Fri Mar 05 19:26:40 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.219805	98.923153	0.000000
-0.543204	92.704957	0.005005
-1.630628	58.095734	0.010010
-3.592267	17.838650	0.015014
-7.693960	2.512372	0.020019
-12.574966	5.669240	0.025024
-17.248529	2.964630	0.030029
-22.210444	10.904689	0.035034
-25.626861	7.113300	0.040038
-30.062738	11.049166	0.045043
-33.292172	4.045681	0.050048
-36.861199	-1.034939	0.055053
-40.100571	10.966951	0.060058
-43.652250	2.061054	0.065062
-48.359985	12.109991	0.070067
-52.256673	3.746425	0.075072
-55.574467	6.969372	0.080077
-59.611876	16.201760	0.085082
-62.925515	2.314188	0.090086
-66.740552	8.896529	0.095091
-70.928412	11.242760	0.100096
-74.175207	12.328681	0.105101
-78.005501	9.245219	0.110106
-81.944502	3.468340	0.115110
-85.907079	8.948312	0.120115
-89.622990	0.625354	0.125120
-92.945185	-0.396084	0.130125
-97.054465	6.100788	0.135130
-100.972397	3.750435	0.140134
-105.071662	5.303577	0.145139
-108.617448	6.107669	0.150144
-112.174477	-0.545387	0.155149
-116.078650	13.883938	0.160154
-119.652805	3.918885	0.165158
-123.734173	22.336212	0.170163
-127.399950	9.859519	0.175168
-130.858853	12.944236	0.180173
-135.009276	8.420160	0.185178
-138.234999	4.576429	0.190182
-141.974790	13.714143	0.195187
-146.000201	8.727016	0.200192
-149.726271	14.647164	0.205197
-153.333286	16.434068	0.210202
-157.176469	8.008525	0.215206
-161.339284	12.424596	0.220211
-164.855845	5.697351	0.225216
-168.621793	2.652654	0.230221
-172.418591	14.500816	0.235226
-175.980155	4.992733	0.240230
-179.791003	11.360113	0.245235
-183.513853	10.140969	0.250240
-187.353399	7.377705	0.255245
-191.224673	12.229841	0.260250
-194.621243	5.865113	0.265254
-198.536779	15.319540	0.270259
-202.651220	7.492452	0.275264
-206.305539	3.117981	0.280269
-210.288393	6.768978	0.285274
-213.745591	4.381545	0.290278
-217.356127	10.445776	0.295283
-221.040780	3.414290	0.300288
-224.678650	4.424060	0.305293
-228.540017	10.684460	0.310298
-232.642971	1.633464	0.315302
-236.291846	11.185731	0.320307
-240.211251	4.980217	0.325312
-243.660856	4.578564	0.330317
-247.784725	11.931138	0.335322
-251.373379	7.163059	0.340326
-255.305511	17.227346	0.345331
-258.907053	6.456335	0.350336
-262.282363	4.964221	0.355341
-266.413011	9.930416	0.360346
-269.711664	15.618511	0.365350
-273.557793	19.232018	0.370355
-277.625175	5.151281	0.375360
-281.632468	-2.591839	0.380365
-285.622226	7.569995	0.385370
-289.158910	4.348544	0.390374
-293.050160	3.375650	0.395379
-296.390326	1.620933	0.400384
-300.018193	2.913069	0.405389
-304.204506	9.132421	0.410394
-307.369744	7.215751	0.415398
-311.752463	8.797148	0.420403
-314.985947	6.013028	0.425408
-318.919740	5.466435	0.430413
-323.225930	10.973257	0.435418
-326.707032	1.313799	0.440422
-330.426147	5.615160	0.445427
-334.143401	4.794325	0.450432
-337.671923	5.935039	0.455437
-341.554040	4.356798	0.460442
-345.201105	5.875993	0.465446
-349.126043	11.722532	0.470451
-353.169258	7.596463	0.475456
-356.319770	2.362780	0.480461
-360.788573	5.279486	0.485466
-364.196007	5.997208	0.490470
-368.203722	4.109485	0.495475
-371.834429	9.007068	0.500480
-375.449565	3.987946	0.505485
-379.215358	1.187989	0.510490
-383.106197	-2.530274	0.515494
-386.946497	5.860603	0.520499
-390.749407	-0.435793	0.525504
-394.202250	11.255264	0.530509
-398.222851	-1.681545	0.535514
-401.682957	-5.730330	0.540518
-405.431573	7.141788	0.545523
-409.273200	0.093098	0.550528
-413.180162	0.029650	0.555533
-417.095283	7.588860	0.560538
-420.326857	5.829591	0.565542
-424.366044	-4.770328	0.570547
-428.368781	0.866408	0.575552
-431.747672	-3.375073	0.580557
-435.765126	7.696581	0.585562
-439.458237	6.752207	0.590566
-443.583443	-1.641997	0.595571
-447.049809	-5.453172	0.600576
-450.631077	-2.132426	0.605581
-454.570693	2.455070	0.610586
-458.044530	-1.881595	0.615590
-461.897921	-5.971555	0.620595
-466.151951	-4.845667	0.625600
-469.326439	2.098598	0.630605
-473.294723	7.975908	0.635610
-477.072834	2.290700	0.640614
-480.965660	-0.163955	0.645619
-484.571603	3.865675	0.650624
-488.169949	-5.921453	0.655629
-492.126014	-1.725506	0.660634
-496.024591	-2.159160	0.665638
-499.883235	10.771670	0.670643
-503.614123	2.249936	0.675648
-506.945863	-2.945128	0.680653
-510.878771	6.321737	0.685658
-514.125307	1.259727	0.690662
-518.200524	-5.628464	0.695667
-522.490877	0.497486	0.700672
-526.014481	5.529572	0.705677
-529.953810	2.060571	0.710682
-533.467151	2.896376	0.715686
-537.539358	4.641468	0.720691
-540.928493	0.542130	0.725696
-544.823830	1.085739	0.730701
-548.655995	7.993242	0.735706
-552.224410	2.184775	0.740710
-556.046927	2.169573	0.745715
-559.890121	4.188774	0.750720
-563.421938	-1.363749	0.755725
-567.586352	4.012039	0.760730
-571.027180	0.854550	0.765734
-574.992526	5.720737	0.770739
-579.093676	12.770610	0.775744
-582.299002	1.845368	0.780749
-586.089265	5.846249	0.785754
-589.744396	0.419121	0.790758
-593.902849	2.944479	0.795763
-597.793154	0.711963	0.800768
-601.466288	-0.257424	0.805773
-604.844410	1.108809	0.810778
-608.317328	-5.935373	0.815782
-612.046961	4.292640	0.820787
-616.109807	11.517800	0.825792
-620.368022	5.721882	0.830797
-624.018707	7.286231	0.835802
-627.517469	-0.315183	0.840806
-631.638582	-2.234799	0.845811
-634.987919	5.779967	0.850816
-638.590542	2.626353	0.855821
-642.824074	7.166500	0.860826
-646.198066	6.354384	0.865830
-650.113929	9.634275	0.870835
-653.692081	9.294758	0.875840
-657.629608	-2.101567	0.880845
-661.439914	12.275713	0.885850
-664.851726	-0.422000	0.890854
-669.086970	5.553476	0.895859
-672.802118	1.372389	0.900864
-676.382603	-5.525190	0.905869
-680.397613	8.304515	0.910874
-684.471551	1.222452	0.915878
-687.998491	5.667107	0.920883
-691.457995	4.966492	0.925888
-694.891476	-4.362529	0.930893
-699.023462	7.295537	0.935898
-703.026528	-2.046525	0.940902
-706.540878	7.383987	0.945907
-710.299205	2.807743	0.950912
-713.846380	2.185826	0.955917
-717.782966	5.618946	0.960922
-721.286126	4.830736	0.965926
-724.897854	-0.521110	0.970931
-729.008452	-0.207721	0.975936
-733.243683	5.238014	0.980941
-736.955661	3.940736	0.985946
-740.644338	-1.849788	0.990950
-744.109173	2.750599	0.995955
-748.159496	9.505624	1.000960
-751.446027	1.681249	1.005965
-755.165016	14.249522	1.010970
-759.304333	6.821655	1.015974
-763.081077	9.179064	1.020979
-767.071737	8.555573	1.025984
-770.328110	7.243871	1.030989
-774.449355	12.390766	1.035994
-777.904457	9.740484	1.040998
-781.418376	11.784679	1.046003
-785.536912	12.135705	1.051008
-789.373814	8.761157	1.056013
-793.315780	12.789766	1.061018
-796.495133	7.296377	1.066022
-800.490101	9.860614	1.071027
-804.435471	17.109884	1.076032
-807.970049	13.560883	1.081037
-812.295406	18.563856	1.086042
-815.688149	7.504915	1.091046
-819.572023	14.171951	1.096051
-823.069017	16.789082	1.101056
-826.838480	14.610168	1.106061
-830.566066	16.527746	1.111066
-834.100369	13.645784	1.116070
-838.437752	11.243872	1.121075
-842.212222	18.555767	1.126080
-845.527955	12.056088	1.131085
-849.834912	15.581754	1.136090
-853.108424	0.526791	1.141094
-857.081260	8.955346	1.146099
-860.853285	4.815196	1.151104
-864.446451	10.317778	1.156109
-868.094691	14.909821	1.161114
-871.811830	8.928517	1.166118
-875.532058	4.114645	1.171123
-879.587464	11.332741	1.176128
-883.227459	5.306007	1.181133
-887.302565	20.695775	1.186138
-890.911214	14.037996	1.191142
-894.870095	11.656094	1.196147
-898.447151	7.655140	1.201152
-901.877607	5.751723	1.206157
-905.734257	10.605801	1.211162
-909.613180	6.528554	1.216166
-913.348052	18.213363	1.221171
-917.139130	11.159027	1.226176
-921.217199	3.280126	1.231181
-924.896507	4.739129	1.236186
-928.263613	2.182234	1.241190
-932.226810	6.857852	1.246195
-936.044742	-0.283615	1.251200
-939.529374	-0.593497	1.256205
-943.649498	-2.429140	1.261210
-947.137769	0.639354	1.266214
-951.121876	-2.512687	1.271219
-954.682744	5.600988	1.276224
-958.396635	5.835568	1.281229
-962.449491	8.246910	1.286234
-966.125234	2.419991	1.291238
-970.048093	1.592043	1.296243
-973.443691	1.168627	1.301248
-977.231349	6.306669	1.306253
-981.568168	17.701499	1.311258
-985.024553	8.278818	1.316262
-988.468557	10.827792	1.321267
-992.252474	7.300033	1.326272
-996.017123	11.451999	1.331277
-1000.159821	25.767833	1.336282
-1003.806168	11.297843	1.341286
-1007.645330	12.637465	1.346291
-1011.437900	9.620469	1.351296
-1014.767279	-0.170974	1.356301
-1018.457296	6.895868	1.361306
-1022.514596	7.906134	1.366310
-1026.138620	11.956809	1.371315
-1030.174344	12.446404	1.376320
-1034.123568	3.162557	1.381325
-1037.874919	13.492446	1.386330
-1041.445314	7.885338	1.391334
-1045.203811	13.466672	1.396339
-1048.930937	8.373493	1.401344
-1052.326425	4.835740	1.406349
-1056.289106	13.310301	1.411354
-1059.997259	1.972625	1.416358
-1063.682177	10.625111	1.421363
-1067.716526	12.049670	1.426368
-1071.584485	8.567024	1.431373
-1075.479532	12.066627	1.436378
-1078.897010	8.679085	1.441382
-1082.680065	11.564705	1.446387
-1086.258674	8.073643	1.451392
-1090.094055	4.987935	1.456397
-1094.353839	20.368150	1.461402
-1097.730539	15.867106	1.466406
-1101.293006	14.231106	1.471411
-1105.169154	3.915423	1.476416
-1108.783268	-2.279081	1.481421
-1112.939338	7.257817	1.486426
-1116.531436	3.489846	1.491430
-1120.473439	14.205170	1.496435
-1124.382073	11.216392	1.501440
-1127.451616	3.326323	1.506445
-1131.435766	6.300963	1.511450
-1135.063898	0.474590	1.516454
-1138.913123	10.812403	1.521459
-1143.209673	2.480020	1.526464
-1146.873462	10.861172	1.531469
-1150.644695	2.553560	1.536474
-1154.023682	1.334556	1.541478
-1157.646605	2.034284	1.546483
-1161.470496	9.233149	1.551488
-1165.453605	1.244889	1.556493
-1169.375654	10.897400	1.561498
-1173.188155	6.259629	1.566502
-1176.809077	5.976642	1.571507
-1180.406350	1.782254	1.576512
-1183.802122	2.757906	1.581517
-1187.852836	10.300608	1.586522
-1191.888255	11.966822	1.591526
-1195.831235	8.146316	1.596531
-1199.362218	4.499581	1.601536
-1203.205005	4.357793	1.606541
-1207.057191	5.198363	1.611546
-1210.727793	13.246393	1.616550
-1214.086011	12.292230	1.621555
-1217.888026	7.234971	1.626560
-1221.569258	3.771585	1.631565
-1225.841671	13.179065	1.636570
-1229.436738	0.420120	1.641574
-1233.523638	3.928607	1.646579
-1237.106555	3.622286	1.651584
-1240.390471	14.487941	1.656589
-1244.365277	8.662033	1.661594
-1248.231084	8.829927	1.666598
-1252.072416	1.399441	1.671603
-1255.896566	4.742914	1.676608
-1259.162947	1.985888	1.681613
-1263.276735	2.508881	1.686618
-1266.681333	-0.541397	1.691622
-1270.633826	0.145024	1.696627
-1274.575033	9.554768	1.701632
-1278.582235	0.723760	1.706637
-1282.660657	14.539331	1.711642
-1286.219806	13.284703	1.716646
-1289.566845	13.071593	1.721651
-1293.222591	8.326934	1.726656
-1296.577337	2.982181	1.731661
-1300.607097	14.739991	1.736666
-1304.649761	5.963589	1.741670
-1308.360168	13.909330	1.746675
-1311.987726	12.437038	1.751680
-1315.678280	2.833180	1.756685
-1319.722407	17.751900	1.761690
-1323.722468	7.592057	1.766694
-1327.405067	8.421449	1.771699
-1331.066145	8.533055	1.776704
-1334.390120	2.018087	1.781709
-1338.087489	1.291860	1.786714
-1341.962643	11.418100	1.791718
-1346.048962	4.903765	1.796723
-1350.098148	17.975190	1.801728
-1353.370370	7.012922	1.806733
-1357.254349	5.597524	1.811738
-1360.604067	0.092794	1.816742
-1365.014405	16.957790	1.821747
-1368.907049	19.454568	1.826752
-1372.605734	7.614450	1.831757
-1376.358762	12.405387	1.836762
-1379.653033	12.707498	1.841766
-1383.006984	10.857207	1.846771
-1387.174303	10.769261	1.851776
-1391.103403	12.210643	1.856781
-1395.084058	10.233632	1.861786
-1398.549770	12.468142	1.866790
-1402.522726	11.377720	1.871795
-1406.171726	7.467936	1.876800
-1409.945884	9.199926	1.881805
-1413.719473	11.460100	1.886810
-1417.872179	17.598714	1.891814
-1421.081744	18.024514	1.896819
-1424.571275	11.094648	1.901824
-1428.508427	2.117084	1.906829
-1432.964392	16.106890	1.911834
-1436.176894	6.934457	1.916838
-1440.269387	9.529584	1.921843
-1444.004076	13.969192	1.926848
-1447.119064	1.341897	1.931853
-1451.321705	8.001061	1.936858
-1454.687559	2.699326	1.941862
-1458.663421	6.259808	1.946867
-1462.911210	8.767882	1.951872
-1466.628540	4.990563	1.956877
-1470.524880	12.969479	1.961882
-1473.432964	9.647615	1.966886
-1477.433111	8.239986	1.971891
-1481.406119	8.565784	1.976896
-1485.260295	0.887034	1.981901
-1489.345206	2.948034	1.986906
-1492.574879	1.262504	1.991910
-1495.982750	5.238276	1.996915
-1500.008560	-1.901229	2.006912
-1501.537843	7.797192	2.016909
-1499.218663	8.210892	2.026906
-1495.834914	8.902521	2.036902
-1493.444359	0.175370	2.046899
-1491.651944	5.735518	2.056896
-1490.204183	6.355101	2.066893
-1488.360530	6.352339	2.076890
-1486.171774	8.266406	2.086886
-1484.178171	3.267552	2.096883
-1482.496198	5.507518	2.106880
-1480.692670	9.111171	2.116877
-1478.696902	16.828759	2.126874
-1476.616769	12.712889	2.136870
-1474.813771	12.366124	2.146867
-1472.691594	11.772457	2.156864
-1471.119678	16.227943	2.166861
-1469.160438	17.274050	2.176858
-1467.148558	17.945415	2.186854
-1465.041571	16.149456	2.196851
-1463.714210	11.685200	2.206848
-1461.957692	18.571122	2.216845
-1459.490351	12.875898	2.226842
-1457.593801	7.867342	2.236838
-1455.888429	13.032517	2.246835
-1454.169881	8.035100	2.256832
-1452.186715	6.187929	2.266829
-1450.158498	8.151423	2.276826
-1448.413192	9.118122	2.286822
-1446.604928	9.950004	2.296819
-1444.535638	5.973267	2.306816
-1442.645000	4.158289	2.316813
-1441.010686	8.643277	2.326810
-1438.594021	4.656711	2.336806
-1437.086252	4.399880	2.346803
-1435.569546	11.382642	2.356800
-1433.261274	9.409218	2.366797
-1431.296057	7.174940	2.376794
-1429.402071	6.692062	2.386790
-1427.778656	7.195138	2.396787
-1425.764142	6.096124	2.406784
-1424.145458	13.837826	2.416781
-1422.014675	22.253850	2.426778
-1420.063571	13.584493	2.436774
-1418.464171	7.919339	2.446771
-1416.470741	12.128952	2.456768
-1414.510289	16.288585	2.466765
-1412.757856	10.867350	2.476762
-1410.537842	6.485985	2.486758
-1408.855001	10.121652	2.496755
-1407.016649	12.627163	2.506752
-1405.100780	14.952897	2.516749
-1403.225027	13.383489	2.526746
-1401.317828	10.616948	2.536742
-1399.583619	12.322827	2.546739
-1397.460556	6.198055	2.556736
-1395.591417	8.714434	2.566733
-1394.098698	8.834251	2.576730
-1392.067418	14.899399	2.586726
-1389.966434	5.779757	2.596723
-1388.047791	4.295074	2.606720
-1386.374746	7.349697	2.616717
-1384.364524	7.648770	2.626714
-1382.497326	3.628653	2.636710
-1380.613293	2.234781	2.646707
-1378.795699	5.057846	2.656704
-1377.177346	4.443878	2.666701
-1374.949111	4.431739	2.676698
-1373.486236	2.502144	2.686694
-1371.333056	5.151489	2.696691
-1369.445153	4.254372	2.706688
-1367.469429	5.926346	2.716685
-1365.364427	7.214468	2.726682
-1363.967296	9.782757	2.736678
-1361.948689	6.467887	2.746675
-1359.888175	4.448937	2.756672
-1358.291686	11.674772	2.766669
-1356.398970	14.774778	2.776666
-1354.523192	-1.620860	2.786662
-1352.255030	3.223771	2.796659
-1350.550947	3.950829	2.806656
-1349.145609	5.327290	2.816653
-1346.892206	5.802201	2.826650
-1344.811077	3.462596	2.836646
-1343.077280	3.303853	2.846643
-1341.316393	4.896558	2.856640
-1339.498177	7.632715	2.866637
-1337.278264	9.016151	2.876634
-1335.779989	6.646703	2.886630
-1333.545554	0.786789	2.896627
-1331.666909	3.773803	2.906624
-1329.883805	1.270343	2.916621
-1328.267689	2.548338	2.926618
-1326.103992	7.537615	2.936614
-1324.489321	3.745861	2.946611
-1322.588936	5.767828	2.956608
-1320.720115	5.555908	2.966605
-1318.726464	9.323470	2.976602
-1316.868197	5.636411	2.986598
-1314.796464	4.837806	2.996595
-1313.060716	6.009821	3.006592
-1311.183818	4.771883	3.016589
-1309.614769	5.621638	3.026586
-1307.589059	8.741448	3.036582
-1305.453617	11.857907	3.046579
-1303.580074	7.318941	3.056576
-1301.899938	6.211978	3.066573
-1300.060306	9.132634	3.076570
-1298.054358	5.761423	3.086566
-1296.306206	4.375157	3.096563
-1294.315761	6.248522	3.106560
-1292.459814	6.618158	3.116557
-1290.549411	8.854863	3.126554
-1288.583617	11.546914	3.136550
-1286.937282	-0.383019	3.146547
-1284.712904	5.408162	3.156544
-1283.139486	7.469865	3.166541
-1281.267855	7.546474	3.176538
-1278.922310	2.257771	3.186534
-1277.327338	4.773921	3.196531
-1275.594364	3.590625	3.206528
-1274.230073	6.075806	3.216525
-1271.647872	6.701848	3.226522
-1269.708046	5.174397	3.236518
-1267.937195	7.883457	3.246515
-1266.137379	4.641580	3.256512
-1264.557158	8.967991	3.266509
-1262.625967	6.017721	3.276506
-1260.567252	3.056517	3.286502
-1258.487631	3.924064	3.296499
-1256.781781	6.327746	3.306496
-1254.974260	16.101461	3.316493
-1252.873072	13.774515	3.326490
-1251.126790	11.272267	3.336486
-1249.315722	4.791766	3.346483
-1247.467100	12.364175	3.356480
-1245.396385	7.487381	3.366477
-1243.627821	10.507879	3.376474
-1241.718403	11.682155	3.386470
-1239.910948	4.763292	3.396467
-1238.189987	17.664554	3.406464
-1236.015172	16.696363	3.416461
-1234.286041	14.852134	3.426458
-1232.274570	16.913243	3.436454
-1230.529221	10.138534	3.446451
-1228.379146	5.275897	3.456448
-1226.869756	11.244721	3.466445
-1225.000830	11.784440	3.476442
-1223.107896	13.900842	3.486438
-1221.084964	17.207493	3.496435
-1219.387804	13.969445	3.506432
-1217.394537	21.954527	3.516429
-1215.599994	21.669316	3.526426
-1213.619749	17.677023	3.536422
-1211.567259	15.564748	3.546419
-1209.942710	19.800425	3.556416
-1208.278814	23.158229	3.566413
-1205.916832	15.793804	3.576410
-1204.141217	22.416361	3.586406
-1202.415656	16.851150	3.596403
-1200.509167	16.061721	3.606400
-1198.777661	17.465030	3.616397
-1196.597767	15.938695	3.626394
-1194.745680	8.415879	3.636390
-1193.173485	9.123106	3.646387
-1191.232533	15.041847	3.656384
-1188.813861	12.779416	3.666381
-1187.447966	20.361233	3.676378
-1185.535718	17.301949	3.686374
-1183.641800	12.698232	3.696371
-1181.584550	11.444168	3.706368
-1179.635785	16.801144	3.716365
-1178.056832	11.223095	3.726362
-1175.855820	16.159185	3.736358
-1174.207697	8.612178	3.746355
-1172.842082	9.515106	3.756352
-1170.520773	6.044592	3.766349
-1168.640649	10.444664	3.776346
-1166.489720	13.209831	3.786342
-1164.805900	11.709219	3.796339
-1162.834678	7.899992	3.806336
-1160.997948	7.255967	3.816333
-1159.386389	12.575336	3.826330
-1157.198403	14.489846	3.836326
-1155.490913	12.794400	3.846323
-1153.568813	6.544095	3.856320
-1151.635725	14.279917	3.866317
-1149.977002	15.615960	3.876314
-1148.027525	10.837593	3.886310
-1145.952754	13.273912	3.896307
-1144.193832	13.417613	3.906304
-1142.299513	11.581757	3.916301
-1140.306504	8.328010	3.926298
-1138.522684	7.575626	3.936294
-1136.706288	11.349608	3.946291
-1134.792584	12.128550	3.956288
-1133.007002	19.837466	3.966285
-1130.809737	10.825783	3.976282
-1128.869626	10.889980	3.986278
-1127.561585	10.422147	3.996275
-1125.109609	8.481295	4.006272
-1123.564617	12.541868	4.016269
-1122.109036	6.460963	4.026266
-1120.282570	10.017031	4.036262
-1117.769425	11.072715	4.046259
-1115.774654	15.519229	4.056256
-1114.425904	13.546470	4.066253
-1112.142640	10.576307	4.076250
-1110.229930	6.075432	4.086246
-1108.385794	12.491313	4.096243
-1106.603653	12.509749	4.106240
-1104.980667	10.125227	4.116237
-1102.954207	12.150894	4.126234
-1101.076464	9.427197	4.136230
-1098.925285	3.745023	4.146227
-1097.352088	9.618468	4.156224
-1095.503594	9.714718	4.166221
-1093.369778	8.446903	4.176218
-1091.866859	10.730019	4.186214
-1089.658116	9.879694	4.196211
-1088.041747	10.499400	4.206208
-1086.071346	8.501419	4.216205
-1084.081952	14.497769	4.226202
-1082.133748	13.168078	4.236198
-1080.567771	9.482166	4.246195
-1078.503517	8.699177	4.256192
-1076.271624	14.748320	4.266189
-1074.933259	9.549875	4.276186
-1072.907627	13.550965	4.286182
-1071.091785	9.782456	4.296179
-1069.281599	7.274855	4.306176
-1067.217234	10.271858	4.316173
-1065.342796	14.571877	4.326170
-1063.377155	14.191518	4.336166
-1061.411932	14.490175	4.346163
-1059.771915	9.208748	4.356160
-1057.982429	8.919730	4.366157
-1056.281121	12.472187	4.376154
-1054.047536	17.769505	4.386150
-1052.026635	18.417685	4.396147
-1050.377030	18.383153	4.406144
-1048.331926	17.961675	4.416141
-1046.672213	12.481315	4.426138
-1044.756461	8.523160	4.436134
-1042.958428	10.296471	4.446131
-1040.933767	9.186690	4.456128
-1039.096456	7.865299	4.466125
-1037.335977	16.446731	4.476122
-1035.181560	9.925669	4.486118
-1033.509525	9.301772	4.496115
-1031.728812	9.388388	4.506112
-1029.915256	14.863439	4.516109
-1027.623732	13.905195	4.526106
-1025.994869	11.478733	4.536102
-1023.955371	6.667118	4.546099
-1022.019124	2.789388	4.556096
-1020.609014	11.003714	4.566093
-1018.864354	13.316108	4.576090
-1016.803855	5.027453	4.586086
-1014.298389	7.320793	4.596083
-1012.632614	1.894753	4.606080
-1010.855905	4.811499	4.616077
-1009.345674	12.182451	4.626074
-1007.262507	4.078073	4.636070
-1005.240105	6.019212	4.646067
-1003.475098	9.670468	4.656064
-1001.615039	11.443365	4.666061
-999.657873	10.682309	4.676058
-997.586198	11.652416	4.686054
-995.796762	12.751349	4.696051
-994.150175	12.257866	4.706048
-992.366632	8.883003	4.716045
-990.529826	9.377521	4.726042
-988.414158	7.623229	4.736038
-986.430562	11.226909	4.746035
-984.459360	5.475721	4.756032
-982.815778	9.754309	4.766029
-981.214724	7.439694	4.776026
-979.170801	12.925313	4.786022
-977.088881	11.125902	4.796019
-974.881067	4.872670	4.806016
-973.260514	7.470209	4.816013
-971.864286	10.572574	4.826010
-969.483146	10.189002	4.836006
-968.038054	7.937233	4.846003
-966.287635	11.183484	4.856000
-963.891418	12.619614	4.865997
-962.122032	16.623890	4.875994
-960.286471	12.307571	4.885990
-958.391109	11.780644	4.895987
-956.463656	9.241741	4.905984
-954.593991	4.844185	4.915981
-952.922321	11.262517	4.925978
-950.922872	12.509480	4.935974
-948.761477	6.186325	4.945971
-947.232611	7.263807	4.955968
-945.321609	12.745450	4.965965
-943.280384	9.703627	4.975962
-941.528302	8.489098	4.985958
-940.079042	10.201421	4.995955
-937.821365	12.701840	5.005952
-935.930131	4.222421	5.015949
-934.040045	9.781629	5.025946
-932.179561	5.077663	5.035942
-930.029125	8.479449	5.045939
-928.286178	2.993753	5.055936
-926.602088	7.046431	5.065933
-924.628863	10.647087	5.075930
-922.600097	9.816224	5.085926
-921.063804	13.595699	5.095923
-918.914357	15.099758	5.105920
-917.043902	12.780000	5.115917
-915.430512	17.527681	5.125914
-913.618497	20.472020	5.135910
-911.782523	12.895136	5.145907
-909.181202	12.807998	5.155904
-907.894257	9.689444	5.165901
-905.840971	17.466272	5.175898
-904.012637	13.051676	5.185894
-902.050350	14.134097	5.195891
-900.005251	8.710632	5.205888
-898.560297	10.297354	5.215885
-896.559074	17.490409	5.225882
-894.591626	12.151996	5.235878
-892.775979	13.714188	5.245875
-890.877428	6.181000	5.255872
-888.999567	10.420621	5.265869
-887.336811	12.018315	5.275866
-885.164075	10.967096	5.285862
-883.237951	13.324791	5.295859
-881.618126	7.737232	5.305856
-879.593122	12.404915	5.315853
-877.659271	12.989796	5.325850
-875.792600	9.950674	5.335846
-874.028190	12.291600	5.345843
-872.157745	9.746090	5.355840
-870.266049	9.379293	5.365837
-868.354006	8.881350	5.375834
-866.372607	8.806531	5.385830
-864.464828	14.857184	5.395827
-862.815080	12.114860	5.405824
-861.150078	7.140619	5.415821
-858.970290	12.014100	5.425818
-856.882603	14.225987	5.435814
-855.110702	15.420991	5.445811
-853.337804	10.233714	5.455808
-851.375632	13.883571	5.465805
-849.630826	15.771334	5.475802
-847.906864	8.801354	5.485798
-845.583337	10.866598	5.495795
-843.877091	12.422634	5.505792
-842.229417	8.314862	5.515789
-840.206211	14.189188	5.525786
-838.286183	12.079461	5.535782
-836.437963	12.098591	5.545779
-834.718035	10.279805	5.555776
-832.643181	6.770065	5.565773
-830.894746	7.220416	5.575770
-829.307221	11.083343	5.585766
-827.040587	9.082426	5.595763
-824.857583	8.727517	5.605760
-823.117929	5.468741	5.615757
-821.603205	9.373312	5.625754
-819.476155	10.516304	5.635750
-817.774928	5.476301	5.645747
-815.919685	11.246445	5.655744
-813.604690	8.707283	5.665741
-812.198466	10.325514	5.675738
-810.495936	12.044801	5.685734
-808.304762	4.641739	5.695731
-806.499988	7.336265	5.705728
-804.473768	7.038017	5.715725
-802.864053	12.124262	5.725722
-800.835527	19.459885	5.735718
-798.722222	14.952443	5.745715
-796.915494	9.982430	5.755712
-795.286334	7.835550	5.765709
-793.369325	18.669017	5.775706
-791.329456	16.407539	5.785702
-789.563322	10.518753	5.795699
-787.666739	14.392309	5.805696
-785.611204	11.842541	5.815693
-783.982618	14.461039	5.825690
-782.130576	19.679094	5.835686
-780.180428	11.277206	5.845683
-778.228409	13.583482	5.855680
-776.413701	11.680114	5.865677
-774.607884	12.241335	5.875674
-772.441550	16.392313	5.885670
-770.885827	16.755091	5.895667
-769.072648	13.642494	5.905664
-766.725698	16.725657	5.915661
-765.174977	16.179761	5.925658
-763.225534	10.457484	5.935654
-761.465856	6.338179	5.945651
-759.355880	9.072382	5.955648
-758.119303	9.651969	5.965645
-755.912918	9.996020	5.975642
-753.708662	7.484088	5.985638
-751.881755	9.709330	5.995635
-750.316828	6.319057	6.005632
-748.295171	8.126331	6.015629
-746.137299	12.261318	6.025626
-744.546400	7.676366	6.035622
-742.720960	13.547654	6.045619
-740.968371	8.313175	6.055616
-738.599010	11.353310	6.065613
-737.089149	11.848177	6.075610
-735.067417	13.852820	6.085606
-732.932862	13.141001	6.095603
-731.620509	11.000586	6.105600
-729.625845	16.090099	6.115597
-727.748112	14.249326	6.125594
-725.768691	11.834931	6.135590
-723.946564	14.531488	6.145587
-721.804782	10.512195	6.155584
-720.058142	14.717667	6.165581
-718.338844	10.050632	6.175578
-716.492662	7.152275	6.185574
-714.304508	14.088253	6.195571
-712.429441	10.484227	6.205568
-710.657303	9.397714	6.215565
-708.992733	9.259977	6.225562
-707.033027	11.362979	6.235558
-705.246600	13.294726	6.245555
-703.413608	11.015857	6.255552
-701.383876	10.289239	6.265549
-699.379284	13.318236	6.275546
-697.655503	10.867350	6.285542
-695.668709	16.392364	6.295539
-693.800944	10.749509	6.305536
-691.942761	13.525593	6.315533
-690.212778	12.878466	6.325530
-688.304703	15.044998	6.335526
-686.313642	14.321415	6.345523
-684.336883	11.981690	6.355520
-682.633457	9.969859	6.365517
-680.715563	15.850109	6.375514
-678.795192	11.880444	6.385510
-677.074436	5.826883	6.395507
-675.056445	12.456933	6.405504
-673.288907	14.199092	6.415501
-671.293211	14.167941	6.425498
-669.540422	14.998245	6.435494
-667.555894	14.782566	6.445491
-665.678343	7.203948	6.455488
-663.975593	12.727010	6.465485
-661.957044	10.221151	6.475482
-659.827718	15.562368	6.485478
-657.973224	8.694812	6.495475
-656.412878	13.953266	6.505472
-654.484033	12.423331	6.515469
-652.602804	16.752614	6.525466
-650.745071	17.416162	6.535462
-649.035452	10.371234	6.545459
-646.944841	12.044420	6.555456
-645.020371	21.040510	6.565453
-643.235764	15.963612	6.575450
-641.405579	18.028944	6.585446
-639.139388	16.748278	6.595443
-637.460187	14.252451	6.605440
-635.754881	15.234052	6.615437
-633.667421	13.404051	6.625434
-632.104373	16.236815	6.635430
-630.004437	12.791131	6.645427
-628.206675	10.206893	6.655424
-625.979039	5.030802	6.665421
-624.554237	12.290945	6.675418
-622.699574	12.067632	6.685414
-620.706583	12.392221	6.695411
-618.799447	13.838957	6.705408
-617.047252	6.807775	6.715405
-615.091761	11.248381	6.725402
-612.971314	14.001574	6.735398
-611.349405	16.494946	6.745395
-609.608199	17.663463	6.755392
-607.408150	17.904455	6.765389
-605.548028	14.692898	6.775386
-603.755999	11.473274	6.785382
-602.067559	9.184418	6.795379
-599.941937	14.246808	6.805376
-598.059520	11.822752	6.815373
-596.448796	14.340027	6.825370
-594.504228	13.679212	6.835366
-592.694354	9.457266	6.845363
-590.828858	9.480143	6.855360
-588.718979	9.178187	6.865357
-586.656028	13.666388	6.875354
-584.975606	15.256742	6.885350
-583.118638	9.933062	6.895347
-581.303204	12.273958	6.905344
-579.334981	14.213075	6.915341
-577.501392	5.103641	6.925338
-575.618178	8.106346	6.935334
-573.928683	12.142640	6.945331
-571.832838	17.538238	6.955328
-570.421357	16.378393	6.965325
-568.070209	14.841061	6.975322
-566.093703	15.593070	6.985318
-564.246815	11.196282	6.995315
-562.510129	7.871846	7.005312
-560.615229	9.475321	7.015309
-558.705426	11.895896	7.025306
-557.060303	10.968736	7.035302
-555.199831	10.768231	7.045299
-552.892103	9.049955	7.055296
-551.367957	13.283208	7.065293
-549.368162	13.551507	7.075290
-547.494330	15.403098	7.085286
-545.197818	8.755538	7.095283
-544.051032	3.393758	7.105280
-542.092368	16.974504	7.115277
-540.003504	14.050141	7.125274
-538.191870	5.842666	7.135270
-536.280203	12.082459	7.145267
-534.130579	10.675247	7.155264
-532.432209	8.223799	7.165261
-530.701785	10.106206	7.175258
-528.915907	11.608701	7.185254
-527.000923	9.338972	7.195251
-524.987430	16.465674	7.205248
-523.206412	13.154708	7.215245
-521.005699	13.357779	7.225242
-519.092741	11.873121	7.235238
-517.588222	13.242146	7.245235
-515.682518	9.297055	7.255232
-513.731835	9.792704	7.265229
-511.947506	11.533882	7.275226
-509.951206	15.548060	7.285222
-508.124059	7.827604	7.295219
-506.060940	6.607921	7.305216
-504.390354	9.911493	7.315213
-502.672726	12.065966	7.325210
-500.599610	15.505774	7.335206
-498.658769	16.495643	7.345203
-496.600479	14.210942	7.355200
-494.983886	14.644706	7.365197
-493.253046	10.497034	7.375194
-491.194671	13.129199	7.385190
-489.461991	14.878644	7.395187
-487.643082	12.690607	7.405184
-485.312199	12.126073	7.415181
-483.806470	13.477557	7.425178
-481.841749	11.869397	7.435174
-479.980302	11.807744	7.445171
-477.911618	6.516642	7.455168
-476.150448	12.103151	7.465165
-474.513631	13.027913	7.475162
-472.388022	10.178266	7.485158
-470.388841	11.970424	7.495155
-468.873727	11.660934	7.505152
-466.626232	13.707123	7.515149
-465.079286	13.207814	7.525146
-463.395153	15.227139	7.535142
-461.032373	22.340750	7.545139
-459.483992	12.386407	7.555136
-457.406325	7.502837	7.565133
-455.438313	11.347895	7.575130
-453.673512	13.120658	7.585126
-451.786600	9.525987	7.595123
-449.674840	10.992287	7.605120
-448.183314	9.876571	7.615117
-446.187787	12.840921	7.625114
-444.252657	12.628580	7.635110
-442.408994	10.790310	7.645107
-440.416333	10.848259	7.655104
-438.296729	13.009637	7.665101
-436.883729	16.643347	7.675098
-435.296921	14.103991	7.685094
-433.206727	15.425328	7.695091
-431.053669	13.831342	7.705088
-429.104215	9.479853	7.715085
-427.054576	10.875566	7.725082
-425.926182	12.786298	7.735078
-423.818208	12.004788	7.745075
-422.024841	8.052444	7.755072
-419.517680	7.955616	7.765069
-417.828725	8.474193	7.775066
-416.191321	7.147305	7.785062
-414.483559	12.459759	7.795059
-412.184262	12.492449	7.805056
-410.190908	9.731871	7.815053
-408.980769	12.299037	7.825050
-407.077827	12.459763	7.835046
-404.676916	8.868312	7.845043
-403.251304	11.168965	7.855040
-401.180008	18.510764	7.865037
-399.068703	13.282392	7.875034
-397.209658	13.709085	7.885030
-395.406743	9.376285	7.895027
-393.821776	15.305210	7.905024
-391.939836	15.616146	7.915021
-389.704678	8.806414	7.925018
-387.741820	13.380255	7.935014
-386.174241	11.330320	7.945011
-384.534446	11.897823	7.955008
-382.334804	8.622745	7.965005
-380.838470	14.914783	7.975002
-378.840550	14.569309	7.984998
-376.539863	13.438118	7.994995
-375.159404	15.679683	8.004992
-372.615013	15.916436	8.014989
-370.987095	16.271107	8.024986
-369.179558	15.324456	8.034982
-367.604091	16.429616	8.044979
-365.389575	13.204282	8.054976
-363.531648	16.043832	8.064973
-361.915846	12.765676	8.074970
-359.876607	11.802563	8.084966
-357.979979	10.290639	8.094963
-356.284586	10.866653	8.104960
-354.240210	9.639038	8.114957
-352.673198	13.974531	8.124954
-350.318570	20.448503	8.134950
-348.541533	16.895135	8.144947
-346.952661	9.141778	8.154944
-344.696133	1.884988	8.164941
-342.675487	8.565445	8.174938
-341.117548	9.618157	8.184934
-339.258051	16.752248	8.194931
-337.388774	15.265233	8.204928
-335.530476	13.214704	8.214925
-333.632598	12.799977	8.224922
-331.633326	12.718013	8.234918
-329.732364	16.335463	8.244915
-327.985740	8.793774	8.254912
-326.118514	5.729714	8.264909
-324.324106	10.827875	8.274906
-322.507343	6.720286	8.284902
-320.530641	-2.010766	8.294899
-318.512240	12.326451	8.304896
-316.412686	14.584299	8.314893
-315.005090	8.680444	8.324890
-313.185841	15.778351	8.334886
-311.110230	10.105747	8.344883
-308.880933	5.622831	8.354880
-307.282038	0.643713	8.364877
-305.502257	8.586352	8.374874
-303.654131	12.772789	8.384870
-301.649448	7.642048	8.394867
-300.054213	4.646693	8.404864
-298.090114	13.054129	8.414861
-296.113060	12.961531	8.424858
-294.049081	6.842374	8.434854
-292.573119	7.335041	8.444851
-290.575455	11.860777	8.454848
-288.383297	18.596015	8.464845
-286.321509	15.979348	8.474842
-284.937198	21.203012	8.484838
-283.187114	21.629821	8.494835
-280.717700	16.199113	8.504832
-279.131685	17.700546	8.514829
-277.312005	11.342501	8.524826
-275.418878	10.767524	8.534822
-273.730680	15.222676	8.544819
-271.813011	13.265350	8.554816
-269.916907	14.458339	8.564813
-267.784066	16.726708	8.574810
-266.329743	17.186530	8.584807
-264.044334	18.757910	8.594803
-262.034805	13.350105	8.604800
-260.421723	13.603008	8.614797
-258.538115	15.495902	8.624794
-256.990954	14.665109	8.634791
-254.790216	12.940508	8.644787
-252.736786	11.457320	8.654784
-250.930961	10.621558	8.664781
-248.903103	12.241958	8.674778
-247.311281	12.913530	8.684775
-245.622357	19.275976	8.694771
-243.597121	12.670403	8.704768
-241.454926	8.801454	8.714765
-239.985649	9.219432	8.724762
-238.026058	15.950787	8.734759
-235.784740	17.292387	8.744755
-233.958100	14.842773	8.754752
-232.485441	13.959149	8.764749
-230.424226	17.221100	8.774746
-228.697058	14.024727	8.784743
-226.481468	12.687785	8.794739
-224.635179	12.701381	8.804736
-223.027738	13.563110	8.814733
-220.870374	16.789196	8.824730
-219.531375	10.365807	8.834727
-217.474165	15.071579	8.844723
-215.197953	13.366547	8.854720
-213.508236	10.520377	8.864717
-211.582067	11.790720	8.874714
-209.947543	17.457657	8.884711
-207.960390	12.680314	8.894707
-206.069877	13.866352	8.904704
-203.921073	11.990610	8.914701
-202.534144	15.784945	8.924698
-200.259855	11.217573	8.934695
-198.410554	13.382836	8.944691
-196.496345	7.219763	8.954688
-194.650564	4.936072	8.964685
-192.771105	14.527126	8.974682
-190.869529	4.208664	8.984679
-188.933228	-0.746862	8.994675
-187.040169	5.619359	9.004672
-185.405465	6.539920	9.014669
-183.591826	7.577190	9.024666
-181.555918	5.954751	9.034663
-179.745557	5.874641	9.044659
-177.788371	5.270569	9.054656
-175.922680	5.265317	9.064653
-174.222989	7.786056	9.074650
-172.533256	8.167313	9.084647
-170.277932	8.453570	9.094643
-168.125568	13.155254	9.104640
-166.756917	8.222438	9.114637
-164.691355	8.910041	9.124634
-163.036427	7.961055	9.134631
-161.263162	11.452179	9.144627
-159.142739	9.287318	9.154624
-157.171805	9.271601	9.164621
-155.247824	3.994377	9.174618
-153.294016	12.752539	9.184615
-151.634067	17.973352	9.194611
-149.854014	8.943795	9.204608
-147.804298	11.842912	9.214605
-145.890574	16.145327	9.224602
-144.391648	15.164406	9.234599
-142.212244	11.591185	9.244595
-140.096022	10.085439	9.254592
-138.346507	9.329799	9.264589
-136.901932	14.371831	9.274586
-134.963097	12.927554	9.284583
-132.900976	9.709376	9.294579
-130.583073	7.453027	9.304576
-129.039278	6.577062	9.314573
-127.580815	17.860109	9.324570
-125.194766	13.619183	9.334567
-123.388506	7.347072	9.344563
-121.665739	9.218372	9.354560
-119.794208	7.720109	9.364557
-118.043236	3.927904	9.374554
-115.881728	4.687082	9.384551
-114.011590	4.188531	9.394547
-111.693190	10.310104	9.404544
-110.153294	9.504247	9.414541
-108.714128	1.002804	9.424538
-107.052506	5.765480	9.434535
-105.005545	10.133511	9.444531
-102.703222	3.846998	9.454528
-100.677618	11.071629	9.464525
-99.304445	10.200802	9.474522
-97.310920	11.833126	9.484519
-95.163515	7.331884	9.494515
-93.409580	9.405075	9.504512
-91.422264	10.709970	9.514509
-89.881351	11.184505	9.524506
-87.720490	16.082280	9.534503
-85.889626	17.707410	9.544499
-84.038198	16.586596	9.554496
-81.867805	18.288610	9.564493
-80.517637	19.256222	9.574490
-78.857082	19.997467	9.584487
-76.463400	19.080671	9.594483
-74.384891	14.606226	9.604480
-73.129723	15.279522	9.614477
-70.787188	10.584533	9.624474
-68.911395	11.109862	9.634471
-67.278830	11.296627	9.644467
-65.204641	8.648165	9.654464
-63.201248	10.905792	9.664461
-61.693774	14.417294	9.674458
-59.890942	17.103244	9.684455
-57.655213	14.181117	9.694451
-55.677384	14.623861	9.704448
-54.057874	16.326946	9.714445
-52.627725	10.058044	9.724442
-50.375024	14.920675	9.734439
-48.473270	14.797661	9.744435
-46.673245	12.134532	9.754432
-44.694635	11.640834	9.764429
-42.800610	11.012209	9.774426
-41.010832	11.649179	9.784423
-39.049209	11.104510	9.794419
-37.039604	14.415919	9.804416
-35.146166	12.371061	9.814413
-33.672448	10.738958	9.824410
-31.577893	11.341523	9.834407
-29.648544	10.539902	9.844403
-27.798582	10.349376	9.854400
-25.708761	13.327467	9.864397
-24.134538	8.909829	9.874394
-22.247065	5.072228	9.884391
-19.820865	14.426211	9.894387
-18.539684	15.957502	9.904384
-16.606902	10.238442	9.914381
-14.865519	13.142653	9.924378
-12.695110	11.582581	9.934375
-10.558668	19.572785	9.944371
-9.116347	10.376137	9.954368
-7.473386	20.601935	9.964365
-5.958135	37.967685	9.974362
-4.329195	60.855934	9.984359
-2.715701	98.536945	9.994355
-1.131690	143.887131	10.004352
0.000000	174.068660	10.009357
0.806646	207.543768	10.014362
1.234486	234.298402	10.019367
1.624835	253.752944	10.024371
2.137543	280.142459	10.029376
2.654511	295.148708	10.034381
2.720696	308.919566	10.039386
2.557089	312.095089	10.044391
2.997004	302.071215	10.049395
3.098265	307.079514	10.054400
3.098774	311.867339	10.059405
3.580840	318.117482	10.064410
3.353533	317.944199	10.069415
3.488976	319.244299	10.074419
3.294556	323.489202	10.079424
3.732711	321.066648	10.084429
3.365818	326.494992	10.089434
3.294302	325.754376	10.094439
3.609118	319.112571	10.099443
3.400309	334.062745	10.104448
3.348926	329.939444	10.109453
3.500577	333.805864	10.114458
3.792502	354.452671	10.119463
4.349410	348.406183	10.124467
3.618847	347.586189	10.129472
4.086333	338.944060	10.134477
3.703083	334.635572	10.139482
3.761124	342.252799	10.144487
3.964606	337.861754	10.149491
3.874177	344.816678	10.154496
3.924790	371.087681	10.159501
4.216516	366.144798	10.164506
4.178730	371.009716	10.169511
4.286868	381.627863	10.174515
4.124698	390.019850	10.179520
4.470528	382.007397	10.184525
4.004408	379.968785	10.189530
4.052767	381.298552	10.194535
4.192845	385.439650	10.199539
4.521329	382.750723	10.204544
4.543064	382.501442	10.209549
4.026622	392.597896	10.214554
4.059754	388.640873	10.219559
4.592802	385.460409	10.224563
4.561607	398.832139	10.229568
4.599218	391.788232	10.234573
4.564423	393.353620	10.239578
4.356950	414.906519	10.244583
4.964453	420.972690	10.249587
4.804225	442.448706	10.254592
5.067986	428.100342	10.259597
5.023619	434.305197	10.264602
4.996344	441.737385	10.269607
5.348537	430.251350	10.274611
4.650562	435.527539	10.279616
4.918859	430.332899	10.284621
5.101455	429.234766	10.289626
5.154208	436.234705	10.294631
5.452984	432.943365	10.299635
5.088815	442.868903	10.304640
5.095697	439.233029	10.309645
5.575070	445.876329	10.314650
5.131251	447.029140	10.319655
5.570076	438.669076	10.324659
5.453566	450.619398	10.329664
5.672661	441.069059	10.334669
5.692791	444.484967	10.339674
5.327963	449.242804	10.344679
5.703693	453.877779	10.349683
5.393654	453.295056	10.354688
5.982063	459.943047	10.359693
6.051365	473.924882	10.364698
5.882315	464.381249	10.369703
5.896187	461.250470	10.374707
5.743702	464.829541	10.379712
5.941179	481.870812	10.384717
6.274414	486.785397	10.389722
6.302127	486.107793	10.394727
6.179010	478.477608	10.399731
6.249351	485.954173	10.404736
6.506805	482.398170	10.409741
6.372863	465.277767	10.414746
6.183192	469.717502	10.419751
6.463753	452.109935	10.424755
6.475179	468.712502	10.429760
6.472717	460.741372	10.434765
6.363886	462.287038	10.439770
6.420697	484.099088	10.444775
6.750961	500.913401	10.449779
6.464337	501.837708	10.454784
6.503854	510.399447	10.459789
6.681628	506.747336	10.464794
6.522634	499.226945	10.469799
6.979131	491.221223	10.474803
6.584620	495.331720	10.479808
7.033051	493.383753	10.484813
6.803938	503.335098	10.489818
6.683436	506.535327	10.494823
6.826991	498.017320	10.499827
6.697442	507.528572	10.504832
6.875623	508.191072	10.509837
6.982896	516.423452	10.514842
7.263783	532.845909	10.519847
7.367816	527.496083	10.524851
7.109365	531.347547	10.529856
7.209491	546.712299	10.534861
7.443977	539.737844	10.539866
7.376370	545.400811	10.544871
7.520220	542.599377	10.549875
7.473208	549.112219	10.554880
7.439263	546.922638	10.559885
7.565236	551.482364	10.564890
7.492770	560.806343	10.569895
7.838496	552.965708	10.574899
7.678880	552.549803	10.579904
7.789088	547.706781	10.584909
7.763401	540.403232	10.589914
7.604081	549.403580	10.594919
7.824966	549.475777	10.599923
7.632195	556.142765	10.604928
7.865737	546.902299	10.609933
7.796379	555.216496	10.614938
7.887260	557.465199	10.619943
8.026990	553.510051	10.624947
8.304595	569.977230	10.629952
8.188841	564.749185	10.634957
8.018105	565.153521	10.639962
8.145685	577.142284	10.644967
8.464899	578.649644	10.649971
8.246657	584.454931	10.654976
8.726265	587.061115	10.659981
8.635371	595.949648	10.664986
7.960651	594.321184	10.669991
8.443968	593.771179	10.674995
8.612854	596.191956	10.680000
8.537815	590.921136	10.685005
8.581000	582.830690	10.690010
8.592254	591.064236	10.695015
9.018411	593.284695	10.700019
8.691500	599.760205	10.705024
8.771075	598.178581	10.710029
8.817875	601.872557	10.715034
8.848040	601.180364	10.720039
8.657716	597.973315	10.725043
8.486488	601.588526	10.730048
9.043120	609.552152	10.735053
8.982618	626.641054	10.740058
9.130702	628.524238	10.745063
9.539724	635.749728	10.750067
8.864862	633.096222	10.755072
9.368008	638.262887	10.760077
9.269571	637.619593	10.765082
8.916046	643.730346	10.770087
9.075146	632.621897	10.775091
9.043025	632.600408	10.780096
9.059642	637.639670	10.785101
9.135777	652.368092	10.790106
9.257733	670.413576	10.795111
9.767086	663.712197	10.800115
9.514640	676.952311	10.805120
9.640111	674.877636	10.810125
9.587507	667.669783	10.815130
9.569805	672.924276	10.820135
9.814964	660.882676	10.825139
9.699170	676.673109	10.830144
9.854567	669.943030	10.835149
10.072624	674.306748	10.840154
9.918737	671.371427	10.845159
10.155180	673.768823	10.850163
9.735304	694.103864	10.855168
10.416438	702.076068	10.860173
10.453763	701.631898	10.865178
10.336875	707.984063	10.870183
10.540037	694.228602	10.875187
10.085604	683.080783	10.880192
10.311287	698.083453	10.885197
10.335881	709.532064	10.890202
10.623777	707.947161	10.895207
10.744818	710.120111	10.900211
10.569393	723.789549	10.905216
10.544535	723.858368	10.910221
10.804022	714.769783	10.915226
10.767339	722.891197	10.920231
11.082296	712.364980	10.925235
10.651725	714.376752	10.930240
10.597940	716.355231	10.935245
10.978032	711.937479	10.940250
11.074093	719.903670	10.945255
11.288327	718.966057	10.950259
10.583112	724.068452	10.955264
10.602448	728.687824	10.960269
11.020835	716.798326	10.965274
10.823127	726.008342	10.970279
11.012053	720.261686	10.975283
11.119476	723.342023	10.980288
11.033923	727.833040	10.985293
11.043492	718.893133	10.990298
10.826068	728.385429	10.995303
11.329538	740.468914	11.000307
11.226296	756.967093	11.005312
11.304254	743.043893	11.010317
11.424272	752.931830	11.015322
11.444172	752.998241	11.020327
11.937436	750.959508	11.025331
11.899595	757.136651	11.030336
11.697278	754.833540	11.035341
11.805274	755.813191	11.040346
11.674168	763.978077	11.045351
12.362037	750.664087	11.050355
11.734184	764.303225	11.055360
11.762407	754.224859	11.060365
11.767585	758.103719	11.065370
11.823304	760.613542	11.070375
12.057810	753.621635	11.075379
11.731104	759.775468	11.080384
12.075737	759.771154	11.085389
11.736741	763.585062	11.090394
12.297084	778.275799	11.095399
12.188250	785.984536	11.100403
12.441233	790.453112	11.105408
12.448886	794.279544	11.110413
12.092178	796.569718	11.115418
12.293634	801.432889	11.120423
12.507093	794.275577	11.125427
12.310643	796.642695	11.130432
12.458899	804.436595	11.135437
12.546642	805.279124	11.140442
12.538649	806.919133	11.145447
12.899641	798.159675	11.150451
12.386500	810.604090	11.155456
12.751808	812.566195	11.160461
12.642526	804.924169	11.165466
12.655884	797.642648	11.170471
12.791477	814.758841	11.175475
12.957071	834.503919	11.180480
13.113204	826.664994	11.185485
13.022040	834.724194	11.190490
13.097316	840.894368	11.195495
13.353807	835.117966	11.200499
13.227462	840.998586	11.205504
13.306765	844.766291	11.210509
12.923364	835.712368	11.215514
13.090638	840.584159	11.220519
12.999130	835.602898	11.225523
13.037974	847.653350	11.230528
13.157041	831.861025	11.235533
13.393654	836.475736	11.240538
12.961085	842.736382	11.245543
13.617287	855.219824	11.250547
13.647813	870.010938	11.255552
13.661065	867.820088	11.260557
13.894192	874.018715	11.265562
13.860150	878.138842	11.270567
13.937155	868.126738	11.275571
13.869518	884.926905	11.280576
13.718137	870.789415	11.285581
14.077456	874.433610	11.290586
13.775584	876.241937	11.295591
14.039598	873.865997	11.300595
13.861939	872.418422	11.305600
14.087629	876.323643	11.310605
14.352006	879.561913	11.315610
14.005552	877.406361	11.320615
14.238994	874.497527	11.325619
13.768984	886.931973	11.330624
13.887006	873.956367	11.335629
13.908949	888.189020	11.340634
14.043804	896.560727	11.345639
14.610710	906.256052	11.350643
14.713824	906.004820	11.355648
14.635390	912.037107	11.360653
14.391560	909.743748	11.365658
14.326375	920.361550	11.370663
14.413886	914.159459	11.375667
14.774136	920.094963	11.380672
14.745177	921.444999	11.385677
14.660786	908.143661	11.390682
14.639007	915.876430	11.395687
15.017940	913.232980	11.400691
14.532893	911.457519	11.405696
14.336722	922.028404	11.410701
14.704887	939.397821	11.415706
14.766478	944.111452	11.420711
15.019701	944.523868	11.425715
15.085961	956.957991	11.430720
15.148128	957.099667	11.435725
15.657170	950.902865	11.440730
15.089938	957.744892	11.445735
15.007860	950.803391	11.450739
15.631390	953.621667	11.455744
15.190978	956.959762	11.460749
15.403784	949.564344	11.465754
15.301683	959.396385	11.470759
15.669237	966.598692	11.475763
15.632801	974.344869	11.480768
15.696860	979.018692	11.485773
16.024863	978.334168	11.490778
15.856865	972.108151	11.495783
15.788399	953.172581	11.500787
15.526852	961.691141	11.505792
15.696513	970.349094	11.510797
16.025323	975.838600	11.515802
16.002932	988.198576	11.520807
16.188896	982.018601	11.525811
16.003377	993.709123	11.530816
16.074258	990.512363	11.535821
16.313192	997.782514	11.540826
16.140504	990.032226	11.545831
15.968408	994.948740	11.550835
16.171288	989.031009	11.555840
15.883932	993.499101	11.560845
16.045679	987.021769	11.565850
15.774218	999.464065	11.570855
15.817889	996.804689	11.575859
16.075265	1015.589141	11.580864
16.134061	1019.606183	11.585869
16.331769	1022.758920	11.590874
16.252009	1034.497264	11.595879
16.414903	1031.214850	11.600883
16.461569	1035.115553	11.605888
16.864566	1047.805143	11.610893
16.939630	1038.271080	11.615898
16.825914	1045.972848	11.620903
16.905668	1036.729795	11.625907
16.886165	1043.479760	11.630912
16.812080	1047.853921	11.635917
17.338329	1041.487167	11.640922
17.101132	1052.564618	11.645927
17.225077	1041.715373	11.650931
17.384421	1051.210861	11.655936
17.189775	1040.970716	11.660941
17.144764	1033.349858	11.665946
17.137455	1040.119956	11.670951
17.652693	1043.040685	11.675955
17.770508	1043.946245	11.680960
17.581717	1034.698717	11.685965
17.437232	1024.903197	11.690970
17.060581	1024.099246	11.695975
17.312521	1030.162467	11.700979
17.332672	1049.577777	11.705984
17.623427	1049.848583	11.710989
17.775501	1058.031544	11.715994
17.548417	1052.551404	11.720999
17.449585	1050.029875	11.726003
17.425388	1057.726832	11.731008
17.482841	1053.915570	11.736013
17.754676	1049.563876	11.741018
17.392497	1057.656967	11.746023
17.746910	1071.215403	11.751027
17.840134	1089.650794	11.756032
17.835690	1089.613849	11.761037
18.103739	1089.766844	11.766042
18.000628	1093.727726	11.771047
18.280270	1087.412906	11.776051
18.363042	1087.161762	11.781056
18.184668	1095.421111	11.786061
18.190958	1095.149049	11.791066
18.179300	1106.040742	11.796071
18.152388	1091.958882	11.801075
17.977091	1100.487422	11.806080
18.461988	1117.325886	11.811085
18.821159	1126.146104	11.816090
18.386230	1121.161174	11.821095
18.364355	1124.106091	11.826099
18.645426	1130.423346	11.831104
18.480930	1127.518011	11.836109
18.894847	1131.069977	11.841114
18.725476	1131.851029	11.846119
18.939525	1131.213064	11.851123
18.848187	1132.133067	11.856128
18.878053	1130.663401	11.861133
19.136405	1130.715434	11.866138
18.921813	1132.197609	11.871143
19.160709	1128.436238	11.876147
19.195622	1129.184704	11.881152
19.330990	1120.759110	11.886157
18.972449	1124.566765	11.891162
19.234490	1125.193839	11.896167
19.161843	1122.453639	11.901171
18.898093	1125.668967	11.906176
19.053952	1123.187230	11.911181
19.356539	1130.198117	11.916186
19.389538	1157.274501	11.921191
19.864442	1151.038903	11.926195
19.580292	1153.101498	11.931200
19.478506	1134.093731	11.936205
19.854617	1144.377933	11.941210
19.643069	1147.411462	11.946215
20.036649	1147.257407	11.951219
19.873793	1135.698423	11.956224
19.650657	1124.231072	11.961229
20.097608	1133.223387	11.966234
19.701654	1150.557238	11.971239
20.047453	1147.584693	11.976243
19.879360	1153.825362	11.981248
19.958899	1156.009731	11.986253
19.942286	1158.379761	11.991258
19.710869	1171.788870	11.996263
19.833457	1162.999409	12.001267
19.754802	1177.992770	12.006272
19.998295	1170.967689	12.011277
20.286231	1164.422838	12.016282
19.770719	1168.086797	12.021287
19.999932	1172.833693	12.026291
20.419170	1184.360087	12.031296
20.518949	1185.470398	12.036301
20.535559	1167.095034	12.041306
20.182902	1165.681651	12.046311
20.214950	1162.140939	12.051315
20.281619	1171.493581	12.056320
20.410613	1167.793889	12.061325
20.366167	1166.714572	12.066330
20.140520	1165.214692	12.071335
20.560592	1165.613118	12.076339
20.355325	1165.292792	12.081344
20.459578	1164.555636	12.086349
20.549399	1161.024632	12.091354
20.494524	1170.814587	12.096359
20.342665	1158.623001	12.101363
20.492755	1162.417348	12.106368
20.323874	1162.453944	12.111373
20.552313	1160.977835	12.116378
20.419941	1175.979762	12.121383
20.325377	1162.056870	12.126387
20.372010	1163.543115	12.131392
19.953176	1146.494162	12.136397
20.215057	1151.067094	12.141402
20.203304	1163.335629	12.146407
20.463693	1161.537431	12.151411
20.421856	1161.437059	12.156416
20.217581	1160.846896	12.161421
20.280763	1144.657839	12.166426
20.461362	1136.751762	12.171431
20.394283	1136.671188	12.176435
20.410592	1138.480835	12.181440
19.931599	1132.435253	12.186445
19.929720	1126.043889	12.191450
20.145363	1137.788816	12.196455
20.793600	1140.199459	12.201459
20.172459	1138.679084	12.206464
20.390984	1138.658616	12.211469
20.594723	1128.984111	12.216474
20.205106	1130.550979	12.221479
20.361087	1137.749271	12.226483
19.984540	1138.009819	12.231488
20.465705	1145.717681	12.236493
20.301303	1141.433968	12.241498
20.238361	1140.018533	12.246503
20.156372	1135.403107	12.251507
20.488393	1144.675556	12.256512
20.465649	1144.004394	12.261517
20.543244	1149.133462	12.266522
20.209773	1148.243763	12.271527
20.374923	1139.084801	12.276531
20.470622	1137.743415	12.281536
20.382964	1136.786119	12.286541
20.479133	1137.199938	12.291546
20.098410	1141.320241	12.296551
20.543727	1131.827990	12.301555
20.539039	1143.256380	12.306560
20.234046	1134.976720	12.311565
20.431774	1125.777875	12.316570
20.139338	1130.530691	12.321575
20.098048	1118.502865	12.326579
20.285515	1135.948654	12.331584
20.417063	1139.476273	12.336589
20.229617	1131.884392	12.341594
19.981018	1133.102313	12.346599
20.364893	1139.023101	12.351603
20.148186	1138.773991	12.356608
20.018044	1154.097263	12.361613
20.484886	1151.449211	12.366618
20.220358	1155.839588	12.371623
20.507751	1147.651523	12.376627
20.436146	1138.399430	12.381632
20.378762	1133.494630	12.386637
20.287031	1120.211617	12.391642
19.899708	1124.468596	12.396647
20.138409	1127.170084	12.401651
20.121465	1142.372777	12.406656
20.534205	1147.714910	12.411661
20.283770	1141.850502	12.416666
19.934676	1139.971318	12.421671
20.132487	1149.142166	12.426675
20.467296	1154.190781	12.431680
20.634728	1152.670783	12.436685
20.520250	1125.765503	12.441690
20.252018	1124.669841	12.446695
20.384848	1113.926366	12.451699
20.516804	1119.303815	12.456704
20.243657	1123.189318	12.461709
20.236994	1117.882167	12.466714
20.468405	1120.532773	12.471719
20.448712	1122.638342	12.476723
20.396295	1126.236306	12.481728
20.235731	1118.603871	12.486733
20.674443	1120.354023	12.491738
20.538250	1128.814836	12.496743
20.644324	1117.921073	12.501747
20.217088	1122.231730	12.506752
20.082860	1126.483034	12.511757
20.233399	1113.568265	12.516762
19.999918	1125.171918	12.521767
20.183262	1125.436203	12.526771
20.261400	1124.810456	12.531776
20.520989	1131.623184	12.536781
20.705875	1117.222065	12.541786
20.203381	1111.024111	12.546791
19.935179	1103.719536	12.551795
20.680237	1108.625419	12.556800
20.096438	1115.878622	12.561805
20.200642	1105.351046	12.566810
20.111129	1110.902600	12.571815
20.376834	1117.078789	12.576819
20.519562	1127.095832	12.581824
20.192950	1114.580473	12.586829
20.373336	1097.133198	12.591834
19.996365	1110.365181	12.596839
20.144009	1105.534927	12.601843
20.320751	1119.501823	12.606848
20.223225	1121.164034	12.611853
20.444670	1116.721002	12.616858
20.114731	1115.412818	12.621863
20.283285	1119.590590	12.626867
20.194650	1115.179672	12.631872
20.337149	1120.612215	12.636877
20.885353	1114.292394	12.641882
20.638399	1105.618689	12.646887
20.010196	1095.070743	12.651891
20.264699	1097.258736	12.656896
20.522154	1098.673496	12.661901
20.530618	1100.039658	12.666906
20.262945	1098.097025	12.671911
20.511084	1084.034381	12.676915
20.256115	1097.369902	12.681920
19.835650	1098.821830	12.686925
20.478456	1097.126655	12.691930
20.283511	1110.761718	12.696935
20.244415	1101.575431	12.701939
20.099526	1104.716598	12.706944
20.043298	1102.992567	12.711949
20.361895	1100.544803	12.716954
20.142732	1104.017961	12.721959
20.134663	1099.608391	12.726963
19.977806	1106.088538	12.731968
20.044802	1111.246095	12.736973
20.561644	1100.655855	12.741978
20.366477	1103.529055	12.746983
20.408687	1098.154186	12.751987
20.387693	1110.860998	12.756992
20.071976	1111.431987	12.761997
20.409849	1108.137416	12.767002
20.355026	1109.217185	12.772007
20.644957	1097.183855	12.777011
20.481998	1101.810345	12.782016
20.529672	1109.117369	12.787021
20.629364	1098.029082	12.792026
20.312457	1106.567597	12.797031
20.176054	1106.715716	12.802035
20.301936	1100.333948	12.807040
20.407186	1099.319073	12.812045
20.388733	1079.817078	12.817050
20.005636	1078.903758	12.822055
20.066476	1079.826293	12.827059
20.225836	1101.633952	12.832064
20.243872	1108.224984	12.837069
20.563524	1110.344235	12.842074
20.464073	1106.293040	12.847079
20.519607	1084.427832	12.852083
20.273084	1080.034225	12.857088
20.115437	1076.613684	12.862093
20.464758	1074.470128	12.867098
20.365202	1081.674458	12.872103
20.263327	1078.830111	12.877107
20.183398	1080.957899	12.882112
19.871798	1083.922212	12.887117
20.498145	1084.970601	12.892122
20.097493	1085.995137	12.897127
20.064588	1084.690042	12.902131
20.277611	1093.006814	12.907136
20.220946	1095.643439	12.912141
20.369802	1091.443822	12.917146
20.092217	1092.191667	12.922151
20.287080	1088.565073	12.927155
20.117066	1091.552538	12.932160
20.038860	1094.768227	12.937165
20.518125	1097.956499	12.942170
20.178394	1100.387524	12.947175
20.498909	1086.403226	12.952179
20.064716	1096.324604	12.957184
20.325470	1093.972806	12.962189
20.580385	1085.671675	12.967194
20.100018	1092.804282	12.972199
20.080994	1088.964206	12.977203
20.209575	1088.357223	12.982208
19.941201	1096.110498	12.987213
20.259057	1093.550881	12.992218
20.271061	1112.981769	12.997223
20.334330	1115.156111	13.002227
20.674407	1107.289271	13.007232
20.234231	1107.780757	13.012237
20.505223	1092.383415	13.017242
20.253986	1100.062990	13.022247
20.211882	1090.503425	13.027251
20.314586	1094.578145	13.032256
20.006074	1092.864393	13.037261
20.574631	1086.530299	13.042266
20.137609	1088.407521	13.047271
20.131968	1097.580826	13.052275
20.158407	1097.605191	13.057280
20.414396	1100.007428	13.062285
20.365524	1093.303430	13.067290
20.107345	1097.938799	13.072295
20.018268	1094.198211	13.077299
20.238242	1091.983815	13.082304
20.162746	1099.725250	13.087309
20.364481	1093.085363	13.092314
20.381645	1098.531581	13.097319
20.183722	1094.483480	13.102323
20.284621	1100.061432	13.107328
19.914309	1098.272377	13.112333
20.343024	1092.971485	13.117338
19.805370	1103.059192	13.122343
20.372615	1112.275174	13.127347
20.530296	1111.966346	13.132352
20.326796	1110.202723	13.137357
20.416028	1097.699900	13.142362
20.313288	1098.631182	13.147367
20.371798	1090.754067	13.152371
20.441400	1090.730544	13.157376
20.166075	1100.383715	13.162381
20.496328	1087.673708	13.167386
20.296185	1101.785866	13.172391
20.513241	1100.292653	13.177395
20.693833	1099.795653	13.182400
20.293824	1102.311993	13.187405
20.361244	1094.496537	13.192410
20.397644	1102.857259	13.197415
20.340325	1104.017856	13.202419
20.321981	1097.914580	13.207424
20.201897	1101.698386	13.212429
20.870145	1100.913850	13.217434
20.445379	1096.550247	13.222439
20.225563	1078.818300	13.227443
20.025134	1066.237120	13.232448
19.892926	1073.593321	13.237453
20.282170	1089.872961	13.242458
20.428549	1109.154667	13.247463
20.378192	1103.466532	13.252467
20.410843	1082.981755	13.257472
20.128968	1082.831358	13.262477
20.347646	1067.783032	13.267482
19.868205	1072.281788	13.272487
19.990796	1084.448397	13.277491
20.448493	1098.121280	13.282496
20.591907	1103.399117	13.287501
20.546652	1089.980975	13.292506
20.604646	1075.486590	13.297511
20.493684	1072.847135	13.302515
20.399852	1075.078071	13.307520
19.984631	1075.983497	13.312525
20.412553	1071.884462	13.317530
20.121055	1076.449440	13.322535
20.083067	1076.681215	13.327539
20.026103	1078.538816	13.332544
20.014384	1077.192492	13.337549
20.070555	1071.626158	13.342554
19.707030	1079.284207	13.347559
20.021967	1088.545151	13.352563
20.601130	1096.967537	13.357568
20.321816	1110.198135	13.362573
20.709923	1093.676587	13.367578
20.568984	1090.833738	13.372583
20.608472	1072.320793	13.377587
20.104873	1075.197451	13.382592
19.891758	1085.537752	13.387597
19.979087	1073.451597	13.392602
20.038040	1084.630077	13.397607
20.422659	1093.121341	13.402611
20.516267	1093.716929	13.407616
20.347330	1088.905638	13.412621
20.156855	1071.107515	13.417626
20.206049	1078.578296	13.422631
19.984222	1074.991362	13.427635
20.454107	1086.224151	13.432640
20.437622	1085.935219	13.437645
20.214259	1078.509956	13.442650
19.921779	1083.330577	13.447655
20.460326	1080.541781	13.452659
20.521186	1082.667613	13.457664
20.102921	1079.553590	13.462669
20.521669	1073.325405	13.467674
20.255071	1082.086132	13.472679
20.205191	1075.675636	13.477683
20.146470	1070.331071	13.482688
19.986689	1087.406386	13.487693
20.169746	1073.308398	13.492698
19.977298	1083.159665	13.497703
20.147683	1084.563079	13.502707
20.272640	1104.242461	13.507712
20.226954	1112.439651	13.512717
20.059010	1117.223071	13.517722
20.085423	1113.587067	13.522727
20.250325	1112.201528	13.527731
20.483967	1115.170344	13.532736
20.068412	1114.115532	13.537741
20.255306	1109.001452	13.542746
20.316758	1116.394598	13.547751
20.585415	1120.564287	13.552755
20.269983	1119.469847	13.557760
20.304965	1127.510664	13.562765
20.832044	1105.109704	13.567770
19.932146	1105.488428	13.572775
19.877607	1090.108319	13.577779
19.910317	1105.292014	13.582784
19.885205	1119.306878	13.587789
20.328762	1121.109877	13.592794
20.383122	1126.917630	13.597799
20.339160	1126.338169	13.602803
20.352144	1123.320939	13.607808
20.209813	1128.753183	13.612813
20.494406	1122.339780	13.617818
20.805847	1128.270541	13.622823
20.054795	1106.573387	13.627827
20.366676	1106.902330	13.632832
20.267179	1106.620331	13.637837
20.350290	1091.060558	13.642842
19.949565	1099.596668	13.647847
20.249555	1114.242539	13.652851
20.481465	1116.136072	13.657856
20.149503	1109.262742	13.662861
19.990557	1100.412564	13.667866
20.309388	1116.104180	13.672871
20.320854	1128.950920	13.677875
20.322720	1137.848643	13.682880
20.151815	1123.690365	13.687885
20.563087	1116.458762	13.692890
20.472761	1112.144316	13.697895
20.183115	1106.505389	13.702899
20.352810	1094.158480	13.707904
19.949391	1096.911922	13.712909
20.139505	1091.849378	13.717914
19.960908	1101.676368	13.722919
20.291263	1120.868815	13.727923
20.184115	1127.246418	13.732928
20.312044	1136.258082	13.737933
20.530134	1125.800641	13.742938
20.111424	1124.593355	13.747943
20.367239	1119.860968	13.752947
20.082517	1115.393013	13.757952
19.878753	1127.594368	13.762957
20.311914	1132.818112	13.767962
20.321014	1131.987318	13.772967
20.416524	1138.332600	13.777971
20.565836	1134.673833	13.782976
20.614505	1123.212016	13.787981
20.642182	1104.098475	13.792986
20.620820	1109.964034	13.797991
20.233699	1101.585522	13.802995
20.368964	1108.113697	13.808000
20.292722	1105.886620	13.813005
20.318638	1104.237801	13.818010
19.758165	1108.211714	13.823015
19.660241	1095.681971	13.828019
20.202168	1102.566353	13.833024
