223.419611	39.206580
2687.439714	407785.766731	39.211597
2689.661256	408345.459561	39.216615
2692.691932	408907.244555	39.221632
2695.390567	409475.002947	39.226650
2698.187439	410039.668171	39.231668
2701.044760	410603.882337	39.236685
2703.752154	411183.773228	39.241703
2706.365880	411743.062065	39.246720
2709.043376	412330.766998	39.251738
2711.676212	412915.907564	39.256756
2714.394812	413492.380734	39.261773
2717.138231	414072.158594	39.266791
2720.020178	414651.244095	39.271808
2722.641693	415255.169262	39.276826
2725.355657	415842.189679	39.281844
2728.456105	416424.600884	39.286861
2731.018390	417017.449791	39.291879
2734.314523	417596.866666	39.296896
2737.197102	418184.420548	39.301914
2739.798722	418756.271210	39.306932
2742.836788	419347.095737	39.311949
2745.614363	419935.161922	39.316967
2748.599743	420514.340086	39.321984
2751.012500	421098.258886	39.327002
2754.054779	421680.621559	39.332020
2757.312095	422258.250792	39.337037
2759.482364	422845.540781	39.342055
2763.017236	423423.076262	39.347072
2765.901523	424004.072004	39.352090
2768.701424	424577.975276	39.357108
2771.718641	425154.390645	39.362125
2774.307262	425724.477756	39.367143
2777.325649	426294.307422	39.372160
2779.658608	426874.391451	39.377178
2782.355850	427439.738560	39.382196
2785.213763	428016.801550	39.387213
2787.617779	428598.153935	39.392231
2790.672490	429174.400619	39.397248
2793.592767	429745.235601	39.402266
2796.113649	430297.429135	39.407284
2798.507825	430835.599491	39.412301
2801.153077	431385.496117	39.417319
2803.861280	431916.756010	39.422336
2806.236380	432484.071490	39.427354
2809.082258	433036.256545	39.432372
2811.867188	433599.202501	39.437389
2813.899764	434172.359629	39.442407
2816.343908	434752.883924	39.447424
2819.119287	435338.103278	39.452442
2821.693914	435926.582173	39.457460
2824.765213	436528.034893	39.462477
2827.350947	437138.210014	39.467495
2830.164777	437739.092015	39.472512
2832.317434	438363.966500	39.477530
2835.214438	438979.161921	39.482548
2838.268311	439606.293064	39.487565
2840.528392	440247.762781	39.492583
2844.049569	440876.661070	39.497600
2846.558480	441514.007382	39.502618
2849.025542	442168.963781	39.507636
2852.123738	442811.195388	39.512653
2855.303932	443474.509593	39.517671
2858.463568	444117.557351	39.522688
2861.209791	444772.348156	39.527706
2864.052663	445428.523210	39.532724
2867.145360	446076.540703	39.537741
2869.855906	446739.180357	39.542759
2873.000784	447402.036367	39.547776
2875.867856	448067.246166	39.552794
2878.644066	448744.498664	39.557812
2881.669797	449408.430289	39.562829
2884.407165	450081.246316	39.567847
2887.483015	450746.801967	39.572864
2890.708886	451421.576773	39.577882
2893.434486	452094.943189	39.582900
2896.956765	452755.966707	39.587917
2899.808208	453430.032937	39.592935
2903.213012	454094.528075	39.597952
2906.290809	454750.958572	39.602970
2909.338278	455416.989456	39.607988
2912.406708	456074.647854	39.613005
2915.202921	456736.125041	39.618023
2918.434338	457391.694763	39.623040
2921.252440	458039.720841	39.628058
2924.393929	458696.581695	39.633076
2927.432311	459350.049413	39.638093
2930.329596	460006.100257	39.643111
2933.358130	460649.563858	39.648128
2936.760898	461289.660845	39.653146
2939.330545	461935.536760	39.658164
2942.375432	462594.824994	39.663181
2945.334367	463245.456492	39.668199
2948.447132	463879.502871	39.673216
2951.679316	464508.857945	39.678234
2954.177549	465123.793760	39.683252
2957.161811	465709.450255	39.688269
2959.723902	466317.765976	39.693287
2962.494824	466920.518231	39.698304
2965.532826	467526.346649	39.703322
2968.136248	468123.274727	39.708340
2971.455525	468735.345440	39.713357
2974.196014	469355.682309	39.718375
2977.532868	469958.358610	39.723392
2980.500651	470567.346240	39.728410
2983.362483	471187.861888	39.733428
2986.436231	471809.538860	39.738445
2989.294015	472445.844055	39.743463
2991.953493	473059.306790	39.748480
2995.164399	473695.618283	39.753498
2997.791049	474328.817091	39.758516
3000.728362	474963.969240	39.763533
3003.677127	475616.490761	39.768551
3006.789715	476251.220717	39.773568
3009.897982	476896.395632	39.778586
3012.396902	477556.861941	39.783604
3015.605783	478209.662199	39.788621
3018.675709	478879.295286	39.793639
3021.467652	479536.616543	39.798656
3024.370057	480202.895263	39.803674
3027.327349	480883.041855	39.808692
3030.543618	481556.098727	39.813709
3033.600792	482234.312533	39.818727
3036.926553	482916.705319	39.823744
3040.308324	483579.204875	39.828762
3043.344595	484262.404611	39.833780
3046.795370	484930.152895	39.838797
3049.542286	485613.906269	39.843815
3052.606195	486284.548804	39.848832
3056.033719	486965.266042	39.853850
3059.015507	487640.976979	39.858868
3061.724556	488320.849850	39.863885
3064.956819	489017.034781	39.868903
3067.980562	489697.515539	39.873920
3071.123383	490377.750720	39.878938
3074.103580	491075.970373	39.883956
3077.479960	491770.262180	39.888973
3080.472534	492453.122638	39.893991
3083.676605	493137.389249	39.899008
3086.748088	493837.561454	39.904026
3089.714984	494527.571881	39.909044
3092.823437	495207.231138	39.914061
3096.236573	495903.937165	39.919079
3099.294941	496590.471643	39.924096
3102.633685	497281.783665	39.929114
3105.696977	497978.112017	39.934132
3108.950466	498672.919087	39.939149
3111.931888	499366.328582	39.944167
3114.759768	500067.662577	39.949184
3117.618376	500736.399086	39.954202
3120.593087	501418.269171	39.959220
3123.307421	502070.267298	39.964237
3126.371264	502722.489044	39.969255
3129.334958	503388.635332	39.974272
3132.330207	504054.953352	39.979290
3135.115618	504740.763483	39.984308
3138.008088	505406.188304	39.989325
3141.232075	506098.538525	39.994343
3143.869143	506790.853098	39.999360
3147.031741	507481.340964	40.004378
3149.838276	508193.003332	40.009396
3153.022293	508903.567317	40.014413
3155.810554	509629.908966	40.019431
3158.933269	510352.331901	40.024448
3162.057598	511078.104752	40.029466
3164.977298	511828.653153	40.034484
3168.419918	512551.234910	40.039501
3171.349654	513300.051548	40.044519
3174.398987	514060.570814	40.049536
3177.751747	514809.455196	40.054554
3180.996661	515583.898877	40.059572
3184.226776	516333.642412	40.064589
3187.588124	517109.005674	40.069607
3190.961278	517866.627006	40.074624
3194.400667	518629.902403	40.079642
3197.331550	519406.335597	40.084660
3201.129948	520167.263808	40.089677
3204.721415	520940.040152	40.094695
3207.924070	521697.713459	40.099712
3211.388780	522458.032932	40.104730
3214.931988	523216.791686	40.109748
3218.248597	523981.853079	40.114765
3221.534055	524744.463057	40.119783
3225.058981	525506.797296	40.124800
3228.475745	526251.014361	40.129818
3231.722314	527007.422826	40.134836
3234.986356	527767.119462	40.139853
3238.487140	528513.687371	40.144871
3241.745272	529266.861155	40.149888
3245.215577	530017.042190	40.154906
3248.375858	530769.353154	40.159924
3251.716557	531516.358344	40.164941
3254.945039	532268.989576	40.169959
3258.204424	533016.540494	40.174976
3261.779896	533765.718635	40.179994
3264.839266	534519.023373	40.185012
3267.819971	535275.629079	40.190029
3271.225145	536032.331988	40.195047
3273.815640	536799.705828	40.200064
3277.582066	537560.407137	40.205082
3280.793027	538317.329963	40.210100
3283.798253	539086.588452	40.215117
3287.079128	539843.776705	40.220135
3290.205626	540613.039171	40.225152
3293.938100	541363.532224	40.230170
3296.958483	542087.006378	40.235188
3299.653377	542820.065114	40.240205
3303.096658	543531.769783	40.245223
3306.196952	544277.684566	40.250240
3309.204815	544995.380081	40.255258
3312.003833	545728.782525	40.260276
3315.394773	546486.271279	40.265293
3318.555113	547223.066488	40.270311
3321.513511	547994.742707	40.275328
3325.051078	548746.201853	40.280346
3328.087121	549513.708256	40.285364
3331.337448	550296.340775	40.290381
3334.604854	551072.788146	40.295399
3337.507270	551863.041218	40.300416
3341.225718	552637.018178	40.305434
3344.382475	553442.744970	40.310452
3348.137958	554227.801754	40.315469
3351.833953	555020.523206	40.320487
3354.988026	555813.085007	40.325504
3358.882927	556610.114069	40.330522
3362.488529	557414.740496	40.335540
3365.399745	558207.860792	40.340557
3369.097878	559018.971041	40.345575
3372.260337	559829.817350	40.350592
3376.048465	560636.142053	40.355610
3379.552070	561450.964722	40.360628
3382.974580	562255.040711	40.365645
3386.507424	563075.094335	40.370663
3389.946127	563885.861946	40.375680
3393.559165	564691.375387	40.380698
3397.234931	565507.088553	40.385716
3400.648371	566324.101849	40.390733
3404.281019	567119.012372	40.395751
3407.634816	567943.076954	40.400768
3411.207097	568757.506453	40.405786
3414.910738	569583.879222	40.410804
3418.303953	570392.860483	40.415821
3421.915891	571199.446791	40.420839
3425.115147	572016.352068	40.425856
3428.833253	572824.934601	40.430874
3432.413603	573653.036528	40.435892
3435.669672	574469.833127	40.440909
3439.380510	575275.404165	40.445927
3442.732006	576109.518717	40.450944
3446.516304	576915.229499	40.455962
3449.921401	577732.203061	40.460980
3453.288956	578558.223298	40.465997
3457.093283	579359.662180	40.471015
3460.418634	580194.375400	40.476032
3464.141708	581000.246414	40.481050
3467.949939	581815.544976	40.486068
3471.385118	582629.545624	40.491085
3475.036643	583440.146885	40.496103
3478.596380	584242.226578	40.501120
3482.060526	585033.769340	40.506125
3485.671427	585772.264427	40.511130
3488.989646	586468.136060	40.516135
3492.305563	587087.225117	40.521140
3495.269172	587665.025076	40.526144
3498.315050	588154.372952	40.531149
3501.321217	588606.170517	40.536154
3503.735709	588989.563977	40.541159
3506.186197	589293.793366	40.546164
3507.876320	589568.902686	40.551168
3510.077088	589780.177608	40.556173
3512.035422	589942.482175	40.561178
3513.723231	590057.835233	40.566183
3515.620225	590102.917807	40.571188
3516.646493	590131.484361	40.576192
3518.095266	590096.791428	40.581197
3519.546238	590044.538845	40.586202
3520.247880	589962.769979	40.591207
3521.139094	589834.732339	40.596212
3521.776811	589695.312112	40.601216
3522.622798	589523.404282	40.606221
3523.349275	589314.732162	40.611226
3523.753690	589105.151482	40.616231
3524.252308	588854.795182	40.621236
3524.174243	588611.569683	40.626240
3524.450034	588341.664488	40.631245
3524.863310	588079.078658	40.636250
3524.669849	587795.699717	40.641255
3524.982714	587486.720646	40.646260
3525.268271	587190.621412	40.651264
3525.207924	586879.069708	40.656269
3525.486809	586563.631947	40.661274
3525.271348	586237.594973	40.666279
3525.450295	585902.277075	40.671284
3524.999130	585580.639243	40.676288
3524.827372	585249.184780	40.681293
3524.786289	584912.567103	40.686298
3524.505110	584584.787086	40.691303
3524.660511	584245.251792	40.696308
3524.320030	583920.887052	40.701312
3524.146184	583576.453104	40.706317
3524.012040	583242.474356	40.711322
3523.466618	582918.972562	40.716327
3523.256641	582583.377833	40.721332
3523.018076	582256.589052	40.726336
3522.749390	581934.277476	40.731341
3523.041871	581606.784241	40.736346
3522.763138	581285.767137	40.741351
3522.519821	580966.498704	40.746356
3522.109043	580649.564990	40.751360
3521.632172	580319.744121	40.756365
3521.294207	580013.759969	40.761370
3520.992097	579716.776246	40.766375
3521.158408	579412.007485	40.771380
3520.813804	579115.772138	40.776384
3520.420189	578820.343541	40.781389
3520.305316	578517.663026	40.786394
3520.002576	578229.559027	40.791399
3520.001769	577935.156311	40.796404
3519.527858	577656.282720	40.801408
3519.149915	577371.948903	40.806413
3519.115407	577096.317924	40.811418
3518.350575	576826.387066	40.816423
3518.543735	576555.342337	40.821428
3518.124132	576305.643580	40.826432
3517.506957	576040.911441	40.831437
3517.826751	575791.388324	40.836442
3517.160427	575540.656376	40.841447
3517.221015	575282.098128	40.846452
3516.961785	575042.071678	40.851456
3516.985813	574798.067086	40.856461
3516.695528	574567.103964	40.861466
3515.988206	574337.663583	40.866471
3516.175922	574081.832457	40.871476
3516.035437	573864.837706	40.876480
3515.779367	573641.560612	40.881485
3515.838717	573428.255046	40.886490
3515.258749	573205.324105	40.891495
3514.946375	572988.846057	40.896500
3514.780081	572780.251061	40.901504
3514.964049	572583.285770	40.906509
3514.662771	572375.008076	40.911514
3514.245398	572166.292052	40.916519
3514.303235	571955.280824	40.921524
3514.092872	571761.539908	40.926528
3513.365184	571574.075239	40.931533
3513.303795	571381.615293	40.936538
3513.085496	571184.390733	40.941543
3513.019788	571015.254869	40.946548
3512.737128	570845.899232	40.951552
3512.520723	570657.837116	40.956557
3512.620577	570489.222749	40.961562
3512.382169	570313.605258	40.966567
3512.653051	570170.154420	40.971572
3512.204185	569995.876188	40.976576
3512.076560	569822.099238	40.981581
3511.645435	569659.252606	40.986586
3511.280674	569523.756449	40.991591
3511.744097	569359.253067	40.996596
3511.404759	569204.550070	41.001600
3511.220488	569058.034992	41.006605
3511.343767	568908.698035	41.011610
3510.676739	568748.397450	41.016615
3511.127858	568629.444130	41.021620
3510.792650	568462.788303	41.026624
3510.364568	568346.944826	41.031629
3510.698036	568191.922366	41.036634
3510.441287	568067.532329	41.041639
3510.475710	567929.991666	41.046644
3509.959087	567808.059432	41.051648
3509.640723	567683.322832	41.056653
3509.866180	567534.609821	41.061658
3509.684242	567433.637897	41.066663
3509.972124	567295.445974	41.071668
3510.029823	567188.487121	41.076672
3509.618284	567054.233750	41.081677
3509.725927	566937.134384	41.086682
3509.444460	566816.012941	41.091687
3509.453043	566695.146999	41.096692
3509.315230	566584.938155	41.101696
3509.098268	566474.035284	41.106701
3509.151234	566354.621017	41.111706
3508.674114	566268.455440	41.116711
3508.833509	566138.790429	41.121716
3508.999312	566036.140275	41.126720
3508.880832	565934.945632	41.131725
3508.740079	565834.257819	41.136730
3508.641269	565728.269997	41.141735
3508.903750	565618.746208	41.146740
3508.287319	565509.713300	41.151744
3508.373198	565421.789994	41.156749
3508.425052	565331.603162	41.161754
3508.280207	565217.805500	41.166759
3508.144669	565107.634830	41.171764
3508.296903	565047.070368	41.176768
3508.012954	564934.149290	41.181773
3508.037092	564848.601300	41.186778
3507.861611	564764.445388	41.191783
3508.395342	564657.694017	41.196788
3508.046150	564565.750787	41.201792
3507.689060	564484.192794	41.206797
3507.992660	564387.709066	41.211802
3507.454263	564303.859752	41.216807
3507.769694	564213.825587	41.221812
3507.845698	564136.431667	41.226816
3507.604154	564064.683256	41.231821
3507.585865	563975.355638	41.236826
3507.331812	563890.904336	41.241831
3507.215891	563826.041387	41.246836
3507.168787	563735.103551	41.251840
3507.344402	563661.270577	41.256845
3507.405583	563595.571938	41.261850
3507.436787	563511.980688	41.266855
3507.460128	563426.373594	41.271860
3507.491885	563353.973324	41.276864
3506.976918	563278.634177	41.281869
3507.083067	563188.172675	41.286874
3507.022385	563116.542004	41.291879
3506.882093	563048.402242	41.296884
3506.911154	562976.605416	41.301888
3506.695735	562893.452738	41.306893
3507.029119	562824.329516	41.311898
3506.722509	562770.129680	41.316903
3506.835813	562698.267682	41.321908
3506.726028	562620.945067	41.326912
3506.584671	562558.853162	41.331917
3507.006559	562494.604826	41.336922
3506.332062	562439.705572	41.341927
3506.583777	562359.148024	41.346932
3506.417727	562295.848803	41.351936
3506.276719	562232.595754	41.356941
3506.462240	562169.391649	41.361946
3506.405570	562104.662535	41.366951
3506.598566	562042.162542	41.371956
3506.396309	561981.489428	41.376960
3506.016551	561920.995362	41.381965
3506.296254	561858.178319	41.386970
3505.922473	561814.271091	41.391975
3506.324916	561746.240843	41.396980
3506.343082	561688.103065	41.401984
3505.908347	561633.666939	41.406989
3506.176361	561555.320687	41.411994
3506.126654	561509.798218	41.416999
3506.121740	561453.074909	41.422004
3506.152530	561398.917242	41.427008
3506.389676	561333.785154	41.432013
3506.356327	561279.939696	41.437018
3505.895695	561229.287755	41.442023
3506.134225	561174.087933	41.447028
3505.996489	561116.325369	41.452032
3506.012428	561059.345048	41.457037
3506.448376	560998.163400	41.462042
3506.041059	560938.274501	41.467047
3506.054541	560884.067149	41.472052
3505.957001	560826.498727	41.477056
3505.989450	560761.598018	41.482061
3505.953819	560712.793151	41.487066
3505.830923	560664.203603	41.492071
3505.883894	560603.030330	41.497076
3506.306790	560579.667439	41.502080
3505.809729	560532.296339	41.507085
3505.952535	560466.065766	41.512090
3505.633574	560442.618193	41.517095
3505.550468	560378.692050	41.522100
3505.979212	560329.056068	41.527104
3505.761644	560283.354427	41.532109
3505.930607	560212.630613	41.537114
3505.702985	560146.709204	41.542119
3505.849636	560077.501027	41.547124
3506.093926	560030.666606	41.552128
3505.499754	559976.904763	41.557133
3505.874380	559921.577637	41.562138
3505.699161	559869.009846	41.567143
3505.508317	559835.052100	41.572148
3505.769768	559789.121856	41.577152
3505.731993	559740.717360	41.582157
3505.688492	559686.110950	41.587162
3505.102138	559640.768066	41.592167
3505.436428	559577.226153	41.597172
3505.412135	559546.065377	41.602176
3505.313753	559501.804777	41.607181
3505.527682	559444.937879	41.612186
3505.461616	559416.607439	41.617191
3505.573986	559365.152175	41.622196
3505.091545	559318.430235	41.627200
3505.099670	559274.555521	41.632205
3505.129669	559225.079514	41.637210
3504.966737	559200.747895	41.642215
3504.981049	559148.450028	41.647220
3505.507950	559116.596026	41.652224
3505.156143	559068.844006	41.657229
3505.432956	559040.156033	41.662234
3505.004892	559007.595396	41.667239
3505.314990	558936.388972	41.672244
3505.261153	558934.481319	41.677248
3505.535182	558881.838830	41.682253
3505.158613	558826.020943	41.687258
3504.959398	558789.237844	41.692263
3504.770853	558763.194851	41.697268
3504.978987	558713.840187	41.702272
3504.788246	558670.549766	41.707277
3505.232949	558637.245152	41.712282
3505.110955	558600.903243	41.717287
3504.947636	558575.259371	41.722292
3504.708903	558516.997735	41.727296
3504.874356	558506.986201	41.732301
3505.315178	558454.870511	41.737306
3505.057003	558416.885378	41.742311
3504.789897	558382.936173	41.747316
3505.214093	558350.945376	41.752320
3504.893837	558307.623876	41.757325
3505.030416	558274.568837	41.762330
3504.790533	558237.992458	41.767335
3504.836714	558202.934207	41.772340
3505.164947	558174.841548	41.777344
3504.881360	558138.322251	41.782349
3504.966094	558087.270154	41.787354
3504.973097	558062.506238	41.792359
3504.872432	558016.324839	41.797364
3504.996463	557979.488537	41.802368
3504.902644	557939.710945	41.807373
3504.997694	557901.517294	41.812378
3504.693585	557874.885709	41.817383
3504.786290	557826.000094	41.822388
3505.165745	557796.587285	41.827392
3504.727342	557770.834120	41.832397
3505.212205	557728.594033	41.837402
3505.258734	557698.073631	41.842407
3504.776257	557653.313138	41.847412
3505.239714	557613.749165	41.852416
3505.029424	557575.703762	41.857421
3504.954210	557547.623185	41.862426
3504.899154	557515.907988	41.867431
3505.272432	557465.463707	41.872436
3505.134895	557432.096968	41.877440
3504.603542	557390.167789	41.882445
3505.036368	557360.291713	41.887450
3505.056776	557313.634954	41.892455
3505.006667	557278.539192	41.897460
3505.184119	557246.231839	41.902464
3504.952468	557205.414791	41.907469
3505.018943	557160.818163	41.912474
3504.628659	557128.953330	41.917479
3504.741137	557087.778931	41.922484
3504.911431	557066.316329	41.927488
3504.594512	557034.086625	41.932493
3504.631639	557000.086012	41.937498
3504.461629	556977.617867	41.942503
3504.533139	556946.284891	41.947508
3504.862075	556931.051305	41.952512
3504.847301	556906.994938	41.957517
3505.040769	556872.263177	41.962522
3504.708052	556848.458713	41.967527
3504.876597	556814.134254	41.972532
3504.936536	556781.340031	41.977536
3504.778548	556747.621841	41.982541
3504.486075	556699.247159	41.987546
3504.558897	556680.169998	41.992551
3504.749701	556649.473217	41.997556
3504.987581	556623.106686	42.002560
3504.826041	556589.388681	42.007565
3504.867645	556551.452031	42.012570
3504.561696	556526.028738	42.017575
3504.873929	556488.301344	42.022580
3504.622130	556453.638931	42.027584
3504.445548	556423.403243	42.032589
3505.113354	556389.503248	42.037594
3504.982595	556352.198586	42.042599
3504.791716	556311.019437	42.047604
3504.834670	556286.549374	42.052608
3504.718913	556258.170008	42.057613
3504.790623	556213.872217	42.062618
3504.831324	556172.555186	42.067623
3504.735864	556130.200299	42.072628
3504.806065	556093.569366	42.077632
3504.731377	556064.376068	42.082637
3504.958188	556033.571385	42.087642
3504.504846	555995.005298	42.092647
3504.450817	555955.720258	42.097652
3504.217225	555927.661504	42.102656
3504.353922	555900.754769	42.107661
3504.632847	555868.226477	42.112666
3504.321411	555846.686844	42.117671
3504.407942	555815.702092	42.122676
3504.712567	555783.169545	42.127680
3504.476912	555774.379644	42.132685
3504.625348	555739.500906	42.137690
3504.372070	555700.751075	42.142695
3504.558959	555671.868725	42.147700
3504.621382	555648.605105	42.152704
3504.159488	555617.303059	42.157709
3504.527365	555590.863628	42.162714
3504.123147	555565.555030	42.167719
3504.537094	555536.737407	42.172724
3504.540729	555507.581030	42.177728
3504.468617	555490.946443	42.182733
3504.460479	555453.670486	42.187738
3504.367613	555430.178836	42.192743
3504.512572	555404.682270	42.197748
3504.321348	555361.180031	42.202752
3504.113047	555339.118893	42.207757
3504.355504	555321.324633	42.212762
3504.240625	555313.776450	42.217767
3504.209782	555290.325210	42.222772
3504.442123	555252.405395	42.227776
3504.596691	555229.126527	42.232781
3504.593652	555198.053701	42.237786
3504.382350	555172.310361	42.242791
3504.396747	555142.041765	42.247796
3504.733471	555108.039721	42.252800
3504.399529	555089.579605	42.257805
3504.517744	555058.386422	42.262810
3504.381926	555043.627830	42.267815
3504.353813	554999.896932	42.272820
3504.467836	554969.359999	42.277824
3504.384517	554943.747354	42.282829
3504.503080	554929.755560	42.287834
3504.355525	554913.788008	42.292839
3504.567345	554859.475734	42.297844
3504.431758	554833.921598	42.302848
3504.348790	554804.928808	42.307853
3504.200874	554797.738691	42.312858
3504.278978	554752.930894	42.317863
3504.047283	554729.914043	42.322868
3504.273377	554706.522127	42.327872
3504.093809	554705.188678	42.332877
3504.484345	554666.889186	42.337882
3504.173503	554647.617711	42.342887
3504.420237	554622.709016	42.347892
3504.461793	554596.874228	42.352896
3504.120938	554583.509613	42.357901
3504.565486	554537.129836	42.362906
3504.063495	554540.942416	42.367911
3504.169242	554509.649113	42.372916
3504.348060	554471.786133	42.377920
3504.372580	554451.502903	42.382925
3504.541307	554434.627234	42.387930
3504.550698	554406.880209	42.392935
3504.323774	554364.288618	42.397940
3504.118681	554350.347410	42.402944
3504.389406	554304.599718	42.407949
3504.423690	554284.718287	42.412954
3504.002301	554271.820133	42.417959
3504.115389	554248.394882	42.422964
3504.453977	554208.084477	42.427968
3504.744899	554211.822272	42.432973
3504.452753	554147.446984	42.437978
3504.381111	554140.547168	42.442983
3504.399051	554115.673752	42.447988
3504.327910	554073.510704	42.452992
3504.250330	554068.327024	42.457997
3504.447058	554020.420853	42.463002
3504.273325	554016.261316	42.468007
3504.218919	553981.662587	42.473012
3504.449244	553958.823715	42.478016
3504.034821	553930.940956	42.483021
3504.387208	553907.073739	42.488026
3503.965383	553877.426344	42.493031
3504.021944	553865.259463	42.498036
3504.503730	553845.710287	42.503040
3504.177074	553828.559057	42.508045
3504.260535	553789.246325	42.513050
3504.374592	553778.281061	42.518055
3504.168264	553745.320143	42.523060
3504.374323	553718.095642	42.528064
3504.248200	553702.577394	42.533069
3504.514644	553675.343268	42.538074
3504.491151	553655.318747	42.543079
3504.492984	553626.360617	42.548084
3504.457753	553585.502148	42.553088
3504.190445	553577.825789	42.558093
3504.579497	553546.838757	42.563098
3504.361834	553509.843098	42.568103
3504.301898	553495.020464	42.573108
3504.482153	553463.208601	42.578112
3504.307534	553429.686994	42.583117
3504.108708	553414.482626	42.588122
3503.951959	553388.071596	42.593127
3504.289878	553367.131895	42.598132
3504.415639	553350.463544	42.603136
3504.377628	553323.630024	42.608141
3504.427329	553286.087025	42.613146
3504.369316	553274.997219	42.618151
3504.161874	553237.393831	42.623156
3504.348837	553223.591366	42.628160
3504.360633	553191.250564	42.633165
3504.563532	553170.079661	42.638170
3504.072869	553134.891974	42.643175
3504.236483	553105.503614	42.648180
3504.179509	553091.890930	42.653184
3504.049436	553083.940358	42.658189
3504.172408	553055.668252	42.663194
3504.206611	553033.060712	42.668199
3504.069377	553009.370293	42.673204
3504.095802	552994.432590	42.678208
3504.437538	552966.125733	42.683213
3504.372843	552936.672208	42.688218
3503.837004	552919.603402	42.693223
3504.187636	552905.673860	42.698228
3504.482712	552861.330382	42.703232
3504.001382	552853.788364	42.708237
3504.254505	552807.483709	42.713242
3504.165110	552803.108679	42.718247
3503.852768	552783.582667	42.723252
3504.337552	552760.752128	42.728256
3504.122688	552732.179613	42.733261
3504.039929	552711.103635	42.738266
3503.969424	552687.603950	42.743271
3504.053973	552661.203900	42.748276
3504.387455	552640.970188	42.753280
3503.805946	552618.711574	42.758285
3504.077050	552609.738724	42.763290
3504.134004	552587.480061	42.768295
3504.103749	552563.771999	42.773300
3504.409002	552534.713262	42.778304
3504.124281	552521.136033	42.783309
3504.228824	552485.650871	42.788314
3504.338924	552479.730603	42.793319
3504.196917	552422.437811	42.798324
3504.254025	552417.989054	42.803329
3503.992327	552406.880317	42.808333
3504.462905	552371.387477	42.813338
3504.238814	552339.384766	42.818343
3503.957293	552341.851266	42.823348
3504.082441	552290.973853	42.828353
3503.538488	552309.627201	42.833357
3504.297311	552273.281294	42.838362
3504.184879	552250.947974	42.843367
3504.069626	552236.687785	42.848372
3504.181713	552210.030284	42.853377
3504.210188	552189.137780	42.858381
3504.311434	552165.610099	42.863386
3504.080647	552142.488040	42.868391
3503.756337	552125.586677	42.873396
3503.936810	552110.220071	42.878401
3503.948811	552085.798176	42.883405
3504.221038	552055.179588	42.888410
3503.948858	552042.861303	42.893415
3503.795518	552027.749189	42.898420
3504.012413	552008.794398	42.903425
3503.806137	551987.787339	42.908429
3503.911560	551969.960133	42.913434
3504.058491	551963.630190	42.918439
3503.904685	551933.078677	42.923444
3503.863038	551918.402895	42.928449
3504.002292	551899.964788	42.933453
3504.209577	551864.865506	42.938458
3503.884514	551857.651455	42.943463
3504.048636	551824.324850	42.948468
3504.117360	551815.888053	42.953473
3504.079645	551793.037655	42.958477
3503.849459	551772.488166	42.963482
3504.349601	551752.025045	42.968487
3504.159635	551743.023617	42.973492
3504.051070	551705.652882	42.978497
3503.957351	551685.989916	42.983501
3504.195530	551662.641599	42.988506
3504.193467	551645.285089	42.993511
3504.116954	551631.522744	42.998516
3504.204704	551605.019344	43.003521
3504.412937	551594.441188	43.008525
3504.172197	551564.558572	43.013530
3504.203898	551553.655089	43.018535
3504.090358	551522.238576	43.023540
3504.359646	551495.756741	43.028545
3504.015423	551469.775479	43.033549
3504.323135	551444.902107	43.038554
3504.256859	551424.174844	43.043559
3504.064057	551416.939667	43.048564
3504.470886	551386.550677	43.053569
3504.261074	551368.368893	43.058573
3504.275422	551339.757392	43.063578
3504.399008	551319.100886	43.068583
3504.182349	551289.768931	43.073588
3504.328646	551273.952719	43.078593
3504.208237	551245.665077	43.083597
3504.218279	551212.815537	43.088602
3504.376958	551195.332166	43.093607
3503.922461	551174.363155	43.098612
3504.657882	551141.499725	43.103617
3504.187477	551112.661639	43.108621
3503.998457	551096.847772	43.113626
3503.916542	551085.255475	43.118631
3504.003932	551047.902529	43.123636
3504.222051	551037.221487	43.128641
3504.013109	551015.507013	43.133645
3504.006073	550998.402807	43.138650
3504.420345	550963.066791	43.143655
3503.805267	550953.375175	43.148660
3504.181550	550927.480898	43.153665
3503.988206	550906.823437	43.158669
3504.087680	550889.147218	43.163674
3503.653555	550876.248021	43.168679
3503.988217	550860.552965	43.173684
3504.298048	550827.402874	43.178689
3504.181552	550823.889335	43.183693
3504.110099	550787.267254	43.188698
3504.164762	550777.974264	43.193703
3503.985233	550753.479472	43.198708
3504.246068	550715.745040	43.203713
3504.062672	550699.324332	43.208717
3504.256090	550673.206205	43.213722
3504.012901	550662.547337	43.218727
3504.150807	550636.336998	43.223732
3504.249235	550611.697115	43.228737
3503.997779	550597.103613	43.233741
3504.018297	550572.122756	43.238746
3504.145017	550547.982896	43.243751
3504.090708	550536.032574	43.248756
3504.473708	550508.824520	43.253761
3504.451856	550488.845805	43.258765
3504.367062	550461.358372	43.263770
3503.902174	550431.761147	43.268775
3503.682074	550395.615718	43.273780
3504.119392	550383.284803	43.278785
3503.768036	550381.725792	43.283789
3503.851488	550346.541483	43.288794
3504.201911	550330.389215	43.293799
3503.936889	550311.659757	43.298804
3503.856041	550294.970077	43.303809
3503.925004	550292.184016	43.308813
3504.083235	550251.638764	43.313818
3504.186954	550240.823835	43.318823
3504.111784	550221.862409	43.323828
3504.052181	550194.824643	43.328833
3503.856467	550178.708062	43.333837
3503.690378	550150.627349	43.338842
3503.862366	550141.466794	43.343847
3503.841975	550137.635128	43.348852
3504.002310	550106.878726	43.353857
3503.607974	550106.184330	43.358861
3503.655485	550076.707243	43.363866
3503.638682	550063.640440	43.368871
3503.485941	550053.320063	43.373876
3503.990362	550044.409678	43.378881
3503.818213	550019.811557	43.383885
3503.704217	550005.548969	43.388890
3503.836894	549983.778958	43.393895
3503.989160	549971.896447	43.398900
3504.119133	549951.691148	43.403905
3504.036317	549922.789435	43.408909
3504.059776	549904.114781	43.413914
3504.280468	549893.331569	43.418919
3503.866419	549865.844585	43.423924
3504.086999	549843.202604	43.428929
3503.745945	549836.797472	43.433933
3503.761804	549813.178543	43.438938
3503.843030	549794.343230	43.443943
3503.967707	549775.198247	43.448948
3503.888204	549768.499431	43.453953
3503.774674	549736.120249	43.458957
3503.812741	549720.319452	43.463962
3503.851404	549719.758453	43.468967
3503.807476	549690.496890	43.473972
3504.192077	549665.608322	43.478977
3503.752189	549656.695559	43.483981
3504.077618	549635.045953	43.488986
3503.954153	549617.403423	43.493991
3503.658892	549590.048534	43.498996
3504.070006	549584.180439	43.504001
3503.750774	549573.835571	43.509005
3503.738638	549537.554212	43.514010
3503.781620	549521.903815	43.519015
3503.853401	549520.227368	43.524020
3504.075590	549491.983089	43.529025
3503.827987	549487.379737	43.534029
3503.646341	549457.231118	43.539034
3503.925500	549445.227195	43.544039
3503.923735	549433.116268	43.549044
3503.934046	549406.822952	43.554049
3503.760845	549399.331347	43.559053
3503.792265	549386.003992	43.564058
3504.037379	549365.123645	43.569063
3503.933279	549364.988912	43.574068
3504.025982	549336.361081	43.579073
3504.084710	549306.981594	43.584077
3504.062642	549297.144674	43.589082
3503.942978	549281.973908	43.594087
3503.767018	549270.748279	43.599092
3504.206970	549234.798433	43.604097
3504.056035	549217.311155	43.609101
3503.965019	549205.264610	43.614106
3504.166974	549166.526169	43.619111
3504.224793	549166.063052	43.624116
3504.091128	549132.222220	43.629121
3503.898120	549114.539607	43.634125
3503.893758	549088.954552	43.639130
3504.048301	549071.721612	43.644135
3504.062816	549048.555846	43.649140
3503.893303	549024.712610	43.654145
3503.768301	549017.314121	43.659149
3503.944435	548990.791984	43.664154
3504.281494	548985.389547	43.669159
3503.654874	548972.620010	43.674164
3504.412919	548927.939009	43.679169
3504.050410	548920.174280	43.684173
3504.077885	548889.083046	43.689178
3504.123789	548882.616334	43.694183
