Fri Mar 05 19:30:12 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.106300	96.366300	0.000000
-0.435439	89.362032	0.005005
-1.429756	64.212182	0.010010
-2.616011	12.967654	0.015014
-6.285688	-6.942487	0.020019
-11.579928	-22.759911	0.025024
-16.981146	-21.666439	0.030029
-21.972106	-20.430239	0.035034
-25.943922	-24.371281	0.040038
-29.627675	-14.585230	0.045043
-33.257752	-16.931289	0.050048
-36.611183	-22.823866	0.055053
-40.568285	-8.950906	0.060058
-43.986909	-18.108392	0.065062
-48.049983	-12.227819	0.070067
-51.706001	-22.586899	0.075072
-55.213845	-15.698913	0.080077
-59.402165	-19.220588	0.085082
-62.930638	-23.911956	0.090086
-66.890556	-15.688702	0.095091
-70.702548	-15.726999	0.100096
-74.145130	-25.621776	0.105101
-78.197947	-15.406196	0.110106
-81.624326	-12.585493	0.115110
-85.617158	-23.901605	0.120115
-89.530425	-16.332306	0.125120
-93.242739	-16.075811	0.130125
-97.049217	-13.471987	0.135130
-100.543133	-22.188443	0.140134
-103.956732	-18.147617	0.145139
-108.110721	-10.992464	0.150144
-112.151563	-14.898697	0.155149
-116.134467	-9.067075	0.160154
-119.360820	-12.144466	0.165158
-123.052376	-14.977317	0.170163
-126.860768	-15.577491	0.175168
-130.301462	-24.901630	0.180173
-134.538113	-19.379576	0.185178
-138.077833	-22.498402	0.190182
-142.328936	-16.877834	0.195187
-146.044056	-15.072253	0.200192
-149.820308	-12.868982	0.205197
-154.014421	-15.430785	0.210202
-157.264205	-12.409498	0.215206
-160.694888	-14.771411	0.220211
-164.965917	-19.744681	0.225216
-168.726298	-23.533142	0.230221
-172.474378	-10.082846	0.235226
-175.909792	-18.231363	0.240230
-179.544535	-17.331106	0.245235
-183.433615	-12.681288	0.250240
-187.170238	-22.120543	0.255245
-191.472083	-13.593374	0.260250
-194.868142	-21.519484	0.265254
-198.612671	-17.261716	0.270259
-202.482529	-13.802373	0.275264
-205.796030	-19.568615	0.280269
-210.134236	-14.135880	0.285274
-213.805189	-22.208901	0.290278
-217.645548	-14.759849	0.295283
-221.549740	-13.841758	0.300288
-224.784366	-18.977169	0.305293
-228.715118	-15.661031	0.310298
-232.336628	-20.313641	0.315302
-235.600969	-12.032405	0.320307
-239.396440	-16.248814	0.325312
-243.008788	-19.570355	0.330317
-247.362266	-7.620770	0.335322
-251.167844	-16.936954	0.340326
-255.034334	-11.339733	0.345331
-258.907328	-9.254894	0.350336
-262.435268	-9.201031	0.355341
-266.313523	-8.663897	0.360346
-270.105632	-21.563431	0.365350
-273.740832	-8.682938	0.370355
-277.692908	-15.162431	0.375360
-281.171796	-19.760461	0.380365
-284.999710	-7.297041	0.385370
-288.797648	-21.627476	0.390374
-292.677977	-13.086995	0.395379
-296.634212	-16.099674	0.400384
-300.194799	-25.347645	0.405389
-303.983430	-5.133499	0.410394
-307.563509	-15.307172	0.415398
-311.324849	-13.978081	0.420403
-315.101930	-15.704159	0.425408
-318.620115	-13.399900	0.430413
-322.677299	-7.445706	0.435418
-326.703372	-20.146946	0.440422
-331.192788	-18.260053	0.445427
-334.827510	-17.096218	0.450432
-338.106205	-21.377617	0.455437
-341.789998	-4.617883	0.460442
-345.093570	-10.303513	0.465446
-348.608847	-14.886172	0.470451
-352.640624	-17.746349	0.475456
-356.287771	-25.149585	0.480461
-360.392031	-16.218441	0.485466
-364.194585	-12.886282	0.490470
-368.295165	-16.536533	0.495475
-372.015873	-24.964049	0.500480
-375.128093	-25.531474	0.505485
-379.173567	-13.786965	0.510490
-382.996577	-15.530833	0.515494
-386.655284	-16.443073	0.520499
-390.486411	-12.936002	0.525504
-394.179308	-20.746610	0.530509
-398.083465	-16.910903	0.535514
-401.800019	-16.833028	0.540518
-405.776542	-17.345989	0.545523
-409.385216	-13.197902	0.550528
-412.506048	-26.425141	0.555533
-416.624827	-14.974795	0.560538
-420.390436	-23.368254	0.565542
-424.262313	-24.241666	0.570547
-427.994393	-17.957597	0.575552
-431.865131	-21.447319	0.580557
-435.613208	-18.869641	0.585562
-439.134408	-19.420561	0.590566
-442.931845	-24.088903	0.595571
-446.585985	-19.564499	0.600576
-450.263522	-24.909558	0.605581
-454.484521	-12.871976	0.610586
-458.354587	-13.739315	0.615590
-462.035876	-12.900585	0.620595
-465.697472	-15.937954	0.625600
-468.986377	-24.388535	0.630605
-473.261950	-20.911284	0.635610
-476.953025	-21.815062	0.640614
-481.155541	-16.824565	0.645619
-484.817136	-19.056089	0.650624
-487.842641	-14.274053	0.655629
-491.728674	-14.033354	0.660634
-495.696371	-10.283536	0.665638
-499.410167	-18.804988	0.670643
-503.330094	-14.602323	0.675648
-507.069041	-25.226529	0.680653
-510.811902	-16.245630	0.685658
-514.582142	-20.899275	0.690662
-518.161523	-20.988205	0.695667
-522.259224	-11.900151	0.700672
-525.689565	-17.626769	0.705677
-529.702207	-15.462424	0.710682
-533.413354	-14.252967	0.715686
-537.209699	-15.212376	0.720691
-541.014513	-10.542339	0.725696
-544.357355	-14.232888	0.730701
-548.382365	-8.428543	0.735706
-551.793116	-19.466220	0.740710
-555.702521	-22.692518	0.745715
-560.166640	-8.007673	0.750720
-563.501181	-16.165405	0.755725
-567.460345	-17.144488	0.760730
-570.852737	-17.179630	0.765734
-574.710682	-12.791211	0.770739
-578.540530	-16.424416	0.775744
-582.074374	-19.016812	0.780749
-586.141010	-10.999625	0.785754
-589.999582	-17.256974	0.790758
-593.535205	-16.684160	0.795763
-596.917049	-12.034298	0.800768
-601.144239	-21.530111	0.805773
-604.974018	-17.955113	0.810778
-608.490346	-15.316421	0.815782
-612.446658	-18.549324	0.820787
-616.236008	-14.357876	0.825792
-619.974523	-18.286298	0.830797
-623.788928	-10.167421	0.835802
-627.302231	-18.706499	0.840806
-631.101138	-14.108229	0.845811
-635.355208	-15.562049	0.850816
-638.591866	-18.165571	0.855821
-642.451449	-14.402826	0.860826
-646.136873	-17.868184	0.865830
-649.804202	-22.821897	0.870835
-653.849330	-12.295981	0.875840
-657.238350	-28.764766	0.880845
-661.236399	-16.827123	0.885850
-665.135867	-21.556067	0.890854
-669.006208	-17.479329	0.895859
-672.848143	-20.689404	0.900864
-676.114599	-27.034904	0.905869
-680.013742	-21.766118	0.910874
-683.821514	-19.810868	0.915878
-687.502291	-22.409588	0.920883
-691.435165	-20.718184	0.925888
-695.066183	-33.366747	0.930893
-698.969506	-22.130152	0.935898
-702.418044	-22.685983	0.940902
-706.162205	-25.350237	0.945907
-710.417086	-20.633252	0.950912
-713.930644	-22.788725	0.955917
-717.688045	-23.287293	0.960922
-721.767648	-26.016188	0.965926
-725.324797	-21.754448	0.970931
-729.235147	-13.213231	0.975936
-732.407387	-20.359021	0.980941
-736.122445	-15.531141	0.985946
-740.070864	-24.847315	0.990950
-744.204296	-22.205999	0.995955
-748.345082	-13.126461	1.000960
-751.577880	-20.998974	1.005965
-755.285591	-14.210535	1.010970
-758.486028	-24.259643	1.015974
-762.444759	-29.179217	1.020979
-766.523088	-23.126306	1.025984
-770.053414	-28.223144	1.030989
-774.442452	-24.254149	1.035994
-778.273737	-25.390507	1.040998
-781.584148	-29.767125	1.046003
-785.461344	-18.635495	1.051008
-788.973683	-30.591675	1.056013
-792.830499	-16.907085	1.061018
-796.890829	-24.420184	1.066022
-800.497369	-19.425051	1.071027
-804.468781	-19.119732	1.076032
-808.144204	-24.645899	1.081037
-811.891878	-7.559932	1.086042
-815.114992	-15.443364	1.091046
-819.019741	-16.195758	1.096051
-823.197243	-10.371320	1.101056
-826.630503	-18.042950	1.106061
-830.812379	-23.600088	1.111066
-834.486038	-24.537627	1.116070
-838.069414	-13.840805	1.121075
-841.559023	-16.408339	1.126080
-845.182164	-23.584390	1.131085
-849.290016	-15.413532	1.136090
-853.104710	-17.501733	1.141094
-856.805702	-16.495243	1.146099
-860.652366	-12.688485	1.151104
-864.363804	-21.253859	1.156109
-868.295713	-15.353491	1.161114
-871.578913	-9.690860	1.166118
-875.755237	-14.103955	1.171123
-879.495077	-12.052022	1.176128
-883.176711	-20.857092	1.181133
-887.431419	-11.278146	1.186138
-890.909286	-16.140340	1.191142
-894.290779	-19.904623	1.196147
-897.823583	-19.634576	1.201152
-901.601023	-25.779783	1.206157
-906.037190	-15.902143	1.211162
-909.764901	-16.201727	1.216166
-913.322146	-23.569549	1.221171
-917.174184	-15.190325	1.226176
-920.441738	-25.228463	1.231181
-924.565554	-17.409738	1.236186
-928.607918	-7.905672	1.241190
-932.014593	-19.769714	1.246195
-936.052743	-21.194432	1.251200
-939.445689	-35.194229	1.256205
-943.426583	-12.824355	1.261210
-947.299987	-17.235292	1.266214
-950.836767	-12.411935	1.271219
-954.802110	-16.746659	1.276224
-958.057200	-29.529009	1.281229
-961.643945	-23.227954	1.286234
-965.955023	-19.802500	1.291238
-969.806881	-27.675043	1.296243
-973.884242	-21.749672	1.301248
-976.620971	-28.469596	1.306253
-980.927397	-22.763045	1.311258
-985.043605	-30.881865	1.316262
-988.503963	-25.230177	1.321267
-992.429781	-19.150814	1.326272
-996.089670	-18.063948	1.331277
-999.582150	-8.572012	1.336282
-1003.392722	-22.400855	1.341286
-1007.207931	-24.137064	1.346291
-1011.189135	-18.933469	1.351296
-1014.827235	-24.353307	1.356301
-1019.208225	-13.858248	1.361306
-1022.589805	-14.824856	1.366310
-1026.058637	-19.273554	1.371315
-1030.163967	-11.090182	1.376320
-1033.412771	-25.601738	1.381325
-1037.208259	-11.819357	1.386330
-1040.989724	-19.116424	1.391334
-1044.611573	-17.291257	1.396339
-1049.056526	-12.327235	1.401344
-1052.822929	-19.894767	1.406349
-1056.856603	-11.336464	1.411354
-1060.174548	-16.695477	1.416358
-1063.519457	-16.543542	1.421363
-1067.246467	-17.100026	1.426368
-1071.192069	-14.092377	1.431373
-1075.203049	-13.359232	1.436378
-1078.776749	-13.307872	1.441382
-1082.465499	-19.793388	1.446387
-1086.313037	-5.668295	1.451392
-1089.803120	-22.996988	1.456397
-1093.721888	-15.567163	1.461402
-1097.508882	-18.067815	1.466406
-1101.444701	-13.795409	1.471411
-1105.441093	-9.272036	1.476416
-1108.789763	-23.638194	1.481421
-1112.779458	-17.909535	1.486426
-1116.273064	-16.573120	1.491430
-1120.004907	-17.259630	1.496435
-1123.999154	-13.884573	1.501440
-1127.607811	-8.928036	1.506445
-1131.540738	-13.745446	1.511450
-1135.095822	-13.840478	1.516454
-1139.017767	-25.167599	1.521459
-1142.797968	-20.033791	1.526464
-1146.355479	-24.532768	1.531469
-1150.307270	-17.006109	1.536474
-1154.106910	-13.693674	1.541478
-1157.533286	-22.058158	1.546483
-1161.490350	-25.573841	1.551488
-1164.819898	-22.677216	1.556493
-1169.291830	-23.062315	1.561498
-1173.038531	-11.108886	1.566502
-1176.305690	-20.402395	1.571507
-1180.362622	-17.148099	1.576512
-1183.750876	-25.986986	1.581517
-1188.222313	-18.783969	1.586522
-1191.748015	-19.456039	1.591526
-1195.728322	-15.469668	1.596531
-1199.256677	-14.250570	1.601536
-1202.764730	-25.315800	1.606541
-1206.487716	-23.368549	1.611546
-1210.346438	-17.192338	1.616550
-1213.982789	-23.996672	1.621555
-1218.028617	-22.309974	1.626560
-1221.655311	-27.531031	1.631565
-1225.482641	-15.690780	1.636570
-1229.177377	-24.997785	1.641574
-1232.880844	-22.135846	1.646579
-1237.335060	-18.866764	1.651584
-1240.515906	-22.066559	1.656589
-1244.534567	-13.846237	1.661594
-1248.198313	-13.081630	1.666598
-1251.595447	-20.381493	1.671603
-1255.538155	-16.788963	1.676608
-1259.005509	-22.431267	1.681613
-1263.036427	-11.851452	1.686618
-1267.147599	-13.820559	1.691622
-1270.719234	-20.960005	1.696627
-1274.519676	-8.546823	1.701632
-1277.831140	-22.464511	1.706637
-1281.640692	-16.685556	1.711642
-1285.708763	-19.549334	1.716646
-1289.399053	-20.723182	1.721651
-1293.601448	-13.827950	1.726656
-1296.952204	-24.840932	1.731661
-1300.597552	-17.914998	1.736666
-1304.529910	-22.815769	1.741670
-1308.095981	-20.915547	1.746675
-1312.063163	-11.765084	1.751680
-1315.822089	-28.640356	1.756685
-1319.452811	-19.859122	1.761690
-1323.165012	-19.305833	1.766694
-1326.611095	-20.192286	1.771699
-1331.073848	-19.756966	1.776704
-1334.589695	-24.468890	1.781709
-1338.482238	-20.961521	1.786714
-1341.967197	-20.900307	1.791718
-1345.755730	-18.417226	1.796723
-1349.845825	-14.080293	1.801728
-1353.160715	-16.156206	1.806733
-1357.133108	-9.176255	1.811738
-1361.079692	-9.384887	1.816742
-1364.809965	-22.309742	1.821747
-1368.321448	-11.465983	1.826752
-1371.805715	-19.748326	1.831757
-1375.635406	-21.882142	1.836762
-1379.652397	-13.370134	1.841766
-1383.499856	-19.946434	1.846771
-1387.439099	-10.507013	1.851776
-1391.002599	-23.605173	1.856781
-1394.794317	-14.069513	1.861786
-1398.425260	-21.044718	1.866790
-1402.315637	-23.943041	1.871795
-1405.717910	-15.963056	1.876800
-1409.553909	-15.520694	1.881805
-1413.791689	-24.600100	1.886810
-1417.398601	-18.362950	1.891814
-1421.048344	-26.360102	1.896819
-1424.869091	-17.825826	1.901824
-1428.490905	-21.462524	1.906829
-1432.021628	-19.037928	1.911834
-1436.031151	-20.344928	1.916838
-1439.719211	-21.908389	1.921843
-1443.243288	-16.881345	1.926848
-1447.356366	-22.940350	1.931853
-1451.273598	-14.567198	1.936858
-1455.034380	-6.484007	1.941862
-1458.697086	-21.231398	1.946867
-1462.742597	-11.841072	1.951872
-1466.212971	-14.046462	1.956877
-1469.772263	-14.286959	1.961882
-1473.798334	-14.304477	1.966886
-1477.507217	-21.656569	1.971891
-1481.462065	-10.951387	1.976896
-1484.983641	-14.041086	1.981901
-1488.841165	-15.118449	1.986906
-1492.182271	-12.165895	1.991910
-1495.912485	-13.194248	1.996915
-1500.531764	-9.423362	2.006912
-1500.987180	-10.409662	2.016909
-1498.581377	-16.014649	2.026906
-1495.672749	-16.867021	2.036902
-1493.674026	-18.285785	2.046899
-1491.864410	-11.436942	2.056896
-1489.946067	-11.821258	2.066893
-1487.851206	-13.503306	2.076890
-1485.969648	-16.654345	2.086886
-1484.271594	-18.828634	2.096883
-1482.265650	-16.264883	2.106880
-1480.443930	-12.856897	2.116877
-1478.497669	-17.433020	2.126874
-1476.390674	-18.900685	2.136870
-1474.655077	-15.502590	2.146867
-1472.885378	-17.344134	2.156864
-1470.936718	-19.275912	2.166861
-1468.926576	-14.203887	2.176858
-1467.134601	-14.271110	2.186854
-1465.306323	-19.246749	2.196851
-1463.327870	-18.525937	2.206848
-1461.305211	-12.701176	2.216845
-1459.442244	-20.049195	2.226842
-1457.664888	-20.960380	2.236838
-1455.657144	-16.817955	2.246835
-1453.979597	-20.269458	2.256832
-1452.230136	-17.873033	2.266829
-1450.333545	-19.794878	2.276826
-1448.089845	-18.876524	2.286822
-1446.484486	-25.139606	2.296819
-1444.364507	-23.490918	2.306816
-1442.563029	-20.332292	2.316813
-1440.879095	-23.427968	2.326810
-1438.541046	-27.217317	2.336806
-1436.826611	-21.493186	2.346803
-1434.912880	-18.505683	2.356800
-1433.328815	-16.676443	2.366797
-1431.222659	-18.172354	2.376794
-1429.426713	-18.559129	2.386790
-1427.754033	-21.438259	2.396787
-1425.630110	-19.180713	2.406784
-1423.878678	-15.508797	2.416781
-1421.855040	-18.756743	2.426778
-1419.804489	-24.870033	2.436774
-1418.129207	-20.505400	2.446771
-1416.212298	-13.353146	2.456768
-1414.488173	-23.072576	2.466765
-1412.420295	-21.060254	2.476762
-1410.689869	-23.148095	2.486758
-1408.613572	-24.024998	2.496755
-1406.885567	-23.587724	2.506752
-1405.194083	-16.637792	2.516749
-1403.358988	-12.263994	2.526746
-1401.008554	-16.664762	2.536742
-1399.317949	-13.150456	2.546739
-1397.478331	-19.163645	2.556736
-1395.438230	-16.175813	2.566733
-1393.601214	-19.382806	2.576730
-1391.985692	-15.565950	2.586726
-1389.867064	-20.256437	2.596723
-1387.876194	-15.787565	2.606720
-1386.319683	-20.182799	2.616717
-1384.316663	-19.379010	2.626714
-1382.508150	-17.028299	2.636710
-1380.845478	-18.464223	2.646707
-1378.640093	-19.930183	2.656704
-1376.755479	-16.693232	2.666701
-1374.841634	-17.386205	2.676698
-1372.973599	-23.154452	2.686694
-1371.116710	-15.659394	2.696691
-1369.499932	-14.531658	2.706688
-1367.503533	-13.066796	2.716685
-1365.505400	-22.735321	2.726682
-1363.275582	-18.050468	2.736678
-1361.826708	-21.414777	2.746675
-1360.099529	-13.868944	2.756672
-1358.381963	-18.605731	2.766669
-1355.986834	-18.587838	2.776666
-1354.389737	-16.675366	2.786662
-1352.343636	-21.725262	2.796659
-1350.538140	-18.998255	2.806656
-1348.530482	-13.365196	2.816653
-1346.701527	-13.105087	2.826650
-1345.060794	-14.805894	2.836646
-1342.927451	-22.271317	2.846643
-1340.703440	-10.628695	2.856640
-1339.154175	-15.389056	2.866637
-1337.321559	-16.803204	2.876634
-1335.714854	-21.759070	2.886630
-1333.830602	-15.784142	2.896627
-1331.766252	-21.092731	2.906624
-1329.880767	-16.895884	2.916621
-1327.775845	-17.579929	2.926618
-1326.212825	-16.053559	2.936614
-1323.980199	-19.462768	2.946611
-1322.607585	-14.162249	2.956608
-1320.460526	-13.724089	2.966605
-1318.466822	-16.784000	2.976602
-1316.454176	-24.050081	2.986598
-1314.741527	-15.552943	2.996595
-1312.993702	-18.756652	3.006592
-1311.310208	-21.021646	3.016589
-1309.320581	-14.018302	3.026586
-1307.431329	-19.913054	3.036582
-1305.248535	-21.888485	3.046579
-1303.766158	-18.778146	3.056576
-1301.574036	-16.454030	3.066573
-1299.628757	-20.265645	3.076570
-1298.069714	-23.191234	3.086566
-1296.324396	-13.690365	3.096563
-1294.006724	-13.126329	3.106560
-1292.225818	-15.894793	3.116557
-1290.509061	-13.125113	3.126554
-1288.230474	-15.532700	3.136550
-1286.883766	-15.629573	3.146547
-1284.750441	-15.476549	3.156544
-1282.959798	-12.016058	3.166541
-1281.123137	-12.218182	3.176538
-1279.195943	-17.498462	3.186534
-1277.362757	-11.130047	3.196531
-1275.391561	-10.853173	3.206528
-1273.410228	-12.439493	3.216525
-1271.621386	-14.568162	3.226522
-1269.613567	-14.620827	3.236518
-1268.126997	-14.787440	3.246515
-1266.174073	-19.624986	3.256512
-1264.032266	-19.566458	3.266509
-1261.888025	-17.027799	3.276506
-1260.689740	-18.053006	3.286502
-1258.849219	-18.723097	3.296499
-1256.508108	-18.394879	3.306496
-1254.612845	-15.088476	3.316493
-1253.054252	-18.940805	3.326490
-1250.892656	-14.289129	3.336486
-1249.297350	-16.217863	3.346483
-1247.273080	-13.756306	3.356480
-1245.331383	-14.553104	3.366477
-1243.401454	-14.596440	3.376474
-1241.649591	-17.540218	3.386470
-1239.705228	-8.792726	3.396467
-1237.936365	-9.287124	3.406464
-1236.196229	-13.918492	3.416461
-1234.145734	-15.405321	3.426458
-1232.216748	-19.879010	3.436454
-1230.575742	-14.859800	3.446451
-1228.450427	-12.147554	3.456448
-1226.439013	-11.720758	3.466445
-1224.866275	-13.243234	3.476442
-1222.675123	-9.832571	3.486438
-1221.129502	-14.235436	3.496435
-1219.137192	-20.163981	3.506432
-1217.156782	-16.577488	3.516429
-1215.180429	-17.807700	3.526426
-1213.443561	-19.465377	3.536422
-1211.660029	-19.613156	3.546419
-1210.067012	-16.106774	3.556416
-1207.761990	-17.237992	3.566413
-1205.942051	-16.148963	3.576410
-1204.026232	-17.154743	3.586406
-1202.250530	-15.026004	3.596403
-1200.434794	-16.015767	3.606400
-1198.651804	-13.842402	3.616397
-1196.513167	-14.601197	3.626394
-1194.794148	-15.747586	3.636390
-1192.761815	-15.624107	3.646387
-1191.056910	-19.779280	3.656384
-1188.895469	-16.965409	3.666381
-1187.341618	-18.535364	3.676378
-1185.184089	-18.264543	3.686374
-1183.421181	-19.602681	3.696371
-1181.476951	-16.645103	3.706368
-1179.906663	-16.062424	3.716365
-1178.111053	-17.890527	3.726362
-1175.816877	-21.292078	3.736358
-1173.827154	-22.230710	3.746355
-1172.177911	-18.761719	3.756352
-1170.152490	-18.633957	3.766349
-1168.511808	-19.253057	3.776346
-1166.668783	-16.806641	3.786342
-1164.447260	-12.616046	3.796339
-1162.793837	-22.638214	3.806336
-1161.277308	-13.684833	3.816333
-1159.279025	-16.235347	3.826330
-1157.188005	-16.056490	3.836326
-1155.316445	-13.759892	3.846323
-1153.579535	-17.918581	3.856320
-1151.327904	-13.715422	3.866317
-1149.599432	-16.022235	3.876314
-1147.772864	-17.601058	3.886310
-1145.874675	-12.603980	3.896307
-1144.245224	-17.767049	3.906304
-1142.092460	-18.965422	3.916301
-1140.354381	-18.504297	3.926298
-1138.126201	-22.481042	3.936294
-1136.402818	-19.255989	3.946291
-1134.856804	-16.553611	3.956288
-1133.095139	-19.852563	3.966285
-1130.780055	-15.760586	3.976282
-1129.261473	-10.563818	3.986278
-1126.894158	-18.175439	3.996275
-1125.143451	-20.620002	4.006272
-1123.431305	-23.363130	4.016269
-1121.587476	-23.597855	4.026266
-1119.751479	-22.942379	4.036262
-1117.557804	-20.616754	4.046259
-1115.794641	-20.928569	4.056256
-1113.967746	-18.599530	4.066253
-1112.109355	-12.530268	4.076250
-1110.214058	-19.488471	4.086246
-1108.613162	-17.429590	4.096243
-1106.908188	-8.972100	4.106240
-1104.588301	-11.438225	4.116237
-1102.736166	-16.499521	4.126234
-1100.798393	-16.589783	4.136230
-1098.951803	-13.166514	4.146227
-1096.998895	-16.510242	4.156224
-1095.308435	-9.090946	4.166221
-1093.442023	-17.212937	4.176218
-1091.541311	-16.038843	4.186214
-1089.676490	-13.096903	4.196211
-1087.549891	-14.894199	4.206208
-1085.912888	-15.683180	4.216205
-1084.094489	-13.305388	4.226202
-1082.270413	-13.366395	4.236198
-1079.978356	-12.179100	4.246195
-1078.471066	-12.225749	4.256192
-1076.598560	-20.637648	4.266189
-1074.498015	-14.472878	4.276186
-1072.543437	-18.558959	4.286182
-1070.937475	-22.237170	4.296179
-1069.135147	-18.456272	4.306176
-1067.220678	-17.985411	4.316173
-1065.116658	-14.402764	4.326170
-1063.170184	-23.139115	4.336166
-1061.457057	-21.216573	4.346163
-1059.553475	-13.873970	4.356160
-1057.917753	-21.977982	4.366157
-1056.051853	-17.479348	4.376154
-1053.932306	-21.222326	4.386150
-1052.285677	-13.897039	4.396147
-1050.209251	-13.455225	4.406144
-1048.348430	-13.338925	4.416141
-1046.246020	-14.197579	4.426138
-1044.967839	-15.619141	4.436134
-1042.791348	-11.040695	4.446131
-1040.491990	-10.045580	4.456128
-1039.006180	-16.042977	4.466125
-1036.988197	-13.701805	4.476122
-1035.264788	-15.802464	4.486118
-1033.164602	-16.641803	4.496115
-1031.633152	-9.583866	4.506112
-1029.893683	-11.407617	4.516109
-1027.524933	-12.293061	4.526106
-1025.891685	-19.708239	4.536102
-1023.690261	-15.661132	4.546099
-1022.079092	-17.729620	4.556096
-1020.338975	-16.662415	4.566093
-1018.349722	-12.003474	4.576090
-1016.439550	-18.575566	4.586086
-1014.317600	-21.294158	4.596083
-1012.733952	-15.791925	4.606080
-1010.800280	-10.058299	4.616077
-1009.030667	-16.693171	4.626074
-1007.022996	-13.942955	4.636070
-1005.322161	-11.865245	4.646067
-1003.319336	-15.163198	4.656064
-1001.370984	-16.753491	4.666061
-999.595114	-14.291462	4.676058
-997.805958	-22.118396	4.686054
-995.729507	-13.028644	4.696051
-993.829509	-19.608566	4.706048
-992.176026	-20.272222	4.716045
-990.411648	-7.559398	4.726042
-988.046113	-12.274818	4.736038
-986.339321	-20.066469	4.746035
-984.627586	-10.804697	4.756032
-982.656820	-11.612243	4.766029
-980.480218	-12.953229	4.776026
-978.883295	-19.579411	4.786022
-977.336918	-21.899613	4.796019
-975.410380	-21.708501	4.806016
-973.230575	-21.589466	4.816013
-971.328250	-16.485531	4.826010
-969.266306	-14.181329	4.836006
-967.498215	-21.324349	4.846003
-966.084419	-18.668606	4.856000
-963.941315	-15.409482	4.865997
-962.128339	-16.905464	4.875994
-960.160963	-20.633502	4.885990
-958.057114	-20.262307	4.895987
-956.534321	-13.438196	4.905984
-954.682790	-18.031917	4.915981
-952.740236	-15.850715	4.925978
-950.929025	-13.207982	4.935974
-948.794746	-17.033752	4.945971
-947.073085	-14.697225	4.955968
-945.368374	-13.613249	4.965965
-943.163412	-16.515579	4.975962
-941.156695	-16.891469	4.985958
-939.528134	-15.550577	4.995955
-937.573070	-19.718734	5.005952
-935.731387	-18.786126	5.015949
-933.887277	-15.360745	5.025946
-931.916052	-13.236215	5.035942
-930.165917	-19.370548	5.045939
-928.505817	-17.788375	5.055936
-926.436267	-11.256925	5.065933
-924.463304	-12.817932	5.075930
-922.567765	-11.052345	5.085926
-920.756352	-12.977520	5.095923
-918.777182	-16.454779	5.105920
-917.104423	-15.438306	5.115917
-915.249186	-11.302582	5.125914
-913.164923	-7.121368	5.135910
-911.245084	-14.945457	5.145907
-909.402156	-11.650919	5.155904
-907.847720	-8.979729	5.165901
-905.744650	-14.718897	5.175898
-903.884548	-16.479737	5.185894
-902.161468	-6.799707	5.195891
-899.938212	-13.003350	5.205888
-898.307235	-18.212295	5.215885
-896.409148	-12.367089	5.225882
-894.479775	-10.958993	5.235878
-892.652416	-13.147223	5.245875
-890.519731	-9.420572	5.255872
-888.749809	-11.572774	5.265869
-887.363965	-8.183036	5.275866
-885.167833	-15.830225	5.285862
-883.235178	-8.102109	5.295859
-881.166230	-8.142108	5.305856
-879.211914	-12.292733	5.315853
-877.557235	-14.996503	5.325850
-875.872020	-9.965143	5.335846
-874.039716	-18.019947	5.345843
-872.021404	-17.164473	5.355840
-870.095009	-13.147457	5.365837
-868.140396	-7.680735	5.375834
-866.272659	-12.831195	5.385830
-864.307906	-7.921881	5.395827
-862.660731	-2.646005	5.405824
-860.859183	-11.659047	5.415821
-858.844028	-13.068850	5.425818
-856.679561	-13.716204	5.435814
-854.906660	-9.867267	5.445811
-853.265118	-10.596813	5.455808
-851.334162	-6.932613	5.465805
-849.622679	-5.604911	5.475802
-847.810496	-13.282272	5.485798
-845.738933	-13.973185	5.495795
-843.564766	-14.262077	5.505792
-841.881451	-8.134594	5.515789
-840.100091	-8.207532	5.525786
-838.279494	-10.028324	5.535782
-836.399312	-14.978645	5.545779
-834.158559	-9.172369	5.555776
-832.590986	-13.992191	5.565773
-830.807315	-11.237591	5.575770
-828.791727	-16.275866	5.585766
-826.767329	-11.301844	5.595763
-825.082789	-12.834034	5.605760
-823.429563	-18.423857	5.615757
-821.273832	-13.526087	5.625754
-819.656110	-14.332328	5.635750
-817.458178	-14.380257	5.645747
-815.808202	-6.308472	5.655744
-813.738554	-11.911169	5.665741
-811.772999	-11.915633	5.675738
-809.891263	-14.957231	5.685734
-808.514250	-18.996575	5.695731
-806.046116	-10.900822	5.705728
-804.120428	-9.231535	5.715725
-802.717169	-5.081893	5.725722
-800.556314	-8.652837	5.735718
-798.847302	-8.701549	5.745715
-797.150157	-6.692567	5.755712
-794.981645	-0.860491	5.765709
-793.399821	-5.690464	5.775706
-791.053556	-11.340513	5.785702
-789.478103	-12.582084	5.795699
-787.799012	-16.172330	5.805696
-785.455817	-9.652903	5.815693
-783.732720	-12.331231	5.825690
-781.697523	-6.694153	5.835686
-780.244286	-4.253016	5.845683
-778.078508	-4.897349	5.855680
-776.296827	-7.810826	5.865677
-774.447304	-4.229860	5.875674
-772.503810	-0.594437	5.885670
-770.443184	-4.986181	5.895667
-768.940591	-7.163466	5.905664
-767.078613	-5.108175	5.915661
-765.000711	-8.537934	5.925658
-762.836131	-11.893123	5.935654
-761.172788	-15.652940	5.945651
-759.392272	-17.678846	5.955648
-757.718383	-11.570319	5.965645
-755.645727	-14.190807	5.975642
-753.834509	-8.600014	5.985638
-751.775806	-5.947727	5.995635
-749.961992	-10.347377	6.005632
-748.006080	-11.466566	6.015629
-746.360980	-8.171857	6.025626
-744.248686	-10.413407	6.035622
-742.670030	-15.648630	6.045619
-741.016349	-12.974238	6.055616
-738.709884	-6.005205	6.065613
-736.902211	-8.191751	6.075610
-735.072076	-12.448735	6.085606
-733.021407	-10.679361	6.095603
-731.022918	-18.211149	6.105600
-729.130279	-10.215972	6.115597
-727.691146	-10.071504	6.125594
-725.589131	-9.788228	6.135590
-723.760648	-7.618601	6.145587
-721.936856	-4.440851	6.155584
-719.843057	-3.848361	6.165581
-718.249412	-5.558585	6.175578
-716.289963	-8.858848	6.185574
-714.270060	-9.148232	6.195571
-712.348692	-7.468704	6.205568
-710.584976	-7.589252	6.215565
-708.523845	-11.262600	6.225562
-706.980749	-8.633670	6.235558
-705.004004	-14.548275	6.245555
-703.075144	-14.186784	6.255552
-701.291953	-14.147805	6.265549
-699.338763	-10.035448	6.275546
-697.447216	-10.740099	6.285542
-695.636008	-8.817164	6.295539
-693.562557	-9.917195	6.305536
-692.015209	-13.462642	6.315533
-690.281872	-7.673035	6.325530
-688.145995	-6.190395	6.335526
-686.105892	-6.945617	6.345523
-684.202109	-8.700637	6.355520
-682.715804	-10.488423	6.365517
-680.684832	-7.106902	6.375514
-678.415620	-10.862421	6.385510
-676.724649	-8.170256	6.395507
-674.668717	-8.069047	6.405504
-673.180364	-5.425030	6.415501
-671.316295	-10.603183	6.425498
-669.429024	-17.725574	6.435494
-667.476024	-10.144199	6.445491
-665.480172	-10.931806	6.455488
-663.803815	-15.329957	6.465485
-661.871024	-12.629051	6.475482
-659.759591	-12.719854	6.485478
-658.068602	-12.146635	6.495475
-656.123608	-13.063478	6.505472
-654.259123	-11.131655	6.515469
-652.383274	-10.404808	6.525466
-650.541530	-9.568300	6.535462
-648.783649	-10.639979	6.545459
-646.917513	-8.593150	6.555456
-645.039975	-15.180282	6.565453
-643.148249	-12.505958	6.575450
-641.254595	-24.997787	6.585446
-639.136139	-19.250726	6.595443
-637.210657	-25.812351	6.605440
-635.742023	-19.677255	6.615437
-634.091290	-14.164936	6.625434
-631.561559	-18.184666	6.635430
-629.980884	-14.584316	6.645427
-627.894733	-18.601069	6.655424
-625.927412	-9.652991	6.665421
-624.490972	-14.764368	6.675418
-622.505967	-11.640716	6.685414
-620.384687	-14.627282	6.695411
-618.751454	-14.257966	6.705408
-616.875372	-16.799564	6.715405
-614.908532	-14.246164	6.725402
-612.991707	-16.982163	6.735398
-611.220063	-14.790736	6.745395
-609.506693	-15.220535	6.755392
-607.352114	-17.947144	6.765389
-605.389929	-13.040351	6.775386
-603.591381	-9.665841	6.785382
-601.804963	-12.456789	6.795379
-599.872818	-12.304160	6.805376
-597.890394	-10.849030	6.815373
-596.184449	-15.742917	6.825370
-594.327075	-12.802537	6.835366
-592.485009	-13.672885	6.845363
-590.426614	-18.981494	6.855360
-588.635767	-20.836819	6.865357
-586.770889	-15.582886	6.875354
-584.770950	-18.237403	6.885350
-583.192217	-16.984616	6.895347
-581.206894	-12.163602	6.905344
-579.244015	-16.316939	6.915341
-577.353376	-15.469238	6.925338
-575.345654	-18.634993	6.935334
-573.483938	-16.907927	6.945331
-571.840636	-19.843361	6.955328
-570.140589	-17.747834	6.965325
-568.151446	-13.495844	6.975322
-566.073989	-17.601157	6.985318
-564.238186	-18.214692	6.995315
-562.496191	-20.510618	7.005312
-560.333383	-23.469027	7.015309
-558.519072	-23.367016	7.025306
-557.065338	-17.905278	7.035302
-554.915086	-21.377995	7.045299
-552.782118	-17.052650	7.055296
-551.060598	-17.605289	7.065293
-549.633702	-14.392426	7.075290
-547.165545	-16.100118	7.085286
-545.148289	-18.255262	7.095283
-543.686426	-17.506414	7.105280
-541.932322	-16.831087	7.115277
-539.990900	-12.179868	7.125274
-538.000905	-18.361725	7.135270
-535.938904	-20.462428	7.145267
-534.038905	-19.322502	7.155264
-532.284051	-14.668320	7.165261
-530.557697	-15.987509	7.175258
-528.851622	-12.373959	7.185254
-526.851254	-16.801666	7.195251
-524.699124	-14.989893	7.205248
-522.919271	-13.587608	7.215245
-521.369729	-13.711702	7.225242
-519.174608	-11.717315	7.235238
-517.198151	-19.049632	7.245235
-515.500817	-17.918374	7.255232
-513.684340	-15.238240	7.265229
-511.629097	-11.440443	7.275226
-509.593483	-22.132746	7.285222
-508.094419	-16.878742	7.295219
-505.874502	-18.906746	7.305216
-504.119355	-20.274726	7.315213
-502.661890	-19.551993	7.325210
-500.745552	-16.605165	7.335206
-498.534792	-20.561185	7.345203
-496.532270	-18.943388	7.355200
-494.779039	-20.909480	7.365197
-492.924032	-19.587070	7.375194
-490.852443	-19.150306	7.385190
-489.187028	-23.268696	7.395187
-487.355554	-20.616201	7.405184
-485.452111	-13.787805	7.415181
-483.516862	-18.200341	7.425178
-481.746398	-12.797028	7.435174
-479.746009	-14.939951	7.445171
-477.964142	-19.356408	7.455168
-476.276358	-18.981495	7.465165
-474.422506	-16.743091	7.475162
-472.404142	-17.654134	7.485158
-470.420572	-22.398061	7.495155
-468.342769	-16.074341	7.505152
-466.435579	-20.656067	7.515149
-464.693069	-18.076189	7.525146
-463.167432	-14.163773	7.535142
-461.077376	-15.157309	7.545139
-459.132325	-14.191885	7.555136
-457.325545	-14.094910	7.565133
-455.510377	-18.057193	7.575130
-453.215546	-22.727654	7.585126
-451.393456	-17.403616	7.595123
-449.802618	-19.754272	7.605120
-448.397508	-13.858377	7.615117
-446.159026	-14.184018	7.625114
-444.100854	-10.762419	7.635110
-442.204024	-15.115105	7.645107
-440.554746	-18.466672	7.655104
-438.452077	-10.951622	7.665101
-436.657886	-7.350493	7.675098
-434.780889	-7.335767	7.685094
-432.862637	-10.712913	7.695091
-430.800220	-8.485672	7.705088
-429.187373	-9.344557	7.715085
-427.313004	-17.494196	7.725082
-425.387168	-17.428840	7.735078
-423.485555	-16.312765	7.745075
-421.740818	-13.783736	7.755072
-419.957242	-12.217755	7.765069
-417.904601	-12.103167	7.775066
-416.144910	-7.501769	7.785062
-413.991663	-14.484869	7.795059
-411.982560	-12.269625	7.805056
-409.498648	-8.085441	7.815053
-407.841076	-14.768336	7.825050
-407.026191	-13.751888	7.835046
-404.993311	-16.627837	7.845043
-402.698303	-11.619270	7.855040
-401.043749	-12.369532	7.865037
-399.056813	-4.583328	7.875034
-397.285299	-8.897025	7.885030
-395.280934	-12.660526	7.895027
-393.892745	-14.715105	7.905024
-392.421336	-18.497718	7.915021
-390.085245	-15.079393	7.925018
-387.947392	-15.330492	7.935014
-385.973548	-14.495922	7.945011
-384.135226	-13.886030	7.955008
-382.347327	-18.098119	7.965005
-380.363811	-14.554017	7.975002
-378.695046	-13.018622	7.984998
-376.340675	-15.997983	7.994995
-374.539961	-12.378900	8.004992
-372.717377	-12.309648	8.014989
-371.133649	-17.226506	8.024986
-368.955345	-16.737199	8.034982
-367.170992	-18.959223	8.044979
-365.579448	-13.454620	8.054976
-363.534492	-21.348814	8.064973
-361.488885	-15.405119	8.074970
-359.752048	-15.671118	8.084966
-358.021151	-15.524058	8.094963
-356.039078	-15.396572	8.104960
-354.131877	-15.075550	8.114957
-352.192839	-16.155409	8.124954
-350.359405	-18.511574	8.134950
-348.332061	-17.837094	8.144947
-346.475035	-16.448574	8.154944
-344.831470	-16.723355	8.164941
-342.893425	-18.554633	8.174938
-340.890946	-20.675670	8.184934
-339.290634	-18.121944	8.194931
-337.206919	-18.852253	8.204928
-335.496112	-18.608812	8.214925
-333.427978	-21.506120	8.224922
-331.630598	-19.339114	8.234918
-329.376568	-16.821845	8.244915
-327.947656	-15.481810	8.254912
-326.092213	-18.651477	8.264909
-324.221631	-13.925605	8.274906
-322.219975	-10.676455	8.284902
-320.344358	-22.119926	8.294899
-318.349508	-22.019712	8.304896
-316.378821	-19.754044	8.314893
-314.640061	-18.341883	8.324890
-313.002920	-15.675595	8.334886
-311.380557	-12.762208	8.344883
-308.886057	-15.591767	8.354880
-307.124344	-19.243830	8.364877
-305.311072	-17.208815	8.374874
-303.298148	-20.743079	8.384870
-301.599549	-21.050301	8.394867
-299.711468	-23.835154	8.404864
-297.980041	-24.532879	8.414861
-296.111817	-16.865008	8.424858
-293.881862	-20.073906	8.434854
-291.936097	-21.385318	8.444851
-290.121397	-22.431070	8.454848
-288.233665	-15.814734	8.464845
-286.659135	-20.052698	8.474842
-284.993342	-15.919373	8.484838
-282.736215	-19.353653	8.494835
-280.936697	-18.151693	8.504832
-279.178007	-17.893750	8.514829
-277.068888	-23.644417	8.524826
-275.431634	-19.214423	8.534822
-273.393263	-19.956388	8.544819
-271.361371	-16.994655	8.554816
-269.838067	-20.946535	8.564813
-267.740301	-12.967905	8.574810
-265.764495	-19.782031	8.584807
-263.844065	-26.445208	8.594803
-262.137795	-20.358841	8.604800
-260.573824	-17.988734	8.614797
-258.676756	-19.949195	8.624794
-256.715887	-19.949296	8.634791
-254.469564	-18.610208	8.644787
-252.750550	-19.324868	8.654784
-250.968172	-14.954334	8.664781
-248.827967	-17.829917	8.674778
-247.126456	-17.796510	8.684775
-245.381636	-19.260552	8.694771
-243.151636	-21.247296	8.704768
-241.340000	-21.569359	8.714765
-239.792439	-16.150805	8.724762
-237.992348	-21.097376	8.734759
-235.692077	-17.204228	8.744755
-234.080725	-19.592758	8.754752
-232.043843	-24.512379	8.764749
-230.125571	-25.936197	8.774746
-228.424308	-23.930616	8.784743
-226.405774	-24.339372	8.794739
-224.459912	-23.067568	8.804736
-222.757252	-23.069064	8.814733
-220.951761	-24.755931	8.824730
-219.153751	-21.232613	8.834727
-217.123049	-23.839637	8.844723
-215.141874	-17.926579	8.854720
-213.400269	-22.513270	8.864717
-211.665503	-19.169328	8.874714
-209.655585	-22.164612	8.884711
-207.616944	-19.320744	8.894707
-206.011369	-23.536771	8.904704
-204.353915	-24.958419	8.914701
-202.194422	-26.335448	8.924698
-200.210499	-24.248639	8.934695
-198.314514	-24.497287	8.944691
-196.450063	-28.710408	8.954688
-194.390336	-20.520376	8.964685
-192.770754	-14.893806	8.974682
-190.912885	-18.880084	8.984679
-188.806140	-20.149209	8.994675
-187.212013	-22.705488	9.004672
-185.225978	-17.314236	9.014669
-183.344350	-21.381668	9.024666
-181.589680	-19.240889	9.034663
-179.764277	-23.122502	9.044659
-177.835049	-22.743276	9.054656
-175.891556	-25.437404	9.064653
-173.954793	-21.590399	9.074650
-172.280910	-25.105193	9.084647
-170.104741	-25.063790	9.094643
-168.413064	-18.469752	9.104640
-166.572692	-17.629492	9.114637
-164.420422	-16.998474	9.124634
-162.625330	-18.996275	9.134631
-160.800361	-19.361458	9.144627
-159.035666	-20.860189	9.154624
-157.091263	-19.584939	9.164621
-155.149688	-18.915556	9.174618
-153.449549	-17.456061	9.184615
-151.624386	-21.624988	9.194611
-149.459664	-24.695451	9.204608
-147.844216	-18.142919	9.214605
-145.918944	-22.168340	9.224602
-143.900230	-14.789615	9.234599
-141.968681	-22.071854	9.244595
-140.248612	-30.818779	9.254592
-138.322391	-28.716396	9.264589
-136.371160	-22.528490	9.274586
-134.771080	-24.520416	9.284583
-132.681981	-22.380857	9.294579
-130.724541	-20.539239	9.304576
-128.995963	-22.223241	9.314573
-127.056185	-20.678804	9.324570
-125.016691	-19.679228	9.334567
-123.310294	-16.016478	9.344563
-121.307596	-18.391587	9.354560
-119.892809	-13.231240	9.364557
-117.731223	-15.705908	9.374554
-115.940575	-8.784982	9.384551
-113.719050	-14.387664	9.394547
-112.207386	-11.544895	9.404544
-110.056659	-14.650989	9.414541
-108.292243	-13.478035	9.424538
-106.660723	-12.013874	9.434535
-104.530675	-14.497710	9.444531
-102.552443	-12.689385	9.454528
-100.958520	-12.142915	9.464525
-98.972657	-7.010505	9.474522
-97.093092	-12.280718	9.484519
-95.078895	-10.508125	9.494515
-93.619634	-9.384370	9.504512
-91.439160	-17.623668	9.514509
-89.276716	-17.000523	9.524506
-87.652837	-13.477740	9.534503
-86.306099	-9.557052	9.544499
-83.861780	-18.811079	9.554496
-81.669242	-17.941673	9.564493
-80.410664	-14.859558	9.574490
-78.266413	-20.953569	9.584487
-76.431760	-20.671280	9.594483
-74.457882	-27.679166	9.604480
-72.607847	-28.411443	9.614477
-70.987097	-24.777625	9.624474
-68.868532	-21.344802	9.634471
-66.813191	-24.497220	9.644467
-65.355887	-24.876310	9.654464
-63.477063	-22.139454	9.664461
-61.500898	-15.045974	9.674458
-59.501134	-21.448502	9.684455
-57.466069	-18.346561	9.694451
-55.776918	-25.506384	9.704448
-54.000953	-17.296213	9.714445
-52.033174	-21.969404	9.724442
-50.082004	-18.711967	9.734439
-48.381856	-21.411389	9.744435
-46.139935	-15.487670	9.754432
-44.455232	-18.160941	9.764429
-42.786214	-16.787982	9.774426
-40.525375	-15.932592	9.784423
-38.899633	-20.508579	9.794419
-37.296302	-19.489879	9.804416
-35.389160	-23.264427	9.814413
-33.405941	-16.353629	9.824410
-31.357430	-23.147599	9.834407
-29.359135	-16.769734	9.844403
-27.559016	-10.058670	9.854400
-25.742706	-19.199835	9.864397
-23.931578	-15.515822	9.874394
-21.908592	-19.220418	9.884391
-20.201075	-20.196767	9.894387
-18.210953	-22.170309	9.904384
-16.218934	-20.799907	9.914381
-14.654411	-23.534514	9.924378
-12.788573	-24.736641	9.934375
-10.837327	-25.668175	9.944371
-8.810897	-25.648532	9.954368
-7.277991	-21.092752	9.964365
-5.301992	-7.550700	9.974362
-4.021759	18.135660	9.984359
-2.727488	52.204169	9.994355
-1.070843	105.216370	10.004352
0.000000	146.763881	10.009357
0.782774	170.378773	10.014362
1.200820	215.120196	10.019367
1.626246	227.718695	10.024371
2.195729	253.889324	10.029376
2.571783	267.307875	10.034381
2.811816	278.411052	10.039386
2.995930	297.783376	10.044391
3.282177	302.992337	10.049395
3.311913	314.565908	10.054400
2.993614	312.093627	10.059405
3.390608	311.054273	10.064410
3.740130	320.282335	10.069415
3.658246	314.763462	10.074419
3.648873	319.000850	10.079424
3.338336	326.965377	10.084429
3.892508	325.784256	10.089434
3.595608	336.515795	10.094439
3.712578	326.904466	10.099443
3.851865	332.807096	10.104448
3.809446	335.319808	10.109453
3.929328	332.394425	10.114458
3.603447	335.242515	10.119463
3.873549	331.619800	10.124467
4.031225	334.324528	10.129472
3.867890	333.830295	10.134477
4.290477	342.111566	10.139482
4.310513	344.950217	10.144487
4.153719	334.545170	10.149491
4.283875	322.219328	10.154496
3.918685	327.898063	10.159501
4.139814	329.419395	10.164506
3.980741	345.897563	10.169511
4.480312	343.591297	10.174515
4.309406	345.935268	10.179520
4.221669	357.917127	10.184525
4.386464	360.934545	10.189530
4.202499	367.033831	10.194535
4.509514	366.677468	10.199539
4.402608	360.842440	10.204544
4.473363	363.292950	10.209549
4.947788	358.394973	10.214554
4.396146	367.869307	10.219559
4.709150	357.206379	10.224563
4.694552	365.659900	10.229568
4.556126	368.120121	10.234573
4.629782	364.941901	10.239578
4.306370	373.913048	10.244583
4.773551	379.988906	10.249587
4.918517	384.687409	10.254592
5.140546	388.547279	10.259597
5.336868	384.494761	10.264602
5.263823	386.547155	10.269607
5.205649	388.266011	10.274611
5.261257	390.236383	10.279616
5.174688	393.049467	10.284621
5.214568	392.953337	10.289626
5.220181	396.682144	10.294631
5.212809	389.254238	10.299635
5.228787	394.544188	10.304640
4.983400	399.979909	10.309645
5.245088	393.078380	10.314650
5.208288	415.439800	10.319655
5.607296	421.223767	10.324659
5.588916	426.774682	10.329664
5.487775	434.401508	10.334669
5.680133	430.188757	10.339674
5.625973	444.324237	10.344679
5.689450	441.772114	10.349683
6.076620	438.364096	10.354688
5.915842	442.622515	10.359693
6.288084	439.636358	10.364698
6.064658	443.859037	10.369703
6.068739	443.741808	10.374707
6.033757	442.384982	10.379712
5.983028	443.921302	10.384717
5.986413	447.325616	10.389722
5.713890	450.712435	10.394727
6.154800	448.505399	10.399731
6.232596	451.390052	10.404736
6.141402	476.007462	10.409741
6.732349	477.086612	10.414746
6.708177	477.847547	10.419751
6.597912	465.999914	10.424755
6.463609	459.741850	10.429760
6.276016	461.467163	10.434765
6.667275	472.830229	10.439770
6.648730	483.565577	10.444775
6.716213	487.276653	10.449779
6.940159	488.236140	10.454784
6.928384	492.412459	10.459789
6.954283	487.601749	10.464794
6.886959	485.918908	10.469799
6.482638	495.380865	10.474803
6.616322	488.811954	10.479808
6.689348	495.223551	10.484813
6.899936	499.157817	10.489818
6.739785	498.765575	10.494823
6.730822	496.215536	10.499827
7.119629	496.497426	10.504832
7.314947	526.033624	10.509837
7.321534	527.054591	10.514842
7.330931	521.349187	10.519847
7.638724	538.323983	10.524851
7.874432	533.796772	10.529856
7.845016	537.570627	10.534861
7.727974	533.522316	10.539866
7.417643	530.061520	10.544871
7.763156	525.649265	10.549875
7.893825	527.350632	10.554880
7.405409	534.734919	10.559885
7.772518	534.597634	10.564890
8.012081	532.862686	10.569895
7.788484	522.542278	10.574899
7.846458	512.296819	10.579904
7.217845	506.420361	10.584909
7.448008	525.091763	10.589914
7.432405	540.001803	10.594919
7.439321	530.657061	10.599923
8.064637	538.866685	10.604928
7.717520	540.576449	10.609933
8.036948	537.458343	10.614938
7.902988	546.710047	10.619943
8.028414	562.521743	10.624947
8.140509	557.836038	10.629952
8.179750	574.741744	10.634957
8.272281	578.732710	10.639962
8.109238	576.555752	10.644967
8.269866	572.329097	10.649971
8.344146	578.075032	10.654976
8.578914	579.906463	10.659981
8.536739	573.414450	10.664986
8.247870	576.895372	10.669991
8.416621	581.326785	10.674995
8.857436	594.076120	10.680000
8.932194	607.730708	10.685005
9.051084	608.782657	10.690010
8.820131	599.739171	10.695015
8.840878	605.201909	10.700019
9.188238	607.862241	10.705024
8.858582	611.477415	10.710029
8.889827	613.366545	10.715034
8.660288	624.379298	10.720039
9.143419	616.177578	10.725043
9.434499	619.018784	10.730048
8.930594	626.430819	10.735053
9.281039	618.251838	10.740058
9.217634	626.659676	10.745063
9.108961	628.427616	10.750067
9.246014	620.459295	10.755072
9.248658	629.919509	10.760077
9.030667	628.366343	10.765082
9.244831	635.520343	10.770087
9.516627	642.914323	10.775091
9.513463	658.708785	10.780096
9.481221	664.296695	10.785101
10.102239	656.834659	10.790106
9.796851	656.973378	10.795111
9.724418	659.328501	10.800115
9.958323	660.005702	10.805120
9.829386	661.644409	10.810125
9.646983	660.430930	10.815130
9.742010	670.508820	10.820135
10.204154	686.713241	10.825139
10.366993	689.005610	10.830144
10.274479	692.188724	10.835149
10.606786	690.530432	10.840154
10.539326	698.915303	10.845159
10.258541	690.141495	10.850163
10.140943	677.066359	10.855168
10.052243	683.101694	10.860173
10.503247	686.589217	10.865178
10.383573	696.390696	10.870183
10.676961	694.505211	10.875187
10.294916	697.329211	10.880192
10.394498	702.971807	10.885197
10.291983	697.875567	10.890202
10.159855	704.348365	10.895207
10.378833	704.211051	10.900211
10.793655	700.856912	10.905216
10.499096	708.019546	10.910221
10.452162	703.803880	10.915226
10.574398	708.419377	10.920231
10.770101	716.416916	10.925235
11.274172	725.831910	10.930240
11.174546	720.055502	10.935245
11.006719	711.553837	10.940250
11.046911	706.054770	10.945255
10.647050	721.073595	10.950259
11.152321	724.968807	10.955264
11.040134	739.459198	10.960269
11.381990	739.368520	10.965274
11.171633	742.275536	10.970279
11.002907	745.002439	10.975283
11.400734	736.569818	10.980288
11.028793	748.747146	10.985293
11.193253	748.585410	10.990298
11.028990	744.550880	10.995303
11.271758	752.768025	11.000307
11.335619	759.504491	11.005312
11.172163	772.744622	11.010317
11.767206	772.585175	11.015322
11.748037	781.798218	11.020327
11.547218	783.819006	11.025331
12.055837	776.480499	11.030336
11.623386	774.275514	11.035341
12.017997	776.884185	11.040346
11.626716	775.197785	11.045351
11.935898	780.218748	11.050355
11.972080	773.395588	11.055360
11.899859	784.060078	11.060365
12.011649	773.674958	11.065370
11.770188	776.843998	11.070375
12.001910	778.366843	11.075379
12.261489	791.946392	11.080384
11.842785	804.676879	11.085389
12.120440	801.969101	11.090394
12.526500	809.431643	11.095399
12.435790	812.344822	11.100403
12.778511	809.716555	11.105408
12.475789	815.672534	11.110413
12.538392	808.283719	11.115418
12.497167	815.148942	11.120423
12.477585	817.587128	11.125427
12.540591	813.287660	11.130432
12.449048	811.296391	11.135437
12.416289	817.668230	11.140442
12.380147	818.065219	11.145447
12.623841	822.415362	11.150451
12.712317	828.856183	11.155456
12.655953	842.626528	11.160461
13.033620	837.614509	11.165466
12.990253	841.559411	11.170471
12.858999	840.538042	11.175475
13.023869	842.226107	11.180480
12.803991	845.989417	11.185485
13.096747	845.069162	11.190490
13.295333	845.002913	11.195495
13.418730	840.465134	11.200499
13.761121	842.039724	11.205504
13.427998	839.790499	11.210509
13.604400	841.273286	11.215514
13.690422	840.332386	11.220519
13.443574	845.492523	11.225523
13.901660	841.965863	11.230528
13.634029	842.849231	11.235533
13.340646	845.752162	11.240538
13.555648	845.481433	11.245543
13.663521	847.199090	11.250547
13.738324	848.458373	11.255552
13.556498	853.762692	11.260557
13.831573	842.635503	11.265562
13.974458	851.736006	11.270567
13.790600	851.486314	11.275571
14.030261	845.919107	11.280576
13.915251	851.116569	11.285581
14.302439	847.716339	11.290586
13.987779	844.623606	11.295591
13.925458	848.920059	11.300595
14.202668	856.758011	11.305600
14.457915	886.775844	11.310605
14.265642	882.007686	11.315610
14.660007	892.402284	11.320615
14.492706	879.396398	11.325619
14.543367	854.337130	11.330624
14.016510	861.964267	11.335629
14.441524	872.784494	11.340634
14.547453	877.448380	11.345639
14.716918	885.743528	11.350643
14.822324	882.566440	11.355648
14.872499	885.376733	11.360653
14.646187	887.783246	11.365658
14.796742	887.730965	11.370663
14.613398	894.100046	11.375667
14.569669	892.426010	11.380672
14.482057	889.409024	11.385677
14.671681	884.426982	11.390682
14.674174	891.649565	11.395687
14.586859	889.416323	11.400691
15.200564	899.236591	11.405696
14.829953	919.250189	11.410701
15.031733	916.816282	11.415706
15.123468	918.320466	11.420711
15.098320	918.092771	11.425715
15.385635	915.556907	11.430720
15.364158	922.100467	11.435725
15.258508	920.513580	11.440730
15.232427	910.598234	11.445735
15.258848	924.733944	11.450739
15.546457	913.120549	11.455744
15.369880	921.567109	11.460749
15.575269	919.832835	11.465754
15.548116	918.943100	11.470759
15.306282	932.533365	11.475763
15.906703	942.753199	11.480768
15.723657	956.067588	11.485773
15.876258	952.917652	11.490778
16.263866	947.656413	11.495783
15.630769	952.212678	11.500787
16.239202	941.661487	11.505792
15.981216	952.590710	11.510797
16.382454	952.578876	11.515802
16.242321	932.938688	11.520807
16.022514	923.019537	11.525811
16.277533	916.388501	11.530816
16.223224	931.976938	11.535821
16.339622	940.513985	11.540826
16.423766	944.889613	11.545831
16.302901	950.321447	11.550835
16.469558	940.674979	11.555840
16.079504	946.976121	11.560845
16.493858	946.824991	11.565850
16.610878	959.353465	11.570855
16.274230	958.733877	11.575859
16.339707	954.392970	11.580864
16.351360	958.836939	11.585869
16.398734	954.792250	11.590874
16.337196	954.199751	11.595879
16.433495	962.358370	11.600883
16.909073	961.943570	11.605888
16.832274	983.241425	11.610893
16.904460	978.601377	11.615898
17.487654	980.400944	11.620903
16.933233	982.907115	11.625907
17.270140	986.638430	11.630912
17.148666	986.825092	11.635917
17.253729	982.938362	11.640922
16.976586	982.189427	11.645927
17.137532	988.598258	11.650931
17.100032	983.650830	11.655936
17.232611	987.405272	11.660941
17.224821	983.076043	11.665946
17.420367	987.626317	11.670951
17.368132	986.505596	11.675955
17.648747	976.863007	11.680960
17.597967	987.103153	11.685965
17.659914	981.944309	11.690970
17.394477	981.958378	11.695975
17.354493	985.708802	11.700979
17.647833	978.984887	11.705984
17.428060	994.910463	11.710989
17.522456	982.520376	11.715994
18.082797	989.348085	11.720999
17.550258	998.163721	11.726003
18.046364	996.252175	11.731008
18.117802	1012.479852	11.736013
18.290685	1009.437064	11.741018
18.112529	993.138335	11.746023
17.953281	993.824640	11.751027
18.521700	998.283904	11.756032
18.057123	986.755726	11.761037
18.324509	999.626128	11.766042
18.260612	1007.540646	11.771047
18.618027	1019.669683	11.776051
18.777056	1001.852077	11.781056
18.408520	991.573376	11.786061
18.439206	980.746852	11.791066
18.368789	983.740413	11.796071
18.215986	998.094026	11.801075
18.770128	1008.154121	11.806080
18.700325	1016.383420	11.811085
18.919194	1023.831772	11.816090
18.943208	1014.480838	11.821095
18.574973	1006.212827	11.826099
18.942252	1007.097446	11.831104
18.983323	1027.403522	11.836109
18.770425	1011.943001	11.841114
18.772640	1017.121824	11.846119
18.759898	1025.228479	11.851123
19.018453	1023.113528	11.856128
19.039908	1023.807285	11.861133
18.939138	1020.989503	11.866138
19.379379	1027.262336	11.871143
18.862612	1018.338296	11.876147
18.969754	1024.870850	11.881152
18.735889	1028.844610	11.886157
19.097849	1022.989729	11.891162
19.007323	1031.783775	11.896167
19.017290	1043.717497	11.901171
19.367192	1043.800590	11.906176
19.320761	1044.983025	11.911181
19.174928	1046.309056	11.916186
19.500676	1045.989120	11.921191
19.537577	1052.879844	11.926195
19.651653	1043.973451	11.931200
19.630834	1045.817321	11.936205
19.556795	1053.064807	11.941210
19.688148	1058.680396	11.946215
19.867749	1076.296056	11.951219
20.034994	1071.930997	11.956224
19.995635	1080.899851	11.961229
20.049639	1082.843764	11.966234
20.594696	1083.245839	11.971239
19.908202	1063.840860	11.976243
20.066500	1071.798827	11.981248
20.226452	1072.319099	11.986253
20.389579	1069.260507	11.991258
20.576212	1068.822400	11.996263
20.174602	1055.614013	12.001267
20.426772	1055.777353	12.006272
20.333830	1055.897959	12.011277
20.380450	1060.396311	12.016282
20.287055	1052.570173	12.021287
20.293158	1070.357010	12.026291
20.619383	1064.384802	12.031296
20.148902	1072.892519	12.036301
20.385136	1077.467874	12.041306
20.613411	1074.370503	12.046311
20.287156	1071.555555	12.051315
20.447820	1074.696794	12.056320
20.329466	1077.552930	12.061325
20.473107	1073.185327	12.066330
20.407375	1067.844953	12.071335
20.383332	1067.173924	12.076339
20.579600	1045.970678	12.081344
20.464019	1052.024646	12.086349
20.574229	1048.976075	12.091354
20.758677	1046.915521	12.096359
20.278594	1055.169276	12.101363
20.776900	1045.006187	12.106368
20.593003	1053.435066	12.111373
20.582509	1049.502090	12.116378
20.857832	1049.120806	12.121383
20.685566	1051.026681	12.126387
20.712888	1047.764234	12.131392
20.483533	1047.367242	12.136397
20.560560	1047.728840	12.141402
20.762275	1034.305965	12.146407
20.376825	1037.311933	12.151411
20.590544	1031.602127	12.156416
20.414546	1026.828171	12.161421
20.629426	1031.692365	12.166426
20.244871	1034.576756	12.171431
19.865280	1039.808598	12.176435
20.187901	1029.429096	12.181440
20.058914	1027.427998	12.186445
20.448788	1049.586715	12.191450
20.493429	1048.450538	12.196455
20.391801	1053.097119	12.201459
20.393571	1034.282620	12.206464
20.392841	1045.156688	12.211469
20.210100	1033.334345	12.216474
20.462332	1046.970503	12.221479
20.790978	1052.130393	12.226483
20.599387	1047.549742	12.231488
20.238290	1042.026236	12.236493
20.286435	1040.514161	12.241498
20.559444	1042.404213	12.246503
20.439087	1042.128618	12.251507
20.631841	1041.049249	12.256512
20.692887	1042.190886	12.261517
20.515920	1043.818371	12.266522
20.578396	1040.327953	12.271527
20.354212	1041.962968	12.276531
20.556424	1031.485966	12.281536
20.793294	1035.099199	12.286541
20.530858	1037.956228	12.291546
20.805590	1033.537765	12.296551
20.472053	1040.522261	12.301555
20.652485	1029.745939	12.306560
20.089526	1021.736073	12.311565
20.481926	1025.266146	12.316570
20.498494	1035.831498	12.321575
20.359380	1033.141262	12.326579
20.701628	1010.291991	12.331584
20.294772	1017.365446	12.336589
20.049197	1009.478442	12.341594
20.371019	1015.109371	12.346599
20.664448	1025.528049	12.351603
20.654467	1013.417953	12.356608
20.257571	1016.499864	12.361613
20.450560	1008.897749	12.366618
20.750138	1003.833469	12.371623
20.270891	1008.354172	12.376627
20.420478	1006.078396	12.381632
20.171042	1001.574799	12.386637
20.166313	1008.640887	12.391642
20.387900	1011.974259	12.396647
20.156565	1008.410853	12.401651
20.299029	1023.094315	12.406656
20.475815	1040.041707	12.411661
20.484985	1045.782442	12.416666
20.227817	1023.393056	12.421671
20.466511	1036.574016	12.426675
20.457988	1028.422097	12.431680
20.317658	1017.707983	12.436685
20.404113	1027.218170	12.441690
20.646507	1016.293194	12.446695
20.325988	1013.422146	12.451699
20.245726	1009.129700	12.456704
20.077937	1025.220494	12.461709
20.479066	1041.425584	12.466714
20.628413	1045.680449	12.471719
20.459994	1046.689940	12.476723
20.291137	1024.931484	12.481728
20.223452	1038.583964	12.486733
20.379049	1048.168298	12.491738
20.645549	1053.754445	12.496743
20.519111	1044.190928	12.501747
20.434797	1026.304865	12.506752
20.302263	1022.279390	12.511757
20.087722	1021.638747	12.516762
20.522767	1029.621941	12.521767
20.306795	1044.715855	12.526771
20.576544	1044.144635	12.531776
20.333380	1021.503842	12.536781
20.105307	1029.032945	12.541786
20.293020	1036.823764	12.546791
20.378855	1048.505676	12.551795
20.883856	1045.466683	12.556800
20.371798	1034.333997	12.561805
20.058574	1024.109532	12.566810
20.327499	1039.586603	12.571815
20.157815	1058.547986	12.576819
20.814428	1057.662733	12.581824
20.657252	1052.739100	12.586829
20.640039	1034.318740	12.591834
20.492918	1024.026779	12.596839
20.311184	1026.711652	12.601843
20.632181	1020.027465	12.606848
20.609176	1023.950244	12.611853
20.448515	1015.672776	12.616858
20.271912	1008.116993	12.621863
20.034650	1001.201712	12.626867
19.874348	999.781238	12.631872
19.934112	1004.099268	12.636877
20.034979	1016.439543	12.641882
20.234503	1021.134283	12.646887
20.423818	1022.797968	12.651891
20.410269	1027.193935	12.656896
20.120132	1036.257956	12.661901
20.226723	1033.758783	12.666906
20.542778	1030.861900	12.671911
20.423177	1036.840804	12.676915
20.630601	1032.034080	12.681920