19.917906	1103.567594	13.838029
20.351878	1107.562665	13.843034
19.734675	1117.344504	13.848039
20.007204	1127.974824	13.853043
20.689938	1132.367070	13.858048
20.524075	1142.627328	13.863053
20.550770	1120.069602	13.868058
20.056702	1117.136409	13.873063
20.377613	1109.949187	13.878067
20.390815	1105.369053	13.883072
20.078678	1115.313555	13.888077
20.194812	1103.971887	13.893082
19.941933	1109.210431	13.898087
20.339124	1118.379421	13.903091
20.636074	1125.302890	13.908096
20.547580	1118.214087	13.913101
20.213326	1107.414226	13.918106
20.106324	1114.804277	13.923111
20.403530	1107.775390	13.928115
20.217437	1106.764406	13.933120
20.179577	1117.900002	13.938125
20.542788	1107.040930	13.943130
20.262229	1113.526619	13.948135
20.098575	1106.878773	13.953139
20.301766	1107.896884	13.958144
20.331701	1108.789655	13.963149
20.131815	1107.716212	13.968154
20.015862	1105.239985	13.973159
20.536078	1110.497147	13.978163
20.353781	1103.735573	13.983168
20.188671	1114.088738	13.988173
20.440739	1110.101327	13.993178
20.117743	1115.535575	13.998183
20.194879	1106.562573	14.003187
20.165635	1116.974498	14.008192
20.336766	1107.687465	14.013210
20.312942	1102.602667	14.018227
20.156509	1111.499780	14.023245
20.319113	1114.200124	14.028263
20.385133	1113.195626	14.033280
19.938629	1113.916712	14.038298
20.390675	1108.527914	14.043315
20.272970	1114.090292	14.048333
20.314717	1116.655756	14.053351
20.356791	1117.495539	14.058368
20.359960	1134.237150	14.063386
20.710586	1126.320908	14.068403
20.358294	1124.502229	14.073421
20.375000	1130.571716	14.078439
20.548684	1128.783970	14.083456
20.420579	1147.643406	14.088474
20.648766	1143.218402	14.093491
20.746937	1140.236172	14.098509
20.354804	1128.678826	14.103527
20.599364	1137.571767	14.108544
20.656831	1139.686410	14.113562
21.023060	1135.189051	14.118579
20.386741	1128.333166	14.123597
20.220596	1122.427911	14.128615
20.753336	1136.212672	14.133632
20.454759	1146.479008	14.138650
20.768181	1140.818150	14.143667
20.387474	1154.994031	14.148685
20.375053	1155.999813	14.153703
20.645342	1151.737980	14.158720
20.570294	1149.242708	14.163738
20.738892	1147.782965	14.168755
20.642419	1147.002588	14.173773
20.720029	1148.115133	14.178791
20.784615	1143.134198	14.183808
20.594851	1153.335990	14.188826
20.997578	1161.181235	14.193843
21.042673	1163.593588	14.198861
20.898839	1150.939528	14.203879
20.808970	1153.681725	14.208896
21.116252	1163.473899	14.213914
21.044602	1158.289744	14.218931
20.904161	1161.403383	14.223949
21.122086	1168.837657	14.228967
21.210166	1155.317603	14.233984
20.938903	1159.863135	14.239002
21.061702	1160.152061	14.244019
20.975637	1165.739299	14.249037
20.847599	1182.037845	14.254055
21.074651	1179.333929	14.259072
21.038252	1192.072212	14.264090
21.494390	1175.569125	14.269107
21.122357	1181.519741	14.274125
21.171183	1188.117393	14.279143
21.408780	1171.896140	14.284160
21.171237	1184.386498	14.289178
21.044230	1180.672530	14.294195
21.205769	1181.299775	14.299213
20.770808	1179.286633	14.304231
21.274689	1188.835103	14.309248
21.037021	1183.065503	14.314266
21.219292	1174.417878	14.319283
21.137886	1180.326855	14.324301
21.035200	1195.108096	14.329319
21.315667	1185.266585	14.334336
21.218042	1194.840219	14.339354
21.376163	1200.644927	14.344371
21.507821	1217.029505	14.349389
21.533489	1218.129892	14.354407
21.485357	1216.668532	14.359424
21.514897	1232.809863	14.364442
21.644333	1215.665126	14.369459
21.655299	1215.673012	14.374477
21.688005	1227.017587	14.379495
21.868581	1211.101120	14.384512
21.276282	1211.335797	14.389530
21.498339	1211.281696	14.394547
21.673994	1212.658611	14.399565
21.547087	1214.942676	14.404583
21.916752	1215.082112	14.409600
21.645347	1219.840046	14.414618
21.830458	1219.190932	14.419635
21.719816	1221.428358	14.424653
21.519580	1225.356953	14.429671
21.838032	1218.227603	14.434688
21.673756	1224.245771	14.439706
21.736170	1216.406915	14.444723
22.092502	1212.150216	14.449741
21.841249	1218.352146	14.454759
21.823635	1222.306667	14.459776
21.607501	1224.494853	14.464794
21.779074	1219.759526	14.469811
21.784836	1212.893991	14.474829
21.291699	1232.609303	14.479847
21.598294	1220.076820	14.484864
21.979242	1230.176619	14.489882
21.895807	1247.767469	14.494899
22.212085	1246.392700	14.499917
22.142611	1253.899603	14.504935
22.021637	1248.424401	14.509952
21.996701	1249.943431	14.514970
22.353056	1246.882242	14.519987
22.545926	1246.776167	14.525005
21.826718	1227.751697	14.530023
22.090494	1224.752473	14.535040
21.996635	1248.297430	14.540058
22.075830	1255.620168	14.545075
22.410043	1243.061237	14.550093
22.016882	1246.581729	14.555111
22.221687	1244.381583	14.560128
22.393610	1255.104638	14.565146
22.295063	1248.855060	14.570163
22.431508	1244.458817	14.575181
22.357656	1247.528818	14.580199
22.424107	1243.412733	14.585216
22.344500	1251.514294	14.590234
22.177618	1256.560741	14.595251
22.382697	1249.024734	14.600269
22.152780	1253.647071	14.605287
22.580572	1246.888811	14.610304
22.493444	1245.477714	14.615322
22.465041	1243.640390	14.620339
22.705751	1250.993992	14.625357
22.431922	1259.422273	14.630375
22.623772	1254.713588	14.635392
22.225440	1258.689522	14.640410
22.305080	1254.267729	14.645427
22.509492	1250.203569	14.650445
22.653505	1249.098529	14.655463
22.708239	1249.206401	14.660480
22.506249	1247.181257	14.665498
22.451934	1248.937785	14.670515
22.742937	1242.814839	14.675533
22.611397	1249.658371	14.680551
23.082286	1258.777986	14.685568
23.041188	1252.807112	14.690586
22.937425	1249.540886	14.695603
22.880392	1254.185985	14.700621
23.089812	1251.143514	14.705639
23.048893	1248.592444	14.710656
22.697770	1247.453124	14.715674
23.007027	1241.959636	14.720691
23.297097	1244.631808	14.725709
22.927481	1245.683562	14.730727
23.104618	1242.358373	14.735744
22.770032	1251.829840	14.740762
22.998884	1248.862923	14.745779
23.173370	1250.784307	14.750797
23.114622	1248.187316	14.755815
23.340445	1251.041200	14.760832
22.873141	1245.136741	14.765850
22.873666	1248.665223	14.770867
23.244659	1243.106830	14.775885
23.272776	1250.337037	14.780903
23.311343	1236.812221	14.785920
23.076750	1249.747340	14.790938
23.112040	1244.878010	14.795955
23.297487	1244.952448	14.800973
23.311633	1249.981028	14.805991
23.183553	1241.741526	14.811008
22.957900	1247.280274	14.816026
22.917233	1254.186392	14.821043
23.311922	1264.381554	14.826061
23.032588	1279.920958	14.831079
23.392841	1277.106113	14.836096
23.184413	1282.374706	14.841114
23.363149	1286.466242	14.846131
23.706175	1279.007318	14.851149
23.249025	1281.084516	14.856167
23.721159	1284.632164	14.861184
23.608577	1288.578255	14.866202
23.617495	1287.999715	14.871219
23.571278	1279.945339	14.876237
23.418938	1282.634602	14.881255
23.678738	1284.435414	14.886272
23.897579	1289.258320	14.891290
23.558231	1288.722747	14.896307
23.734135	1286.037982	14.901325
23.561893	1294.283334	14.906343
23.607799	1286.859216	14.911360
23.576804	1284.029697	14.916378
23.476841	1286.075089	14.921395
23.783795	1274.234651	14.926413
23.762804	1285.765593	14.931431
23.523182	1281.720342	14.936448
23.740264	1271.989560	14.941466
23.915787	1283.410501	14.946483
23.988140	1274.042585	14.951501
23.958613	1278.828025	14.956519
23.924554	1275.722138	14.961536
24.211184	1272.538357	14.966554
24.016031	1274.910397	14.971571
24.130972	1268.659791	14.976589
24.094167	1278.322881	14.981607
24.094403	1276.141203	14.986624
24.217874	1276.645534	14.991642
24.219512	1272.338427	14.996659
23.985595	1278.097160	15.001677
24.149148	1269.527972	15.006695
24.377457	1271.075823	15.011712
24.304572	1272.679583	15.016730
24.163682	1283.847395	15.021747
24.516657	1267.467630	15.026765
24.226167	1271.618278	15.031783
24.292543	1261.466366	15.036800
24.120774	1262.845220	15.041818
24.099426	1257.697050	15.046835
24.389680	1263.782735	15.051853
24.100504	1275.782747	15.056871
24.123607	1280.770583	15.061888
24.114948	1282.225670	15.066906
23.976801	1283.087918	15.071923
23.990260	1274.399520	15.076941
24.130759	1282.311829	15.081959
24.072688	1288.528593	15.086976
24.230060	1285.634420	15.091994
24.358604	1303.051521	15.097011
24.645295	1296.087651	15.102029
24.302049	1301.456409	15.107047
24.683594	1302.054858	15.112064
24.942498	1303.984806	15.117082
24.745746	1311.236755	15.122099
25.141139	1298.235425	15.127117
24.876671	1294.933474	15.132135
24.821676	1289.109524	15.137152
24.610560	1272.619952	15.142170
24.333764	1276.928869	15.147187
24.213813	1282.200653	15.152205
24.505131	1295.283163	15.157223
24.655247	1304.614427	15.162240
24.882637	1310.016437	15.167258
24.636425	1314.723192	15.172275
25.031300	1308.654438	15.177293
25.013861	1311.114544	15.182311
24.846429	1312.069556	15.187328
24.955545	1301.116400	15.192346
24.849183	1316.544881	15.197363
24.965960	1307.514358	15.202381
24.790450	1313.329857	15.207399
24.951778	1309.363791	15.212416
25.104377	1307.552645	15.217434
25.178390	1315.349731	15.222451
24.927438	1303.868828	15.227469
25.288232	1305.162737	15.232487
25.200262	1309.943352	15.237504
25.129326	1301.213343	15.242522
24.922243	1313.049276	15.247539
24.858656	1309.174144	15.252557
25.414232	1308.064801	15.257575
24.935876	1313.975799	15.262592
25.188682	1315.307384	15.267610
25.142147	1316.343788	15.272627
25.459963	1307.731094	15.277645
25.532712	1307.603280	15.282663
25.018273	1312.837323	15.287680
25.460975	1314.251877	15.292698
25.167413	1310.753210	15.297715
25.196333	1306.927819	15.302733
25.287253	1313.706008	15.307751
25.147138	1318.779668	15.312768
25.316059	1305.768838	15.317786
25.416848	1314.812240	15.322803
25.696113	1327.712654	15.327821
25.607631	1340.648143	15.332839
25.121133	1329.376256	15.337856
25.548445	1328.279505	15.342874
25.433910	1340.102272	15.347891
25.467180	1335.834146	15.352909
25.568901	1336.087112	15.357927
25.693650	1345.727623	15.362944
25.885964	1335.401410	15.367962
25.354734	1351.316134	15.372979
25.714811	1337.708479	15.377997
25.897619	1341.785224	15.383015
25.697393	1341.999834	15.388032
26.036146	1343.482884	15.393050
25.725589	1342.365401	15.398067
25.652734	1341.463265	15.403085
25.825255	1343.907233	15.408103
25.565335	1346.012756	15.413120
25.737838	1333.724941	15.418138
25.995496	1341.236339	15.423155
25.765729	1334.553038	15.428173
25.893838	1339.100989	15.433191
25.941274	1347.808420	15.438208
26.010107	1340.086453	15.443226
26.109244	1344.255199	15.448243
25.995739	1343.446066	15.453261
26.303951	1357.996758	15.458279
25.882208	1361.760943	15.463296
26.194866	1364.654482	15.468314
25.905792	1372.803680	15.473331
26.224829	1377.103318	15.478349
26.606276	1363.098176	15.483367
26.669030	1365.816067	15.488384
26.328026	1349.331396	15.493402
26.194083	1348.741034	15.498419
25.997409	1332.503927	15.503437
26.112998	1348.642672	15.508455
26.232393	1366.394799	15.513472
26.497044	1367.002459	15.518490
26.498569	1375.165868	15.523507
26.246839	1366.091054	15.528525
26.678220	1371.133350	15.533543
26.292576	1364.478045	15.538560
26.668235	1369.082477	15.543578
26.333477	1370.193174	15.548595
26.579574	1364.473755	15.553613
26.263250	1370.862313	15.558631
26.254721	1378.269893	15.563648
26.629539	1364.469520	15.568666
26.695888	1375.270068	15.573683
26.603903	1365.222784	15.578701
26.897638	1363.582605	15.583719
26.795923	1375.658193	15.588736
26.760269	1362.667360	15.593754
26.690073	1377.414502	15.598771
26.864421	1370.942798	15.603789
26.838496	1373.960349	15.608807
26.671859	1372.477763	15.613824
26.995194	1357.966714	15.618842
27.112971	1367.103396	15.623859
26.879683	1369.440634	15.628877
27.176658	1369.042665	15.633895
27.032417	1366.833681	15.638912
27.205473	1367.240441	15.643930
27.011088	1373.361004	15.648947
26.794389	1364.094194	15.653965
27.110478	1369.173757	15.658983
27.145759	1371.699398	15.664000
26.994686	1361.393332	15.669018
26.991366	1374.437967	15.674035
26.838642	1377.704626	15.679053
27.065381	1358.269538	15.684071
26.995467	1379.968037	15.689088
27.361654	1381.707846	15.694106
27.166684	1403.475093	15.699123
27.426668	1397.626026	15.704141
27.493241	1395.789264	15.709159
27.170054	1406.422301	15.714176
27.554459	1400.238772	15.719194
27.811890	1398.260664	15.724211
27.136246	1385.753365	15.729229
27.458962	1374.642597	15.734247
27.452900	1389.381880	15.739264
27.438644	1390.708879	15.744282
27.134112	1392.755455	15.749299
27.420914	1391.781790	15.754317
27.722693	1393.946378	15.759335
27.667856	1403.869625	15.764352
28.010372	1392.280617	15.769370
27.965405	1387.250217	15.774387
27.511652	1370.629345	15.779405
27.344129	1375.407727	15.784423
27.613137	1386.635294	15.789440
27.916662	1382.464837	15.794458
27.415305	1387.543444	15.799475
27.398192	1388.277850	15.804493
27.731394	1385.879444	15.809511
27.430563	1398.307719	15.814528
27.588310	1389.931302	15.819546
27.617674	1395.273693	15.824563
27.508614	1397.568311	15.829581
27.890353	1404.035091	15.834599
27.728097	1402.063363	15.839616
27.958698	1408.757180	15.844634
28.106940	1411.094130	15.849651
28.051006	1414.069284	15.854669
28.448516	1408.943128	15.859687
27.940498	1411.812635	15.864704
28.310020	1410.962632	15.869722
28.351684	1409.969077	15.874739
28.036201	1410.156454	15.879757
28.508092	1410.407006	15.884775
28.084696	1406.825202	15.889792
28.044657	1421.387461	15.894810
28.589748	1406.665594	15.899827
28.151337	1409.844905	15.904845
28.240455	1400.906829	15.909863
28.230171	1406.053408	15.914880
28.372157	1410.489053	15.919898
28.673542	1402.184102	15.924915
28.527601	1408.699660	15.929933
28.897042	1399.365288	15.934951
28.520423	1401.165379	15.939968
28.825030	1395.357962	15.944986
28.593488	1388.896722	15.950003
28.401042	1388.386478	15.955021
28.693835	1379.569301	15.960039
28.487581	1385.221414	15.965056
28.332838	1390.313950	15.970074
28.784547	1391.625613	15.975091
28.639823	1403.677409	15.980109
28.533095	1408.586108	15.985127
28.812621	1413.721071	15.990144
28.563700	1407.762046	15.995162
28.767449	1404.715730	16.000179
28.905827	1403.550228	16.005197
29.099520	1403.440875	16.010215
28.841747	1409.662802	16.015232
28.913611	1408.419031	16.020250
29.340157	1401.120548	16.025267
28.901201	1407.582167	16.030285
28.924348	1403.895315	16.035303
29.009717	1409.247655	16.040320
29.063384	1409.746608	16.045338
28.817594	1408.882278	16.050355
28.681011	1404.907861	16.055373
28.903621	1410.184040	16.060391
28.896857	1413.686983	16.065408
28.834191	1404.722777	16.070426
28.998876	1404.287705	16.075443
28.534485	1411.159236	16.080461
28.928959	1411.864958	16.085479
29.145723	1424.767562	16.090496
29.407906	1430.352051	16.095514
29.844475	1432.469976	16.100531
29.117342	1430.314632	16.105549
29.424318	1423.378928	16.110567
29.399362	1433.537323	16.115584
29.644086	1433.597588	16.120602
29.583068	1420.906486	16.125619
29.296921	1424.609731	16.130637
29.568458	1424.632684	16.135655
29.541224	1433.321401	16.140672
29.906402	1429.220537	16.145690
29.299984	1412.667227	16.150707
29.445201	1429.428994	16.155725
29.447122	1425.924066	16.160743
29.554309	1430.199308	16.165760
29.462616	1432.005866	16.170778
29.770668	1423.442642	16.175795
29.781315	1435.004050	16.180813
29.512469	1429.712821	16.185831
29.559763	1431.258101	16.190848
29.884948	1427.483738	16.195866
29.953832	1433.217042	16.200883
29.957256	1434.813367	16.205901
29.612454	1430.220116	16.210919
29.872011	1436.095259	16.215936
29.979608	1443.439516	16.220954
30.002741	1439.773894	16.225971
29.741294	1438.030348	16.230989
29.586284	1434.916191	16.236007
29.763103	1444.384076	16.241024
30.187967	1467.928448	16.246042
30.207583	1463.441445	16.251059
30.122077	1470.633254	16.256077
30.409720	1454.865404	16.261095
30.388541	1461.759861	16.266112
30.014337	1457.433995	16.271130
30.272097	1458.653901	16.276147
30.251720	1468.023476	16.281165
30.609454	1462.904433	16.286183
30.079204	1461.317810	16.291200
30.051557	1469.402552	16.296218
30.760853	1464.191250	16.301235
30.241166	1472.427626	16.306253
30.091901	1471.677675	16.311271
30.361933	1472.753261	16.316288
30.172302	1472.893820	16.321306
30.369517	1463.760705	16.326323
30.240796	1463.861661	16.331341
30.636084	1469.491003	16.336359
30.508558	1464.092273	16.341376
30.553848	1466.213625	16.346394
30.819728	1457.591824	16.351411
30.721888	1469.941374	16.356429
30.547790	1462.537315	16.361447
30.976364	1469.393070	16.366464
30.722501	1481.986963	16.371482
31.005461	1473.316023	16.376499
30.720310	1468.124911	16.381517
30.586369	1471.214769	16.386535
30.734542	1488.420528	16.391552
30.968743	1489.668577	16.396570
31.619571	1483.263186	16.401587
31.510534	1468.298731	16.406605
31.061273	1459.612455	16.411623
31.073010	1441.234054	16.416640
31.016863	1449.451537	16.421658
31.227184	1441.371882	16.426675
30.883104	1446.749477	16.431693
31.198672	1446.482252	16.436711
31.399953	1449.641336	16.441728
31.016476	1451.981307	16.446746
31.052786	1450.489150	16.451763
31.137953	1472.140241	16.456781
31.530981	1473.819149	16.461799
31.645448	1479.365082	16.466816
31.373992	1474.333811	16.471834
31.330760	1454.372202	16.476851
31.247856	1467.461075	16.481869
31.431553	1471.432319	16.486887
31.823869	1469.269873	16.491904
31.511542	1475.734919	16.496922
31.661822	1460.229656	16.501939
31.478621	1459.234998	16.506957
31.729878	1464.162122	16.511975
31.595375	1450.882585	16.516992
31.290708	1458.040130	16.522010
31.721020	1467.186801	16.527027
31.636932	1473.459705	16.532045
31.759489	1477.818243	16.537063
31.679055	1482.244555	16.542080
31.553799	1494.313771	16.547098
31.801911	1480.635750	16.552115
31.724474	1486.670850	16.557133
31.584350	1495.437389	16.562151
32.028066	1487.966231	16.567168
31.689174	1485.479952	16.572186
32.266970	1477.807295	16.577203
32.022867	1481.757900	16.582221
32.011381	1481.345421	16.587239
31.812096	1491.191877	16.592256
31.574271	1497.931351	16.597274
31.718922	1482.345948	16.602291
31.891645	1488.185411	16.607309
32.034041	1505.535262	16.612327
32.009635	1512.399583	16.617344
32.114140	1512.131416	16.622362
32.499010	1511.414245	16.627379
32.489158	1517.135758	16.632397
32.142457	1517.869256	16.637415
32.162176	1515.686795	16.642432
31.898321	1521.275785	16.647450
32.287859	1511.025746	16.652467
32.456816	1517.652365	16.657485
32.196776	1526.069947	16.662503
32.445012	1514.666561	16.667520
32.292835	1515.863767	16.672538
32.241932	1524.745872	16.677555
32.245575	1539.540391	16.682573
32.252302	1544.742510	16.687591
32.551314	1544.964797	16.692608
32.693639	1552.583580	16.697626
33.077063	1546.679371	16.702643
32.714470	1554.270150	16.707661
32.712274	1555.773000	16.712679
33.029392	1543.323509	16.717696
32.636231	1557.869868	16.722714
32.968538	1548.235359	16.727731
32.843521	1553.791205	16.732749
32.873814	1550.347005	16.737767
33.192864	1539.891103	16.742784
32.908301	1547.333360	16.747802
33.400385	1545.302860	16.752819
33.050852	1536.794906	16.757837
33.023883	1545.081724	16.762855
33.566057	1539.728733	16.767872
33.405481	1541.350442	16.772890
33.537297	1536.604051	16.777907
32.923748	1533.290868	16.782925
33.060772	1542.792694	16.787943
33.316520	1538.459134	16.792960
33.122388	1539.264256	16.797978
33.240457	1528.285905	16.802995
33.337957	1531.251553	16.808013
33.126060	1536.833835	16.813031
33.437453	1529.370392	16.818048
33.173600	1534.952308	16.823066
33.501716	1539.049978	16.828083
33.374897	1546.106050	16.833101
33.040178	1540.981809	16.838119
33.418897	1538.517915	16.843136
33.192623	1543.743042	16.848154
33.531688	1553.391980	16.853171
33.811163	1561.080131	16.858189
33.547825	1567.110309	16.863207
33.768490	1563.045044	16.868224
33.675170	1573.463777	16.873242
33.972764	1565.998583	16.878259
34.017715	1564.945503	16.883277
33.646570	1569.500799	16.888295
33.976818	1564.219358	16.893312
33.967532	1569.084252	16.898330
34.234327	1561.546106	16.903347
34.367511	1558.416628	16.908365
34.054310	1540.366796	16.913383
34.126848	1527.035288	16.918400
34.272166	1526.432622	16.923418
34.118882	1526.845034	16.928435
33.958343	1530.869629	16.933453
33.994875	1535.192354	16.938471
34.179515	1524.210467	16.943488
34.161097	1556.441498	16.948506
34.245473	1558.384375	16.953523
34.322393	1553.174021	16.958541
34.165772	1562.330998	16.963559
34.482397	1555.554149	16.968576
34.268669	1565.136319	16.973594
34.508636	1556.427354	16.978611
34.795980	1562.036197	16.983629
34.428796	1563.045896	16.988647
34.931396	1559.850415	16.993664
34.567492	1547.279878	16.998682
34.429691	1537.762834	17.003699
34.561417	1544.223937	17.008717
34.551123	1556.765672	17.013735
34.689488	1554.397532	17.018752
34.521858	1561.785750	17.023770
34.706406	1558.324809	17.028787
34.915789	1562.745032	17.033805
34.413706	1560.274544	17.038823
35.010611	1559.335567	17.043840
34.940791	1559.976136	17.048858
34.971318	1564.788273	17.053875
34.439378	1555.897253	17.058893
34.157607	1562.795569	17.063911
34.582511	1558.008714	17.068928
34.641321	1563.017694	17.073946
34.736171	1581.072886	17.078963
34.775593	1588.397416	17.083981
35.064197	1592.097118	17.088999
35.336204	1586.504834	17.094016
35.160176	1598.004908	17.099034
35.322469	1599.974691	17.104051
35.271028	1588.759053	17.109069
35.247792	1592.618612	17.114087
35.343734	1600.408422	17.119104
35.386174	1590.861808	17.124122
35.456826	1592.688897	17.129139
35.174503	1585.659915	17.134157
35.244544	1594.562885	17.139175
35.223963	1589.480546	17.144192
35.326901	1590.360987	17.149210
35.385355	1595.909607	17.154227
35.314159	1588.795036	17.159245
35.370685	1587.426276	17.164263
35.507876	1606.518494	17.169280
36.011158	1609.675848	17.174298
35.997692	1614.723904	17.179315
35.523262	1593.720275	17.184333
35.393454	1611.450314	17.189351
35.730742	1615.191023	17.194368
35.669203	1619.275360	17.199386
35.664742	1613.138825	17.204403
35.814985	1613.686091	17.209421
35.728316	1620.174984	17.214439
35.728072	1615.028828	17.219456
35.638147	1625.222103	17.224474
35.830377	1617.503117	17.229491
36.059154	1625.752334	17.234509
35.900714	1646.272941	17.239527
36.447617	1643.613095	17.244544
36.558796	1641.847056	17.249562
36.226879	1628.776606	17.254579
36.471039	1613.717909	17.259597
36.371010	1614.619715	17.264615
36.349184	1606.502276	17.269632
36.249439	1605.743632	17.274650
36.551409	1616.257440	17.279667
36.654142	1606.377927	17.284685
36.498118	1613.397788	17.289703
36.357135	1613.618683	17.294720
36.611087	1612.016286	17.299738
36.605289	1615.284732	17.304755
36.896234	1608.064408	17.309773
36.503352	1619.710779	17.314791
36.429054	1614.835209	17.319808
36.291133	1616.567363	17.324826
36.510459	1634.217357	17.329843
36.910275	1636.704563	17.334861
36.894273	1639.443720	17.339879
37.084402	1642.290791	17.344896
36.867629	1645.411989	17.349914
36.803671	1635.939734	17.354931
37.101090	1626.290289	17.359949
36.929569	1629.728323	17.364967
37.056456	1631.224749	17.369984
36.922679	1634.057413	17.375002
36.862062	1639.203451	17.380019
37.438072	1630.577701	17.385037
37.012849	1648.173212	17.390055
37.187606	1634.950362	17.395072
37.288218	1645.507321	17.400090
36.973189	1647.436050	17.405107
37.377279	1647.139759	17.410125
37.010385	1650.159055	17.415143
36.955853	1642.395254	17.420160
37.101867	1640.743215	17.425178
36.944195	1639.187594	17.430195
37.269707	1630.025259	17.435213
37.015459	1643.184881	17.440231
37.659340	1651.039123	17.445248
37.063230	1663.095488	17.450266
37.370535	1675.368791	17.455283
37.647057	1672.782744	17.460301
37.545954	1670.389857	17.465319
37.553240	1678.434535	17.470336
37.568388	1674.568769	17.475354
37.541587	1683.830177	17.480371
37.604810	1671.084432	17.485389
37.488260	1672.415188	17.490407
37.761782	1676.834654	17.495424
37.834256	1674.672856	17.500442
37.838205	1677.934255	17.505459
38.354885	1682.946539	17.510477
38.108793	1676.364789	17.515495
38.126514	1671.060010	17.520512
38.164935	1665.143140	17.525530
38.025683	1676.269304	17.530547
37.944565	1671.884825	17.535565
37.999426	1689.030983	17.540583
38.253596	1698.171288	17.545600
38.453839	1699.228921	17.550618
38.145907	1706.391040	17.555635
38.107527	1708.594990	17.560653
38.177811	1708.521838	17.565671
38.545585	1700.522324	17.570688
38.533968	1700.308858	17.575706
38.325417	1700.808746	17.580723
38.980177	1699.568721	17.585741
38.346134	1705.128734	17.590759
38.363935	1700.933759	17.595776
38.769596	1699.491994	17.600794
38.375958	1703.666294	17.605811
38.646589	1695.248887	17.610829
38.298847	1706.145620	17.615847
38.466452	1703.762567	17.620864
38.575512	1700.290037	17.625882
38.611314	1695.882182	17.630899
38.849546	1695.961575	17.635917
38.662378	1700.963431	17.640935
38.922819	1719.056880	17.645952
39.062520	1723.282189	17.650970
39.088508	1718.981291	17.655987
39.390164	1711.531107	17.661005
38.964773	1706.000463	17.666023
39.267765	1702.674761	17.671040
39.500771	1698.373884	17.676058
38.919961	1697.078455	17.681075
39.354352	1681.630678	17.686093
39.256925	1688.425713	17.691111
39.387344	1695.643757	17.696128
39.401665	1685.650084	17.701146
39.074226	1694.075366	17.706163
39.580986	1700.593129	17.711181
39.749887	1704.859396	17.716199
39.496778	1694.144630	17.721216
39.599123	1683.628018	17.726234
39.440234	1686.372671	17.731251
39.612808	1682.612361	17.736269
39.897138	1685.423179	17.741287
39.713494	1686.313943	17.746304
40.199526	1675.040824	17.751322
39.466656	1685.184103	17.756339
39.549478	1682.105893	17.761357
39.730558	1690.059145	17.766375
39.825482	1694.476428	17.771392
40.100257	1706.845400	17.776410
39.847889	1709.767785	17.781427
40.174912	1699.555116	17.786445
39.954423	1708.298419	17.791463
39.693820	1707.708580	17.796480
40.229523	1707.279605	17.801498
40.344879	1710.260532	17.806515
40.017527	1708.708372	17.811533
40.045251	1714.080245	17.816551
39.744456	1710.422962	17.821568
40.312281	1710.526867	17.826586
40.198984	1708.155583	17.831603
40.299541	1701.577520	17.836621
40.493530	1712.114128	17.841639
39.997184	1708.302410	17.846656
40.337280	1706.574572	17.851674
40.197778	1709.465583	17.856691
40.337607	1713.498163	17.861709
40.266956	1714.164828	17.866727
40.412686	1733.858353	17.871744
40.335177	1737.533902	17.876762
40.435233	1742.786490	17.881779
40.516269	1742.415091	17.886797
40.499665	1744.836595	17.891815
40.022581	1747.510097	17.896832
40.739166	1739.943377	17.901850
40.466932	1759.433815	17.906867
40.888897	1764.051439	17.911885
40.873996	1767.582508	17.916903
40.926786	1768.186226	17.921920
41.291529	1769.710797	17.926938
41.006646	1776.382395	17.931955
41.197292	1763.694113	17.936973
41.434765	1763.701265	17.941991
41.673740	1771.274860	17.947008
41.535281	1746.751061	17.952026
40.884978	1747.408719	17.957043
41.220355	1749.143263	17.962061
41.429632	1757.431061	17.967079
41.575104	1765.215418	17.972096
41.545273	1749.545869	17.977114
41.441969	1752.942376	17.982131
41.518887	1748.971565	17.987149
41.805050	1736.709330	17.992167
41.578609	1744.626934	17.997184
41.444398	1728.428187	18.002202
41.425451	1750.391257	18.007219
41.733485	1761.575137	18.012237
41.804811	1758.696170	18.017255
41.516533	1764.359937	18.022272
41.730258	1752.377459	18.027290
41.780514	1753.131026	18.032307
41.956685	1757.455140	18.037325
42.032020	1753.423229	18.042343
41.496583	1764.547369	18.047360
41.717218	1758.086202	18.052378
41.632828	1754.966217	18.057395
41.710764	1751.912368	18.062413
42.150920	1772.026984	18.067431
41.883643	1782.771718	18.072448
42.434915	1785.828644	18.077466
42.459758	1790.644908	18.082483
42.556805	1775.856490	18.087501
42.184649	1765.917327	18.092519
41.925532	1781.519324	18.097536
42.455042	1789.257383	18.102554
42.632713	1782.700806	18.107571
42.379748	1784.061196	18.112589
42.620181	1795.576800	18.117607
42.503142	1797.642291	18.122624
42.484298	1786.234887	18.127642
42.240040	1796.544926	18.132659
42.435464	1792.611046	18.137677
42.819511	1790.724383	18.142695
42.690717	1798.299233	18.147712
42.551174	1792.637226	18.152730
42.364491	1798.127491	18.157747
42.383030	1798.964775	18.162765
42.643934	1800.375344	18.167783
42.715859	1819.961987	18.172800
43.111706	1811.267336	18.177818
42.903749	1818.237374	18.182835
43.005038	1817.934320	18.187853
42.885606	1813.784012	18.192871
42.783346	1815.597808	18.197888
43.041444	1815.111644	18.202906
43.056217	1815.504337	18.207923
43.139602	1811.576525	18.212941
43.082654	1822.230321	18.217959
43.149326	1815.332763	18.222976
43.490289	1827.064393	18.227994
43.438601	1834.668650	18.233011
43.468802	1842.437613	18.238029
43.616466	1834.605278	18.243047
43.425145	1843.429744	18.248064
43.796390	1844.952501	18.253082
43.452006	1844.593109	18.258099
43.420790	1839.630363	18.263117
43.988216	1840.362010	18.268135
43.776214	1838.697836	18.273152
44.023078	1834.323918	18.278170
43.835586	1842.266039	18.283187
43.829184	1837.839703	18.288205
44.065166	1831.501906	18.293223
43.879242	1838.299328	18.298240
44.199890	1835.300350	18.303258
44.201490	1840.890380	18.308275
44.147597	1841.995639	18.313293
44.149948	1841.528243	18.318311
43.837463	1837.118480	18.323328
44.197659	1833.241684	18.328346
44.364998	1833.732746	18.333363
44.316439	1835.366509	18.338381
44.631976	1836.421495	18.343399
43.947070	1837.820895	18.348416
44.448447	1827.921695	18.353434
44.206314	1827.625437	18.358451
44.286127	1840.182147	18.363469
44.322861	1823.292170	18.368487
44.361925	1847.155115	18.373504
44.429332	1858.827364	18.378522
44.905014	1855.879949	18.383539
44.735495	1872.261392	18.388557
45.171117	1863.587109	18.393575
44.919409	1872.875858	18.398592
44.833323	1868.632121	18.403610
45.032645	1869.869250	18.408627
44.700765	1869.010756	18.413645
45.031852	1856.347974	18.418663
44.635601	1871.834291	18.423680
44.733194	1867.292252	18.428698
44.720950	1869.256876	18.433715
44.649537	1864.924277	18.438733
44.920090	1870.173313	18.443751
44.603250	1868.669798	18.448768
44.950255	1883.552267	18.453786
45.008717	1891.557437	18.458803
45.153951	1899.709230	18.463821
45.426081	1895.189683	18.468839
45.192485	1902.867826	18.473856
45.397040	1893.717541	18.478874
45.448643	1892.431340	18.483891
45.608829	1892.691509	18.488909
45.813701	1884.289988	18.493927
45.791328	1891.760603	18.498944
45.585200	1894.723629	18.503962
45.496008	1893.954633	18.508979
45.681766	1896.063082	18.513997
45.754340	1886.376179	18.519015
45.797368	1907.924521	18.524032
46.052310	1915.918816	18.529050
46.512324	1914.576909	18.534067
46.056727	1910.495137	18.539085
46.027557	1892.590698	18.544103
46.093987	1897.133718	18.549120
46.119976	1892.834342	18.554138
46.164066	1894.321978	18.559155
46.265086	1912.881572	18.564173
46.254338	1900.277209	18.569191
46.543469	1909.367237	18.574208
46.193902	1895.938327	18.579226
46.402015	1897.388789	18.584243
46.473015	1908.539012	18.589261
46.670816	1904.703045	18.594279
46.487457	1910.068543	18.599296
46.640425	1917.575703	18.604314
46.639185	1916.397822	18.609331
46.562066	1918.249309	18.614349
46.777128	1905.481500	18.619367
46.428939	1914.566213	18.624384
46.460490	1912.910376	18.629402
46.518986	1909.792737	18.634419
46.493974	1911.420393	18.639437
46.735291	1910.538114	18.644455
46.538179	1913.368349	18.649472
46.759363	1925.768867	18.654490
47.264534	1943.350048	18.659507
46.978731	1950.167386	18.664525
47.271248	1945.517148	18.669543
47.231147	1951.555923	18.674560
47.061120	1947.791199	18.679578
47.447299	1941.463221	18.684595
46.961246	1945.388828	18.689613
46.977133	1945.323565	18.694631
47.033766	1948.719777	18.699648
46.783445	1947.291379	18.704666
47.334316	1962.057250	18.709683
47.221107	1971.843892	18.714701
47.636400	1968.150195	18.719719
47.411485	1973.740225	18.724736
47.622443	1969.653586	18.729754
47.957832	1962.785462	18.734771
47.616519	1974.977632	18.739789
47.655030	1967.698288	18.744807
47.742685	1964.684533	18.749824
47.814395	1966.149680	18.754842
47.737038	1967.128907	18.759859
47.680432	1967.421296	18.764877
48.412892	1960.464669	18.769895
48.399863	1959.928932	18.774912
48.569045	1960.094066	18.779930
48.621096	1954.441551	18.784947
48.270462	1958.612208	18.789965
48.852940	1957.482016	18.794983
48.614657	1959.950713	18.800000
48.639175	1952.959919	18.805018
48.835458	1956.349590	18.810035
48.502862	1951.640957	18.815053
48.393769	1930.587218	18.820071
48.476443	1944.962889	18.825088
48.727712	1954.840833	18.830106
48.965434	1952.029676	18.835123
48.683665	1955.189622	18.840141
48.482928	1951.207196	18.845159
48.410827	1954.063906	18.850176
48.475477	1953.924794	18.855194
48.716537	1959.586796	18.860211
48.626980	1960.598644	18.865229
48.846799	1957.850907	18.870247
48.762985	1957.541979	18.875264
48.909113	1956.965125	18.880282
49.008227	1956.273064	18.885299
48.983330	1984.789545	18.890317
49.042609	1978.027592	18.895335
49.165825	1988.793569	18.900352
49.390590	1984.703151	18.905370
49.374996	1983.132697	18.910387
49.485705	1987.015044	18.915405
49.669778	1974.462919	18.920423
49.535305	1982.020678	18.925440
49.067716	1992.403444	18.930458
49.508116	1991.271528	18.935475
49.307498	1985.877182	18.940493
49.434299	1988.750154	18.945511
49.617406	1983.812167	18.950528
49.383484	1993.203556	18.955546
49.828503	1996.146906	18.960563
49.445414	2011.352825	18.965581
49.544138	2014.942914	18.970599
49.461686	2016.260396	18.975616
49.591333	2020.973497	18.980634
49.992404	2006.854492	18.985651
50.044141	2012.749647	18.990669
50.009746	2018.752144	18.995687
49.810993	2016.680751	19.000704
50.063962	2033.827180	19.005722
50.510565	2040.524594	19.010739
50.484796	2049.448630	19.015757
50.681238	2053.832526	19.020775
50.756434	2031.564669	19.025792
50.278569	2031.676481	19.030810
50.524257	2015.570201	19.035827
50.232172	2022.054281	19.040845
50.243282	2039.070180	19.045863
50.699219	2046.387499	19.050880
50.760328	2051.614162	19.055898
50.855472	2047.098415	19.060915
50.502851	2051.810577	19.065933
50.602421	2044.279979	19.070951
50.707832	2041.429342	19.075968
50.381788	2048.930382	19.080986
50.439843	2048.942556	19.086003
50.770471	2070.210867	19.091021
50.982406	2068.342970	19.096039
51.334607	2071.688921	19.101056
51.148531	2081.160831	19.106074
51.410870	2077.963448	19.111091
51.424709	2079.772917	19.116109
51.034991	2074.261610	19.121127
51.284772	2070.407870	19.126144
51.212024	2080.393427	19.131162
51.703802	2074.007648	19.136179
51.392286	2076.713791	19.141197
51.394202	2070.753812	19.146215
51.648642	2077.065795	19.151232
51.598962	2080.392472	19.156250
52.063672	2069.504729	19.161267
51.920723	2078.829748	19.166285
51.753617	2076.780042	19.171303
51.633398	2073.810432	19.176320
51.384235	2084.146625	19.181338
51.979665	2101.546849	19.186355
51.981900	2102.484286	19.191373
51.954712	2103.717450	19.196391
52.311308	2106.559300	19.201408
51.908476	2112.302825	19.206426
52.613960	2104.427781	19.211443
52.170817	2109.738825	19.216461
51.995145	2105.906528	19.221479
52.207586	2102.043004	19.226496
51.919932	2106.728303	19.231514
52.330165	2107.032758	19.236531
52.406380	2113.976488	19.241549
52.782562	2120.359529	19.246567
52.762521	2127.985635	19.251584
52.675165	2131.809943	19.256602
52.966158	2124.566549	19.261619
52.559762	2129.556322	19.266637
52.764227	2130.399366	19.271655
52.604793	2129.024885	19.276672
52.516012	2130.088535	19.281690
53.048838	2136.555933	19.286707
53.149459	2136.045323	19.291725
53.063052	2129.820172	19.296743
52.900172	2120.136060	19.301760
52.642646	2133.297430	19.306778
53.044739	2129.945601	19.311795
52.931156	2132.911218	19.316813
53.110684	2142.013369	19.321831
53.477413	2159.031680	19.326848
53.473093	2162.521041	19.331866
53.173853	2161.382805	19.336883
53.275679	2166.429181	19.341901
53.164534	2159.549596	19.346919
53.366409	2153.246205	19.351936
53.155720	2155.719972	19.356954
53.152327	2161.495768	19.361971
53.366198	2177.612678	19.366989
53.435721	2188.545469	19.372007
53.852890	2178.347194	19.377024
53.763780	2188.517920	19.382042
54.021307	2186.468116	19.387059
53.721797	2184.507946	19.392077
53.800793	2188.470131	19.397095
54.005847	2203.185217	19.402112
53.927780	2218.766667	19.407130
54.404268	2213.419195	19.412147
54.284676	2227.946966	19.417165
53.971503	2215.932521	19.422183
54.073369	2211.076635	19.427200
54.126271	2220.129812	19.432218
54.361309	2216.480537	19.437235
54.720852	2216.096955	19.442253
54.374175	2214.247346	19.447271
54.961076	2212.605940	19.452288
54.821405	2219.420545	19.457306
55.374308	2213.935818	19.462323
55.191823	2214.268741	19.467341
55.017044	2212.766913	19.472359
54.986516	2210.447631	19.477376
55.128587	2206.186282	19.482394
55.207011	2208.556524	19.487411
55.137870	2210.612859	19.492429
55.105399	2210.008634	19.497447
55.327984	2208.005302	19.502464
54.906818	2209.529422	19.507482
55.127380	2211.822719	19.512499
55.014648	2207.344798	19.517517
55.264771	2231.279323	19.522535
55.607721	2230.205409	19.527552
55.358643	2225.639108	19.532570
55.270355	2243.174511	19.537587
55.180239	2238.876247	19.542605
55.359226	2238.960376	19.547623
55.641740	2231.041034	19.552640
55.459740	2234.329857	19.557658
55.443597	2231.128091	19.562675
55.810701	2237.746247	19.567693
55.677810	2260.120762	19.572711
55.922448	2259.152197	19.577728
56.431004	2264.276893	19.582746
55.921929	2258.746795	19.587763
56.215025	2258.170873	19.592781
56.204276	2270.170550	19.597799
56.461955	2259.285799	19.602816
56.183767	2270.527390	19.607834
56.365300	2263.067772	19.612851
56.575774	2257.275031	19.617869
56.343284	2264.478088	19.622887
56.456367	2256.162574	19.627904
56.306832	2268.078198	19.632922
56.169133	2262.060964	19.637939
56.379009	2259.634110	19.642957
56.259034	2261.208519	19.647975
56.884921	2268.172413	19.652992
56.976209	2283.037872	19.658010
57.051269	2292.965389	19.663027
57.111550	2289.611409	19.668045
56.816303	2298.402383	19.673063
57.147463	2290.594811	19.678080
57.197075	2291.102308	19.683098
56.998879	2289.402055	19.688115
57.200887	2290.287190	19.693133
56.963608	2285.061403	19.698151
57.291690	2284.378429	19.703168
57.262630	2294.597073	19.708186
57.168816	2282.365884	19.713203
57.258527	2281.168748	19.718221
57.170735	2291.799488	19.723239
57.492369	2293.505617	19.728256
57.469439	2312.890168	19.733274
57.627836	2318.342104	19.738291
57.986370	2318.270170	19.743309
57.907003	2318.596087	19.748327
58.259940	2314.703020	19.753344
57.980244	2322.074098	19.758362
58.137245	2314.878726	19.763379
58.057383	2312.263674	19.768397
57.985470	2313.598379	19.773415
58.317102	2317.381078	19.778432
58.160296	2324.318812	19.783450
58.134983	2316.557071	19.788467
58.128569	2304.766571	19.793485
57.993590	2317.999019	19.798503
58.513235	2308.794286	19.803520
58.335962	2306.144430	19.808538
58.085171	2315.238239	19.813555
58.266164	2325.821414	19.818573
58.561419	2342.895390	19.823591
58.521982	2339.311101	19.828608
58.719182	2351.175422	19.833626
58.360780	2346.160858	19.838643
58.570691	2346.148026	19.843661
58.376804	2345.295808	19.848679
58.857677	2359.161593	19.853696
58.950605	2367.853726	19.858714
58.971942	2389.060138	19.863731
59.205260	2373.265356	19.868749
59.031274	2375.475303	19.873767
58.955567	2373.945071	19.878784
59.106719	2370.694568	19.883802
59.300144	2371.055635	19.888819
59.384380	2368.312929	19.893837
59.408147	2374.764878	19.898855
59.592147	2359.882555	19.903872
59.627846	2372.860505	19.908890
59.447109	2381.606520	19.913907
59.634448	2381.349512	19.918925
59.651315	2410.557868	19.923943
59.830499	2401.741682	19.928960
59.614319	2401.447563	19.933978
59.725673	2400.676444	19.938995
59.898140	2403.268483	19.944013
59.911586	2403.214619	19.949031
60.581605	2387.624690	19.954048
60.557573	2396.375611	19.959066
60.387023	2389.686308	19.964083
60.906677	2392.784595	19.969101
60.524276	2399.519223	19.974119
60.664907	2397.448705	19.979136
60.682296	2396.340967	19.984154
60.529695	2394.442288	19.989171
60.644558	2388.355615	19.994189
60.421524	2397.214575	19.999207
60.735685	2390.569884	20.004224
60.954049	2387.596549	20.009242
60.787449	2385.992715	20.014259
60.875130	2384.184714	20.019277
60.551560	2387.898097	20.024295
60.575804	2391.166645	20.029312
60.824711	2394.815467	20.034330
60.847477	2423.699619	20.039347
60.972866	2427.498725	20.044365
60.953242	2430.801808	20.049383
61.256625	2417.114886	20.054400
61.166369	2422.863736	20.059418
61.101986	2425.089247	20.064435
61.443859	2423.210021	20.069453
61.370994	2430.903704	20.074471
61.647277	2438.595193	20.079488
61.668001	2449.658672	20.084506
61.812682	2454.985419	20.089523
61.773822	2451.756551	20.094541
61.620215	2459.991720	20.099559
61.950146	2455.293666	20.104576
61.772288	2457.213203	20.109594
61.733526	2461.217055	20.114611
62.041340	2446.970916	20.119629
61.953057	2449.729619	20.124647
62.068626	2451.186247	20.129664
62.400828	2446.739544	20.134682
62.329082	2449.048038	20.139699
62.309669	2443.418532	20.144717
62.224380	2452.713354	20.149735
62.263277	2448.543117	20.154752
62.539215	2450.609734	20.159770
62.434288	2474.895475	20.164787
62.748385	2478.197257	20.169805
62.883756	2475.488852	20.174823
62.839026	2472.539371	20.179840
62.726170	2479.312849	20.184858
62.858935	2481.782232	20.189875
62.774980	2481.672323	20.194893
62.560373	2478.988273	20.199911
62.850300	2478.313738	20.204928
63.195961	2479.314414	20.209946
62.663890	2481.521708	20.214963
63.209128	2486.468369	20.219981
62.929354	2501.322439	20.224999
63.118875	2505.148306	20.230016
63.282998	2505.625748	20.235034
63.375518	2510.019278	20.240051
63.470698	2506.692720	20.245069
63.366730	2502.458728	20.250087
63.749339	2501.610517	20.255104
64.166115	2499.436946	20.260122
63.649610	2508.810806	20.265139
63.874139	2505.115155	20.270157
63.863042	2509.030442	20.275175
63.611672	2522.675723	20.280192
64.125179	2526.494758	20.285210
63.872627	2534.549886	20.290227
64.095863	2526.661865	20.295245
64.087423	2533.932364	20.300263
63.924758	2531.282496	20.305280
64.393479	2535.294313	20.310298
64.336677	2533.413373	20.315315
64.667631	2533.326960	20.320333
64.744698	2536.529693	20.325351
64.437348	2540.259406	20.330368
64.419429	2543.437961	20.335386
64.206746	2551.368749	20.340403
64.770349	2561.716447	20.345421
64.469045	2564.896942	20.350439
64.555519	2566.150559	20.355456
64.737095	2558.642014	20.360474
64.846577	2566.863599	20.365491
65.012878	2576.348059	20.370509
65.455113	2586.048881	20.375527
65.388680	2581.533569	20.380544
65.734017	2571.961602	20.385562
65.490989	2560.660142	20.390579
65.628698	2547.030987	20.395597
65.369517	2545.440327	20.400615
65.129295	2554.493268	20.405632
65.583330	2562.309072	20.410650
65.334959	2580.018291	20.415667
65.713433	2580.522903	20.420685
65.854375	2574.299058	20.425703
65.974496	2582.397031	20.430720
66.076385	2577.519782	20.435738
65.894687	2576.637288	20.440755
66.249407	2578.687426	20.445773
66.205881	2578.833006	20.450791
66.184871	2581.774508	20.455808
66.012623	2571.495346	20.460826
66.207551	2588.049149	20.465843
66.181800	2578.487594	20.470861
66.403865	2576.070545	20.475879
66.305077	2584.898790	20.480896
66.640702	2587.585975	20.485914
66.427620	2593.653392	20.490931
67.048070	2597.854196	20.495949
66.811848	2600.841826	20.500967
66.504539	2604.503901	20.505984
66.906983	2603.143589	20.511002
66.877842	2607.330012	20.516019
66.646600	2608.926136	20.521037
66.823095	2600.506708	20.526055
66.894965	2612.816783	20.531072
66.641373	2601.524056	20.536090
66.691639	2633.033848	20.541107
66.999441	2628.664924	20.546125
66.996364	2645.034057	20.551143
67.141033	2644.237947	20.556160
67.474017	2638.625315	20.561178
67.468257	2654.137487	20.566195
67.597218	2664.837759	20.571213
67.839933	2663.124560	20.576231
67.851728	2669.264693	20.581248
67.807877	2656.369193	20.586266
67.658313	2668.311103	20.591283
67.901243	2663.810926	20.596301
67.968379	2662.379805	20.601319
67.748855	2669.594365	20.606336
67.892432	2665.531654	20.611354
67.986172	2677.924036	20.616371
68.064316	2690.571417	20.621389
68.353497	2694.736199	20.626407
68.399219	2702.374141	20.631424
68.789277	2686.570541	20.636442
68.354630	2698.613795	20.641459
68.596770	2690.392296	20.646477
68.724608	2691.723494	20.651495
68.506832	2692.594587	20.656512
68.763086	2682.673344	20.661530
68.852336	2696.950382	20.666547
68.570957	2684.691348	20.671565
68.954487	2696.003925	20.676583
68.828041	2714.747915	20.681600
69.459677	2715.549609	20.686618
69.238046	2733.334196	20.691635
69.197198	2718.349715	20.696653
69.091520	2711.777348	20.701671
69.190369	2723.813407	20.706688
69.339716	2722.082843	20.711706
69.380466	2721.261613	20.716723
69.452852	2718.028315	20.721741
69.792164	2724.981504	20.726759
69.968121	2739.531080	20.731776
70.123884	2739.153245	20.736794
69.948414	2736.209617	20.741811
69.821128	2734.077951	20.746829
70.207878	2731.904417	20.751847
69.924818	2746.795443	20.756864
70.408422	2745.514995	20.761882
70.615514	2746.109090	20.766899
70.249412	2745.332297	20.771917
70.470294	2741.026760	20.776935
70.419002	2743.095268	20.781952
70.533963	2740.562337	20.786970
70.163225	2743.119149	20.791987
70.376095	2746.030462	20.797005
70.796220	2735.123383	20.802023
70.488382	2734.650368	20.807040
70.673538	2734.031863	20.812058
70.807815	2750.217165	20.817075
70.935223	2765.735748	20.822093
71.167230	2756.879460	20.827111
71.026492	2772.668935	20.832128
71.161563	2770.426198	20.837146
70.806806	2769.680631	20.842163
71.074545	2770.663080	20.847181
71.409440	2769.551084	20.852199
71.303465	2768.348935	20.857216
71.792335	2781.243172	20.862234
71.608594	2780.983987	20.867251
71.754698	2795.244186	20.872269
71.787534	2791.650619	20.877287
71.839099	2799.050123	20.882304
71.833095	2790.326169	20.887322
71.982850	2797.824857	20.892339
71.708521	2793.329265	20.897357
72.562238	2786.170425	20.902375
72.286778	2789.538778	20.907392
72.276719	2798.032849	20.912410
72.335006	2797.707530	20.917427
72.135088	2798.581287	20.922445
72.290428	2790.236707	20.927463
72.452101	2804.286766	20.932480
72.435325	2794.659137	20.937498
72.101609	2795.248241	20.942515
72.294137	2811.760991	20.947533
72.878938	2810.959964	20.952551
72.720391	2822.969509	20.957568
72.554266	2825.547191	20.962586
72.620506	2820.555195	20.967603
72.378470	2823.724718	20.972621
72.851964	2837.776207	20.977639
72.842742	2858.534298	20.982656
73.126291	2855.253132	20.987674
73.076228	2865.300895	20.992691
73.106019	2862.629710	20.997709
73.279076	2861.892778	21.002727
73.292078	2876.047640	21.007744
73.247643	2880.028913	21.012762
73.558015	2879.170178	21.017779
73.640401	2890.317763	21.022797
73.872422	2886.368318	21.027815
73.795438	2887.990212	21.032832
74.117635	2880.292313	21.037850
74.089999	2872.352872	21.042867
74.173088	2875.054431	21.047885
74.380792	2869.807804	21.052903
74.318521	2887.279259	21.057920
74.811452	2898.959202	21.062938
75.057205	2868.054910	21.067955
74.904141	2868.062212	21.072973
75.079126	2865.638466	21.077991
74.935939	2872.828364	21.083008
75.082560	2850.631250	21.088026
74.913752	2862.188586	21.093043
75.068700	2861.825038	21.098061
75.205205	2851.264383	21.103079
75.002610	2852.495693	21.108096
74.979901	2853.087900	21.113114
75.046717	2855.837675	21.118131
75.063685	2856.599756	21.123149
75.133048	2854.260506	21.128167
74.947803	2862.424644	21.133184
75.250780	2875.238487	21.138202
75.381557	2885.659383	21.143219
75.165618	2893.575929	21.148237
75.554046	2892.574953	21.153255
75.182238	2900.421968	21.158272
75.493399	2910.678814	21.163290
76.050674	2917.152893	21.168307
76.181870	2925.711823	21.173325
76.028997	2919.275895	21.178343
76.214216	2938.259939	21.183360
76.208777	2924.988364	21.188378
76.061373	2927.490708	21.193395
76.068348	2929.860664	21.198413
76.237042	2935.741472	21.203431
76.278882	2930.809967	21.208448
76.352003	2933.850587	21.213466
76.573296	2925.246052	21.218483
76.214784	2933.859492	21.223501
76.305182	2950.095278	21.228519
76.605838	2961.509381	21.233536
76.752735	2963.503834	21.238554
76.802239	2958.033834	21.243571
76.347441	2964.888031	21.248589
76.989890	2970.277171	21.253607
77.090791	2986.596277	21.258624
77.421644	2976.867461	21.263642
77.637108	2984.479265	21.268659
77.215095	2984.719038	21.273677
77.507543	2981.502502	21.278695
77.460846	2985.218286	21.283712
77.539768	2985.622018	21.288730
77.589098	2981.646622	21.293747
77.440092	2992.728142	21.298765
77.783380	2988.767217	21.303783
78.134559	3006.072972	21.308800
78.142423	3012.018006	21.313818
78.282107	3007.717475	21.318835
77.938196	3023.733133	21.323853
78.189082	3010.897293	21.328871
77.930587	3020.533962	21.333888
77.887219	3019.205386	21.338906
78.251325	3013.234455	21.343923
78.266166	3027.063507	21.348941
78.497550	3035.164439	21.353959
78.888339	3029.370957	21.358976
78.980903	3032.485585	21.363994
79.251482	3031.648922	21.369011
79.576794	3032.784253	21.374029
79.582260	3025.136794	21.379047
78.957303	3020.332844	21.384064
79.150441	3021.171457	21.389082
79.520713	3018.166690	21.394099
79.380482	3025.792767	21.399117
79.662647	3024.630167	21.404135
79.742478	3022.427667	21.409152
79.560903	3026.253075	21.414170
79.784043	3019.779945	21.419187
79.571990	3026.718955	21.424205
79.501769	3026.701245	21.429223
79.604999	3027.189204	21.434240
79.458736	3021.807041	21.439258
79.460566	3020.898393	21.444275
79.640533	3047.847209	21.449293
79.749972	3053.693464	21.454311
80.091345	3051.413849	21.459328
80.300786	3060.776111	21.464346
80.168643	3059.836125	21.469363
80.105486	3067.571858	21.474381
80.620399	3077.969384	21.479399
80.428912	3080.816249	21.484416
80.367919	3079.119977	21.489434
80.289084	3073.698722	21.494451
80.340176	3079.359209	21.499469
80.355727	3092.112889	21.504487
80.669830	3101.622890	21.509504
80.447118	3107.483596	21.514522
80.690052	3114.085774	21.519539
80.849444	3132.838201	21.524557
80.903135	3133.331705	21.529575
81.040406	3141.305326	21.534592
81.283582	3143.851609	21.539610
81.732525	3143.471058	21.544627
81.668457	3156.278397	21.549645
81.870009	3161.601840	21.554663
81.849708	3158.542128	21.559680
81.562016	3168.110393	21.564698
81.876719	3166.872583	21.569715
81.656801	3166.034691	21.574733
82.034839	3162.348220	21.579751
82.143535	3160.709831	21.584768
81.613708	3172.938562	21.589786
82.415172	3173.680951	21.594803
82.356266	3197.121998	21.599821
82.154019	3197.810503	21.604839
82.299963	3195.105787	21.609856
82.363952	3198.453132	21.614874
82.533587	3194.305884	21.619891
82.616628	3222.926345	21.624909
82.761845	3218.864794	21.629927
82.828638	3219.194164	21.634944
82.771336	3229.130842	21.639962
83.194778	3218.178041	21.644979
83.108890	3233.282755	21.649997
83.030478	3244.442096	21.655015
83.475614	3248.609699	21.660032
83.535778	3256.522523	21.665050
83.790459	3249.026353	21.670067
84.016972	3252.219569	21.675085
83.961659	3250.527877	21.680103
84.172611	3245.306559	21.685120
84.169588	3245.599080	21.690138
84.085905	3236.444373	21.695155
84.037714	3242.418893	21.700173
84.177220	3240.858965	21.705191
84.349804	3240.860742	21.710208
84.260203	3240.673063	21.715226
84.477361	3232.200377	21.720243
84.379894	3243.930708	21.725261
84.759259	3230.861008	21.730279
84.944172	3229.411049	21.735296
84.261032	3242.587012	21.740314
84.736491	3250.033988	21.745331
84.425408	3263.042863	21.750349
85.004283	3272.529627	21.755367
84.857298	3271.923169	21.760384
85.092044	3274.949096	21.765402
85.266942	3270.214941	21.770419
84.902274	3274.586435	21.775437
85.144256	3271.570612	21.780455
85.652137	3270.503364	21.785472
85.181704	3282.544933	21.790490
85.427581	3292.084033	21.795507
85.772976	3307.111387	21.800525
85.586698	3305.745006	21.805543
85.690140	3298.536456	21.810560
85.866460	3306.415836	21.815578
85.671621	3300.792738	21.820595
85.851995	3312.372616	21.825613
85.992339	3320.621169	21.830631
86.147425	3327.449848	21.835648
85.633809	3342.162706	21.840666
86.304276	3332.239470	21.845683
86.404755	3339.366348	21.850701
86.442393	3354.340570	21.855719
86.736262	3360.075723	21.860736
86.469836	3365.708296	21.865754
86.778948	3359.423474	21.870771
86.586429	3367.510387	21.875789
86.580967	3364.115515	21.880807
87.153599	3379.385174	21.885824
87.217766	3392.310717	21.890842
87.536266	3387.799842	21.895859
87.553114	3381.364174	21.900877
87.641257	3386.263693	21.905895
87.891200	3387.190027	21.910912
87.598959	3387.634873	21.915930
88.179175	3376.654592	21.920947
88.249172	3383.208169	21.925965
88.068904	3386.264909	21.930983
88.299132	3386.299972	21.936000
87.934796	3379.081029	21.941018
87.952962	3385.415534	21.946035
88.279544	3385.889124	21.951053
88.210935	3379.730611	21.956071
88.104683	3375.235564	21.961088
88.179604	3390.324233	21.966106
88.689306	3401.282914	21.971123
88.623992	3408.588876	21.976141
88.448104	3411.161923	21.981159
88.808091	3407.783489	21.986176
88.434398	3412.279178	21.991194
88.840846	3408.643181	21.996211
89.195116	3437.307335	22.001229
88.925290	3440.700895	22.006247
89.359585	3442.865119	22.011264
89.151476	3449.958668	22.016282
89.529463	3443.919273	22.021299
89.348581	3447.905154	22.026317
89.185917	3446.436662	22.031335
89.423814	3445.929289	22.036352
89.495337	3464.938443	22.041370
89.603067	3459.851508	22.046387
89.520545	3464.928522	22.051405
89.725876	3469.466400	22.056423
90.270848	3466.369964	22.061440
90.330501	3479.984621	22.066458
90.149986	3487.103679	22.071475
90.211220	3492.169575	22.076493
90.128119	3504.276201	22.081511
90.668464	3494.658377	22.086528
90.256168	3504.722655	22.091546
90.269796	3498.244184	22.096563
90.705065	3506.322302	22.101581
90.539346	3520.555062	22.106599
90.991313	3516.870087	22.111616
90.850448	3531.591337	22.116634
91.178487	3529.867580	22.121651
91.337314	3515.041595	22.126669
91.408149	3522.789238	22.131687
91.919748	3519.817685	22.136704
91.507071	3530.452363	22.141722
91.746428	3535.124073	22.146739
91.827452	3543.430198	22.151757
91.985922	3548.835387	22.156775
92.350185	3543.913614	22.161792
92.023876	3552.892790	22.166810
92.395275	3544.544004	22.171827
92.735324	3545.548016	22.176845
92.451208	3548.433342	22.181863
92.592820	3537.541772	22.186880
92.418894	3535.904363	22.191898
92.702584	3544.777597	22.196915
92.818425	3553.245732	22.201933
92.608351	3539.926784	22.206951
92.726939	3535.620024	22.211968
92.623748	3546.168384	22.216986
92.386687	3539.285416	22.222003
92.552533	3548.281284	22.227021
92.526940	3572.926703	22.232039
92.864778	3571.129794	22.237056
93.050361	3579.755166	22.242074
93.190769	3598.991864	22.247091
93.801104	3607.632897	22.252109
93.975290	3612.608448	22.257127
93.945312	3602.058859	22.262144
93.628575	3613.757589	22.267162
93.961895	3602.811797	22.272179
93.998011	3609.021603	22.277197
93.865197	3618.923388	22.282215
94.186439	3604.128836	22.287232
94.188022	3615.901093	22.292250
94.258097	3627.263600	22.297267
94.471838	3632.605725	22.302285
94.361651	3637.757223	22.307303
94.179871	3641.862871	22.312320
93.981424	3641.687825	22.317338
94.042169	3656.111156	22.322355
94.415694	3659.315630	22.327373
94.319455	3669.173855	22.332391
94.787042	3673.837531	22.337408
95.011716	3692.149960	22.342426
94.842260	3704.652839	22.347443
95.181160	3700.024552	22.352461
95.068220	3704.423677	22.357479
95.282835	3699.830157	22.362496
95.571584	3718.276359	22.367514
95.610745	3710.027666	22.372531
96.116117	3716.515891	22.377549
95.856211	3722.086200	22.382567
96.180451	3723.675664	22.387584
96.164147	3718.248130	22.392602
96.165257	3715.970763	22.397619
96.386083	3725.349729	22.402637
96.045177	3720.744105	22.407655
96.470321	3738.040506	22.412672
96.470910	3747.626103	22.417690
96.658408	3752.127580	22.422707
96.608606	3754.384005	22.427725
96.729800	3758.439793	22.432743
97.192225	3756.169088	22.437760
97.011407	3750.197448	22.442778
97.015701	3746.785986	22.447795
97.043100	3763.743078	22.452813
97.042020	3769.705579	22.457831
97.383280	3778.738906	22.462848
96.985634	3787.495175	22.467866
97.237519	3787.964959	22.472883
97.339556	3798.896129	22.477901
97.362143	3812.070179	22.482919
97.489486	3810.501119	22.487936
97.780397	3828.139207	22.492954
97.812181	3843.375249	22.497971
97.809759	3842.757510	22.502989
97.765749	3854.696136	22.508007
98.109243	3854.193936	22.513024
98.118796	3861.274209	22.518042
98.319936	3878.335885	22.523059
98.536811	3876.479565	22.528077
98.488448	3880.246974	22.533095
98.600443	3889.627668	22.538112
98.799874	3898.203819	22.543130
99.249187	3912.120176	22.548147
99.625584	3908.533692	22.553165
99.149956	3912.373969	22.558183
99.237393	3910.970957	22.563200
99.038559	3908.910315	22.568218
99.262134	3907.978836	22.573235
99.663291	3921.024955	22.578253
99.427472	3941.773514	22.583271
99.461870	3939.514404	22.588288
99.789035	3937.917396	22.593306
99.995529	3943.178977	22.598323
99.931366	3940.119017	22.603341
100.057284	3959.171269	22.608359
100.339684	3965.102013	22.613376
100.360739	3975.675705	22.618394
100.451287	3975.713381	22.623411
100.949942	3976.408141	22.628429
100.807643	3976.058934	22.633447
100.752479	3976.591854	22.638464
101.286347	3968.238160	22.643482
101.265158	3975.133802	22.648499
101.090000	3972.882932	22.653517
100.871332	3973.795932	22.658535
101.080744	3975.869449	22.663552
100.936486	3980.948619	22.668570
100.983691	3998.663539	22.673587
101.529625	3994.179932	22.678605
101.407254	4006.707812	22.683623
101.585001	4011.225871	22.688640
102.014949	4022.501399	22.693658
101.652873	4029.028983	22.698675
102.065208	4028.839912	22.703693
101.916735	4025.536136	22.708711
102.162106	4021.124055	22.713728
102.229592	4019.186913	22.718746
102.276806	4050.428047	22.723763
102.865915	4044.528596	22.728781
102.677002	4047.117202	22.733799
102.508790	4062.644183	22.738816
102.837796	4054.577211	22.743834
102.759899	4061.248292	22.748851
102.893938	4066.771637	22.753869
103.002375	4086.471920	22.758887
103.301814	4086.285120	22.763904
103.568803	4093.425144	22.768922
103.191973	4087.843353	22.773939
103.882439	4082.210142	22.778957
103.736582	4088.475919	22.783975
103.951249	4092.439012	22.788992
103.899775	4104.609529	22.794010
103.712606	4108.245729	22.799027
103.994071	4108.221491	22.804045
104.211991	4110.948192	22.809063
104.522963	4106.828497	22.814080
104.458849	4097.538755	22.819098
104.283065	4112.228393	22.824115
104.610749	4120.939198	22.829133
104.945327	4135.203686	22.834151
104.690904	4142.285285	22.839168
105.160015	4136.079248	22.844186
105.179624	4150.076161	22.849203
105.114712	4144.454831	22.854221
104.951671	4139.836441	22.859239
105.288041	4141.541234	22.864256
105.015794	4133.785657	22.869274
104.835882	4157.191677	22.874291
105.618040	4159.092852	22.879309
105.359508	4173.628970	22.884327
105.070276	4169.454719	22.889344
105.663896	4192.429053	22.894362
105.797812	4204.295532	22.899379
106.078329	4204.483852	22.904397
106.016412	4212.784044	22.909415
106.026049	4216.045888	22.914432
106.755974	4224.488854	22.919450
106.374888	4241.340143	22.924467
106.402317	4241.027582	22.929485
106.732991	4240.292983	22.934503
106.502736	4231.672378	22.939520
107.002016	4240.069534	22.944538
106.850742	4254.537491	22.949555
107.286620	4253.162268	22.954573
107.066960	4270.330843	22.959591
107.358010	4264.408037	22.964608
107.918898	4264.382507	22.969626
107.431018	4273.203012	22.974643
107.758068	4263.194684	22.979661
107.894084	4263.269165	22.984679
107.565719	4288.843588	22.989696
107.748201	4291.122839	22.994714
107.845357	4293.464473	22.999731
107.940876	4288.438990	23.004749
108.297126	4308.032395	23.009767
108.495915	4322.525621	23.014784
108.758037	4313.673040	23.019802
108.543635	4322.871629	23.024819
108.742390	4318.957792	23.029837
108.994254	4318.263292	23.034855
108.971865	4320.821455	23.039872
108.948402	4316.392371	23.044890
109.133961	4333.704871	23.049907
109.311428	4341.125196	23.054925
109.554547	4352.452014	23.059943
109.542437	4338.205510	23.064960
109.632623	4332.648269	23.069978
110.106748	4336.101968	23.074995
110.024802	4339.056687	23.080013
110.264665	4331.935227	23.085031
110.166957	4328.004944	23.090048
110.448327	4326.913178	23.095066
110.477692	4342.129668	23.100083
110.763513	4335.526391	23.105101
110.611920	4339.395342	23.110119
110.435749	4357.121143	23.115136
110.857020	4359.435487	23.120154
110.889287	4365.330761	23.125171
111.009319	4362.550510	23.130189
110.991149	4355.024920	23.135207
111.102115	4364.751442	23.140224
111.328024	4367.697979	23.145242
111.080397	4369.388156	23.150259
111.230371	4361.854627	23.155277
111.527307	4388.873003	23.160295
111.580298	4396.597992	23.165312
111.505362	4388.930391	23.170330
111.660854	4395.190721	23.175347
111.539242	4399.169765	23.180365
111.825377	4419.170996	23.185383
112.045061	4429.091058	23.190400
111.827716	4419.356677	23.195418
112.178859	4429.472904	23.200435
112.404391	4439.148163	23.205453
112.215595	4446.462531	23.210471
112.423460	4455.829086	23.215488
112.842407	4444.442626	23.220506
112.978561	4464.006829	23.225523
113.148358	4476.902320	23.230541
113.238748	4484.578122	23.235559
113.188869	4494.325661	23.240576
113.433604	4489.677532	23.245594
113.379146	4497.747765	23.250611
113.529993	4483.974689	23.255629
114.003180	4502.408199	23.260647
113.798872	4514.760767	23.265664
114.139589	4501.299613	23.270682
114.193638	4516.038750	23.275699
113.940850	4515.693774	23.280717
114.321073	4507.603441	23.285735
114.338732	4517.173443	23.290752
114.573094	4527.012560	23.295770
114.572831	4541.583376	23.300787
114.801498	4536.668742	23.305805
114.880880	4542.562867	23.310823
114.960886	4547.512062	23.315840
115.170687	4535.492545	23.320858
115.230878	4550.771992	23.325875
115.278285	4563.267762	23.330893
115.544886	4569.801530	23.335911
115.401976	4567.892363	23.340928
115.801833	4559.597473	23.345946
116.044103	4564.845707	23.350963
115.748248	4560.825808	23.355981
115.969106	4571.438082	23.360999
115.806841	4591.468573	23.366016
116.268139	4587.313760	23.371034
116.014706	4589.170095	23.376051
115.993077	4596.729293	23.381069
115.873094	4606.850758	23.386087