3504.103030	548853.702692	43.699188
3503.946917	548837.729765	43.704193
3503.575174	548815.785402	43.709197
3503.678158	548783.925015	43.714202
3504.104748	548777.398089	43.719207
3503.861478	548762.750984	43.724212
3504.047952	548744.301413	43.729217
3503.818550	548731.115616	43.734221
3503.728306	548701.758456	43.739226
3503.923213	548686.991554	43.744231
3503.880990	548678.570474	43.749236
3504.079884	548642.253536	43.754241
3504.016397	548643.575919	43.759245
3503.960503	548625.164505	43.764250
3503.956997	548608.410201	43.769255
3503.810581	548596.422377	43.774260
3504.181307	548571.029468	43.779265
3504.002938	548554.908347	43.784269
3503.659411	548536.744151	43.789274
3504.036801	548512.965043	43.794279
3503.423277	548505.996777	43.799284
3504.153156	548468.535670	43.804289
3503.745242	548457.396542	43.809293
3503.943046	548455.649588	43.814298
3503.938960	548429.962401	43.819303
3503.778841	548430.189786	43.824308
3504.030218	548399.819140	43.829313
3504.260903	548373.892877	43.834317
3503.856960	548355.788472	43.839322
3504.056450	548324.265107	43.844327
3503.850452	548329.748424	43.849332
3503.959593	548292.990592	43.854337
3503.660643	548280.723808	43.859341
3503.894418	548271.956062	43.864346
3504.416265	548239.170328	43.869351
3503.999636	548228.890365	43.874356
3504.119860	548192.433340	43.879361
3504.235505	548173.994246	43.884365
3504.066475	548155.751527	43.889370
3504.363973	548137.485521	43.894375
3503.832020	548110.114796	43.899380
3504.381065	548078.535655	43.904385
3504.032278	548066.125160	43.909389
3503.939128	548030.408021	43.914394
3504.442283	548031.640902	43.919399
3503.819903	548008.018989	43.924404
3503.916146	547988.270530	43.929409
3503.791555	547966.639114	43.934413
3503.953805	547949.756920	43.939418
3504.183033	547929.835956	43.944423
3504.015364	547910.482389	43.949428
3503.851979	547886.535389	43.954433
3503.900852	547869.872901	43.959437
3503.807560	547866.657796	43.964442
3503.857898	547844.291976	43.969447
3503.306045	547825.554184	43.974452
3503.479598	547803.572587	43.979457
3503.363739	547799.099287	43.984461
3503.637444	547793.454078	43.989466
3503.404705	547781.529699	43.994471
3503.421068	547761.894499	43.999476
3503.801636	547739.627737	44.004481
3503.640213	547764.938949	44.009485
3503.789873	547739.276721	44.014490
3503.999053	547712.696578	44.019495
3503.719110	547708.350125	44.024500
3503.821165	547689.609749	44.029505
3503.711781	547666.461378	44.034509
3503.693876	547664.243720	44.039514
3503.581616	547640.389178	44.044519
3503.537460	547623.185939	44.049524
3503.884395	547603.447810	44.054529
3503.740359	547604.631606	44.059533
3503.190066	547580.997609	44.064538
3503.864757	547561.308564	44.069543
3503.529228	547567.115460	44.074548
3503.720244	547553.811684	44.079553
3503.244381	547536.424220	44.084557
3503.469135	547522.963670	44.089562
3503.678028	547517.076245	44.094567
3503.463680	547518.119747	44.099572
3503.725112	547488.654102	44.104577
3503.562812	547474.144321	44.109581
3503.519954	547468.902317	44.114586
3503.750389	547454.431387	44.119591
3503.686305	547439.249924	44.124596
3503.846387	547420.903803	44.129601
3503.926144	547420.437165	44.134605
3503.631370	547395.197877	44.139610
3503.818188	547384.771473	44.144615
3503.611123	547383.643567	44.149620
3504.116894	547360.649845	44.154625
3503.832875	547338.739871	44.159629
3503.765756	547330.372422	44.164634
3503.963300	547291.983023	44.169639
3503.497683	547285.344094	44.174644
3503.515447	547278.780178	44.179649
3503.248056	547258.583493	44.184653
3503.587381	547240.562120	44.189658
3503.703323	547239.080321	44.194663
3503.468823	547246.284586	44.199668
3504.075373	547207.022774	44.204673
3503.831424	547190.557212	44.209677
3503.624738	547183.473537	44.214682
3504.160088	547150.481353	44.219687
3503.565436	547142.146701	44.224692
3503.551624	547127.714053	44.229697
3503.891006	547112.771318	44.234701
3503.662053	547097.009892	44.239706
3503.992196	547094.484778	44.244711
3503.683923	547071.972572	44.249716
3503.816832	547045.100442	44.254721
3503.627434	547051.389170	44.259725
3503.270246	547036.203143	44.264730
3503.530360	547011.582110	44.269735
3503.567933	547012.989612	44.274740
3503.540576	546999.770321	44.279745
3503.434589	546995.850414	44.284749
3503.741590	546971.726631	44.289754
3503.667829	546953.164523	44.294759
3503.508511	546948.697832	44.299764
3503.658871	546940.649097	44.304769
3504.050316	546919.944035	44.309773
3503.654910	546905.369588	44.314778
3503.941665	546886.598997	44.319783
3503.607576	546878.828688	44.324788
3503.538167	546859.054420	44.329793
3503.507375	546860.220376	44.334797
3503.439329	546837.114637	44.339802
3503.647254	546814.015718	44.344807
3503.208970	546815.347029	44.349812
3503.643299	546803.417370	44.354817
3503.234724	546811.961665	44.359821
3503.243936	546793.032927	44.364826
3503.356595	546770.251837	44.369831
3503.332927	546758.091687	44.374836
3503.641638	546762.080979	44.379841
3503.499388	546769.422317	44.384845
3503.539572	546739.333986	44.389850
3503.903394	546721.863317	44.394855
3503.451427	546726.830894	44.399860
3503.428558	546716.941895	44.404865
3503.587246	546681.080724	44.409869
3503.130762	546672.320175	44.414874
3503.353671	546663.553191	44.419879
3503.672600	546658.707982	44.424884
3503.709330	546661.074653	44.429889
3503.524865	546634.251935	44.434893
3503.537466	546625.063902	44.439898
3504.041688	546608.529913	44.444903
3503.772703	546596.761720	44.449908
3503.836799	546574.442269	44.454913
3504.108516	546561.680057	44.459917
3503.880264	546537.892531	44.464922
3504.036405	546532.164474	44.469927
3503.644211	546507.342851	44.474932
3503.867353	546479.546892	44.479937
3504.179770	546470.008530	44.484941
3503.640590	546451.065078	44.489946
3503.797749	546433.980053	44.494951
3503.442062	546431.714647	44.499956
3503.661691	546409.875110	44.504961
3504.169647	546388.948991	44.509965
3503.676180	546376.711354	44.514970
3503.824480	546359.122895	44.519975
3503.644373	546345.321460	44.524980
3503.460086	546326.776031	44.529985
3503.719745	546326.583775	44.534989
3503.499013	546305.015582	44.539994
3503.825438	546288.812187	44.544999
3503.735295	546291.905620	44.550004
3503.770053	546264.340930	44.555009
3503.963289	546246.089057	44.560013
3503.914214	546241.402826	44.565018
3503.907611	546202.437152	44.570023
3503.709507	546201.661064	44.575028
3503.798835	546183.526488	44.580033
3503.980936	546167.901000	44.585037
3503.498230	546153.289129	44.590042
3503.749320	546136.643194	44.595047
3503.622575	546118.593164	44.600052
3503.617214	546093.255423	44.605057
3504.031398	546094.754916	44.610061
3503.608200	546077.660254	44.615066
3503.772449	546054.264194	44.620071
3503.461646	546061.228717	44.625076
3503.969027	546030.408913	44.630081
3503.780922	546008.784654	44.635085
3503.715560	546016.114213	44.640090
3503.943181	545976.151879	44.645095
3503.770330	545962.752748	44.650100
3503.791638	545964.112445	44.655105
3503.771031	545937.817800	44.660109
3503.362645	545917.591081	44.665114
3503.971710	545905.532131	44.670119
3503.460715	545902.130231	44.675124
3503.750158	545870.738824	44.680129
3503.812715	545866.892930	44.685133
3503.492887	545866.640828	44.690138
3504.012266	545830.619632	44.695143
3503.638100	545820.583647	44.700148
3503.478308	545801.327012	44.705153
3503.417011	545802.497872	44.710157
3503.649564	545778.484861	44.715162
3503.808679	545765.083560	44.720167
3503.507848	545765.484652	44.725172
3503.315643	545737.096743	44.730177
3503.692042	545719.875288	44.735181
3503.581948	545721.861499	44.740186
3503.707131	545707.960740	44.745191
3503.575199	545694.605376	44.750196
3503.837832	545675.029426	44.755201
3503.756742	545671.054754	44.760205
3503.831452	545660.190557	44.765210
3503.980176	545626.448444	44.770215
3503.863070	545636.209281	44.775220
3503.722994	545613.668260	44.780225
3503.933669	545593.999461	44.785229
3503.393120	545596.760406	44.790234
3503.767920	545566.768232	44.795239
3503.682488	545545.631842	44.800244
3503.847026	545535.409565	44.805249
3503.937696	545515.557718	44.810253
3503.833375	545493.919462	44.815258
3504.332273	545489.247341	44.820263
3503.763381	545472.275958	44.825268
3503.605787	545456.652931	44.830273
3503.786155	545431.940915	44.835277
3503.691840	545418.882223	44.840282
3503.701634	545398.437265	44.845287
3503.620263	545395.522603	44.850292
3503.430519	545384.296176	44.855297
3503.611391	545353.122744	44.860301
3503.702468	545343.416728	44.865306
3503.709634	545336.449798	44.870311
3503.713698	545321.204904	44.875316
3503.719246	545304.344450	44.880321
3503.915821	545291.794935	44.885325
3503.810773	545277.273939	44.890330
3503.968792	545248.123039	44.895335
3503.658793	545248.172242	44.900340
3503.642779	545227.579691	44.905345
3503.674527	545206.474775	44.910349
3503.707025	545203.542078	44.915354
3503.650135	545186.640880	44.920359
3503.755491	545171.127429	44.925364
3503.550378	545155.965904	44.930369
3503.803433	545151.534449	44.935373
3503.486894	545122.559263	44.940378
3503.890207	545102.859366	44.945383
3503.887426	545110.330920	44.950388
3503.509345	545082.173048	44.955393
3503.692642	545066.950044	44.960397
3503.800819	545065.519735	44.965402
3503.928578	545044.550852	44.970407
3503.634647	545027.535499	44.975412
3503.398154	545013.388375	44.980417
3503.783245	545003.888065	44.985421
3503.530997	544977.527366	44.990426
3503.511972	544963.396303	44.995431
3503.657433	544966.250857	45.000436
3503.850172	544950.016649	45.005441
3503.979219	544933.742010	45.010445
3503.587309	544921.789989	45.015450
3503.808812	544900.907046	45.020455
3503.578191	544888.626627	45.025460
3503.470527	544873.954210	45.030465
3503.767662	544863.508595	45.035469
3503.556590	544848.196257	45.040474
3503.277450	544841.375304	45.045479
3503.077877	544836.813374	45.050484
3503.471071	544830.542393	45.055489
3503.475144	544834.277480	45.060493
3503.434344	544810.407065	45.065498
3503.938575	544788.469676	45.070503
3503.692013	544782.299789	45.075508
3503.589388	544763.789971	45.080513
3503.597078	544735.772389	45.085517
3503.722690	544735.146980	45.090522
3503.609255	544730.167559	45.095527
3503.460892	544712.270670	45.100532
3503.583701	544686.455940	45.105537
3503.708650	544688.102257	45.110541
3503.357001	544689.218134	45.115546
3503.534652	544667.988430	45.120551
3503.477075	544642.000211	45.125556
3503.523230	544635.783999	45.130561
3503.607088	544626.886347	45.135565
3503.503990	544613.525449	45.140570
3503.467888	544586.019314	45.145575
3503.318773	544587.305111	45.150580
3503.503615	544579.552530	45.155585
3503.383865	544583.509174	45.160589
3503.360677	544580.433712	45.165594
3503.703196	544544.588791	45.170599
3503.435402	544551.597702	45.175604
3503.463017	544540.235318	45.180609
3503.636102	544532.888419	45.185613
3503.342579	544514.307499	45.190618
3503.578071	544493.118885	45.195623
3503.399280	544487.140089	45.200628
3503.680594	544484.521293	45.205633
3503.735393	544471.539162	45.210637
3503.501249	544444.972729	45.215642
3503.678301	544432.879906	45.220647
3503.411930	544440.898271	45.225652
3503.695262	544420.661139	45.230657
3503.888398	544390.846747	45.235661
3503.373595	544386.889796	45.240666
3503.530680	544386.057472	45.245671
3503.335858	544371.448815	45.250676
3503.242394	544352.987518	45.255681
3503.360180	544346.810345	45.260685
3503.266132	544340.313279	45.265690
3503.708612	544339.132955	45.270695
3503.615890	544331.575559	45.275700
3503.379837	544307.583750	45.280705
3503.597312	544302.299476	45.285709
3503.377250	544294.913633	45.290714
3503.792924	544276.422253	45.295719
3503.348437	544266.901144	45.300724
3503.494111	544248.856259	45.305729
3503.397426	544252.052115	45.310733
3503.407123	544248.214157	45.315738
3503.575557	544227.338656	45.320743
3503.328825	544223.642184	45.325748
3503.270199	544215.069698	45.330753
3503.726199	544204.800441	45.335757
3503.420509	544202.122926	45.340762
3503.374658	544180.523995	45.345767
3503.216692	544173.380688	45.350772
3503.350278	544154.025060	45.355777
3503.310961	544150.699647	45.360781
3502.970360	544162.617034	45.365786
3503.605502	544145.857686	45.370791
3503.464298	544149.716871	45.375796
3503.519873	544124.164203	45.380801
3503.781036	544109.028877	45.385805
3503.732861	544094.750147	45.390810
3503.907529	544097.347840	45.395815
3503.628542	544087.447080	45.400820
3503.590215	544070.592160	45.405825
3503.435566	544055.572981	45.410829
3502.998450	544037.418020	45.415834
3503.523594	544025.572747	45.420839
3503.783099	544024.976629	45.425844
3503.510146	544018.911560	45.430849
3503.794404	544001.702680	45.435853
3503.386260	543978.898645	45.440858
3503.658797	543959.823701	45.445863
3503.483962	543959.245745	45.450868
3503.876377	543956.053985	45.455873
3503.771430	543929.668143	45.460877
3503.283630	543925.000036	45.465882
3503.603531	543915.509338	45.470887
3503.773988	543894.734017	45.475892
3503.420696	543885.046798	45.480897
3503.400702	543878.083476	45.485901
3503.335450	543882.082175	45.490906
3503.521644	543857.720004	45.495911
3503.359838	543840.884339	45.500916
3503.031078	543828.214685	45.505921
3503.495061	543819.458406	45.510925
3503.118828	543825.222708	45.515930
3503.303662	543825.395637	45.520935
3503.227632	543822.934172	45.525940
3503.034519	543797.824117	45.530945
3503.427863	543783.727724	45.535949
3503.197789	543772.203548	45.540954
3503.690398	543776.417006	45.545959
3503.440847	543766.864765	45.550964
3503.283516	543771.736269	45.555969
3503.591410	543735.491004	45.560973
3503.481913	543727.077728	45.565978
3503.433484	543726.479785	45.570983
3503.721054	543718.811488	45.575988
3503.605561	543704.290604	45.580993
3503.645250	543691.411149	45.585997
3503.376731	543695.088637	45.591002
3503.719569	543675.850767	45.596007
3503.382959	543657.982360	45.601012
3503.459069	543644.996140	45.606017
3503.545769	543620.396886	45.611021
3503.741265	543627.837847	45.616026
3503.410038	543614.158718	45.621031
3503.439171	543592.900472	45.626036
3503.125173	543589.517378	45.631041
3503.716540	543577.358379	45.636045
3503.654035	543568.331775	45.641050
3504.017811	543554.088386	45.646055
3503.610108	543537.897055	45.651060
3503.434467	543542.973465	45.656065
3503.633923	543513.711647	45.661069
3503.769839	543501.271179	45.666074
3503.692691	543483.412039	45.671079
3503.633460	543493.165135	45.676084
3503.643067	543478.068928	45.681089
3503.317384	543445.860898	45.686093
3503.546941	543447.591789	45.691098
3503.308753	543440.763718	45.696103
3503.657430	543439.901061	45.701108
3503.473153	543403.934718	45.706113
3503.831553	543381.059097	45.711117
3503.377694	543388.905719	45.716122
3503.355183	543381.639653	45.721127
3503.449500	543354.363054	45.726132
3503.453770	543341.337438	45.731137
3503.641750	543339.591443	45.736141
3503.432690	543341.492641	45.741146
3503.565220	543324.054536	45.746151
3503.443970	543313.825418	45.751156
3503.608867	543312.234523	45.756161
3503.448250	543300.244637	45.761165
3503.568435	543290.431711	45.766170
3503.368759	543271.783919	45.771175
3503.075532	543265.418833	45.776180
3503.231682	543241.312831	45.781185
3503.657047	543245.486585	45.786189
3503.578063	543252.567233	45.791194
3503.475179	543228.754578	45.796199
3503.406462	543206.350080	45.801204
3503.458270	543213.410074	45.806209
3503.510413	543201.285510	45.811213
3503.458443	543194.024009	45.816218
3503.298388	543166.938727	45.821223
3503.466666	543143.133564	45.826228
3503.652331	543153.756919	45.831233
3503.834778	543147.417574	45.836237
3503.424495	543127.540744	45.841242
3503.340140	543120.284325	45.846247
3503.450187	543110.321426	45.851252
3503.409609	543111.438736	45.856257
3503.741954	543105.883456	45.861261
3503.115488	543079.931936	45.866266
3503.250634	543062.644571	45.871271
3503.262176	543065.823574	45.876276
3503.297444	543064.707515	45.881281
3503.599687	543048.100527	45.886285
3503.610704	543055.873848	45.891290
3503.516679	543036.047883	45.896295
3503.343373	543022.393737	45.901300
3503.338809	543016.740214	45.906305
3503.565181	543014.432765	45.911309
3503.674701	542996.089162	45.916314
3503.558819	542970.763562	45.921319
3503.320794	542969.387772	45.926324
3503.497741	542963.150191	45.931329
3503.584052	542952.433643	45.936333
3503.472545	542945.484349	45.941338
3503.453589	542931.250373	45.946343
3503.630073	542915.268952	45.951348
3503.445555	542915.752701	45.956353
3503.682049	542897.792802	45.961357
3503.466428	542879.248012	45.966362
3503.577869	542868.123539	45.971367
3503.497383	542880.960081	45.976372
3503.504990	542852.434104	45.981377
3503.560830	542825.213106	45.986381
3503.156732	542824.772314	45.991386
3503.039411	542827.264919	45.996391
3503.556309	542821.579392	46.001396
3503.459005	542808.619853	46.006401
3503.330445	542783.194964	46.011405
3503.367511	542774.606525	46.016410
3503.303095	542770.376005	46.021415
3503.318950	542769.868836	46.026420
3503.150142	542772.823972	46.031425
3503.485892	542757.675489	46.036429
3503.394154	542744.513067	46.041434
3503.481907	542723.698702	46.046439
3503.525801	542723.439536	46.051444
3503.282474	542724.084048	46.056449
3503.494219	542717.033070	46.061453
3503.329510	542693.835180	46.066458
3503.140779	542673.165418	46.071463
3503.141060	542678.214316	46.076468
3502.906515	542677.898182	46.081473
3503.650321	542672.479660	46.086477
3502.991543	542672.382039	46.091482
3503.313078	542669.908034	46.096487
3503.601594	542667.136324	46.101492
3503.321757	542653.145265	46.106497
3503.465626	542638.784301	46.111501
3503.209824	542636.805440	46.116506
3503.346616	542623.354354	46.121511
3503.442556	542621.471360	46.126516
3503.304800	542606.498539	46.131521
3503.533446	542584.601473	46.136525
3503.190503	542578.546877	46.141530
3503.323054	542571.205421	46.146535
3503.236531	542574.198077	46.151540
3502.990550	542580.447146	46.156545
3503.410411	542567.001758	46.161549
3503.121959	542565.431950	46.166554
3503.340275	542555.704008	46.171559
3503.114377	542549.883340	46.176564
3503.266670	542540.165823	46.181569
3503.535841	542534.418366	46.186573
3503.389899	542546.407248	46.191578
3503.344174	542527.784682	46.196583
3503.361645	542496.025243	46.201588
3503.091502	542497.734250	46.206593
3503.382684	542487.439380	46.211597
3503.404743	542488.294397	46.216602
3503.765438	542492.327122	46.221607
3503.549236	542467.067012	46.226612
3503.163608	542458.898615	46.231617
3503.493575	542435.420188	46.236621
3503.208636	542439.605458	46.241626
3503.092968	542436.746123	46.246631
3503.514574	542430.469653	46.251636
3503.195349	542424.562709	46.256641
3503.525315	542404.567918	46.261645
3503.241017	542386.891672	46.266650
3503.426056	542390.548280	46.271655
3503.702924	542393.079632	46.276660
3503.659936	542384.554110	46.281665
3503.725267	542355.614156	46.286669
3503.688627	542349.813985	46.291674
3503.634564	542336.544272	46.296679
3503.914814	542305.146804	46.301684
3503.465922	542297.240761	46.306689
3503.932297	542302.266607	46.311693
3503.553563	542277.637728	46.316698
3503.359338	542263.077397	46.321703
3503.644941	542258.387501	46.326708
3503.755721	542247.313160	46.331713
3503.989934	542225.212735	46.336717
3503.726276	542210.764305	46.341722
3503.644946	542206.839232	46.346727
3503.440176	542185.464486	46.351732
3503.551308	542174.491013	46.356737
3503.535124	542166.819445	46.361741
3503.394124	542171.638397	46.366746
3503.428658	542138.714257	46.371751
3503.632327	542122.374270	46.376756
3503.226081	542121.075477	46.381761
3503.457295	542104.781606	46.386765
3503.383175	542116.204098	46.391770
3503.398380	542096.107177	46.396775
3503.339839	542083.292351	46.401780
3503.548734	542068.213713	46.406785
3503.367061	542061.224608	46.411789
3503.381847	542061.071010	46.416794
3503.095553	542064.145832	46.421799
3503.415678	542022.340650	46.426804
3503.171467	542018.946166	46.431809
3503.675079	542011.545790	46.436813
3503.305510	542012.917138	46.441818
3503.595963	542022.716903	46.446823
3503.574244	542013.935361	46.451828
3503.615234	541990.855338	46.456833
3503.941229	541966.114564	46.461837
3503.715191	541961.454952	46.466842
3503.512037	541928.769876	46.471847
3503.550448	541927.956175	46.476852
3503.582814	541913.511161	46.481857
3503.372209	541903.194220	46.486861
3503.420167	541887.282507	46.491866
3503.680337	541873.962720	46.496871
3503.583095	541861.860682	46.501876
3503.254873	541877.817133	46.506881
3503.478254	541847.437497	46.511885
3503.284504	541835.956573	46.516890
3503.327788	541823.327392	46.521895
3503.588896	541819.348094	46.526900
3503.366038	541824.432547	46.531905
3503.525029	541799.818874	46.536909
3503.562408	541788.856777	46.541914
3503.229178	541782.648850	46.546919
3503.513081	541777.050247	46.551924
3503.261297	541789.561365	46.556929
3503.664655	541757.436431	46.561933
3503.455037	541751.006992	46.566938
3503.486278	541738.581605	46.571943
3503.294325	541731.341518	46.576948
3503.096913	541731.423417	46.581953
3503.275283	541722.711061	46.586957
3503.213062	541720.852953	46.591962
3503.450108	541690.975746	46.596967
3503.632934	541678.677824	46.601972
3503.679564	541683.770221	46.606977
3503.389222	541668.921559	46.611981
3503.288721	541660.808642	46.616986
3503.151695	541646.945541	46.621991
3503.567872	541634.964137	46.626996
3503.471791	541643.260027	46.632001
3503.453651	541627.156522	46.637005
3503.307655	541603.146131	46.642010
3503.556733	541589.221953	46.647015
3503.264083	541594.014568	46.652020
3503.105841	541585.708771	46.657025
3503.378862	541579.505923	46.662029
3503.306811	541589.060321	46.667034
3503.168561	541577.368462	46.672039
3503.328444	541542.857981	46.677044
3502.925592	541529.137769	46.682049
3502.995114	541531.197127	46.687053
3502.879672	541532.427370	46.692058
3503.130684	541536.780637	46.697063
3503.206357	541543.130772	46.702068
3502.846284	541540.562349	46.707073
3503.228562	541519.800746	46.712077
3503.090634	541530.728856	46.717082
3503.279465	541529.588413	46.722087
3503.231471	541524.850032	46.727092
3503.498871	541528.746291	46.732097
3503.536825	541504.252248	46.737101
3503.184406	541493.250560	46.742106
3503.349316	541494.486987	46.747111
3503.168067	541494.768298	46.752116
3503.076615	541490.036775	46.757121
3503.612171	541484.246816	46.762125
3503.010834	541465.811728	46.767130
3503.035527	541442.733439	46.772135
3503.442833	541436.913241	46.777140
3503.325409	541441.779192	46.782145
3503.343532	541426.124164	46.787149
3503.278584	541435.677536	46.792154
3503.400289	541425.459218	46.797159
3503.682380	541416.275868	46.802164
3503.404051	541402.535858	46.807169
3503.755640	541393.139543	46.812173
3503.540522	541390.295726	46.817178
3503.252838	541379.334215	46.822183
3503.645677	541348.270396	46.827188
3503.555397	541344.296019	46.832193
3503.684269	541340.943398	46.837197
3503.477695	541339.713959	46.842202
3503.846006	541312.895257	46.847207
3503.679180	541295.754567	46.852212
3503.687287	541286.412473	46.857217
3503.837508	541251.347439	46.862221
3503.771274	541252.721402	46.867226
3503.725839	541253.284204	46.872231
3503.971772	541224.818448	46.877236
3503.465435	541212.477591	46.882241
3503.856171	541199.792971	46.887245
3503.749441	541185.924657	46.892250
3503.458255	541170.772681	46.897255
3503.601755	541155.703464	46.902260
3503.383797	541158.111266	46.907265
3503.495147	541139.209687	46.912269
3503.538676	541127.791704	46.917274
3503.417982	541126.851629	46.922279
3503.661390	541110.756726	46.927284
3503.545825	541087.801046	46.932289
3503.789364	541070.241791	46.937293
3503.680661	541068.542426	46.942298
3503.708505	541057.783274	46.947303
3503.671522	541026.231304	46.952308
3503.603832	541026.646154	46.957313
3503.791457	541015.306296	46.962317
3503.674700	540989.725023	46.967322
3503.485653	540985.362217	46.972327
3503.248740	540982.622752	46.977332
3503.333688	540979.983896	46.982337
3503.417716	540976.840254	46.987341
3503.221987	540957.280079	46.992346
3503.212246	540936.680619	46.997351
3503.436839	540927.253593	47.002356
3503.220981	540926.480026	47.007361
3503.562482	540912.742589	47.012365
3503.530190	540911.435076	47.017370
3503.227809	540901.535897	47.022375
3503.769037	540882.717534	47.027380
3503.710364	540883.080469	47.032385
3503.575481	540874.518120	47.037389
3503.704023	540851.725472	47.042394
3503.402214	540835.262006	47.047399
3504.187458	540833.522312	47.052404
3503.464829	540821.922228	47.057409
3503.564918	540796.659808	47.062413
3503.477887	540787.130467	47.067418
3503.480445	540773.850424	47.072423
3503.620476	540762.770368	47.077428
3503.376077	540748.266990	47.082433
3503.613369	540729.092523	47.087437
3503.258891	540736.722837	47.092442
3503.541342	540740.919887	47.097447
3503.691929	540705.298091	47.102452
3503.205171	540699.063485	47.107457
3503.558829	540684.314039	47.112461
3503.372104	540691.311935	47.117466
3503.330942	540663.243951	47.122471
3503.459274	540656.912112	47.127476
3503.335892	540645.166684	47.132481
3503.714187	540642.784370	47.137485
3503.272631	540648.459218	47.142490
3503.185884	540626.154704	47.147495
3503.589190	540609.933006	47.152500
3502.917827	540593.780156	47.157505
3503.304216	540589.578758	47.162509
3503.049835	540594.315145	47.167514
3502.927640	540590.901050	47.172519
3503.353073	540577.553999	47.177524
3503.265495	540591.958943	47.182529
3503.483986	540582.280195	47.187533
3503.455186	540563.652518	47.192538
3503.365433	540546.852254	47.197543
3503.688408	540534.278775	47.202548
3503.575613	540542.577912	47.207553
3503.312977	540518.988181	47.212557
3503.392673	540501.201687	47.217562
3503.073445	540491.506879	47.222567
3503.684935	540483.028321	47.227572
3503.319244	540491.821909	47.232577
3503.395993	540480.398184	47.237581
3503.512831	540472.805716	47.242586
3503.394755	540447.324719	47.247591
3503.639047	540438.752688	47.252596
3503.365848	540445.410900	47.257601
3503.583660	540430.430204	47.262605
3503.608618	540400.937426	47.267610
3503.451426	540390.409023	47.272615
3503.566049	540386.805967	47.277620
3503.601882	540388.315362	47.282625
3503.503826	540365.103339	47.287629
3503.461178	540350.365710	47.292634
3503.246090	540349.692980	47.297639
3503.653760	540343.316859	47.302644
3503.623045	540336.454576	47.307649
3503.630059	540314.841715	47.312653
3503.523221	540305.567676	47.317658
3503.261424	540299.701309	47.322663
3503.666354	540285.448325	47.327668
3503.812842	540285.475876	47.332673
3503.726772	540258.979595	47.337677
3503.724220	540251.860345	47.342682
3503.242257	540235.828660	47.347687
3503.708781	540204.851834	47.352692
3503.173338	540217.308095	47.357697
3502.988340	540209.662210	47.362701
3503.400621	540202.628858	47.367706
3503.256004	540207.550000	47.372711
3503.427068	540189.647707	47.377716
3503.271769	540172.453420	47.382721
3503.585391	540159.174168	47.387725
3503.756758	540155.057131	47.392730
3503.560700	540163.218148	47.397735
3503.757587	540123.598496	47.402740
3503.324639	540120.031426	47.407745
3503.498972	540111.419771	47.412749
3503.358522	540114.774909	47.417754
3503.356389	540091.193831	47.422759
3503.471166	540081.026195	47.427764
3503.315262	540083.424358	47.432769
3503.406814	540073.310884	47.437773
3503.603652	540063.837211	47.442778
3503.191626	540049.460646	47.447783
3503.693109	540027.870215	47.452788
3503.354268	540022.571376	47.457793
3503.602347	540014.907439	47.462797
3503.639983	540011.467951	47.467802
3503.279520	539992.084048	47.472807
3503.351584	539982.377564	47.477812
3502.981835	539988.142301	47.482817
3503.237642	539970.983801	47.487821
3503.668627	539959.352207	47.492826
3503.047120	539966.419154	47.497831
3503.157713	539966.704861	47.502836
3503.200393	539939.480720	47.507841
3503.539633	539928.217078	47.512845
3503.051228	539920.366516	47.517850
3503.079544	539911.424350	47.522855
3503.205484	539909.031311	47.527860
3502.913137	539918.116618	47.532865
3503.424470	539908.189169	47.537869
3503.567704	539911.247033	47.542874
3503.146539	539898.689646	47.547879
3503.489108	539871.619972	47.552884
3503.564250	539871.810291	47.557889
3503.273671	539874.734739	47.562893
3503.231677	539873.883140	47.567898
3503.349885	539870.228899	47.572903
3503.259832	539849.135680	47.577908
3503.007288	539831.148425	47.582913
3503.391844	539826.240151	47.587917
3503.412438	539812.855418	47.592922
3503.352055	539831.953004	47.597927
3503.589780	539812.120847	47.602932
3503.329134	539805.143173	47.607937
3503.466798	539779.923612	47.612941
3503.117399	539773.212435	47.617946
3502.971614	539770.407848	47.622951
3503.247138	539762.941434	47.627956
3503.355622	539766.105814	47.632961
3503.408922	539763.623239	47.637965
3503.651332	539750.304387	47.642970
3503.135953	539731.096125	47.647975
3503.475744	539724.376994	47.652980
3503.569245	539718.908720	47.657985
3503.284969	539718.297394	47.662989
3503.217403	539718.207286	47.667994
3503.361822	539698.894701	47.672999
3503.629408	539683.198436	47.678004
3503.167014	539672.970257	47.683009
3503.270112	539682.397183	47.688013
3503.381380	539664.251233	47.693018
3503.345024	539657.389533	47.698023
3503.492352	539633.986110	47.703028
3503.138004	539625.912216	47.708033
3503.315674	539614.774873	47.713037
3503.456330	539624.902866	47.718042
3503.567315	539624.279562	47.723047
3503.557476	539595.598673	47.728052
3503.345678	539588.360689	47.733057
3503.488284	539573.694019	47.738061
3503.494990	539574.703121	47.743066
3503.759522	539574.712017	47.748071
3503.627871	539542.262949	47.753076
3503.155115	539532.541291	47.758081
3503.571866	539529.496255	47.763085
3503.556706	539510.461141	47.768090
3503.494991	539515.116914	47.773095
3503.621256	539511.915795	47.778100
3503.352722	539505.494705	47.783105
3503.373514	539490.544219	47.788109
3503.712968	539473.573928	47.793114
3503.519483	539454.415434	47.798119
3503.653876	539441.113383	47.803124
3503.384240	539435.096424	47.808129
3503.501315	539437.906027	47.813133
3503.456548	539411.502729	47.818138
3503.157511	539405.086418	47.823143
3503.448783	539386.103713	47.828148
3503.463192	539381.455792	47.833153
3503.372758	539392.276944	47.838157
3503.408557	539367.880770	47.843162
3503.114431	539363.837092	47.848167
3503.388525	539343.342094	47.853172
3503.337208	539343.956395	47.858177
3503.291001	539333.662206	47.863181
3503.569806	539338.314712	47.868186
3503.223384	539322.664621	47.873191
3503.446936	539307.530412	47.878196
3503.245256	539303.320610	47.883201
3503.253604	539297.411155	47.888205
3503.461883	539301.620332	47.893210
3503.306506	539286.444995	47.898215
3503.611522	539270.691889	47.903220
3503.154488	539274.501240	47.908225
3503.485517	539248.139260	47.913229
3503.651066	539234.478612	47.918234
3503.267673	539246.356148	47.923239
3503.829561	539216.170211	47.928244
3503.517942	539211.725265	47.933249
3503.631995	539202.971125	47.938253
3503.593320	539207.219359	47.943258
3503.630792	539174.591276	47.948263
3503.568119	539171.520946	47.953268
3503.533463	539149.105020	47.958273
3504.037849	539142.107122	47.963277
3503.635168	539123.385266	47.968282
3503.447731	539120.385144	47.973287
3503.609217	539110.663968	47.978292
3503.506057	539087.905284	47.983297
3503.177935	539062.253154	47.988301
3503.740024	539058.983057	47.993306
3503.087838	539064.742282	47.998311
3503.111284	539047.669963	48.003316
3503.180102	539062.506140	48.008321
3503.318947	539047.839555	48.013325
3503.139471	539020.749875	48.018330
3502.842258	539019.484068	48.023335
3503.583173	539012.095230	48.028340
3503.323829	539007.894459	48.033345
3503.152020	539009.386311	48.038349
3503.687248	539005.665951	48.043354
3503.172371	539003.424553	48.048359
3503.649786	538960.374045	48.053364
3503.097438	538972.177499	48.058369
3503.000840	538949.922568	48.063373
3503.561705	538958.318098	48.068378
3502.833810	538957.877853	48.073383
3503.001612	538952.195561	48.078388
3503.327396	538954.669269	48.083393
3503.205447	538947.719776	48.088397
3503.350394	538925.073133	48.093402
3503.025022	538912.348285	48.098407
3503.362376	538903.306179	48.103412
3503.597013	538907.460800	48.108417
3503.484513	538890.308791	48.113421
3503.562127	538898.780733	48.118426
3503.376903	538872.802697	48.123431
3503.362471	538858.362156	48.128436
3503.371917	538854.270359	48.133441
3503.201355	538847.227503	48.138445
3503.218741	538847.881465	48.143450
3503.306185	538848.423354	48.148455
3503.352970	538830.488599	48.153460
3502.969270	538820.045402	48.158465
3502.924691	538812.982618	48.163469
3503.221356	538796.270836	48.168474
3502.904964	538808.239125	48.173479
3502.964778	538808.229879	48.178484
3503.448770	538796.993021	48.183489