20.515429	1036.234932	12.686925
20.270515	1035.979204	12.691930
20.853303	1023.615272	12.696935
20.442971	1034.721830	12.701939
20.349366	1038.312074	12.706944
20.324124	1036.991489	12.711949
20.207556	1039.609196	12.716954
20.282011	1032.767193	12.721959
20.242570	1039.392524	12.726963
20.498810	1035.857009	12.731968
20.169234	1041.774781	12.736973
20.431587	1037.610621	12.741978
20.585350	1030.240271	12.746983
20.314827	1029.318377	12.751987
20.416628	1030.377814	12.756992
20.500345	1030.468667	12.761997
20.332574	1041.598048	12.767002
20.479797	1036.737842	12.772007
20.147743	1045.177730	12.777011
20.448911	1034.002076	12.782016
20.243475	1044.232234	12.787021
20.415552	1046.113152	12.792026
20.519831	1043.418790	12.797031
20.436210	1049.149093	12.802035
20.703608	1050.907568	12.807040
20.533521	1050.745568	12.812045
20.487468	1043.955899	12.817050
20.715124	1045.495192	12.822055
19.874446	1035.234990	12.827059
20.404799	1039.413314	12.832064
20.278604	1046.749546	12.837069
20.086031	1047.357584	12.842074
20.495854	1040.522016	12.847079
20.189500	1051.955802	12.852083
20.371270	1044.084204	12.857088
20.372848	1047.761778	12.862093
20.597257	1052.987183	12.867098
20.810479	1040.630138	12.872103
20.513430	1055.230758	12.877107
20.684759	1044.679819	12.882112
20.457412	1035.074052	12.887117
20.086439	1032.181083	12.892122
20.658369	1027.633213	12.897127
20.367665	1030.154104	12.902131
20.339749	1010.685159	12.907136
20.304444	1019.676985	12.912141
20.029297	1026.995961	12.917146
20.551295	1032.735327	12.922151
20.533533	1049.680642	12.927155
20.296945	1042.976559	12.932160
20.413278	1045.451457	12.937165
20.718492	1045.413936	12.942170
20.700204	1028.622859	12.947175
20.365569	1031.105022	12.952179
20.362626	1019.432221	12.957184
20.383089	1021.629073	12.962189
20.358367	1024.452916	12.967194
20.462346	1019.746280	12.972199
20.292412	1025.518727	12.977203
20.693472	1015.927870	12.982208
20.216859	1015.226517	12.987213
20.482185	1015.190626	12.992218
20.301376	1018.941441	12.997223
20.201518	1024.606511	13.002227
20.448416	1017.957799	13.007232
20.142641	1026.048110	13.012237
19.980285	1025.272978	13.017242
20.557597	1031.069758	13.022247
20.580739	1053.875216	13.027251
20.528250	1034.637255	13.032256
20.377444	1031.161932	13.037261
20.435716	1024.172694	13.042266
20.588581	1015.696976	13.047271
20.152096	1026.962251	13.052275
20.492906	1018.625301	13.057280
20.386688	1020.359778	13.062285
20.190804	1028.451487	13.067290
20.198160	1027.073661	13.072295
20.181801	1036.959822	13.077299
20.330825	1051.569721	13.082304
20.544599	1060.575465	13.087309
20.485918	1063.053048	13.092314
20.658949	1040.055665	13.097319
20.244395	1035.359182	13.102323
20.322050	1026.136889	13.107328
20.268700	1023.002439	13.112333
20.688814	1044.976540	13.117338
20.906458	1035.785533	13.122343
20.511641	1038.184250	13.127347
20.460540	1020.543649	13.132352
20.429880	1026.197682	13.137357
20.174797	1030.250525	13.142362
20.529979	1019.870567	13.147367
19.940875	1026.809081	13.152371
20.203246	1031.249356	13.157376
19.949235	1026.276517	13.162381
19.932724	1046.260621	13.167386
20.317069	1055.827400	13.172391
20.507977	1064.945612	13.177395
20.680409	1060.122381	13.182400
20.410292	1061.051892	13.187405
20.743873	1058.735722	13.192410
20.748200	1050.846686	13.197415
20.182756	1045.368388	13.202419
20.230133	1037.620737	13.207424
20.425418	1030.239034	13.212429
20.324620	1039.794865	13.217434
20.315689	1028.561435	13.222439
20.458171	1039.516743	13.227443
20.496014	1042.513550	13.232448
20.318751	1039.657498	13.237453
20.388116	1044.227915	13.242458
20.816649	1025.078838	13.247463
20.657114	1036.063388	13.252467
20.326841	1033.170237	13.257472
20.622760	1032.415059	13.262477
20.387938	1035.368615	13.267482
20.581007	1028.878304	13.272487
20.408152	1030.443626	13.277491
20.717387	1029.246325	13.282496
20.602192	1033.481874	13.287501
20.445670	1031.267534	13.292506
20.745153	1022.646994	13.297511
20.175465	1030.998611	13.302515
20.306307	1028.757362	13.307520
20.457126	1025.847409	13.312525
20.662022	1024.870190	13.317530
20.825765	1028.280605	13.322535
20.716632	1025.798492	13.327539
20.315573	1004.354664	13.332544
20.380231	998.790078	13.337549
20.378462	1002.605379	13.342554
20.360044	990.944531	13.347559
20.272222	991.941163	13.352563
20.393347	994.555646	13.357568
20.296640	999.146229	13.362573
20.164787	1012.589708	13.367578
20.597243	1025.728716	13.372583
20.312716	1023.824971	13.377587
20.463109	1024.028200	13.382592
20.373298	1023.104294	13.387597
20.483600	1034.716056	13.392602
20.547430	1019.306013	13.397607
20.284875	1005.078792	13.402611
20.116003	1005.544268	13.407616
20.395250	1014.014380	13.412621
20.537932	1027.133370	13.417626
20.389316	1030.207226	13.422631
20.042319	1032.921612	13.427635
20.444688	1025.046381	13.432640
20.369498	1035.269952	13.437645
20.297057	1035.161769	13.442650
20.698331	1032.647136	13.447655
20.787308	1029.702888	13.452659
20.356877	1021.928945	13.457664
20.403439	1009.249978	13.462669
20.064709	1011.772218	13.467674
20.365641	1015.753722	13.472679
20.457443	1033.195663	13.477683
20.820889	1023.863130	13.482688
20.756787	1017.286100	13.487693
20.621284	1012.824256	13.492698
20.834891	1010.982998	13.497703
20.466345	1003.178693	13.502707
20.336022	1005.669269	13.507712
20.829691	1008.697453	13.512717
20.318235	1016.388450	13.517722
20.416774	1008.821901	13.522727
20.071173	1010.654486	13.527731
20.509820	1011.947221	13.532736
20.475312	1008.631561	13.537741
20.134888	1016.188039	13.542746
20.626337	1006.544922	13.547751
20.868360	1012.216964	13.552755
20.234524	1005.527369	13.557760
20.263769	1010.452704	13.562765
20.206417	1009.682905	13.567770
20.314324	1007.656643	13.572775
20.203478	1012.703677	13.577779
20.367975	1010.035989	13.582784
20.213305	1011.182065	13.587789
20.311488	1016.490671	13.592794
20.248328	1007.253000	13.597799
19.997665	1016.943113	13.602803
20.188150	1006.966350	13.607808
20.222851	1008.556916	13.612813
20.034753	1013.485377	13.617818
20.451104	1014.024680	13.622823
20.217694	1018.539295	13.627827
20.517377	1031.814609	13.632832
20.362716	1030.481548	13.637837
20.451900	1019.822296	13.642842
20.376601	1017.878873	13.647847
20.441989	1013.673589	13.652851
20.420258	1023.066979	13.657856
20.461546	1018.378227	13.662861
20.181367	1012.354515	13.667866
20.469419	1018.583804	13.672871
20.484286	1023.093517	13.677875
20.424080	1016.780812	13.682880
20.415411	1017.482528	13.687885
20.086485	1022.417682	13.692890
20.346614	1027.787201	13.697895
20.385213	1039.506603	13.702899
20.714311	1037.814090	13.707904
20.576680	1024.243485	13.712909
20.379496	1018.271193	13.717914
20.249993	1014.585882	13.722919
20.163094	1025.284431	13.727923
20.379825	1026.107903	13.732928
20.350560	1018.549117	13.737933
20.400567	1021.616524	13.742938
20.571769	1024.823885	13.747943
20.510562	1028.661289	13.752947
20.014816	1022.416471	13.757952
20.533396	1023.466208	13.762957
20.524994	1029.930455	13.767962
20.321938	1024.222466	13.772967
20.344112	1028.759402	13.777971
20.314630	1028.929814	13.782976
20.533310	1023.100941	13.787981
20.226979	1028.333711	13.792986
20.360374	1028.389831	13.797991
20.443649	1035.318884	13.802995
20.165426	1032.497861	13.808000
20.322798	1034.458399	13.813005
20.604983	1044.645479	13.818010
20.745839	1039.565499	13.823015
20.473062	1033.425472	13.828019
20.211548	1027.487093	13.833024
20.404107	1021.769626	13.838029
20.300748	1025.339344	13.843034
20.638898	1014.865905	13.848039
20.809270	1019.330312	13.853043
20.550732	1028.616386	13.858048
20.474652	1024.156100	13.863053
20.391238	1027.106007	13.868058
20.643937	1020.301818	13.873063
20.638299	1027.511572	13.878067
20.292299	1021.313838	13.883072
20.598021	1022.973151	13.888077
20.229601	1029.778690	13.893082
20.638856	1020.104516	13.898087
20.212943	1025.219154	13.903091
20.334049	1025.395513	13.908096
20.267629	1017.397923	13.913101
20.111683	1027.878813	13.918106
20.754855	1027.621798	13.923111
20.381810	1031.568868	13.928115
20.248808	1023.318525	13.933120
20.637296	1019.208374	13.938125
20.300245	1024.119591	13.943130
20.342390	1021.830985	13.948135
20.381415	1023.037638	13.953139
20.581378	1023.368588	13.958144
20.529103	1022.306222	13.963149
20.559353	1034.340787	13.968154
20.950946	1027.993867	13.973159
20.448708	1027.884844	13.978163
20.356387	1029.530367	13.983168
20.520024	1025.698943	13.988173
20.477947	1022.751943	13.993178
20.243068	998.658970	13.998183
19.983256	1009.877129	14.003187
20.330958	1013.296049	14.008192
20.551355	1019.709708	14.013210
20.436694	1026.037562	14.018227
20.571011	1027.878733	14.023245
20.542200	1030.842329	14.028263
20.204619	1025.549542	14.033280
20.507271	1024.529254	14.038298
20.383972	1027.951516	14.043315
20.507558	1026.368326	14.048333
20.683745	1031.199453	14.053351
20.165452	1037.681352	14.058368
20.727829	1033.111766	14.063386
20.439897	1033.787024	14.068403
20.421735	1027.996548	14.073421
20.405103	1037.110348	14.078439
20.573537	1032.776629	14.083456
20.726514	1030.948076	14.088474
20.532460	1035.778482	14.093491
20.612868	1031.954309	14.098509
20.397381	1031.122054	14.103527
20.445521	1030.672473	14.108544
20.794268	1029.931125	14.113562
20.340795	1042.767194	14.118579
20.678246	1034.538417	14.123597
20.701955	1041.578816	14.128615
20.676840	1059.855356	14.133632
21.001300	1068.850279	14.138650
20.803243	1069.904465	14.143667
20.939883	1068.224806	14.148685
20.899390	1072.895450	14.153703
20.863604	1065.512706	14.158720
21.226707	1071.317634	14.163738
20.382424	1066.107222	14.168755
20.693956	1060.242125	14.173773
20.824967	1070.782740	14.178791
20.839612	1069.413552	14.183808
21.013466	1064.249967	14.188826
21.005571	1078.578601	14.193843
21.121695	1077.229406	14.198861
21.013928	1066.960600	14.203879
20.949433	1072.320917	14.208896
21.008356	1069.066456	14.213914
20.716332	1075.940150	14.218931
21.043997	1071.467763	14.223949
20.960417	1066.378270	14.228967
20.792386	1079.757161	14.233984
21.334567	1083.647456	14.239002
21.388554	1096.482859	14.244019
21.340095	1084.927270	14.249037
21.228237	1082.087013	14.254055
21.080867	1075.233300	14.259072
21.300047	1088.737633	14.264090
21.273573	1102.922961	14.269107
21.721400	1088.618758	14.274125
21.462183	1085.149191	14.279143
21.069969	1082.668258	14.284160
21.149799	1094.483352	14.289178
20.772841	1102.103643	14.294195
21.415323	1109.029652	14.299213
21.398225	1107.777209	14.304231
21.209356	1119.512483	14.309248
21.470783	1104.682709	14.314266
21.445085	1116.461169	14.319283
21.586271	1110.355804	14.324301
21.456664	1108.573886	14.329319
21.491142	1115.291702	14.334336
21.673694	1112.940890	14.339354
21.682428	1110.687016	14.344371
21.724551	1108.281524	14.349389
21.465100	1117.470283	14.354407
21.479245	1109.477077	14.359424
21.827008	1109.001727	14.364442
21.675332	1111.130772	14.369459
21.596275	1110.261023	14.374477
21.822451	1115.626906	14.379495
21.784560	1122.505707	14.384512
21.529417	1112.864424	14.389530
21.723584	1115.061007	14.394547
21.598366	1114.008281	14.399565
21.755945	1118.741731	14.404583
21.702834	1119.156168	14.409600
22.025552	1113.570841	14.414618
21.614717	1114.696719	14.419635
21.595887	1116.068392	14.424653
21.921279	1123.655325	14.429671
21.833220	1132.733385	14.434688
22.101480	1124.775147	14.439706
21.867962	1142.647724	14.444723
21.885497	1131.979782	14.449741
21.780920	1141.480487	14.454759
21.748790	1140.861231	14.459776
21.999241	1137.742950	14.464794
21.974588	1149.167334	14.469811
21.884625	1146.367617	14.474829
22.355531	1142.616415	14.479847
22.170556	1136.147776	14.484864
22.171333	1137.336996	14.489882
22.047817	1139.857962	14.494899
22.035190	1136.751753	14.499917
21.998574	1142.928780	14.504935
22.212719	1139.460781	14.509952
22.482838	1131.148307	14.514970
22.274976	1143.363262	14.519987
22.362001	1141.817352	14.525005
22.325826	1138.714898	14.530023
22.239090	1143.326872	14.535040
22.369212	1135.533807	14.540058
22.323738	1137.908617	14.545075
22.571792	1137.192763	14.550093
22.739114	1134.547071	14.555111
22.171185	1143.640326	14.560128
22.419353	1131.680308	14.565146
22.510862	1146.713610	14.570163
22.678455	1131.356073	14.575181
22.784509	1131.734113	14.580199
22.575121	1138.879377	14.585216
22.424181	1128.820336	14.590234
22.528125	1129.934899	14.595251
22.799941	1136.275092	14.600269
22.741182	1131.713307	14.605287
22.475590	1142.822179	14.610304
22.642984	1128.995252	14.615322
22.556749	1140.229675	14.620339
22.682041	1137.293380	14.625357
22.929231	1135.427766	14.630375
23.045102	1143.076441	14.635392
23.115129	1134.069130	14.640410
22.862102	1128.599222	14.645427
22.566643	1114.838266	14.650445
22.551643	1120.248909	14.655463
22.417953	1129.571776	14.660480
22.773494	1129.617437	14.665498
22.725009	1139.014811	14.670515
22.400843	1134.303444	14.675533
22.846240	1135.988047	14.680551
23.074988	1130.079496	14.685568
22.893488	1130.646547	14.690586
22.817675	1135.931613	14.695603
22.692675	1127.166201	14.700621
23.002487	1125.145879	14.705639
22.556772	1132.366587	14.710656
23.165183	1133.108103	14.715674
22.985785	1135.409889	14.720691
22.826940	1131.177104	14.725709
22.939641	1138.706731	14.730727
23.080644	1152.564944	14.735744
23.164095	1158.895864	14.740762
23.410532	1161.862778	14.745779
23.170891	1155.792965	14.750797
23.316554	1134.296164	14.755815
23.173637	1140.375312	14.760832
23.559795	1138.322363	14.765850
23.338175	1139.394469	14.770867
22.915331	1137.796172	14.775885
23.228854	1139.995745	14.780903
23.199432	1152.495284	14.785920
23.321121	1158.709992	14.790938
23.600572	1167.016867	14.795955
23.543019	1159.398443	14.800973
23.676882	1152.089272	14.805991
23.078516	1140.860449	14.811008
23.251824	1148.828734	14.816026
23.698495	1153.509794	14.821043
23.252207	1160.364086	14.826061
23.471097	1162.012458	14.831079
23.631901	1161.862659	14.836096
23.705845	1154.303491	14.841114
23.681873	1163.465732	14.846131
23.529682	1147.918505	14.851149
23.368483	1143.560248	14.856167
23.431095	1158.090076	14.861184
23.539395	1157.527074	14.866202
23.759712	1161.934349	14.871219
23.592623	1166.499370	14.876237
23.672311	1165.000247	14.881255
23.825780	1168.582895	14.886272
23.515316	1156.638021	14.891290
23.703654	1162.749290	14.896307
23.477903	1166.389275	14.901325
23.854134	1162.156085	14.906343
23.751514	1164.999344	14.911360
23.582829	1164.601644	14.916378
23.567313	1169.564069	14.921395
23.557474	1158.543391	14.926413
23.730939	1156.433126	14.931431
23.614858	1169.830556	14.936448
23.756276	1183.059511	14.941466
23.944146	1189.880313	14.946483
24.090506	1190.703392	14.951501
24.218415	1191.184915	14.956519
24.049556	1191.049942	14.961536
23.946158	1195.071549	14.966554
24.494683	1184.447869	14.971571
24.089954	1188.613491	14.976589
24.620215	1187.209245	14.981607
24.328134	1180.625532	14.986624
24.407162	1162.903632	14.991642
24.037812	1151.602093	14.996659
23.838182	1157.492090	15.001677
24.236150	1160.922481	15.006695
24.336775	1169.528444	15.011712
24.430729	1174.709368	15.016730
24.608344	1162.622148	15.021747
24.203262	1164.862405	15.026765
24.011104	1160.660093	15.031783
24.369070	1170.571544	15.036800
24.478890	1178.778063	15.041818
24.620198	1179.874085	15.046835
24.174672	1181.880118	15.051853
24.487684	1181.168060	15.056871
24.597627	1186.727117	15.061888
24.566171	1183.855139	15.066906
24.522402	1183.645158	15.071923
24.488977	1188.678087	15.076941
24.212313	1190.721684	15.081959
24.270861	1189.266830	15.086976
24.583787	1187.455220	15.091994
24.429797	1186.934050	15.097011
24.160744	1189.748802	15.102029
24.526948	1182.257839	15.107047
24.936627	1186.400534	15.112064
24.453213	1195.371801	15.117082
24.742567	1188.678045	15.122099
24.351498	1191.828442	15.127117
24.446054	1194.866778	15.132135
24.560158	1200.274164	15.137152
24.641601	1208.417585	15.142170
24.867364	1218.109475	15.147187
24.875429	1226.709785	15.152205
25.143220	1219.472030	15.157223
24.948766	1217.517967	15.162240
25.097246	1220.049049	15.167258
25.236666	1222.776635	15.172275
24.829559	1204.705922	15.177293
24.785009	1200.760060	15.182311
24.768358	1209.902286	15.187328
24.978537	1214.908955	15.192346
25.426198	1218.098622	15.197363
25.016600	1228.406245	15.202381
25.323048	1217.958007	15.207399
25.484138	1225.991206	15.212416
25.038687	1208.194023	15.217434
25.127243	1189.569210	15.222451
25.101397	1220.024654	15.227469
25.665684	1207.671228	15.232487
25.119601	1204.558850	15.237504
25.118918	1195.658735	15.242522
25.429199	1201.547648	15.247539
25.257584	1209.276817	15.252557
25.557113	1204.392019	15.257575
25.325872	1195.432720	15.262592
24.827051	1190.837282	15.267610
25.442570	1204.198284	15.272627
25.640813	1221.141634	15.277645
25.429260	1214.335844	15.282663
25.822508	1220.005462	15.287680
25.532078	1217.067815	15.292698
25.956255	1201.710180	15.297715
25.174611	1198.736048	15.302733
25.524311	1206.411958	15.307751
25.541191	1212.729924	15.312768
25.606903	1221.335193	15.317786
25.867057	1214.597318	15.322803
25.903050	1219.021424	15.327821
25.604371	1199.056767	15.332839
25.787670	1199.274622	15.337856
25.458140	1195.297134	15.342874
25.880870	1211.657245	15.347891
25.606324	1212.948586	15.352909
25.734208	1214.701144	15.357927
25.892334	1214.921440	15.362944
25.668450	1219.418456	15.367962
25.936497	1217.945915	15.372979
25.727992	1228.668214	15.377997
25.816368	1226.308809	15.383015
25.716267	1221.641903	15.388032
26.011846	1222.743211	15.393050
26.007265	1224.669484	15.398067
25.664378	1223.706524	15.403085
25.765821	1218.771515	15.408103
25.980281	1223.447162	15.413120
26.106937	1227.060844	15.418138
25.866471	1212.392808	15.423155
25.891715	1219.569904	15.428173
25.644920	1223.103145	15.433191
26.034562	1221.933687	15.438208
25.951652	1244.120860	15.443226
26.475758	1243.442772	15.448243
26.263840	1258.103004	15.453261
26.258002	1245.941153	15.458279
26.133443	1238.962598	15.463296
25.836204	1256.183219	15.468314
26.138862	1242.869452	15.473331
26.149746	1249.660308	15.478349
26.186084	1247.409875	15.483367
26.544630	1245.378619	15.488384
26.264374	1249.167320	15.493402
26.534622	1246.822951	15.498419
26.096271	1256.402133	15.503437
26.407847	1246.799364	15.508455
26.708188	1240.689011	15.513472
26.481188	1254.826244	15.518490
26.711400	1256.549901	15.523507
26.277481	1252.030610	15.528525
26.382695	1252.455979	15.533543
26.509863	1247.913268	15.538560
26.250800	1251.579037	15.543578
26.625909	1262.590532	15.548595
26.948844	1277.609082	15.553613
26.873798	1273.115919	15.558631
27.143125	1264.787765	15.563648
26.744035	1254.244385	15.568666
26.798846	1251.072339	15.573683
26.822762	1239.347777	15.578701
26.714401	1228.740744	15.583719
26.873140	1248.949802	15.588736
26.969323	1261.827386	15.593754
27.156782	1256.976176	15.598771
26.958154	1256.419650	15.603789
26.884286	1247.682190	15.608807
27.202702	1236.330667	15.613824
26.982129	1250.570693	15.618842
26.679492	1250.131432	15.623859
27.127344	1259.190166	15.628877
27.311185	1265.972321	15.633895
27.476284	1267.932886	15.638912
26.825065	1259.252894	15.643930
26.998827	1255.468831	15.648947
27.256560	1268.397735	15.653965
27.289550	1281.063614	15.658983
27.552221	1268.056656	15.664000
27.265959	1261.258041	15.669018
27.532696	1250.702853	15.674035
27.259135	1244.345824	15.679053
27.225634	1245.801648	15.684071
27.446421	1240.893215	15.689088
27.324077	1250.242665	15.694106
27.191824	1235.236442	15.699123
27.307759	1256.325385	15.704141
27.418752	1272.601575	15.709159
27.637076	1261.583755	15.714176
27.516175	1267.514723	15.719194
27.445148	1275.386764	15.724211
27.824883	1269.551606	15.729229
27.461104	1262.098376	15.734247
27.617195	1267.865614	15.739264
27.693188	1265.816498	15.744282
27.734632	1257.060640	15.749299
27.931806	1260.866008	15.754317
27.768774	1246.973691	15.759335
27.616445	1241.470375	15.764352
27.682351	1238.710276	15.769370
27.847107	1252.264342	15.774387
27.913501	1261.069305	15.779405
27.660112	1256.132673	15.784423
27.532938	1254.345630	15.789440
27.441928	1266.660031	15.794458
27.687587	1268.357630	15.799475
27.908261	1266.082514	15.804493
27.711215	1275.429736	15.809511
27.894870	1259.119373	15.814528
28.039559	1271.091011	15.819546
28.231227	1268.476020	15.824563
28.344831	1270.954471	15.829581
28.076943	1260.920282	15.834599
28.269264	1263.466403	15.839616
27.991738	1271.725316	15.844634
28.246731	1270.353955	15.849651
28.457646	1270.564260	15.854669
28.012914	1270.117774	15.859687
28.161424	1267.688995	15.864704
28.195101	1268.242181	15.869722
28.502496	1271.133327	15.874739
28.221792	1263.292457	15.879757
28.177286	1267.888296	15.884775
28.141461	1264.252491	15.889792
28.236795	1262.425239	15.894810
28.174540	1258.236788	15.899827
28.085218	1259.380611	15.904845
28.153774	1284.592281	15.909863
28.498494	1281.372416	15.914880
28.497554	1288.854178	15.919898
28.726383	1290.219401	15.924915
28.756399	1296.319798	15.929933
28.591784	1290.975729	15.934951
28.929155	1286.588249	15.939968
28.611253	1294.507540	15.944986
28.458087	1282.889840	15.950003
28.640979	1284.960830	15.955021
28.379562	1294.647101	15.960039
28.935369	1296.392768	15.965056
28.938856	1304.548676	15.970074
28.971521	1306.634191	15.975091
28.902157	1300.913122	15.980109
29.039819	1302.620085	15.985127
28.837886	1283.690688	15.990144
28.565097	1281.080557	15.995162
28.423225	1288.029504	16.000179
29.013908	1293.524513	16.005197
28.888139	1303.140390	16.010215
29.114255	1301.234071	16.015232
29.023486	1295.956876	16.020250
28.906254	1300.018471	16.025267
29.209102	1297.499003	16.030285
29.141948	1298.271197	16.035303
29.081087	1291.969887	16.040320
29.296121	1292.091444	16.045338
29.030913	1300.139190	16.050355
28.969501	1293.441555	16.055373
28.609249	1297.862814	16.060391
28.866214	1287.353205	16.065408
28.824112	1298.149690	16.070426
29.182497	1314.826929	16.075443
29.652210	1322.762193	16.080461
29.555820	1328.462755	16.085479
29.783940	1318.601108	16.090496
29.669299	1292.899881	16.095514
29.417068	1293.586759	16.100531
29.634092	1280.852918	16.105549
29.309544	1295.148897	16.110567
29.459949	1284.928425	16.115584
29.687481	1293.182304	16.120602
29.588887	1296.070565	16.125619
29.579320	1289.558150	16.130637
29.431070	1300.016054	16.135655
29.840501	1310.709072	16.140672
29.870193	1316.070187	16.145690
29.626542	1308.678000	16.150707
30.095873	1309.812953	16.155725
29.816464	1297.545249	16.160743
29.706273	1289.707058	16.165760
29.777608	1297.177296	16.170778
29.879447	1308.871076	16.175795
30.146005	1307.206850	16.180813
29.811481	1303.398446	16.185831
29.792104	1295.756558	16.190848
29.730793	1308.590089	16.195866
29.915249	1325.516882	16.200883
30.139150	1315.898163	16.205901
29.855962	1322.888542	16.210919
29.832740	1321.070753	16.215936
29.516642	1327.484348	16.220954
29.831443	1327.770896	16.225971
30.055748	1322.460744	16.230989
29.706258	1321.643551	16.236007
30.112584	1323.509020	16.241024
30.128302	1314.363964	16.246042
30.328902	1337.589905	16.251059
30.420520	1342.624966	16.256077
30.464427	1341.211759	16.261095
30.234363	1336.606443	16.266112
30.412439	1331.213995	16.271130
30.434031	1342.697225	16.276147
30.431392	1334.299146	16.281165
30.492927	1350.466904	16.286183
30.657884	1347.728741	16.291200
30.477984	1328.630599	16.296218
30.667796	1322.680990	16.301235
30.592619	1315.924190	16.306253
30.350716	1315.722211	16.311271
30.442652	1338.731098	16.316288
30.810672	1337.126194	16.321306
30.436318	1340.760034	16.326323
30.874937	1333.070250	16.331341
30.601304	1342.805693	16.336359
30.735551	1342.306188	16.341376
30.706991	1344.885979	16.346394
30.499792	1343.775523	16.351411
30.767532	1334.170250	16.356429
30.653453	1342.064924	16.361447
30.598242	1344.425589	16.366464
30.723531	1346.425549	16.371482
30.656289	1351.021894	16.376499
30.953313	1342.568152	16.381517
30.771329	1353.695311	16.386535
30.993419	1367.736644	16.391552
31.182128	1365.919656	16.396570
31.137371	1377.046182	16.401587
31.153174	1371.464090	16.406605
31.066348	1376.204356	16.411623
31.123630	1377.901339	16.416640
31.400878	1371.116620	16.421658
31.598418	1371.914243	16.426675
31.511043	1359.032249	16.431693
31.070140	1360.150355	16.436711
31.238838	1367.738813	16.441728
31.485118	1368.505853	16.446746
31.431272	1381.099935	16.451763
31.655617	1374.502983	16.456781
31.634074	1379.983195	16.461799
31.337561	1357.947021	16.466816
31.547773	1357.998560	16.471834
31.600681	1376.165524	16.476851
31.874627	1362.082275	16.481869
31.596406	1354.159160	16.486887
31.371404	1352.954012	16.491904
31.741660	1346.734934	16.496922
31.698929	1363.403842	16.501939
31.982352	1355.875655	16.506957
31.760788	1344.539382	16.511975
31.780004	1338.706639	16.516992
31.479217	1335.448140	16.522010
31.741282	1350.438721	16.527027
31.973592	1362.531745	16.532045
31.834878	1363.458505	16.537063
31.833411	1369.279227	16.542080
32.004348	1374.705929	16.547098
31.625690	1376.245917	16.552115
31.398101	1370.347916	16.557133
31.727977	1369.945414	16.562151
31.979181	1371.865519	16.567168
31.900005	1362.553091	16.572186
31.819573	1368.678999	16.577203
31.867501	1361.173424	16.582221
31.852999	1375.670937	16.587239
32.045299	1383.178558	16.592256
32.500103	1390.343858	16.597274
32.251709	1402.432569	16.602291
32.229945	1389.794922	16.607309
32.633730	1400.443288	16.612327
32.459228	1394.079045	16.617344
32.395142	1384.048447	16.622362
32.467057	1391.871797	16.627379
32.825848	1374.731104	16.632397
32.664012	1368.858797	16.637415
32.655784	1365.238228	16.642432
32.712438	1361.737878	16.647450
32.579007	1368.192359	16.652467
32.650716	1368.947128	16.657485
32.857392	1365.747690	16.662503
32.618509	1368.346872	16.667520
32.761515	1364.421390	16.672538
32.640645	1360.457768	16.677555
32.687342	1367.121054	16.682573
32.781226	1374.877181	16.687591
32.523347	1373.039394	16.692608
32.707975	1365.106949	16.697626
32.454053	1372.037626	16.702643
32.902742	1379.858295	16.707661
32.908330	1390.983094	16.712679
32.496283	1392.664480	16.717696
32.858916	1396.768335	16.722714
32.665037	1398.847522	16.727731
33.088035	1391.459869	16.732749
33.082846	1396.769161	16.737767
32.885111	1396.077202	16.742784
33.154104	1389.501437	16.747802
33.167047	1399.324924	16.752819
33.381760	1393.792898	16.757837
33.239733	1400.967660	16.762855
32.931099	1398.520532	16.767872
33.059942	1392.679722	16.772890
33.066341	1398.885392	16.777907
33.404320	1397.285273	16.782925
33.186726	1391.001838	16.787943
33.325489	1395.967263	16.792960
33.520208	1393.661660	16.797978
33.177656	1399.543873	16.802995
33.632240	1409.509294	16.808013
33.922218	1410.510835	16.813031
33.507834	1399.733825	16.818048
33.649275	1396.951425	16.823066
33.610053	1393.539506	16.828083
33.507913	1391.952952	16.833101
33.571624	1396.213811	16.838119
33.767127	1407.485305	16.843136
33.673146	1407.069390	16.848154
33.368181	1421.208207	16.853171
33.473520	1425.142314	16.858189
33.732460	1422.728932	16.863207
33.617338	1426.048519	16.868224
33.576174	1423.117479	16.873242
33.759758	1430.301674	16.878259
33.953158	1423.843346	16.883277
33.879061	1424.058211	16.888295
33.738606	1431.311391	16.893312
34.024088	1419.441930	16.898330
33.982368	1422.274740	16.903347
33.908718	1435.346311	16.908365
34.287773	1434.258754	16.913383
34.402348	1447.577965	16.918400
34.309128	1443.548561	16.923418
33.896882	1435.682171	16.928435
34.291467	1440.593438	16.933453
34.782465	1444.603686	16.938471
34.086301	1438.759939	16.943488
34.327799	1441.859839	16.948506
34.447937	1446.749597	16.953523
34.142776	1442.727253	16.958541
34.899036	1445.913374	16.963559
34.570171	1447.046651	16.968576
34.384146	1443.373406	16.973594
34.229221	1450.403166	16.978611
34.744131	1436.639291	16.983629
34.927905	1441.077649	16.988647
34.827431	1454.189697	16.993664
34.867339	1447.765278	16.998682
34.622967	1441.450698	17.003699
34.762321	1440.601938	17.008717
34.808633	1446.618785	17.013735
34.960118	1442.153936	17.018752
34.989586	1444.164473	17.023770
34.678196	1445.887228	17.028787
34.919587	1447.919810	17.033805
35.374777	1442.211768	17.038823
35.212036	1441.398605	17.043840
34.775986	1426.533448	17.048858
34.850523	1426.695505	17.053875
34.989747	1435.886162	17.058893
34.956787	1442.670729	17.063911
34.923811	1445.789236	17.068928
34.885014	1444.193360	17.073946
34.958713	1440.703643	17.078963
35.082559	1444.896722	17.083981
35.082602	1439.818143	17.088999
35.053160	1441.271766	17.094016
34.986765	1434.737673	17.099034
34.828129	1446.160850	17.104051
34.909893	1461.209404	17.109069
35.448204	1471.049039	17.114087
35.688214	1473.945468	17.119104
35.642377	1475.634526	17.124122
35.447681	1470.331369	17.129139
35.356763	1475.116367	17.134157
35.651604	1472.447131	17.139175
35.447517	1481.374021	17.144192
35.815016	1474.426204	17.149210
35.428696	1465.412030	17.154227
35.393131	1479.833565	17.159245
35.756360	1467.052648	17.164263
35.815252	1470.004706	17.169280
35.597643	1467.430572	17.174298
35.740495	1468.664016	17.179315
35.444455	1475.424487	17.184333
35.736619	1471.889695	17.189351
35.917150	1486.165870	17.194368
35.965515	1503.837409	17.199386
35.995926	1503.189286	17.204403
36.163053	1510.706494	17.209421
36.366035	1503.268929	17.214439
36.244797	1498.626541	17.219456
36.482434	1486.665552	17.224474
36.188035	1473.711864	17.229491
36.098089	1464.719638	17.234509
36.032749	1462.738655	17.239527
36.098186	1482.842579	17.244544
36.137225	1488.807119	17.249562
36.440505	1490.578143	17.254579
36.336322	1495.775839	17.259597
36.875872	1490.213206	17.264615
36.556736	1491.361452	17.269632
36.527152	1495.491709	17.274650
36.692496	1495.867382	17.279667
36.504589	1497.502019	17.284685
36.704502	1484.872981	17.289703
36.736506	1500.266939	17.294720
36.665395	1499.646019	17.299738
37.059148	1491.066648	17.304755
36.574719	1475.671948	17.309773
36.733511	1474.902673	17.314791
36.676209	1476.736710	17.319808
36.776366	1484.835615	17.324826
36.806079	1493.858936	17.329843
36.727210	1491.460093	17.334861
36.817818	1491.879934	17.339879
36.707958	1493.374703	17.344896
36.670351	1485.052903	17.349914
36.839709	1489.191544	17.354931
37.179040	1495.400000	17.359949
36.846396	1493.637831	17.364967
36.728011	1503.126815	17.369984
36.905696	1495.878127	17.375002
36.960598	1498.725429	17.380019
37.028028	1514.579386	17.385037
37.296753	1509.652994	17.390055
37.453816	1511.505545	17.395072
37.651304	1522.237242	17.400090
37.785835	1509.015331	17.405107
37.294329	1490.806702	17.410125
37.461427	1484.835480	17.415143
37.465257	1481.400157	17.420160
37.528346	1482.915321	17.425178
37.601132	1475.890233	17.430195
37.329540	1486.205128	17.435213
37.573618	1487.864466	17.440231
37.533223	1504.681819	17.445248
37.552111	1515.342105	17.450266
37.604964	1512.681568	17.455283
37.798557	1517.012201	17.460301
37.733902	1509.070669	17.465319
37.782438	1525.254067	17.470336
37.759384	1521.949656	17.475354
37.945367	1513.203627	17.480371
37.951272	1515.236808	17.485389
38.054334	1516.475816	17.490407
37.788237	1520.922238	17.495424
37.495475	1519.017632	17.500442
37.810683	1513.794377	17.505459
37.833508	1518.489673	17.510477
37.880706	1517.014573	17.515495
37.984993	1537.313732	17.520512
37.932065	1543.593423	17.525530
38.072358	1541.326365	17.530547
38.012585	1548.134135	17.535565
38.231614	1542.224610	17.540583
38.160883	1547.178666	17.545600
38.128409	1542.152430	17.550618
38.120987	1544.692703	17.555635
38.054870	1554.959931	17.560653
38.477621	1560.275753	17.565671
38.274740	1568.599222	17.570688
38.405812	1580.305862	17.575706
38.534420	1571.137134	17.580723
38.402560	1581.354302	17.585741
38.675706	1578.346359	17.590759
38.879102	1576.439696	17.595776
38.597899	1579.165219	17.600794
38.964526	1567.399106	17.605811
38.888093	1582.222894	17.610829
38.721170	1570.513558	17.615847
38.903738	1568.174471	17.620864
38.715260	1575.590331	17.625882
39.063246	1569.922935	17.630899
38.772062	1577.926996	17.635917
38.805699	1573.622482	17.640935
38.653963	1570.893099	17.645952
39.049023	1578.796366	17.650970
39.126631	1580.461028	17.655987
39.027095	1594.608936	17.661005
39.415732	1597.480899	17.666023
39.504520	1601.893556	17.671040
39.282477	1594.953973	17.676058
39.291345	1592.498647	17.681075
39.043189	1598.055984	17.686093
39.589953	1593.883567	17.691111
39.606941	1588.966622	17.696128
39.719067	1599.851997	17.701146
39.629900	1593.367085	17.706163
39.703570	1589.925317	17.711181
39.616714	1577.477221	17.716199
39.692357	1563.664516	17.721216
39.278113	1567.414103	17.726234
39.985325	1578.519172	17.731251
39.688183	1593.086362	17.736269
39.892251	1591.393531	17.741287
39.846500	1599.101260	17.746304
39.514108	1593.256063	17.751322
39.623248	1587.747881	17.756339
39.735352	1593.744858	17.761357
39.921013	1596.564246	17.766375
40.118396	1593.927050	17.771392
40.250852	1590.004764	17.776410
40.184034	1592.719694	17.781427
40.096224	1595.251560	17.786445
40.149934	1593.754177	17.791463
40.160618	1597.159136	17.796480
39.908880	1589.686292	17.801498
40.261164	1588.584904	17.806515
40.185941	1596.652851	17.811533
40.229885	1592.728164	17.816551
39.997598	1590.234217	17.821568
40.047984	1586.391091	17.826586
39.930212	1592.486867	17.831603
40.285296	1620.363081	17.836621
40.445371	1618.887273	17.841639
40.547054	1619.757617	17.846656
40.398116	1627.549461	17.851674
40.532306	1622.229976	17.856691
40.534461	1628.715646	17.861709
40.419805	1628.859114	17.866727
40.624209	1627.888279	17.871744
40.422591	1626.911410	17.876762
41.100934	1622.707775	17.881779
41.051077	1629.253653	17.886797
40.947109	1624.276546	17.891815
40.847823	1628.200869	17.896832
40.755900	1625.889820	17.901850
40.937127	1623.126201	17.906867
41.182724	1623.724256	17.911885
41.123397	1618.780932	17.916903
41.534407	1616.062468	17.921920
40.707225	1620.429297	17.926938
41.172660	1612.761834	17.931955
40.896721	1619.807829	17.936973
40.826846	1636.997356	17.941991
41.318185	1642.988928	17.947008
41.258766	1644.336449	17.952026
41.472787	1648.483742	17.957043
41.423792	1647.570624	17.962061
41.592668	1648.757460	17.967079
41.745822	1646.696771	17.972096
41.515531	1651.018752	17.977114
41.697238	1637.685376	17.982131
42.027836	1642.380392	17.987149
41.825905	1649.256502	17.992167
42.309730	1643.260658	17.997184
41.775942	1638.643907	18.002202
41.589894	1612.842598	18.007219
41.692913	1625.223102	18.012237
41.825870	1640.229855	18.017255
41.878253	1641.974843	18.022272
41.968732	1651.209592	18.027290
42.256947	1649.988637	18.032307
41.948118	1653.957398	18.037325
41.754641	1656.636695	18.042343
41.981030	1648.197976	18.047360
41.945772	1651.080138	18.052378
41.948613	1649.142528	18.057395
41.818219	1639.909667	18.062413
41.850071	1643.232605	18.067431
42.354803	1644.932192	18.072448
42.246636	1650.006303	18.077466
42.371385	1656.533785	18.082483
42.328625	1669.551873	18.087501
42.284533	1674.743982	18.092519
42.329290	1672.048525	18.097536
42.110325	1677.664161	18.102554
42.112928	1674.856657	18.107571
42.164042	1676.063849	18.112589
42.183875	1675.450441	18.117607
42.509562	1681.434627	18.122624
42.683973	1702.536916	18.127642
42.919711	1702.081778	18.132659
43.076476	1703.165151	18.137677
42.670417	1706.800203	18.142695
43.222295	1698.592704	18.147712
42.948456	1695.067900	18.152730
43.070148	1700.075480	18.157747
43.097052	1703.514058	18.162765
43.187175	1697.293103	18.167783
42.940165	1686.339740	18.172800
42.957872	1693.869075	18.177818
43.185762	1694.233206	18.182835
43.368516	1700.233903	18.187853
43.158268	1698.791979	18.192871
43.383379	1691.062124	18.197888
43.217099	1698.057632	18.202906
43.033562	1693.056223	18.207923
43.056282	1706.524823	18.212941
42.928414	1704.534902	18.217959
43.534549	1689.176840	18.222976
43.062193	1702.209987	18.227994
43.210169	1693.231586	18.233011
43.617093	1711.480156	18.238029
43.419308	1732.987933	18.243047
43.788376	1720.003720	18.248064
43.572700	1728.015485	18.253082
43.687563	1728.605293	18.258099
43.973680	1728.108298	18.263117
43.834360	1728.704823	18.268135
43.890479	1722.328824	18.273152
43.920474	1729.697334	18.278170
43.647183	1735.183221	18.283187
43.744383	1735.466730	18.288205
43.752418	1723.199228	18.293223
43.985142	1717.471503	18.298240
43.854023	1726.559160	18.303258
44.233861	1737.862864	18.308275
44.364273	1738.272431	18.313293
44.443500	1746.101885	18.318311
44.550178	1732.026081	18.323328
44.475928	1720.160263	18.328346
44.110981	1721.788551	18.333363
44.726129	1717.390465	18.338381
44.128250	1731.120094	18.343399
44.627530	1739.862601	18.348416
44.605868	1739.369072	18.353434
44.554213	1742.485902	18.358451
44.925585	1742.010705	18.363469
44.587757	1749.304959	18.368487
44.767789	1738.515483	18.373504
44.910740	1745.767667	18.378522
44.777671	1743.042353	18.383539
45.188704	1737.846997	18.388557
44.576548	1737.521579	18.393575
45.024906	1734.831746	18.398592
45.058034	1732.530625	18.403610
44.995034	1729.457492	18.408627
44.831040	1735.446649	18.413645
44.910180	1737.256598	18.418663
45.165783	1731.317567	18.423680
45.080314	1732.758917	18.428698
45.124938	1743.800679	18.433715
45.329907	1740.755597	18.438733
45.081183	1744.697492	18.443751
45.093601	1740.553624	18.448768
44.993766	1742.843601	18.453786
45.107444	1753.845254	18.458803
45.385847	1763.808344	18.463821
45.556707	1768.148971	18.468839
45.634937	1765.186235	18.473856
45.473445	1777.225214	18.478874
45.535791	1772.490534	18.483891
45.567658	1767.179450	18.488909
45.316432	1772.450248	18.493927
45.448770	1769.942951	18.498944
45.353941	1783.105520	18.503962
45.764861	1781.772958	18.508979
45.932223	1788.953626	18.513997
45.855779	1802.558473	18.519015
45.924057	1793.756326	18.524032
45.843387	1803.920650	18.529050
45.711232	1801.041014	18.534067
45.722603	1804.636259	18.539085
45.847382	1807.431577	18.544103
46.242644	1799.066518	18.549120
46.344017	1799.182612	18.554138
46.272547	1791.715522	18.559155
46.495144	1782.880905	18.564173
46.329703	1793.520452	18.569191
46.416214	1785.393416	18.574208
46.598567	1792.009305	18.579226
46.771841	1812.380435	18.584243
46.777519	1795.071397	18.589261
46.752017	1793.012438	18.594279
46.819455	1791.636335	18.599296
46.984976	1789.304652	18.604314
46.814300	1791.878084	18.609331
46.975852	1788.176061	18.614349
46.802036	1797.969823	18.619367
46.733704	1793.130915	18.624384
46.885783	1785.324563	18.629402
46.459094	1791.899151	18.634419
47.393751	1809.126100	18.639437
47.146913	1818.817470	18.644455
47.306727	1811.597433	18.649472
47.126953	1798.426173	18.654490
47.323188	1806.157556	18.659507
47.614209	1803.162448	18.664525
47.174670	1786.138370	18.669543
47.292968	1785.220586	18.674560
47.661765	1786.197787	18.679578
47.242529	1783.938127	18.684595
47.762317	1781.313977	18.689613
47.521775	1782.695115	18.694631
47.578605	1785.089109	18.699648
47.439635	1780.226861	18.704666
47.803034	1806.610006	18.709683
47.948248	1799.363987	18.714701
47.448526	1793.546181	18.719719
47.671072	1800.787271	18.724736
47.826456	1810.124247	18.729754
47.737793	1820.092432	18.734771
48.106593	1814.914796	18.739789
47.799350	1823.843402	18.744807
47.996428	1809.382635	18.749824
47.858619	1818.756151	18.754842
47.654082	1814.803388	18.759859
48.048259	1810.549849	18.764877
48.020921	1806.350951	18.769895
47.878579	1816.440958	18.774912
48.130182	1820.263751	18.779930
47.994855	1817.263487	18.784947
48.081459	1827.454637	18.789965
48.383099	1839.135069	18.794983
48.503570	1849.691304	18.800000
48.389110	1833.532457	18.805018
48.115135	1846.193512	18.810035
48.449935	1842.083148	18.815053
48.162065	1845.036312	18.820071
48.237359	1844.063245	18.825088
48.450699	1851.719560	18.830106
48.383002	1868.065817	18.835123
48.855127	1874.911614	18.840141
48.707994	1875.033519	18.845159
48.712320	1876.999359	18.850176
49.042414	1876.330955	18.855194
49.016513	1887.181139	18.860211
49.079309	1879.304814	18.865229
49.259612	1879.188870	18.870247
49.005083	1874.687963	18.875264
49.314749	1875.440991	18.880282
49.043533	1881.458319	18.885299
49.340256	1874.752065	18.890317
49.605631	1870.015650	18.895335
49.289264	1869.384274	18.900352
49.315381	1875.246420	18.905370
49.195531	1868.483116	18.910387
49.772948	1873.299304	18.915405
49.571607	1875.573241	18.920423
49.387429	1873.990278	18.925440
49.544705	1874.310617	18.930458
49.704650	1896.428588	18.935475
49.720153	1901.146413	18.940493
49.782546	1901.263219	18.945511
49.580080	1896.628151	18.950528
49.968659	1895.944126	18.955546
50.092770	1910.831439	18.960563
50.188682	1894.616949	18.965581
50.154750	1897.946504	18.970599
49.647895	1899.232476	18.975616
50.230225	1896.607771	18.980634
50.207237	1891.970038	18.985651
50.484705	1889.832071	18.990669
50.277184	1895.315394	18.995687
50.250739	1890.992838	19.000704
50.441840	1900.357999	19.005722
50.019986	1897.129689	19.010739
50.393580	1890.850859	19.015757
50.357151	1889.350517	19.020775
50.299194	1894.628290	19.025792
50.441249	1887.250588	19.030810
50.314013	1897.829059	19.035827
50.579547	1903.929905	19.040845
50.763269	1918.323981	19.045863
50.693854	1923.734949	19.050880
51.099604	1921.648883	19.055898
50.865573	1924.230082	19.060915
51.098688	1930.232282	19.065933
50.928523	1932.025383	19.070951
50.868849	1932.521905	19.075968
51.343611	1919.389303	19.080986
50.914439	1924.783709	19.086003
51.377204	1922.445501	19.091021
51.287403	1925.522046	19.096039
51.070197	1919.836108	19.101056
51.433918	1919.907218	19.106074
51.128159	1920.424108	19.111091
51.316384	1921.843064	19.116109
51.428934	1924.718225	19.121127
51.009681	1924.927577	19.126144
51.366849	1918.929799	19.131162
51.316244	1925.373675	19.136179
51.556872	1933.529085	19.141197
51.715839	1938.674744	19.146215
51.623155	1939.965458	19.151232
51.986289	1939.698437	19.156250
51.554936	1943.471296	19.161267
51.648495	1940.667326	19.166285
51.742371	1943.536031	19.171303
51.768910	1945.068084	19.176320
51.812320	1929.651643	19.181338
52.043585	1950.764890	19.186355
52.112404	1960.836265	19.191373
52.090779	1971.359404	19.196391
52.301811	1977.600330	19.201408
52.335215	1968.731275	19.206426
52.295799	1976.679669	19.211443
52.622908	1967.011814	19.216461
52.492914	1965.768649	19.221479
52.220786	1971.927742	19.226496
52.700528	1972.175417	19.231514
52.388960	1975.335321	19.236531
52.817855	1968.950890	19.241549
52.799208	1967.578275	19.246567
52.537589	1972.579435	19.251584
52.563635	1968.706268	19.256602
52.495800	1979.106998	19.261619
52.489685	1972.282245	19.266637
52.718518	1978.624947	19.271655
52.661482	1994.810758	19.276672
52.921397	1998.357760	19.281690
53.025987	2000.990369	19.286707
53.138768	2007.208436	19.291725
53.161721	1998.178209	19.296743
53.159008	1997.272632	19.301760
53.424026	2000.472730	19.306778
53.425263	2000.966619	19.311795
53.481143	1992.497476	19.316813
53.572233	1990.975213	19.321831
53.227845	1993.409631	19.326848
53.648750	1983.137666	19.331866
53.526511	1991.061521	19.336883
53.556383	1990.006019	19.341901
53.683966	1993.486815	19.346919
53.528747	1997.237673	19.351936
54.145888	1998.499351	19.356954
54.011477	1996.563133	19.361971
53.748682	1995.959389	19.366989
54.226381	2000.540608	19.372007
53.684729	2004.074651	19.377024
53.738843	2015.509177	19.382042
54.060605	2023.791708	19.387059
54.075291	2026.057172	19.392077
54.312307	2021.236349	19.397095
53.993863	2022.504081	19.402112
54.375115	2026.788421	19.407130
54.366143	2027.983201	19.412147
53.986742	2024.400427	19.417165
54.151917	2015.221657	19.422183
54.111144	2032.606798	19.427200
54.220249	2038.244187	19.432218
54.805177	2046.479255	19.437235
54.528379	2046.171134	19.442253
54.927439	2039.472082	19.447271
54.796934	2045.152406	19.452288
55.137825	2045.375821	19.457306
54.777213	2045.313892	19.462323
54.609272	2048.650695	19.467341
55.149277	2041.279455	19.472359
54.837537	2048.383278	19.477376
54.845177	2045.327916	19.482394
55.011419	2041.917686	19.487411
55.016470	2051.397566	19.492429
55.478021	2071.839497	19.497447
55.330565	2081.052685	19.502464
55.451399	2077.534849	19.507482
55.231185	2075.166317	19.512499
55.311258	2091.568701	19.517517
55.555969	2076.321365	19.522535
55.198896	2084.432171	19.527552
55.520291	2076.048846	19.532570
55.465084	2082.079787	19.537587
55.654490	2075.566751	19.542605
55.801404	2071.909466	19.547623
55.501693	2079.243425	19.552640
55.382711	2081.000064	19.557658
55.557890	2094.813612	19.562675
55.758169	2109.972934	19.567693
56.083571	2104.134317	19.572711
56.180168	2110.266912	19.577728
56.614016	2101.318182	19.582746
56.346617	2101.530060	19.587763
56.574523	2109.288017	19.592781
56.955931	2103.501034	19.597799
56.397922	2105.960100	19.602816
56.505452	2096.759795	19.607834
56.471855	2097.118445	19.612851
56.059783	2103.651510	19.617869
56.443973	2099.800636	19.622887
56.304273	2097.261157	19.627904
56.350789	2109.134304	19.632922
56.138513	2110.734352	19.637939
56.295490	2115.210228	19.642957
56.655776	2122.969105	19.647975
56.415668	2137.204456	19.652992
56.710270	2133.735978	19.658010
57.090536	2130.912206	19.663027
56.875885	2145.951320	19.668045
57.526700	2125.747437	19.673063
57.502827	2121.218319	19.678080
57.622838	2114.026505	19.683098
58.049856	2110.510958	19.688115
57.992092	2110.569058	19.693133
58.230425	2108.685073	19.698151
57.837413	2106.019237	19.703168
57.868710	2088.038748	19.708186
57.949282	2076.615961	19.713203
57.780018	2079.490476	19.718221
58.070195	2070.426240	19.723239
57.736065	2072.066954	19.728256
57.770361	2074.153892	19.733274
57.973429	2065.404023	19.738291
57.717150	2070.913278	19.743309
57.820475	2066.853928	19.748327
57.549198	2077.859800	19.753344
57.943770	2087.817959	19.758362
58.185990	2097.271843	19.763379
58.057813	2105.573477	19.768397
58.315920	2110.645181	19.773415
58.096546	2110.688939	19.778432
58.318232	2104.494811	19.783450
58.112084	2106.648417	19.788467
58.084786	2104.846911	19.793485
58.025046	2102.976641	19.798503
58.000496	2110.547540	19.803520
58.300392	2131.057811	19.808538
58.507151	2131.481958	19.813555
58.307508	2150.852728	19.818573
58.572804	2149.954741	19.823591
58.710996	2143.520634	19.828608
58.470995	2139.130594	19.833626
58.410070	2155.052913	19.838643
58.646980	2175.014820	19.843661
59.284382	2171.453908	19.848679
58.971204	2175.800273	19.853696
59.106000	2167.129664	19.858714
59.444309	2167.589467	19.863731
59.271743	2171.771821	19.868749
59.527636	2165.435348	19.873767
59.357670	2165.678883	19.878784
59.439893	2170.213893	19.883802
59.624421	2161.255334	19.888819
59.515294	2160.380876	19.893837
59.659552	2154.601804	19.898855
59.508596	2160.498598	19.903872
59.589043	2166.493781	19.908890
59.814647	2155.596835	19.913907
59.529403	2169.299822	19.918925
59.890159	2182.512014	19.923943
60.039556	2191.097434	19.928960
60.064840	2193.303813	19.933978
60.059008	2194.662502	19.938995
60.015783	2197.302989	19.944013
60.484524	2192.111644	19.949031
60.417964	2193.190556	19.954048
60.108070	2195.016984	19.959066
60.342481	2186.775681	19.964083
60.253082	2191.695176	19.969101
60.259589	2187.895859	19.974119
60.662859	2187.148127	19.979136
60.525098	2193.970995	19.984154
60.595630	2184.225143	19.989171
60.471945	2199.254525	19.994189
60.656409	2205.161556	19.999207
60.812507	2218.361585	20.004224
60.753996	2224.473343	20.009242
60.958794	2221.722372	20.014259
60.881689	2224.011158	20.019277
61.210488	2220.429446	20.024295
61.232259	2215.652325	20.029312
60.713866	2229.432666	20.034330
60.741669	2225.361719	20.039347
60.826468	2227.225101	20.044365
61.204990	2239.366333	20.049383
61.594132	2240.341110	20.054400
61.359797	2251.969700	20.059418
61.822797	2251.790579	20.064435
61.727987	2255.063064	20.069453
61.678554	2254.802056	20.074471
62.036059	2252.029872	20.079488
62.411470	2236.895245	20.084506
62.523634	2234.215679	20.089523
62.152299	2220.836250	20.094541
62.171383	2205.364403	20.099559
62.106252	2210.429485	20.104576
62.000491	2201.991504	20.109594
62.360465	2202.861595	20.114611
62.288529	2197.316776	20.119629
62.423342	2199.700762	20.124647
62.389125	2207.149760	20.129664
62.317046	2198.130632	20.134682
62.415045	2194.762714	20.139699
62.426133	2195.097722	20.144717
62.341454	2185.479664	20.149735
62.467557	2201.059934	20.154752
62.438532	2216.640576	20.159770
62.770525	2221.759530	20.164787
62.527220	2234.670094	20.169805
62.848425	2256.135202	20.174823
62.854167	2253.495415	20.179840
62.817982	2262.695692	20.184858
63.381228	2252.155425	20.189875
63.028803	2258.114278	20.194893
63.151099	2259.774252	20.199911
63.294003	2253.591052	20.204928
63.323175	2257.290546	20.209946
63.319841	2256.095589	20.214963
63.160799	2255.778121	20.219981
62.886291	2258.127498	20.224999
63.399029	2274.889777	20.230016
63.317996	2283.128145	20.235034
63.467162	2280.994854	20.240051
63.537747	2289.630656	20.245069
63.222757	2283.170437	20.250087
63.773344	2285.659606	20.255104
63.483745	2293.644138	20.260122
63.895839	2307.845649	20.265139
63.761512	2316.843726	20.270157
63.731057	2313.669316	20.275175
64.085884	2312.501401	20.280192
64.096869	2324.068114	20.285210
64.043854	2316.926605	20.290227
64.253777	2310.110503	20.295245
64.136962	2314.726069	20.300263
64.725442	2334.873610	20.305280
64.629640	2349.491247	20.310298
64.922647	2341.082409	20.315315
65.138814	2329.729831	20.320333
65.114280	2315.123778	20.325351
64.931944	2311.948419	20.330368
64.974896	2303.383621	20.335386
65.026191	2305.560699	20.340403
64.988454	2313.419337	20.345421
65.006515	2304.420378	20.350439
64.978481	2308.654448	20.355456
64.500817	2307.465912	20.360474
65.441996	2310.081576	20.365491
65.147792	2333.651526	20.370509
65.283143	2336.453913	20.375527
65.059663	2335.318443	20.380544
64.907907	2343.647569	20.385562
65.330882	2337.678457	20.390579
65.231817	2341.240318	20.395597
65.173136	2347.606223	20.400615
65.461210	2344.213464	20.405632
65.564487	2364.848239	20.410650
65.875215	2351.744559	20.415667
65.971937	2361.390150	20.420685
65.696166	2359.491371	20.425703
66.114229	2359.737883	20.430720
66.092147	2367.258179	20.435738
66.192894	2357.269843	20.440755
65.926201	2362.536238	20.445773
66.147432	2359.511248	20.450791
66.188043	2350.802849	20.455808
65.952336	2362.037664	20.460826
66.097238	2356.523491	20.465843
66.260836	2375.597506	20.470861
66.685900	2376.314856	20.475879
66.730724	2387.066034	20.480896
66.532365	2399.551109	20.485914
66.802147	2385.727117	20.490931
66.648790	2396.480804	20.495949
66.401231	2386.291565	20.500967
66.931827	2387.092769	20.505984
66.607567	2394.666777	20.511002
66.820659	2402.745037	20.516019
67.032186	2416.885823	20.521037
66.992108	2418.446642	20.526055
67.067506	2417.331934	20.531072
67.118311	2420.252438	20.536090
67.373008	2420.672883	20.541107
67.355965	2414.405001	20.546125
67.397568	2409.115729	20.551143
67.452953	2410.019463	20.556160
67.484685	2435.685784	20.561178
67.502684	2437.855606	20.566195
67.718508	2444.258795	20.571213
68.147733	2444.830751	20.576231
68.195484	2441.303246	20.581248
67.692894	2452.020636	20.586266
67.727609	2443.631693	20.591283
67.659962	2443.891164	20.596301
67.610522	2447.329508	20.601319
68.129612	2460.649638	20.606336
68.060900	2467.445102	20.611354
68.677419	2469.750739	20.616371
68.573993	2461.456969	20.621389
68.428064	2473.258846	20.626407
69.079021	2461.537135	20.631424
68.921097	2448.440460	20.636442
69.115300	2443.301464	20.641459
69.324751	2460.594508	20.646477
69.231329	2449.449315	20.651495
69.074895	2437.785588	20.656512
69.045699	2432.702673	20.661530
68.805439	2427.444972	20.666547
69.048754	2437.731908	20.671565
69.247530	2450.277974	20.676583
69.478580	2440.999547	20.681600
69.157707	2470.505679	20.686618
69.480039	2459.522289	20.691635
69.662418	2458.762576	20.696653
69.124173	2464.423921	20.701671
69.593119	2451.584388	20.706688
69.288414	2460.286434	20.711706
69.254222	2461.542693	20.716723
69.725527	2453.744072	20.721741
69.481264	2460.703611	20.726759
69.624574	2452.684349	20.731776
69.495331	2481.044551	20.736794
70.066465	2475.824194	20.741811
70.324465	2481.093482	20.746829
69.615030	2482.769706	20.751847
70.090072	2476.694697	20.756864
70.084900	2478.285353	20.761882
69.892986	2488.380582	20.766899
70.200319	2509.970199	20.771917
70.250995	2515.549444	20.776935
70.303325	2512.468766	20.781952
70.363262	2517.553338	20.786970
70.637353	2518.133520	20.791987
70.825159	2511.615826	20.797005
70.372992	2532.065681	20.802023
70.625316	2539.783005	20.807040
70.833776	2545.043697	20.812058
70.591959	2548.294068	20.817075
70.886638	2547.217535	20.822093
70.638844	2550.908569	20.827111
71.025862	2566.219506	20.832128
71.228698	2571.388285	20.837146
71.168783	2569.775202	20.842163
71.302771	2572.190844	20.847181
71.138405	2582.386363	20.852199
71.635863	2576.815883	20.857216
71.632684	2586.462609	20.862234
71.926202	2606.838486	20.867251
72.051071	2603.382023	20.872269
71.907776	2606.263511	20.877287
71.971617	2602.972528	20.882304
71.693827	2610.267857	20.887322
72.178258	2609.669204	20.892339
72.407795	2596.536564	20.897357
72.195526	2611.624546	20.902375
72.528675	2600.260969	20.907392
72.230544	2602.684174	20.912410
72.519880	2609.708142	20.917427
72.777944	2603.811632	20.922445
72.603127	2603.995378	20.927463
72.854742	2596.794926	20.932480
72.655662	2605.434589	20.937498
72.793563	2601.924133	20.942515
72.848088	2595.519690	20.947533
72.859879	2609.558793	20.952551
73.056565	2600.667248	20.957568
73.035643	2602.737111	20.962586
72.921803	2601.602225	20.967603
73.097270	2601.476823	20.972621
72.994798	2607.730261	20.977639
73.206198	2622.080503	20.982656
73.296354	2628.146696	20.987674
73.122677	2625.371841	20.992691
73.445936	2619.151860	20.997709
73.523360	2630.971734	21.002727
73.812185	2620.313715	21.007744
73.966805	2622.240742	21.012762
73.652844	2625.259574	21.017779
73.919449	2619.962662	21.022797
73.857867	2625.796619	21.027815
74.034088	2640.530847	21.032832
74.081841	2653.002059	21.037850
74.276023	2655.290912	21.042867
74.521248	2646.699162	21.047885
74.300019	2656.897507	21.052903
73.985745	2651.775026	21.057920
74.477963	2657.851840	21.062938
74.318457	2658.216424	21.067955
74.199677	2652.257281	21.072973
74.338421	2662.240903	21.077991
74.518309	2677.572404	21.083008
75.169483	2685.259237	21.088026
74.680435	2686.495233	21.093043
75.171467	2674.680866	21.098061
75.071829	2690.177308	21.103079
74.942469	2691.632830	21.108096
75.154419	2684.231782	21.113114
75.164374	2682.592598	21.118131
75.155574	2683.525464	21.123149
75.399326	2687.013859	21.128167
75.733860	2705.563124	21.133184
75.953048	2705.658080	21.138202
75.844007	2718.170085	21.143219
76.554781	2694.637944	21.148237
75.868362	2690.927760	21.153255
76.061508	2672.636777	21.158272
75.959648	2670.575712	21.163290
75.924516	2673.254324	21.168307
76.027132	2678.904796	21.173325
76.233781	2700.459623	21.178343
76.318013	2699.506313	21.183360
76.275047	2701.745679	21.188378
76.381104	2713.260569	21.193395
76.557664	2709.024175	21.198413
76.519431	2706.554147	21.203431
76.605896	2704.678576	21.208448
76.764023	2706.220403	21.213466
76.489841	2712.954355	21.218483
76.946630	2707.498079	21.223501
76.713697	2704.654784	21.228519
76.797419	2700.781665	21.233536
76.867276	2696.994138	21.238554
76.615859	2706.159009	21.243571
76.957614	2718.694304	21.248589
76.997070	2727.739648	21.253607
77.158290	2736.901662	21.258624
77.407218	2732.553034	21.263642
77.237767	2731.982353	21.268659
77.367819	2734.216944	21.273677
76.851546	2743.462619	21.278695
77.423581	2760.307251	21.283712
77.792286	2766.473818	21.288730
77.406476	2778.652437	21.293747
77.795227	2775.368597	21.298765
77.684479	2773.234207	21.303783
77.657286	2771.267413	21.308800
77.940319	2778.014008	21.313818
78.001601	2792.141361	21.318835
78.375116	2789.791298	21.323853
78.252304	2796.089750	21.328871
78.235809	2785.297021	21.333888
78.526055	2784.809565	21.338906
78.712637	2803.546164	21.343923
78.878870	2810.038445	21.348941
79.019935	2817.743769	21.353959