116.066629	4624.399914	23.391104
116.594399	4632.762859	23.396122
116.638994	4655.673640	23.401139
116.930104	4663.230987	23.406157
117.408336	4658.040501	23.411175
116.964322	4669.267877	23.416192
117.328255	4664.950773	23.421210
117.229724	4659.796407	23.426227
117.634384	4686.079094	23.431245
117.779258	4686.285121	23.436263
117.937314	4686.210548	23.441280
117.942027	4684.627125	23.446298
117.924657	4696.809212	23.451315
117.980484	4694.087914	23.456333
117.732852	4692.073490	23.461351
117.964690	4715.594103	23.466368
118.178936	4716.538807	23.471386
118.222351	4726.469086	23.476403
118.426559	4748.777894	23.481421
118.751994	4753.564504	23.486439
118.507813	4754.933980	23.491456
118.859741	4756.504199	23.496474
119.075945	4779.099865	23.501491
119.055927	4791.601861	23.506509
119.813603	4780.261040	23.511527
119.917459	4788.464315	23.516544
120.005708	4777.236546	23.521562
120.268132	4788.882390	23.526579
119.762680	4787.335470	23.531597
120.295207	4784.821354	23.536615
120.346839	4803.227276	23.541632
120.562594	4812.968066	23.546650
120.540913	4809.526670	23.551667
120.590053	4820.632247	23.556685
120.755162	4813.568108	23.561703
120.432987	4822.333403	23.566720
120.709042	4818.252124	23.571738
120.849034	4823.397179	23.576755
120.727039	4840.252673	23.581773
121.307477	4843.922411	23.586791
121.246328	4846.126528	23.591808
121.673185	4836.336341	23.596826
121.955722	4848.283487	23.601843
122.098024	4845.007893	23.606861
122.614885	4835.473199	23.611879
122.361256	4830.223138	23.616896
122.277691	4829.466460	23.621914
122.405964	4831.446047	23.626931
122.695243	4850.413612	23.631949
122.562081	4855.876018	23.636967
122.531529	4863.414747	23.641984
122.619067	4853.265631	23.647002
123.088590	4863.762936	23.652019
122.827500	4866.124816	23.657037
123.163403	4857.528418	23.662055
122.712090	4876.095668	23.667072
122.977675	4886.653047	23.672090
123.301205	4889.418911	23.677107
123.309885	4890.440465	23.682125
123.477466	4890.715253	23.687143
123.032831	4906.546034	23.692160
123.485795	4910.133057	23.697178
123.553611	4911.404802	23.702195
123.706765	4924.921706	23.707213
124.175970	4929.753893	23.712231
123.882844	4954.803821	23.717248
124.087353	4949.590013	23.722266
124.192164	4966.198638	23.727283
123.952262	4981.993704	23.732301
124.411429	4977.419011	23.737319
124.852175	4993.371460	23.742336
124.919920	5002.136045	23.747354
125.226769	5006.799039	23.752371
125.243839	5006.186010	23.757389
125.558577	4998.896519	23.762407
125.185606	5002.140878	23.767424
125.557269	5026.763141	23.772442
125.718982	5031.007931	23.777459
125.674254	5031.714665	23.782477
125.884936	5036.847736	23.787495
126.284006	5061.794541	23.792512
126.059813	5053.784564	23.797530
126.280346	5066.146943	23.802547
125.742839	5077.438313	23.807565
126.618072	5082.514202	23.812583
126.280594	5098.443749	23.817600
126.202955	5103.473341	23.822618
126.918207	5113.392725	23.827635
126.908363	5133.866179	23.832653
127.217742	5132.240417	23.837671
127.160872	5134.111103	23.842688
127.385261	5151.711826	23.847706
127.669684	5162.052406	23.852723
127.736470	5159.964961	23.857741
128.021928	5166.274915	23.862759
128.179972	5179.777112	23.867776
128.222191	5196.449476	23.872794
128.253156	5193.246633	23.877811
128.498794	5200.812296	23.882829
128.570948	5204.130476	23.887847
128.354971	5199.666527	23.892864
128.609034	5217.852652	23.897882
129.082047	5215.709073	23.902899
128.768875	5224.342569	23.907917
128.822900	5225.589791	23.912935
129.187921	5245.520560	23.917952
129.305113	5254.453639	23.922970
129.738876	5260.086200	23.927987
129.881378	5260.213940	23.933005
129.992097	5259.261828	23.938023
129.881265	5262.883775	23.943040
130.334533	5280.817136	23.948058
130.340722	5276.996697	23.953075
130.061326	5283.685513	23.958093
130.649372	5288.199905	23.963111
130.622403	5281.690934	23.968128
130.512704	5283.595240	23.973146
131.000537	5288.548882	23.978163
131.079842	5311.808395	23.983181
131.225506	5312.070165	23.988199
131.406298	5316.959488	23.993216
131.371681	5314.652954	23.998234
131.575565	5310.405246	24.003251
131.337313	5322.450775	24.008269
131.751973	5315.186106	24.013287
131.939889	5333.902177	24.018304
131.675703	5340.926895	24.023322
132.078180	5337.354011	24.028339
132.066060	5355.120932	24.033357
132.404687	5338.738939	24.038375
132.601362	5365.111079	24.043392
132.802921	5370.542326	24.048410
133.436551	5365.092366	24.053427
133.094642	5374.169537	24.058445
133.402788	5368.278973	24.063463
133.585001	5364.866300	24.068480
133.326696	5366.669221	24.073498
133.758638	5373.850441	24.078515
133.516037	5371.553462	24.083533
133.767104	5369.676559	24.088551
133.746828	5383.798229	24.093568
133.599414	5396.066930	24.098586
133.900273	5390.142116	24.103603
133.820012	5411.446978	24.108621
134.092256	5414.411515	24.113639
134.222830	5428.926151	24.118656
134.560157	5437.909994	24.123674
134.591398	5452.755982	24.128691
134.654328	5466.363299	24.133709
134.963196	5455.691474	24.138727
134.981024	5466.240787	24.143744
135.188536	5484.815455	24.148762
135.600927	5487.162871	24.153779
135.278000	5505.630184	24.158797
135.481255	5494.957864	24.163815
135.400750	5509.245822	24.168832
135.784709	5521.436972	24.173850
136.047687	5526.139386	24.178867
135.775952	5534.742850	24.183885
136.147444	5544.899089	24.188903
136.618517	5559.276159	24.193920
136.581973	5570.964791	24.198938
136.851819	5551.722642	24.203955
136.608677	5562.546519	24.208973
137.204558	5576.159428	24.213991
137.502379	5572.386031	24.219008
137.454601	5578.938913	24.224026
137.501970	5575.505210	24.229043
137.392124	5589.933248	24.234061
137.385434	5581.007126	24.239079
137.558622	5597.431683	24.244096
137.565324	5610.067792	24.249114
138.282187	5596.714820	24.254131
138.053174	5605.822121	24.259149
138.159216	5623.044963	24.264167
138.707689	5633.409857	24.269184
138.536311	5636.434954	24.274202
138.661652	5636.727509	24.279219
138.667912	5648.802759	24.284237
138.930654	5657.563387	24.289255
139.124004	5676.677916	24.294272
138.820563	5677.918452	24.299290
139.089104	5671.738260	24.304307
139.512605	5700.354877	24.309325
139.432655	5696.563800	24.314343
139.844650	5694.607696	24.319360
139.506447	5718.970598	24.324378
140.101376	5724.199991	24.329395
140.168174	5736.873831	24.334413
140.093704	5732.167646	24.339431
140.542443	5744.707418	24.344448
140.499326	5770.046150	24.349466
141.050066	5758.526738	24.354483
140.828291	5761.584287	24.359501
141.167115	5779.406689	24.364519
141.675980	5784.560135	24.369536
141.704947	5780.696595	24.374554
142.085100	5785.141229	24.379571
141.870712	5790.545334	24.384589
142.011027	5784.158166	24.389607
141.924352	5783.168262	24.394624
141.793658	5783.633039	24.399642
141.868989	5788.304878	24.404659
142.502994	5811.895286	24.409677
142.455188	5822.180735	24.414695
142.511858	5812.042966	24.419712
142.943555	5838.107035	24.424730
143.324900	5848.136816	24.429747
143.584707	5840.430816	24.434765
143.485959	5846.655204	24.439783
143.637625	5839.074238	24.444800
143.420276	5845.267183	24.449818
143.850348	5833.174515	24.454835
143.778192	5843.422161	24.459853
143.888083	5852.359128	24.464871
143.991170	5856.832230	24.469888
144.174475	5859.172966	24.474906
144.229453	5866.371267	24.479923
144.138420	5886.755640	24.484941
144.325471	5895.730683	24.489959
144.847983	5893.767159	24.494976
144.509145	5905.532583	24.499994
145.032946	5913.927583	24.505011
145.284998	5917.976478	24.510029
145.432926	5925.910575	24.515047
145.446288	5922.302829	24.520064
145.504134	5927.617939	24.525082
145.888417	5945.518266	24.530099
146.007349	5950.608066	24.535117
146.103945	5952.608592	24.540135
146.271004	5952.485375	24.545152
146.048897	5963.420273	24.550170
146.310058	5961.057031	24.555187
146.640797	5978.839265	24.560205
146.350701	5989.378256	24.565223
146.689471	5982.683197	24.570240
146.657609	6009.433606	24.575258
146.843595	6007.718066	24.580275
147.247913	6022.352498	24.585293
147.175570	6037.804891	24.590311
147.679301	6045.849114	24.595328
147.144498	6066.453987	24.600346
147.609134	6063.562607	24.605363
147.785702	6082.273568	24.610381
147.935429	6092.410473	24.615399
148.288800	6101.761955	24.620416
148.075203	6118.261356	24.625434
148.472262	6122.972480	24.630451
148.500819	6132.042177	24.635469
148.825692	6142.717677	24.640487
149.670863	6123.405078	24.645504
149.697407	6133.062042	24.650522
150.045744	6127.888620	24.655539
150.098802	6130.612879	24.660557
150.469820	6129.239186	24.665575
150.614483	6123.663935	24.670592
150.500567	6129.469926	24.675610
150.495542	6122.944497	24.680627
150.478354	6123.767270	24.685645
150.587256	6129.287532	24.690663
151.064448	6116.006148	24.695680
150.575096	6139.130256	24.700698
150.625820	6156.471118	24.705715
151.091872	6157.607084	24.710733
151.040166	6156.562011	24.715751
151.483890	6169.372029	24.720768
151.748710	6192.257155	24.725786
151.737202	6191.861855	24.730803
151.696738	6193.479857	24.735821
151.449173	6203.577908	24.740839
152.014551	6203.187394	24.745856
151.755611	6224.364556	24.750874
152.250200	6220.432948	24.755891
152.497911	6238.467133	24.760909
152.150635	6255.601704	24.765927
152.586006	6260.144683	24.770944
152.603559	6271.114762	24.775962
152.844036	6277.950869	24.780979
152.971793	6288.145701	24.785997
152.712564	6301.139524	24.791015
152.987502	6319.780023	24.796032
153.099952	6327.313216	24.801050
153.451761	6345.207403	24.806067
153.593283	6349.319678	24.811085
153.558017	6367.684752	24.816103
153.919754	6377.925737	24.821120
154.120557	6395.631628	24.826138
154.190063	6410.371762	24.831155
154.388180	6419.838685	24.836173
154.433632	6432.859573	24.841191
155.258401	6443.279334	24.846208
155.343849	6452.332287	24.851226
155.272984	6447.074533	24.856243
155.329746	6447.882384	24.861261
155.508912	6462.675111	24.866279
155.649738	6474.000990	24.871296
155.515223	6486.388915	24.876314
155.725572	6498.254494	24.881331
156.372641	6505.848090	24.886349
155.775210	6522.801761	24.891367
156.443324	6523.133677	24.896384
156.692775	6543.468592	24.901402
156.629723	6546.068242	24.906419
157.026824	6556.910345	24.911437
156.931624	6572.516433	24.916455
157.251025	6569.355424	24.921472
157.647721	6588.200300	24.926490
157.607113	6603.578195	24.931507
157.898493	6613.327000	24.936525
157.828666	6607.724398	24.941543
158.101660	6625.633066	24.946560
158.254099	6635.372568	24.951578
158.275958	6645.977941	24.956595
158.619425	6637.135403	24.961613
158.920077	6669.774452	24.966631
159.024479	6668.580132	24.971648
159.063318	6679.311860	24.976666
158.926598	6682.724263	24.981683
159.489165	6695.259285	24.986701
159.286517	6713.611348	24.991719
159.857609	6709.539164	24.996736
159.754426	6722.464409	25.001754
160.039939	6739.878668	25.006771
160.443703	6739.410055	25.011789
160.423660	6744.557696	25.016807
160.664711	6745.620221	25.021824
160.538905	6766.967335	25.026842
160.845669	6775.579194	25.031859
161.622353	6772.734705	25.036877
161.172316	6785.478478	25.041895
161.186043	6777.624758	25.046912
161.474453	6800.503913	25.051930
161.484080	6800.094998	25.056947
161.935463	6800.122359	25.061965
162.114255	6809.338469	25.066983
161.886290	6805.717059	25.072000
161.994323	6834.728442	25.077018
162.023261	6835.839746	25.082035
162.084247	6837.639922	25.087053
162.047994	6862.422348	25.092071
162.381288	6857.928535	25.097088
162.618783	6882.853036	25.102106
162.582363	6899.270758	25.107123
163.059616	6913.048599	25.112141
163.121313	6938.397001	25.117159
163.421323	6937.552298	25.122176
163.466366	6956.123245	25.127194
163.475104	6965.678940	25.132211
163.957969	6973.421708	25.137229
164.054181	6998.185598	25.142247
164.162232	7007.474484	25.147264
164.544626	7013.548675	25.152282
164.670688	7034.948072	25.157299
164.894139	7034.371293	25.162317
165.045168	7036.410498	25.167335
165.346330	7049.833355	25.172352
165.513908	7062.503274	25.177370
165.683902	7062.896537	25.182387
165.811487	7067.214238	25.187405
165.824561	7100.981207	25.192423
165.890777	7093.629612	25.197440
166.092499	7102.586917	25.202458
166.348263	7128.161209	25.207475
166.479555	7123.169194	25.212493
166.512294	7136.991371	25.217511
166.766315	7151.663476	25.222528
166.893476	7161.551347	25.227546
166.998767	7173.794593	25.232563
167.528696	7186.586242	25.237581
167.590969	7197.520760	25.242599
167.471632	7206.594236	25.247616
167.959687	7207.728356	25.252634
167.932711	7223.376965	25.257651
168.312677	7229.453994	25.262669
168.358891	7258.564974	25.267687
168.623703	7260.587641	25.272704
168.871355	7261.521682	25.277722
168.865437	7272.353822	25.282739
169.463091	7272.424747	25.287757
169.297385	7290.188571	25.292775
169.519053	7277.550420	25.297792
170.050002	7291.274415	25.302810
169.888188	7310.527154	25.307827
170.173426	7314.848903	25.312845
170.386742	7324.719211	25.317863
170.284135	7321.983354	25.322880
170.578419	7321.220590	25.327898
170.287873	7339.750315	25.332915
170.793753	7343.442030	25.337933
170.830807	7353.189385	25.342951
170.799494	7358.173009	25.347968
171.245893	7368.262695	25.352986
170.808217	7380.698127	25.358003
171.268389	7389.621084	25.363021
171.300848	7410.026407	25.368039
171.391505	7417.359832	25.373056
171.675101	7441.413160	25.378074
171.264562	7449.666096	25.383091
171.854783	7472.096862	25.388109
172.063916	7492.002796	25.393127
172.508306	7512.532211	25.398144
172.698403	7515.724303	25.403162
172.672626	7536.944047	25.408179
173.378194	7542.221766	25.413197
173.289341	7544.501515	25.418215
173.407071	7563.763513	25.423232
173.786305	7570.972313	25.428250
173.990097	7574.348722	25.433267
174.277240	7574.566734	25.438285
174.501677	7608.229545	25.443303
174.555533	7612.223168	25.448320
174.978751	7614.360690	25.453338
174.879146	7619.384403	25.458355
175.145707	7632.320724	25.463373
175.313838	7640.480709	25.468391
175.262832	7645.748481	25.473408
175.667042	7654.524721	25.478426
175.323870	7675.201968	25.483443
175.732718	7662.175621	25.488461
176.163870	7679.386779	25.493479
176.481761	7692.127692	25.498496
176.868256	7687.117618	25.503514
176.861816	7697.507927	25.508531
176.940718	7685.719200	25.513549
177.036472	7708.731191	25.518567
177.226848	7723.823184	25.523584
177.634180	7715.565494	25.528602
177.156799	7737.643618	25.533619
177.597088	7743.480687	25.538637
177.729086	7765.757553	25.543655
177.818088	7769.448962	25.548672
178.140405	7781.647088	25.553690
178.614968	7794.662908	25.558707
178.933899	7791.061856	25.563725
179.197474	7793.759150	25.568743
179.101856	7797.661772	25.573760
179.634772	7808.465041	25.578778
179.406295	7821.578819	25.583795
179.652836	7821.764753	25.588813
179.662143	7824.305087	25.593831
179.703092	7830.618190	25.598848
180.045047	7843.852705	25.603866
180.143836	7858.577013	25.608883
179.994491	7856.456769	25.613901
180.265941	7869.390943	25.618919
180.529891	7873.986153	25.623936
180.673533	7883.550040	25.628954
180.461404	7902.676219	25.633971
180.612952	7908.881228	25.638989
180.895167	7928.901995	25.644007
181.037718	7948.739680	25.649024
181.249198	7960.187230	25.654042
181.218564	7980.145423	25.659059
181.585091	7999.253821	25.664077
181.650396	8020.384187	25.669095
182.145561	8031.757838	25.674112
182.657828	8051.700384	25.679130
182.527480	8065.123715	25.684148
182.945544	8057.869776	25.689165
183.051202	8075.733691	25.694183
182.705485	8092.850440	25.699200
183.121330	8104.967033	25.704218
183.563423	8119.183609	25.709236
183.895979	8124.510393	25.714253
184.171305	8137.739662	25.719271
183.985088	8149.613134	25.724288
184.239100	8147.112202	25.729306
184.471428	8175.004324	25.734324
184.461595	8189.305615	25.739341
185.073508	8198.664023	25.744359
184.887463	8210.274691	25.749376
185.573789	8215.252768	25.754394
185.522599	8228.182040	25.759412
185.815025	8241.367756	25.764429
185.752071	8254.881234	25.769447
186.053464	8256.944635	25.774464
186.914150	8258.812629	25.779482
186.760988	8283.398473	25.784500
186.653748	8283.970142	25.789517
186.840517	8286.077398	25.794535
187.090697	8296.779739	25.799552
187.207760	8304.758981	25.804570
187.265316	8316.699949	25.809588
187.304094	8321.381169	25.814605
187.551405	8343.821893	25.819623
187.533328	8348.446479	25.824640
188.191595	8360.248423	25.829658
188.053212	8387.069655	25.834676
188.460663	8390.995698	25.839693
188.897140	8406.361153	25.844711
188.818776	8412.434631	25.849728
188.912790	8422.090189	25.854746
189.107387	8438.203250	25.859764
189.155100	8447.819780	25.864781
189.374654	8464.294016	25.869799
189.758210	8477.339898	25.874816
190.197817	8470.729171	25.879834
190.228334	8484.233855	25.884852
190.389647	8496.595948	25.889869
190.786142	8501.124578	25.894887
190.773962	8500.508988	25.899904
191.010621	8499.692404	25.904922
191.430022	8510.156238	25.909940
192.275286	8512.046400	25.914957
192.563334	8513.415544	25.919975
192.009065	8523.837903	25.924992
192.740520	8517.143638	25.930010
192.505612	8511.643364	25.935028
192.796577	8514.753097	25.940045
192.998263	8512.744009	25.945063
193.259046	8517.252576	25.950080
193.230599	8505.569241	25.955098
193.240829	8514.101518	25.960116
193.232832	8516.998448	25.965133
193.464799	8525.759782	25.970151
193.586788	8536.135705	25.975168
193.892661	8531.438812	25.980186
193.969882	8554.228034	25.985204
193.991182	8574.311334	25.990221
194.316328	8571.200540	25.995239
194.031349	8594.764457	26.000256
194.551492	8602.846024	26.005274
194.764491	8615.720130	26.010292
194.830686	8635.513457	26.015309
195.268701	8649.812638	26.020327
195.208627	8677.427712	26.025344
195.640667	8674.919951	26.030362
195.545681	8697.553494	26.035380
195.734533	8716.228035	26.040397
196.303796	8716.397940	26.045415
196.274371	8740.678757	26.050432
196.369926	8752.933508	26.055450
196.176457	8767.148557	26.060468
196.873792	8769.083194	26.065485
197.291703	8789.222767	26.070503
197.235970	8805.333642	26.075520
197.972211	8811.137327	26.080538
197.891677	8818.026970	26.085556
197.642049	8838.510694	26.090573
198.243824	8838.693518	26.095591
198.245551	8877.351197	26.100608
198.381117	8879.477719	26.105626
198.577577	8889.094818	26.110644
198.929026	8895.410802	26.115661
199.279624	8904.248269	26.120679
199.427266	8923.793696	26.125696
199.820630	8931.876770	26.130714
199.614183	8928.802657	26.135732
199.785932	8945.075720	26.140749
200.345687	8959.676467	26.145767
200.131205	8970.006789	26.150784
200.812595	8977.659546	26.155802
201.130864	8984.993651	26.160820
201.442409	8988.970166	26.165837
201.583993	8984.447665	26.170855
201.195344	9001.267352	26.175872
201.193997	9021.183308	26.180890
201.770100	9025.803473	26.185908
201.565939	9040.197153	26.190925
201.914617	9051.954183	26.195943
202.064901	9061.343852	26.200960
202.210427	9081.638994	26.205978
202.312029	9100.749334	26.210996
202.564099	9120.949634	26.216013
203.074679	9127.562207	26.221031
203.016270	9158.809669	26.226048
203.036233	9161.215931	26.231066
203.463335	9178.545151	26.236084
203.125487	9208.290516	26.241101
203.870885	9218.743008	26.246119
203.920800	9234.883929	26.251136
204.555029	9245.054728	26.256154
205.035186	9247.279425	26.261172
205.534376	9255.153000	26.266189
205.917228	9244.706318	26.271207
205.546971	9263.198396	26.276224
205.799550	9269.090788	26.281242
206.114217	9281.901254	26.286260
205.985082	9290.990143	26.291277
206.373556	9301.584592	26.296295
206.255246	9322.598121	26.301312
206.714871	9323.920314	26.306330
206.863024	9342.706003	26.311348
207.109829	9348.727228	26.316365
207.673002	9342.187712	26.321383
207.635660	9372.303758	26.326400
207.898875	9384.256465	26.331418
207.972986	9388.371280	26.336436
207.663999	9396.541011	26.341453
208.153983	9407.293663	26.346471
208.128461	9424.427371	26.351488
208.468820	9442.659210	26.356506
208.565759	9455.293631	26.361524
208.456798	9474.455332	26.366541
209.227871	9484.233817	26.371559
209.126463	9505.499096	26.376576
209.255166	9524.199973	26.381594
209.815632	9532.860732	26.386612
209.583805	9557.131067	26.391629
209.801681	9574.970221	26.396647
210.234060	9597.886194	26.401664
210.330891	9616.845673	26.406682
210.815833	9632.790173	26.411700
210.834437	9655.732855	26.416717
210.980668	9662.658344	26.421735
211.054870	9691.272220	26.426752
211.269696	9702.653286	26.431770
211.518678	9722.633354	26.436788
211.521477	9744.889297	26.441805
211.870770	9763.146464	26.446823
212.135124	9793.092089	26.451840
212.357522	9795.465783	26.456858
212.664251	9821.559902	26.461876
212.463154	9837.444008	26.466893
213.058248	9840.463430	26.471911
213.433679	9869.621825	26.476928
213.979183	9883.736242	26.481946
214.026288	9901.678956	26.486964
214.120667	9903.419484	26.491981
214.712822	9920.756302	26.496999
215.072139	9936.154915	26.502016
214.847957	9935.280699	26.507034
215.252777	9953.173918	26.512052
215.201261	9959.191404	26.517069
215.792787	9963.939654	26.522087
216.018209	9983.912021	26.527104
215.856022	9987.638124	26.532122
216.505329	9988.600390	26.537140
216.182133	10012.110047	26.542157
216.640954	10023.323782	26.547175
216.610112	10043.589316	26.552192
216.920429	10059.336638	26.557210
217.000583	10075.243049	26.562228
216.945925	10099.570218	26.567245
217.669585	10103.665093	26.572263
218.135641	10126.096434	26.577280
218.147218	10133.821559	26.582298
218.414720	10147.933328	26.587316
218.401043	10164.362803	26.592333
218.763567	10177.381256	26.597351
219.001533	10195.599641	26.602368
219.335110	10205.673830	26.607386
219.488975	10220.755667	26.612404
219.544008	10234.080151	26.617421
219.963585	10244.418861	26.622439
220.260841	10267.650559	26.627456
220.149894	10271.331967	26.632474
220.833450	10279.557210	26.637492
220.788771	10297.384777	26.642509
221.204726	10304.593777	26.647527
221.254267	10317.618178	26.652544
221.643428	10334.634472	26.657562
221.818991	10341.478865	26.662580
221.967802	10362.991539	26.667597
222.365627	10357.029255	26.672615
222.818172	10369.163481	26.677632
222.892142	10383.359450	26.682650
223.332950	10394.804373	26.687668
223.258241	10400.237438	26.692685
223.333887	10390.954737	26.697703
223.588143	10420.224617	26.702720
223.513037	10423.796067	26.707738
223.854840	10431.279420	26.712756
224.123208	10456.413906	26.717773
224.378421	10459.600581	26.722791
224.496345	10463.864143	26.727808
224.440113	10479.485394	26.732826
224.938689	10487.171623	26.737844
224.880155	10509.976401	26.742861
225.139471	10522.962420	26.747879
225.551096	10529.362768	26.752896
225.649983	10548.921228	26.757914
225.872215	10549.117379	26.762932
225.908546	10584.624651	26.767949
226.413736	10589.687906	26.772967
226.927566	10601.372997	26.777984
227.180030	10607.501257	26.783002
227.647278	10613.398127	26.788020
227.800704	10631.624222	26.793037
228.076921	10636.256897	26.798055
228.414566	10638.972026	26.803072
228.258293	10643.568979	26.808090
228.642459	10649.708134	26.813108
228.902023	10668.488341	26.818125
228.990809	10675.023645	26.823143
229.074943	10684.913621	26.828160
228.918116	10712.521091	26.833178
229.362644	10713.432633	26.838196
229.761101	10733.645606	26.843213
229.942783	10746.018898	26.848231
230.222767	10762.197184	26.853248
230.234705	10780.464510	26.858266
230.521186	10783.103216	26.863284
230.878073	10820.729007	26.868301
230.981422	10815.056687	26.873319
231.168030	10840.909640	26.878336
231.167101	10862.659400	26.883354
231.491472	10873.180576	26.888372
231.463554	10893.940258	26.893389
232.120914	10918.541275	26.898407
232.240477	10927.722540	26.903424
232.198759	10948.450260	26.908442
232.526450	10967.495837	26.913460
232.677287	10989.653277	26.918477
233.303681	11013.139026	26.923495
233.389140	11019.793854	26.928512
233.467825	11045.334590	26.933530
234.154331	11061.514499	26.938548
234.047837	11075.678499	26.943565
234.405766	11087.103517	26.948583
234.627102	11105.925387	26.953600
234.928226	11122.118004	26.958618
235.168990	11133.678220	26.963636
235.357569	11152.859938	26.968653
235.634188	11171.690392	26.973671
236.046980	11181.301625	26.978688
236.222118	11187.588449	26.983706
236.708892	11199.673422	26.988724
237.213252	11215.913232	26.993741
237.596245	11221.406242	26.998759
237.616074	11214.168644	27.003776
237.300629	11209.843879	27.008794
237.894002	11224.264785	27.013812
237.886033	11243.131647	27.018829
237.970027	11250.778307	27.023847
238.419674	11261.227051	27.028864
238.412786	11279.686285	27.033882
238.357978	11280.823667	27.038900
238.843983	11313.796872	27.043917
238.697165	11318.833867	27.048935
239.421774	11340.150868	27.053952
239.402746	11354.830879	27.058970
239.488181	11378.774933	27.063988
239.568934	11397.493254	27.069005
239.485569	11427.114649	27.074023
239.971940	11452.149925	27.079040
240.378764	11475.750304	27.084058
240.438046	11490.043905	27.089076
240.807985	11521.489273	27.094093
241.115761	11551.032223	27.099111
241.528315	11562.261767	27.104128
241.727174	11595.448813	27.109146
242.172467	11595.266649	27.114164
242.145478	11615.848505	27.119181
242.405650	11636.214797	27.124199
242.739286	11656.148711	27.129216
242.753975	11687.497971	27.134234
243.137284	11697.465667	27.139252
243.215877	11716.995815	27.144269
243.802906	11739.838841	27.149287
244.570275	11760.476074	27.154304
244.575484	11769.232360	27.159322
245.039534	11787.459324	27.164340
245.087310	11805.637955	27.169357
245.326169	11815.187200	27.174375
245.379078	11828.053570	27.179392
245.369768	11853.878880	27.184410
245.716129	11866.863594	27.189428
246.313599	11884.993452	27.194445
246.027395	11910.250249	27.199463
246.486478	11911.371673	27.204480
246.560254	11949.292943	27.209498
247.170386	11959.331305	27.214516
247.290382	11976.501769	27.219533
247.102654	12001.621412	27.224551
247.609291	12005.849023	27.229568
248.201506	12039.345253	27.234586
248.622814	12052.130257	27.239604
248.472247	12072.686584	27.244621
248.923313	12082.272811	27.249639
249.493957	12091.789214	27.254656
249.336238	12115.787559	27.259674
250.014272	12107.971360	27.264692
250.703676	12100.183459	27.269709
250.465612	12119.016267	27.274727
250.575741	12122.804949	27.279744
251.033477	12133.385243	27.284762
251.252749	12135.667327	27.289780
251.433292	12153.508596	27.294797
251.607522	12171.059662	27.299815
251.699573	12167.745239	27.304832
251.725180	12181.324460	27.309850
252.372109	12197.247828	27.314868
252.534769	12210.154288	27.319885
252.580130	12234.460477	27.324903
252.868325	12248.130722	27.329920
253.126699	12267.557749	27.334938
252.740286	12279.531702	27.339956
253.181673	12296.413192	27.344973
253.537257	12328.721265	27.349991
253.811973	12335.712510	27.355008
253.944250	12373.711310	27.360026
254.394675	12387.993974	27.365044
254.494964	12416.554927	27.370061
254.284551	12435.371712	27.375079
255.084292	12447.713397	27.380096
255.013806	12482.451279	27.385114
255.298791	12498.528300	27.390132
255.832195	12527.549560	27.395149
255.677969	12549.941312	27.400167
256.315871	12562.323451	27.405184
256.761056	12588.254658	27.410202
257.358904	12594.799373	27.415220
257.804459	12618.943595	27.420237
257.747678	12626.754090	27.425255
257.926673	12644.491297	27.430272
258.276831	12648.077927	27.435290
258.497795	12658.903744	27.440308
259.108245	12685.794459	27.445325
259.099725	12695.638924	27.450343
259.750209	12701.303938	27.455360
260.041930	12715.815686	27.460378
259.725402	12726.601489	27.465396
260.387368	12741.980502	27.470413
260.869501	12739.058146	27.475431
261.375186	12743.578345	27.480448
261.902596	12755.843462	27.485466
261.782167	12763.982374	27.490484
262.131533	12771.249029	27.495501
262.187281	12769.967143	27.500519
262.414140	12764.478672	27.505536
262.488960	12786.050860	27.510554
262.409183	12795.432498	27.515572
262.952464	12811.998421	27.520589
262.581073	12834.435048	27.525607
262.995246	12843.315870	27.530624
263.292421	12871.754982	27.535642
263.193715	12882.709648	27.540660
263.682839	12903.709627	27.545677
263.461119	12929.781086	27.550695
263.977493	12946.459874	27.555712
263.920960	12987.159814	27.560730
263.832140	13007.777022	27.565748
264.315871	13024.632601	27.570765
264.661723	13058.179504	27.575783
265.118788	13089.567497	27.580800
265.411190	13109.227306	27.585818
265.609958	13138.916076	27.590836
265.931616	13162.305366	27.595853
266.128669	13193.361711	27.600871
266.381685	13197.537602	27.605888
267.033584	13220.829076	27.610906
267.174465	13240.887209	27.615924
267.421170	13255.861334	27.620941
267.701724	13286.087507	27.625959
268.266194	13305.083126	27.630976
268.425675	13330.230979	27.635994
268.539652	13344.232944	27.641012
269.112937	13358.503434	27.646029
269.157499	13387.729718	27.651047
269.656304	13408.882940	27.656064
269.870619	13428.580897	27.661082
269.694565	13453.217546	27.666100
270.518136	13471.492641	27.671117
270.266493	13487.436236	27.676135
270.626001	13512.640766	27.681152
271.006292	13540.860850	27.686170
271.443883	13561.124593	27.691188
271.935322	13583.596379	27.696205
271.796471	13603.612990	27.701223
272.063458	13624.837806	27.706240
272.555136	13655.575958	27.711258
272.781022	13668.839615	27.716276
272.922796	13692.484414	27.721293
273.489050	13712.508717	27.726311
273.730717	13742.529034	27.731328
274.146400	13746.712208	27.736346
273.968157	13767.263417	27.741364
274.592644	13790.250080	27.746381
274.658260	13801.135520	27.751399
274.682911	13826.030657	27.756416
274.947498	13847.204014	27.761434
275.270647	13874.530912	27.766452
275.749675	13898.576776	27.771469
275.565468	13919.536021	27.776487
276.011671	13939.099469	27.781504
276.613608	13967.926774	27.786522
277.011014	13980.099364	27.791540
277.528102	13995.779447	27.796557
277.832710	14014.242227	27.801575
278.367239	14029.379741	27.806592
278.277331	14036.846424	27.811610
278.310505	14069.778141	27.816628
278.627744	14072.801605	27.821645
278.966375	14093.939393	27.826663
279.357390	14108.413690	27.831680
279.747708	14121.480117	27.836698
279.806149	14149.401339	27.841716
280.247582	14149.103960	27.846733
280.648015	14178.888657	27.851751
280.526396	14193.734961	27.856768
280.940427	14201.685430	27.861786
280.810538	14222.899163	27.866804
281.034381	14249.139972	27.871821
281.395311	14269.772206	27.876839
282.322129	14272.211256	27.881856
282.816135	14279.765644	27.886874
283.195824	14297.861667	27.891892
283.446907	14305.018673	27.896909
283.554892	14319.492554	27.901927
283.699024	14322.331016	27.906944
283.850175	14335.485739	27.911962
284.302628	14360.409691	27.916980
285.020055	14359.727844	27.921997
284.994468	14370.783998	27.927015
285.414554	14369.582748	27.932032
285.876596	14384.916677	27.937050
285.628687	14408.715819	27.942068
286.198205	14406.627264	27.947085
286.203328	14426.608616	27.952103
286.581786	14434.262092	27.957120
287.153786	14454.298854	27.962138
286.963718	14475.489859	27.967156
287.125024	14484.353696	27.972173
287.361350	14508.951399	27.977191
287.549958	14522.047469	27.982208
287.987747	14542.097769	27.987226
288.014973	14558.167866	27.992244
288.412535	14573.855691	27.997261
288.669896	14608.486607	28.002279
288.821664	14633.037961	28.007296
289.123401	14652.193358	28.012314
289.405256	14680.524132	28.017332
289.889446	14701.759317	28.022349
289.831893	14726.740855	28.027367
290.251413	14753.533205	28.032384
290.545048	14786.202547	28.037402
290.605651	14818.252641	28.042420
291.029283	14822.797671	28.047437
291.278483	14855.012622	28.052455
291.651572	14881.915924	28.057472
292.032815	14902.627648	28.062490
292.165457	14929.051940	28.067508
292.814103	14956.237862	28.072525
292.835145	14974.285279	28.077543
293.215246	15001.662681	28.082560
293.620351	15014.573412	28.087578
293.600080	15039.757646	28.092596
294.111439	15054.359520	28.097613
294.413395	15076.901300	28.102631
294.313618	15104.234434	28.107648
294.590960	15124.631880	28.112666
294.779648	15157.342948	28.117684
295.603189	15174.674108	28.122701
295.606033	15195.645721	28.127719
295.868184	15225.507832	28.132736
296.524528	15258.314817	28.137754
296.256646	15286.463910	28.142772
297.036272	15298.865162	28.147789
297.180786	15331.959563	28.152807
297.451767	15353.377446	28.157824
298.060377	15372.247761	28.162842
298.121894	15402.919136	28.167860
298.554306	15410.220465	28.172877
298.696523	15430.775168	28.177895
299.616076	15450.571647	28.182912
299.692766	15469.347173	28.187930
299.735171	15487.073431	28.192948
300.254687	15510.307629	28.197965
300.322505	15526.504137	28.202983
300.722240	15537.724105	28.208000
301.552295	15548.941623	28.213018
301.794696	15566.841575	28.218036
302.158069	15582.630260	28.223053
302.389145	15599.204107	28.228071
302.806879	15617.673522	28.233088
303.385865	15630.933380	28.238106
303.231200	15634.192198	28.243124
303.621052	15653.005617	28.248141
303.728075	15666.499766	28.253159
304.000907	15698.693135	28.258176
304.717388	15707.002917	28.263194
304.362135	15739.325810	28.268212
304.602833	15751.186750	28.273229
304.723463	15778.576288	28.278247
304.973065	15806.529097	28.283264
305.778789	15815.210290	28.288282
305.525254	15848.711721	28.293300
306.105936	15871.745601	28.298317
306.349668	15892.571906	28.303335
306.537913	15921.052154	28.308352
307.314756	15941.461311	28.313370
307.652720	15951.400650	28.318388
307.824318	15968.129829	28.323405
308.444236	15992.127789	28.328423
308.865827	16008.481576	28.333440
309.335195	16011.611877	28.338458
309.475106	16029.517091	28.343476
309.944533	16039.956533	28.348493
310.087815	16053.987104	28.353511
310.138490	16083.840992	28.358528
310.451888	16082.942321	28.363546
310.680861	16117.515123	28.368564
311.124003	16117.250615	28.373581
311.091582	16142.353457	28.378599
311.493729	16157.365776	28.383616
311.933817	16166.662671	28.388634
311.812617	16194.391657	28.393652
312.322857	16210.798255	28.398669
312.473374	16236.060062	28.403687
312.725489	16258.994155	28.408704
313.173914	16279.085677	28.413722
313.156817	16311.786135	28.418740
313.495857	16332.443923	28.423757
313.452066	16341.493477	28.428775
314.031215	16382.929053	28.433792
314.516646	16408.589094	28.438810
314.557485	16443.488056	28.443828
314.892687	16476.747415	28.448845
315.231766	16501.666638	28.453863
315.265443	16540.023138	28.458880
315.637715	16558.411174	28.463898
315.825225	16598.504758	28.468916
316.203524	16629.334752	28.473933
316.693044	16665.454127	28.478951
316.868315	16700.673946	28.483968
317.750996	16718.597386	28.488986
317.700400	16763.841155	28.494004
317.950723	16783.345665	28.499021
318.739554	16806.651487	28.504039
318.688198	16849.963485	28.509056
318.842907	16875.664811	28.514074
319.686877	16901.723021	28.519092
320.074263	16937.293994	28.524109
320.526522	16954.697768	28.529127
320.623071	16985.933201	28.534144
321.406274	17011.012169	28.539162
321.108838	17036.409078	28.544180
321.562770	17063.610966	28.549197
322.412922	17077.248518	28.554215
322.704510	17108.821399	28.559232
323.173087	17128.635240	28.564250
323.248254	17140.498437	28.569268
323.759758	17170.468755	28.574285
324.187783	17186.396805	28.579303
323.867452	17214.424300	28.584320
324.414258	17234.056918	28.589338
324.439994	17260.413269	28.594356
324.738765	17282.959374	28.599373
325.425962	17305.613281	28.604391
325.230787	17340.625892	28.609408
325.877349	17369.376690	28.614426
325.893830	17401.743988	28.619444
326.829903	17415.294921	28.624461
327.092040	17440.348192	28.629479
327.335104	17470.879184	28.634496
327.531049	17486.511472	28.639514
328.026126	17511.196639	28.644532
327.929881	17541.157850	28.649549
328.873559	17551.838079	28.654567
328.819813	17580.278063	28.659584
329.339678	17599.465843	28.664602
329.331804	17620.656620	28.669620
329.485852	17639.983856	28.674637
330.154742	17673.154412	28.679655
329.728568	17697.569785	28.684672
330.265473	17727.310365	28.689690
330.550431	17759.096646	28.694708
330.791574	17794.398607	28.699725
330.891718	17818.352727	28.704743
331.133504	17869.323151	28.709760
331.379885	17896.689897	28.714778
332.079069	17934.520741	28.719796
332.316239	17967.216246	28.724813
332.592534	17996.726437	28.729831
333.255775	18041.563694	28.734848
334.515491	18051.790356	28.739866
334.886532	18073.363880	28.744884
335.036743	18102.829013	28.749901
335.743729	18111.610723	28.754919
336.199877	18135.535364	28.759936
336.818894	18138.299536	28.764954
337.043652	18150.982194	28.769972
337.253040	18168.458723	28.774989
337.217723	18175.753243	28.780007
337.682390	18197.258473	28.785024
337.963488	18213.960618	28.790042
338.235654	18235.565875	28.795060
338.609538	18250.998917	28.800077
338.789049	18280.460898	28.805095
339.102822	18300.055237	28.810112
339.274123	18321.616845	28.815130
339.593541	18351.770066	28.820148
339.622620	18379.232140	28.825165
339.774009	18405.073144	28.830183
339.825375	18436.987415	28.835200
339.926897	18475.508158	28.840218
340.508085	18518.973603	28.845236
340.485818	18558.892287	28.850253
341.289246	18595.430123	28.855271
341.228718	18637.222113	28.860288
341.999901	18677.624118	28.865306
342.706891	18711.113671	28.870324
342.853343	18742.592524	28.875341
343.463799	18760.843635	28.880359
343.644464	18795.350374	28.885376
344.232275	18820.792571	28.890394
344.685933	18848.536640	28.895412
344.602111	18883.703087	28.900429
345.706775	18905.249037	28.905447
346.031940	18929.802900	28.910464
346.220624	18947.233599	28.915482
346.904699	18960.614629	28.920500
347.154161	18976.580461	28.925517
347.508429	18975.537515	28.930535
347.630693	19001.138069	28.935552
347.985251	19020.617753	28.940570
348.143818	19048.545833	28.945588
348.472870	19073.384756	28.950605
349.223975	19083.857755	28.955623
349.846305	19097.110152	28.960640
349.803267	19117.947909	28.965658
350.201767	19133.740138	28.970676
350.074642	19156.219032	28.975693
350.413077	19179.177741	28.980711
350.753992	19202.696765	28.985728
351.273997	19223.039776	28.990746
351.986608	19254.256581	28.995764
351.743805	19277.536436	29.000781
351.973133	19308.609880	29.005799
352.501429	19334.893580	29.010816
352.603030	19368.999583	29.015834
353.279770	19392.928013	29.020852
353.095271	19422.804921	29.025869
353.712951	19452.994634	29.030887
353.537516	19495.031660	29.035904
354.098755	19524.431214	29.040922
354.506571	19556.337028	29.045940
354.768075	19596.619870	29.050957
355.225433	19631.144599	29.055975
355.435822	19669.963568	29.060992
355.700317	19708.800391	29.066010
356.068762	19746.114662	29.071028
356.257228	19787.325488	29.076045
357.055535	19816.978790	29.081063
357.676646	19853.097792	29.086080
357.666149	19889.978250	29.091098
358.317833	19916.153489	29.096116
358.745273	19952.257123	29.101133
359.356942	19981.116359	29.106151
359.968681	20012.338550	29.111168
360.121475	20029.925802	29.116186
360.717126	20051.621802	29.121204
360.856225	20088.726164	29.126221
361.482424	20104.834317	29.131239
361.590329	20129.399883	29.136256
361.900200	20163.008608	29.141274
362.221803	20183.776280	29.146292
362.676252	20209.803891	29.151309
363.407005	20233.976221	29.156327
363.586082	20257.988441	29.161344
363.869594	20285.301087	29.166362
364.183060	20317.171118	29.171380
364.250708	20349.097716	29.176397
364.777738	20381.693803	29.181415
365.014568	20403.905423	29.186432
364.972016	20441.881433	29.191450
365.480860	20468.743461	29.196468
365.747283	20491.126894	29.201485
366.378361	20529.473791	29.206503
366.712501	20552.841174	29.211520
367.035394	20580.921416	29.216538
367.362938	20598.872468	29.221556
367.702763	20641.992059	29.226573
368.152538	20664.650509	29.231591
368.196566	20692.907700	29.236608
368.693700	20731.366217	29.241626
369.327436	20758.308067	29.246644
369.258385	20792.656995	29.251661
369.426234	20829.994788	29.256679
370.041185	20861.975388	29.261696
370.133439	20897.318713	29.266714
370.828859	20929.464613	29.271732
370.868068	20969.959272	29.276749
371.503947	21005.385528	29.281767
371.889939	21048.249220	29.286784
372.433057	21079.332868	29.291802
372.828179	21116.382314	29.296820
373.155272	21148.603899	29.301837
373.683532	21192.343133	29.306855
373.884312	21215.558702	29.311872
374.191902	21251.437915	29.316890
374.812593	21279.071860	29.321908
375.022038	21317.524891	29.326925
375.522749	21348.755230	29.331943
376.047416	21397.337606	29.336960
376.161405	21427.505072	29.341978
376.535610	21462.352662	29.346996
376.980762	21496.379389	29.352013
377.575187	21519.435801	29.357031
377.902517	21561.800673	29.362048
378.401278	21581.204643	29.367066
378.733343	21621.331393	29.372084
378.785114	21648.347036	29.377101
379.335414	21681.543829	29.382119
379.908931	21721.496889	29.387136
379.652031	21760.510472	29.392154
380.441487	21805.032029	29.397172
380.868357	21834.098971	29.402189
381.377341	21863.929452	29.407207
381.347089	21897.448408	29.412224
381.662162	21939.284615	29.417242
382.250785	21969.315257	29.422260
382.811936	21999.043956	29.427277
383.396282	22030.629343	29.432295
383.819876	22062.826391	29.437312
384.182591	22100.318860	29.442330
385.197867	22114.138142	29.447348
385.373834	22151.545502	29.452365
385.319476	22175.956208	29.457383
385.651456	22206.991454	29.462400
386.046308	22227.865144	29.467418
386.316457	22250.838834	29.472436
386.503427	22295.625551	29.477453
386.638826	22320.503228	29.482471
387.255560	22351.761171	29.487488
387.532540	22386.587700	29.492506
387.844732	22422.331005	29.497524
387.986109	22456.652376	29.502541
388.595467	22484.912470	29.507559
389.399796	22509.450706	29.512576
389.587612	22549.880045	29.517594
390.226438	22569.886719	29.522612
390.325212	22613.880277	29.527629
390.596309	22642.214248	29.532647
390.958789	22678.243906	29.537664
390.929115	22718.902093	29.542682
391.731637	22751.133100	29.547700
392.413348	22788.198295	29.552717
392.894084	22832.532502	29.557735
393.001639	22864.458610	29.562752
393.072766	22893.609394	29.567770
393.833903	22923.813636	29.572788
394.045537	22983.669293	29.577805
395.091690	22994.610284	29.582823
395.855308	23012.440247	29.587840
396.341230	23040.302760	29.592858
396.821402	23062.080789	29.597876
397.102683	23095.974817	29.602893
397.869152	23095.934789	29.607911
398.606265	23100.910533	29.612928
398.834793	23133.949773	29.617946
399.419311	23138.868717	29.622964
399.476677	23159.891150	29.627981
399.575149	23177.835171	29.632999
399.863169	23191.661027	29.638016
399.772512	23228.508488	29.643034
400.136906	23247.494041	29.648052
400.784774	23283.482748	29.653069
400.900643	23320.091928	29.658087
401.265902	23353.189391	29.663104
401.353800	23389.008425	29.668122
401.603325	23424.162192	29.673140
402.120375	23464.100295	29.678157
402.398101	23497.232486	29.683175
403.127534	23534.236686	29.688192
403.484733	23581.405483	29.693210
403.948177	23601.432747	29.698228
404.286728	23638.623933	29.703245
404.445928	23673.725690	29.708263
405.212797	23713.233918	29.713280
405.472848	23747.870785	29.718298
405.835796	23778.322855	29.723316
406.314685	23819.983531	29.728333
406.766226	23864.229172	29.733351
407.462416	23891.814700	29.738368
407.514488	23936.283313	29.743386
407.902359	23956.735824	29.748404
408.280168	23991.204004	29.753421
409.045487	24015.209644	29.758439
409.355613	24041.214585	29.763456
409.482719	24085.481819	29.768474
409.852302	24119.468722	29.773492
410.277681	24155.264846	29.778509
410.707897	24190.518333	29.783527
411.570195	24205.149191	29.788544
411.742714	24230.571405	29.793562
412.078126	24263.917346	29.798580
412.951874	24282.800916	29.803597
413.855018	24309.580654	29.808615
414.470543	24323.749168	29.813632
414.234927	24356.942891	29.818650
414.818191	24365.718325	29.823668
415.149333	24404.928263	29.828685
415.452201	24431.467500	29.833703
415.735229	24463.397210	29.838720
415.874604	24498.339307	29.843738
415.985524	24527.049549	29.848756
416.335564	24568.471188	29.853773
416.329077	24614.705300	29.858791
417.015253	24652.608349	29.863808
417.375210	24696.280091	29.868826
417.667719	24738.523496	29.873844
418.142087	24785.870182	29.878861
418.685389	24829.314560	29.883879
418.956281	24862.372688	29.888896
419.504060	24908.908477	29.893914
419.841850	24944.851096	29.898932
420.192011	24995.358169	29.903949
420.654799	25039.912502	29.908967
421.200352	25080.579577	29.913984
421.530572	25131.082379	29.919002
422.149525	25172.806984	29.924020
422.714726	25216.407264	29.929037
423.239190	25254.499789	29.934055
424.067515	25288.039529	29.939072
424.448081	25320.873158	29.944090
425.049960	25355.178596	29.949108
425.846511	25394.934413	29.954125
425.780448	25426.573475	29.959143
426.231722	25443.574428	29.964160
426.468843	25484.030922	29.969178
426.645406	25518.780251	29.974196
426.873697	25554.726719	29.979213
427.523947	25597.186382	29.984231
428.041117	25629.705822	29.989248
428.117407	25676.361509	29.994266
428.763181	25725.611376	29.999284
429.408241	25751.892665	30.004301
429.785083	25790.392853	30.009319
430.120298	25816.708652	30.014336
430.451835	25870.189068	30.019354
430.857323	25907.855424	30.024372
431.157467	25944.132430	30.029389
431.334454	25988.736516	30.034407
432.089266	26021.470193	30.039424
432.361840	26061.279643	30.044442
432.760702	26102.825881	30.049460
433.160864	26147.956554	30.054477
433.744771	26176.245382	30.059495
434.288398	26213.749426	30.064512
434.530175	26250.260162	30.069530
435.145499	26278.458293	30.074548
435.835895	26320.610165	30.079565
436.043696	26358.636809	30.084583
436.472655	26384.210654	30.089600
436.969120	26426.565450	30.094618
437.463651	26463.217595	30.099636
437.802942	26500.663480	30.104653
438.344767	26547.094675	30.109671
438.722792	26586.311930	30.114688
439.118616	26630.642636	30.119706
439.347957	26673.671699	30.124724
439.924388	26700.992817	30.129741
439.920503	26751.928170	30.134759
440.417769	26792.474133	30.139776
441.053423	26847.285697	30.144794
441.501899	26887.115643	30.149812
441.714376	26936.580860	30.154829
441.951257	26991.636082	30.159847
442.431969	27033.218161	30.164864
442.589152	27087.496979	30.169882
443.334470	27133.483815	30.174900
444.609246	27171.260431	30.179917
445.055251	27213.004500	30.184935
445.887470	27248.882158	30.189952
446.198408	27275.648565	30.194970
446.754338	27306.316890	30.199988
447.456729	27342.114596	30.205005
447.915961	27373.704505	30.210023
448.906255	27384.802427	30.215040
449.032673	27411.057981	30.220058
449.448462	27441.846590	30.225076
449.973370	27466.481904	30.230093
450.296768	27502.764229	30.235111
450.433172	27518.211859	30.240128
451.153136	27569.983847	30.245146
451.353767	27592.386171	30.250164
451.445766	27629.458863	30.255181
451.560235	27665.803206	30.260199
452.070713	27709.846788	30.265216
452.568777	27748.641980	30.270234
452.778773	27794.492234	30.275252
453.464529	27833.951068	30.280269
453.482507	27888.166508	30.285287
453.978695	27918.706846	30.290304
454.550938	27964.197311	30.295322
454.814073	28005.428913	30.300340
455.151556	28056.792234	30.305357
455.331418	28100.183593	30.310375
456.241047	28137.338331	30.315392
456.812438	28187.221352	30.320410
457.151832	28230.762558	30.325428
457.266593	28269.141018	30.330445
457.375091	28321.945724	30.335463
457.897336	28372.261043	30.340480
458.325376	28424.022391	30.345498
458.937176	28484.883509	30.350516
459.378394	28530.873921	30.355533
459.778283	28587.041630	30.360551
460.392603	28634.840630	30.365568
460.950716	28690.679346	30.370586
461.139371	28742.358507	30.375604
462.437346	28789.680285	30.380621
462.550269	28833.320647	30.385639
462.797821	28880.914060	30.390656
463.582002	28921.265995	30.395674
464.484826	28972.524803	30.400692
465.044390	29007.682346	30.405709
465.206366	29048.579711	30.410727
466.223185	29091.268313	30.415744
466.415844	29128.254317	30.420762
466.542864	29166.585663	30.425780
467.408966	29200.087352	30.430797
467.927170	29244.248908	30.435815
468.254022	29284.011147	30.440832
468.706984	29325.833615	30.445850
468.987963	29362.908516	30.450868
470.459445	29381.327018	30.455885
471.280936	29418.903754	30.460903
472.082285	29432.088229	30.465920
472.566069	29451.915472	30.470938
473.055006	29483.065072	30.475956
473.612065	29494.925329	30.480973
473.904458	29514.723255	30.485991
474.506282	29524.789278	30.491008
474.950230	29551.918055	30.496026
475.104468	29578.027690	30.501044
475.625583	29602.400523	30.506061
475.428643	29632.378433	30.511079
475.706702	29658.473197	30.516096
476.212163	29687.437850	30.521114
476.278109	29745.506638	30.526132
476.613640	29769.682349	30.531149
476.845792	29820.291065	30.536167
477.336543	29861.677071	30.541184
477.832837	29913.797910	30.546202
477.987727	29960.523533	30.551220
478.616936	30013.052182	30.556237
479.121069	30072.432889	30.561255
479.425931	30120.874982	30.566272
479.861027	30164.527462	30.571290
480.290494	30224.117617	30.576308
480.777220	30262.367433	30.581325
481.327765	30319.324029	30.586343
481.783312	30363.473382	30.591360
482.235055	30414.624200	30.596378
482.597342	30459.999066	30.601396
483.440686	30496.057081	30.606413
483.550950	30553.018441	30.611431
483.976389	30602.070013	30.616448
484.404910	30652.624799	30.621466
484.551374	30714.599116	30.626484
485.344428	30772.568310	30.631501
486.014256	30829.644794	30.636519
486.209272	30886.560710	30.641536
486.519016	30942.443547	30.646554
486.739106	30995.931016	30.651572
487.939899	31048.337249	30.656589
487.943547	31106.387681	30.661607
488.179809	31166.232693	30.666624
489.064457	31221.232105	30.671642
489.596348	31294.783637	30.676660
490.796699	31333.089330	30.681677
491.706533	31387.601418	30.686695
492.102744	31439.014882	30.691712
492.624980	31479.695429	30.696730
493.078024	31523.999613	30.701748
493.763400	31561.284585	30.706765
494.033482	31613.724268	30.711783
494.639645	31656.242280	30.716800
495.559226	31691.709184	30.721818
495.438046	31747.571992	30.726836
496.128631	31785.624234	30.731853
496.781757	31829.213309	30.736871
497.406473	31879.437988	30.741888
497.837012	31906.640580	30.746906
498.304114	31951.276248	30.751924
499.436014	31978.620990	30.756941
499.868409	32008.577048	30.761959
500.288904	32048.542285	30.766976
500.922531	32091.463705	30.771994
500.890661	32125.569977	30.777012
501.538382	32161.954422	30.782029
502.375428	32208.982846	30.787047
502.349286	32243.666916	30.792064
502.658459	32283.199661	30.797082
503.140593	32322.985513	30.802100
503.680857	32361.108745	30.807117
504.286713	32410.335572	30.812135
504.433197	32467.386050	30.817152
504.817594	32508.987975	30.822170
505.322925	32559.930444	30.827188
505.974845	32612.208438	30.832205
506.240129	32657.765595	30.837223
506.899338	32718.141529	30.842240
507.377377	32755.515831	30.847258
507.790493	32809.169158	30.852276
508.196075	32850.168011	30.857293
508.493890	32899.525759	30.862311
508.959796	32950.354338	30.867328
509.751019	32992.817944	30.872346
509.949116	33037.724813	30.877364
510.354253	33086.815392	30.882381
510.866182	33146.931045	30.887399
511.206913	33203.492835	30.892416
511.796052	33259.588067	30.897434
511.882836	33319.458389	30.902452
512.465916	33379.183658	30.907469
513.152988	33443.071407	30.912487
513.181371	33517.977264	30.917504
514.285475	33575.911499	30.922522
514.761912	33632.423181	30.927540
515.201788	33684.459329	30.932557
515.875589	33753.662674	30.937575
516.706048	33810.818467	30.942592
517.335463	33849.756939	30.947610
517.679540	33919.796954	30.952628
518.453641	33964.212594	30.957645
519.023656	34024.645329	30.962663
519.591233	34074.578384	30.967680
519.963197	34126.448603	30.972698
521.037477	34179.044168	30.977716
521.408126	34231.061528	30.982733
521.751477	34276.910208	30.987751
522.315217	34336.380317	30.992768
522.966658	34380.261715	30.997786
523.138549	34425.400357	31.002804
523.468534	34478.544222	31.007821
524.147384	34542.637714	31.012839
524.757937	34594.162403	31.017856
525.521131	34648.997099	31.022874
525.999876	34706.401172	31.027892
526.606824	34752.289568	31.032909
527.250641	34808.375010	31.037927
527.480998	34858.156043	31.042944
528.037681	34902.430685	31.047962
528.650267	34951.520523	31.052980
529.041251	35012.891830	31.057997
529.501775	35062.118146	31.063015
530.071429	35113.917380	31.068032
530.843818	35172.773937	31.073050
531.582507	35212.937311	31.078068
532.481842	35257.880346	31.083085
533.536238	35289.523112	31.088103
534.132777	35336.422155	31.093120
534.733754	35354.374419	31.098138
534.980137	35405.825623	31.103156
535.778455	35427.911667	31.108173
536.556524	35460.311359	31.113191
536.792233	35493.984627	31.118208
537.291499	35530.242462	31.123226
537.742970	35552.486395	31.128244
538.024068	35579.130777	31.133261
538.294772	35619.054373	31.138279
538.717099	35658.296497	31.143296
539.286387	35689.104488	31.148314
539.360492	35732.417690	31.153332
539.362899	35779.409465	31.158349
539.961618	35832.924731	31.163367
540.154602	35898.622193	31.168384
540.669448	35948.955515	31.173402
541.080515	36011.445065	31.178420
542.454888	36052.918649	31.183437
543.561707	36099.101613	31.188455
543.853479	36142.934580	31.193472
544.891717	36178.207738	31.198490
545.221993	36226.064530	31.203508
545.542058	36274.574215	31.208525
546.203329	36308.067816	31.213543
546.555710	36357.012461	31.218560
546.969887	36402.472575	31.223578
547.871228	36452.567687	31.228596
548.254507	36501.629231	31.233613
548.959353	36551.238809	31.238631
548.889731	36606.726565	31.243648
549.736474	36658.683519	31.248666
550.062399	36707.595560	31.253684
550.202351	36764.144633	31.258701
551.087500	36815.347052	31.263719
551.722273	36872.361609	31.268736
552.329609	36927.113505	31.273754
552.853643	36980.273813	31.278772
553.112080	37040.070192	31.283789
553.854661	37101.085685	31.288807
553.756593	37169.417050	31.293824
554.673190	37232.902753	31.298842
555.485940	37279.000215	31.303860
556.529269	37319.671957	31.308877
557.817570	37365.845272	31.313895
557.995874	37413.699689	31.318912
558.548930	37439.594190	31.323930
559.067968	37492.337507	31.328948
559.429121	37541.016157	31.333965
560.266016	37587.626204	31.338983
560.570762	37638.414300	31.344000
561.066900	37689.435376	31.349018
561.522764	37744.671305	31.354036
561.856553	37803.947527	31.359053
562.540145	37855.620395	31.364071
563.240684	37912.497125	31.369088
563.647387	37955.781985	31.374106
563.928508	38011.503876	31.379124
564.246860	38070.097602	31.384141
564.912754	38115.260499	31.389159
565.481566	38190.195731	31.394176
565.949983	38250.521122	31.399194
566.378155	38300.194109	31.404212
566.592626	38373.546742	31.409229
567.448830	38428.642297	31.414247
567.671434	38489.676251	31.419264
568.399927	38552.410056	31.424282
568.999022	38617.304432	31.429300
569.589045	38689.155830	31.434317
569.999942	38741.557599	31.439335
570.275201	38811.125956	31.444352
570.685472	38873.124797	31.449370
571.268704	38946.015919	31.454388
571.595656	39018.781028	31.459405
572.592622	39089.763534	31.464423
573.359598	39171.428346	31.469440
573.856408	39232.627861	31.474458
574.535030	39313.547379	31.479476
575.281636	39371.131258	31.484493
575.990896	39442.079064	31.489511
576.221030	39504.080512	31.494528
576.894949	39575.472878	31.499546
577.191185	39642.926674	31.504564
577.722517	39724.100253	31.509581
578.507238	39787.573962	31.514599
579.276868	39869.598083	31.519616
579.693817	39938.202319	31.524634
580.252951	40006.911916	31.529652
581.035418	40083.089314	31.534669
581.535381	40148.207165	31.539687
582.141924	40229.090469	31.544704
582.806176	40286.770983	31.549722
583.618860	40351.158550	31.554740
584.028610	40433.780447	31.559757
584.726304	40495.155924	31.564775
585.431643	40571.511791	31.569792
585.822810	40645.243454	31.574810
586.789094	40691.245312	31.579828
587.214592	40767.318608	31.584845
588.379049	40829.295900	31.589863
589.135695	40886.619934	31.594880
589.852148	40946.174164	31.599898
590.490826	41004.372128	31.604916
590.830461	41067.270169	31.609933
591.547806	41113.136185	31.614951
592.022400	41164.876047	31.619968
592.732712	41220.789240	31.624986
593.452963	41275.855732	31.630004
594.045648	41332.740566	31.635021
594.521576	41374.444449	31.640039
595.011655	41429.298917	31.645056
595.553270	41486.984084	31.650074
596.315656	41543.706960	31.655092
596.497397	41608.682333	31.660109
597.204616	41661.910106	31.665127
597.610419	41720.939289	31.670144
598.102960	41782.582307	31.675162
598.522639	41847.151643	31.680180
599.257192	41899.748110	31.685197
599.781227	41955.068827	31.690215
600.432841	42013.511027	31.695232
600.873915	42077.178859	31.700250
601.400203	42124.771842	31.705268
601.369701	42193.852224	31.710285
602.435535	42268.331897	31.715303
603.138298	42334.539209	31.720320
603.372075	42413.962340	31.725338
604.075507	42474.224198	31.730356
604.412903	42546.751853	31.735373
605.117110	42624.378758	31.740391
605.547978	42693.652622	31.745408
606.544876	42761.448687	31.750426
607.242343	42821.510827	31.755444
607.710360	42903.075428	31.760461
608.771241	42965.376596	31.765479
609.807317	43030.063533	31.770496
610.103631	43090.117945	31.775514
611.180124	43147.326021	31.780532
611.856747	43209.358052	31.785549
612.440155	43260.667334	31.790567
612.768083	43329.045341	31.795584
613.498581	43380.501894	31.800602
614.023838	43438.388615	31.805620
614.454903	43506.795060	31.810637
615.002554	43569.675404	31.815655
615.732834	43646.192350	31.820672
616.390908	43717.216438	31.825690
617.112904	43787.145467	31.830708
617.126191	43844.862716	31.835725
617.974805	43911.989747	31.840743
618.612067	43982.440945	31.845760
619.308299	44054.362551	31.850778
619.980108	44120.048495	31.855796
620.587667	44179.921460	31.860813
621.416165	44246.056121	31.865831
622.162023	44312.620611	31.870848
622.736257	44373.578444	31.875866
623.364479	44437.379726	31.880884
623.980625	44513.303504	31.885901
624.925852	44555.823641	31.890919
625.405978	44621.002550	31.895936
625.869675	44688.837445	31.900954
626.857807	44735.565906	31.905972
627.164295	44804.366399	31.910989
627.760320	44875.591230	31.916007
628.258210	44939.822073	31.921024
628.894224	44998.655402	31.926042
629.397291	45065.551676	31.931060
629.933818	45140.446627	31.936077
630.957371	45202.752314	31.941095
631.289451	45266.774154	31.946112
631.634118	45346.943877	31.951130
632.424838	45398.762778	31.956148
632.884085	45478.324898	31.961165
633.173036	45533.561960	31.966183
633.843380	45598.496537	31.971200
634.443019	45665.531161	31.976218
635.061970	45740.999215	31.981236
635.639755	45817.060967	31.986253
636.488170	45892.713977	31.991271
637.222813	45955.402782	31.996288
637.582123	46032.566637	32.001306
638.769458	46088.397487	32.006324
639.003272	46151.819834	32.011341
639.573135	46225.701366	32.016359
640.696442	46298.867224	32.021376
641.168266	46374.869395	32.026394
641.756115	46444.994498	32.031412
641.905091	46518.953756	32.036429
642.718414	46582.966864	32.041447
643.160559	46665.023282	32.046464
643.799800	46743.183701	32.051482
644.880417	46821.154284	32.056500
645.188150	46905.444961	32.061517
645.540749	46981.074345	32.066535
646.308398	47069.839125	32.071552
646.782357	47153.763761	32.076570
647.718804	47239.508258	32.081588
648.218890	47326.490086	32.086605
649.118608	47407.347531	32.091623
650.113245	47482.192138	32.096640
650.630948	47568.449805	32.101658
651.396728	47637.232428	32.106676
652.222696	47719.257871	32.111693
652.729168	47799.065923	32.116711
653.753621	47888.718426	32.121728
654.201907	47954.119874	32.126746
654.843524	48026.915258	32.131764
655.787353	48110.839033	32.136781
656.186503	48177.164179	32.141799
656.747604	48237.875632	32.146816
657.536813	48323.125046	32.151834
658.692514	48393.804856	32.156852
659.204114	48463.413706	32.161869
659.831921	48537.399821	32.166887
660.987397	48602.271377	32.171904
662.308930	48644.826709	32.176922
663.014459	48694.390663	32.181940
663.648314	48746.881809	32.186957
664.252650	48793.429762	32.191975
665.139816	48846.515114	32.196992
665.683697	48910.513306	32.202010
666.924096	48946.910163	32.207028
667.491992	48989.983930	32.212045
667.970766	49029.045570	32.217063
668.407480	49077.451154	32.222080
668.927470	49133.173888	32.227098
669.463399	49163.514324	32.232116
669.732570	49221.050681	32.237133
670.278124	49280.073654	32.242151
671.217180	49332.470600	32.247168
671.133507	49384.478333	32.252186
671.603834	49447.483545	32.257204
671.990258	49518.340828	32.262221
672.800734	49583.258288	32.267239
673.603220	49647.312620	32.272256
673.997300	49714.613087	32.277274
674.708174	49783.990262	32.282292
676.088072	49832.888306	32.287309
676.654970	49897.315550	32.292327
677.620674	49960.089066	32.297344
678.184109	50029.156172	32.302362
678.525787	50092.439759	32.307380
679.385975	50151.324002	32.312397
679.836195	50221.356591	32.317415
680.402795	50291.825346	32.322432
681.304631	50371.682976	32.327450
682.019905	50426.422468	32.332468
682.710607	50498.002034	32.337485
683.138183	50571.460448	32.342503
684.018358	50635.957235	32.347520
684.389927	50713.313080	32.352538
684.979447	50793.588398	32.357556
685.970104	50859.447490	32.362573
686.247667	50935.231880	32.367591
686.638181	51008.000542	32.372608
687.377253	51095.338290	32.377626
688.349300	51173.351601	32.382644
689.722628	51241.082564	32.387661
690.205889	51307.472234	32.392679
691.302141	51375.345658	32.397696
691.794450	51452.142644	32.402714
692.501352	51519.658870	32.407732
693.248770	51585.133308	32.412749
693.932654	51653.540527	32.417767
694.599209	51724.721714	32.422784
695.030530	51799.371203	32.427802
695.640450	51870.451526	32.432820
696.037030	51952.003051	32.437837
696.529157	52036.522183	32.442855
697.224121	52114.750970	32.447872
697.621460	52195.160984	32.452890
698.450660	52281.417079	32.457908
699.179594	52368.153498	32.462925
699.833208	52456.515097	32.467943
700.959392	52536.655931	32.472960
701.071853	52634.550840	32.477978
701.962506	52712.422820	32.482996
702.693590	52797.788032	32.488013
703.800916	52886.142613	32.493031