3503.035817	538803.017535	48.188493
3503.252732	538791.923886	48.193498
3502.973290	538805.199347	48.198503
3503.545816	538793.392990	48.203508
3503.255935	538784.500450	48.208513
3503.174811	538760.323782	48.213517
3503.225972	538753.801343	48.218522
3503.159065	538752.398112	48.223527
3503.204035	538742.594116	48.228532
3503.200314	538748.957975	48.233537
3503.278511	538738.189215	48.238541
3503.178072	538748.658903	48.243546
3502.907961	538746.530281	48.248551
3503.401160	538729.888365	48.253556
3503.080852	538725.949654	48.258561
3503.070943	538717.315828	48.263565
3503.619750	538708.846194	48.268570
3503.146876	538710.385658	48.273575
3503.302312	538705.715241	48.278580
3503.560438	538712.896241	48.283585
3503.160981	538682.962191	48.288589
3503.398066	538665.047664	48.293594
3502.773066	538669.186716	48.298599
3503.254051	538650.476112	48.303604
3502.960532	538657.542323	48.308609
3502.817642	538660.797166	48.313613
3503.242748	538657.750638	48.318618
3503.040814	538655.510226	48.323623
3503.458050	538658.373535	48.328628
3503.506984	538654.275444	48.333633
3503.354800	538643.442027	48.338637
3503.255577	538615.985434	48.343642
3502.875347	538624.024884	48.348647
3503.007355	538591.229103	48.353652
3503.182959	538605.695341	48.358657
3503.293232	538596.335438	48.363661
3503.531381	538601.499608	48.368666
3503.531303	538599.176782	48.373671
3503.393031	538586.573592	48.378676
3503.609504	538571.086262	48.383681
3503.180255	538559.387556	48.388685
3503.187284	538567.820338	48.393690
3503.373064	538567.185170	48.398695
3503.788011	538560.857657	48.403700
3503.406468	538546.828350	48.408705
3503.352276	538543.251540	48.413709
3503.572139	538535.288312	48.418714
3503.093286	538525.314461	48.423719
3503.476328	538516.365908	48.428724
3503.481546	538503.487463	48.433729
3503.505327	538482.424852	48.438733
3503.489885	538477.427863	48.443738
3503.400438	538475.674659	48.448743
3503.296594	538466.298017	48.453748
3503.524775	538441.617442	48.458753
3503.195792	538432.781377	48.463757
3503.450914	538433.751293	48.468762
3503.233981	538433.028264	48.473767
3503.421593	538420.120921	48.478772
3503.135425	538434.407798	48.483777
3503.164426	538407.334574	48.488781
3503.252890	538403.482676	48.493786
3503.103462	538391.638611	48.498791
3503.658358	538377.107630	48.503796
3503.496761	538364.709948	48.508801
3503.379539	538351.547716	48.513805
3503.292438	538344.339929	48.518810
3503.337820	538330.747964	48.523815
3503.412977	538307.808422	48.528820
3503.504128	538306.531674	48.533825
3503.642867	538302.469797	48.538829
3503.640706	538284.946151	48.543834
3503.314894	538264.342508	48.548839
3503.204991	538267.945735	48.553844
3503.390985	538256.856585	48.558849
3503.481350	538264.367325	48.563853
3503.369775	538245.497370	48.568858
3503.217578	538227.088332	48.573863
3503.181186	538209.519507	48.578868
3503.018168	538205.606301	48.583873
3503.141525	538212.505825	48.588877
3503.604452	538194.252037	48.593882
3503.298467	538211.976413	48.598887
3503.689963	538192.117839	48.603892
3503.427548	538180.543979	48.608897
3503.194869	538165.379739	48.613901
3503.633238	538153.947610	48.618906
3503.463539	538157.307802	48.623911
3503.371249	538140.555772	48.628916
3503.270604	538129.814848	48.633921
3503.147870	538118.673387	48.638925
3503.541137	538103.410152	48.643930
3503.301190	538112.235740	48.648935
3503.323960	538108.848674	48.653940
3503.363302	538097.126052	48.658945
3503.226746	538081.290000	48.663949
3503.158189	538068.776367	48.668954
3503.025654	538058.242444	48.673959
3503.240632	538066.541631	48.678964
3503.151671	538069.434556	48.683969
3503.251796	538063.106094	48.688973
3503.658753	538057.486676	48.693978
3502.987653	538073.551825	48.698983
3503.146759	538051.608683	48.703988
3503.267349	538025.984887	48.708993
3503.306161	538025.827451	48.713997
3503.442708	538015.907507	48.719002
3503.050518	538018.646356	48.724007
3503.248397	538012.655944	48.729012
3503.506307	538012.564885	48.734017
3503.223914	538011.953188	48.739021
3503.204796	537980.240539	48.744026
3503.331086	537973.200861	48.749031
3503.215205	537971.300268	48.754036
3503.546468	537958.824358	48.759041
3503.218750	537969.280000	48.764045
3503.165076	537960.804171	48.769050
3503.118991	537966.468010	48.774055
3503.455134	537939.951448	48.779060
3503.282998	537926.747024	48.784065
3503.027455	537934.514611	48.789069
3503.220905	537933.019651	48.794074
3503.014090	537930.577890	48.799079
3503.194159	537928.782025	48.804084
3503.219894	537929.131688	48.809089
3503.315434	537929.116795	48.814093
3503.637246	537907.854776	48.819098
3503.130920	537890.763883	48.824103
3503.263406	537886.046340	48.829108
3502.810799	537881.572781	48.834113
3502.966605	537878.871684	48.839117
3503.267042	537873.218531	48.844122
3503.233804	537879.991446	48.849127
3503.236348	537875.597457	48.854132
3502.996306	537877.605236	48.859137
3503.233462	537871.608560	48.864141
3503.228993	537862.013825	48.869146
3503.293109	537847.256889	48.874151
3503.400335	537834.917294	48.879156
3503.507995	537831.415742	48.884161
3503.136593	537827.030339	48.889165
3503.410901	537818.553096	48.894170
3503.433176	537810.216691	48.899175
3503.153675	537800.160350	48.904180
3503.266390	537782.668473	48.909185
3503.004862	537779.881809	48.914189
3503.249195	537768.076031	48.919194
3502.830237	537779.404787	48.924199
3503.137906	537771.023253	48.929204
3503.071409	537778.811544	48.934209
3503.039241	537772.251352	48.939213
3503.450579	537772.338058	48.944218
3503.258620	537763.530450	48.949223
3503.166356	537747.687050	48.954228
3503.319809	537737.158208	48.959233
3503.270801	537739.337827	48.964237
3503.462483	537735.772469	48.969242
3503.427799	537724.162268	48.974247
3503.334974	537725.944783	48.979252
3503.129513	537709.109158	48.984257
3503.052861	537693.667266	48.989261
3503.248788	537680.505464	48.994266
3503.225496	537683.287075	48.999271
3503.145975	537675.673741	49.004276
3503.211893	537686.673409	49.009281
3503.165198	537669.206598	49.014285
3503.369405	537673.568384	49.019290
3503.528054	537671.624363	49.024295
3503.544177	537652.986011	49.029300
3503.193411	537636.324782	49.034305
3502.959825	537649.442487	49.039309
3503.488386	537626.379753	49.044314
3503.236286	537633.995437	49.049319
3503.299837	537639.086522	49.054324
3503.425353	537624.673196	49.059329
3502.781269	537615.633936	49.064333
3503.096356	537587.150423	49.069338
3503.247862	537595.712422	49.074343
3503.083466	537582.809502	49.079348
3503.193189	537592.640715	49.084353
3503.122235	537589.773390	49.089357
3503.063910	537578.217319	49.094362
3503.012613	537580.700348	49.099367
3503.145028	537578.305922	49.104372
3503.333465	537573.326917	49.109377
3503.220615	537583.294323	49.114381
3503.396728	537557.105416	49.119386
3503.306286	537549.897781	49.124391
3503.173162	537537.090889	49.129396
3503.585915	537529.652200	49.134401
3503.054009	537535.493992	49.139405
3503.426215	537528.718270	49.144410
3503.189289	537534.866972	49.149415
3503.193042	537506.483021	49.154420
3503.258858	537484.402295	49.159425
3503.053931	537485.748014	49.164429
3503.436225	537484.576696	49.169434
3503.109188	537487.355846	49.174439
3503.254594	537477.939199	49.179444
3503.322787	537476.312478	49.184449
3503.492861	537469.720191	49.189453
3503.674584	537444.843328	49.194458
3503.318656	537438.536183	49.199463
3503.276322	537429.654228	49.204468
3503.282909	537438.441239	49.209473
3503.375576	537434.234898	49.214477
3503.465294	537412.655339	49.219482
3503.349998	537405.754594	49.224487
3503.130186	537387.557247	49.229492
3503.319716	537381.870938	49.234497
3503.018303	537385.706661	49.239501
3503.020249	537388.231811	49.244506
3503.219187	537386.331891	49.249511
3503.013837	537388.637281	49.254516
3503.241596	537389.914620	49.259521
3503.123988	537370.691000	49.264525
3503.467970	537349.071164	49.269530
3503.007680	537356.871405	49.274535
3503.154493	537349.121126	49.279540
3503.200477	537331.134228	49.284545
3503.170567	537343.310909	49.289549
3503.480463	537346.746992	49.294554
3503.327945	537335.155119	49.299559
3503.128081	537316.803020	49.304564
3502.949116	537297.487995	49.309569
3503.110043	537298.422368	49.314573
3503.361846	537295.554481	49.319578
3503.069526	537290.045305	49.324583
3503.187021	537290.633006	49.329588
3503.684956	537282.322144	49.334593
3503.111072	537287.514095	49.339597
3503.285328	537278.698831	49.344602
3503.041736	537253.484835	49.349607
3502.762420	537243.781635	49.354612
3503.027514	537228.689303	49.359617
3502.687858	537240.460473	49.364621
3503.015872	537234.802727	49.369626
3502.753485	537241.864670	49.374631
3503.098453	537244.386134	49.379636
3503.054555	537239.140709	49.384641
3502.946399	537233.450889	49.389645
3503.102437	537243.376018	49.394650
3502.933501	537243.049388	49.399655
3502.955568	537229.965182	49.404660
3503.082067	537241.915202	49.409665
3502.798898	537250.394579	49.414669
3503.391183	537228.583812	49.419674
3503.024402	537241.571401	49.424679
3503.307981	537231.072148	49.429684
3503.266311	537232.897141	49.434689
3503.068870	537233.029566	49.439693
3503.386692	537233.636113	49.444698
3503.416622	537220.348634	49.449703
3503.382536	537192.323619	49.454708
3503.555116	537185.730814	49.459713
3503.278635	537190.724275	49.464717
3503.787793	537182.815630	49.469722
3503.225246	537176.844067	49.474727
3503.306037	537158.346408	49.479732
3503.545102	537149.773354	49.484737
3503.458743	537149.989234	49.489741
3503.492010	537151.903404	49.494746
3503.553473	537139.267446	49.499751
3503.772594	537114.384135	49.504756
3503.781736	537103.473618	49.509761
3503.265463	537106.838310	49.514765
3503.621656	537095.519393	49.519770
3503.232742	537065.125939	49.524775
3503.501344	537067.507985	49.529780
3503.571164	537050.123062	49.534785
3503.565883	537044.921973	49.539789
3503.500236	537028.316028	49.544794
3503.233118	537011.842921	49.549799
3503.339891	536998.290573	49.554804
3503.273727	537005.574142	49.559809
3503.031626	537000.258949	49.564813
3503.662982	536993.947095	49.569818
3503.394811	536981.918676	49.574823
3503.311152	536963.800318	49.579828
3503.372915	536955.457205	49.584833
3503.322867	536969.657624	49.589837
3503.437353	536960.245546	49.594842
3503.402280	536946.058987	49.599847
3503.233011	536922.499412	49.604852
3502.954316	536909.007909	49.609857
3502.995711	536913.799699	49.614861
3503.136174	536906.807798	49.619866
3503.263653	536901.131118	49.624871
3503.183975	536908.315856	49.629876
3503.587038	536899.413703	49.634881
3503.382667	536898.335066	49.639885
3503.507485	536872.001574	49.644890
3503.088153	536878.835956	49.649895
3503.224039	536864.218247	49.654900
3503.584609	536870.323286	49.659905
3503.452095	536871.152545	49.664909
3503.503533	536851.548007	49.669914
3503.322097	536838.192589	49.674919
3503.648649	536823.039638	49.679924
3503.646547	536814.605529	49.684929
3503.439541	536816.254675	49.689933
3503.385978	536790.201770	49.694938
3503.589524	536785.119108	49.699943
3503.304901	536765.416053	49.704948
3503.468853	536761.450797	49.709953
3503.324702	536759.655534	49.714957
3503.646784	536745.260818	49.719962
3503.431400	536735.547189	49.724967
3503.351784	536730.610278	49.729972
3503.275523	536736.733906	49.734977
3503.332527	536721.673965	49.739981
3503.562793	536703.960247	49.744986
3503.498060	536693.566186	49.749991
3503.419387	536678.022573	49.754996
3503.719216	536674.237848	49.760001
3503.372336	536670.050262	49.765005
3503.474579	536646.901915	49.770010
3503.240476	536632.948553	49.775015
3503.062264	536632.118300	49.780020
3503.176247	536626.948727	49.785025
3503.334515	536627.479503	49.790029
3503.491348	536614.676516	49.795034
3503.050032	536594.998007	49.800039
3502.836480	536590.738819	49.805044
3503.384025	536576.257803	49.810049
3503.046687	536585.150170	49.815053
3503.206382	536574.973095	49.820058
3503.363942	536576.261600	49.825063
3503.307211	536586.978400	49.830068
3503.412006	536574.840204	49.835073
3502.970039	536579.253926	49.840077
3503.362281	536543.382157	49.845082
3503.105695	536536.907412	49.850087
3503.186716	536531.035906	49.855092
3503.247017	536532.188264	49.860097
3503.184865	536530.228489	49.865101
3503.257620	536519.155978	49.870106
3503.554227	536531.332206	49.875111
3503.294117	536517.534373	49.880116
3503.400903	536492.566791	49.885121
3503.396615	536485.547069	49.890125
3503.614912	536476.471843	49.895130
3503.250520	536484.257367	49.900135
3503.114820	536483.268863	49.905140
3503.607453	536465.260862	49.910145
3503.251958	536447.538413	49.915149
3503.065649	536442.517256	49.920154
3503.338411	536434.797116	49.925159
3503.223936	536423.804636	49.930164
3503.331672	536430.000322	49.935169
3503.109532	536432.106474	49.940173
3503.275268	536430.817782	49.945178
3503.528811	536405.372290	49.950183
3503.246098	536397.335860	49.955188
3503.575941	536391.121924	49.960193
3503.210554	536402.948310	49.965197
3503.273272	536386.826464	49.970202
3503.223594	536396.986690	49.975207
3503.389212	536366.756743	49.980212
3503.313591	536356.717733	49.985217
3503.202008	536360.018623	49.990221
3503.194890	536340.826753	49.995226
3503.344159	536346.763366	50.000231
3503.179645	536346.385508	50.005236
3503.345784	536341.005561	50.010241
3502.986974	536333.688243	50.015245
3502.889909	536309.611227	50.020250
3503.030528	536305.548524	50.025255
3503.004922	536289.996130	50.030260
3503.286385	536288.083032	50.035265
3502.929093	536288.594289	50.040269
3503.140548	536290.833964	50.045274
3503.086664	536285.842333	50.050279
3502.913276	536299.860833	50.055284
3503.098820	536294.831363	50.060289
3503.064079	536293.119769	50.065293
3503.050971	536294.081712	50.070298
3503.305569	536289.192852	50.075303
3503.335455	536288.632741	50.080308
3503.388341	536288.675099	50.085313
3503.476822	536261.689689	50.090317
3503.515683	536251.329464	50.095322
3503.204030	536243.146000	50.100327
3503.273000	536241.923096	50.105332
3503.437997	536242.705366	50.110337
3503.498610	536222.492468	50.115341
3503.223568	536208.848243	50.120346
3502.947444	536206.972754	50.125351
3503.053245	536206.602678	50.130356
3503.002413	536202.368171	50.135361
3502.863328	536201.127639	50.140365
3503.040291	536192.008269	50.145370
3503.198810	536207.035082	50.150375
3503.213047	536194.102756	50.155380
3503.168147	536193.857515	50.160385
3503.285630	536202.375164	50.165389
3503.190632	536184.661747	50.170394
3502.994704	536174.591123	50.175399
3502.951878	536156.010774	50.180404
3503.056613	536147.761448	50.185409
3502.864790	536162.490114	50.190413
3503.066294	536137.709020	50.195418
3503.232190	536146.623121	50.200423
3502.847134	536150.270333	50.205428
3503.106095	536145.734302	50.210433
3503.143162	536141.889959	50.215437
3502.903720	536132.230258	50.220442
3503.082696	536146.647787	50.225447
3503.247276	536134.449285	50.230452
3503.258101	536134.599309	50.235457
3503.020953	536155.648786	50.240461
3503.294216	536138.937802	50.245466
3503.453104	536126.184593	50.250471
3502.948366	536109.546033	50.255476
3503.160005	536093.147794	50.260481
3503.045864	536100.641413	50.265485
3503.173881	536087.185921	50.270490
3503.134735	536089.616762	50.275495
3502.896849	536104.504291	50.280500
3503.609498	536112.069265	50.285505
3503.305771	536124.795285	50.290509
3503.399144	536104.324507	50.295514
3503.414790	536089.573537	50.300519
3503.043061	536086.955505	50.305524
3503.245916	536075.003453	50.310529
3503.143304	536075.474463	50.315533
3503.198521	536075.465943	50.320538
3502.987706	536077.822900	50.325543
3503.439118	536067.195308	50.330548
3503.074488	536062.050682	50.335553
3503.047726	536059.327613	50.340557
3503.222191	536012.528483	50.345562
3503.166416	536010.719163	50.350567
3503.357285	535997.304168	50.355572
3503.449144	536000.017375	50.360577
3503.411081	535990.679323	50.365581
3503.070886	535999.471460	50.370586
3503.123436	535994.008326	50.375591
3502.838082	535975.415581	50.380596
3503.245788	535975.300840	50.385601
3502.968686	535963.828637	50.390605
3503.062172	535946.034645	50.395610
3503.402127	535954.567778	50.400615
3503.178078	535945.006546	50.405620
3503.537439	535949.142265	50.410625
3502.777319	535951.333512	50.415629
3502.962411	535941.606591	50.420634
3503.072644	535952.246935	50.425639
3503.065017	535947.752981	50.430644
3503.563637	535951.058534	50.435649
3503.200162	535928.336279	50.440653
3503.055328	535917.449254	50.445658
3503.250760	535904.083966	50.450663
3503.076723	535895.979586	50.455668
3503.221030	535913.231369	50.460673
3503.054656	535909.974731	50.465677
3503.297570	535904.430968	50.470682
3503.195255	535907.932529	50.475687
3503.140156	535900.668021	50.480692
3503.558475	535890.803187	50.485697
3503.125770	535866.626995	50.490701
3503.351220	535858.105884	50.495706
3503.239044	535856.608520	50.500711
3503.070697	535847.796074	50.505716
3503.307467	535841.748158	50.510721
3503.132749	535855.565232	50.515725
3503.307507	535837.758269	50.520730
3503.127580	535816.421121	50.525735
3503.125034	535797.581421	50.530740
3503.272948	535754.927544	50.535745
3502.738087	535720.311613	50.540749
3502.768619	535663.381556	50.545754
3502.815788	535604.983843	50.550759
3502.613143	535522.481081	50.555764
3502.686335	535439.530188	50.560769
3502.406874	535352.189557	50.565773
3502.159701	535228.272598	50.570778
3502.034279	535127.520629	50.575783
3501.687111	535008.567927	50.580788
3501.980356	534875.167323	50.585793
3501.815908	534743.656400	50.590797
3501.260798	534593.818946	50.595802
3501.292356	534438.482240	50.600807
3501.003378	534281.376087	50.605812
3500.955442	534097.406365	50.610817
3500.248195	533935.008124	50.615821
3499.994085	533735.204542	50.620826
3499.985606	533550.009671	50.625831
3499.372667	533367.535073	50.630836
3498.936011	533149.970386	50.635841
3498.625665	532955.621690	50.640845
3498.233025	532740.368207	50.645850
3497.880967	532523.135015	50.650855
3497.449568	532296.665867	50.655860
3497.083708	532071.547174	50.660865
3496.428192	531841.570268	50.665869
3496.515332	531597.275372	50.670874
3496.143910	531356.535342	50.675879
3495.425619	531121.353710	50.680884
3495.583449	530839.899548	50.685889
3494.867802	530577.930333	50.690893
3494.373127	530313.799637	50.695898
3493.927362	530046.776620	50.700903
3493.124180	529773.135627	50.705908
3493.072376	529485.222513	50.710913
3492.587484	529203.436393	50.715917
3492.306375	528918.934806	50.720922
3491.843633	528621.318099	50.725927
3490.848431	528335.453406	50.730932
3490.442502	528027.406456	50.735937
3489.905875	527737.314584	50.740941
3489.464597	527429.665905	50.745946
3489.098970	527120.382089	50.750951
3488.403423	526802.401115	50.755956
3487.906143	526483.725432	50.760961
3487.222928	526177.455389	50.765965
3487.133719	525853.193621	50.770970
3486.018534	525531.462986	50.775975
3485.403448	525214.398004	50.780980
3485.130551	524877.307258	50.785985
3484.464185	524553.767522	50.790989
3483.921397	524220.850471	50.795994
3483.391577	523880.948796	50.800999
3482.449102	523537.162318	50.806004
3482.161006	523196.854181	50.811009
3481.486477	522869.895059	50.816013
3480.905943	522531.540121	50.821018
3480.792213	522177.685431	50.826023
3479.741028	521841.058768	50.831028
3479.490311	521479.576749	50.836033
3478.658780	521132.941187	50.841037
3478.178405	520772.288700	50.846042
3477.171161	520421.975067	50.851047
3476.366330	520070.357928	50.856052
3476.034812	519719.619095	50.861057
3475.348951	519369.080465	50.866061
3474.898602	519011.064282	50.871066
3474.170987	518650.707599	50.876071
3473.505110	518293.013268	50.881076
3472.691965	517934.424260	50.886081
3472.109414	517586.562007	50.891085
3471.492836	517219.380444	50.896090
3471.180387	516854.974610	50.901095
3470.229286	516498.500287	50.906100
3469.938305	516119.611550	50.911105
3469.089305	515767.302943	50.916109
3468.381823	515400.247322	50.921114
3468.012551	515030.196786	50.926119
3467.036148	514665.595188	50.931124
3466.526259	514296.612793	50.936129
3466.110774	513928.568373	50.941133
3465.023124	513554.097309	50.946138
3464.646094	513183.805001	50.951143
3463.885996	512815.841330	50.956148
3463.563452	512445.271309	50.961153
3462.573137	512074.292888	50.966157
3462.014842	511699.595887	50.971162
3461.474625	511321.245512	50.976167
3460.685706	510943.836619	50.981172
3460.081813	510568.008970	50.986177
3459.249531	510197.470529	50.991181
3458.843763	509810.970968	50.996186
3457.726944	509436.211347	51.001191
3456.724678	509060.970086	51.006196
3456.686411	508692.550303	51.011201
3455.872472	508316.099342	51.016205
3455.027965	507945.160045	51.021210
3454.453018	507572.045055	51.026215
3453.558893	507208.282684	51.031220
3452.692321	506838.537513	51.036225
3451.987412	506463.040980	51.041229
3451.650047	506092.234843	51.046234
3450.854720	505724.984831	51.051239
3450.194659	505356.541801	51.056244
3449.559782	504980.951654	51.061249
3448.937013	504617.395878	51.066253
3448.183076	504239.986825	51.071258
3447.395190	503870.368757	51.076263
3446.764215	503502.185796	51.081268
3445.996439	503129.006298	51.086273
3445.389767	502767.990888	51.091277
3444.816373	502396.739047	51.096282
3444.198485	502028.371446	51.101287
3443.067624	501660.279745	51.106292
3442.663058	501286.649684	51.111297
3441.938038	500929.411749	51.116301
3441.053281	500557.968223	51.121306
3440.638985	500190.239030	51.126311
3439.791627	499828.898257	51.131316
3439.164807	499460.833332	51.136321
3438.156924	499106.742206	51.141325
3437.787257	498739.431795	51.146330
3437.187261	498371.239065	51.151335
3435.869435	498012.922975	51.156340
3435.355736	497651.283195	51.161345
3434.473238	497299.921199	51.166349
3434.162642	496945.626797	51.171354
3433.715518	496583.094494	51.176359
3432.828566	496224.269873	51.181364
3432.416470	495864.350486	51.186369
3431.378023	495504.168591	51.191373
3430.669549	495145.091993	51.196378
3430.030839	494786.604932	51.201383
3429.184876	494429.308235	51.206388
3428.858760	494071.365405	51.211393
3427.987362	493714.666469	51.216397
3427.250401	493357.990011	51.221402
3426.705737	492992.110569	51.226407
3426.089273	492638.236958	51.231412
3425.454897	492279.244662	51.236417
3424.558618	491921.704801	51.241421
3423.847062	491565.800078	51.246426
3423.393855	491204.985877	51.251431
3422.426104	490852.653114	51.256436
3421.812187	490495.598333	51.261441
3420.910634	490142.937847	51.266445
3419.918921	489789.626554	51.271450
3419.254124	489438.840016	51.276455
3418.617624	489098.324361	51.281460
3418.019851	488749.742969	51.286465
3417.082840	488411.642999	51.291469
3416.605751	488066.828787	51.296474
3416.194878	487716.577906	51.301479
3415.193996	487381.660797	51.306484
3414.981506	487019.917808	51.311489
3414.037928	486688.018732	51.316493
3413.221619	486338.515739	51.321498
3412.508679	485993.701200	51.326503
3411.775186	485655.368034	51.331508
3411.413905	485300.860212	51.336513
3410.228843	484967.398978	51.341517
3409.450758	484627.078951	51.346522
3409.207382	484281.804765	51.351527
3408.299209	483953.905731	51.356532
3407.522663	483603.688023	51.361537
3406.992022	483269.891294	51.366541
3406.497964	482933.803057	51.371546
3405.715074	482595.119981	51.376551
3404.555140	482264.800139	51.381556
3404.328825	481922.166596	51.386561
3403.345076	481593.732931	51.391565
3402.728349	481260.118003	51.396570
3402.176510	480922.433422	51.401575
3401.281823	480588.749658	51.406580
3400.638378	480246.304736	51.411585
3399.842634	479915.786300	51.416589
3399.225696	479585.690120	51.421594
3398.775576	479250.139752	51.426599
3397.700030	478928.061154	51.431604
3397.343634	478597.248477	51.436609
3396.354036	478264.503268	51.441613
3395.566963	477937.345828	51.446618
3395.258606	477597.640085	51.451623
3394.516361	477291.750467	51.456628
3393.884169	476954.466958	51.461633
3393.417978	476633.825988	51.466637
3392.511220	476295.155671	51.471642
3392.091658	475966.488717	51.476647
3391.217482	475641.081407	51.481652
3390.710021	475297.617457	51.486657
3389.817863	474974.178955	51.491661
3389.023458	474654.419986	51.496666
3388.753234	474317.693953	51.501671
3387.542847	473985.064710	51.506676
3387.127120	473661.377838	51.511681
3386.548820	473336.748396	51.516685
3385.866736	473000.521865	51.521690
3385.203530	472675.540477	51.526695
3384.396872	472351.641154	51.531700
3383.920822	472026.417088	51.536705
3383.093908	471705.400296	51.541709
3382.335883	471368.550627	51.546714
3381.797941	471034.043368	51.551719
3380.988324	470709.611653	51.556724
3380.268099	470392.663983	51.561729
3379.473604	470073.796651	51.566733
3378.881450	469737.350422	51.571738
3378.477022	469409.893699	51.576743
3377.278004	469095.638312	51.581748
3376.761405	468761.090971	51.586753
3376.015167	468446.297882	51.591757
3375.461024	468129.441543	51.596762
3374.827123	467802.857826	51.601767
3373.929663	467490.203837	51.606772
3373.593733	467174.718300	51.611777
3372.606835	466852.789832	51.616781
3372.071055	466529.010362	51.621786
3371.522771	466209.639497	51.626791
3370.494127	465891.556768	51.631796
3369.859900	465559.512492	51.636801
3369.168871	465247.147592	51.641805
3368.436930	464935.443812	51.646810
3367.871360	464613.211826	51.651815
3366.948014	464303.202547	51.656820
3366.230278	463988.338498	51.661825
3365.461588	463679.867834	51.666829
3364.779510	463366.003273	51.671834
3364.246654	463060.630726	51.676839
3363.543341	462754.925780	51.681844
3362.762533	462445.881434	51.686849
3361.982797	462140.281288	51.691853
3361.221709	461829.196290	51.696858
3360.760466	461526.630931	51.701863
3359.842841	461225.756546	51.706868
3359.335813	460917.965804	51.711873
3358.843621	460616.153461	51.716877
3357.659317	460314.091323	51.721882
3357.254161	460003.076071	51.726887
3356.220647	459712.191456	51.731892
3356.082914	459406.958622	51.736897
3355.183608	459108.740520	51.741901
3354.255530	458804.182248	51.746906
3354.020588	458492.611411	51.751911
3352.961217	458208.711175	51.756916
3352.345581	457904.953428	51.761921
3351.721733	457604.794505	51.766925
3351.165347	457304.215017	51.771930
3350.361455	457003.112571	51.776935
3349.686783	456712.334569	51.781940
3349.089426	456409.365142	51.786945
3348.348116	456110.828006	51.791949
3347.573438	455816.705858	51.796954
3346.975361	455517.377166	51.801959
3346.307047	455229.014029	51.806964
3345.799484	454922.154518	51.811969
3344.845865	454622.920856	51.816973
3344.197845	454330.382725	51.821978
3343.830379	454037.593494	51.826983
3342.962711	453739.653668	51.831988
3342.463932	453446.065756	51.836993
3341.390006	453143.939495	51.841997
3340.893639	452853.032657	51.847002
3340.664987	452559.187614	51.852007
3339.625492	452263.082214	51.857012
3338.988687	451966.249665	51.862017
3338.471091	451677.817500	51.867021
3337.228204	451373.208170	51.872026
3336.984460	451085.181926	51.877031
3336.316680	450792.956680	51.882036
3335.532860	450493.235950	51.887041
3334.900523	450195.364927	51.892045
3334.019744	449913.615637	51.897050
3333.595899	449607.077355	51.902055
3332.908660	449322.245505	51.907060
3332.307024	449025.927737	51.912065
3331.401677	448736.555942	51.917069
3330.495734	448442.410281	51.922074
3330.010627	448147.179381	51.927079
3329.068847	447862.471438	51.932084
3328.543192	447569.269654	51.937089
3328.078161	447296.101296	51.942093
3327.389915	447003.374917	51.947098
3326.820807	446722.299090	51.952103
3325.640026	446434.414244	51.957108
3325.249301	446139.701485	51.962113
3324.335371	445860.903093	51.967117
3323.768840	445574.687045	51.972122
3323.260755	445282.722948	51.977127
3322.503411	445006.884330	51.982132
3321.979606	444719.788387	51.987137
3321.278817	444430.331391	51.992141
3320.187393	444150.627402	51.997146
3319.724442	443874.373846	52.002151
3319.111597	443587.582948	52.007156
3318.333720	443306.245999	52.012161
3317.549217	443028.003179	52.017165
3316.971881	442750.638079	52.022170
3316.709210	442460.428176	52.027175
3315.697709	442196.221797	52.032180
3315.033156	441903.124578	52.037185
3314.156664	441623.357272	52.042189
3313.408118	441345.038659	52.047194
3312.919682	441066.371146	52.052199
3312.188239	440787.434291	52.057204
3311.709028	440507.439055	52.062209
3310.784713	440242.030079	52.067213
3310.365521	439955.165634	52.072218
3309.917172	439678.354345	52.077223
3308.704749	439396.355550	52.082228
3308.103127	439108.469347	52.087233
3307.674290	438829.919323	52.092237
3306.996588	438554.933995	52.097242
3306.290116	438283.732531	52.102247
3305.181796	438008.377697	52.107252
3304.771473	437722.653659	52.112257
3304.034349	437453.047271	52.117261
3303.214309	437182.054846	52.122266
3302.692817	436904.894145	52.127271
3302.136710	436639.109082	52.132276
3301.391604	436363.932534	52.137281
3300.631239	436094.188251	52.142285
3300.046282	435811.465709	52.147290
3299.208022	435544.114279	52.152295
3298.608032	435277.230095	52.157300
3298.021023	435000.795035	52.162305
3297.094396	434730.859373	52.167309
3296.324664	434467.141685	52.172314
3295.798969	434186.930512	52.177319
3294.781557	433926.927820	52.182324
3294.113335	433664.886858	52.187329
3293.757778	433394.211969	52.192333
3292.989297	433136.853199	52.197338
3292.228235	432866.998575	52.202343
3291.436059	432621.546500	52.207348
3291.113645	432348.697132	52.212353
3290.395065	432084.007331	52.217357
3289.674378	431817.461570	52.222362
3289.210779	431545.590920	52.227367
3288.468894	431286.533607	52.232372
3287.825088	431014.736674	52.237377
3286.927464	430748.385649	52.242381
3286.091240	430488.852847	52.247386
3285.761849	430218.394477	52.252391
3284.932298	429963.299175	52.257396
3284.303082	429699.129602	52.262401
3283.735199	429434.922273	52.267405
3282.715021	429188.762804	52.272410
3282.178869	428923.250216	52.277415
3281.848196	428671.186959	52.282420
3280.928402	428399.330347	52.287425
3280.622732	428135.297070	52.292429
3279.547674	427873.135121	52.297434
3278.841616	427604.131607	52.302439
3277.840835	427351.399905	52.307444
3277.741580	427091.818664	52.312449
3276.983624	426828.174084	52.317453
3276.032619	426573.344638	52.322458
3275.732520	426298.371750	52.327463
3274.497097	426050.541036	52.332468
3274.063283	425791.787409	52.337473
3273.477431	425539.734889	52.342477
3272.953210	425286.552762	52.347482
3272.308049	425018.859732	52.352487
3271.493590	424767.598099	52.357492
3271.030889	424493.877032	52.362497
3270.423259	424237.574270	52.367501
3269.425462	423980.441837	52.372506
3269.060019	423724.908708	52.377511
3267.954030	423472.512848	52.382516
3267.441089	423211.130966	52.387521
3266.548667	422953.591198	52.392525
3266.370555	422691.592605	52.397530
3265.662773	422447.455575	52.402535
3264.891819	422196.061791	52.407540
3264.461857	421929.015645	52.412545
3263.693898	421668.675471	52.417549
3262.492413	421411.957604	52.422554
3262.073062	421154.122991	52.427559
3261.424716	420890.733801	52.432564
3260.863236	420639.775390	52.437569
3260.295828	420387.062899	52.442573
3259.670076	420130.521567	52.447578
3258.925252	419869.297204	52.452583
3258.077046	419625.106760	52.457588
3257.503349	419359.836913	52.462593
3256.927805	419099.899581	52.467597
3256.040844	418844.962826	52.472602
3255.590905	418594.984619	52.477607
3254.483026	418344.396950	52.482612
3254.325900	418080.344797	52.487617
3253.448999	417827.886913	52.492621
3252.541898	417580.766575	52.497626
3252.286865	417315.350941	52.502631
3251.418680	417066.136769	52.507636
3250.984575	416819.366910	52.512641
3250.331421	416557.055863	52.517645
3249.280769	416296.278835	52.522650
3248.622594	416042.855967	52.527655
3248.100101	415799.267091	52.532660
3247.315336	415539.940130	52.537665
3246.596575	415289.899308	52.542669
3246.063054	415042.189883	52.547674
3245.517781	414780.709452	52.552679
3244.444213	414535.774296	52.557684
3243.838946	414287.510817	52.562689
3243.534492	414018.693430	52.567693
3242.660483	413772.729387	52.572698
3241.748731	413515.742005	52.577703
3241.124122	413277.229826	52.582708
3240.565519	413027.144260	52.587713
3240.141140	412781.507327	52.592717
3239.227061	412529.974634	52.597722
3238.719729	412264.755986	52.602727
3237.878986	412028.453102	52.607732
3237.236800	411780.606250	52.612737
3236.782121	411531.635036	52.617741
3235.632936	411280.128919	52.622746
3235.017259	411025.614080	52.627751
3234.306503	410778.735333	52.632756
3233.616295	410536.730200	52.637761
3232.978471	410295.578806	52.642765
3232.173801	410060.271065	52.647770
3231.718708	409810.701128	52.652775
3230.980178	409573.727370	52.657780
3230.354590	409330.482543	52.662785
3229.755766	409089.010378	52.667789
3229.213561	408847.654393	52.672794