79.241274	2809.665459	21.358976
79.101886	2789.386096	21.363994
79.070308	2778.062454	21.369011
79.264166	2794.391635	21.374029
79.104026	2800.631539	21.379047
79.113314	2806.157713	21.384064
79.363454	2803.670786	21.389082
79.267094	2811.734121	21.394099
79.424516	2810.655073	21.399117
79.546745	2793.977581	21.404135
79.375652	2797.122334	21.409152
79.431421	2803.604696	21.414170
79.695761	2805.448962	21.419187
79.694678	2819.304679	21.424205
79.745456	2823.503517	21.429223
79.778135	2824.357409	21.434240
80.026220	2824.985802	21.439258
79.773517	2834.858124	21.444275
80.173282	2819.820488	21.449293
79.992940	2830.822646	21.454311
80.335878	2845.271698	21.459328
80.404012	2857.634428	21.464346
80.208893	2863.949946	21.469363
80.488683	2864.541034	21.474381
80.239338	2871.787118	21.479399
80.217429	2872.888850	21.484416
80.451110	2860.881749	21.489434
80.670415	2889.119509	21.494451
80.794823	2888.833912	21.499469
81.210139	2890.853127	21.504487
80.877110	2903.045457	21.509504
81.145043	2893.296758	21.514522
80.956281	2894.901004	21.519539
81.292116	2897.962579	21.524557
81.711403	2912.428626	21.529575
81.818949	2922.923198	21.534592
81.741444	2922.108153	21.539610
81.661175	2919.327785	21.544627
81.767236	2913.611143	21.549645
81.834839	2923.088693	21.554663
81.738498	2912.659436	21.559680
82.035087	2921.033811	21.564698
81.862664	2915.109860	21.569715
81.967509	2914.928857	21.574733
82.095183	2913.389654	21.579751
82.105318	2928.709158	21.584768
82.500565	2932.834216	21.589786
82.292248	2946.834015	21.594803
82.448807	2949.529305	21.599821
82.400353	2952.697012	21.604839
82.637921	2954.499942	21.609856
82.676076	2945.826192	21.614874
82.334486	2962.369167	21.619891
82.732781	2970.491365	21.624909
82.902040	2979.793056	21.629927
82.710668	2985.346577	21.634944
83.219896	2986.623989	21.639962
82.951583	2993.062149	21.644979
83.007910	2995.009620	21.649997
83.338348	3008.718253	21.655015
83.342210	3011.388349	21.660032
83.801714	3006.776366	21.665050
83.378118	3015.872918	21.670067
83.819717	3012.542055	21.675085
84.088314	3009.181358	21.680103
83.550110	3009.769171	21.685120
84.313827	3020.543833	21.690138
84.710013	3026.948410	21.695155
84.463762	3028.262920	21.700173
84.251965	3017.992019	21.705191
84.473520	3026.830731	21.710208
84.552607	3031.217050	21.715226
84.610469	3029.609519	21.720243
84.884357	3021.926252	21.725261
85.146702	3026.810386	21.730279
84.646038	3028.360550	21.735296
85.209160	3023.069700	21.740314
85.195380	3026.623632	21.745331
84.897206	3022.913590	21.750349
85.232428	3019.534400	21.755367
85.128625	3032.714469	21.760384
85.407685	3022.119861	21.765402
85.295440	3022.244861	21.770419
85.258822	3032.093083	21.775437
85.418098	3019.599785	21.780455
85.076735	3028.403192	21.785472
85.176993	3031.485057	21.790490
85.291277	3036.698803	21.795507
85.339821	3052.902773	21.800525
85.624170	3055.218216	21.805543
85.631235	3056.727534	21.810560
86.049501	3065.376788	21.815578
86.064480	3079.511802	21.820595
86.285184	3081.027958	21.825613
86.127981	3079.113321	21.830631
86.231266	3089.917837	21.835648
86.359256	3076.827708	21.840666
86.629627	3079.403399	21.845683
86.776351	3077.315220	21.850701
86.761341	3076.579090	21.855719
86.994600	3097.229569	21.860736
87.011371	3100.032923	21.865754
86.848666	3107.685366	21.870771
86.848996	3107.091527	21.875789
87.433437	3105.206504	21.880807
87.214243	3109.826845	21.885824
87.611197	3097.849366	21.890842
87.419324	3102.922380	21.895859
87.230428	3109.639765	21.900877
87.138133	3100.458898	21.905895
87.817774	3111.878701	21.910912
87.668962	3123.094733	21.915930
87.878120	3138.415757	21.920947
87.850155	3131.460220	21.925965
88.134255	3132.930873	21.930983
87.794461	3138.117164	21.936000
88.247197	3138.858465	21.941018
88.362615	3136.204176	21.946035
88.277356	3136.054272	21.951053
88.319081	3142.898515	21.956071
88.404635	3160.876064	21.961088
88.569638	3160.635907	21.966106
88.499584	3166.987462	21.971123
88.631292	3166.731375	21.976141
89.098789	3162.343834	21.981159
88.678890	3169.506346	21.986176
89.024189	3173.027438	21.991194
88.928627	3190.948950	21.996211
89.129952	3194.757316	22.001229
89.096375	3190.149178	22.006247
88.977534	3199.032837	22.011264
89.261843	3191.573585	22.016282
89.625703	3198.977699	22.021299
89.704781	3204.613249	22.026317
89.725552	3197.666428	22.031335
89.831427	3210.703878	22.036352
89.792880	3196.394955	22.041370
90.070198	3197.070623	22.046387
90.003228	3209.824914	22.051405
90.280309	3198.552415	22.056423
90.502001	3203.505236	22.061440
90.244838	3194.258564	22.066458
90.282722	3201.999425	22.071475
90.635501	3196.656313	22.076493
90.858097	3192.856102	22.081511
90.559130	3203.868016	22.086528
90.668335	3210.630733	22.091546
90.955915	3221.607337	22.096563
91.156974	3233.208176	22.101581
91.368365	3220.538056	22.106599
91.279138	3227.628199	22.111616
91.378329	3236.025582	22.116634
91.676620	3230.776105	22.121651
91.507381	3229.856102	22.126669
91.705339	3225.232269	22.131687
91.728993	3233.609445	22.136704
91.528098	3227.726878	22.141722
91.601557	3224.645828	22.146739
91.533053	3228.647479	22.151757
91.922453	3226.903674	22.156775
91.783212	3245.767529	22.161792
91.922462	3245.164904	22.166810
92.023861	3252.679338	22.171827
91.787629	3256.024941	22.176845
91.999661	3254.694869	22.181863
92.102393	3281.112816	22.186880
92.148660	3282.308329	22.191898
92.484519	3289.069551	22.196915
92.681906	3286.542973	22.201933
92.810053	3285.533065	22.206951
92.656438	3304.018553	22.211968
92.632203	3309.872785	22.216986
92.946756	3309.529328	22.222003
93.138497	3311.866661	22.227021
93.048086	3312.132137	22.232039
92.959085	3332.417418	22.237056
93.239564	3349.238430	22.242074
93.591342	3342.960894	22.247091
93.702883	3347.419225	22.252109
93.717156	3342.932418	22.257127
93.854247	3348.066334	22.262144
94.027246	3338.183019	22.267162
94.441894	3336.352577	22.272179
93.547994	3344.072185	22.277197
94.418166	3337.652201	22.282215
94.719885	3349.375530	22.287232
95.044073	3351.673656	22.292250
95.219168	3342.309975	22.297267
95.333374	3332.885212	22.302285
94.962327	3315.234834	22.307303
94.688070	3318.334790	22.312320
94.929376	3312.044991	22.317338
95.278889	3315.360133	22.322355
95.016753	3322.250555	22.327373
95.433356	3313.770325	22.332391
95.202196	3313.115062	22.337408
95.089177	3319.323285	22.342426
95.113627	3319.110259	22.347443
95.304768	3343.286452	22.352461
95.620001	3340.691514	22.357479
95.640491	3348.941037	22.362496
95.386755	3349.256156	22.367514
95.610319	3348.925635	22.372531
95.315816	3360.543455	22.377549
95.933754	3373.198110	22.382567
96.106745	3379.333217	22.387584
95.975328	3380.181844	22.392602
96.175034	3379.072414	22.397619
95.966751	3381.911709	22.402637
96.450804	3405.407260	22.407655
96.351316	3419.422405	22.412672
96.136509	3419.835943	22.417690
96.470661	3420.582011	22.422707
96.547209	3434.982876	22.427725
96.937833	3438.791013	22.432743
97.235710	3445.267305	22.437760
97.236684	3448.620751	22.442778
97.443527	3445.317790	22.447795
97.234928	3449.862602	22.452813
97.445375	3434.944207	22.457831
97.330467	3448.935881	22.462848
97.550246	3467.884367	22.467866
97.821325	3466.957852	22.472883
97.653775	3474.545966	22.477901
97.385884	3476.608922	22.482919
97.645790	3483.994360	22.487936
97.820585	3496.014948	22.492954
97.956868	3499.919511	22.497971
98.104728	3509.669410	22.502989
97.847390	3508.049157	22.508007
98.362786	3532.073263	22.513024
98.472180	3534.866650	22.518042
98.674810	3533.026729	22.523059
98.385321	3545.653171	22.528077
98.793210	3536.851674	22.533095
99.042531	3552.895170	22.538112
98.856101	3566.929040	22.543130
99.233311	3568.916671	22.548147
99.278171	3571.016299	22.553165
99.480202	3562.699154	22.558183
99.661788	3568.128128	22.563200
99.446487	3565.588646	22.568218
99.907539	3559.946517	22.573235
99.343290	3571.587065	22.578253
99.449458	3579.270036	22.583271
99.745625	3584.652425	22.588288
99.548769	3591.093609	22.593306
99.979644	3586.861250	22.598323
100.100905	3595.064162	22.603341
100.308664	3614.998862	22.608359
100.344304	3629.838318	22.613376
100.452724	3629.186315	22.618394
100.690538	3623.279257	22.623411
100.493530	3632.410853	22.628429
100.912834	3633.405311	22.633447
101.054291	3623.319157	22.638464
101.171443	3626.670638	22.643482
101.130600	3621.988790	22.648499
100.893025	3628.577294	22.653517
101.391171	3647.981152	22.658535
101.583068	3657.485770	22.663552
101.461876	3657.605121	22.668570
101.928598	3645.843419	22.673587
101.549265	3650.566556	22.678605
101.665322	3649.422460	22.683623
101.904097	3643.293403	22.688640
101.553855	3655.640137	22.693658
101.994865	3666.833327	22.698675
102.308055	3668.588890	22.703693
102.283049	3678.070683	22.708711
102.390105	3684.412312	22.713728
101.970125	3673.168793	22.718746
102.739968	3684.672213	22.723763
102.725626	3695.230042	22.728781
103.229750	3694.508644	22.733799
103.357683	3697.531957	22.738816
103.231113	3693.487579	22.743834
103.504761	3691.149371	22.748851
103.258554	3699.730324	22.753869
103.653995	3692.577990	22.758887
103.546721	3691.301945	22.763904
103.239707	3702.153460	22.768922
103.528466	3694.153596	22.773939
103.749444	3695.299258	22.778957
103.871998	3704.010995	22.783975
104.149351	3709.601750	22.788992
104.024310	3722.933717	22.794010
104.196079	3721.088467	22.799027
104.107774	3731.692730	22.804045
104.162104	3728.063174	22.809063
104.267250	3721.298530	22.814080
104.133325	3732.089427	22.819098
104.796450	3735.429391	22.824115
104.729784	3747.714462	22.829133
104.442134	3750.149551	22.834151
104.662836	3754.177600	22.839168
105.032576	3755.198065	22.844186
104.898607	3762.362467	22.849203
104.841521	3776.134404	22.854221
105.208754	3784.648267	22.859239
105.447854	3785.422099	22.864256
104.968604	3795.031468	22.869274
105.391598	3792.918016	22.874291
105.669295	3813.995089	22.879309
105.696973	3819.973406	22.884327
105.632198	3819.544107	22.889344
105.757744	3816.339775	22.894362
106.212860	3818.492806	22.899379
105.975695	3824.445704	22.904397
106.159670	3843.501865	22.909415
106.832132	3837.634761	22.914432
107.213019	3839.009029	22.919450
107.438080	3837.671323	22.924467
107.270519	3831.715543	22.929485
107.112218	3827.733614	22.934503
107.677990	3822.262703	22.939520
107.666320	3814.000733	22.944538
107.722538	3793.971201	22.949555
107.745641	3794.571796	22.954573
107.627475	3781.480172	22.959591
108.015481	3781.920314	22.964608
107.697318	3785.029727	22.969626
107.762568	3788.245561	22.974643
107.970869	3796.299401	22.979661
107.753087	3813.500907	22.984679
107.846000	3811.734302	22.989696
108.006239	3819.979899	22.994714
107.966029	3818.029199	22.999731
108.126167	3831.351190	23.004749
108.376019	3841.693929	23.009767
108.578716	3848.391686	23.014784
108.108750	3852.534616	23.019802
108.201567	3852.144694	23.024819
108.626768	3877.477823	23.029837
108.700672	3879.893040	23.034855
109.016865	3879.583925	23.039872
108.901839	3886.353603	23.044890
109.456853	3902.119028	23.049907
109.583083	3908.962741	23.054925
109.666703	3920.045555	23.059943
109.930483	3914.212909	23.064960
109.813666	3915.078903	23.069978
109.766421	3912.706083	23.074995
109.936680	3905.773637	23.080013
109.896041	3909.394999	23.085031
110.381369	3910.110696	23.090048
110.425355	3924.620289	23.095066
110.476033	3941.300052	23.100083
110.628199	3939.623103	23.105101
110.575969	3944.803152	23.110119
110.870760	3943.691894	23.115136
110.503481	3946.115324	23.120154
110.715058	3934.439706	23.125171
111.190851	3940.989331	23.130189
111.265106	3960.108767	23.135207
111.252482	3960.676520	23.140224
111.305180	3961.985919	23.145242
111.557566	3956.187327	23.150259
111.428859	3959.062816	23.155277
111.306696	3958.176165	23.160295
111.646246	3959.419369	23.165312
111.346940	3985.647810	23.170330
111.641281	3995.067871	23.175347
111.955996	3998.240039	23.180365
111.707641	4007.590884	23.185383
112.135901	4020.920640	23.190400
112.374102	4027.999077	23.195418
112.611540	4028.849497	23.200435
112.667429	4025.324247	23.205453
112.382266	4028.890229	23.210471
112.915106	4032.725408	23.215488
112.897391	4047.162359	23.220506
112.593525	4055.674830	23.225523
113.151988	4051.466838	23.230541
113.104647	4060.317588	23.235559
113.172010	4064.028755	23.240576
113.019203	4083.719502	23.245594
113.312052	4072.015082	23.250611
113.554776	4085.786704	23.255629
113.750906	4106.140082	23.260647
113.854170	4099.774413	23.265664
113.926596	4106.895843	23.270682
114.214620	4091.426323	23.275699
114.888142	4102.480506	23.280717
115.022660	4110.316573	23.285735
115.249892	4090.935128	23.290752
114.867904	4091.005598	23.295770
115.128103	4084.459149	23.300787
115.080988	4085.580724	23.305805
115.131358	4106.423061	23.310823
115.523831	4106.284290	23.315840
115.198535	4120.173266	23.320858
115.360244	4116.357355	23.325875
115.658504	4107.542322	23.330893
115.341142	4118.028411	23.335911
115.744976	4109.292518	23.340928
115.786276	4104.483348	23.345946
116.056804	4122.916393	23.350963
116.320748	4139.014054	23.355981
115.869424	4143.184772	23.360999
116.570392	4136.058244	23.366016
116.364739	4136.095089	23.371034
116.224507	4141.651115	23.376051
116.469247	4140.064799	23.381069
116.449771	4163.324825	23.386087
117.012043	4171.835349	23.391104
116.868550	4186.025019	23.396122
116.768445	4172.639092	23.401139
117.101673	4167.477330	23.406157
116.842361	4178.641770	23.411175
117.309835	4189.212021	23.416192
117.069196	4196.705957	23.421210
117.323359	4210.390123	23.426227
117.457329	4200.594270	23.431245
117.563952	4228.538691	23.436263
117.936432	4234.081439	23.441280
117.977976	4238.752596	23.446298
117.791145	4238.581901	23.451315
118.186346	4240.476291	23.456333
118.105468	4261.973849	23.461351
118.395376	4259.668362	23.466368
118.405355	4257.996744	23.471386
118.580887	4271.405576	23.476403
118.885071	4278.247833	23.481421
118.888989	4288.222596	23.486439
119.324725	4306.266076	23.491456
118.909440	4302.599550	23.496474
119.211349	4294.423407	23.501491
119.578885	4296.382791	23.506509
119.171335	4304.386426	23.511527
119.669604	4322.480529	23.516544
119.927049	4323.813955	23.521562
119.708090	4330.460377	23.526579
120.000107	4324.963707	23.531597
119.886163	4341.159608	23.536615
120.144833	4343.100169	23.541632
120.550154	4351.832499	23.546650
120.446839	4346.999108	23.551667
120.784045	4346.904551	23.556685
120.745146	4358.966216	23.561703
120.984991	4373.426140	23.566720
121.470139	4370.784266	23.571738
120.989456	4386.171753	23.576755
121.546312	4374.602005	23.581773
121.241968	4373.959932	23.586791
121.295058	4375.912825	23.591808
121.477049	4373.386159	23.596826
121.636124	4398.194628	23.601843
121.985346	4389.747345	23.606861
121.988462	4404.630530	23.611879
122.053845	4391.650700	23.616896
122.458996	4394.494643	23.621914
122.458781	4393.494903	23.626931
122.739264	4399.326941	23.631949
122.848191	4410.246390	23.636967
123.104196	4421.158129	23.641984
123.133389	4419.922408	23.647002
122.995843	4427.553428	23.652019
123.443450	4423.937302	23.657037
123.333647	4432.624373	23.662055
123.364332	4434.053757	23.667072
123.270680	4429.349390	23.672090
123.466987	4429.758760	23.677107
123.542109	4425.416900	23.682125
123.617701	4431.442109	23.687143
123.726335	4444.036516	23.692160
124.037383	4452.809901	23.697178
123.975155	4455.895162	23.702195
124.218952	4454.527667	23.707213
124.276115	4466.316064	23.712231
124.208293	4465.564683	23.717248
124.433939	4473.233006	23.722266
124.501848	4482.281975	23.727283
124.778022	4482.337970	23.732301
124.709474	4502.384804	23.737319
124.746909	4509.592253	23.742336
124.516501	4515.106941	23.747354
124.685524	4521.154264	23.752371
125.334906	4533.162966	23.757389
125.218338	4553.328452	23.762407
125.296817	4551.288713	23.767424
125.416917	4556.362040	23.772442
126.092534	4572.948378	23.777459
126.621052	4567.411549	23.782477
126.517017	4577.205471	23.787495
126.806381	4567.132851	23.792512
126.682749	4561.062776	23.797530
126.651780	4564.800764	23.802547
126.900307	4557.505448	23.807565
126.869683	4566.876209	23.812583
126.747878	4569.120562	23.817600
127.050089	4587.598701	23.822618
127.037700	4595.194904	23.827635
127.080730	4596.387895	23.832653
127.006073	4603.528298	23.837671
127.688003	4614.256620	23.842688
127.940166	4618.691344	23.847706
127.744568	4633.014838	23.852723
128.354901	4619.257969	23.857741
128.091853	4627.432267	23.862759
128.138086	4622.541897	23.867776
128.448175	4631.552342	23.872794
128.347425	4653.601978	23.877811
128.727605	4658.603976	23.882829
128.618794	4653.469262	23.887847
128.688338	4648.963803	23.892864
129.055453	4646.677416	23.897882
129.115514	4672.546103	23.902899
129.432565	4675.935182	23.907917
129.289067	4679.032662	23.912935
129.357430	4680.011567	23.917952
129.617336	4672.719888	23.922970
129.370842	4686.587388	23.927987
129.505439	4701.715031	23.933005
130.035464	4709.921048	23.938023
129.964097	4712.073201	23.943040
130.096132	4711.383559	23.948058
129.745619	4736.340723	23.953075
130.289048	4739.014784	23.958093
130.552552	4742.279462	23.963111
130.632298	4738.324624	23.968128
130.836128	4751.976412	23.973146
130.783463	4771.348435	23.978163
130.898391	4773.186101	23.983181
131.289147	4778.180160	23.988199
131.147741	4775.642841	23.993216
131.321020	4791.260829	23.998234
131.108966	4813.274166	24.003251
131.499385	4802.773818	24.008269
131.635649	4812.915860	24.013287
132.024534	4835.524153	24.018304
132.161175	4836.475661	24.023322
132.043927	4841.657737	24.028339
132.246717	4837.189979	24.033357
132.401951	4841.984024	24.038375
132.464174	4848.573256	24.043392
132.813870	4860.382195	24.048410
132.952827	4868.907916	24.053427
133.203577	4859.494236	24.058445
133.334594	4851.731318	24.063463
133.805263	4853.857642	24.068480
134.014790	4852.730021	24.073498
133.867352	4853.170613	24.078515
134.228347	4857.714719	24.083533
134.144016	4870.888606	24.088551
134.315218	4878.579197	24.093568
134.582503	4872.434862	24.098586
134.430164	4877.836535	24.103603
134.335715	4882.947332	24.108621
134.608550	4875.780941	24.113639
134.175807	4887.411772	24.118656
134.535869	4881.058319	24.123674
134.987693	4909.280988	24.128691
134.743162	4907.847346	24.133709
134.880897	4914.533922	24.138727
135.256879	4919.770338	24.143744
135.306125	4928.785581	24.148762
135.561544	4945.548698	24.153779
135.813558	4950.232153	24.158797
135.933249	4939.935368	24.163815
135.727523	4951.117806	24.168832
136.038005	4958.328354	24.173850
135.883007	4954.212633	24.178867
135.880574	4963.962289	24.183885
136.420516	4984.269930	24.188903
136.326574	4998.458772	24.193920
136.679946	4994.863831	24.198938
136.656684	5001.694913	24.203955
137.094082	5012.386208	24.208973
137.216975	5020.632141	24.213991
137.119724	5031.215948	24.219008
137.148094	5025.075815	24.224026
137.302440	5039.842693	24.229043
137.506800	5053.939968	24.234061
137.553762	5057.800185	24.239079
137.710062	5063.450100	24.244096
137.955540	5073.119388	24.249114
137.833053	5091.156073	24.254131
137.974548	5094.612579	24.259149
138.322629	5097.809567	24.264167
138.210267	5118.975096	24.269184
138.252062	5115.887687	24.274202
138.482864	5130.555924	24.279219
138.842111	5143.925245	24.284237
139.061699	5141.110017	24.289255
139.250206	5149.679138	24.294272
139.567217	5143.316703	24.299290
139.197774	5159.981438	24.304307
139.911932	5171.226642	24.309325
140.271485	5168.131041	24.314343
140.159902	5173.337506	24.319360
140.470290	5169.625072	24.324378
140.572065	5174.164978	24.329395
140.706505	5166.153526	24.334413
140.899963	5172.150804	24.339431
140.875185	5165.271684	24.344448
141.049522	5183.001528	24.349466
141.098408	5195.029424	24.354483
141.306137	5194.180571	24.359501
141.478418	5191.632501	24.364519
141.661720	5187.160665	24.369536
141.691987	5180.609486	24.374554
142.008234	5188.958430	24.379571
141.989472	5185.276445	24.384589
142.147671	5202.834231	24.389607
142.470556	5223.290890	24.394624
142.406117	5221.093682	24.399642
142.301297	5220.975195	24.404659
142.284547	5214.245826	24.409677
142.360182	5223.917906	24.414695
142.481812	5246.397933	24.419712
142.557215	5249.033426	24.424730
142.747294	5262.617073	24.429747
143.042080	5287.479355	24.434765
143.157792	5286.913450	24.439783
142.953859	5294.130657	24.444800
143.382572	5304.467940	24.449818
143.408755	5318.881041	24.454835
143.598701	5331.437280	24.459853
143.770152	5341.233413	24.464871
143.907704	5354.368419	24.469888
144.267215	5351.353036	24.474906
144.770861	5365.139328	24.479923
144.689408	5373.943591	24.484941
144.913312	5369.528954	24.489959
144.935460	5383.900277	24.494976
144.982125	5375.899560	24.499994
145.404846	5391.632615	24.505011
145.634679	5407.787458	24.510029
146.069753	5393.725025	24.515047
146.428864	5397.480489	24.520064
146.350771	5376.563885	24.525082
146.063866	5366.652627	24.530099
145.968534	5371.855783	24.535117
146.494332	5374.253481	24.540135
146.329207	5383.001856	24.545152
146.470417	5383.210766	24.550170
146.727294	5379.327433	24.555187
146.673507	5386.845674	24.560205
146.929334	5380.860307	24.565223
147.111500	5407.673798	24.570240
147.166605	5409.052177	24.575258
147.219997	5413.025542	24.580275
147.395132	5407.395268	24.585293
147.661756	5424.456111	24.590311
147.697978	5437.206102	24.595328
147.499136	5433.006760	24.600346
147.825253	5444.892312	24.605363
148.131017	5456.832258	24.610381
148.244043	5467.730595	24.615399
148.242531	5466.233759	24.620416
148.474838	5472.491676	24.625434
148.513987	5502.971612	24.630451
148.368774	5497.554454	24.635469
148.789600	5508.785322	24.640487
148.732081	5530.578396	24.645504
149.223174	5532.626826	24.650522
148.970905	5551.496699	24.655539
149.263283	5564.020282	24.660557
149.571104	5569.155294	24.665575
149.616015	5581.055108	24.670592
149.992336	5590.766816	24.675610
150.492646	5601.022872	24.680627
150.620921	5613.447566	24.685645
151.294860	5621.692521	24.690663
151.106031	5626.941357	24.695680
151.145861	5618.217776	24.700698
151.351136	5622.341642	24.705715
151.268509	5626.761604	24.710733
151.702918	5614.964952	24.715751
151.749089	5627.418484	24.720768
151.617997	5623.996623	24.725786
151.658633	5633.754802	24.730803
151.492565	5647.615096	24.735821
151.929024	5638.869962	24.740839
152.435455	5652.176941	24.745856
152.506089	5664.509376	24.750874
152.755245	5664.953632	24.755891
152.865652	5667.512809	24.760909
153.147988	5664.479773	24.765927
153.428823	5671.110046	24.770944
153.251362	5668.981145	24.775962
153.635141	5662.482750	24.780979
153.345112	5676.982021	24.785997
154.089299	5672.400157	24.791015
153.960564	5694.957763	24.796032
153.761502	5691.076236	24.801050
153.995395	5687.558402	24.806067
153.957432	5695.724934	24.811085
154.394477	5694.725411	24.816103
154.470491	5713.684767	24.821120
154.387825	5716.929329	24.826138
154.751291	5728.898061	24.831155
154.506718	5733.631046	24.836173
154.632171	5742.949344	24.841191
154.808724	5754.888104	24.846208
154.978278	5758.961056	24.851226
155.408190	5770.004212	24.856243
155.326029	5790.954244	24.861261
155.497047	5785.421257	24.866279
155.450282	5808.156365	24.871296
155.864171	5817.618335	24.876314
156.012941	5831.017906	24.881331
155.778784	5858.138558	24.886349
156.620359	5858.722825	24.891367
156.522567	5866.411188	24.896384
156.897859	5881.406464	24.901402
156.938526	5877.573998	24.906419
157.018334	5878.473269	24.911437
157.415842	5895.523230	24.916455
157.688331	5904.961380	24.921472
157.920563	5902.738013	24.926490
158.067855	5897.445589	24.931507
158.151720	5906.976757	24.936525
158.692651	5912.380780	24.941543
158.675507	5921.020905	24.946560
158.686368	5929.101103	24.951578
159.284583	5927.760370	24.956595
158.996571	5920.713584	24.961613
159.168374	5921.385759	24.966631
159.253836	5928.499698	24.971648
159.499587	5930.427587	24.976666
159.800157	5933.038317	24.981683
159.484235	5947.342137	24.986701
159.558998	5952.192649	24.991719
159.507010	5953.284456	24.996736
159.739925	5966.040521	25.001754
160.156424	5976.495884	25.006771
160.344687	5976.860953	25.011789
160.791694	5981.733950	25.016807
160.900937	5997.150993	25.021824
160.967473	6007.079167	25.026842
161.438573	6009.932590	25.031859
161.230620	6012.116935	25.036877
161.914100	5999.830228	25.041895
161.547269	5998.896698	25.046912
161.489278	6014.009186	25.051930
162.319642	6019.317536	25.056947
162.146643	6036.272152	25.061965
162.466917	6028.742018	25.066983
162.208122	6034.065881	25.072000
162.279102	6034.798984	25.077018
162.461612	6032.801466	25.082035
162.516898	6054.851126	25.087053
162.937457	6059.167387	25.092071
163.098947	6059.465129	25.097088
162.950234	6071.640113	25.102106
163.339740	6082.368150	25.107123
163.106414	6094.666006	25.112141
163.056311	6103.982624	25.117159
163.350346	6125.127281	25.122176
163.317446	6135.473445	25.127194
163.697773	6144.101470	25.132211
163.945960	6168.212624	25.137229
163.760511	6179.396685	25.142247
164.420240	6194.495636	25.147264
164.434917	6200.488793	25.152282
165.152039	6208.683924	25.157299
165.333315	6223.340688	25.162317
165.382472	6217.732555	25.167335
165.310615	6229.220343	25.172352
165.759980	6234.240966	25.177370
166.100626	6246.350660	25.182387
166.136638	6261.891380	25.187405
166.472366	6251.895991	25.192423
166.893370	6239.547866	25.197440
166.744921	6240.233350	25.202458
166.965246	6244.991512	25.207475
167.056634	6251.753749	25.212493
167.360425	6263.057358	25.217511
167.512225	6276.813270	25.222528
167.313308	6280.069407	25.227546
167.863483	6271.525293	25.232563
167.552064	6283.903420	25.237581
167.835236	6285.808869	25.242599
168.152762	6303.399210	25.247616
167.797981	6308.814793	25.252634
168.295469	6311.133766	25.257651
168.257857	6323.689363	25.262669
168.228510	6336.039872	25.267687
168.490560	6336.697679	25.272704
168.349646	6357.984401	25.277722
168.965384	6358.486682	25.282739
168.811738	6379.357671	25.287757
169.133425	6385.721322	25.292775
169.621875	6389.426525	25.297792
169.627095	6418.370042	25.302810
169.816209	6421.161499	25.307827
169.708657	6432.541048	25.312845
170.162029	6449.985589	25.317863
170.387319	6464.472705	25.322880
170.514917	6464.408420	25.327898
171.055267	6458.454369	25.332915
171.425725	6472.216515	25.337933
171.834078	6475.363287	25.342951
172.073229	6476.242698	25.347968
171.962378	6463.058616	25.352986
171.883078	6464.881826	25.358003
172.188436	6467.670496	25.363021
172.225654	6466.607210	25.368039
172.179326	6470.199419	25.373056
172.158249	6478.639859	25.378074
172.530248	6471.596947	25.383091
172.560070	6487.898162	25.388109
172.355422	6504.754498	25.393127
172.548166	6505.746742	25.398144
172.859350	6529.269348	25.403162
173.310848	6539.718745	25.408179
173.427405	6537.911856	25.413197
173.349329	6562.510776	25.418215
173.816649	6573.622533	25.423232
173.641430	6580.371563	25.428250
174.151066	6591.412855	25.433267
174.058563	6602.154387	25.438285
174.314044	6614.014377	25.443303
175.018899	6610.086059	25.448320
174.735873	6632.380925	25.453338
175.158975	6636.598600	25.458355
175.259613	6636.744759	25.463373
175.309100	6640.494047	25.468391
175.603509	6663.579708	25.473408
175.818730	6663.777627	25.478426
175.848810	6661.215000	25.483443
176.350329	6674.715674	25.488461
176.132216	6688.562416	25.493479
176.410503	6694.201377	25.498496
176.376288	6705.304283	25.503514
176.419838	6719.282438	25.508531
176.629519	6731.569988	25.513549
176.879181	6747.328149	25.518567
177.332180	6757.988332	25.523584
177.241585	6768.297712	25.528602
177.873050	6785.678849	25.533619
177.797044	6789.895886	25.538637
177.957226	6809.445933	25.543655
178.221283	6792.310926	25.548672
178.540531	6804.869047	25.553690
178.488687	6809.426081	25.558707
178.946733	6811.214808	25.563725
178.843962	6822.728440	25.568743
179.103580	6835.724915	25.573760
178.973457	6857.888731	25.578778
179.114199	6852.701662	25.583795
179.604315	6876.109739	25.588813
179.450437	6882.534476	25.593831
179.879147	6889.364397	25.598848
179.874357	6907.611129	25.603866
180.175600	6909.274583	25.608883
180.443913	6918.953246	25.613901
180.458328	6915.493723	25.618919
180.839640	6935.021270	25.623936
180.863469	6949.322240	25.628954
181.277026	6931.080555	25.633971
181.101531	6948.086176	25.638989
181.109798	6966.258509	25.644007
181.555765	6958.034340	25.649024
181.355605	6989.007911	25.654042
181.724212	7001.923423	25.659059
182.488316	7010.516738	25.664077
182.379812	7033.175436	25.669095
182.716291	7039.349745	25.674112
182.502118	7048.442109	25.679130
182.535466	7053.247653	25.684148
182.827593	7066.266687	25.689165
183.060467	7074.223199	25.694183
183.345507	7097.983386	25.699200
183.157491	7109.321986	25.704218
183.032901	7124.328979	25.709236
183.737008	7126.531740	25.714253
183.838627	7154.763389	25.719271
184.271042	7164.622990	25.724288
184.436740	7174.595937	25.729306
184.710117	7187.701473	25.734324
184.984033	7197.528139	25.739341
185.125904	7210.348577	25.744359
185.202517	7223.505185	25.749376
185.260248	7230.781539	25.754394
185.720343	7235.661527	25.759412
186.054732	7252.404442	25.764429
185.869463	7271.892143	25.769447
186.283800	7266.042847	25.774464
186.104097	7286.950735	25.779482
186.642911	7304.359843	25.784500
187.490871	7290.639757	25.789517
187.236214	7298.242132	25.794535
187.551721	7300.489563	25.799552
187.863522	7312.047638	25.804570
187.878084	7314.525600	25.809588
188.228930	7314.963930	25.814605
187.912726	7317.277453	25.819623
188.384093	7311.250661	25.824640
188.493133	7335.634542	25.829658
188.551437	7342.046105	25.834676
188.757042	7344.527450	25.839693
188.493357	7353.487832	25.844711
188.979936	7362.600073	25.849728
188.991575	7375.664883	25.854746
189.377037	7380.322334	25.859764
189.809154	7394.355630	25.864781
189.675260	7404.974507	25.869799
189.795887	7406.877692	25.874816
189.973913	7437.599120	25.879834
190.022072	7439.675169	25.884852
190.278412	7451.512874	25.889869
190.110809	7477.483339	25.894887
190.600544	7478.128509	25.899904
190.903285	7489.876227	25.904922
191.285085	7502.554013	25.909940
191.388634	7504.467802	25.914957
191.072281	7530.397550	25.919975
191.647060	7537.689982	25.924992
191.746560	7549.433953	25.930010
191.924313	7570.720387	25.935028
192.311159	7570.829585	25.940045
192.483155	7590.985450	25.945063
192.582396	7600.658464	25.950080
192.973090	7614.649000	25.955098
192.719610	7622.915470	25.960116
193.358664	7635.073940	25.965133
193.930130	7631.387742	25.970151
194.219389	7617.996425	25.975168
194.412183	7644.829576	25.980186
194.576088	7652.612480	25.985204
194.655492	7654.158734	25.990221
194.381100	7662.078401	25.995239
194.636415	7661.933163	26.000256
195.077957	7676.496363	26.005274
195.347408	7693.120295	26.010292
195.510859	7691.738573	26.015309
195.355892	7698.554908	26.020327
195.360548	7709.882919	26.025344
195.692774	7718.854745	26.030362
195.877245	7742.289310	26.035380
196.283820	7745.782081	26.040397
196.226554	7767.166853	26.045415
196.443589	7784.376811	26.050432
196.878148	7791.051992	26.055450
197.356365	7788.244616	26.060468
197.870016	7784.722614	26.065485
197.932235	7791.369024	26.070503
198.238832	7789.908604	26.075520
198.192678	7787.065219	26.080538
198.172066	7800.953897	26.085556
198.754778	7782.724341	26.090573
198.606920	7800.936745	26.095591
198.722912	7811.106895	26.100608
199.020020	7816.636270	26.105626
198.912624	7820.351850	26.110644
199.257215	7827.850304	26.115661
199.329343	7852.742945	26.120679
199.700213	7842.598472	26.125696
199.952870	7867.437964	26.130714
200.090072	7884.893684	26.135732
200.177615	7882.736375	26.140749
200.187870	7897.900482	26.145767
200.458938	7914.555092	26.150784
200.741931	7922.999022	26.155802
200.683784	7933.398066	26.160820
200.897156	7951.241458	26.165837
200.879944	7958.747296	26.170855
201.338706	7969.424747	26.175872
201.908969	7975.005849	26.180890
202.291856	7972.534295	26.185908
202.694822	7966.743986	26.190925
202.796894	7993.082323	26.195943
203.088506	7994.634521	26.200960
203.590901	7998.343817	26.205978
203.158437	8003.054745	26.210996
204.073378	7990.256208	26.216013
204.380471	7988.066638	26.221031
204.443366	7983.837824	26.226048
204.879301	7977.380481	26.231066
204.820167	7978.184392	26.236084
204.888934	7976.146523	26.241101
204.513967	7970.112359	26.246119
204.670719	7976.432961	26.251136
204.795338	7973.539102	26.256154
205.253811	7992.066621	26.261172
205.452916	7997.045915	26.266189
205.451573	8000.217022	26.271207
205.812725	8001.127049	26.276224
205.929692	8007.366661	26.281242
205.550070	8026.859968	26.286260
206.027992	8031.938039	26.291277
206.181569	8055.392186	26.296295
206.316987	8064.472713	26.301312
206.310525	8090.183665	26.306330
206.709029	8103.491180	26.311348
206.959671	8114.157848	26.316365
207.042438	8136.490674	26.321383
207.445542	8151.455885	26.326400
207.835616	8161.526317	26.331418
207.642343	8183.241830	26.336436
207.900062	8188.117809	26.341453
207.910322	8220.523233	26.346471
208.213643	8240.076340	26.351488
208.569462	8246.615164	26.356506
208.811522	8266.593950	26.361524
208.817718	8273.127142	26.366541
209.108542	8294.371403	26.371559
209.253390	8303.953405	26.376576
209.686258	8318.183003	26.381594
209.702054	8343.432468	26.386612
210.252888	8357.562639	26.391629
210.386105	8361.361966	26.396647
210.334072	8380.970726	26.401664
210.704146	8388.093587	26.406682
211.109129	8415.012727	26.411700
211.775317	8421.921967	26.416717
211.820919	8430.348159	26.421735
211.867290	8438.840334	26.426752
212.095869	8449.687815	26.431770
212.382344	8467.678735	26.436788
212.540803	8460.338436	26.441805
212.529412	8461.488086	26.446823
212.593413	8478.996695	26.451840
212.728539	8492.226147	26.456858
213.179431	8505.035815	26.461876
213.000152	8515.393587	26.466893
213.610686	8522.866524	26.471911
213.546876	8550.461845	26.476928
213.921631	8561.594184	26.481946
213.687211	8571.721168	26.486964
214.010164	8587.422774	26.491981
214.480118	8604.622476	26.496999
214.339974	8627.137543	26.502016
214.854802	8637.947792	26.507034
215.018658	8654.468837	26.512052
215.407337	8662.990771	26.517069
215.514729	8681.287100	26.522087
215.609916	8699.595627	26.527104
216.131005	8704.622195	26.532122
216.330478	8726.316804	26.537140
216.403790	8724.794334	26.542157
216.881657	8754.657383	26.547175
217.098023	8750.758399	26.552192
217.700764	8762.675312	26.557210
217.640798	8781.978959	26.562228
217.953676	8778.463557	26.567245
218.001163	8769.253344	26.572263
217.943171	8801.582768	26.577280
218.353059	8813.713821	26.582298
218.314398	8825.378126	26.587316
218.735023	8842.187384	26.592333
219.046280	8858.380220	26.597351
219.155234	8873.082601	26.602368
219.499611	8876.057527	26.607386
219.612857	8894.113561	26.612404
219.915752	8913.124631	26.617421
219.962964	8920.347220	26.622439
220.070552	8930.959764	26.627456
220.353317	8948.438376	26.632474
220.505351	8963.168210	26.637492
220.867701	8982.038864	26.642509
220.905534	8991.152823	26.647527
221.154450	9018.030644	26.652544
221.640984	9028.629279	26.657562
221.246139	9052.639464	26.662580
221.918568	9062.492762	26.667597
222.112555	9081.423825	26.672615
222.040025	9095.121701	26.677632
222.716654	9112.169032	26.682650
222.777128	9125.174859	26.687668
222.986045	9139.968592	26.692685
223.368792	9151.355857	26.697703
223.534047	9164.541359	26.702720
224.166336	9176.088748	26.707738
224.438172	9186.730771	26.712756
224.612490	9186.186468	26.717773
225.003305	9186.588590	26.722791
224.762279	9206.696399	26.727808
225.114687	9204.916913	26.732826
225.070598	9207.554846	26.737844
225.236217	9215.264320	26.742861
225.742700	9232.623397	26.747879
225.802981	9243.458542	26.752896
226.201465	9249.494832	26.757914
226.274015	9273.775549	26.762932
226.414450	9275.288635	26.767949
226.713955	9285.906250	26.772967
226.823834	9294.289236	26.777984
227.321760	9297.515992	26.783002
227.741105	9321.238638	26.788020
227.327310	9334.506364	26.793037
227.597556	9341.405969	26.798055
228.014104	9363.206188	26.803072
227.975632	9357.331477	26.808090
228.494436	9389.306193	26.813108
228.468965	9403.160142	26.818125
228.995361	9412.545887	26.823143
228.881992	9432.669455	26.828160
229.112643	9449.049306	26.833178
229.481052	9457.543842	26.838196
229.745739	9471.641598	26.843213
230.016268	9489.210539	26.848231
229.877454	9507.224072	26.853248
230.398271	9526.303488	26.858266
230.399272	9539.477335	26.863284
230.783017	9560.474851	26.868301
231.033465	9571.507354	26.873319
231.222284	9598.291914	26.878336
231.422387	9605.515644	26.883354
231.815151	9627.638370	26.888372
232.436521	9636.076945	26.893389
232.907446	9646.978740	26.898407
233.031284	9661.326169	26.903424
233.498021	9653.933001	26.908442
233.685839	9664.990116	26.913460
233.454926	9662.358798	26.918477
234.051261	9676.703718	26.923495
234.135349	9689.671248	26.928512
234.335149	9682.574025	26.933530
234.779857	9698.706755	26.938548
234.949590	9708.827919	26.943565
235.104534	9714.247273	26.948583
235.276150	9719.050127	26.953600
235.616491	9736.830552	26.958618
235.714081	9747.825773	26.963636
235.861356	9755.009204	26.968653
236.106924	9758.663880	26.973671
235.968147	9779.077241	26.978688
236.207045	9789.141789	26.983706
236.612440	9794.613719	26.988724
236.580733	9806.825417	26.993741
236.705707	9821.922028	26.998759
236.934682	9845.791930	27.003776
236.979032	9848.736575	27.008794
237.257344	9863.161488	27.013812
237.340502	9887.400187	27.018829
237.851626	9903.960118	27.023847
237.823502	9921.833731	27.028864
238.058909	9934.727772	27.033882
238.662709	9958.742328	27.038900
239.039151	9967.430262	27.043917
239.383504	9986.539575	27.048935
239.425486	9993.073320	27.053952
239.974211	10009.358615	27.058970
239.864174	10026.884573	27.063988
240.309702	10046.732958	27.069005
240.858834	10061.175096	27.074023
241.014056	10073.577966	27.079040
241.089196	10074.234664	27.084058
241.363128	10096.541507	27.089076
241.341273	10109.843055	27.094093
241.538284	10118.079609	27.099111
241.340997	10147.039398	27.104128
241.792165	10159.582470	27.109146
242.332340	10174.050149	27.114164
242.675765	10204.437659	27.119181
242.886111	10209.723621	27.124199
243.128452	10231.843671	27.129216
243.086409	10244.927014	27.134234
243.593166	10265.673348	27.139252
244.019124	10281.922631	27.144269
244.088297	10295.318833	27.149287
244.241139	10318.727841	27.154304
244.258276	10332.099709	27.159322
244.865302	10341.413376	27.164340
244.727244	10365.653085	27.169357
245.300450	10373.223024	27.174375
245.594991	10396.358705	27.179392
245.791406	10409.203490	27.184410
246.033873	10422.515123	27.189428
246.453183	10445.150713	27.194445
246.626779	10458.069222	27.199463
246.970392	10474.634448	27.204480
247.303780	10473.421358	27.209498
247.531563	10492.964656	27.214516
247.743421	10509.527706	27.219533
248.286820	10511.754264	27.224551
248.236495	10528.757360	27.229568
248.587342	10539.298029	27.234586
249.036291	10551.545076	27.239604
249.242892	10567.449502	27.244621
249.383080	10561.979886	27.249639
248.951821	10580.657162	27.254656
249.576712	10582.653128	27.259674
250.307999	10595.973964	27.264692
250.183341	10618.388402	27.269709
250.553062	10618.826203	27.274727
250.397274	10631.718268	27.279744
250.584965	10651.631770	27.284762
251.038179	10659.891925	27.289780
250.819347	10675.879232	27.294797
251.092215	10686.275029	27.299815
251.302144	10714.396162	27.304832
251.543271	10729.752990	27.309850
251.815805	10761.607755	27.314868
251.663371	10786.669732	27.319885
252.674948	10788.169647	27.324903
253.069344	10806.687258	27.329920
253.313479	10823.652800	27.334938
253.833596	10836.543551	27.339956
254.020103	10849.631519	27.344973
254.327016	10858.981936	27.349991
254.549770	10862.749919	27.355008
254.698681	10881.044274	27.360026
254.920743	10888.325724	27.365044
255.100353	10893.380715	27.370061
255.486864	10915.230870	27.375079
255.560656	10922.871252	27.380096
255.816923	10946.111274	27.385114
256.164760	10948.919216	27.390132
256.208576	10967.470869	27.395149
256.380165	10984.682302	27.400167
256.507796	11011.806147	27.405184
256.623679	11025.920029	27.410202
257.111746	11040.560558	27.415220
257.008076	11069.371029	27.420237
257.717508	11085.059297	27.425255
258.131154	11107.708986	27.430272
258.268722	11122.244904	27.435290
258.711488	11142.677596	27.440308
258.875813	11162.273590	27.445325
259.070474	11166.715125	27.450343
259.328953	11190.312100	27.455360
259.857394	11207.880898	27.460378
260.524924	11213.134875	27.465396
260.542540	11219.625417	27.470413
261.123197	11219.708890	27.475431
261.749555	11231.892798	27.480448
261.872138	11235.862391	27.485466
261.937508	11237.783141	27.490484
261.909880	11249.969185	27.495501
262.111015	11243.376707	27.500519
262.120319	11263.693303	27.505536
262.042388	11280.615067	27.510554
262.500432	11300.103229	27.515572
262.490293	11314.138495	27.520589
262.560249	11339.921913	27.525607
263.174987	11362.327817	27.530624
263.243964	11380.969234	27.535642
263.291325	11392.922274	27.540660
263.535706	11420.637432	27.545677
263.686252	11440.167704	27.550695
264.162033	11458.673538	27.555712
264.306946	11489.205074	27.560730
265.052136	11503.772801	27.565748
264.743562	11531.218574	27.570765
265.035223	11546.463104	27.575783
265.458711	11553.004009	27.580800
265.757678	11585.526885	27.585818
266.346464	11586.886495	27.590836
266.295172	11621.370005	27.595853
266.920978	11633.195812	27.600871
267.303814	11653.273937	27.605888
267.416150	11676.474270	27.610906
267.784220	11678.253953	27.615924
267.940017	11699.697710	27.620941
268.136568	11716.086249	27.625959
268.566613	11739.823400	27.630976
268.863583	11755.664497	27.635994
269.181171	11766.149936	27.641012
269.050316	11780.674371	27.646029
269.673356	11791.781543	27.651047
269.758607	11812.886057	27.656064
269.910880	11831.044465	27.661082
270.498670	11849.964645	27.666100
270.506412	11870.184309	27.671117
270.825130	11901.148830	27.676135
271.676518	11902.772598	27.681152
271.663060	11924.299731	27.686170
271.897442	11931.448278	27.691188
272.088617	11939.969523	27.696205
272.197085	11955.480975	27.701223
272.831159	11973.311674	27.706240
272.748674	11986.031062	27.711258
273.205205	11995.544881	27.716276
273.442117	12025.980582	27.721293
273.701452	12037.233079	27.726311
274.242683	12051.536322	27.731328
274.298459	12061.839177	27.736346
275.011233	12071.376153	27.741364
274.856071	12096.837230	27.746381
275.160868	12111.934033	27.751399
275.560647	12122.400125	27.756416
275.377484	12145.913727	27.761434
276.075126	12152.501321	27.766452
276.392378	12161.058283	27.771469
276.229918	12182.783285	27.776487
276.639630	12194.229369	27.781504
276.703991	12212.480760	27.786522
277.233898	12234.100399	27.791540
277.271161	12260.128890	27.796557
277.747777	12279.911507	27.801575
277.922845	12293.128879	27.806592
278.098098	12323.323718	27.811610
278.433749	12326.197032	27.816628
278.843069	12351.806469	27.821645
278.772451	12371.192548	27.826663
279.419279	12377.143691	27.831680
279.423148	12399.536140	27.836698
279.816798	12415.612625	27.841716
279.886817	12432.688798	27.846733
279.982217	12461.847210	27.851751
280.506488	12477.235855	27.856768
280.473742	12509.497946	27.861786
280.781924	12528.731953	27.866804
281.339170	12545.316959	27.871821
281.356133	12575.604631	27.876839
281.677354	12589.260420	27.881856
282.097670	12609.319475	27.886874
282.550003	12625.245146	27.891892
282.775559	12647.029002	27.896909
283.123065	12667.704453	27.901927
283.996715	12683.175764	27.906944
283.879236	12702.681703	27.911962
284.278641	12708.210366	27.916980
284.273138	12726.930245	27.921997
284.457494	12752.591170	27.927015
285.323961	12763.551835	27.932032
285.200316	12778.839596	27.937050
285.495611	12792.345815	27.942068
285.783912	12822.614541	27.947085
286.415203	12837.368196	27.952103
286.775829	12846.809088	27.957120
286.844098	12875.173371	27.962138
287.042652	12879.328173	27.967156
287.162932	12904.082248	27.972173
287.535855	12920.780875	27.977191
288.090802	12936.579827	27.982208
288.273230	12957.774246	27.987226
288.542745	12969.056708	27.992244
288.728208	12985.037493	27.997261
288.800154	12995.506164	28.002279
289.305747	13016.443023	28.007296
289.506135	13037.548399	28.012314
289.878233	13056.739925	28.017332
290.266366	13079.991523	28.022349
290.691059	13091.611632	28.027367
291.092029	13095.417697	28.032384
291.171907	13115.441847	28.037402
291.930867	13118.624894	28.042420
292.382246	13134.814656	28.047437
292.207153	13150.382066	28.052455
292.766964	13145.897077	28.057472
292.678766	13175.268639	28.062490
293.117121	13180.377912	28.067508
293.472821	13199.161039	28.072525
293.310822	13213.377232	28.077543
293.432996	13235.270900	28.082560
293.677180	13256.597680	28.087578
294.022574	13275.588314	28.092596
294.299406	13296.759205	28.097613
294.587493	13310.124557	28.102631
295.039077	13329.716923	28.107648
295.235125	13353.714500	28.112666
295.270543	13356.661842	28.117684
295.758139	13387.646951	28.122701
296.088273	13405.112551	28.127719
296.645731	13433.803823	28.132736
296.751093	13449.739907	28.137754
296.963966	13470.439286	28.142772
297.161510	13497.720452	28.147789
297.173383	13514.769516	28.152807
297.726490	13530.953327	28.157824
298.049848	13546.365930	28.162842
298.450998	13576.436428	28.167860
298.703654	13592.954626	28.172877
298.941252	13609.482720	28.177895
299.533905	13624.933956	28.182912
299.669604	13648.536115	28.187930
299.888333	13672.697363	28.192948
300.193607	13687.162858	28.197965
300.435464	13708.952328	28.202983
300.987507	13731.700582	28.208000
301.291440	13750.050633	28.213018
301.877845	13770.671207	28.218036
301.812079	13783.922256	28.223053
302.323850	13806.673104	28.228071
302.730198	13826.423280	28.233088
302.741849	13846.275945	28.238106
302.843391	13871.706150	28.243124
303.171279	13885.821864	28.248141
303.408600	13913.261661	28.253159
303.845834	13934.917387	28.258176
303.938942	13965.731565	28.263194
304.834709	13974.411863	28.268212
305.190147	13999.805556	28.273229
305.361079	14023.663145	28.278247
305.711486	14040.037343	28.283264
305.687848	14060.962473	28.288282
306.032779	14084.403326	28.293300
306.511802	14091.455945	28.298317
306.726496	14119.283285	28.303335
306.922769	14138.037382	28.308352
307.261374	14153.190259	28.313370
307.512979	14177.492010	28.318388
307.775430	14201.388526	28.323405
307.710316	14222.895546	28.328423
308.079103	14248.418791	28.333440
308.386652	14279.810204	28.338458
308.548907	14304.492453	28.343476
308.961368	14339.668939	28.348493
308.794854	14373.645853	28.353511
309.823657	14402.728976	28.358528
310.104333	14430.458688	28.363546
310.421232	14450.157603	28.368564
311.091106	14478.143904	28.373581
311.274871	14493.050302	28.378599
311.642182	14500.482155	28.383616
311.870175	14520.502940	28.388634
312.033741	14549.370872	28.393652
312.447823	14560.534645	28.398669
312.686219	14585.139575	28.403687
312.912024	14597.381383	28.408704
313.308809	14622.427073	28.413722
313.465621	14630.707030	28.418740
314.238436	14648.850785	28.423757
314.733675	14674.532897	28.428775
314.911206	14686.562832	28.433792
315.081237	14708.725037	28.438810
315.451164	14732.553001	28.443828
315.512089	14740.633382	28.448845
315.698130	14771.828087	28.453863
315.922087	14789.344667	28.458880
315.998545	14820.124935	28.463898
316.249877	14846.718081	28.468916
316.873675	14877.982971	28.473933
317.208712	14907.830056	28.478951
317.423799	14934.475874	28.483968
317.777524	14960.668917	28.488986
318.013411	14998.338268	28.494004
318.579784	15011.820572	28.499021
318.562936	15050.815325	28.504039
319.062301	15065.956378	28.509056
319.662504	15096.618697	28.514074
319.669479	15129.726182	28.519092
320.290913	15155.351200	28.524109
320.475859	15186.367129	28.529127
320.860936	15202.677904	28.534144
321.218858	15220.062523	28.539162
321.306827	15251.903545	28.544180
321.950333	15279.240214	28.549197
321.860284	15304.609642	28.554215
322.307072	15324.218717	28.559232
322.973788	15357.084661	28.564250
323.189246	15386.265922	28.569268
323.598185	15394.795335	28.574285
323.742058	15428.249005	28.579303
324.130525	15456.084139	28.584320
324.256922	15474.711757	28.589338
324.827276	15516.111745	28.594356
325.208093	15543.213724	28.599373
325.119737	15558.001655	28.604391
325.765389	15580.881423	28.609408
325.938528	15616.236849	28.614426
326.096622	15628.147606	28.619444
326.653857	15657.995673	28.624461
327.108730	15683.876433	28.629479
327.563435	15726.659591	28.634496
328.015609	15741.219448	28.639514
328.172046	15773.525176	28.644532
328.652452	15774.906998	28.649549
328.764751	15806.270550	28.654567
328.862244	15815.675311	28.659584
329.212945	15836.636393	28.664602
329.409589	15875.845042	28.669620
329.735677	15887.243858	28.674637
329.957291	15914.513380	28.679655
330.111007	15943.548273	28.684672
330.198318	15969.614649	28.689690
330.662893	16008.559900	28.694708
330.813492	16029.985760	28.699725
330.967351	16069.903209	28.704743
331.572708	16099.625187	28.709760
332.530896	16124.998968	28.714778
332.970078	16149.406410	28.719796
333.383782	16184.057947	28.724813
333.647071	16213.551620	28.729831
333.597403	16239.383812	28.734848
334.344902	16262.158808	28.739866
334.487097	16283.993796	28.744884
335.081393	16308.921399	28.749901
335.555987	16330.246244	28.754919
336.073683	16339.910310	28.759936
336.815500	16341.720362	28.764954
336.789692	16363.462563	28.769972
337.147637	16383.963834	28.774989
337.566348	16402.417261	28.780007
337.585805	16427.099099	28.785024
337.916479	16440.830245	28.790042
338.211155	16464.709891	28.795060
338.381306	16479.340587	28.800077
339.016838	16486.208862	28.805095
338.952552	16519.391799	28.810112
339.303865	16532.068652	28.815130
339.561440	16568.388306	28.820148
339.960428	16598.240387	28.825165
340.365127	16625.605207	28.830183
340.635816	16650.692012	28.835200
341.093242	16670.314101	28.840218
341.152861	16703.205267	28.845236
341.936546	16718.698184	28.850253
342.337024	16745.686753	28.855271
342.589697	16772.178884	28.860288
342.843570	16788.221032	28.865306
343.423081	16817.110386	28.870324
343.774358	16836.026228	28.875341
344.081090	16863.242329	28.880359
344.688211	16882.370393	28.885376
344.732420	16897.917165	28.890394
345.000313	16918.622462	28.895412
345.417425	16935.220798	28.900429
345.825233	16957.901953	28.905447
345.679605	16984.835850	28.910464
345.975120	17003.155898	28.915482
346.416072	17031.735668	28.920500
346.709819	17050.270214	28.925517
347.244155	17074.254334	28.930535
347.375703	17108.545452	28.935552
347.923229	17123.647301	28.940570
347.877411	17154.124854	28.945588
348.357764	17172.346359	28.950605
348.747512	17195.891133	28.955623
348.998829	17223.841272	28.960640
349.600586	17240.649478	28.965658
349.785098	17273.626278	28.970676
350.018829	17291.843133	28.975693
350.538618	17324.939440	28.980711
351.201987	17341.521411	28.985728
351.668485	17362.871219	28.990746
351.733175	17396.723250	28.995764
352.013683	17423.003404	29.000781
352.676502	17433.644806	29.005799
352.880132	17463.561578	29.010816
353.315047	17477.892767	29.015834
353.739153	17499.352665	29.020852
353.815115	17523.527060	29.025869
353.956635	17546.420209	29.030887
354.444602	17564.240579	29.035904
355.245329	17586.717329	29.040922
355.620707	17612.332700	29.045940
356.039910	17632.600281	29.050957
356.115142	17657.883249	29.055975
356.123138	17686.987939	29.060992
356.700936	17708.698829	29.066010
356.911273	17742.647694	29.071028
357.221308	17769.840256	29.076045
357.312629	17800.348796	29.081063
357.452866	17830.742909	29.086080
358.120956	17858.725808	29.091098
358.378537	17902.497382	29.096116
358.550409	17935.529963	29.101133
358.820757	17967.360697	29.106151
359.220174	18012.689512	29.111168
359.796277	18035.137748	29.116186
360.166952	18069.135003	29.121204
360.789682	18107.280014	29.126221
361.263910	18131.156452	29.131239
361.305769	18163.225969	29.136256
361.836373	18185.556868	29.141274
362.010294	18235.225883	29.146292
362.234682	18262.700677	29.151309
362.891131	18295.408766	29.156327
362.991285	18330.424922	29.161344
363.284732	18363.658335	29.166362
363.615109	18396.441432	29.171380
364.175901	18441.502859	29.176397
364.717017	18460.259524	29.181415
365.073237	18503.229639	29.186432
365.745641	18522.887147	29.191450
365.796517	18554.248129	29.196468
366.199203	18581.090324	29.201485
366.594585	18605.433618	29.206503
366.776515	18639.897255	29.211520
367.869746	18638.059311	29.216538
368.361808	18657.773683	29.221556
368.542678	18680.279140	29.226573
368.686298	18691.383695	29.231591
368.757306	18719.996785	29.236608
369.311824	18744.995683	29.241626
369.610882	18772.833120	29.246644
370.047313	18798.522218	29.251661
370.676213	18826.160331	29.256679
370.378914	18856.517104	29.261696
370.696376	18881.144916	29.266714
370.936522	18917.454729	29.271732
371.478066	18947.942201	29.276749
371.494374	18980.492697	29.281767
371.735661	19020.628026	29.286784
372.649772	19051.566605	29.291802
373.068530	19089.245308	29.296820
373.472551	19119.651478	29.301837
374.968154	19120.070021	29.306855
375.404090	19145.303436	29.311872
375.645587	19166.628976	29.316890
376.249029	19183.540611	29.321908
376.091405	19199.615978	29.326925
376.761634	19209.087648	29.331943
376.568852	19233.407526	29.336960
376.680987	19257.691060	29.341978
376.884628	19289.504807	29.346996
377.092438	19323.018501	29.352013
377.680254	19343.263809	29.357031
377.963929	19383.337799	29.362048
378.468540	19408.767803	29.367066
378.772425	19452.146940	29.372084
378.985615	19485.534129	29.377101
379.415728	19518.993132	29.382119
379.776643	19562.932445	29.387136
380.219211	19587.394570	29.392154
380.811039	19618.236009	29.397172
380.816552	19655.428716	29.402189
381.296871	19691.777263	29.407207
381.676316	19733.554407	29.412224
382.216050	19753.902015	29.417242
382.736150	19797.832766	29.422260
382.962607	19831.481995	29.427277
383.537141	19857.705623	29.432295
383.390093	19896.603736	29.437312
384.131995	19922.131428	29.442330
384.602966	19951.075212	29.447348
384.818894	19972.927254	29.452365
385.784590	20009.118084	29.457383
385.814515	20043.865369	29.462400
386.004397	20070.642840	29.467418
386.538957	20098.241147	29.472436
386.663517	20128.385893	29.477453
387.305035	20162.322107	29.482471
387.155543	20188.262782	29.487488
387.711693	20217.079690	29.492506
388.094797	20249.642495	29.497524
388.137895	20279.237434	29.502541
388.617797	20316.261221	29.507559
388.924538	20361.521053	29.512576
389.683599	20393.791145	29.517594
389.810786	20434.766518	29.522612
389.820442	20473.703696	29.527629
390.270026	20512.261372	29.532647
390.577609	20563.654167	29.537664
390.921929	20600.713615	29.542682
391.786653	20632.668098	29.547700
392.341828	20671.630674	29.552717
392.832112	20710.221728	29.557735
392.879096	20748.118806	29.562752
393.354487	20783.985937	29.567770
393.733528	20825.200200	29.572788
394.279200	20861.919463	29.577805
394.935567	20899.940322	29.582823
395.185843	20937.015549	29.587840
395.827571	20954.660155	29.592858
396.816491	20986.633374	29.597876
397.118220	21013.610420	29.602893
397.537500	21029.034991	29.607911
397.744675	21063.567271	29.612928
398.055469	21079.280885	29.617946
398.676436	21104.345428	29.622964
398.574982	21137.060523	29.627981
399.223954	21169.663204	29.632999
399.615617	21193.631120	29.638016
400.435049	21209.787552	29.643034
400.812916	21234.923328	29.648052
401.170701	21267.047300	29.653069
401.873255	21277.707074	29.658087
402.169199	21317.169347	29.663104
402.210071	21335.340923	29.668122
402.710627	21356.576184	29.673140
402.805875	21392.914026	29.678157
403.355017	21415.181226	29.683175
403.684309	21451.004638	29.688192
403.560634	21479.753011	29.693210
403.819514	21511.838898	29.698228
404.103616	21558.762853	29.703245
404.677627	21584.074281	29.708263
405.389912	21627.521546	29.713280
405.511627	21662.625579	29.718298