704.795373	52943.998347	32.498048
705.426040	53025.138700	32.503066
706.118626	53097.157550	32.508084
707.204227	53169.019424	32.513101
707.806249	53247.832881	32.518119
708.609030	53292.003212	32.523136
709.099862	53357.547030	32.528154
709.718643	53430.147084	32.533172
710.453445	53490.785559	32.538189
710.705882	53576.296935	32.543207
711.637251	53640.184011	32.548224
712.195130	53713.583974	32.553242
712.532540	53802.034047	32.558260
713.247959	53874.756215	32.563277
713.709593	53966.640360	32.568295
714.143886	54050.496323	32.573312
714.909915	54147.323159	32.578330
715.663290	54229.326835	32.583348
716.771958	54305.933634	32.588365
717.548704	54403.239902	32.593383
718.090771	54482.093508	32.598400
719.120119	54567.012368	32.603418
719.935574	54656.387921	32.608436
720.896169	54728.651494	32.613453
721.551542	54818.855082	32.618471
722.362815	54897.282525	32.623488
722.988403	54994.912730	32.628506
723.529383	55065.558851	32.633524
724.422744	55140.192710	32.638541
725.040985	55222.386508	32.643559
725.905762	55309.430999	32.648576
726.839948	55403.848183	32.653594
727.152003	55483.175187	32.658612
727.721686	55568.478083	32.663629
728.546998	55657.847492	32.668647
729.814088	55728.929826	32.673664
730.223296	55819.969866	32.678682
730.983549	55910.866079	32.683700
731.422585	55991.961761	32.688717
731.994969	56088.662405	32.693735
732.775279	56173.300074	32.698752
733.918979	56261.984072	32.703770
734.333300	56361.994356	32.708788
735.420877	56443.604347	32.713805
735.721148	56541.439790	32.718823
736.465962	56627.338455	32.723840
736.975037	56730.340953	32.728858
737.540301	56823.031081	32.733876
738.607449	56914.615786	32.738893
739.230149	57019.227598	32.743911
740.312707	57113.456315	32.748928
741.319001	57196.487411	32.753946
741.967279	57287.102025	32.758964
742.750346	57374.462900	32.763981
743.253940	57473.445298	32.768999
744.098374	57553.173161	32.774016
744.800393	57646.483361	32.779034
745.629119	57735.186712	32.784052
746.748589	57800.163316	32.789069
747.474422	57872.874425	32.794087
748.833755	57932.493695	32.799104
749.245602	58017.166916	32.804122
749.586578	58087.398701	32.809140
750.683531	58157.481984	32.814157
751.254725	58229.537182	32.819175
752.326190	58299.918672	32.824192
753.010343	58378.936845	32.829210
753.248160	58457.069799	32.834228
754.053335	58533.925667	32.839245
754.524517	58622.106111	32.844263
755.563120	58707.071028	32.849280
755.969712	58796.032932	32.854298
756.572062	58887.092057	32.859316
757.051033	58972.762938	32.864333
757.693731	59083.713457	32.869351
758.343700	59179.941159	32.874368
758.882264	59286.650317	32.879386
759.677303	59391.289111	32.884404
760.660493	59484.213317	32.889421
761.199025	59595.934905	32.894439
762.298932	59692.002054	32.899456
763.427865	59796.056369	32.904474
764.211074	59896.402701	32.909492
764.948887	59987.609813	32.914509
765.493497	60088.298270	32.919527
766.414794	60181.062136	32.924544
767.247984	60287.966912	32.929562
767.792759	60389.039009	32.934580
768.681863	60482.365207	32.939597
769.163292	60594.695449	32.944615
770.590360	60686.876103	32.949632
771.178246	60782.029426	32.954650
771.554272	60882.133261	32.959668
772.483119	60983.321079	32.964685
773.163572	61092.862902	32.969703
773.915607	61186.110217	32.974720
774.505872	61302.424882	32.979738
775.354901	61415.724575	32.984756
776.385084	61517.429615	32.989773
776.979789	61633.221443	32.994791
778.023597	61731.622543	32.999808
778.985492	61829.822472	33.004826
779.498698	61929.947925	33.009844
780.963227	62026.786828	33.014861
781.600414	62125.876790	33.019879
782.629073	62208.939256	33.024896
783.667600	62294.384645	33.029914
784.144565	62390.687913	33.034932
785.024452	62482.080282	33.039949
785.970342	62566.881665	33.044967
786.750760	62650.648733	33.049984
787.873893	62731.052181	33.055002
788.566543	62816.062360	33.060020
789.679302	62887.465033	33.065037
789.939582	62961.997366	33.070055
790.819760	63033.835509	33.075072
791.477178	63119.054760	33.080090
792.032899	63204.953749	33.085108
793.216583	63278.434001	33.090125
793.611278	63367.068876	33.095143
794.191250	63455.829410	33.100160
795.145164	63529.817750	33.105178
796.273050	63618.599196	33.110196
797.673061	63672.444811	33.115213
798.338309	63754.517125	33.120231
799.467623	63826.950216	33.125248
800.155407	63888.501748	33.130266
801.027331	63961.819525	33.135284
802.017392	64036.176733	33.140301
802.505808	64106.584367	33.145319
803.300269	64187.175782	33.150336
804.107357	64255.448893	33.155354
804.575089	64334.937073	33.160372
805.360848	64410.174637	33.165389
805.823500	64494.894164	33.170407
806.616937	64577.069620	33.175424
807.169301	64664.450582	33.180442
807.849601	64763.392671	33.185460
808.796341	64850.263240	33.190477
809.603963	64950.572482	33.195495
810.598285	65039.612354	33.200512
811.383160	65126.146742	33.205530
811.843526	65214.985022	33.210548
813.380683	65309.390911	33.215565
813.911220	65405.760886	33.220583
814.709643	65490.980911	33.225600
815.594930	65585.662473	33.230618
815.954783	65683.276965	33.235636
816.752991	65775.029742	33.240653
817.402367	65873.268684	33.245671
818.133417	65976.456961	33.250688
818.551199	66075.409694	33.255706
819.330807	66189.184688	33.260724
820.294863	66293.266150	33.265741
821.040867	66412.805658	33.270759
822.448413	66510.099645	33.275776
824.199354	66598.208255	33.280794
824.922143	66686.133486	33.285812
826.078252	66761.027568	33.290829
827.205511	66843.759699	33.295847
827.730586	66936.745929	33.300864
828.621893	67015.643970	33.305882
829.134778	67111.020851	33.310900
829.900036	67195.903087	33.315917
830.782986	67281.916695	33.320935
831.143077	67368.727757	33.325952
832.243370	67462.686249	33.330970
832.647260	67548.113976	33.335988
833.411194	67630.705147	33.341005
833.960060	67722.339448	33.346023
834.348148	67816.248762	33.351040
835.579302	67915.564713	33.356058
836.297182	68007.937867	33.361076
837.164255	68096.421415	33.366093
837.519614	68202.189390	33.371111
837.936982	68306.829862	33.376128
838.902461	68417.025253	33.381146
839.521819	68534.320500	33.386164
840.359758	68648.416516	33.391181
841.185139	68766.697511	33.396199
841.765992	68883.565063	33.401216
842.508369	69002.618824	33.406234
843.018125	69127.585896	33.411252
844.118401	69247.108557	33.416269
845.088792	69369.122916	33.421287
846.126152	69491.171600	33.426304
847.274175	69606.468480	33.431322
848.195527	69732.890212	33.436340
848.973974	69850.578694	33.441357
849.974252	69971.928651	33.446375
850.943460	70097.662760	33.451392
852.076563	70207.784689	33.456410
852.588805	70332.146170	33.461428
853.581974	70443.890196	33.466445
854.291334	70566.048308	33.471463
855.042842	70689.337765	33.476480
855.997591	70801.146796	33.481498
856.964720	70914.015979	33.486516
858.342484	71021.778353	33.491533
859.693891	71134.840375	33.496551
860.567347	71247.328310	33.501568
861.267475	71359.402174	33.506586
862.240421	71474.662037	33.511604
862.859902	71580.203958	33.516621
864.136473	71686.652841	33.521639
864.527990	71794.715407	33.526656
865.522810	71895.441315	33.531674
866.098439	72009.889227	33.536692
866.941078	72122.102690	33.541709
867.842703	72240.272350	33.546727
868.393707	72359.244138	33.551744
869.640883	72468.848681	33.556762
871.005894	72573.247248	33.561780
872.034043	72671.835997	33.566797
873.154543	72781.544572	33.571815
874.070570	72888.486971	33.576832
875.132800	72975.090957	33.581850
875.887953	73075.109020	33.586868
876.638225	73159.008339	33.591885
877.898479	73263.781070	33.596903
878.981210	73357.132285	33.601920
879.329012	73452.894765	33.606938
879.857048	73556.610195	33.611956
880.653389	73644.409500	33.616973
881.405071	73733.025166	33.621991
881.800288	73835.575154	33.627008
882.866841	73933.064460	33.632026
883.685581	74037.096315	33.637044
884.281125	74133.890595	33.642061
885.516819	74243.803724	33.647079
886.638171	74353.027872	33.652096
887.153840	74448.294428	33.657114
888.105820	74560.352517	33.662132
888.986366	74668.605578	33.667149
889.773140	74770.990593	33.672167
890.170675	74894.217047	33.677184
891.171387	75009.240111	33.682202
891.832811	75129.468396	33.687220
892.634485	75261.309747	33.692237
893.702088	75374.068094	33.697255
894.227130	75502.232684	33.702272
895.282473	75635.445428	33.707290
895.704762	75754.628470	33.712308
896.876270	75883.343543	33.717325
897.819317	76009.675237	33.722343
898.757834	76149.071945	33.727360
899.813089	76271.336271	33.732378
900.881246	76406.258465	33.737396
901.586509	76549.303826	33.742413
902.615903	76673.641383	33.747431
903.259923	76810.435013	33.752448
904.126235	76927.424355	33.757466
905.140391	77067.453672	33.762484
906.029219	77198.023355	33.767501
907.558574	77325.217976	33.772519
908.173676	77467.481442	33.777536
909.285461	77594.617784	33.782554
909.821460	77724.867756	33.787572
910.437341	77865.351479	33.792589
911.624962	77997.736971	33.797607
912.474899	78132.199664	33.802624
914.014406	78266.427091	33.807642
915.259064	78392.940464	33.812660
915.857679	78508.236934	33.817677
917.531394	78624.323729	33.822695
918.195950	78748.087246	33.827712
919.139013	78857.932872	33.832730
920.532516	78970.153596	33.837748
922.039412	79057.344945	33.842765
923.407847	79169.823587	33.847783
924.019859	79269.838105	33.852800
924.871278	79368.133618	33.857818
925.539951	79477.052775	33.862836
926.458818	79575.964331	33.867853
927.568015	79681.887805	33.872871
927.992320	79796.966384	33.877888
928.753910	79902.604961	33.882906
929.367685	80011.756914	33.887924
929.893251	80106.561588	33.892941
930.690235	80224.851329	33.897959
931.501458	80336.438877	33.902976
932.487087	80455.641795	33.907994
933.145173	80581.907948	33.913012
933.677097	80703.024010	33.918029
934.850893	80823.261098	33.923047
935.286527	80956.518544	33.928064
935.941209	81092.302215	33.933082
936.936251	81222.071350	33.938100
938.535345	81346.371788	33.943117
939.937175	81470.464135	33.948135
940.871947	81585.698976	33.953152
942.330264	81700.421267	33.958170
943.070390	81822.617014	33.963188
945.077114	81926.449377	33.968205
946.995088	82003.150434	33.973223
947.684785	82119.426069	33.978240
948.762883	82208.348929	33.983258
949.687456	82292.068371	33.988276
949.989849	82398.134072	33.993293
950.686116	82492.094268	33.998311
951.371973	82614.221089	34.003328
952.119518	82724.643016	34.008346
952.842745	82841.568492	34.013364
953.777690	82965.364683	34.018381
954.477847	83087.529912	34.023399
955.117894	83207.252405	34.028416
955.555977	83342.497176	34.033434
956.629907	83474.385670	34.038452
957.819082	83620.589335	34.043469
958.671092	83748.702502	34.048487
959.543010	83886.922784	34.053504
960.615482	84029.746405	34.058522
961.539814	84166.000217	34.063540
962.251208	84304.659733	34.068557
963.814904	84439.112815	34.073575
964.516410	84585.963462	34.078592
965.238213	84711.978785	34.083610
966.379872	84842.347604	34.088628
967.550276	84989.885159	34.093645
968.870791	85113.796980	34.098663
969.690647	85255.442439	34.103680
971.139589	85381.168998	34.108698
972.139938	85515.731184	34.113716
972.478316	85651.000224	34.118733
973.547559	85778.452470	34.123751
974.341496	85922.249967	34.128768
975.264510	86056.948009	34.133786
976.184196	86192.981599	34.138804
976.575410	86342.378693	34.143821
977.940024	86478.918713	34.148839
978.872867	86625.405149	34.153856
979.813591	86769.874216	34.158874
981.009190	86906.077102	34.163892
981.873687	87031.634463	34.168909
983.010360	87157.408511	34.173927
984.111908	87292.433696	34.178944
984.667376	87422.228599	34.183962
985.878353	87555.031142	34.188980
986.518731	87692.484545	34.193997
987.827880	87815.964857	34.199015
988.203829	87963.156070	34.204032
989.361254	88104.045752	34.209050
990.391201	88256.573241	34.214068
991.079893	88405.741286	34.219085
992.612701	88537.373045	34.224103
993.635391	88677.396248	34.229120
994.364950	88829.728938	34.234138
995.497612	88983.446735	34.239156
996.501270	89125.082125	34.244173
997.357608	89261.315903	34.249191
998.203550	89412.691890	34.254208
999.168373	89551.243788	34.259226
1000.549920	89704.029065	34.264244
1001.275863	89859.430407	34.269261
1002.780986	89998.506306	34.274279
1003.855145	90156.099448	34.279296
1004.851754	90295.511112	34.284314
1006.002056	90439.383154	34.289332
1006.552122	90588.063285	34.294349
1008.050845	90736.935016	34.299367
1008.798715	90885.832348	34.304384
1009.861791	91034.895576	34.309402
1011.171110	91185.767403	34.314420
1011.999856	91320.595383	34.319437
1013.238723	91476.622293	34.324455
1014.268750	91613.855025	34.329472
1014.970079	91757.111418	34.334490
1016.374526	91899.023558	34.339508
1017.162934	92054.126912	34.344525
1018.277401	92207.237761	34.349543
1019.448873	92356.412858	34.354560
1020.160874	92506.477972	34.359578
1021.053947	92651.145409	34.364596
1021.704172	92813.644641	34.369613
1023.088173	92960.006992	34.374631
1024.048962	93127.911303	34.379648
1024.749618	93282.195975	34.384666
1025.668922	93439.230011	34.389684
1026.410798	93617.217222	34.394701
1027.647841	93771.900672	34.399719
1029.013038	93935.085009	34.404736
1030.759339	94069.954531	34.409754
1032.354755	94206.025397	34.414772
1033.179668	94353.086763	34.419789
1034.745169	94479.992178	34.424807
1035.804545	94622.621814	34.429824
1036.883934	94760.973102	34.434842
1037.806834	94884.813939	34.439860
1038.611636	95014.683587	34.444877
1039.287652	95135.781809	34.449895
1040.316187	95276.238156	34.454912
1041.148427	95408.566410	34.459930
1042.053545	95535.228611	34.464948
1043.106299	95678.074754	34.469965
1044.177856	95811.657771	34.474983
1045.010100	95949.600227	34.480000
1045.630803	96100.020271	34.485018
1047.061238	96246.485295	34.490036
1047.759756	96393.687648	34.495053
1048.725603	96541.221669	34.500071
1049.474938	96698.223296	34.505088
1050.220293	96859.401893	34.510106
1051.553830	97008.961766	34.515124
1052.111858	97184.355766	34.520141
1052.925877	97349.999563	34.525159
1054.299410	97526.405202	34.530176
1055.179699	97705.098573	34.535194
1056.352083	97872.043001	34.540212
1057.547871	98040.117365	34.545229
1058.713433	98206.274513	34.550247
1059.542619	98390.542379	34.555264
1060.763604	98568.220339	34.560282
1062.295037	98726.826033	34.565300
1063.094883	98903.517031	34.570317
1064.422805	99067.383310	34.575335
1066.122966	99232.634056	34.580352
1066.724643	99408.341842	34.585370
1067.935582	99570.977603	34.590388
1068.912191	99743.996322	34.595405
1069.862165	99907.789510	34.600423
1070.784360	100085.166075	34.605440
1071.844040	100250.766426	34.610458
1073.579966	100412.824770	34.615476
1074.504729	100580.157260	34.620493
1075.826608	100734.773377	34.625511
1077.034573	100899.576532	34.630528
1078.000176	101062.109946	34.635546
1079.474658	101221.779522	34.640564
1080.558777	101388.908997	34.645581
1081.178681	101553.240857	34.650599
1082.565427	101711.984964	34.655616
1083.462942	101872.351883	34.660634
1084.962979	102027.505071	34.665652
1085.741970	102192.638706	34.670669
1086.779163	102350.974512	34.675687
1088.005387	102510.603808	34.680704
1088.971371	102659.676640	34.685722
1090.715696	102817.441197	34.690740
1091.835982	102977.672676	34.695757
1092.828290	103124.732029	34.700775
1094.225413	103269.196757	34.705792
1095.012168	103426.383675	34.710810
1096.245198	103547.304675	34.715828
1097.472204	103690.394236	34.720845
1098.418433	103824.252418	34.725863
1099.590185	103956.221361	34.730880
1100.643456	104097.822287	34.735898
1101.759776	104233.199789	34.740916
1102.754764	104379.424889	34.745933
1103.755996	104515.581693	34.750951
1104.774815	104662.931173	34.755968
1105.369890	104811.760177	34.760986
1106.799884	104954.388437	34.766004
1107.695442	105108.082294	34.771021
1108.608386	105260.869413	34.776039
1109.590876	105418.677576	34.781056
1110.629647	105581.762134	34.786074
1111.918638	105751.465641	34.791092
1113.119865	105899.129168	34.796109
1114.462710	106039.986793	34.801127
1116.089588	106185.863004	34.806144
1116.876317	106347.657522	34.811162
1118.320663	106489.210461	34.816180
1119.105171	106647.570844	34.821197
1120.004246	106805.382427	34.826215
1121.259498	106958.138589	34.831232
1122.023627	107117.017940	34.836250
1123.099712	107283.892822	34.841268
1124.041840	107457.764718	34.846285
1125.190844	107615.276033	34.851303
1126.660365	107787.060115	34.856320
1127.686640	107959.384267	34.861338
1128.904312	108118.343635	34.866356
1129.883868	108288.297787	34.871373
1131.053662	108455.950669	34.876391
1132.378278	108622.871201	34.881408
1133.407641	108794.934962	34.886426
1134.686064	108959.314422	34.891444
1135.858681	109128.344964	34.896461
1136.577538	109300.765490	34.901479
1138.235560	109463.170142	34.906496
1139.684384	109614.450128	34.911514
1141.291786	109775.459746	34.916532
1142.625391	109934.513799	34.921549
1143.482229	110080.301739	34.926567
1145.221605	110225.652692	34.931584
1146.205358	110382.011860	34.936602
1147.626385	110535.232527	34.941620
1148.002896	110688.044249	34.946637
1149.216890	110836.140898	34.951655
1150.258479	110991.766804	34.956672
1151.418242	111158.794136	34.961690
1152.467089	111323.922247	34.966708
1153.592348	111477.505975	34.971725
1154.046178	111647.813894	34.976743
1155.391808	111817.398786	34.981760
1156.169701	111994.854903	34.986778
1157.170667	112155.672662	34.991796
1158.111200	112315.633827	34.996813
1159.432472	112481.251725	35.001831
1160.091129	112651.438988	35.006848
1161.054424	112822.237323	35.011866
1162.670165	112978.487047	35.016884
1164.162710	113149.583282	35.021901
1165.136039	113317.015597	35.026919
1166.582522	113477.296237	35.031936
1167.561198	113655.890720	35.036954
1168.917804	113820.866156	35.041972
1169.959070	113985.930806	35.046989
1171.153832	114157.302846	35.052007
1172.779045	114323.599970	35.057024
1173.469291	114506.228405	35.062042
1174.615652	114667.849515	35.067060
1176.061780	114836.907098	35.072077
1176.886259	115024.031850	35.077095
1178.209775	115197.112488	35.082112
1179.450573	115381.381716	35.087130
1180.780538	115542.871589	35.092148
1181.858308	115719.799842	35.097165
1182.945791	115901.260885	35.102183
1184.686811	116071.033208	35.107200
1185.725956	116256.277859	35.112218
1187.026086	116428.952742	35.117236
1188.021296	116613.162306	35.122253
1188.870095	116797.700385	35.127271
1190.147213	116987.920613	35.132288
1191.092148	117168.298991	35.137306
1192.350150	117345.944295	35.142324
1193.383692	117536.682184	35.147341
1194.319457	117722.308437	35.152359
1195.581847	117917.558848	35.157376
1196.704137	118126.528479	35.162394
1197.672149	118322.911486	35.167412
1199.041757	118523.936650	35.172429
1200.302293	118727.038570	35.177447
1201.790195	118919.531660	35.182464
1202.869371	119112.002523	35.187482
1204.111554	119310.084361	35.192500
1205.134949	119519.460861	35.197517
1205.961068	119726.147612	35.202535
1207.363174	119921.523860	35.207552
1208.595345	120139.192563	35.212570
1210.199126	120339.352331	35.217588
1211.293381	120544.470509	35.222605
1212.301419	120749.907951	35.227623
1213.721035	120948.657879	35.232640
1214.771053	121155.066998	35.237658
1216.030870	121366.966301	35.242676
1217.404720	121571.199471	35.247693
1218.853673	121771.521408	35.252711
1220.358042	121981.005701	35.257728
1221.132693	122180.196751	35.262746
1222.513019	122360.434136	35.267764
1223.963668	122543.384652	35.272781
1225.134513	122725.139687	35.277799
1226.083615	122913.922691	35.282816
1227.116086	123104.884959	35.287834
1228.514112	123296.271773	35.292852
1230.089297	123468.784818	35.297869
1231.256756	123661.350845	35.302887
1232.852469	123838.194802	35.307904
1234.136522	124022.359897	35.312922
1235.116288	124205.763992	35.317940
1236.453019	124396.433765	35.322957
1237.705075	124585.066380	35.327975
1238.465669	124779.668418	35.332992
1239.987830	124968.159433	35.338010
1241.401234	125146.408978	35.343028
1242.394028	125342.447493	35.348045
1243.421417	125548.780153	35.353063
1244.802457	125745.089191	35.358080
1245.830007	125941.278510	35.363098
1246.843317	126146.021885	35.368116
1248.232373	126348.249596	35.373133
1249.104032	126564.647237	35.378151
1250.469356	126779.904030	35.383168
1251.776019	126971.078042	35.388186
1253.255410	127189.246137	35.393204
1254.675213	127390.323903	35.398221
1255.565516	127605.244662	35.403239
1256.958960	127809.674012	35.408256
1258.497849	128026.572493	35.413274
1259.544918	128242.423404	35.418292
1261.295037	128432.992340	35.423309
1262.569448	128642.792799	35.428327
1264.159256	128846.603190	35.433344
1265.339880	129056.371015	35.438362
1266.870398	129263.766431	35.443380
1268.324681	129465.005831	35.448397
1269.141311	129670.642798	35.453415
1270.563235	129875.627615	35.458432
1271.852535	130070.474461	35.463450
1272.635925	130281.188812	35.468468
1273.906495	130482.718130	35.473485
1275.195155	130703.427348	35.478503
1276.780555	130904.858966	35.483520
1277.962335	131109.966998	35.488538
1279.114501	131322.708322	35.493556
1280.559659	131535.518695	35.498573
1281.519243	131758.176267	35.503591
1282.758603	131969.882344	35.508608
1283.918837	132193.449005	35.513626
1285.120319	132402.351594	35.518644
1286.635521	132620.923858	35.523661
1287.650247	132850.157035	35.528679
1288.884080	133060.402352	35.533696
1290.446615	133266.327017	35.538714
1291.767752	133475.370482	35.543732
1293.043593	133669.230582	35.548749
1294.101267	133880.054756	35.553767
1295.248243	134081.033726	35.558784
1296.882008	134287.841354	35.563802
1297.593781	134504.870477	35.568820
1299.202084	134703.106865	35.573837
1300.405487	134909.341134	35.578855
1301.757089	135117.732769	35.583872
1303.283252	135334.309193	35.588890
1304.335373	135538.785323	35.593908
1306.402189	135736.803834	35.598925
1308.002717	135945.136488	35.603943
1309.225000	136135.321508	35.608960
1311.049589	136337.133429	35.613978
1312.225560	136532.321082	35.618996
1313.172450	136727.419730	35.624013
1314.368306	136931.021059	35.629031
1315.656980	137139.348425	35.634048
1317.189752	137348.664913	35.639066
1318.045900	137557.089331	35.644084
1319.390463	137764.030943	35.649101
1320.994029	137985.417500	35.654119
1322.325913	138187.396467	35.659136
1323.838089	138392.022084	35.664154
1325.225342	138610.786433	35.669172
1326.456182	138819.337581	35.674189
1327.664702	139031.911060	35.679207
1328.664683	139244.912066	35.684224
1329.993029	139462.323334	35.689242
1330.874199	139696.345822	35.694260
1332.341797	139919.605976	35.699277
1333.545641	140143.087143	35.704295
1334.760000	140375.503124	35.709312
1335.953692	140602.601263	35.714330
1337.226874	140850.295927	35.719348
1338.702810	141082.168815	35.724365
1340.238197	141318.419200	35.729383
1341.625860	141545.556945	35.734400
1343.033752	141781.210167	35.739418
1344.092671	142019.430171	35.744436
1345.547423	142256.194942	35.749453
1347.111408	142493.983484	35.754471
1348.131387	142730.998475	35.759488
1350.053990	142959.164380	35.764506
1350.583522	143206.197868	35.769524
1352.203973	143448.623760	35.774541
1353.738087	143684.588410	35.779559
1355.374045	143922.224447	35.784576
1356.904181	144159.308748	35.789594
1357.971499	144404.263658	35.794612
1359.545532	144635.780214	35.799629
1360.574586	144873.507316	35.804647
1361.930907	145105.011258	35.809664
1363.353123	145337.976806	35.814682
1364.687014	145561.261251	35.819700
1366.474187	145786.870955	35.824717
1367.287401	146014.944083	35.829735
1368.595778	146234.079690	35.834752
1370.066491	146454.585378	35.839770
1371.236527	146690.123546	35.844788
1372.684035	146912.905140	35.849805
1374.124733	147152.865748	35.854823
1375.543580	147380.598934	35.859840
1376.937244	147601.150194	35.864858
1377.888671	147844.261482	35.869876
1379.319507	148070.679328	35.874893
1380.487506	148310.691989	35.879911
1381.822024	148559.427001	35.884928
1383.331013	148796.764994	35.889946
1384.660197	149051.145895	35.894964
1386.191531	149287.000734	35.899981
1387.715068	149538.426168	35.904999
1388.702297	149795.795715	35.910016
1390.112086	150051.198530	35.915034
1391.456718	150292.237392	35.920052
1393.171060	150539.938416	35.925069
1394.791911	150798.812570	35.930087
1396.344128	151044.869730	35.935104
1397.766147	151287.475682	35.940122
1398.902546	151545.824188	35.945140
1400.247152	151797.625085	35.950157
1401.552379	152048.204377	35.955175
1402.664903	152314.194970	35.960192
1404.225913	152573.194014	35.965210
1405.494339	152837.959581	35.970228
1407.206499	153092.387069	35.975245
1408.327835	153366.245410	35.980263
1409.986498	153625.959808	35.985280
1412.016682	153869.172650	35.990298
1412.907941	154152.316896	35.995316
1414.517265	154396.132956	36.000333
1416.467977	154649.228407	36.005351
1417.581890	154904.639576	36.010368
1419.594917	155158.502375	36.015386
1420.680857	155414.695276	36.020404
1422.238667	155667.721303	36.025421
1423.756638	155925.193423	36.030439
1424.985395	156186.365215	36.035456
1426.895754	156433.102450	36.040474
1428.026610	156688.486258	36.045492
1429.575198	156933.877112	36.050509
1431.195518	157184.381086	36.055527
1432.970906	157410.719110	36.060544
1434.851487	157653.031753	36.065562
1436.045074	157900.527419	36.070580
1437.905696	158127.769574	36.075597
1439.394252	158361.108285	36.080615
1441.040506	158597.390769	36.085632
1442.545371	158807.321417	36.090650
1443.587542	159037.527362	36.095668
1444.699849	159248.524818	36.100685
1446.088416	159460.646289	36.105703
1447.294719	159690.919199	36.110720
1448.267155	159904.364891	36.115738
1449.606893	160145.144885	36.120756
1450.711650	160376.376806	36.125773
1452.292521	160613.101696	36.130791
1453.375807	160858.251627	36.135808
1454.794596	161101.219432	36.140826
1456.010612	161357.955315	36.145844
1457.220540	161608.391192	36.150861
1458.647816	161869.041182	36.155879
1459.936514	162133.862064	36.160896
1461.251218	162397.235012	36.165914
1462.411753	162672.847230	36.170932
1464.067249	162942.878827	36.175949
1465.490517	163222.790785	36.180967
1466.944010	163506.060925	36.185984
1468.351097	163773.233890	36.191002
1469.741870	164053.334938	36.196020
1471.064018	164335.452891	36.201037
1473.205056	164618.749217	36.206055
1475.010033	164888.898261	36.211072
1476.921721	165156.609881	36.216090
1478.735152	165422.119518	36.221108
1480.253789	165689.656464	36.226125
1481.657460	165961.005885	36.231143
1482.883554	166234.008960	36.236160
1484.785986	166496.036881	36.241178
1485.956081	166773.086106	36.246196
1487.186526	167048.275978	36.251213
1488.542046	167324.297792	36.256231
1490.148891	167600.192903	36.261248
1492.689230	167858.691644	36.266266
1493.983823	168133.828484	36.271284
1495.675884	168395.167338	36.276301
1497.347280	168656.752265	36.281319
1498.402140	168926.973417	36.286336
1500.060241	169183.883578	36.291354
1501.885116	169456.231233	36.296372
1503.275448	169717.715830	36.301389
1504.742039	169979.380349	36.306407
1505.793395	170250.042603	36.311424
1507.742052	170506.040151	36.316442
1509.347396	170767.814784	36.321460
1510.959183	171034.169400	36.326477
1512.620670	171293.680722	36.331495
1513.502053	171569.427752	36.336512
1515.339321	171829.536254	36.341530
1516.717899	172109.077041	36.346548
1517.788676	172380.968703	36.351565
1519.615735	172643.583195	36.356583
1520.776324	172928.124388	36.361600
1522.479018	173187.628906	36.366618
1523.802572	173448.019913	36.371636
1525.575834	173699.587990	36.376653
1526.926446	173951.389706	36.381671
1528.152788	174210.456399	36.386688
1529.974205	174466.309458	36.391706
1531.283879	174727.954172	36.396724
1532.721406	174993.132386	36.401741
1534.855181	175242.458085	36.406759
1536.135330	175519.678602	36.411776
1537.316281	175767.408167	36.416794
1538.575714	176048.682516	36.421812
1540.040728	176315.907461	36.426829
1541.468569	176595.306547	36.431847
1542.840346	176877.545571	36.436864
1544.565977	177153.183895	36.441882
1545.739219	177450.060891	36.446900
1547.151314	177734.760585	36.451917
1548.734469	178029.736961	36.456935
1550.299438	178321.812933	36.461952
1551.922237	178610.303933	36.466970
1553.626863	178911.750386	36.471988
1554.931044	179204.533633	36.477005
1556.689667	179498.908770	36.482023
1558.125806	179810.858782	36.487040
1560.008505	180087.201837	36.492058
1561.419511	180389.377829	36.497076
1562.910336	180696.973680	36.502093
1564.843134	181003.321529	36.507111
1566.502791	181309.714935	36.512128
1568.113839	181605.777375	36.517146
1569.446822	181907.456135	36.522164
1571.345246	182208.171659	36.527181
1573.263266	182507.871057	36.532199
1574.317953	182810.577240	36.537216
1575.923024	183115.862670	36.542234
1577.772667	183413.472769	36.547252
1579.219945	183720.779546	36.552269
1581.014169	184021.523948	36.557287
1582.620063	184332.552945	36.562304
1584.576793	184629.278596	36.567322
1585.628276	184930.159753	36.572340
1587.225951	185235.689218	36.577357
1589.110090	185542.304581	36.582375
1590.359268	185849.961883	36.587392
1591.952340	186150.117926	36.592410
1593.944617	186452.357053	36.597428
1596.818494	186726.718654	36.602445
1599.583675	186990.947415	36.607463
1601.782059	187250.635962	36.612480
1603.447114	187511.057858	36.617498
1605.298896	187763.748792	36.622516
1606.608607	188021.044819	36.627533
1608.614296	188273.447574	36.632551
1610.228091	188530.127044	36.637568
1611.397894	188773.503007	36.642586
1613.424650	189004.066578	36.647604
1614.421467	189230.683212	36.652621
1616.018423	189445.137091	36.657639
1617.462561	189671.392898	36.662656
1618.707956	189914.280466	36.667674
1620.160424	190154.116031	36.672692
1621.218099	190398.812542	36.677709
1622.738195	190637.713365	36.682727
1623.598626	190909.221077	36.687744
1624.886055	191163.859880	36.692762
1626.613943	191437.288676	36.697780
1627.897426	191709.165151	36.702797
1629.000785	191989.980829	36.707815
1630.542111	192274.700859	36.712832
1632.038389	192569.176494	36.717850
1633.399766	192869.449819	36.722868
1634.825572	193173.001776	36.727885
1636.747399	193470.994125	36.732903
1638.164341	193780.566902	36.737920
1639.692568	194099.642570	36.742938
1641.294141	194415.345329	36.747956
1642.582936	194740.453520	36.752973
1644.374238	195059.556919	36.757991
1646.078334	195388.156987	36.763008
1647.737097	195708.262762	36.768026
1649.619477	196027.738492	36.773044
1651.099602	196361.393701	36.778061
1653.422142	196677.897051	36.783079
1654.985307	196992.923705	36.788096
1656.473728	197325.949169	36.793114
1658.634057	197647.370706	36.798132
1660.071813	197976.270607	36.803149
1661.574967	198305.758717	36.808167
1663.142038	198636.837991	36.813184
1664.635078	198965.519457	36.818202
1666.464128	199305.801573	36.823220
1668.107028	199649.770955	36.828237
1670.263199	199978.442140	36.833255
1671.953289	200307.049710	36.838272
1673.239043	200647.896173	36.843290
1675.393521	200979.277292	36.848308
1677.027091	201318.892213	36.853325
1678.683871	201645.799486	36.858343
1680.678333	201978.722514	36.863360
1682.544126	202300.472293	36.868378
1684.298010	202629.870529	36.873396
1686.212387	202954.713571	36.878413
1688.223407	203266.481295	36.883431
1689.977556	203586.263220	36.888448
1691.512873	203905.624710	36.893466
1693.245273	204221.059644	36.898484
1694.926207	204544.742884	36.903501
1696.831623	204854.771550	36.908519
1699.061431	205170.475413	36.913536
1700.704851	205462.662886	36.918554
1702.473919	205758.881333	36.923572
1703.864504	206047.341667	36.928589
1705.634983	206324.673578	36.933607
1707.154191	206625.772606	36.938624
1708.635031	206911.518888	36.943642
1710.648477	207192.776944	36.948660
1711.708539	207496.834928	36.953677
1713.282509	207794.833635	36.958695
1715.000501	208095.832289	36.963712
1716.487379	208403.114981	36.968730
1718.502349	208709.058565	36.973748
1719.578945	209023.074324	36.978765
1721.604003	209327.521372	36.983783
1723.810707	209632.829726	36.988800
1725.473676	209948.889829	36.993818
1727.234123	210243.785845	36.998836
1729.120740	210563.152364	37.003853
1730.748167	210872.113398	37.008871
1732.608096	211192.122088	37.013888
1734.178729	211511.810148	37.018906
1736.126090	211819.696633	37.023924
1737.515705	212150.753700	37.028941
1739.313565	212468.379125	37.033959
1740.898423	212787.842707	37.038976
1742.320512	213116.525422	37.043994
1744.284560	213439.220165	37.049012
1745.912237	213778.042884	37.054029
1747.604395	214103.957999	37.059047
1749.187345	214434.589565	37.064064
1751.536683	214757.026365	37.069082
1754.126773	215072.494389	37.074100
1755.742048	215403.519136	37.079117
1758.038049	215715.342236	37.084135
1760.159460	216028.743422	37.089152
1761.746479	216339.132961	37.094170
1763.591615	216641.788873	37.099188
1765.038369	216965.318875	37.104205
1766.908554	217283.082392	37.109223
1768.656195	217594.581981	37.114240
1770.889627	217909.954465	37.119258
1772.503125	218224.080918	37.124276
1774.077447	218537.135739	37.129293
1775.900309	218847.029040	37.134311
1777.958680	219152.328098	37.139328
1779.237599	219474.854936	37.144346
1780.608694	219793.013491	37.149364
1782.534283	220111.986872	37.154381
1784.363355	220423.269813	37.159399
1786.124198	220760.048045	37.164416
1787.494755	221150.218002	37.169434
1789.329202	221474.671445	37.174452
1790.837340	221815.417944	37.179469
1792.207316	222156.060915	37.184487
1793.979660	222483.080655	37.189504
1795.744957	222820.819566	37.194522
1798.004919	223141.034990	37.199540
1799.713827	223465.796054	37.204557
1801.463742	223768.991353	37.209575
1803.461107	224084.477974	37.214592
1805.098747	224398.257961	37.219610
1807.039704	224700.169380	37.224628
1809.134409	225030.424472	37.229645
1810.698509	225339.153338	37.234663
1812.845408	225654.647726	37.239680
1814.410618	225977.981429	37.244698
1816.515587	226295.376911	37.249716
1817.984276	226625.979020	37.254733
1819.576447	226952.220062	37.259751
1821.658399	227277.190978	37.264768
1823.174852	227610.354367	37.269786
1825.103534	227931.314057	37.274804
1826.714493	228276.629956	37.279821
1828.513236	228614.958704	37.284839
1830.569047	228949.844769	37.289856
1832.062135	229288.656366	37.294874
1834.115062	229614.910437	37.299892
1836.279429	229959.459327	37.304909
1837.879506	230307.781700	37.309927
1839.992644	230641.496695	37.314944
1841.574392	230997.088228	37.319962
1843.508007	231329.742119	37.324980
1845.514259	231680.240172	37.329997
1846.986267	232025.719397	37.335015
1849.447285	232370.839707	37.340032
1850.880100	232717.775334	37.345050
1853.255092	233056.765479	37.350068
1855.276945	233403.838645	37.355085
1857.129167	233740.399738	37.360103
1859.307774	234083.970875	37.365120
1860.716695	234435.488048	37.370138
1863.281817	234768.637672	37.375156
1864.648659	235107.261478	37.380173
1866.500243	235453.124247	37.385191
1868.566533	235793.721975	37.390208
1870.514858	236152.169453	37.395226
1872.607032	236487.964974	37.400244
1874.377549	236820.231370	37.405261
1876.511645	237159.984586	37.410279
1878.294485	237509.852652	37.415296
1879.648270	237854.811711	37.420314
1881.543141	238190.974039	37.425332
1883.545545	238543.299669	37.430349
1885.073773	238887.319875	37.435367
1887.759548	239228.109470	37.440384
1889.494626	239571.997323	37.445402
1891.522810	239917.287458	37.450420
1893.402585	240261.636985	37.455437
1895.306392	240600.192565	37.460455
1897.549118	240938.771520	37.465472
1899.226414	241278.711168	37.470490
1901.072973	241592.462949	37.475508
1903.126830	241905.395234	37.480525
1904.552104	242224.854299	37.485543
1906.519383	242536.150913	37.490560
1908.510038	242853.261237	37.495578
1910.211378	243170.113468	37.500596
1912.347868	243488.497641	37.505613
1913.986442	243812.549708	37.510631
1916.077235	244126.015016	37.515648
1917.222188	244462.339247	37.520666
1919.242569	244794.588297	37.525684
1921.581859	245130.445245	37.530701
1923.602108	245466.125047	37.535719
1925.940411	245787.378351	37.540736
1927.888490	246116.441577	37.545754
1929.677845	246445.149746	37.550772
1931.516543	246765.290721	37.555789
1933.326502	247108.424876	37.560807
1935.394864	247437.040219	37.565824
1937.124806	247782.296931	37.570842
1939.372531	248111.367920	37.575860
1941.775972	248444.860127	37.580877
1943.320811	248786.109701	37.585895
1945.197132	249123.217801	37.590912
1947.036355	249466.022423	37.595930
1948.757952	249816.695494	37.600948
1950.632110	250164.703356	37.605965
1952.405647	250519.154518	37.610983
1954.511246	250867.381146	37.616000
1956.317400	251231.176427	37.621018
1958.557163	251589.086676	37.626036
1960.729547	251930.548007	37.631053
1962.711289	252297.492871	37.636071
1965.038482	252647.339011	37.641088
1966.813252	252997.756120	37.646106
1968.752877	253350.637123	37.651124
1970.764801	253705.768092	37.656141
1972.858272	254069.117048	37.661159
1974.982334	254416.763324	37.666176
1976.798040	254778.430323	37.671194
1979.050271	255137.386874	37.676212
1981.200334	255479.518580	37.681229
1982.873673	255828.534303	37.686247
1985.893072	256164.712055	37.691264
1987.681671	256515.260147	37.696282
1989.495298	256848.531192	37.701300
1991.645269	257182.968679	37.706317
1993.477225	257523.528306	37.711335
1995.631044	257874.096752	37.716352
1997.758400	258225.482794	37.721370
1999.506882	258554.041735	37.726388
2001.511300	258898.233914	37.731405
2003.291213	259257.932396	37.736423
2005.221626	259592.585853	37.741440
2007.584501	259926.459840	37.746458
2009.657476	260255.655326	37.751476
2011.384089	260570.782218	37.756493
2013.218214	260891.658838	37.761511
2015.300425	261207.009441	37.766528
2017.290257	261535.609925	37.771546
2019.281527	261860.831954	37.776564
2021.395753	262177.169200	37.781581
2023.042005	262505.647405	37.786599
2025.047458	262836.380617	37.791616
2026.973870	263170.759323	37.796634
2028.688840	263508.906142	37.801652
2030.575167	263848.524875	37.806669
2032.323502	264206.151180	37.811687
2034.842524	264538.455693	37.816704
2037.010980	264887.963203	37.821722
2039.104956	265231.081245	37.826740
2041.485303	265563.840460	37.831757
2043.524434	265919.593122	37.836775
2045.652761	266259.556539	37.841792
2047.595189	266612.022667	37.846810
2049.739376	266953.050997	37.851828
2051.819918	267311.236836	37.856845
2053.433286	267662.079285	37.861863
2055.512748	268013.254462	37.866880
2057.434942	268372.888689	37.871898
2059.690376	268734.908975	37.876916
2061.859177	269093.945616	37.881933
2063.701745	269470.054425	37.886951
2065.973995	269822.393948	37.891968
2067.934170	270192.209831	37.896986
2069.913179	270562.276922	37.902004
2072.077889	270930.917516	37.907021
2073.599139	271308.678522	37.912039
2075.999776	271689.196136	37.917056
2078.026436	272064.743324	37.922074
2080.237501	272456.468726	37.927092
2082.645699	272822.607130	37.932109
2084.559008	273195.124157	37.937127
2086.599355	273569.526348	37.942144
2088.950904	273950.458705	37.947162
2090.927218	274326.395345	37.952180
2092.981258	274712.709675	37.957197
2094.818258	275095.501966	37.962215
2097.481653	275479.712770	37.967232
2099.542770	275856.728317	37.972250
2101.216609	276241.934359	37.977268
2104.118545	276608.629688	37.982285
2106.349435	276986.050034	37.987303
2108.630450	277348.830003	37.992320
2110.864030	277718.552546	37.997338
2113.267846	278081.008031	38.002356
2115.157497	278452.004300	38.007373
2117.286033	278819.202862	38.012391
2119.253629	279192.193388	38.017408
2121.455162	279543.274380	38.022426
2123.248040	279892.972066	38.027444
2125.712635	280229.963007	38.032461
2127.602212	280575.123266	38.037479
2129.610199	280917.800460	38.042496
2131.610433	281272.900923	38.047514
2133.229855	281618.128914	38.052532
2135.423876	281967.228480	38.057549
2137.334183	282328.718817	38.062567
2139.499591	282683.157166	38.067584
2141.724230	283039.795963	38.072602
2143.619816	283403.116934	38.077620
2146.314533	283762.119359	38.082637
2147.806886	284138.281522	38.087655
2150.353247	284512.167732	38.092672
2152.217701	284882.859368	38.097690
2154.165017	285265.578591	38.102708
2156.506445	285633.221729	38.107725
2158.628633	286023.660406	38.112743
2160.645865	286407.510536	38.117760
2162.801638	286786.562521	38.122778
2164.798481	287182.659274	38.127796
2167.256327	287574.287738	38.132813
2169.585818	287962.278071	38.137831
2171.504936	288357.522020	38.142848
2173.925038	288763.405992	38.147866
2176.119166	289142.855543	38.152884
2178.263587	289545.784623	38.157901
2180.395353	289948.562715	38.162919
2182.816446	290338.211948	38.167936
2185.355092	290736.783697	38.172954
2187.714807	291119.531987	38.177972
2190.291942	291504.963292	38.182989
2192.336320	291896.651301	38.188007
2194.876748	292284.068596	38.193024
2196.774240	292679.563584	38.198042
2198.957389	293068.153947	38.203060
2200.930805	293463.152891	38.208077
2202.959885	293859.539428	38.213095
2205.561637	294253.192587	38.218112
2208.212492	294636.320713	38.223130
2210.635610	295024.996519	38.228148
2213.541932	295392.714417	38.233165
2215.971715	295769.575750	38.238183
2218.511597	296139.179326	38.243200
2220.470980	296512.151104	38.248218
2222.650722	296875.282063	38.253236
2224.715922	297252.528517	38.258253
2226.828547	297643.661467	38.263271
2229.101536	298021.432215	38.268288
2231.169640	298401.952629	38.273306
2232.970746	298786.121587	38.278324
2235.733640	299159.900328	38.283341
2237.644945	299540.468484	38.288359
2239.673977	299924.116080	38.293376
2241.969736	300299.033198	38.298394
2243.613292	300670.064852	38.303412
2245.986564	301020.862099	38.308429
2247.733945	301386.058708	38.313447
2249.956413	301757.148399	38.318464
2252.033460	302124.043660	38.323482
2253.960524	302501.782658	38.328500
2255.827383	302875.694691	38.333517
2257.825391	303266.781398	38.338535
2259.776253	303661.786253	38.343552
2262.224340	304062.375544	38.348570
2264.121634	304474.836953	38.353588
2266.206295	304878.123199	38.358605
2268.240700	305304.429121	38.363623
2270.279574	305730.275777	38.368640
2272.773867	306158.792098	38.373658
2274.463521	306599.550542	38.378676
2276.707702	307039.863954	38.383693
2278.852996	307487.405158	38.388711
2281.292600	307925.220690	38.393728
2283.469219	308374.861946	38.398746
2285.897669	308831.598975	38.403764
2288.725644	309270.668904	38.408781
2291.365845	309728.384932	38.413799
2293.380987	310182.667742	38.418816
2296.293940	310619.661792	38.423834
2298.393303	311076.010483	38.428852
2300.829029	311528.443316	38.433869
2303.468590	311969.386982	38.438887
2306.154373	312416.112542	38.443904
2308.425653	312867.600793	38.448922
2310.594222	313323.319643	38.453940
2313.687432	313748.817852	38.458957
2316.168806	314183.885031	38.463975
2318.387967	314624.503443	38.468992
2321.029680	315064.646603	38.474010
2323.149658	315498.571797	38.479028
2326.111181	315926.901095	38.484045
2328.430836	316353.247668	38.489063
2330.795343	316784.944261	38.494080
2332.961837	317214.384529	38.499098
2334.973505	317660.000399	38.504116
2337.700409	318079.290454	38.509133
2340.028947	318515.683539	38.514151
2342.210735	318963.526682	38.519168
2344.684356	319389.327365	38.524186
2346.870030	319825.152803	38.529204
2348.988479	320268.986875	38.534221
2351.444812	320704.917555	38.539239
2354.017424	321147.557818	38.544256
2356.554320	321584.919024	38.549274
2358.467956	322031.925938	38.554292
2360.967565	322470.202886	38.559309
2363.483435	322905.833810	38.564327
2365.447529	323352.952835	38.569344
2368.015227	323768.431978	38.574362
2370.010003	324193.599516	38.579380
2372.336371	324609.823800	38.584397
2374.693031	325021.546151	38.589415
2377.129757	325433.507687	38.594432
2379.429915	325843.939655	38.599450
2381.826355	326278.886048	38.604468
2383.795392	326692.058039	38.609485
2385.673251	327117.558871	38.614503
2387.886815	327556.742769	38.619520
2390.646570	327993.196560	38.624538
2392.645012	328434.060224	38.629556
2395.131136	328874.437731	38.634573
2397.616076	329334.848902	38.639591
2400.033464	329783.078807	38.644608
2402.395573	330227.454901	38.649626
2404.833145	330684.081544	38.654644
2407.397711	331138.145851	38.659661
2409.915052	331584.926889	38.664679
2412.326491	332045.053414	38.669696
2415.066126	332502.814185	38.674714
2417.007698	332953.436110	38.679732
2419.260475	333420.536526	38.684749
2421.606931	333892.341994	38.689767
2424.149942	334365.204970	38.694784
2426.481006	334836.676315	38.699802
2429.016079	335312.327151	38.704820
2432.050201	335774.260092	38.709837
2434.718394	336251.990721	38.714855
2436.967676	336724.274349	38.719872
2439.858448	337178.171148	38.724890
2442.864497	337636.058343	38.729908
2445.876410	338088.304583	38.734925
2448.544966	338525.849996	38.739943
2451.629845	338975.513967	38.744960
2454.157585	339421.099022	38.749978
2456.506788	339862.215150	38.754996
2459.083423	340299.661350	38.760013
2461.560333	340732.270808	38.765031
2463.442439	341172.029870	38.770048
2466.050291	341616.291684	38.775066
2468.869308	342060.262914	38.780084
2471.217492	342497.094978	38.785101
2473.092314	342943.113564	38.790119
2475.534952	343398.635832	38.795136
2478.362145	343836.194679	38.800154
2480.232501	344296.675374	38.805172
2482.558749	344753.297368	38.810189
2485.176290	345210.453559	38.815207
2487.378923	345672.774860	38.820224
2489.992293	346121.368807	38.825242
2492.621564	346581.051041	38.830260
2495.084111	347050.885496	38.835277
2497.719603	347510.711538	38.840295
2499.659152	347968.993957	38.845312
2502.293761	348420.282700	38.850330
2504.607997	348869.435309	38.855348
2506.704889	349308.870396	38.860365
2509.241173	349748.283108	38.865383
2511.274735	350191.655967	38.870400
2513.096711	350643.512131	38.875418
2516.072742	351101.350283	38.880436
2518.298208	351558.161121	38.885453
2520.885221	352025.140878	38.890471
2523.100857	352503.877711	38.895488
2525.589123	352976.449327	38.900506
2527.696073	353455.753147	38.905524
2529.942185	353949.321688	38.910541
2532.548620	354438.665479	38.915559
2534.891999	354944.240964	38.920576
2537.414840	355433.766162	38.925594
2540.062903	355947.431415	38.930612
2542.516468	356447.415559	38.935629
2545.206241	356958.246371	38.940647
2547.533192	357488.470677	38.945664
2550.165275	358006.000734	38.950682
2552.705956	358529.809092	38.955700
2555.413877	359056.758002	38.960717
2558.077439	359578.276649	38.965735
2560.650795	360115.540072	38.970752
2563.174097	360642.196317	38.975770
2565.758589	361180.943432	38.980788
2568.366150	361711.787573	38.985805
2571.517654	362240.686818	38.990823
2574.127744	362776.670568	38.995840
2577.367912	363291.864313	39.000858
2579.977552	363828.724217	39.005876
2582.281834	364354.840332	39.010893
2584.967471	364877.692297	39.015911
2587.455304	365418.740184	39.020928
2590.331115	365942.133394	39.025946
2592.948373	366484.822858	39.030964
2595.411706	367004.919147	39.035981
2598.154131	367545.672534	39.040999
2600.670221	368093.256013	39.046016
2603.649277	368610.612473	39.051034
2606.330211	369149.477944	39.056052
2608.922629	369680.788829	39.061069
2612.080133	370197.184521	39.066087
2614.361305	370736.068069	39.071104
2617.288490	371263.525402	39.076122
2620.328061	371798.342254	39.081140
2622.636053	372324.438077	39.086157
2625.445393	372846.311968	39.091175
2627.824677	373369.313117	39.096192
2630.348482	373895.507128	39.101210
2633.104469	374414.426433	39.106228
2635.805411	374940.299894	39.111245
2638.805445	375451.657158	39.116263
2641.743604	375976.566236	39.121280
2644.238198	376475.939066	39.126298
2647.237968	376962.286432	39.131316
2649.662742	377440.245130	39.136333
2652.031753	377909.276521	39.141351
2654.497731	378402.134903	39.146368
2656.760631	378875.839712	39.151386
2659.308225	379366.922540	39.156404
2661.776110	379861.512754	39.161421
2664.489521	380355.043020	39.166439
2666.902986	380867.615505	39.171456
2669.126095	381360.550973	39.176474
2671.802968	381870.785191	39.181492
2673.952779	382392.080179	39.186509
2676.645432	382906.813393	39.191527
2679.196950	383439.039654	39.196544
2682.191423	383969.869153	39.201562
2685.090841	384500.477865	39.206580
2686.857799	385040.491480	39.211597
2689.873957	385585.828995	39.216615
2692.645037	386139.821322	39.221632
2695.256783	386693.044198	39.226650
2698.212978	387245.443192	39.231668
2700.684820	387795.526282	39.236685
2703.738053	388342.338476	39.241703
2706.589276	388907.841503	39.246720
2709.544015	389455.337094	39.251738
2712.486511	390008.938483	39.256756
2714.897121	390579.430320	39.261773
2717.837688	391130.503593	39.266791
2720.285487	391700.692344	39.271808
2722.738717	392265.240858	39.276826
2725.738628	392825.889578	39.281844
2728.292095	393402.601895	39.286861
2731.622191	393962.317584	39.291879
2734.419965	394541.381177	39.296896
2737.360836	395105.907204	39.301914
2740.157369	395671.359564	39.306932
2742.457468	396245.654788	39.311949
2745.419179	396807.790738	39.316967
2748.507351	397385.643740	39.321984
2751.551376	397952.641176	39.327002
2754.505160	398511.427871	39.332020
2757.131613	399078.979189	39.337037
2760.018805	399644.045304	39.342055
2762.932751	400212.013165	39.347072
2765.823447	400763.190333	39.352090
2768.684280	401321.411158	39.357108
2771.545601	401885.275996	39.362125
2774.588798	402450.014808	39.367143
2777.391596	403004.159043	39.372160
2779.995595	403565.677141	39.377178
2783.074008	404109.414812	39.382196
2785.699731	404657.676552	39.387213
2788.892470	405206.168474	39.392231
2792.130645	405744.985149	39.397248
2795.149386	406271.557961	39.402266
2797.889672	406762.220584	39.407284
2800.104789	407272.274423	39.412301
2802.859966	407773.210218	39.417319
2805.596437	408276.827668	39.422336
2808.520434	408777.213298	39.427354
2811.127113	409287.957246	39.432372
2813.123754	409798.966587	39.437389
2816.178813	410312.765204	39.442407
2818.300489	410838.640740	39.447424
2820.954043	411365.385942	39.452442
2823.826915	411905.469271	39.457460
2825.972608	412460.509803	39.462477
2828.797315	413008.412095	39.467495
2831.600767	413570.398583	39.472512
2834.068216	414124.469757	39.477530
2836.560448	414705.161571	39.482548
2839.128282	415290.771521	39.487565
2842.298893	415861.094580	39.492583
2844.465699	416456.931691	39.497600
2847.214322	417061.710887	39.502618
2849.970263	417664.296886	39.507636
2852.708278	418282.203327	39.512653
2855.947758	418897.660382	39.517671
2858.723838	419513.405415	39.522688
2861.164297	420133.750882	39.527706
2864.506217	420755.232072	39.532724
2867.799043	421382.103864	39.537741
2870.589149	421997.133113	39.542759
2873.735176	422635.502313	39.547776
2875.832463	423274.098715	39.552794
2879.538353	423892.183445	39.557812
2882.699209	424522.272626	39.562829
2886.324145	425145.155091	39.567847
2889.406057	425763.751954	39.572864
2892.695462	426376.095408	39.577882
2895.836629	426993.793261	39.582900
2898.491247	427608.919430	39.587917
2901.527980	428214.092078	39.592935
2904.366889	428835.594507	39.597952
2906.886404	429447.001219	39.602970
2910.207899	430066.143898	39.607988
2913.212775	430679.800559	39.613005
2915.560417	431310.490739	39.618023
2919.044345	431919.027513	39.623040
2922.074566	432541.145884	39.628058
2925.024953	433157.335698	39.633076
2927.812018	433773.992397	39.638093
2931.001142	434387.075818	39.643111
2933.849782	435009.998587	39.648128
2936.346003	435629.999032	39.653146
2939.833602	436245.826392	39.658164
2942.759624	436875.705145	39.663181
2945.513385	437502.582105	39.668199
2948.574424	438116.759760	39.673216
2951.390660	438719.617685	39.678234
2954.440079	439310.751846	39.683252
2956.965954	439891.523416	39.688269
2959.976703	440460.963298	39.693287
2963.002564	441045.983101	39.698304
2965.617738	441638.902096	39.703322
2969.044577	442204.032834	39.708340
2972.066926	442792.201012	39.713357
2974.914266	443374.560100	39.718375
2977.947693	443949.939487	39.723392
2980.403417	444533.345026	39.728410
2984.290918	445114.434035	39.733428
2986.393785	445714.978214	39.738445
2989.935608	446311.837037	39.743463
2992.871047	446913.585891	39.748480
2995.562760	447515.459183	39.753498
2998.299128	448120.853366	39.758516
3001.112940	448734.824782	39.763533
3003.822567	449353.250825	39.768551
3007.269489	449969.468461	39.773568
3009.694569	450614.074291	39.778586
3012.849413	451250.296674	39.783604
3015.743968	451889.680543	39.788621
3018.858638	452522.837255	39.793639
3022.020923	453157.588326	39.798656
3024.728782	453804.589960	39.803674
3027.847594	454456.366234	39.808692
3031.204681	455110.312555	39.813709
3033.864564	455765.514033	39.818727
3036.863333	456417.049993	39.823744
3040.219468	457079.743572	39.828762
3043.631151	457733.300853	39.833780
3046.658180	458400.915075	39.838797
3049.765379	459056.049907	39.843815
3053.374117	459711.642374	39.848832
3055.648906	460382.148688	39.853850
3058.836329	461046.368484	39.858868
3061.824100	461713.634929	39.863885
3064.598151	462382.584024	39.868903
3068.111839	463067.684096	39.873920
3070.674937	463756.251319	39.878938
3073.998253	464427.933162	39.883956
3076.803410	465120.060124	39.888973
3080.050654	465804.659389	39.893991
3083.184721	466482.729860	39.899008
3086.128169	467183.466933	39.904026
3089.039085	467882.617983	39.909044
3092.064464	468585.975717	39.914061
3094.822277	469291.324361	39.919079
3097.826887	470010.010959	39.924096
3100.978553	470726.980617	39.929114
3104.361310	471430.134839	39.934132
3107.300094	472146.937051	39.939149
3110.653412	472860.968781	39.944167
3113.774251	473577.944831	39.949184
3116.770362	474266.804530	39.954202
3120.095630	474941.887695	39.959220
3122.892952	475622.390709	39.964237
3125.925256	476273.765004	39.969255
3128.783091	476957.246462	39.974272
3131.675154	477644.389319	39.979290
3135.123332	478312.717427	39.984308
3138.181970	478997.714652	39.989325
3141.095625	479685.238357	39.994343
3144.287688	480377.394589	39.999360
3147.563504	481070.625099	40.004378
3150.222861	481758.369184	40.009396
3153.821007	482459.130980	40.014413
3156.765695	483155.018324	40.019431
3159.500500	483882.447406	40.024448
3162.716509	484598.908458	40.029466
3166.114689	485316.627807	40.034484
3169.216649	486030.425896	40.039501
3172.325371	486766.225970	40.044519
3175.378803	487488.920396	40.049536
3178.444528	488229.015778	40.054554
3181.616307	488974.218548	40.059572
3184.767447	489711.766733	40.064589
3188.041067	490466.088716	40.069607
3191.498737	491204.388438	40.074624
3194.450287	491970.066458	40.079642
3197.889221	492720.027969	40.084660
3200.888800	493486.898506	40.089677
3204.047492	494252.853365	40.094695
3206.937548	495019.576348	40.099712
3210.116241	495788.241660	40.104730
3213.544001	496557.087683	40.109748
3217.210720	497336.417490	40.114765
3220.830221	498118.145025	40.119783
3223.964015	498880.424918	40.124800
3227.021552	499670.151992	40.129818
3230.657841	500436.982008	40.134836
3234.581604	501192.525443	40.139853
3237.856639	501949.956852	40.144871
3241.929782	502707.027740	40.149888
3245.248852	503471.151792	40.154906
3248.443998	504215.828018	40.159924
3251.871365	504972.449318	40.164941
3254.891190	505735.966836	40.169959
3258.054718	506470.961933	40.174976
3261.331297	507237.754583	40.179994
3264.673552	507990.271002	40.185012
3267.956455	508750.283346	40.190029
3271.020436	509501.112414	40.195047
3274.433428	510265.376956	40.200064
3277.944260	511020.862467	40.205082
3281.112049	511760.424434	40.210100
3284.733558	512523.141874	40.215117
3287.775768	513260.337333	40.220135
3291.055327	514008.107955	40.225152
3293.939823	514759.439115	40.230170
3297.405274	515467.917451	40.235188
3300.369878	516186.382265	40.240205
3303.472082	516891.931829	40.245223
3306.806186	517601.853366	40.250240
3310.258236	518309.758760	40.255258
3313.085081	519036.292595	40.260276
3316.499229	519755.237478	40.265293
3319.026523	520495.723900	40.270311
3322.273428	521223.657742	40.275328
3324.976103	521974.185373	40.280346
3328.082898	522731.774535	40.285364
3331.142588	523510.411611	40.290381
3333.991770	524294.691275	40.295399
3337.369008	525075.521774	40.300416
3340.252483	525861.685742	40.305434
3343.660924	526670.564181	40.310452
3346.714528	527478.600722	40.315469
3349.939241	528298.716876	40.320487
3353.445320	529131.649230	40.325504
3356.615686	529952.393789	40.330522
3360.417683	530794.263481	40.335540
3364.008537	531630.426682	40.340557
3367.150921	532475.081918	40.345575
3371.007235	533301.085460	40.350592
3374.324790	534146.831460	40.355610
3377.750701	534991.304839	40.360628
3381.178287	535830.240095	40.365645
3384.402584	536680.194561	40.370663
3387.959239	537532.064304	40.375680
3391.451790	538401.728605	40.380698
3394.837085	539259.926109	40.385716
3398.704734	540107.975660	40.390733
3402.023831	540976.562576	40.395751
3405.962536	541827.727424	40.400768
3409.171927	542682.383635	40.405786
3412.885003	543535.652455	40.410804
3416.243408	544394.517626	40.415821
3419.763424	545261.715991	40.420839
3423.407953	546111.121731	40.425856
3426.880574	546975.357212	40.430874
3430.365435	547833.196976	40.435892
3433.918397	548693.089948	40.440909
3437.388764	549539.757531	40.445927
3441.135258	550392.019761	40.450944
3444.899395	551233.508998	40.455962
3448.607298	552079.588186	40.460980
3452.151086	552939.381942	40.465997
3455.557473	553767.343485	40.471015
3459.071106	554634.638802	40.476032
3462.652448	555478.726124	40.481050
3465.808716	556306.730912	40.486068
3469.445079	557163.086117	40.491085
3473.318114	557996.865532	40.496103
3476.987812	558837.468923	40.501120
3480.006330	559662.470510	40.506125
3483.017312	560432.919484	40.511130
3486.749879	561164.386464	40.516135
3489.482632	561836.023441	40.521140
3492.699749	562443.268460	40.526144
3495.730429	562996.672060	40.531149
3498.286305	563468.810407	40.536154
3500.791094	563905.752611	40.541159
3502.700608	564292.918295	40.546164
3505.098424	564594.853230	40.551168
3506.888296	564873.134886	40.556173
3508.500583	565086.260973	40.561178
3510.214318	565259.343952	40.566183
3511.877454	565397.702137	40.571188
3513.055804	565476.403334	40.576192
3514.079421	565528.412931	40.581197
3515.310347	565547.423571	40.586202
3516.394948	565530.164434	40.591207
3516.828764	565497.381984	40.596212
3517.820908	565431.242498	40.601216
3518.855280	565324.870822	40.606221
3519.308715	565208.558950	40.611226
3520.097341	565066.182337	40.616231
3520.248502	564909.286368	40.621236
3520.745339	564729.750418	40.626240
3521.160781	564537.420740	40.631245
3521.507050	564341.318474	40.636250
3521.402531	564107.425273	40.641255
3521.814485	563885.243095	40.646260
3522.097432	563651.180104	40.651264
3522.096527	563387.867123	40.656269
3522.291127	563140.147069	40.661274
3522.057852	562877.214013	40.666279
3521.855648	562622.287436	40.671284
3521.879135	562349.875735	40.676288
3521.882363	562084.419775	40.681293
3521.797431	561812.619713	40.686298
3521.883896	561533.425733	40.691303
3521.874537	561259.182699	40.696308
3521.686989	560978.256124	40.701312
3521.403342	560693.204281	40.706317
3520.967624	560420.777020	40.711322
3521.510882	560132.910515	40.716327
3520.778136	559849.626962	40.721332
3520.782893	559569.196399	40.726336
3520.773148	559296.175658	40.731341
3520.473028	559027.229941	40.736346
3520.613370	558729.715697	40.741351
3520.284611	558453.198806	40.746356
3519.906930	558188.132614	40.751360
3519.617315	557897.578135	40.756365
3519.595579	557631.335668	40.761370
3519.289975	557370.075816	40.766375
3518.818630	557116.201177	40.771380
3518.726749	556830.889435	40.776384
3518.722362	556576.981767	40.781389
3518.238971	556326.171668	40.786394
3518.305735	556067.653598	40.791399
3517.785075	555822.035909	40.796404
3517.338899	555574.989810	40.801408
3517.414070	555328.109241	40.806413
3517.245780	555093.369549	40.811418
3517.141093	554852.158945	40.816423
3516.594293	554621.153816	40.821428
3516.555199	554388.500852	40.826432
3516.598327	554161.683047	40.831437
3516.019325	553938.642721	40.836442
3515.820324	553706.760680	40.841447
3515.714888	553492.013140	40.846452
3515.113451	553275.120946	40.851456
3515.402671	553064.138893	40.856461
3514.950205	552865.581336	40.861466
3515.146989	552641.136924	40.866471
3514.822968	552451.180819	40.871476
3514.641997	552246.113727	40.876480
3514.357869	552045.096435	40.881485
3513.994699	551853.372711	40.886490
3513.935585	551655.493145	40.891495
3513.929105	551463.960158	40.896500
3513.787526	551283.092591	40.901504
3513.609326	551104.852391	40.906509
3513.082990	550921.064066	40.911514
3512.912031	550728.689544	40.916519
3512.819371	550567.080916	40.921524
3512.360857	550388.472529	40.926528
3512.311733	550240.982442	40.931533
3511.934066	550078.202344	40.936538
3512.071924	549909.485282	40.941543
3512.152904	549747.184075	40.946548
3511.759545	549590.456577	40.951552
3511.662771	549448.062815	40.956557
3511.387689	549289.698531	40.961562
3511.353895	549132.909279	40.966567
3511.003317	549005.690889	40.971572
3511.016405	548862.062865	40.976576
3510.726432	548708.539383	40.981581
3510.661224	548574.660988	40.986586
3510.657928	548431.485526	40.991591
3510.428253	548310.045754	40.996596
3510.231508	548178.909806	41.001600
3510.012806	548049.391162	41.006605
3509.894027	547922.934217	41.011610
3509.964062	547795.891168	41.016615
3509.886753	547674.018281	41.021620
3509.717997	547544.790107	41.026624
3509.468435	547435.762034	41.031629
3509.551395	547332.181987	41.036634
3509.601671	547202.159105	41.041639
3509.175401	547094.367755	41.046644
3509.391386	546979.458396	41.051648
3508.985527	546868.280490	41.056653
3509.112225	546767.112258	41.061658
3509.245317	546646.762274	41.066663
3508.904943	546546.827251	41.071668
3508.732679	546440.959459	41.076672
3509.049406	546333.246995	41.081677
3508.631115	546228.880339	41.086682
3508.814478	546129.213031	41.091687
3508.322467	546036.213672	41.096692
3508.366004	545935.709068	41.101696
3508.175980	545830.798753	41.106701
3508.227938	545744.122105	41.111706