3228.516543	408593.284325	52.677799
3227.810769	408349.663125	52.682804
3227.033954	408103.789456	52.687809
3226.388251	407870.218464	52.692813
3225.576041	407643.254090	52.697818
3225.218550	407405.008723	52.702823
3224.222349	407175.782768	52.707828
3223.539530	406930.266015	52.712833
3223.001795	406683.453646	52.717837
3222.445202	406445.638970	52.722842
3221.734476	406198.214728	52.727847
3220.648952	405969.222665	52.732852
3220.141561	405724.456439	52.737857
3219.691767	405479.577514	52.742861
3218.823632	405251.536966	52.747866
3218.630756	405005.164999	52.752871
3217.524200	404778.404070	52.757876
3216.981251	404528.805098	52.762881
3216.550214	404285.845463	52.767885
3215.728793	404054.637206	52.772890
3215.168693	403815.252635	52.777895
3214.551919	403572.698124	52.782900
3213.664230	403331.404618	52.787905
3212.761953	403087.595288	52.792909
3212.069580	402849.723941	52.797914
3211.521418	402600.491808	52.802919
3210.855608	402372.906770	52.807924
3210.157836	402134.395491	52.812929
3209.668801	401896.001920	52.817933
3208.999641	401667.827776	52.822938
3208.206168	401428.462158	52.827943
3207.210136	401194.795145	52.832948
3206.769854	400940.652659	52.837953
3206.449188	400694.089527	52.842957
3205.163956	400460.386686	52.847962
3205.002567	400218.776893	52.852967
3204.080193	399985.953748	52.857972
3203.545122	399750.424016	52.862977
3202.776354	399503.998987	52.867981
3201.887581	399282.807820	52.872986
3201.459489	399044.332759	52.877991
3200.711412	398810.151798	52.882996
3200.042001	398571.711475	52.888001
3199.470906	398342.176579	52.893005
3198.854073	398111.223743	52.898010
3198.236882	397867.558760	52.903015
3197.622177	397640.339210	52.908020
3196.901036	397407.694732	52.913025
3196.035440	397167.877130	52.918029
3195.226748	396940.352996	52.923034
3194.841807	396706.633555	52.928039
3194.405230	396482.326877	52.933044
3193.669898	396237.753445	52.938049
3192.980155	396003.670554	52.943053
3192.128871	395770.628497	52.948058
3191.746075	395538.731016	52.953063
3190.733716	395305.406147	52.958068
3189.945066	395076.620470	52.963073
3189.582023	394836.274506	52.968077
3188.542441	394612.025346	52.973082
3188.083093	394373.648963	52.978087
3187.423578	394152.540050	52.983092
3186.634436	393917.594042	52.988097
3186.378232	393681.443438	52.993101
3185.376792	393453.748342	52.998106
3184.859544	393217.254471	53.003111
3184.128954	392993.378028	53.008116
3183.232515	392760.042834	53.013121
3182.938575	392523.000370	53.018125
3182.139331	392300.884635	53.023130
3181.533456	392064.854547	53.028135
3180.533274	391839.106367	53.033140
3179.801624	391610.568246	53.038145
3179.250329	391377.092871	53.043149
3178.047064	391161.085172	53.048154
3177.875224	390933.521959	53.053159
3176.784287	390718.434536	53.058164
3176.674555	390488.315961	53.063169
3175.741580	390263.080941	53.068173
3175.059644	390048.916368	53.073178
3174.591479	389818.316162	53.078183
3173.813659	389592.874334	53.083188
3173.236110	389368.925040	53.088193
3172.449001	389143.685251	53.093197
3171.654528	388922.666219	53.098202
3171.238804	388699.755085	53.103207
3170.413475	388478.153340	53.108212
3169.449255	388257.411331	53.113217
3169.098423	388032.782088	53.118221
3168.480725	387822.357385	53.123226
3167.981790	387586.661925	53.128231
3167.151909	387371.996135	53.133236
3166.370785	387154.168154	53.138241
3166.260483	386925.577898	53.143245
3165.277948	386713.704144	53.148250
3164.630820	386479.728702	53.153255
3164.096890	386266.153884	53.158260
3163.369176	386034.349859	53.163265
3162.693153	385802.510760	53.168269
3161.705737	385590.504116	53.173274
3161.451336	385361.214833	53.178279
3160.586842	385140.361834	53.183284
3159.664300	384917.202513	53.188289
3159.377710	384687.456388	53.193293
3158.575324	384472.260635	53.198298
3157.636728	384250.727420	53.203303
3157.064680	384033.102164	53.208308
3156.358000	383813.055528	53.213313
3155.624415	383592.121750	53.218317
3155.138543	383378.395501	53.223322
3154.720980	383145.125599	53.228327
3153.915403	382929.768879	53.233332
3152.874105	382708.624269	53.238337
3152.924520	382480.845848	53.243341
3151.846406	382262.476569	53.248346
3151.493728	382035.700246	53.253351
3150.487435	381822.149257	53.258356
3149.782562	381601.326452	53.263361
3149.283557	381377.875633	53.268365
3148.384286	381172.620665	53.273370
3147.816626	380939.589856	53.278375
3146.931098	380721.104984	53.283380
3146.034854	380504.350051	53.288385
3145.694478	380286.107097	53.293389
3144.860721	380083.252154	53.298394
3144.208218	379869.608893	53.303399
3143.712087	379648.156869	53.308404
3142.979015	379425.316751	53.313409
3142.697281	379217.333958	53.318413
3141.731175	379009.916157	53.323418
3141.503612	378776.665926	53.328423
3140.688552	378564.465577	53.333428
3139.469256	378346.859517	53.338433
3139.011180	378135.948429	53.343437
3137.953681	377920.629011	53.348442
3137.317598	377695.423679	53.353447
3136.909003	377496.023585	53.358452
3136.221711	377279.624687	53.363457
3135.773375	377071.021034	53.368461
3134.831862	376867.454326	53.373466
3134.273382	376643.349941	53.378471
3133.293428	376435.564727	53.383476
3132.673052	376232.045722	53.388481
3132.433429	376019.003077	53.393485
3131.398321	375811.503164	53.398490
3130.817020	375597.393141	53.403495
3130.325489	375392.425054	53.408500
3129.617007	375178.536434	53.413505
3128.889367	374961.495514	53.418509
3128.231132	374757.949644	53.423514
3127.956314	374545.871441	53.428519
3127.407957	374339.304486	53.433524
3126.519787	374123.810764	53.438529
3125.729673	373893.546474	53.443533
3124.928817	373686.507429	53.448538
3124.512992	373476.684552	53.453543
3123.879233	373269.540663	53.458548
3123.063282	373055.734288	53.463553
3122.623046	372828.639371	53.468557
3121.581946	372623.413715	53.473562
3121.109075	372409.804121	53.478567
3120.544851	372193.256985	53.483572
3119.521128	371985.710511	53.488577
3119.250107	371768.555131	53.493581
3118.620924	371560.206395	53.498586
3118.163109	371341.475696	53.503591
3117.223875	371125.847338	53.508596
3116.614138	370910.140306	53.513601
3116.311035	370700.590957	53.518605
3114.823241	370488.862118	53.523610
3114.389894	370262.744425	53.528615
3113.672924	370054.936427	53.533620
3113.000378	369843.558756	53.538625
3112.464762	369630.428432	53.543629
3111.837054	369419.906555	53.548634
3111.227498	369205.233955	53.553639
3110.635149	368992.262096	53.558644
3109.572268	368786.130915	53.563649
3109.167212	368555.674831	53.568653
3108.262654	368358.293717	53.573658
3107.393881	368140.145988	53.578663
3106.927240	367945.594017	53.583668
3106.603120	367733.235033	53.588673
3105.912228	367516.913282	53.593677
3104.911852	367304.481140	53.598682
3104.329067	367086.537340	53.603687
3103.867882	366881.217890	53.608692
3102.992105	366674.996291	53.613697
3103.039216	366451.021684	53.618701
3101.843740	366245.255754	53.623706
3101.185096	366033.119640	53.628711
3100.533775	365826.298861	53.633716
3099.611841	365609.291982	53.638721
3098.905776	365392.682424	53.643725
3098.316370	365189.868884	53.648730
3097.686252	364984.389354	53.653735
3097.168005	364777.873461	53.658740
3096.403866	364565.365477	53.663745
3095.906192	364354.188279	53.668749
3095.240282	364160.058441	53.673754
3094.698132	363943.721345	53.678759
3093.912109	363734.113525	53.683764
3092.922933	363514.969996	53.688769
3092.455438	363305.411591	53.693773
3091.693455	363104.829715	53.698778
3091.300830	362888.463994	53.703783
3090.302456	362687.078052	53.708788
3089.577755	362479.872042	53.713793
3089.099838	362266.570253	53.718797
3088.308366	362059.601941	53.723802
3087.423676	361851.298889	53.728807
3086.812781	361653.383995	53.733812
3086.292185	361449.881521	53.738817
3085.761968	361242.664704	53.743821
3085.367785	361045.730768	53.748826
3084.703419	360823.495211	53.753831
3083.507271	360613.989155	53.758836
3082.631346	360418.960921	53.763841
3082.676798	360206.355805	53.768845
3081.589741	360005.710351	53.773850
3081.051785	359799.531746	53.778855
3080.412886	359586.065226	53.783860
3079.703950	359391.031827	53.788865
3079.430558	359178.294491	53.793869
3078.497215	358972.531161	53.798874
3078.115144	358763.600703	53.803879
3077.361242	358552.819697	53.808884
3076.412945	358343.875253	53.813889
3076.219944	358122.901307	53.818893
3075.173350	357927.279297	53.823898
3074.817528	357706.354687	53.828903
3074.062624	357497.757738	53.833908
3073.261073	357289.192737	53.838913
3072.624970	357082.916380	53.843917
3071.978753	356881.246747	53.848922
3071.179569	356663.441328	53.853927
3070.688073	356458.233740	53.858932
3069.874204	356247.554165	53.863937
3069.210280	356034.890493	53.868941
3068.420436	355821.889576	53.873946
3067.589768	355634.164131	53.878951
3067.143871	355429.912151	53.883956
3066.276737	355228.067246	53.888961
3066.038539	355006.857607	53.893965
3065.167526	354806.487646	53.898970
3064.430635	354603.499920	53.903975
3064.143731	354394.281602	53.908980
3063.141532	354188.331273	53.913985
3062.681334	353978.655159	53.918989
3061.943556	353773.882873	53.923994
3061.052598	353555.213373	53.928999
3060.268899	353353.805970	53.934004
3059.630515	353154.258036	53.939009
3059.206731	352946.200736	53.944013
3058.190105	352749.561441	53.949018
3058.025556	352544.210060	53.954023
3057.598480	352336.736200	53.959028
3056.390242	352137.147323	53.964033
3056.131988	351923.664425	53.969037
3055.512262	351719.221710	53.974042
3054.839551	351506.133569	53.979047
3054.103422	351300.206109	53.984052
3053.340548	351083.720225	53.989057
3052.654419	350869.537305	53.994061
3052.099592	350671.493799	53.999066
3051.579671	350459.039021	54.004071
3050.901487	350255.541636	54.009076
3049.799741	350051.754206	54.014081
3049.476829	349842.294469	54.019085
3048.503632	349630.442643	54.024090
3048.024319	349417.035673	54.029095
3047.577709	349210.214544	54.034100
3046.720833	349008.827776	54.039105
3045.917413	348796.462283	54.044109
3045.018676	348594.189827	54.049114
3044.275350	348387.285309	54.054119
3043.895847	348183.503895	54.059124
3043.040940	347992.421022	54.064129
3042.569274	347780.711785	54.069133
3041.885873	347577.638000	54.074138
3041.363308	347374.945257	54.079143
3040.510455	347175.103785	54.084148
3039.553425	346974.819953	54.089153
3039.156304	346763.705944	54.094157
3038.345750	346571.694943	54.099162
3037.904464	346371.378263	54.104167
3037.382230	346164.430579	54.109172
3036.803780	345970.140998	54.114177
3035.968562	345759.398039	54.119181
3035.070370	345555.791060	54.124186
3034.630907	345351.474441	54.129191
3033.937133	345152.211586	54.134196
3032.953494	344951.339472	54.139201
3032.720148	344739.326703	54.144205
3031.410708	344545.275293	54.149210
3031.035786	344348.504553	54.154215
3030.595896	344149.274454	54.159220
3029.854289	343951.898631	54.164225
3029.349091	343749.470375	54.169229
3028.624618	343558.937544	54.174234
3028.178282	343345.528061	54.179239
3027.499777	343137.067152	54.184244
3026.679723	342934.355054	54.189249
3026.285709	342721.138692	54.194253
3025.259433	342529.479459	54.199258
3024.762733	342319.256056	54.204263
3024.170833	342115.181473	54.209268
3023.117042	341914.793826	54.214273
3022.917325	341711.775810	54.219277
3022.487176	341502.888137	54.224282
3021.986185	341294.774602	54.229287
3020.943179	341087.535241	54.234292
3020.350970	340872.612851	54.239297
3019.841712	340662.538470	54.244301
3019.021991	340461.930852	54.249306
3018.407668	340252.788092	54.254311
3017.735595	340040.980982	54.259316
3016.615578	339829.422237	54.264321
3016.748337	339624.588347	54.269325
3015.423070	339420.111831	54.274330
3014.715322	339208.791217	54.279335
3014.046033	339003.522235	54.284340
3013.338695	338800.422342	54.289345
3012.809496	338593.500707	54.294349
3011.883298	338402.347466	54.299354
3011.452888	338198.972733	54.304359
3010.882781	337992.259282	54.309364
3009.884077	337788.667730	54.314369
3009.552229	337587.922903	54.319373
3008.672295	337384.718585	54.324378
3008.294137	337170.920773	54.329383
3007.494076	336966.506068	54.334388
3006.611966	336773.559110	54.339393
3006.095691	336566.654429	54.344397
3004.994750	336374.911941	54.349402
3004.844527	336170.111895	54.354407
3004.393501	335976.585252	54.359412
3003.234737	335776.016702	54.364417
3002.603850	335570.043509	54.369421
3001.962532	335369.162730	54.374426
3001.427524	335162.307578	54.379431
3000.865173	334962.838687	54.384436
2999.802342	334765.128601	54.389441
2999.356323	334562.788919	54.394445
2998.604425	334371.240052	54.399450
2997.848852	334163.831260	54.404455
2997.393178	333968.568515	54.409460
2997.057892	333764.274185	54.414465
2996.223925	333552.726382	54.419469
2995.417415	333359.477690	54.424474
2994.705357	333158.041563	54.429479
2994.237083	332946.586787	54.434484
2993.513549	332763.811958	54.439489
2992.877497	332555.666637	54.444493
2992.490119	332353.413076	54.449498
2991.668256	332150.056635	54.454503
2990.879261	331951.124142	54.459508
2990.330307	331751.618477	54.464513
2989.957331	331542.690266	54.469517
2989.020705	331339.884315	54.474522
2988.205058	331129.039214	54.479527
2987.402430	330931.888159	54.484532
2986.588839	330724.249340	54.489537
2986.362584	330530.697476	54.494541
2985.411675	330333.186395	54.499546
2984.832227	330133.910244	54.504551
2984.197875	329921.378142	54.509556
2983.594008	329728.851382	54.514561
2982.858987	329518.829044	54.519565
2982.297666	329324.257780	54.524570
2981.592007	329123.344055	54.529575
2980.984311	328915.209313	54.534580
2980.078842	328719.519831	54.539585
2979.880474	328512.108429	54.544589
2979.020618	328310.987820	54.549594
2978.204390	328109.961613	54.554599
2977.543279	327909.037624	54.559604
2976.846085	327711.734097	54.564609
2976.486282	327498.056963	54.569613
2975.678116	327306.905769	54.574618
2975.169082	327101.245545	54.579623
2974.448311	326903.128980	54.584628
2973.647691	326703.089593	54.589633
2972.995449	326502.007809	54.594637
2972.365273	326291.450848	54.599642
2971.656986	326088.314614	54.604647
2971.054189	325896.796505	54.609652
2970.106606	325690.030857	54.614657
2969.864652	325485.037051	54.619661
2969.003965	325294.118456	54.624666
2968.374526	325086.893534	54.629671
2967.977601	324888.542484	54.634676
2966.715754	324692.186489	54.639681
2966.225009	324489.139102	54.644685
2965.826109	324283.708823	54.649690
2965.093592	324082.684645	54.654695
2964.396014	323888.605273	54.659700
2963.637377	323683.052224	54.664705
2963.139319	323475.980683	54.669709
2962.294487	323281.286686	54.674714
2961.624536	323071.848018	54.679719
2961.320873	322882.236049	54.684724
2960.637895	322681.200674	54.689729
2959.981717	322469.186755	54.694733
2959.244444	322266.605860	54.699738
2958.575026	322060.169070	54.704743
2958.076198	321848.001407	54.709748
2957.223764	321656.691297	54.714753
2956.583447	321440.216572	54.719757
2955.842509	321244.483050	54.724762
2955.025179	321046.647861	54.729767
2954.677491	320834.912132	54.734772
2953.789666	320642.434177	54.739777
2953.425470	320434.290228	54.744781
2952.465546	320245.820352	54.749786
2952.038806	320035.393803	54.754791
2951.195370	319824.217939	54.759796
2950.320696	319627.610874	54.764801
2949.842864	319425.287958	54.769805
2948.916241	319230.521540	54.774810
2948.217305	319024.795339	54.779815
2947.774576	318822.236380	54.784820
2946.876216	318631.309042	54.789825
2946.747638	318426.051400	54.794829
2945.899522	318229.589932	54.799834
2945.109321	318014.709442	54.804839
2944.682566	317821.999810	54.809844
2943.722158	317620.513252	54.814849
2943.570390	317408.178446	54.819853
2942.792707	317220.361074	54.824858
2942.011412	317010.925953	54.829863
2941.556409	316807.473434	54.834868
2940.601852	316603.462996	54.839873
2939.998907	316402.986756	54.844877
2939.369926	316192.812803	54.849882
2938.482797	315984.970949	54.854887
2938.037912	315776.294755	54.859892
2937.229331	315582.418904	54.864897
2936.544614	315367.235777	54.869901
2935.644669	315176.327345	54.874906
2935.194406	314982.750103	54.879911
2934.723803	314778.404687	54.884916
2933.736368	314581.448696	54.889921
2933.378070	314375.200401	54.894925
2932.746820	314172.305169	54.899930
2932.293345	313978.573763	54.904935
2931.711657	313769.278532	54.909940
2930.663956	313557.815850	54.914945
2930.487202	313345.578272	54.919949
2929.606458	313147.074859	54.924954
2928.670578	312937.604879	54.929959
2928.316772	312732.142034	54.934964
2927.658885	312531.845192	54.939969
2927.079813	312323.667124	54.944973
2926.218469	312119.123776	54.949978
2925.389048	311908.438144	54.954983
2924.985210	311698.779694	54.959988
2924.036787	311502.703087	54.964993
2923.639026	311290.776591	54.969997
2922.740833	311095.480710	54.975002
2922.180562	310893.510266	54.980007
2921.367493	310668.177712	54.985012
2920.877580	310478.698406	54.990017
2920.141376	310278.053410	54.995021
2919.314686	310079.052119	55.000026
2919.007965	309890.510497	55.005031
2918.534506	309683.049302	55.010036
2917.420464	309475.892869	55.015041
2916.952284	309276.196839	55.020045
2916.531197	309071.934829	55.025050
2915.240275	308865.671134	55.030055
2914.663496	308666.093135	55.035060
2914.010834	308459.269332	55.040065
2913.497677	308264.111486	55.045069
2912.820120	308059.735577	55.050074
2912.210813	307848.982276	55.055079
2911.630336	307645.583448	55.060084
2910.791417	307451.978327	55.065089
2910.100215	307243.732544	55.070093
2909.354490	307040.613546	55.075098
2908.440782	306845.058516	55.080103
2907.895586	306642.416440	55.085108
2907.515360	306445.604940	55.090113
2906.673443	306242.729093	55.095117
2906.074056	306048.498219	55.100122
2905.458039	305842.300955	55.105127
2904.761153	305636.421757	55.110132
2903.993879	305452.148103	55.115137
2903.823618	305245.293634	55.120141
2903.114678	305042.573152	55.125146
2901.935120	304838.526266	55.130151
2901.325124	304626.392696	55.135156
2900.437919	304437.400042	55.140161
2899.726472	304237.250793	55.145165
2899.345367	304047.489907	55.150170
2898.657613	303849.882925	55.155175
2898.280072	303652.837731	55.160180
2897.364275	303455.546426	55.165185
2897.018386	303252.129206	55.170189
2896.438830	303051.244353	55.175194
2895.264457	302853.305581	55.180199
2895.154275	302646.794280	55.185204
2894.048350	302435.245271	55.190209
2893.566028	302224.386677	55.195213
2893.069731	302023.996560	55.200218
2892.300879	301830.270518	55.205223
2891.885527	301628.822950	55.210228
2890.937528	301444.496324	55.215233
2890.552616	301226.541318	55.220237
2889.911194	301021.181482	55.225242
2889.245838	300814.297187	55.230247
2888.622592	300600.937507	55.235252
2887.542181	300396.181151	55.240257
2887.023947	300186.242247	55.245261
2886.371613	299986.740068	55.250266
2885.510179	299785.335300	55.255271
2885.438575	299573.313042	55.260276
2884.386740	299381.997185	55.265281
2883.852064	299173.689445	55.270285
2883.220993	298961.525788	55.275290
2882.470264	298766.901836	55.280295
2881.852779	298565.660708	55.285300
2881.016493	298359.589854	55.290305
2880.325353	298147.765769	55.295309
2879.716642	297937.660114	55.300314
2878.632976	297739.853451	55.305319
2878.670513	297536.953961	55.310324
2877.566417	297337.367415	55.315329
2877.133457	297133.090357	55.320333
2876.888658	296932.195840	55.325338
2875.863403	296723.402603	55.330343
2875.423563	296522.003719	55.335348
2874.313107	296323.282961	55.340353
2874.000842	296104.953378	55.345357
2873.245681	295895.097785	55.350362
2872.130041	295691.665799	55.355367
2872.191230	295491.357989	55.360372
2871.246425	295300.555679	55.365377
2870.282612	295087.548875	55.370381
2869.908518	294883.565711	55.375386
2869.018964	294677.728452	55.380391
2868.607904	294467.409403	55.385396
2867.746222	294276.669375	55.390401
2867.169547	294073.557906	55.395405
2866.319429	293867.204262	55.400410
2865.707609	293668.860350	55.405415
2865.096800	293471.509322	55.410420
2864.173181	293265.701558	55.415425
2863.799448	293068.134360	55.420429
2863.494767	292869.231751	55.425434
2862.505734	292663.051780	55.430439
2861.975874	292444.472687	55.435444
2861.378516	292248.188091	55.440449
2860.675517	292036.894253	55.445453
2860.047485	291834.196368	55.450458
2858.954688	291633.507433	55.455463
2858.491431	291432.438510	55.460468
2857.825600	291225.314752	55.465473
2857.395169	291012.932697	55.470477
2856.632034	290814.075502	55.475482
2855.861430	290609.540056	55.480487
2855.501072	290404.353736	55.485492
2854.482190	290201.945629	55.490497
2854.263219	289991.617602	55.495501
2853.481145	289786.854128	55.500506
2852.463894	289595.854834	55.505511
2852.203548	289378.325525	55.510516
2850.953237	289180.894047	55.515521
2850.454730	288974.098592	55.520525
2850.050765	288771.413800	55.525530
2849.265097	288568.993050	55.530535
2848.864187	288365.467058	55.535540
2847.925248	288159.148257	55.540545
2847.485238	287951.273179	55.545549
2846.715036	287753.153505	55.550554
2846.022118	287559.478350	55.555559
2845.797230	287345.558391	55.560564
2844.965217	287132.804079	55.565569
2844.198345	286918.332964	55.570573
2843.853778	286708.812030	55.575578
2842.946892	286506.256360	55.580583
2842.482998	286296.193776	55.585588
2841.374566	286086.080321	55.590593
2840.998142	285869.432896	55.595597
2840.373077	285661.789460	55.600602
2839.194968	285468.495583	55.605607
2838.859593	285259.558123	55.610612
2838.361601	285058.999826	55.615617
2837.460928	284845.210856	55.620621
2836.752262	284644.634778	55.625626
2836.146725	284445.850508	55.630631
2835.610040	284234.677739	55.635636
2834.426290	284028.599082	55.640641
2834.208830	283819.845973	55.645645
2833.434440	283614.364477	55.650650
2832.506692	283418.992566	55.655655
2832.151027	283205.574925	55.660660
2831.544914	283005.185622	55.665665
2830.958282	282805.506263	55.670669
2830.164835	282590.527719	55.675674
2829.524678	282393.887394	55.680679
2829.160312	282189.893947	55.685684
2828.291410	281981.599783	55.690689
2827.709700	281770.713242	55.695693
2827.184434	281563.714330	55.700698
2826.068835	281363.430574	55.705703
2825.751758	281148.248713	55.710708
2825.144490	280949.667111	55.715713
2824.368371	280741.867203	55.720717
2823.645617	280531.919445	55.725722
2822.818869	280318.371595	55.730727
2822.323632	280113.761500	55.735732
2821.258297	279917.977258	55.740737
2821.010190	279704.719634	55.745741
2820.649973	279499.527699	55.750746
2819.719998	279300.767553	55.755751
2819.102860	279090.751759	55.760756
2818.574295	278888.820824	55.765761
2817.853811	278676.121662	55.770765
2816.871473	278461.044432	55.775770
2816.291922	278261.464540	55.780775
2815.753661	278046.546126	55.785780
2814.949044	277853.699987	55.790785
2814.407607	277635.420185	55.795789
2813.799769	277435.284344	55.800794
2813.009106	277232.019351	55.805799
2812.359727	277026.847301	55.810804
2811.376176	276818.086169	55.815809
2810.799901	276613.590145	55.820813
2810.228814	276413.830401	55.825818
2809.634594	276213.870558	55.830823
2809.382568	275998.422670	55.835828
2808.494893	275796.777422	55.840833
2807.657116	275591.304004	55.845837
2807.143048	275385.753849	55.850842
2806.560375	275177.769586	55.855847
2805.732781	274963.813565	55.860852
2805.065732	274762.820999	55.865857
2804.319792	274557.358490	55.870861
2803.832929	274352.160576	55.875866
2802.895383	274146.830292	55.880871
2802.731046	273929.483830	55.885876
2801.833358	273736.168330	55.890881
2801.228915	273534.147149	55.895885
2800.838483	273315.053742	55.900890
2800.048516	273111.508400	55.905895
2799.117797	272893.366517	55.910900
2798.537038	272693.251782	55.915905
2797.918877	272479.313664	55.920909
2797.228502	272272.823774	55.925914
2796.493985	272067.130420	55.930919
2796.044083	271849.421891	55.935924
2795.236355	271647.662320	55.940929
2794.370198	271441.913502	55.945933
2793.718953	271241.631849	55.950938
2793.230065	271032.028573	55.955943
2792.793118	270817.374381	55.960948
2791.900763	270617.360243	55.965953
2791.275367	270405.002667	55.970957
2790.704970	270194.291870	55.975962
2789.634541	269995.350270	55.980967
2789.122994	269778.568796	55.985972
2788.703231	269575.041830	55.990977
2787.719699	269369.719547	55.995981
2787.539806	269164.040835	56.000986
2786.658470	268960.612604	56.005991
2786.023697	268748.664449	56.010996
2785.445426	268534.822761	56.016001
2784.373463	268330.100562	56.021005
2783.947230	268121.303118	56.026010
2783.185222	267928.451105	56.031015
2782.813397	267704.567990	56.036020
2782.129574	267504.037799	56.041025
2781.432074	267295.283612	56.046029
2781.076379	267088.512830	56.051034
2779.859201	266880.452346	56.056039
2779.313805	266652.725989	56.061044
2778.602240	266453.983364	56.066049
2777.987386	266257.874193	56.071053
2777.629689	266042.827007	56.076058
2776.497520	265837.555002	56.081063
2776.130431	265621.643585	56.086068
2775.554047	265422.650780	56.091073
2774.691909	265217.972998	56.096077
2774.146089	265006.037750	56.101082
2773.283921	264795.757200	56.106087
2772.818624	264588.953965	56.111092
2771.824033	264383.609939	56.116097
2771.272593	264172.032573	56.121101
2770.862308	263962.444941	56.126106
2769.922888	263758.493254	56.131111
2769.658202	263552.346443	56.136116
2768.830117	263348.377353	56.141121
2768.085778	263135.837880	56.146125
2767.461183	262933.186605	56.151130
2766.921853	262718.399208	56.156135
2766.214187	262505.064812	56.161140
2765.575354	262310.158413	56.166145
2764.843552	262095.019885	56.171149
2764.132654	261880.311145	56.176154
2763.362718	261682.064133	56.181159
2763.152578	261465.671893	56.186164
2762.463168	261266.877571	56.191169
2761.660793	261051.725476	56.196173
2760.750526	260843.365055	56.201178
2760.110299	260622.304536	56.206183
2759.850215	260409.231786	56.211188
2758.891827	260210.251575	56.216193
2758.184388	259991.621627	56.221197
2757.794209	259778.086077	56.226202
2756.828597	259568.054501	56.231207
2756.471233	259357.035385	56.236212
2755.660982	259151.996658	56.241217
2754.964561	258933.696909	56.246221
2754.638353	258731.485156	56.251226
2753.744971	258517.138967	56.256231
2752.983116	258301.727960	56.261236
2752.423184	258090.589170	56.266241
2751.681874	257879.301018	56.271245
2751.093750	257666.842753	56.276250
2750.228785	257463.596807	56.281255
2749.732519	257251.659182	56.286260
2748.987330	257043.759559	56.291265
2748.264480	256832.851435	56.296269
2747.520511	256612.422061	56.301274
2746.778891	256411.093031	56.306279
2746.297570	256204.222016	56.311284
2745.749008	255994.789651	56.316289
2744.815237	255779.459162	56.321293
2744.408587	255573.977622	56.326298
2743.556726	255369.203477	56.331303
2743.145781	255161.430969	56.336308
2742.632027	254953.394814	56.341313
2741.804017	254740.187883	56.346317
2741.073591	254520.700810	56.351322
2740.282419	254318.388410	56.356327
2739.957090	254112.411577	56.361332
2738.746319	253903.493693	56.366337
2738.094587	253694.411086	56.371341
2737.863088	253479.659411	56.376346
2737.087461	253287.175870	56.381351
2736.868068	253075.478766	56.386356
2735.472134	252855.869785	56.391361
2735.146413	252646.736696	56.396365
2734.718433	252429.597992	56.401370
2733.870421	252215.964094	56.406375
2733.506584	252011.116193	56.411380
2732.808496	251811.924153	56.416385
2731.875051	251583.686634	56.421389
2731.403077	251365.282854	56.426394
2730.445403	251150.496143	56.431399
2729.807078	250953.893212	56.436404
2729.055781	250741.620985	56.441409
2728.297112	250521.022630	56.446413
2727.655041	250314.387214	56.451418
2726.775046	250123.502564	56.456423
2726.216591	249900.912398	56.461428
2725.591618	249699.215536	56.466433
2724.882067	249489.790538	56.471437
2724.989228	249279.090462	56.476442
2723.708574	249080.681526	56.481447
2723.447038	248871.873965	56.486452
2722.575081	248655.650823	56.491457
2722.279159	248437.299440	56.496461
2721.665301	248221.316149	56.501466
2720.797344	248024.218363	56.506471
2720.225973	247798.602733	56.511476
2719.541661	247581.816594	56.516481
2718.838296	247368.115177	56.521485
2718.313814	247151.991927	56.526490
2717.232238	246938.911290	56.531495
2716.855309	246725.693881	56.536500
2716.369599	246516.262968	56.541505
2715.473615	246287.466899	56.546509
2714.373994	246081.011507	56.551514
2713.680164	245877.446167	56.556519
2713.372561	245652.938034	56.561524
2712.592456	245451.780757	56.566529
2711.732059	245235.790007	56.571533
2711.200376	245027.489075	56.576538
2710.514592	244825.604733	56.581543
2710.058616	244606.393181	56.586548
2709.318995	244406.835354	56.591553
2708.756025	244193.753144	56.596557
2708.174020	243974.919104	56.601562
2707.372047	243765.440599	56.606567
2706.710020	243552.757093	56.611572
2706.120893	243349.764665	56.616577
2705.281246	243137.008113	56.621581
2704.794188	242922.158842	56.626586
2704.317000	242719.404328	56.631591
2703.740967	242494.078219	56.636596
2702.857905	242277.943115	56.641601
2702.176067	242070.791134	56.646605
2701.405065	241866.658493	56.651610
2700.893867	241657.595760	56.656615
2700.321485	241422.365139	56.661620
2699.574872	241210.233741	56.666625
2698.634103	241002.335165	56.671629
2698.178555	240781.933272	56.676634
2697.491664	240574.937415	56.681639
2697.262987	240357.352416	56.686644
2696.390771	240143.103768	56.691649
2695.451960	239930.393935	56.696653
2695.167149	239712.335192	56.701658
2694.289486	239500.074820	56.706663
2693.639355	239282.074756	56.711668
2693.003957	239059.998467	56.716673
2692.009465	238851.195496	56.721677
2691.592480	238635.935348	56.726682
2690.896218	238424.335777	56.731687
2690.205603	238204.816340	56.736692
2689.284365	237995.748711	56.741697
2688.844240	237787.267329	56.746701
2688.500130	237574.187600	56.751706
2687.418547	237372.251030	56.756711
2686.888808	237147.997369	56.761716
2686.419152	236939.624138	56.766721
2685.584001	236729.093852	56.771725
2685.026343	236521.371970	56.776730
2684.112361	236311.440663	56.781735
2683.196404	236085.646190	56.786740
2683.169877	235877.535865	56.791745
2681.886234	235668.020892	56.796749
2681.562893	235456.215274	56.801754
2680.661438	235242.439126	56.806759
2680.155126	235034.941226	56.811764
2679.483683	234828.615758	56.816769
2678.905791	234622.046717	56.821773
2678.599869	234409.018259	56.826778
2677.585428	234187.877862	56.831783
2677.306172	233975.329898	56.836788
2676.527398	233770.042123	56.841793
2675.465286	233555.760263	56.846797
2674.904806	233337.936428	56.851802
2674.499709	233123.016700	56.856807
2673.988106	232912.264773	56.861812
2673.273931	232691.513025	56.866817
2672.567109	232477.864737	56.871821
2671.745833	232262.198035	56.876826
2670.932213	232046.887083	56.881831
2670.309953	231832.157404	56.886836
2669.548822	231633.542559	56.891841
2668.891892	231420.423449	56.896845
2668.592537	231193.727607	56.901850
2667.626842	230995.706690	56.906855
2667.146919	230774.107492	56.911860
2666.605348	230567.948734	56.916865
2665.752157	230354.175673	56.921869
2664.953171	230126.823188	56.926874
2664.207953	229927.420144	56.931879
2663.610704	229708.184619	56.936884
2663.180682	229507.841390	56.941889
2662.291379	229299.780016	56.946893
2661.919261	229071.445927	56.951898
2660.792199	228868.388288	56.956903
2660.416209	228645.301038	56.961908
2659.882338	228447.650125	56.966913
2658.935814	228236.417596	56.971917
2658.653429	228027.448286	56.976922
2657.939151	227807.013838	56.981927
2657.147633	227586.668571	56.986932
2656.506899	227379.310740	56.991937
2655.679538	227166.763406	56.996941
2655.209311	226953.829023	57.001946
2653.961528	226740.763747	57.006951
2653.526309	226537.041811	57.011956
2653.073443	226323.597036	57.016961
2652.332863	226116.665477	57.021965
2651.558317	225906.506272	57.026970
2650.916916	225698.325181	57.031975
2650.458266	225482.973902	57.036980
2649.940402	225279.382696	57.041985
2649.422018	225072.813176	57.046989
2648.794019	224844.976471	57.051994
2647.972638	224639.805460	57.056999
2647.413258	224417.407636	57.062004
2646.730988	224208.320224	57.067009
2646.133789	223993.567680	57.072013
2645.258262	223777.421301	57.077018
2644.528898	223566.153439	57.082023
2644.269823	223340.172052	57.087028
2643.206392	223134.648604	57.092033
2642.010249	222922.756258	57.097037
2641.895150	222703.704459	57.102042
2640.954491	222497.654028	57.107047
2640.378348	222290.655296	57.112052
2639.664789	222083.780726	57.117057
2639.379121	221876.113317	57.122061
2639.096049	221659.484281	57.127066
2637.774442	221448.532380	57.132071
2637.786785	221224.996429	57.137076
2636.878314	221012.350876	57.142081
2635.705467	220804.241371	57.147085
2635.530227	220577.007261	57.152090
2634.686195	220363.564089	57.157095
2634.122941	220150.293442	57.162100