405.757292	21706.104879	29.723316
406.001513	21749.920831	29.728333
406.866857	21778.624789	29.733351
407.183525	21821.868629	29.738368
407.487804	21856.125689	29.743386
408.300852	21887.582962	29.748404
408.443036	21926.226948	29.753421
409.086489	21948.761837	29.758439
409.323512	21982.518733	29.763456
409.444825	22000.349825	29.768474
410.301881	22037.327808	29.773492
410.522627	22081.561914	29.778509
411.034542	22108.462450	29.783527
411.340113	22148.178089	29.788544
411.578734	22189.393088	29.793562
412.244507	22212.064994	29.798580
412.106520	22248.914534	29.803597
412.762150	22276.471386	29.808615
413.030497	22321.388533	29.813632
413.236870	22359.646078	29.818650
413.986612	22387.132207	29.823668
414.565276	22432.606698	29.828685
414.963665	22464.348576	29.833703
415.264186	22493.840883	29.838720
415.825224	22545.671540	29.843738
416.501316	22573.102779	29.848756
416.470512	22619.061641	29.853773
417.047928	22644.235605	29.858791
417.397435	22691.440774	29.863808
417.491495	22729.598173	29.868826
418.248568	22772.546025	29.873844
418.406526	22820.008149	29.878861
419.136055	22849.785632	29.883879
419.205568	22901.076673	29.888896
419.089842	22940.588894	29.893914
419.909719	22980.939077	29.898932
420.433929	23031.841456	29.903949
420.913812	23082.657330	29.908967
421.229897	23134.864483	29.913984
421.782342	23180.013690	29.919002
422.150057	23219.396017	29.924020
422.626072	23264.977469	29.929037
422.948009	23306.472745	29.934055
423.419367	23346.158667	29.939072
423.730290	23390.155202	29.944090
425.019835	23429.097374	29.949108
425.205925	23470.354001	29.954125
425.639005	23501.413447	29.959143
426.593612	23535.750902	29.964160
426.811620	23573.691294	29.969178
427.414992	23606.503194	29.974196
427.560541	23643.786552	29.979213
428.098495	23652.936605	29.984231
428.573037	23681.040692	29.989248
428.843146	23723.343242	29.994266
429.416374	23754.947206	29.999284
429.862587	23780.939451	30.004301
430.154761	23820.665347	30.009319
430.890024	23841.858679	30.014336
431.841988	23862.983644	30.019354
432.499418	23872.543298	30.024372
432.981443	23904.759955	30.029389
433.275629	23906.278365	30.034407
433.488201	23922.856449	30.039424
433.490015	23947.776816	30.044442
433.894454	23958.103091	30.049460
434.156126	23993.461737	30.054477
434.285389	24012.858993	30.059495
434.843589	24053.695501	30.064512
435.147300	24080.280453	30.069530
435.398498	24101.894698	30.074548
435.621997	24146.966725	30.079565
436.241490	24180.097053	30.084583
436.604569	24217.314012	30.089600
436.483227	24265.934049	30.094618
437.414172	24299.838958	30.099636
437.426238	24348.719209	30.104653
437.754561	24386.153208	30.109671
438.209268	24441.896773	30.114688
438.655242	24484.341898	30.119706
439.169067	24528.268288	30.124724
439.131601	24585.555160	30.129741
439.663873	24641.027110	30.134759
440.208229	24689.919701	30.139776
440.510733	24751.056251	30.144794
441.133456	24795.992456	30.149812
441.390008	24855.176815	30.154829
442.079697	24911.581737	30.159847
442.814145	24953.860835	30.164864
443.165085	24999.627089	30.169882
443.997107	25040.943203	30.174900
444.367498	25082.544090	30.179917
444.844430	25129.954391	30.184935
445.545502	25171.608386	30.189952
445.712988	25225.676029	30.194970
446.418503	25261.222791	30.199988
446.833476	25301.934845	30.205005
447.634791	25334.274466	30.210023
448.562592	25355.788915	30.215040
448.778510	25385.233095	30.220058
449.559780	25417.106565	30.225076
449.620134	25452.072747	30.230093
450.262756	25476.184402	30.235111
451.224527	25503.649243	30.240128
450.968045	25547.189884	30.245146
451.400650	25569.231762	30.250164
451.968393	25609.303427	30.255181
452.387994	25639.945357	30.260199
452.656808	25668.864055	30.265216
452.758398	25708.003438	30.270234
453.500156	25741.771394	30.275252
453.874541	25780.449964	30.280269
454.420143	25810.885440	30.285287
454.874007	25850.722968	30.290304
454.931542	25877.622705	30.295322
455.397296	25911.790287	30.300340
455.696016	25948.481882	30.305357
455.962816	25976.143336	30.310375
456.582087	26013.466249	30.315392
456.827035	26071.153811	30.320410
457.550054	26096.937926	30.325428
457.546081	26147.911540	30.330445
457.781966	26187.861048	30.335463
458.618386	26228.830529	30.340480
458.978958	26280.439762	30.345498
459.475908	26317.971946	30.350516
460.150568	26370.762005	30.355533
460.628065	26422.962842	30.360551
460.940737	26464.455969	30.365568
461.183565	26508.089042	30.370586
461.847553	26547.438669	30.375604
462.402451	26605.193788	30.380621
462.364969	26657.568028	30.385639
462.971137	26696.276477	30.390656
463.312274	26749.580221	30.395674
463.940598	26801.632202	30.400692
464.098729	26846.463811	30.405709
464.843860	26899.292434	30.410727
465.404474	26954.579568	30.415744
466.001337	27006.793218	30.420762
466.418862	27055.465047	30.425780
466.956829	27091.381334	30.430797
467.243201	27144.973222	30.435815
467.983476	27193.461689	30.440832
468.324019	27239.045311	30.445850
468.928143	27290.154135	30.450868
469.681446	27336.200146	30.455885
470.149707	27384.552887	30.460903
470.627715	27421.844055	30.465920
471.258172	27455.289831	30.470938
472.320947	27478.712780	30.475956
473.147422	27508.974362	30.480973
473.436653	27540.358436	30.485991
474.135877	27566.540278	30.491008
474.549577	27612.407966	30.496026
474.659087	27633.408202	30.501044
475.018370	27669.144664	30.506061
475.758705	27692.920265	30.511079
476.203494	27723.172145	30.516096
476.026873	27769.709477	30.521114
476.424044	27797.425773	30.526132
477.088212	27839.711846	30.531149
477.267562	27883.901604	30.536167
477.712776	27923.394231	30.541184
477.899348	27977.012652	30.546202
478.222113	28023.650799	30.551220
478.681051	28079.389748	30.556237
479.070055	28133.072560	30.561255
479.482475	28183.374836	30.566272
479.640894	28240.766398	30.571290
480.285357	28291.949176	30.576308
480.706605	28341.845549	30.581325
480.820885	28406.243013	30.586343
481.257975	28458.064473	30.591360
481.602812	28523.125347	30.596378
482.160839	28584.301119	30.601396
482.717883	28634.625878	30.606413
482.878183	28695.966285	30.611431
483.762994	28758.932849	30.616448
484.091434	28824.158278	30.621466
484.680511	28881.516589	30.626484
485.088889	28941.677459	30.631501
485.603807	29005.849578	30.636519
486.386770	29048.468152	30.641536
486.837164	29107.940577	30.646554
487.424942	29167.905082	30.651572
488.080353	29224.784413	30.656589
488.517228	29281.911505	30.661607
489.628811	29332.838766	30.666624
490.108132	29381.219333	30.671642
490.405027	29428.215485	30.676660
491.157077	29472.654003	30.681677
491.437629	29525.896933	30.686695
492.287398	29567.971980	30.691712
492.572099	29620.488043	30.696730
493.114910	29661.584704	30.701748
493.925633	29706.042879	30.706765
493.906129	29754.634820	30.711783
494.570621	29794.721147	30.716800
494.904449	29849.977048	30.721818
495.441712	29884.062039	30.726836
496.388718	29934.418526	30.731853
496.796011	29985.173190	30.736871
497.528868	30029.734484	30.741888
498.145405	30077.069281	30.746906
498.530804	30104.826058	30.751924
499.023217	30153.178461	30.756941
499.398211	30193.617629	30.761959
500.215304	30231.573590	30.766976
500.567705	30274.765134	30.771994
501.003843	30314.556573	30.777012
501.471348	30360.533757	30.782029
501.592707	30404.983870	30.787047
502.098276	30444.534464	30.792064
502.678644	30496.698916	30.797082
503.310576	30549.146889	30.802100
503.501610	30594.836225	30.807117
503.797742	30654.152877	30.812135
504.620356	30697.987741	30.817152
504.768204	30760.958072	30.822170
505.058119	30803.770098	30.827188
505.927468	30861.388597	30.832205
506.275305	30918.928034	30.837223
507.035496	30953.646428	30.842240
507.500397	31010.396833	30.847258
507.721030	31058.172641	30.852276
508.523765	31094.504785	30.857293
508.865140	31154.440174	30.862311
509.546935	31189.422157	30.867328
509.999518	31242.006514	30.872346
510.167463	31291.209895	30.877364
510.984040	31324.498435	30.882381
510.933755	31390.093881	30.887399
511.636296	31433.792228	30.892416
512.131205	31492.643655	30.897434
512.410916	31546.619882	30.902452
512.911818	31602.570643	30.907469
513.469793	31665.898365	30.912487
514.411085	31712.771627	30.917504
515.031091	31761.772009	30.922522
515.238403	31818.022454	30.927540
515.940075	31861.222430	30.932557
516.155662	31923.459801	30.937575
517.066863	31977.057867	30.942592
517.584797	32023.903305	30.947610
517.898329	32077.286388	30.952628
518.944393	32121.678961	30.957645
519.471838	32175.118130	30.962663
520.241148	32217.751869	30.967680
520.809377	32264.359853	30.972698
520.911354	32311.658537	30.977716
521.634111	32358.155481	30.982733
521.698089	32414.251099	30.987751
522.649463	32455.822449	30.992768
522.865678	32516.510944	30.997786
523.459657	32561.170590	31.002804
524.399286	32592.153398	31.007821
524.967602	32652.242504	31.012839
525.399422	32693.767959	31.017856
526.006922	32751.302382	31.022874
526.219430	32797.241876	31.027892
527.113880	32838.664057	31.032909
527.463759	32893.823594	31.037927
527.869878	32938.490539	31.042944
528.644473	32988.631658	31.047962
528.788501	33035.831137	31.052980
529.448508	33076.202042	31.057997
529.539273	33131.859192	31.063015
530.285191	33187.180458	31.068032
530.942370	33236.171415	31.073050
531.458153	33298.714509	31.078068
532.300951	33343.117528	31.083085
532.572415	33399.167668	31.088103
532.572815	33452.803680	31.093120
533.170868	33503.712200	31.098138
533.874526	33552.699843	31.103156
534.913231	33605.356003	31.108173
535.196352	33649.927807	31.113191
536.345822	33685.452222	31.118208
537.048023	33732.351969	31.123226
537.064597	33773.835926	31.128244
537.977397	33806.098985	31.133261
538.462029	33841.780074	31.138279
538.786396	33882.537443	31.143296
539.251362	33921.465997	31.148314
539.837834	33962.180237	31.153332
540.112524	34005.340331	31.158349
540.587307	34062.750690	31.163367
541.269124	34104.753762	31.168384
541.543240	34144.465174	31.173402
541.946328	34201.822800	31.178420
542.352057	34244.682044	31.183437
542.757323	34297.509080	31.188455
543.108054	34360.095069	31.193472
543.357163	34423.498299	31.198490
543.642746	34495.249429	31.203508
544.629321	34543.023649	31.208525
545.037715	34614.590206	31.213543
545.511405	34675.540373	31.218560
546.596430	34732.887374	31.223578
546.665066	34806.657566	31.228596
547.501159	34866.934317	31.233613
547.920072	34926.284559	31.238631
548.484012	34994.407042	31.243648
548.992174	35050.700922	31.248666
549.511538	35121.523644	31.253684
550.705140	35179.312069	31.258701
551.078928	35239.731588	31.263719
551.553304	35302.766483	31.268736
552.084261	35363.451492	31.273754
552.589810	35426.816108	31.278772
553.517235	35480.323600	31.283789
554.100242	35538.123810	31.288807
554.165671	35600.706284	31.293824
554.971737	35652.822664	31.298842
555.161481	35724.070921	31.303860
556.032785	35787.290360	31.308877
556.653829	35846.769328	31.313895
557.514727	35898.595538	31.318912
558.277924	35945.286846	31.323930
558.766234	36006.398766	31.328948
559.247665	36058.790411	31.333965
559.970448	36108.673286	31.338983
560.368455	36164.561204	31.344000
561.357070	36209.443693	31.349018
561.625250	36269.338245	31.354036
562.189750	36321.268151	31.359053
562.833080	36380.382846	31.364071
562.823310	36433.382053	31.369088
563.684143	36487.223421	31.374106
563.929829	36560.206892	31.379124
564.543340	36616.337898	31.384141
565.050622	36670.362292	31.389159
565.325981	36730.511179	31.394176
565.721361	36788.552118	31.399194
566.089392	36854.063028	31.404212
566.931024	36917.264649	31.409229
567.362293	36987.029269	31.414247
567.646628	37044.087597	31.419264
568.914161	37104.395132	31.424282
569.537889	37166.084103	31.429300
570.265172	37209.858341	31.434317
571.019267	37264.901708	31.439335
571.508195	37328.244609	31.444352
572.035349	37372.588795	31.449370
572.447202	37426.090005	31.454388
573.279785	37477.742702	31.459405
574.373354	37519.422309	31.464423
574.964046	37563.260214	31.469440
575.933119	37605.186908	31.474458
576.139261	37647.323508	31.479476
576.599578	37702.159663	31.484493
576.853201	37743.394938	31.489511
577.409215	37801.494193	31.494528
577.971165	37853.074464	31.499546
578.233948	37914.410550	31.504564
578.825135	37971.733761	31.509581
579.602609	38032.203083	31.514599
579.929397	38094.789456	31.519616
580.503352	38151.671374	31.524634
580.776560	38213.900911	31.529652
581.379993	38273.074322	31.534669
582.354021	38343.398276	31.539687
582.505710	38409.988772	31.544704
583.231375	38468.066451	31.549722
583.739894	38543.809134	31.554740
583.943119	38611.390329	31.559757
584.582540	38679.690732	31.564775
585.184027	38744.313997	31.569792
585.807059	38824.481601	31.574810
586.438478	38887.006613	31.579828
587.899222	38937.180848	31.584845
588.637463	39001.581477	31.589863
589.556728	39068.476485	31.594880
589.985318	39122.656857	31.599898
590.174072	39191.177737	31.604916
590.845528	39244.350048	31.609933
591.559075	39302.946573	31.614951
591.433813	39356.723909	31.619968
592.080441	39424.050070	31.624986
592.387240	39494.734202	31.630004
593.043613	39558.423031	31.635021
593.967405	39622.216163	31.640039
594.520955	39694.053964	31.645056
595.462433	39759.486357	31.650074
595.757332	39819.177901	31.655092
596.489269	39891.967395	31.660109
596.922672	39950.631262	31.665127
597.606676	40013.268731	31.670144
598.177675	40076.610396	31.675162
598.658856	40144.446718	31.680180
599.405184	40202.870806	31.685197
599.841619	40252.015144	31.690215
600.439137	40322.148622	31.695232
601.307320	40373.280917	31.700250
601.405110	40434.464700	31.705268
602.090214	40495.473167	31.710285
602.806827	40563.115958	31.715303
603.324204	40624.949555	31.720320
604.101436	40676.135089	31.725338
604.686202	40734.728655	31.730356
605.339523	40796.963861	31.735373
606.164393	40850.750708	31.740391
606.541330	40924.586768	31.745408
607.446017	40984.732498	31.750426
607.562604	41051.428779	31.755444
607.975343	41114.277491	31.760461
608.819405	41179.792343	31.765479
609.329555	41251.996856	31.770496
610.284163	41318.715274	31.775514
610.746900	41385.531205	31.780532
610.881713	41453.039907	31.785549
611.705031	41514.178236	31.790567
612.613124	41581.580072	31.795584
613.259855	41657.571619	31.800602
613.746824	41732.797240	31.805620
614.186266	41790.439753	31.810637
615.014961	41854.587549	31.815655
615.488198	41935.799792	31.820672
616.334377	42004.982671	31.825690
616.857188	42073.501307	31.830708
617.618600	42130.248346	31.835725
618.256212	42196.616907	31.840743
618.672769	42271.039132	31.845760
619.214559	42336.770553	31.850778
619.493137	42410.780060	31.855796
620.321899	42492.799439	31.860813
621.456181	42556.834947	31.865831
621.846356	42640.968888	31.870848
622.373102	42696.764692	31.875866
623.376884	42771.934627	31.880884
623.708179	42848.890118	31.885901
624.800792	42907.514311	31.890919
625.045056	42983.481157	31.895936
625.880124	43031.904380	31.900954
626.562218	43106.950352	31.905972
627.262377	43173.170756	31.910989
627.621767	43239.092377	31.916007
628.116078	43306.992705	31.921024
628.929645	43379.372313	31.926042
629.327770	43445.320095	31.931060
629.846829	43516.520070	31.936077
630.640285	43580.455921	31.941095
630.907442	43661.926750	31.946112
631.884463	43735.726599	31.951130
632.479415	43806.899908	31.956148
633.068646	43866.970287	31.961165
634.326190	43923.022758	31.966183
634.630923	43990.832921	31.971200
635.372366	44038.450518	31.976218
636.279820	44097.814863	31.981236
636.484771	44153.663447	31.986253
637.261510	44210.856523	31.991271
637.830008	44278.272485	31.996288
638.454802	44333.322911	32.001306
638.744002	44392.546957	32.006324
639.556559	44459.767026	32.011341
640.343627	44516.170790	32.016359
640.490072	44587.131633	32.021376
641.260506	44668.747865	32.026394
641.692622	44732.701330	32.031412
642.230144	44800.729957	32.036429
643.169997	44873.502644	32.041447
643.613270	44950.228775	32.046464
644.163241	45023.512149	32.051482
644.762487	45101.252033	32.056500
645.062046	45189.924113	32.061517
646.314668	45252.379638	32.066535
647.192755	45331.019440	32.071552
647.813277	45404.359429	32.076570
649.080649	45470.466716	32.081588
649.667216	45536.550153	32.086605
650.651918	45592.755567	32.091623
650.757974	45661.891055	32.096640
651.368618	45725.501081	32.101658
652.106140	45788.482234	32.106676
652.501352	45862.670837	32.111693
653.379810	45925.983397	32.116711
653.908717	46004.053988	32.121728
654.632570	46071.079848	32.126746
655.251849	46146.978680	32.131764
655.570221	46215.842763	32.136781
656.627669	46280.576252	32.141799
657.054377	46355.897732	32.146816
657.585629	46421.788237	32.151834
658.577521	46493.773777	32.156852
658.784308	46583.373175	32.161869
659.991858	46643.244223	32.166887
660.665924	46727.655565	32.171904
661.425829	46795.132783	32.176922
662.208648	46851.387003	32.181940
662.361410	46922.715976	32.186957
663.299479	46986.679139	32.191975
663.899211	47062.591347	32.196992
664.382226	47136.708243	32.202010
664.871635	47217.213681	32.207028
665.370984	47286.987073	32.212045
666.305439	47363.879032	32.217063
667.122165	47450.404045	32.222080
667.601437	47515.994554	32.227098
668.393934	47581.753147	32.232116
668.714020	47658.586449	32.237133
669.610367	47714.131190	32.242151
669.765267	47793.364145	32.247168
670.420454	47863.812322	32.252186
671.340809	47933.073181	32.257204
671.520570	48022.242439	32.262221
672.194382	48102.192452	32.267239
672.646092	48180.521627	32.272256
673.099538	48262.403819	32.277274
673.966495	48341.510074	32.282292
674.518136	48439.059719	32.287309
675.759674	48511.957216	32.292327
676.273786	48601.470577	32.297344
676.994170	48686.319351	32.302362
678.389132	48772.840806	32.307380
678.602974	48848.721145	32.312397
679.534614	48925.087063	32.317415
680.070191	48997.559371	32.322432
680.570116	49090.049935	32.327450
681.146719	49161.572879	32.332468
681.829438	49253.457727	32.337485
682.899835	49338.477931	32.342503
683.204011	49431.443214	32.347520
683.967996	49516.443630	32.352538
684.886608	49589.737774	32.357556
685.420901	49677.173789	32.362573
686.462308	49748.669266	32.367591
687.043187	49840.339838	32.372608
687.551179	49926.219213	32.377626
688.179552	50011.473945	32.382644
688.633485	50092.092738	32.387661
689.131935	50191.822105	32.392679
689.527581	50269.257396	32.397696
690.319583	50370.607246	32.402714
691.086380	50460.073930	32.407732
691.663238	50569.619958	32.412749
692.687322	50656.313755	32.417767
693.475496	50749.893641	32.422784
694.023202	50844.272856	32.427802
695.177045	50935.337102	32.432820
695.689440	51025.727596	32.437837
696.259476	51103.602637	32.442855
697.243201	51199.567979	32.447872
698.001058	51291.517611	32.452890
698.644839	51377.625329	32.457908
699.162510	51469.939173	32.462925
699.759228	51551.311842	32.467943
700.891590	51643.471905	32.472960
701.406542	51738.684739	32.477978
702.528518	51818.160299	32.482996
703.238116	51918.354820	32.488013
704.075318	51995.260163	32.493031
704.476895	52076.773580	32.498048
704.953802	52164.729510	32.503066
705.939709	52237.708169	32.508084
706.686678	52325.214753	32.513101
706.833693	52397.936262	32.518119
707.674825	52474.489540	32.523136
708.114214	52562.421819	32.528154
708.855741	52636.551955	32.533172
709.424619	52724.316067	32.538189
710.047977	52812.400174	32.543207
711.152164	52904.725823	32.548224
711.044445	53006.618813	32.553242
712.407071	53084.594006	32.558260
713.004934	53174.845944	32.563277
713.713102	53269.265960	32.568295
714.550598	53359.439636	32.573312
715.535075	53443.978491	32.578330
716.667656	53529.226423	32.583348
717.210319	53605.440622	32.588365
718.387831	53675.197239	32.593383
719.533349	53752.013626	32.598400
720.013457	53825.319097	32.603418
721.002311	53896.489081	32.608436
721.306590	53972.146217	32.613453
721.630757	54056.013420	32.618471
722.699446	54129.308481	32.623488
723.458464	54215.414520	32.628506
724.021625	54292.158612	32.633524
724.489503	54384.640441	32.638541
725.340524	54457.526417	32.643559
725.918368	54550.379824	32.648576
726.152013	54644.023961	32.653594
727.222647	54728.656083	32.658612
727.870148	54823.592553	32.663629
728.287593	54911.495498	32.668647
729.248348	55001.840771	32.673664
730.001205	55106.004319	32.678682
730.918856	55188.699542	32.683700
731.590781	55283.770247	32.688717
732.213316	55365.856679	32.693735
733.454524	55446.935881	32.698752
733.916193	55546.410194	32.703770
734.490685	55631.419049	32.708788
735.487517	55725.313393	32.713805
736.156878	55808.846427	32.718823
737.088468	55902.654209	32.723840
737.499300	55995.680430	32.728858
738.042786	56086.255316	32.733876
738.981361	56181.872223	32.738893
740.511520	56259.442908	32.743911
741.216117	56339.730748	32.748928
741.992305	56424.739578	32.753946
742.735999	56497.758098	32.758964
743.642667	56585.487010	32.763981
743.935214	56659.840721	32.768999
744.790631	56733.694738	32.774016
745.395832	56819.881705	32.779034
746.255747	56895.595048	32.784052
746.818994	56976.703700	32.789069
747.097998	57055.506063	32.794087
748.006816	57143.120482	32.799104
748.144006	57237.626618	32.804122
749.088990	57305.713577	32.809140
749.834607	57403.100705	32.814157
750.286300	57497.996923	32.819175
750.952696	57581.200671	32.824192
751.957638	57679.094131	32.829210
752.812088	57765.634145	32.834228
753.333227	57864.814742	32.839245
754.259407	57962.690670	32.844263
754.877714	58047.653178	32.849280
755.654356	58153.140362	32.854298
756.299496	58241.995340	32.859316
757.046995	58348.353320	32.864333
757.697621	58445.609506	32.869351
758.339102	58546.829889	32.874368
758.948531	58656.409811	32.879386
760.164661	58751.149708	32.884404
760.771849	58862.903351	32.889421
761.594885	58963.112049	32.894439
762.746439	59056.755596	32.899456
763.145710	59170.533244	32.904474
764.007478	59277.036205	32.909492
765.277535	59368.092428	32.914509
765.755925	59468.412377	32.919527
766.729458	59563.356048	32.924544
767.261646	59663.832664	32.929562
768.119763	59761.065844	32.934580
768.852924	59866.370739	32.939597
769.402766	59970.429818	32.944615
770.256688	60059.193919	32.949632
770.836723	60172.576315	32.954650
771.857754	60274.803393	32.959668
772.752613	60372.715911	32.964685
773.368439	60485.712450	32.969703
774.299006	60587.074693	32.974720
775.231775	60694.392213	32.979738
775.628046	60790.513867	32.984756
776.861151	60894.431421	32.989773
777.470417	60990.179176	32.994791
778.842104	61077.185853	32.999808
779.687105	61178.331246	33.004826
780.501583	61265.099097	33.009844
781.695880	61350.553311	33.014861
782.582614	61443.562592	33.019879
783.114403	61521.244712	33.024896
783.961057	61611.886645	33.029914
784.866009	61697.735836	33.034932
785.610034	61789.212798	33.039949
785.987462	61884.240992	33.044967
786.832166	61967.969542	33.049984
787.423666	62062.250909	33.055002
787.904295	62147.563398	33.060020
789.020405	62238.980155	33.065037
789.170658	62325.545988	33.070055
790.201275	62406.676447	33.075072
791.185522	62490.015635	33.080090
791.986513	62567.018168	33.085108
792.871858	62656.057930	33.090125
793.573421	62743.883165	33.095143
794.863222	62824.667851	33.100160
795.419502	62911.733835	33.105178
796.071269	62997.682911	33.110196
796.979897	63083.667282	33.115213
797.552281	63181.001491	33.120231
798.306448	63262.182775	33.125248
799.160898	63348.600134	33.130266
799.857029	63440.380067	33.135284
800.521946	63544.187893	33.140301
800.779779	63646.614709	33.145319
801.849294	63748.164431	33.150336
802.154235	63849.144775	33.155354
802.887754	63955.467200	33.160372
804.137472	64060.002694	33.165389
804.675174	64174.047430	33.170407
805.416006	64274.262704	33.175424
806.015617	64389.195775	33.180442
806.861788	64495.667500	33.185460
807.840779	64606.356941	33.190477
808.250560	64734.166579	33.195495
809.473594	64829.090680	33.200512
810.312818	64951.076004	33.205530
810.650993	65069.194042	33.210548
811.867443	65185.887606	33.215565
812.708160	65310.587927	33.220583
813.577663	65419.530850	33.225600
814.304957	65526.728365	33.230618
815.121503	65644.138976	33.235636
815.837697	65766.313292	33.240653
816.391971	65897.417631	33.245671
817.657246	66007.681107	33.250688
818.450947	66125.701544	33.255706
819.311097	66236.501414	33.260724
820.351799	66354.727140	33.265741
821.016457	66479.529379	33.270759
822.141199	66592.986523	33.275776
822.861759	66712.326646	33.280794
823.459567	66822.085099	33.285812
824.641603	66937.272338	33.290829
825.211963	67055.210815	33.295847
826.216318	67160.503433	33.300864
826.835880	67280.652779	33.305882
827.608841	67385.629684	33.310900
828.980453	67503.304384	33.315917
829.983940	67611.815091	33.320935
830.714258	67706.541188	33.325952
831.532512	67813.490530	33.330970
832.384535	67916.941551	33.335988
833.541824	68006.623028	33.341005
833.919220	68116.183813	33.346023
834.895893	68204.726215	33.351040
835.590970	68297.186491	33.356058
836.485602	68402.970805	33.361076
837.633678	68489.339245	33.366093
838.311685	68600.257417	33.371111
839.178344	68690.891724	33.376128
839.855573	68794.956451	33.381146
840.585521	68893.428460	33.386164
841.763107	68996.422744	33.391181
842.896955	69078.424160	33.396199
843.861029	69176.260144	33.401216
844.894722	69268.904891	33.406234
845.358925	69372.659112	33.411252
846.260155	69456.177521	33.416269
847.046667	69563.716436	33.421287
847.869142	69663.201102	33.426304
848.476911	69756.825731	33.431322
849.240402	69856.554530	33.436340
849.873368	69959.059291	33.441357
850.665218	70069.070495	33.446375
851.643409	70175.944128	33.451392
852.446591	70287.376334	33.456410
853.111301	70407.430310	33.461428
853.979008	70513.969541	33.466445
854.002006	70641.835345	33.471463
855.166542	70759.846931	33.476480
856.329057	70880.317393	33.481498
857.123703	70997.302504	33.486516
858.093816	71112.781866	33.491533
858.474803	71245.510358	33.496551
859.892206	71359.953252	33.501568
860.785640	71478.972695	33.506586
861.151287	71604.003698	33.511604
862.157726	71717.736873	33.516621
862.935406	71849.344746	33.521639
863.713396	71972.442119	33.526656
864.404692	72106.175895	33.531674
865.108778	72236.635393	33.536692
866.414368	72365.831036	33.541709
866.875501	72504.709750	33.546727
867.783750	72629.844103	33.551744
869.131916	72753.392682	33.556762
870.032829	72881.000498	33.561780
871.331211	73003.244195	33.566797
872.015999	73125.238736	33.571815
873.135854	73235.676616	33.576832
874.011315	73359.171471	33.581850
874.575518	73486.817783	33.586868
875.577178	73609.200876	33.591885
876.493701	73732.426093	33.596903
877.306564	73850.499359	33.601920
878.400654	73972.187476	33.606938
878.921133	74094.909202	33.611956
879.693881	74205.060100	33.616973
880.434066	74321.833264	33.621991
881.467828	74432.184012	33.627008
881.954243	74550.812586	33.632026
882.509156	74676.496245	33.637044
883.728432	74799.913659	33.642061
884.551291	74931.401916	33.647079
885.136845	75052.166348	33.652096
886.343155	75178.552083	33.657114
887.041448	75315.516597	33.662132
888.366692	75438.826264	33.667149
889.024294	75571.204480	33.672167
890.004526	75700.233236	33.677184
890.940629	75837.928155	33.682202
891.698831	75957.235894	33.687220
893.172132	76069.314209	33.692237
894.088502	76196.074763	33.697255
894.963011	76321.250106	33.702272
896.130083	76437.259723	33.707290
896.676274	76563.259857	33.712308
897.894745	76680.065343	33.717325
898.558154	76809.303254	33.722343
899.573785	76930.642469	33.727360
900.637129	77058.971408	33.732378
901.158045	77191.716915	33.737396
902.232457	77306.393676	33.742413
903.098337	77437.922940	33.747431
903.914249	77558.469695	33.752448
904.795681	77677.603581	33.757466
905.466766	77816.327417	33.762484
906.416971	77948.326910	33.767501
907.525886	78076.446412	33.772519
908.201479	78213.320274	33.777536
909.218389	78335.324980	33.782554
909.855446	78481.055761	33.787572
910.983054	78610.009963	33.792589
912.130665	78740.257565	33.797607
913.448641	78866.326067	33.802624
914.361979	78996.062651	33.807642
915.034794	79118.006660	33.812660
916.114016	79239.210378	33.817677
917.377246	79367.155353	33.822695
919.022828	79473.232607	33.827712
920.741946	79566.403676	33.832730
921.437749	79678.966849	33.837748
922.956252	79752.828046	33.842765
923.993236	79852.657660	33.847783
924.826693	79957.368508	33.852800
926.145108	80024.132191	33.857818
926.864482	80107.843870	33.862836
927.717055	80188.576334	33.867853
928.818247	80284.712512	33.872871
929.583412	80372.779681	33.877888
930.217065	80451.986635	33.882906
930.739084	80547.343837	33.887924
931.720590	80617.355346	33.892941
932.447792	80708.457939	33.897959
932.971540	80802.450606	33.902976
933.681051	80897.450867	33.907994
934.020120	81000.570450	33.913012
934.820149	81103.383304	33.918029
935.564786	81221.370980	33.923047
936.219946	81344.234897	33.928064
937.107944	81453.780667	33.933082
937.591716	81581.736906	33.938100
938.450241	81701.883848	33.943117
939.272935	81834.826141	33.948135
940.082624	81976.950636	33.953152
941.226409	82098.546422	33.958170
942.000628	82241.778363	33.963188
943.029278	82369.968827	33.968205
943.726649	82516.287334	33.973223
944.913381	82660.215140	33.978240
945.948601	82785.922544	33.983258
946.662467	82932.057986	33.988276
947.523322	83076.034168	33.993293
948.602455	83221.354845	33.998311
949.784742	83360.318907	34.003328
950.531941	83501.831443	34.008346
951.385578	83647.494407	34.013364
952.828320	83793.330189	34.018381
953.601024	83943.313605	34.023399
954.084721	84089.462076	34.028416
955.458975	84225.119935	34.033434
956.404162	84377.721794	34.038452
957.578009	84521.537909	34.043469
958.437841	84664.089854	34.048487
959.186438	84821.537705	34.053504
960.113542	84956.974226	34.058522
961.006588	85110.569672	34.063540
961.968182	85267.500086	34.068557
963.012146	85419.221166	34.073575
963.757690	85582.580680	34.078592
964.846180	85720.146168	34.083610
965.870189	85880.453940	34.088628
966.902801	86028.362074	34.093645
968.224994	86174.347207	34.098663
968.835553	86330.993521	34.103680
969.833119	86484.948971	34.108698
970.825664	86644.047100	34.113716
971.756785	86797.085851	34.118733
972.603283	86946.370465	34.123751
973.928986	87103.243779	34.128768
974.957631	87255.410304	34.133786
975.711694	87409.702001	34.138804
976.784055	87563.197993	34.143821
977.768541	87722.204207	34.148839
978.942524	87869.855920	34.153856
980.332394	88018.226809	34.158874
980.939181	88159.002108	34.163892
981.998600	88284.466200	34.168909
983.319711	88421.809629	34.173927
984.234446	88548.392276	34.178944
985.774677	88669.197374	34.183962
986.478847	88811.814301	34.188980
987.311892	88945.703665	34.193997
988.047827	89076.769859	34.199015
988.940883	89208.368358	34.204032
990.018016	89344.902712	34.209050
990.347527	89488.804215	34.214068
991.735277	89630.052952	34.219085
992.781765	89772.153734	34.224103
993.387945	89935.024507	34.229120
994.748905	90058.661136	34.234138
995.477319	90208.012311	34.239156
996.467736	90363.849501	34.244173
997.803057	90509.033334	34.249191
998.616223	90656.432513	34.254208
999.806324	90802.906273	34.259226
1000.667812	90950.862618	34.264244
1001.466157	91095.958675	34.269261
1003.128873	91241.613889	34.274279
1003.613379	91409.188814	34.279296
1005.243579	91544.036140	34.284314
1006.243007	91685.106924	34.289332
1007.027799	91838.400494	34.294349
1008.621836	91978.524730	34.299367
1009.509739	92133.043598	34.304384
1010.457017	92273.228315	34.309402
1011.358865	92412.219419	34.314420
1012.266301	92552.671565	34.319437
1013.637110	92704.473786	34.324455
1014.317916	92859.201441	34.329472
1015.578970	92990.144212	34.334490
1016.438654	93141.632253	34.339508
1017.165512	93291.693999	34.344525
1018.157941	93429.266559	34.349543
1019.225573	93588.656339	34.354560
1020.475862	93734.747796	34.359578
1021.560711	93894.737927	34.364596
1022.246824	94043.356394	34.369613
1023.488810	94193.399195	34.374631
1024.158884	94359.518360	34.379648
1025.260620	94518.150298	34.384666
1026.191399	94671.750129	34.389684
1027.172116	94820.364845	34.394701
1028.582384	94980.829674	34.399719
1029.629366	95138.177957	34.404736
1030.994960	95274.007231	34.409754
1032.227687	95415.899540	34.414772
1033.174296	95566.055443	34.419789
1035.094010	95693.695789	34.424807
1036.107048	95818.868505	34.429824
1037.344359	95950.173981	34.434842
1038.259548	96068.645556	34.439860
1039.165615	96194.128361	34.444877
1040.205610	96311.986720	34.449895
1040.997825	96435.787285	34.454912
1041.813094	96551.942983	34.459930
1042.594366	96676.221057	34.464948
1043.678665	96809.453689	34.469965
1044.702624	96926.868644	34.474983
1045.610509	97079.432046	34.480000
1046.506477	97208.521683	34.485018
1047.929888	97346.315356	34.490036
1048.610216	97492.161258	34.495053
1049.716114	97627.470284	34.500071
1050.315404	97770.876233	34.505088
1051.247884	97910.421574	34.510106
1052.167896	98055.227049	34.515124
1052.740392	98213.829907	34.520141
1054.128402	98365.072892	34.525159
1054.934958	98529.290324	34.530176
1055.979510	98685.714606	34.535194
1057.156757	98843.852363	34.540212
1058.232357	99016.508255	34.545229
1058.985024	99179.334372	34.550247
1059.835032	99356.514387	34.555264
1061.093938	99519.338311	34.560282
1062.491473	99684.197585	34.565300
1063.584957	99865.796942	34.570317
1064.685073	100026.201163	34.575335
1065.882607	100185.357225	34.580352
1066.857377	100348.447310	34.585370
1068.373072	100509.864393	34.590388
1069.195850	100677.561823	34.595405
1070.307981	100836.584091	34.600423
1070.937201	101007.984489	34.605440
1072.416796	101170.848206	34.610458
1073.489110	101333.195724	34.615476
1074.646033	101506.268541	34.620493
1075.922156	101660.607053	34.625511
1076.831984	101841.605674	34.630528
1078.014136	102002.548329	34.635546
1079.030974	102158.487947	34.640564
1079.925953	102331.013742	34.645581
1081.516974	102483.978802	34.650599
1082.806161	102637.239649	34.655616
1084.107349	102790.322411	34.660634
1085.288249	102943.349369	34.665652
1086.168436	103101.772181	34.670669
1087.649072	103253.418310	34.675687
1088.815950	103407.899606	34.680704
1090.450478	103544.734769	34.685722
1091.528390	103685.823079	34.690740
1092.277109	103839.462474	34.695757
1093.640281	103981.272875	34.700775
1094.127093	104129.241547	34.705792
1094.797834	104277.631189	34.710810
1096.082243	104427.803639	34.715828
1096.612845	104576.426269	34.720845
1097.798184	104708.030209	34.725863
1098.789409	104857.758401	34.730880
1099.853562	105014.228295	34.735898
1101.390734	105156.758470	34.740916
1102.141740	105321.918450	34.745933
1103.129230	105462.474803	34.750951
1104.175656	105621.672749	34.755968
1105.002662	105782.735606	34.760986
1106.328560	105941.543167	34.766004
1106.916096	106109.424242	34.771021
1108.447715	106261.745989	34.776039
1109.398413	106438.900104	34.781056
1110.519236	106588.428668	34.786074
1112.211843	106737.576106	34.791092
1113.700175	106901.617109	34.796109
1114.613620	107052.776413	34.801127
1115.781866	107213.649037	34.806144
1117.161933	107365.622148	34.811162
1117.967741	107521.725455	34.816180
1118.777621	107688.417641	34.821197
1120.243572	107848.652219	34.826215
1121.288197	108010.189045	34.831232
1122.042343	108176.994723	34.836250
1123.402076	108336.932962	34.841268
1124.266552	108501.609361	34.846285
1126.086701	108661.900584	34.851303
1126.993167	108825.021813	34.856320
1128.306518	108985.838820	34.861338
1129.538659	109141.922722	34.866356
1130.307764	109309.100886	34.871373
1132.232839	109457.582506	34.876391
1133.528516	109608.038669	34.881408
1134.388941	109766.559259	34.886426
1135.603405	109914.776884	34.891444
1136.497221	110080.427700	34.896461
1137.639559	110233.108485	34.901479
1138.599139	110394.687281	34.906496
1139.721555	110555.867784	34.911514
1140.948838	110710.183773	34.916532
1141.800394	110888.430484	34.921549
1143.275194	111044.987970	34.926567
1144.366411	111215.659987	34.931584
1145.261333	111376.014818	34.936602
1146.679986	111542.009777	34.941620
1147.371327	111711.780303	34.946637
1148.179659	111881.754941	34.951655
1149.608711	112059.348538	34.956672
1150.362423	112230.821844	34.961690
1152.093222	112404.223620	34.966708
1152.651151	112595.620309	34.971725
1153.925003	112770.793825	34.976743
1154.664832	112944.730432	34.981760
1155.846347	113136.361285	34.986778
1156.761889	113302.220089	34.991796
1157.690302	113486.442865	34.996813
1158.867231	113655.282114	35.001831
1159.968382	113834.086310	35.006848
1161.454834	113998.770067	35.011866
1163.575943	114152.560109	35.016884
1164.828098	114314.864859	35.021901
1166.037483	114484.901032	35.026919
1167.417156	114637.723038	35.031936
1168.590354	114789.401257	35.036954
1170.046175	114946.663632	35.041972
1171.112341	115100.437277	35.046989
1172.460426	115246.595161	35.052007
1173.985047	115402.083081	35.057024
1174.932928	115558.879225	35.062042
1176.345100	115706.055201	35.067060
1177.033006	115865.794222	35.072077
1178.458806	116024.011393	35.077095
1179.360296	116182.882725	35.082112
1180.387521	116350.478532	35.087130
1181.503678	116503.746214	35.092148
1182.571290	116674.724974	35.097165
1183.339638	116854.147883	35.102183
1184.511250	117022.738159	35.107200
1185.527170	117198.844434	35.112218
1186.473816	117376.273555	35.117236
1187.432232	117572.500447	35.122253
1188.507858	117763.075060	35.127271
1190.047718	117937.988724	35.132288
1191.780959	118113.512329	35.137306
1193.840709	118287.193332	35.142324
1195.146764	118448.382426	35.147341
1196.727045	118612.454226	35.152359
1198.178472	118766.954783	35.157376
1199.161379	118931.186901	35.162394
1200.447798	119083.106834	35.167412
1201.250836	119259.191353	35.172429
1202.248600	119421.435964	35.177447
1203.343638	119586.528210	35.182464
1203.474605	119771.606926	35.187482
1204.933069	119956.539209	35.192500
1205.700093	120144.406894	35.197517
1206.794330	120333.730975	35.202535
1207.993524	120529.789954	35.207552
1208.892015	120726.455452	35.212570
1210.342968	120924.731663	35.217588
1211.263581	121138.810785	35.222605
1212.255355	121342.545717	35.227623
1213.896402	121537.186801	35.232640
1214.841736	121747.378756	35.237658
1215.856267	121945.858681	35.242676
1217.057139	122155.658622	35.247693
1218.305607	122362.894233	35.252711
1219.826476	122566.541799	35.257728
1221.371162	122761.447844	35.262746
1222.831247	122944.260326	35.267764
1224.215727	123127.415395	35.272781
1224.998224	123308.805539	35.277799
1226.348823	123489.321302	35.282816
1227.645779	123679.739018	35.287834
1229.023042	123851.564058	35.292852
1230.446576	124043.332179	35.297869
1231.547759	124218.762679	35.302887
1233.013705	124397.226939	35.307904
1233.526452	124593.779691	35.312922
1235.238892	124778.793877	35.317940
1236.228418	124961.416258	35.322957
1237.278711	125157.532987	35.327975
1239.112196	125334.323668	35.332992
1240.165649	125524.451132	35.338010
1241.685865	125710.882952	35.343028
1243.638503	125876.131233	35.348045
1245.496048	126039.584231	35.353063
1247.118237	126207.597840	35.358080
1248.322880	126383.608621	35.363098
1249.451368	126545.863158	35.368116
1250.676598	126706.861866	35.373133
1251.802707	126872.754293	35.378151
1252.824289	127039.310392	35.383168
1254.257146	127217.380423	35.388186
1255.358444	127386.142809	35.393204
1256.675518	127557.114146	35.398221
1257.778388	127737.811591	35.403239
1259.048685	127918.838311	35.408256
1259.818617	128089.823926	35.413274
1261.372787	128264.929779	35.418292
1262.573109	128449.568876	35.423309
1263.314589	128633.889426	35.428327
1264.309399	128818.804353	35.433344
1265.546289	129021.367325	35.438362
1266.447475	129228.925912	35.443380
1267.590164	129420.231669	35.448397
1268.881568	129628.440651	35.453415
1270.152571	129831.561522	35.458432
1270.904817	130054.301961	35.463450
1272.470520	130259.355460	35.468468
1273.595802	130471.537220	35.473485
1274.665760	130689.924670	35.478503
1276.189478	130904.010103	35.483520
1276.841153	131125.786811	35.488538
1278.079761	131344.583291	35.493556
1279.424058	131574.070565	35.498573
1280.681362	131801.229614	35.503591
1282.187304	132029.947369	35.508608
1283.455463	132260.579928	35.513626
1284.622164	132479.117857	35.518644
1286.292075	132706.066514	35.523661
1287.883466	132938.971836	35.528679
1288.830898	133161.211566	35.533696
1290.139897	133380.392638	35.538714
1291.190567	133595.941974	35.543732
1292.557912	133813.102452	35.548749
1293.139147	134023.737360	35.553767
1294.845100	134237.882256	35.558784
1296.041980	134454.352427	35.563802
1297.612316	134663.453648	35.568820
1299.138733	134877.010943	35.573837
1300.560063	135088.926581	35.578855
1301.999566	135296.938104	35.583872
1303.510080	135517.902715	35.588890
1304.625866	135723.814602	35.593908
1306.112175	135941.124199	35.598925
1307.192538	136155.395368	35.603943
1308.620666	136354.672763	35.608960
1310.010746	136567.516494	35.613978
1311.506800	136780.725086	35.618996
1312.917055	136992.871737	35.624013
1314.150993	137213.120119	35.629031
1315.884185	137420.618524	35.634048
1317.350349	137617.718812	35.639066
1318.965961	137827.608498	35.644084
1320.303249	138032.398864	35.649101
1321.336344	138238.341513	35.654119
1323.017126	138431.585979	35.659136
1324.216946	138645.906954	35.664154
1325.443710	138854.839215	35.669172
1327.109307	139054.401234	35.674189
1328.522771	139255.132564	35.679207
1330.103593	139449.616134	35.684224
1331.293076	139661.690226	35.689242
1332.257305	139858.416223	35.694260
1334.071969	140063.410799	35.699277
1334.816517	140268.044568	35.704295
1336.318451	140466.602775	35.709312
1337.634037	140677.231870	35.714330
1338.562546	140889.634907	35.719348
1340.466774	141088.944384	35.724365
1341.422511	141307.974434	35.729383
1343.025140	141518.766541	35.734400
1344.337507	141728.795101	35.739418
1345.863673	141929.348871	35.744436
1347.309246	142135.835645	35.749453
1348.411569	142358.436762	35.754471
1350.329309	142567.335580	35.759488
1351.259830	142778.712160	35.764506
1352.538311	142986.156463	35.769524
1354.008563	143188.311690	35.774541
1355.365662	143409.675838	35.779559
1356.386258	143617.634344	35.784576
1357.482740	143831.818264	35.789594
1358.806920	144058.376345	35.794612
1360.252488	144278.160941	35.799629
1361.245579	144502.379280	35.804647
1362.436819	144717.872475	35.809664
1363.660435	144947.102153	35.814682
1365.062332	145167.888648	35.819700
1366.685093	145370.414115	35.824717
1367.534136	145576.169391	35.829735
1369.132996	145787.612342	35.834752
1370.220368	146010.812447	35.839770
1371.289782	146234.511347	35.844788
1372.732173	146458.101855	35.849805
1373.597249	146696.198428	35.854823
1375.084745	146915.513151	35.859840
1376.652099	147156.201602	35.864858
1377.526713	147392.324379	35.869876
1379.210401	147630.221801	35.874893
1379.998869	147878.176349	35.879911
1382.004483	148115.696637	35.884928
1383.329205	148369.210891	35.889946
1385.161069	148592.209391	35.894964
1388.153573	148802.233956	35.899981
1389.830771	149025.323427	35.904999
1391.359505	149235.304541	35.910016
1393.025759	149440.853502	35.915034
1394.212117	149651.804488	35.920052
1395.894862	149852.320562	35.925069
1397.230007	150055.466633	35.930087
1398.896204	150259.981248	35.935104
1400.135000	150469.281132	35.940122
1401.460652	150672.584693	35.945140
1403.018583	150874.610187	35.950157
1404.390184	151077.351142	35.955175
1405.931647	151284.490949	35.960192
1406.830159	151491.594775	35.965210
1407.756294	151708.457630	35.970228
1409.646291	151914.189465	35.975245
1410.925951	152126.409399	35.980263
1412.295681	152349.532415	35.985280
1414.089527	152568.621199	35.990298
1414.773126	152782.486817	35.995316
1416.443709	153002.485544	36.000333
1417.654884	153232.777722	36.005351
1419.062936	153446.456411	36.010368
1420.343972	153671.047756	36.015386
1421.527710	153912.506341	36.020404
1422.694395	154133.809758	36.025421
1424.033193	154381.003334	36.030439
1424.995511	154614.767897	36.035456
1426.739827	154850.742804	36.040474
1427.863195	155100.448334	36.045492
1429.762703	155340.751017	36.050509
1430.801008	155586.936076	36.055527
1431.996041	155833.212127	36.060544
1433.901370	156080.340751	36.065562
1434.736943	156332.776468	36.070580
1436.461984	156580.761542	36.075597
1438.222019	156836.705889	36.080615
1439.691658	157078.712138	36.085632
1441.458591	157318.682060	36.090650
1443.067103	157553.695476	36.095668
1444.463015	157761.976053	36.100685
1446.005285	157987.340517	36.105703
1447.731105	158201.429671	36.110720
1449.212302	158419.261741	36.115738
1450.187031	158633.929394	36.120756
1451.624753	158840.561299	36.125773
1453.292832	159067.003297	36.130791
1455.181625	159283.723484	36.135808
1456.779675	159495.063748	36.140826
1457.994697	159712.083844	36.145844
1459.690738	159927.392984	36.150861
1460.917328	160148.078768	36.155879
1462.031581	160367.325428	36.160896
1463.552572	160599.152139	36.165914
1464.575114	160839.213730	36.170932
1465.960571	161066.208022	36.175949
1467.567903	161296.668632	36.180967
1468.768311	161541.601788	36.185984
1470.592220	161768.048970	36.191002
1471.962124	162019.337394	36.196020
1473.468710	162243.948392	36.201037
1474.594141	162494.340506	36.206055
1476.057827	162739.214617	36.211072
1478.174623	162971.811703	36.216090
1479.001709	163229.535881	36.221108
1480.848398	163477.068130	36.226125
1482.299396	163735.685989	36.231143
1484.036457	163960.905117	36.236160
1485.937987	164198.870907	36.241178
1487.143426	164430.873812	36.246196
1489.170121	164668.391547	36.251213
1490.799030	164911.427646	36.256231
1492.322963	165158.642031	36.261248
1494.142535	165382.246014	36.266266
1495.355723	165625.657240	36.271284
1497.054177	165849.930120	36.276301
1498.428309	166072.886082	36.281319
1499.974144	166309.463379	36.286336
1501.626838	166542.194800	36.291354
1502.841287	166782.569342	36.296372
1504.612088	167014.980528	36.301389
1505.992603	167245.197458	36.306407
1507.257055	167482.676647	36.311424
1509.008264	167716.249485	36.316442
1509.866283	167963.550116	36.321460
1511.652404	168205.885000	36.326477
1513.214752	168448.193554	36.331495
1514.733250	168681.682448	36.336512
1516.049834	168927.432434	36.341530
1517.547691	169174.829525	36.346548
1519.118645	169416.039300	36.351565
1520.477327	169667.774360	36.356583
1521.833231	169917.520027	36.361600
1523.695215	170156.569875	36.366618
1524.750527	170395.723972	36.371636
1526.507470	170616.641528	36.376653
1528.329852	170840.505512	36.381671
1529.809226	171063.245570	36.386688
1531.971305	171275.946097	36.391706
1533.522385	171492.791372	36.396724
1535.228815	171703.930228	36.401741
1536.880363	171923.578019	36.406759
1538.041160	172141.249975	36.411776
1539.863342	172348.872762	36.416794
1541.083391	172568.300915	36.421812
1542.528694	172791.868020	36.426829
1543.987454	173005.653687	36.431847
1545.106010	173251.335442	36.436864
1546.509628	173479.010476	36.441882
1547.313976	173720.317711	36.446900
1549.050448	173969.635329	36.451917
1550.654576	174222.210425	36.456935
1551.726256	174476.152965	36.461952
1553.695837	174724.664371	36.466970
1554.979592	174999.660784	36.471988
1556.474641	175257.663967	36.477005
1557.894080	175519.461319	36.482023
1559.682864	175779.387521	36.487040
1561.485071	176048.269904	36.492058
1562.762660	176312.200804	36.497076
1564.165264	176579.082214	36.502093
1565.465224	176847.757792	36.507111
1566.998329	177126.737841	36.512128
1568.984069	177406.548635	36.517146
1570.345589	177684.747713	36.522164
1571.902715	177966.647572	36.527181
1573.688533	178228.276974	36.532199
1575.559212	178503.926614	36.537216
1577.188563	178773.615283	36.542234
1578.550133	179052.508511	36.547252
1580.387691	179316.826168	36.552269
1582.307809	179593.680359	36.557287
1583.413817	179880.739650	36.562304
1585.356690	180127.549332	36.567322
1587.518463	180404.459203	36.572340
1589.169020	180662.191840	36.577357
1590.947969	180928.393870	36.582375
1592.560099	181193.989631	36.587392
1594.418335	181448.471205	36.592410
1595.994144	181715.002152	36.597428
1597.647662	181977.766657	36.602445
1599.520117	182234.483692	36.607463
1600.703149	182497.871639	36.612480
1602.510986	182751.696311	36.617498
1604.221916	183000.462409	36.622516
1605.738789	183255.617733	36.627533
1607.309642	183504.979900	36.632551
1609.114084	183756.628412	36.637568
1610.943113	183992.235736	36.642586
1612.350300	184248.695740	36.647604
1613.581304	184479.451928	36.652621
1615.440231	184709.716212	36.657639
1616.799628	184956.468032	36.662656
1618.235067	185195.760570	36.667674
1619.387259	185433.931944	36.672692
1620.656051	185681.032016	36.677709
1622.215387	185926.348837	36.682727
1623.599148	186191.731511	36.687744
1625.308917	186457.038567	36.692762
1627.020475	186717.803990	36.697780
1628.551545	186987.393499	36.702797
1630.351731	187255.317550	36.707815
1631.790247	187533.795072	36.712832
1633.410434	187797.372843	36.717850
1635.174531	188065.903716	36.722868
1636.948151	188334.371166	36.727885
1638.501580	188606.402971	36.732903
1639.802223	188881.547517	36.737920
1641.706172	189162.549587	36.742938
1643.128799	189450.990157	36.747956
1644.661106	189724.630719	36.752973
1646.964834	189995.485340	36.757991
1648.660052	190270.892514	36.763008
1650.751024	190536.580849	36.768026
1652.566404	190815.626959	36.773044
1654.013430	191078.514365	36.778061
1655.711589	191353.978012	36.783079
1657.562225	191616.474270	36.788096
1659.184860	191876.254204	36.793114
1660.694415	192164.126076	36.798132
1661.804775	192445.768224	36.803149
1664.262232	192708.453165	36.808167
1665.278723	193006.535821	36.813184
1667.040516	193284.259218	36.818202
1668.905647	193561.815457	36.823220
1670.191780	193845.138270	36.828237
1672.125203	194137.040919	36.833255
1673.443141	194432.660109	36.838272
1675.242343	194707.466363	36.843290
1677.008932	195002.446508	36.848308
1678.406472	195294.669373	36.853325
1680.143532	195583.997006	36.858343
1681.507522	195884.744840	36.863360
1683.735840	196177.462720	36.868378
1686.131381	196451.764806	36.873396
1687.898266	196730.343900	36.878413
1690.300855	197000.319727	36.883431
1691.972707	197277.177994	36.888448
1694.159320	197530.563904	36.893466
1695.815245	197802.972444	36.898484
1697.216833	198078.189744	36.903501
1698.776342	198347.202108	36.908519
1700.015622	198612.915819	36.913536
1701.225554	198893.206750	36.918554
1702.695626	199155.738720	36.923572
1704.403989	199414.933997	36.928589
1706.113320	199684.538546	36.933607
1707.195875	199961.631265	36.938624
1708.993261	200230.615287	36.943642
1710.545339	200504.894526	36.948660
1711.453155	200793.176444	36.953677
1713.065830	201071.663026	36.958695
1714.782077	201368.996801	36.963712
1716.239675	201667.515642	36.968730
1717.991354	201979.787152	36.973748
1719.934700	202276.531211	36.978765
1721.708827	202572.948290	36.983783
1723.348473	202885.572667	36.988800
1725.784672	203162.402997	36.993818
1727.935877	203453.535024	36.998836
1730.121584	203738.570025	37.003853
1732.783422	204016.523826	37.008871
1734.543686	204288.110121	37.013888
1736.361949	204564.728009	37.018906
1738.451487	204831.148896	37.023924
1740.391972	205104.677993	37.028941
1742.666547	205348.273225	37.033959
1744.250565	205617.215248	37.038976
1746.047444	205861.002702	37.043994
1748.188952	206121.861121	37.049012
1749.672929	206384.157995	37.054029
1751.621265	206641.076021	37.059047
1753.054012	206905.630244	37.064064
1754.537606	207158.003474	37.069082
1756.073043	207425.361880	37.074100
1757.624185	207697.631819	37.079117
1759.433813	207965.418787	37.084135
1760.906711	208247.211970	37.089152
1762.464830	208522.721666	37.094170
1763.987810	208805.372717	37.099188
1765.636957	209094.517554	37.104205
1767.206724	209379.283864	37.109223
1768.876464	209679.066590	37.114240
1770.551244	209969.379376	37.119258
1772.772107	210261.536484	37.124276
1774.275118	210555.941714	37.129293
1775.933785	210855.198608	37.134311
1777.236663	211159.236074	37.139328
1779.274255	211457.420010	37.144346
1781.200071	211756.042027	37.149364
1782.490205	212070.127973	37.154381
1784.569769	212360.971389	37.159399
1786.440370	212672.924107	37.164416
1788.104986	212980.264369	37.169434
1790.869178	213272.145774	37.174452
1792.588230	213576.915628	37.179469
1794.375539	213870.592513	37.184487
1796.360726	214173.164545	37.189504
1797.904246	214459.658711	37.194522
1800.243408	214727.986671	37.199540
1801.616589	215012.605813	37.204557
1803.427083	215276.969803	37.209575
1804.995452	215549.029077	37.214592
1806.635982	215829.025844	37.219610
1808.755586	216094.753207	37.224628
1810.236453	216372.898467	37.229645
1812.109896	216652.468005	37.234663
1813.914867	216933.547715	37.239680
1815.078963	217223.998747	37.244698
1817.008762	217514.342125	37.249716
1818.367982	217817.296145	37.254733
1820.415945	218108.930947	37.259751
1822.121318	218420.110816	37.264768
1823.526924	218732.710863	37.269786
1825.329638	219045.541252	37.274804
1827.166762	219364.906429	37.279821
1829.181052	219670.989247	37.284839
1830.929787	219992.136056	37.289856
1832.517747	220316.153919	37.294874
1834.420875	220641.723000	37.299892
1836.361680	220974.499513	37.304909
1838.381213	221309.677472	37.309927
1840.018911	221675.137081	37.314944
1841.808694	222011.687808	37.319962
1843.753862	222334.921156	37.324980
1845.217330	222678.154627	37.329997
1847.283175	223001.409684	37.335015
1849.235795	223340.936934	37.340032
1851.063495	223680.764819	37.345050
1853.702733	224004.415485	37.350068
1855.243036	224348.088433	37.355085
1857.316153	224677.431367	37.360103
1859.676578	225008.850577	37.365120
1861.335518	225338.846026	37.370138
1863.294579	225662.103355	37.375156
1865.377703	225988.973880	37.380173
1867.412480	226298.685622	37.385191
1869.617183	226626.758360	37.390208
1871.607090	226946.536492	37.395226
1874.020299	227252.686995	37.400244
1875.782820	227565.189391	37.405261
1878.005305	227865.302604	37.410279
1880.311877	228165.987636	37.415296
1882.242303	228472.574647	37.420314
1883.989797	228776.829859	37.425332
1885.419464	229079.079414	37.430349
1887.747827	229379.409581	37.435367
1889.648484	229675.745109	37.440384
1891.246023	229987.088630	37.445402
1893.080147	230278.230281	37.450420
1894.695044	230591.427112	37.455437
1896.722744	230890.768717	37.460455
1898.878767	231192.935442	37.465472
1900.501535	231493.079779	37.470490
1902.117185	231783.448117	37.475508
1903.782734	232065.021824	37.480525
1905.561867	232349.905448	37.485543
1907.337160	232635.654058	37.490560
1908.808559	232940.017630	37.495578
1911.189627	233230.446676	37.500596
1912.697530	233531.377572	37.505613
1914.591625	233825.771570	37.510631
1916.580719	234126.069157	37.515648
1918.576904	234433.147873	37.520666
1920.882955	234731.415909	37.525684
1922.406308	235040.958957	37.530701
1924.528250	235336.159369	37.535719
1926.590600	235646.177480	37.540736
1928.220837	235963.046540	37.545754
1930.001635	236267.802853	37.550772
1931.696330	236581.336312	37.555789
1933.394655	236893.777966	37.560807
1935.960630	237218.756947	37.565824
1937.532801	237542.650053	37.570842
1939.687698	237861.981403	37.575860
1941.736087	238193.547606	37.580877
1943.422838	238510.008808	37.585895
1945.518991	238838.597636	37.590912
1947.537851	239166.361504	37.595930
1949.509132	239484.482050	37.600948
1951.014971	239821.752419	37.605965
1953.178348	240157.319253	37.610983
1955.193211	240491.335830	37.616000
1957.048585	240831.677809	37.621018
1959.273708	241162.513334	37.626036
1961.349209	241491.595513	37.631053
1963.550684	241827.160995	37.636071
1965.648050	242163.810714	37.641088
1967.405081	242502.928361	37.646106
1969.461351	242828.892932	37.651124
1971.684292	243159.632547	37.656141
1973.962482	243492.269276	37.661159
1976.266709	243811.745317	37.666176
1978.486828	244131.337085	37.671194
1980.968735	244449.618064	37.676212
1982.596912	244771.997751	37.681229
1984.558573	245094.325295	37.686247