3508.404330	545634.760991	41.116711
3508.025003	545545.425572	41.121716
3508.090635	545451.324837	41.126720
3507.917550	545372.657093	41.131725
3507.850872	545278.677130	41.136730
3507.867670	545185.137685	41.141735
3507.992518	545102.282149	41.146740
3507.794583	545012.208133	41.151744
3507.707387	544931.909130	41.156749
3507.080069	544843.264906	41.161754
3507.863130	544750.611206	41.166759
3507.212053	544676.760466	41.171764
3507.331270	544602.434240	41.176768
3507.151687	544522.854357	41.181773
3507.205753	544442.479897	41.186778
3507.255891	544365.841264	41.191783
3507.282967	544298.191652	41.196788
3507.240923	544209.299687	41.201792
3507.106079	544131.881371	41.206797
3506.706690	544057.129566	41.211802
3507.172087	543986.531744	41.216807
3506.974656	543914.372410	41.221812
3506.915801	543853.802000	41.226816
3506.641044	543776.000080	41.231821
3506.876508	543699.934527	41.236826
3506.884933	543639.655515	41.241831
3506.682208	543568.555508	41.246836
3506.936179	543498.947998	41.251840
3506.659545	543434.119115	41.256845
3506.397999	543362.573060	41.261850
3506.958589	543289.533612	41.266855
3506.507290	543225.387738	41.271860
3506.751629	543157.395693	41.276864
3506.572545	543084.977015	41.281869
3506.591932	543023.280173	41.286874
3506.453232	542957.720612	41.291879
3506.232123	542901.816729	41.296884
3506.434165	542835.243528	41.301888
3506.879099	542773.175472	41.306893
3506.598947	542715.260742	41.311898
3506.321884	542659.314309	41.316903
3505.922954	542587.988206	41.321908
3506.252785	542518.010723	41.326912
3506.335440	542472.811136	41.331917
3506.133261	542421.143458	41.336922
3506.532092	542350.750382	41.341927
3505.933195	542309.899058	41.346932
3506.064362	542236.770882	41.351936
3506.009153	542174.476466	41.356941
3505.704409	542123.126904	41.361946
3506.306790	542063.353525	41.366951
3506.158914	542017.078235	41.371956
3506.088034	541953.523138	41.376960
3505.890224	541887.008924	41.381965
3505.829031	541841.375760	41.386970
3506.032048	541780.604087	41.391975
3505.738636	541746.266684	41.396980
3505.928284	541682.012882	41.401984
3506.128026	541621.140100	41.406989
3505.717005	541577.631555	41.411994
3505.559465	541510.553906	41.416999
3505.816689	541462.597155	41.422004
3505.595894	541410.020089	41.427008
3505.825595	541367.369002	41.432013
3505.901629	541306.564991	41.437018
3505.975747	541249.295488	41.442023
3505.661153	541214.455296	41.447028
3505.707420	541157.290829	41.452032
3506.064345	541100.379999	41.457037
3505.818670	541041.191037	41.462042
3505.591749	541000.428827	41.467047
3505.676385	540963.303259	41.472052
3505.329523	540903.927779	41.477056
3505.398379	540851.151496	41.482061
3505.421063	540814.843249	41.487066
3505.451939	540762.325127	41.492071
3505.387210	540718.254421	41.497076
3505.376369	540664.379215	41.502080
3505.641196	540623.891718	41.507085
3505.183145	540581.700574	41.512090
3505.341010	540536.483276	41.517095
3505.284774	540493.470956	41.522100
3505.293769	540447.519502	41.527104
3505.535235	540395.269785	41.532109
3505.589327	540351.886157	41.537114
3505.524938	540306.349834	41.542119
3505.393923	540277.891359	41.547124
3505.261196	540223.225917	41.552128
3505.402093	540170.486363	41.557133
3505.070493	540137.363221	41.562138
3505.480337	540088.570044	41.567143
3505.467060	540045.347672	41.572148
3505.498949	539992.877209	41.577152
3505.186394	539964.446837	41.582157
3505.023439	539911.905897	41.587162
3505.382351	539871.603501	41.592167
3505.109417	539823.018382	41.597172
3504.878246	539790.282580	41.602176
3505.041609	539740.214316	41.607181
3504.945279	539714.274156	41.612186
3504.974901	539668.721052	41.617191
3505.164577	539631.323120	41.622196
3505.184718	539583.044389	41.627200
3504.978039	539563.837608	41.632205
3504.792127	539522.660941	41.637210
3505.311068	539486.119569	41.642215
3504.801318	539446.306829	41.647220
3504.750683	539412.531710	41.652224
3504.859208	539368.328686	41.657229
3504.452096	539335.367216	41.662234
3504.686149	539296.244492	41.667239
3504.510907	539272.134000	41.672244
3504.987012	539235.295802	41.677248
3505.076076	539205.386554	41.682253
3504.783934	539170.083599	41.687258
3505.025584	539126.414318	41.692263
3504.917346	539090.981112	41.697268
3504.823943	539047.314062	41.702272
3504.910323	539020.838840	41.707277
3505.038490	538983.903530	41.712282
3504.742864	538953.246594	41.717287
3504.433251	538922.894806	41.722292
3504.628926	538879.888582	41.727296
3504.426578	538856.337213	41.732301
3504.646046	538833.931139	41.737306
3505.066064	538787.758181	41.742311
3504.801366	538766.893047	41.747316
3504.773830	538728.820217	41.752320
3504.549571	538690.677385	41.757325
3504.871406	538664.770335	41.762330
3504.731104	538623.483015	41.767335
3504.694159	538594.602499	41.772340
3504.775871	538551.461856	41.777344
3505.021602	538513.951308	41.782349
3504.868375	538478.321779	41.787354
3505.007662	538444.160976	41.792359
3504.579669	538419.735569	41.797364
3504.605687	538385.340029	41.802368
3504.673185	538346.645201	41.807373
3504.497531	538320.311180	41.812378
3504.580544	538279.947166	41.817383
3504.395321	538257.351700	41.822388
3504.467542	538224.160545	41.827392
3504.663847	538196.656468	41.832397
3504.352625	538171.909191	41.837402
3504.345343	538137.013330	41.842407
3504.181266	538112.444707	41.847412
3504.473727	538081.036522	41.852416
3504.675354	538062.874362	41.857421
3504.545271	538038.704270	41.862426
3504.656891	537995.506821	41.867431
3504.534146	537972.244517	41.872436
3504.059922	537943.179366	41.877440
3504.814063	537911.697859	41.882445
3504.486913	537891.144413	41.887450
3504.424720	537845.448845	41.892455
3504.327974	537822.990259	41.897460
3504.449897	537784.436911	41.902464
3504.481505	537768.472933	41.907469
3504.490937	537734.836103	41.912474
3504.833907	537710.136183	41.917479
3504.917750	537670.730000	41.922484
3504.957810	537642.593068	41.927488
3504.859778	537597.710488	41.932493
3504.637106	537581.533985	41.937498
3504.882056	537536.344491	41.942503
3505.175435	537504.177407	41.947508
3504.590362	537468.361250	41.952512
3504.640012	537433.606295	41.957517
3504.463128	537410.402196	41.962522
3504.588712	537376.746217	41.967527
3504.124660	537338.284363	41.972532
3504.367623	537304.963209	41.977536
3504.542707	537279.228519	41.982541
3504.269590	537263.211167	41.987546
3504.421147	537230.712387	41.992551
3504.369693	537214.003375	41.997556
3504.353209	537177.541100	42.002560
3504.369948	537144.861424	42.007565
3504.294230	537124.721754	42.012570
3504.535557	537086.602325	42.017575
3504.609750	537067.196474	42.022580
3504.456570	537036.563667	42.027584
3504.808987	537005.143795	42.032589
3504.307385	536982.747965	42.037594
3504.198408	536942.107722	42.042599
3504.147426	536917.721325	42.047604
3504.430346	536896.969096	42.052608
3504.512556	536864.783539	42.057613
3504.382642	536845.106628	42.062618
3504.592377	536808.961266	42.067623
3504.397712	536780.102244	42.072628
3504.153103	536756.655322	42.077632
3504.308563	536724.255863	42.082637
3504.271684	536708.251096	42.087642
3504.184135	536693.062437	42.092647
3504.262157	536654.563687	42.097652
3504.305244	536632.283278	42.102656
3504.406417	536611.559391	42.107661
3504.055006	536581.563095	42.112666
3504.239222	536545.471653	42.117671
3504.257842	536537.791718	42.122676
3504.255818	536507.588530	42.127680
3504.753054	536475.437572	42.132685
3504.545321	536452.135878	42.137690
3504.244205	536426.323500	42.142695
3504.265625	536389.398783	42.147700
3504.301685	536367.321134	42.152704
3504.597482	536336.868501	42.157709
3504.174008	536316.681719	42.162714
3504.265746	536289.998879	42.167719
3504.399885	536254.773315	42.172724
3504.153683	536237.538423	42.177728
3504.488032	536200.260737	42.182733
3504.091221	536178.604799	42.187738
3504.184565	536153.285210	42.192743
3504.222985	536142.823948	42.197748
3504.357509	536107.648495	42.202752
3504.439336	536070.662955	42.207757
3504.273539	536059.779331	42.212762
3504.339299	536018.654435	42.217767
3504.431249	536003.992326	42.222772
3504.146504	535983.126551	42.227776
3504.270716	535952.498240	42.232781
3504.212095	535926.394142	42.237786
3504.222450	535898.006150	42.242791
3504.196387	535873.210074	42.247796
3504.272687	535838.901879	42.252800
3504.718841	535826.860651	42.257805
3504.020424	535799.796752	42.262810
3504.246891	535775.011111	42.267815
3504.427640	535744.171407	42.272820
3503.926036	535727.481416	42.277824
3504.597669	535689.341011	42.282829
3504.112814	535664.364562	42.287834
3504.235016	535641.211529	42.292839
3504.496327	535616.167571	42.297844
3504.232925	535585.751329	42.302848
3504.408591	535558.498334	42.307853
3504.146500	535532.425727	42.312858
3504.211901	535506.402335	42.317863
3504.212515	535484.227996	42.322868
3504.143181	535462.014171	42.327872
3503.871451	535438.519008	42.332877
3503.975920	535424.511017	42.337882
3503.850314	535396.093078	42.342887
3504.103112	535382.364673	42.347892
3503.769814	535367.971221	42.352896
3504.410681	535331.501680	42.357901
3503.809306	535318.817443	42.362906
3504.055744	535279.278389	42.367911
3503.714901	535280.746792	42.372916
3503.803853	535256.386149	42.377920
3503.865051	535250.971882	42.382925
3503.871352	535231.574443	42.387930
3504.050449	535207.351010	42.392935
3503.833060	535183.493283	42.397940
3503.800254	535168.597537	42.402944
3504.179360	535153.384106	42.407949
3503.877583	535129.842708	42.412954
3504.204837	535113.122061	42.417959
3504.040975	535083.800368	42.422964
3503.815508	535071.864711	42.427968
3503.937172	535020.726807	42.432973
3504.252372	535026.385125	42.437978
3504.430815	534990.492998	42.442983
3504.184713	534976.590526	42.447988
3504.164835	534941.790405	42.452992
3504.339801	534915.597158	42.457997
3504.138465	534902.546266	42.463002
3504.011132	534875.794575	42.468007
3504.035350	534841.593417	42.473012
3503.993560	534836.195284	42.478016
3503.998575	534806.088668	42.483021
3503.742313	534792.389689	42.488026
3503.877646	534765.798343	42.493031
3503.726635	534750.870364	42.498036
3503.807958	534737.117976	42.503040
3504.260841	534712.345354	42.508045
3503.518171	534696.955190	42.513050
3503.945029	534670.469143	42.518055
3504.252629	534668.652728	42.523060
3503.822770	534628.713766	42.528064
3504.148955	534607.598016	42.533069
3503.997756	534594.538939	42.538074
3504.225439	534567.275970	42.543079
3503.909194	534551.414143	42.548084
3503.885869	534534.495713	42.553088
3504.089593	534505.872535	42.558093
3503.633965	534492.002743	42.563098
3503.806629	534478.791348	42.568103
3503.967643	534454.114960	42.573108
3503.647646	534437.293831	42.578112
3504.121405	534420.448249	42.583117
3503.750723	534405.100024	42.588122
3503.917418	534385.423595	42.593127
3503.998611	534357.627748	42.598132
3504.160008	534353.258143	42.603136
3504.218232	534316.272123	42.608141
3503.868116	534307.740088	42.613146
3504.075145	534271.892289	42.618151
3504.111392	534260.924941	42.623156
3503.846235	534238.235152	42.628160
3504.189820	534213.226431	42.633165
3504.230675	534194.327382	42.638170
3504.121513	534169.794277	42.643175
3504.184880	534140.839000	42.648180
3503.887345	534134.925372	42.653184
3504.241824	534108.601353	42.658189
3503.943031	534078.642372	42.663194
3504.055986	534057.155448	42.668199
3504.221583	534029.648767	42.673204
3504.185609	534013.540022	42.678208
3503.893057	533993.430525	42.683213
3503.683771	533966.791245	42.688218
3503.840043	533939.487942	42.693223
3504.072530	533938.491579	42.698228
3503.761208	533906.311525	42.703232
3503.977405	533886.323539	42.708237
3503.911580	533873.351390	42.713242
3503.866095	533851.080960	42.718247
3503.801181	533843.059269	42.723252
3503.834912	533821.028858	42.728256
3504.070619	533811.039998	42.733261
3503.840295	533780.513933	42.738266
3503.937641	533764.636441	42.743271
3503.848902	533750.303854	42.748276
3503.785566	533730.713470	42.753280
3503.730183	533721.225217	42.758285
3503.806842	533695.550614	42.763290
3504.048059	533677.528572	42.768295
3503.907631	533648.149932	42.773300
3504.004511	533643.739809	42.778304
3503.957713	533614.598892	42.783309
3503.827117	533604.819351	42.788314
3503.842544	533579.507857	42.793319
3504.024025	533551.037983	42.798324
3503.901671	533554.088572	42.803329
3504.274389	533515.636438	42.808333
3503.981112	533512.449854	42.813338
3503.965219	533486.486428	42.818343
3503.881221	533458.007828	42.823348
3503.926341	533440.875312	42.828353
3503.873605	533424.212907	42.833357
3503.832260	533398.202838	42.838362
3503.994757	533370.644960	42.843367
3504.187002	533348.336231	42.848372
3503.852424	533341.266233	42.853377
3504.183213	533314.439429	42.858381
3503.965017	533291.488237	42.863386
3503.741264	533261.768406	42.868391
3504.145467	533255.996114	42.873396
3503.857659	533227.751381	42.878401
3504.191199	533208.148125	42.883405
3503.726943	533194.379566	42.888410
3504.107094	533164.917726	42.893415
3503.780401	533139.255439	42.898420
3503.985471	533126.947112	42.903425
3503.866132	533117.519118	42.908429
3503.820423	533100.653178	42.913434
3503.768157	533069.036667	42.918439
3503.985710	533062.182384	42.923444
3504.013417	533040.101297	42.928449
3504.079271	533008.011318	42.933453
3504.296560	533002.824191	42.938458
3503.905073	532965.198759	42.943463
3504.146698	532951.621528	42.948468
3503.738175	532936.328344	42.953473
3504.156791	532913.781132	42.958477
3504.155284	532879.630229	42.963482
3504.032776	532858.229384	42.968487
3504.100460	532842.355638	42.973492
3503.865132	532816.880456	42.978497
3504.249261	532798.481168	42.983501
3503.548473	532773.130006	42.988506
3503.930422	532761.197593	42.993511
3503.811213	532738.280457	42.998516
3503.710330	532732.537288	43.003521
3503.671803	532701.625142	43.008525
3503.633921	532698.852703	43.013530
3503.863233	532671.333546	43.018535
3503.767791	532644.370877	43.023540
3503.605191	532639.092114	43.028545
3503.808260	532629.814944	43.033549
3503.660726	532596.646392	43.038554
3503.785642	532587.735196	43.043559
3503.998046	532569.059655	43.048564
3503.766506	532561.265723	43.053569
3503.658677	532536.931908	43.058573
3503.903066	532522.646574	43.063578
3504.136984	532490.680526	43.068583
3503.786719	532480.480309	43.073588
3503.597086	532445.903499	43.078593
3504.109028	532444.307139	43.083597
3503.703659	532430.882241	43.088602
3503.983465	532391.734720	43.093607
3503.638890	532386.838284	43.098612
3503.600187	532377.397094	43.103617
3504.135991	532352.304478	43.108621
3504.083107	532342.511858	43.113626
3503.763839	532318.261643	43.118631
3503.869323	532306.827277	43.123636
3503.897877	532280.299074	43.128641
3504.068453	532268.349174	43.133645
3503.828446	532247.117626	43.138650
3503.847127	532229.533259	43.143655
3503.992324	532221.224910	43.148660
3503.510345	532200.132589	43.153665
3503.956066	532177.024287	43.158669
3503.965857	532158.986547	43.163674
3503.730205	532139.067739	43.168679
3503.792212	532109.957326	43.173684
3503.733280	532106.480797	43.178689
3503.913520	532080.837679	43.183693
3503.735491	532060.960185	43.188698
3503.692370	532052.833081	43.193703
3504.026025	532021.658667	43.198708
3504.155382	532003.803939	43.203713
3503.453132	531987.949976	43.208717
3503.392030	531957.696716	43.213722
3503.555629	531946.505514	43.218727
3503.791424	531951.571241	43.223732
3503.658501	531926.331028	43.228737
3503.938364	531908.300833	43.233741
3503.782878	531898.574675	43.238746
3503.903014	531861.775118	43.243751
3503.841845	531848.396358	43.248756
3503.770972	531838.959928	43.253761
3503.565587	531819.389588	43.258765
3503.867960	531806.812225	43.263770
3503.807887	531789.239809	43.268775
3503.884539	531769.271164	43.273780
3503.551682	531764.978960	43.278785
3503.895738	531732.286623	43.283789
3503.919552	531721.167879	43.288794
3503.766172	531700.022940	43.293799
3503.901134	531686.966706	43.298804
3503.920761	531675.545449	43.303809
3504.099580	531648.891373	43.308813
3503.447608	531637.879387	43.313818
3503.709878	531600.298892	43.318823
3504.005577	531595.301001	43.323828
3503.795328	531580.884573	43.328833
3503.906211	531552.725352	43.333837
3504.049157	531548.458928	43.338842
3503.891108	531505.589088	43.343847
3503.738758	531503.137675	43.348852
3503.950330	531474.962399	43.353857
3503.656612	531470.866023	43.358861
3503.397326	531464.288510	43.363866
3503.777855	531425.072122	43.368871
3503.797778	531410.669679	43.373876
3503.367470	531402.755010	43.378881
3503.654741	531388.057666	43.383885
3503.302920	531374.522343	43.388890
3503.639922	531357.897172	43.393895
3503.679914	531347.584001	43.398900
3503.240828	531331.131998	43.403905
3503.422196	531316.754475	43.408909
3503.363294	531304.688537	43.413914
3503.618578	531307.124099	43.418919
3503.637985	531294.136327	43.423924
3503.454516	531272.692416	43.428929
3504.005834	531257.953214	43.433933
3503.809997	531242.271069	43.438938
3503.457113	531226.866358	43.443943
3503.487007	531214.129488	43.448948
3503.372273	531191.714623	43.453953
3503.982117	531167.416810	43.458957
3503.567173	531169.453080	43.463962
3503.678388	531133.512151	43.468967
3503.803740	531126.469494	43.473972
3503.306318	531129.731416	43.478977
3503.503338	531099.233594	43.483981
3503.359376	531095.467127	43.488986
3503.646181	531076.727519	43.493991
3503.538455	531076.290010	43.498996
3503.303722	531048.336089	43.504001
3503.281433	531034.596806	43.509005
3503.266569	531035.559339	43.514010
3503.864831	531028.492414	43.519015
3503.919839	531006.505187	43.524020
3503.385660	530993.301512	43.529025
3503.736382	530976.774821	43.534029
3503.567177	530972.961789	43.539034
3503.592975	530952.191724	43.544039
3503.590102	530930.870377	43.549044
3503.644511	530927.830406	43.554049
3503.362353	530908.119482	43.559053
3503.710117	530914.431002	43.564058
3503.669952	530892.963920	43.569063
3503.412339	530869.611180	43.574068
3503.255756	530856.802442	43.579073
3503.808238	530851.056359	43.584077
3503.674011	530842.033550	43.589082
3503.759044	530821.708688	43.594087
3503.720486	530813.630744	43.599092
3503.885463	530789.907930	43.604097
3504.101129	530767.238128	43.609101
3503.586682	530762.115395	43.614106
3503.724381	530729.403058	43.619111
3503.834186	530730.093270	43.624116
3503.685252	530702.529383	43.629121
3503.788230	530691.094234	43.634125
3503.569414	530680.164682	43.639130
3503.575867	530652.626673	43.644135
3503.759812	530634.660702	43.649140
3503.364546	530641.696103	43.654145
3503.572773	530606.243903	43.659149
3503.182093	530605.699524	43.664154
3503.625251	530597.545326	43.669159
3503.872794	530580.377675	43.674164
3503.455092	530546.085347	43.679169
3503.532769	530547.033283	43.684173
3503.173927	530542.239573	43.689178
3503.459085	530523.145874	43.694183
3503.632318	530505.585668	43.699188
3503.464258	530495.607986	43.704193
3503.673095	530489.612926	43.709197
3503.493054	530468.672647	43.714202
3503.166489	530456.749419	43.719207
3503.620021	530440.155387	43.724212
3503.430967	530456.606947	43.729217
3503.491497	530422.137701	43.734221
3503.291952	530405.747916	43.739226
3503.401446	530405.326581	43.744231
3503.376684	530397.549409	43.749236
3503.392106	530389.967992	43.754241
3503.696475	530371.831103	43.759245
3503.446121	530357.419886	43.764250
3503.311149	530358.704612	43.769255
3503.475823	530344.935174	43.774260
3503.434379	530316.545171	43.779265
3503.319161	530300.243003	43.784269
3503.450976	530313.157555	43.789274
3503.428092	530292.091143	43.794279
3503.538786	530271.812041	43.799284
3503.159831	530272.175304	43.804289
3503.183916	530263.177667	43.809293
3503.226336	530268.173451	43.814298
3503.441750	530251.263160	43.819303
3503.627989	530230.769951	43.824308
3503.521490	530228.159505	43.829313
3503.733120	530223.629224	43.834317
3503.460794	530194.719683	43.839322
3503.374494	530188.720630	43.844327
3503.249009	530179.746587	43.849332
3502.949053	530193.335827	43.854337
3503.185704	530173.996730	43.859341
3503.385065	530167.800931	43.864346
3503.431445	530136.415537	43.869351
3503.808807	530139.337273	43.874356
3503.535794	530132.357139	43.879361
3503.558662	530107.796771	43.884365
3503.598620	530102.283015	43.889370
3503.505433	530095.324969	43.894375
3503.704657	530068.766042	43.899380
3503.510607	530061.773395	43.904385
3503.772981	530044.602816	43.909389
3503.400150	530032.838164	43.914394
3503.587014	530011.081346	43.919399
3503.690817	530010.105081	43.924404
3503.700648	529989.791029	43.929409
3503.759623	529966.538490	43.934413
3503.517952	529964.606245	43.939418
3503.559563	529946.459870	43.944423
3503.705015	529918.140664	43.949428
3503.476842	529913.477694	43.954433
3503.758883	529905.752843	43.959437
3503.615203	529887.635687	43.964442
3503.432105	529866.897207	43.969447
3503.530053	529862.132144	43.974452
3503.411413	529853.864246	43.979457
3503.585258	529832.210298	43.984461
3503.729782	529827.134685	43.989466
3503.697665	529805.816434	43.994471
3503.780674	529790.139290	43.999476
3503.325938	529782.530836	44.004481
3503.529889	529772.544423	44.009485
3503.491014	529752.288293	44.014490
3503.839946	529741.318876	44.019495
3503.716143	529727.897675	44.024500
3503.646869	529701.481629	44.029505
3503.846927	529679.671738	44.034509
3503.443399	529686.254099	44.039514
3503.637181	529664.141998	44.044519
3503.693971	529643.567426	44.049524
3503.540635	529651.474570	44.054529
3503.643648	529611.185859	44.059533
3503.387475	529606.224041	44.064538
3503.659883	529594.104419	44.069543
3503.462121	529585.141461	44.074548
3503.578260	529568.953557	44.079553
3503.585543	529548.386686	44.084557
3503.435454	529548.208482	44.089562
3503.450585	529517.332098	44.094567
3503.470347	529499.693967	44.099572
3503.513114	529502.264466	44.104577
3503.462680	529485.597499	44.109581
3503.514850	529483.416625	44.114586
3503.306836	529469.098961	44.119591
3503.614919	529460.207568	44.124596
3503.273579	529469.407791	44.129601
3503.521957	529428.186081	44.134605
3503.494327	529430.767719	44.139610
3503.591822	529424.789854	44.144615
3503.463008	529412.632450	44.149620
3503.530585	529391.853721	44.154625
3503.557211	529370.778251	44.159629
3503.615191	529376.883542	44.164634
3503.626947	529340.044676	44.169639
3503.879597	529336.973063	44.174644
3503.825358	529324.803804	44.179649
3504.047117	529297.330453	44.184653
3503.505544	529293.121087	44.189658
3503.828131	529276.495999	44.194663
3503.749620	529253.314672	44.199668
3503.672581	529242.462771	44.204673
3503.845233	529215.653951	44.209677
3503.659813	529213.308468	44.214682
3503.542607	529183.564044	44.219687
3503.633876	529164.549880	44.224692
3503.711742	529157.614913	44.229697
3503.681851	529138.619869	44.234701
3503.565678	529125.348545	44.239706
3503.539625	529101.804980	44.244711
3504.079016	529087.722556	44.249716
3503.675983	529083.743894	44.254721
3503.836125	529049.306431	44.259725
3503.817211	529046.277687	44.264730
3503.712073	529018.501797	44.269735
3503.935936	529008.410690	44.274740
3503.552482	528986.793139	44.279745
3503.799229	528962.599858	44.284749
3503.476067	528968.310761	44.289754
3503.689445	528953.218569	44.294759
3503.761162	528928.699175	44.299764
3503.698696	528924.565576	44.304769
3503.504223	528888.465709	44.309773
3503.843507	528873.757800	44.314778
3503.619775	528876.926385	44.319783
3503.595751	528845.246352	44.324788
3503.780925	528821.618449	44.329793
3504.072935	528821.572487	44.334797
3503.665177	528802.283036	44.339802
3503.561186	528787.645114	44.344807
3503.603545	528766.465284	44.349812
3503.626030	528759.892628	44.354817
3503.790259	528751.225709	44.359821
3503.324787	528743.113115	44.364826
3503.241876	528714.575182	44.369831
3503.706490	528702.070764	44.374836
3503.464650	528709.891302	44.379841
3503.958332	528688.791630	44.384845
3503.581348	528668.132752	44.389850
3503.468649	528659.408488	44.394855
3503.828693	528635.398933	44.399860
3503.425827	528623.890641	44.404865
3503.490762	528614.077070	44.409869
3503.389632	528608.079759	44.414874
3503.331231	528581.963322	44.419879
3503.393107	528571.089002	44.424884
3503.372609	528571.092436	44.429889
3503.397765	528563.003266	44.434893
3503.596256	528556.857509	44.439898
3503.445689	528529.239541	44.444903
3503.731976	528517.925444	44.449908
3503.437829	528513.221951	44.454913
3503.668260	528491.910959	44.459917
3503.385151	528481.242710	44.464922
3503.618238	528477.112811	44.469927
3503.743845	528454.807659	44.474932
3503.506379	528440.493717	44.479937
3503.959133	528424.756775	44.484941
3503.680204	528403.324040	44.489946
3503.596422	528392.876895	44.494951
3503.776599	528381.882678	44.499956
3503.750590	528358.590670	44.504961
3503.735813	528337.267695	44.509965
3503.594610	528326.475842	44.514970
3503.489731	528304.004772	44.519975
3503.812668	528281.466047	44.524980
3503.644898	528274.215778	44.529985
3503.559866	528259.018488	44.534989
3503.553192	528236.178057	44.539994
3503.696366	528241.057488	44.544999
3503.713085	528215.686593	44.550004
3503.437103	528204.663286	44.555009
3503.497344	528202.278821	44.560013
3503.492434	528186.260240	44.565018
3503.597058	528155.872401	44.570023
3503.925940	528142.681509	44.575028
3503.504004	528135.067070	44.580033
3503.378367	528117.147169	44.585037
3503.547320	528104.486876	44.590042
3503.383887	528096.679953	44.595047
3503.589365	528085.327786	44.600052
3503.467891	528062.050432	44.605057
3503.205927	528054.157992	44.610061
3503.463237	528050.984325	44.615066
3503.376383	528035.382826	44.620071
3503.736908	528022.035226	44.625076
3503.491059	528024.853728	44.630081
3503.496291	528020.052231	44.635085
3503.493423	527993.976582	44.640090
3503.304527	527977.279374	44.645095
3503.379071	527973.477618	44.650100
3503.184665	527979.370666	44.655105
3503.537710	527952.986014	44.660109
3503.481526	527940.917068	44.665114
3503.483712	527925.857280	44.670119
3503.797710	527924.140163	44.675124
3503.431994	527911.412621	44.680129
3503.579708	527886.626924	44.685133
3503.695503	527875.389854	44.690138
3503.618484	527866.406833	44.695143
3503.770625	527840.609646	44.700148
3503.505051	527839.135738	44.705153
3503.484792	527817.257034	44.710157
3503.664638	527796.003640	44.715162
3503.676706	527791.605282	44.720167
3503.259054	527774.337585	44.725172
3503.264806	527764.633917	44.730177
3503.364275	527747.436061	44.735181
3503.454910	527735.394288	44.740186
3503.487653	527740.493474	44.745191
3503.682538	527717.974191	44.750196
3503.274298	527703.534966	44.755201
3503.453977	527688.547971	44.760205
3503.302854	527688.673125	44.765210
3503.112971	527677.585305	44.770215
3503.416900	527656.312111	44.775220
3503.285395	527648.550457	44.780225
3503.384996	527643.178027	44.785229
3503.582167	527644.410471	44.790234
3503.472663	527617.239252	44.795239
3503.492863	527595.454921	44.800244
3503.444473	527601.325028	44.805249
3503.742951	527590.210491	44.810253
3503.481494	527567.308295	44.815258
3503.364374	527550.093924	44.820263
3503.529687	527546.429329	44.825268
3503.074852	527535.181142	44.830273
3503.208816	527514.136771	44.835277
3503.277583	527500.733778	44.840282
3503.165149	527489.077676	44.845287
3503.238191	527499.578039	44.850292
3503.327938	527499.008140	44.855297
3503.178910	527483.618074	44.860301
3503.299271	527468.943471	44.865306
3503.095267	527470.390951	44.870311
3503.309093	527453.983296	44.875316
3503.242614	527460.361687	44.880321
3503.373416	527455.186411	44.885325
3503.456727	527427.024182	44.890330
3503.203685	527417.007447	44.895335
3503.231217	527391.077614	44.900340
3502.984723	527411.331725	44.905345
3503.369317	527396.008840	44.910349
3503.140841	527412.065497	44.915354
3503.444538	527386.395229	44.920359
3503.495664	527364.908918	44.925364
3503.083358	527365.176433	44.930369
3503.206104	527359.547562	44.935373
3503.456657	527358.699552	44.940378
3503.219311	527338.825466	44.945383
3503.341827	527322.785872	44.950388
3503.345914	527324.149936	44.955393
3503.597539	527312.183472	44.960397
3503.350849	527296.657049	44.965402
3503.126434	527286.938932	44.970407
3503.643803	527273.616453	44.975412
3503.163657	527280.464604	44.980417
3503.448895	527266.622894	44.985421
3503.421785	527251.011181	44.990426
3503.669407	527237.832385	44.995431
3503.605448	527228.998553	45.000436
3503.759271	527231.349716	45.005441
3503.522769	527204.501093	45.010445
3503.512782	527183.832806	45.015450
3503.124968	527191.929852	45.020455
3503.652539	527158.087201	45.025460
3503.203809	527150.880827	45.030465
3503.434505	527133.914256	45.035469
3503.569490	527139.806086	45.040474
3503.364752	527129.073999	45.045479
3503.427890	527105.210140	45.050484
3503.216804	527102.514630	45.055489
3502.941960	527089.772063	45.060493
3503.136087	527096.564252	45.065498
3503.165672	527094.740389	45.070503
3503.125077	527079.939253	45.075508
3503.122048	527063.919243	45.080513
3503.452149	527052.041256	45.085517
3503.533377	527046.974761	45.090522
3503.527028	527042.629645	45.095527
3503.792330	527029.245728	45.100532
3503.241417	527020.842521	45.105537
3503.373910	527011.522668	45.110541
3503.504896	527000.686889	45.115546
3503.270215	526992.284220	45.120551
3503.574204	526959.841034	45.125556
3503.188919	526965.057083	45.130561
3503.125257	526951.977793	45.135565
3503.100429	526950.314130	45.140570
3503.389974	526947.034073	45.145575
3503.652798	526916.517781	45.150580
3503.267994	526911.828139	45.155585
3503.652907	526911.211564	45.160589
3503.816923	526886.724966	45.165594
3503.553417	526867.561972	45.170599
3503.668367	526848.743448	45.175604
3503.683378	526852.228469	45.180609
3503.690899	526820.539409	45.185613
3503.441364	526821.033899	45.190618
3503.382957	526801.888946	45.195623
3503.355768	526776.269998	45.200628
3503.518437	526770.280833	45.205633
3503.318307	526762.377974	45.210637
3503.714359	526768.936228	45.215642
3503.365628	526752.313536	45.220647
3503.144965	526735.013570	45.225652
3503.191090	526723.635081	45.230657
3503.339429	526724.167763	45.235661
3503.441432	526715.155794	45.240666
3503.389436	526690.096564	45.245671
3503.609884	526683.592837	45.250676
3503.403664	526677.004930	45.255681
3503.642819	526662.411886	45.260685
3503.885041	526647.919424	45.265690
3503.484889	526631.355273	45.270695
3503.794740	526615.032657	45.275700
3503.485434	526594.057137	45.280705
3503.834500	526592.688118	45.285709
3503.647443	526568.458684	45.290714
3503.241035	526566.754215	45.295719
3503.568720	526553.157879	45.300724
3503.280626	526562.705142	45.305729
3503.254799	526529.959435	45.310733
3503.487394	526514.861892	45.315738
3503.436157	526522.198512	45.320743
3503.533512	526498.075636	45.325748
3503.393539	526486.372612	45.330753
3503.537809	526460.473353	45.335757
3503.416831	526457.965651	45.340762
3503.436529	526468.272965	45.345767
3503.467764	526442.745327	45.350772
3503.400657	526421.276433	45.355777
3503.141801	526411.209441	45.360781
3503.174906	526398.670347	45.365786
3502.929737	526415.337131	45.370791
3503.404934	526402.930323	45.375796
3503.052854	526393.282380	45.380801
3503.314924	526375.299232	45.385805
3503.493200	526368.448259	45.390810
3503.191258	526368.597261	45.395815
3503.254179	526357.721264	45.400820
3503.388759	526354.415040	45.405825
3503.417486	526327.624096	45.410829
3503.388530	526325.253450	45.415834
3503.396599	526330.710774	45.420839
3503.400265	526316.255719	45.425844
3503.490857	526289.404392	45.430849
3503.245879	526292.172517	45.435853
3503.411649	526280.218851	45.440858
3503.242376	526284.743944	45.445863
3503.524878	526269.031790	45.450868
3503.243725	526241.481028	45.455873
3503.364764	526240.653433	45.460877
3503.450876	526233.564264	45.465882
3503.316637	526229.946718	45.470887
3503.330655	526201.388949	45.475892
3503.233986	526193.065125	45.480897
3503.340236	526186.478165	45.485901
3503.761497	526194.397286	45.490906
3503.232837	526171.585857	45.495911
3503.305954	526148.426569	45.500916
3503.521859	526137.728406	45.505921
3503.388290	526135.626974	45.510925
3503.350786	526126.586183	45.515930
3503.044912	526108.641967	45.520935
3503.453249	526098.166068	45.525940
3503.234831	526091.074431	45.530945
3503.597356	526096.526350	45.535949
3503.525885	526079.454797	45.540954
3503.121378	526059.049579	45.545959
3503.331204	526045.218733	45.550964
3503.428225	526048.185550	45.555969
3503.387942	526041.773318	45.560973
3503.400951	526014.428375	45.565978
3503.125689	526007.699478	45.570983
3503.455200	525998.297352	45.575988
3503.260646	525991.757859	45.580993
3503.580288	525989.079352	45.585997
3503.598901	525972.549407	45.591002
3503.270387	525957.893824	45.596007
3503.483182	525945.578681	45.601012
3503.458900	525953.214553	45.606017
3503.253615	525923.376861	45.611021
3503.409083	525912.789185	45.616026
3503.028253	525903.347657	45.621031
3503.300497	525903.810240	45.626036
3502.937124	525909.376962	45.631041
3503.315006	525887.129423	45.636045
3503.380108	525869.783348	45.641050
3503.123547	525863.203061	45.646055
3503.472828	525854.859113	45.651060
3502.870309	525861.676667	45.656065
3503.105800	525851.682809	45.661069
3503.279540	525852.969641	45.666074
3503.161582	525839.240971	45.671079
3503.358312	525828.798344	45.676084
3503.223446	525825.180805	45.681089
3503.280944	525814.608550	45.686093
3503.651609	525813.741476	45.691098
3503.026914	525794.027774	45.696103
3503.146284	525781.171305	45.701108
3503.082792	525777.643558	45.706113
3502.764210	525765.664983	45.711117
3503.242071	525774.535675	45.716122
3503.372960	525773.655957	45.721127
3503.334305	525765.727080	45.726132
3503.232551	525746.436086	45.731137
3503.197484	525727.690497	45.736141
3503.190161	525725.771226	45.741146
3502.868389	525722.739177	45.746151
3503.373178	525722.457410	45.751156
3503.187719	525718.595130	45.756161
3503.475342	525716.325981	45.761165
3503.202210	525694.029449	45.766170
3503.150391	525683.575472	45.771175
3503.160289	525673.920419	45.776180
3503.003647	525683.043084	45.781185
3503.110084	525672.058657	45.786189
3503.309412	525668.438801	45.791194
3502.986661	525658.027632	45.796199
3503.231075	525647.173007	45.801204
3503.172758	525631.059213	45.806209
3503.174325	525635.608028	45.811213
3503.284276	525635.439213	45.816218
3503.464327	525624.948548	45.821223
3503.675394	525599.744940	45.826228
3503.103299	525594.326364	45.831233
3503.207991	525584.403558	45.836237
3503.455527	525577.996189	45.841242
3503.188656	525578.493454	45.846247
3502.951457	525545.425339	45.851252
3502.928508	525542.497651	45.856257
3502.952777	525532.587524	45.861261
3503.086900	525524.277414	45.866266
3503.112717	525530.692529	45.871271
3503.482644	525528.410345	45.876276
3503.130434	525534.784124	45.881281
3503.287943	525524.903476	45.886285
3503.436343	525508.251450	45.891290
3503.158424	525499.854827	45.896295
3503.286140	525486.693542	45.901300
3503.251482	525488.215518	45.906305
3503.180071	525479.280808	45.911309
3503.509676	525479.228903	45.916314
3503.366006	525456.355597	45.921319
3503.608651	525440.901650	45.926324
3503.473293	525437.081926	45.931329
3503.396677	525428.754533	45.936333
3503.644996	525405.970827	45.941338
3503.313364	525395.409260	45.946343
3503.537416	525391.987609	45.951348
3503.219768	525372.578658	45.956353
3503.303098	525358.312320	45.961357
3503.253129	525343.157250	45.966362
3503.282095	525347.651272	45.971367
3503.534792	525331.841823	45.976372
3503.455439	525319.117484	45.981377
3503.492189	525307.385662	45.986381
3503.595225	525302.820608	45.991386
3503.400088	525297.797243	45.996391
3503.427770	525277.019446	46.001396
3503.275695	525268.147913	46.006401
3503.515804	525269.828654	46.011405
3503.631989	525263.694643	46.016410
3503.395817	525243.312318	46.021415
3503.609026	525213.912595	46.026420
3503.107251	525213.031761	46.031425
3503.467340	525216.159328	46.036429
3503.493661	525189.215228	46.041434
3503.649549	525172.612215	46.046439
3503.561542	525168.886031	46.051444
3503.520350	525163.535023	46.056449
3503.616990	525135.113927	46.061453
3503.657869	525131.367362	46.066458
3503.638655	525127.529206	46.071463
3504.000421	525099.318862	46.076468
3503.681574	525090.271412	46.081473
3503.184248	525078.219485	46.086477
3503.649973	525056.108544	46.091482
3503.441086	525046.285516	46.096487
3503.454446	525039.611679	46.101492
3503.458229	525031.625186	46.106497
3503.351738	525004.954493	46.111501
3503.206217	525006.089678	46.116506
3502.970008	524996.523663	46.121511
3503.515376	524986.025382	46.126516
3503.046212	524998.078901	46.131521
3503.045992	524975.586595	46.136525
3503.401620	524957.940887	46.141530
3503.026571	524946.071712	46.146535
3503.238996	524946.341600	46.151540
3503.330384	524942.334281	46.156545
3503.274039	524940.321575	46.161549
3503.421748	524925.033773	46.166554
3503.233242	524915.662351	46.171559
3503.449884	524900.363630	46.176564
3503.400808	524898.097042	46.181569
3503.435284	524892.026350	46.186573
3503.576767	524861.171505	46.191578
3503.224916	524852.129137	46.196583
3503.692422	524852.004889	46.201588
3503.504076	524837.326123	46.206593
3503.682244	524817.029400	46.211597
3503.290725	524811.127103	46.216602
3503.236732	524806.182364	46.221607
3503.514632	524792.693499	46.226612
3503.513876	524761.203853	46.231617
3503.060384	524762.488826	46.236621
3503.296449	524765.231721	46.241626
3503.476188	524759.643474	46.246631
3504.025554	524730.745737	46.251636
3503.651046	524717.107203	46.256641
3503.625805	524704.677098	46.261645
3503.743769	524675.594722	46.266650
3503.386921	524665.895940	46.271655
3503.692228	524659.933989	46.276660
3503.445547	524640.917303	46.281665
3503.372401	524626.068495	46.286669
3503.171672	524617.810846	46.291674
3503.515246	524618.110556	46.296679
3503.685889	524594.023777	46.301684
3503.448021	524587.288370	46.306689
3503.603321	524568.410244	46.311693
3503.506289	524555.890279	46.316698
3503.218654	524541.328028	46.321703
3503.358363	524537.211878	46.326708
3503.498505	524532.438555	46.331713
3503.326223	524520.638107	46.336717
3503.339352	524486.466764	46.341722
3503.352146	524481.915742	46.346727
3503.266832	524472.527749	46.351732
3503.088153	524470.736507	46.356737
3503.339293	524474.690189	46.361741
3503.362060	524451.233130	46.366746
3503.160656	524444.946819	46.371751
3502.890845	524437.559291	46.376756
3502.804452	524434.237055	46.381761
3503.276252	524428.551983	46.386765
3503.539629	524429.470934	46.391770
3503.469643	524430.088752	46.396775
3503.491845	524395.460861	46.401780
3503.040842	524396.138905	46.406785
3502.838408	524386.668281	46.411789
3503.514236	524381.355318	46.416794
3503.282348	524386.446857	46.421799
3503.067773	524370.053214	46.426804
3503.221499	524355.774860	46.431809
3502.994033	524354.800069	46.436813
3503.299563	524355.459627	46.441818
3503.348119	524357.170744	46.446823
3503.683345	524341.953843	46.451828
3503.379196	524324.563371	46.456833
3503.359850	524314.912124	46.461837
3503.515688	524299.015878	46.466842
3503.379264	524305.356032	46.471847
3503.384285	524268.910886	46.476852
3503.221419	524256.451642	46.481857
3503.673412	524245.967640	46.486861
3503.709411	524249.298269	46.491866
3503.149374	524233.211829	46.496871
3503.485449	524216.073874	46.501876
3503.286489	524205.136718	46.506881
3503.378056	524203.707109	46.511885
3503.317253	524198.005047	46.516890
3503.106143	524178.577811	46.521895
3503.273567	524160.000576	46.526900
3503.427203	524161.998390	46.531905
3503.221097	524164.103614	46.536909
3503.484894	524151.728490	46.541914
3502.881925	524134.233403	46.546919
3503.020331	524108.988397	46.551924
3503.539243	524105.974798	46.556929
3503.080634	524110.900069	46.561933
3503.406092	524103.519390	46.566938
3503.072939	524098.113082	46.571943
3502.990739	524071.032618	46.576948
3503.085621	524068.692611	46.581953
3503.128727	524061.255447	46.586957
3503.212914	524058.664390	46.591962
3503.029666	524057.783686	46.596967
3503.034125	524063.646735	46.601972
3503.070164	524064.702739	46.606977
3503.157565	524060.089257	46.611981
3503.226654	524057.904969	46.616986
3503.357739	524038.372926	46.621991
3503.118264	524020.466423	46.626996
3503.427326	524026.534078	46.632001
3503.658332	524017.955138	46.637005
3503.627701	524004.514383	46.642010
3503.257814	523989.256960	46.647015
3503.468570	523970.217723	46.652020
3503.717011	523967.499591	46.657025
3503.502524	523946.859452	46.662029
3503.665347	523930.506804	46.667034
3503.502091	523927.499903	46.672039
3503.431683	523909.768746	46.677044
3503.112448	523894.351581	46.682049
3503.114279	523881.411077	46.687053
3503.147100	523867.404144	46.692058
3502.744411	523874.949171	46.697063
3503.071507	523876.161375	46.702068
3503.010261	523876.828381	46.707073
3502.935788	523877.598574	46.712077
3502.780511	523873.579431	46.717082
3503.080611	523868.224595	46.722087
3503.147881	523860.884616	46.727092
3503.077930	523848.157626	46.732097
3503.076210	523835.217646	46.737101
3503.356851	523815.358402	46.742106
3502.815950	523827.879069	46.747111
3503.328402	523818.194014	46.752116
3503.065590	523822.987326	46.757121
3503.076422	523826.473666	46.762125
3503.141307	523823.380135	46.767130
3503.067144	523802.161594	46.772135
3503.119464	523785.826267	46.777140
3502.860166	523786.878423	46.782145
3503.120805	523783.400100	46.787149
3503.454499	523781.578341	46.792154
3503.153352	523786.226076	46.797159
3503.388620	523772.136513	46.802164
3503.314720	523755.265068	46.807169
3503.168824	523733.552287	46.812173
3503.275372	523725.245608	46.817178
3503.323946	523728.827102	46.822183
3503.469254	523725.720840	46.827188
3503.201961	523705.341483	46.832193
3503.345963	523693.136591	46.837197
3503.260229	523681.220749	46.842202
3503.122765	523691.352492	46.847207
3503.172534	523679.516328	46.852212
3502.825507	523691.652612	46.857217
3503.058469	523678.523764	46.862221
3503.254050	523672.983187	46.867226
3503.116030	523656.425069	46.872231
3503.046317	523639.856137	46.877236
3503.076068	523637.779109	46.882241
3503.277733	523634.411176	46.887245
3503.408607	523628.173122	46.892250
3503.003532	523638.701043	46.897255
3503.427652	523631.203457	46.902260
3503.558703	523611.721453	46.907265
3503.596855	523605.144201	46.912269
3503.464777	523596.672978	46.917274
3503.125168	523578.579614	46.922279
3503.046286	523559.130730	46.927284
3503.131396	523559.572416	46.932289
3502.971148	523548.527596	46.937293
3503.148507	523544.961287	46.942298
3502.947348	523554.446040	46.947303
3503.359193	523546.242661	46.952308
3503.279091	523549.844534	46.957313
3503.097589	523533.343712	46.962317
3503.163275	523514.478518	46.967322
3503.105038	523508.371410	46.972327
3503.190246	523500.118538	46.977332
3503.180646	523508.612595	46.982337
3502.791207	523498.614961	46.987341
3503.533264	523491.370353	46.992346
3503.163775	523478.993716	46.997351
3502.999084	523462.338515	47.002356
3503.263851	523459.567169	47.007361
3502.959043	523462.800181	47.012365
3503.031508	523460.564729	47.017370
3502.768234	523462.577980	47.022375
3503.027463	523460.919605	47.027380
3502.986745	523468.458155	47.032385
3502.512066	523460.394862	47.037389
3502.975997	523459.664577	47.042394
3502.764184	523467.887319	47.047399
3503.302833	523461.230897	47.052404
3503.109831	523456.459366	47.057409
3502.779956	523443.874241	47.062413
3503.046466	523431.498138	47.067418
3502.861512	523420.861534	47.072423
3503.138953	523416.925529	47.077428
3503.341680	523414.163981	47.082433
3503.091294	523411.524605	47.087437
3502.990821	523414.978077	47.092442
3502.895473	523412.566945	47.097447
3503.218631	523412.465509	47.102452
3503.289631	523407.702783	47.107457
3502.864029	523382.242493	47.112461
3503.008038	523369.076904	47.117466
3502.947529	523371.159216	47.122471
3502.851052	523360.963539	47.127476
3503.288156	523369.235409	47.132481
3503.037462	523360.732261	47.137485
3503.356690	523364.372155	47.142490
3503.109486	523361.024565	47.147495
3503.326094	523360.333369	47.152500
3503.240361	523333.858828	47.157505
3503.601330	523326.472184	47.162509
3503.409003	523320.992803	47.167514
3502.820071	523337.616009	47.172519
3503.315885	523312.313265	47.177524
3503.503242	523298.028660	47.182529
3503.133778	523292.577269	47.187533
3503.813801	523267.295888	47.192538
3503.386106	523285.511274	47.197543
3503.291793	523243.872828	47.202548
3503.393908	523238.801831	47.207553
3503.186405	523238.278769	47.212557
3503.596851	523227.446824	47.217562
3503.439787	523216.957329	47.222567
3503.279938	523188.219489	47.227572
3503.320435	523186.949516	47.232577
3503.578546	523179.073556	47.237581
3503.703721	523171.976866	47.242586
3503.497209	523146.532124	47.247591
3503.642932	523133.618827	47.252596
3503.213688	523131.715387	47.257601
3503.207605	523109.878566	47.262605
3503.677416	523082.203681	47.267610
3503.137695	523088.506957	47.272615
3503.178527	523087.995187	47.277620
3503.451500	523078.802505	47.282625
3503.259302	523068.065712	47.287629
3503.249046	523050.020797	47.292634
3503.203332	523042.344449	47.297639
3503.013103	523044.447307	47.302644
3503.348940	523032.413799	47.307649
3502.986974	523037.121912	47.312653
3503.417877	523013.648804	47.317658
3503.034719	523001.728922	47.322663
3503.255736	522990.876211	47.327668
3503.116833	522983.568424	47.332673
3503.140701	522996.101563	47.337677
3503.534572	522980.318049	47.342682
3503.045713	522964.623499	47.347687
3502.873093	522954.287946	47.352692
3502.694214	522944.256685	47.357697
3502.815211	522945.703744	47.362701
3503.031379	522947.894032	47.367706
3502.815876	522951.264682	47.372711
3503.012600	522945.572023	47.377716
3503.280595	522946.136473	47.382721
3503.120519	522945.909213	47.387725
3503.441616	522940.702407	47.392730
3503.186547	522942.310013	47.397735
3503.227700	522921.375397	47.402740
3503.509257	522914.051669	47.407745
3503.437961	522901.779110	47.412749
3503.345191	522895.778331	47.417754
3503.329560	522906.447375	47.422759
3503.444144	522872.357682	47.427764
3503.203091	522869.817844	47.432769
3503.118102	522865.635684	47.437773
3503.170745	522861.785630	47.442778
3503.233273	522857.832909	47.447783
3503.163914	522851.171241	47.452788
3503.040847	522830.313017	47.457793
3503.044122	522822.780477	47.462797
3503.286709	522808.992230	47.467802
3503.014467	522815.101676	47.472807
3503.026182	522816.616573	47.477812
3502.970000	522817.838892	47.482817
3502.848145	522819.829868	47.487821
3503.114127	522806.037920	47.492826
3503.168018	522804.411937	47.497831
3502.871157	522799.403868	47.502836
3502.980046	522776.790146	47.507841
3502.647845	522775.326291	47.512845
3503.485529	522753.254515	47.517850
3503.325833	522765.109119	47.522855
3503.226919	522757.339941	47.527860
3503.171885	522760.938026	47.532865
3503.067701	522755.141208	47.537869
3503.277291	522740.397630	47.542874
3503.013278	522722.645221	47.547879
3503.141938	522724.192194	47.552884
3503.420615	522720.913003	47.557889
3503.032130	522718.649206	47.562893
3503.326077	522718.501833	47.567898
3503.136440	522712.111880	47.572903
3502.996240	522686.200963	47.577908
3503.341733	522679.473651	47.582913
3503.244895	522674.888896	47.587917
3503.472433	522668.079120	47.592922
3503.201695	522674.441142	47.597927
3503.208590	522653.511595	47.602932
3502.988976	522640.958968	47.607937
3502.816486	522635.172903	47.612941
3503.019147	522617.953243	47.617946
3502.641973	522620.389020	47.622951
3503.018966	522614.667750	47.627956
3503.152225	522620.005440	47.632961
3503.096017	522620.317833	47.637965
3503.101601	522615.615767	47.642970
3503.006561	522620.332361	47.647975
3503.163266	522617.679059	47.652980
3503.365235	522610.367775	47.657985
3502.953378	522590.667044	47.662989
3503.221852	522586.075073	47.667994
3503.202100	522579.253795	47.672999
3503.018249	522584.034990	47.678004
3503.066682	522572.956517	47.683009
3503.235576	522577.783061	47.688013
3503.264962	522561.702887	47.693018
3503.312558	522549.360714	47.698023
3503.153883	522531.187024	47.703028
3502.902331	522531.580848	47.708033
3503.127301	522529.927796	47.713037
3503.591910	522515.194257	47.718042
3503.372934	522521.295394	47.723047
3503.054104	522497.990600	47.728052
3503.105553	522495.000046	47.733057
3503.192796	522490.942223	47.738061
3503.313571	522471.207709	47.743066
3503.158320	522491.200825	47.748071
3503.285430	522481.171463	47.753076
3503.321822	522454.473968	47.758081
3502.817965	522452.329475	47.763085
3503.127075	522434.587265	47.768090
3503.049557	522448.198466	47.773095
3503.352000	522431.063942	47.778100
3503.417846	522436.007923	47.783105
3503.226991	522430.831324	47.788109
3503.609561	522403.371285	47.793114
3503.240436	522393.925838	47.798119
3503.202067	522386.197465	47.803124
3503.207351	522381.950357	47.808129
3503.154712	522382.868829	47.813133
3503.558955	522354.849197	47.818138
3503.412209	522349.615047	47.823143
3503.474502	522328.929091	47.828148
3503.452304	522340.054525	47.833153
3503.513778	522319.975327	47.838157
3503.235006	522305.915190	47.843162
3502.947018	522308.033595	47.848167
3503.234475	522295.248888	47.853172
3503.441418	522290.211580	47.858177
3503.262093	522284.022042	47.863181
3503.279025	522271.937273	47.868186
3503.390528	522264.033492	47.873191
3503.433016	522248.355364	47.878196
3503.282885	522250.148664	47.883201
3503.686867	522236.132206	47.888205
3503.728640	522216.157102	47.893210
3503.352839	522214.295657	47.898215
3503.629916	522190.340138	47.903220
3503.591689	522166.889407	47.908225
3503.287951	522161.225026	47.913229
3503.955541	522154.143262	47.918234
3503.526779	522141.067214	47.923239
3503.457679	522133.697455	47.928244
3503.135434	522128.541528	47.933249
3503.235349	522129.334792	47.938253
3503.604268	522104.201888	47.943258
3503.004852	522088.928394	47.948263
3503.551922	522074.889181	47.953268
3503.418372	522072.130007	47.958273
3503.182503	522071.864159	47.963277
3503.377640	522042.309864	47.968282
3503.255024	522035.959605	47.973287
3503.222903	522026.359565	47.978292
3503.508423	522031.066730	47.983297
3503.188353	522020.400008	47.988301
3503.473601	521996.089031	47.993306
3503.236388	521988.998552	47.998311
3502.764008	521986.950129	48.003316
3503.159403	521984.360104	48.008321
3503.034936	521981.447815	48.013325
3503.420587	521985.077523	48.018330
3503.348517	521966.383967	48.023335
3502.945140	521952.191555	48.028340
3502.990199	521942.427602	48.033345
3502.863447	521936.330731	48.038349
3503.447085	521927.644393	48.043354
3503.023271	521937.771938	48.048359
3503.213393	521931.321650	48.053364
3503.380618	521930.132656	48.058369
3502.925768	521912.915071	48.063373
3503.203462	521897.199426	48.068378
3503.164546	521893.464725	48.073383
3502.877745	521887.140359	48.078388
3503.076092	521891.962453	48.083393
3502.964489	521886.014832	48.088397
3503.263243	521882.378418	48.093402
3502.909034	521879.451871	48.098407
3502.977311	521876.913536	48.103412
3503.276424	521848.050219	48.108417
3502.940470	521844.362458	48.113421
3503.391868	521837.618060	48.118426
3503.287308	521839.353646	48.123431
3503.077238	521835.443766	48.128436
3503.404593	521831.196161	48.133441
3502.871820	521822.231241	48.138445
3503.361407	521795.916024	48.143450
3503.287195	521798.506254	48.148455
3503.234845	521796.138638	48.153460
3503.518128	521802.969533	48.158465
3503.535202	521790.985494	48.163469
3503.243231	521763.378223	48.168474
3503.393675	521758.501347	48.173479
3503.001864	521738.493080	48.178484
3502.997910	521737.482795	48.183489
3502.965286	521741.937001	48.188493
3503.278371	521739.056618	48.193498
3503.108641	521743.330274	48.198503
3503.067025	521730.394920	48.203508
3503.316717	521711.852432	48.208513
3503.437427	521702.025822	48.213517
3503.464290	521695.146249	48.218522
3503.293893	521700.431129	48.223527
3503.379040	521672.966316	48.228532
3502.955970	521659.181203	48.233537
3502.818666	521661.478094	48.238541
3503.136249	521645.452569	48.243546
3503.124503	521648.336281	48.248551
3503.164648	521645.701246	48.253556
3503.001699	521646.030529	48.258561
3502.690114	521653.208294	48.263565
3503.037460	521646.834152	48.268570
3503.003515	521658.669686	48.273575
3503.003550	521629.145479	48.278580
3503.179378	521608.592328	48.283585
3503.283100	521614.693351	48.288589
3503.457213	521599.903794	48.293594
3503.039920	521605.531063	48.298599
3503.303100	521605.792991	48.303604
3503.301857	521583.902797	48.308609
3503.067052	521561.139489	48.313613
3503.240973	521562.780531	48.318618
3503.355542	521562.257058	48.323623
3503.166481	521561.326577	48.328628
3503.366072	521550.021292	48.333633
3502.862005	521528.261058	48.338637
3503.255592	521514.801739	48.343642
3503.277069	521510.703512	48.348647
3503.009574	521508.673197	48.353652
3503.380818	521511.344727	48.358657
3503.094919	521512.199007	48.363661
3503.406396	521498.145982	48.368666
3503.418863	521474.787352	48.373671
3503.570531	521457.928418	48.378676
3503.334690	521459.836464	48.383681
3503.197292	521460.060600	48.388685
3503.592356	521444.679860	48.393690
3503.374799	521432.176528	48.398695
3503.219459	521420.977812	48.403700
3503.373040	521412.611961	48.408705
3503.160692	521411.836821	48.413709
3503.235967	521395.849353	48.418714
3503.562099	521397.567465	48.423719
3503.109666	521389.347949	48.428724
3503.339791	521380.514976	48.433729
3503.351200	521377.429433	48.438733
3503.284499	521345.539115	48.443738
3503.260513	521340.386348	48.448743
3502.832566	521336.207447	48.453748
3503.323995	521330.518198	48.458753
3502.960245	521337.299894	48.463757
3502.952596	521333.661235	48.468762
3502.946585	521331.336783	48.473767
3503.376777	521325.707768	48.478772
3503.212971	521297.270544	48.483777
3502.964200	521293.771102	48.488781
3503.068508	521285.059078	48.493786
3503.119952	521292.836853	48.498791
3502.940962	521294.685375	48.503796
3502.962910	521293.670969	48.508801
3502.929827	521290.592442	48.513805
3502.970209	521282.851097	48.518810
3502.853208	521284.133699	48.523815
3503.170761	521271.950113	48.528820
3503.349895	521266.006866	48.533825
3502.776792	521247.897247	48.538829
3503.288118	521229.464526	48.543834
3502.987936	521234.871184	48.548839
3503.146228	521224.431666	48.553844
3503.424920	521229.039030	48.558849
3503.221707	521229.930810	48.563853
3503.266152	521208.437344	48.568858
3503.089986	521201.892996	48.573863
3503.142408	521193.947478	48.578868
3503.201727	521189.792632	48.583873
3502.900218	521196.261207	48.588877
3503.193336	521180.592992	48.593882
3503.192014	521187.620804	48.598887
3503.199394	521182.412471	48.603892
3503.257468	521161.472915	48.608897
3503.206659	521154.554834	48.613901
3503.351731	521134.713746	48.618906
3503.386087	521134.202939	48.623911
3503.234157	521132.710436	48.628916
3502.983817	521105.954939	48.633921
3502.982642	521101.051276	48.638925
3503.070324	521085.567114	48.643930
3503.177654	521089.999376	48.648935
3502.994374	521096.449302	48.653940
3503.246975	521087.107047	48.658945
3502.968768	521092.763064	48.663949
3503.202005	521088.075130	48.668954
3502.991035	521094.074419	48.673959
3503.295886	521063.793207	48.678964
3503.144583	521053.756418	48.683969
3502.882386	521050.663503	48.688973
3502.846526	521045.461962	48.693978
3503.077064	521048.661384	48.698983
3503.070194	521047.954862	48.703988
3503.267212	521045.294933	48.708993
3503.020037	521041.592955	48.713997
3502.854194	521038.080349	48.719002
3502.406751	521046.038213	48.724007
3502.871787	521043.942607	48.729012
3503.088453	521038.094460	48.734017
3503.244196	521044.490818	48.739021
3503.098226	521011.500116	48.744026
3503.017594	521001.351008	48.749031
3502.927742	521004.853870	48.754036
3503.036192	521002.207934	48.759041
3502.768093	521004.576148	48.764045
3503.241527	521002.731997	48.769050
3503.083642	521012.160832	48.774055
3502.789266	521007.505715	48.779060
3503.374160	520995.330224	48.784065
3503.155725	520989.854179	48.789069
3502.876892	520969.877666	48.794074
3502.844116	520972.663706	48.799079
3503.168149	520949.710094	48.804084
3503.288623	520954.797565	48.809089
3503.067090	520950.535378	48.814093
3503.226205	520945.808562	48.819098
3502.882164	520957.541947	48.824103
3502.887718	520946.873607	48.829108
3503.057766	520945.835769	48.834113
3502.962440	520939.278537	48.839117
3503.318715	520913.994127	48.844122
3503.050088	520914.946821	48.849127
3502.933736	520904.803300	48.854132
3503.062497	520901.446328	48.859137
3503.093023	520905.789665	48.864141
3503.210406	520895.305845	48.869146
3502.915318	520897.425552	48.874151
3503.208425	520896.014355	48.879156
3503.183815	520876.300890	48.884161
3503.005242	520859.796886	48.889165
3503.218951	520853.999698	48.894170
3503.114541	520854.875880	48.899175
3502.980392	520853.026636	48.904180
3503.168304	520843.593351	48.909185
3502.970200	520856.365457	48.914189
3503.299552	520845.291963	48.919194
3503.002591	520829.362778	48.924199
3503.183195	520822.458536	48.929204
3503.040177	520808.729550	48.934209
3503.014246	520804.941989	48.939213
3503.203390	520808.198559	48.944218
3503.460559	520805.225736	48.949223
3503.364736	520803.218753	48.954228
3503.441391	520780.708472	48.959233
3503.084919	520769.187193	48.964237
3503.113364	520756.745573	48.969242
3502.874942	520765.732257	48.974247
3503.044337	520763.784463	48.979252
3503.085606	520749.318483	48.984257
3502.998635	520758.584580	48.989261
3503.269508	520749.087570	48.994266
3503.120727	520737.128973	48.999271
3502.971440	520720.872990	49.004276
3503.462153	520710.886183	49.009281
3502.875551	520719.877368	49.014285
3503.134029	520706.691534	49.019290
3503.199964	520718.461402	49.024295
3503.146023	520711.543629	49.029300
3503.272653	520699.389796	49.034305
3503.169047	520684.491633	49.039309
3503.226905	520681.600851	49.044314
3503.205770	520670.228730	49.049319
3503.492285	520668.363530	49.054324
3503.427951	520664.531447	49.059329
3502.870517	520663.507466	49.064333
3503.024786	520641.439751	49.069338
3503.134535	520634.293836	49.074343
3502.942672	520637.610666	49.079348
3503.156673	520632.318939	49.084353
3503.491324	520639.799467	49.089357
3503.323784	520626.832583	49.094362
3503.098134	520616.150013	49.099367
3503.045184	520590.323084	49.104372
3502.960582	520587.454803	49.109377
3502.586850	520584.682782	49.114381
3503.112884	520579.088923	49.119386
3503.313158	520574.658847	49.124391
3503.202088	520591.007076	49.129396
3503.521767	520574.019555	49.134401
3503.401197	520566.151635	49.139405
3503.608191	520545.845016	49.144410
3502.984314	520544.224822	49.149415
3502.887468	520538.072140	49.154420
3503.350230	520535.622919	49.159425
3503.070502	520531.875410	49.164429
3503.075797	520530.459118	49.169434
3503.353947	520494.114001	49.174439
3503.141507	520499.810386	49.179444
3503.062480	520499.570276	49.184449
3503.184689	520494.748046	49.189453
3503.031976	520485.267279	49.194458
3502.962133	520485.986339	49.199463
3503.021456	520495.431697	49.204468
3503.402096	520478.485001	49.209473
3503.105112	520472.717843	49.214477
3503.269953	520444.126066	49.219482
3502.961608	520448.927562	49.224487
3503.093586	520453.356101	49.229492
3503.238561	520446.002300	49.234497
3503.145408	520448.494618	49.239501
3503.485365	520430.846475	49.244506
3503.095913	520417.712265	49.249511
3503.092327	520408.865152	49.254516
3503.318003	520405.189405	49.259521
3503.148753	520403.042301	49.264525
3502.982062	520395.434385	49.269530
3503.097692	520395.517421	49.274535
3503.112647	520377.566677	49.279540
3503.186854	520363.196268	49.284545
3503.158510	520352.937374	49.289549
3503.447625	520354.408652	49.294554
3503.116470	520350.416434	49.299559
3503.006679	520359.130209	49.304564
3503.085284	520340.309853	49.309569
3503.141051	520343.435921	49.314573
3503.357984	520311.549311	49.319578
3503.122666	520315.833707	49.324583
3503.234380	520310.456926	49.329588
3503.404108	520298.194864	49.334593
3502.889561	520304.343546	49.339597
3503.351645	520291.529672	49.344602
3503.103265	520277.311297	49.349607
3502.774294	520266.847070	49.354612
3503.104303	520254.458521	49.359617
3503.244500	520265.104662	49.364621
3503.357586	520252.902080	49.369626
3503.278903	520262.268267	49.374631
3503.076582	520251.682891	49.379636
3503.130572	520223.007131	49.384641
3502.929161	520228.449066	49.389645
3503.112973	520213.201683	49.394650
3503.385100	520213.512782	49.399655
3503.116038	520213.858865	49.404660
3503.528917	520218.950906	49.409665
3503.538476	520193.669629	49.414669
3503.417577	520173.009897	49.419674
3503.287675	520173.586785	49.424679
3503.144107	520168.604229	49.429684
3503.144023	520160.464269	49.434689
3502.700022	520140.108367	49.439693
3503.103815	520124.472209	49.444698
3503.146450	520122.493817	49.449703
3502.992376	520123.934050	49.454708
3503.291652	520117.920837	49.459713
3503.279961	520116.608314	49.464717
3503.035933	520108.456327	49.469722
3503.240056	520109.587141	49.474727
3503.114594	520104.702824	49.479732
3503.167307	520077.644939	49.484737
3503.194231	520081.432901	49.489741
3503.502245	520055.851434	49.494746
3503.436114	520076.895187	49.499751
3503.087088	520073.714690	49.504756
3503.274714	520044.461331	49.509761
3503.264971	520027.221953	49.514765
3503.154003	520028.857622	49.519770
3502.969064	520019.786163	49.524775
3502.899965	520020.960170	49.529780
3502.972252	520017.409703	49.534785
3502.602873	520031.776900	49.539789
3503.105818	520024.770810	49.544794
3503.286956	520017.057178	49.549799
3502.994304	520005.676953	49.554804
3503.193385	519985.016966	49.559809
3503.204872	519984.661420	49.564813
3503.117476	519977.799185	49.569818
3503.125627	519983.764243	49.574823
3503.138241	519972.841349	49.579828
3503.263315	519975.703729	49.584833
3503.179374	519982.593436	49.589837
3503.126181	519954.288072	49.594842
3503.025903	519941.310012	49.599847