2633.310583	219943.567647	57.167105
2632.641069	219728.494723	57.172109
2632.347135	219512.013599	57.177114
2631.304321	219294.913455	57.182119
2630.683526	219076.448695	57.187124
2630.354998	218874.677333	57.192129
2629.362898	218652.428416	57.197133
2629.028231	218438.591878	57.202138
2627.955356	218223.714575	57.207143
2627.181048	218004.666358	57.212148
2626.499798	217794.234414	57.217153
2625.957338	217582.215421	57.222157
2625.556831	217366.954116	57.227162
2624.896231	217162.337942	57.232167
2624.119893	216944.515289	57.237172
2623.616797	216730.074101	57.242177
2622.839023	216511.298347	57.247181
2622.233576	216294.799896	57.252186
2621.629802	216078.289123	57.257191
2621.118567	215862.999054	57.262196
2620.361077	215651.860055	57.267201
2619.592255	215425.843648	57.272205
2618.803142	215212.979903	57.277210
2618.273676	215011.505982	57.282215
2617.922619	214786.112840	57.287220
2617.179470	214567.108653	57.292225
2616.130311	214351.043028	57.297229
2615.731559	214122.502984	57.302234
2614.823748	213922.339638	57.307239
2614.196876	213695.008207	57.312244
2613.693128	213491.689133	57.317249
2613.063615	213269.629103	57.322253
2612.460212	213045.096398	57.327258
2611.748044	212832.635302	57.332263
2611.338375	212611.866382	57.337268
2610.569449	212396.793686	57.342273
2609.764356	212176.190713	57.347277
2609.076881	211951.484152	57.352282
2608.294558	211741.023294	57.357287
2607.624922	211521.355684	57.362292
2607.024648	211310.358266	57.367297
2606.527724	211089.213783	57.372301
2605.757052	210862.385919	57.377306
2604.871909	210658.168806	57.382311
2604.237332	210444.494120	57.387316
2603.577293	210222.894835	57.392321
2602.465076	210013.955622	57.397325
2602.295416	209799.140330	57.402330
2601.631075	209591.620684	57.407335
2601.011703	209371.277987	57.412340
2600.190055	209160.157358	57.417345
2599.728909	208951.474901	57.422349
2599.103787	208725.408060	57.427354
2598.141123	208516.182896	57.432359
2597.556131	208299.084039	57.437364
2597.053314	208092.600188	57.442369
2596.447618	207879.858819	57.447373
2595.923670	207655.752606	57.452378
2594.820179	207455.704221	57.457383
2594.572849	207231.657560	57.462388
2593.742918	207012.425775	57.467393
2593.009716	206796.208483	57.472397
2592.383264	206577.875112	57.477402
2591.797755	206372.924742	57.482407
2590.890151	206150.755779	57.487412
2590.721827	205938.359229	57.492417
2589.761309	205729.767001	57.497421
2589.092776	205509.242495	57.502426
2588.305468	205297.760840	57.507431
2587.722628	205074.348162	57.512436
2587.260621	204859.520349	57.517441
2586.383907	204644.020903	57.522445
2585.791414	204421.426752	57.527450
2585.087996	204221.122280	57.532455
2584.421609	204003.046603	57.537460
2584.057271	203786.043808	57.542465
2582.935760	203564.465814	57.547469
2582.318602	203348.484659	57.552474
2581.635212	203136.090876	57.557479
2580.970197	202924.140389	57.562484
2580.394859	202713.932683	57.567489
2579.559665	202497.187571	57.572493
2579.379780	202282.871924	57.577498
2578.298473	202073.968476	57.582503
2577.642162	201858.915480	57.587508
2577.344200	201640.663243	57.592513
2576.330660	201430.275264	57.597517
2575.737533	201214.387566	57.602522
2574.944377	201008.776598	57.607527
2574.334417	200790.131744	57.612532
2573.733483	200581.692263	57.617537
2572.914163	200373.020943	57.622541
2572.286392	200161.902217	57.627546
2571.574520	199954.437115	57.632551
2570.879884	199738.456772	57.637556
2570.709497	199528.006097	57.642561
2570.092567	199314.305694	57.647565
2569.391183	199101.026727	57.652570
2568.610728	198886.297736	57.657575
2568.136540	198667.449020	57.662580
2567.372749	198452.617323	57.667585
2566.312580	198240.136692	57.672589
2566.158980	198015.577194	57.677594
2565.458513	197811.630652	57.682599
2564.712234	197590.399012	57.687604
2564.239982	197371.160850	57.692609
2563.314565	197156.232770	57.697613
2562.731047	196942.867432	57.702618
2561.662853	196725.024330	57.707623
2561.533585	196507.593230	57.712628
2560.922814	196297.212414	57.717633
2560.039424	196075.194530	57.722637
2559.392915	195858.662483	57.727642
2558.796825	195650.559648	57.732647
2557.901259	195427.541249	57.737652
2557.285055	195208.462258	57.742657
2556.652125	195006.564614	57.747661
2556.322353	194790.763055	57.752666
2555.545998	194574.995007	57.757671
2554.612679	194357.076928	57.762676
2553.932219	194139.895882	57.767681
2553.114189	193925.104234	57.772685
2552.866550	193708.009144	57.777690
2552.116215	193495.575254	57.782695
2551.265978	193271.808437	57.787700
2550.827716	193057.711024	57.792705
2550.287205	192838.973850	57.797709
2549.470604	192618.919959	57.802714
2548.583911	192418.383448	57.807719
2547.911838	192196.094623	57.812724
2547.438169	191987.923889	57.817729
2546.720440	191773.889034	57.822733
2546.125997	191555.865875	57.827738
2545.391973	191349.571277	57.832743
2544.518668	191126.288595	57.837748
2544.125824	190909.381469	57.842753
2543.430995	190690.207552	57.847757
2542.521602	190486.450868	57.852762
2542.122090	190281.545503	57.857767
2541.764615	190049.381680	57.862772
2540.891878	189842.873741	57.867777
2540.060002	189626.601762	57.872781
2539.678066	189405.132156	57.877786
2538.592734	189186.586782	57.882791
2538.074628	188974.835504	57.887796
2537.619796	188753.902110	57.892801
2536.815824	188546.269297	57.897805
2536.111898	188323.367220	57.902810
2535.336648	188121.227862	57.907815
2534.690390	187900.786807	57.912820
2533.877049	187685.398601	57.917825
2533.013759	187485.400571	57.922829
2532.433912	187272.394503	57.927834
2531.784258	187063.407963	57.932839
2531.418336	186852.901629	57.937844
2531.028356	186634.881317	57.942849
2530.219534	186426.508089	57.947853
2529.532497	186216.399038	57.952858
2528.405055	186001.513700	57.957863
2527.741142	185782.764798	57.962868
2527.525689	185579.835372	57.967873
2526.661626	185368.524251	57.972877
2525.948562	185165.853633	57.977882
2525.330676	184954.645357	57.982887
2524.598790	184740.937264	57.987892
2524.401971	184527.374367	57.992897
2523.629712	184324.602402	57.997901
2523.271460	184103.154368	58.002906
2521.969945	183890.838163	58.007911
2521.525770	183682.139856	58.012916
2520.803179	183458.157617	58.017921
2520.104638	183253.012675	58.022925
2519.523877	183037.736765	58.027930
2519.124432	182829.111689	58.032935
2518.211893	182610.964601	58.037940
2517.661260	182399.045347	58.042945
2517.048840	182182.773663	58.047949
2516.596008	181968.385863	58.052954
2516.079846	181757.634545	58.057959
2515.391554	181537.638179	58.062964
2514.885974	181305.211410	58.067969
2513.950826	181089.975756	58.072973
2513.377833	180862.357665	58.077978
2512.453900	180652.757554	58.082983
2511.456265	180431.747301	58.087988
2511.041440	180212.566566	58.092993
2510.111948	180009.534107	58.097997
2510.027244	179787.555655	58.103002
2509.010277	179580.799372	58.108007
2508.367149	179360.895965	58.113012
2507.733100	179149.222045	58.118017
2506.765881	178933.060991	58.123021
2506.319609	178716.971107	58.128026
2505.585490	178500.571793	58.133031
2504.918864	178296.208418	58.138036
2504.341607	178073.248520	58.143041
2503.613819	177870.512292	58.148045
2503.309632	177652.675477	58.153050
2502.372455	177450.712193	58.158055
2501.682068	177225.866813	58.163060
2501.261622	177000.827227	58.168065
2500.244580	176794.936799	58.173069
2499.727641	176577.330101	58.178074
2498.982229	176363.042281	58.183079
2498.485827	176145.727135	58.188084
2497.967117	175927.678968	58.193089
2496.995390	175726.645313	58.198093
2496.585363	175494.642314	58.203098
2495.914264	175283.960473	58.208103
2495.084300	175072.236526	58.213108
2494.721372	174854.283841	58.218113
2493.515130	174641.286316	58.223117
2493.294527	174426.213193	58.228122
2492.607118	174220.181683	58.233127
2491.823133	173998.484800	58.238132
2491.388001	173778.183724	58.243137
2490.479568	173566.734436	58.248141
2489.907575	173352.880077	58.253146
2489.390401	173136.970557	58.258151
2488.653946	172923.665995	58.263156
2487.831944	172699.336959	58.268161
2487.197889	172497.286539	58.273165
2486.792555	172272.054485	58.278170
2485.968848	172061.006704	58.283175
2485.405154	171841.525175	58.288180
2484.893162	171617.801709	58.293185
2483.551994	171409.739034	58.298189
2483.352510	171190.966445	58.303194
2482.707811	170981.854549	58.308199
2482.096784	170763.798156	58.313204
2481.606293	170539.543292	58.318209
2480.780141	170329.751475	58.323213
2480.105521	170108.237033	58.328218
2479.376971	169891.844647	58.333223
2478.563982	169674.691117	58.338228
2478.284511	169445.284177	58.343233
2477.375259	169245.290681	58.348237
2476.774687	169018.976490	58.353242
2476.219650	168804.037833	58.358247
2475.259832	168580.860599	58.363252
2474.510511	168362.089367	58.368257
2473.848982	168152.194273	58.373261
2473.241443	167929.562673	58.378266
2472.332573	167725.914727	58.383271
2471.530240	167521.577024	58.388276
2471.314043	167298.670911	58.393281
2470.721790	167093.081464	58.398285
2469.990548	166875.218764	58.403290
2469.393968	166660.502251	58.408295
2468.565696	166445.276904	58.413300
2468.092634	166223.600433	58.418305
2467.502273	166014.545160	58.423309
2466.816012	165794.481774	58.428314
2465.724089	165583.257744	58.433319
2465.232972	165369.498297	58.438324
2464.867660	165149.693016	58.443329
2463.922665	164947.528135	58.448333
2462.955711	164730.935970	58.453338
2462.554120	164521.541281	58.458343
2461.556217	164331.772789	58.463348
2461.802754	164049.992408	58.468353
2460.741516	163832.530412	58.473357
2460.543999	163614.640351	58.478362
2459.557730	163400.996222	58.483367
2458.874627	163185.016629	58.488372
2458.375959	162957.642147	58.493377
2457.530081	162747.883001	58.498381
2457.245651	162530.496346	58.503386
2456.279611	162317.007950	58.508391
2455.262749	162090.140623	58.513396
2455.212737	161872.250330	58.518401
2454.503099	161668.273570	58.523405
2453.642438	161442.669696	58.528410
2452.855195	161223.844917	58.533415
2452.106624	160999.789892	58.538420
2451.919790	160783.326432	58.543425
2451.088242	160574.531220	58.548429
2450.285371	160348.658096	58.553434
2449.613389	160124.710852	58.558439
2448.793569	159916.375339	58.563444
2448.345860	159694.098886	58.568449
2447.199189	159492.670274	58.573453
2447.054874	159267.665871	58.578458
2446.356794	159059.443248	58.583463
2445.827560	158835.799379	58.588468
2445.176463	158605.362010	58.593473
2444.352151	158402.629944	58.598477
2443.702712	158180.992548	58.603482
2442.926544	157956.172998	58.608487
2442.068639	157745.364673	58.613492
2441.676896	157527.466294	58.618497
2440.858435	157313.399877	58.623501
2440.062607	157096.432725	58.628506
2439.589749	156885.962678	58.633511
2438.674637	156663.334666	58.638516
2438.272719	156447.694804	58.643521
2437.607447	156255.755580	58.648525
2436.846475	156029.318980	58.653530
2436.340769	155817.805566	58.658535
2435.737386	155600.524969	58.663540
2435.013781	155376.489343	58.668545
2434.305702	155179.147658	58.673549
2433.831399	154947.689735	58.678554
2432.508849	154741.219246	58.683559
2432.148273	154525.114640	58.688564
2431.630634	154309.125294	58.693569
2430.894995	154101.485190	58.698573
2430.059397	153885.269310	58.703578
2429.497036	153671.159716	58.708583
2428.900325	153461.404172	58.713588
2428.202254	153245.196034	58.718593
2427.782134	153041.516476	58.723597
2427.035852	152821.174914	58.728602
2426.245691	152602.684845	58.733607
2425.399187	152388.615797	58.738612
2424.961057	152175.843438	58.743617
2424.636635	151965.253361	58.748621
2423.625684	151754.989538	58.753626
2423.061480	151543.728364	58.758631
2422.421871	151328.743634	58.763636
2421.752610	151112.252478	58.768641
2421.056436	150905.795401	58.773645
2420.204797	150682.624977	58.778650
2419.693090	150473.434113	58.783655
2418.655230	150260.082858	58.788660
2418.289288	150050.312353	58.793665
2417.689500	149835.280267	58.798669
2417.165538	149619.576674	58.803674
2415.844384	149413.800049	58.808679
2415.375053	149196.285835	58.813684
2414.956533	148991.525367	58.818689
2414.373059	148785.063864	58.823693
2413.654297	148577.138137	58.828698
2412.856197	148357.025443	58.833703
2412.191022	148156.401760	58.838708
2411.711249	147923.989923	58.843713
2410.762308	147728.510247	58.848717
2410.553241	147512.643735	58.853722
2409.868096	147307.161022	58.858727
2409.303776	147091.175755	58.863732
2408.695305	146872.441173	58.868737
2407.743737	146662.785580	58.873741
2407.230142	146448.397920	58.878746
2406.679453	146231.234450	58.883751
2405.913368	146018.541824	58.888756
2405.185852	145795.106057	58.893761
2404.523645	145581.904285	58.898765
2404.392072	145369.750849	58.903770
2403.663396	145154.364019	58.908775
2402.800433	144930.371305	58.913780
2402.099374	144712.060325	58.918785
2401.377244	144503.094376	58.923789
2400.827486	144279.552272	58.928794
2400.046648	144066.061940	58.933799
2399.066025	143850.978196	58.938804
2398.800560	143623.990137	58.943809
2397.829032	143412.084833	58.948813
2397.345265	143200.268843	58.953818
2396.684754	142987.084547	58.958823
2396.380264	142777.199928	58.963828
2395.717999	142545.352385	58.968833
2394.901681	142334.230417	58.973837
2394.208932	142109.684711	58.978842
2393.595325	141892.599605	58.983847
2392.713532	141677.184996	58.988852
2391.946019	141454.892304	58.993857
2391.011511	141236.553975	58.998861
2390.835185	141011.947172	59.003866
2390.202613	140808.570154	59.008871
2389.217063	140593.560853	59.013876
2388.928504	140368.989309	59.018881
2387.893610	140161.004619	59.023885
2387.504652	139946.146748	59.028890
2387.031524	139730.211060	59.033895
2385.980846	139509.781754	59.038900
2385.499269	139286.582968	59.043905
2384.847059	139075.368725	59.048909
2384.214332	138854.090237	59.053914
2383.386624	138649.068929	59.058919
2382.963251	138431.178099	59.063924
2382.292453	138196.709841	59.068929
2381.358156	137984.455407	59.073933
2380.985382	137764.566752	59.078938
2380.081825	137554.686334	59.083943
2379.361585	137339.328017	59.088948
2378.863516	137122.347966	59.093953
2378.153141	136906.483056	59.098957
2377.708469	136691.416093	59.103962
2376.953455	136483.603269	59.108967
2376.132459	136261.599024	59.113972
2375.862425	136037.260468	59.118977
2374.917264	135829.634877	59.123981
2374.182908	135608.117308	59.128986
2373.796008	135390.230452	59.133991
2372.844397	135166.057467	59.138996
2372.133520	134944.744479	59.144001
2371.337510	134736.378921	59.149005
2370.822630	134512.942057	59.154010
2370.223986	134304.141802	59.159015
2369.425746	134087.257292	59.164020
2369.050439	133863.130043	59.169025
2368.288256	133658.120538	59.174029
2367.776118	133439.963333	59.179034
2366.712607	133225.464728	59.184039
2366.193056	133002.243560	59.189044
2365.465005	132783.185574	59.194049
2364.723828	132570.851038	59.199053
2364.308148	132347.707426	59.204058
2363.848204	132146.471576	59.209063
2363.169896	131932.988602	59.214068
2362.457840	131704.155565	59.219073
2361.406114	131490.697017	59.224077
2360.820134	131270.319824	59.229082
2360.573557	131052.545240	59.234087
2359.658195	130839.489147	59.239092
2358.486747	130625.573445	59.244097
2357.724569	130416.281389	59.249101
2357.390600	130195.453478	59.254106
2357.050246	129998.100631	59.259111
2356.137972	129784.175643	59.264116
2355.752970	129561.023764	59.269121
2354.906270	129350.622650	59.274125
2354.425386	129127.870468	59.279130
2353.736975	128920.381449	59.284135
2352.814984	128706.796485	59.289140
2352.257220	128476.987308	59.294145
2351.667770	128270.732124	59.299149
2351.013414	128048.676532	59.304154
2350.482204	127836.979494	59.309159
2349.916751	127628.248699	59.314164
2349.427542	127403.098614	59.319169
2348.676995	127183.186184	59.324173
2347.649875	126965.262480	59.329178
2347.052674	126746.332538	59.334183
2346.520029	126531.826367	59.339188
2346.109181	126316.540576	59.344193
2345.355812	126097.805679	59.349197
2344.640693	125877.567917	59.354202
2344.266235	125658.585965	59.359207
2343.175030	125439.363843	59.364212
2342.737613	125217.322175	59.369217
2341.890271	124997.391892	59.374221
2341.313169	124773.775909	59.379226
2340.732753	124550.797248	59.384231
2340.072496	124339.046182	59.389236
2339.616932	124106.895510	59.394241
2338.734942	123887.449610	59.399245
2337.937601	123655.776080	59.404250
2337.224035	123443.926221	59.409255
2336.469123	123227.627476	59.414260
2336.159706	122998.574301	59.419265
2335.412780	122786.493667	59.424269
2334.759692	122573.968106	59.429274
2333.948967	122350.079197	59.434279
2332.988097	122130.444353	59.439284
2332.397138	121910.346341	59.444289
2331.841905	121691.933269	59.449293
2330.978272	121477.380152	59.454298
2330.741153	121266.741806	59.459303
2329.962512	121048.217103	59.464308
2329.376911	120826.298843	59.469313
2328.558892	120603.492419	59.474317
2327.621626	120391.435739	59.479322
2327.509522	120179.516557	59.484327
2326.533587	119964.612658	59.489332
2326.201420	119733.090073	59.494337
2325.242760	119527.773004	59.499341
2324.759912	119300.702893	59.504346
2324.301340	119087.647675	59.509351
2323.286860	118865.350612	59.514356
2322.964192	118635.131277	59.519361
2322.256103	118413.887703	59.524365
2321.501667	118184.496244	59.529370
2320.725076	117969.869197	59.534375
2320.135213	117758.254940	59.539380
2319.664859	117535.495777	59.544385
2318.985458	117311.578313	59.549389
2318.302812	117087.568094	59.554394
2317.834266	116873.371050	59.559399
2316.781986	116653.263550	59.564404
2316.207820	116433.577228	59.569409
2315.510598	116209.107271	59.574413
2314.708278	115980.238152	59.579418
2314.125425	115760.565335	59.584423
2313.189998	115541.527926	59.589428
2312.943108	115321.951600	59.594433
2312.031728	115107.877657	59.599437
2311.823853	114889.384250	59.604442
2311.373262	114665.586969	59.609447
2310.165277	114444.495014	59.614452
2309.672580	114214.913559	59.619457
2309.047881	113990.350145	59.624461
2308.286920	113758.454333	59.629466
2307.795015	113537.091754	59.634471
2307.024968	113317.723681	59.639476
2306.776332	113087.656831	59.644481
2305.950315	112873.480414	59.649485
2305.084693	112649.728780	59.654490
2304.386662	112416.572420	59.659495
2303.441979	112199.780443	59.664500
2303.174384	111974.632649	59.669505
2302.380321	111750.953884	59.674509
2302.008292	111527.940025	59.679514
2301.363483	111306.335867	59.684519
2300.581111	111084.400119	59.689524
2299.914659	110849.209977	59.694529
2298.993383	110625.225196	59.699533
2298.561592	110403.132082	59.704538
2298.086199	110176.891289	59.709543
2297.086675	109953.629418	59.714548
2296.606028	109721.568122	59.719553
2295.842646	109491.603538	59.724557
2295.266219	109265.501381	59.729562
2294.463326	109037.114718	59.734567
2293.699370	108821.834004	59.739572
2293.482692	108598.580895	59.744577
2292.746968	108370.627654	59.749581
2291.718292	108142.088465	59.754586
2291.208481	107918.526387	59.759591
2290.453484	107696.604265	59.764596
2289.755994	107471.559541	59.769601
2288.935168	107250.349922	59.774605
2288.279485	107032.187177	59.779610
2287.498228	106813.100901	59.784615
2287.109405	106594.316044	59.789620
2286.511488	106368.256950	59.794625
2285.727951	106148.885208	59.799629
2284.876265	105926.214274	59.804634
2284.390481	105702.034424	59.809639
2283.742519	105482.247555	59.814644
2283.111307	105259.027587	59.819649
2282.235373	105054.323993	59.824653
2281.524291	104829.274429	59.829658
2281.527005	104602.749723	59.834663
2280.465445	104379.695057	59.839668
2280.046723	104157.993394	59.844673
2279.165680	103935.371066	59.849677
2278.385585	103713.375588	59.854682
2278.254783	103490.454471	59.859687
2277.265955	103269.447889	59.864692
2276.716586	103043.260362	59.869697
2275.864835	102820.802483	59.874701
2275.125212	102595.816720	59.879706
2274.881459	102371.674328	59.884711
2274.003350	102151.567852	59.889716
2273.424062	101909.942412	59.894721
2272.867634	101695.111618	59.899725
2272.081930	101481.689385	59.904730
2271.436179	101256.168722	59.909735
2270.561132	101027.705148	59.914740
2270.146346	100806.376987	59.919745
2269.131191	100584.010679	59.924750
2268.728512	100361.898244	59.929754
2268.510680	100136.745558	59.934759
2267.355501	99910.329185	59.939764
2267.053943	99673.529107	59.944769
2266.454337	99448.963794	59.949774
2265.622583	99222.033476	59.954778
2265.093348	98985.498566	59.959783
2264.324093	98758.524842	59.964788
2263.896177	98520.158230	59.969793
2263.047609	98304.320560	59.974798
2262.222638	98068.406496	59.979802
2261.779997	97830.429947	59.984807
2260.913268	97608.918701	59.989812
2260.339127	97367.136910	59.994817
2259.744142	97145.035266	59.999822
2258.989767	96918.140849	60.004826
2258.087442	96696.701192	60.009831
2257.493299	96466.449803	60.014836
2257.269779	96233.046973	60.019841
2256.051969	96004.573529	60.024846
2255.529222	95774.584212	60.029850
2255.442850	95538.319198	60.034855
2254.230304	95316.942230	60.039860
2253.552150	95079.907028	60.044865
2253.150698	94861.684637	60.049870
2252.420138	94626.355787	60.054874
2251.928302	94402.203632	60.059879
2251.146595	94172.943954	60.064884
2250.365463	93931.542459	60.069889
2249.590562	93713.295343	60.074894
2248.882758	93484.259293	60.079898
2248.347891	93252.642596	60.084903
2247.642493	93030.002918	60.089908
2247.197084	92796.956318	60.094913
2246.338990	92571.320683	60.099918
2245.777894	92341.867279	60.104922
2245.506237	92113.778049	60.109927
2244.549345	91879.319385	60.114932
2244.032355	91645.719203	60.119937
2243.242224	91425.556656	60.124942
2242.386198	91184.304676	60.129946
2242.127991	90958.412800	60.134951
2241.575622	90728.308991	60.139956
2240.656648	90484.703266	60.144961
2239.788416	90258.845588	60.149966
2238.903741	90026.582668	60.154970
2238.566103	89795.110415	60.159975
2237.883181	89573.611606	60.164980
2237.009437	89337.968545	60.169985
2236.297475	89119.756849	60.174990
2235.797728	88882.658210	60.179994
2234.999387	88651.220445	60.184999
2234.319378	88424.717889	60.190004
2233.597114	88195.200266	60.195009
2232.960828	87970.762322	60.200014
2232.314258	87743.114073	60.205018
2231.902585	87514.207399	60.210023
2230.924663	87299.270430	60.215028
2230.383272	87063.909998	60.220033
2229.732836	86844.025137	60.225038
2228.919289	86606.253149	60.230042
2228.658279	86378.412345	60.235047
2227.550928	86152.863565	60.240052
2227.147696	85932.505073	60.245057
2226.353102	85710.531045	60.250062
2225.851210	85475.511397	60.255066
2225.119606	85248.334117	60.260071
2224.238776	85028.605855	60.265076
2223.888711	84789.740941	60.270081
2223.249301	84578.276647	60.275086
2222.451490	84349.319231	60.280090
2222.093407	84117.600588	60.285095
2221.386286	83892.215082	60.290100
2220.716715	83657.559045	60.295105
2220.019734	83428.728690	60.300110
2219.283706	83197.042042	60.305114
2218.659892	82961.993489	60.310119
2218.154120	82744.194311	60.315124
2217.652090	82499.427692	60.320129
2216.889047	82273.618330	60.325134
2215.767509	82045.320358	60.330138
2215.210309	81812.745935	60.335143
2214.754246	81585.437549	60.340148
2214.197610	81351.391422	60.345153
2213.384788	81133.385146	60.350158
2212.696606	80897.565037	60.355162
2212.092794	80656.081026	60.360167
2211.450007	80434.189124	60.365172
2210.918065	80193.453253	60.370177
2210.140121	79962.734323	60.375182
2209.368455	79731.909229	60.380186
2209.049710	79497.054048	60.385191
2208.041780	79272.152570	60.390196
2207.456203	79045.057258	60.395201
2206.762681	78817.392217	60.400206
2206.091896	78580.968324	60.405210
2205.455863	78345.143642	60.410215
2204.607806	78122.371235	60.415220
2204.153682	77879.679211	60.420225
2203.428083	77663.691743	60.425230
2202.607597	77434.249854	60.430234
2202.374960	77195.503882	60.435239
2201.188280	76977.188896	60.440244
2200.630163	76750.520138	60.445249
2199.745442	76520.718509	60.450254
2199.521047	76290.795714	60.455258
2198.642220	76062.728130	60.460263
2197.706790	75840.254249	60.465268
2197.223343	75607.592359	60.470273
2196.393361	75391.987666	60.475278
2195.591101	75164.456596	60.480282
2195.357642	74935.133501	60.485287
2194.696641	74715.948438	60.490292
2194.072698	74490.107343	60.495297
2193.057297	74264.216833	60.500302
2192.542433	74035.974974	60.505306
2192.397701	73817.547747	60.510311
2191.360117	73585.833349	60.515316
2190.739073	73368.158127	60.520321
2190.226164	73131.962642	60.525326
2189.089276	72914.823985	60.530330
2188.831702	72678.225904	60.535335
2188.005870	72456.437211	60.540340
2187.432901	72238.608275	60.545345
2186.664626	72007.921052	60.550350
2186.282102	71782.775349	60.555354
2185.706515	71547.007659	60.560359
2184.916297	71328.919073	60.565364
2184.099654	71095.760554	60.570369
2183.509958	70867.611115	60.575374
2183.046714	70640.153711	60.580378
2182.288428	70404.403256	60.585383
2181.317155	70191.993578	60.590388
2180.906909	69957.529801	60.595393
2180.396903	69729.545554	60.600398
2179.438135	69498.841775	60.605402
2178.808988	69264.750351	60.610407
2178.079480	69045.568894	60.615412
2177.492217	68825.689589	60.620417
2176.866950	68589.496403	60.625422
2176.428316	68368.015190	60.630426
2175.949943	68131.595212	60.635431
2175.125351	67914.974986	60.640436
2174.299769	67673.561388	60.645441
2173.701846	67449.202428	60.650446
2173.045753	67222.176244	60.655450
2172.532090	66979.132086	60.660455
2171.470159	66765.817642	60.665460
2171.069857	66532.640998	60.670465
2170.376318	66299.754339	60.675470
2169.260144	66073.470067	60.680474
2168.443316	65852.055342	60.685479
2167.786456	65630.627277	60.690484
2167.606660	65402.796408	60.695489
2166.682117	65187.422587	60.700494
2166.064097	64962.899315	60.705498
2165.807393	64741.386326	60.710503
2164.898553	64524.161989	60.715508
2164.130869	64293.467567	60.720513
2163.879366	64064.083990	60.725518
2162.883341	63839.339379	60.730522
2162.271565	63613.532792	60.735527
2161.658984	63390.831760	60.740532
2161.179781	63153.282421	60.745537
2160.382437	62929.998705	60.750542
2159.678088	62700.453235	60.755546
2159.490396	62469.590691	60.760551
2158.307234	62243.536408	60.765556
2157.742126	62015.319464	60.770561
2157.199322	61782.745569	60.775566
2156.223588	61556.783706	60.780570
2155.937762	61333.108387	60.785575
2154.920556	61120.533568	60.790580
2154.283030	60888.109169	60.795585
2153.659790	60656.587572	60.800590
2152.634776	60433.334598	60.805594
2152.304385	60203.313755	60.810599
2151.643792	59985.829724	60.815604
2151.051244	59766.688204	60.820609
2150.406228	59529.372137	60.825614
2149.524463	59309.525310	60.830618
2148.919995	59082.166823	60.835623
2148.118226	58875.125790	60.840628
2147.838822	58651.155351	60.845633
2147.111779	58422.320835	60.850638
2146.119277	58196.864210	60.855642
2145.868661	57968.731990	60.860647
2144.848357	57745.345776	60.865652
2144.589165	57524.579301	60.870657
2143.962248	57296.220688	60.875662
2143.009644	57063.577324	60.880666
2142.491543	56844.417214	60.885671
2141.641953	56624.131772	60.890676
2140.988336	56404.950900	60.895681
2140.490982	56170.651436	60.900686
2139.552654	55952.739582	60.905690
2138.895620	55723.104448	60.910695
2138.302586	55506.070381	60.915700
2137.863861	55280.004463	60.920705
2136.982882	55055.372305	60.925710
2136.179540	54833.325580	60.930714
2135.688221	54613.713083	60.935719
2135.257938	54389.900499	60.940724
2134.564790	54166.195652	60.945729
2133.865747	53945.168464	60.950734
2133.098846	53727.420424	60.955738
2132.655120	53487.684914	60.960743
2131.915965	53276.117941	60.965748
2131.372398	53029.901536	60.970753
2130.613809	52817.744925	60.975758
2129.741634	52589.259164	60.980762
2129.096630	52360.904779	60.985767
2128.300003	52146.306640	60.990772
2127.888782	51930.602571	60.995777
2127.194305	51696.467738	61.000782
2126.142111	51484.740372	61.005786
2125.977456	51247.287315	61.010791
2125.037829	51031.541778	61.015796
2124.458831	50812.777004	61.020801
2123.902094	50592.840718	61.025806
2123.207455	50367.132823	61.030810
2122.561632	50141.964199	61.035815
2121.851042	49929.795977	61.040820
2120.951285	49706.280318	61.045825
2120.201652	49480.044998	61.050830
2119.475507	49269.560672	61.055834
2119.230220	49047.262330	61.060839
2118.565364	48824.052619	61.065844
2117.911662	48608.990056	61.070849
2117.095029	48382.896334	61.075854
2116.499859	48156.156637	61.080858
2115.812028	47934.609894	61.085863
2114.739030	47723.275169	61.090868
2114.408991	47498.586474	61.095873
2114.070262	47281.433838	61.100878
2112.921570	47055.868400	61.105882
2112.479768	46842.163328	61.110887
2111.416449	46624.352419	61.115892
2110.792429	46411.333093	61.120897
2110.398237	46193.734483	61.125902
2109.681495	45975.370506	61.130906
2109.054806	45754.518295	61.135911
2108.106543	45539.568260	61.140916
2107.477481	45322.327674	61.145921
2107.114085	45109.415611	61.150926
2106.085772	44898.733931	61.155930
2105.713475	44677.412115	61.160935
2104.937803	44465.765688	61.165940
2104.517395	44248.495830	61.170945
2103.707835	44031.878692	61.175950
2103.070525	43824.048147	61.180954
2102.609679	43587.946513	61.185959
2101.916816	43383.558344	61.190964
2101.055127	43160.834353	61.195969
2100.936401	42940.266018	61.200974
2099.797732	42727.268863	61.205978
2099.023378	42511.190058	61.210983
2098.597119	42288.433476	61.215988
2098.393820	42064.581828	61.220993
2097.205460	41853.687308	61.225998
2096.515421	41631.932901	61.231002
2096.021114	41412.158310	61.236007
2094.872713	41194.583692	61.241012
2094.402521	40983.345535	61.246017
2093.584827	40771.662335	61.251022
2092.860322	40559.609639	61.256026
2092.283051	40338.521203	61.261031
2091.624529	40131.649082	61.266036
2090.724709	39918.013190	61.271041
2090.573723	39703.802658	61.276046
2089.466098	39495.877513	61.281050
2089.202855	39275.274685	61.286055
2088.676182	39063.292917	61.291060
2087.878333	38852.902920	61.296065
2087.091012	38637.834487	61.301070
2086.640918	38428.121752	61.306074
2085.909451	38210.422491	61.311079
2084.949666	37993.220682	61.316084
2084.196073	37773.393284	61.321089
2083.836158	37565.994313	61.326094
2082.910347	37362.429307	61.331098
2082.282495	37139.218448	61.336103
2081.483615	36930.464781	61.341108
2080.983225	36725.659143	61.346113
2080.673297	36508.249970	61.351118
2079.811138	36304.028475	61.356122
2079.390892	36097.956381	61.361127
2078.367902	35879.615770	61.366132
2077.872090	35659.139574	61.371137
2077.176537	35449.697135	61.376142
2076.465538	35248.020253	61.381146
2075.686449	35033.127570	61.386151
2074.839107	34827.793167	61.391156
2074.187275	34609.707317	61.396161
2073.771666	34395.397333	61.401166
2073.001925	34199.534820	61.406170
2072.746899	33992.221722	61.411175
2071.749152	33788.920033	61.416180
2071.125782	33563.407494	61.421185
2070.381275	33351.870311	61.426190
2069.655836	33139.605829	61.431194
2069.479145	32928.127738	61.436199
2068.598882	32723.319114	61.441204
2067.759100	32505.368063	61.446209
2067.044062	32296.145290	61.451214
2066.136432	32096.541519	61.456218
2065.803059	31887.833808	61.461223
2064.944503	31683.344324	61.466228
2064.382541	31474.352585	61.471233
2063.757793	31264.765088	61.476238
2062.975337	31063.878733	61.481242
2062.622586	30838.875457	61.486247
2061.671877	30638.278555	61.491252
2060.992202	30442.487229	61.496257
2060.267593	30229.694308	61.501262
2059.279307	30027.249506	61.506266
2058.795321	29826.545789	61.511271
2057.799561	29627.311419	61.516276
2057.665774	29416.569885	61.521281
2057.259635	29219.934468	61.526286
2056.185789	29022.035978	61.531290
2055.879379	28803.191394	61.536295
2054.958234	28601.060090	61.541300
2054.631349	28401.358498	61.546305
2054.070664	28197.403933	61.551310
2053.077208	27990.992834	61.556314
2052.409417	27781.663693	61.561319
2051.732009	27576.901279	61.566324
2050.939528	27370.071220	61.571329
2050.261949	27165.582587	61.576334
2049.402861	26979.610065	61.581338
2048.889603	26769.531711	61.586343
2048.242870	26579.637612	61.591348
2047.538739	26372.239156	61.596353
2047.101268	26168.090721	61.601358
2046.240453	25964.753702	61.606362
2045.977556	25761.363847	61.611367
2044.815426	25559.768389	61.616372
2044.208595	25360.129750	61.621377
2043.833855	25157.299176	61.626382
2042.789918	24967.461040	61.631386
2042.451820	24761.671129	61.636391
2041.704157	24566.490570	61.641396
2040.921536	24361.727997	61.646401
2040.519073	24158.382942	61.651406
2039.593445	23960.119332	61.656410
2038.598794	23758.848453	61.661415
2038.086169	23574.172828	61.666420
2037.551332	23373.110234	61.671425
2036.966634	23173.158126	61.676430
2035.890103	22983.385824	61.681434
2035.370279	22781.488875	61.686439
2034.791181	22593.088168	61.691444
2033.997241	22401.175088	61.696449
2033.595528	22206.749444	61.701454