1986.736546	245406.814605	37.691264
1988.039280	245729.070382	37.696282
1990.314773	246041.901262	37.701300
1992.466024	246363.185641	37.706317
1994.396093	246684.912253	37.711335
1996.372730	247001.704401	37.716352
1998.087828	247327.606907	37.721370
2000.454559	247646.751657	37.726388
2002.566853	247969.874638	37.731405
2004.760057	248287.879830	37.736423
2006.850601	248593.480755	37.741440
2008.572736	248900.207590	37.746458
2010.419777	249202.596977	37.751476
2012.490777	249492.987348	37.756493
2014.195641	249792.276040	37.761511
2016.437048	250086.907892	37.766528
2018.310828	250384.570579	37.771546
2020.159720	250671.264263	37.776564
2022.050895	250977.637993	37.781581
2023.893713	251289.862334	37.786599
2026.100639	251589.531828	37.791616
2027.896685	251899.630943	37.796634
2029.838945	252204.373025	37.801652
2031.994140	252517.616868	37.806669
2033.581706	252825.134268	37.811687
2035.546684	253149.941833	37.816704
2037.512169	253482.776909	37.821722
2039.466800	253800.246063	37.826740
2041.326172	254137.773087	37.831757
2043.343400	254481.067333	37.836775
2045.539813	254815.315978	37.841792
2047.218810	255164.507545	37.846810
2049.313533	255501.745504	37.851828
2051.730961	255838.043733	37.856845
2053.586729	256192.568853	37.861863
2055.896489	256544.050455	37.866880
2057.532089	256887.993436	37.871898
2059.833471	257244.786572	37.876916
2061.776703	257600.697184	37.881933
2063.822998	257949.834916	37.886951
2066.375707	258305.294268	37.891968
2068.186531	258661.405276	37.896986
2070.367406	259017.381883	37.902004
2072.833992	259377.936949	37.907021
2074.184093	259746.138010	37.912039
2076.600177	260092.095508	37.917056
2078.799182	260462.703157	37.922074
2080.919454	260816.430923	37.927092
2082.990328	261168.820609	37.932109
2084.994862	261531.788827	37.937127
2087.579510	261876.400784	37.942144
2089.292509	262243.734577	37.947162
2091.516933	262613.680380	37.952180
2094.155702	262965.245332	37.957197
2096.277522	263327.663518	37.962215
2098.657325	263676.755376	37.967232
2101.647993	264004.132688	37.972250
2104.295018	264344.139316	37.977268
2106.319191	264679.139018	37.982285
2108.313542	265011.247779	37.987303
2110.212790	265338.113446	37.992320
2112.320181	265680.315258	37.997338
2113.934954	266015.126938	38.002356
2116.256510	266349.852165	38.007373
2118.511305	266682.657575	38.012391
2120.401142	267019.026740	38.017408
2122.385516	267364.729524	38.022426
2124.214606	267677.585348	38.027444
2126.489167	268001.294099	38.032461
2128.126439	268321.064985	38.037479
2130.209845	268625.066043	38.042496
2132.283969	268945.682480	38.047514
2134.141242	269280.457706	38.052532
2136.215843	269599.829606	38.057549
2138.113942	269944.734586	38.062567
2140.121045	270270.823946	38.067584
2142.150529	270614.946264	38.072602
2143.796007	270973.253884	38.077620
2145.971121	271325.025172	38.082637
2148.061316	271687.352444	38.087655
2150.274705	272045.646547	38.092672
2152.089453	272407.763668	38.097690
2154.074799	272772.800610	38.102708
2156.737287	273141.108887	38.107725
2158.743946	273512.112383	38.112743
2160.985921	273874.289028	38.117760
2163.314411	274258.019487	38.122778
2165.439862	274629.918778	38.127796
2168.132048	274993.624513	38.132813
2170.034499	275371.478175	38.137831
2172.558391	275740.189656	38.142848
2175.006779	276108.938490	38.147866
2176.829704	276483.629258	38.152884
2179.316582	276851.101730	38.157901
2181.295743	277227.444231	38.162919
2183.690088	277593.915103	38.167936
2186.392844	277970.981001	38.172954
2188.625126	278342.989921	38.177972
2190.586822	278712.882349	38.182989
2192.619547	279082.153707	38.188007
2195.560235	279450.518845	38.193024
2197.925740	279819.203677	38.198042
2200.178139	280184.197397	38.203060
2202.699245	280546.811232	38.208077
2204.512447	280909.359320	38.213095
2206.728351	281269.785692	38.218112
2208.957242	281638.745306	38.223130
2211.051385	282004.880899	38.228148
2213.626340	282359.432351	38.233165
2215.437868	282742.911890	38.238183
2217.962981	283108.063897	38.243200
2219.913399	283471.376125	38.248218
2221.970425	283854.002984	38.253236
2223.998782	284221.315974	38.258253
2225.820239	284602.506168	38.263271
2228.298848	284980.264012	38.268288
2230.660428	285371.503694	38.273306
2232.446530	285753.866957	38.278324
2235.197310	286134.247857	38.283341
2237.154484	286521.536796	38.288359
2239.827118	286900.354291	38.293376
2242.169019	287261.060704	38.298394
2243.903584	287625.419432	38.303412
2246.181009	287968.810501	38.308429
2248.847833	288312.926943	38.313447
2251.418220	288649.945497	38.318464
2254.267893	288978.739689	38.323482
2256.224692	289314.508423	38.328500
2259.051478	289629.333977	38.333517
2260.987210	289971.481357	38.338535
2263.391626	290297.524906	38.343552
2265.576376	290635.440519	38.348570
2267.463129	290980.617283	38.353588
2269.864185	291310.064049	38.358605
2271.915077	291665.730520	38.363623
2273.728448	292014.600858	38.368640
2276.032850	292368.016086	38.373658
2278.172393	292727.832930	38.378676
2280.557621	293084.079327	38.383693
2282.285813	293455.188094	38.388711
2284.806465	293822.919104	38.393728
2286.564829	294192.218272	38.398746
2288.830627	294573.197576	38.403764
2291.370079	294948.950756	38.408781
2293.138511	295336.942291	38.413799
2295.461671	295727.588555	38.418816
2297.769911	296120.878218	38.423834
2299.922078	296527.248433	38.428852
2302.660802	296918.156631	38.433869
2304.743632	297325.806204	38.438887
2306.885550	297728.492148	38.443904
2309.379358	298117.633078	38.448922
2311.454598	298533.206454	38.453940
2314.310893	298935.420768	38.458957
2316.878807	299347.103828	38.463975
2319.165781	299736.299283	38.468992
2321.341167	300142.505071	38.474010
2323.402092	300552.538192	38.479028
2326.143242	300968.736550	38.484045
2328.106649	301385.158700	38.489063
2330.337005	301799.733927	38.494080
2332.961328	302212.238885	38.499098
2335.002530	302628.670700	38.504116
2337.160412	303046.810108	38.509133
2339.602623	303479.381744	38.514151
2341.906104	303895.565144	38.519168
2343.736739	304323.836816	38.524186
2346.191345	304750.357217	38.529204
2349.391874	305168.858473	38.534221
2352.155896	305578.842260	38.539239
2354.811606	305995.852470	38.544256
2358.094187	306401.204841	38.549274
2360.246185	306807.598764	38.554292
2363.433311	307196.225001	38.559309
2365.660885	307599.099196	38.564327
2368.489156	307971.777860	38.569344
2370.778437	308343.296236	38.574362
2373.211860	308697.518728	38.579380
2375.716047	309039.791063	38.584397
2377.716334	309390.930593	38.589415
2379.728386	309746.842352	38.594432
2382.131100	310093.369470	38.599450
2383.870781	310456.840508	38.604468
2385.770961	310813.300120	38.609485
2387.676145	311196.046126	38.614503
2389.860844	311586.264704	38.619520
2392.084365	311967.205073	38.624538
2393.958011	312367.198075	38.629556
2396.588803	312764.453514	38.634573
2398.832748	313159.736894	38.639591
2400.491776	313582.516792	38.644608
2403.337804	313996.522118	38.649626
2405.626114	314416.862246	38.654644
2407.736934	314840.581393	38.659661
2410.283825	315277.081240	38.664679
2412.197873	315705.882242	38.669696
2414.862880	316140.226174	38.674714
2416.956888	316582.151114	38.679732
2419.725799	317022.113053	38.684749
2422.282634	317472.748280	38.689767
2424.326466	317925.113543	38.694784
2426.957199	318373.574005	38.699802
2429.394390	318837.809402	38.704820
2432.170327	319290.737796	38.709837
2434.669579	319741.930009	38.714855
2437.358328	320198.067777	38.719872
2440.100450	320632.328036	38.724890
2442.373000	321093.276436	38.729908
2445.005221	321546.343265	38.734925
2447.951703	321991.434234	38.739943
2450.293911	322441.063048	38.744960
2453.191372	322885.420681	38.749978
2455.581482	323329.678623	38.754996
2458.375216	323767.826015	38.760013
2461.050578	324201.799552	38.765031
2463.351637	324647.105834	38.770048
2466.214755	325073.146963	38.775066
2468.447958	325529.912601	38.780084
2470.737898	325953.424199	38.785101
2473.813550	326385.494201	38.790119
2476.434371	326819.259206	38.795136
2479.285652	327247.398423	38.800154
2481.744064	327673.565963	38.805172
2484.874611	328091.193636	38.810189
2487.719287	328499.544559	38.815207
2490.279158	328903.875327	38.820224
2493.551889	329297.577771	38.825242
2495.707659	329695.035703	38.830260
2498.198033	330095.841286	38.835277
2500.895365	330488.435097	38.840295
2502.965184	330892.197882	38.845312
2505.319176	331274.811376	38.850330
2507.263878	331658.249504	38.855348
2509.571992	332026.493616	38.860365
2511.831215	332405.561055	38.865383
2513.910703	332790.571518	38.870400
2516.429008	333168.425742	38.875418
2518.296904	333564.435209	38.880436
2520.492340	333952.620398	38.885453
2522.681274	334357.614226	38.890471
2525.198014	334785.762267	38.895488
2527.202313	335202.283047	38.900506
2529.541189	335624.182132	38.905524
2531.811416	336055.484409	38.910541
2534.163609	336502.488329	38.915559
2536.146267	336957.673046	38.920576
2539.109529	337401.958740	38.925594
2541.629016	337870.357090	38.930612
2543.742191	338329.269448	38.935629
2546.344806	338785.993558	38.940647
2548.733774	339268.011843	38.945664
2551.504588	339739.708267	38.950682
2553.736237	340225.705063	38.955700
2556.492990	340710.726238	38.960717
2559.282748	341190.990507	38.965735
2561.429133	341680.340860	38.970752
2564.164488	342166.064866	38.975770
2566.879467	342669.586002	38.980788
2569.400118	343166.583369	38.985805
2572.327466	343657.723547	38.990823
2574.719224	344160.140840	38.995840
2577.806900	344644.392527	39.000858
2580.482055	345145.994840	39.005876
2583.634743	345639.850037	39.010893
2586.362785	346112.950407	39.015911
2588.766371	346610.419432	39.020928
2591.927845	347097.558389	39.025946
2594.691344	347581.202012	39.030964
2596.831903	348070.322146	39.035981
2599.680291	348554.121617	39.040999
2602.013454	349048.914600	39.046016
2605.038909	349538.770110	39.051034
2607.663712	350018.454189	39.056052
2610.323454	350514.299153	39.061069
2612.938494	351002.048694	39.066087
2615.194316	351500.233236	39.071104
2618.071985	351985.495221	39.076122
2620.718504	352481.019406	39.081140
2623.165395	352981.063592	39.086157
2626.248676	353467.548550	39.091175
2629.002297	353959.817946	39.096192
2631.395197	354450.312154	39.101210
2634.069547	354943.016218	39.106228
2636.627859	355430.276500	39.111245
2639.761777	355910.206761	39.116263
2642.188185	356410.499958	39.121280
2644.757119	356879.418174	39.126298
2647.135440	357349.808951	39.131316
2649.678868	357807.325790	39.136333
2652.604632	358253.584436	39.141351
2654.822841	358713.885566	39.146368
2657.389177	359170.827628	39.151386
2659.825225	359632.583037	39.156404
2662.480871	360099.350022	39.161421
2665.292183	360558.803566	39.166439
2667.664227	361049.362412	39.171456
2670.409754	361516.405824	39.176474
2673.209605	361987.852089	39.181492
2675.670644	362483.153303	39.186509
2678.345104	362963.365522	39.191527
2680.578132	363457.804172	39.196544
2683.149707	363951.574803	39.201562
2685.654252	364452.202914	39.206580
2688.182342	364964.318111	39.211597
2691.392113	365466.904349	39.216615
2694.055569	365971.221040	39.221632
2697.164863	366463.051921	39.226650
2699.846094	366973.901821	39.231668
2702.529770	367485.532117	39.236685
2705.388210	367989.236709	39.241703
2708.258479	368499.607564	39.246720
2711.028910	369005.014576	39.251738
2713.572503	369527.097988	39.256756
2716.570796	370034.030155	39.261773
2719.275716	370546.686774	39.266791
2721.736719	371066.709126	39.271808
2724.627422	371582.495655	39.276826
2727.450960	372112.242223	39.281844
2729.793419	372637.567133	39.286861
2732.894418	373161.547379	39.291879
2735.717661	373684.499318	39.296896
2738.665099	374196.463932	39.301914
2741.633883	374723.921329	39.306932
2744.494196	375242.508851	39.311949
2747.552379	375750.909704	39.316967
2750.402553	376280.674488	39.321984
2753.158579	376789.896588	39.327002
2756.108466	377310.092429	39.332020
2758.546550	377833.330852	39.337037
2761.321388	378354.530163	39.342055
2763.991294	378874.648287	39.347072
2766.601845	379394.971859	39.352090
2769.127771	379921.745637	39.357108
2771.717219	380459.765930	39.362125
2774.555201	380981.858744	39.367143
2777.039547	381522.265454	39.372160
2780.427175	382048.467788	39.377178
2783.355656	382580.113411	39.382196
2785.857964	383120.596015	39.387213
2788.795385	383648.318649	39.392231
2791.452712	384182.140730	39.397248
2794.062778	384694.680649	39.402266
2796.948940	385217.442819	39.407284
2799.680557	385716.251934	39.412301
2802.407856	386207.876700	39.417319
2804.763742	386710.079941	39.422336
2807.281877	387221.609944	39.427354
2810.248841	387721.064582	39.432372
2812.637662	388247.742735	39.437389
2815.391352	388764.539886	39.442407
2818.102966	389296.173409	39.447424
2820.763604	389832.245463	39.452442
2823.399392	390362.074300	39.457460
2826.027931	390908.000904	39.462477
2829.032080	391442.294859	39.467495
2831.696456	392005.748580	39.472512
2834.344546	392559.406651	39.477530
2837.695943	393108.329006	39.482548
2840.476475	393667.020320	39.487565
2843.346301	394219.348608	39.492583
2846.310015	394778.474576	39.497600
2849.297596	395338.627241	39.502618
2852.349773	395902.209060	39.507636
2854.931563	396471.535959	39.512653
2858.069536	397029.785543	39.517671
2860.588693	397609.347179	39.522688
2863.886819	398180.357136	39.527706
2867.156571	398740.433399	39.532724
2869.741955	399318.002148	39.537741
2872.660892	399893.149895	39.542759
2876.068040	400459.133331	39.547776
2879.133988	401014.182641	39.552794
2882.326273	401573.436427	39.557812
2885.041856	402152.886233	39.562829
2888.333029	402710.279094	39.567847
2891.232096	403280.374965	39.572864
2893.928566	403846.968761	39.577882
2897.117130	404407.415540	39.582900
2899.665055	404984.254255	39.587917
2902.492279	405554.218887	39.592935
2905.363057	406136.258045	39.597952
2907.956001	406704.261359	39.602970
2910.776606	407292.725412	39.607988
2913.797984	407877.648330	39.613005
2916.666542	408462.204023	39.618023
2919.406248	409045.907069	39.623040
2922.178596	409639.985936	39.628058
2925.196315	410229.629335	39.633076
2927.650577	410830.451845	39.638093
2931.212077	411425.865878	39.643111
2934.276615	412019.749925	39.648128
2937.307607	412608.609190	39.653146
2940.528490	413190.989299	39.658164
2942.995843	413799.504765	39.663181
2946.257868	414380.156728	39.668199
2949.239544	414975.007853	39.673216
2951.606510	415561.682631	39.678234
2955.010705	416129.175344	39.683252
2957.686868	416682.175762	39.688269
2960.469671	417230.942128	39.693287
2963.264195	417799.157092	39.698304
2966.269185	418363.095715	39.703322
2969.280566	418927.528867	39.708340
2971.613176	419500.191742	39.713357
2974.596162	420070.104880	39.718375
2977.284720	420652.797651	39.723392
2979.915943	421239.414503	39.728410
2983.126041	421822.861660	39.733428
2985.829628	422425.226385	39.738445
2988.876405	423033.654707	39.743463
2992.250084	423636.368186	39.748480
2994.987587	424236.103614	39.753498
2998.138474	424838.141733	39.758516
3001.103277	425459.246204	39.763533
3004.198149	426074.666688	39.768551
3007.248536	426690.282756	39.773568
3010.217510	427316.105955	39.778586
3013.924027	427916.923187	39.783604
3016.910147	428530.860380	39.788621
3019.613401	429161.950681	39.793639
3022.736006	429784.525022	39.798656
3025.859422	430401.588235	39.803674
3029.073427	431024.371861	39.808692
3031.844051	431653.871690	39.813709
3034.918195	432276.090189	39.818727
3038.270871	432907.518784	39.823744
3040.950600	433544.153983	39.828762
3044.243871	434176.472396	39.833780
3047.347182	434817.288624	39.838797
3050.366551	435460.786189	39.843815
3054.273977	436082.552082	39.848832
3057.721782	436695.284772	39.853850
3061.753054	437308.517867	39.858868
3064.310840	437933.059467	39.863885
3067.822089	438533.810962	39.868903
3071.347767	439149.990429	39.873920
3074.212938	439759.220398	39.878938
3077.255401	440360.558599	39.883956
3080.330883	440960.459031	39.888973
3083.598084	441571.555078	39.893991
3086.522947	442170.740657	39.899008
3089.772113	442787.378513	39.904026
3092.765512	443388.092646	39.909044
3095.270742	444007.652243	39.914061
3098.152966	444618.985171	39.919079
3101.815956	445224.255669	39.924096
3104.837344	445844.090947	39.929114
3107.779049	446459.467755	39.934132
3110.798459	447070.563972	39.939149
3113.435858	447696.992226	39.944167
3116.407797	448329.222666	39.949184
3119.243793	448947.132585	39.954202
3122.081382	449543.210027	39.959220
3124.923219	450151.216717	39.964237
3127.688940	450749.957064	39.969255
3130.771162	451350.403220	39.974272
3133.409053	451959.760957	39.979290
3136.498984	452579.608454	39.984308
3139.449687	453204.572588	39.989325
3142.061024	453833.672391	39.994343
3145.042660	454480.003325	39.999360
3147.798468	455124.074248	40.004378
3151.376387	455766.630371	40.009396
3154.285871	456440.747875	40.014413
3157.174511	457104.981309	40.019431
3160.539552	457774.432347	40.024448
3163.146047	458462.602744	40.029466
3166.500925	459130.698751	40.034484
3169.700126	459824.399460	40.039501
3172.259139	460523.086863	40.044519
3175.610929	461227.747906	40.049536
3178.587552	461951.618546	40.054554
3181.796416	462654.485179	40.059572
3185.153086	463383.660481	40.064589
3187.733682	464109.392897	40.069607
3191.564852	464836.268576	40.074624
3194.272102	465593.999351	40.079642
3197.583439	466332.539469	40.084660
3201.361768	467074.419098	40.089677
3204.385043	467823.118424	40.094695
3207.608868	468561.088378	40.099712
3210.715062	469318.621880	40.104730
3214.489099	470077.084101	40.109748
3217.542945	470820.310496	40.114765
3220.893102	471570.340168	40.119783
3224.761391	472320.715581	40.124800
3228.400347	473066.448042	40.129818
3231.552626	473816.123313	40.134836
3234.577134	474559.724126	40.139853
3237.962874	475300.055423	40.144871
3241.424134	476048.385740	40.149888
3244.646790	476802.893310	40.154906
3248.076124	477543.792139	40.159924
3251.448067	478298.674509	40.164941
3254.811221	479053.782289	40.169959
3258.199151	479789.144777	40.174976
3261.162869	480561.594951	40.179994
3264.189461	481302.568246	40.185012
3267.755264	482051.261757	40.190029
3270.653367	482814.435176	40.195047
3273.953344	483558.918077	40.200064
3277.529303	484319.145577	40.205082
3280.599096	485086.093234	40.210100
3283.998959	485841.690031	40.215117
3286.962317	486598.033373	40.220135
3291.041875	487353.715454	40.225152
3294.192618	488098.803389	40.230170
3297.206605	488821.704757	40.235188
3300.418873	489528.683957	40.240205
3303.681216	490228.657209	40.245223
3307.308951	490935.113537	40.250240
3309.949575	491649.730872	40.255258
3313.392446	492359.092206	40.260276
3316.406019	493077.687048	40.265293
3319.618671	493815.768965	40.270311
3322.530066	494536.797972	40.275328
3325.486882	495278.043465	40.280346
3328.669341	496032.606167	40.285364
3332.292404	496785.754956	40.290381
3335.227920	497543.879455	40.295399
3338.626613	498306.140555	40.300416
3341.593252	499079.798691	40.305434
3345.163217	499845.552502	40.310452
3348.794636	500624.643366	40.315469
3351.793540	501409.101286	40.320487
3355.528291	502173.870790	40.325504
3359.131560	502951.299080	40.330522
3362.274158	503746.181523	40.335540
3365.684823	504535.635026	40.340557
3369.279455	505336.077971	40.345575
3372.969934	506108.809835	40.350592
3375.891896	506903.533204	40.355610
3379.744930	507703.473073	40.360628
3383.326354	508498.069429	40.365645
3386.116611	509305.975691	40.370663
3389.910240	510106.822537	40.375680
3393.907812	510892.260068	40.380698
3397.771474	511690.851749	40.385716
3401.438608	512471.878812	40.390733
3404.980773	513270.144158	40.395751
3408.324712	514043.279124	40.400768
3411.429886	514858.993768	40.405786
3414.878377	515650.703573	40.410804
3418.085594	516445.238731	40.415821
3421.356059	517245.375213	40.420839
3425.196987	518041.247010	40.425856
3428.744223	518844.893889	40.430874
3432.157365	519641.058694	40.435892
3435.678276	520441.353534	40.440909
3438.978238	521252.133093	40.445927
3442.737758	522047.218276	40.450944
3446.301563	522852.430440	40.455962
3449.478780	523652.369527	40.460980
3452.893538	524452.987668	40.465997
3456.211006	525276.167326	40.471015
3459.424886	526084.096470	40.476032
3462.971471	526899.745712	40.481050
3466.142974	527718.184850	40.486068
3469.703015	528525.431286	40.491085
3472.639742	529353.248745	40.496103
3476.444844	530181.893460	40.501120
3479.753987	530999.847056	40.506125
3482.916411	531770.201066	40.511130
3486.257092	532483.299160	40.516135
3489.387117	533150.122646	40.521140
3492.521135	533752.457401	40.526144
3494.970628	534301.583547	40.531149
3497.517567	534788.290694	40.536154
3500.336251	535224.528537	40.541159
3502.214873	535598.319747	40.546164
3504.643154	535909.534445	40.551168
3506.220020	536190.117489	40.556173
3507.974139	536407.936328	40.561178
3510.168033	536574.568907	40.566183
3511.257708	536715.868078	40.571188
3512.851228	536798.801452	40.576192
3514.104508	536850.221471	40.581197
3514.936243	536875.848553	40.586202
3515.980071	536850.177822	40.591207
3516.242436	536821.347608	40.596212
3517.493971	536764.329641	40.601216
3518.079711	536671.354499	40.606221
3518.528948	536572.137419	40.611226
3519.627010	536434.885617	40.616231
3519.736368	536300.718342	40.621236
3520.065534	536122.875329	40.626240
3520.501442	535934.002265	40.631245
3520.617857	535746.086560	40.636250
3520.981951	535545.400641	40.641255
3521.025590	535336.680879	40.646260
3521.137244	535107.540518	40.651264
3521.127790	534885.235172	40.656269
3521.024337	534641.675104	40.661274
3521.321596	534396.936540	40.666279
3521.234227	534164.782750	40.671284
3521.334890	533907.337586	40.676288
3521.421989	533644.484942	40.681293
3521.251695	533392.024728	40.686298
3521.321428	533118.759195	40.691303
3520.844937	532870.228846	40.696308
3520.965126	532598.714388	40.701312
3520.939548	532332.775599	40.706317
3520.619006	532066.727322	40.711322
3520.921932	531796.938299	40.716327
3520.448682	531535.906908	40.721332
3520.244696	531258.205890	40.726336
3520.304917	530994.605429	40.731341
3519.933043	530720.862430	40.736346
3519.990474	530464.024068	40.741351
3519.574959	530205.437229	40.746356
3519.068561	529929.427912	40.751360
3518.835113	529673.582661	40.756365
3518.639920	529430.056743	40.761370
3518.608849	529168.966635	40.766375
3518.007339	528928.175365	40.771380
3517.946211	528678.754899	40.776384
3517.973573	528442.152161	40.781389
3517.449746	528203.965352	40.786394
3517.481140	527954.923138	40.791399
3517.292601	527734.565870	40.796404
3517.207854	527494.024872	40.801408
3517.117812	527259.292917	40.806413
3516.969192	527032.905612	40.811418
3516.875245	526811.054978	40.816423
3516.608744	526579.979720	40.821428
3516.648215	526349.408704	40.826432
3516.326759	526132.588116	40.831437
3515.892819	525909.868944	40.836442
3515.762946	525689.271952	40.841447
3515.295564	525491.267628	40.846452
3515.406819	525283.313321	40.851456
3515.124263	525068.342299	40.856461
3514.645507	524870.483741	40.861466
3514.593322	524669.573114	40.866471
3514.518072	524475.436867	40.871476
3514.645907	524290.162484	40.876480
3514.165154	524091.536450	40.881485
3513.851317	523904.659361	40.886490
3513.785452	523704.850925	40.891495
3513.320800	523546.098739	40.896500
3513.355982	523366.034982	40.901504
3513.415115	523187.987460	40.906509
3512.971771	523014.364794	40.911514
3512.860076	522837.149229	40.916519
3512.684935	522679.454916	40.921524
3512.537301	522493.697951	40.926528
3512.551817	522343.047780	40.931533
3512.357472	522183.430657	40.936538
3512.313182	522018.682270	40.941543
3511.803586	521868.211639	40.946548
3511.644749	521713.993649	40.951552
3511.947250	521560.055174	40.956557
3511.580923	521415.371615	40.961562
3511.696724	521267.324393	40.966567
3511.174929	521119.831612	40.971572
3511.349641	520966.413301	40.976576
3510.786573	520835.557892	40.981581
3510.737908	520699.918206	40.986586
3510.840084	520561.118911	40.991591
3510.639215	520440.517081	40.996596
3510.327026	520303.398982	41.001600
3510.394244	520165.966969	41.006605
3510.082711	520051.598643	41.011610
3510.139505	519925.845702	41.016615
3510.082152	519802.739017	41.021620
3510.135801	519674.153222	41.026624
3510.130056	519548.508397	41.031629
3509.661782	519424.402021	41.036634
3509.818774	519307.325218	41.041639
3509.545712	519202.096728	41.046644
3509.627306	519081.187446	41.051648
3509.356326	518968.372629	41.056653
3509.362821	518850.456780	41.061658
3509.724890	518740.473064	41.066663
3509.516920	518641.399556	41.071668
3509.173252	518524.446882	41.076672
3509.280056	518419.153353	41.081677
3508.782624	518302.830194	41.086682
3508.849461	518196.681945	41.091687
3508.609146	518100.088035	41.096692
3508.747002	517996.809560	41.101696
3508.697761	517900.032582	41.106701
3508.433217	517809.761674	41.111706
3508.454734	517705.488422	41.116711
3508.068087	517608.712500	41.121716
3507.950872	517516.798537	41.126720
3508.290924	517434.470358	41.131725
3507.933622	517345.779200	41.136730
3508.429716	517242.591108	41.141735
3507.902138	517171.321645	41.146740
3507.874720	517071.552796	41.151744
3507.642849	516987.492290	41.156749
3507.500548	516903.518341	41.161754
3507.453045	516817.405035	41.166759
3507.344420	516735.902859	41.171764
3507.393849	516666.259427	41.176768
3507.431440	516584.480546	41.181773
3507.120274	516507.560650	41.186778
3507.352324	516444.208825	41.191783
3507.404796	516375.018836	41.196788
3507.085578	516292.890343	41.201792
3507.021037	516224.679088	41.206797
3507.216457	516145.603998	41.211802
3506.957155	516071.455366	41.216807
3507.008783	516009.242999	41.221812
3507.160027	515931.893350	41.226816
3507.053748	515861.714862	41.231821
3506.917477	515794.878661	41.236826
3507.227723	515716.238549	41.241831
3507.016290	515655.027337	41.246836
3506.661669	515576.845667	41.251840
3506.711016	515505.427308	41.256845
3506.343332	515451.472161	41.261850
3506.278785	515373.142542	41.266855
3506.388696	515325.180459	41.271860
3506.603615	515263.091229	41.276864
3506.482824	515204.139913	41.281869
3506.092263	515155.093213	41.286874
3506.689683	515088.289952	41.291879
3506.801066	515022.271304	41.296884
3506.558231	514972.239782	41.301888
3506.695495	514904.041815	41.306893
3506.663846	514835.061048	41.311898
3506.293591	514773.922289	41.316903
3506.413183	514708.760908	41.321908
3506.542168	514653.106234	41.326912
3506.294603	514592.200305	41.331917
3505.792812	514530.626255	41.336922
3506.195807	514477.001354	41.341927
3506.209486	514422.274531	41.346932
3506.244016	514375.838971	41.351936
3506.259281	514319.341344	41.356941
3506.056629	514266.671318	41.361946
3506.129400	514206.927233	41.366951
3505.791848	514150.687114	41.371956
3505.704010	514096.885686	41.376960
3505.921299	514058.108291	41.381965
3505.656028	514006.307183	41.386970
3505.915404	513947.443100	41.391975
3506.018979	513905.598012	41.396980
3505.726196	513854.964103	41.401984
3505.653710	513808.290994	41.406989
3505.772813	513746.717095	41.411994
3505.925312	513703.548704	41.416999
3505.782479	513654.256143	41.422004
3505.789586	513603.472920	41.427008
3506.112630	513554.814555	41.432013
3505.783242	513513.745046	41.437018
3505.733171	513456.850208	41.442023
3505.897087	513404.928834	41.447028
3505.591044	513365.524432	41.452032
3505.740431	513318.207930	41.457037
3505.409008	513270.410897	41.462042
3505.894904	513211.457862	41.467047
3505.761380	513178.449561	41.472052
3505.840996	513116.879604	41.477056
3505.852482	513065.790582	41.482061
3505.458412	513026.500464	41.487066
3505.537258	512973.377247	41.492071
3505.626576	512930.975594	41.497076
3505.443509	512876.173681	41.502080
3505.612619	512837.906919	41.507085
3505.241577	512801.394662	41.512090
3506.038535	512743.402480	41.517095
3505.188593	512700.035884	41.522100
3504.985696	512655.656418	41.527104
3505.489944	512618.904260	41.532109
3505.315271	512586.204802	41.537114
3505.603834	512539.774619	41.542119
3505.607761	512502.039037	41.547124
3505.422228	512454.773054	41.552128
3505.400395	512413.652257	41.557133
3505.314289	512355.646569	41.562138
3505.803787	512318.137335	41.567143
3505.633513	512278.456019	41.572148
3505.269527	512232.836307	41.577152
3505.389017	512181.120535	41.582157
3505.416161	512152.839755	41.587162
3505.221941	512111.138458	41.592167
3505.374168	512070.596333	41.597172
3504.860243	512011.594809	41.602176
3505.277986	511988.158738	41.607181
3505.243202	511959.381575	41.612186
3505.271131	511909.652258	41.617191
3505.129266	511882.004759	41.622196
3505.114999	511832.585395	41.627200
3505.542938	511786.738147	41.632205
3504.945162	511756.026205	41.637210
3504.970831	511711.304627	41.642215
3505.125514	511680.018349	41.647220
3505.307886	511629.252086	41.652224
3505.300653	511597.030115	41.657229
3505.035240	511555.895152	41.662234
3505.288006	511515.588743	41.667239
3505.016563	511480.423722	41.672244
3505.212764	511447.005828	41.677248
3505.310997	511399.641469	41.682253
3505.066278	511380.963229	41.687258
3505.107488	511331.685401	41.692263
3504.926605	511294.785733	41.697268
3504.837006	511254.735165	41.702272
3505.033688	511217.421546	41.707277
3504.793900	511198.236455	41.712282
3505.140980	511138.792291	41.717287
3505.095382	511121.650501	41.722292
3504.817235	511080.819926	41.727296
3505.149097	511055.827935	41.732301
3505.144328	511020.822166	41.737306
3504.837431	510979.237076	41.742311
3505.117918	510939.026097	41.747316
3505.071152	510900.232624	41.752320
3505.085421	510863.604706	41.757325
3504.663645	510833.065629	41.762330
3505.023414	510788.895882	41.767335
3504.851722	510748.199449	41.772340
3504.805472	510728.882062	41.777344
3504.872964	510686.630022	41.782349
3504.773294	510677.034043	41.787354
3505.387675	510631.356575	41.792359
3504.777474	510597.002103	41.797364
3504.833077	510559.152864	41.802368
3505.087970	510514.037791	41.807373
3504.795940	510492.027166	41.812378
3505.075516	510440.533751	41.817383
3504.923832	510422.699775	41.822388
3504.641557	510392.239038	41.827392
3504.572535	510350.766587	41.832397
3504.880276	510323.703161	41.837402
3505.004228	510278.203443	41.842407
3504.679877	510251.037447	41.847412
3504.789553	510215.455449	41.852416
3504.733583	510182.378476	41.857421
3504.457589	510168.358143	41.862426
3504.900396	510137.327039	41.867431
3504.770059	510109.624250	41.872436
3504.747791	510073.911040	41.877440
3505.133721	510032.517683	41.882445
3504.901666	510003.515443	41.887450
3504.882157	509968.054530	41.892455
3504.975018	509942.441007	41.897460
3505.111250	509901.440935	41.902464
3505.026964	509865.686502	41.907469
3504.651604	509841.108062	41.912474
3504.791919	509794.238510	41.917479
3504.758583	509764.850318	41.922484
3504.673470	509741.743603	41.927488
3504.846969	509703.469106	41.932493
3504.774901	509666.295761	41.937498
3504.808314	509636.745025	41.942503
3504.644722	509605.302884	41.947508
3504.508794	509576.891830	41.952512
3504.834138	509543.095659	41.957517
3504.608239	509518.695501	41.962522
3504.649601	509489.446808	41.967527
3505.056229	509457.205979	41.972532
3504.794402	509420.770387	41.977536
3504.870037	509391.819664	41.982541
3504.832081	509351.705881	41.987546
3504.743150	509316.659334	41.992551
3504.868203	509290.382044	41.997556
3504.318310	509261.833526	42.002560
3504.930636	509221.161323	42.007565
3504.449281	509218.859649	42.012570
3504.965610	509168.539227	42.017575
3504.852293	509134.356245	42.022580
3504.803999	509105.475221	42.027584
3504.815548	509084.679637	42.032589
3504.839656	509047.388564	42.037594
3504.766451	509009.404480	42.042599
3504.706629	508986.596312	42.047604
3504.676385	508943.343547	42.052608
3505.177854	508915.538970	42.057613
3504.534257	508880.832170	42.062618
3504.585689	508851.833769	42.067623
3505.031019	508818.877312	42.072628
3504.848261	508794.317522	42.077632
3504.489910	508756.630919	42.082637
3504.663234	508730.648711	42.087642
3504.710700	508693.100207	42.092647
3504.770130	508676.040558	42.097652
3504.765646	508636.172787	42.102656
3504.684448	508602.388430	42.107661
3504.507677	508569.074466	42.112666
3504.476069	508546.564825	42.117671
3504.542020	508521.206412	42.122676
3504.338332	508501.456043	42.127680
3504.605584	508466.098491	42.132685
3504.014231	508442.766469	42.137690
3504.368949	508407.192591	42.142695
3504.454573	508395.390444	42.147700
3504.045612	508366.969948	42.152704
3504.650094	508335.960639	42.157709
3504.336402	508318.605440	42.162714
3504.628774	508292.350777	42.167719
3504.386086	508263.954427	42.172724
3504.221363	508236.760009	42.177728
3504.620859	508214.687756	42.182733
3504.209144	508181.258388	42.187738
3504.354270	508166.663897	42.192743
3504.607382	508143.552172	42.197748
3504.386904	508109.991247	42.202752
3504.417737	508080.235861	42.207757
3504.377321	508059.042480	42.212762
3504.442351	508029.382794	42.217767
3504.371637	508000.604653	42.222772
3504.431925	507978.130343	42.227776
3504.362691	507952.488880	42.232781
3504.286958	507929.732425	42.237786
3504.228941	507904.190311	42.242791
3504.486523	507881.583498	42.247796
3504.264703	507864.618096	42.252800
3504.300836	507823.983075	42.257805
3504.277648	507808.655927	42.262810
3504.275397	507781.232724	42.267815
3504.361955	507765.483415	42.272820
3504.316378	507734.069799	42.277824
3504.270350	507717.582441	42.282829
3504.295843	507688.636783	42.287834
3504.402347	507668.937628	42.292839
3504.412294	507650.569250	42.297844
3504.205961	507620.901155	42.302848
3504.553986	507601.163750	42.307853
3504.215456	507566.051896	42.312858
3504.032462	507546.600749	42.317863
3504.333859	507535.472283	42.322868
3504.318508	507513.970685	42.327872
3504.604902	507470.815976	42.332877
3504.139901	507457.987059	42.337882
3504.190809	507430.099513	42.342887
3504.066150	507414.686858	42.347892
3504.002912	507392.939687	42.352896
3504.116723	507363.119353	42.357901
3503.840438	507342.265965	42.362906
3504.379946	507332.465894	42.367911
3504.289274	507313.354084	42.372916
3504.028805	507285.313124	42.377920
3504.242246	507264.382239	42.382925
3504.157508	507248.305343	42.387930
3504.517679	507218.395223	42.392935
3504.197576	507195.878821	42.397940
3504.192678	507170.883817	42.402944
3504.415873	507152.582404	42.407949
3504.215886	507126.909785	42.412954
3504.080222	507097.786214	42.417959
3504.513134	507086.484876	42.422964
3504.463434	507078.093370	42.427968
3504.386635	507030.997627	42.432973
3504.229542	507015.033149	42.437978
3504.429808	506986.210492	42.442983
3504.485312	506970.667768	42.447988
3503.996566	506935.578376	42.452992
3504.370677	506908.600302	42.457997
3503.986606	506892.165588	42.463002
3504.144412	506869.117827	42.468007
3504.243916	506839.450654	42.473012
3503.963018	506831.601570	42.478016
3504.288171	506800.937266	42.483021
3504.200244	506787.795252	42.488026
3504.226526	506763.351335	42.493031
3504.051430	506742.380030	42.498036
3503.583707	506727.982392	42.503040
3504.024689	506699.070612	42.508045
3503.877745	506687.354660	42.513050
3504.004606	506665.930734	42.518055
3504.139659	506647.288517	42.523060
3504.012050	506629.699807	42.528064
3504.388364	506596.851232	42.533069
3504.079415	506594.471347	42.538074
3504.133116	506554.437781	42.543079
3504.356061	506550.759403	42.548084
3504.048734	506519.334355	42.553088
3504.171920	506502.211885	42.558093
3504.418452	506475.455708	42.563098
3504.125716	506457.690518	42.568103
3504.476817	506426.009431	42.573108
3504.028535	506400.830392	42.578112
3503.855260	506377.733105	42.583117
3503.944809	506375.492612	42.588122
3504.029093	506356.858108	42.593127
3504.096123	506343.792469	42.598132
3504.174034	506332.597354	42.603136
3504.455191	506292.628438	42.608141
3504.264189	506281.830005	42.613146
3504.406700	506254.735718	42.618151
3504.073855	506230.955034	42.623156
3504.124214	506204.533058	42.628160
3504.478673	506185.805067	42.633165
3504.405869	506166.840975	42.638170
3504.443069	506131.869238	42.643175
3504.307947	506113.319753	42.648180
3504.005340	506077.591981	42.653184
3504.396062	506061.843656	42.658189
3504.158802	506031.874116	42.663194
3504.112354	506022.671949	42.668199
3504.179220	506001.307290	42.673204
3503.783628	505971.312069	42.678208
3504.195841	505965.731361	42.683213
3504.159286	505938.057655	42.688218
3504.122753	505921.111666	42.693223
3504.283669	505882.274072	42.698228
3503.893440	505878.338249	42.703232
3504.047848	505844.612479	42.708237
3504.087173	505830.791791	42.713242
3504.271758	505811.483014	42.718247
3504.344925	505787.536345	42.723252
3504.172596	505765.854983	42.728256
3504.164792	505742.730700	42.733261
3504.247642	505731.332006	42.738266
3504.098437	505693.605676	42.743271
3504.357597	505682.533307	42.748276
3504.108591	505658.333762	42.753280
3504.400281	505641.335625	42.758285
3504.233602	505619.956808	42.763290
3504.091573	505593.513710	42.768295
3504.206045	505578.517062	42.773300
3503.929372	505559.837550	42.778304
3504.103275	505520.946496	42.783309
3503.810411	505527.115963	42.788314
3503.979602	505491.565438	42.793319
3504.113196	505479.247689	42.798324
3504.023240	505452.087691	42.803329
3504.222836	505436.622031	42.808333
3504.360117	505410.488738	42.813338
3504.350019	505396.220080	42.818343
3504.435701	505365.338082	42.823348
3504.036439	505345.969256	42.828353
3504.325399	505302.403932	42.833357
3503.865118	505306.170924	42.838362
3504.000116	505278.114825	42.843367
3504.111229	505265.041411	42.848372
3504.290103	505239.508543	42.853377
3504.170970	505204.964494	42.858381
3504.128000	505199.354278	42.863386
3504.142833	505171.367605	42.868391
3504.082024	505155.436807	42.873396
3504.102566	505129.878199	42.878401
3503.965306	505112.036456	42.883405
3503.973765	505087.694217	42.888410
3503.963209	505076.967725	42.893415
3503.929807	505051.164503	42.898420
3503.854684	505037.614303	42.903425
3504.115464	505011.106657	42.908429
3503.859880	504998.141607	42.913434
3503.717546	504975.644836	42.918439
3504.273828	504961.944176	42.923444
3503.772126	504941.427167	42.928449
3504.108858	504921.384882	42.933453
3503.865400	504906.191203	42.938458
3503.750398	504894.823236	42.943463
3503.846998	504888.229353	42.948468
3503.768920	504879.790667	42.953473
3504.174899	504845.668970	42.958477
3503.980987	504842.764602	42.963482
3503.836201	504814.802587	42.968487
3503.937995	504799.706064	42.973492
3503.967098	504780.167694	42.978497
3504.402717	504756.212932	42.983501
3503.999752	504750.052198	42.988506
3504.111051	504723.719562	42.993511
3504.129299	504705.751614	42.998516
3504.168782	504688.843022	43.003521
3504.428121	504653.124729	43.008525
3503.884883	504643.949748	43.013530
3503.694669	504615.184893	43.018535
3503.999046	504618.527534	43.023540
3503.653717	504587.712287	43.028545
3503.650575	504579.362825	43.033549
3503.660451	504563.319103	43.038554
3503.855332	504546.132779	43.043559
3503.537192	504522.549866	43.048564
3503.718381	504532.440258	43.053569
3504.091629	504504.547691	43.058573
3503.903092	504487.168876	43.063578
3503.920175	504463.684722	43.068583
3503.846285	504440.670377	43.073588
3503.655337	504430.427464	43.078593
3503.764923	504422.515573	43.083597
3503.340243	504403.048505	43.088602
3503.504372	504389.409381	43.093607
3503.584446	504392.028412	43.098612
3503.847328	504375.944529	43.103617
3503.929818	504361.609787	43.108621
3503.816867	504353.783646	43.113626
3503.786226	504335.823046	43.118631
3503.817223	504308.034868	43.123636
3503.831146	504298.518607	43.128641
3504.337697	504272.173430	43.133645
3504.022454	504260.026980	43.138650
3503.921235	504252.148331	43.143655
3504.398562	504225.453451	43.148660
3503.824513	504216.434937	43.153665
3504.010289	504188.672715	43.158669
3503.930948	504179.930245	43.163674
3503.723947	504170.904302	43.168679
3504.046299	504139.729699	43.173684
3503.990273	504127.947050	43.178689
3504.197844	504098.814829	43.183693
3503.771554	504086.533987	43.188698
3503.666805	504069.445163	43.193703
3504.095268	504044.933876	43.198708
3503.818934	504028.276996	43.203713
3504.156964	504014.812529	43.208717
3504.016829	504011.140400	43.213722
3503.955889	503979.266971	43.218727
3504.176675	503958.280358	43.223732
3503.979400	503945.912612	43.228737
3504.234893	503924.566214	43.233741
3503.899471	503900.580329	43.238746
3503.800701	503890.575574	43.243751
3504.052344	503857.336697	43.248756
3503.555279	503861.767719	43.253761
3503.719220	503837.652214	43.258765
3503.577065	503820.265407	43.263770
3503.732328	503807.082712	43.268775
3504.204094	503794.507897	43.273780
3503.655556	503773.743877	43.278785
3503.812432	503762.230986	43.283789
3503.782384	503759.199319	43.288794
3503.707914	503726.619046	43.293799
3503.910913	503717.072586	43.298804
3503.979081	503706.079769	43.303809
3503.943387	503674.252406	43.308813
3503.263622	503673.803263	43.313818
3503.523390	503665.917905	43.318823
3503.585597	503650.978480	43.323828
3503.588467	503628.457031	43.328833
3503.410578	503628.181610	43.333837
3503.273102	503626.179086	43.338842
3503.709623	503608.447561	43.343847
3503.510463	503583.427520	43.348852
3503.633742	503585.786795	43.353857
3503.713485	503576.563397	43.358861
3503.935435	503561.092554	43.363866
3503.412342	503533.744995	43.368871
3504.264184	503526.423919	43.373876
3503.958266	503509.012079	43.378881
3503.974730	503479.504162	43.383885
3503.482324	503472.446138	43.388890
3503.518794	503462.318544	43.393895
3504.154939	503446.933965	43.398900
3503.661860	503446.910797	43.403905
3503.865441	503430.784815	43.408909
3503.567962	503406.286160	43.413914
3503.630113	503398.077647	43.418919
3503.501341	503386.052949	43.423924
3503.481534	503370.670759	43.428929
3503.676155	503352.926602	43.433933
3503.790566	503350.681794	43.438938
3503.725038	503337.786696	43.443943
3503.744982	503316.932284	43.448948
3503.329471	503312.696211	43.453953
3503.770431	503298.050895	43.458957
3503.891655	503282.950000	43.463962
3503.482910	503274.157923	43.468967
3503.932200	503253.539238	43.473972
3503.651504	503235.262764	43.478977
3503.936070	503212.595040	43.483981
3503.725948	503213.994851	43.488986
3503.484106	503197.939058	43.493991
3503.845595	503171.716387	43.498996
3503.606822	503163.352885	43.504001
3503.784049	503154.873018	43.509005
3503.978587	503136.622551	43.514010
3503.633875	503131.464251	43.519015
3503.733030	503120.364950	43.524020
3503.722269	503097.288259	43.529025
3503.988007	503076.242881	43.534029
3503.615802	503072.860289	43.539034
3503.628409	503053.626273	43.544039
3503.812280	503027.482073	43.549044
3503.830623	503032.793447	43.554049
3503.894649	503011.931707	43.559053
3503.944246	502995.526000	43.564058
3504.031660	502985.440692	43.569063
3504.091771	502951.521825	43.574068
3503.901842	502937.836317	43.579073
3503.991461	502925.675565	43.584077
3503.695304	502902.340060	43.589082
3504.008467	502901.227842	43.594087
3503.769803	502871.809845	43.599092
3503.552892	502860.709726	43.604097
3503.910689	502840.712358	43.609101
3503.842172	502830.449162	43.614106
3503.650487	502812.461850	43.619111
3503.723633	502795.191838	43.624116
3503.678901	502790.036635	43.629121
3503.706011	502758.956869	43.634125
3504.037788	502763.510219	43.639130
3503.987352	502748.638446	43.644135
3504.168966	502718.951320	43.649140
3503.476865	502731.815019	43.654145
3503.537608	502689.342145	43.659149
3503.869827	502674.865337	43.664154
3503.739168	502666.332675	43.669159
3503.797321	502647.091018	43.674164
3503.521856	502643.996725	43.679169
3503.871889	502620.255041	43.684173
3503.654467	502607.079743	43.689178
3503.656560	502584.152187	43.694183
3503.908781	502575.356516	43.699188
3503.949066	502574.641695	43.704193
3504.105056	502541.364848	43.709197
3503.820826	502541.106216	43.714202
3503.498995	502511.093414	43.719207
3503.849414	502494.993983	43.724212
3503.556934	502488.561925	43.729217
3503.878857	502474.491482	43.734221
3503.377892	502453.819609	43.739226
3503.473420	502443.783322	43.744231
3503.575649	502429.292053	43.749236
3503.419834	502435.137259	43.754241
3503.546376	502407.229759	43.759245
3503.767693	502399.046239	43.764250
3503.356044	502392.126852	43.769255
3503.727742	502382.401171	43.774260
3503.664977	502377.349924	43.779265
3503.967200	502354.830150	43.784269
3503.736802	502348.337615	43.789274
3503.819534	502332.685250	43.794279
3504.059968	502290.790376	43.799284
3504.043370	502298.081404	43.804289
3503.792815	502266.740981	43.809293
3504.116646	502256.111759	43.814298
3503.915872	502246.830778	43.819303
3504.055075	502217.149515	43.824308
3503.788905	502197.756177	43.829313
3503.740878	502184.300724	43.834317
3503.584711	502166.307141	43.839322
3503.622589	502166.706180	43.844327
3503.855892	502142.577399	43.849332
3503.562096	502125.162276	43.854337
3503.775172	502113.639430	43.859341
3503.735885	502118.909573	43.864346
3503.847459	502087.410369	43.869351
3503.838172	502069.697155	43.874356
3503.436729	502066.622672	43.879361
3503.908778	502039.368576	43.884365
3503.947406	502031.669286	43.889370
3503.727482	502031.147412	43.894375
3503.884331	501992.453716	43.899380
3503.846145	501992.257414	43.904385
3503.858429	501978.893500	43.909389
3503.618280	501949.828502	43.914394
3503.699738	501945.918460	43.919399
3503.872708	501932.174815	43.924404
3503.756088	501918.831230	43.929409
3503.881914	501896.439984	43.934413
3503.704509	501891.001804	43.939418
3503.866079	501873.008317	43.944423
3503.774099	501847.968877	43.949428
3503.758886	501848.730615	43.954433
3503.803507	501823.720164	43.959437
3503.579323	501801.485348	43.964442
3503.927600	501799.709526	43.969447
3503.990338	501772.570330	43.974452
3503.586714	501771.217035	43.979457
3503.450571	501754.535848	43.984461
3503.779500	501749.473128	43.989466
3503.619545	501724.241798	43.994471
3503.954955	501706.828043	43.999476
3503.508868	501701.128583	44.004481
3503.498721	501681.238681	44.009485
3503.526499	501666.556097	44.014490
3503.356399	501664.609120	44.019495
3503.688026	501655.142450	44.024500
3503.565649	501646.405526	44.029505
3503.562442	501614.417476	44.034509
3503.773718	501617.016183	44.039514
3503.583136	501616.034123	44.044519
3503.845420	501589.774180	44.049524
3503.663900	501575.377677	44.054529
3503.570740	501569.217470	44.059533
3503.760529	501544.234297	44.064538
3503.589447	501530.797797	44.069543
3503.925478	501519.406978	44.074548
3503.703530	501512.457263	44.079553
3503.795032	501484.148928	44.084557
3503.827475	501474.425757	44.089562
3503.547675	501471.888712	44.094567
3504.145027	501445.322519	44.099572
3503.882112	501431.444919	44.104577
3503.681796	501411.028001	44.109581
3503.678277	501395.337827	44.114586
3503.662503	501392.202267	44.119591
3503.915850	501381.381201	44.124596
3503.417113	501365.566810	44.129601
3503.556303	501346.665246	44.134605
3504.134304	501331.692957	44.139610
3503.962404	501318.863816	44.144615
3504.114194	501292.266587	44.149620
3503.991759	501283.934422	44.154625
3503.745088	501264.435750	44.159629
3504.043004	501258.567936	44.164634
3503.922477	501231.203800	44.169639
3503.775210	501207.640063	44.174644
3503.612684	501212.575640	44.179649
3503.808395	501181.466462	44.184653
3503.773080	501168.058846	44.189658
3503.700128	501166.096458	44.194663
3503.829069	501134.238507	44.199668
3504.064400	501127.924995	44.204673
3503.789511	501116.681095	44.209677
3503.744541	501096.694811	44.214682
3503.402777	501074.730751	44.219687
3503.865922	501060.333171	44.224692
3503.376496	501047.503404	44.229697
3503.882023	501025.860915	44.234701
3503.838679	501017.971676	44.239706
3503.613826	501017.956716	44.244711
3503.773780	500990.699729	44.249716
3503.467924	500989.027218	44.254721
3503.672209	500979.428467	44.259725
3503.511320	500955.613465	44.264730
3503.839141	500938.301394	44.269735
3503.805471	500922.716804	44.274740
3503.500303	500928.231791	44.279745
3503.595091	500904.123225	44.284749
3503.935500	500893.693040	44.289754
3503.605502	500894.099636	44.294759
3503.933370	500868.486286	44.299764
3503.678871	500854.201967	44.304769
3503.615093	500841.507244	44.309773
3503.812551	500836.869984	44.314778
3503.655507	500813.560358	44.319783
3503.870693	500790.293102	44.324788
3503.613982	500785.373291	44.329793
3503.750892	500768.344317	44.334797
3503.938679	500755.255450	44.339802
3503.653021	500752.415521	44.344807
3503.622472	500723.872182	44.349812
3503.646151	500719.515446	44.354817
3503.645096	500699.774863	44.359821
3503.440774	500690.493628	44.364826
3503.564389	500678.730906	44.369831
3503.860053	500660.765620	44.374836
3503.967316	500655.737627	44.379841
3503.785210	500632.735431	44.384845
3503.857254	500619.664758	44.389850
3503.603718	500609.935699	44.394855
3503.825454	500581.807818	44.399860
3503.451232	500579.589275	44.404865
3503.768756	500558.887060	44.409869
3503.663722	500552.677760	44.414874
3503.488306	500543.594352	44.419879
3503.984435	500530.810911	44.424884
3503.719444	500528.625716	44.429889
3503.700221	500506.660594	44.434893
3503.380908	500493.094884	44.439898
3503.303679	500492.550408	44.444903
3503.613935	500482.225986	44.449908
3503.669291	500468.803513	44.454913
3503.598098	500446.137874	44.459917
3503.709814	500438.476962	44.464922
3503.279509	500434.191911	44.469927
3503.875728	500400.790862	44.474932
3503.478182	500398.778456	44.479937
3503.629226	500394.199037	44.484941
3503.610575	500382.762317	44.489946
3503.645472	500362.357638	44.494951
3503.471766	500343.403229	44.499956
3503.631246	500347.883200	44.504961
3503.509775	500344.106119	44.509965
3503.381722	500324.030863	44.514970
3503.031048	500313.355239	44.519975
3503.992010	500286.274286	44.524980
3503.507783	500298.803162	44.529985
3503.559595	500281.888413	44.534989
3503.881363	500258.553001	44.539994
3503.477984	500255.883455	44.544999
3503.576645	500242.049016	44.550004
3503.636449	500233.282604	44.555009
3503.810269	500211.286607	44.560013
3503.530134	500204.193719	44.565018
3503.576429	500207.982948	44.570023
3503.749563	500183.861027	44.575028
3503.458763	500168.873229	44.580033
3503.699291	500160.381932	44.585037
3503.632823	500152.394725	44.590042
3503.404298	500134.208046	44.595047
3503.810103	500115.212419	44.600052
3503.369980	500113.459807	44.605057
3503.427802	500103.580020	44.610061
3503.619002	500074.241304	44.615066
3503.407437	500069.921592	44.620071
3503.870315	500067.317579	44.625076
3503.704326	500057.878097	44.630081
3503.575663	500033.348098	44.635085
3503.842795	500013.665608	44.640090
3503.787170	500018.685856	44.645095
3503.740928	499986.701689	44.650100
3503.684237	499978.459762	44.655105
3503.299459	499965.967011	44.660109
3503.724456	499966.001196	44.665114
3503.402210	499948.335338	44.670119
3503.370780	499933.154488	44.675124
3503.405012	499923.885768	44.680129
3503.645918	499925.265165	44.685133
3503.365718	499918.273413	44.690138
3502.996023	499902.234844	44.695143
3503.337112	499881.275022	44.700148
3503.273932	499883.816124	44.705153
3503.415240	499877.213313	44.710157
3503.548160	499882.051939	44.715162
3503.354530	499880.310963	44.720167
3503.946405	499852.224674	44.725172
3503.535059	499837.255651	44.730177
3503.280576	499842.256758	44.735181
3503.320618	499841.592487	44.740186
3503.253766	499831.023574	44.745191
3503.294548	499789.356859	44.750196
3503.376874	499784.130082	44.755201
3503.228752	499773.573981	44.760205
3503.555758	499775.850946	44.765210
3503.181123	499786.287426	44.770215
3503.590865	499769.872443	44.775220
3503.419467	499751.220762	44.780225
3503.504361	499725.644182	44.785229
3503.771232	499727.880037	44.790234
3503.289962	499731.499650	44.795239
3503.542802	499703.719817	44.800244
3503.259048	499687.869953	44.805249
3503.376889	499677.575482	44.810253
3503.638017	499674.902059	44.815258
3503.227087	499678.611806	44.820263
3503.527927	499676.539554	44.825268
3503.727583	499643.250394	44.830273
3503.320059	499637.999757	44.835277
3503.380272	499626.398228	44.840282
3503.709199	499625.131461	44.845287
3503.594619	499608.697961	44.850292
3503.394301	499598.099386	44.855297
3503.329448	499594.313198	44.860301
3503.789517	499590.899629	44.865306
3503.360465	499576.490014	44.870311
3503.647878	499553.614702	44.875316
3503.539661	499550.645293	44.880321
3503.534750	499541.180079	44.885325
3503.730804	499537.403261	44.890330
3503.170950	499518.610252	44.895335
3503.756260	499508.697387	44.900340
3503.503521	499501.245541	44.905345
3503.350932	499504.104554	44.910349
3503.528912	499477.702971	44.915354
3503.209476	499464.642710	44.920359
3503.485612	499458.220920	44.925364
3503.673818	499452.724206	44.930369
3503.640721	499452.729556	44.935373
3503.986206	499427.010120	44.940378
3503.323324	499419.673687	44.945383
3503.375313	499406.605298	44.950388
3503.395459	499411.714983	44.955393
3503.652713	499391.172810	44.960397
3503.908755	499368.352843	44.965402
3503.417078	499359.571926	44.970407
3503.816584	499350.751391	44.975412
3503.838093	499325.943581	44.980417
3503.526028	499315.008149	44.985421
3503.602487	499309.174703	44.990426
3503.277887	499294.444622	44.995431
3503.358294	499270.285507	45.000436
3503.691447	499260.716091	45.005441
3503.399359	499266.988844	45.010445
3503.478301	499262.774884	45.015450
3503.609964	499253.692906	45.020455
3503.621188	499237.188560	45.025460
3503.588507	499225.803941	45.030465
3504.060699	499211.302207	45.035469
3503.974372	499187.827418	45.040474
3503.574276	499175.437780	45.045479
3503.647165	499161.404093	45.050484
3503.407387	499149.191585	45.055489
3503.441424	499131.671096	45.060493
3503.989581	499125.509925	45.065498
3503.655940	499117.513864	45.070503
3503.565241	499087.053782	45.075508
3503.576124	499078.345161	45.080513
3503.657122	499075.447010	45.085517
3503.909264	499065.181583	45.090522
3503.507098	499057.196325	45.095527
3503.608499	499040.475057	45.100532
3503.624158	499045.737421	45.105537
3503.755934	499019.393090	45.110541
3503.814088	498997.616378	45.115546
3503.617775	498995.825117	45.120551
3503.997556	498973.845673	45.125556
3503.904823	498964.191546	45.130561
3504.012694	498952.227691	45.135565
3503.555993	498917.674119	45.140570
3503.213913	498907.907504	45.145575
3503.495695	498895.460520	45.150580
3503.606736	498894.835615	45.155585
3503.470657	498885.340164	45.160589
3503.747850	498863.073064	45.165594
3503.513681	498859.769087	45.170599
3503.462266	498857.144944	45.175604
3503.526640	498842.403635	45.180609
3503.349894	498820.461344	45.185613
3503.671119	498801.427076	45.190618
3503.243562	498813.239304	45.195623
3503.525905	498799.627837	45.200628
3503.703093	498782.337497	45.205633
3503.615541	498766.101446	45.210637
3503.655204	498755.565688	45.215642
3503.669750	498757.132824	45.220647
3503.562115	498736.191969	45.225652
3503.612950	498721.705817	45.230657
3503.326711	498719.118769	45.235661
3503.631358	498707.478013	45.240666
3503.424379	498691.463264	45.245671
3503.516044	498671.452676	45.250676
3503.528926	498666.995902	45.255681
3503.454303	498658.705579	45.260685
3503.481283	498656.625873	45.265690
3503.168213	498628.225098	45.270695
3503.091777	498619.833796	45.275700
3503.556865	498609.129465	45.280705
3503.675703	498609.667659	45.285709
3503.882736	498602.547758	45.290714
3503.374648	498590.782266	45.295719
3503.597303	498560.626131	45.300724
3503.903581	498557.591043	45.305729
3503.532696	498552.536789	45.310733
3503.893850	498534.407155	45.315738
3503.526064	498526.871840	45.320743
3503.608857	498515.873511	45.325748
3503.256232	498510.057002	45.330753
3503.348716	498493.235387	45.335757
3503.414160	498480.670439	45.340762
3503.262341	498486.161934	45.345767
3503.536352	498474.728365	45.350772
3503.306537	498470.208654	45.355777
3503.264769	498445.055263	45.360781
3503.686927	498425.650279	45.365786
3503.067859	498432.329370	45.370791
3503.166186	498421.531024	45.375796
3503.354511	498429.145609	45.380801
3503.414800	498422.808192	45.385805