3503.047700	519930.082274	49.604852
3503.189932	519929.099331	49.609857
3503.235175	519936.777609	49.614861
3503.408811	519922.391098	49.619866
3502.922394	519924.844535	49.624871
3502.965761	519902.136065	49.629876
3503.260703	519889.398859	49.634881
3503.185530	519899.775915	49.639885
3503.222833	519887.837845	49.644890
3503.126463	519881.280353	49.649895
3502.991118	519894.852262	49.654900
3503.334854	519881.601728	49.659905
3503.250263	519881.564732	49.664909
3503.334518	519854.501493	49.669914
3503.071673	519845.745617	49.674919
3503.068612	519843.066560	49.679924
3503.144151	519842.498642	49.684929
3503.137146	519848.011096	49.689933
3502.944792	519843.845130	49.694938
3503.227566	519839.098449	49.699943
3502.817366	519812.467225	49.704948
3502.895358	519799.005824	49.709953
3502.910381	519790.762170	49.714957
3503.178566	519784.703189	49.719962
3503.029215	519786.901123	49.724967
3502.739254	519783.155059	49.729972
3503.102594	519782.288841	49.734977
3503.316940	519787.867449	49.739981
3502.841269	519789.864157	49.744986
3502.886752	519787.683029	49.749991
3503.162623	519788.650842	49.754996
3502.921705	519782.116159	49.760001
3502.971974	519786.608355	49.765005
3503.143944	519760.188392	49.770010
3503.078382	519746.193464	49.775015
3503.066078	519741.695644	49.780020
3503.052176	519734.872251	49.785025
3502.828624	519731.772976	49.790029
3502.902626	519731.003052	49.795034
3503.021137	519738.113667	49.800039
3502.591482	519743.490718	49.805044
3503.212060	519733.887283	49.810049
3503.133634	519741.281833	49.815053
3503.478547	519735.109582	49.820058
3503.273447	519718.608619	49.825063
3502.758079	519701.954436	49.830068
3502.783775	519696.843859	49.835073
3503.010656	519696.403699	49.840077
3503.240175	519693.232800	49.845082
3503.085343	519696.139474	49.850087
3503.141586	519700.125135	49.855092
3503.012969	519698.123200	49.860097
3503.111488	519700.079719	49.865101
3503.340568	519682.701106	49.870106
3503.419358	519664.233876	49.875111
3502.887738	519664.924841	49.880116
3503.266128	519638.724862	49.885121
3503.195816	519647.432774	49.890125
3503.193504	519650.264786	49.895130
3502.876401	519643.337596	49.900135
3503.207223	519633.830466	49.905140
3503.171635	519623.471137	49.910145
3503.113820	519610.081609	49.915149
3502.982678	519597.664336	49.920154
3503.171533	519605.471754	49.925159
3503.098759	519598.607049	49.930164
3503.275172	519605.961378	49.935169
3503.092146	519587.029828	49.940173
3502.879750	519585.698426	49.945178
3503.047177	519570.908093	49.950183
3502.550357	519561.278935	49.955188
3502.933818	519553.027485	49.960193
3502.896356	519557.533612	49.965197
3503.055292	519548.963717	49.970202
3502.799817	519548.346988	49.975207
3502.680399	519555.191919	49.980212
3503.154264	519553.954287	49.985217
3502.749309	519551.338708	49.990221
3502.973592	519551.354013	49.995226
3503.036955	519548.664408	50.000231
3502.773860	519556.745536	50.005236
3503.001104	519560.501954	50.010241
3503.153216	519564.169123	50.015245
3503.032355	519555.795144	50.020250
3503.315660	519554.992128	50.025255
3503.062519	519539.762626	50.030260
3503.218074	519526.187618	50.035265
3503.106641	519521.250347	50.040269
3503.177626	519509.862860	50.045274
3503.322271	519516.615506	50.050279
3503.120753	519504.816031	50.055284
3502.978238	519508.681469	50.060289
3503.104012	519519.027004	50.065293
3503.210691	519481.088763	50.070298
3503.240364	519476.280862	50.075303
3502.951598	519472.939035	50.080308
3503.205847	519459.196684	50.085313
3502.886881	519460.157416	50.090317
3502.966838	519457.010113	50.095322
3503.172808	519468.000313	50.100327
3503.154775	519457.941477	50.105332
3503.298697	519450.284024	50.110337
3503.077482	519426.554911	50.115341
3503.099856	519416.034602	50.120346
3503.319192	519415.949564	50.125351
3502.940248	519423.290634	50.130356
3503.297459	519407.661159	50.135361
3503.240020	519422.181829	50.140365
3503.322388	519396.078818	50.145370
3503.088227	519377.407920	50.150375
3503.052187	519374.380063	50.155380
3503.533283	519359.337709	50.160385
3503.521412	519371.272532	50.165389
3503.261218	519355.336099	50.170394
3503.385492	519333.776993	50.175399
3503.305872	519332.222332	50.180404
3503.425196	519325.124897	50.185409
3503.320630	519336.366521	50.190413
3503.070985	519306.978716	50.195418
3502.728308	519290.701320	50.200423
3502.921437	519277.474106	50.205428
3503.075328	519280.028676	50.210433
3502.854835	519277.990649	50.215437
3502.736225	519281.397297	50.220442
3503.131030	519270.514650	50.225447
3502.833518	519286.438583	50.230452
3502.985309	519277.616862	50.235457
3503.141507	519271.929334	50.240461
3502.935066	519276.765625	50.245466
3503.410750	519281.949157	50.250471
3502.991734	519279.436883	50.255476
3503.311345	519255.268096	50.260481
3502.901754	519243.855262	50.265485
3502.886852	519239.812780	50.270490
3503.093360	519228.150862	50.275495
3503.219456	519235.159370	50.280500
3503.571373	519231.665660	50.285505
3502.864435	519235.013624	50.290509
3503.152762	519225.968043	50.295514
3503.306482	519206.628885	50.300519
3502.696952	519200.051108	50.305524
3503.272094	519174.476610	50.310529
3503.166504	519181.572327	50.315533
3503.134144	519173.285289	50.320538
3503.176221	519173.733900	50.325543
3503.104917	519174.453249	50.330548
3503.196089	519173.933400	50.335553
3502.768424	519169.652767	50.340557
3503.302118	519147.068001	50.345562
3502.936567	519144.243875	50.350567
3502.943117	519144.091345	50.355572
3503.151483	519135.311169	50.360577
3503.327189	519147.216504	50.365581
3503.103240	519147.252097	50.370586
3503.217712	519143.391395	50.375591
3502.911733	519128.473242	50.380596
3503.646724	519104.693646	50.385601
3503.165298	519107.500356	50.390605
3503.044604	519098.873301	50.395610
3503.123668	519096.130578	50.400615
3502.853375	519109.421085	50.405620
3503.169877	519093.443804	50.410625
3502.861373	519095.009663	50.415629
3503.058897	519090.630187	50.420634
3503.386166	519061.504696	50.425639
3503.163878	519059.972560	50.430644
3502.961996	519042.711956	50.435649
3502.921601	519055.460533	50.440653
3502.782347	519052.802875	50.445658
3503.134317	519045.112348	50.450663
3503.092916	519054.321640	50.455668
3503.159450	519046.827922	50.460673
3503.151689	519039.244818	50.465677
3503.152157	519022.356716	50.470682
3503.390480	519008.060308	50.475687
3503.248959	519011.369506	50.480692
3503.402846	519000.322508	50.485697
3502.975895	519000.339625	50.490701
3503.290860	518984.160227	50.495706
3503.144604	518971.542614	50.500711
3502.654016	518977.789127	50.505716
3503.068526	518970.594317	50.510721
3502.676776	518960.948196	50.515725
3502.818473	518960.774301	50.520730
3503.080568	518957.294731	50.525735
3502.882605	518930.931911	50.530740
3502.879548	518895.335603	50.535745
3502.974033	518853.403291	50.540749
3502.791941	518784.007636	50.545754
3502.751921	518721.819955	50.550759
3502.884432	518652.020064	50.555764
3502.785068	518547.467833	50.560769
3502.206486	518451.283401	50.565773
3501.903402	518361.729521	50.570778
3502.096459	518247.976795	50.575783
3502.018050	518129.715230	50.580788
3501.665767	517994.455135	50.585793
3501.627645	517861.672631	50.590797
3501.221568	517710.136094	50.595802
3501.252556	517550.488761	50.600807
3500.716450	517396.289796	50.605812
3500.366451	517213.589600	50.610817
3500.134029	517052.108048	50.615821
3500.018369	516867.192504	50.620826
3499.895104	516666.902599	50.625831
3499.434247	516478.446771	50.630836
3499.149000	516280.554672	50.635841
3498.731582	516064.576135	50.640845
3498.645684	515844.698829	50.645850
3498.328429	515623.793145	50.650855
3497.761331	515391.898766	50.655860
3497.630367	515151.384996	50.660865
3497.148562	514915.576227	50.665869
3496.208095	514676.650302	50.670874
3495.990517	514420.865538	50.675879
3495.656281	514161.150207	50.680884
3495.550412	513888.952296	50.685889
3494.536755	513633.736603	50.690893
3494.277525	513358.165497	50.695898
3494.685281	513087.441451	50.700903
3493.820225	512808.972829	50.705908
3493.172661	512508.866185	50.710913
3492.768160	512230.011729	50.715917
3492.312487	511939.779154	50.720922
3491.842531	511630.371821	50.725927
3491.383159	511338.156696	50.730932
3490.738867	511026.793052	50.735937
3490.190212	510726.841626	50.740941
3489.388423	510414.277562	50.745946
3489.178753	510100.349417	50.750951
3488.521365	509801.258962	50.755956
3488.254263	509472.150968	50.760961
3487.448280	509161.537787	50.765965
3487.108599	508824.384522	50.770970
3486.844310	508501.784146	50.775975
3485.912181	508171.592688	50.780980
3485.628333	507833.702863	50.785985
3484.488638	507507.629880	50.790989
3483.975547	507164.298618	50.795994
3483.834044	506818.624809	50.800999
3483.034321	506475.173413	50.806004
3482.901377	506132.672470	50.811009
3482.297225	505789.379026	50.816013
3481.554101	505444.987500	50.821018
3480.923675	505086.148912	50.826023
3480.457198	504722.216428	50.831028
3480.044254	504371.780045	50.836033
3479.279579	504008.183521	50.841037
3478.368036	503652.295298	50.846042
3478.070024	503275.805717	50.851047
3477.350248	502922.352339	50.856052
3476.733687	502550.148986	50.861057
3475.880529	502194.424576	50.866061
3475.339109	501817.537506	50.871066
3474.962358	501446.791502	50.876071
3474.068352	501087.811971	50.881076
3473.757749	500699.425359	50.886081
3473.041627	500337.011199	50.891085
3472.474777	499956.292355	50.896090
3471.926347	499572.980838	50.901095
3470.857502	499204.980597	50.906100
3469.870524	498821.469244	50.911105
3469.208159	498455.161197	50.916109
3468.830293	498080.143845	50.921114
3468.491216	497704.251929	50.926119
3467.402339	497340.722506	50.931124
3467.077372	496950.738361	50.936129
3466.224108	496573.486680	50.941133
3465.805687	496220.714122	50.946138
3465.478367	495821.339524	50.951143
3464.429254	495437.158764	50.956148
3464.149706	495060.949627	50.961153
3463.463958	494666.872348	50.966157
3462.672897	494278.626350	50.971162
3462.016569	493895.667703	50.976167
3460.930972	493513.680430	50.981172
3460.764618	493122.576853	50.986177
3460.019821	492743.355535	50.991181
3459.463254	492353.208894	50.996186
3458.509121	491965.041292	51.001191
3457.831510	491581.481020	51.006196
3457.158402	491180.034768	51.011201
3456.349663	490799.365836	51.016205
3456.057397	490417.493281	51.021210
3455.109713	490035.108784	51.026215
3454.112661	489650.039933	51.031220
3453.730426	489262.789368	51.036225
3452.880752	488884.721791	51.041229
3452.071289	488504.259662	51.046234
3451.581108	488109.455422	51.051239
3450.683923	487733.499709	51.056244
3450.040239	487349.239793	51.061249
3449.495571	486979.443900	51.066253
3448.693334	486591.242605	51.071258
3448.291686	486205.300315	51.076263
3446.979982	485839.402877	51.081268
3446.750320	485454.786021	51.086273
3445.918328	485072.485735	51.091277
3445.183881	484700.548014	51.096282
3444.465873	484315.732243	51.101287
3444.057964	483932.987628	51.106292
3443.151118	483561.663144	51.111297
3442.537677	483178.480102	51.116301
3441.895566	482798.891333	51.121306
3440.922260	482415.699451	51.126311
3440.409594	482052.542546	51.131316
3439.902113	481670.782408	51.136321
3439.078412	481294.993231	51.141325
3438.212519	480920.520958	51.146330
3437.834658	480548.599330	51.151335
3436.984020	480172.539526	51.156340
3436.321331	479793.199668	51.161345
3435.812322	479426.446328	51.166349
3434.624776	479038.408132	51.171354
3434.245302	478668.326296	51.176359
3433.399937	478303.936470	51.181364
3432.865617	477932.547761	51.186369
3432.365316	477553.899513	51.191373
3431.625451	477182.123867	51.196378
3431.119432	476810.253645	51.201383
3430.255546	476432.857988	51.206388
3429.349076	476051.052472	51.211393
3428.349881	475688.311796	51.216397
3427.886221	475313.011255	51.221402
3427.550741	474936.416299	51.226407
3426.721758	474578.291897	51.231412
3426.201322	474194.159929	51.236417
3425.495850	473823.482615	51.241421
3424.689399	473459.708375	51.246426
3423.989720	473094.187253	51.251431
3423.250851	472721.011272	51.256436
3422.318637	472346.693105	51.261441
3421.754316	471981.029278	51.266445
3421.060855	471616.241161	51.271450
3420.460587	471248.136613	51.276455
3419.573367	470889.804599	51.281460
3419.076550	470519.287934	51.286465
3418.219987	470153.739250	51.291469
3417.429656	469791.570492	51.296474
3416.558417	469429.306801	51.301479
3415.949152	469075.513149	51.306484
3415.571627	468711.485763	51.311489
3414.747734	468365.420681	51.316493
3414.126150	468003.751872	51.321498
3413.543164	467629.141060	51.326503
3412.451570	467274.480500	51.331508
3411.831620	466922.376107	51.336513
3411.118438	466561.660362	51.341517
3410.420360	466211.584733	51.346522
3410.071120	465843.953612	51.351527
3409.008297	465493.822362	51.356532
3408.713357	465124.243210	51.361537
3407.558096	464791.508707	51.366541
3406.972063	464432.967934	51.371546
3406.641635	464071.642220	51.376551
3405.535896	463729.044984	51.381556
3404.802942	463372.436786	51.386561
3403.988092	463021.667899	51.391565
3403.611881	462669.657458	51.396570
3402.773320	462311.831177	51.401575
3402.008060	461977.013354	51.406580
3401.156870	461626.328951	51.411585
3400.569038	461282.596540	51.416589
3399.587249	460936.942880	51.421594
3399.175429	460584.853451	51.426599
3398.222601	460255.415182	51.431604
3397.253296	459912.380839	51.436609
3396.893885	459576.701047	51.441613
3396.043536	459234.296676	51.446618
3395.364004	458892.975908	51.451623
3394.734739	458574.772915	51.456628
3394.531109	458225.656217	51.461633
3393.538995	457890.050730	51.466637
3392.709082	457554.668144	51.471642
3392.312681	457213.733201	51.476647
3391.294484	456881.008108	51.481652
3390.321882	456544.973343	51.486657
3389.928688	456223.858354	51.491661
3389.161452	455892.194901	51.496666
3388.600955	455557.754270	51.501671
3387.805606	455244.045057	51.506676
3387.461829	454891.702033	51.511681
3386.622497	454566.879510	51.516685
3385.845949	454239.251911	51.521690
3385.267744	453896.265770	51.526695
3384.356275	453571.389595	51.531700
3383.849165	453237.667151	51.536705
3383.273478	452916.178680	51.541709
3382.166966	452580.207381	51.546714
3381.817279	452254.563936	51.551719
3380.941546	451929.963107	51.556724
3380.492685	451602.854574	51.561729
3379.863295	451283.736467	51.566733
3378.859346	450948.587604	51.571738
3378.390343	450612.182161	51.576743
3377.812168	450295.782419	51.581748
3377.050900	449979.255059	51.586753
3376.161911	449647.621281	51.591757
3375.407084	449325.146686	51.596762
3374.778205	449004.677591	51.601767
3373.994321	448680.726979	51.606772
3373.471572	448351.198957	51.611777
3372.859968	448033.657211	51.616781
3371.960174	447707.072451	51.621786
3371.509283	447386.908265	51.626791
3370.529107	447074.030130	51.631796
3370.008875	446739.454657	51.636801
3369.051787	446440.927342	51.641805
3368.244494	446115.219412	51.646810
3367.700742	445798.601095	51.651815
3366.488837	445496.143322	51.656820
3366.317255	445188.390875	51.661825
3365.352390	444888.424082	51.666829
3364.902357	444569.541306	51.671834
3364.202110	444268.814283	51.676839
3363.638953	443953.189656	51.681844
3363.180545	443633.737395	51.686849
3362.488299	443325.332683	51.691853
3361.751694	443004.494788	51.696858
3360.986021	442698.631673	51.701863
3360.191520	442390.941830	51.706868
3359.644796	442074.477804	51.711873
3358.569019	441766.926038	51.716877
3357.903988	441467.275281	51.721882
3357.614397	441148.727998	51.726887
3356.559003	440844.461015	51.731892
3355.706226	440548.636011	51.736897
3354.945395	440248.782382	51.741901
3354.123513	439945.990278	51.746906
3354.033915	439643.027873	51.751911
3353.157834	439355.365687	51.756916
3352.683216	439043.496280	51.761921
3351.960663	438740.673652	51.766925
3351.370206	438427.342491	51.771930
3350.724588	438130.592602	51.776935
3349.744707	437825.794068	51.781940
3348.954393	437518.220159	51.786945
3348.346218	437232.394907	51.791949
3347.594837	436925.264483	51.796954
3347.210118	436626.399138	51.801959
3345.829460	436336.014660	51.806964
3345.700794	436044.870312	51.811969
3344.826357	435742.187642	51.816973
3344.130983	435454.528028	51.821978
3343.762673	435158.003725	51.826983
3342.948377	434864.720036	51.831988
3342.233130	434559.789241	51.836993
3341.290364	434269.667197	51.841997
3340.699208	433969.508229	51.847002
3340.240780	433673.031627	51.852007
3339.236770	433398.625540	51.857012
3338.687495	433095.072817	51.862017
3338.304823	432805.810401	51.867021
3337.603887	432509.587203	51.872026
3336.819018	432214.770378	51.877031
3336.051216	431924.441757	51.882036
3335.573169	431628.655627	51.887041
3335.063706	431333.074222	51.892045
3333.996147	431038.110947	51.897050
3333.581892	430760.079384	51.902055
3332.398526	430467.438669	51.907060
3331.980082	430176.806717	51.912065
3331.561184	429888.761728	51.917069
3330.763562	429596.278791	51.922074
3330.253437	429301.741005	51.927079
3329.573802	429008.724986	51.932084
3329.041205	428722.335807	51.937089
3328.279698	428426.355107	51.942093
3327.229952	428136.740045	51.947098
3326.863732	427827.687867	51.952103
3326.224661	427550.978473	51.957108
3325.525829	427263.076070	51.962113
3324.943141	426972.993514	51.967117
3323.803709	426682.818080	51.972122
3323.446782	426388.147507	51.977127
3322.438264	426103.126012	51.982132
3322.041107	425812.544393	51.987137
3321.386241	425527.587848	51.992141
3320.659768	425243.071378	51.997146
3319.693536	424945.839999	52.002151
3318.857669	424675.430780	52.007156
3318.095893	424387.558316	52.012161
3317.577922	424103.123885	52.017165
3317.021447	423824.585167	52.022170
3316.615673	423539.517529	52.027175
3315.814959	423259.487708	52.032180
3315.146134	422970.467995	52.037185
3314.418682	422688.769758	52.042189
3313.271556	422412.951706	52.047194
3312.780235	422134.309296	52.052199
3312.195809	421850.141391	52.057204
3311.457973	421563.988131	52.062209
3310.771213	421293.344130	52.067213
3310.293811	421024.594906	52.072218
3309.578057	420741.655686	52.077223
3308.556163	420472.682422	52.082228
3307.955240	420199.016737	52.087233
3307.406350	419922.342624	52.092237
3306.438898	419644.207799	52.097242
3306.077514	419373.468308	52.102247
3305.231734	419098.662059	52.107252
3304.449259	418832.836025	52.112257
3303.796032	418556.317391	52.117261
3303.217900	418279.758772	52.122266
3302.781380	418010.415319	52.127271
3301.972610	417748.444729	52.132276
3301.090670	417460.240028	52.137281
3300.586308	417194.507076	52.142285
3299.826364	416915.448834	52.147290
3299.428010	416644.536704	52.152295
3298.443020	416386.138273	52.157300
3297.773459	416117.372746	52.162305
3297.235761	415846.576751	52.167309
3296.407888	415582.658479	52.172314
3296.063722	415292.847954	52.177319
3295.130517	415039.434404	52.182324
3295.040360	414765.330799	52.187329
3294.086171	414491.285046	52.192333
3293.099211	414227.735305	52.197338
3292.781506	413957.242577	52.202343
3291.865652	413689.586042	52.207348
3291.106916	413410.061859	52.212353
3291.068853	413141.067279	52.217357
3290.144497	412864.206602	52.222362
3289.651027	412595.329881	52.227367
3288.227836	412320.601141	52.232372
3287.951573	412051.786756	52.237377
3287.388677	411779.457885	52.242381
3286.071811	411516.774563	52.247386
3285.696721	411237.245368	52.252391
3284.952166	410983.055509	52.257396
3284.319775	410714.336189	52.262401
3283.610159	410451.445792	52.267405
3282.805735	410190.702629	52.272410
3282.169648	409916.233801	52.277415
3281.511171	409658.639373	52.282420
3280.991037	409401.173335	52.287425
3280.152143	409141.519255	52.292429
3279.614205	408880.087307	52.297434
3279.262903	408620.783653	52.302439
3278.320883	408352.524275	52.307444
3277.633250	408091.134632	52.312449
3276.967838	407825.774774	52.317453
3276.290146	407563.235447	52.322458
3275.673763	407293.720832	52.327463
3274.635714	407038.985180	52.332468
3274.119219	406772.906484	52.337473
3273.485814	406506.462769	52.342477
3272.461468	406255.632278	52.347482
3272.171553	405991.798320	52.352487
3271.307876	405747.063246	52.357492
3270.980871	405484.476175	52.362497
3269.964637	405239.710408	52.367501
3269.290096	404971.836767	52.372506
3268.918358	404705.031228	52.377511
3268.037127	404466.719075	52.382516
3267.392709	404202.493988	52.387521
3266.940728	403941.057462	52.392525
3265.861886	403686.987071	52.397530
3265.437544	403431.057348	52.402535
3264.866325	403180.384691	52.407540
3264.222472	402919.757994	52.412545
3263.237623	402661.013151	52.417549
3262.732069	402399.928220	52.422554
3262.200403	402147.461929	52.427559
3261.292580	401895.205652	52.432564
3260.450235	401639.759751	52.437569
3259.999248	401379.394989	52.442573
3259.236896	401132.244227	52.447578
3258.546828	400872.218204	52.452583
3257.800763	400633.881382	52.457588
3257.344003	400374.704117	52.462593
3256.680406	400117.540213	52.467597
3255.789290	399876.043333	52.472602
3255.193645	399610.044056	52.477607
3254.373410	399366.015619	52.482612
3253.604728	399117.782871	52.487617
3253.066882	398867.808559	52.492621
3252.186788	398627.342942	52.497626
3251.661177	398377.159595	52.502631
3250.761879	398130.439870	52.507636
3250.306851	397887.639147	52.512641
3249.840394	397643.211483	52.517645
3249.142867	397388.268629	52.522650
3248.675196	397133.058662	52.527655
3247.666174	396894.736266	52.532660
3247.196540	396648.827322	52.537665
3246.859007	396402.971939	52.542669
3245.892964	396147.553628	52.547674
3245.315463	395896.470033	52.552679
3244.581346	395640.807798	52.557684
3243.995591	395388.348884	52.562689
3243.247852	395143.235601	52.567693
3242.377238	394900.529783	52.572698
3241.909211	394649.699256	52.577703
3240.916824	394398.898978	52.582708
3240.266273	394149.288553	52.587713
3239.903878	393905.147764	52.592717
3239.064803	393672.165655	52.597722
3238.622179	393420.762739	52.602727
3237.735268	393178.809983	52.607732
3237.268965	392922.245950	52.612737
3236.846810	392675.207430	52.617741
3235.494685	392432.763678	52.622746
3235.067061	392172.552146	52.627751
3234.604096	391923.582386	52.632756
3233.744999	391686.267677	52.637761
3233.057338	391441.804957	52.642765
3232.571271	391190.596127	52.647770
3232.039363	390941.909955	52.652775
3230.895687	390701.353578	52.657780
3230.298708	390458.446093	52.662785
3229.795511	390201.639022	52.667789
3228.740228	389979.371080	52.672794
3228.608882	389723.061101	52.677799
3227.793516	389483.970121	52.682804
3227.096507	389246.155613	52.687809
3226.376331	388996.722703	52.692813
3225.512533	388750.845250	52.697818
3225.109841	388492.713101	52.702823
3223.975497	388264.013640	52.707828
3223.300481	388021.330705	52.712833
3222.779234	387785.614674	52.717837
3221.791466	387555.234659	52.722842
3221.462277	387313.305970	52.727847
3220.670353	387081.086498	52.732852
3219.999509	386835.902888	52.737857
3219.151953	386606.537261	52.742861
3218.897342	386369.701804	52.747866
3218.284318	386137.956605	52.752871
3217.448949	385908.457516	52.757876
3216.695033	385654.683803	52.762881
3216.275213	385421.301415	52.767885
3215.526362	385192.699657	52.772890
3214.891552	384940.326282	52.777895
3214.103585	384708.498032	52.782900
3212.896620	384476.353155	52.787905
3212.234928	384248.316688	52.792909
3211.817791	384013.424569	52.797914
3211.477924	383774.475158	52.802919
3210.531478	383545.411325	52.807924
3209.792393	383309.650183	52.812929
3209.251491	383079.832693	52.817933
3208.300197	382851.197733	52.822938
3207.898180	382621.202882	52.827943
3207.288462	382391.493813	52.832948
3206.648656	382166.340523	52.837953
3205.973537	381936.613612	52.842957
3205.291007	381702.969839	52.847962
3204.507213	381466.822794	52.852967
3203.494501	381246.707916	52.857972
3203.106019	381008.231954	52.862977
3202.717639	380777.181046	52.867981
3201.803501	380562.413092	52.872986
3201.285780	380324.055068	52.877991
3200.468494	380096.399747	52.882996
3199.883915	379874.123711	52.888001
3199.113619	379641.574958	52.893005
3198.406560	379411.074986	52.898010
3198.062664	379175.785389	52.903015
3197.161998	378958.971670	52.908020
3196.471756	378732.051305	52.913025
3196.080813	378497.350072	52.918029
3195.332774	378270.894014	52.923034
3194.419197	378030.117401	52.928039
3193.827063	377807.347552	52.933044
3193.283115	377578.489747	52.938049
3192.602852	377348.482150	52.943053
3191.875069	377123.567893	52.948058
3191.598726	376885.074474	52.953063
3190.736349	376659.568433	52.958068
3189.887697	376430.319827	52.963073
3189.368224	376188.401398	52.968077
3188.595566	375970.279267	52.973082
3187.773835	375730.568009	52.978087
3187.119218	375500.265940	52.983092
3186.243886	375280.553810	52.988097
3186.021030	375063.942330	52.993101
3184.902468	374839.077131	52.998106
3184.360830	374613.737854	53.003111
3183.491025	374397.047124	53.008116
3182.520304	374175.461753	53.013121
3182.604073	373944.983197	53.018125
3181.988997	373724.254883	53.023130
3181.327730	373492.721528	53.028135
3180.339786	373273.906775	53.033140
3180.019418	373045.369562	53.038145
3179.072702	372819.652102	53.043149
3178.383478	372597.683029	53.048154
3177.929263	372368.705381	53.053159
3177.321237	372151.223742	53.058164
3176.382289	371923.872122	53.063169
3176.014406	371706.121229	53.068173
3174.889238	371485.105602	53.073178
3174.565626	371253.938872	53.078183
3173.882550	371032.800053	53.083188
3172.907480	370797.103904	53.088193
3172.574337	370581.020739	53.093197
3171.552025	370360.746167	53.098202
3171.334688	370128.895061	53.103207
3170.589581	369910.253353	53.108212
3169.870123	369692.522323	53.113217
3169.224739	369459.132581	53.118221
3168.521432	369242.821386	53.123226
3167.869028	369018.817953	53.128231
3167.170481	368799.094727	53.133236
3166.643939	368574.382180	53.138241
3166.088412	368341.837190	53.143245
3165.106892	368115.387940	53.148250
3164.912768	367888.787493	53.153255
3164.108660	367676.300665	53.158260
3163.127778	367449.542574	53.163265
3162.772614	367215.128103	53.168269
3161.740001	366999.239520	53.173274
3161.100113	366765.173015	53.178279
3160.221773	366551.598508	53.183284
3159.844261	366327.079875	53.188289
3159.149468	366105.536190	53.193293
3158.220313	365887.565002	53.198298
3157.817245	365663.912125	53.203303
3157.179952	365442.992131	53.208308
3156.318132	365225.261501	53.213313
3155.919675	365007.889035	53.218317
3154.999678	364790.598046	53.223322
3154.441632	364560.705203	53.228327
3154.072825	364347.014154	53.233332
3153.159645	364123.205381	53.238337
3152.944078	363905.162614	53.243341
3151.931806	363683.835404	53.248346
3151.576710	363453.803102	53.253351
3150.895197	363228.630222	53.258356
3150.000473	363005.296513	53.263361
3149.183590	362768.158608	53.268365
3148.535634	362552.747731	53.273370
3148.214598	362328.556657	53.278375
3147.479649	362105.498673	53.283380
3146.469663	361871.949008	53.288385
3146.074127	361641.379786	53.293389
3145.035828	361430.554693	53.298394
3144.349708	361203.591606	53.303399
3143.600973	360990.734007	53.308404
3143.234344	360769.392574	53.313409
3142.294467	360553.357139	53.318413
3141.773767	360340.816779	53.323418
3141.215978	360116.957998	53.328423
3140.351678	359894.342624	53.333428
3140.048198	359678.304315	53.338433
3139.376675	359451.992169	53.343437
3138.340002	359239.426787	53.348442
3137.936216	359011.314423	53.353447
3137.033849	358794.043713	53.358452
3136.473594	358579.008084	53.363457
3135.701511	358363.750558	53.368461
3135.263347	358146.098145	53.373466
3134.660286	357918.953727	53.378471
3133.915488	357713.486070	53.383476
3133.118149	357483.520320	53.388481
3132.511099	357257.391364	53.393485
3131.670098	357050.689256	53.398490
3131.102630	356832.746136	53.403495
3130.491779	356628.168883	53.408500
3129.770835	356407.423510	53.413505
3129.226982	356180.847051	53.418509
3128.759956	355965.327237	53.423514
3128.072818	355743.224854	53.428519
3126.914134	355527.659925	53.433524
3126.320598	355302.563365	53.438529
3126.231894	355089.906493	53.443533
3125.143150	354880.079060	53.448538
3124.564908	354653.908374	53.453543
3123.921111	354429.273979	53.458548
3123.227060	354222.740612	53.463553
3122.735087	353990.801932	53.468557
3121.871497	353784.369980	53.473562
3121.468983	353550.022961	53.478567
3120.319594	353341.929380	53.483572
3119.789645	353118.340129	53.488577
3119.380352	352894.908972	53.493581
3118.197792	352694.834615	53.498586
3118.021672	352476.480121	53.503591
3117.192844	352262.859853	53.508596
3116.558934	352042.870872	53.513601
3115.927863	351816.696196	53.518605
3115.113576	351609.458914	53.523610
3114.513092	351381.114290	53.528615
3113.750149	351171.805719	53.533620
3113.258799	350954.767351	53.538625
3112.642906	350740.954566	53.543629
3111.813646	350532.468406	53.548634
3111.310844	350310.084636	53.553639
3110.926802	350100.813737	53.558644
3110.117998	349882.803260	53.563649
3109.312347	349653.083977	53.568653
3108.326976	349444.592886	53.573658
3107.936647	349230.356684	53.578663
3107.306060	349011.729150	53.583668
3106.753511	348790.314202	53.588673
3106.442014	348563.260902	53.593677
3105.764675	348349.244853	53.598682
3104.710128	348118.184165	53.603687
3104.287727	347897.050473	53.608692
3103.362831	347668.283513	53.613697
3102.777024	347453.765958	53.618701
3102.090233	347237.074688	53.623706
3101.424414	347011.954604	53.628711
3100.841525	346801.862780	53.633716
3099.803255	346579.014260	53.638721
3099.368825	346366.046668	53.643725
3098.612172	346152.416601	53.648730
3097.813621	345936.043483	53.653735
3097.413641	345711.894298	53.658740
3096.233013	345502.299531	53.663745
3096.064257	345290.533094	53.668749
3095.331137	345081.655025	53.673754
3094.787362	344856.507160	53.678759
3093.977164	344646.468883	53.683764
3093.423456	344421.244552	53.688769
3092.876082	344201.567194	53.693773
3092.191136	343986.594228	53.698778
3091.639315	343765.465099	53.703783
3090.754630	343552.889347	53.708788
3089.960325	343333.324201	53.713793
3089.269632	343116.363596	53.718797
3088.476142	342901.887504	53.723802
3088.356796	342677.733240	53.728807
3087.280925	342476.078244	53.733812
3086.634591	342260.685683	53.738817
3086.187110	342036.046426	53.743821
3085.542071	341831.317492	53.748826
3084.834645	341605.063244	53.753831
3083.941604	341390.724826	53.758836
3082.989078	341166.238658	53.763841
3082.666967	340961.073888	53.768845
3081.833259	340755.887581	53.773850
3080.961657	340536.222734	53.778855
3080.678116	340318.042257	53.783860
3079.810976	340111.815458	53.788865
3079.541639	339903.024217	53.793869
3078.669196	339694.124086	53.798874
3077.951482	339481.635024	53.803879
3077.478408	339261.775359	53.808884
3076.759181	339047.808663	53.813889
3076.168291	338834.915527	53.818893
3075.262785	338623.802460	53.823898
3074.703716	338410.011922	53.828903
3074.117414	338183.878882	53.833908
3073.155828	337980.816634	53.838913
3072.670556	337758.662700	53.843917
3072.019998	337551.069616	53.848922
3071.606748	337337.736122	53.853927
3070.715739	337131.834411	53.858932
3070.212192	336907.745792	53.863937
3069.651666	336686.745660	53.868941
3068.710304	336475.173070	53.873946
3068.022661	336253.173345	53.878951
3067.244775	336039.256939	53.883956
3066.491760	335841.271863	53.888961
3066.071079	335622.206231	53.893965
3065.275064	335413.076585	53.898970
3064.710164	335196.221689	53.903975
3063.844105	334987.916436	53.908980
3063.417338	334778.089960	53.913985
3062.851640	334557.414570	53.918989
3062.090673	334350.083568	53.923994
3061.922037	334130.693202	53.928999
3060.899831	333907.389483	53.934004
3060.262420	333703.320998	53.939009
3059.837379	333478.292099	53.944013
3058.815032	333267.842466	53.949018
3058.186816	333046.077462	53.954023
3057.441789	332835.455350	53.959028
3056.631517	332624.690186	53.964033
3056.513150	332404.828191	53.969037
3055.289711	332199.575177	53.974042
3054.967403	331986.032323	53.979047
3054.222560	331760.030227	53.984052
3053.505118	331549.272645	53.989057
3053.268484	331332.048279	53.994061
3052.167863	331130.566074	53.999066
3051.664229	330894.772481	54.004071
3050.772068	330685.185673	54.009076
3050.426942	330470.929111	54.014081
3049.840567	330252.687613	54.019085
3048.894288	330041.885511	54.024090
3048.356393	329825.238986	54.029095
3047.836419	329605.406614	54.034100
3046.936331	329390.852873	54.039105
3046.223637	329166.670744	54.044109
3045.458624	328953.036362	54.049114
3044.798232	328747.990070	54.054119
3044.274164	328541.954190	54.059124
3043.171731	328322.541232	54.064129
3043.170896	328106.237569	54.069133
3042.029824	327907.553602	54.074138
3040.992929	327689.757874	54.079143
3040.712188	327478.257710	54.084148
3039.987314	327273.854174	54.089153
3039.292901	327063.029389	54.094157
3038.469238	326850.060397	54.099162
3038.380512	326642.091969	54.104167
3037.396995	326431.744067	54.109172
3036.584339	326223.558137	54.114177
3036.273679	326010.123781	54.119181
3035.475657	325811.303820	54.124186
3034.801150	325598.104175	54.129191
3034.616972	325385.972076	54.134196
3033.582561	325171.453404	54.139201
3033.108043	324961.046539	54.144205
3032.511539	324745.693616	54.149210
3031.681338	324525.055830	54.154215
3030.914713	324318.436269	54.159220
3030.215603	324112.925780	54.164225
3029.541362	323881.720809	54.169229
3028.973412	323674.202525	54.174234
3028.150821	323471.077865	54.179239
3027.832601	323255.906174	54.184244
3026.949275	323042.682043	54.189249
3026.574065	322830.013480	54.194253
3025.756079	322623.092333	54.199258
3025.163368	322397.013565	54.204263
3024.425786	322185.546516	54.209268
3023.816010	321974.618871	54.214273
3023.118747	321761.336639	54.219277
3022.251473	321548.437256	54.224282
3021.559929	321332.810605	54.229287
3021.120307	321118.162017	54.234292
3020.459415	320907.800048	54.239297
3019.692204	320691.470877	54.244301
3018.597544	320480.820089	54.249306
3018.051229	320265.829864	54.254311
3017.552466	320054.447205	54.259316
3017.041313	319857.426622	54.264321
3016.612586	319637.018329	54.269325
3015.643536	319434.671336	54.274330
3015.040342	319218.261750	54.279335
3014.425010	319008.270077	54.284340
3013.974157	318796.189442	54.289345
3013.518577	318584.338233	54.294349
3012.753873	318377.526119	54.299354
3011.792381	318146.758987	54.304359
3011.132424	317924.982784	54.309364
3010.299739	317727.270154	54.314369
3009.803300	317510.534169	54.319373
3009.026324	317295.879122	54.324378
3008.389999	317082.449010	54.329383
3007.841859	316873.460473	54.334388
3007.121561	316659.940871	54.339393
3006.552846	316437.382909	54.344397
3005.640088	316235.605824	54.349402
3005.019261	316025.201051	54.354407
3004.645747	315807.576074	54.359412
3003.866908	315598.952369	54.364417
3003.191368	315376.281620	54.369421
3002.388555	315170.589096	54.374426
3001.706524	314957.136170	54.379431
3001.156226	314750.842631	54.384436
3000.336428	314528.676663	54.389441
2999.761654	314320.399981	54.394445
2999.182676	314114.084241	54.399450
2998.275494	313896.386874	54.404455
2997.693458	313688.415640	54.409460
2996.802331	313491.162226	54.414465
2996.532005	313275.450788	54.419469
2995.415884	313061.731657	54.424474
2995.039687	312858.946299	54.429479
2994.235757	312653.147130	54.434484
2993.534309	312445.243300	54.439489
2993.152644	312232.475750	54.444493
2992.169672	312033.884606	54.449498
2991.761719	311816.205841	54.454503
2991.365804	311600.460020	54.459508
2990.488519	311394.288136	54.464513
2989.711692	311182.141329	54.469517
2988.687796	310978.792958	54.474522
2988.355113	310783.228756	54.479527
2987.606452	310566.874716	54.484532
2987.004188	310362.541780	54.489537
2986.642404	310142.382422	54.494541
2985.776996	309945.373250	54.499546
2985.012508	309742.312662	54.504551
2984.670890	309526.274210	54.509556
2983.555811	309326.909844	54.514561
2983.347749	309116.502659	54.519565
2982.329065	308901.563372	54.524570
2982.118700	308692.760087	54.529575
2981.079590	308476.015271	54.534580
2980.342042	308278.193684	54.539585
2980.099051	308059.590487	54.544589
2979.156356	307854.976086	54.549594
2978.780698	307636.978836	54.554599
2978.050542	307428.612192	54.559604
2976.956948	307223.893317	54.564609
2976.498246	307006.952187	54.569613
2975.660263	306796.869938	54.574618
2975.304582	306589.588567	54.579623
2974.512584	306379.167306	54.584628
2973.708609	306166.735838	54.589633
2973.420521	305957.252736	54.594637
2972.726080	305748.393866	54.599642
2972.243321	305534.535393	54.604647
2971.522577	305328.990536	54.609652
2970.747852	305120.168855	54.614657
2970.353636	304898.833950	54.619661
2969.733098	304681.379820	54.624666
2968.563945	304460.192346	54.629671
2967.964428	304253.124197	54.634676
2967.277969	304053.021647	54.639681
2966.961122	303838.624935	54.644685
2966.128699	303624.640571	54.649690
2965.663733	303417.269765	54.654695
2965.123427	303193.612421	54.659700
2964.548735	302979.840951	54.664705
2963.992570	302762.577396	54.669709
2962.682897	302545.814797	54.674714
2962.056652	302325.734965	54.679719
2961.844834	302109.765635	54.684724
2960.734797	301895.542556	54.689729
2960.241784	301672.104612	54.694733
2959.214767	301457.511244	54.699738
2958.539086	301249.355842	54.704743
2957.920352	301036.836415	54.709748
2957.310878	300828.568103	54.714753
2956.582799	300623.577979	54.719757
2956.238471	300417.482718	54.724762
2955.792252	300198.160802	54.729767
2954.922268	299989.550637	54.734772
2954.128902	299778.279564	54.739777
2953.689646	299561.655130	54.744781
2953.061249	299346.180882	54.749786
2952.391492	299131.629699	54.754791
2951.370840	298911.913145	54.759796
2950.568284	298700.744028	54.764801
2950.518469	298489.506414	54.769805
2949.561247	298275.152463	54.774810
2949.066384	298060.903316	54.779815
2948.545937	297846.989027	54.784820
2947.598428	297633.065691	54.789825
2946.983294	297415.193058	54.794829
2946.304035	297211.948276	54.799834
2945.608752	296985.734698	54.804839
2944.903335	296767.951987	54.809844
2944.309340	296562.808441	54.814849
2943.715722	296347.019428	54.819853
2942.865694	296136.669762	54.824858
2942.198052	295919.644103	54.829863
2941.915133	295698.711771	54.834868
2940.963350	295493.241720	54.839873
2940.417417	295273.904041	54.844877
2939.664002	295060.227202	54.849882
2938.952824	294846.823589	54.854887
2938.335167	294636.002598	54.859892
2937.577593	294429.278294	54.864897
2936.970307	294206.536578	54.869901
2936.136755	293990.833942	54.874906
2935.762245	293785.856535	54.879911
2935.089359	293566.766356	54.884916
2934.425275	293352.615224	54.889921
2933.429131	293132.557098	54.894925
2932.797166	292927.084835	54.899930
2932.275146	292720.092402	54.904935
2931.654103	292499.974273	54.909940
2930.857611	292282.990739	54.914945
2930.564800	292060.095211	54.919949
2929.917085	291857.094836	54.924954
2929.096589	291642.482993	54.929959
2928.670058	291431.323105	54.934964
2927.515633	291212.408806	54.939969
2927.211423	290987.272955	54.944973
2926.352726	290787.106535	54.949978
2926.000682	290569.567231	54.954983
2925.232936	290346.261471	54.959988
2924.403307	290134.833250	54.964993
2923.641054	289929.048018	54.969997
2923.057591	289722.623099	54.975002
2922.493499	289500.710584	54.980007
2921.983785	289278.305396	54.985012
2921.060491	289079.064771	54.990017
2920.874136	288854.927184	54.995021
2919.880770	288650.374593	55.000026
2919.311714	288422.782712	55.005031
2918.716187	288201.918359	55.010036
2917.960937	287985.586944	55.015041
2917.457541	287766.872459	55.020045
2916.580220	287555.984731	55.025050
2915.883470	287333.556783	55.030055
2915.347040	287117.037325	55.035060
2914.798628	286906.708332	55.040065
2914.135338	286672.024567	55.045069
2913.164286	286453.281384	55.050074
2912.796896	286238.288152	55.055079
2911.854329	286021.755907	55.060084
2911.095123	285809.600469	55.065089
2910.455487	285580.056782	55.070093
2909.784508	285369.033188	55.075098
2908.918077	285148.668179	55.080103
2908.323066	284936.562666	55.085108
2907.493958	284735.878340	55.090113
2907.381819	284524.689413	55.095117
2906.781191	284311.030913	55.100122
2906.110337	284092.926506	55.105127
2905.171376	283884.873418	55.110132
2904.529264	283667.324550	55.115137
2904.175373	283443.897737	55.120141
2903.068535	283233.884421	55.125146
2902.528091	283023.552120	55.130151
2902.173392	282802.621022	55.135156
2901.126019	282593.234726	55.140161
2900.767337	282372.049393	55.145165
2899.820862	282151.517339	55.150170
2899.157565	281943.445264	55.155175
2898.774062	281734.055399	55.160180
2897.998944	281523.479523	55.165185
2897.439393	281296.162264	55.170189
2896.544908	281090.113024	55.175194
2895.860885	280871.907495	55.180199
2895.423428	280659.265878	55.185204
2894.573446	280443.123954	55.190209
2893.937458	280222.694876	55.195213
2893.236214	280015.494118	55.200218
2892.574065	279803.855629	55.205223
2891.984520	279594.319459	55.210228
2891.275887	279378.180331	55.215233
2890.785592	279153.678434	55.220237
2889.766072	278947.597484	55.225242
2889.105535	278732.291048	55.230247
2889.247784	278519.251477	55.235252
2888.297833	278299.100857	55.240257
2887.609113	278080.538807	55.245261
2887.205366	277865.369825	55.250266
2886.642434	277645.157809	55.255271
2885.685528	277417.316695	55.260276
2884.707771	277202.187568	55.265281
2884.180956	276978.913536	55.270285
2883.235675	276767.497599	55.275290
2882.418266	276546.230597	55.280295
2882.245415	276322.569359	55.285300
2881.526434	276109.614895	55.290305
2880.779689	275901.580213	55.295309
2880.161460	275692.786586	55.300314
2879.309784	275468.061235	55.305319
2878.734453	275250.958103	55.310324
2877.847467	275050.153150	55.315329
2877.430900	274831.802389	55.320333
2876.752640	274618.281124	55.325338
2876.142131	274409.791874	55.330343
2875.395609	274176.288739	55.335348
2874.743563	273976.592673	55.340353
2874.114756	273757.435087	55.345357
2873.675570	273542.526177	55.350362
2873.057538	273324.054559	55.355367
2872.529816	273101.621060	55.360372
2871.566229	272897.313680	55.365377
2871.463498	272666.943198	55.370381
2870.403039	272454.526792	55.375386
2869.395161	272234.869069	55.380391
2869.132131	272018.811812	55.385396
2868.318805	271799.709118	55.390401
2867.649128	271577.680319	55.395405
2866.940824	271361.922892	55.400410
2866.402635	271138.396188	55.405415
2865.778959	270920.358761	55.410420
2864.918216	270707.656333	55.415425
2864.468837	270476.144118	55.420429
2863.873376	270268.264231	55.425434
2862.706225	270060.831476	55.430439
2862.580515	269835.711658	55.435444
2861.596902	269622.213959	55.440449
2861.282808	269399.823735	55.445453
2860.285215	269185.487917	55.450458
2859.694859	268964.873415	55.455463
2859.408451	268744.618343	55.460468
2858.180873	268525.556581	55.465473
2858.070282	268298.320980	55.470477
2857.482119	268081.959625	55.475482
2856.419495	267861.063728	55.480487
2855.898350	267640.133106	55.485492
2855.264627	267424.823406	55.490497
2854.610003	267204.041434	55.495501
2854.052556	266995.316091	55.500506
2853.390725	266763.431309	55.505511
2853.265235	266533.601027	55.510516
2852.144525	266317.044558	55.515521
2851.584351	266080.992688	55.520525
2850.717657	265861.110811	55.525530
2849.604412	265640.835125	55.530535
2849.368185	265411.965251	55.535540
2848.763437	265190.590541	55.540545
2847.780823	264968.842829	55.545549
2846.995952	264747.165793	55.550554
2846.393275	264530.859255	55.555559
2845.636273	264309.152580	55.560564
2844.835275	264108.158509	55.565569
2844.637297	263878.646741	55.570573
2843.774009	263661.872602	55.575578
2843.001344	263445.670004	55.580583
2842.661117	263228.354868	55.585588
2841.637890	263010.307585	55.590593
2841.545551	262785.058403	55.595597
2840.742347	262574.234917	55.600602
2839.824090	262346.366287	55.605607
2839.645354	262130.528886	55.610612
2838.378592	261921.434644	55.615617
2838.106073	261687.173656	55.620621
2837.430896	261464.335264	55.625626
2836.660127	261249.738278	55.630631
2836.286333	261019.110270	55.635636
2835.390546	260803.209078	55.640641
2834.741556	260574.713357	55.645645
2833.947893	260352.658600	55.650650
2833.198493	260135.308536	55.655655
2832.737169	259912.055450	55.660660
2831.894835	259699.559309	55.665665
2831.413914	259470.757735	55.670669
2831.073687	259245.957962	55.675674
2829.755729	259032.748181	55.680679
2829.538964	258802.810248	55.685684
2828.636414	258589.687854	55.690689
2828.048479	258363.170821	55.695693
2827.315521	258154.962643	55.700698
2826.492300	257932.456202	55.705703
2826.247174	257711.513799	55.710708
2825.502838	257495.387606	55.715713
2824.564394	257270.607958	55.720717
2823.899199	257049.146951	55.725722
2823.260543	256837.206755	55.730727
2823.046457	256602.609971	55.735732
2821.777041	256395.303274	55.740737
2821.703181	256174.844570	55.745741
2820.897097	255955.393406	55.750746
2820.020169	255743.211852	55.755751
2819.589103	255513.234704	55.760756
2818.741155	255296.184765	55.765761
2818.076309	255077.399753	55.770765
2817.746032	254842.008339	55.775770
2816.818702	254628.817213	55.780775
2816.304020	254406.596542	55.785780
2815.127164	254193.852869	55.790785
2814.660049	253963.144628	55.795789
2814.227670	253754.078113	55.800794
2813.317288	253531.615494	55.805799
2812.953957	253301.018939	55.810804
2812.272948	253084.123244	55.815809
2811.391862	252877.089706	55.820813
2811.119431	252644.722344	55.825818
2809.703470	252434.972658	55.830823
2809.354781	252203.611139	55.835828
2808.734125	251989.712257	55.840833
2808.247553	251771.539449	55.845837
2807.363022	251562.852619	55.850842
2806.627364	251332.521253	55.855847
2806.376399	251109.193153	55.860852
2805.506403	250898.645754	55.865857
2804.795699	250677.097291	55.870861
2804.397612	250458.937591	55.875866
2803.534747	250232.575170	55.880871
2803.121667	250011.336981	55.885876
2802.023115	249802.253281	55.890881
2801.534350	249568.574588	55.895885
2800.827296	249353.495788	55.900890
2799.929418	249139.950013	55.905895
2799.635987	248909.883028	55.910900
2799.003908	248695.760963	55.915905
2798.347147	248474.359758	55.920909
2797.663679	248250.009022	55.925914
2797.058592	248034.024563	55.930919
2796.280557	247807.601228	55.935924
2795.288935	247583.860533	55.940929
2795.306685	247356.191330	55.945933
2794.337846	247137.591836	55.950938
2793.435960	246931.460385	55.955943
2792.838735	246707.378422	55.960948
2792.136765	246486.573029	55.965953
2791.938648	246266.935998	55.970957
2791.070725	246052.167498	55.975962
2790.357892	245823.928831	55.980967
2790.016115	245595.428038	55.985972
2789.312106	245385.294823	55.990977
2788.396675	245152.556447	55.995981
2787.830195	244926.613445	56.000986
2786.845339	244703.436431	56.005991
2786.381152	244478.572990	56.010996
2785.761127	244267.078520	56.016001
2785.242418	244033.591661	56.021005
2784.625218	243818.455898	56.026010
2783.832284	243596.498140	56.031015
2783.351263	243367.590256	56.036020
2782.374384	243155.670251	56.041025
2781.754674	242925.486387	56.046029
2781.283337	242700.168751	56.051034
2780.543122	242480.802012	56.056039
2780.062548	242251.870586	56.061044
2779.266958	242033.990371	56.066049
2778.738642	241807.562896	56.071053
2777.876963	241578.463886	56.076058
2777.030928	241361.535049	56.081063
2776.464026	241129.410796	56.086068
2775.408555	240912.083032	56.091073
2775.228456	240694.158643	56.096077
2774.622781	240469.834020	56.101082
2773.703152	240249.939471	56.106087
2773.122742	240022.581397	56.111092
2772.361301	239809.665386	56.116097
2772.154154	239593.096933	56.121101
2771.121514	239365.149693	56.126106
2770.416823	239144.917609	56.131111
2769.731486	238918.647827	56.136116
2769.013861	238696.636151	56.141121
2768.610549	238480.966660	56.146125
2767.897530	238246.324860	56.151130
2766.899166	238033.195049	56.156135
2766.466114	237812.897078	56.161140
2765.754634	237602.370925	56.166145
2765.321044	237372.830461	56.171149
2764.322612	237154.176671	56.176154
2763.603392	236930.233530	56.181159
2763.317401	236711.111294	56.186164
2762.048713	236496.805040	56.191169
2761.866400	236274.738938	56.196173
2761.480805	236059.326064	56.201178
2760.863559	235837.558946	56.206183
2759.997917	235599.585864	56.211188
2759.138989	235394.231065	56.216193
2758.526575	235159.503679	56.221197
2757.950608	234948.197416	56.226202
2757.157394	234726.969818	56.231207
2756.782230	234498.928699	56.236212
2756.156244	234281.011278	56.241217
2755.259042	234054.428870	56.246221
2754.903301	233832.828376	56.251226
2754.055567	233606.799337	56.256231
2753.585717	233383.842911	56.261236
2752.619544	233163.028109	56.266241
2751.717340	232929.599524	56.271245
2751.418639	232713.441576	56.276250
2750.419364	232495.001578	56.281255
2750.089638	232268.613489	56.286260
2749.408585	232052.415737	56.291265
2748.683914	231818.019600	56.296269
2748.130969	231604.628924	56.301274
2747.163740	231386.746563	56.306279
2747.054703	231156.252164	56.311284
2746.378994	230945.199514	56.316289
2745.697521	230707.030870	56.321293
2744.980706	230482.159740	56.326298
2744.258926	230259.785242	56.331303
2743.655038	230022.344483	56.336308
2742.755801	229805.295327	56.341313
2741.978747	229572.339037	56.346317
2741.158003	229352.121245	56.351322
2740.838722	229131.977329	56.356327
2740.113390	228915.030081	56.361332
2739.445124	228694.025902	56.366337
2738.811068	228469.630450	56.371341
2738.157308	228248.676011	56.376346
2737.649154	228027.266217	56.381351
2737.250554	227793.974570	56.386356
2736.316450	227573.855555	56.391361
2735.625047	227347.689771	56.396365
2735.080033	227116.103597	56.401370
2734.488029	226890.305193	56.406375
2733.797429	226658.539632	56.411380
2732.698976	226440.919299	56.416385
2732.099862	226206.416147	56.421389
2731.613914	225976.567809	56.426394
2730.363196	225762.627003	56.431399
2730.410384	225537.634833	56.436404
2729.544772	225322.641184	56.441409
2728.902500	225100.725599	56.446413
2727.892869	224875.648039	56.451418
2727.472834	224647.855263	56.456423
2726.995162	224429.403521	56.461428
2726.047349	224218.868652	56.466433
2725.682011	223991.234550	56.471437
2725.068762	223759.974085	56.476442
2724.348069	223539.310022	56.481447
2723.936594	223308.006174	56.486452
2723.139649	223084.020179	56.491457
2722.188672	222860.721181	56.496461
2721.528273	222631.750145	56.501466
2720.885800	222406.443157	56.506471
2720.526913	222185.420054	56.511476
2719.388117	221960.574880	56.516481
2719.077016	221736.337569	56.521485
2718.366965	221516.594072	56.526490
2717.574423	221292.918055	56.531495
2716.920956	221062.295709	56.536500
2716.414950	220848.492040	56.541505
2715.600752	220612.371854	56.546509
2715.092209	220390.473846	56.551514
2714.157480	220176.625435	56.556519
2713.493448	219940.661788	56.561524
2712.837943	219725.115602	56.566529
2712.473402	219493.841292	56.571533
2711.936410	219273.567760	56.576538
2711.008487	219055.737207	56.581543
2710.454710	218816.259118	56.586548
2709.939425	218593.298309	56.591553
2709.096455	218370.033678	56.596557
2708.321133	218141.756447	56.601562
2707.839927	217929.433891	56.606567
2707.308577	217692.476342	56.611572
2706.505856	217472.403130	56.616577
2706.091309	217244.618955	56.621581
2705.381825	217019.122539	56.626586
2704.246473	216803.762911	56.631591
2703.742049	216559.994890	56.636596
2703.143163	216341.764060	56.641601
2702.446482	216118.279670	56.646605
2701.957064	215895.806924	56.651610
2701.223133	215657.717272	56.656615
2700.738354	215435.143443	56.661620
2699.991662	215221.432790	56.666625
2699.419165	214985.891080	56.671629
2699.041375	214752.139522	56.676634
2697.809795	214522.966288	56.681639
2697.234791	214291.869638	56.686644
2696.402283	214068.629841	56.691649
2695.797779	213844.514590	56.696653
2695.088949	213616.878132	56.701658
2694.235255	213393.694856	56.706663
2693.923974	213166.098784	56.711668
2692.932186	212952.841468	56.716673
2692.333917	212726.857948	56.721677
2691.772056	212504.191482	56.726682
2691.170656	212285.477750	56.731687
2690.704130	212061.104852	56.736692
2690.040252	211832.691028	56.741697
2689.359905	211601.569561	56.746701
2688.875939	211380.371047	56.751706
2687.849806	211157.604564	56.756711
2687.648788	210927.084157	56.761716
2686.457063	210700.590789	56.766721
2685.887447	210474.636053	56.771725
2685.376546	210243.976298	56.776730
2684.187416	210028.048913	56.781735
2683.513447	209809.329670	56.786740
2683.032870	209583.669481	56.791745
2682.418283	209364.267822	56.796749
2681.747298	209134.757527	56.801754
2680.933080	208921.714612	56.806759
2680.599894	208694.061543	56.811764
2679.678303	208482.768076	56.816769
2679.094627	208258.058138	56.821773
2678.487400	208030.056398	56.826778
2677.843318	207817.664895	56.831783
2677.291716	207597.814095	56.836788
2676.674571	207371.025472	56.841793
2675.813746	207149.443494	56.846797
2675.442953	206914.675868	56.851802
2674.556450	206705.610247	56.856807
2674.103622	206467.522902	56.861812
2673.231293	206252.716779	56.866817
2672.198392	206026.597273	56.871821
2671.975621	205803.328339	56.876826
2671.122641	205586.892536	56.881831
2670.410858	205358.332083	56.886836
2670.125100	205144.378827	56.891841
2669.325189	204915.452264	56.896845
2668.850024	204694.276512	56.901850
2667.791977	204473.003054	56.906855
2667.449767	204241.499507	56.911860
2666.777493	204022.266513	56.916865
2665.718444	203793.741774	56.921869
2665.541463	203577.817205	56.926874
2664.716810	203351.229667	56.931879
2664.057083	203126.843980	56.936884
2663.528644	202904.703630	56.941889
2662.794108	202678.638990	56.946893
2662.287976	202460.429208	56.951898
2661.594831	202237.668545	56.956903
2661.023205	202000.521929	56.961908
2660.285970	201776.688377	56.966913
2659.169695	201556.389931	56.971917
2658.784050	201319.089482	56.976922
2658.088419	201105.788982	56.981927
2657.744239	200869.158352	56.986932
2656.796921	200652.514451	56.991937
2656.299523	200422.374634	56.996941
2655.561554	200193.419197	57.001946
2654.654354	199981.390955	57.006951
2654.431422	199741.475533	57.011956
2653.851196	199523.709006	57.016961
2652.719698	199293.890755	57.021965
2652.345959	199063.737090	57.026970
2651.840086	198839.560738	57.031975
2651.211104	198609.576710	57.036980
2650.196574	198388.002420	57.041985
2649.786805	198159.029055	57.046989
2649.063038	197919.939164	57.051994
2648.230326	197700.731225	57.056999
2647.790069	197467.680971	57.062004
2646.780699	197247.764861	57.067009
2646.171462	197020.596778	57.072013
2645.764388	196786.309983	57.077018
2644.884493	196566.350768	57.082023
2644.709010	196335.668551	57.087028
2643.563689	196118.769014	57.092033
2642.996588	195889.385113	57.097037
2642.407862	195662.601440	57.102042
2641.408600	195438.759524	57.107047
2640.994067	195204.493784	57.112052
2640.456756	194980.275289	57.117057
2639.688934	194750.215718	57.122061
2638.797395	194519.693272	57.127066
2638.220336	194295.382296	57.132071
2637.644121	194068.540096	57.137076
2637.034520	193848.295227	57.142081
2636.296055	193630.985518	57.147085
2635.901618	193392.704198	57.152090
2634.945352	193175.456422	57.157095
2634.490393	192947.811193	57.162100
2633.903318	192717.974015	57.167105
2632.968281	192496.870557	57.172109
2632.168911	192268.188782	57.177114
2631.546264	192050.791274	57.182119
2631.070647	191820.533452	57.187124
2630.424358	191602.518220	57.192129
2629.808311	191368.226005	57.197133
2629.430300	191135.894751	57.202138
2628.280643	190911.982419	57.207143
2627.969001	190687.823821	57.212148
2626.952013	190452.708923	57.217153
2626.491299	190233.843415	57.222157
2625.962932	190001.223347	57.227162
2625.053800	189783.079815	57.232167
2624.786342	189546.667341	57.237172
2624.100708	189324.228325	57.242177
2622.783898	189089.727417	57.247181
2622.378318	188867.793233	57.252186
2621.617431	188641.883317	57.257191
2621.341885	188412.716932	57.262196
2620.375067	188184.004706	57.267201
2619.415181	187964.910658	57.272205
2619.144549	187748.418281	57.277210
2618.674920	187520.495624	57.282215
2617.740509	187283.564038	57.287220
2617.005766	187063.967812	57.292225
2616.580127	186843.560315	57.297229
2615.859807	186609.664275	57.302234
2614.829345	186384.456809	57.307239
2614.660962	186153.821505	57.312244
2613.764380	185938.174633	57.317249
2613.146009	185707.561990	57.322253
2612.298416	185478.030015	57.327258
2611.486633	185257.716751	57.332263
2611.296205	185027.192391	57.337268
2610.581149	184817.424889	57.342273
2609.803920	184596.931253	57.347277
2608.917331	184361.177564	57.352282
2608.185037	184136.709966	57.357287
2607.880466	183917.658597	57.362292
2607.554925	183692.683516	57.367297
2606.557887	183469.736875	57.372301
2605.944936	183236.006572	57.377306
2604.862745	183017.693456	57.382311
2604.516012	182785.259048	57.387316
2603.452504	182570.074542	57.392321
2602.945412	182346.254483	57.397325
2602.935918	182127.508634	57.402330
2601.797971	181900.101780	57.407335
2600.938204	181674.076739	57.412340
2600.253218	181454.042017	57.417345
2599.720995	181236.909921	57.422349
2599.234536	181011.388857	57.427354
2598.463906	180799.244994	57.432359
2598.007011	180564.753670	57.437364
2597.131278	180352.285203	57.442369
2596.342730	180127.732474	57.447373
2596.051778	179891.882885	57.452378
2595.065420	179671.765059	57.457383
2594.449952	179448.867503	57.462388
2594.103453	179232.479263	57.467393
2593.008905	179002.282386	57.472397
2592.536726	178783.448686	57.477402
2591.645821	178560.739346	57.482407
2591.348683	178335.545781	57.487412
2590.345515	178112.691236	57.492417
2590.036577	177886.535245	57.497421
2589.488740	177652.939272	57.502426
2588.474293	177434.007714	57.507431
2587.957297	177217.148038	57.512436
2587.245216	176999.976984	57.517441
2586.458385	176772.936077	57.522445
2586.167082	176547.725754	57.527450
2585.045847	176335.469008	57.532455
2584.723380	176100.942966	57.537460
2584.251898	175883.001930	57.542465
2583.270840	175658.160142	57.547469
2582.974842	175428.772156	57.552474
2581.983779	175212.824835	57.557479
2581.516592	174977.717638	57.562484
2580.756125	174749.119315	57.567489
2580.210281	174518.237085	57.572493
2579.760049	174287.608102	57.577498
2578.629915	174080.769798	57.582503
2578.329272	173841.483870	57.587508
2577.639998	173618.756497	57.592513
2576.934294	173391.403548	57.597517
2576.440792	173161.029505	57.602522
2575.447011	172931.702640	57.607527
2574.866113	172704.982425	57.612532
2574.230010	172479.620341	57.617537
2573.651431	172251.910341	57.622541
2572.942166	172023.713649	57.627546
2572.131611	171803.889822	57.632551
2571.739305	171562.190280	57.637556
2570.863081	171338.233522	57.642561
2569.999715	171118.676233	57.647565
2569.932192	170886.785377	57.652570
2568.978092	170659.614621	57.657575
2568.082707	170429.549073	57.662580
2567.639277	170206.293226	57.667585
2566.690862	169975.564754	57.672589
2566.080651	169748.739036	57.677594
2565.584224	169541.099158	57.682599
2564.639740	169298.788978	57.687604
2564.030786	169075.731192	57.692609
2563.580966	168859.045975	57.697613
2562.771960	168632.588955	57.702618
2561.872856	168417.032917	57.707623
2561.504049	168184.392120	57.712628
2560.672773	167964.695029	57.717633
2560.117985	167742.513850	57.722637
2559.371666	167516.587597	57.727642
2558.698430	167300.531575	57.732647
2558.083571	167068.890308	57.737652
2557.700546	166850.908876	57.742657
2557.130359	166629.474194	57.747661
2556.639681	166393.722855	57.752666
2555.704972	166172.526659	57.757671
2555.108668	165933.526991	57.762676
2554.207585	165714.159238	57.767681
2553.483128	165487.834797	57.772685
2552.990241	165260.483223	57.777690
2552.300588	165058.061002	57.782695
2551.829639	164751.631970	57.787700
2550.805010	164526.060310	57.792705
2550.426610	164309.911260	57.797709
2549.754281	164069.333532	57.802714
2548.913267	163847.576879	57.807719
2548.467440	163622.440337	57.812724
2547.776637	163397.941603	57.817729
2546.888932	163175.357242	57.822733
2546.304315	162941.969576	57.827738
2545.733674	162725.720482	57.832743
2545.078085	162500.649538	57.837748
2544.515664	162276.353522	57.842753
2543.852411	162045.323545	57.847757
2543.220922	161813.272868	57.852762
2542.438257	161588.596460	57.857767
2541.808841	161358.442805	57.862772
2541.166185	161140.193074	57.867777
2540.202060	160909.764785	57.872781
2539.538601	160677.205249	57.877786
2539.005756	160459.641533	57.882791
2538.298829	160236.436415	57.887796
2538.002700	160004.357030	57.892801
2537.091989	159785.357123	57.897805
2536.345833	159543.740628	57.902810
2535.272014	159323.218393	57.907815
2535.078983	159105.126026	57.912820
2534.525745	158881.447423	57.917825
2533.959376	158669.506575	57.922829
2533.401340	158428.617997	57.927834
2532.823769	158212.308393	57.932839
2532.092449	157981.544486	57.937844
2531.639449	157747.305529	57.942849
2530.986063	157514.015228	57.947853
2530.032802	157277.316183	57.952858
2529.256131	157055.642454	57.957863
2528.833358	156813.930017	57.962868
2528.117271	156583.363690	57.967873
2527.260533	156358.694292	57.972877
2526.745346	156118.247194	57.977882
2525.870123	155916.580052	57.982887
2525.682945	155680.240912	57.987892
2524.860983	155438.703126	57.992897
2524.009012	155204.341314	57.997901
2523.236598	154979.426088	58.002906
2522.357246	154750.779345	58.007911
2522.141991	154519.321304	58.012916
2521.551026	154286.360878	58.017921
2520.452388	154062.228011	58.022925
2519.917246	153824.444283	58.027930
2519.258158	153613.095936	58.032935
2518.736168	153377.372515	58.037940
2517.843385	153147.785438	58.042945
2517.064513	152921.423194	58.047949
2516.837200	152693.818364	58.052954
2516.079551	152466.705896	58.057959
2515.483735	152235.501883	58.062964
2514.442526	152007.954489	58.067969
2513.697743	151789.627697	58.072973
2513.330098	151549.888912	58.077978
2512.336876	151334.426240	58.082983
2512.096642	151107.584264	58.087988
2511.290000	150881.926715	58.092993