2032.756735	22017.753214	61.706458
2032.431722	21799.075479	61.711463
2031.204373	21623.327594	61.716468
2030.161686	21433.653719	61.721473
2029.686582	21237.855579	61.726478
2028.966413	21055.576989	61.731482
2028.859172	20863.508797	61.736487
2027.996072	20673.867649	61.741492
2027.036910	20490.294408	61.746497
2026.436283	20309.566414	61.751502
2025.862611	20123.654466	61.756506
2025.375165	19940.336084	61.761511
2024.496945	19763.636068	61.766516
2023.859655	19563.421686	61.771521
2023.542088	19385.430173	61.776526
2022.784086	19205.494607	61.781530
2021.944734	19014.345579	61.786535
2021.103243	18821.443432	61.791540
2020.407066	18624.167886	61.796545
2020.104793	18445.539229	61.801550
2019.251756	18268.276954	61.806554
2018.447223	18070.073129	61.811559
2017.838333	17893.808543	61.816564
2016.864623	17715.525708	61.821569
2016.175181	17537.483981	61.826574
2015.583675	17353.039736	61.831578
2015.197011	17176.585374	61.836583
2014.760703	17001.549544	61.841588
2013.686794	16828.146687	61.846593
2013.127425	16633.807723	61.851598
2011.733995	16449.834585	61.856602
2011.468378	16264.493900	61.861607
2010.753012	16085.132424	61.866612
2010.039368	15910.046757	61.871617
2009.494457	15737.612473	61.876622
2008.371443	15569.890508	61.881626
2007.799005	15405.403765	61.886631
2006.986373	15243.366015	61.891636
2006.395992	15067.302067	61.896641
2005.417850	14914.023032	61.901646
2004.611569	14763.025571	61.906650
2004.039255	14597.757067	61.911655
2002.726344	14452.047745	61.916660
2001.616277	14302.955294	61.921665
2001.218732	14151.826051	61.926670
1999.932471	14018.940527	61.931674
1999.323632	13878.406621	61.936679
1998.752995	13739.404863	61.941684
1997.855395	13616.149652	61.946689
1996.935250	13487.042042	61.951694
1996.051707	13362.521353	61.956698
1995.536732	13239.265365	61.961703
1994.889581	13124.295581	61.966708
1993.881541	13007.704869	61.971713
1993.393084	12891.185158	61.976718
1992.825121	12786.322631	61.981722
1991.910372	12669.734193	61.986727
1990.730280	12558.104110	61.991732
1990.279573	12441.313157	61.996737
1989.883449	12331.243847	62.001742
1988.860927	12236.658800	62.006746
1988.705913	12118.336648	62.011751
1987.921350	12014.025268	62.016756
1987.079255	11911.221881	62.021761
1986.446007	11791.515344	62.026766
1985.686036	11694.362091	62.031770
1984.820847	11585.303185	62.036775
1984.331718	11487.994038	62.041780
1984.072748	11390.253645	62.046785
1983.437450	11280.557371	62.051790
1982.442648	11182.194161	62.056794
1982.114455	11078.668577	62.061799
1981.294964	10977.318644	62.066804
1980.467043	10870.617299	62.071809
1979.970280	10763.017478	62.076814
1979.313454	10665.963920	62.081818
1978.569830	10557.239309	62.086823
1978.059986	10460.092725	62.091828
1977.686682	10352.405999	62.096833
1977.167647	10247.306744	62.101838
1976.222160	10147.457073	62.106842
1975.570257	10034.222025	62.111847
1975.029326	9938.552888	62.116852
1974.202582	9831.383699	62.121857
1973.844809	9725.194549	62.126862
1972.848680	9622.082013	62.131866
1972.223735	9521.176077	62.136871
1971.686808	9416.337136	62.141876
1971.205730	9306.288276	62.146881
1970.429258	9209.272145	62.151886
1969.778522	9099.943659	62.156890
1969.289731	8995.965902	62.161895
1968.556788	8895.538115	62.166900
1967.636523	8806.964469	62.171905
1967.284526	8694.557960	62.176910
1966.315584	8592.222524	62.181914
1965.883757	8482.609737	62.186919
1965.035057	8381.293323	62.191924
1964.359123	8277.052423	62.196929
1964.006835	8183.858700	62.201934
1962.888428	8086.078884	62.206938
1962.380604	7973.471354	62.211943
1961.636130	7876.823232	62.216948
1960.912261	7780.846188	62.221953
1960.789174	7674.244152	62.226958
1960.093901	7596.841564	62.231962
1959.443125	7486.409340	62.236967
1958.429025	7387.569886	62.241972
1957.926497	7281.972804	62.246977
1957.350631	7176.216135	62.251982
1956.369643	7079.747973	62.256986
1956.078212	6975.654684	62.261991
1955.495450	6875.984949	62.266996
1954.779836	6773.181954	62.272001
1954.216443	6665.430338	62.277006
1953.063331	6569.730371	62.282010
1952.820469	6472.080877	62.287015
1952.022491	6377.819826	62.292020
1951.216901	6273.843029	62.297025
1950.921740	6167.297203	62.302030
1949.727613	6074.398570	62.307034
1949.526369	5968.090893	62.312039
1948.461299	5867.210824	62.317044
1947.878704	5777.345371	62.322049
1947.372362	5674.471388	62.327054
1946.816634	5574.538674	62.332058
1946.012062	5477.199429	62.337063
1945.535062	5383.014418	62.342068
1944.800403	5284.777961	62.347073
1944.284951	5178.222925	62.352078
1943.225856	5087.111376	62.357082
1942.599388	4984.996370	62.362087
1941.789524	4892.592330	62.367092
1940.973353	4804.125720	62.372097
1940.704234	4704.421548	62.377102
1939.845647	4616.472322	62.382106
1939.539453	4513.564369	62.387111
1938.600414	4420.008576	62.392116
1938.047719	4329.919213	62.397121
1937.723356	4223.917269	62.402126
1936.587667	4134.551832	62.407130
1935.907093	4045.086295	62.412135
1935.098863	3954.647801	62.417140
1934.430537	3854.761138	62.422145
1933.611607	3761.798539	62.427150
1933.091213	3675.307638	62.432154
1932.555499	3583.905392	62.437159
1931.390050	3502.197167	62.442164
1930.751451	3421.055626	62.447169
1930.610595	3317.692837	62.452174
1929.531760	3239.161701	62.457178
1928.670110	3161.596528	62.462183
1928.166119	3075.910978	62.467188
1927.268324	2993.746681	62.472193
1926.664389	2916.369022	62.477198
1925.808981	2848.126327	62.482202
1925.337112	2772.542340	62.487207
1924.295391	2700.345705	62.492212
1923.469945	2630.480198	62.497217
1923.090687	2541.467289	62.502222
1921.699751	2482.782727	62.507226
1921.345288	2421.209172	62.512231
1920.642263	2359.636797	62.517236
1919.723935	2289.287680	62.522241
1919.182274	2237.609385	62.527246
1918.189780	2181.525129	62.532250
1917.545978	2109.619957	62.537255
1916.637980	2061.150127	62.542260
1915.692424	2006.473844	62.547265
1915.285023	1948.263802	62.552270
1914.560963	1904.861982	62.557274
1913.825031	1856.956171	62.562279
1913.405858	1813.466790	62.567284
1912.751000	1754.598906	62.572289
1912.204736	1703.689734	62.577294
1911.283113	1660.296350	62.582298
1910.502302	1604.795010	62.587303
1910.220578	1555.550836	62.592308
1909.163796	1524.480285	62.597313
1909.063051	1454.759267	62.602318
1908.160592	1414.234752	62.607322
1907.785222	1359.400191	62.612327
1906.703032	1308.111444	62.617332
1906.044638	1261.526371	62.622337
1905.526992	1212.918536	62.627342
1904.543077	1175.236169	62.632346
1904.068131	1128.807707	62.637351
1903.519651	1079.437165	62.642356
1902.474276	1038.659608	62.647361
1901.876428	985.359225	62.652366
1901.393508	951.651800	62.657370
1900.832086	903.159192	62.662375
1900.032042	865.644784	62.667380
1899.487680	821.308484	62.672385
1898.629230	763.566683	62.677390
1897.622227	734.071719	62.682394
1897.011389	690.487590	62.687399
1896.668001	657.859479	62.692404
1895.915368	624.783874	62.697409
1895.537677	568.523068	62.702414
1894.726312	537.585992	62.707418
1894.007572	493.166410	62.712423
1893.063167	460.109012	62.717428
1892.624782	423.960810	62.722433
1892.265996	376.562208	62.727438
1891.263455	349.125334	62.732442
1890.903907	303.512275	62.737447
1890.038938	276.977826	62.742452
1889.225378	238.793806	62.747457
1888.549855	198.922657	62.752462
1887.669611	168.685669	62.757466
1887.162624	121.533787	62.762471
1886.382420	97.195578	62.767476
1885.277540	68.048685	62.772481
1885.214684	48.430131	62.777486
1883.871500	22.957693	62.782490
1883.320533	-11.271285	62.787495
1882.105801	-31.397563	62.792500
1881.397684	-48.697885	62.797505
1880.554866	-57.469031	62.802510
1879.744363	-52.088815	62.807514
1879.163504	-57.872186	62.812519
1878.468441	-64.312365	62.817524
1877.283825	-72.523024	62.822529
1876.189189	-53.354383	62.827534
1874.547803	-16.124527	62.832538
1873.963534	-0.465198	62.837543
1873.304903	14.780170	62.842548
1873.208969	22.798791	62.847553
1873.060847	29.291298	62.852558
1873.007560	24.550097	62.857562
1872.736563	20.409601	62.862567
1872.649758	21.469131	62.867572
1872.020237	10.737009	62.872577
1871.086374	5.042781	62.877582
1868.779960	35.971093	62.882586
1868.048774	30.607381	62.887591
1867.869569	47.342606	62.892596
1866.700744	43.451893	62.897601
1866.816423	41.981332	62.902606
1866.235132	42.554816	62.907610
1866.004843	41.728980	62.912615
1865.842099	41.024885	62.917620
1865.187582	41.345063	62.922625
1864.620245	31.407317	62.927630
1863.339205	43.266409	62.932634
1862.266387	34.533310	62.937639
1861.416353	41.236621	62.942644
1860.770533	48.402684	62.947649
1860.563700	47.036948	62.952654
1859.827656	50.345842	62.957658
1859.773562	52.458337	62.962663
1859.266069	51.837367	62.967668
1858.366172	44.781528	62.972673
1857.673081	46.749473	62.977678
1856.339005	49.724384	62.982682
1855.705442	48.973619	62.987687
1855.246308	56.939538	62.992692
1854.781750	58.756078	62.997697
1854.333136	48.913015	63.002702
1853.457749	56.620169	63.007706
1852.645992	59.130518	63.012711
1851.778756	63.247163	63.017716
1851.490164	65.836873	63.022721
1851.161830	54.927590	63.027726
1850.644891	57.419513	63.032730
1849.714405	57.438154	63.037735
1849.176025	51.819895	63.042740
1848.208840	61.855065	63.047745
1847.435821	54.441605	63.052750
1846.841149	67.910652	63.057754
1846.497377	69.165533	63.062759
1845.758477	66.291525	63.067764
1844.722660	67.284124	63.072769
1844.210218	59.248956	63.077774
1843.448720	78.137792	63.082778
1843.517234	71.268806	63.087783
1843.107297	65.969200	63.092788
1841.699181	69.515708	63.097793
1841.357633	66.794654	63.102798
1840.536634	75.291139	63.107802
1839.915804	65.970588	63.112807
1839.635387	73.075491	63.117812
1838.579280	72.394977	63.122817
1837.869798	69.983088	63.127822
1836.952572	68.774310	63.132826
1836.255130	65.622481	63.137831
1835.550173	67.615973	63.142836
1834.797007	68.951632	63.147841
1834.498614	70.826949	63.152846
1834.301217	71.460911	63.157850
1833.639135	72.842034	63.162855
1833.495308	67.891266	63.167860
1831.893196	76.942304	63.172865
1830.823465	65.759652	63.177870
1830.174797	74.323394	63.182874
1829.973252	69.384945	63.187879
1829.620028	72.528982	63.192884
1828.706056	77.086729	63.197889
1828.214618	67.294617	63.202894
1827.456246	69.082123	63.207898
1826.797940	77.281537	63.212903
1825.797231	75.253370	63.217908
1825.256913	78.327767	63.222913
1824.418193	69.467605	63.227918
1823.996217	70.622941	63.232922
1823.719393	69.206818	63.237927
1823.286447	68.250735	63.242932
1822.157326	74.700338	63.247937
1821.174217	64.166271	63.252942
1820.500295	81.079437	63.257946
1820.497282	74.521436	63.262951
1820.108874	80.419750	63.267956
1818.860395	80.386394	63.272961
1817.986321	74.561238	63.277966
1817.491767	88.906982	63.282970
1817.210921	77.365662	63.287975
1816.519148	67.017150	63.292980
1815.023086	71.180045	63.297985
1814.876496	73.567434	63.302990
1814.529843	78.052445	63.307994
1814.015457	68.756000	63.312999
1813.084475	73.005787	63.318004
1811.860442	74.121329	63.323009
1811.866214	74.861804	63.328014
1811.105218	79.505655	63.333018
1810.705056	79.518945	63.338023
1809.792560	67.658461	63.343028
1808.274290	77.472075	63.348033
1808.326434	72.901782	63.353038
1808.168648	81.020141	63.358042
1807.569978	67.066049	63.363047
1806.408443	75.976172	63.368052
1805.172320	80.507813	63.373057
1804.779470	75.088802	63.378062
1804.315028	75.102839	63.383066
1804.089923	70.944011	63.388071
1803.288913	66.960220	63.393076
1801.710489	78.718351	63.398081
1802.130337	77.177405	63.403086
1801.925694	80.739407	63.408090
1800.811352	70.669319	63.413095
1799.687624	77.957031	63.418100
1798.636664	82.411962	63.423105
1798.298600	79.562624	63.428110
1797.380406	80.825151	63.433114
1797.552914	77.472101	63.438119
1797.013836	81.325338	63.443124
1795.561123	80.061259	63.448129
1795.220064	74.268164	63.453134
1794.366648	82.944858	63.458138
1793.712243	87.333663	63.463143
1793.203628	75.025835	63.468148
1792.223984	82.022583	63.473153
1792.033456	76.084155	63.478158
1791.375120	75.829358	63.483162
1790.831801	80.523803	63.488167
1790.316386	72.914902	63.493172
1789.373578	82.201892	63.498177
1788.913485	73.202765	63.503182
1788.453661	72.542699	63.508186
1787.732513	84.434364	63.513191
1786.851318	77.820279	63.518196
1785.424119	85.509439	63.523201
1785.136604	74.803414	63.528206
1784.986210	76.756160	63.533210
1783.939847	80.026049	63.538215
1782.990144	65.479573	63.543220
1782.730468	79.412686	63.548225
1782.957096	81.447488	63.553230
1782.112190	81.086701	63.558234
1781.115566	74.587148	63.563239
1780.087652	72.424546	63.568244
1779.348876	76.123414	63.573249
1778.954701	74.692816	63.578254
1777.717024	83.182951	63.583258
1776.736409	80.571281	63.588263
1776.688099	80.210148	63.593268
1776.263565	83.581564	63.598273
1775.614448	78.209563	63.603278
1775.199024	78.395597	63.608282
1773.869105	74.975215	63.613287
1773.155978	72.950284	63.618292
1772.658408	71.491953	63.623297
1772.566903	71.022559	63.628302
1771.831964	70.213796	63.633306
1771.080969	72.511089	63.638311
1770.556131	71.795117	63.643316
1769.524809	81.154518	63.648321
1769.232965	75.809361	63.653326
1768.595795	73.609939	63.658330
1767.423716	77.119000	63.663335
1766.656686	73.777964	63.668340
1765.661493	76.511442	63.673345
1765.836678	70.292584	63.678350
1765.036860	77.935729	63.683354
1764.140921	76.392430	63.688359
1763.527161	66.851580	63.693364
1762.830415	76.295042	63.698369
1762.336607	76.058278	63.703374
1761.564767	75.051946	63.708378
1760.957656	74.185037	63.713383
1760.825642	68.928043	63.718388
1760.007847	77.630623	63.723393
1759.681685	72.494350	63.728398
1758.358169	70.826568	63.733402
1757.334189	73.563043	63.738407
1756.804347	64.898290	63.743412
1756.004324	74.799709	63.748417
1755.478201	69.871818	63.753422
1755.222385	74.282480	63.758426
1754.708074	78.306836	63.763431
1754.019594	69.047520	63.768436
1753.345805	81.232870	63.773441
1752.920613	68.224246	63.778446
1752.294809	73.885871	63.783450
1750.681731	78.439555	63.788455
1750.233216	69.567915	63.793460
1749.078129	78.144291	63.798465
1749.595799	68.614565	63.803470
1748.481948	84.012741	63.808474
1747.744110	71.552098	63.813479
1747.274946	69.012180	63.818484
1746.564921	80.589839	63.823489
1746.023236	68.082277	63.828494
1745.617264	79.045506	63.833498
1744.737652	72.298724	63.838503
1743.659544	74.796214	63.843508
1742.522855	76.799951	63.848513
1742.712074	78.615181	63.853518
1741.833061	79.727998	63.858522
1740.999362	77.108779	63.863527
1740.404572	78.302614	63.868532
1739.591553	79.318217	63.873537
1739.155251	78.837354	63.878542
1738.739529	70.271174	63.883546
1738.619026	70.702115	63.888551
1737.835388	70.287457	63.893556
1736.892194	77.554402	63.898561
1736.012378	73.070629	63.903566
1735.501014	72.108092	63.908570
1734.231274	76.061617	63.913575
1734.044589	76.903624	63.918580
1733.393461	82.357962	63.923585
1732.940351	74.289739	63.928590
1732.318409	77.976371	63.933594
1730.999611	78.280661	63.938599
1730.328131	75.269821	63.943604
1729.854408	82.843836	63.948609
1729.559125	80.959137	63.953614
1728.741735	74.959430	63.958618
1727.900547	76.312253	63.963623
1727.722000	71.701332	63.968628
1727.196391	83.629758	63.973633
1726.555333	77.619391	63.978638
1725.569015	78.560019	63.983642
1724.752293	73.454358	63.988647
1724.198739	73.438408	63.993652
1723.624984	83.436367	63.998657
1723.130045	75.130358	64.003662
1722.216264	77.298976	64.008666
1721.001320	79.542237	64.013671
1720.529711	72.725929	64.018676
1719.815108	79.579674	64.023681
1719.501857	71.247963	64.028686
1718.743262	81.727875	64.033690
1717.726802	77.866643	64.038695
1717.563568	80.655657	64.043700
1716.407005	82.503287	64.048705
1716.138801	77.703174	64.053710
1715.684105	71.497629	64.058714
1715.214122	82.215558	64.063719
1715.137099	74.838248	64.068724
1713.636332	79.609086	64.073729
1712.742403	73.008096	64.078734
1712.121122	77.073103	64.083738
1711.520772	77.510874	64.088743
1711.099667	74.103872	64.093748
1710.497478	79.208234	64.098753
1710.015039	74.498923	64.103758
1708.598910	77.799186	64.108762
1707.794649	75.802943	64.113767
1706.941450	64.959710	64.118772
1707.053419	73.913595	64.123777
1706.618853	67.831014	64.128782
1705.802506	68.563298	64.133786
1705.029725	70.066115	64.138791
1704.897933	71.418232	64.143796
1703.877557	74.887452	64.148801
1702.791779	69.499679	64.153806
1702.057786	75.287310	64.158810
1701.146403	77.144888	64.163815
1700.946083	64.387576	64.168820
1700.450538	75.218373	64.173825
1700.151674	72.610412	64.178830
1699.689163	82.068722	64.183834
1698.930131	67.782167	64.188839
1697.897692	72.741977	64.193844
1696.835564	77.143522	64.198849
1696.381868	70.764354	64.203854
1696.135041	79.187018	64.208858
1695.195016	77.696478	64.213863
1694.014308	69.598760	64.218868
1693.025547	78.322204	64.223873
1693.254265	75.105305	64.228878
1692.437403	82.971953	64.233882
1691.777585	76.917268	64.238887
1691.215791	80.843517	64.243892
1690.669355	72.734937	64.248897
1690.528138	76.531300	64.253902
1689.373909	75.170984	64.258906
1687.940330	75.890929	64.263911
1687.595216	61.656910	64.268916
1686.805528	68.333344	64.273921
1686.558818	69.115501	64.278926
1685.993865	75.986481	64.283930
1685.368702	77.371237	64.288935
1685.142812	72.193818	64.293940
1684.140608	72.052019	64.298945
1682.724993	77.454333	64.303950
1682.286754	78.921363	64.308954
1681.575292	77.558528	64.313959
1681.531905	66.670249	64.318964
1680.691991	78.366321	64.323969
1680.524579	68.830292	64.328974
1679.441601	74.443124	64.333978
1678.396021	75.817391	64.338983
1678.179662	68.069554	64.343988
1677.175865	68.543035	64.348993
1676.824385	74.602653	64.353998
1676.369399	72.771716	64.359002
1674.876241	75.360396	64.364007
1674.531624	69.780785	64.369012
1673.611381	76.593085	64.374017
1673.305603	77.059767	64.379022
1672.871596	72.158265	64.384026
1672.329255	72.927460	64.389031
1672.012863	68.890387	64.394036
1670.485700	71.285770	64.399041
1669.655075	67.757747	64.404046
1669.312661	66.347332	64.409050
1668.704960	71.955632	64.414055
1668.300568	71.493367	64.419060
1667.687945	75.831401	64.424065
1667.171843	76.803014	64.429070
1666.022217	63.761263	64.434074
1664.760895	76.476776	64.439079
1664.954002	65.385348	64.444084
1664.074001	76.199949	64.449089
1663.539505	66.380032	64.454094
1663.430466	75.115126	64.459098
1662.155578	73.483825	64.464103
1661.088870	67.755569	64.469108
1660.647336	79.306358	64.474113
1660.165746	74.191639	64.479118
1659.804170	75.022008	64.484122
1659.162437	75.483712	64.489127
1658.229785	74.419379	64.494132
1657.366127	78.626980	64.499137
1656.783665	76.639676	64.504142
1656.434823	71.290978	64.509146
1655.345123	83.619685	64.514151
1655.246973	72.123504	64.519156
1654.006608	81.926163	64.524161
1653.112023	73.141178	64.529166
1652.382141	76.826049	64.534170
1651.768422	76.065873	64.539175
1651.455568	69.858312	64.544180
1650.840110	70.490890	64.549185
1650.776133	73.347716	64.554190
1650.293238	75.250784	64.559194
1648.983139	81.606198	64.564199
1647.965079	74.681171	64.569204
1647.360519	75.042354	64.574209
1647.050724	70.452293	64.579214
1646.793604	70.890747	64.584218
1645.714388	77.427107	64.589223
1644.722779	72.254640	64.594228
1643.641183	74.309591	64.599233
1642.820870	73.482888	64.604238
1643.216725	77.654411	64.609242
1642.375079	76.093068	64.614247
1642.332338	71.731824	64.619252
1641.523877	74.792079	64.624257
1640.748642	66.814483	64.629262
1639.684170	71.664282	64.634266
1638.837569	73.276618	64.639271
1638.412965	69.258318	64.644276
1637.808269	76.749065	64.649281
1637.078723	68.191767	64.654286
1636.181287	63.264549	64.659290
1635.203378	77.354333	64.664295
1635.034831	64.632989	64.669300
1634.368307	77.250867	64.674305
1634.079078	72.107173	64.679310
1633.799984	71.569813	64.684314
1632.314411	73.316779	64.689319
1631.666927	65.836142	64.694324
1630.697958	63.309419	64.699329
1630.445701	74.513162	64.704334
1629.909989	69.222544	64.709338
1629.484409	71.714186	64.714343
1628.918955	64.088052	64.719348
1627.645494	80.095095	64.724353
1626.931858	69.340111	64.729358
1626.556211	71.659814	64.734362
1625.684719	81.164179	64.739367
1625.657516	74.474415	64.744372
1624.035436	75.482967	64.749377
1623.556350	68.631603	64.754382
1623.058040	72.200841	64.759386
1622.446450	75.266095	64.764391
1622.237219	74.938415	64.769396
1621.603994	77.732712	64.774401
1620.792950	71.785657	64.779406
1619.859141	63.497366	64.784410
1619.025351	77.059623	64.789415
1618.588057	69.906724	64.794420
1617.903084	79.408266	64.799425
1617.534422	77.416967	64.804430
1616.797631	76.250567	64.809434
1615.777040	79.745085	64.814439
1615.155714	68.920246	64.819444
1614.112436	75.622797	64.824449
1613.994275	78.276917	64.829454
1613.656844	74.509705	64.834458
1612.910592	78.354884	64.839463
1612.270727	73.184897	64.844468
1611.270496	71.450061	64.849473
1610.916185	74.558023	64.854478
1610.234265	72.004625	64.859482
1608.957318	83.563564	64.864487
1608.599957	75.710401	64.869492
1607.733643	83.146524	64.874497
1607.480743	67.319312	64.879502
1607.014562	70.935488	64.884506
1606.131238	72.977877	64.889511
1605.207600	61.273812	64.894516
1604.450194	80.838546	64.899521
1603.780931	76.616267	64.904526
1603.384677	70.961293	64.909530
1602.728194	81.059142	64.914535
1602.567531	72.044035	64.919540
1601.283051	78.906340	64.924545
1600.419297	78.165402	64.929550
1600.033270	73.243677	64.934554
1599.204744	82.744376	64.939559
1598.885733	77.312099	64.944564
1598.410114	75.315719	64.949569
1597.942561	71.701651	64.954574
1596.841883	67.658308	64.959578
1596.182428	76.692165	64.964583
1595.669008	70.248393	64.969588
1594.867652	72.918017	64.974593
1593.850373	74.748300	64.979598
1593.364579	73.228209	64.984602
1592.486294	73.998754	64.989607
1592.333761	71.389637	64.994612
1591.488278	75.472942	64.999617
1591.294521	64.864038	65.004622
1590.554805	71.453708	65.009626
1589.236337	72.608011	65.014631
1588.815971	65.512358	65.019636
1588.236327	72.150714	65.024641
1587.894191	72.485985	65.029646
1587.256321	69.454078	65.034650
1585.885840	68.400987	65.039655
1585.062372	67.245215	65.044660
1584.475685	76.470942	65.049665
1584.286064	68.340397	65.054670
1583.961915	67.625695	65.059674
1583.286514	79.084333	65.064679
1582.574160	65.479558	65.069684
1581.612833	73.701924	65.074689
1581.279799	71.493655	65.079694
1580.592100	85.393842	65.084698
1579.295958	75.929932	65.089703
1578.512166	75.196797	65.094708
1578.139967	76.848896	65.099713
1577.723666	74.243842	65.104718
1577.143655	72.152087	65.109722
1576.588556	72.847632	65.114727
1575.679618	71.585593	65.119732
1574.922598	67.104451	65.124737
1574.151215	75.041169	65.129742
1573.915297	66.623086	65.134746
1573.344852	72.507763	65.139751
1572.741626	70.080647	65.144756
1571.440809	83.395419	65.149761
1570.859984	78.212908	65.154766
1570.273926	77.844180	65.159770
1569.921401	75.905519	65.164775
1569.363416	70.416602	65.169780
1568.418301	72.290622	65.174785
1567.197600	71.511792	65.179790
1567.075313	69.878754	65.184794
1566.553373	75.255823	65.189799
1566.309308	72.344279	65.194804
1565.297292	74.613713	65.199809
1563.998737	85.226760	65.204814
1563.962087	81.649888	65.209818
1562.938508	77.772507	65.214823
1562.848384	67.937208	65.219828
1562.219771	70.998870	65.224833
1561.148320	77.330594	65.229838
1560.186053	65.996968	65.234842
1559.664603	73.788317	65.239847
1559.419555	71.760040	65.244852
1558.503481	74.616639	65.249857
1557.075860	68.292909	65.254862
1556.954587	76.356571	65.259866
1555.786482	76.457230	65.264871
1556.071211	69.091848	65.269876
1555.352440	68.534472	65.274881
1555.059116	67.970998	65.279886
1554.363006	79.842945	65.284890
1553.408036	74.354031	65.289895
1552.703731	66.860371	65.294900
1551.924266	69.144899	65.299905
1551.444038	76.238982	65.304910
1550.930651	73.108456	65.309914
1549.771823	80.422335	65.314919
1549.646751	73.055834	65.319924
1549.033044	71.699584	65.324929
1547.565571	71.043555	65.329934
1547.096016	71.339153	65.334938
1546.146761	73.474040	65.339943
1546.216203	72.483910	65.344948
1545.595475	72.437670	65.349953
1545.035713	63.552227	65.354958
1543.717444	70.651738	65.359962
1542.805195	66.619481	65.364967
1542.513996	69.108705	65.369972
1541.763184	64.841059	65.374977
1541.570258	67.415594	65.379982
1541.184909	60.464203	65.384986
1539.869077	69.534554	65.389991
1539.159226	63.066819	65.394996
1538.428677	72.380066	65.400001
1537.985248	66.174353	65.405006
1538.123355	66.483782	65.410010
1536.737852	81.426850	65.415015
1536.389395	62.230644	65.420020
1535.499885	75.551028	65.425025
1535.110396	74.274271	65.430030
1534.237290	66.493621	65.435034
1532.994903	74.707045	65.440039
1532.740987	66.239791	65.445044
1531.967165	71.980169	65.450049
1531.245267	70.112826	65.455054
1531.238136	71.065088	65.460058
1529.919543	71.369447	65.465063
1529.252693	72.748246	65.470068
1528.714307	71.465189	65.475073
1528.226373	75.393921	65.480078
1527.651936	75.136899	65.485082
1526.961126	73.568975	65.490087
1525.895184	72.574757	65.495092
1525.211625	73.746474	65.500097
1524.622607	70.667397	65.505102
1524.285964	64.782193	65.510106
1523.651324	82.841912	65.515111
1523.297807	71.987163	65.520116
1522.147828	71.840524	65.525121
1521.364516	64.624365	65.530126
1521.257618	65.288122	65.535130
1520.359856	73.803184	65.540135
1519.874496	72.005491	65.545140
1518.664685	84.026889	65.550145
1517.963795	69.750099	65.555150
1517.614349	66.459486	65.560154
1516.944881	80.618558	65.565159
1516.892840	68.597825	65.570164
1515.650023	70.834567	65.575169
1514.961439	74.083969	65.580174
1514.463968	63.242643	65.585178
1513.085773	69.951137	65.590183
1512.218233	72.016279	65.595188
1512.248398	67.566187	65.600193
1511.776890	69.751324	65.605198
1511.113918	56.034660	65.610202
1510.527677	62.549490	65.615207
1510.064925	60.200996	65.620212
1508.956237	67.454876	65.625217
1507.985514	66.978555	65.630222
1507.782451	72.517849	65.635226
1506.917833	75.814151	65.640231
1506.909603	75.317342	65.645236
1505.365641	75.920884	65.650241
1504.406219	72.690936	65.655246
1504.277348	63.043160	65.660250
1503.735047	75.313298	65.665255
1503.485021	65.396186	65.670260
1502.748867	67.274869	65.675265
1501.669309	63.505765	65.680270
1500.951654	59.803731	65.685274
1500.249761	71.485784	65.690279
1500.223776	59.878819	65.695284
1499.458052	64.211250	65.700289
1498.047742	68.075252	65.705294
1497.622613	66.737933	65.710298
1496.950790	66.534242	65.715303
1496.579639	63.805334	65.720308
1495.978986	69.811518	65.725313
1495.113941	80.093916	65.730318
1494.237813	68.541624	65.735322
1493.268797	84.948194	65.740327
1493.455347	62.268585	65.745332
1493.004724	67.177003	65.750337
1491.855495	68.758630	65.755342
1491.269392	63.342015	65.760346
1490.325852	75.451989	65.765351
1490.228599	69.637557	65.770356
1489.198023	69.688004	65.775361
1487.563143	67.511597	65.780366
1487.620370	64.424447	65.785370
1486.925304	68.352986	65.790375
1486.532179	76.524504	65.795380
1486.051297	78.088229	65.800385
1485.909512	76.193362	65.805390
1485.246634	66.259862	65.810394
1484.221928	67.440072	65.815399
1483.456299	67.396375	65.820404
1482.118168	73.049826	65.825409
1481.309369	66.776034	65.830414
1481.066263	67.619138	65.835418
1480.385265	77.697244	65.840423
1479.998188	72.370427	65.845428
1479.481177	72.631000	65.850433
1479.230232	72.895022	65.855438
1478.177551	66.682068	65.860442
1477.224747	71.149896	65.865447
1476.710150	66.521450	65.870452
1476.324558	69.552392	65.875457
1475.147252	70.264841	65.880462
1474.719208	62.856618	65.885466
1473.740272	82.653694	65.890471
1473.365679	71.524759	65.895476
1473.004308	79.615538	65.900481
1472.117658	75.490928	65.905486
1471.135446	81.587725	65.910490
1470.461109	84.759179	65.915495
1470.389085	84.354512	65.920500
1469.840336	74.189981	65.925505
1468.658410	80.736418	65.930510
1467.739962	66.267144	65.935514
1467.035662	79.348371	65.940519
1466.943170	67.592701	65.945524
1466.584823	73.618730	65.950529
1464.985498	72.789736	65.955534
1464.622805	71.078216	65.960538
1463.871619	72.363200	65.965543
1463.612850	73.931052	65.970548
1463.144096	77.795245	65.975553
1462.291588	71.873764	65.980558
1461.664614	66.269684	65.985562
1460.804429	77.601584	65.990567
1460.478210	68.612814	65.995572
1459.380994	75.265639	66.000577
1458.324418	73.930912	66.005582
1457.945737	69.681420	66.010586
1456.807785	76.410109	66.015591
1456.582482	69.031167	66.020596
1456.065292	74.052675	66.025601
1456.039682	73.107613	66.030606
1455.837995	66.705800	66.035610
1454.193038	67.918368	66.040615
1453.599914	73.377730	66.045620
1453.104312	65.641198	66.050625
1451.535018	68.131711	66.055630
1451.425071	64.773083	66.060634
1450.699388	66.145481	66.065639
1450.457374	62.298479	66.070644
1449.870528	64.498803	66.075649
1449.074729	72.448888	66.080654
1448.219385	56.624441	66.085658
1447.562304	68.699929	66.090663
1447.011173	67.262794	66.095668
1446.619662	63.187237	66.100673
1445.353822	68.222077	66.105678
1445.039222	66.602267	66.110682
1444.102233	67.377460	66.115687
1444.004125	64.777054	66.120692
1443.423906	66.944787	66.125697
1442.026400	67.821561	66.130702
1441.453187	55.647139	66.135706
1440.911631	73.376660	66.140711
1440.519233	60.080649	66.145716
1439.796652	63.067383	66.150721
1438.844276	71.635300	66.155726
1438.220311	68.482952	66.160730
1437.661379	72.068161	66.165735
1437.287716	64.659188	66.170740
1436.469543	66.126717	66.175745
1435.553073	68.910877	66.180750
1435.202568	60.060021	66.185754
1434.344783	72.977982	66.190759
1434.162786	58.591956	66.195764
1433.041689	67.475276	66.200769
1432.139157	74.090859	66.205774
1431.594496	65.431712	66.210778
1430.946975	74.973061	66.215783
1430.408453	70.100842	66.220788
1429.916331	72.786017	66.225793
1428.496200	81.362057	66.230798
1428.394666	75.250260	66.235802
1427.691370	77.137934	66.240807
1427.245838	80.875437	66.245812
1427.167608	68.106661	66.250817
1425.989733	77.771734	66.255822
1425.266556	69.937336	66.260826
1424.159017	83.921619	66.265831
1423.818431	77.522960	66.270836
1423.583508	69.855389	66.275841
1422.217242	71.029988	66.280846
1421.988725	71.720965	66.285850
1421.308942	68.549108	66.290855
1420.798545	61.601851	66.295860
1419.949092	76.975425	66.300865
1418.619207	76.018476	66.305870
1418.403996	60.918628	66.310874
1417.869854	77.508398	66.315879
1417.705221	74.838140	66.320884
1416.601995	63.068093	66.325889
1415.643750	75.781250	66.330894
1415.284420	61.693076	66.335898
1414.716119	76.496828	66.340903
1414.067905	61.667660	66.345908
1412.806042	65.474992	66.350913
1412.514247	76.741787	66.355918
1412.164055	66.258709	66.360922
1411.388996	73.617293	66.365927
1410.857202	66.761749	66.370932
1409.661617	69.210232	66.375937
1408.672962	69.530019	66.380942
1408.618580	59.879881	66.385946
1408.127593	74.661880	66.390951
1407.551670	66.804084	66.395956
1406.768248	71.926266	66.400961
1405.900233	74.447264	66.405966
1405.635202	69.471654	66.410970
1404.582907	65.371826	66.415975
1404.094937	67.505980	66.420980
1403.243181	69.704267	66.425985
1402.438097	77.168554	66.430990
1402.023842	73.490863	66.435994
1401.248365	72.849503	66.440999
1401.163451	66.496948	66.446004
1400.084571	69.721681	66.451009
1399.247688	67.479988	66.456014
1399.190067	63.990042	66.461018
1398.423610	63.404022	66.466023
1397.031382	70.032797	66.471028
1396.638292	69.806904	66.476033
1395.757339	72.719475	66.481038
1395.616740	69.791507	66.486042
1395.049453	72.589562	66.491047
1394.048487	76.148850	66.496052
1393.151266	66.372485	66.501057
1392.872986	67.186494	66.506062
1392.562930	64.462085	66.511066
1391.433436	72.865779	66.516071
1390.686469	65.852053	66.521076
1390.376446	73.048408	66.526081
1389.544559	74.532325	66.531086
1389.399606	63.888895	66.536090
1387.938972	75.913931	66.541095
1387.118522	69.430711	66.546100
1386.777726	66.600800	66.551105
1385.937673	74.263040	66.556110
1385.780694	68.147449	66.561114
1385.278980	72.524677	66.566119
1384.078397	74.778421	66.571124
1383.483220	68.846029	66.576129
1382.997823	79.022369	66.581134
1382.457891	70.338829	66.586138
1381.353015	72.695634	66.591143
1380.441715	70.675515	66.596148
1380.070483	69.777510	66.601153
1379.446836	72.139821	66.606158
1379.250389	61.703279	66.611162
1378.530248	73.293633	66.616167
1377.749029	70.961095	66.621172
1376.910895	70.815413	66.626177
1376.385097	72.506147	66.631182
1375.834332	72.802069	66.636186
1374.838083	69.418755	66.641191
1374.210950	77.097615	66.646196
1374.124420	75.086738	66.651201
1373.111494	64.614406	66.656206
1372.312697	65.924330	66.661210
1371.372255	74.526641	66.666215
1370.811640	71.720637	66.671220
1370.642630	62.069801	66.676225