3503.725849	498413.494941	45.390810
3503.445390	498399.617758	45.395815
3503.763224	498387.620343	45.400820
3503.599769	498380.356415	45.405825
3503.225207	498372.012119	45.410829
3503.454974	498347.220668	45.415834
3503.470856	498342.965836	45.420839
3503.304437	498344.308490	45.425844
3503.386154	498344.751311	45.430849
3503.161948	498341.546912	45.435853
3503.402756	498326.929167	45.440858
3503.261210	498306.094421	45.445863
3503.397780	498303.187363	45.450868
3503.300637	498298.950385	45.455873
3503.463641	498303.784683	45.460877
3503.504023	498295.324142	45.465882
3503.728152	498276.861537	45.470887
3503.700600	498258.337444	45.475892
3503.685845	498249.227478	45.480897
3503.666001	498242.447042	45.485901
3504.206004	498213.505782	45.490906
3503.810439	498201.216003	45.495911
3503.666504	498183.368349	45.500916
3503.751326	498166.446391	45.505921
3503.628679	498167.934013	45.510925
3503.774229	498149.838072	45.515930
3503.726104	498132.734596	45.520935
3503.502922	498115.000650	45.525940
3503.740549	498109.951341	45.530945
3503.564290	498091.703706	45.535949
3503.754165	498076.081309	45.540954
3503.542324	498064.268648	45.545959
3503.720935	498053.052392	45.550964
3503.786593	498028.134567	45.555969
3503.720963	498022.677539	45.560973
3504.040852	498009.464544	45.565978
3503.633245	497991.050872	45.570983
3503.594454	497972.781388	45.575988
3503.758344	497978.172512	45.580993
3503.666387	497956.266392	45.585997
3504.058926	497927.297357	45.591002
3503.826531	497928.903596	45.596007
3503.682076	497904.879443	45.601012
3503.612482	497883.273453	45.606017
3503.473307	497887.649368	45.611021
3503.799086	497870.891551	45.616026
3503.363701	497845.192031	45.621031
3503.734380	497824.022639	45.626036
3503.743085	497825.894534	45.631041
3503.497517	497818.339604	45.636045
3503.596968	497782.734061	45.641050
3503.554396	497783.804051	45.646055
3503.530935	497780.922204	45.651060
3503.536429	497778.795167	45.656065
3503.611867	497763.747473	45.661069
3503.729806	497743.174819	45.666074
3503.173742	497757.893725	45.671079
3503.603227	497737.828709	45.676084
3503.404205	497717.356750	45.681089
3503.347281	497701.874290	45.686093
3503.344040	497687.345229	45.691098
3503.503560	497698.407252	45.696103
3503.528859	497690.961334	45.701108
3503.543535	497674.606891	45.706113
3503.237715	497656.429919	45.711117
3503.644328	497641.582911	45.716122
3503.214250	497652.788777	45.721127
3503.512569	497641.553346	45.726132
3503.156893	497621.055411	45.731137
3503.139152	497599.694018	45.736141
3503.535917	497606.415358	45.741146
3503.323335	497601.740825	45.746151
3503.356039	497600.166357	45.751156
3503.362228	497599.203596	45.756161
3503.668965	497596.421408	45.761165
3503.760913	497569.018102	45.766170
3503.250784	497571.427667	45.771175
3503.511258	497566.577102	45.776180
3503.473422	497557.622315	45.781185
3503.100198	497545.986701	45.786189
3503.469471	497516.818182	45.791194
3503.572456	497522.067188	45.796199
3503.182512	497517.724426	45.801204
3503.315978	497500.844784	45.806209
3503.359037	497504.786975	45.811213
3503.427756	497487.259408	45.816218
3503.268505	497472.046058	45.821223
3503.469553	497466.394832	45.826228
3503.393822	497465.799399	45.831233
3503.396050	497468.938023	45.836237
3503.517142	497461.628751	45.841242
3503.280181	497444.200084	45.846247
3503.285515	497428.707550	45.851252
3503.363293	497417.709346	45.856257
3503.358050	497416.343367	45.861261
3503.725013	497413.146618	45.866266
3503.608809	497408.355548	45.871271
3503.179684	497379.819269	45.876276
3503.678840	497368.450672	45.881281
3503.460762	497379.066301	45.886285
3503.737354	497365.302784	45.891290
3503.602095	497350.136168	45.896295
3503.678518	497329.164589	45.901300
3503.744714	497321.155157	45.906305
3503.340378	497303.803436	45.911309
3503.500602	497288.792574	45.916314
3503.495686	497291.679222	45.921319
3503.220302	497278.661036	45.926324
3503.736565	497273.972474	45.931329
3503.277509	497253.439835	45.936333
3503.558404	497237.903584	45.941338
3503.302520	497243.766294	45.946343
3503.559682	497226.208690	45.951348
3503.759010	497223.797815	45.956353
3503.483408	497209.210164	45.961357
3503.703617	497190.038287	45.966362
3503.631579	497190.809204	45.971367
3503.718598	497170.240787	45.976372
3503.704692	497142.752312	45.981377
3503.619434	497143.930342	45.986381
3503.864029	497132.753716	45.991386
3503.494607	497117.573287	45.996391
3503.459738	497108.870948	46.001396
3503.599732	497097.609577	46.006401
3503.403305	497096.628187	46.011405
3503.828591	497059.501517	46.016410
3503.377259	497055.117717	46.021415
3503.481580	497052.013046	46.026420
3503.512445	497048.160565	46.031425
3503.334443	497037.303814	46.036429
3503.627719	497004.906295	46.041434
3503.534974	497008.566290	46.046439
3503.822097	497001.635615	46.051444
3503.625198	496982.377561	46.056449
3503.174384	496971.513262	46.061453
3503.562010	496953.782890	46.066458
3503.395032	496956.290181	46.071463
3503.720695	496947.935805	46.076468
3503.544093	496918.498206	46.081473
3503.323532	496916.103028	46.086477
3503.436317	496909.351758	46.091482
3503.320941	496908.053777	46.096487
3503.458529	496900.437902	46.101492
3503.328075	496881.473009	46.106497
3503.219617	496873.490984	46.111501
3503.520877	496860.330727	46.116506
3503.282760	496869.025941	46.121511
3503.252781	496864.626126	46.126516
3503.497986	496857.904535	46.131521
3503.440229	496856.344301	46.136525
3503.251370	496836.932936	46.141530
3503.124711	496822.979603	46.146535
3503.464514	496818.521330	46.151540
3503.272925	496820.019958	46.156545
3503.203871	496822.916817	46.161549
3503.695137	496809.574606	46.166554
3503.323811	496794.748608	46.171559
3503.269487	496782.606441	46.176564
3503.394732	496775.650637	46.181569
3503.285508	496782.756031	46.186573
3503.315103	496773.233283	46.191578
3503.305038	496772.526191	46.196583
3503.873158	496745.603295	46.201588
3503.796002	496725.009694	46.206593
3503.384207	496724.973641	46.211597
3503.648274	496721.641149	46.216602
3503.529426	496696.801285	46.221607
3503.615319	496689.649152	46.226612
3503.405661	496671.050960	46.231617
3503.270531	496674.363319	46.236621
3503.520991	496663.793026	46.241626
3503.036818	496651.566824	46.246631
3503.560348	496636.498000	46.251636
3503.607742	496627.225508	46.256641
3503.365915	496635.212613	46.261645
3503.693590	496619.060892	46.266650
3503.479896	496604.361710	46.271655
3503.293171	496596.594451	46.276660
3503.281884	496584.445349	46.281665
3503.084062	496584.628622	46.286669
3503.251974	496569.362805	46.291674
3503.060824	496585.391970	46.296679
3503.176141	496583.348693	46.301684
3503.470063	496562.949404	46.306689
3503.451063	496548.877585	46.311693
3503.682587	496539.778462	46.316698
3503.575535	496538.529767	46.321703
3503.212175	496530.942287	46.326708
3503.343065	496500.240305	46.331713
3503.383256	496496.183715	46.336717
3503.515721	496489.682326	46.341722
3503.362089	496491.276240	46.346727
3503.251109	496485.218363	46.351732
3503.700249	496474.616558	46.356737
3503.227198	496460.413918	46.361741
3503.329010	496450.980846	46.366746
3503.327026	496449.107984	46.371751
3503.426917	496441.953542	46.376756
3503.735115	496442.968169	46.381761
3503.607435	496418.534357	46.386765
3503.517887	496400.575089	46.391770
3503.601032	496398.536877	46.396775
3503.079056	496394.214711	46.401780
3503.422742	496384.186448	46.406785
3503.082998	496370.570225	46.411789
3503.370719	496352.601910	46.416794
3503.198252	496356.780935	46.421799
3502.919805	496355.053019	46.426804
3502.965695	496346.793218	46.431809
3503.120040	496355.882314	46.436813
3503.586252	496348.214268	46.441818
3503.471338	496358.561037	46.446823
3503.293593	496334.337544	46.451828
3503.699501	496302.832313	46.456833
3503.590218	496307.811442	46.461837
3503.783094	496299.984058	46.466842
3503.403629	496286.728460	46.471847
3503.108943	496265.611790	46.476852
3503.396081	496263.085650	46.481857
3503.323793	496262.337742	46.486861
3503.525902	496253.496277	46.491866
3503.538944	496262.405233	46.496871
3503.160306	496236.188158	46.501876
3503.556304	496215.266044	46.506881
3503.491686	496211.124696	46.511885
3503.770025	496201.359813	46.516890
3503.538400	496201.801583	46.521895
3503.386244	496177.421946	46.526900
3503.554458	496165.497345	46.531905
3503.858001	496168.183525	46.536909
3503.652255	496151.254985	46.541914
3503.435235	496134.631993	46.546919
3502.920689	496128.232740	46.551924
3502.970479	496106.150090	46.556929
3502.833002	496111.437512	46.561933
3503.001911	496113.334893	46.566938
3503.194602	496111.481856	46.571943
3503.168008	496112.397527	46.576948
3503.432074	496115.393739	46.581953
3503.231988	496111.729455	46.586957
3503.768621	496105.923506	46.591962
3503.348554	496097.534717	46.596967
3503.420791	496082.587398	46.601972
3503.793493	496074.174558	46.606977
3503.400234	496077.072148	46.611981
3503.225148	496057.050206	46.616986
3503.469282	496045.619833	46.621991
3503.561366	496026.872029	46.626996
3503.872372	496024.899022	46.632001
3503.562979	496014.669995	46.637005
3503.801680	495993.114288	46.642010
3503.497077	495989.871546	46.647015
3503.434330	495976.565662	46.652020
3503.737128	495969.935904	46.657025
3503.636525	495948.788191	46.662029
3503.725525	495929.331940	46.667034
3503.818717	495943.088961	46.672039
3503.645117	495913.851786	46.677044
3503.602568	495900.643916	46.682049
3503.299212	495911.020724	46.687053
3503.511029	495890.633660	46.692058
3503.646075	495871.676381	46.697063
3503.443998	495855.202666	46.702068
3503.463656	495845.225322	46.707073
3503.422246	495848.016705	46.712077
3503.449593	495841.582331	46.717082
3503.348864	495822.206585	46.722087
3503.253627	495803.690683	46.727092
3503.549723	495798.985915	46.732097
3502.908934	495798.074686	46.737101
3503.415515	495787.159616	46.742106
3503.377297	495788.279666	46.747111
3503.256439	495782.628168	46.752116
3503.633199	495754.772060	46.757121
3503.363018	495759.827401	46.762125
3503.473906	495753.734213	46.767130
3503.310957	495754.570190	46.772135
3503.129732	495754.295163	46.777140
3503.308575	495736.394083	46.782145
3503.089026	495732.783430	46.787149
3503.265861	495702.731054	46.792154
3503.117846	495708.475942	46.797159
3503.313521	495711.280504	46.802164
3503.195888	495696.312247	46.807169
3502.910492	495706.382542	46.812173
3503.241868	495695.697637	46.817178
3502.884127	495701.121254	46.822183
3503.302155	495705.055201	46.827188
3503.616601	495695.334972	46.832193
3503.095619	495674.000226	46.837197
3503.378501	495652.285239	46.842202
3503.715888	495654.966147	46.847207
3503.248640	495650.331361	46.852212
3503.446479	495645.743347	46.857217
3503.625983	495634.120406	46.862221
3503.554778	495615.904306	46.867226
3503.619044	495604.805879	46.872231
3503.245683	495598.130963	46.877236
3503.587883	495596.051716	46.882241
3503.120325	495581.442465	46.887245
3503.553208	495553.374652	46.892250
3503.297767	495552.554399	46.897255
3503.218400	495543.858345	46.902260
3503.493363	495546.802296	46.907265
3503.359202	495547.380573	46.912269
3503.392079	495523.072079	46.917274
3503.612172	495516.100804	46.922279
3503.369057	495515.278602	46.927284
3503.507096	495507.611443	46.932289
3503.333585	495515.588238	46.937293
3503.377852	495491.429798	46.942298
3503.116920	495474.559984	46.947303
3503.202880	495466.040290	46.952308
3503.430535	495463.118384	46.957313
3503.178380	495465.234282	46.962317
3503.414007	495458.463059	46.967322
3503.104551	495467.322112	46.972327
3503.278380	495453.218970	46.977332
3503.544314	495425.531775	46.982337
3503.055424	495426.469917	46.987341
3503.226923	495422.544232	46.992346
3503.223660	495427.354946	46.997351
3502.968471	495417.927135	47.002356
3503.378810	495419.583900	47.007361
3503.359911	495415.485777	47.012365
3503.172150	495400.427097	47.017370
3503.336503	495384.857057	47.022375
3503.266069	495378.134180	47.027380
3503.680753	495370.676401	47.032385
3503.553053	495375.709327	47.037389
3503.362801	495362.524414	47.042394
3503.045754	495337.308961	47.047399
3503.186517	495336.274178	47.052404
3503.557438	495330.241014	47.057409
3503.052237	495340.700680	47.062413
3502.951410	495327.805403	47.067418
3503.018794	495323.693623	47.072423
3503.071403	495325.508203	47.077428
3503.623077	495323.497083	47.082433
3503.315835	495326.786255	47.087437
3503.400088	495301.861755	47.092442
3503.224453	495285.839041	47.097447
3503.305031	495281.674533	47.102452
3503.533155	495283.106946	47.107457
3503.509636	495280.629774	47.112461
3504.071597	495271.579059	47.117466
3503.564378	495248.064426	47.122471
3503.363004	495235.590039	47.127476
3503.414226	495228.746613	47.132481
3503.376041	495231.081883	47.137485
3503.762837	495200.995497	47.142490
3503.661224	495192.454690	47.147495
3503.285616	495187.602767	47.152500
3503.416794	495182.417578	47.157505
3503.188955	495171.111891	47.162509
3503.386591	495144.042664	47.167514
3503.542488	495146.347268	47.172519
3503.476034	495152.585772	47.177524
3503.982741	495143.695627	47.182529
3503.294160	495126.893084	47.187533
3503.576448	495103.861077	47.192538
3503.485265	495101.040141	47.197543
3503.576323	495096.823302	47.202548
3503.592195	495072.010563	47.207553
3503.379398	495065.765773	47.212557
3503.120766	495052.692711	47.217562
3503.378855	495051.133033	47.222567
3503.192014	495042.909428	47.227572
3503.512185	495043.820977	47.232577
3503.714677	495026.168632	47.237581
3503.349932	495014.985755	47.242586
3503.362856	495009.515406	47.247591
3503.256656	495002.544875	47.252596
3503.355176	494991.136861	47.257601
3503.362100	494992.857428	47.262605
3503.244083	494971.508801	47.267610
3503.453795	494961.906006	47.272615
3503.097066	494955.987730	47.277620
3503.322029	494952.711733	47.282625
3503.378274	494958.829641	47.287629
3503.302426	494956.512597	47.292634
3503.202277	494950.503131	47.297639
3502.959581	494937.022397	47.302644
3503.204030	494913.084723	47.307649
3502.767321	494912.191824	47.312653
3503.248780	494899.457380	47.317658
3503.159728	494894.357551	47.322663
3503.094795	494905.254216	47.327668
3503.375547	494907.336581	47.332673
3503.268763	494901.885120	47.337677
3503.149528	494907.068738	47.342682
3502.854463	494904.887604	47.347687
3503.284003	494903.402083	47.352692
3503.420487	494896.190619	47.357697
3503.255666	494884.672259	47.362701
3503.264151	494867.252961	47.367706
3503.474541	494860.738677	47.372711
3502.989080	494871.043587	47.377716
3503.514394	494852.631176	47.382721
3503.395711	494865.207282	47.387725
3503.413689	494844.799057	47.392730
3503.290500	494830.337310	47.397735
3503.036507	494832.706740	47.402740
3503.211448	494827.362631	47.407745
3502.841826	494831.168092	47.412749
3503.418951	494821.608419	47.417754
3503.428465	494813.708114	47.422759
3503.002970	494815.446410	47.427764
3503.224825	494809.284735	47.432769
3503.040141	494809.820385	47.437773
3503.191434	494815.619514	47.442778
3503.092052	494793.255051	47.447783
3503.259153	494773.835862	47.452788
3503.357348	494772.098896	47.457793
3503.733700	494773.659824	47.462797
3503.570642	494760.419544	47.467802
3503.464935	494757.448949	47.472807
3503.493502	494747.267061	47.477812
3503.381469	494728.246383	47.482817
3503.679051	494716.857369	47.487821
3503.333829	494724.203401	47.492826
3503.391768	494705.915349	47.497831
3503.255902	494686.290781	47.502836
3503.456096	494667.372593	47.507841
3503.058337	494681.208162	47.512845
3503.386111	494672.497976	47.517850
3503.338551	494680.809668	47.522855
3503.245756	494681.381432	47.527860
3503.571047	494654.595113	47.532865
3503.383303	494641.409283	47.537869
3503.347683	494629.414630	47.542874
3503.795818	494630.457880	47.547879
3503.280848	494619.956754	47.552884
3503.222874	494610.497355	47.557889
3503.127840	494606.866797	47.562893
3503.424293	494594.971539	47.567898
3503.410927	494597.049793	47.572903
3503.198166	494600.881143	47.577908
3503.417514	494606.112600	47.582913
3503.297828	494601.220070	47.587917
3503.107961	494579.224091	47.592922
3503.160804	494573.089051	47.597927
3503.212150	494549.282694	47.602932
3503.411567	494542.618127	47.607937
3503.284519	494544.764990	47.612941
3503.227899	494542.748664	47.617946
3503.608062	494543.600122	47.622951
3503.069785	494526.317555	47.627956
3503.324095	494503.896836	47.632961
3503.257081	494512.566124	47.637965
3503.312740	494505.012837	47.642970
3502.984198	494501.014086	47.647975
3503.285825	494502.485579	47.652980
3503.845928	494490.548583	47.657985
3503.578731	494485.071717	47.662989
3503.674727	494474.322036	47.667994
3503.361627	494458.320324	47.672999
3502.927542	494462.946211	47.678004
3503.293931	494449.216942	47.683009
3503.239744	494453.327069	47.688013
3503.447325	494444.737043	47.693018
3503.321595	494418.933100	47.698023
3503.074287	494411.174484	47.703028
3503.194266	494398.901911	47.708033
3503.099909	494405.955242	47.713037
3503.308494	494411.036551	47.718042
3503.412053	494406.868212	47.723047
3503.487718	494406.350019	47.728052
3503.304161	494384.605985	47.733057
3503.074870	494371.072081	47.738061
3503.306176	494369.263403	47.743066
3503.171497	494357.334864	47.748071
3503.179341	494363.359351	47.753076
3503.689539	494361.202780	47.758081
3503.332134	494369.918033	47.763085
3503.370903	494345.860223	47.768090
3503.573880	494328.105860	47.773095
3503.400978	494321.550697	47.778100
3503.186512	494316.571801	47.783105
3503.273701	494328.660015	47.788109
3503.113878	494314.001108	47.793114
3503.213484	494307.909224	47.798119
3503.180103	494292.521417	47.803124
3503.396483	494270.916579	47.808129
3503.435062	494268.986446	47.813133
3503.168167	494268.117308	47.818138
3503.315898	494264.752126	47.823143
3503.330327	494264.598057	47.828148
3503.263922	494267.596172	47.833153
3503.164082	494247.509720	47.838157
3503.423247	494230.708460	47.843162
3503.308223	494221.916141	47.848167
3503.245078	494225.673285	47.853172
3503.572819	494222.077100	47.858177
3503.222324	494218.740021	47.863181
3503.324137	494214.369372	47.868186
3503.755531	494195.515428	47.873191
3503.717998	494186.103214	47.878196
3503.869699	494171.344319	47.883201
3503.595031	494163.893739	47.888205
3503.373151	494135.015803	47.893210
3503.483504	494133.530036	47.898215
3503.218522	494136.407652	47.903220
3503.701109	494125.444755	47.908225
3503.241569	494104.706096	47.913229
3503.357470	494094.813859	47.918234
3503.334335	494077.196266	47.923239
3503.216990	494087.747246	47.928244
3503.449331	494086.900463	47.933249
3503.116687	494089.434327	47.938253
3503.456184	494074.038039	47.943258
3503.418927	494059.460829	47.948263
3503.459318	494047.504418	47.953268
3503.655451	494039.169194	47.958273
3503.392216	494034.653656	47.963277
3503.276181	494028.342581	47.968282
3503.350917	494006.759820	47.973287
3503.277108	493996.289880	47.978292
3503.367221	493986.857389	47.983297
3503.163419	493996.105541	47.988301
3503.328807	493986.559879	47.993306
3503.528601	493987.237328	47.998311
3503.299945	493974.006848	48.003316
3503.375684	493957.234331	48.008321
3503.479184	493950.939167	48.013325
3503.342843	493944.378090	48.018330
3503.104302	493933.782242	48.023335
3503.331664	493944.278821	48.028340
3503.772259	493935.854274	48.033345
3503.393970	493915.760834	48.038349
3503.321289	493904.531114	48.043354
3503.595422	493895.120128	48.048359
3503.302897	493897.951497	48.053364
3503.272777	493890.917882	48.058369
3503.630549	493871.568877	48.063373
3503.306938	493855.669574	48.068378
3503.134497	493854.431029	48.073383
3503.281452	493859.522232	48.078388
3503.344807	493850.752178	48.083393
3503.425269	493846.131633	48.088397
3503.476757	493826.223349	48.093402
3503.538733	493801.502881	48.098407
3503.018845	493814.598850	48.103412
3503.197696	493808.393001	48.108417
3503.328464	493811.106842	48.113421
3503.237683	493795.018776	48.118426
3503.592247	493789.392792	48.123431
3503.270182	493773.999544	48.128436
3503.412707	493757.317562	48.133441
3503.402316	493761.218373	48.138445
3503.235165	493752.282158	48.143450
3503.719122	493746.838257	48.148455
3503.409206	493725.062778	48.153460
3503.354601	493711.450140	48.158465
3503.396205	493714.431274	48.163469
3503.166363	493712.492872	48.168474
3503.327022	493704.416289	48.173479
3503.228186	493704.330755	48.178484
3503.333406	493679.603288	48.183489
3503.158334	493678.871519	48.188493
3503.184419	493665.803103	48.193498
3503.590217	493667.055651	48.198503
3503.111100	493663.637525	48.203508
3503.093321	493647.082056	48.208513
3503.647615	493637.930481	48.213517
3503.536911	493615.313188	48.218522
3503.191908	493596.378798	48.223527
3503.320953	493583.344687	48.228532
3503.534467	493568.930002	48.233537
3503.298058	493576.309928	48.238541
3503.008643	493579.495317	48.243546
3503.358527	493574.629569	48.248551
3503.246913	493559.405428	48.253556
3503.215112	493539.408724	48.258561
3503.171964	493547.365767	48.263565
3503.344264	493539.692373	48.268570
3503.352942	493529.259767	48.273575
3502.966759	493536.005093	48.278580
3503.299930	493524.812269	48.283585
3503.412355	493532.846004	48.288589
3503.293028	493503.039390	48.293594
3503.253614	493491.095233	48.298599
3503.091620	493497.450673	48.303604
3503.067491	493480.389681	48.308609
3503.123727	493487.470199	48.313613
3503.196374	493472.216862	48.318618
3503.252761	493472.106792	48.323623
3503.006692	493482.729102	48.328628
3503.135812	493468.631505	48.333633
3503.336383	493483.639346	48.338637
3502.948887	493473.066775	48.343642
3503.124102	493449.897710	48.348647
3503.070324	493442.310647	48.353652
3502.935129	493440.661083	48.358657
3503.217818	493449.933890	48.363661
3503.366569	493444.390969	48.368666
3503.273190	493447.747946	48.373671
3502.773643	493452.181878	48.378676
3503.187704	493436.165619	48.383681
3503.326118	493447.233557	48.388685
3503.050575	493452.189100	48.393690
3503.271802	493437.165439	48.398695
3503.208564	493436.314708	48.403700
3503.406559	493408.382027	48.408705
3503.095451	493397.594787	48.413709
3503.040871	493397.552894	48.418714
3503.570044	493389.114100	48.423719
3502.886344	493394.995016	48.428724
3503.085450	493383.418193	48.433729
3503.072336	493389.547587	48.438733
3502.624984	493392.757970	48.443738
3503.273328	493385.110546	48.448743
3503.338263	493389.455272	48.453748
3503.386042	493382.763618	48.458753
3503.331093	493360.491666	48.463757
3503.171472	493345.528126	48.468762
3503.581639	493337.310671	48.473767
3503.188094	493347.298071	48.478772
3503.447761	493341.129930	48.483777
3503.543607	493341.368090	48.488781
3503.449316	493317.937628	48.493786
3503.441407	493296.873482	48.498791
3502.981753	493297.199443	48.503796
3503.339726	493286.407662	48.508801
3503.412917	493294.700893	48.513805
3503.356916	493287.316671	48.518810
3503.474388	493266.182034	48.523815
3503.197675	493262.782479	48.528820
3503.508743	493251.846177	48.533825
3503.336495	493239.872213	48.538829
3503.427452	493240.870724	48.543834
3503.596826	493234.463627	48.548839
3503.282818	493215.726500	48.553844
3503.383652	493197.328893	48.558849
3503.280847	493197.243984	48.563853
3503.573204	493185.854852	48.568858
3503.386282	493191.049650	48.573863
3503.457944	493182.986907	48.578868
3503.452650	493155.744276	48.583873
3503.526360	493157.555737	48.588877
3503.466139	493157.514734	48.593882
3503.209967	493156.542569	48.598887
3503.271091	493151.469159	48.603892
3503.559169	493125.040971	48.608897
3503.397693	493116.052911	48.613901
3503.269333	493107.211529	48.618906
3503.529100	493107.221228	48.623911
3503.234739	493115.370079	48.628916
3503.234927	493098.811279	48.633921
3503.575635	493075.564948	48.638925
3503.287524	493067.913491	48.643930
3503.259108	493062.094625	48.648935
3503.223740	493071.873644	48.653940
3503.605253	493061.179289	48.658945
3503.480929	493068.693618	48.663949
3503.255977	493039.409339	48.668954
3503.550448	493022.601401	48.673959
3503.009244	493030.333553	48.678964
3503.334625	493015.748839	48.683969
3503.445688	493022.365119	48.688973
3503.332379	493008.761240	48.693978
3503.321603	492988.558060	48.698983
3503.441741	492982.057380	48.703988
3503.157216	492973.088699	48.708993
3503.164206	492975.974145	48.713997
3503.224403	492971.356584	48.719002
3503.298555	492966.483621	48.724007
3502.915022	492977.127947	48.729012
3503.244950	492967.049361	48.734017
3503.281130	492960.207469	48.739021
3503.307616	492936.402958	48.744026
3503.110808	492925.242901	48.749031
3503.027048	492926.370323	48.754036
3503.278525	492927.546036	48.759041
3503.465824	492924.680750	48.764045
3503.123196	492932.533474	48.769050
3503.342592	492916.800731	48.774055
3503.332042	492911.130911	48.779060
3503.112447	492895.568815	48.784065
3503.009224	492880.292148	48.789069
3503.051738	492879.677873	48.794074
3503.288382	492882.121920	48.799079
3503.289899	492882.223077	48.804084
3502.998622	492873.356694	48.809089
3503.237815	492879.851493	48.814093
3503.331696	492873.253646	48.819098
3503.331283	492866.468143	48.824103
3503.249052	492856.100165	48.829108
3503.303909	492839.633771	48.834113
3503.303512	492825.859993	48.839117
3503.291241	492822.165361	48.844122
3503.167562	492820.159444	48.849127
3503.157890	492822.338594	48.854132
3503.308387	492814.465787	48.859137
3503.152351	492824.770406	48.864141
3503.054601	492816.075964	48.869146
3503.280858	492791.530738	48.874151
3503.140641	492784.514103	48.879156
3503.155236	492777.776835	48.884161
3503.376095	492775.969655	48.889165
3503.234875	492783.132292	48.894170
3503.318044	492776.941221	48.899175
3503.074540	492779.562452	48.904180
3503.489579	492769.976704	48.909185
3503.335765	492756.024564	48.914189
3503.086003	492736.162720	48.919194
3503.384936	492724.620347	48.924199
3503.311020	492729.189734	48.929204
3503.360712	492728.776880	48.934209
3503.270818	492727.170731	48.939213
3503.275126	492730.006000	48.944218
3503.240853	492709.958149	48.949223
3502.870967	492705.307220	48.954228
3503.194877	492686.620647	48.959233
3503.428287	492693.015147	48.964237
3503.439272	492690.481532	48.969242
3503.614538	492679.262517	48.974247
3503.080237	492683.499563	48.979252
3502.987819	492686.350126	48.984257
3503.118035	492685.468784	48.989261
3502.931640	492664.229568	48.994266
3503.634584	492645.381765	48.999271
3502.918288	492647.166221	49.004276
3503.165318	492631.023747	49.009281
3503.132917	492634.725715	49.014285
3503.126713	492638.929941	49.019290
3503.293154	492633.485262	49.024295
3502.995618	492637.583616	49.029300
3503.045594	492637.373275	49.034305
3503.036683	492638.083763	49.039309
3503.139255	492636.042065	49.044314
3503.208410	492625.447470	49.049319
3503.060639	492638.738652	49.054324
3503.273842	492620.677193	49.059329
3503.245569	492606.097415	49.064333
3503.337152	492604.563852	49.069338
3503.482142	492587.627226	49.074343
3503.455381	492586.264288	49.079348
3503.032532	492589.065813	49.084353
3503.267587	492590.750546	49.089357
3503.552774	492568.069398	49.094362
3503.348204	492541.768885	49.099367
3503.562544	492547.305564	49.104372
3503.545978	492533.027720	49.109377
3503.643921	492528.505364	49.114381
3503.236798	492505.579080	49.119386
3503.216956	492494.998477	49.124391
3503.136948	492493.289465	49.129396
3503.368093	492492.037678	49.134401
3503.123612	492495.823834	49.139405
3503.210057	492494.797479	49.144410
3503.461542	492481.084914	49.149415
3503.174050	492474.395282	49.154420
3503.331032	492457.963048	49.159425
3503.281040	492441.158387	49.164429
3503.238569	492450.938857	49.169434
3503.402887	492439.215021	49.174439
3503.303441	492437.205232	49.179444
3503.539684	492435.193025	49.184449
3503.552943	492410.225194	49.189453
3503.350110	492397.749112	49.194458
3503.526345	492382.529145	49.199463
3503.475877	492396.514092	49.204468
3503.593224	492386.013025	49.209473
3503.677045	492349.082732	49.214477
3503.429614	492345.627737	49.219482
3503.722380	492342.796333	49.224487
3503.533085	492336.394976	49.229492
3503.701265	492310.592270	49.234497
3503.041058	492312.215968	49.239501
3503.177649	492314.017572	49.244506
3503.517420	492295.986433	49.249511
3503.166478	492301.561891	49.254516
3503.508413	492287.531040	49.259521
3503.473472	492258.367416	49.264525
3502.986077	492253.886869	49.269530
3503.317399	492250.239098	49.274535
3503.284622	492254.194406	49.279540
3503.414670	492240.905987	49.284545
3503.370636	492250.838732	49.289549
3503.064653	492230.073691	49.294554
3503.123262	492208.238174	49.299559
3503.166862	492205.344849	49.304564
3503.431684	492205.606958	49.309569
3503.628693	492202.588102	49.314573
3503.166083	492209.295346	49.319578
3503.365456	492201.110707	49.324583
3503.143555	492206.767080	49.329588
3503.403639	492180.341971	49.334593
3503.380530	492173.762367	49.339597
3503.230436	492165.886155	49.344602
3503.683738	492160.041508	49.349607
3503.392678	492171.735147	49.354612
3502.987470	492157.619725	49.359617
3503.369608	492129.200238	49.364621
3503.321312	492128.499009	49.369626
3503.145205	492120.474965	49.374631
3503.026072	492126.773459	49.379636
3503.099405	492123.774138	49.384641
3503.216057	492123.502611	49.389645
3502.964525	492118.984751	49.394650
3503.502527	492117.735079	49.399655
3503.247985	492122.839580	49.404660
3503.223472	492118.387121	49.409665
3503.231299	492088.355564	49.414669
3503.081348	492080.580577	49.419674
3503.209198	492081.066903	49.424679
3503.067377	492073.948969	49.429684
3503.344951	492064.384586	49.434689
3503.054493	492065.038314	49.439693
3503.007317	492078.465922	49.444698
3503.150151	492062.896481	49.449703
3503.225615	492066.480229	49.454708
3503.168411	492063.450890	49.459713
3503.416770	492062.702770	49.464717
3502.909973	492040.146156	49.469722
3503.117937	492034.137680	49.474727
3502.802703	492021.375259	49.479732
3502.918445	492019.635263	49.484737
3503.125899	492024.210993	49.489741
3503.015907	492033.749146	49.494746
3503.415242	492019.151962	49.499751
3503.335468	492024.684642	49.504756
3503.081537	492024.117195	49.509761
3503.486713	492016.811498	49.514765
3503.216052	492027.033392	49.519770
3503.356964	492007.412868	49.524775
3503.084699	491993.478875	49.529780
3503.221474	491976.644274	49.534785
3503.198457	491970.874854	49.539789
3503.258094	491976.284229	49.544794
3503.383087	491965.275297	49.549799
3503.001628	491968.981926	49.554804
3502.972042	491966.201415	49.559809
3503.198256	491967.988888	49.564813
3502.866000	491969.307570	49.569818
3503.123785	491969.469511	49.574823
3502.930756	491969.044362	49.579828
3503.374121	491960.213349	49.584833
3503.309973	491949.031735	49.589837
3503.140259	491945.564382	49.594842
3503.291006	491934.146225	49.599847
3503.323025	491925.380212	49.604852
3503.427109	491931.491564	49.609857
3503.471052	491935.991876	49.614861
3503.418061	491912.654391	49.619866
3503.858770	491886.959948	49.624871
3503.481940	491880.486790	49.629876
3503.487385	491882.866229	49.634881
3503.475817	491866.713323	49.639885
3503.230927	491851.812695	49.644890
3503.272398	491834.739818	49.649895
3503.426872	491834.766163	49.654900
3503.270619	491829.574822	49.659905
3503.481449	491829.035195	49.664909
3503.544846	491816.719210	49.669914
3503.807555	491788.216795	49.674919
3503.420045	491796.026449	49.679924
3503.049683	491793.046562	49.684929
3503.437227	491783.971078	49.689933
3503.213973	491787.247598	49.694938
3503.354876	491764.790844	49.699943
3503.197505	491753.066779	49.704948
3503.020545	491755.829562	49.709953
3503.322761	491744.691203	49.714957
3503.060432	491743.871862	49.719962
3503.405910	491737.132560	49.724967
3503.126458	491741.684033	49.729972
3503.154415	491740.970737	49.734977
3503.367543	491739.164680	49.739981
3502.993355	491710.965383	49.744986
3503.187155	491705.212253	49.749991
3503.332294	491705.138788	49.754996
3503.345879	491694.552446	49.760001
3503.178730	491689.413431	49.765005
3503.027859	491691.260532	49.770010
3503.521789	491683.991320	49.775015
3502.967201	491694.916628	49.780020
3503.370237	491688.320139	49.785025
3503.730925	491666.132384	49.790029
3503.171089	491662.220212	49.795034
3503.246687	491651.674686	49.800039
3503.384314	491641.777707	49.805044
3503.284602	491637.640875	49.810049
3503.434179	491636.857710	49.815053
3503.019320	491622.490190	49.820058
3503.172741	491603.221763	49.825063
3503.179549	491596.890441	49.830068
3503.171389	491599.626566	49.835073
3503.331637	491603.247646	49.840077
3503.125480	491600.241774	49.845082
3503.410056	491589.561897	49.850087
3503.282876	491589.379546	49.855092
3503.211901	491581.895724	49.860097
3503.199924	491568.578630	49.865101
3503.238819	491573.130471	49.870106
3503.753382	491558.970501	49.875111
3503.652064	491557.264770	49.880116
3503.759617	491554.006735	49.885121
3503.753439	491526.204777	49.890125
3503.443052	491523.823085	49.895130
3503.406991	491512.180980	49.900135
3503.196747	491521.380738	49.905140
3503.256426	491500.455798	49.910145
3503.361557	491471.116870	49.915149
3502.931982	491479.996812	49.920154
3503.462470	491467.657413	49.925159
3503.013551	491471.982522	49.930164
3503.056173	491468.987950	49.935169
3503.399218	491468.781918	49.940173
3503.232521	491468.656454	49.945178
3503.246715	491457.462161	49.950183
3503.415303	491445.281235	49.955188
3503.396382	491427.609810	49.960193
3503.496054	491417.617425	49.965197
3503.166606	491427.342504	49.970202
3503.389302	491421.483433	49.975207
3503.523244	491425.716427	49.980212
3503.243008	491399.173038	49.985217
3503.572174	491390.562381	49.990221
3503.339385	491387.712615	49.995226
3503.388493	491371.093897	50.000231
3503.342997	491375.962986	50.005236
3503.290916	491371.818566	50.010241
3503.873075	491344.176564	50.015245
3503.458198	491341.862006	50.020250
3503.306651	491336.821715	50.025255
3503.104823	491332.954173	50.030260
3502.996119	491332.313106	50.035265
3503.419152	491326.118478	50.040269
3502.993891	491309.473396	50.045274
3503.074144	491285.860846	50.050279
3503.079747	491286.417160	50.055284
3503.139576	491274.759751	50.060289
3503.403151	491277.858125	50.065293
3503.078141	491281.809185	50.070298
3503.111597	491277.195431	50.075303
3503.170848	491283.820520	50.080308
3503.291838	491281.725120	50.085313
3503.261083	491279.451129	50.090317
3503.331875	491270.172242	50.095322
3503.398625	491236.635574	50.100327
3503.269130	491234.579759	50.105332
3503.277466	491238.275565	50.110337
3503.186253	491221.577605	50.115341
3503.221221	491231.447764	50.120346
3503.196173	491227.805478	50.125351
3503.380254	491220.635706	50.130356
3502.869240	491206.688214	50.135361
3503.214590	491197.922979	50.140365
3502.935734	491188.598028	50.145370
3503.419058	491180.621282	50.150375
3503.050787	491183.971472	50.155380
3503.067128	491185.032532	50.160385
3503.068152	491186.197302	50.165389
3502.949379	491194.167306	50.170394
3502.982952	491182.412701	50.175399
3503.025600	491185.394078	50.180404
3503.067279	491172.118864	50.185409
3503.345594	491180.735128	50.190413
3503.362377	491196.634821	50.195418
3503.779730	491168.664100	50.200423
3503.342167	491147.868002	50.205428
3503.306374	491137.086571	50.210433
3503.218077	491123.882510	50.215437
3503.172413	491144.198164	50.220442
3503.445724	491132.861433	50.225447
3503.581839	491118.609015	50.230452
3503.177753	491099.630763	50.235457
3503.142018	491096.040785	50.240461
3503.110945	491094.880996	50.245466
3503.286662	491078.545872	50.250471
3503.081315	491086.023163	50.255476
3503.200006	491086.460320	50.260481
3503.190544	491077.244666	50.265485
3503.226657	491080.632247	50.270490
3503.593728	491050.035791	50.275495
3503.596775	491042.438764	50.280500
3503.301071	491040.915643	50.285505
3503.291491	491033.776408	50.290509
3503.380300	491040.244979	50.295514
3503.483332	491028.327365	50.300519
3503.338746	491016.854038	50.305524
3503.309705	490999.639607	50.310529
3503.220948	490993.778985	50.315533
3503.336639	491005.409064	50.320538
3503.424019	490990.303294	50.325543
3503.196838	490988.769338	50.330548
3503.276691	490958.167484	50.335553
3503.276462	490954.267999	50.340557
3502.942812	490947.888979	50.345562
3503.278595	490943.176712	50.350567
3503.006323	490942.865352	50.355572
3503.303055	490948.895933	50.360577
3503.417961	490940.825382	50.365581
3502.868732	490955.346047	50.370586
3503.178234	490942.028338	50.375591
3503.211614	490939.744168	50.380596
3503.303014	490927.727039	50.385601
3503.521014	490903.028694	50.390605
3503.356849	490902.548312	50.395610
3503.214310	490898.418084	50.400615
3503.131085	490905.065828	50.405620
3503.384156	490899.708241	50.410625
3503.198649	490891.685152	50.415629
3503.058717	490888.668696	50.420634
3503.263113	490865.593087	50.425639
3503.395117	490849.973701	50.430644
3503.346178	490849.930909	50.435649
3503.291908	490852.269273	50.440653
3503.509857	490846.005613	50.445658
3503.528264	490838.558011	50.450663
3503.339598	490825.825408	50.455668
3502.649240	490819.654659	50.460673
3503.439702	490809.350183	50.465677
3503.241075	490814.243622	50.470682
3503.436736	490818.011193	50.475687
3503.416034	490817.913293	50.480692
3503.165372	490810.812078	50.485697
3503.411867	490800.542931	50.490701
3503.311045	490772.450938	50.495706
3503.257494	490765.470487	50.500711
3503.210570	490758.894146	50.505716
3502.957627	490756.199403	50.510721
3503.214600	490748.410186	50.515725
3503.151505	490752.725121	50.520730
3503.409432	490730.197981	50.525735
3503.458725	490708.868633	50.530740
3503.084750	490670.538655	50.535745
3503.078374	490621.514928	50.540749
3502.850647	490567.005677	50.545754
3502.844165	490493.772961	50.550759
3502.839196	490421.096827	50.555764
3502.636457	490344.551903	50.560769
3502.865412	490231.726128	50.565773
3502.400336	490143.117297	50.570778
3502.019220	490025.727196	50.575783
3502.094052	489908.416235	50.580788
3501.653185	489778.068262	50.585793
3501.628029	489640.714871	50.590797
3501.355035	489498.132195	50.595802
3501.371765	489340.358587	50.600807
3500.989636	489177.986950	50.605812
3500.383990	489013.420644	50.610817
3500.437168	488833.654955	50.615821
3500.117345	488651.262012	50.620826
3500.111323	488464.664293	50.625831
3499.629833	488261.374102	50.630836
3499.345616	488063.014486	50.635841
3498.874713	487853.184066	50.640845
3497.954059	487644.992669	50.645850
3497.991739	487422.565656	50.650855
3497.779009	487198.504010	50.655860
3497.008430	486971.184642	50.660865
3497.132947	486730.803797	50.665869
3496.449574	486493.840298	50.670874
3495.815016	486246.532051	50.675879
3495.789847	485999.073621	50.680884
3495.332761	485745.550564	50.685889
3494.977232	485477.722169	50.690893
3494.129140	485222.936853	50.695898
3494.193964	484954.325465	50.700903
3493.779225	484680.010721	50.705908
3493.012971	484399.668167	50.710913
3492.642415	484112.216839	50.715917
3492.119898	483835.069974	50.720922
3491.584483	483541.708560	50.725927
3491.115132	483250.156202	50.730932
3490.584291	482959.369164	50.735937
3490.198363	482652.189508	50.740941
3489.435567	482352.411359	50.745946
3488.938252	482039.007513	50.750951
3488.663536	481727.894224	50.755956
3487.777637	481431.110840	50.760961
3487.661295	481108.207222	50.765965
3487.042213	480791.661024	50.770970
3486.394890	480457.784210	50.775975
3485.668460	480141.244489	50.780980
3484.977340	479823.427240	50.785985
3484.977656	479491.813344	50.790989
3483.959482	479164.814337	50.795994
3483.741373	478823.341970	50.800999
3483.499319	478490.938775	50.806004
3482.527264	478153.577566	50.811009
3481.791173	477812.169670	50.816013
3481.189546	477456.898993	50.821018
3480.539871	477113.995749	50.826023
3479.926631	476771.587676	50.831028
3479.493719	476426.509738	50.836033
3479.041297	476070.177178	50.841037
3478.084706	475730.339774	50.846042
3477.800816	475368.646264	50.851047
3477.096246	475010.864922	50.856052
3476.293967	474660.645075	50.861057
3475.620199	474309.689216	50.866061
3475.148584	473953.677117	50.871066
3474.516127	473583.491039	50.876071
3473.856321	473230.385338	50.881076
3473.055392	472874.051559	50.886081
3472.918531	472504.781376	50.891085
3472.060983	472152.296593	50.896090
3471.250614	471781.497636	50.901095
3470.513515	471416.763829	50.906100
3469.953501	471056.152644	50.911105
3469.499267	470692.527302	50.916109
3468.575810	470330.794854	50.921114
3468.290179	469953.137222	50.926119
3467.205959	469581.885716	50.931124
3466.449222	469225.126885	50.936129
3466.179954	468846.736736	50.941133
3465.184834	468487.011551	50.946138
3464.411495	468114.619988	50.951143
3463.997565	467752.305824	50.956148
3463.225714	467389.382812	50.961153
3462.864012	467016.602445	50.966157
3462.033599	466650.988530	50.971162
3461.526935	466275.124842	50.976167
3460.716261	465906.198902	50.981172
3460.074650	465538.659673	50.986177
3459.270155	465161.656981	50.991181
3458.605438	464782.952032	50.996186
3458.028205	464424.511396	51.001191
3457.574712	464054.178331	51.006196
3456.714444	463676.296066	51.011201
3456.135770	463308.353441	51.016205
3455.153288	462936.918247	51.021210
3454.752055	462556.712221	51.026215
3453.932187	462195.483279	51.031220
3453.006737	461832.895592	51.036225
3452.505636	461455.019003	51.041229
3451.788495	461100.146152	51.046234
3450.848303	460724.811544	51.051239
3450.197353	460356.982279	51.056244
3449.744475	459989.267669	51.061249
3448.831265	459629.075989	51.066253
3447.973389	459272.369610	51.071258
3447.601244	458904.776206	51.076263
3447.028384	458530.969099	51.081268
3446.130208	458171.765669	51.086273
3445.558913	457802.562108	51.091277
3444.644550	457435.638675	51.096282
3443.858609	457071.225331	51.101287
3443.685691	456708.332464	51.106292
3442.526415	456350.003205	51.111297
3442.087999	455972.783475	51.116301
3441.147111	455623.641220	51.121306
3440.664976	455254.787174	51.126311
3439.659492	454895.040497	51.131316
3439.014414	454537.108286	51.136321
3438.521356	454176.913981	51.141325
3437.544629	453827.089933	51.146330
3437.077517	453463.024167	51.151335
3436.433336	453103.445517	51.156340
3435.610232	452749.267801	51.161345
3434.814694	452388.128860	51.166349
3433.904911	452041.311120	51.171354
3433.612187	451684.445254	51.176359
3432.915594	451330.935920	51.181364
3432.023410	450985.317222	51.186369
3431.471546	450621.929965	51.191373
3430.410245	450272.572265	51.196378
3429.715724	449921.019991	51.201383
3429.451606	449580.304733	51.206388
3428.732401	449218.089025	51.211393
3428.157413	448863.203274	51.216397
3427.119685	448521.833587	51.221402
3426.168179	448164.966796	51.226407
3425.734136	447815.422233	51.231412
3424.797450	447484.831149	51.236417
3424.326253	447130.866955	51.241421
3423.655800	446785.303035	51.246426
3423.064158	446444.949132	51.251431
3422.351682	446092.225556	51.256436
3421.620128	445755.132072	51.261441
3420.993072	445397.613744	51.266445
3420.039129	445053.388989	51.271450
3419.349639	444724.699701	51.276455
3419.124486	444370.553857	51.281460
3418.042802	444039.633071	51.286465
3417.483423	443683.347309	51.291469
3416.340273	443351.969923	51.296474
3415.702157	443010.000779	51.301479
3415.136774	442669.791915	51.306484
3414.372907	442343.162976	51.311489
3413.993418	441998.346739	51.316493
3412.819410	441660.656506	51.321498
3412.307784	441342.756207	51.326503
3411.817330	440997.841794	51.331508
3411.123590	440664.935199	51.336513
3410.545193	440328.046109	51.341517
3409.647257	439992.725900	51.346522
3408.782809	439660.441845	51.351527
3408.062685	439327.698958	51.356532
3407.211524	438998.703781	51.361537
3406.651908	438667.551209	51.366541
3405.826478	438355.246452	51.371546
3405.309930	438022.098423	51.376551
3404.661192	437693.180836	51.381556
3403.591569	437382.171738	51.386561
3403.073602	437051.194135	51.391565
3402.603156	436724.114168	51.396570
3401.829331	436408.933575	51.401575
3401.037955	436083.673080	51.406580
3400.295316	435757.309011	51.411585
3399.869612	435431.398365	51.416589
3399.055082	435114.050033	51.421594
3398.026060	434797.899507	51.426599
3397.494311	434472.044053	51.431604
3396.800530	434155.807138	51.436609
3396.452224	433841.035042	51.441613
3395.654095	433525.441542	51.446618
3394.901873	433204.809653	51.451623
3394.556143	432888.044994	51.456628
3393.417658	432576.556083	51.461633
3393.038705	432249.429397	51.466637
3392.282822	431929.315386	51.471642
3391.529707	431614.503827	51.476647
3390.998962	431288.455424	51.481652
3389.754605	430977.446415	51.486657
3389.272965	430657.324115	51.491661
3388.570061	430353.738245	51.496666
3388.129992	430032.611380	51.501671
3387.468650	429726.142216	51.506676
3386.539733	429410.265284	51.511681
3386.251592	429092.302496	51.516685
3385.342872	428778.725644	51.521690
3384.653199	428469.681477	51.526695
3384.138156	428160.377528	51.531700
3383.434535	427846.554025	51.536705
3382.538508	427525.798836	51.541709
3381.738335	427222.014483	51.546714
3381.227223	426907.412975	51.551719
3380.513940	426591.188955	51.556724
3379.675890	426292.022172	51.561729
3379.043094	425969.581270	51.566733
3378.245159	425671.620288	51.571738
3377.509660	425359.372652	51.576743
3376.976353	425049.349850	51.581748
3376.086792	424749.869296	51.586753
3375.473967	424451.586201	51.591757
3374.929570	424150.164957	51.596762
3373.990285	423844.484969	51.601767
3373.404827	423533.843526	51.606772
3372.679514	423239.730438	51.611777
3372.127977	422928.289363	51.616781
3371.339132	422631.182595	51.621786
3370.437803	422337.595667	51.626791
3370.020062	422023.252926	51.631796
3369.180916	421741.054754	51.636801
3368.565217	421438.344926	51.641805
3367.638133	421143.352304	51.646810
3367.183589	420846.224278	51.651815
3366.742989	420543.781832	51.656820
3365.783703	420257.142201	51.661825
3365.185523	419957.004528	51.666829
3364.314606	419661.047439	51.671834
3363.682772	419360.070397	51.676839
3363.311498	419067.051024	51.681844
3362.369853	418779.021710	51.686849
3361.668222	418480.764507	51.691853
3360.760530	418193.155719	51.696858
3360.207940	417902.388513	51.701863
3359.564759	417619.279487	51.706868
3358.992557	417325.994415	51.711873
3358.315578	417034.679102	51.716877
3357.448084	416742.476344	51.721882
3356.578246	416455.733221	51.726887
3356.130661	416172.807588	51.731892
3355.233064	415885.783698	51.736897
3354.611411	415592.234642	51.741901
3354.288953	415317.614175	51.746906
3353.549206	415017.141896	51.751911
3352.594907	414740.202194	51.756916
3351.373241	414462.514496	51.761921
3351.088828	414177.053603	51.766925
3350.575297	413896.733164	51.771930
3349.404215	413614.506760	51.776935
3349.113476	413332.951500	51.781940
3348.425086	413059.663452	51.786945
3347.638952	412773.277274	51.791949
3346.992405	412499.189727	51.796954
3346.290258	412217.688857	51.801959
3345.604270	411931.939329	51.806964
3344.842554	411675.598352	51.811969
3344.564789	411375.676389	51.816973
3343.572490	411109.660295	51.821978
3342.923525	410831.060076	51.826983
3342.373589	410557.295085	51.831988
3341.510202	410283.729625	51.836993
3340.857805	410004.029579	51.841997
3340.050389	409732.279866	51.847002
3339.516762	409449.633553	51.852007
3339.116189	409177.153796	51.857012
3338.248968	408908.176040	51.862017
3337.863696	408629.589989	51.867021
3337.282019	408353.395829	51.872026
3336.223092	408069.599911	51.877031
3335.788754	407790.149899	51.882036
3335.071587	407521.415710	51.887041
3334.294161	407233.374296	51.892045
3333.475696	406967.700918	51.897050
3332.634368	406694.328380	51.902055
3332.504541	406425.059687	51.907060
3331.365640	406154.423347	51.912065
3330.963772	405872.587232	51.917069
3330.350759	405602.218715	51.922074
3329.449513	405311.586636	51.927079
3328.948382	405048.693123	51.932084
3327.957530	404774.386944	51.937089
3327.454473	404506.838105	51.942093
3326.582886	404233.880793	51.947098
3325.848893	403967.355106	51.952103
3325.335575	403694.514373	51.957108
3324.477957	403432.019530	51.962113
3323.987229	403163.516910	51.967117
3323.166079	402898.876851	51.972122
3322.449480	402635.107663	51.977127
3321.711210	402366.891630	51.982132
3320.922162	402114.313347	51.987137
3320.224919	401837.673073	51.992141
3319.337773	401587.749624	51.997146
3319.038621	401322.276816	52.002151
3318.477057	401046.752100	52.007156
3317.749598	400798.856181	52.012161
3317.342509	400533.876909	52.017165
3316.668664	400270.488230	52.022170
3315.906788	400011.559747	52.027175
3315.117881	399736.085246	52.032180
3314.035958	399477.355643	52.037185
3313.711186	399217.868746	52.042189
3312.723151	398955.942651	52.047194
3311.988099	398708.870879	52.052199
3311.833872	398434.937380	52.057204
3311.183745	398183.069129	52.062209
3310.506565	397920.373839	52.067213
3309.877262	397657.821417	52.072218
3308.808747	397395.921069	52.077223
3308.475311	397136.953011	52.082228
3307.768254	396879.109745	52.087233
3307.136488	396607.677166	52.092237
3306.473596	396353.076884	52.097242
3305.406740	396091.242292	52.102247
3305.453565	395822.365394	52.107252
3304.227882	395560.424669	52.112257
3303.376996	395300.634444	52.117261
3302.743341	395048.536551	52.122266
3302.205705	394784.930175	52.127271
3301.490848	394526.332823	52.132276
3300.692262	394279.594276	52.137281
3299.774348	394017.770917	52.142285
3299.236067	393771.597705	52.147290
3298.301573	393521.010682	52.152295
3297.750143	393265.072923	52.157300
3297.039935	393022.226724	52.162305
3296.534030	392774.414053	52.167309
3295.651077	392526.023604	52.172314
3295.180559	392271.997990	52.177319
3294.419432	392022.287966	52.182324
3293.643474	391782.418249	52.187329
3293.050667	391531.711904	52.192333
3292.286821	391282.352965	52.197338
3291.406502	391040.765678	52.202343
3290.930793	390794.637681	52.207348
3290.341705	390549.695514	52.212353
3289.762840	390315.175008	52.217357
3289.114514	390063.322741	52.222362
3288.304936	389815.689660	52.227367
3287.885405	389564.713034	52.232372
3286.821088	389331.534150	52.237377
3286.167911	389080.107930	52.242381
3285.675192	388841.470194	52.247386
3284.909224	388597.305344	52.252391
3284.180229	388345.148529	52.257396
3283.729163	388110.389843	52.262401
3283.238270	387861.421375	52.267405
3282.140554	387620.786062	52.272410
3281.753053	387379.451954	52.277415
3281.173082	387137.205802	52.282420
3280.125877	386894.625062	52.287425
3279.755662	386642.908196	52.292429
3279.045810	386407.925100	52.297434
3278.091297	386164.561948	52.302439
3277.879784	385916.909161	52.307444
3276.915656	385682.444788	52.312449
3276.232602	385439.110176	52.317453
3275.837780	385197.533926	52.322458
3274.998544	384947.608867	52.327463
3274.801710	384699.843852	52.332468
3273.504894	384465.958412	52.337473
3272.775056	384212.043871	52.342477
3272.200734	383979.007477	52.347482
3271.481312	383742.177869	52.352487
3270.934262	383495.630075	52.357492
3270.020265	383256.691919	52.362497
3269.247895	383009.133866	52.367501
3268.866325	382783.536527	52.372506
3267.818327	382555.601754	52.377511
3267.681845	382302.343405	52.382516
3266.448554	382084.150260	52.387521
3266.047428	381840.188116	52.392525
3265.648973	381604.184463	52.397530
3264.653478	381370.028658	52.402535
3264.127210	381131.219237	52.407540
3263.294441	380900.697194	52.412545
3262.747047	380658.530976	52.417549
3261.999671	380431.934802	52.422554
3261.262356	380194.526358	52.427559
3261.140946	379952.568103	52.432564
3259.922237	379721.235302	52.437569
3259.315674	379490.414721	52.442573
3259.083466	379250.199143	52.447578
3258.197259	379022.370409	52.452583
3257.636824	378776.633672	52.457588
3256.839405	378534.951584	52.462593
3256.266427	378299.387780	52.467597
3255.439212	378066.228247	52.472602
3254.559884	377829.285720	52.477607
3254.402991	377594.999969	52.482612
3253.298883	377365.746292	52.487617
3252.672985	377124.486286	52.492621
3252.135917	376891.401129	52.497626
3251.449506	376664.773553	52.502631
3250.667650	376416.004863	52.507636
3249.885697	376190.763273	52.512641
3249.344020	375948.261908	52.517645
3248.887497	375725.815129	52.522650
3247.953724	375501.331360	52.527655
3247.636968	375252.202113	52.532660
3246.590608	375022.722424	52.537665
3245.853274	374796.245027	52.542669
3245.254135	374558.094197	52.547674
3244.644177	374335.079012	52.552679
3244.214982	374097.788935	52.557684
3242.920688	373861.244832	52.562689
3242.667692	373627.968783	52.567693
3241.987589	373405.773664	52.572698
3241.084187	373180.839906	52.577703
3240.891622	372939.384743	52.582708
3239.942416	372715.651311	52.587713
3239.146375	372487.873143	52.592717
3238.719985	372253.319421	52.597722
3237.765970	372028.056735	52.602727
3237.574834	371794.557106	52.607732
3236.391664	371566.606211	52.612737
3236.030874	371336.259897	52.617741
3235.340214	371111.179599	52.622746
3234.615998	370880.735652	52.627751
3234.064515	370653.850137	52.632756
3232.953399	370424.151787	52.637761
3232.337802	370195.264219	52.642765
3231.760032	369976.647265	52.647770
3230.984872	369752.692519	52.652775
3230.543246	369523.595760	52.657780
3229.722717	369304.606738	52.662785
3229.187035	369075.293510	52.667789
3228.306950	368842.980645	52.672794
3227.534172	368629.348664	52.677799
3227.311787	368400.923626	52.682804
3226.668571	368178.568085	52.687809
3225.899045	367949.921939	52.692813
3225.380554	367726.170535	52.697818
3224.334615	367500.160796	52.702823
3223.462534	367266.515314	52.707828
3222.789657	367049.348858	52.712833
3222.172560	366832.299721	52.717837
3221.509033	366611.084359	52.722842
3220.721303	366401.234781	52.727847
3220.350278	366166.283009	52.732852
3219.225466	365959.435988	52.737857
3219.025863	365743.892938	52.742861
3218.343293	365524.405298	52.747866
3217.563799	365302.743832	52.752871
3216.899895	365080.248815	52.757876
3216.107622	364865.965691	52.762881
3215.775300	364645.655077	52.767885
3215.078006	364421.355636	52.772890
3214.324392	364211.668554	52.777895
3213.775277	363981.364289	52.782900
3213.204445	363767.549834	52.787905
3212.262133	363542.572411	52.792909
3211.637016	363320.088107	52.797914
3210.770777	363102.373472	52.802919
3210.301008	362880.066023	52.807924
3209.484041	362667.277722	52.812929
3208.668194	362448.381601	52.817933
3208.385887	362232.529731	52.822938
3207.528520	362020.355532	52.827943
3207.020137	361795.326429	52.832948
3206.328326	361581.750033	52.837953
3205.381164	361362.945939	52.842957
3204.970140	361145.124712	52.847962
3204.265642	360931.216588	52.852967
3203.827808	360704.771626	52.857972
3202.957642	360503.203347	52.862977
3202.293687	360275.876075	52.867981
3201.608267	360061.502998	52.872986
3200.858063	359841.108542	52.877991
3200.333220	359622.127842	52.882996
3199.760172	359402.314051	52.888001
3198.849889	359178.862907	52.893005
3198.223376	358971.244339	52.898010
3197.303706	358757.615011	52.903015
3196.946210	358531.986829	52.908020
3195.991722	358322.508883	52.913025
3195.456181	358102.097996	52.918029
3194.897055	357891.537788	52.923034
3194.315632	357686.985694	52.928039
3193.679015	357462.516407	52.933044
3192.905740	357248.119367	52.938049
3191.952582	357040.467946	52.943053
3191.534685	356834.410508	52.948058
3190.798860	356618.223501	52.953063
3190.314406	356398.738493	52.958068
3189.249443	356189.421666	52.963073
3188.917978	355973.015213	52.968077
3188.332137	355766.369193	52.973082
3187.262127	355550.205000	52.978087
3186.515345	355334.879433	52.983092
3185.890719	355136.507630	52.988097
3184.927549	354920.756468	52.993101
3184.424585	354719.259088	52.998106
3183.713675	354511.482559	53.003111
3183.459496	354301.749728	53.008116
3182.738934	354102.294790	53.013121
3181.990000	353890.908035	53.018125
3181.605968	353676.536051	53.023130
3180.600568	353473.688129	53.028135
3180.067067	353264.198863	53.033140
3179.103334	353055.056759	53.038145
3178.471857	352843.774401	53.043149
3178.051623	352635.664408	53.048154
3177.551358	352432.656173	53.053159
3176.720306	352221.377430	53.058164
3175.900724	352014.193446	53.063169
3175.239331	351809.757663	53.068173
3174.654460	351596.706881	53.073178