2510.491557	150663.946354	58.097997
2510.097880	150430.396993	58.103002
2509.197888	150215.613232	58.108007
2508.433019	149980.689693	58.113012
2508.029212	149741.783286	58.118017
2507.017161	149535.461083	58.123021
2506.757867	149301.110508	58.128026
2505.980659	149085.539461	58.133031
2505.548387	148856.506693	58.138036
2504.681344	148626.387913	58.143041
2503.791032	148403.912741	58.148045
2503.323306	148173.365332	58.153050
2502.537199	147945.577083	58.158055
2501.835049	147724.309575	58.163060
2501.416787	147498.563183	58.168065
2500.763553	147284.179201	58.173069
2500.257093	147057.725503	58.178074
2499.257360	146832.851227	58.183079
2498.704274	146606.115836	58.188084
2498.009693	146384.093921	58.193089
2497.346987	146163.377473	58.198093
2496.937399	145925.148539	58.203098
2495.806455	145702.006006	58.208103
2495.538652	145476.212027	58.213108
2494.934421	145252.925646	58.218113
2493.908198	145030.597300	58.223117
2493.413806	144804.119721	58.228122
2492.862300	144569.392801	58.233127
2491.828614	144347.731297	58.238132
2491.416828	144124.168313	58.243137
2490.560862	143888.745035	58.248141
2490.329002	143666.897741	58.253146
2489.412984	143440.242766	58.258151
2488.812387	143215.902989	58.263156
2488.222266	142989.504630	58.268161
2487.325375	142777.210509	58.273165
2487.112615	142547.782135	58.278170
2486.186756	142317.248659	58.283175
2485.599838	142083.511919	58.288180
2484.913055	141866.133516	58.293185
2484.300890	141634.881997	58.298189
2483.829440	141400.712855	58.303194
2482.921751	141179.727610	58.308199
2482.236615	140948.581810	58.313204
2481.582051	140726.987951	58.318209
2481.116434	140509.736645	58.323213
2480.285495	140261.631192	58.328218
2479.973701	140039.174849	58.333223
2479.332172	139813.545150	58.338228
2478.269662	139587.424829	58.343233
2477.444090	139357.584030	58.348237
2477.365579	139120.625844	58.353242
2476.449521	138902.364867	58.358247
2475.682102	138668.543351	58.363252
2475.223284	138425.971692	58.368257
2474.254383	138203.696658	58.373261
2473.503611	137970.411594	58.378266
2473.083548	137752.614020	58.383271
2472.371449	137519.745628	58.388276
2471.830719	137292.098942	58.393281
2470.745589	137060.195338	58.398285
2470.529167	136834.508094	58.403290
2469.488196	136614.797319	58.408295
2468.844029	136378.204777	58.413300
2468.111492	136159.401336	58.418305
2467.233936	135940.038129	58.423309
2467.207622	135702.476509	58.428314
2466.579428	135489.403749	58.433319
2466.012336	135257.190903	58.438324
2465.445253	135018.691568	58.443329
2464.606620	134800.639243	58.448333
2463.852689	134556.558325	58.453338
2463.304503	134335.262170	58.458343
2462.725772	134098.118815	58.463348
2461.894715	133875.524473	58.468353
2460.900407	133639.212964	58.473357
2460.174755	133414.458651	58.478362
2459.832425	133190.686966	58.483367
2459.360954	132948.581941	58.488372
2458.657528	132720.920596	58.493377
2457.983813	132504.104377	58.498381
2457.119033	132263.629924	58.503386
2456.522413	132044.861491	58.508391
2455.520613	131809.938138	58.513396
2455.274326	131581.248049	58.518401
2454.382988	131359.711728	58.523405
2453.705517	131118.505958	58.528410
2452.941539	130901.068481	58.533415
2452.350376	130673.443852	58.538420
2452.176970	130455.458919	58.543425
2451.136886	130227.146966	58.548429
2450.896540	129987.596286	58.553434
2449.958571	129769.623571	58.558439
2449.478449	129542.587464	58.563444
2448.780176	129306.595356	58.568449
2448.050000	129064.983732	58.573453
2447.333344	128831.132339	58.578458
2446.672511	128608.717525	58.583463
2446.123696	128379.110811	58.588468
2445.240275	128138.166574	58.593473
2444.639501	127917.017849	58.598477
2444.129369	127680.273097	58.603482
2443.527981	127461.947606	58.608487
2442.762530	127224.269322	58.613492
2442.013960	126989.257436	58.618497
2441.351268	126759.047245	58.623501
2440.849835	126523.581064	58.628506
2440.079193	126293.798292	58.633511
2439.405228	126065.627682	58.638516
2438.770770	125835.331888	58.643521
2437.547188	125614.808433	58.648525
2437.134465	125372.340711	58.653530
2436.675735	125151.267976	58.658535
2436.035941	124922.809448	58.663540
2435.560685	124694.783925	58.668545
2434.588839	124463.092871	58.673549
2434.091490	124229.652333	58.678554
2433.293908	124003.118719	58.683559
2432.608023	123773.000995	58.688564
2432.002514	123550.986837	58.693569
2431.045722	123325.398470	58.698573
2430.412379	123086.592603	58.703578
2429.934302	122872.297116	58.708583
2429.070432	122648.998090	58.713588
2428.841802	122416.902115	58.718593
2428.116606	122199.337045	58.723597
2427.687628	121958.350239	58.728602
2426.832416	121726.981814	58.733607
2426.238360	121498.964241	58.738612
2425.534800	121274.368899	58.743617
2424.548148	121046.430169	58.748621
2424.375532	120816.066151	58.753626
2423.594681	120589.393855	58.758631
2422.715846	120345.560046	58.763636
2422.221186	120121.944464	58.768641
2421.383587	119896.582223	58.773645
2421.129737	119658.191493	58.778650
2420.521427	119426.727952	58.783655
2419.574209	119199.967082	58.788660
2419.009589	118968.195966	58.793665
2417.914001	118736.015948	58.798669
2417.392474	118505.467303	58.803674
2417.052475	118270.899045	58.808679
2416.405028	118042.939058	58.813684
2415.805767	117809.730101	58.818689
2414.912515	117579.058203	58.823693
2414.462075	117341.202328	58.828698
2413.509793	117122.198349	58.833703
2412.759545	116893.198405	58.838708
2412.408953	116654.006393	58.843713
2411.595048	116427.369302	58.848717
2411.147191	116195.661677	58.853722
2410.253738	115963.474578	58.858727
2409.678227	115733.860636	58.863732
2409.088991	115499.953818	58.868737
2408.607310	115266.819151	58.873741
2408.205096	115024.946653	58.878746
2406.887049	114799.406820	58.883751
2406.436953	114559.209299	58.888756
2406.001338	114317.774095	58.893761
2404.871611	114082.950519	58.898765
2404.416290	113860.722310	58.903770
2403.847011	113636.146761	58.908775
2403.183152	113398.056901	58.913780
2402.658779	113157.516390	58.918785
2401.942267	112930.216024	58.923789
2401.475918	112687.709705	58.928794
2400.741187	112459.172573	58.933799
2399.921372	112219.049675	58.938804
2399.650749	111972.311556	58.943809
2398.831387	111740.297560	58.948813
2398.349525	111491.839759	58.953818
2397.459995	111255.760753	58.958823
2396.807683	111013.414451	58.963828
2396.227410	110779.220184	58.968833
2395.240828	110550.340736	58.973837
2394.834599	110304.611652	58.978842
2394.076216	110071.213860	58.983847
2393.422552	109828.441536	58.988852
2392.727266	109587.899238	58.993857
2392.116294	109356.350524	58.998861
2391.557843	109107.954255	59.003866
2391.030679	108867.354297	59.008871
2390.211069	108628.922492	59.013876
2389.480195	108390.275891	59.018881
2388.897165	108157.820354	59.023885
2388.303144	107911.288424	59.028890
2387.336599	107675.370293	59.033895
2386.825461	107438.747722	59.038900
2386.444757	107192.036992	59.043905
2385.682299	106954.875245	59.048909
2384.928856	106710.963271	59.053914
2384.047074	106477.746373	59.058919
2383.684408	106233.828023	59.063924
2383.253798	105986.236560	59.068929
2382.110944	105752.230576	59.073933
2381.784103	105497.946632	59.078938
2380.856867	105272.806448	59.083943
2380.071414	105036.682428	59.088948
2379.319699	104796.488545	59.093953
2378.609180	104551.582951	59.098957
2378.140390	104316.722810	59.103962
2377.359282	104082.828101	59.108967
2376.841070	103848.855942	59.113972
2376.215903	103606.985464	59.118977
2375.258654	103367.187558	59.123981
2375.051107	103125.357288	59.128986
2374.180606	102895.872250	59.133991
2373.452255	102657.973838	59.138996
2373.428761	102416.984426	59.144001
2372.458267	102174.092248	59.149005
2371.365019	101922.797526	59.154010
2370.982209	101694.433170	59.159015
2370.085210	101454.353404	59.164020
2369.916230	101211.807194	59.169025
2368.747361	100977.300698	59.174029
2368.234839	100733.526205	59.179034
2367.373238	100498.170194	59.184039
2366.775522	100259.323957	59.189044
2365.986100	100023.111310	59.194049
2365.216018	99788.331564	59.199053
2364.753374	99554.298337	59.204058
2364.081597	99319.831257	59.209063
2363.383425	99086.487112	59.214068
2362.978866	98848.487458	59.219073
2362.446980	98612.781201	59.224077
2362.010656	98375.888788	59.229082
2361.299391	98136.067677	59.234087
2360.365194	97891.026358	59.239092
2359.806900	97644.564395	59.244097
2359.098130	97408.511670	59.249101
2358.702380	97167.229955	59.254106
2357.687327	96931.864978	59.259111
2356.962792	96682.725221	59.264116
2356.487071	96439.726099	59.269121
2355.529614	96214.944647	59.274125
2354.953900	95962.941542	59.279130
2354.488278	95727.229215	59.284135
2353.493666	95492.307194	59.289140
2353.244572	95250.198143	59.294145
2352.365010	95015.288212	59.299149
2351.805186	94769.961196	59.304154
2351.097406	94530.615196	59.309159
2350.452580	94300.603026	59.314164
2350.091794	94053.432215	59.319169
2349.199293	93811.206055	59.324173
2348.832966	93574.321019	59.329178
2347.941747	93327.660879	59.334183
2347.296129	93086.341954	59.339188
2346.913560	92833.950162	59.344193
2346.050330	92600.083931	59.349197
2345.389544	92349.162187	59.354202
2344.503877	92113.573519	59.359207
2343.884903	91864.521235	59.364212
2343.419927	91626.664377	59.369217
2342.490330	91394.964617	59.374221
2341.997552	91141.563339	59.379226
2341.456706	90893.910919	59.384231
2340.665871	90665.785651	59.389236
2340.243056	90417.993057	59.394241
2339.331627	90174.484487	59.399245
2338.855721	89930.028236	59.404250
2338.150896	89681.958984	59.409255
2337.637924	89442.262975	59.414260
2336.654489	89198.802047	59.419265
2336.146443	88952.282249	59.424269
2335.178615	88707.765534	59.429274
2334.919224	88465.053893	59.434279
2333.651202	88220.875566	59.439284
2333.336347	87975.692949	59.444289
2332.513783	87738.689510	59.449293
2332.300817	87495.239612	59.454298
2331.265041	87262.827109	59.459303
2330.662855	87017.935488	59.464308
2330.488532	86762.334798	59.469313
2329.570932	86524.548318	59.474317
2329.059160	86278.718876	59.479322
2328.331057	86035.310124	59.484327
2327.487162	85788.689511	59.489332
2326.962359	85538.800859	59.494337
2326.094884	85304.728354	59.499341
2325.545641	85046.120469	59.504346
2324.829320	84809.348042	59.509351
2323.689802	84561.843994	59.514356
2323.255274	84314.998010	59.519361
2322.809775	84081.645361	59.524365
2321.900349	83838.474273	59.529370
2321.380781	83596.999926	59.534375
2320.831061	83354.202037	59.539380
2320.033426	83110.299008	59.544385
2319.203395	82869.731557	59.549389
2318.744352	82623.080339	59.554394
2317.906108	82388.078342	59.559399
2317.109997	82145.035570	59.564404
2316.722461	81908.528708	59.569409
2315.703791	81667.358462	59.574413
2315.695176	81433.420782	59.579418
2314.523807	81191.703490	59.584423
2314.110009	80963.038686	59.589428
2313.510719	80716.432155	59.594433
2312.928648	80478.844218	59.599437
2312.248363	80230.862013	59.604442
2311.450553	79985.449062	59.609447
2310.664179	79744.657148	59.614452
2310.412319	79497.560026	59.619457
2309.570836	79256.915607	59.624461
2309.016115	79010.518733	59.629466
2308.493717	78776.578371	59.634471
2307.570671	78521.018971	59.639476
2307.096065	78278.610448	59.644481
2306.207821	78044.299181	59.649485
2305.744604	77785.273103	59.654490
2305.000838	77550.817820	59.659495
2304.020075	77315.065779	59.664500
2303.754126	77064.280495	59.669505
2302.617506	76825.897463	59.674509
2302.001930	76580.889071	59.679514
2301.310126	76349.848310	59.684519
2300.636884	76105.108239	59.689524
2299.984205	75871.836339	59.694529
2299.320286	75641.812989	59.699533
2299.212016	75391.561860	59.704538
2298.565764	75159.849454	59.709543
2297.833457	74908.740201	59.714548
2297.025632	74660.503492	59.719553
2296.349154	74417.577349	59.724557
2295.666584	74173.235915	59.729562
2294.831030	73929.434891	59.734567
2294.148598	73688.659911	59.739572
2293.767121	73442.505659	59.744577
2292.878023	73204.651880	59.749581
2292.325196	72968.698854	59.754586
2291.702051	72725.233550	59.759591
2290.670402	72487.182844	59.764596
2290.226885	72242.928379	59.769601
2289.400106	72008.461865	59.774605
2288.768864	71759.745271	59.779610
2288.075504	71539.979063	59.784615
2287.499961	71289.606129	59.789620
2286.793695	71046.168201	59.794625
2285.862004	70815.913278	59.799629
2285.278298	70579.182647	59.804634
2284.859128	70340.066007	59.809639
2284.366356	70102.180133	59.814644
2283.604294	69861.223373	59.819649
2283.169707	69626.678507	59.824653
2282.289835	69387.519808	59.829658
2281.811624	69142.631337	59.834663
2281.036538	68904.519685	59.839668
2280.606023	68658.812604	59.844673
2279.575793	68430.685060	59.849677
2278.921847	68190.149695	59.854682
2278.265844	67950.859015	59.859687
2277.726204	67710.723113	59.864692
2277.274443	67472.792956	59.869697
2276.539472	67239.749370	59.874701
2275.511922	66986.317256	59.879706
2275.164179	66758.734365	59.884711
2274.071707	66507.193455	59.889716
2273.618783	66269.173727	59.894721
2272.843504	66048.367430	59.899725
2272.385136	65802.314513	59.904730
2271.975532	65553.185549	59.909735
2270.919725	65321.333693	59.914740
2270.271115	65084.708490	59.919745
2269.320917	64848.260689	59.924750
2268.932980	64602.040946	59.929754
2268.379978	64373.461196	59.934759
2267.630191	64137.275325	59.939764
2266.850096	63900.653910	59.944769
2265.881398	63664.714396	59.949774
2265.476631	63420.209558	59.954778
2264.858089	63196.352743	59.959783
2264.238498	62959.679535	59.964788
2264.089109	62719.220999	59.969793
2263.340695	62493.537785	59.974798
2262.754876	62248.316883	59.979802
2262.035093	62004.329753	59.984807
2261.407100	61762.246521	59.989812
2260.452836	61512.661442	59.994817
2259.501705	61278.391798	59.999822
2258.857181	61040.078157	60.004826
2258.380706	60807.787264	60.009831
2257.622395	60575.233709	60.014836
2257.160829	60337.906588	60.019841
2256.483160	60107.232708	60.024846
2255.967440	59863.000315	60.029850
2255.040225	59628.896185	60.034855
2254.615339	59389.891207	60.039860
2253.986971	59138.427831	60.044865
2253.089269	58914.764184	60.049870
2252.387080	58672.419125	60.054874
2251.913153	58432.560546	60.059879
2251.061740	58197.680506	60.064884
2250.444029	57957.043730	60.069889
2249.493781	57727.214766	60.074894
2249.140582	57486.136991	60.079898
2248.111092	57263.625040	60.084903
2247.583860	57026.882148	60.089908
2247.066619	56789.415920	60.094913
2246.201769	56554.910125	60.099918
2245.410323	56329.475738	60.104922
2244.831789	56105.963048	60.109927
2243.955707	55874.094519	60.114932
2243.315387	55635.206854	60.119937
2242.578837	55409.322460	60.124942
2242.112005	55176.957902	60.129946
2241.442482	54960.410579	60.134951
2240.807359	54734.347511	60.139956
2240.742555	54491.734628	60.144961
2239.499878	54267.242072	60.149966
2238.854465	54032.357089	60.154970
2238.530021	53802.278488	60.159975
2237.563725	53573.753912	60.164980
2237.088712	53342.549988	60.169985
2235.964246	53115.034056	60.174990
2235.269496	52875.384177	60.179994
2234.482932	52667.112978	60.184999
2233.851443	52446.260771	60.190004
2233.422177	52212.168719	60.195009
2232.508719	51986.968635	60.200014
2232.010181	51763.259109	60.205018
2231.564824	51543.540128	60.210023
2230.500593	51327.573283	60.215028
2230.070258	51087.610886	60.220033
2229.507151	50861.533979	60.225038
2228.913113	50637.853568	60.230042
2228.226346	50421.261891	60.235047
2227.328341	50202.156293	60.240052
2226.889867	49970.163970	60.245057
2226.297189	49751.964574	60.250062
2225.264766	49525.466428	60.255066
2224.990543	49303.308479	60.260071
2223.923386	49076.217278	60.265076
2223.534605	48848.502523	60.270081
2222.879409	48636.119209	60.275086
2222.263775	48403.884285	60.280090
2221.685898	48182.092177	60.285095
2220.803951	47952.521587	60.290100
2220.307285	47721.061245	60.295105
2219.703025	47507.946265	60.300110
2218.845543	47270.769605	60.305114
2218.274998	47042.284380	60.310119
2217.523585	46823.541907	60.315124
2217.151714	46600.939779	60.320129
2216.222184	46386.529751	60.325134
2215.385578	46146.578145	60.330138
2214.801859	45935.579185	60.335143
2213.902677	45718.433264	60.340148
2213.430127	45497.461550	60.345153
2212.966683	45269.586456	60.350158
2212.213380	45050.635426	60.355162
2211.787791	44827.415875	60.360167
2210.652486	44601.073029	60.365172
2210.105954	44379.491423	60.370177
2209.432602	44164.062152	60.375182
2208.959931	43936.420953	60.380186
2207.903242	43725.027119	60.385191
2207.417591	43503.911890	60.390196
2206.722691	43289.847289	60.395201
2205.698209	43071.021049	60.400206
2205.311574	42848.946515	60.405210
2204.548324	42631.374679	60.410215
2203.967509	42423.589654	60.415220
2203.619673	42206.618196	60.420225
2202.384428	41993.430114	60.425230
2201.857145	41775.945442	60.430234
2201.388105	41562.274295	60.435239
2200.627217	41346.805352	60.440244
2199.959595	41131.558309	60.445249
2199.487690	40924.121892	60.450254
2198.810851	40702.187397	60.455258
2197.887540	40483.608727	60.460263
2197.186834	40272.804592	60.465268
2196.920001	40055.878988	60.470273
2196.168085	39844.400512	60.475278
2195.170036	39627.008225	60.480282
2194.226232	39412.602815	60.485287
2193.380239	39215.323333	60.490292
2193.488559	38992.948099	60.495297
2192.456058	38796.485597	60.500302
2191.803720	38581.957435	60.505306
2190.958468	38371.689756	60.510311
2190.368551	38164.667538	60.515316
2189.786336	37950.362275	60.520321
2188.713506	37754.318158	60.525326
2187.810940	37543.889614	60.530330
2187.564010	37343.817881	60.535335
2186.944581	37143.970426	60.540340
2186.275129	36929.756719	60.545345
2185.489916	36733.154003	60.550350
2184.978691	36530.301229	60.555354
2184.643840	36328.208494	60.560359
2183.263491	36124.191301	60.565364
2182.764153	35921.503611	60.570369
2181.913683	35724.260740	60.575374
2181.184068	35524.238162	60.580378
2180.675203	35328.486800	60.585383
2179.957000	35139.989261	60.590388
2178.855398	34934.462909	60.595393
2178.417983	34753.190827	60.600398
2178.019253	34555.257827	60.605402
2177.536291	34364.112833	60.610407
2176.564640	34172.100872	60.615412
2176.078781	33972.208297	60.620417
2175.013534	33786.164367	60.625422
2174.351485	33594.034079	60.630426
2173.895966	33406.413658	60.635431
2172.806809	33220.942452	60.640436
2172.195344	33032.330082	60.645441
2171.374017	32854.290747	60.650446
2170.728009	32665.438332	60.655450
2169.855753	32488.825373	60.660455
2168.891737	32319.153610	60.665460
2168.257576	32139.293905	60.670465
2167.209338	31978.300386	60.675470
2166.329183	31816.202472	60.680474
2165.715813	31648.687946	60.685479
2164.333388	31500.747751	60.690484
2163.831243	31342.522875	60.695489
2163.082406	31193.723259	60.700494
2162.316110	31045.090512	60.705498
2161.221105	30911.838598	60.710503
2160.077722	30781.787295	60.715508
2159.574588	30632.602978	60.720513
2159.304844	30502.282536	60.725518
2158.092739	30383.106898	60.730522
2157.667471	30247.420317	60.735527
2156.574148	30114.814534	60.740532
2155.809711	29974.070950	60.745537
2155.032410	29870.981308	60.750542
2154.269656	29746.482214	60.755546
2153.812461	29626.640868	60.760551
2152.690135	29522.380496	60.765556
2152.435608	29400.332982	60.770561
2151.809046	29284.847035	60.775566
2151.163799	29175.142822	60.780570
2150.612525	29057.644710	60.785575
2149.756960	28942.357096	60.790580
2149.156483	28816.166175	60.795585
2148.401185	28717.360368	60.800590
2148.174095	28600.705185	60.805594
2147.588686	28486.123651	60.810599
2146.749441	28376.814229	60.815604
2146.278033	28246.005011	60.820609
2145.600623	28133.123133	60.825614
2144.952876	28022.250073	60.830618
2144.347561	27902.176319	60.835623
2143.507271	27788.224688	60.840628
2142.911857	27661.921843	60.845633
2142.382516	27558.199249	60.850638
2142.074099	27440.225607	60.855642
2141.286572	27313.955955	60.860647
2140.419614	27196.001628	60.865652
2140.041764	27065.564638	60.870657
2139.376650	26947.253083	60.875662
2138.419448	26835.235048	60.880666
2137.770468	26710.016028	60.885671
2137.110092	26605.199509	60.890676
2136.588725	26480.046536	60.895681
2135.872303	26378.789197	60.900686
2135.359737	26267.849035	60.905690
2135.037412	26140.936557	60.910695
2134.295032	26022.068246	60.915700
2133.680698	25893.836059	60.920705
2132.822363	25776.670287	60.925710
2132.085494	25662.616130	60.930714
2131.658111	25542.180983	60.935719
2130.975492	25419.795356	60.940724
2130.241223	25296.811502	60.945729
2129.525158	25177.546405	60.950734
2128.941689	25061.421084	60.955738
2128.657049	24943.157057	60.960743
2127.530588	24832.366851	60.965748
2127.200958	24699.662060	60.970753
2126.278844	24582.193687	60.975758
2125.584559	24462.509507	60.980762
2124.905788	24346.863330	60.985767
2124.444738	24229.916690	60.990772
2123.726169	24096.349874	60.995777
2122.997078	23996.257052	61.000782
2122.321311	23871.701702	61.005786
2121.811431	23752.403441	61.010791
2121.035792	23637.113401	61.015796
2120.478410	23509.064188	61.020801
2119.977907	23393.094956	61.025806
2119.243169	23274.680929	61.030810
2118.694424	23153.584905	61.035815
2117.734562	23040.213408	61.040820
2117.538941	22910.405876	61.045825
2116.875790	22789.939615	61.050830
2115.873198	22672.493331	61.055834
2115.497497	22542.686577	61.060839
2114.670594	22420.650036	61.065844
2113.789073	22302.523966	61.070849
2113.371823	22179.360615	61.075854
2112.672204	22067.248199	61.080858
2112.036019	21942.888013	61.085863
2111.402381	21824.686684	61.090868
2110.832672	21704.122237	61.095873
2109.960297	21582.820283	61.100878
2109.476728	21466.920062	61.105882
2108.797841	21346.585699	61.110887
2107.732390	21226.233847	61.115892
2107.493990	21103.079697	61.120897
2106.765979	20992.113252	61.125902
2106.066824	20868.094447	61.130906
2105.444734	20738.077070	61.135911
2104.349783	20632.430719	61.140916
2103.974567	20496.319400	61.145921
2103.085235	20387.644107	61.150926
2102.571548	20271.743226	61.155930
2102.000016	20151.503583	61.160935
2101.288030	20045.092182	61.165940
2100.342605	19927.575901	61.170945
2099.734973	19818.874440	61.175950
2099.187662	19703.256654	61.180954
2098.656768	19580.914410	61.185959
2097.740308	19476.483880	61.190964
2097.468430	19353.406353	61.195969
2096.795758	19240.656048	61.200974
2096.043497	19124.606879	61.205978
2095.462951	18989.917663	61.210983
2094.607756	18887.180701	61.215988
2094.056098	18767.549298	61.220993
2093.782063	18655.263364	61.225998
2092.641531	18534.368130	61.231002
2091.888758	18419.761088	61.236007
2091.310709	18308.224165	61.241012
2090.662347	18190.603908	61.246017
2090.047485	18079.168012	61.251022
2089.319215	17966.878193	61.256026
2088.663289	17843.214316	61.261031
2087.865544	17744.227107	61.266036
2087.085867	17628.509961	61.271041
2086.472458	17516.152271	61.276046
2085.858090	17404.001579	61.281050
2085.371957	17288.388388	61.286055
2084.447190	17180.427378	61.291060
2084.081480	17070.062732	61.296065
2083.588893	16957.983551	61.301070
2082.653764	16843.846467	61.306074
2082.121184	16719.171023	61.311079
2081.145040	16624.650969	61.316084
2080.917864	16513.993589	61.321089
2079.989777	16389.843755	61.326094
2079.325107	16281.384375	61.331098
2078.664260	16168.391768	61.336103
2077.741763	16065.202031	61.341108
2077.088280	15944.192224	61.346113
2076.444626	15850.836933	61.351118
2075.622167	15736.238836	61.356122
2075.112798	15630.248292	61.361127
2074.353608	15525.530824	61.366132
2073.909367	15418.464845	61.371137
2073.286300	15313.337297	61.376142
2072.613687	15216.971178	61.381146
2071.854358	15117.493256	61.386151
2070.548127	15012.737336	61.391156
2070.638286	14901.765372	61.396161
2069.886164	14795.141105	61.401166
2068.974070	14693.805782	61.406170
2068.594080	14584.510953	61.411175
2067.360111	14486.677835	61.416180
2066.619419	14389.664134	61.421185
2066.231137	14296.073512	61.426190
2065.418774	14188.177533	61.431194
2064.754356	14094.474018	61.436199
2064.100309	14003.203512	61.441204
2063.440604	13896.114246	61.446209
2062.660940	13804.385629	61.451214
2061.895649	13713.409941	61.456218
2061.371260	13613.375794	61.461223
2060.614576	13516.877317	61.466228
2059.782735	13433.546648	61.471233
2059.339709	13345.368152	61.476238
2058.386341	13251.012383	61.481242
2057.776103	13159.722293	61.486247
2057.040637	13081.151346	61.491252
2056.430718	12988.762870	61.496257
2055.784592	12905.574982	61.501262
2054.971072	12813.299120	61.506266
2054.377156	12728.580716	61.511271
2053.555072	12651.171103	61.516276
2053.094361	12569.806295	61.521281
2052.379883	12481.368591	61.526286
2051.557777	12387.749191	61.531290
2051.243501	12303.452981	61.536295
2050.467913	12225.055474	61.541300
2049.785430	12130.072779	61.546305
2049.033930	12046.468039	61.551310
2048.369605	11960.889145	61.556314
2047.900586	11872.752381	61.561319
2046.729957	11788.086550	61.566324
2046.262181	11701.205277	61.571329
2045.671130	11624.719435	61.576334
2044.978449	11543.351951	61.581338
2044.338427	11461.637824	61.586343
2043.359737	11382.053011	61.591348
2043.086207	11300.478462	61.596353
2042.218703	11216.942071	61.601358
2041.179328	11144.890095	61.606362
2040.736211	11061.333563	61.611367
2040.128177	10986.851970	61.616372
2039.500120	10910.815115	61.621377
2038.957249	10839.560274	61.626382
2038.095936	10766.699675	61.631386
2037.496796	10686.892767	61.636391
2036.785698	10610.982250	61.641396
2036.348077	10534.757669	61.646401
2035.570045	10458.325933	61.651406
2034.815337	10384.712891	61.656410
2034.299161	10308.065186	61.661415
2033.217781	10226.580061	61.666420
2032.766634	10153.983186	61.671425
2032.361612	10089.680491	61.676430
2031.274772	10010.237430	61.681434
2030.861924	9933.409137	61.686439
2029.967076	9861.408791	61.691444
2029.521856	9789.855015	61.696449
2028.960514	9712.254515	61.701454
2028.099194	9648.262631	61.706458
2027.812643	9573.964209	61.711463
2026.907535	9503.783480	61.716468
2026.645014	9416.845064	61.721473
2025.676273	9353.659687	61.726478
2024.740292	9282.749552	61.731482
2024.429817	9205.311852	61.736487
2023.683875	9142.908198	61.741492
2023.167579	9060.259581	61.746497
2022.171068	8990.409374	61.751502
2021.506030	8912.380928	61.756506
2020.946088	8834.589461	61.761511
2020.141558	8779.062555	61.766516
2019.740959	8698.114733	61.771521
2018.620893	8627.276757	61.776526
2017.879042	8559.349071	61.781530
2017.790221	8485.668418	61.786535
2017.005887	8419.581612	61.791540
2016.130964	8352.556837	61.796545
2015.321898	8288.939565	61.801550
2014.855118	8230.748530	61.806554
2014.206323	8156.932741	61.811559
2013.298327	8098.775568	61.816564
2012.929572	8024.017795	61.821569
2012.292022	7958.818953	61.826574
2011.397652	7894.417333	61.831578
2011.045781	7827.229840	61.836583
2009.937501	7755.529477	61.841588
2009.557423	7686.062428	61.846593
2008.787234	7624.883458	61.851598
2007.879722	7552.293093	61.856602
2007.643115	7487.438156	61.861607
2006.970191	7428.353256	61.866612
2006.495648	7355.708532	61.871617
2005.764711	7295.113190	61.876622
2004.815474	7239.501373	61.881626
2004.586384	7155.139337	61.886631
2003.566592	7097.642799	61.891636
2002.626682	7029.174869	61.896641
2002.337364	6961.040223	61.901646
2001.334813	6901.209040	61.906650
2001.007063	6834.408723	61.911655
2000.057824	6768.848434	61.916660
1999.909837	6714.185020	61.921665
1998.912065	6642.138001	61.926670
1998.266206	6577.752712	61.931674
1997.738369	6505.873143	61.936679
1997.053948	6448.029277	61.941684
1996.491238	6384.601893	61.946689
1995.750303	6321.733164	61.951694
1995.239943	6251.526733	61.956698
1994.455135	6184.489509	61.961703
1993.811048	6122.455810	61.966708
1993.253360	6057.694344	61.971713
1992.552203	5987.729270	61.976718
1991.614046	5925.479612	61.981722
1991.131650	5858.570181	61.986727
1990.320462	5799.028585	61.991732
1989.835503	5726.632468	61.996737
1988.937211	5657.778529	62.001742
1988.185882	5593.842563	62.006746
1987.805566	5536.719102	62.011751
1986.977140	5475.817727	62.016756
1986.348229	5410.854264	62.021761
1986.001785	5349.308188	62.026766
1985.031820	5282.806096	62.031770
1984.552708	5223.464140	62.036775
1983.690077	5158.152389	62.041780
1983.450150	5096.527353	62.046785
1982.588473	5033.533389	62.051790
1981.729377	4969.136873	62.056794
1981.430320	4908.333638	62.061799
1980.458431	4851.051174	62.066804
1979.510439	4772.574658	62.071809
1978.816364	4716.998841	62.076814
1977.990064	4660.466186	62.081818
1977.694817	4597.653912	62.086823
1976.918963	4544.095122	62.091828
1976.170387	4472.967155	62.096833
1975.623116	4426.923023	62.101838
1974.908111	4356.205160	62.106842
1974.768800	4305.326442	62.111847
1973.521053	4254.108036	62.116852
1972.795885	4191.305009	62.121857
1972.366336	4132.578708	62.126862
1971.928532	4074.485707	62.131866
1971.268401	4012.551739	62.136871
1970.705021	3961.566433	62.141876
1970.034750	3898.751205	62.146881
1969.336047	3833.386959	62.151886
1968.654745	3775.420550	62.156890
1968.137501	3707.684060	62.161895
1967.368290	3646.644393	62.166900
1966.362237	3592.522263	62.171905
1965.480239	3524.855561	62.176910
1964.800866	3472.748354	62.181914
1964.487692	3413.394433	62.186919
1963.628510	3367.437045	62.191924
1963.066886	3296.337136	62.196929
1962.536574	3245.309630	62.201934
1962.055769	3191.162381	62.206938
1961.643544	3119.996231	62.211943
1960.480103	3058.744774	62.216948
1959.862542	3003.660923	62.221953
1959.087816	2952.301782	62.226958
1958.329692	2900.172832	62.231962
1957.603739	2835.561835	62.236967
1956.950203	2784.373318	62.241972
1956.123600	2731.008214	62.246977
1955.650905	2679.610756	62.251982
1955.185710	2621.226588	62.256986
1954.251532	2558.352526	62.261991
1953.714301	2507.237994	62.266996
1953.481153	2444.812263	62.272001
1952.545283	2395.146229	62.277006
1952.031875	2339.198210	62.282010
1951.246559	2273.327868	62.287015
1950.310656	2236.236028	62.292020
1949.817407	2166.010045	62.297025
1949.318122	2118.058684	62.302030
1948.872078	2061.945676	62.307034
1948.217027	1991.243090	62.312039
1947.237106	1948.999176	62.317044
1946.735829	1886.580539	62.322049
1946.229228	1829.729662	62.327054
1945.418248	1776.545361	62.332058
1944.821261	1713.522040	62.337063
1943.975022	1664.397850	62.342068
1943.455614	1605.719584	62.347073
1942.692346	1553.395956	62.352078
1941.492434	1502.654318	62.357082
1941.408960	1440.364458	62.362087
1940.518155	1388.172071	62.367092
1939.615121	1332.016923	62.372097
1938.745416	1282.247184	62.377102
1938.228858	1237.406806	62.382106
1937.756360	1186.434869	62.387111
1936.847670	1138.253652	62.392116
1936.281683	1082.694934	62.397121
1935.585937	1037.500385	62.402126
1934.919370	991.848720	62.407130
1934.342556	937.706134	62.412135
1933.506277	891.715844	62.417140
1933.114021	849.184693	62.422145
1932.465710	795.891411	62.427150
1931.930639	750.389951	62.432154
1931.250093	692.823597	62.437159
1930.494671	648.092349	62.442164
1929.744880	601.712332	62.447169
1929.360194	550.227971	62.452174
1928.226531	499.282194	62.457178
1927.718613	445.162044	62.462183
1926.888673	397.130065	62.467188
1926.040040	363.679173	62.472193
1925.954033	316.496062	62.477198
1925.036551	273.009156	62.482202
1924.362622	223.593601	62.487207
1923.609874	186.744432	62.492212
1923.035770	133.572691	62.497217
1922.443863	83.006003	62.502222
1921.764110	44.310782	62.507226
1920.918301	-0.244839	62.512231
1920.026557	-44.558060	62.517236
1918.623314	-81.245707	62.522241
1918.168515	-118.930675	62.527246
1917.409192	-142.016551	62.532250
1916.951956	-172.879041	62.537255
1915.961498	-193.190533	62.542260
1915.142586	-206.581160	62.547265
1914.044109	-205.055107	62.552270
1904.344520	30.720397	62.557274
1902.891268	91.906582	62.562279
1905.118333	112.932440	62.567284
1907.566357	120.400530	62.572289
1909.897100	118.794305	62.577294
1910.443025	122.692883	62.582298
1910.390003	104.909872	62.587303
1909.734665	91.797359	62.592308
1909.250001	75.035419	62.597313
1908.387414	61.014379	62.602318
1906.278562	63.224439	62.607322
1905.306791	60.324302	62.612327
1904.572043	66.340663	62.617332
1904.064848	69.373507	62.622337
1903.448180	64.570337	62.627342
1902.487093	68.006415	62.632346
1902.409259	60.955645	62.637351
1901.713149	60.937052	62.642356
1901.094338	63.145506	62.647361
1900.867750	58.417602	62.652366
1899.398288	61.114364	62.657370
1898.952718	60.150802	62.662375
1897.699907	63.270492	62.667380
1897.737467	63.829284	62.672385
1897.502828	73.181996	62.677390
1896.390046	67.840997	62.682394
1895.656465	57.161620	62.687399
1894.995374	60.990045	62.692404
1893.906031	66.400375	62.697409
1893.524143	67.068345	62.702414
1892.850270	77.157866	62.707418
1892.364476	74.691513	62.712423
1891.687501	72.619800	62.717428
1890.847294	73.584475	62.722433
1890.784235	71.647103	62.727438
1890.396285	76.513977	62.732442
1889.706156	70.645391	62.737447
1888.336254	69.486389	62.742452
1888.045301	74.842497	62.747457
1887.578234	77.140406	62.752462
1886.521328	81.594670	62.757466
1886.477928	77.364389	62.762471
1885.511647	80.091655	62.767476
1884.579989	81.600721	62.772481
1884.092605	74.089839	62.777486
1882.772952	82.466790	62.782490
1881.969499	75.927055	62.787495
1881.263118	82.248012	62.792500
1881.292420	87.816631	62.797505
1881.609587	78.301382	62.802510
1880.447895	77.907279	62.807514
1879.982306	73.004429	62.812519
1878.371058	79.689842	62.817524
1877.737416	81.405485	62.822529
1877.317870	81.721461	62.827534
1876.353760	83.751357	62.832538
1876.174133	73.526500	62.837543
1875.252674	83.412485	62.842548
1874.499011	85.207112	62.847553
1874.390171	80.805868	62.852558
1873.802533	81.563283	62.857562
1872.860525	75.129132	62.862567
1872.143986	75.044403	62.867572
1871.618784	80.543368	62.872577
1871.316343	73.372138	62.877582
1869.950373	82.760991	62.882586
1869.752084	83.956489	62.887591
1869.521503	85.978725	62.892596
1868.150026	85.621092	62.897601
1867.312759	74.841480	62.902606
1866.862192	89.096649	62.907610
1866.668638	86.247997	62.912615
1865.997734	84.530148	62.917620
1864.377925	92.554220	62.922625
1864.416175	82.059791	62.927630
1863.709383	87.884068	62.932634
1863.357520	87.531695	62.937639
1862.724464	87.834267	62.942644
1861.295578	80.236341	62.947649
1861.152360	87.333645	62.952654
1860.702599	91.026023	62.957658
1859.876149	82.037728	62.962663
1858.542206	90.536814	62.967668
1858.437574	88.522462	62.972673
1858.177243	85.052043	62.977678
1857.209566	88.932320	62.982682
1856.467629	86.845699	62.987687
1855.564935	81.606975	62.992692
1855.031453	79.753765	62.997697
1854.920589	82.813574	63.002702
1853.514874	83.946908	63.007706
1853.266014	76.850752	63.012711
1852.728687	79.587187	63.017716
1851.574701	91.604346	63.022721
1851.381086	84.507299	63.027726
1850.201845	89.832578	63.032730
1850.086210	81.389017	63.037735
1849.379272	81.917795	63.042740
1848.319232	83.422028	63.047745
1848.139419	81.653010	63.052750
1846.961693	92.218381	63.057754
1846.457419	74.890286	63.062759
1846.084192	78.863829	63.067764
1845.023414	85.895522	63.072769
1844.703665	83.798634	63.077774
1844.249267	89.597029	63.082778
1843.294503	81.548501	63.087783
1842.531818	77.903963	63.092788
1841.607917	82.444358	63.097793
1841.526251	82.501677	63.102798
1840.564352	84.040791	63.107802
1839.691616	83.526703	63.112807
1839.586066	77.928007	63.117812
1838.569933	81.716633	63.122817
1838.221984	84.896094	63.127822
1837.659485	84.011035	63.132826
1837.044864	84.657623	63.137831
1836.361363	87.871447	63.142836
1835.672352	92.566939	63.147841
1835.255311	81.777375	63.152846
1834.153018	88.752586	63.157850
1833.409845	81.848471	63.162855
1832.748695	83.073318	63.167860
1831.732633	85.578269	63.172865
1831.838580	74.924861	63.177870
1830.891848	81.061641	63.182874
1830.016929	79.571747	63.187879
1829.084470	85.334094	63.192884
1828.333766	85.508697	63.197889
1828.915229	81.310079	63.202894
1827.902364	75.888586	63.207898
1827.237299	83.084529	63.212903
1826.460626	85.149334	63.217908
1825.479361	86.207394	63.222913
1825.175902	85.724335	63.227918
1824.261844	93.628467	63.232922
1823.724295	86.248566	63.237927
1822.577172	83.218606	63.242932
1822.246214	85.065971	63.247937
1821.895021	81.977424	63.252942
1820.479666	87.589374	63.257946
1819.864488	76.700394	63.262951
1819.603841	84.431370	63.267956
1819.146944	85.393544	63.272961
1818.438546	79.620921	63.277966
1817.519199	79.992624	63.282970
1817.111243	81.122071	63.287975
1816.923788	79.127184	63.292980
1815.671436	89.493099	63.297985
1815.565589	73.133094	63.302990
1814.495110	82.087104	63.307994
1813.537647	85.920040	63.312999
1812.623933	90.293245	63.318004
1812.028815	85.904574	63.323009
1812.136677	82.946559	63.328014
1810.892323	86.877097	63.333018
1810.365144	84.467797	63.338023
1809.631321	87.311141	63.343028
1808.876252	78.642700	63.348033
1808.637133	74.391467	63.353038
1807.882294	89.734192	63.358042
1807.466651	90.062176	63.363047
1807.140377	90.486356	63.368052
1806.031128	94.586258	63.373057
1804.986103	80.690418	63.378062
1803.945856	87.042337	63.383066
1803.496929	77.251352	63.388071
1803.374639	81.448405	63.393076
1802.477737	87.295001	63.398081
1802.004803	81.415601	63.403086
1801.067477	80.463919	63.408090
1800.682868	76.885511	63.413095
1800.178323	77.077800	63.418100
1799.422429	92.837022	63.423105
1799.030661	83.877490	63.428110
1797.743215	86.461823	63.433114
1796.606038	76.168274	63.438119
1796.654456	70.851069	63.443124
1795.788634	84.613930	63.448129
1795.477751	76.117808	63.453134
1794.658131	89.193655	63.458138
1794.257078	83.708126	63.463143
1794.191498	79.413563	63.468148
1792.870443	86.160173	63.473153
1791.807863	80.902712	63.478158
1790.777246	84.043937	63.483162
1790.448876	83.954354	63.488167
1789.785387	73.412112	63.493172
1788.789850	83.361923	63.498177
1788.570039	78.002157	63.503182
1788.044048	86.402916	63.508186
1787.375683	81.393515	63.513191
1787.096736	87.596145	63.518196
1786.477662	89.072947	63.523201
1786.227126	75.954556	63.528206
1784.613315	83.733280	63.533210
1783.732683	81.337542	63.538215
1783.352452	80.559169	63.543220
1782.444165	81.993593	63.548225
1782.375740	78.896415	63.553230
1781.596174	77.594826	63.558234
1781.084521	87.409443	63.563239
1780.649851	82.347158	63.568244
1779.087438	87.886288	63.573249
1778.406233	84.913240	63.578254
1777.868412	80.080233	63.583258
1777.209868	82.112096	63.588263
1776.696372	77.887097	63.593268
1775.768120	96.523313	63.598273
1775.653383	78.073638	63.603278
1775.124741	90.562370	63.608282
1774.535939	91.198564	63.613287
1774.254567	82.383936	63.618292
1772.629341	82.689565	63.623297
1771.913275	70.782127	63.628302
1770.996378	82.247550	63.633306
1770.635545	77.102578	63.638311
1770.311270	73.998728	63.643316
1769.250743	80.241910	63.648321
1769.272033	67.947700	63.653326
1768.796579	79.787720	63.658330
1768.355688	72.346757	63.663335
1767.632537	76.825326	63.668340
1765.894494	91.493145	63.673345
1765.628378	81.438162	63.678350
1764.556587	77.957864	63.683354
1764.349615	77.547799	63.688359
1764.108129	82.613779	63.693364
1763.045354	85.465226	63.698369
1762.069448	79.681492	63.703374
1761.500046	79.095598	63.708378
1760.997788	82.272766	63.713383
1760.359477	80.606541	63.718388
1759.883257	93.651511	63.723393
1759.506061	74.639545	63.728398
1758.820547	75.215407	63.733402
1757.502032	82.347988	63.738407
1756.899490	74.574727	63.743412
1755.849049	87.531119	63.748417
1755.629530	74.940832	63.753422
1754.750555	82.162877	63.758426
1754.619472	76.024186	63.763431
1754.084122	76.945214	63.768436
1753.806938	73.081665	63.773441
1752.634780	77.620515	63.778446
1751.353793	80.407274	63.783450
1750.819200	80.200637	63.788455
1750.312865	81.497111	63.793460
1749.634150	77.456059	63.798465
1749.191891	75.299796	63.803470
1748.685781	81.256226	63.808474
1748.240195	83.520782	63.813479
1747.109834	81.596817	63.818484
1745.840347	83.888156	63.823489
1745.896993	76.691454	63.828494
1745.196508	86.942928	63.833498
1744.810610	82.423273	63.838503
1744.190102	71.994073	63.843508
1743.357238	80.607582	63.848513
1742.629715	81.912380	63.853518
1741.735190	85.976622	63.858522
1741.191794	80.436442	63.863527
1740.764042	86.921335	63.868532
1740.219118	86.199090	63.873537
1739.665696	79.632309	63.878542
1738.490709	88.005269	63.883546
1737.556585	80.956474	63.888551
1736.989036	75.838035	63.893556
1736.101975	79.880590	63.898561
1735.997038	80.961918	63.903566
1735.231225	82.296456	63.908570
1734.783359	90.574424	63.913575
1734.353545	86.482801	63.918580
1733.471886	90.477192	63.923585
1732.606382	85.606355	63.928590
1731.900646	86.436177	63.933594
1731.337051	84.720245	63.938599
1731.149469	73.104200	63.943604
1730.534136	84.879710	63.948609
1729.384418	87.532086	63.953614
1728.235057	90.280603	63.958618
1727.553253	79.845370	63.963623
1727.746856	81.059054	63.968628
1726.616594	78.605217	63.973633
1726.535209	76.465755	63.978638
1725.734325	81.712057	63.983642
1724.418756	82.342275	63.988647
1723.805847	77.382435	63.993652
1723.141951	82.282120	63.998657
1722.652996	75.490636	64.003662
1722.177159	86.892322	64.008666
1721.477224	78.387049	64.013671
1721.411470	70.041248	64.018676
1720.180458	83.647660	64.023681
1719.785912	71.741212	64.028686
1718.691025	88.172462	64.033690
1718.064202	79.371719	64.038695
1717.867891	81.006891	64.043700
1716.327975	86.561405	64.048705
1715.871663	77.148517	64.053710
1715.025939	81.157704	64.058714
1714.632531	81.901648	64.063719
1714.217425	83.073247	64.068724
1713.511472	86.864688	64.073729
1712.985479	88.192677	64.078734
1712.138675	85.127680	64.083738
1712.055825	83.972490	64.088743
1711.358270	78.174527	64.093748
1709.961312	80.640675	64.098753
1709.605667	82.220731	64.103758
1708.715209	77.312868	64.108762
1708.768912	79.548582	64.113767
1707.791479	78.510264	64.118772
1706.615836	85.774717	64.123777
1706.431355	73.877481	64.128782
1705.553984	82.242598	64.133786
1705.217534	84.707448	64.138791
1704.656444	81.852541	64.143796
1703.312014	84.072224	64.148801
1702.914934	74.205223	64.153806
1701.767013	86.325542	64.158810
1701.289933	74.755489	64.163815
1701.123707	70.152064	64.168820
1700.203649	87.086990	64.173825
1700.029571	88.767518	64.178830
1699.727674	90.685975	64.183834
1698.444171	86.144908	64.188839
1697.730873	84.958977	64.193844
1697.104422	85.091802	64.198849
1696.587342	79.870736	64.203854
1695.844528	89.726813	64.208858
1694.677659	90.084261	64.213863
1693.923641	73.256380	64.218868
1693.157454	78.617028	64.223873
1692.948327	76.013726	64.228878
1692.420258	82.471979	64.233882
1691.739232	84.220423	64.238887
1691.697857	75.146913	64.243892
1690.696491	81.224603	64.248897
1689.883115	81.366623	64.253902
1689.173734	89.908493	64.258906
1688.436267	86.107031	64.263911
1688.212771	75.337231	64.268916
1687.075301	86.773060	64.273921
1686.103600	79.769683	64.278926
1685.306220	82.542727	64.283930
1684.875313	84.076394	64.288935
1684.579633	79.119788	64.293940
1684.034602	86.369230	64.298945
1683.766846	77.162946	64.303950
1682.857036	86.846852	64.308954
1681.716146	83.563651	64.313959
1681.669171	76.741389	64.318964
1680.560088	92.034749	64.323969
1679.990099	75.358990	64.328974
1678.776010	84.447824	64.333978
1678.251545	80.533679	64.338983
1678.108944	82.598723	64.343988
1677.213824	83.181096	64.348993
1676.868762	74.463345	64.353998
1676.232981	82.009483	64.359002
1675.261769	84.359128	64.364007
1674.491995	79.708079	64.369012
1673.481071	86.722446	64.374017
1673.215928	73.589059	64.379022
1673.164059	89.157599	64.384026
1672.274595	79.969655	64.389031
1671.255800	72.732490	64.394036
1670.397844	88.810717	64.399041
1670.080933	80.509547	64.404046
1669.565053	84.846400	64.409050
1668.652675	86.081236	64.414055
1667.792356	79.561653	64.419060
1666.699618	92.084813	64.424065
1666.103128	78.218724	64.429070
1665.873952	82.347601	64.434074
1665.385628	89.870319	64.439079
1665.099802	81.896954	64.444084
1664.667470	85.058298	64.449089
1663.918017	77.150706	64.454094
1662.923832	76.383154	64.459098
1661.942093	81.719706	64.464103
1661.782491	81.497670	64.469108
1660.387788	86.267461	64.474113
1660.054157	84.620669	64.479118
1658.699373	81.328882	64.484122
1658.290064	90.181062	64.489127
1658.176883	83.255774	64.494132
1657.732461	87.300574	64.499137
1657.366227	82.041361	64.504142
1656.569951	82.136519	64.509146
1655.368186	80.960392	64.514151
1655.150331	77.317671	64.519156
1654.623228	81.276256	64.524161
1653.469584	74.579350	64.529166
1652.459022	80.021411	64.534170
1651.685301	83.408885	64.539175
1651.584824	76.579356	64.544180
1650.652186	81.862379	64.549185
1650.850652	79.295253	64.554190
1649.787932	80.836260	64.559194
1648.574750	89.559103	64.564199
1647.957014	81.179571	64.569204
1647.190573	84.800860	64.574209
1647.285011	78.921248	64.579214
1646.751502	86.391219	64.584218
1645.594735	79.532382	64.589223
1644.991455	76.714156	64.594228
1644.022020	81.681322	64.599233
1643.431778	79.077072	64.604238
1643.292274	85.856807	64.609242
1641.912197	79.965447	64.614247
1641.594104	80.413579	64.619252
1640.390576	78.356205	64.624257
1640.400741	74.169472	64.629262
1639.779685	83.973094	64.634266
1639.458808	85.527134	64.639271
1638.486153	79.837558	64.644276
1637.282582	84.745730	64.649281
1636.885215	79.338500	64.654286
1636.621580	83.982219	64.659290
1635.808834	93.614449	64.664295
1635.048048	75.045101	64.669300
1633.800410	80.655724	64.674305
1633.524461	84.632758	64.679310
1633.015040	83.747198	64.684314
1632.091670	83.279072	64.689319
1632.489587	71.595257	64.694324
1630.975946	82.381224	64.699329
1630.537268	79.098448	64.704334
1629.580580	82.984938	64.709338
1628.774890	83.857476	64.714343
1628.558411	76.322545	64.719348
1627.997078	79.904942	64.724353
1627.019495	70.574903	64.729358
1626.350321	81.652487	64.734362
1625.316022	79.071484	64.739367
1625.176038	73.509823	64.744372
1624.740724	83.865843	64.749377
1624.306936	83.179583	64.754382
1623.124603	81.658179	64.759386
1622.235510	84.852675	64.764391
1621.947926	81.547471	64.769396
1621.555968	91.082884	64.774401
1620.500079	85.097449	64.779406
1619.517061	88.445644	64.784410
1618.943857	80.134742	64.789415
1618.827338	81.435538	64.794420
1617.901250	83.352248	64.799425
1617.324469	85.459470	64.804430
1616.219965	92.692157	64.809434
1615.690007	89.966368	64.814439
1615.515332	87.094242	64.819444
1614.654877	89.374271	64.824449
1614.250092	83.454127	64.829454
1613.177502	85.394116	64.834458
1612.354332	86.701531	64.839463
1611.968253	79.261358	64.844468
1611.364709	85.788386	64.849473
1610.395689	79.871159	64.854478
1609.412769	81.927791	64.859482
1608.940003	89.238304	64.864487
1608.520268	87.911136	64.869492
1607.667521	85.435336	64.874497
1607.607869	85.389815	64.879502
1607.381018	83.019576	64.884506
1606.114730	81.087311	64.889511
1605.533813	87.662786	64.894516
1604.636242	85.162570	64.899521
1604.332247	80.587351	64.904526
1603.287166	88.349928	64.909530
1601.933777	94.360579	64.914535
1601.555520	78.852892	64.919540
1601.204214	88.607354	64.924545
1600.784950	84.107221	64.929550
1600.500349	88.817354	64.934554
1599.544694	92.691076	64.939559
1598.914283	78.899789	64.944564
1598.107244	86.441613	64.949569
1597.722740	79.792839	64.954574
1596.651297	78.312176	64.959578
1595.396266	79.420128	64.964583
1595.039491	78.778408	64.969588
1594.648019	82.075197	64.974593
1594.237635	74.749281	64.979598
1593.725866	80.127877	64.984602
1592.862544	78.844386	64.989607
1591.815029	78.574200	64.994612
1590.978978	70.904331	64.999617
1590.329875	71.775654	65.004622
1590.286360	77.843106	65.009626
1589.647167	81.160333	65.014631
1589.722815	76.887501	65.019636
1588.697508	87.271039	65.024641
1587.564409	76.439206	65.029646
1587.169489	89.979049	65.034650
1585.747849	79.926359	65.039655
1584.909201	70.011282	65.044660
1584.284247	77.976766	65.049665
1583.650079	79.955915	65.054670
1583.574344	78.110458	65.059674
1583.102656	77.680969	65.064679
1583.093464	84.739622	65.069684
1581.499311	87.379100	65.074689
1580.645610	77.865387	65.079694
1580.384401	75.249873	65.084698
1579.863821	76.597527	65.089703
1579.141238	74.167290	65.094708
1578.028119	85.545665	65.099713
1577.467759	79.848951	65.104718
1576.949257	81.804991	65.109722
1576.500163	75.229566	65.114727
1575.499995	85.071360	65.119732
1574.379901	79.630749	65.124737
1573.693702	84.455159	65.129742
1573.377613	81.474620	65.134746
1572.834476	82.750165	65.139751
1572.718787	85.343956	65.144756
1572.169129	89.646769	65.149761
1571.026405	83.623115	65.154766
1570.267469	78.989304	65.159770
1569.561727	86.026174	65.164775
1569.653047	78.563769	65.169780
1568.322861	91.667170	65.174785
1567.711112	77.863469	65.179790
1567.182548	72.677381	65.184794
1566.300346	88.398347	65.189799
1565.657815	84.469874	65.194804
1564.470064	81.918011	65.199809
1563.885999	80.427726	65.204814
1563.388606	84.760081	65.209818
1562.777017	87.577756	65.214823
1562.646391	76.036273	65.219828
1562.236691	79.659243	65.224833
1561.695553	84.203557	65.229838
1560.600881	88.408470	65.234842
1559.924628	86.991182	65.239847
1559.461779	85.756031	65.244852
1558.257988	84.521924	65.249857
1557.793887	80.828456	65.254862
1557.132853	85.044888	65.259866
1556.701510	91.563487	65.264871
1555.926562	73.906349	65.269876
1555.020402	87.385502	65.274881
1554.449778	85.535108	65.279886
1554.289214	81.968451	65.284890
1553.048643	91.026850	65.289895
1552.213487	78.605400	65.294900
1551.172833	87.091123	65.299905
1551.085718	78.206250	65.304910
1550.340458	79.190637	65.309914
1549.887396	87.482061	65.314919
1549.596104	76.929647	65.319924
1548.460010	87.937939	65.324929
1547.668655	78.379640	65.329934
1547.133537	82.612334	65.334938
1546.628131	88.576565	65.339943
1546.344667	76.769207	65.344948
1545.003596	82.383677	65.349953
1544.213644	85.064116	65.354958
1543.724985	85.615060	65.359962
1543.366055	92.797102	65.364967
1542.910336	84.579517	65.369972
1541.877019	87.661337	65.374977
1541.145830	80.487338	65.379982
1540.547464	78.996178	65.384986
1539.634978	89.118947	65.389991
1539.520532	84.259721	65.394996
1539.062956	86.354323	65.400001
1537.880354	81.324216	65.405006
1537.423718	75.768729	65.410010
1536.541514	83.044962	65.415015
1536.284509	79.791684	65.420020
1535.067162	81.321038	65.425025
1534.112761	80.216047	65.430030
1533.810179	83.079240	65.435034
1533.530861	78.739814	65.440039
1533.135037	85.147110	65.445044
1532.388783	83.417674	65.450049
1531.304552	84.607325	65.455054
1530.559680	77.681515	65.460058
1529.840673	86.415756	65.465063
1529.682761	78.250202	65.470068
1528.248003	81.466786	65.475073
1527.473056	81.495515	65.480078
1527.186081	76.936529	65.485082
1526.756469	87.200186	65.490087
1526.430573	77.424421	65.495092
1525.815097	82.631847	65.500097
1525.109646	79.588611	65.505102
1524.649400	76.449637	65.510106
1523.483697	83.387721	65.515111
1523.158631	75.482126	65.520116
1521.663890	87.421071	65.525121
1521.196817	80.310763	65.530126
1520.797421	80.964222	65.535130
1520.168498	87.263482	65.540135
1520.095031	81.410557	65.545140
1518.425158	88.296301	65.550145
1517.640540	83.117799	65.555150
1517.199666	81.822392	65.560154
1516.606194	84.285530	65.565159
1516.497499	78.843489	65.570164
1515.599448	81.659388	65.575169
1514.597671	83.987139	65.580174
1514.135561	78.117130	65.585178
1513.249290	91.148425	65.590183
1513.234966	83.554573	65.595188
1512.616834	87.264293	65.600193
1511.560906	75.707443	65.605198
1511.209167	77.100818	65.610202
1510.246658	85.408551	65.615207
1509.768749	78.572788	65.620212
1508.682962	83.626299	65.625217
1508.255885	76.422907	65.630222
1507.830171	83.981420	65.635226
1507.115517	87.539321	65.640231
1506.524211	76.815397	65.645236
1505.365186	90.058777	65.650241
1504.718520	82.220064	65.655246
1504.187327	78.881054	65.660250
1503.637119	87.531702	65.665255
1502.973600	82.184146	65.670260
1501.993317	86.350400	65.675265
1501.405630	83.882977	65.680270
1501.022024	86.866285	65.685274
1500.450752	90.065503	65.690279
1500.085318	92.311051	65.695284
1498.789767	80.082645	65.700289
1497.929670	82.261726	65.705294
1497.754463	85.402728	65.710298
1497.055184	86.302550	65.715303
1496.760959	80.361708	65.720308
1495.900570	90.477785	65.725313
1494.640992	84.863834	65.730318
1494.875154	83.339720	65.735322
1494.027739	85.653984	65.740327
1492.938266	79.028964	65.745332
1492.008967	84.555938	65.750337
1491.319538	84.903829	65.755342
1491.102832	76.168874	65.760346
1490.282933	80.438952	65.765351
1490.255135	78.311487	65.770356
1488.795611	79.778425	65.775361
1488.196223	73.939705	65.780366
1487.677272	68.968158	65.785370
1487.076394	83.461685	65.790375
1487.129869	70.962117	65.795380
1485.962747	78.021865	65.800385
1485.172956	82.823334	65.805390
1484.679216	72.689475	65.810394
1483.688277	79.484676	65.815399
1482.661597	80.012329	65.820404
1482.135229	81.324651	65.825409
1481.315246	78.324864	65.830414
1481.115381	78.361556	65.835418
1480.555008	82.612468	65.840423
1480.669892	72.385031	65.845428
1479.811737	81.133509	65.850433
1478.690641	74.616028	65.855438
1478.335646	69.851817	65.860442
1476.889721	80.179229	65.865447
1476.223693	78.202090	65.870452
1475.723195	78.978859	65.875457
1475.113469	75.180821	65.880462
1474.555729	80.461082	65.885466
1474.146525	81.844672	65.890471
1473.249719	81.310880	65.895476
1472.203766	81.874717	65.900481
1471.984801	80.968257	65.905486
1471.598562	76.223204	65.910490
1470.700520	85.061606	65.915495
1469.820052	84.099433	65.920500
1469.108606	79.970628	65.925505
1468.553993	90.515936	65.930510
1468.233057	82.775276	65.935514
1467.433373	88.387315	65.940519
1466.476847	81.845257	65.945524
1466.031721	90.348320	65.950529
1465.091063	90.302480	65.955534
1464.927840	83.445094	65.960538
1463.937931	94.494840	65.965543
1463.251809	84.432558	65.970548
1462.256596	76.750188	65.975553
1461.686488	80.912762	65.980558
1461.262688	83.289017	65.985562
1461.187726	88.470471	65.990567
1460.650652	81.831784	65.995572
1459.772374	83.252085	66.000577
1458.979239	82.750706	66.005582
1458.155687	72.279763	66.010586
1456.678408	76.231706	66.015591
1456.689997	79.841344	66.020596
1456.080919	83.284702	66.025601
1455.582613	85.207592	66.030606
1455.002633	74.469271	66.035610
1453.893227	80.436474	66.040615
1453.400876	76.462087	66.045620
1452.802436	83.119218	66.050625
1452.187185	78.498880	66.055630
1451.700609	73.881746	66.060634
1450.521542	83.283647	66.065639
1450.068786	77.885262	66.070644
1449.287048	80.752081	66.075649
1448.956659	81.796712	66.080654
1448.752984	75.839910	66.085658
1447.292605	82.362805	66.090663
1446.943569	78.655805	66.095668
1446.221260	76.834279	66.100673
1445.280253	79.384211	66.105678
1444.498730	73.867772	66.110682
1443.738920	78.435823	66.115687
1443.443311	74.138426	66.120692
1442.847373	66.477762	66.125697
1442.590676	77.966053	66.130702
1442.073570	72.320852	66.135706
1440.792372	73.407805	66.140711
1440.464543	58.146070	66.145716
1439.840749	67.798753	66.150721
1438.828429	69.469027	66.155726
1438.140822	66.203785	66.160730
1437.092920	76.340209	66.165735
1436.843790	58.938620	66.170740
1436.781851	71.812074	66.175745
1435.674426	65.650420	66.180750
1434.475454	62.439655	66.185754
1433.989484	77.548860	66.190759
1433.703579	69.167124	66.195764
1433.247650	76.131190	66.200769
1432.365453	67.555651	66.205774
1431.641842	69.687824	66.210778
1430.596605	67.763092	66.215783
1430.482429	74.464673	66.220788
1430.094429	71.315813	66.225793
1429.093912	79.497141	66.230798
1428.210763	66.175048	66.235802
1427.539417	78.207074	66.240807
1427.089180	75.952792	66.245812
1426.772974	71.778523	66.250817
1425.699184	79.540984	66.255822
1425.054556	72.905215	66.260826
1424.201709	74.114900	66.265831
1424.100003	76.878360	66.270836
1423.202894	71.053869	66.275841
1422.269481	81.011250	66.280846
1421.801854	69.012426	66.285850
1420.869867	70.597397	66.290855
1420.509563	67.248592	66.295860
1419.501151	77.530135	66.300865
1418.677209	77.341177	66.305870
1418.538435	67.772246	66.310874
1417.780329	77.441558	66.315879
1417.449295	74.592732	66.320884
1416.398586	69.284679	66.325889
1415.389515	75.627035	66.330894
1415.051940	62.770168	66.335898
1414.489738	76.412286	66.340903
1414.343727	76.569734	66.345908
1413.378397	72.703661	66.350913
1412.311644	82.411001	66.355918
1411.921648	74.889497	66.360922
1411.561993	81.800417	66.365927
1410.452989	78.330926	66.370932
1409.520726	81.068718	66.375937
1408.702687	79.495814	66.380942
1408.631889	72.183772	66.385946
1407.768651	78.701649	66.390951
1407.589357	75.748278	66.395956
1406.840296	78.028009	66.400961
1405.915669	79.193916	66.405966
1405.693170	76.947592	66.410970
1404.642783	84.360984	66.415975
1403.835284	74.956703	66.420980
1403.145200	77.569264	66.425985
1402.228116	82.286909	66.430990
1402.252137	66.431494	66.435994
1401.313649	83.041383	66.440999
1400.429290	82.401558	66.446004
1399.719067	89.401327	66.451009
1399.125626	84.465294	66.456014
1399.101751	75.177722	66.461018
1397.902588	78.330112	66.466023
1397.101280	75.169689	66.471028
1396.481765	80.492900	66.476033
1395.836099	78.121455	66.481038
1395.778502	66.383894	66.486042
1394.400609	85.105825	66.491047
1393.583344	72.530220	66.496052
1393.274955	74.681552	66.501057
1392.900280	84.498080	66.506062
1392.779881	77.637054	66.511066
1391.637484	73.310274	66.516071
1390.866713	80.592484	66.521076
1390.176869	79.823967	66.526081
1389.187616	81.947919	66.531086
1388.374803	73.257285	66.536090
1387.621827	81.621629	66.541095
1387.363306	80.456533	66.546100
1386.834047	79.835956	66.551105
1386.409822	72.610064	66.556110
1385.603441	68.518459	66.561114
1384.646800	82.291099	66.566119
1384.201543	82.038798	66.571124
1383.692275	77.917304	66.576129
1382.703947	69.369697	66.581134
1381.853275	79.498440	66.586138
1380.777579	85.059759	66.591143
1380.657360	72.961560	66.596148
1380.405618	78.975371	66.601153
1379.860319	82.153134	66.606158
1379.219478	77.568426	66.611162
1378.193677	84.134234	66.616167
1377.503555	77.032617	66.621172
1376.855520	75.893175	66.626177
1376.086310	70.970903	66.631182
1375.270981	69.943215	66.636186
1374.582997	76.433239	66.641191
1374.186927	72.049321	66.646196
1373.962910	75.292704	66.651201
1372.885294	77.004924	66.656206
1372.581234	73.910540	66.661210
1371.759624	79.317924	66.666215
1371.023505	82.193283	66.671220
1369.986968	80.838058	66.676225
1369.155419	77.048506	66.681230
1368.652739	81.703433	66.686234
1368.338513	78.464006	66.691239
1367.858999	76.657521	66.696244
1367.232015	78.550419	66.701249
1366.089603	78.293836	66.706254
1365.762154	73.932127	66.711258
1365.278436	74.774058	66.716263
1364.509144	71.316816	66.721268
1363.678345	73.287850	66.726273
1362.992711	76.301842	66.731278
1362.752154	75.375171	66.736282
1361.353980	78.622296	66.741287
1360.675272	73.026463	66.746292
1360.076585	71.308315	66.751297
1359.530079	78.922312	66.756302
1359.406124	72.516028	66.761306
1358.037143	82.621524	66.766311
1357.354461	80.582410	66.771316
1357.187386	74.153017	66.776321
1356.306796	75.067509	66.781326
1356.036754	78.996311	66.786330
1355.233304	78.818309	66.791335
1354.115452	76.353211	66.796340
1353.552848	82.250864	66.801345
1352.970373	75.933247	66.806350
1352.660835	76.846838	66.811354
1351.806428	68.632775	66.816359
1350.753725	72.066256	66.821364
1350.544802	76.147770	66.826369
1349.829535	82.454477	66.831374
1349.668296	75.909038	66.836378
1348.361748	81.191675	66.841383
1347.577621	72.343531	66.846388
1347.170691	73.949130	66.851393
1346.442503	76.205058	66.856398
1345.704302	71.232135	66.861402
1344.632927	86.842862	66.866407
1344.521769	77.249045	66.871412
1344.207682	76.370336	66.876417
1343.107575	79.514887	66.881422
1342.921353	69.135059	66.886426
1341.561082	71.887304	66.891431
1341.235424	75.479590	66.896436
1340.769129	75.569692	66.901441
1339.776227	70.052207	66.906446
1339.157158	65.741601	66.911450
1338.326930	72.673721	66.916455
1338.265185	72.240602	66.921460
1337.220013	73.752133	66.926465
1336.034585	77.424347	66.931470
1335.842716	78.104762	66.936474
1334.864479	80.914545	66.941479
1334.560444	76.041331	66.946484
1334.504266	75.888029	66.951489
1333.148023	79.505399	66.956494
1332.533759	76.050327	66.961498
1331.645534	82.542236	66.966503
1331.330573	81.163766	66.971508
1330.872669	79.790676	66.976513
1330.057034	77.132456	66.981518
1329.365170	68.673359	66.986522
1328.540559	72.160471	66.991527
1328.359797	75.319706	66.996532
1327.435955	76.073925	67.001537
1326.458510	72.793296	67.006542
1326.359746	62.491035	67.011546
1324.995934	73.961379	67.016551
1324.136628	70.936362	67.021556
1323.680125	68.720946	67.026561
1322.985048	68.910505	67.031566
1323.003791	72.864356	67.036570
1322.432298	77.481343	67.041575
1321.487226	74.988788	67.046580
1320.635588	73.444911	67.051585
1320.198178	81.522547	67.056590
1319.753836	67.124625	67.061594
1318.535379	82.479615	67.066599
1317.605922	77.524492	67.071604
1317.342831	72.277337	67.076609
1316.732879	71.727954	67.081614
1316.539900	67.284949	67.086618
1315.508351	66.444627	67.091623
1314.566084	70.972331	67.096628
1314.150138	69.581535	67.101633
1313.342843	69.990793	67.106638
1313.229353	65.215025	67.111642
1312.238616	66.667446	67.116647
1311.094580	75.144444	67.121652
1310.793668	68.105550	67.126657
1310.123209	70.916865	67.131662
1309.880060	78.410093	67.136666
1308.776059	80.393045	67.141671
1308.255717	72.308810	67.146676
1307.918944	71.701800	67.151681
1306.871051	82.030657	67.156686
1306.450148	76.362309	67.161690
1305.404813	84.699039	67.166695
1304.781224	71.911327	67.171700
1303.848507	72.655926	67.176705
1302.989279	80.907869	67.181710
1302.523808	73.716942	67.186714
1302.159514	78.740963	67.191719
1301.951950	72.160320	67.196724
1301.597049	71.666582	67.201729
1300.588164	81.451488	67.206734
1299.468021	64.447053	67.211738
1298.990269	72.770801	67.216743
1298.079105	75.760744	67.221748