1369.582059	72.148334	66.681230
1368.965492	65.721023	66.686234
1367.911325	71.095992	66.691239
1367.474857	63.873641	66.696244
1367.332326	63.292526	66.701249
1366.695611	73.710541	66.706254
1365.807874	62.281588	66.711258
1364.871623	64.598976	66.716263
1364.439592	68.100945	66.721268
1363.901762	66.300587	66.726273
1363.047105	70.145713	66.731278
1362.261600	63.231167	66.736282
1361.473805	73.488694	66.741287
1361.234600	66.865775	66.746292
1360.649213	63.056025	66.751297
1359.649333	64.091986	66.756302
1359.056196	68.299244	66.761306
1357.973267	71.295976	66.766311
1357.692299	71.930641	66.771316
1357.389270	69.260313	66.776321
1356.717096	66.237079	66.781326
1355.861114	65.307329	66.786330
1354.697550	72.235671	66.791335
1354.496046	62.667275	66.796340
1354.363487	67.540916	66.801345
1353.424529	74.696907	66.806350
1352.551886	62.935972	66.811354
1351.797976	67.999857	66.816359
1351.311710	68.451113	66.821364
1350.792835	62.908733	66.826369
1349.424826	67.163483	66.831374
1349.151830	71.930140	66.836378
1348.406112	74.568911	66.841383
1348.247413	63.031950	66.846388
1347.512074	70.496198	66.851393
1346.434987	65.398957	66.856398
1345.680690	63.006958	66.861402
1345.013887	69.359580	66.866407
1344.912587	60.497513	66.871412
1343.873394	62.754002	66.876417
1343.110812	73.557889	66.881422
1342.661542	67.797859	66.886426
1342.119536	71.206927	66.891431
1341.459014	71.802585	66.896436
1340.730660	68.736246	66.901441
1339.529166	74.186688	66.906446
1339.499894	68.243191	66.911450
1339.066751	69.810390	66.916455
1338.291813	71.364117	66.921460
1337.445580	68.281826	66.926465
1336.602272	72.602980	66.931470
1336.374485	66.795125	66.936474
1334.905012	79.343571	66.941479
1334.152648	72.870047	66.946484
1334.133207	66.972298	66.951489
1333.073647	77.175266	66.956494
1333.105469	67.054105	66.961498
1332.249583	73.665454	66.966503
1331.088949	72.711605	66.971508
1330.608374	75.229379	66.976513
1330.156860	71.685362	66.981518
1329.956353	70.619871	66.986522
1328.562008	75.870740	66.991527
1328.086021	71.449083	66.996532
1327.881827	69.128906	67.001537
1326.492955	77.942875	67.006542
1325.745824	65.477587	67.011546
1324.992335	66.386078	67.016551
1324.248929	61.981709	67.021556
1323.908193	71.117899	67.026561
1323.406314	64.872645	67.031566
1323.273342	62.946429	67.036570
1322.743137	59.167341	67.041575
1321.480066	57.321447	67.046580
1321.199372	64.495792	67.051585
1320.225643	65.541803	67.056590
1319.107993	63.092461	67.061594
1318.122643	67.453548	67.066599
1317.874008	64.028670	67.071604
1317.704896	68.323064	67.076609
1317.269682	78.109802	67.081614
1316.762047	67.552430	67.086618
1315.438358	72.367863	67.091623
1314.742546	69.365746	67.096628
1314.694349	58.498789	67.101633
1313.366929	68.996660	67.106638
1312.535281	60.223907	67.111642
1311.957176	68.715005	67.116647
1311.372193	67.715376	67.121652
1311.148786	67.781067	67.126657
1310.565341	64.456731	67.131662
1309.748980	61.174157	67.136666
1308.660784	59.655285	67.141671
1308.199446	66.123481	67.146676
1307.973921	61.316653	67.151681
1306.916443	71.150281	67.156686
1306.015345	59.379702	67.161690
1305.209385	64.648995	67.166695
1304.715065	60.121450	67.171700
1304.623373	66.620763	67.176705
1303.905266	68.853026	67.181710
1303.011261	67.522480	67.186714
1302.273560	66.474594	67.191719
1301.702849	72.537553	67.196724
1301.679975	67.491919	67.201729
1299.889406	61.790618	67.206734
1299.645688	67.766892	67.211738
1298.859367	66.982207	67.216743
1298.547256	68.930720	67.221748
1298.090257	69.497184	67.226753
1296.451492	77.168165	67.231758
1296.265350	71.213342	67.236762
1295.653264	72.796383	67.241767
1295.294227	75.539269	67.246772
1294.852363	68.748307	67.251777
1293.623067	70.241822	67.256782
1293.253405	72.912280	67.261786
1292.324623	69.619200	67.266791
1291.928816	68.349797	67.271796
1291.317133	62.506793	67.276801
1290.303753	78.516744	67.281806
1289.944912	69.783938	67.286810
1288.927312	73.535144	67.291815
1287.979430	71.222828	67.296820
1287.446413	68.795663	67.301825
1286.558144	71.376689	67.306830
1286.300180	63.504648	67.311834
1286.335062	64.912281	67.316839
1285.818709	65.246907	67.321844
1284.990885	64.617061	67.326849
1283.794678	64.017403	67.331854
1283.177904	69.051615	67.336858
1281.872657	68.179132	67.341863
1281.239338	67.185619	67.346868
1281.019095	63.152249	67.351873
1280.275151	72.358861	67.356878
1280.236870	65.153644	67.361882
1279.473549	71.993142	67.366887
1279.055149	67.057709	67.371892
1278.221984	65.247560	67.376897
1277.221212	67.895364	67.381902
1276.518892	59.485268	67.386906
1275.310063	62.565128	67.391911
1274.701510	62.665254	67.396916
1274.389533	58.271152	67.401921
1273.420982	65.025008	67.406926
1273.517423	65.238544	67.411930
1273.128581	65.319504	67.416935
1272.407862	66.153413	67.421940
1271.630971	48.198712	67.426945
1270.674398	67.318877	67.431950
1270.043224	58.173639	67.436954
1268.906646	66.341953	67.441959
1268.560203	61.305195	67.446964
1268.238540	64.141489	67.451969
1267.447895	67.684723	67.456974
1266.800173	63.102730	67.461978
1265.691408	66.499426	67.466983
1265.280137	65.133137	67.471988
1264.795530	61.655900	67.476993
1264.407900	69.889633	67.481998
1263.323963	62.446983	67.487002
1262.233633	67.813545	67.492007
1261.758421	70.026120	67.497012
1261.469507	62.458631	67.502017
1261.046068	68.349941	67.507022
1260.081889	64.264554	67.512026
1259.081557	65.817873	67.517031
1258.435511	68.087576	67.522036
1258.140836	57.439595	67.527041
1257.444098	68.091096	67.532046
1256.803955	58.939404	67.537050
1256.011762	70.523885	67.542055
1255.537264	67.330474	67.547060
1255.359773	65.769315	67.552065
1253.841196	77.469305	67.557070
1253.337116	71.829976	67.562074
1252.546375	66.934832	67.567079
1252.114837	69.586748	67.572084
1252.007912	60.025412	67.577089
1250.320384	71.471563	67.582094
1249.867657	65.180665	67.587098
1249.478939	67.660190	67.592103
1248.631819	66.109317	67.597108
1248.679297	70.812402	67.602113
1247.575320	68.412959	67.607118
1246.878922	68.050813	67.612122
1245.937622	67.391716	67.617127
1245.468825	63.699077	67.622132
1245.225033	69.929259	67.627137
1244.140012	64.352351	67.632142
1243.379867	64.809332	67.637146
1242.774537	65.834638	67.642151
1242.502511	70.063396	67.647156
1241.922225	66.115670	67.652161
1240.677897	71.180296	67.657166
1240.523638	66.171329	67.662170
1240.023072	72.697814	67.667175
1238.686828	69.633555	67.672180
1238.110266	70.020342	67.677185
1237.553944	78.932199	67.682190
1237.142227	63.437859	67.687194
1236.306788	67.937563	67.692199
1235.451178	67.551853	67.697204
1234.873465	67.837898	67.702209
1234.434338	62.164594	67.707214
1233.990676	68.341402	67.712218
1232.881768	63.012731	67.717223
1232.122721	71.228258	67.722228
1231.681677	64.739962	67.727233
1230.723709	74.562523	67.732238
1230.728705	68.362846	67.737242
1229.699759	58.230612	67.742247
1229.027441	71.898143	67.747252
1228.751105	61.550029	67.752257
1228.012228	75.933056	67.757262
1227.191722	64.730021	67.762266
1226.458356	70.776280	67.767271
1225.831934	71.527396	67.772276
1224.849981	69.237870	67.777281
1223.399937	73.376417	67.782286
1223.241637	64.569161	67.787290
1222.598687	71.104097	67.792295
1222.435050	71.627076	67.797300
1221.850493	64.327385	67.802305
1221.529259	66.674754	67.807310
1221.226298	50.666391	67.812314
1220.247636	60.851786	67.817319
1219.230713	73.667360	67.822324
1218.019021	67.523974	67.827329
1217.022900	81.186237	67.832334
1216.722831	75.113920	67.837338
1216.371227	66.277480	67.842343
1215.855770	69.374837	67.847348
1215.702322	70.642105	67.852353
1214.945011	71.390384	67.857358
1214.032458	64.814648	67.862362
1213.485931	65.868456	67.867367
1212.158295	69.422984	67.872372
1211.468767	55.810017	67.877377
1210.809920	67.232947	67.882382
1210.234195	73.366106	67.887386
1209.769945	69.183888	67.892391
1208.973967	64.511947	67.897396
1208.943690	63.870412	67.902401
1208.155001	74.281078	67.907406
1207.400853	67.189712	67.912410
1206.918959	70.477279	67.917415
1205.674780	69.563584	67.922420
1205.226470	69.237691	67.927425
1204.069866	74.334115	67.932430
1203.754044	73.517214	67.937434
1203.483941	66.861388	67.942439
1203.072190	73.340637	67.947444
1202.277144	66.692599	67.952449
1201.227919	67.082024	67.957454
1200.812581	64.081070	67.962458
1200.156356	69.118418	67.967463
1198.986920	72.578407	67.972468
1198.667531	62.880552	67.977473
1198.308756	71.819341	67.982478
1197.729962	63.402243	67.987482
1196.285141	70.621381	67.992487
1195.271713	74.048676	67.997492
1195.108302	61.220953	68.002497
1194.303686	71.629422	68.007502
1194.493714	67.387310	68.012506
1193.579429	67.990247	68.017511
1192.749498	76.970853	68.022516
1192.243712	65.544314	68.027521
1191.672037	74.360842	68.032526
1190.713466	67.473884	68.037530
1189.511102	78.038657	68.042535
1188.987739	68.390587	68.047540
1188.886565	61.386197	68.052545
1188.538660	69.436996	68.057550
1187.713242	67.272404	68.062554
1186.655183	64.422557	68.067559
1185.994388	71.510701	68.072564
1185.647066	61.900872	68.077569
1184.869127	74.251088	68.082574
1183.975118	67.234015	68.087578
1183.232265	75.558945	68.092583
1182.711620	65.558781	68.097588
1182.681903	64.699535	68.102593
1181.106740	70.674677	68.107598
1180.704857	68.518422	68.112602
1180.268779	69.676098	68.117607
1179.583485	71.026376	68.122612
1178.954805	66.189065	68.127617
1177.792810	63.614376	68.132622
1177.567256	62.281644	68.137626
1177.124222	65.290217	68.142631
1176.278227	70.777227	68.147636
1175.453435	60.934253	68.152641
1174.693879	72.251781	68.157646
1174.244591	70.450001	68.162650
1173.786970	71.948577	68.167655
1172.510426	68.914285	68.172660
1172.114534	59.581848	68.177665
1171.315566	72.821669	68.182670
1171.035306	66.109116	68.187674
1170.728533	58.533449	68.192679
1169.646237	68.353718	68.197684
1168.834174	64.152712	68.202689
1168.109639	74.685648	68.207694
1167.771081	73.003454	68.212698
1166.895837	69.425939	68.217703
1165.583390	74.258579	68.222708
1165.415622	75.547051	68.227713
1164.679390	78.340483	68.232718
1164.456506	69.264381	68.237722
1163.975487	69.582372	68.242727
1163.072489	69.548003	68.247732
1162.653021	59.921271	68.252737
1161.703190	69.313615	68.257742
1161.049049	64.008844	68.262746
1160.132654	58.190692	68.267751
1159.163061	64.602545	68.272756
1159.029744	59.087205	68.277761
1158.464283	68.016288	68.282766
1158.073914	68.406596	68.287770
1156.837543	65.020566	68.292775
1155.686599	67.116703	68.297780
1155.827226	56.833180	68.302785
1155.090020	68.014688	68.307790
1154.848974	66.588227	68.312794
1153.872187	60.953149	68.317799
1153.075384	62.365325	68.322804
1152.680012	65.385244	68.327809
1151.891918	67.288051	68.332814
1151.004157	56.717082	68.337818
1150.499258	67.801716	68.342823
1149.777512	64.305452	68.347828
1149.392821	49.290989	68.352833
1147.837052	60.012900	68.357838
1147.187315	55.593695	68.362842
1146.916455	50.874530	68.367847
1146.382586	63.603820	68.372852
1146.343903	63.288479	68.377857
1145.442192	63.961973	68.382862
1144.747718	56.481095	68.387866
1144.445552	61.283938	68.392871
1143.019230	66.166238	68.397876
1142.286785	65.262645	68.402881
1141.377002	68.883211	68.407886
1141.597129	53.739429	68.412890
1140.937852	55.117117	68.417895
1139.556514	64.620678	68.422900
1139.163010	56.166246	68.427905
1138.515149	62.019145	68.432910
1138.183241	57.828513	68.437914
1137.340426	65.689947	68.442919
1136.135503	58.444805	68.447924
1135.923556	55.244356	68.452929
1135.459229	60.255921	68.457934
1134.797568	55.966351	68.462938
1133.752579	63.754285	68.467943
1133.005608	58.207244	68.472948
1132.750604	57.475298	68.477953
1132.034967	70.345472	68.482958
1130.963605	63.426020	68.487962
1130.277282	53.649356	68.492967
1129.538241	68.434542	68.497972
1129.291802	62.815770	68.502977
1128.902019	70.521569	68.507982
1128.425129	61.039598	68.512986
1127.594727	63.855901	68.517991
1126.685552	68.562909	68.522996
1126.346873	61.623114	68.528001
1125.081981	73.285963	68.533006
1124.331028	57.683199	68.538010
1124.038550	62.169108	68.543015
1123.362280	73.880258	68.548020
1123.173036	55.578257	68.553025
1121.797743	63.645819	68.558030
1120.978269	63.014699	68.563034
1120.504645	62.921510	68.568039
1120.011357	72.115089	68.573044
1119.950683	59.138576	68.578049
1118.508723	63.231734	68.583054
1118.047446	58.117078	68.588058
1117.664176	60.351320	68.593063
1117.008937	63.858862	68.598068
1116.031367	57.947957	68.603073
1114.888580	62.485544	68.608078
1114.673454	64.773467	68.613082
1114.173259	57.118191	68.618087
1113.655585	64.139424	68.623092
1113.070531	53.935067	68.628097
1111.886445	65.772722	68.633102
1111.588373	61.994609	68.638106
1111.046796	62.367975	68.643111
1109.750650	61.934110	68.648116
1109.142896	52.589663	68.653121
1108.445180	65.830728	68.658126
1108.186601	58.154366	68.663130
1108.075446	63.880897	68.668135
1106.982097	63.211345	68.673140
1106.454643	58.370572	68.678145
1105.581663	66.236812	68.683150
1105.001819	68.697871	68.688154
1103.971850	57.170244	68.693159
1103.076259	63.277026	68.698164
1102.719621	56.292785	68.703169
1102.061197	67.840243	68.708174
1101.917234	60.519391	68.713178
1101.008198	61.539423	68.718183
1100.185897	62.891014	68.723188
1099.672529	57.874536	68.728193
1098.939106	63.146535	68.733198
1098.271203	56.770058	68.738202
1097.644078	57.589125	68.743207
1096.629104	71.893081	68.748212
1096.272005	61.903201	68.753217
1095.680696	63.773144	68.758222
1094.641650	60.510302	68.763226
1093.812981	65.974075	68.768231
1093.429965	67.303099	68.773236
1093.209111	64.649702	68.778241
1092.905644	61.026994	68.783246
1091.755109	65.162119	68.788250
1090.968984	63.357168	68.793255
1090.182753	65.448933	68.798260
1089.925921	57.042159	68.803265
1088.803653	70.579428	68.808270
1087.633652	55.793984	68.813274
1087.514783	60.182891	68.818279
1086.615460	74.589881	68.823284
1086.705038	57.049367	68.828289
1086.110604	62.471149	68.833294
1085.320187	69.702935	68.838298
1084.721259	66.409507	68.843303
1084.058427	69.850456	68.848308
1082.931126	67.473723	68.853313
1081.911199	62.725491	68.858318
1081.426191	65.791217	68.863322
1081.005131	64.544791	68.868327
1080.190673	70.345358	68.873332
1080.328430	64.301195	68.878337
1078.985307	64.024631	68.883342
1078.165202	56.652072	68.888346
1077.720775	58.517575	68.893351
1077.669905	66.134767	68.898356
1076.571663	66.404305	68.903361
1075.341895	64.048608	68.908366
1075.187299	67.910184	68.913370
1074.935026	60.715377	68.918375
1073.587888	72.813958	68.923380
1073.213647	61.552617	68.928385
1072.461851	62.564991	68.933390
1072.030210	61.859574	68.938394
1071.573516	64.946030	68.943399
1070.162366	64.735487	68.948404
1069.902449	63.545430	68.953409
1069.541365	62.185384	68.958414
1068.384516	66.237944	68.963418
1067.639736	60.387798	68.968423
1066.876610	69.914472	68.973428
1066.415818	65.566156	68.978433
1065.692021	62.108093	68.983438
1065.468819	55.003284	68.988442
1064.587672	58.234536	68.993447
1063.812870	66.219210	68.998452
1063.172743	50.939477	69.003457
1062.720477	59.162999	69.008462
1062.211635	64.894449	69.013466
1061.509802	58.009288	69.018471
1060.562711	59.312935	69.023476
1060.171331	59.783844	69.028481
1058.908018	68.092244	69.033486
1058.162036	65.382043	69.038490
1057.697737	53.967882	69.043495
1057.331711	66.355084	69.048500
1056.934747	57.907530	69.053505
1056.507287	62.121602	69.058510
1055.333586	60.189086	69.063514
1054.681460	53.830616	69.068519
1054.224233	66.506721	69.073524
1053.346896	55.375892	69.078529
1052.238123	60.710770	69.083534
1051.906574	61.880222	69.088538
1051.496012	49.833035	69.093543
1051.115380	64.496551	69.098548
1050.582655	54.919410	69.103553
1049.613927	62.406653	69.108558
1048.912738	63.959768	69.113562
1047.524456	59.265424	69.118567
1046.828131	70.859923	69.123572
1046.260125	58.856702	69.128577
1045.670461	65.386344	69.133582
1045.428530	63.725068	69.138586
1045.452007	63.688425	69.143591
1044.272185	63.094160	69.148596
1043.766522	59.762252	69.153601
1042.875458	65.803676	69.158606
1042.001837	54.741648	69.163610
1041.071147	59.967773	69.168615
1040.038624	71.041743	69.173620
1039.797025	60.817458	69.178625
1039.425159	67.836005	69.183630
1039.108864	62.089588	69.188634
1038.731444	63.862435	69.193639
1037.577083	75.711163	69.198644
1037.310214	60.302660	69.203649
1036.116359	64.925675	69.208654
1035.203858	67.496444	69.213658
1034.536100	61.985720	69.218663
1033.953750	66.203938	69.223668
1033.572581	64.361387	69.228673
1033.257475	65.528225	69.233678
1032.034897	64.656913	69.238682
1031.508399	59.420187	69.243687
1030.748633	73.470666	69.248692
1030.323181	62.340488	69.253697
1029.845016	73.319956	69.258702
1028.878016	67.226053	69.263706
1028.448457	67.297760	69.268711
1027.806279	62.207173	69.273716
1026.798553	63.805911	69.278721
1025.791697	70.308893	69.283726
1025.140319	62.408031	69.288730
1025.082095	64.424988	69.293735
1024.509601	69.296083	69.298740
1024.132586	61.198604	69.303745
1022.917373	62.951782	69.308750
1022.297543	65.029707	69.313754
1022.033730	51.867915	69.318759
1020.546549	70.110594	69.323764
1020.134662	68.287124	69.328769
1019.696047	64.108758	69.333774
1018.980604	66.372210	69.338778
1018.677969	70.432386	69.343783
1017.473110	70.233206	69.348788
1016.886789	61.322196	69.353793
1016.411431	70.601242	69.358798
1015.860684	67.416862	69.363802
1015.230221	58.328372	69.368807
1013.946892	72.115221	69.373812
1013.662626	54.567970	69.378817
1013.187204	67.686947	69.383822
1012.332198	61.619390	69.388826
1011.554937	68.177310	69.393831
1010.771097	66.078705	69.398836
1010.373630	57.355273	69.403841
1009.537081	63.714465	69.408846
1009.495689	55.763867	69.413850
1008.875920	58.459956	69.418855
1007.849775	68.922632	69.423860
1007.460508	58.966281	69.428865
1006.611609	66.054422	69.433870
1005.396729	58.840900	69.438874
1004.907294	60.320910	69.443879
1004.512763	69.530325	69.448884
1004.115155	62.289268	69.453889
1003.377244	62.698626	69.458894
1002.282604	65.848749	69.463898
1001.809840	55.747990	69.468903
1001.441308	67.802853	69.473908
1000.468978	67.601376	69.478913
999.316564	67.040618	69.483918
998.960915	65.794838	69.488922
998.825655	59.737347	69.493927
998.071112	65.518938	69.498932
997.564000	59.668849	69.503937
996.475371	81.103003	69.508942
995.730203	72.698245	69.513946
995.815579	62.691603	69.518951
994.101401	67.006339	69.523956
993.681494	60.688208	69.528961
993.295674	64.818391	69.533966
992.319166	67.927644	69.538970
992.138280	67.675934	69.543975
991.334585	71.610833	69.548980
990.637301	60.861393	69.553985
989.645766	63.793262	69.558990
989.489354	64.340336	69.563994
988.503415	62.530943	69.568999
987.529165	67.858636	69.574004
987.039735	60.111794	69.579009
986.256889	69.135414	69.584014
986.439687	64.254197	69.589018
985.823427	56.201106	69.594023
984.472761	71.214522	69.599028
983.840883	65.728066	69.604033
983.435811	63.678013	69.609038
982.720228	61.469208	69.614042
982.012307	64.419031	69.619047
980.892040	63.189262	69.624052
980.472331	53.527928	69.629057
980.131804	63.592927	69.634062
979.424244	61.048529	69.639066
978.886443	60.823650	69.644071
978.005055	68.352214	69.649076
977.654150	64.347560	69.654081
976.833712	65.217917	69.659086
975.601432	62.413235	69.664090
975.184540	63.407039	69.669095
974.418104	65.052559	69.674100
974.063432	61.802298	69.679105
974.193300	61.349752	69.684110
972.922441	64.261419	69.689114
972.622008	59.546985	69.694119
971.523480	60.882646	69.699124
970.221813	52.151718	69.704129
969.602804	57.064914	69.709134
969.191053	66.439497	69.714138
968.971520	52.773926	69.719143
968.388713	63.684886	69.724148
967.891069	58.553974	69.729153
966.930455	68.271366	69.734158
966.024837	70.410550	69.739162
965.653121	55.769394	69.744167
964.672966	65.318003	69.749172
964.051745	55.617775	69.754177
963.334172	57.815346	69.759182
962.588444	58.601279	69.764186
962.737657	64.209104	69.769191
961.411102	69.100853	69.774196
960.669021	60.030142	69.779201
960.153394	58.600089	69.784206
959.608837	64.378236	69.789210
959.592485	55.761332	69.794215
958.123142	57.908219	69.799220
957.764823	54.661697	69.804225
957.235705	58.789454	69.809230
956.020175	58.181989	69.814234
955.562676	59.336801	69.819239
954.807622	66.867344	69.824244
954.830471	57.827880	69.829249
953.437540	61.599506	69.834254
952.481011	65.897783	69.839258
952.594659	53.987980	69.844263
951.966569	66.571429	69.849268
950.923805	54.427751	69.854273
950.065244	62.397391	69.859278
949.426782	60.296174	69.864282
949.284949	62.411592	69.869287
948.320743	64.107514	69.874292
947.558642	56.924476	69.879297
946.659181	59.857478	69.884302
946.181243	62.852714	69.889306
945.895584	53.222099	69.894311
945.136310	59.155842	69.899316
944.548737	62.540689	69.904321
943.872004	66.945833	69.909326
943.089473	57.857914	69.914330
942.696609	59.836659	69.919335
941.211804	65.819631	69.924340
940.664352	54.371429	69.929345
940.114882	60.260748	69.934350
939.338352	65.698919	69.939354
939.322159	63.052396	69.944359
938.727240	70.156910	69.949364
937.808865	63.350406	69.954369
937.345766	62.528593	69.959374
936.688292	63.874506	69.964378
935.608243	63.089371	69.969383
934.623466	63.202141	69.974388
934.064207	61.613454	69.979393
933.719070	54.006096	69.984398
932.812136	60.948946	69.989402
933.048828	57.475273	69.994407
932.002257	68.073686	69.999412
930.965752	61.571416	70.004417
930.641099	60.177210	70.009422
930.255287	67.663190	70.014426
929.023544	52.876635	70.019431
928.304324	64.050585	70.024436
928.020942	56.613173	70.029441
927.765269	54.362735	70.034446
926.246490	63.031967	70.039450
925.685371	59.970689	70.044455
925.226899	59.646464	70.049460
924.848966	56.456686	70.054465
923.867058	51.718249	70.059470
922.802549	52.362534	70.064474
922.433436	55.059753	70.069479
921.699464	61.948273	70.074484
921.458838	50.571101	70.079489
920.975420	61.379514	70.084494
920.064769	61.666575	70.089498
919.482907	54.076393	70.094503
918.516837	53.944916	70.099508
917.772021	61.161595	70.104513
917.306096	49.828164	70.109518
916.313178	51.301583	70.114522
916.223332	59.719755	70.119527
915.452261	54.605565	70.124532
914.446554	59.342191	70.129537
913.997630	53.916533	70.134542
913.286511	62.241190	70.139546
912.976511	48.638920	70.144551
911.689806	51.581520	70.149556
911.225289	51.799161	70.154561
910.545422	56.234770	70.159566
909.948212	58.305965	70.164570
909.825645	56.113194	70.169575
908.710615	63.965966	70.174580
908.273181	59.776399	70.179585
907.547931	52.943908	70.184590
906.225980	56.620681	70.189594
905.725130	54.204260	70.194599
904.931203	61.469759	70.199604
904.618446	48.970231	70.204609
904.216772	50.811609	70.209614
903.888933	53.100134	70.214618
903.002740	51.249671	70.219623
901.841626	58.889002	70.224628
901.444419	60.179308	70.229633
901.186965	56.978245	70.234638
899.918588	60.862540	70.239642
899.786583	56.228547	70.244647
898.821864	68.529685	70.249652
898.193650	62.429233	70.254657
897.015090	54.369469	70.259662
896.320387	62.771943	70.264666
896.281455	60.460204	70.269671
895.285253	66.516826	70.274676
895.046990	60.937793	70.279681
894.218770	56.963391	70.284686
893.315378	66.375224	70.289690
892.916404	61.692256	70.294695
892.089727	66.567557	70.299700
891.604054	56.746432	70.304705
890.794111	61.098669	70.309710
889.894261	62.694483	70.314714
889.698721	59.409449	70.319719
889.387966	69.370366	70.324724
888.515620	54.126086	70.329729
887.536060	64.833694	70.334734
886.596486	70.187442	70.339738
886.308685	57.168270	70.344743
885.246360	71.692704	70.349748
884.790392	52.266268	70.354753
884.080792	60.376221	70.359758
883.398715	61.535249	70.364762
883.625805	63.796958	70.369767
882.290180	73.025277	70.374772
881.591644	62.529971	70.379777
881.287256	60.388217	70.384782
880.283027	62.639319	70.389786
879.722241	59.975396	70.394791
879.208326	68.194559	70.399796
878.898099	64.361646	70.404801
877.871745	65.416198	70.409806
877.195462	60.324780	70.414810
877.001305	50.007830	70.419815
875.669157	68.333121	70.424820
875.041671	61.910860	70.429825
874.469379	58.720485	70.434830
873.431008	57.559734	70.439834
872.455910	46.157550	70.444839
871.898141	65.647968	70.449844
871.628250	55.939163	70.454849
871.406279	54.276308	70.459854
870.692556	67.496299	70.464858
870.194502	59.178423	70.469863
868.684662	60.838216	70.474868
868.288852	57.053623	70.479873
868.233730	57.571966	70.484878
867.231133	61.213699	70.489882
866.267880	53.023488	70.494887
866.010314	53.195581	70.499892
865.064080	61.415742	70.504897
864.120674	63.501050	70.509902
863.598619	61.807110	70.514906
863.421521	57.312763	70.519911
862.796642	64.393670	70.524916
862.080905	64.600842	70.529921
861.112764	57.668253	70.534926
860.397125	60.221938	70.539930
859.797301	52.934258	70.544935
858.449638	59.657118	70.549940
858.094219	53.650458	70.554945
857.183839	54.773291	70.559950
856.579251	63.409013	70.564954
856.435492	51.836661	70.569959
855.828392	61.182417	70.574964
855.471295	62.070527	70.579969
854.977864	54.277053	70.584974
853.800067	64.849065	70.589978
853.310721	59.559165	70.594983
852.548934	63.861170	70.599988
851.847365	55.088413	70.604993
850.878905	55.570783	70.609998
849.774197	62.144588	70.615002
849.686679	52.830965	70.620007
849.263016	54.734199	70.625012
848.837072	56.372867	70.630017
848.754477	55.728627	70.635022
847.586167	51.385750	70.640026
846.914222	56.074004	70.645031
845.975170	51.128505	70.650036
844.904360	53.541606	70.655041
844.216330	52.225754	70.660046
843.586837	62.707338	70.665050
843.770036	50.737591	70.670055
842.959791	54.730339	70.675060
842.159850	59.863173	70.680065
841.130582	57.062518	70.685070
840.735845	54.253903	70.690074
840.270121	49.217295	70.695079
839.137078	60.395625	70.700084
838.523980	58.474907	70.705089
838.087335	53.428938	70.710094
837.463411	60.475002	70.715098
836.918316	56.009273	70.720103
835.597277	54.981843	70.725108
835.132157	57.740087	70.730113
834.889836	49.165476	70.735118
834.267327	57.811935	70.740122
833.410894	53.722199	70.745127
832.343039	58.626442	70.750132
831.710671	58.659502	70.755137
831.474659	56.041667	70.760142
830.899386	59.503426	70.765146
830.209567	54.802114	70.770151
829.121618	60.420771	70.775156
828.721992	58.250030	70.780161
828.406694	54.831101	70.785166
827.905178	56.953314	70.790170
826.784959	59.396366	70.795175
826.018152	59.742566	70.800180
825.441813	58.032044	70.805185
825.046301	62.047092	70.810190
823.866781	64.449122	70.815194
823.237378	55.707466	70.820199
822.930623	58.588738	70.825204
822.565900	53.794678	70.830209
821.700370	57.397261	70.835214
820.645278	61.085213	70.840218
820.231975	60.449463	70.845223
819.932061	66.619202	70.850228
818.608125	62.163914	70.855233
817.799843	59.682908	70.860238
817.096075	56.371552	70.865242
816.708242	52.508428	70.870247
816.213323	67.645881	70.875252
816.086981	64.479150	70.880257
815.241142	63.732480	70.885262
814.440421	60.367170	70.890266
813.950840	59.986416	70.895271
812.785636	67.508163	70.900276
811.988467	69.943952	70.905281
811.711514	64.916720	70.910286
811.136735	69.614750	70.915290
810.500331	61.646923	70.920295
809.461374	63.342180	70.925300
809.027968	64.690303	70.930305
808.719610	63.227288	70.935310
807.135526	69.254521	70.940314
806.766820	58.156380	70.945319
806.174895	60.960046	70.950324
805.521010	67.112017	70.955329
805.489566	58.456528	70.960334
804.479240	63.335856	70.965338
803.814962	62.303242	70.970343
803.035654	64.420796	70.975348
802.115533	59.147444	70.980353
801.308109	65.434245	70.985358
800.468540	62.765835	70.990362
800.225735	57.499781	70.995367
799.801347	71.891143	71.000372
799.460554	59.457599	71.005377
798.816922	52.602694	71.010382
797.561130	65.497398	71.015386
797.419562	56.283848	71.020391
796.655456	61.464607	71.025396
795.450928	70.501779	71.030401
795.008579	56.324510	71.035406
794.108670	66.393409	71.040410
793.775637	55.863611	71.045415
793.267593	59.387216	71.050420
792.502476	65.514318	71.055425
791.669501	53.554952	71.060430
790.969300	67.364163	71.065434
791.023349	60.007101	71.070439
789.455467	69.693482	71.075444
788.898570	56.736100	71.080449
788.285845	68.850341	71.085454
787.693746	59.016225	71.090458
787.741582	51.770545	71.095463
786.808729	64.705305	71.100468
785.430813	50.757409	71.105473
785.450045	53.370743	71.110478
784.685690	60.888608	71.115482
783.450177	48.211158	71.120487
782.627236	58.332457	71.125492
782.265625	57.666407	71.130497
781.893329	54.592454	71.135502
781.491418	59.190424	71.140506
781.182527	53.668388	71.145511
779.891615	58.638124	71.150516
779.167058	63.560277	71.155521
778.798980	57.207138	71.160526
777.950994	60.680785	71.165530
776.876775	61.615263	71.170535
776.335029	63.600387	71.175540
775.836917	63.331386	71.180545
775.602778	54.921062	71.185550
774.735681	66.921257	71.190554
773.920194	57.767691	71.195559
773.258924	69.139026	71.200564
772.889747	58.275938	71.205569
772.205871	53.690394	71.210574
771.389928	64.469757	71.215578
770.653698	53.048515	71.220583
770.049588	57.189818	71.225588
768.942157	62.045194	71.230593
768.475510	57.537031	71.235598
767.651566	64.974502	71.240602
767.761297	58.168401	71.245607
767.262600	63.791042	71.250612
766.001254	65.075440	71.255617
765.213998	61.580269	71.260622
764.923645	67.081432	71.265626
764.515897	60.141672	71.270631
763.198955	65.112408	71.275636
762.347153	65.833285	71.280641
762.212839	64.903967	71.285646
761.496604	59.836294	71.290650
760.792747	58.956651	71.295655
759.448899	59.495666	71.300660
759.330243	62.741239	71.305665
758.854692	59.376220	71.310670
758.469436	66.116218	71.315674
757.575080	53.252000	71.320679
756.804713	58.954163	71.325684
756.320103	58.790251	71.330689
755.663106	56.994817	71.335694
754.340730	64.128442	71.340698
754.003992	56.262740	71.345703
753.408745	55.763203	71.350708
752.784975	53.853669	71.355713
752.481256	54.231819	71.360718
751.179830	61.281684	71.365722
750.701201	57.664843	71.370727
750.251456	63.593508	71.375732
749.424600	58.250137	71.380737
749.037026	49.326504	71.385742
748.022058	61.862757	71.390746
747.537490	53.003451	71.395751
747.074347	61.272889	71.400756
746.211011	54.206974	71.405761
745.530824	55.390968	71.410766
744.834476	66.190721	71.415770
744.524775	55.824378	71.420775
743.803958	63.417324	71.425780
742.829575	57.286883	71.430785
742.459949	58.386739	71.435790
741.407556	63.239671	71.440794
741.077574	55.103236	71.445799
740.262379	60.686384	71.450804
739.249158	54.557398	71.455809
738.772378	50.061897	71.460814
738.515687	65.382195	71.465818
737.800214	47.572531	71.470823
736.649655	51.226827	71.475828
736.190566	62.704745	71.480833
736.117451	50.280647	71.485838
735.022956	58.879267	71.490842
734.146449	47.094023	71.495847
733.587352	52.690011	71.500852
732.874874	66.947465	71.505857
732.778097	60.628410	71.510862
731.158081	66.016427	71.515866
730.877224	54.137917	71.520871
730.406851	49.275542	71.525876
729.277855	49.480742	71.530881
729.513796	50.965155	71.535886
728.261254	55.545603	71.540890
727.571211	55.684066	71.545895
727.078202	54.767708	71.550900
726.397165	55.524485	71.555905
726.114538	48.821863	71.560910
724.925261	57.990668	71.565914
724.397717	54.258619	71.570919
723.846662	55.784760	71.575924
723.507452	51.779872	71.580929
722.683455	58.461992	71.585934
721.594257	52.997977	71.590938
721.158707	56.153656	71.595943
720.550727	53.472058	71.600948
719.374199	54.552160	71.605953
718.880652	48.917612	71.610958
718.363004	59.972764	71.615962
717.922694	54.862751	71.620967
717.588073	58.800306	71.625972
716.356206	58.246023	71.630977
715.651621	56.339905	71.635982
715.267302	59.982596	71.640986
714.659438	54.686372	71.645991
713.650517	65.876523	71.650996
712.831526	61.963798	71.656001
712.544894	56.416151	71.661006
711.816826	56.656868	71.666010
711.386487	60.019879	71.671015
710.533284	62.729549	71.676020
709.515262	59.868813	71.681025
709.283426	62.397543	71.686030
708.699651	62.779290	71.691034
708.095302	52.201253	71.696039
707.214490	54.636196	71.701044
706.435627	61.243326	71.706049
706.241859	49.475539	71.711054
705.242374	51.420019	71.716058
704.400646	52.290699	71.721063
703.716369	50.070690	71.726068
703.215661	52.274798	71.731073
702.997884	53.345749	71.736078
701.993584	47.130208	71.741082
701.202337	54.575099	71.746087
700.513943	53.040149	71.751092
699.724587	49.576878	71.756097
699.889103	48.910644	71.761102
698.694093	56.574370	71.766106
698.262432	56.425693	71.771111
697.612705	57.667929	71.776116
696.828238	53.019579	71.781121
695.999391	52.420057	71.786126
695.099819	58.612744	71.791130
694.629689	51.709746	71.796135