3173.500507	351395.554130	53.078183
3173.030313	351196.888364	53.083188
3172.550697	350986.618013	53.088193
3171.808423	350785.448734	53.093197
3171.302507	350582.841531	53.098202
3170.482194	350380.614163	53.103207
3169.955148	350172.155123	53.108212
3169.025417	349977.909624	53.113217
3168.032076	349777.158070	53.118221
3168.123462	349571.652989	53.123226
3167.105841	349365.406350	53.128231
3166.640282	349163.550996	53.133236
3166.046975	348958.304644	53.138241
3165.303433	348754.073897	53.143245
3164.695759	348544.094323	53.148250
3163.632044	348346.504648	53.153255
3163.586899	348135.136500	53.158260
3162.607996	347937.201080	53.163265
3161.934478	347736.111521	53.168269
3161.321927	347525.976167	53.173274
3160.304258	347325.575881	53.178279
3159.838447	347118.470027	53.183284
3159.260431	346929.248598	53.188289
3158.407059	346725.485952	53.193293
3157.912781	346523.651044	53.198298
3157.118106	346318.706844	53.203303
3156.823951	346108.439494	53.208308
3155.978872	345919.282413	53.213313
3155.093953	345720.433526	53.218317
3154.522392	345510.742383	53.223322
3153.731076	345312.106353	53.228327
3152.879618	345114.344559	53.233332
3152.572439	344924.462788	53.238337
3151.895423	344711.094743	53.243341
3151.391982	344512.461341	53.248346
3150.562561	344314.158827	53.253351
3150.045880	344102.774010	53.258356
3149.408447	343907.723242	53.263361
3148.536890	343695.018622	53.268365
3148.060639	343494.977538	53.273370
3147.136260	343299.206556	53.278375
3146.660947	343093.335060	53.283380
3145.945621	342887.577192	53.288385
3145.569877	342686.117529	53.293389
3144.816004	342476.291705	53.298394
3143.964474	342286.945783	53.303399
3143.315176	342074.582052	53.308404
3142.550156	341882.930293	53.313409
3141.745150	341681.815201	53.318413
3140.695757	341475.469023	53.323418
3140.181585	341284.972061	53.328423
3139.692198	341091.008747	53.333428
3139.162997	340907.513036	53.338433
3138.475486	340698.816065	53.343437
3138.363488	340500.438405	53.348442
3137.202609	340298.967824	53.353447
3136.918799	340088.906725	53.358452
3135.862746	339896.505733	53.363457
3135.406706	339693.699831	53.368461
3134.907046	339497.034918	53.373466
3133.815737	339295.601016	53.378471
3133.249110	339091.232439	53.383476
3132.056645	338895.413484	53.388481
3131.414866	338702.688753	53.393485
3130.995482	338504.327989	53.398490
3130.387393	338319.258953	53.403495
3129.825499	338118.475786	53.408500
3129.227840	337922.661568	53.413505
3128.617160	337720.077508	53.418509
3128.092219	337530.843719	53.423514
3127.042273	337319.214616	53.428519
3126.629568	337122.121368	53.433524
3125.898106	336934.700469	53.438529
3125.217030	336739.099546	53.443533
3124.895080	336537.662591	53.448538
3123.974085	336345.255071	53.453543
3123.307531	336135.241633	53.458548
3122.514708	335948.693175	53.463553
3121.728893	335743.330500	53.468557
3121.067553	335548.155716	53.473562
3120.174010	335344.489020	53.478567
3119.886234	335158.189393	53.483572
3119.078971	334957.588181	53.488577
3118.565675	334769.082941	53.493581
3117.912247	334572.045714	53.498586
3117.276402	334380.554834	53.503591
3116.528978	334184.600572	53.508596
3116.155908	333996.300132	53.513601
3115.366617	333789.964722	53.518605
3114.523042	333591.427319	53.523610
3113.981877	333397.856663	53.528615
3113.566512	333196.042706	53.533620
3112.710273	333003.462749	53.538625
3112.136873	332802.589147	53.543629
3111.480624	332602.313615	53.548634
3110.292464	332408.511652	53.553639
3110.251015	332214.374962	53.558644
3109.456483	332017.938378	53.563649
3108.715318	331818.259609	53.568653
3107.777059	331613.087012	53.573658
3107.479769	331420.439776	53.578663
3106.991134	331221.788644	53.583668
3106.244495	331024.119759	53.588673
3105.109418	330830.101464	53.593677
3104.715789	330621.912137	53.598682
3104.001253	330435.565689	53.603687
3103.522872	330247.271988	53.608692
3102.822018	330067.338062	53.613697
3102.343536	329877.312230	53.618701
3101.711610	329679.392440	53.623706
3100.360449	329489.172738	53.628711
3100.050692	329285.167122	53.633716
3099.334243	329086.622657	53.638721
3098.661712	328893.468086	53.643725
3098.193423	328698.753141	53.648730
3097.383477	328501.825872	53.653735
3096.801549	328305.167525	53.658740
3096.220941	328114.084102	53.663745
3095.380424	327906.085234	53.668749
3095.070114	327706.098081	53.673754
3094.118461	327516.344869	53.678759
3093.691870	327307.693316	53.683764
3092.959947	327116.885967	53.688769
3092.007926	326916.361827	53.693773
3091.622038	326719.235607	53.698778
3090.791337	326525.438169	53.703783
3090.241497	326334.472805	53.708788
3089.604843	326134.991558	53.713793
3088.779336	325930.193044	53.718797
3088.409692	325734.971325	53.723802
3087.241586	325535.114392	53.728807
3086.871555	325330.395033	53.733812
3086.023113	325143.344065	53.738817
3085.324653	324953.009980	53.743821
3084.945963	324755.113968	53.748826
3084.401430	324562.463160	53.753831
3083.563749	324364.180544	53.758836
3082.764007	324162.046866	53.763841
3081.893026	323966.925705	53.768845
3081.787628	323771.326483	53.773850
3080.794899	323576.478282	53.778855
3080.312705	323377.093156	53.783860
3079.532299	323182.286824	53.788865
3078.730862	322996.012857	53.793869
3078.301408	322796.847165	53.798874
3077.121804	322601.949904	53.803879
3076.679097	322397.642199	53.808884
3076.091301	322208.786572	53.813889
3075.452190	322017.570737	53.818893
3074.869010	321821.100559	53.823898
3073.950751	321624.530193	53.828903
3073.234299	321429.404222	53.833908
3072.776524	321235.968275	53.838913
3071.784762	321057.435132	53.843917
3071.254837	320857.262414	53.848922
3070.642469	320669.094817	53.853927
3069.888884	320476.646111	53.858932
3069.232350	320298.007468	53.863937
3068.689564	320109.140209	53.868941
3068.095645	319913.227659	53.873946
3067.107064	319724.888462	53.878951
3066.747246	319531.306016	53.883956
3065.879918	319340.298771	53.888961
3065.068881	319161.147634	53.893965
3064.721672	318968.656882	53.898970
3064.006734	318778.897473	53.903975
3063.357891	318584.874992	53.908980
3062.723880	318398.030177	53.913985
3062.121528	318203.592149	53.918989
3061.511234	318014.884054	53.923994
3060.574836	317829.562794	53.928999
3060.070724	317633.885841	53.934004
3059.292153	317435.883888	53.939009
3058.444827	317254.392286	53.944013
3058.314321	317066.624898	53.949018
3057.410553	316895.606775	53.954023
3056.965890	316705.749523	53.959028
3056.340512	316529.848745	53.964033
3055.610749	316331.098383	53.969037
3055.144032	316121.687890	53.974042
3054.018462	315939.881393	53.979047
3053.459061	315742.248727	53.984052
3052.917757	315559.457860	53.989057
3052.161926	315363.026839	53.994061
3051.959287	315155.278565	53.999066
3051.137604	314950.785291	54.004071
3050.310104	314756.376041	54.009076
3049.234638	314566.207136	54.014081
3048.492539	314374.864726	54.019085
3048.213402	314185.282070	54.024090
3047.433318	314009.248593	54.029095
3046.897775	313810.207908	54.034100
3046.313280	313624.797670	54.039105
3045.471753	313434.666063	54.044109
3045.293614	313234.600104	54.049114
3044.220355	313045.573954	54.054119
3043.993527	312854.325473	54.059124
3043.175556	312651.864224	54.064129
3042.339733	312456.280693	54.069133
3041.768543	312253.270363	54.074138
3040.744126	312074.165749	54.079143
3040.440680	311877.936717	54.084148
3039.652797	311679.746872	54.089153
3039.108415	311495.421587	54.094157
3038.269016	311298.996245	54.099162
3037.758160	311114.333990	54.104167
3037.219891	310912.563743	54.109172
3036.251225	310720.308535	54.114177
3035.745175	310519.551065	54.119181
3035.344578	310328.656763	54.124186
3034.240815	310141.845894	54.129191
3033.741843	309950.559104	54.134196
3033.148627	309750.094200	54.139201
3032.069881	309554.416751	54.144205
3031.568288	309363.333133	54.149210
3030.832478	309182.192046	54.154215
3030.171500	308984.155711	54.159220
3029.523590	308797.856250	54.164225
3028.488190	308609.071343	54.169229
3028.530064	308409.293074	54.174234
3027.323822	308228.403259	54.179239
3026.907829	308042.600694	54.184244
3026.580441	307851.818153	54.189249
3025.500122	307664.923307	54.194253
3024.890872	307461.706912	54.199258
3024.216648	307276.860813	54.204263
3023.598337	307083.602096	54.209268
3022.865545	306902.380769	54.214273
3021.940366	306708.737141	54.219277
3021.381570	306520.535728	54.224282
3021.006196	306339.435293	54.229287
3020.464772	306148.251149	54.234292
3019.838411	305954.610028	54.239297
3018.965583	305768.698182	54.244301
3018.526516	305573.142416	54.249306
3017.753405	305389.378817	54.254311
3016.888350	305190.452073	54.259316
3016.213373	305001.146393	54.264321
3015.741715	304814.634949	54.269325
3015.119586	304617.145917	54.274330
3014.111281	304437.314491	54.279335
3013.500829	304261.239714	54.284340
3012.996603	304069.868467	54.289345
3012.026204	303884.962647	54.294349
3011.784651	303692.199626	54.299354
3011.062585	303515.021082	54.304359
3010.533696	303321.946514	54.309364
3010.058016	303130.849604	54.314369
3009.182297	302938.084074	54.319373
3008.450647	302739.514713	54.324378
3007.579250	302552.197705	54.329383
3007.136487	302362.316945	54.334388
3006.382423	302175.031819	54.339393
3005.872327	301980.628272	54.344397
3005.172296	301787.145849	54.349402
3004.197603	301605.064558	54.354407
3003.939814	301409.194237	54.359412
3003.048322	301220.223449	54.364417
3002.480065	301036.421849	54.369421
3001.885304	300832.887861	54.374426
3001.169477	300661.485790	54.379431
3000.492167	300470.188227	54.384436
3000.021097	300274.070114	54.389441
2999.210151	300077.216097	54.394445
2998.724864	299890.038473	54.399450
2997.763446	299704.947846	54.404455
2997.123705	299504.042338	54.409460
2996.349246	299318.132224	54.414465
2995.547943	299140.120781	54.419469
2995.260927	298945.703672	54.424474
2994.765640	298761.098483	54.429479
2994.192035	298567.184702	54.434484
2993.285805	298376.073751	54.439489
2992.424372	298185.184700	54.444493
2992.011856	297979.835689	54.449498
2991.061442	297803.374468	54.454503
2990.540279	297610.724663	54.459508
2990.052407	297420.590595	54.464513
2988.872417	297239.606601	54.469517
2988.579884	297037.191670	54.474522
2987.711562	296854.273415	54.479527
2987.171911	296666.336911	54.484532
2986.479498	296484.816597	54.489537
2985.543196	296295.236221	54.494541
2985.251966	296104.101933	54.499546
2984.580803	295922.552251	54.504551
2983.988287	295722.704626	54.509556
2983.182303	295536.158920	54.514561
2982.772898	295355.153020	54.519565
2981.944068	295161.632599	54.524570
2981.220782	294982.815282	54.529575
2980.543915	294789.143114	54.534580
2979.936104	294603.049049	54.539585
2979.204215	294408.290143	54.544589
2978.731483	294217.361051	54.549594
2977.549024	294047.223526	54.554599
2977.115405	293849.360822	54.559604
2976.543064	293658.090453	54.564609
2975.829000	293486.783248	54.569613
2974.987493	293287.965904	54.574618
2974.475487	293112.449782	54.579623
2973.853212	292919.327559	54.584628
2973.390058	292730.942385	54.589633
2972.451824	292548.235087	54.594637
2972.215519	292355.255030	54.599642
2971.357225	292174.979657	54.604647
2970.419777	291994.258261	54.609652
2969.918615	291795.411216	54.614657
2969.230503	291616.993077	54.619661
2968.999465	291414.155496	54.624666
2968.181947	291232.013833	54.629671
2967.680087	291039.915186	54.634676
2966.760887	290844.826343	54.639681
2965.850604	290653.887161	54.644685
2965.345204	290452.671227	54.649690
2964.500730	290276.747250	54.654695
2963.915284	290094.720849	54.659700
2963.886111	289907.487266	54.664705
2962.855614	289712.797216	54.669709
2962.322857	289513.978871	54.674714
2961.311030	289336.399906	54.679719
2960.711428	289146.225442	54.684724
2960.009148	288950.285922	54.689729
2959.247404	288761.257452	54.694733
2958.806371	288569.707715	54.699738
2958.256838	288389.406337	54.704743
2957.581286	288195.219364	54.709748
2956.959927	288004.640123	54.714753
2956.118628	287813.917306	54.719757
2955.596751	287618.203041	54.724762
2954.891130	287431.788056	54.729767
2954.490602	287237.506020	54.734772
2953.761050	287052.699085	54.739777
2952.922120	286857.161892	54.744781
2952.409883	286658.211102	54.749786
2951.479988	286476.364382	54.754791
2950.861694	286285.605384	54.759796
2950.357110	286090.829809	54.764801
2949.639515	285896.138785	54.769805
2948.973438	285704.062710	54.774810
2947.896692	285521.041761	54.779815
2947.347829	285324.057075	54.784820
2946.862386	285138.115387	54.789825
2946.575256	284955.453067	54.794829
2945.890962	284746.264859	54.799834
2945.095792	284562.027362	54.804839
2944.229477	284375.941874	54.809844
2943.997466	284177.836814	54.814849
2943.086222	283986.741053	54.819853
2942.519542	283783.391425	54.824858
2941.599397	283598.867688	54.829863
2941.085325	283406.562742	54.834868
2940.548518	283213.420868	54.839873
2939.697592	283025.498685	54.844877
2939.110062	282820.369173	54.849882
2938.813127	282632.435548	54.854887
2937.714969	282434.110323	54.859892
2937.032233	282241.551483	54.864897
2936.375914	282052.452073	54.869901
2935.504627	281861.400109	54.874906
2935.040535	281670.920325	54.879911
2934.423583	281475.753053	54.884916
2934.132949	281285.856926	54.889921
2933.148066	281092.403217	54.894925
2932.812334	280897.751549	54.899930
2931.989022	280692.021905	54.904935
2931.011880	280515.223061	54.909940
2930.872172	280305.233753	54.914945
2929.749014	280107.726733	54.919949
2929.301810	279908.711896	54.924954
2928.343672	279729.617713	54.929959
2927.686865	279539.448005	54.934964
2927.533846	279333.255328	54.939969
2926.555471	279150.191170	54.944973
2925.843827	278942.940767	54.949978
2925.315062	278745.925111	54.954983
2924.248508	278545.276178	54.959988
2923.835941	278344.854762	54.964993
2923.248635	278159.054343	54.969997
2922.536994	277959.393323	54.975002
2921.699916	277773.377706	54.980007
2921.095902	277575.737059	54.985012
2920.532150	277382.623383	54.990017
2919.907614	277197.185286	54.995021
2919.284816	276999.038174	55.000026
2918.732616	276811.118153	55.005031
2917.897877	276613.412049	55.010036
2917.416709	276416.796031	55.015041
2916.726761	276220.238518	55.020045
2915.899832	276013.871882	55.025050
2915.129682	275829.220778	55.030055
2914.423961	275635.161631	55.035060
2914.099621	275440.991161	55.040065
2913.122217	275261.670274	55.045069
2912.878219	275051.620267	55.050074
2912.041465	274870.265104	55.055079
2911.301702	274663.553536	55.060084
2910.666919	274471.673422	55.065089
2909.855912	274278.420448	55.070093
2909.358096	274089.447522	55.075098
2908.513209	273899.663625	55.080103
2907.738660	273709.155486	55.085108
2907.595465	273515.236511	55.090113
2906.694977	273317.107816	55.095117
2906.278288	273119.895808	55.100122
2905.462535	272934.513388	55.105127
2904.731122	272727.189357	55.110132
2904.269574	272528.660149	55.115137
2903.264579	272349.063598	55.120141
2902.536574	272141.637223	55.125146
2901.606076	271961.952516	55.130151
2901.017514	271768.791869	55.135156
2900.727359	271578.334589	55.140161
2899.885431	271388.575935	55.145165
2899.477549	271189.401708	55.150170
2898.655657	270999.538073	55.155175
2897.693151	270813.593390	55.160180
2897.515766	270612.294374	55.165185
2896.896622	270426.448211	55.170189
2896.342570	270220.726486	55.175194
2895.297343	270036.679709	55.180199
2894.809486	269832.093669	55.185204
2894.395261	269636.893829	55.190209
2893.099924	269455.764700	55.195213
2892.773704	269255.737513	55.200218
2892.298313	269068.187991	55.205223
2891.532712	268865.556307	55.210228
2890.886805	268675.588932	55.215233
2890.363360	268478.343767	55.220237
2889.847515	268272.107163	55.225242
2889.067523	268084.376931	55.230247
2888.365625	267881.633598	55.235252
2887.804503	267687.323499	55.240257
2887.078823	267490.390825	55.245261
2886.408157	267282.549114	55.250266
2885.635116	267091.252557	55.255271
2884.889479	266889.306024	55.260276
2884.271431	266681.125133	55.265281
2883.744765	266492.591290	55.270285
2883.023216	266293.850173	55.275290
2882.268564	266108.739843	55.280295
2881.455827	265912.127181	55.285300
2881.196809	265708.601472	55.290305
2880.305517	265517.018642	55.295309
2879.390398	265321.237429	55.300314
2878.697164	265124.988216	55.305319
2877.865269	264927.207496	55.310324
2877.261569	264727.582507	55.315329
2876.683436	264548.429890	55.320333
2876.331467	264359.792898	55.325338
2875.548499	264166.639992	55.330343
2875.242963	263975.678243	55.335348
2874.598195	263770.279004	55.340353
2873.486324	263573.511084	55.345357
2872.977849	263383.320346	55.350362
2872.373967	263182.753882	55.355367
2871.743165	262987.081643	55.360372
2870.979126	262790.488297	55.365377
2870.053043	262601.357356	55.370381
2869.806057	262403.587247	55.375386
2868.994152	262210.261714	55.380391
2867.918981	262025.356915	55.385396
2867.446741	261829.431041	55.390401
2866.648057	261638.141191	55.395405
2866.347715	261448.173284	55.400410
2865.548900	261257.724129	55.405415
2864.993051	261063.798471	55.410420
2864.347996	260858.299222	55.415425
2863.693784	260671.087424	55.420429
2863.159409	260477.387964	55.425434
2862.425794	260285.171844	55.430439
2861.618721	260090.904602	55.435444
2861.233629	259891.451672	55.440449
2860.472573	259701.787071	55.445453
2859.826668	259495.728663	55.450458
2859.018791	259307.115929	55.455463
2858.807547	259110.030011	55.460468
2857.961000	258905.710165	55.465473
2857.018279	258714.241373	55.470477
2856.885896	258511.031207	55.475482
2855.806487	258313.828693	55.480487
2855.003791	258118.670859	55.485492
2854.580531	257917.264496	55.490497
2853.909324	257722.519107	55.495501
2853.567564	257522.322609	55.500506
2852.667523	257333.624094	55.505511
2851.746176	257126.210552	55.510516
2851.451744	256921.066396	55.515521
2850.677373	256726.490977	55.520525
2850.291440	256518.305589	55.525530
2849.507907	256325.030804	55.530535
2848.518340	256130.973858	55.535540
2848.182231	255922.246329	55.540545
2847.773654	255731.383022	55.545549
2847.209268	255521.571468	55.550554
2846.284180	255313.599942	55.555559
2845.816891	255106.549352	55.560564
2845.163649	254904.188903	55.565569
2844.278669	254699.700643	55.570573
2844.098962	254489.523615	55.575578
2843.410105	254284.469910	55.580583
2842.425486	254073.554893	55.585588
2841.628154	253860.343881	55.590593
2840.797339	253659.464431	55.595597
2840.746108	253457.392132	55.600602
2839.677972	253253.418248	55.605607
2839.177349	253041.510909	55.610612
2838.709395	252829.853305	55.615617
2837.780507	252639.712027	55.620621
2836.831389	252427.341602	55.625626
2836.121098	252213.278265	55.630631
2835.445492	252017.189231	55.635636
2835.013128	251817.114548	55.640641
2834.189004	251621.915336	55.645645
2833.590015	251411.757210	55.650650
2833.069230	251205.890818	55.655655
2832.325110	251006.604960	55.660660
2831.879918	250807.730397	55.665665
2831.183516	250606.043590	55.670669
2830.594345	250396.776482	55.675674
2829.740562	250183.604229	55.680679
2828.838627	249972.884658	55.685684
2828.265927	249777.087487	55.690689
2827.243763	249571.633557	55.695693
2826.845007	249379.247287	55.700698
2826.240182	249174.848296	55.705703
2825.319009	248966.246789	55.710708
2824.961056	248775.637427	55.715713
2824.246851	248577.699499	55.720717
2823.506641	248374.468967	55.725722
2822.971167	248170.162168	55.730727
2821.985031	247970.001590	55.735732
2821.357202	247775.947336	55.740737
2820.938318	247575.060798	55.745741
2820.420104	247371.694587	55.750746
2819.430483	247180.626991	55.755751
2818.762349	246979.042214	55.760756
2818.491822	246778.769910	55.765761
2817.388867	246586.320409	55.770765
2816.555827	246377.759452	55.775770
2815.813312	246176.213035	55.780775
2815.252535	245973.161106	55.785780
2814.590053	245779.420579	55.790785
2813.778677	245599.760983	55.795789
2813.227522	245402.921992	55.800794
2812.629341	245204.944773	55.805799
2812.011515	245018.481412	55.810804
2811.591804	244813.244256	55.815809
2810.626338	244620.317300	55.820813
2810.166256	244435.968863	55.825818
2809.608665	244233.173645	55.830823
2808.847968	244030.920208	55.835828
2808.285259	243833.372291	55.840833
2807.623470	243643.683693	55.845837
2807.264540	243436.401797	55.850842
2806.427254	243234.390903	55.855847
2805.438006	243036.020455	55.860852
2805.226790	242837.221520	55.865857
2804.356282	242637.101251	55.870861
2803.536956	242434.350285	55.875866
2803.105712	242244.754567	55.880871
2802.397726	242038.243239	55.885876
2801.873498	241830.913738	55.890881
2800.974116	241646.256883	55.895885
2800.357595	241435.886864	55.900890
2799.559630	241238.583961	55.905895
2798.998852	241042.593452	55.910900
2798.632578	240837.048623	55.915905
2797.821507	240638.220887	55.920909
2797.046873	240430.144021	55.925914
2796.502926	240227.556819	55.930919
2795.631893	240022.042404	55.935924
2795.039413	239825.651483	55.940929
2794.442055	239644.209350	55.945933
2793.588755	239429.475006	55.950938
2793.118807	239231.868854	55.955943
2792.597048	239035.977361	55.960948
2792.258129	238835.600986	55.965953
2791.088252	238636.044098	55.970957
2790.511442	238434.203713	55.975962
2789.989670	238219.470077	55.980967
2789.516102	238019.192871	55.985972
2788.669158	237815.028217	55.990977
2787.927724	237624.725158	55.995981
2787.292101	237407.541111	56.000986
2786.590226	237203.889365	56.005991
2785.771376	237001.249620	56.010996
2785.304819	236799.191059	56.016001
2784.429186	236604.556715	56.021005
2783.998925	236402.900575	56.026010
2783.154221	236202.329003	56.031015
2782.654098	235995.133605	56.036020
2782.016544	235784.701032	56.041025
2781.185053	235596.860347	56.046029
2780.885445	235386.706082	56.051034
2780.018615	235183.822784	56.056039
2779.193812	234990.278316	56.061044
2778.901930	234785.420451	56.066049
2778.041291	234587.655496	56.071053
2777.480344	234380.141944	56.076058
2776.771741	234171.048019	56.081063
2776.063155	233975.781043	56.086068
2775.498679	233766.079483	56.091073
2774.780873	233571.578652	56.096077
2774.047666	233357.626878	56.101082
2773.818347	233149.885121	56.106087
2772.765935	232953.885262	56.111092
2772.193996	232737.897727	56.116097
2771.461046	232540.574962	56.121101
2770.840513	232329.001104	56.126106
2770.175446	232129.529556	56.131111
2769.187053	231929.091126	56.136116
2768.905117	231726.835234	56.141121
2768.329988	231528.929382	56.146125
2767.826384	231312.017590	56.151130
2766.659588	231101.882495	56.156135
2765.729514	230907.522524	56.161140
2765.130137	230697.298474	56.166145
2764.480207	230510.813750	56.171149
2763.908158	230301.986697	56.176154
2763.295273	230099.659438	56.181159
2762.807716	229903.780154	56.186164
2762.554000	229698.443296	56.191169
2761.449032	229501.058559	56.196173
2760.636606	229283.309294	56.201178
2760.110131	229087.896258	56.206183
2759.285916	228883.619169	56.211188
2758.994794	228682.746377	56.216193
2758.147568	228486.290610	56.221197
2757.376736	228279.180211	56.226202
2756.877117	228080.225977	56.231207
2755.990648	227877.183237	56.236212
2755.618719	227668.508875	56.241217
2755.001073	227469.065503	56.246221
2754.330909	227257.333077	56.251226
2753.881344	227051.778788	56.256231
2752.677889	226854.619297	56.261236
2752.464930	226645.463940	56.266241
2751.899309	226442.730231	56.271245
2751.475176	226234.525935	56.276250
2750.345168	226021.761867	56.281255
2749.609553	225823.041221	56.286260
2748.961233	225613.499089	56.291265
2748.481193	225415.146311	56.296269
2747.373540	225202.533564	56.301274
2746.814918	225002.450165	56.306279
2746.367173	224799.854554	56.311284
2745.726704	224590.402895	56.316289
2744.694302	224384.616510	56.321293
2744.432065	224180.949179	56.326298
2743.896084	223978.675118	56.331303
2742.888957	223773.000863	56.336308
2742.304578	223570.455435	56.341313
2741.442020	223373.517626	56.346317
2740.822703	223164.779218	56.351322
2740.089898	222959.381870	56.356327
2739.339812	222765.075604	56.361332
2739.044558	222566.789685	56.366337
2738.057438	222366.729827	56.371341
2737.860997	222154.630079	56.376346
2737.026641	221960.313707	56.381351
2736.289300	221759.312035	56.386356
2735.525565	221552.382991	56.391361
2734.881912	221349.114382	56.396365
2734.136419	221142.870963	56.401370
2733.784474	220943.057903	56.406375
2733.192048	220735.798430	56.411380
2732.425354	220541.564059	56.416385
2731.601006	220344.729759	56.421389
2730.934155	220132.608308	56.426394
2730.572681	219933.410456	56.431399
2729.704323	219734.077024	56.436404
2729.382086	219517.587451	56.441409
2728.564742	219317.725154	56.446413
2727.887539	219110.623652	56.451418
2727.285351	218905.623922	56.456423
2726.304957	218699.933646	56.461428
2725.911722	218493.527214	56.466433
2725.069330	218295.797468	56.471437
2724.478848	218088.812431	56.476442
2723.978489	217882.424713	56.481447
2723.168202	217683.253171	56.486452
2722.439237	217471.594808	56.491457
2721.939276	217265.246997	56.496461
2720.916668	217058.167916	56.501466
2720.411707	216862.552619	56.506471
2719.317435	216665.312807	56.511476
2719.286788	216460.000427	56.516481
2718.252591	216258.564438	56.521485
2717.606712	216046.248025	56.526490
2717.070342	215852.957171	56.531495
2716.127355	215655.518051	56.536500
2715.946291	215442.226122	56.541505
2715.169808	215248.542219	56.546509
2714.438468	215033.645811	56.551514
2714.082699	214834.079456	56.556519
2713.210850	214628.282071	56.561524
2712.547776	214426.970863	56.566529
2711.733094	214224.525979	56.571533
2711.435393	214014.362746	56.576538
2710.796922	213805.985214	56.581543
2709.572614	213607.145573	56.586548
2709.038281	213398.880098	56.591553
2708.266867	213201.993731	56.596557
2707.689972	212998.471177	56.601562
2707.116398	212806.276828	56.606567
2706.315551	212610.606067	56.611572
2705.822813	212399.727879	56.616577
2705.047588	212205.505276	56.621581
2704.552457	212002.036501	56.626586
2703.905128	211795.194093	56.631591
2703.022722	211604.885036	56.636596
2702.714561	211399.924817	56.641601
2702.190715	211188.406368	56.646605
2701.215570	210985.793235	56.651610
2700.997873	210777.116870	56.656615
2699.957519	210579.606480	56.661620
2699.446755	210365.899507	56.666625
2698.550850	210164.651032	56.671629
2698.188272	209947.192788	56.676634
2697.339267	209749.743773	56.681639
2696.418197	209548.284887	56.686644
2696.233515	209340.549877	56.691649
2695.281221	209139.873634	56.696653
2694.460884	208936.758923	56.701658
2694.302652	208729.836320	56.706663
2693.512429	208535.194602	56.711668
2692.987295	208313.122332	56.716673
2692.100120	208121.997291	56.721677
2691.437797	207904.657323	56.726682
2690.917159	207704.719194	56.731687
2689.976905	207502.850035	56.736692
2689.600436	207283.850655	56.741697
2688.778030	207083.936924	56.746701
2688.185391	206872.991323	56.751706
2687.488786	206667.382803	56.756711
2686.627331	206475.088009	56.761716
2686.354555	206256.852288	56.766721
2685.174047	206058.080496	56.771725
2684.636793	205860.098344	56.776730
2684.111896	205653.460708	56.781735
2683.148381	205449.820422	56.786740
2682.573224	205243.879426	56.791745
2682.320971	205042.991373	56.796749
2681.363738	204836.145116	56.801754
2680.502882	204635.469416	56.806759
2679.898944	204435.428212	56.811764
2679.480801	204224.922587	56.816769
2678.835794	204029.890780	56.821773
2678.224042	203818.437376	56.826778
2677.745141	203613.848632	56.831783
2676.870746	203415.495506	56.836788
2676.042460	203205.771258	56.841793
2675.430860	203005.430816	56.846797
2674.792364	202793.654560	56.851802
2674.229319	202602.763354	56.856807
2673.349610	202399.298737	56.861812
2673.220640	202185.216987	56.866817
2672.361609	201983.761301	56.871821
2671.311529	201774.981044	56.876826
2670.844111	201566.249245	56.881831
2669.993754	201369.286624	56.886836
2669.736127	201164.022692	56.891841
2669.227536	200960.466345	56.896845
2668.291048	200748.770490	56.901850
2667.719417	200537.615751	56.906855
2666.813797	200336.389766	56.911860
2666.818065	200123.554690	56.916865
2665.819425	199921.174223	56.921869
2664.984849	199707.277471	56.926874
2664.542263	199494.922855	56.931879
2663.434442	199295.145267	56.936884
2663.049771	199082.452236	56.941889
2662.376478	198875.099459	56.946893
2661.924000	198662.660610	56.951898
2661.406715	198455.361090	56.956903
2660.323371	198259.413737	56.961908
2659.777466	198040.158803	56.966913
2658.846806	197844.277865	56.971917
2658.319146	197630.086272	56.976922
2657.781920	197417.818517	56.981927
2657.106539	197218.081997	56.986932
2656.499323	197010.013440	56.991937
2655.943264	196803.031929	56.996941
2655.482750	196587.726893	57.001946
2654.937166	196378.085952	57.006951
2653.838665	196173.763249	57.011956
2653.417090	195954.802714	57.016961
2652.618371	195746.451431	57.021965
2651.884581	195539.070483	57.026970
2651.440705	195323.106398	57.031975
2650.515950	195125.300640	57.036980
2650.094376	194908.876692	57.041985
2649.018942	194699.224732	57.046989
2648.618944	194493.500180	57.051994
2648.078568	194281.054931	57.056999
2647.432114	194082.852859	57.062004
2646.738938	193863.028181	57.067009
2645.936556	193653.388187	57.072013
2645.272248	193448.307791	57.077018
2644.664148	193237.913491	57.082023
2643.794781	193027.943183	57.087028
2643.053669	192805.344232	57.092033
2642.843053	192602.536593	57.097037
2641.874825	192395.269314	57.102042
2641.278859	192192.295382	57.107047
2640.550593	191980.436789	57.112052
2639.895259	191761.811399	57.117057
2638.844279	191563.034551	57.122061
2638.219439	191368.631442	57.127066
2637.627270	191150.507707	57.132071
2636.920987	190957.556871	57.137076
2636.471994	190749.450888	57.142081
2635.688076	190546.526284	57.147085
2635.128478	190341.938436	57.152090
2634.569998	190136.918695	57.157095
2633.745872	189942.133017	57.162100
2633.211236	189732.429168	57.167105
2632.723528	189518.889218	57.172109
2631.786953	189321.630198	57.177114
2631.169829	189105.542594	57.182119
2630.472757	188900.588275	57.187124
2630.299481	188694.686711	57.192129
2629.469649	188487.223407	57.197133
2628.752126	188288.127369	57.202138
2628.267948	188064.873387	57.207143
2627.271083	187859.703912	57.212148
2626.695246	187645.219471	57.217153
2625.945989	187445.203304	57.222157
2624.943953	187237.213028	57.227162
2624.836796	187027.326233	57.232167
2623.950292	186817.792866	57.237172
2623.324822	186611.908489	57.242177
2622.551832	186402.002801	57.247181
2621.880866	186205.350911	57.252186
2621.155110	185993.035151	57.257191
2620.530971	185804.646795	57.262196
2619.895158	185582.408364	57.267201
2619.457784	185373.789990	57.272205
2618.710284	185175.589874	57.277210
2617.818289	184965.022658	57.282215
2617.442711	184763.356018	57.287220
2617.013123	184552.386693	57.292225
2616.165045	184353.239275	57.297229
2615.737689	184137.640928	57.302234
2615.316859	183935.412695	57.307239
2614.105295	183719.457200	57.312244
2613.602977	183509.343895	57.317249
2612.947754	183302.754122	57.322253
2612.178761	183088.792380	57.327258
2611.676430	182882.485639	57.332263
2610.981594	182663.654764	57.337268
2610.318352	182443.471550	57.342273
2609.758425	182237.711219	57.347277
2608.774633	182033.100277	57.352282
2608.204024	181817.141538	57.357287
2607.462209	181621.131547	57.362292
2607.076764	181397.398655	57.367297
2606.588222	181185.322535	57.372301
2605.597236	180990.397943	57.377306
2605.075006	180767.783920	57.382311
2604.086125	180554.607161	57.387316
2603.412302	180344.866891	57.392321
2602.654277	180150.214457	57.397325
2601.885084	179940.440387	57.402330
2601.614347	179733.997348	57.407335
2600.874919	179530.669661	57.412340
2599.890259	179319.953324	57.417345
2599.474349	179111.005017	57.422349
2598.863273	178911.819356	57.427354
2598.274602	178697.545390	57.432359
2597.255562	178490.565513	57.437364
2596.772976	178281.479216	57.442369
2596.075363	178076.434705	57.447373
2595.100292	177884.561738	57.452378
2594.894149	177661.977422	57.457383
2594.000495	177466.163144	57.462388
2593.663442	177258.432573	57.467393
2592.951151	177058.063373	57.472397
2592.329911	176847.314526	57.477402
2591.910538	176647.435095	57.482407
2590.789999	176441.626151	57.487412
2590.400482	176216.000582	57.492417
2589.486174	176011.318533	57.497421
2589.068198	175814.368272	57.502426
2588.259489	175590.466009	57.507431
2587.381585	175388.464969	57.512436
2586.931875	175181.169675	57.517441
2586.540455	174973.535511	57.522445
2585.521068	174769.130684	57.527450
2585.036065	174553.742422	57.532455
2584.103249	174358.317946	57.537460
2583.626534	174149.862081	57.542465
2583.129911	173938.269013	57.547469
2581.989437	173747.090166	57.552474
2581.614595	173528.192377	57.557479
2580.776387	173323.308290	57.562484
2580.344644	173117.114467	57.567489
2579.706513	172912.595034	57.572493
2579.027083	172707.192935	57.577498
2578.509440	172488.526940	57.582503
2577.681530	172290.069047	57.587508
2577.227174	172074.803673	57.592513
2576.655191	171871.881539	57.597517
2575.767010	171662.346520	57.602522
2574.884303	171445.155783	57.607527
2574.288698	171246.628159	57.612532
2573.710461	171040.010507	57.617537
2572.979457	170831.129029	57.622541
2572.507563	170623.619222	57.627546
2571.966018	170415.460259	57.632551
2570.951638	170208.699917	57.637556
2570.337770	169990.126629	57.642561
2569.541419	169799.866109	57.647565
2568.819890	169593.634899	57.652570
2568.608316	169395.729832	57.657575
2567.847927	169178.646781	57.662580
2567.090358	168968.609576	57.667585
2566.531244	168765.752421	57.672589
2565.930228	168561.046353	57.677594
2565.442022	168348.146770	57.682599
2564.407852	168145.075700	57.687604
2563.825502	167925.301068	57.692609
2563.255276	167719.831643	57.697613
2562.405545	167513.148711	57.702618
2561.933064	167297.810983	57.707623
2561.166709	167101.150153	57.712628
2560.473558	166890.961587	57.717633
2559.815329	166674.359808	57.722637
2559.155420	166477.901530	57.727642
2558.613222	166268.328312	57.732647
2557.778932	166065.948813	57.737652
2557.203316	165851.106182	57.742657
2556.532384	165643.731244	57.747661
2555.933411	165421.570587	57.752666
2555.410493	165175.901022	57.757671
2554.501158	164971.670181	57.762676
2554.368100	164749.096394	57.767681
2553.324297	164541.303518	57.772685
2552.454252	164334.107319	57.777690
2552.091774	164123.678503	57.782695
2551.383252	163916.141182	57.787700
2550.751283	163695.649077	57.792705
2550.047244	163489.499389	57.797709
2549.312321	163292.459561	57.802714
2548.644441	163083.051443	57.807719
2547.899594	162874.050881	57.812724
2547.495680	162656.071847	57.817729
2546.731768	162455.239482	57.822733
2546.024967	162248.919253	57.827738
2545.482846	162026.147134	57.832743
2544.766812	161830.688829	57.837748
2544.052026	161615.130192	57.842753
2543.508571	161403.817649	57.847757
2542.737305	161201.607589	57.852762
2542.179458	160980.077706	57.857767
2541.262742	160782.800667	57.862772
2540.723255	160556.706198	57.867777
2540.082367	160354.225995	57.872781
2539.119461	160148.441560	57.877786
2538.750360	159938.076301	57.882791
2537.729123	159740.287638	57.887796
2537.148091	159519.380776	57.892801
2536.935135	159319.305081	57.897805
2535.874871	159126.026591	57.902810
2535.680998	158904.579116	57.907815
2534.532220	158700.332745	57.912820
2534.115793	158493.238181	57.917825
2533.568785	158280.482813	57.922829
2532.824876	158075.247875	57.927834
2532.434142	157865.038290	57.932839
2531.473766	157665.573580	57.937844
2530.941160	157438.557307	57.942849
2530.367431	157229.257746	57.947853
2529.247033	157027.317679	57.952858
2528.809253	156809.901205	57.957863
2528.051904	156611.262132	57.962868
2527.586176	156399.141043	57.967873
2527.037053	156182.737736	57.972877
2526.028807	155989.926097	57.977882
2525.881784	155771.020921	57.982887
2525.010079	155566.049971	57.987892
2524.534084	155345.013193	57.992897
2523.800726	155130.171180	57.997901
2522.863706	154924.324613	58.002906
2522.321712	154705.323627	58.007911
2521.449569	154502.316763	58.012916
2521.042204	154280.322666	58.017921
2520.227942	154079.444710	58.022925
2519.434049	153864.671169	58.027930
2519.161646	153661.790406	58.032935
2518.006775	153446.936920	58.037940
2517.428147	153240.776892	58.042945
2517.104437	153036.509815	58.047949
2516.233936	152827.309802	58.052954
2515.740344	152614.161825	58.057959
2514.898824	152405.658967	58.062964
2514.468645	152191.270696	58.067969
2513.661292	151980.629684	58.072973
2512.871828	151779.316755	58.077978
2512.633396	151562.677806	58.082983
2511.769359	151355.672257	58.087988
2511.024889	151134.565987	58.092993
2510.520892	150922.777846	58.097997
2509.482548	150729.327593	58.103002
2509.185449	150514.929123	58.108007
2508.271094	150305.078397	58.113012
2507.694534	150099.636673	58.118017
2507.010121	149888.684544	58.123021
2506.004330	149681.127392	58.128026
2505.580767	149463.057329	58.133031
2504.842986	149251.977984	58.138036
2503.881898	149042.028428	58.143041
2503.309990	148838.996041	58.148045
2502.490556	148635.483079	58.153050
2502.167032	148429.134885	58.158055
2501.243458	148232.084589	58.163060
2500.633812	148015.922045	58.168065
2500.261454	147811.987579	58.173069
2499.319349	147623.573405	58.178074
2499.055650	147416.396157	58.183079
2498.107117	147208.223130	58.188084
2497.599390	147002.815643	58.193089
2497.106934	146797.508730	58.198093
2496.157897	146596.405794	58.203098
2495.925660	146387.412930	58.208103
2494.803239	146185.297990	58.213108
2494.360168	145971.118140	58.218113
2493.766896	145760.979349	58.223117
2492.847352	145556.675880	58.228122
2492.279517	145351.962167	58.233127
2491.714362	145152.612131	58.238132
2491.017755	144937.691604	58.243137
2490.270023	144726.148226	58.248141
2489.732681	144525.488870	58.253146
2489.461411	144324.178663	58.258151
2488.469732	144112.436665	58.263156
2487.837057	143890.473228	58.268161
2487.090041	143690.437030	58.273165
2486.270606	143486.487044	58.278170
2485.962970	143283.156177	58.283175
2485.182651	143071.438615	58.288180
2484.378426	142859.535690	58.293185
2483.881478	142660.508499	58.298189
2482.739814	142451.317625	58.303194
2482.483012	142239.421150	58.308199
2481.492985	142047.248808	58.313204
2480.944638	141836.964252	58.318209
2480.565478	141629.017740	58.323213
2479.314408	141414.870330	58.328218
2478.954468	141212.971878	58.333223
2478.276807	141013.424963	58.338228
2477.671088	140809.103131	58.343233
2476.831108	140603.117189	58.348237
2476.506336	140401.942802	58.353242
2475.791693	140194.415051	58.358247
2474.897575	139995.137861	58.363252
2474.655131	139777.220981	58.368257
2473.871134	139573.088233	58.373261
2473.187117	139375.687692	58.378266
2472.529387	139161.068324	58.383271
2472.086460	138958.130835	58.388276
2471.316059	138747.864835	58.393281
2470.834261	138539.168133	58.398285
2469.944746	138327.958374	58.403290
2469.504688	138108.763620	58.408295
2468.547354	137913.690269	58.413300
2468.004611	137699.418930	58.418305
2467.447966	137484.871837	58.423309
2466.532521	137278.463360	58.428314
2465.962684	137071.988839	58.433319
2465.297243	136863.472784	58.438324
2464.361328	136657.973915	58.443329
2464.067814	136441.525146	58.448333
2463.210883	136241.924184	58.453338
2462.636484	136032.345140	58.458343
2461.856965	135840.395253	58.463348
2461.117232	135623.324533	58.468353
2460.636277	135412.172533	58.473357
2460.176337	135216.263292	58.478362
2459.784957	135001.225409	58.483367
2458.700880	134796.182336	58.488372
2457.861546	134582.539738	58.493377
2457.477209	134373.793634	58.498381
2456.685086	134166.472934	58.503386
2456.350179	133948.753502	58.508391
2455.423052	133745.750923	58.513396
2454.943059	133544.482733	58.518401
2454.319163	133323.345898	58.523405
2453.567632	133114.819552	58.528410
2452.607821	132904.879620	58.533415
2451.907940	132696.576781	58.538420
2451.680398	132486.320599	58.543425
2450.755053	132280.050846	58.548429
2449.933474	132067.846810	58.553434
2449.438297	131866.402294	58.558439
2448.637604	131655.836623	58.563444
2447.950322	131460.497106	58.568449
2447.260899	131237.024232	58.573453
2446.429772	131031.167784	58.578458
2445.913509	130827.803297	58.583463
2445.181534	130627.395877	58.588468
2444.651603	130413.367059	58.593473
2444.056011	130214.719192	58.598477
2443.350455	130010.082355	58.603482
2442.850311	129798.009532	58.608487
2442.021710	129592.772879	58.613492
2441.347869	129387.805326	58.618497
2440.875062	129177.638055	58.623501
2440.239007	128971.918201	58.628506
2439.517288	128762.936607	58.633511
2438.695837	128559.459152	58.638516
2438.129786	128349.998757	58.643521
2437.459690	128140.023010	58.648525
2436.698293	127940.350772	58.653530
2436.495612	127727.014620	58.658535
2435.486403	127519.345324	58.663540
2434.808688	127312.780767	58.668545
2434.391292	127104.690573	58.673549
2433.572180	126899.612052	58.678554
2433.040264	126681.154565	58.683559
2432.236874	126486.160419	58.688564
2431.791439	126268.479905	58.693569
2431.306848	126049.880254	58.698573
2430.124063	125849.845525	58.703578
2429.692496	125625.602254	58.708583
2429.097366	125428.271346	58.713588
2428.385175	125220.661304	58.718593
2427.891484	125003.950989	58.723597
2427.320849	124795.255029	58.728602
2426.573760	124577.153303	58.733607
2425.598392	124376.715584	58.738612
2425.025404	124158.424554	58.743617
2424.398966	123942.048568	58.748621
2423.411396	123741.300044	58.753626
2423.455112	123513.659202	58.758631
2422.469512	123311.821507	58.763636
2421.707093	123103.194460	58.768641
2420.793511	122885.767762	58.773645
2420.136204	122679.806673	58.778650
2419.497816	122473.425141	58.783655
2419.003632	122270.082538	58.788660
2418.257546	122061.219789	58.793665
2417.970959	121843.308566	58.798669
2416.963329	121642.921839	58.803674
2416.495410	121429.296459	58.808679
2415.686055	121221.567733	58.813684
2415.225220	121007.258980	58.818689
2414.521633	120795.542585	58.823693
2413.797847	120595.613994	58.828698
2413.055396	120378.790184	58.833703
2412.303023	120168.851447	58.838708
2411.731441	119954.822757	58.843713
2411.224476	119743.921651	58.848717
2410.724685	119540.981862	58.853722
2409.930177	119335.297146	58.858727
2409.237107	119118.368022	58.863732
2408.369659	118906.502420	58.868737
2407.822538	118688.703086	58.873741
2406.881003	118484.318017	58.878746
2406.765980	118276.965976	58.883751
2406.030589	118070.856571	58.888756
2404.965070	117858.580223	58.893761
2404.757494	117642.754469	58.898765
2403.813258	117438.111482	58.903770
2403.213417	117219.285483	58.908775
2402.941907	117007.474247	58.913780
2402.219088	116801.182563	58.918785
2401.365312	116583.119518	58.923789
2400.438340	116370.560531	58.928794
2400.123186	116160.889617	58.933799
2399.058323	115950.215791	58.938804
2398.531571	115746.808630	58.943809
2398.082714	115518.871102	58.948813
2397.241375	115323.425935	58.953818
2396.461407	115102.139431	58.958823
2396.114267	114897.663292	58.963828
2395.467757	114687.504836	58.968833
2395.116231	114477.758342	58.973837
2394.485480	114263.183368	58.978842
2393.674095	114028.671408	58.983847
2392.867817	113816.546239	58.988852
2391.905246	113599.687520	58.993857
2391.636594	113379.839222	58.998861
2390.444355	113183.476141	59.003866
2389.981186	112960.971341	59.008871
2389.512235	112745.349152	59.013876
2389.111235	112532.802470	59.018881
2388.310249	112322.751721	59.023885
2387.763241	112109.971580	59.028890
2387.327053	111889.268083	59.033895
2386.586813	111676.287466	59.038900
2385.778550	111458.470902	59.043905
2385.426342	111230.994802	59.048909
2384.119008	111019.029938	59.053914
2383.462073	110790.279850	59.058919
2382.958101	110575.069135	59.063924
2382.464181	110361.572121	59.068929
2381.884332	110143.394582	59.073933
2380.955328	109929.779912	59.078938
2380.293136	109705.260737	59.083943
2379.450675	109496.046468	59.088948
2378.700342	109287.777581	59.093953
2378.192586	109067.675414	59.098957
2377.368332	108862.892940	59.103962
2376.780867	108638.733392	59.108967
2376.261110	108430.555815	59.113972
2375.447599	108214.539208	59.118977
2375.111472	107999.146820	59.123981
2374.209503	107791.707919	59.128986
2373.806684	107571.983341	59.133991
2373.142518	107356.800950	59.138996
2372.279769	107143.282664	59.144001
2371.487325	106920.484921	59.149005
2370.798660	106711.079861	59.154010
2370.468583	106494.703723	59.159015
2369.647272	106278.654868	59.164020
2368.854193	106061.867472	59.169025
2368.443944	105850.300223	59.174029
2367.741122	105639.168259	59.179034
2367.272421	105416.434633	59.184039
2366.679800	105208.962574	59.189044
2365.692292	104992.609050	59.194049
2365.198193	104772.619971	59.199053
2364.407692	104549.469614	59.204058
2363.685676	104333.587536	59.209063
2363.006717	104116.457097	59.214068
2362.398706	103904.741773	59.219073
2361.805987	103693.070324	59.224077
2360.920582	103482.030841	59.229082
2360.321879	103262.503742	59.234087
2359.836088	103045.022603	59.239092
2358.983763	102839.712312	59.244097
2358.688618	102609.992726	59.249101
2357.995414	102396.934129	59.254106
2357.376065	102171.082918	59.259111
2356.769795	101955.527758	59.264116
2355.947120	101742.337038	59.269121
2355.588614	101520.199877	59.274125
2354.384245	101302.664843	59.279130
2353.707187	101070.204340	59.284135
2353.314576	100855.849742	59.289140
2352.324940	100651.690513	59.294145
2352.080962	100426.018668	59.299149
2351.457119	100208.287629	59.304154
2350.911612	99989.157041	59.309159
2350.190679	99765.508278	59.314164
2349.310177	99547.189830	59.319169
2348.794550	99324.825801	59.324173
2347.939358	99112.704619	59.329178
2347.395801	98892.531179	59.334183
2346.668755	98669.401441	59.339188
2345.855707	98451.780389	59.344193
2345.284673	98235.626258	59.349197
2344.731206	98021.082425	59.354202
2344.224572	97798.928347	59.359207
2343.370267	97574.859012	59.364212
2342.862791	97365.280274	59.369217
2342.676821	97138.312194	59.374221
2340.919083	96922.193749	59.379226
2340.673731	96699.913799	59.384231
2340.255486	96480.587225	59.389236
2339.251744	96265.370232	59.394241
2338.987327	96032.476630	59.399245
2338.217692	95808.747399	59.404250
2337.596800	95591.693973	59.409255
2336.944365	95377.913746	59.414260
2335.986530	95160.290042	59.419265
2335.490518	94935.283065	59.424269
2334.719115	94718.661444	59.429274
2334.074462	94492.490210	59.434279
2333.585050	94276.937933	59.439284
2332.624851	94065.451245	59.444289
2331.888523	93835.851343	59.449293
2331.455275	93625.521850	59.454298
2330.865574	93406.423609	59.459303
2330.228483	93183.257549	59.464308
2329.470806	92970.354017	59.469313
2328.928204	92740.113223	59.474317
2327.749655	92532.188729	59.479322
2327.181490	92306.205062	59.484327
2326.945206	92092.827770	59.489332
2326.288403	91873.228971	59.494337
2325.713959	91646.739407	59.499341
2324.614974	91421.781055	59.504346
2323.930639	91208.806724	59.509351
2323.533430	91002.243773	59.514356
2322.778402	90782.893324	59.519361
2322.120164	90561.748006	59.524365
2321.569980	90346.820523	59.529370
2320.971570	90130.349377	59.534375
2320.573803	89907.096020	59.539380
2319.189703	89684.692446	59.544385
2318.870628	89461.982762	59.549389
2318.269670	89251.905373	59.554394
2317.401328	89028.735613	59.559399
2317.068133	88812.381291	59.564404
2316.310408	88595.310279	59.569409
2315.919052	88370.524665	59.574413
2314.941551	88153.518282	59.579418
2314.640388	87923.131214	59.584423
2314.124582	87693.173700	59.589428
2313.201104	87482.746146	59.594433
2312.554558	87243.982946	59.599437
2311.534786	87022.100431	59.604442
2311.194380	86795.389542	59.609447
2310.393844	86586.821391	59.614452
2309.766991	86360.255605	59.619457
2309.453606	86137.756706	59.624461
2308.438965	85916.296851	59.629466
2307.513558	85689.430502	59.634471
2307.055825	85480.634915	59.639476
2305.813233	85248.473342	59.644481
2305.803340	85034.501831	59.649485
2304.966108	84817.646348	59.654490
2304.277319	84597.200763	59.659495
2303.885929	84381.952472	59.664500
2303.105675	84164.682592	59.669505
2302.863178	83935.755282	59.674509
2301.851235	83720.333214	59.679514
2301.010272	83489.743507	59.684519
2300.522902	83270.103786	59.689524
2299.769103	83061.062011	59.694529
2299.162113	82830.207883	59.699533
2298.355136	82607.088972	59.704538
2297.703050	82391.287480	59.709543
2297.283641	82173.397754	59.714548
2296.362038	81955.963876	59.719553
2296.104069	81726.689060	59.724557
2295.331265	81504.489120	59.729562
2294.522540	81290.333633	59.734567
2293.902328	81060.128526	59.739572
2293.113456	80839.104364	59.744577
2292.646803	80619.482768	59.749581
2291.764017	80395.328399	59.754586
2291.266248	80170.830198	59.759591
2290.482600	79961.982552	59.764596
2289.668324	79736.861134	59.769601
2289.051450	79506.032626	59.774605
2288.114630	79292.329958	59.779610
2287.581312	79078.470450	59.784615
2286.904408	78869.661259	59.789620
2286.583516	78649.891661	59.794625
2285.933802	78421.837094	59.799629
2285.004894	78207.472694	59.804634
2284.509208	77986.768350	59.809639
2284.052742	77769.329933	59.814644
2283.073105	77552.870267	59.819649
2282.537103	77321.178957	59.824653
2281.879524	77108.215096	59.829658
2281.049205	76892.461106	59.834663
2280.611848	76672.420672	59.839668
2279.777136	76454.561977	59.844673
2279.278020	76229.067839	59.849677
2278.362431	76018.431009	59.854682
2277.916382	75795.911286	59.859687
2277.113218	75575.414827	59.864692
2276.267829	75363.747210	59.869697
2276.169849	75136.623914	59.874701
2275.217586	74918.914389	59.879706
2274.692809	74706.011658	59.884711
2274.014853	74483.885266	59.889716
2273.050626	74269.289165	59.894721
2272.607303	74044.558115	59.899725
2271.894627	73824.915386	59.904730
2271.249322	73610.383436	59.909735
2270.456178	73391.708528	59.914740
2269.701339	73180.816061	59.919745
2269.156008	72956.480817	59.924750
2268.624812	72740.818734	59.929754
2267.770767	72518.551957	59.934759
2267.218077	72307.890040	59.939764
2266.479019	72093.807333	59.944769
2266.008184	71871.949440	59.949774
2265.057407	71661.528538	59.954778
2264.346336	71458.964999	59.959783
2263.921438	71252.132873	59.964788
2263.074355	71047.580661	59.969793
2262.603046	70835.242753	59.974798
2261.778220	70613.904821	59.979802
2261.195674	70401.525865	59.984807
2260.681720	70184.875270	59.989812
2260.003149	69972.598505	59.994817
2259.364056	69748.770429	59.999822
2258.595650	69530.355791	60.004826
2258.076253	69308.185964	60.009831
2257.538270	69089.112605	60.014836
2256.661986	68875.612231	60.019841
2255.728947	68664.137364	60.024846
2255.192851	68447.237072	60.029850
2254.578048	68231.149720	60.034855
2253.889001	68002.219154	60.039860
2253.339045	67791.921697	60.044865
2252.809994	67559.981477	60.049870
2251.904201	67350.517914	60.054874
2251.201872	67129.206209	60.059879
2250.610509	66908.348091	60.064884
2249.830101	66691.297089	60.069889
2249.413495	66479.523357	60.074894
2248.552122	66260.453903	60.079898
2247.969755	66047.922709	60.084903
2247.317619	65840.841779	60.089908
2246.436826	65626.782474	60.094913
2246.307282	65406.216555	60.099918
2245.062462	65199.793803	60.104922
2244.437960	64977.816762	60.109927
2244.117288	64763.602216	60.114932
2243.308166	64562.560091	60.119937
2242.497605	64344.907016	60.124942
2241.814820	64128.546955	60.129946
2241.479252	63909.344869	60.134951
2240.796963	63699.138288	60.139956
2239.851730	63487.550980	60.144961
2239.492376	63261.790433	60.149966
2238.501222	63051.497501	60.154970
2237.986840	62837.560028	60.159975
2237.484193	62619.633992	60.164980
2236.663109	62414.861546	60.169985
2236.211327	62201.336038	60.174990
2235.439348	61978.571947	60.179994
2234.581819	61758.866391	60.184999
2233.953572	61545.170486	60.190004
2232.926620	61336.561105	60.195009
2232.712857	61119.581540	60.200014
2232.061108	60916.450942	60.205018
2231.385247	60697.852723	60.210023
2230.833706	60481.377266	60.215028
2230.049052	60272.867847	60.220033
2229.483473	60065.769472	60.225038
2228.611189	59844.683068	60.230042
2228.119516	59634.640151	60.235047
2227.495924	59418.340317	60.240052
2226.547663	59213.401235	60.245057
2226.078853	58988.782177	60.250062
2225.156930	58784.682436	60.255066
2224.498236	58568.964590	60.260071
2224.018914	58361.542204	60.265076
2223.083696	58162.575909	60.270081
2222.823385	57947.248364	60.275086
2222.138239	57731.534920	60.280090
2221.441049	57520.295010	60.285095
2220.690430	57310.445947	60.290100
2219.980374	57108.688965	60.295105
2219.619655	56881.362610	60.300110
2218.750420	56677.711263	60.305114
2217.990913	56463.189086	60.310119
2217.788650	56256.417256	60.315124
2216.755944	56045.484774	60.320129
2216.156493	55829.678639	60.325134
2215.505679	55617.149226	60.330138
2214.855074	55398.042752	60.335143
2214.230603	55185.707197	60.340148
2213.242211	54983.489123	60.345153
2212.782101	54762.078303	60.350158
2211.817482	54555.810460	60.355162
2211.500373	54348.913750	60.360167
2210.650388	54133.736928	60.365172
2209.841341	53926.081280	60.370177
2209.404763	53716.653783	60.375182
2208.802790	53514.760904	60.380186
2207.765308	53306.809957	60.385191
2207.219635	53092.296486	60.390196
2206.413995	52896.432865	60.395201
2205.982737	52678.969653	60.400206
2204.969727	52482.216270	60.405210
2204.066732	52287.298627	60.410215
2203.659424	52083.052449	60.415220
2202.910177	51879.464002	60.420225
2202.279017	51675.495246	60.425230
2201.546019	51482.381831	60.430234
2200.805591	51279.235394	60.435239
2200.602371	51079.622461	60.440244
2199.329660	50890.559149	60.445249
2198.971702	50687.994664	60.450254
2198.395692	50486.321299	60.455258
2197.754520	50291.927886	60.460263
2197.223292	50080.668692	60.465268
2196.545751	49884.390346	60.470273
2195.900287	49678.978517	60.475278
2195.226415	49487.800719	60.480282
2194.330134	49286.593456	60.485287
2194.046323	49086.971190	60.490292
2192.896930	48885.935143	60.495297
2192.253733	48679.003277	60.500302
2191.740721	48485.289348	60.505306
2190.968485	48289.100512	60.510311
2190.384960	48090.115881	60.515316
2189.621955	47896.242405	60.520321
2188.969138	47703.916279	60.525326
2187.787326	47507.608089	60.530330
2187.211703	47313.587890	60.535335
2186.705899	47130.288595	60.540340
2185.857389	46950.132900	60.545345
2185.317088	46762.113836	60.550350
2184.391219	46580.180643	60.555354
2183.406306	46401.285833	60.560359
2182.665802	46210.346864	60.565364
2181.374713	46043.796142	60.570369
2180.720339	45877.705851	60.575374
2179.724261	45717.026347	60.580378
2178.620485	45560.455160	60.585383
2178.113223	45403.227729	60.590388
2177.051477	45255.021832	60.595393
2176.656970	45095.438693	60.600398
2175.571597	44956.120549	60.605402
2174.841260	44814.365553	60.610407
2174.331790	44668.025338	60.615412
2173.664685	44537.569713	60.620417
2173.155447	44390.887035	60.625422
2171.790319	44252.747999	60.630426
2171.227002	44122.256875	60.635431
2170.792220	43983.023560	60.640436
2169.602506	43864.098595	60.645441
2169.120263	43726.016597	60.650446
2168.321407	43600.462563	60.655450
2167.918261	43471.554365	60.660455
2167.139978	43344.275287	60.665460
2166.247919	43225.939988	60.670465
2165.593428	43092.099744	60.675470
2164.713024	42971.152064	60.680474
2164.327545	42851.192475	60.685479
2163.868425	42722.573857	60.690484
2162.943480	42612.144698	60.695489
2162.452609	42485.300697	60.700494
2161.549618	42364.167931	60.705498
2160.834367	42250.412571	60.710503
2160.333145	42120.480060	60.715508
2159.727906	42014.766537	60.720513
2159.220367	41890.029354	60.725518
2158.667100	41778.221540	60.730522
2157.717298	41654.789525	60.735527
2157.253764	41526.639037	60.740532
2156.483140	41419.171883	60.745537
2156.204625	41296.246251	60.750542
2155.616713	41169.322961	60.755546
2154.485309	41055.575101	60.760551
2153.784496	40936.289142	60.765556
2152.998657	40825.609034	60.770561
2152.633766	40710.211376	60.775566
2151.742620	40596.289309	60.780570
2150.780475	40482.875709	60.785575
2150.882219	40358.656917	60.790580
2150.238023	40246.294833	60.795585
2149.530759	40133.690531	60.800590
2148.525638	40012.157334	60.805594