1297.428939	69.069128	67.226753
1296.790453	78.907103	67.231758
1296.365500	71.332838	67.236762
1295.640395	77.402996	67.241767
1295.081061	74.964236	67.246772
1294.000515	74.559074	67.251777
1293.012019	79.665003	67.256782
1292.896276	71.483322	67.261786
1292.269122	77.247742	67.266791
1292.046058	74.887978	67.271796
1291.145120	66.807499	67.276801
1290.069918	79.504588	67.281806
1289.672929	78.120244	67.286810
1289.193449	70.447417	67.291815
1288.640952	71.375994	67.296820
1287.552331	67.103796	67.301825
1286.897652	83.501418	67.306830
1286.648366	64.269020	67.311834
1285.667869	72.887180	67.316839
1284.944795	70.364072	67.321844
1284.350307	72.724913	67.326849
1283.822854	74.308685	67.331854
1283.607738	68.637585	67.336858
1282.151514	68.948188	67.341863
1281.436824	66.191933	67.346868
1280.942495	79.194056	67.351873
1280.449970	70.179722	67.356878
1280.251207	67.111188	67.361882
1278.537234	72.914386	67.366887
1278.166812	75.496646	67.371892
1277.889982	70.027752	67.376897
1277.361832	73.325809	67.381902
1276.451126	67.123491	67.386906
1275.638316	76.216470	67.391911
1274.524874	74.245878	67.396916
1274.569509	73.174517	67.401921
1273.918594	73.382299	67.406926
1273.509535	74.180835	67.411930
1272.256408	76.725263	67.416935
1271.606830	73.058202	67.421940
1271.381889	70.481117	67.426945
1270.774425	78.904346	67.431950
1270.003981	73.621180	67.436954
1268.928329	81.644191	67.441959
1268.251687	73.595861	67.446964
1268.252228	69.658261	67.451969
1267.149860	82.101055	67.456974
1266.559945	73.915930	67.461978
1265.717478	71.421275	67.466983
1265.331386	69.182058	67.471988
1265.220386	65.047728	67.476993
1263.863968	70.559106	67.481998
1263.383369	72.181163	67.487002
1262.626392	72.058879	67.492007
1261.745539	70.532285	67.497012
1261.143637	72.457488	67.502017
1260.348645	65.881957	67.507022
1260.091492	64.864895	67.512026
1259.712542	76.708516	67.517031
1259.014874	75.703156	67.522036
1258.063709	69.403199	67.527041
1257.195915	79.857973	67.532046
1257.034143	72.420064	67.537050
1255.622800	74.188556	67.542055
1254.734009	81.647262	67.547060
1254.213264	75.721987	67.552065
1253.542637	79.194096	67.557070
1253.685866	76.765048	67.562074
1253.061444	73.677473	67.567079
1252.252019	72.868086	67.572084
1251.923003	78.126202	67.577089
1250.720559	76.942493	67.582094
1249.504379	76.060595	67.587098
1248.717765	84.258427	67.592103
1248.159450	79.935028	67.597108
1248.008921	74.140118	67.602113
1247.250632	82.349214	67.607118
1247.153867	74.085671	67.612122
1246.691320	75.808941	67.617127
1245.709145	71.838383	67.622132
1245.068676	72.593299	67.627137
1244.228193	71.640618	67.632142
1243.213908	71.567144	67.637146
1242.523413	75.988600	67.642151
1241.978457	76.963297	67.647156
1241.509730	71.283648	67.652161
1241.150762	81.536081	67.657166
1240.176957	71.784576	67.662170
1239.027302	74.730463	67.667175
1238.679694	80.839950	67.672180
1238.419695	67.403080	67.677185
1237.690942	74.475209	67.682190
1236.673470	73.703644	67.687194
1235.895173	76.249848	67.692199
1235.522027	76.908636	67.697204
1235.206506	71.108429	67.702209
1234.347039	78.486780	67.707214
1233.338970	70.968996	67.712218
1232.894307	69.295772	67.717223
1232.083419	73.988692	67.722228
1231.640824	67.945341	67.727233
1230.422143	77.322077	67.732238
1230.015826	71.047447	67.737242
1229.692835	70.987044	67.742247
1229.239951	70.595632	67.747252
1228.879738	65.367093	67.752257
1227.425349	80.545162	67.757262
1227.017127	69.708645	67.762266
1226.434205	71.083626	67.767271
1225.153845	71.993929	67.772276
1224.248081	67.523944	67.777281
1223.714120	69.980829	67.782286
1223.676546	67.205216	67.787290
1223.021048	72.226668	67.792295
1222.638997	76.480801	67.797300
1221.841888	65.359201	67.802305
1221.002823	66.823806	67.807310
1220.314019	67.603761	67.812314
1220.016972	74.906862	67.817319
1219.338117	63.108859	67.822324
1218.498240	67.068367	67.827329
1217.603465	64.047455	67.832334
1216.972285	65.846434	67.837338
1216.051376	63.260193	67.842343
1215.270851	64.379594	67.847348
1214.830515	62.458101	67.852353
1214.444099	70.871410	67.857358
1214.096584	63.873066	67.862362
1213.399240	72.047239	67.867367
1212.412369	73.057531	67.872372
1211.719708	66.688097	67.877377
1211.483274	68.613534	67.882382
1210.408869	67.338518	67.887386
1209.362485	62.793133	67.892391
1208.855970	69.765264	67.897396
1208.473198	70.193771	67.902401
1208.302468	69.577714	67.907406
1207.171763	64.104286	67.912410
1206.349526	70.670886	67.917415
1205.693991	65.300083	67.922420
1205.681987	61.097975	67.927425
1204.272796	64.738019	67.932430
1203.707423	55.833074	67.937434
1202.865599	67.859118	67.942439
1202.804344	77.346676	67.947444
1201.763998	66.847251	67.952449
1200.796801	72.369296	67.957454
1200.413837	62.553808	67.962458
1199.786324	68.860778	67.967463
1199.279300	68.572601	67.972468
1198.845405	62.562570	67.977473
1197.814930	73.215116	67.982478
1196.915291	65.949769	67.987482
1196.518510	67.758781	67.992487
1196.293438	69.294476	67.997492
1195.366724	67.628542	68.002497
1194.638172	64.161727	68.007502
1193.892285	63.340677	68.012506
1193.360730	66.057385	68.017511
1192.114810	65.601298	68.022516
1191.832912	59.366819	68.027521
1191.047139	77.344918	68.032526
1191.019087	63.265614	68.037530
1190.209814	75.824238	68.042535
1189.010117	69.412451	68.047540
1188.466193	64.785581	68.052545
1187.852320	67.291452	68.057550
1187.357956	64.052323	68.062554
1186.464457	71.831917	68.067559
1185.407421	74.372005	68.072564
1185.306353	67.722403	68.077569
1184.388413	74.010915	68.082574
1184.647288	63.492518	68.087578
1183.795298	74.307494	68.092583
1182.540290	75.937618	68.097588
1182.123292	75.490044	68.102593
1181.217557	67.046095	68.107598
1180.728843	63.361362	68.112602
1179.509884	63.255812	68.117607
1178.787532	71.657899	68.122612
1179.069841	69.758670	68.127617
1178.556695	65.803429	68.132622
1177.636367	65.828580	68.137626
1176.621258	72.083661	68.142631
1175.969066	68.074842	68.147636
1175.691172	65.771123	68.152641
1174.710731	74.225302	68.157646
1173.898003	64.806187	68.162650
1173.357118	64.988609	68.167655
1172.854491	76.210074	68.172660
1172.670514	63.406115	68.177665
1171.144357	72.574729	68.182670
1170.463347	74.969857	68.187674
1170.045845	72.232598	68.192679
1169.418636	70.824968	68.197684
1169.335055	63.185403	68.202689
1167.999789	76.586219	68.207694
1167.412682	62.294640	68.212698
1166.865788	70.998408	68.217703
1166.026331	79.147890	68.222708
1165.370751	67.294163	68.227713
1164.745536	72.219345	68.232718
1164.626105	74.146676	68.237722
1164.190668	68.151089	68.242727
1163.116592	73.764265	68.247732
1162.233468	76.003883	68.252737
1161.233118	77.468930	68.257742
1160.997010	69.705388	68.262746
1160.132584	65.389706	68.267751
1158.917456	69.074601	68.272756
1158.967337	69.325486	68.277761
1158.376188	69.298284	68.282766
1157.770231	66.848051	68.287770
1156.667643	67.252288	68.292775
1156.108953	71.514023	68.297780
1155.689935	71.760644	68.302785
1155.156803	82.058129	68.307790
1154.371734	66.333030	68.312794
1153.493387	73.227118	68.317799
1152.732459	69.421684	68.322804
1152.556287	70.317237	68.327809
1151.747867	81.294032	68.332814
1151.056586	75.775962	68.337818
1150.242966	69.782185	68.342823
1149.648755	77.558341	68.347828
1149.206026	70.251873	68.352833
1147.646111	75.636402	68.357838
1147.391496	66.737233	68.362842
1146.832269	70.625312	68.367847
1146.533235	74.957712	68.372852
1146.278091	66.862884	68.377857
1145.178680	71.913962	68.382862
1144.406994	63.344629	68.387866
1143.674626	72.899507	68.392871
1143.114561	71.243081	68.397876
1142.002177	65.533378	68.402881
1141.204915	64.666900	68.407886
1140.839058	70.200543	68.412890
1140.646448	69.300963	68.417895
1140.063929	71.852321	68.422900
1139.609436	65.014514	68.427905
1138.409559	66.990707	68.432910
1137.700002	66.269552	68.437914
1137.643316	73.845085	68.442919
1135.678892	72.697484	68.447924
1135.480184	63.024593	68.452929
1134.924011	72.302284	68.457934
1134.542051	73.049221	68.462938
1134.384577	69.887402	68.467943
1133.078406	70.779779	68.472948
1132.282194	60.941736	68.477953
1131.846456	67.986197	68.482958
1131.415500	70.893498	68.487962
1130.887925	64.828996	68.492967
1129.612719	71.056081	68.497972
1129.069058	68.247435	68.502977
1128.431808	70.522069	68.507982
1127.958208	72.184037	68.512986
1127.033732	74.647867	68.517991
1125.885421	72.608774	68.522996
1125.778124	71.736624	68.528001
1125.099615	71.297543	68.533006
1125.028484	68.453155	68.538010
1124.222688	68.855925	68.543015
1123.192232	72.226028	68.548020
1122.851289	66.803631	68.553025
1121.794425	67.943363	68.558030
1120.995125	68.475991	68.563034
1120.491180	67.061381	68.568039
1119.829637	65.190866	68.573044
1119.857464	60.309058	68.578049
1118.786546	70.349886	68.583054
1118.164928	75.110500	68.588058
1117.653194	66.249085	68.593063
1116.769312	66.963905	68.598068
1115.613114	65.817061	68.603073
1114.701831	73.269917	68.608078
1114.659868	69.736482	68.613082
1114.242248	66.808440	68.618087
1113.356198	78.918817	68.623092
1112.765652	67.706055	68.628097
1111.736086	74.826064	68.633102
1111.341712	73.353024	68.638106
1111.134428	68.029216	68.643111
1110.009497	71.772325	68.648116
1109.283474	69.498903	68.653121
1108.687762	71.732241	68.658126
1108.330796	66.408590	68.663130
1107.712804	68.852056	68.668135
1106.724321	78.401955	68.673140
1106.213908	76.923721	68.678145
1105.421031	79.664672	68.683150
1103.968571	78.932398	68.688154
1103.349379	75.766761	68.693159
1102.795111	81.106455	68.698164
1102.892098	60.904387	68.703169
1102.147117	74.984037	68.708174
1101.818980	73.848973	68.713178
1101.147435	77.947321	68.718183
1099.888381	81.235528	68.723188
1099.231482	66.884110	68.728193
1099.114215	72.450752	68.733198
1098.872143	65.809400	68.738202
1097.295571	67.457603	68.743207
1096.614943	70.437744	68.748212
1096.287352	65.388548	68.753217
1095.410898	71.206855	68.758222
1094.655742	64.106227	68.763226
1094.396048	68.643685	68.768231
1093.891690	76.077544	68.773236
1093.264627	61.297181	68.778241
1091.614627	68.675171	68.783246
1091.058941	71.263272	68.788250
1090.731164	65.893980	68.793255
1090.204064	70.527597	68.798260
1090.301968	66.322201	68.803265
1088.795464	71.917464	68.808270
1088.011843	70.723976	68.813274
1087.821753	72.328231	68.818279
1086.880433	66.545610	68.823284
1086.019264	67.308867	68.828289
1085.002005	70.989124	68.833294
1085.107381	69.124343	68.838298
1084.635897	68.423677	68.843303
1083.564477	80.251312	68.848308
1083.000005	73.213390	68.853313
1082.215883	75.312703	68.858318
1081.761163	79.046973	68.863322
1081.166634	71.588051	68.868327
1079.852400	73.645544	68.873332
1079.862917	74.479861	68.878337
1079.285424	69.800012	68.883342
1078.461727	73.496787	68.888346
1077.503835	70.553779	68.893351
1076.347799	72.138245	68.898356
1076.218466	63.712752	68.903361
1075.515740	77.345711	68.908366
1075.226242	79.262254	68.913370
1074.859851	69.713821	68.918375
1073.540782	69.867102	68.923380
1073.225634	69.654082	68.928385
1072.697345	73.083085	68.933390
1071.856798	75.658162	68.938394
1071.290426	74.677700	68.943399
1070.606690	80.074267	68.948404
1069.758167	75.495886	68.953409
1068.591822	76.025423	68.958414
1067.937221	74.570138	68.963418
1067.570836	81.813315	68.968423
1067.027463	78.933672	68.973428
1066.862262	72.067201	68.978433
1065.887626	74.116404	68.983438
1064.985649	75.411292	68.988442
1064.503890	77.957675	68.993447
1063.924805	75.787046	68.998452
1063.093396	77.018668	69.003457
1062.027311	78.527327	69.008462
1061.607532	77.868902	69.013466
1061.260836	76.424555	69.018471
1060.718081	82.585604	69.023476
1060.094667	69.337485	69.028481
1058.774520	76.306622	69.033486
1058.629757	76.377158	69.038490
1058.106771	73.098456	69.043495
1056.684246	79.929340	69.048500
1056.136638	77.941364	69.053505
1055.687621	77.509945	69.058510
1055.377859	74.787105	69.063514
1055.302578	78.905716	69.068519
1053.959199	81.390488	69.073524
1053.188464	77.118285	69.078529
1052.349695	74.692505	69.083534
1052.182660	72.495745	69.088538
1051.444743	62.612190	69.093543
1050.252619	80.073058	69.098548
1050.230365	75.278065	69.103553
1049.423013	72.481430	69.108558
1048.725153	73.975663	69.113562
1048.072411	74.813005	69.118567
1047.160815	78.435466	69.123572
1046.806626	66.040241	69.128577
1045.613317	76.039066	69.133582
1044.611431	74.260568	69.138586
1044.341985	75.082659	69.143591
1043.806412	75.428268	69.148596
1043.567524	70.322388	69.153601
1043.035760	69.248117	69.158606
1041.772524	74.695889	69.163610
1041.230317	69.583077	69.168615
1040.385204	76.877191	69.173620
1040.294904	73.334104	69.178625
1039.594576	77.392889	69.183630
1038.619268	73.916497	69.188634
1038.009101	73.665265	69.193639
1037.422335	68.393961	69.198644
1037.212065	62.794670	69.203649
1035.882356	72.157602	69.208654
1035.220144	68.803286	69.213658
1034.960655	62.639386	69.218663
1034.165439	72.019778	69.223668
1033.459185	63.369115	69.228673
1032.308793	63.164415	69.233678
1031.762750	68.886011	69.238682
1031.550518	66.895144	69.243687
1030.955973	74.072119	69.248692
1029.755611	65.153141	69.253697
1029.265567	67.396490	69.258702
1028.751538	71.206435	69.263706
1028.507938	72.037031	69.268711
1027.711289	69.981454	69.273716
1026.942745	69.440030	69.278721
1026.208878	70.391212	69.283726
1025.671198	75.277263	69.288730
1024.978538	64.104438	69.293735
1024.296712	71.918204	69.298740
1023.990978	65.682815	69.303745
1022.863307	74.018537	69.308750
1022.091451	68.600068	69.313754
1021.574213	66.134178	69.318759
1020.845037	69.956280	69.323764
1020.314166	65.177565	69.328769
1019.437522	67.657475	69.333774
1018.648683	69.371198	69.338778
1018.524735	65.290990	69.343783
1017.524933	72.448870	69.348788
1016.474975	71.783492	69.353793
1015.415014	68.899329	69.358798
1014.984179	65.956063	69.363802
1014.727057	62.472641	69.368807
1014.098830	64.906716	69.373812
1014.016006	68.067724	69.378817
1013.401823	65.992581	69.383822
1012.650113	74.218022	69.388826
1011.958937	70.209147	69.393831
1010.586047	70.227521	69.398836
1009.750554	70.057881	69.403841
1009.372097	74.089112	69.408846
1008.891032	72.770234	69.413850
1008.483032	71.272572	69.418855
1008.210249	72.289165	69.423860
1007.330671	66.909920	69.428865
1006.399603	71.254589	69.433870
1005.810653	72.599037	69.438874
1005.266787	64.002970	69.443879
1003.948460	72.722278	69.448884
1003.494379	75.872977	69.453889
1002.915614	67.391273	69.458894
1002.857216	70.187269	69.463898
1002.064309	71.997840	69.468903
1001.094162	64.825800	69.473908
1000.711189	62.075197	69.478913
999.790050	68.206572	69.483918
998.601011	68.616749	69.488922
998.062414	63.877118	69.493927
997.476493	67.515578	69.498932
997.338299	66.424423	69.503937
996.723093	64.768921	69.508942
995.603454	62.509284	69.513946
994.975554	60.231323	69.518951
994.342384	77.738879	69.523956
994.096565	70.847401	69.528961
992.914904	62.635107	69.533966
992.010317	66.116116	69.538970
991.788459	64.522604	69.543975
990.950975	68.782999	69.548980
990.777549	65.827163	69.553985
990.190505	68.729358	69.558990
989.099350	62.505418	69.563994
988.616172	63.872462	69.568999
988.065191	72.990070	69.574004
986.938628	65.185331	69.579009
985.956021	72.706342	69.584014
985.590644	74.399999	69.589018
985.625122	61.269580	69.594023
984.928772	70.269969	69.599028
983.777080	64.571333	69.604033
983.057690	64.419497	69.609038
982.525771	63.310571	69.614042
982.242608	60.886291	69.619047
980.864029	73.693242	69.624052
980.531156	67.752341	69.629057
979.793562	71.616794	69.634062
979.396019	69.303756	69.639066
979.154471	66.535382	69.644071
978.091012	66.898776	69.649076
977.674865	62.363595	69.654081
976.691480	64.955122	69.659086
975.528810	65.439961	69.664090
975.337466	62.969531	69.669095
974.523482	65.294402	69.674100
974.015750	62.350766	69.679105
973.320877	69.822838	69.684110
972.365205	61.508360	69.689114
972.188447	61.774806	69.694119
971.378555	62.892644	69.699124
970.735126	63.204970	69.704129
969.551989	60.635324	69.709134
968.541064	70.278717	69.714138
968.440732	57.798968	69.719143
967.809486	72.571749	69.724148
967.630063	66.953365	69.729153
967.255702	66.191533	69.734158
966.430561	64.388097	69.739162
965.495955	67.678348	69.744167
965.039131	68.345760	69.749172
963.733502	72.056183	69.754177
963.101657	67.284090	69.759182
962.239363	72.773748	69.764186
962.122878	63.049958	69.769191
961.778662	66.293565	69.774196
960.868154	56.707178	69.779201
960.044333	64.131961	69.784206
959.377713	64.902146	69.789210
959.305108	60.698656	69.794215
958.037743	64.238986	69.799220
957.290689	59.652391	69.804225
956.519038	66.270926	69.809230
956.164987	63.334377	69.814234
956.023150	57.892945	69.819239
954.491990	63.314003	69.824244
954.145205	63.031915	69.829249
953.642110	60.623716	69.834254
952.701879	67.601822	69.839258
951.924068	58.145710	69.844263
951.125501	70.833557	69.849268
950.966667	57.637715	69.854273
950.284224	61.345160	69.859278
949.817943	59.659664	69.864282
948.612601	60.592858	69.869287
947.856666	67.677255	69.874292
947.636222	60.945756	69.879297
947.166860	55.873421	69.884302
946.600209	64.774323	69.889306
945.617264	60.824522	69.894311
944.809927	64.512422	69.899316
944.397876	62.611712	69.904321
943.571385	59.955359	69.909326
942.654918	59.577853	69.914330
942.209357	56.947611	69.919335
941.526714	67.229476	69.924340
941.068141	61.357477	69.929345
940.114274	64.920463	69.934350
938.954779	73.471017	69.939354
938.673348	58.008081	69.944359
938.103073	61.901107	69.949364
937.663435	52.181449	69.954369
937.598743	63.312724	69.959374
936.468417	65.555486	69.964378
935.939797	55.995068	69.969383
935.337355	67.063693	69.974388
934.332210	62.738956	69.979393
933.776938	64.406070	69.984398
932.918406	68.813335	69.989402
932.575845	62.213238	69.994407
931.291147	66.319317	69.999412
930.930862	66.720631	70.004417
930.958749	57.357076	70.009422
930.090155	60.901763	70.014426
929.040968	60.687312	70.019431
928.199615	62.071948	70.024436
927.771650	63.258326	70.029441
927.609692	56.702029	70.034446
926.371070	72.358386	70.039450
925.808109	58.419458	70.044455
925.189384	58.854021	70.049460
924.448562	59.986112	70.054465
923.428568	68.350461	70.059470
922.726671	60.784103	70.064474
922.268525	51.877956	70.069479
921.645076	63.216432	70.074484
921.512953	55.523124	70.079489
920.564252	62.631896	70.084494
919.749457	62.946277	70.089498
919.406028	62.053372	70.094503
918.571070	68.107976	70.099508
917.536904	62.021660	70.104513
916.798211	61.231090	70.109518
916.050706	63.870252	70.114522
915.907074	59.972963	70.119527
915.637265	62.961879	70.124532
914.766958	58.077945	70.129537
914.051382	65.099154	70.134542
913.450125	70.170383	70.139546
912.443496	59.027077	70.144551
911.574112	68.286832	70.149556
910.810273	62.830859	70.154561
910.468948	63.749559	70.159566
910.053150	62.716785	70.164570
909.616236	59.553734	70.169575
908.486136	63.040700	70.174580
907.750451	59.005829	70.179585
907.625160	60.218154	70.184590
906.809731	65.331355	70.189594
905.909001	59.471392	70.194599
905.102577	62.744415	70.199604
904.794460	59.903067	70.204609
904.246148	62.991504	70.209614
902.719661	68.399233	70.214618
902.480266	53.267094	70.219623
901.800408	59.002119	70.224628
901.588395	62.565315	70.229633
900.925343	58.354881	70.234638
899.495361	59.677094	70.239642
899.368596	59.410458	70.244647
898.503499	62.918327	70.249652
898.295913	63.505079	70.254657
897.728988	60.711233	70.259662
896.639029	59.361560	70.264666
896.180604	60.317824	70.269671
895.490702	61.463896	70.274676
894.646341	59.028026	70.279681
893.915541	57.009325	70.284686
893.075823	59.961218	70.289690
893.054956	56.213128	70.294695
892.541778	60.114421	70.299700
891.224504	51.479070	70.304705
890.946393	54.092412	70.309710
889.926248	53.751929	70.314714
889.351265	50.811135	70.319719
888.290523	62.988777	70.324724
887.708125	60.747759	70.329729
887.308088	61.994354	70.334734
886.793425	65.075862	70.339738
886.780648	57.136479	70.344743
885.381797	63.623046	70.349748
884.803903	63.880807	70.354753
884.486253	64.384152	70.359758
883.726504	66.607376	70.364762
882.826187	59.730212	70.369767
881.981730	63.759932	70.374772
881.372610	58.001799	70.379777
881.088771	61.257880	70.384782
879.951558	62.225995	70.389786
879.620274	55.488498	70.394791
878.905647	66.926650	70.399796
878.389446	63.080782	70.404801
877.200428	60.690316	70.409806
876.574501	59.337755	70.414810
876.189921	54.583106	70.419815
875.829638	57.679465	70.424820
874.985918	59.416158	70.429825
874.280722	55.982002	70.434830
873.242386	64.158471	70.439834
872.951273	51.169789	70.444839
872.511041	58.795309	70.449844
871.578642	56.595814	70.454849
870.887514	57.305268	70.459854
869.815755	62.195926	70.464858
869.723554	53.641556	70.469863
869.094896	62.061900	70.474868
868.558263	61.314875	70.479873
867.948083	52.910765	70.484878
867.038362	51.133444	70.489882
866.252153	52.652825	70.494887
865.075990	59.476117	70.499892
864.760097	56.766903	70.504897
864.118785	50.898783	70.509902
863.392214	54.502884	70.514906
863.521636	53.791767	70.519911
862.543748	62.923721	70.524916
861.506609	60.116422	70.529921
861.097307	61.870703	70.534926
860.552616	60.975151	70.539930
859.645502	57.801800	70.544935
859.068402	58.881040	70.549940
858.226656	63.364502	70.554945
857.787678	59.236686	70.559950
857.062620	66.800317	70.564954
856.297948	53.141113	70.569959
855.579841	57.007222	70.574964
855.341916	54.662494	70.579969
854.911585	54.193444	70.584974
853.868492	65.455225	70.589978
853.083237	54.478567	70.594983
852.440945	63.202286	70.599988
852.133311	59.807354	70.604993
850.922090	51.085760	70.609998
850.239710	55.441351	70.615002
849.936684	56.235689	70.620007
849.029316	63.476676	70.625012
847.925514	60.115441	70.630017
847.395312	65.254218	70.635022
846.894793	61.393246	70.640026
846.629025	59.704238	70.645031
846.164170	63.209912	70.650036
845.382188	55.404019	70.655041
844.429324	62.783138	70.660046
843.575277	66.812820	70.665050
843.601786	53.934433	70.670055
842.738688	61.143143	70.675060
841.702615	53.844482	70.680065
841.265604	48.677138	70.685070
840.535970	59.584666	70.690074
840.050857	62.186810	70.695079
838.906975	66.327287	70.700084
838.465365	58.839376	70.705089
838.047847	58.880804	70.710094
837.654116	63.193604	70.715098
836.955643	61.644441	70.720103
835.997257	61.975399	70.725108
835.086570	57.638825	70.730113
834.458944	55.430253	70.735118
833.173455	65.830179	70.740122
832.659868	58.282764	70.745127
832.244616	61.119795	70.750132
832.031090	59.075539	70.755137
831.723245	61.651042	70.760142
831.343122	62.115453	70.765146
830.598517	50.515743	70.770151
829.614062	61.886467	70.775156
828.865618	60.457226	70.780161
827.904830	58.311154	70.785166
827.347365	65.807109	70.790170
826.795383	60.656490	70.795175
825.668115	73.275262	70.800180
824.947250	65.439141	70.805185
824.386553	58.006462	70.810190
823.834167	65.268218	70.815194
823.688788	59.206040	70.820199
823.214285	69.385405	70.825204
822.184897	63.962276	70.830209
821.447592	61.840553	70.835214
820.512295	70.756007	70.840218
820.330716	63.739217	70.845223
819.294405	60.157515	70.850228
818.412614	62.433301	70.855233
818.141425	61.601452	70.860238
817.750291	67.025604	70.865242
816.639633	62.028583	70.870247
815.862371	63.447206	70.875252
815.355111	69.973223	70.880257
815.019075	60.134597	70.885262
814.119314	71.077107	70.890266
813.089481	57.750294	70.895271
812.440739	61.025048	70.900276
812.193211	63.422215	70.905281
812.073703	59.722948	70.910286
810.948758	64.661520	70.915290
810.368679	61.261082	70.920295
809.478945	62.017940	70.925300
808.810706	63.857606	70.930305
808.179708	59.497017	70.935310
807.191542	64.330236	70.940314
806.903729	64.537102	70.945319
806.513889	68.669513	70.950324
805.714741	61.173874	70.955329
804.998872	62.666306	70.960334
803.962560	67.940859	70.965338
803.691059	69.483974	70.970343
803.034910	67.928083	70.975348
802.152130	73.099347	70.980353
801.718945	64.805847	70.985358
800.840107	65.876367	70.990362
800.356960	62.610310	70.995367
799.343580	75.351310	71.000372
798.706390	63.699809	71.005377
798.221282	62.176614	71.010382
797.657344	73.459906	71.015386
797.382536	57.713680	71.020391
796.508928	65.162199	71.025396
795.573766	69.166962	71.030401
795.107195	64.993088	71.035406
793.954135	64.382066	71.040410
793.357292	61.692359	71.045415
792.602075	65.244270	71.050420
792.345279	69.339732	71.055425
792.231486	55.147996	71.060430
791.220069	57.564278	71.065434
790.638984	52.714775	71.070439
790.144795	55.075519	71.075444
788.861830	64.752810	71.080449
787.828294	57.945783	71.085454
787.086831	61.782513	71.090458
786.624891	64.273743	71.095463
785.903442	66.311123	71.100468
785.988233	64.924280	71.105473
785.682211	61.172707	71.110478
784.505299	59.007445	71.115482
784.197128	59.756877	71.120487
783.434763	62.436288	71.125492
782.591231	64.740689	71.130497
781.545113	59.091585	71.135502
780.795590	61.552908	71.140506
780.758402	60.868313	71.145511
779.534110	64.844996	71.150516
778.593468	60.588908	71.155521
778.369020	53.523761	71.160526
777.672321	59.660466	71.165530
777.946743	54.854533	71.170535
776.868809	59.651590	71.175540
775.791852	56.782861	71.180545
775.297768	50.385124	71.185550
774.221753	59.125867	71.190554
773.265361	55.233416	71.195559
772.872051	57.327364	71.200564
772.259288	56.583020	71.205569
772.111439	56.827531	71.210574
771.420054	69.216066	71.215578
771.023911	55.154445	71.220583
770.031256	65.331153	71.225588
769.097049	66.919859	71.230593
768.610879	62.206636	71.235598
767.678723	56.984100	71.240602
766.794488	56.642529	71.245607
766.546510	54.266295	71.250612
765.860441	57.403499	71.255617
765.801630	52.917129	71.260622
764.297027	64.664004	71.265626
763.615382	55.536440	71.270631
763.369253	64.624454	71.275636
762.431542	61.053887	71.280641
762.583315	61.667012	71.285646
761.170684	56.839526	71.290650
760.615377	63.948790	71.295655
760.321780	55.093759	71.300660
759.311025	53.763077	71.305665
758.501686	57.165916	71.310670
757.896137	63.562506	71.315674
757.648481	52.046129	71.320679
756.644945	57.780681	71.325684
755.397923	57.473222	71.330689
755.373132	58.469277	71.335694
754.746042	57.236782	71.340698
754.531076	49.501498	71.345703
753.420368	57.129703	71.350708
752.409365	59.350390	71.355713
752.124117	48.407710	71.360718
751.307429	49.995056	71.365722
751.103294	58.084469	71.370727
750.113960	54.148388	71.375732
749.244115	50.147550	71.380737
749.097905	49.805170	71.385742
747.929508	56.903240	71.390746
747.161178	47.232821	71.395751
746.934068	56.056026	71.400756
746.381482	61.608393	71.405761
745.792421	50.539044	71.410766
744.511107	53.999690	71.415770
744.037791	54.111520	71.420775
743.581416	62.023477	71.425780
742.607880	63.979580	71.430785
741.603515	50.065282	71.435790
740.720889	59.314566	71.440794
740.724731	43.579196	71.445799
740.331148	46.226704	71.450804
740.017613	55.252906	71.455809
739.464148	51.025075	71.460814
738.210743	58.765895	71.465818
737.651555	49.585729	71.470823
736.621464	57.354069	71.475828
735.599835	59.748344	71.480833
735.436409	48.330527	71.485838
734.558762	53.814803	71.490842
734.621460	48.053825	71.495847
734.039285	56.373745	71.500852
732.603283	53.937525	71.505857
732.243026	51.982877	71.510862
731.382955	53.175012	71.515866
731.146530	60.039535	71.520871
730.145234	59.573113	71.525876
729.311327	46.547900	71.530881
729.071368	45.758398	71.535886
728.544533	52.680200	71.540890
727.742427	52.215178	71.545895
726.843276	48.217439	71.550900
726.183091	47.135304	71.555905
726.173721	42.743570	71.560910
724.859200	62.092700	71.565914
724.232473	51.228054	71.570919
723.660887	46.047474	71.575924
723.155516	47.124783	71.580929
722.462852	51.284919	71.585934
721.270714	61.234780	71.590938
720.947477	58.381676	71.595943
720.183858	56.056017	71.600948
720.115218	55.959909	71.605953
718.929684	49.117199	71.610958
717.993802	53.768654	71.615962
717.498995	54.981478	71.620967
717.103814	54.574666	71.625972
716.286171	56.684151	71.630977
715.489119	49.287569	71.635982
715.076319	48.323741	71.640986
714.874894	46.189262	71.645991
714.010441	57.903606	71.650996
712.874867	56.611743	71.656001
712.521403	50.019742	71.661006
711.799202	52.544541	71.666010
711.422019	50.296123	71.671015
710.329009	53.319943	71.676020
709.426978	57.576501	71.681025
709.263589	49.869281	71.686030
708.426527	57.308846	71.691034
707.920747	54.133150	71.696039
706.710038	50.899397	71.701044
706.267898	52.297803	71.706049
706.063486	46.036886	71.711054
705.588829	56.435473	71.716058
704.302551	46.918514	71.721063
703.440450	45.255100	71.726068
702.830527	45.631544	71.731073
702.822484	40.471620	71.736078
702.200616	57.092692	71.741082
701.186157	48.391895	71.746087
700.755156	54.003752	71.751092
699.930561	56.262584	71.756097
699.060694	55.874594	71.761102
698.010260	53.392765	71.766106
697.508516	48.497540	71.771111
697.625497	57.111408	71.776116
696.828214	48.372874	71.781121
695.942231	49.510799	71.786126
694.874809	60.413795	71.791130
694.507180	45.619110	71.796135
694.016371	50.194965	71.801140
693.292422	55.516004	71.806145
692.624605	53.231870	71.811150
691.764105	54.829366	71.816154
691.290483	51.344199	71.821159
690.987508	56.306463	71.826164
690.025599	58.555625	71.831169
689.419042	50.825941	71.836174
688.573693	50.560207	71.841178
688.258587	47.893475	71.846183
687.146716	53.135941	71.851188
686.218244	64.232860	71.856193
686.045326	55.521054	71.861198
685.086642	60.368542	71.866202
684.963753	53.910138	71.871207
684.178388	53.243767	71.876212
682.907557	55.316622	71.881217
682.929825	46.356118	71.886222
682.006815	55.414725	71.891226
681.674146	57.702456	71.896231
680.557703	50.747839	71.901236
679.778072	61.873093	71.906241
679.763040	54.916539	71.911246
678.608740	55.791269	71.916250
678.023770	50.119243	71.921255
677.292583	52.285934	71.926260
676.835681	58.851254	71.931265
676.624067	51.181681	71.936270
675.174431	62.259094	71.941274
674.390741	59.138702	71.946279
674.205144	54.175786	71.951284
673.716454	59.366325	71.956289
673.013230	51.410765	71.961294
671.833383	50.815105	71.966298
671.289583	49.704989	71.971303
670.840058	46.361071	71.976308
669.977531	54.332983	71.981313
669.386159	49.127183	71.986318
668.491929	53.737328	71.991322
668.186331	50.982350	71.996327
668.008736	54.347684	72.001332
666.893103	53.768609	72.006337
666.274139	51.986061	72.011342
665.693587	58.900659	72.016346
664.871108	52.077430	72.021351
663.802340	56.092473	72.026356
662.843529	61.367346	72.031361
662.860953	44.879190	72.036366
662.170010	58.040373	72.041370
661.891200	50.021956	72.046375
661.533363	50.877084	72.051380
660.430548	51.395114	72.056385
659.842694	52.069253	72.061390
658.504192	52.344120	72.066394
657.959565	56.281998	72.071399
657.269536	51.992360	72.076404
656.759664	51.586476	72.081409
656.919492	46.013461	72.086414
655.756625	53.965399	72.091418
655.021663	54.599890	72.096423
654.562070	57.302079	72.101428
653.817399	54.697456	72.106433
652.827669	48.088530	72.111438
652.123724	61.206055	72.116442
651.268159	53.853509	72.121447
651.129807	48.575566	72.126452
650.329976	57.114667	72.131457
649.386704	55.090459	72.136462
648.571891	61.572435	72.141466
647.939107	49.890339	72.146471
648.267343	54.818308	72.151476
647.569763	55.850550	72.156481
646.688367	54.855707	72.161486
645.797669	52.480926	72.166490
645.271697	59.814192	72.171495
644.167962	54.492880	72.176500
643.051067	61.073431	72.181505
642.578565	48.096355	72.186510
642.178994	59.003388	72.191514
642.200142	57.926303	72.196519
641.564488	48.778848	72.201524
640.432113	60.887544	72.206529
639.925318	49.723130	72.211534
639.260877	58.819417	72.216538
638.361910	52.326927	72.221543
637.641395	57.221654	72.226548
636.807848	56.897288	72.231553
636.825734	55.808107	72.236558
635.923170	57.265663	72.241562
635.211871	53.789978	72.246567
634.460483	56.567030	72.251572
633.821415	60.698152	72.256577
633.663959	55.290786	72.261582
631.962551	56.552299	72.266586
631.713853	57.497281	72.271591
631.013794	48.790600	72.276596
630.724165	55.404975	72.281601
630.042316	64.936127	72.286606
628.687237	60.427565	72.291610
628.239141	52.035568	72.296615
627.955573	60.002014	72.301620
627.447009	59.638506	72.306625
626.645817	53.109948	72.311630
625.544921	54.860873	72.316634
625.359218	53.256912	72.321639
624.982878	58.760725	72.326644
623.811387	60.992830	72.331649
623.171923	51.557403	72.336654
622.621918	57.664468	72.341658
622.004475	56.356355	72.346663
621.014961	49.771063	72.351668
620.207047	60.295279	72.356673
619.945004	58.583628	72.361678
619.078869	56.405219	72.366682
618.981704	60.598266	72.371687
618.543747	55.468970	72.376692
617.164333	61.998304	72.381697
616.642563	52.604057	72.386702
616.032602	55.480014	72.391706
615.157245	53.072839	72.396711
613.982284	53.258602	72.401716
613.494094	61.730731	72.406721
613.423898	54.786122	72.411726
612.965318	59.260663	72.416730
612.344077	59.440234	72.421735
611.469361	54.240157	72.426740
610.465714	56.800350	72.431745
610.284243	57.482313	72.436750
609.541121	61.563781	72.441754
608.535915	60.315858	72.446759
608.075945	56.396447	72.451764
607.343138	62.821217	72.456769
607.182475	55.509394	72.461774
605.707641	48.294932	72.466778
605.168301	53.206539	72.471783
604.860403	52.293830	72.476788
604.330839	56.019582	72.481793
603.500253	50.276312	72.486798
602.197013	59.867019	72.491802
601.738980	53.044113	72.496807
601.817000	53.082344	72.501812
601.171802	58.062854	72.506817
600.296211	53.678211	72.511822
599.156734	59.106462	72.516826
598.805054	54.595790	72.521831
598.481007	51.553601	72.526836
597.266456	63.033578	72.531841
596.774863	56.939844	72.536846
596.125532	62.647994	72.541850
595.705227	61.836770	72.546855
594.794824	62.582802	72.551860
593.825205	65.771522	72.556865
593.621714	50.945987	72.561870
593.096055	63.677154	72.566874
592.284129	56.385491	72.571879
591.476049	47.606144	72.576884
590.786815	56.239605	72.581889
590.465115	60.813773	72.586894
589.534819	62.039219	72.591898
588.684240	53.296602	72.596903
588.199531	58.486518	72.601908
587.465340	61.596737	72.606913
587.208051	51.539048	72.611918
586.134257	56.657218	72.616922
585.257746	56.905843	72.621927
584.631570	52.374243	72.626932
584.169182	53.477849	72.631937
584.057481	54.352128	72.636942
583.108630	58.378063	72.641946
582.083387	55.595804	72.646951
581.672831	55.555741	72.651956
580.784237	58.061348	72.656961
580.710264	51.916866	72.661966
579.812963	61.435036	72.666970
578.969953	57.412642	72.671975
578.689743	61.062410	72.676980
577.491740	55.781378	72.681985
576.928004	53.258346	72.686990
576.233067	58.882301	72.691994
575.607903	52.261068	72.696999
575.798770	53.989172	72.702004
573.995776	64.181475	72.707009
573.865943	54.166562	72.712014
572.976655	61.515135	72.717018
572.554517	61.114217	72.722023
571.721294	55.946969	72.727028
570.910403	63.372942	72.732033
570.635855	54.754616	72.737038
569.994464	64.712999	72.742042
568.862617	54.009297	72.747047
568.397568	57.369963	72.752052
567.571832	70.606257	72.757057
567.373101	57.915173	72.762062
566.354930	56.975263	72.767066
565.358790	58.564446	72.772071
564.903888	60.803853	72.777076
564.439611	58.063129	72.782081
563.983172	58.921361	72.787086
563.218023	59.000865	72.792090
562.902596	49.835543	72.797095
562.474365	63.664526	72.802100
561.051544	65.641805	72.807105
560.364229	54.887795	72.812110
559.802243	60.340763	72.817114
559.161153	58.159643	72.822119
558.809199	55.459375	72.827124
557.176190	66.514018	72.832129
556.779565	51.047472	72.837134
556.596458	59.887322	72.842138
556.352650	52.393210	72.847143
555.191561	51.512343	72.852148
554.457406	59.787114	72.857153
553.601293	58.526502	72.862158
553.276139	60.418810	72.867162
552.951209	52.690037	72.872167
551.947017	57.964290	72.877172
551.190656	67.111510	72.882177
550.636415	60.267670	72.887182
549.824970	65.627917	72.892186
549.129095	65.453538	72.897191
548.625442	63.045520	72.902196
547.835581	62.329446	72.907201
547.481941	61.610113	72.912206
547.146654	57.218265	72.917210
545.685063	52.581642	72.922215
545.242009	54.295612	72.927220
544.485791	58.330297	72.932225
544.211408	48.926627	72.937230
542.906505	64.363422	72.942234
542.255266	55.401409	72.947239
542.028371	59.451118	72.952244
541.264787	63.535864	72.957249
541.350918	51.231498	72.962254
540.551023	55.263679	72.967258
539.892928	59.183385	72.972263
538.724654	48.979097	72.977268
537.344719	56.894699	72.982273
536.996558	48.532541	72.987278
536.511251	57.997700	72.992282
535.751122	55.037609	72.997287
535.604719	52.241521	73.002292
534.654264	59.823776	73.007297
534.065853	59.684321	73.012302
533.330910	56.330708	73.017306
533.105627	59.815608	73.022311
532.591571	50.364967	73.027316
531.384651	59.208648	73.032321
530.904000	46.799038	73.037326
530.227672	49.330769	73.042330
529.529561	55.791027	73.047335
528.743844	48.965153	73.052340
527.793586	62.509869	73.057345
527.583536	54.065783	73.062350
527.245126	54.481015	73.067354
525.582492	56.540673	73.072359
525.354695	50.242507	73.077364
524.643356	54.508167	73.082369
524.435147	55.038275	73.087374
523.443927	60.155930	73.092378
522.324261	58.809583	73.097383
522.030280	54.419045	73.102388
521.598660	58.723722	73.107393
521.622833	54.276190	73.112398
520.417971	53.962134	73.117402
519.596789	58.257911	73.122407
518.789655	46.846497	73.127412
518.298077	54.153796	73.132417
517.441243	57.422345	73.137422
516.410654	66.581721	73.142426
516.183918	63.030451	73.147431
515.844423	52.758790	73.152436
515.053218	57.461380	73.157441
514.254892	59.966821	73.162446
513.410636	62.159457	73.167450
512.772323	63.524494	73.172455
512.819201	56.226928	73.177460
511.111864	63.179144	73.182465
510.661023	50.876752	73.187470
510.362007	60.340622	73.192474
509.725841	60.949953	73.197479
509.258418	52.743995	73.202484
507.822815	56.984700	73.207489
507.781943	56.430009	73.212494
507.201029	54.387551	73.217498
506.573414	61.241864	73.222503
505.796517	67.236865	73.227508
504.803524	61.634624	73.232513
504.657090	59.554483	73.237518
504.004797	56.799573	73.242522
503.142106	59.799399	73.247527
502.491286	54.204148	73.252532
501.759695	59.639992	73.257537
500.927441	54.899975	73.262542
500.019870	56.022484	73.267546
498.984254	58.769164	73.272551
498.793328	49.257589	73.277556
498.325222	60.702253	73.282561
498.028333	53.374303	73.287566
497.486878	57.800562	73.292570
496.363024	61.267780	73.297575
495.608497	56.345069	73.302580
495.328122	59.884482	73.307585
494.765211	56.008306	73.312590
493.815284	55.797149	73.317594
493.095820	57.156197	73.322599
492.951080	51.910828	73.327604
491.375637	61.680570	73.332609
490.998956	52.791528	73.337614
490.108919	53.428696	73.342618
489.740996	60.348869	73.347623
489.734799	56.753004	73.352628
488.412737	60.619237	73.357633
487.896796	57.993995	73.362638
487.349861	54.701906	73.367642
486.642482	53.266232	73.372647
485.726214	53.483379	73.377652
484.586635	58.034902	73.382657
484.351301	52.747197	73.387662
484.002770	54.433501	73.392666
483.407320	64.671583	73.397671
482.530571	52.055436	73.402676
481.926186	67.800113	73.407681
481.579324	63.873746	73.412686
480.697632	63.713223	73.417690
479.698777	62.320838	73.422695
479.271063	55.343321	73.427700
478.549489	55.685569	73.432705
478.267043	51.901908	73.437710
477.550947	55.704712	73.442714
476.280188	60.570454	73.447719
475.976590	56.678198	73.452724
475.504790	63.321609	73.457729
474.605043	57.176245	73.462734
473.597398	58.038740	73.467738
473.001444	66.015544	73.472743
473.032623	49.704998	73.477748
471.902706	64.519423	73.482753
471.067172	62.550659	73.487758
470.643158	62.378717	73.492762
470.283671	63.399715	73.497767
469.865495	62.425747	73.502772
468.400747	57.644595	73.507777
467.716892	50.403542	73.512782
467.181595	53.103630	73.517786
466.863864	63.234384	73.522791
466.583383	58.983629	73.527796
465.212750	57.617373	73.532801
464.840257	54.865200	73.537806
464.331364	63.342220	73.542810
463.289628	55.361826	73.547815
462.594485	60.315630	73.552820
462.063239	61.237840	73.557825
461.687921	52.265010	73.562830
460.541937	56.311358	73.567834
459.541781	54.023477	73.572839
459.209396	58.553625	73.577844
458.640900	62.749233	73.582849
458.439500	56.208748	73.587854
457.906501	58.574157	73.592858
456.739468	60.547005	73.597863
456.106239	54.613073	73.602868
455.497449	54.325496	73.607873
454.947159	54.459108	73.612878
453.958271	54.331445	73.617882
453.365950	54.460716	73.622887
453.093689	48.929742	73.627892
452.279119	56.189169	73.632897
451.376884	58.376870	73.637902
450.884834	60.581213	73.642906
450.115217	62.208463	73.647911
450.106708	61.501959	73.652916
448.749713	60.748553	73.657921
448.317314	56.689167	73.662926
447.604900	57.007887	73.667930
447.003944	64.077161	73.672935
446.195521	53.421344	73.677940
444.862361	58.046307	73.682945
444.609084	50.367643	73.687950
444.849297	51.258391	73.692954
443.623560	53.302100	73.697959
442.652757	49.396319	73.702964
441.663273	59.582073	73.707969
441.529034	48.405669	73.712974
441.191135	56.409161	73.717978
440.418544	61.391081	73.722983
439.775250	56.598900	73.727988
438.620901	72.981581	73.732993
438.251753	53.522558	73.737998
438.166934	52.804560	73.743002
436.944461	66.069402	73.748007
436.645117	58.339728	73.753012
435.796215	54.077055	73.758017
434.677156	59.705546	73.763022
433.905357	56.121295	73.768026
433.058491	56.838338	73.773031
433.007897	53.117086	73.778036
432.457590	64.544893	73.783041
432.259161	61.602561	73.788046
431.280242	58.368285	73.793050
430.216613	58.594742	73.798055
430.109205	56.866359	73.803060
429.118661	55.811718	73.808065
428.325892	51.278328	73.813070
427.729675	63.044612	73.818074
427.266889	61.229356	73.823079
426.711386	61.396920	73.828084
425.484728	63.227896	73.833089
425.296663	61.291591	73.838094
424.852671	60.072586	73.843098
423.522306	64.487380	73.848103
422.668884	59.779151	73.853108
421.805953	68.249518	73.858113
421.695859	55.143795	73.863118
421.431193	56.133919	73.868122
420.502868	56.118045	73.873127
419.599811	49.976389	73.878132
418.967089	62.704128	73.883137
418.509531	63.523140	73.888142
418.344295	64.107912	73.893146
417.270579	65.550241	73.898151
416.613690	61.739525	73.903156
415.978499	69.572780	73.908161
415.641396	64.719194	73.913166
414.476261	60.038565	73.918170
413.175210	62.851232	73.923175
413.108165	56.866511	73.928180
412.895709	60.999081	73.933185
412.160744	58.672113	73.938190
411.382158	60.002757	73.943194
410.684082	56.818353	73.948199
410.131244	51.814648	73.953204
408.624244	59.479324	73.958209
408.222278	57.107174	73.963214
407.944010	54.634888	73.968218
407.273202	65.801203	73.973223
406.933680	51.044701	73.978228
405.987113	54.707631	73.983233
405.271338	57.363952	73.988238
404.718475	54.903887	73.993242
403.784980	60.422394	73.998247
403.447843	50.721247	74.003252
402.233578	55.109662	74.008257
402.054841	62.580014	74.013262
401.307580	56.717888	74.018266
400.505706	60.045524	74.023271
399.701566	53.831340	74.028276
399.016506	64.399106	74.033281
398.525396	59.902807	74.038286
398.136362	50.345551	74.043290
397.927890	55.277003	74.048295
396.945856	46.631118	74.053300
396.178766	50.456260	74.058305
395.631015	54.525569	74.063310
394.482730	59.192057	74.068314
393.502425	64.653373	74.073319
393.611596	53.166945	74.078324
392.935734	52.316060	74.083329
392.231942	60.407830	74.088334
391.128184	51.431259	74.093338
390.312964	55.290882	74.098343
390.356836	51.254956	74.103348
389.761296	58.536263	74.108353
388.913888	54.927808	74.113358
388.326061	52.386587	74.118362
387.280991	62.089206	74.123367
386.939228	44.625435	74.128372
385.484998	58.024994	74.133377
385.179958	56.627732	74.138382
384.882931	55.454699	74.143386
384.324674	58.820785	74.148391
383.678602	50.608642	74.153396
382.593189	61.535104	74.158401
381.913148	59.681941	74.163406
381.664079	57.555089	74.168410
380.938305	57.628375	74.173415
380.141742	60.508891	74.178420
379.457139	62.496352	74.183425
379.028015	56.902078	74.188430
378.656410	60.580619	74.193434
377.171116	57.518532	74.198439
376.693708	55.249876	74.203444
375.942108	64.210290	74.208449
375.570057	53.743579	74.213454
375.117430	59.056146	74.218458
374.119763	63.222398	74.223463
373.991048	59.236054	74.228468
373.381583	62.383222	74.233473
372.512962	60.169031	74.238478
371.727265	53.458331	74.243482
370.749134	58.963461	74.248487
370.309796	52.818883	74.253492
368.869854	51.017449	74.258497
368.404754	51.159580	74.263502
367.992910	49.720997	74.268506
367.617759	62.525962	74.273511
367.378035	62.966489	74.278516
367.163449	55.601794	74.283521
365.705199	55.017537	74.288526
365.129948	57.676704	74.293530
364.291078	62.997216	74.298535
363.756279	59.996538	74.303540
362.478049	56.160289	74.308545
362.090160	57.387678	74.313550
361.849249	56.551058	74.318554
361.123148	56.045658	74.323559
360.395401	53.714403	74.328564
359.728225	52.931529	74.333569
359.031341	56.379638	74.338574
358.780679	51.166937	74.343578
357.033769	72.179414	74.348583
356.688302	61.065067	74.353588
355.891541	63.223375	74.358593
355.430016	65.432332	74.363598
355.583167	63.277646	74.368602
354.742505	57.807317	74.373607
353.970243	51.908194	74.378612
353.296551	57.956167	74.383617
352.507297	61.130417	74.388622
351.929805	57.384338	74.393626
351.013821	58.547665	74.398631
350.699883	50.976459	74.403636
350.002345	57.337316	74.408641
348.503173	54.151304	74.413646
347.992048	55.541840	74.418650
347.290918	52.537717	74.423655
347.383682	53.499264	74.428660
346.691137	54.794137	74.433665
346.509022	56.986946	74.438670
345.485878	62.996002	74.443674
344.485088	60.484342	74.448679
344.115919	54.435819	74.453684
342.937509	48.555705	74.458689
342.206697	57.814007	74.463694
342.038654	53.524853	74.468698
341.402279	61.823508	74.473703
340.791337	53.217848	74.478708
339.648268	59.334329	74.483713
339.068524	54.139388	74.488718
338.921120	51.952184	74.493722
337.557271	60.179132	74.498727
336.825682	50.886228	74.503732
336.222847	56.598056	74.508737
335.741275	60.858679	74.513742
335.413939	55.106266	74.518746
334.864705	61.175407	74.523751
334.323853	47.132268	74.528756
333.166586	53.217896	74.533761
332.704037	57.712031	74.538766
332.179545	57.821057	74.543770
330.615876	59.977032	74.548775
330.116215	60.783848	74.553780
329.896331	61.538184	74.558785
329.632261	61.277695	74.563790
329.280862	59.260200	74.568794
327.934783	59.246293	74.573799
327.375123	56.443554	74.578804
326.598408	64.326188	74.583809
326.267597	60.163903	74.588814
325.314890	67.186763	74.593818
324.505937	64.002711	74.598823
324.068909	55.821922	74.603828
323.523027	61.824298	74.608833
322.483327	64.760933	74.613838
321.775126	62.167952	74.618842
321.361472	62.451703	74.623847
321.226668	70.858076	74.628852
320.251116	62.504501	74.633857
319.073696	69.033325	74.638862
319.033585	57.529694	74.643866
318.088158	59.776366	74.648871
317.508675	53.709332	74.653876
316.589861	60.130700	74.658881
315.896387	58.746478	74.663886
315.384577	61.362427	74.668890
314.926941	67.153621	74.673895
314.294119	56.670144	74.678900
313.442162	60.671264	74.683905
312.677567	58.341166	74.688910
312.379260	56.260019	74.693914
310.988820	65.642401	74.698919
310.452600	53.378913	74.703924
309.810789	59.016534	74.708929
309.638460	62.519815	74.713934
309.579606	57.180351	74.718938
308.453648	66.184683	74.723943
307.666449	61.081166	74.728948
307.021481	57.932483	74.733953
306.107787	56.704794	74.738958
304.991929	56.627393	74.743962
304.185829	62.895180	74.748967
303.905592	59.409237	74.753972
303.803942	59.613294	74.758977
303.173056	63.571295	74.763982
303.051557	59.257377	74.768986
301.890344	62.459395	74.773991
301.348379	62.661100	74.778996
299.954058	66.977341	74.784001
299.009828	61.435232	74.789006
298.788028	59.609973	74.794010
298.084191	58.006635	74.799015
297.722739	54.049514	74.804020
296.874196	60.448648	74.809025
295.769237	56.327772	74.814030
295.458591	55.702549	74.819034
294.922752	62.722043	74.824039
295.011293	50.262778	74.829044
293.917702	49.942135	74.834049
293.047789	61.578596	74.839054
292.947858	51.778163	74.844058
291.519680	54.402996	74.849063
291.063362	55.847885	74.854068
290.435474	50.413053	74.859073
289.859457	55.335289	74.864078
288.817458	47.323492	74.869082
288.294689	54.344054	74.874087
287.563447	52.344541	74.879092
287.369928	60.818614	74.884097
286.670930	56.913726	74.889102
285.604770	50.957401	74.894106
284.733483	58.579151	74.899111
284.250600	52.132452	74.904116
283.834564	53.112026	74.909121
282.727106	51.703922	74.914126
282.215137	46.103958	74.919130
281.345076	58.076335	74.924135
281.307468	52.683025	74.929140
281.208357	57.713743	74.934145
279.909169	54.081156	74.939150
278.961841	54.681801	74.944154
277.996823	52.448321	74.949159
278.025757	48.761711	74.954164
277.228390	61.804295	74.959169
276.188562	60.533646	74.964174
276.032781	51.379209	74.969178
275.477917	60.166352	74.974183
274.651674	58.927887	74.979188
273.978698	58.928133	74.984193
272.994838	60.594319	74.989198
272.968186	55.897854	74.994202
271.308609	59.888963	74.999207
270.762004	59.895871	75.004212
270.051033	53.266340	75.009217
269.673951	57.048267	75.014222
269.590437	52.045477	75.019226
268.610802	60.946070	75.024231
267.802266	53.939430	75.029236
267.400134	61.101616	75.034241
266.865548	63.919902	75.039246
266.524641	56.135390	75.044250
265.222449	59.739945	75.049255
264.659112	48.081621	75.054260
263.903080	52.960019	75.059265
262.880377	55.539151	75.064270
262.349152	53.291716	75.069274
261.656118	62.780558	75.074279
261.483176	61.128865	75.079284
260.953311	58.064349	75.084289
259.806573	59.642965	75.089294
259.366689	51.170914	75.094298
258.879140	61.814445	75.099303
258.227594	50.460345	75.104308
257.158567	51.660719	75.109313
256.463150	61.093170	75.114318
256.094449	54.705546	75.119322
255.484483	58.179248	75.124327
254.809898	49.646844	75.129332
253.594414	60.368578	75.134337
252.903778	55.175572	75.139342
252.802456	51.236915	75.144346
252.354796	57.053330	75.149351
251.687993	54.043764	75.154356
250.853061	61.251296	75.159361
250.211733	56.706444	75.164366
249.433168	56.326136	75.169370
248.074142	64.784173	75.174375
247.693153	51.114546	75.179380
247.133021	54.473072	75.184385
246.726264	52.680461	75.189390
246.714968	55.601403	75.194394
245.319437	63.838179	75.199399
244.478203	57.189998	75.204404
244.105524	56.879025	75.209409
243.651156	60.551851	75.214414
242.996338	53.035013	75.219418
241.994355	55.333305	75.224423
241.769931	52.688455	75.229428
241.422714	54.562237	75.234433
240.124600	56.057763	75.239438
239.764487	51.545353	75.244442
238.900463	49.842992	75.249447
238.062283	44.802828	75.254452
237.036448	52.423995	75.259457
236.303878	54.092710	75.264462
235.830231	46.266295	75.269466
235.297787	58.377244	75.274471
235.124775	55.648503	75.279476
234.885840	52.780463	75.284481
233.579637	56.748372	75.289486
233.040565	52.983586	75.294490
232.552505	55.898538	75.299495
231.548997	47.043270	75.304500
230.936531	64.352012	75.309505
230.041463	62.848568	75.314510
229.816890	54.285424	75.319514
228.579195	57.017119	75.324519
227.836071	56.224313	75.329524
227.392517	58.413079	75.334529
226.915249	54.886022	75.339534
226.715968	58.636453	75.344538
225.842281	61.824202	75.349543
225.106752	52.016305	75.354548
224.516200	57.156914	75.359553
223.295339	65.323274	75.364558
222.736877	53.957498	75.369562
221.885330	59.445650	75.374567
221.601707	56.412847	75.379572
221.286982	56.053213	75.384577
220.732954	55.268108	75.389582
219.741979	47.312866	75.394586
218.549343	52.290849	75.399591
218.495457	51.836011	75.404596
218.156609	53.467188	75.409601
217.218866	55.017232	75.414606
216.803084	54.691058	75.419610
215.636911	52.948570	75.424615
214.607674	59.808621	75.429620
213.970103	57.240684	75.434625
213.406291	62.682964	75.439630
212.945702	48.776883	75.444634
212.456887	60.354176	75.449639
211.975381	52.216780	75.454644
211.499463	54.136318	75.459649
210.415327	60.270262	75.464654
210.087896	54.510005	75.469658
209.147772	57.284150	75.474663
207.991490	53.002767	75.479668
207.615236	54.557907	75.484673
207.031723	57.790859	75.489678
207.030613	53.924536	75.494682
205.703550	59.043809	75.499687
204.917423	56.931647	75.504692
204.366795	56.035616	75.509697
203.857514	55.457846	75.514702
203.560567	54.152360	75.519706
202.627878	60.544436	75.524711
201.901734	52.761440	75.529716
201.454060	51.445295	75.534721
199.875759	49.667602	75.539726
199.377178	52.656776	75.544730
198.493589	58.769787	75.549735
198.492309	50.224666	75.554740
198.027355	56.589471	75.559745
197.859243	61.325262	75.564750
197.160077	55.911284	75.569754
196.008629	54.338346	75.574759
195.643920	55.733952	75.579764
194.339336	59.059802	75.584769
193.734131	53.274452	75.589774
193.574859	56.968042	75.594778
192.875057	58.724584	75.599783
191.865155	50.132129	75.604788
191.076372	52.166211	75.609793
190.533328	48.506150	75.614798
190.375446	47.631079	75.619802
189.334256	59.315372	75.624807
188.447176	58.472992	75.629812
188.245643	50.907552	75.634817
187.360700	59.182788	75.639822
186.663211	42.671518	75.644826
185.795702	56.641508	75.649831
184.965572	49.783428	75.654836
184.583076	55.955314	75.659841
184.309841	55.819304	75.664846
183.232850	51.457483	75.669850
182.268103	57.261740	75.674855
181.799959	52.496907	75.679860
181.466823	53.020155	75.684865
180.997286	57.777200	75.689870
180.365150	50.920666	75.694874
179.442541	57.095097	75.699879
178.988560	50.635935	75.704884
177.916723	52.108027	75.709889
176.947011	59.321299	75.714894
176.582395	52.013677	75.719898
175.778551	54.786603	75.724903
175.703122	56.142392	75.729908
175.069011	54.785017	75.734913
174.105016	62.005265	75.739918
173.708546	51.134073	75.744922
172.998687	49.771431	75.749927
171.671133	58.609257	75.754932
171.058005	55.110186	75.759937
170.465251	60.241696	75.764942
170.285212	53.477077	75.769946
169.626372	63.706383	75.774951
168.969544	48.674124	75.779956
168.249604	53.985185	75.784961
167.284451	55.627928	75.789966
167.235426	42.903613	75.794970
166.157167	56.716402	75.799975
165.091248	49.377110	75.804980
164.921088	54.808663	75.809985
164.592576	58.261158	75.814990
164.025327	51.944640	75.819994
162.748691	61.521829	75.824999
162.128054	55.885606	75.830004
161.639033	53.240381	75.835009
160.740356	57.906587	75.840014
159.770070	56.301625	75.845018
158.894978	62.274522	75.850023
158.545524	67.860826	75.855028
158.583743	56.242227	75.860033
157.881569	55.698380	75.865038
157.483951	61.450058	75.870042
156.534728	57.586692	75.875047
155.655718	53.485050	75.880052
154.852692	49.036977	75.885057
153.911293	50.625475	75.890062
153.419633	48.321295	75.895066
153.043010	55.604000	75.900071
152.557053	53.303641	75.905076
151.923928	50.616743	75.910081
151.100122	49.303817	75.915086
150.712239	50.209537	75.920090
149.802887	52.647635	75.925095
149.159402	58.272940	75.930100
148.589297	52.680704	75.935105
147.573490	59.712102	75.940110
146.781055	54.098549	75.945114
145.569592	56.494939	75.950119
145.297018	56.712067	75.955124
145.066783	49.543874	75.960129
144.506202	54.228709	75.965134
144.201932	42.005572	75.970138
143.121948	58.710776	75.975143
142.419902	50.690573	75.980148
142.022038	40.841486	75.985153
140.818542	52.209472	75.990158
140.296999	45.898291	75.995162
139.384296	53.520373	76.000167
138.613076	51.621901	76.005172
138.283607	46.751387	76.010177
137.968876	54.103070	76.015182
137.857799	55.207501	76.020186
136.552042	58.691262	76.025191
135.806682	48.486002	76.030196
135.265906	55.302876	76.035201
133.821911	59.742241	76.040206
133.667750	55.799403	76.045210
132.914201	53.089137	76.050215
132.711746	49.518279	76.055220
132.397357	51.434147	76.060225
130.946096	59.526898	76.065230
130.405789	52.091187	76.070234
129.995729	52.139430	76.075239
129.423390	51.289457	76.080244
128.476886	52.244843	76.085249
127.771539	53.045076	76.090254
127.275776	42.298548	76.095258
126.639152	48.796392	76.100263
125.586288	39.428659	76.105268
125.153004	45.074058	76.110273
124.553047	42.916467	76.115278
124.194158	39.490409	76.120282
122.813686	53.972723	76.125287
122.150360	51.607617	76.130292
121.328825	48.364148	76.135297
120.759160	54.624236	76.140302
120.996918	58.983063	76.145306
120.286948	54.510700	76.150311
119.868487	51.294414	76.155316
119.012822	46.733325	76.160321
118.125561	46.868712	76.165326
117.397038	44.621240	76.170330
116.401324	57.343821	76.175335
115.956805	51.681104	76.180340
115.809524	53.382667	76.185345
114.456651	55.787431	76.190350
113.814467	41.192838	76.195354
113.079786	44.607609	76.200359
112.863072	55.286803	76.205364
112.381694	58.605987	76.210369
111.143618	59.849154	76.215374
110.457327	44.252343	76.220378
110.077829	56.070826	76.225383
109.544075	53.639328	76.230388
108.349454	49.531270	76.235393
107.650382	58.256277	76.240398
107.655285	45.285248	76.245402
106.907287	56.593221	76.250407
106.458251	54.121405	76.255412
105.827301	54.638542	76.260417
104.568735	52.475606	76.265422
104.408556	40.431351	76.270426
103.128541	55.982596	76.275431
102.542297	59.105618	76.280436
102.120289	51.479161	76.285441
101.597964	49.048996	76.290446
101.253961	44.133500	76.295450
100.143460	53.315207	76.300455
99.505159	41.577441	76.305460
99.338967	46.054302	76.310465
97.625648	55.761084	76.315470
97.066999	46.715087	76.320474
96.545884	54.817202	76.325479
96.049256	45.559464	76.330484
95.681513	42.095399	76.335489
94.715094	55.081393	76.340494
94.102779	55.819489	76.345498
93.524827	51.371813	76.350503
92.758990	57.754657	76.355508
92.506944	45.534240	76.360513
91.189397	56.447352	76.365518
90.919291	45.691652	76.370522
90.204606	53.539211	76.375527
89.779084	53.764969	76.380532
89.165768	43.718445	76.385537
87.752886	56.042366	76.390542
87.574162	57.326322	76.395546
87.250372	51.444083	76.400551
86.497484	53.062464	76.405556
85.465045	46.531584	76.410561
84.617862	50.421623	76.415566
84.408182	43.108240	76.420570
83.943188	52.595429	76.425575
82.772722	56.641111	76.430580
82.163186	45.849663	76.435585
81.404195	55.525671	76.440590
81.008566	59.838858	76.445594
80.374696	47.693533	76.450599
79.419159	56.692839	76.455604
79.107577	53.312857	76.460609
78.451651	61.031201	76.465614
77.988471	50.533377	76.470618
77.189471	53.028016	76.475623
76.446709	54.190622	76.480628
76.054169	48.910710	76.485633
74.746630	52.304898	76.490638
73.974673	48.388066	76.495642
73.238734	51.574392	76.500647
73.015070	50.676705	76.505652
72.655332	58.614313	76.510657
71.770181	58.486030	76.515662
71.128757	52.920961	76.520666
70.280244	50.328365	76.525671
69.851014	56.268018	76.530676
69.433939	48.725939	76.535681
68.061166	58.558197	76.540686
67.758994	47.127949	76.545690
67.098738	57.791155	76.550695
66.391043	55.239177	76.555700
65.996824	53.783645	76.560705
64.613133	56.778401	76.565710
64.487255	45.870392	76.570714
64.144667	48.823669	76.575719
62.861338	55.175519	76.580724
62.291582	58.247034	76.585729
61.532088	62.689223	76.590734
61.375496	50.224927	76.595738
60.812980	54.668812	76.600743
60.015393	52.709916	76.605748
59.546736	53.075023	76.610753
58.963254	58.466848	76.615758
57.882604	58.711951	76.620762
57.174668	56.599985	76.625767
56.397889	62.609270	76.630772
56.246971	48.956624	76.635777
54.648088	53.822859	76.640782
54.129438	48.572528	76.645786
53.596468	57.624289	76.650791
53.261348	61.636091	76.655796
52.951460	47.149365	76.660801
51.698428	53.387577	76.665806
50.934959	50.377723	76.670810
50.403659	53.217601	76.675815
50.108531	50.905751	76.680820
49.908174	46.815752	76.685825
48.645039	56.072288	76.690830
48.121144	53.872621	76.695834
47.131433	52.108378	76.700839
46.665402	47.330628	76.705844
45.877844	37.703001	76.710849
45.077220	47.880815	76.715854
45.009241	41.759089	76.720858
44.306652	51.377220	76.725863
43.126197	47.653291	76.730868
42.601746	40.163044	76.735873
41.622500	48.499087	76.740878
41.761071	47.559393	76.745882
40.668512	46.330377	76.750887
39.960720	47.837498	76.755892
39.422525	47.627075	76.760897
38.845364	53.437363	76.765902
38.260784	40.901000	76.770906
37.218157	49.139922	76.775911
36.647243	52.897599	76.780916
36.538732	41.613091	76.785921
35.132168	51.365593	76.790926
34.352248	46.298871	76.795930
33.637455	49.833494	76.800935
33.432734	46.228318	76.805940
33.281568	44.090626	76.810945
32.187832	47.215765	76.815950
31.379465	42.122044	76.820954
30.839556	42.094822	76.825959
30.531981	38.982294	76.830964
29.547816	41.340903	76.835969
28.338411	43.456321	76.840974
27.927225	45.685684	76.845978
27.591930	47.593860	76.850983
26.525617	44.995023	76.855988
25.982686	43.411834	76.860993
25.264088	54.011811	76.865998
25.014108	46.257009	76.871002
24.481071	43.254563	76.876007
23.728418	46.285872	76.881012
22.557307	42.241921	76.886017
22.174822	40.462829	76.891022
21.664039	41.979529	76.896026
20.891594	39.269164	76.901031
19.584942	44.599732	76.906036
19.285684	40.020892	76.911041
18.448692	45.129884	76.916046
18.436813	37.865386	76.921050
18.269750	36.416206	76.926055
16.892448	40.341943	76.931060
16.405934	39.636003	76.936065
15.739679	53.605459	76.941070
15.218350	44.015797	76.946074
14.175289	49.485671	76.951079
13.605569	41.720379	76.956084
13.532427	37.285242	76.961089
12.060137	44.665464	76.966094
11.440774	34.465399	76.971098
10.931143	46.626334	76.976103
10.393649	40.600010	76.981108
9.479210	43.557784	76.986113
8.633640	42.032339	76.991118
8.563422	29.472291	76.996122
8.081078	37.289101	77.001127
6.922712	41.261919	77.006132
6.355233	41.245410	77.011137
5.487289	47.762831	77.016142
5.188065	38.248131	77.021147
4.901102	36.045374	77.026151
3.590850	39.671839	77.031156
3.364299	31.000259	77.036161