694.138926	57.484097	71.801140
692.771107	53.814893	71.806145
692.326540	49.085614	71.811150
691.624672	59.357966	71.816154
691.269576	53.521603	71.821159
690.763153	48.963025	71.826164
690.329923	61.143306	71.831169
689.909292	49.277605	71.836174
689.054973	56.357226	71.841178
688.336729	56.153259	71.846183
687.596860	54.642278	71.851188
686.431993	54.589855	71.856193
685.961261	49.882091	71.861198
685.186578	53.433978	71.866202
685.093231	51.884704	71.871207
684.020755	61.809217	71.876212
682.920026	53.216782	71.881217
682.640402	54.493127	71.886222
682.245975	56.243496	71.891226
681.787526	57.109922	71.896231
680.839614	62.340479	71.901236
680.316419	53.515729	71.906241
679.986931	49.812078	71.911246
678.619002	60.773973	71.916250
677.901867	47.820078	71.921255
677.064140	60.848523	71.926260
676.690012	60.982426	71.931265
676.489274	58.603422	71.936270
676.163262	63.897377	71.941274
675.282487	56.053670	71.946279
674.563882	54.646541	71.951284
673.217369	61.116990	71.956289
672.387616	53.433896	71.961294
671.848633	70.439190	71.966298
671.342860	56.951733	71.971303
671.008425	58.298310	71.976308
670.451678	55.764686	71.981313
670.189819	56.800082	71.986318
668.589652	59.245512	71.991322
668.473412	50.895284	71.996327
667.912465	51.642414	72.001332
666.853300	55.848318	72.006337
666.278730	53.707044	72.011342
665.534006	55.396503	72.016346
665.291460	56.919260	72.021351
664.019502	57.732308	72.026356
663.122818	58.006199	72.031361
663.141087	52.760094	72.036366
662.402600	64.847064	72.041370
662.018632	54.554071	72.046375
661.047509	61.089325	72.051380
660.125572	62.488461	72.056385
659.842404	56.197521	72.061390
659.311707	60.100073	72.066394
658.325273	64.466289	72.071399
657.502359	58.947282	72.076404
656.817640	60.228217	72.081409
657.048693	55.303043	72.086414
655.553736	60.240675	72.091418
654.821441	61.149138	72.096423
654.507759	51.554591	72.101428
653.842260	69.573518	72.106433
653.371468	60.172720	72.111438
652.284636	58.154028	72.116442
651.726187	53.357737	72.121447
651.302049	48.229397	72.126452
650.628794	64.396622	72.131457
649.575672	54.691171	72.136462
648.770638	57.465728	72.141466
648.326553	55.321025	72.146471
647.915196	54.379064	72.151476
647.314096	60.965784	72.156481
646.337742	57.622197	72.161486
645.469223	56.894968	72.166490
645.111660	55.599086	72.171495
644.937693	59.181476	72.176500
643.913092	62.073005	72.181505
642.959432	61.542264	72.186510
642.176030	63.807174	72.191514
641.789015	55.739768	72.196519
641.710705	58.704524	72.201524
640.637972	62.095733	72.206529
640.003614	63.999437	72.211534
639.306562	69.235792	72.216538
638.810942	64.703887	72.221543
637.735618	61.525876	72.226548
636.774290	65.866024	72.231553
636.554029	57.235893	72.236558
635.997822	61.527291	72.241562
635.565059	55.916198	72.246567
634.615220	63.309094	72.251572
633.838335	59.487465	72.256577
633.602368	65.990807	72.261582
632.466103	66.026895	72.266586
631.655016	62.641224	72.271591
631.395919	63.941114	72.276596
630.902132	59.153453	72.281601
630.242518	54.182467	72.286606
629.300765	52.476574	72.291610
628.812216	59.581538	72.296615
628.439563	58.300677	72.301620
627.042058	67.162063	72.306625
626.463879	55.879713	72.311630
625.988951	57.844762	72.316634
625.306102	56.531302	72.321639
624.640101	60.039090	72.326644
623.424959	60.798956	72.331649
623.262032	55.745714	72.336654
622.611129	62.403448	72.341658
622.319059	54.857094	72.346663
621.802932	50.527161	72.351668
620.435972	60.892835	72.356673
619.867470	49.233634	72.361678
619.268374	62.258779	72.366682
618.926635	58.145500	72.371687
618.173557	59.257558	72.376692
617.011278	62.368145	72.381697
616.900808	57.111005	72.386702
616.370835	65.121440	72.391706
615.537331	51.260425	72.396711
614.529108	52.580277	72.401716
613.567929	63.133643	72.406721
613.672522	54.029154	72.411726
613.065045	64.931468	72.416730
612.341572	58.390538	72.421735
611.552772	59.189741	72.426740
610.589153	65.421041	72.431745
610.348230	54.105485	72.436750
609.721853	58.989962	72.441754
608.957419	50.758749	72.446759
608.160763	57.919094	72.451764
607.592853	59.063165	72.456769
606.848856	52.703706	72.461774
605.935901	59.620800	72.466778
605.436192	57.754625	72.471783
604.962144	54.782067	72.476788
604.529288	58.747893	72.481793
603.773372	55.612068	72.486798
602.905590	60.369414	72.491802
602.092684	54.432519	72.496807
601.425689	55.903034	72.501812
600.260655	55.353935	72.506817
599.871278	55.381468	72.511822
599.000586	58.393581	72.516826
599.024254	55.483678	72.521831
598.778026	65.858522	72.526836
597.942968	59.469412	72.531841
597.536383	57.719295	72.536846
596.339089	62.138039	72.541850
595.675100	65.287544	72.546855
594.556033	54.602292	72.551860
594.026433	62.179004	72.556865
593.784337	58.258018	72.561870
593.118203	62.199500	72.566874
592.544283	60.162220	72.571879
591.548137	65.728498	72.576884
590.655865	62.511892	72.581889
590.330271	59.428958	72.586894
589.927526	61.182242	72.591898
588.883687	61.649910	72.596903
588.501150	62.507415	72.601908
587.472965	64.656787	72.606913
587.706871	58.330811	72.611918
585.966797	63.715958	72.616922
585.043193	58.498448	72.621927
584.770792	56.562956	72.626932
584.208746	61.352037	72.631937
584.137109	56.732116	72.636942
583.710566	64.234069	72.641946
582.618709	59.521178	72.646951
582.099712	52.958733	72.651956
581.187516	67.642258	72.656961
580.358752	54.356093	72.661966
579.276689	58.989881	72.666970
579.234511	54.931398	72.671975
579.003046	51.658432	72.676980
577.668716	55.326298	72.681985
577.155597	55.362506	72.686990
576.388995	48.836348	72.691994
575.772699	51.681790	72.696999
574.856672	41.279610	72.702004
574.098500	60.382473	72.707009
573.581467	50.274706	72.712014
573.135486	60.039539	72.717018
572.857855	53.683080	72.722023
572.578817	56.268221	72.727028
571.417147	66.470333	72.732033
571.041851	58.287535	72.737038
569.492409	61.768896	72.742042
568.390348	59.071420	72.747047
567.949172	54.152393	72.752052
567.436512	59.739437	72.757057
567.447848	55.697663	72.762062
566.878841	57.521588	72.767066
566.174823	54.683441	72.772071
565.222191	60.225448	72.777076
564.653572	63.952707	72.782081
564.514282	57.859642	72.787086
563.116929	55.094087	72.792090
562.449536	56.835913	72.797095
561.922293	52.979276	72.802100
561.430781	55.032134	72.807105
561.170843	50.997302	72.812110
559.747872	61.720433	72.817114
559.054081	53.965267	72.822119
558.793720	58.006125	72.827124
557.841436	60.003068	72.832129
556.775531	51.566005	72.837134
556.382491	57.332693	72.842138
555.687053	62.002677	72.847143
555.472751	62.495918	72.852148
554.986263	68.113491	72.857153
554.384438	57.224443	72.862158
553.385880	60.056664	72.867162
553.067935	52.948111	72.872167
551.804774	53.769276	72.877172
550.710857	56.279217	72.882177
550.725039	47.924002	72.887182
550.070050	50.151136	72.892186
549.652611	63.205699	72.897191
548.803448	63.170862	72.902196
547.532458	59.202464	72.907201
547.480084	56.372485	72.912206
547.023000	63.281636	72.917210
546.397475	66.074940	72.922215
545.751212	61.302126	72.927220
544.223731	68.457482	72.932225
544.071188	56.482882	72.937230
543.844569	64.527005	72.942234
542.849467	66.571777	72.947239
542.136617	68.019650	72.952244
541.486341	67.500545	72.957249
541.034465	62.215793	72.962254
540.149995	66.863854	72.967258
539.417661	65.053673	72.972263
539.270582	60.281768	72.977268
538.109224	63.009041	72.982273
537.358071	60.022291	72.987278
536.511547	65.388134	72.992282
536.088476	61.043396	72.997287
536.140955	55.312451	73.002292
534.871658	56.383762	73.007297
534.196624	56.915706	73.012302
533.492193	62.386647	73.017306
532.771150	56.517146	73.022311
531.852806	56.255214	73.027316
531.037082	63.896438	73.032321
530.653482	63.516205	73.037326
530.467682	64.823352	73.042330
529.847634	59.432929	73.047335
529.418166	57.386847	73.052340
528.126550	58.952152	73.057345
527.621095	58.179745	73.062350
527.112611	61.380187	73.067354
526.316334	62.494422	73.072359
525.689608	60.443494	73.077364
524.584656	68.231721	73.082369
524.281483	56.790480	73.087374
524.001514	65.887052	73.092378
522.518686	57.117449	73.097383
522.261784	60.353508	73.102388
521.334708	60.433594	73.107393
521.376055	59.184571	73.112398
520.297040	59.905454	73.117402
519.290812	57.408779	73.122407
518.943912	56.546459	73.127412
518.354724	66.357769	73.132417
517.808193	59.189440	73.137422
516.733540	61.387243	73.142426
516.143175	58.764396	73.147431
516.036159	54.590090	73.152436
514.928225	65.777147	73.157441
514.599493	59.061404	73.162446
513.783119	66.604966	73.167450
512.803831	60.489604	73.172455
512.663258	65.705143	73.177460
511.901488	68.498082	73.182465
510.936383	53.907447	73.187470
510.082689	59.865798	73.192474
509.721086	54.090433	73.197479
509.570099	47.245455	73.202484
508.498959	57.213964	73.207489
507.896273	52.274949	73.212494
507.156673	52.456062	73.217498
506.534112	55.365596	73.222503
505.840588	48.856209	73.227508
504.740854	65.685905	73.232513
504.339737	56.072202	73.237518
503.789354	61.013981	73.242522
503.653318	69.269181	73.247527
502.567177	58.105645	73.252532
501.674732	64.694650	73.257537
501.431052	64.044548	73.262542
500.723067	63.399029	73.267546
499.623332	61.112802	73.272551
499.236003	52.285387	73.277556
498.486334	59.130767	73.282561
498.107770	52.497087	73.287566
496.605261	57.268851	73.292570
496.222424	65.161243	73.297575
495.636795	55.498090	73.302580
495.089141	63.781017	73.307585
495.064222	59.601517	73.312590
494.275830	53.383214	73.317594
493.459262	57.072715	73.322599
492.790987	55.097802	73.327604
491.729647	52.890619	73.332609
490.922254	60.644065	73.337614
490.520824	62.084916	73.342618
490.228212	57.031851	73.347623
489.732607	52.064743	73.352628
488.429346	56.375835	73.357633
487.635560	47.873380	73.362638
487.257274	57.567509	73.367642
486.744084	62.556982	73.372647
486.280093	46.829967	73.377652
485.014482	54.773108	73.382657
484.714747	48.776582	73.387662
483.852499	48.764352	73.392666
483.408831	44.328295	73.397671
482.442452	46.206084	73.402676
481.461334	52.484363	73.407681
481.455013	51.063161	73.412686
480.812182	46.505869	73.417690
480.414422	50.474002	73.422695
479.604310	53.787162	73.427700
478.518298	58.185073	73.432705
478.423783	46.869880	73.437710
477.474812	57.068094	73.442714
476.629304	60.218160	73.447719
475.894956	49.604151	73.452724
475.388506	63.005636	73.457729
474.778893	48.990749	73.462734
473.765065	51.095298	73.467738
473.109336	53.145949	73.472743
472.817482	47.621258	73.477748
472.408290	55.336494	73.482753
471.878809	47.979388	73.487758
471.096641	53.566804	73.492762
469.862309	53.301623	73.497767
469.781531	53.967564	73.502772
468.560235	56.855804	73.507777
467.667795	53.877396	73.512782
467.122791	58.933441	73.517786
466.658216	55.946788	73.522791
466.547602	54.192118	73.527796
465.836261	55.193491	73.532801
464.827098	55.280369	73.537806
464.299916	51.906298	73.542810
463.414295	57.194809	73.547815
462.870284	49.020000	73.552820
461.624140	63.671597	73.557825
461.211782	53.346912	73.562830
460.842038	55.776203	73.567834
460.493938	55.721487	73.572839
459.844907	48.339277	73.577844
458.840208	54.719093	73.582849
458.506867	60.761709	73.587854
458.026122	58.815274	73.592858
456.883651	54.384904	73.597863
456.090528	55.670546	73.602868
455.124750	56.931659	73.607873
454.949212	52.743046	73.612878
454.269491	57.265467	73.617882
453.607357	56.792430	73.622887
452.861436	56.480977	73.627892
451.958365	62.344710	73.632897
451.691555	44.921022	73.637902
451.449511	61.101558	73.642906
450.368462	55.846115	73.647911
449.667695	53.324456	73.652916
449.197125	55.801352	73.657921
448.423373	58.730258	73.662926
447.479182	57.671380	73.667930
446.321836	56.121337	73.672935
445.936518	47.572740	73.677940
445.439425	53.766025	73.682945
445.577442	49.499069	73.687950
444.680517	56.019414	73.692954
443.838137	48.552898	73.697959
443.382594	45.608968	73.702964
442.572571	47.882907	73.707969
441.502311	51.743732	73.712974
440.751627	40.815377	73.717978
440.377603	55.380053	73.722983
439.993707	41.611498	73.727988
439.084701	50.410896	73.732993
438.147834	47.630392	73.737998
437.553879	50.346147	73.743002
437.051624	50.800124	73.748007
436.964196	48.584443	73.753012
435.512275	49.465705	73.758017
434.970073	48.614017	73.763022
434.788569	53.506490	73.768026
433.989509	50.377599	73.773031
433.071850	44.520544	73.778036
432.216097	52.478826	73.783041
431.835412	52.434037	73.788046
431.298958	51.553049	73.793050
430.203040	53.610771	73.798055
429.785793	42.183011	73.803060
429.257510	51.815883	73.808065
428.439858	47.224962	73.813070
428.239398	54.876980	73.818074
426.996070	52.752441	73.823079
426.230376	51.702977	73.828084
425.606285	48.215048	73.833089
425.694485	48.284782	73.838094
424.513016	48.936875	73.843098
423.631141	47.704074	73.848103
423.659855	48.239028	73.853108
422.889363	58.197506	73.858113
421.783257	53.531122	73.863118
421.157363	52.186569	73.868122
420.412135	54.806584	73.873127
420.366356	46.391549	73.878132
419.009621	47.394849	73.883137
418.268997	46.765595	73.888142
417.371883	39.003463	73.893146
417.009111	48.980547	73.898151
417.220807	40.010400	73.903156
416.227715	55.867479	73.908161
415.107920	47.910591	73.913166
414.435703	43.217654	73.918170
413.873439	47.540014	73.923175
413.827024	45.658424	73.928180
412.499074	50.757233	73.933185
411.778542	50.038046	73.938190
411.178811	45.603219	73.943194
410.472700	50.867870	73.948199
410.703887	51.304328	73.953204
409.318896	55.076545	73.958209
408.487032	53.033107	73.963214
408.172192	54.725100	73.968218
407.428335	51.664693	73.973223
406.376780	44.297759	73.978228
405.606492	51.002939	73.983233
405.286088	45.060185	73.988238
405.065767	51.322912	73.993242
404.385764	53.557221	73.998247
403.796089	54.338950	74.003252
403.071699	53.352297	74.008257
402.069407	53.625764	74.013262
400.989459	53.481096	74.018266
400.190708	53.897172	74.023271
400.240888	47.866979	74.028276
399.448962	45.985916	74.033281
399.067590	50.213222	74.038286
398.596748	53.366686	74.043290
397.736258	65.738070	74.048295
397.236287	48.116582	74.053300
396.081437	61.361197	74.058305
395.334842	54.513372	74.063310
395.109500	54.806535	74.068314
394.293403	51.882224	74.073319
393.045945	49.685822	74.078324
392.228788	58.894802	74.083329
391.757228	56.371328	74.088334
391.577413	56.316613	74.093338
390.899864	56.170904	74.098343
390.963821	51.518354	74.103348
390.015323	56.354858	74.108353
388.977032	55.060261	74.113358
388.498183	51.851973	74.118362
387.076685	58.731899	74.123367
386.473631	46.516893	74.128372
386.225892	57.893337	74.133377
385.774419	55.259431	74.138382
385.212664	57.134278	74.143386
384.011511	57.234438	74.148391
383.303627	63.543329	74.153396
382.857422	59.123464	74.158401
382.368500	58.228604	74.163406
382.108635	49.663184	74.168410
381.094918	52.026373	74.173415
380.353925	45.470981	74.178420
379.437427	56.332676	74.183425
378.431348	49.008969	74.188430
377.934838	51.598821	74.193434
377.290595	53.636626	74.198439
377.067854	50.652456	74.203444
376.391130	54.929988	74.208449
376.121114	55.580357	74.213454
375.303751	52.274630	74.218458
374.438207	59.543783	74.223463
374.194367	51.447321	74.228468
372.877445	56.495508	74.233473
372.267663	51.478817	74.238478
371.586726	52.286136	74.243482
370.892387	56.714711	74.248487
370.826666	45.166290	74.253492
369.647594	55.270314	74.258497
368.792789	48.177972	74.263502
368.365096	39.890044	74.268506
367.769673	52.708037	74.273511
367.231094	48.014318	74.278516
365.965587	57.471374	74.283521
365.481300	52.119294	74.288526
365.194218	54.554347	74.293530
364.783549	56.957056	74.298535
364.066027	47.734445	74.303540
363.138089	50.134433	74.308545
362.385538	59.385164	74.313550
362.151428	51.414887	74.318554
360.553182	59.497828	74.323559
359.936988	53.775685	74.328564
359.540847	63.239279	74.333569
359.488596	50.450796	74.338574
359.232299	55.090261	74.343578
357.939180	63.230234	74.348583
357.091288	57.519785	74.353588
356.579786	56.365176	74.358593
355.898236	55.130436	74.363598
355.073061	49.011092	74.368602
353.888845	66.499267	74.373607
353.686838	53.173252	74.378612
353.221044	56.951971	74.383617
352.993388	52.823715	74.388622
352.447415	53.242098	74.393626
351.396462	66.006547	74.398631
350.788443	59.084613	74.403636
349.774728	52.528537	74.408641
348.955374	51.244798	74.413646
348.527272	60.358669	74.418650
347.934882	60.678795	74.423655
347.470707	53.998868	74.428660
346.190325	53.515583	74.433665
345.666859	50.776465	74.438670
345.024585	51.916675	74.443674
344.701197	55.658506	74.448679
344.419958	48.689229	74.453684
343.215494	52.498941	74.458689
342.348762	50.134654	74.463694
342.335962	49.272731	74.468698
341.389086	49.691932	74.473703
340.584789	52.862279	74.478708
339.805692	51.848094	74.483713
339.320002	52.471339	74.488718
339.204955	46.470638	74.493722
338.126147	65.750787	74.498727
337.422821	48.212197	74.503732
336.549896	52.197730	74.508737
336.147844	46.001497	74.513742
335.245435	50.179388	74.518746
334.324562	57.621372	74.523751
333.873399	46.747824	74.528756
333.095900	53.257051	74.533761
333.004588	48.998259	74.538766
332.544661	50.174065	74.543770
331.195863	50.985335	74.548775
331.187674	49.936596	74.553780
330.302150	51.443586	74.558785
329.075976	47.553328	74.563790
328.659520	44.059143	74.568794
327.993471	54.773701	74.573799
327.840535	46.255907	74.578804
326.625009	50.982024	74.583809
325.830787	55.085905	74.588814
325.342852	49.300755	74.593818
324.611415	54.683004	74.598823
324.490539	49.500096	74.603828
323.731792	52.396682	74.608833
322.784121	52.981598	74.613838
322.244929	46.400370	74.618842
321.714875	51.310551	74.623847
321.009676	49.098723	74.628852
319.662990	58.625508	74.633857
319.229800	61.993759	74.638862
318.995844	47.726673	74.643866
318.396582	58.036350	74.648871
317.604985	49.585656	74.653876
316.598769	54.289457	74.658881
315.946767	51.842069	74.663886
315.757317	44.913363	74.668890
315.075134	48.039022	74.673895
314.225887	50.349214	74.678900
313.620269	52.402955	74.683905
313.257192	48.427178	74.688910
312.357823	53.790464	74.693914
311.283397	57.483271	74.698919
310.750242	46.767878	74.703924
310.155876	58.363573	74.708929
309.682674	54.438463	74.713934
309.373602	55.770002	74.718938
308.225667	55.339744	74.723943
307.623235	49.516077	74.728948
307.300526	52.365245	74.733953
306.237410	47.013978	74.738958
305.757476	56.399463	74.743962
305.102291	58.235602	74.748967
304.828309	47.193472	74.753972
303.533308	58.970229	74.758977
302.745530	49.807724	74.763982
302.351486	45.225027	74.768986
301.586914	52.191095	74.773991
301.426241	48.030094	74.778996
300.477028	59.836893	74.784001
299.626004	48.298534	74.789006
299.400503	54.634630	74.794010
298.284904	55.380363	74.799015
297.597587	48.501053	74.804020
296.679967	50.784302	74.809025
296.125870	47.176445	74.814030
296.044093	48.277789	74.819034
294.991532	53.635537	74.824039
294.569619	54.862060	74.829044
293.758293	51.806138	74.834049
293.348435	44.658677	74.839054
292.345626	57.447001	74.844058
291.746756	53.748509	74.849063
291.264215	48.009817	74.854068
290.611371	55.672442	74.859073
289.730447	53.083355	74.864078
289.033326	54.946682	74.869082
288.505870	54.264566	74.874087
287.931740	46.465199	74.879092
287.277268	52.912249	74.884097
286.101516	57.229923	74.889102
285.524515	51.326514	74.894106
284.834789	59.315143	74.899111
284.859156	52.803366	74.904116
283.986064	53.231329	74.909121
282.939175	52.606780	74.914126
282.627964	56.654182	74.919130
281.847510	63.761565	74.924135
281.755837	51.455619	74.929140
280.185516	53.253133	74.934145
279.660222	57.995406	74.939150
279.162887	48.792923	74.944154
278.624850	48.140881	74.949159
278.309677	55.735490	74.954164
277.147506	50.712264	74.959169
276.513345	52.407863	74.964174
276.144763	44.571005	74.969178
275.317185	49.011377	74.974183
274.359208	52.136854	74.979188
273.942783	50.088744	74.984193
273.430829	47.008764	74.989198
273.074578	48.915530	74.994202
271.900582	43.346990	74.999207
271.444456	40.931472	75.004212
270.894444	54.762529	75.009217
270.055245	54.623697	75.014222
269.124234	45.359462	75.019226
268.196203	55.062384	75.024231
267.549365	53.792173	75.029236
267.369017	52.326177	75.034241
266.806856	52.472769	75.039246
266.514565	51.381009	75.044250
264.945043	53.471719	75.049255
264.843422	41.433876	75.054260
264.330606	58.242607	75.059265
263.400895	50.775895	75.064270
262.643970	45.869428	75.069274
262.500912	50.913470	75.074279
261.626850	50.559425	75.079284
260.425600	50.613929	75.084289
259.739035	52.770473	75.089294
259.417013	48.575272	75.094298
258.624801	56.405200	75.099303
258.753816	48.206747	75.104308
257.337411	51.897318	75.109313
256.726098	51.230154	75.114318
256.401699	48.175472	75.119322
255.320742	47.614713	75.124327
254.097573	43.908521	75.129332
253.711677	52.518925	75.134337
253.345710	46.991896	75.139342
253.055975	48.247818	75.144346
252.554815	61.049227	75.149351
251.736490	43.041736	75.154356
250.997564	49.256250	75.159361
250.630709	45.087123	75.164366
249.575125	48.146166	75.169370
248.282969	55.174275	75.174375
247.886564	51.323671	75.179380
247.492657	54.805516	75.184385
247.073385	49.786880	75.189390
246.445711	52.982715	75.194394
245.426341	49.392271	75.199399
244.807551	56.431310	75.204404
244.330782	53.318918	75.209409
243.295216	54.529734	75.214414
242.699321	47.891337	75.219418
241.865139	66.351919	75.224423
241.773306	46.922893	75.229428
241.500142	52.750924	75.234433
240.483599	51.109150	75.239438
239.527027	46.303904	75.244442
238.575986	57.830310	75.249447
238.464246	51.277157	75.254452
238.002158	55.596197	75.259457
236.843034	52.658819	75.264462
236.537923	56.270013	75.269466
235.494977	56.403371	75.274471
235.323516	45.243990	75.279476
234.146166	58.840749	75.284481
233.436907	58.536135	75.289486
233.142312	51.165306	75.294490
232.634689	60.283978	75.299495
231.359659	52.722520	75.304500
230.883137	57.953767	75.309505
229.936973	49.832103	75.314510
230.203929	57.357566	75.319514
229.023069	60.286781	75.324519
228.463736	56.389614	75.329524
227.667729	55.425471	75.334529
226.982843	57.761529	75.339534
226.584114	51.351900	75.344538
225.547184	57.306426	75.349543
225.112858	54.207772	75.354548
224.539136	49.907624	75.359553
223.738506	55.983751	75.364558
222.680096	51.294095	75.369562
222.251414	59.416162	75.374567
221.706706	51.925937	75.379572
221.454277	48.626398	75.384577
220.717837	52.558670	75.389582
219.779733	50.857091	75.394586
219.148987	55.195137	75.399591
218.628978	47.347740	75.404596
217.904454	44.363164	75.409601
216.762864	50.932042	75.414606
216.333361	41.803924	75.419610
215.751522	49.858940	75.424615
215.598532	47.798805	75.429620
214.851895	48.706527	75.434625
213.808370	54.911266	75.439630
213.588744	42.682509	75.444634
212.415632	43.970460	75.449639
211.202232	50.749484	75.454644
211.009123	47.741688	75.459649
210.498411	48.083518	75.464654
209.927714	51.644015	75.469658
209.490556	52.912406	75.474663
208.815944	49.699101	75.479668
207.909118	50.123007	75.484673
207.297055	57.105786	75.489678
207.047319	42.360279	75.494682
205.556003	51.714627	75.499687
204.898693	44.541985	75.504692
204.431297	45.965008	75.509697
203.941330	51.953762	75.514702
203.755910	43.486900	75.519706
202.687587	57.760145	75.524711
201.751806	55.198762	75.529716
201.616654	57.002479	75.534721
200.652159	59.682745	75.539726
199.740317	46.799526	75.544730
199.015300	49.654498	75.549735
198.791225	45.438963	75.554740
198.166949	53.704176	75.559745
197.116463	64.476899	75.564750
196.459024	45.216913	75.569754
195.700104	58.721740	75.574759
195.548169	48.924895	75.579764
195.111198	45.041348	75.584769
193.885469	49.747073	75.589774
193.605712	45.956732	75.594778
192.695713	51.343826	75.599783
192.686715	44.744337	75.604788
191.539832	46.075425	75.609793
190.667201	45.484634	75.614798
190.363060	42.844628	75.619802
188.974132	52.904905	75.624807
188.178189	49.728298	75.629812
187.609711	48.835125	75.634817
187.448863	51.321029	75.639822
186.979269	45.055176	75.644826
186.524308	49.953405	75.649831
185.489148	40.111307	75.654836
184.953699	47.215911	75.659841
184.016246	57.251520	75.664846
183.872553	52.269383	75.669850
182.423332	56.255388	75.674855
181.726324	48.910885	75.679860
181.745685	51.197746	75.684865
180.777330	51.298735	75.689870
180.262839	53.836294	75.694874
179.225231	52.715147	75.699879
178.653342	50.874770	75.704884
178.229459	42.059580	75.709889
177.694438	57.200281	75.714894
177.067469	43.767030	75.719898
175.506163	55.972650	75.724903
175.447594	59.057261	75.729908
175.467285	54.668818	75.734913
174.490206	59.416911	75.739918
173.696588	51.613150	75.744922
172.721508	54.585272	75.749927
172.413540	49.165706	75.754932
171.383018	44.805945	75.759937
170.282139	52.008594	75.764942
169.922403	42.326892	75.769946
169.320792	51.015850	75.774951
169.355739	42.028156	75.779956
168.975550	50.995623	75.784961
167.802935	54.587447	75.789966
167.310695	51.878086	75.794970
166.121996	47.767475	75.799975
165.546730	46.190992	75.804980
164.779806	48.631608	75.809985
164.110474	48.869429	75.814990
163.962467	45.520133	75.819994
163.405682	51.752935	75.824999
162.406277	50.960018	75.830004
161.678112	41.608300	75.835009
161.260512	48.042836	75.840014
160.248278	39.556431	75.845018
159.478436	55.105157	75.850023
159.205161	47.773524	75.855028
158.819467	42.907251	75.860033
157.429973	51.846419	75.865038
156.763575	53.865732	75.870042
155.666352	53.241379	75.875047
155.754290	46.657975	75.880052
155.505711	50.058310	75.885057
154.704801	55.942111	75.890062
153.413093	53.790739	75.895066
152.656991	52.282517	75.900071
152.532355	45.633661	75.905076
152.141865	51.765831	75.910081
151.001760	49.520902	75.915086
150.589241	40.901028	75.920090
149.747304	52.216090	75.925095
149.371075	45.392886	75.930100
148.455117	44.214508	75.935105
147.587742	58.301186	75.940110
147.189040	43.573139	75.945114
146.748776	53.557861	75.950119
145.290116	48.999875	75.955124
144.875399	47.440374	75.960129
144.198313	55.873291	75.965134
144.246052	52.180545	75.970138
143.467611	56.210999	75.975143
142.560390	54.198597	75.980148
141.977828	47.785187	75.985153
141.158255	51.213494	75.990158
140.806676	47.805198	75.995162
139.688192	42.568500	76.000167
138.649163	50.245422	76.005172
138.652388	53.522028	76.010177
137.846836	53.015177	76.015182
137.778114	52.996383	76.020186
136.476560	58.605207	76.025191
135.830509	49.697717	76.030196
135.678196	50.453922	76.035201
134.541233	46.128497	76.040206
133.612902	41.637342	76.045210
132.805906	60.642376	76.050215
132.865403	47.766727	76.055220
132.484087	46.255519	76.060225
131.224704	52.217164	76.065230
130.457772	41.392458	76.070234
129.690871	53.974470	76.075239
129.424423	53.670238	76.080244
128.386637	50.945379	76.085249
127.231869	58.883616	76.090254
126.907010	52.067992	76.095258
126.211541	57.640096	76.100263
126.216216	56.250263	76.105268
126.006837	60.804990	76.110273
125.246322	60.048111	76.115278
124.682737	45.973990	76.120282
123.687481	52.905924	76.125287
122.703798	50.953032	76.130292
121.994325	43.224188	76.135297
121.375563	46.137930	76.140302
121.168777	50.479352	76.145306
119.944559	55.148601	76.150311
119.080227	52.560089	76.155316
118.712451	56.506139	76.160321
118.176081	53.065812	76.165326
117.336952	50.560014	76.170330
116.552566	56.430151	76.175335
115.777195	48.648737	76.180340
115.732901	43.716993	76.185345
115.090662	58.800680	76.190350
114.071047	39.817693	76.195354
113.264131	55.175218	76.200359
112.749103	53.981803	76.205364
112.422802	53.106799	76.210369
111.224446	54.495018	76.215374
110.644913	51.102577	76.220378
110.031006	55.378038	76.225383
109.814333	51.281181	76.230388
109.003476	50.437718	76.235393
107.649323	46.091749	76.240398
107.416431	51.769861	76.245402
106.673489	54.157785	76.250407
106.306645	54.274843	76.255412
105.793789	44.895118	76.260417
104.490225	54.019304	76.265422
104.281053	44.739385	76.270426
103.527856	56.522857	76.275431
103.154159	57.166134	76.280436
102.102209	58.937864	76.285441
101.050393	60.518761	76.290446
100.958743	49.616335	76.295450
100.390507	60.020442	76.300455
99.737331	49.836769	76.305460
99.160220	55.189730	76.310465
98.165978	60.870990	76.315470
98.118040	50.365293	76.320474
96.909133	49.427618	76.325479
95.673978	50.028504	76.330484
95.474904	45.211331	76.335489
94.959351	49.852730	76.340494
94.706741	39.789689	76.345498
93.416166	50.368911	76.350503
92.435121	50.922967	76.355508
91.925831	53.494406	76.360513
91.310990	51.911637	76.365518
91.506520	48.800874	76.370522
90.910888	44.023290	76.375527
89.812789	55.412336	76.380532
89.298187	46.307284	76.385537
88.345125	53.856974	76.390542
87.365412	49.982735	76.395546
86.554338	52.141833	76.400551
85.910187	50.593702	76.405556
86.332510	45.568619	76.410561
85.303995	63.845746	76.415566
84.511987	51.940107	76.420570
83.735008	50.577162	76.425575
83.278614	49.538406	76.430580
82.709707	51.203145	76.435585
81.418880	53.702108	76.440590
80.803007	50.055274	76.445594
80.248021	50.380537	76.450599
79.929166	56.846645	76.455604
79.205013	51.969710	76.460609
78.418168	55.733439	76.465614
77.732190	44.837496	76.470618
77.131308	54.276983	76.475623
76.809757	52.503939	76.480628
75.909658	44.084847	76.485633
75.067828	53.476028	76.490638
74.567953	45.582886	76.495642
74.186403	50.844737	76.500647
73.089684	45.546255	76.505652
72.502560	42.806319	76.510657
72.042413	51.212532	76.515662
71.153403	42.077315	76.520666
70.017800	46.390253	76.525671
69.577333	48.428748	76.530676
69.229398	54.587256	76.535681
68.668452	51.680718	76.540686
67.989246	49.103702	76.545690
67.094275	56.442285	76.550695
66.691348	48.486374	76.555700
66.451532	52.426212	76.560705
64.883335	57.276504	76.565710
64.566750	51.724291	76.570714
63.707309	60.769781	76.575719
63.187744	58.105803	76.580724
62.853284	51.272800	76.585729
61.483287	60.541646	76.590734
61.241161	53.194022	76.595738
60.620504	59.402338	76.600743
60.181461	51.928426	76.605748
59.521727	44.582757	76.610753
58.370158	54.734549	76.615758
57.880293	46.571733	76.620762
57.296153	50.511295	76.625767
57.111737	47.006967	76.630772
56.219885	43.563431	76.635777
55.082928	52.586949	76.640782
54.990153	44.674615	76.645786
53.923372	49.755598	76.650791
53.061645	45.100890	76.655796
52.304405	43.708001	76.660801
51.753575	52.716883	76.665806
51.572335	40.712278	76.670810
50.991145	48.857101	76.675815
49.733531	48.362457	76.680820
49.445525	47.664281	76.685825
48.501248	48.496341	76.690830
48.591327	47.203275	76.695834
47.385734	51.787584	76.700839
46.566316	48.457077	76.705844
45.994446	43.746679	76.710849
45.596950	53.560584	76.715854
44.958044	38.197529	76.720858
43.997672	51.132110	76.725863
43.095343	47.661864	76.730868
42.846361	42.120953	76.735873
42.249460	46.996108	76.740878
41.693020	46.067935	76.745882
40.779800	50.490495	76.750887
40.108187	50.189396	76.755892
39.885499	46.747945	76.760897
38.479153	46.083064	76.765902
38.043402	44.831290	76.770906
37.125661	48.742064	76.775911
36.726675	44.820954	76.780916
36.551362	37.434302	76.785921
35.364220	43.822856	76.790926
34.890852	39.156676	76.795930
34.209897	48.121658	76.800935
33.779857	49.338481	76.805940
32.897481	44.103602	76.810945
31.814905	46.253982	76.815950
31.555882	39.927777	76.820954
30.951571	45.007542	76.825959
30.494949	47.054927	76.830964
29.830252	46.218141	76.835969
29.228380	50.080112	76.840974
28.576252	43.774030	76.845978
27.405326	44.197549	76.850983
26.770741	54.482934	76.855988
26.403277	38.608236	76.860993
25.429414	46.288992	76.865998
24.845160	43.217452	76.871002
24.023516	47.168094	76.876007
23.694770	44.159878	76.881012
23.133801	40.346611	76.886017
22.465440	45.116473	76.891022
21.569144	42.591446	76.896026
20.893412	41.278606	76.901031
20.295845	47.311354	76.906036
19.783135	40.681840	76.911041
18.507297	48.516422	76.916046
18.034987	41.104604	76.921050
17.720263	44.001412	76.926055
17.210400	45.404434	76.931060
16.959549	44.003323	76.936065
15.930498	42.929768	76.941070
15.026596	45.829092	76.946074
14.625052	44.652291	76.951079
13.396340	41.573164	76.956084
12.696889	42.971735	76.961089
11.799714	51.740978	76.966094
11.663016	41.381922	76.971098
10.910044	48.674213	76.976103
10.894336	46.108074	76.981108
9.971205	39.972960	76.986113
8.871213	40.434059	76.991118
8.767971	37.336260	76.996122
8.148931	50.093400	77.001127
7.206397	48.726928	77.006132
6.541785	47.937443	77.011137
5.765066	48.102550	77.016142
5.126105	50.377721	77.021147
4.171376	47.794212	77.026151
3.722664	52.789240	77.031156
3.189443	36.649257	77.036161