2148.117982	39892.699319	60.810599
2147.647820	39774.651217	60.815604
2146.828509	39660.271822	60.820609
2146.548043	39533.454149	60.825614
2145.889303	39414.987878	60.830618
2145.263233	39294.613807	60.835623
2144.709564	39166.610659	60.840628
2143.882390	39048.519876	60.845633
2143.214288	38923.598923	60.850638
2142.500352	38799.878143	60.855642
2141.705877	38678.602422	60.860647
2141.137247	38558.265542	60.865652
2140.364143	38439.059065	60.870657
2140.098887	38313.016349	60.875662
2139.386755	38190.975400	60.880666
2138.697964	38073.021195	60.885671
2138.151108	37947.890571	60.890676
2137.221121	37824.735997	60.895681
2136.445806	37698.274496	60.900686
2135.898476	37573.878609	60.905690
2135.319731	37463.275991	60.910695
2134.544107	37332.919118	60.915700
2133.541650	37218.180543	60.920705
2133.280291	37110.054313	60.925710
2132.761148	36995.566196	60.930714
2131.778923	36877.116791	60.935719
2131.243126	36744.673071	60.940724
2130.720858	36626.794206	60.945729
2129.870004	36507.164756	60.950734
2129.242720	36382.501063	60.955738
2128.564734	36268.299150	60.960743
2128.248136	36148.723415	60.965748
2127.623572	36029.968735	60.970753
2126.946975	35906.789530	60.975758
2126.181085	35778.045874	60.980762
2125.409275	35666.417186	60.985767
2124.941591	35537.247138	60.990772
2124.221653	35422.788927	60.995777
2123.519946	35295.741057	61.000782
2122.993591	35174.718229	61.005786
2122.220762	35049.014331	61.010791
2121.544284	34927.580881	61.015796
2120.703187	34812.047604	61.020801
2120.162114	34680.790561	61.025806
2119.461494	34570.913809	61.030810
2119.053096	34443.979171	61.035815
2118.576827	34315.336722	61.040820
2117.880163	34198.853875	61.045825
2116.982195	34065.610026	61.050830
2116.466445	33948.597641	61.055834
2115.531145	33831.241739	61.060839
2114.932606	33701.329063	61.065844
2114.267248	33586.272635	61.070849
2113.556945	33464.826746	61.075854
2112.973581	33343.238332	61.080858
2112.107841	33224.443857	61.085863
2111.641819	33100.978514	61.090868
2111.056476	32984.906871	61.095873
2110.429387	32861.353500	61.100878
2109.920592	32742.611718	61.105882
2109.020487	32617.077525	61.110887
2108.542638	32492.147326	61.115892
2107.693381	32379.726434	61.120897
2107.033545	32251.984000	61.125902
2106.154611	32124.452726	61.130906
2105.620051	32017.235552	61.135911
2104.872525	31896.556089	61.140916
2104.024928	31786.041572	61.145921
2103.511891	31654.364672	61.150926
2103.050874	31549.660878	61.155930
2102.198131	31425.054218	61.160935
2101.661323	31304.996682	61.165940
2100.963440	31189.884633	61.170945
2100.279556	31065.462480	61.175950
2099.816948	30946.288571	61.180954
2098.783868	30833.314829	61.185959
2098.368141	30721.359471	61.190964
2097.520841	30606.082440	61.195969
2097.156534	30486.953144	61.200974
2096.374651	30367.712421	61.205978
2095.432874	30245.383608	61.210983
2095.226447	30123.650053	61.215988
2094.647355	30016.383448	61.220993
2093.976841	29891.162240	61.225998
2093.219085	29769.194890	61.231002
2092.301857	29659.780135	61.236007
2091.866434	29535.143712	61.241012
2091.047308	29416.053284	61.246017
2090.701479	29292.118653	61.251022
2089.890656	29172.978120	61.256026
2089.091763	29044.533762	61.261031
2088.621179	28931.254791	61.266036
2087.944997	28814.673983	61.271041
2086.847618	28690.373393	61.276046
2086.673040	28575.488957	61.281050
2085.845901	28459.832032	61.286055
2085.237704	28331.644253	61.291060
2084.555671	28228.965282	61.296065
2083.839968	28099.074325	61.301070
2083.036751	27985.377592	61.306074
2082.327965	27863.797464	61.311079
2082.170213	27737.825763	61.316084
2081.283786	27634.440461	61.321089
2080.698619	27518.334766	61.326094
2080.197625	27398.614602	61.331098
2079.082385	27275.822159	61.336103
2078.443221	27157.684950	61.341108
2077.815391	27041.779011	61.346113
2077.398138	26922.241810	61.351118
2076.671539	26790.151408	61.356122
2075.815063	26678.996716	61.361127
2075.204972	26552.508076	61.366132
2074.084788	26452.920034	61.371137
2073.763114	26336.277869	61.376142
2072.883643	26221.820511	61.381146
2072.436024	26115.777495	61.386151
2071.814235	26000.156882	61.391156
2071.246146	25888.910530	61.396161
2070.693757	25755.132051	61.401166
2070.175652	25640.754166	61.406170
2069.087144	25532.667605	61.411175
2068.897691	25409.082177	61.416180
2067.958336	25294.046986	61.421185
2067.305010	25169.298609	61.426190
2066.839642	25055.763961	61.431194
2065.953155	24945.755387	61.436199
2065.333888	24817.604337	61.441204
2064.536499	24708.406987	61.446209
2064.069476	24589.887724	61.451214
2063.374159	24476.857253	61.456218
2062.501523	24355.913196	61.461223
2062.062633	24243.589204	61.466228
2061.153029	24135.494729	61.471233
2060.674101	24014.384950	61.476238
2060.184104	23895.658085	61.481242
2059.200834	23775.303000	61.486247
2058.594565	23658.173426	61.491252
2058.046599	23552.203547	61.496257
2057.537586	23431.645491	61.501262
2056.928957	23310.595588	61.506266
2055.950824	23210.029876	61.511271
2055.522650	23091.520296	61.516276
2054.821715	22972.061462	61.521281
2054.121737	22856.789447	61.526286
2053.607291	22729.470829	61.531290
2052.908387	22616.338025	61.536295
2052.433770	22489.375095	61.541300
2051.027579	22380.445854	61.546305
2050.721918	22263.424921	61.551310
2050.069439	22151.305127	61.556314
2048.976162	22040.702692	61.561319
2048.727462	21924.982061	61.566324
2047.778766	21814.952059	61.571329
2047.383121	21696.007114	61.576334
2046.710003	21590.159403	61.581338
2045.571108	21478.018127	61.586343
2044.836271	21358.082530	61.591348
2044.274194	21258.574924	61.596353
2043.776848	21147.336182	61.601358
2043.209314	21028.575134	61.606362
2042.482478	20939.710086	61.611367
2041.938878	20824.110629	61.616372
2040.932267	20719.322859	61.621377
2040.565934	20604.804645	61.626382
2040.082867	20491.351163	61.631386
2039.208477	20378.949910	61.636391
2038.895155	20269.209623	61.641396
2038.024334	20162.050370	61.646401
2037.319938	20052.997392	61.651406
2036.831569	19933.207610	61.656410
2035.818117	19828.837807	61.661415
2035.712191	19716.440526	61.666420
2034.511928	19606.717322	61.671425
2034.054996	19493.744148	61.676430
2033.207601	19379.296198	61.681434
2032.588864	19279.385734	61.686439
2032.078953	19162.862321	61.691444
2031.425649	19050.271277	61.696449
2030.757124	18948.237239	61.701454
2030.129214	18834.717654	61.706458
2029.380014	18727.305348	61.711463
2028.975876	18615.700250	61.716468
2028.316369	18503.775299	61.721473
2027.597265	18396.449699	61.726478
2026.740699	18279.075274	61.731482
2026.063020	18175.308581	61.736487
2025.581927	18052.701476	61.741492
2024.943644	17954.315534	61.746497
2024.048284	17842.574852	61.751502
2023.535591	17719.688818	61.756506
2022.385016	17628.069860	61.761511
2021.885820	17530.412886	61.766516
2021.489765	17429.747128	61.771521
2020.621330	17321.663619	61.776526
2020.219905	17224.137115	61.781530
2019.161835	17106.254090	61.786535
2018.682090	16987.279239	61.791540
2017.720930	16885.225418	61.796545
2016.966076	16772.734821	61.801550
2016.697338	16667.478599	61.806554
2015.566256	16566.435618	61.811559
2015.101998	16457.171511	61.816564
2014.240863	16363.116419	61.821569
2013.695776	16268.112280	61.826574
2012.673177	16169.756602	61.831578
2011.903631	16073.944290	61.836583
2011.542821	15961.214907	61.841588
2010.739951	15868.365198	61.846593
2010.212997	15773.433244	61.851598
2009.713186	15678.661940	61.856602
2009.107841	15593.672926	61.861607
2008.371478	15493.905088	61.866612
2007.570517	15400.070668	61.871617
2006.922421	15301.685745	61.876622
2006.481815	15199.795441	61.881626
2005.290017	15116.453684	61.886631
2004.763462	15021.579371	61.891636
2004.266975	14924.308374	61.896641
2003.283950	14836.787939	61.901646
2002.900231	14756.309446	61.906650
2001.774985	14664.749806	61.911655
2001.647537	14562.513699	61.916660
2000.297030	14476.402287	61.921665
1999.593067	14388.917854	61.926670
1998.920445	14302.738203	61.931674
1998.139783	14220.145525	61.936679
1997.796082	14135.348659	61.941684
1996.682963	14053.628773	61.946689
1995.843650	13975.487140	61.951694
1995.403169	13886.605983	61.956698
1994.623380	13816.482219	61.961703
1994.000777	13733.362592	61.966708
1993.312662	13656.318092	61.971713
1992.560693	13575.333933	61.976718
1992.320491	13493.855925	61.981722
1991.444917	13430.670743	61.986727
1991.108147	13353.539842	61.991732
1990.326785	13279.585959	61.996737
1989.512030	13205.575782	62.001742
1989.058568	13115.759952	62.006746
1988.258665	13040.522517	62.011751
1987.621506	12961.994578	62.016756
1986.983496	12886.636221	62.021761
1985.892152	12814.591898	62.026766
1985.404988	12738.336623	62.031770
1984.822758	12672.914734	62.036775
1984.252379	12585.163227	62.041780
1983.410334	12512.534764	62.046785
1982.460698	12444.084909	62.051790
1982.200304	12361.338905	62.056794
1981.142227	12293.358528	62.061799
1980.764237	12224.319993	62.066804
1979.922880	12154.435779	62.071809
1979.400361	12083.006272	62.076814
1979.338179	12013.257670	62.081818
1978.204622	11939.606775	62.086823
1977.962676	11858.941489	62.091828
1977.157663	11785.299168	62.096833
1976.185157	11715.300287	62.101838
1975.411640	11635.850567	62.106842
1974.541158	11569.500977	62.111847
1974.262510	11490.677546	62.116852
1973.225776	11434.231117	62.121857
1972.584881	11355.224621	62.126862
1972.049301	11281.118238	62.131866
1971.091897	11223.313029	62.136871
1970.915991	11156.420016	62.141876
1970.134472	11096.647809	62.146881
1969.538317	11029.919510	62.151886
1968.987147	10961.945521	62.156890
1968.162715	10897.800376	62.161895
1967.464200	10821.718655	62.166900
1966.752022	10763.843532	62.171905
1966.443940	10688.375551	62.176910
1965.981615	10605.866450	62.181914
1964.946980	10550.089346	62.186919
1964.169859	10480.581595	62.191924
1963.603126	10406.208666	62.196929
1963.135521	10339.219589	62.201934
1962.135297	10271.357462	62.206938
1961.435037	10202.348509	62.211943
1961.254065	10123.770948	62.216948
1960.346098	10061.837888	62.221953
1959.498246	9988.240700	62.226958
1959.181672	9911.286694	62.231962
1958.249012	9846.146941	62.236967
1957.665665	9770.724867	62.241972
1956.890694	9703.028769	62.246977
1955.715314	9646.146708	62.251982
1955.281080	9577.409650	62.256986
1954.714994	9519.000502	62.261991
1954.459992	9445.688999	62.266996
1953.416628	9384.516546	62.272001
1952.540562	9329.977627	62.277006
1952.126809	9255.237358	62.282010
1951.580941	9199.976650	62.287015
1951.017494	9135.717493	62.292020
1950.161185	9063.773552	62.297025
1949.508009	8996.048679	62.302030
1948.989902	8939.383707	62.307034
1948.108127	8879.159277	62.312039
1947.479443	8821.859433	62.317044
1946.679286	8763.030414	62.322049
1946.405477	8700.735433	62.327054
1945.682949	8621.204335	62.332058
1944.981464	8569.192723	62.337063
1944.415651	8507.311757	62.342068
1943.246004	8445.034994	62.347073
1942.379970	8381.026308	62.352078
1942.036678	8320.240155	62.357082
1941.341791	8273.265476	62.362087
1940.992976	8203.347213	62.367092
1940.104075	8138.370840	62.372097
1939.499681	8089.340637	62.377102
1939.014525	8017.820491	62.382106
1938.008332	7966.159134	62.387111
1937.538008	7895.306615	62.392116
1937.116690	7841.481951	62.397121
1936.527091	7778.183793	62.402126
1935.575590	7720.578484	62.407130
1935.029338	7671.633906	62.412135
1934.558741	7601.213562	62.417140
1933.717820	7539.877272	62.422145
1932.959641	7483.212529	62.427150
1932.731547	7411.716403	62.432154
1931.832048	7343.503242	62.437159
1930.998483	7291.676791	62.442164
1930.413622	7226.868723	62.447169
1929.464779	7174.055164	62.452174
1929.004053	7099.961831	62.457178
1928.436681	7053.678364	62.462183
1927.723643	6977.427119	62.467188
1927.432653	6926.851353	62.472193
1926.588046	6861.166296	62.477198
1925.923313	6798.633635	62.482202
1925.298746	6735.883842	62.487207
1924.620064	6678.242410	62.492212
1923.908211	6622.106850	62.497217
1923.331487	6551.268922	62.502222
1922.987968	6484.657188	62.507226
1921.867825	6428.926372	62.512231
1921.344213	6363.894617	62.517236
1920.415220	6299.231988	62.522241
1919.952697	6242.290752	62.527246
1919.261510	6174.259708	62.532250
1918.371510	6117.423098	62.537255
1917.898065	6055.789267	62.542260
1917.314487	5997.253483	62.547265
1916.416869	5941.353499	62.552270
1915.914696	5868.875732	62.557274
1914.992375	5815.415186	62.562279
1914.616801	5752.402449	62.567284
1913.819519	5699.522747	62.572289
1912.997823	5646.137549	62.577294
1912.577370	5582.375418	62.582298
1911.915718	5526.534194	62.587303
1911.196553	5461.580819	62.592308
1910.345081	5398.330412	62.597313
1909.690687	5344.010281	62.602318
1909.210489	5294.532588	62.607322
1908.559425	5231.425398	62.612327
1907.916527	5170.325383	62.617332
1907.330287	5107.142175	62.622337
1906.691903	5051.713940	62.627342
1905.886895	4989.361826	62.632346
1905.409868	4940.100146	62.637351
1904.311155	4873.374963	62.642356
1904.096881	4812.277003	62.647361
1903.310827	4761.858191	62.652366
1902.625071	4696.358638	62.657370
1901.809448	4653.252593	62.662375
1901.337325	4594.709394	62.667380
1900.793704	4531.997487	62.672385
1899.656167	4481.654364	62.677390
1899.419031	4418.958957	62.682394
1898.588914	4369.094283	62.687399
1898.260267	4304.429458	62.692404
1897.250392	4249.440221	62.697409
1896.918409	4191.710836	62.702414
1896.376337	4114.805160	62.707418
1895.329257	4066.834159	62.712423
1894.924974	4010.536637	62.717428
1894.367469	3950.778378	62.722433
1893.398767	3884.698755	62.727438
1892.557753	3829.528117	62.732442
1891.975201	3763.361707	62.737447
1891.081377	3722.598237	62.742452
1890.317069	3666.847387	62.747457
1889.724769	3615.465569	62.752462
1889.423309	3560.267856	62.757466
1888.682844	3502.777166	62.762471
1887.863676	3453.298735	62.767476
1887.466140	3387.439830	62.772481
1886.506982	3336.972150	62.777486
1886.299735	3280.276254	62.782490
1884.937195	3224.818437	62.787495
1884.491503	3171.944036	62.792500
1883.828197	3128.197607	62.797505
1883.176759	3072.100648	62.802510
1882.845235	3008.109174	62.807514
1881.801688	2959.945649	62.812519
1881.343304	2910.070287	62.817524
1880.869374	2857.503554	62.822529
1880.240825	2796.745493	62.827534
1879.402215	2740.558857	62.832538
1878.398466	2688.376529	62.837543
1878.174580	2642.539726	62.842548
1877.568992	2597.628794	62.847553
1876.227689	2541.372893	62.852558
1876.178807	2473.468296	62.857562
1875.335013	2432.049863	62.862567
1874.571887	2368.397047	62.867572
1874.337437	2316.705875	62.872577
1873.559429	2256.864131	62.877582
1872.564283	2209.211148	62.882586
1871.904814	2160.369433	62.887591
1871.123466	2095.611129	62.892596
1870.860630	2053.196217	62.897601
1869.762719	2002.561176	62.902606
1869.318173	1951.779994	62.907610
1868.465703	1907.325182	62.912615
1867.840178	1856.446890	62.917620
1867.367420	1800.932072	62.922625
1866.631863	1754.314996	62.927630
1865.870275	1700.906200	62.932634
1864.988848	1660.994239	62.937639
1864.412785	1612.678137	62.942644
1864.035645	1562.268490	62.947649
1863.403315	1519.234042	62.952654
1862.600471	1467.752036	62.957658
1861.746557	1419.302474	62.962663
1861.239746	1373.552418	62.967668
1860.783115	1333.628320	62.972673
1859.891772	1290.046618	62.977678
1859.181688	1232.388123	62.982682
1858.453121	1185.870327	62.987687
1857.857056	1132.290665	62.992692
1857.429128	1090.133443	62.997697
1856.360451	1052.852729	63.002702
1856.009554	999.580802	63.007706
1854.976474	954.618213	63.012711
1854.390982	911.284790	63.017716
1853.694650	873.446273	63.022721
1852.607588	824.706104	63.027726
1852.419045	779.747171	63.032730
1851.297212	746.217273	63.037735
1850.935737	710.243721	63.042740
1850.463356	672.994684	63.047745
1849.740287	634.462401	63.052750
1849.091286	588.050588	63.057754
1848.315897	553.204496	63.062759
1847.546239	512.181905	63.067764
1846.764407	472.118621	63.072769
1846.037310	435.971978	63.077774
1845.536605	395.432165	63.082778
1844.718713	372.536055	63.087783
1843.960006	334.319326	63.092788
1843.361942	306.359314	63.097793
1842.318087	271.621185	63.102798
1841.795745	233.272573	63.107802
1840.870026	215.725690	63.112807
1839.917792	187.135360	63.117812
1839.534610	157.859415	63.122817
1838.688934	144.628768	63.127822
1838.258007	115.854089	63.132826
1837.207859	94.457173	63.137831
1836.631398	71.292968	63.142836
1836.272006	55.961915	63.147841
1835.202497	44.556781	63.152846
1834.357523	32.800607	63.157850
1832.868872	33.026060	63.162855
1831.929598	43.602338	63.167860
1831.330208	40.843289	63.172865
1830.162331	56.096940	63.177870
1829.923808	54.433365	63.182874
1829.274126	62.295415	63.187879
1828.490774	57.799349	63.192884
1828.457985	56.140954	63.197889
1827.434522	61.887691	63.202894
1827.168178	55.533846	63.207898
1826.029367	60.530907	63.212903
1825.948677	67.107257	63.217908
1825.597926	59.341217	63.222913
1824.428998	63.762731	63.227918
1823.771344	58.128624	63.232922
1822.896625	65.307304	63.237927
1822.114397	64.781912	63.242932
1822.047026	66.800233	63.247937
1821.216951	65.692645	63.252942
1820.857253	62.130696	63.257946
1819.794632	64.822725	63.262951
1819.059062	68.587214	63.267956
1818.455230	67.017916	63.272961
1817.781953	66.358529	63.277966
1817.433630	63.062861	63.282970
1817.173073	65.458795	63.287975
1816.525840	60.326092	63.292980
1815.829815	64.789215	63.297985
1814.647884	65.920051	63.302990
1814.006112	60.026375	63.307994
1813.156112	69.191291	63.312999
1812.242178	62.803079	63.318004
1811.756901	60.912177	63.323009
1811.079728	68.075262	63.328014
1811.091372	57.813659	63.333018
1810.651047	62.147868	63.338023
1809.905110	65.450371	63.343028
1809.012510	63.620995	63.348033
1808.315524	60.224573	63.353038
1807.500368	63.490758	63.358042
1806.757377	61.729092	63.363047
1805.902706	64.919549	63.368052
1805.455202	58.919332	63.373057
1804.434576	66.859216	63.378062
1804.043324	55.579781	63.383066
1803.346607	66.179068	63.388071
1803.283109	66.088343	63.393076
1802.863372	59.249491	63.398081
1801.552717	70.704802	63.403086
1800.873780	60.626978	63.408090
1800.275383	68.427275	63.413095
1799.891983	67.128914	63.418100
1799.743718	63.692668	63.423105
1797.924607	68.633765	63.428110
1797.618206	66.846927	63.433114
1797.345310	61.760445	63.438119
1796.390024	63.219582	63.443124
1796.353165	59.618987	63.448129
1794.618649	66.353878	63.453134
1794.540412	65.492770	63.458138
1794.208118	58.606919	63.463143
1792.965584	61.895242	63.468148
1792.705793	59.451286	63.473153
1791.690081	68.823874	63.478158
1791.446481	60.586653	63.483162
1790.575818	68.158945	63.488167
1789.499136	63.766243	63.493172
1789.418347	59.281628	63.498177
1788.708260	67.135932	63.503182
1787.692236	63.283966	63.508186
1787.132840	55.164709	63.513191
1786.645344	60.510950	63.518196
1786.279313	59.804357	63.523201
1785.227533	72.685163	63.528206
1784.526238	62.252918	63.533210
1783.544653	64.968363	63.538215
1783.079039	65.905033	63.543220
1782.918008	56.233840	63.548225
1781.841614	72.723544	63.553230
1781.374390	62.992158	63.558234
1781.078978	58.347658	63.563239
1779.943515	70.060589	63.568244
1779.200060	71.090270	63.573249
1778.832844	75.330873	63.578254
1777.905971	64.522858	63.583258
1777.398156	71.353122	63.588263
1776.558227	68.080334	63.593268
1776.022202	63.332115	63.598273
1775.434144	74.354135	63.603278
1774.894707	67.288286	63.608282
1773.730495	68.930424	63.613287
1773.384666	67.638716	63.618292
1773.188789	65.197227	63.623297
1771.787297	69.819703	63.628302
1771.459218	65.994114	63.633306
1770.985048	70.586023	63.638311
1769.505676	64.607752	63.643316
1769.904488	64.057248	63.648321
1768.752653	67.613460	63.653326
1768.005363	58.306612	63.658330
1767.307487	61.555760	63.663335
1766.840333	68.650807	63.668340
1766.395373	67.097294	63.673345
1765.489332	63.562192	63.678350
1764.914808	64.757441	63.683354
1764.256492	65.533902	63.688359
1763.490399	70.391373	63.693364
1763.233986	67.904304	63.698369
1762.205752	75.332893	63.703374
1761.980983	61.743548	63.708378
1761.768667	64.253252	63.713383
1760.388948	65.399753	63.718388
1759.412151	61.732385	63.723393
1758.516166	66.129504	63.728398
1758.701571	64.196756	63.733402
1757.378463	62.656547	63.738407
1756.667932	67.673932	63.743412
1756.824104	57.583352	63.748417
1755.410756	66.673739	63.753422
1754.564016	63.301115	63.758426
1754.704811	67.765398	63.763431
1753.741237	59.106352	63.768436
1753.134892	56.764748	63.773441
1752.526438	66.362833	63.778446
1751.698703	64.813341	63.783450
1751.161177	68.100108	63.788455
1750.520239	66.366406	63.793460
1750.479168	61.675208	63.798465
1749.194449	67.640087	63.803470
1747.989271	59.241769	63.808474
1747.397161	69.083270	63.813479
1747.243718	69.205531	63.818484
1746.777749	63.988867	63.823489
1745.734279	64.711382	63.828494
1744.845093	56.437927	63.833498
1744.240363	64.816412	63.838503
1743.292710	64.605905	63.843508
1743.224093	61.073436	63.848513
1742.429196	65.415080	63.853518
1742.221233	58.875353	63.858522
1741.696968	60.226631	63.863527
1740.860531	64.466060	63.868532
1740.592429	57.275129	63.873537
1739.395750	67.324613	63.878542
1738.114369	59.017252	63.883546
1737.389291	69.362430	63.888551
1737.011331	70.688896	63.893556
1736.671388	52.497290	63.898561
1736.032318	70.505568	63.903566
1735.472485	65.851028	63.908570
1735.125601	71.291645	63.913575
1734.037156	74.735300	63.918580
1733.927734	59.996945	63.923585
1732.768447	67.786982	63.928590
1731.636697	64.456479	63.933594
1731.025160	63.255865	63.938599
1729.969231	68.668741	63.943604
1730.246731	62.608589	63.948609
1729.027153	73.149005	63.953614
1728.708853	64.642954	63.958618
1728.342612	66.975253	63.963623
1727.582149	67.335853	63.968628
1727.395579	62.125283	63.973633
1726.405031	64.649778	63.978638
1725.624106	57.950315	63.983642
1724.598402	63.822025	63.988647
1723.587589	56.506203	63.993652
1723.132455	58.710691	63.998657
1722.334163	64.618824	64.003662
1721.674593	63.843742	64.008666
1721.585297	59.201208	64.013671
1720.726816	72.048175	64.018676
1720.785944	64.742192	64.023681
1720.096325	67.685683	64.028686
1719.246982	66.074977	64.033690
1718.219725	64.380564	64.038695
1717.036243	70.944403	64.043700
1716.782265	63.645572	64.048705
1716.255445	67.760138	64.053710
1715.614602	63.621528	64.058714
1715.206722	59.184140	64.063719
1714.419429	67.842367	64.068724
1713.987904	60.535467	64.073729
1712.679278	65.138489	64.078734
1711.790404	65.442217	64.083738
1711.533935	71.918747	64.088743
1710.669703	71.098902	64.093748
1710.497011	61.122057	64.098753
1709.833416	69.650251	64.103758
1709.188488	70.497141	64.108762
1708.702045	62.159731	64.113767
1707.267602	71.467962	64.118772
1706.611882	67.461030	64.123777
1705.571132	70.744152	64.128782
1705.384243	64.188466	64.133786
1704.874456	64.403600	64.138791
1703.954746	70.305793	64.143796
1703.686140	64.609927	64.148801
1703.208947	67.253171	64.153806
1702.446178	67.563681	64.158810
1702.336259	54.866036	64.163815
1701.624950	72.081530	64.168820
1700.415944	65.719730	64.173825
1699.659210	63.774194	64.178830
1698.914917	67.948537	64.183834
1698.488054	68.628326	64.188839
1697.779381	66.900666	64.193844
1697.484706	59.529456	64.198849
1696.436224	72.130634	64.203854
1695.712221	76.169290	64.208858
1695.195823	72.722138	64.213863
1694.430271	67.952046	64.218868
1693.916476	68.681915	64.223873
1693.161791	71.172114	64.228878
1692.462185	63.234427	64.233882
1691.534236	68.634873	64.238887
1690.525508	70.370624	64.243892
1690.710343	65.427500	64.248897
1690.156154	66.843466	64.253902
1689.226250	66.491385	64.258906
1688.809374	65.811806	64.263911
1688.143018	64.943191	64.268916
1687.624375	58.698831	64.273921
1686.111435	58.699563	64.278926
1685.317826	61.564959	64.283930
1684.773735	67.058980	64.288935
1684.176577	63.094794	64.293940
1684.063924	56.434281	64.298945
1683.444188	61.722692	64.303950
1682.701723	58.260991	64.308954
1682.582576	49.584551	64.313959
1681.296439	66.101278	64.318964
1680.502396	59.679886	64.323969
1679.949947	64.136002	64.328974
1679.132144	61.276061	64.333978
1678.828312	57.853500	64.338983
1678.054942	64.435788	64.343988
1677.553889	59.677310	64.348993
1676.409213	69.101956	64.353998
1675.553019	65.158417	64.359002
1675.033938	62.766700	64.364007
1674.319477	64.367403	64.369012
1674.046863	58.590178	64.374017
1673.381970	64.344667	64.379022
1673.109727	62.998707	64.384026
1672.984075	55.455573	64.389031
1671.602428	64.553576	64.394036
1671.082337	61.841893	64.399041
1670.193638	61.021218	64.404046
1669.346392	62.920563	64.409050
1668.168456	56.071292	64.414055
1667.429440	66.849210	64.419060
1667.573792	57.055409	64.424065
1666.651200	58.949376	64.429070
1666.044744	59.829589	64.434074
1665.617424	51.989017	64.439079
1665.281067	57.956251	64.444084
1664.500953	52.404728	64.449089
1663.146676	57.595352	64.454094
1662.418144	55.645349	64.459098
1661.980763	54.331931	64.464103
1661.319293	61.222882	64.469108
1661.057952	52.130629	64.474113
1660.484401	59.345088	64.479118
1659.878416	59.550279	64.484122
1658.922791	56.661775	64.489127
1657.893995	51.712740	64.494132
1657.386014	52.566274	64.499137
1656.751174	62.193791	64.504142
1656.420967	55.752347	64.509146
1655.949997	52.947710	64.514151
1654.535253	64.397528	64.519156
1653.879265	54.300348	64.524161
1653.266137	68.489786	64.529166
1652.937277	66.260249	64.534170
1652.254652	54.106184	64.539175
1651.756857	58.897403	64.544180
1651.373291	57.204847	64.549185
1650.299857	55.084129	64.554190
1649.294912	60.884754	64.559194
1648.609205	56.546708	64.564199
1647.947092	68.873627	64.569204
1647.810513	58.578816	64.574209
1647.482897	55.730907	64.579214
1646.540301	57.558671	64.584218
1645.789414	58.414523	64.589223
1644.690208	67.954960	64.594228
1644.217122	62.174892	64.599233
1643.607645	64.031743	64.604238
1643.046935	53.766464	64.609242
1642.948573	50.459507	64.614247
1641.529701	60.246267	64.619252
1640.531505	57.785588	64.624257
1639.974640	51.695552	64.629262
1639.504286	51.783006	64.634266
1639.192240	55.942311	64.639271
1638.416879	61.496730	64.644276
1638.482062	51.209300	64.649281
1637.286913	59.596432	64.654286
1636.273566	60.172276	64.659290
1635.643404	51.622753	64.664295
1634.963874	59.235680	64.669300
1635.007528	56.612650	64.674305
1633.736944	53.321597	64.679310
1632.687063	69.990050	64.684314
1631.953937	54.649045	64.689319
1631.370962	60.721693	64.694324
1631.160951	60.028186	64.699329
1630.878365	65.119542	64.704334
1630.350283	60.390600	64.709338
1629.413390	49.380829	64.714343
1628.296214	57.642034	64.719348
1627.615255	59.986492	64.724353
1627.112036	53.162525	64.729358
1626.561779	59.597412	64.734362
1626.312316	56.309728	64.739367
1625.268291	58.571513	64.744372
1624.247225	56.625416	64.749377
1623.667120	48.416460	64.754382
1623.162008	55.709938	64.759386
1622.863252	42.282212	64.764391
1622.120343	46.831668	64.769396
1621.459764	44.541295	64.774401
1620.437775	51.519485	64.779406
1619.892289	58.872996	64.784410
1619.662381	48.430594	64.789415
1618.708541	62.581115	64.794420
1617.706385	49.519024	64.799425
1616.995504	56.107164	64.804430
1616.103163	55.697102	64.809434
1616.009812	54.806864	64.814439
1615.230368	54.262170	64.819444
1614.947714	45.155970	64.824449
1614.428613	55.602479	64.829454
1613.099856	60.888422	64.834458
1612.256142	46.719355	64.839463
1611.470967	53.639426	64.844468
1611.501696	56.242991	64.849473
1610.946561	58.307262	64.854478
1610.388671	57.687947	64.859482
1609.824424	44.873268	64.864487
1608.292915	54.289995	64.869492
1608.013021	50.379511	64.874497
1607.584957	48.298211	64.879502
1607.057533	57.050789	64.884506
1606.339484	53.372343	64.889511
1605.141687	51.205169	64.894516
1604.981600	57.259522	64.899521
1604.519149	57.396190	64.904526
1603.649925	53.263937	64.909530
1602.581115	52.164389	64.914535
1601.453577	57.729034	64.919540
1601.063076	50.530769	64.924545
1600.594198	51.069012	64.929550
1599.941759	47.823278	64.934554
1599.735739	49.884125	64.939559
1599.122233	53.764891	64.944564
1598.142080	48.738770	64.949569
1597.231226	49.115415	64.954574
1596.352497	48.225373	64.959578
1596.295040	50.972259	64.964583
1595.616034	65.555372	64.969588
1595.341584	54.057161	64.974593
1594.293957	46.526477	64.979598
1593.324324	56.793827	64.984602
1592.606884	40.447402	64.989607
1592.018017	53.193194	64.994612
1591.676597	49.626807	64.999617
1591.379889	48.166472	65.004622
1590.072755	52.819773	65.009626
1589.374786	49.406230	65.014631
1588.655273	52.445962	65.019636
1588.273400	50.314748	65.024641
1587.961974	54.325722	65.029646
1587.040506	45.937621	65.034650
1585.930758	44.065556	65.039655
1585.145873	55.129892	65.044660
1584.952133	51.713511	65.049665
1584.778075	52.152876	65.054670
1583.996931	56.935505	65.059674
1583.049762	48.237668	65.064679
1582.033766	50.914491	65.069684
1581.556175	48.535131	65.074689
1581.419601	51.430207	65.079694
1580.592974	59.050745	65.084698
1579.525557	56.724093	65.089703
1578.887839	58.134428	65.094708
1578.430916	56.882478	65.099713
1577.925141	59.184922	65.104718
1577.057204	59.583142	65.109722
1576.634334	51.021205	65.114727
1575.446999	63.934634	65.119732
1575.150955	57.777942	65.124737
1574.713177	51.856664	65.129742
1573.648381	52.484862	65.134746
1572.610605	52.717676	65.139751
1572.024036	59.610934	65.144756
1571.608719	57.087636	65.149761
1571.144549	58.744794	65.154766
1570.364670	57.358074	65.159770
1570.345276	52.333859	65.164775
1569.249101	52.539682	65.169780
1568.337633	49.760897	65.174785
1567.983182	56.047984	65.179790
1567.185761	58.817822	65.184794
1566.327379	48.579367	65.189799
1565.147739	56.822132	65.194804
1564.478057	47.521963	65.199809
1564.422261	54.630515	65.204814
1563.506216	62.572777	65.209818
1563.399024	52.776372	65.214823
1562.949229	58.258579	65.219828
1562.459888	56.943974	65.224833
1561.110974	58.580855	65.229838
1560.247261	61.465309	65.234842
1559.966511	52.759367	65.239847
1559.476697	65.893140	65.244852
1558.658697	62.504983	65.249857
1557.755238	58.291451	65.254862
1556.692297	61.289564	65.259866
1556.339342	58.494582	65.264871
1556.049230	62.738721	65.269876
1555.846392	65.062423	65.274881
1554.878647	59.143350	65.279886
1553.548757	55.134774	65.284890
1553.134526	46.681862	65.289895
1552.683313	61.220896	65.294900
1552.295197	54.353428	65.299905
1551.302968	51.899723	65.304910
1550.305255	52.779050	65.309914
1549.856402	53.154845	65.314919
1549.444789	56.339634	65.319924
1549.235257	48.245288	65.324929
1548.385438	56.993904	65.329934
1547.182716	46.191996	65.334938
1547.135452	46.615948	65.339943
1545.647767	52.990056	65.344948
1544.621699	48.261418	65.349953
1544.374589	48.485308	65.354958
1543.865982	52.142832	65.359962
1543.214228	50.745226	65.364967
1542.482526	53.277542	65.369972
1542.289102	53.212199	65.374977
1541.885145	47.323405	65.379982
1540.807031	56.031025	65.384986
1540.230928	51.626712	65.389991
1539.409384	53.774329	65.394996
1538.695944	47.370152	65.400001
1538.250684	47.344825	65.405006
1536.808029	53.584048	65.410010
1536.320152	46.445428	65.415015
1535.664544	47.199437	65.420020
1535.216744	53.531321	65.425025
1535.404721	50.387034	65.430030
1534.659736	51.910619	65.435034
1534.049755	47.130063	65.440039
1532.846007	54.274361	65.445044
1532.156969	47.727534	65.450049
1531.823153	54.676829	65.455054
1530.529740	61.180931	65.460058
1529.905942	56.792084	65.465063
1529.301671	54.612638	65.470068
1529.166990	52.221378	65.475073
1528.617861	48.785780	65.480078
1527.217817	54.817961	65.485082
1526.661015	49.928030	65.490087
1525.767732	56.161966	65.495092
1525.318920	49.113337	65.500097
1525.253724	46.796194	65.505102
1524.784413	52.730944	65.510106
1523.792827	47.099534	65.515111
1522.779375	46.557360	65.520116
1522.281623	51.962033	65.525121
1521.632381	50.647613	65.530126
1520.356147	54.326193	65.535130
1519.815710	42.135403	65.540135
1518.863584	51.570496	65.545140
1518.606379	49.080433	65.550145
1518.325313	40.980117	65.555150
1517.709805	53.408445	65.560154
1517.282405	48.862237	65.565159
1516.939726	52.461859	65.570164
1515.711991	45.677359	65.575169
1515.202161	43.238480	65.580174
1514.419946	55.204436	65.585178
1513.603969	50.388810	65.590183
1512.560571	52.320948	65.595188
1511.686419	49.648220	65.600193
1511.752947	49.088979	65.605198
1510.822729	50.342378	65.610202
1510.860683	45.704877	65.615207
1510.097030	47.657219	65.620212
1509.092513	49.930115	65.625217
1508.526717	44.439214	65.630222
1507.850353	56.889831	65.635226
1507.468115	46.290308	65.640231
1506.281768	53.584817	65.645236
1505.637081	55.452023	65.650241
1505.179523	51.777948	65.655246
1504.299243	58.459264	65.660250
1503.483452	35.374311	65.665255
1502.454672	57.028983	65.670260
1502.049568	51.804286	65.675265
1501.613398	50.020766	65.680270
1500.965551	61.694137	65.685274
1501.196914	46.971077	65.690279
1500.342717	48.448946	65.695284
1499.157071	50.408425	65.700289
1498.577935	51.478302	65.705294
1498.090856	50.187005	65.710298
1496.871075	49.048414	65.715303
1496.089456	56.521467	65.720308
1495.727227	49.932180	65.725313
1495.477135	39.221777	65.730318
1494.827113	51.739170	65.735322
1494.451026	51.817978	65.740327
1493.182990	47.181432	65.745332
1492.627058	56.134098	65.750337
1492.261231	45.038377	65.755342
1490.902185	57.422441	65.760346
1489.916702	50.380255	65.765351
1489.641836	54.163073	65.770356
1489.710182	58.935310	65.775361
1489.707966	44.107445	65.780366
1488.406620	53.236915	65.785370
1487.452118	52.876200	65.790375
1486.339612	51.368900	65.795380
1485.546452	49.618460	65.800385
1485.077406	45.376927	65.805390
1484.518623	59.940940	65.810394
1484.082016	55.787291	65.815399
1483.768387	52.260661	65.820404
1482.963875	56.514009	65.825409
1482.083050	48.647783	65.830414
1481.120387	54.484319	65.835418
1480.905813	54.185795	65.840423
1479.692447	49.781846	65.845428
1478.797941	48.342409	65.850433
1478.194711	52.393456	65.855438
1477.481070	55.482747	65.860442
1477.328470	60.375254	65.865447
1477.050911	53.318342	65.870452
1476.598616	52.404728	65.875457
1475.897705	58.652263	65.880462
1474.571747	52.294984	65.885466
1474.426287	48.243306	65.890471
1473.460361	51.623430	65.895476
1472.647211	51.604540	65.900481
1471.965693	57.163007	65.905486
1471.166411	49.853115	65.910490
1470.879651	49.901961	65.915495
1470.033557	53.709327	65.920500
1469.104089	42.398833	65.925505
1468.653850	45.886240	65.930510
1467.717016	49.488826	65.935514
1467.650774	51.913828	65.940519
1467.262416	45.144194	65.945524
1465.814167	50.351419	65.950529
1465.147082	47.175861	65.955534
1464.173797	54.324560	65.960538
1463.985169	52.139001	65.965543
1463.836374	54.402077	65.970548
1463.454736	57.407068	65.975553
1462.621846	41.899080	65.980558
1461.448277	57.811341	65.985562
1461.353810	46.305065	65.990567
1459.937754	53.916800	65.995572
1458.633618	62.698219	66.000577
1458.402535	53.195914	66.005582
1457.768436	56.794548	66.010586
1457.977103	37.727376	66.015591
1457.194759	44.751108	66.020596
1456.296614	39.693094	66.025601
1455.585256	44.474122	66.030606
1454.872423	48.380163	66.035610
1454.420555	53.779130	66.040615
1454.197134	53.239160	66.045620
1452.920459	50.398610	66.050625
1452.162964	49.098260	66.055630
1451.227824	53.413378	66.060634
1451.110607	47.726617	66.065639
1450.298617	50.505110	66.070644
1449.321347	49.514083	66.075649
1448.833337	45.527889	66.080654
1448.022863	51.013812	66.085658
1447.757284	46.454517	66.090663
1447.509135	45.391767	66.095668
1446.460499	41.661835	66.100673
1445.551345	43.419696	66.105678
1444.870894	43.818124	66.110682
1444.780934	46.059233	66.115687
1443.686232	41.756296	66.120692
1442.737800	43.867335	66.125697
1442.521695	38.500653	66.130702
1441.821797	49.072102	66.135706
1441.109022	51.749671	66.140711
1440.136128	51.076502	66.145716
1439.422244	44.855361	66.150721
1439.240391	43.045627	66.155726
1438.476843	48.533555	66.160730
1437.901361	38.833684	66.165735
1437.045170	42.038680	66.170740
1435.767872	46.605304	66.175745
1435.619571	41.935908	66.180750
1434.779465	41.347294	66.185754
1434.784976	36.623491	66.190759
1433.927383	39.488082	66.195764
1432.798749	41.870620	66.200769
1432.893566	36.394597	66.205774
1431.903373	45.198661	66.210778
1431.340190	44.938201	66.215783
1430.306025	39.398761	66.220788
1429.609320	48.337533	66.225793
1429.505558	37.244338	66.230798
1428.769188	43.369777	66.235802
1427.769139	42.855473	66.240807
1426.721922	47.786085	66.245812
1426.242279	41.830499	66.250817
1426.382170	37.824940	66.255822
1425.208969	48.645085	66.260826
1424.378646	37.064965	66.265831
1423.879348	41.589941	66.270836
1422.703212	45.676860	66.275841
1422.954949	39.767459	66.280846
1421.915421	48.052657	66.285850
1420.996651	39.075993	66.290855
1420.519602	44.169876	66.295860
1419.717745	38.088885	66.300865
1419.838872	43.814679	66.305870
1418.439272	45.805045	66.310874
1417.618794	43.661572	66.315879
1416.938121	47.713899	66.320884
1416.346434	48.995527	66.325889
1416.389065	42.222060	66.330894
1415.574692	35.206337	66.335898
1414.635948	39.116752	66.340903
1413.727052	43.903955	66.345908
1413.180605	41.442533	66.350913
1413.104399	38.447470	66.355918
1411.816823	44.584830	66.360922
1411.049416	41.193419	66.365927
1410.561432	37.990990	66.370932
1409.851131	42.137914	66.375937
1409.898443	46.331580	66.380942
1409.028706	41.663314	66.385946
1408.013983	39.922885	66.390951
1407.390375	44.160112	66.395956
1406.878908	41.052880	66.400961
1406.090011	46.595308	66.405966
1404.753070	47.277869	66.410970
1404.412068	46.253537	66.415975
1403.813082	44.972163	66.420980
1403.343493	46.945603	66.425985
1403.313794	40.760807	66.430990
1401.857573	45.948829	66.435994
1401.016190	32.027094	66.440999
1400.318901	44.558312	66.446004
1400.087425	36.421755	66.451009
1399.824017	43.657909	66.456014
1398.974139	44.494871	66.461018
1398.014952	42.176330	66.466023
1397.733315	42.159713	66.471028
1396.992390	46.093887	66.476033
1396.499986	42.810159	66.481038
1395.671813	45.666933	66.486042
1394.838574	41.882286	66.491047
1394.408398	41.482420	66.496052
1393.545096	54.610901	66.501057
1393.063059	43.733956	66.506062
1392.456297	43.097227	66.511066
1391.678312	46.550007	66.516071
1390.618427	44.920844	66.521076
1389.817893	43.318267	66.526081
1389.574940	48.860654	66.531086
1389.073579	40.505217	66.536090
1388.006161	41.599114	66.541095
1386.993637	46.096864	66.546100
1386.432199	51.557411	66.551105
1386.019766	51.091647	66.556110
1385.641122	49.874601	66.561114
1385.408087	48.497214	66.566119
1384.711997	48.117540	66.571124
1383.455962	47.956185	66.576129
1382.824002	49.439767	66.581134
1382.524794	54.920135	66.586138
1381.637868	48.526242	66.591143
1380.758491	49.385245	66.596148
1379.937422	53.450438	66.601153
1379.464917	45.016296	66.606158
1379.039403	54.435528	66.611162
1378.618464	46.340125	66.616167
1377.730522	52.109620	66.621172
1376.587308	44.876517	66.626177
1376.387133	49.778160	66.631182
1375.681116	53.296778	66.636186
1374.885648	46.637611	66.641191
1374.123400	46.941826	66.646196
1373.114452	46.171910	66.651201
1372.873526	41.212889	66.656206
1372.589184	42.258010	66.661210
1372.270929	43.625494	66.666215
1371.510215	42.871314	66.671220
1370.576522	43.305286	66.676225
1370.236758	37.415792	66.681230
1368.661486	51.013847	66.686234
1368.167630	48.834239	66.691239
1367.557497	47.239250	66.696244
1367.121865	42.155059	66.701249
1366.875554	39.767366	66.706254
1365.393126	46.623282	66.711258
1364.512908	40.814968	66.716263
1364.428734	47.442307	66.721268
1363.725443	52.524855	66.726273
1363.520754	45.612506	66.731278
1362.248426	49.874017	66.736282
1361.603327	52.730086	66.741287
1361.167618	40.940603	66.746292
1360.271822	46.944743	66.751297
1360.332037	46.504775	66.756302
1359.129830	46.057327	66.761306
1357.932764	44.062049	66.766311
1357.953954	47.957086	66.771316
1357.065405	51.728654	66.776321
1357.183927	36.414840	66.781326
1355.881350	54.216350	66.786330
1355.316207	46.798321	66.791335
1354.865570	45.827695	66.796340
1353.448154	49.629720	66.801345
1352.816833	44.743799	66.806350
1352.009069	55.043826	66.811354
1351.473426	49.647523	66.816359
1351.465263	45.715961	66.821364
1350.873905	50.026922	66.826369
1350.509931	39.176957	66.831374
1349.484694	40.928072	66.836378
1348.654494	48.516110	66.841383
1348.295442	36.444786	66.846388
1347.065433	45.900441	66.851393
1346.098804	44.805260	66.856398
1345.934515	53.299860	66.861402
1345.477773	39.211341	66.866407
1344.828049	44.831008	66.871412
1343.651679	51.505817	66.876417
1343.282108	34.845589	66.881422
1342.698758	43.884626	66.886426
1342.412381	47.481621	66.891431
1341.380219	44.249018	66.896436
1340.423523	51.197994	66.901441
1340.333663	45.294006	66.906446
1339.380569	50.531389	66.911450
1338.341311	44.387240	66.916455
1337.291953	40.485583	66.921460
1336.705795	49.457260	66.926465
1336.549868	47.164012	66.931470
1336.014702	47.359597	66.936474
1335.680558	56.116171	66.941479
1335.450729	46.892820	66.946484
1334.096361	51.332969	66.951489
1333.524224	50.285466	66.956494
1333.165712	57.375897	66.961498
1331.832363	49.299396	66.966503
1331.051150	56.900156	66.971508
1330.277550	50.481959	66.976513
1330.270310	39.553210	66.981518
1329.739340	50.235018	66.986522
1329.097248	41.909855	66.991527
1328.281536	39.554341	66.996532
1327.157248	49.072046	67.001537
1326.928425	45.192912	67.006542
1326.127515	50.309910	67.011546
1325.054668	42.915835	67.016551
1324.394051	47.751905	67.021556
1323.841878	48.885343	67.026561
1323.744837	42.674990	67.031566
1323.074427	54.265230	67.036570
1322.146010	49.677288	67.041575
1321.718257	49.676024	67.046580
1320.963457	51.576547	67.051585
1320.587103	47.154733	67.056590
1319.438604	41.783333	67.061594
1318.865216	38.987168	67.066599
1318.442312	33.519339	67.071604
1317.849479	43.386222	67.076609
1316.648449	43.567820	67.081614
1315.630898	47.736807	67.086618
1315.202915	43.133966	67.091623
1314.888701	43.553051	67.096628
1314.278548	47.937971	67.101633
1314.013797	38.773799	67.106638
1312.703969	42.016258	67.111642
1311.949659	42.625162	67.116647
1311.460208	40.919537	67.121652
1311.252648	43.453738	67.126657
1310.781706	40.472551	67.131662
1309.439732	50.141568	67.136666
1308.757804	42.562347	67.141671
1308.657766	44.642631	67.146676
1307.585159	49.536321	67.151681
1306.925829	44.453014	67.156686
1305.846749	45.480989	67.161690
1305.498230	47.493545	67.166695
1305.217915	49.488949	67.171700
1304.852183	57.667065	67.176705
1303.920248	42.408295	67.181710
1303.121627	48.609893	67.186714
1302.344049	50.941404	67.191719
1301.369987	41.655034	67.196724
1300.298247	53.408433	67.201729
1300.059791	47.387722	67.206734
1299.488433	49.104542	67.211738
1298.793786	52.156162	67.216743
1298.935874	46.502311	67.221748
1297.985999	45.415524	67.226753
1297.432162	42.379709	67.231758
1296.547782	51.610122	67.236762
1295.820001	51.364823	67.241767
1295.061270	47.606212	67.246772
1294.224216	46.766421	67.251777
1293.845621	42.114731	67.256782
1293.656789	45.562178	67.261786
1292.532350	45.143399	67.266791
1291.432500	47.934587	67.271796
1290.936735	50.924625	67.276801
1290.783785	41.709564	67.281806
1290.163973	41.593760	67.286810
1288.621978	47.807895	67.291815
1288.309211	38.656093	67.296820
1287.677892	43.545859	67.301825
1287.284873	42.728514	67.306830
1287.016085	44.736279	67.311834
1285.818537	50.618105	67.316839
1285.154726	41.279261	67.321844
1284.278250	46.116543	67.326849
1284.144323	46.051222	67.331854
1282.921737	45.100842	67.336858
1282.081910	48.571369	67.341863
1281.807887	43.590814	67.346868
1281.106057	47.701729	67.351873
1281.026799	46.952771	67.356878
1280.224385	52.249796	67.361882
1278.910923	56.492655	67.366887
1278.832020	46.496255	67.371892
1277.976360	49.723293	67.376897
1277.215447	49.417034	67.381902
1276.244858	43.843901	67.386906
1275.572506	47.513309	67.391911
1275.421128	41.543415	67.396916
1274.633533	53.682157	67.401921
1274.049965	42.939666	67.406926
1273.173272	45.722188	67.411930
1272.721366	52.671348	67.416935
1272.129965	41.986875	67.421940
1271.414381	45.850817	67.426945
1270.770719	50.266305	67.431950
1269.828538	46.519525	67.436954
1268.973204	48.090690	67.441959
1269.244854	35.250469	67.446964
1268.176359	45.565155	67.451969
1266.932532	39.672768	67.456974
1266.218288	43.413494	67.461978
1266.158777	51.336335	67.466983
1265.789949	39.468439	67.471988
1264.468324	51.927062	67.476993
1263.860824	44.531566	67.481998
1263.501974	46.176757	67.487002
1262.740677	48.436302	67.492007
1262.449238	46.257649	67.497012
1261.299199	40.825022	67.502017
1260.506507	50.228524	67.507022
1260.074887	50.767210	67.512026
1259.340957	46.433804	67.517031
1258.878503	37.077149	67.522036
1257.792472	57.279109	67.527041
1257.113563	44.884918	67.532046
1256.989394	46.872845	67.537050
1256.393228	52.841990	67.542055
1255.282308	46.698235	67.547060
1254.137827	50.354409	67.552065
1254.061788	45.996822	67.557070
1253.476481	57.928361	67.562074
1252.818208	51.629052	67.567079
1252.902396	45.285808	67.572084
1251.724801	49.992782	67.577089
1251.143922	46.519725	67.582094
1250.522986	48.372174	67.587098
1249.291096	43.916098	67.592103
1248.525729	48.103357	67.597108
1247.864043	53.231355	67.602113
1247.475822	44.067902	67.607118
1247.186019	45.680038	67.612122
1246.221473	48.684699	67.617127
1245.737893	42.162073	67.622132
1244.843409	51.012477	67.627137
1244.483787	35.858287	67.632142
1243.532079	46.813586	67.637146
1242.459219	42.259686	67.642151
1242.386364	44.908090	67.647156
1242.008155	49.215141	67.652161
1241.151278	45.292381	67.657166
1240.232708	43.399535	67.662170
1239.714323	50.449157	67.667175
1239.179027	41.443137	67.672180
1238.123856	53.685935	67.677185
1237.322478	47.205959	67.682190
1236.783004	39.566265	67.687194
1236.140244	47.829432	67.692199
1236.296134	44.811665	67.697204
1235.197460	51.458391	67.702209
1234.145821	50.930290	67.707214
1233.896654	56.334899	67.712218
1233.159622	55.040824	67.717223
1232.157767	46.911673	67.722228
1230.954684	46.330383	67.727233
1230.674760	41.735556	67.732238
1230.410402	47.148886	67.737242
1230.086130	49.406757	67.742247
1229.488704	42.526919	67.747252
1228.177279	50.617293	67.752257
1227.372256	44.147363	67.757262
1227.164461	39.758691	67.762266
1226.739353	40.539201	67.767271
1225.965837	39.840719	67.772276
1224.703755	44.755106	67.777281
1224.114177	41.568873	67.782286
1223.971136	47.935904	67.787290
1223.481877	43.290787	67.792295
1222.650894	42.604598	67.797300
1221.441020	49.325782	67.802305
1221.097812	47.961201	67.807310
1220.632694	40.344381	67.812314
1219.407933	51.608041	67.817319
1219.214610	38.996303	67.822324
1218.342049	36.654598	67.827329
1217.996431	43.927484	67.832334
1217.388418	45.080862	67.837338
1216.171753	47.852809	67.842343
1215.761945	42.296184	67.847348
1215.023712	40.477174	67.852353
1214.804702	40.048491	67.857358
1213.906257	42.134313	67.862362
1212.717941	42.427481	67.867367
1212.424490	42.833815	67.872372
1211.981720	44.940217	67.877377
1211.633608	44.820650	67.882382
1210.480592	40.173855	67.887386
1209.582475	42.426786	67.892391
1209.408511	47.152374	67.897396
1208.970986	47.546927	67.902401
1208.294231	35.980333	67.907406
1207.239374	44.362653	67.912410
1206.068776	47.128855	67.917415
1206.071506	44.127559	67.922420
1205.460377	51.322822	67.927425
1204.448469	39.445243	67.932430
1203.649215	48.696833	67.937434
1203.342994	45.467121	67.942439
1202.933647	42.378389	67.947444
1201.689329	47.431889	67.952449
1200.916998	45.768118	67.957454
1200.569914	48.486942	67.962458
1200.112764	50.046847	67.967463
1200.073924	36.018080	67.972468
1198.773845	50.964917	67.977473
1198.106581	46.239302	67.982478
1197.724772	41.875152	67.987482
1196.649747	43.620050	67.992487
1195.617510	42.115887	67.997492
1194.942160	54.017593	68.002497
1194.723961	53.650283	68.007502
1194.468828	38.345446	68.012506
1193.364821	49.213014	68.017511
1192.742259	49.558147	68.022516
1192.106821	45.163368	68.027521
1191.562325	52.862132	68.032526
1190.490360	41.956063	68.037530
1189.458195	47.253377	68.042535
1189.440652	42.006542	68.047540
1188.752788	49.903148	68.052545
1188.113771	51.580288	68.057550
1187.935818	46.843092	68.062554
1186.323413	59.436305	68.067559
1186.036649	47.306211	68.072564
1185.487130	45.237999	68.077569
1185.139227	45.522107	68.082574
1184.137116	39.545593	68.087578
1183.224937	44.079495	68.092583
1183.152212	48.442049	68.097588
1182.393908	46.823363	68.102593
1181.168823	57.211872	68.107598
1180.669270	43.518149	68.112602
1179.923546	45.245376	68.117607
1179.686746	41.381724	68.122612
1179.215737	39.791467	68.127617
1178.060503	46.992839	68.132622
1177.290604	46.815775	68.137626
1176.642022	49.383851	68.142631
1176.610764	47.509189	68.147636
1175.953851	45.294054	68.152641
1174.917065	50.912234	68.157646
1174.358599	46.298635	68.162650
1173.624425	44.877966	68.167655
1172.931714	43.445973	68.172660
1171.964132	47.465136	68.177665
1171.283933	45.742567	68.182670
1170.855935	45.561592	68.187674
1170.314096	51.843813	68.192679
1170.034859	39.551681	68.197684
1168.826793	47.945766	68.202689
1167.989744	48.235129	68.207694
1167.873722	51.054405	68.212698
1166.968263	51.785163	68.217703
1165.976222	40.696085	68.222708
1165.304810	42.490346	68.227713
1164.864331	46.324754	68.232718
1164.762505	43.183967	68.237722
1163.954266	47.113134	68.242727
1163.069283	38.618500	68.247732
1162.380623	44.184470	68.252737
1161.882683	45.558477	68.257742
1161.177599	39.955786	68.262746
1159.966809	41.399011	68.267751
1159.599137	42.511023	68.272756
1158.946687	52.926737	68.277761
1158.651651	49.064463	68.282766
1157.675365	45.282152	68.287770
1156.738884	42.130609	68.292775
1156.317903	40.087694	68.297780
1156.005524	41.372264	68.302785
1155.534767	37.033310	68.307790
1154.478303	36.012417	68.312794
1153.644247	46.195233	68.317799
1153.588794	37.466168	68.322804
1152.370994	46.522558	68.327809
1151.466021	42.314165	68.332814
1151.348905	43.083550	68.337818
1150.341804	46.897690	68.342823
1149.957489	39.067763	68.347828
1148.819597	39.630488	68.352833
1148.015175	41.021703	68.357838
1147.876465	39.697149	68.362842
1147.305355	37.618189	68.367847
1147.185630	33.018400	68.372852
1145.611204	44.725630	68.377857
1144.146390	45.184233	68.382862
1143.582900	34.069589	68.387866
1142.520762	41.159970	68.392871
1142.444879	39.147326	68.397876
1142.472577	46.805548	68.402881
1141.709800	41.106381	68.407886
1141.511826	40.062493	68.412890
1140.642522	39.111188	68.417895
1140.291236	33.499543	68.422900
1139.338293	36.816210	68.427905
1138.445050	41.074297	68.432910
1138.088457	36.673034	68.437914
1137.132535	48.877992	68.442919
1136.110112	44.357121	68.447924
1135.745910	48.385984	68.452929
1135.173988	46.368657	68.457934
1135.251483	46.335949	68.462938
1134.278080	48.378527	68.467943
1133.581419	40.792250	68.472948
1133.084207	43.703694	68.477953
1131.712653	51.007302	68.482958
1130.983121	43.512987	68.487962
1130.153248	46.945704	68.492967
1130.243175	39.262704	68.497972
1129.648390	43.325088	68.502977
1128.580669	41.626321	68.507982
1128.101841	36.602674	68.512986
1126.856691	45.783273	68.517991
1126.939353	44.130193	68.522996
1126.369720	41.808149	68.528001
1125.169087	41.370024	68.533006
1125.046083	39.282874	68.538010
1123.785303	47.321079	68.543015
1123.503414	37.948359	68.548020
1122.235920	43.127005	68.553025
1121.573342	46.771237	68.558030
1121.198116	38.345354	68.563034
1120.890679	35.368165	68.568039
1120.645237	29.211406	68.573044
1119.318277	39.371699	68.578049
1118.606755	33.281187	68.583054
1118.277684	35.118779	68.588058
1117.586240	45.233187	68.593063
1117.013290	36.184311	68.598068
1116.005288	39.870871	68.603073
1115.351764	36.057743	68.608078
1114.740021	38.560047	68.613082
1114.180873	37.209330	68.618087
1113.098921	39.226602	68.623092
1112.316880	38.717171	68.628097
1112.105396	38.315685	68.633102
1112.032218	31.609548	68.638106
1111.019820	40.767321	68.643111
1110.098327	27.810964	68.648116
1109.512955	40.114679	68.653121
1108.903056	35.510859	68.658126
1108.538726	36.732734	68.663130
1107.360562	39.774574	68.668135
1106.829980	36.206824	68.673140
1106.304809	38.737938	68.678145
1105.249663	38.145793	68.683150
1104.561555	32.114641	68.688154
1103.731894	41.055690	68.693159
1103.604574	41.807776	68.698164
1103.078733	38.535743	68.703169
1102.763411	39.486469	68.708174
1101.996290	34.481878	68.713178
1100.676917	40.870437	68.718183
1100.521250	33.611288	68.723188
1099.757274	40.020313	68.728193
1098.616826	38.233780	68.733198
1098.337747	35.870257	68.738202
1097.641590	43.328220	68.743207
1097.270922	33.688928	68.748212
1096.045336	37.876889	68.753217
1095.185936	39.127052	68.758222
1095.268991	41.201870	68.763226
1094.579016	47.395699	68.768231
1093.929357	35.392749	68.773236
1093.019813	36.819626	68.778241
1092.673952	34.357916	68.783246
1091.983422	39.547300	68.788250
1090.391671	47.365351	68.793255
1089.856993	38.293048	68.798260
1089.454212	47.511557	68.803265
1088.958336	44.906549	68.808270
1088.582734	42.777579	68.813274
1087.800055	49.035043	68.818279
1087.062941	36.598147	68.823284
1086.426364	39.006636	68.828289
1085.543939	44.160315	68.833294
1085.211466	38.220831	68.838298
1083.842120	48.477775	68.843303
1083.197382	46.494121	68.848308
1082.836498	37.003087	68.853313
1082.489386	38.338922	68.858318
1082.422989	44.375210	68.863322
1081.410507	46.526526	68.868327
1080.479434	38.438234	68.873332
1080.123902	34.520943	68.878337
1079.063351	43.659579	68.883342
1078.718707	37.540681	68.888346
1077.445043	36.522833	68.893351
1077.091766	42.869686	68.898356
1076.692720	37.163147	68.903361
1075.646340	36.675277	68.908366
1075.144749	28.512365	68.913370
1074.117991	42.430152	68.918375
1074.067002	36.933177	68.923380
1073.529692	40.022899	68.928385
1072.195304	36.631911	68.933390
1071.848387	37.090921	68.938394
1071.006129	42.419566	68.943399
1070.806490	34.729018	68.948404
1070.191756	33.978518	68.953409
1068.918444	43.729751	68.958414
1068.746644	34.251221	68.963418
1068.101395	38.741117	68.968423
1067.256846	34.526302	68.973428
1066.144143	37.083077	68.978433
1065.561787	39.498715	68.983438
1065.261411	37.815104	68.988442
1064.776988	40.976840	68.993447
1063.844060	37.733306	68.998452
1063.002579	44.441679	69.003457
1062.436294	41.789531	69.008462
1062.135269	36.127327	69.013466
1061.507920	45.228594	69.018471
1061.108426	34.054774	69.023476
1059.984468	43.798020	69.028481
1059.188731	45.850208	69.033486
1059.126661	32.919582	69.038490
1058.220787	41.552641	69.043495
1057.418599	35.375647	69.048500
1056.676089	31.981975	69.053505
1055.668514	37.541928	69.058510
1055.019544	38.440081	69.063514
1054.608188	40.918405	69.068519
1054.322843	33.269880	69.073524
1053.805910	39.149177	69.078529
1052.676249	38.360748	69.083534
1051.968930	41.329285	69.088538
1051.158964	46.370522	69.093543
1050.790023	41.137020	69.098548
1050.379861	42.446620	69.103553
1049.097377	40.271116	69.108558
1048.686486	35.858007	69.113562
1047.987362	36.379360	69.118567
1047.504018	28.678759	69.123572
1046.552276	37.341193	69.128577
1045.675691	45.207921	69.133582
1045.657224	33.319045	69.138586
1044.826944	36.889046	69.143591
1044.600003	32.727375	69.148596
1043.541400	41.182883	69.153601
1042.687296	35.517207	69.158606
1042.476144	30.424191	69.163610
1040.947091	44.114388	69.168615
1040.197546	42.814479	69.173620
1039.812624	35.126604	69.178625
1039.174580	43.187198	69.183630
1039.037596	33.821407	69.188634
1038.702652	37.385147	69.193639
1038.054058	34.727177	69.198644
1037.292653	22.844542	69.203649
1036.308433	29.879979	69.208654
1035.460350	28.825986	69.213658
1034.506307	30.537508	69.218663
1033.974960	32.276401	69.223668
1033.899690	35.637978	69.228673
1033.114703	40.883404	69.233678
1032.075623	26.723644	69.238682
1031.088525	31.342048	69.243687
1031.118523	28.024183	69.248692
1030.687452	36.253698	69.253697
1029.539665	36.499502	69.258702
1028.807327	31.584023	69.263706
1028.051370	40.098619	69.268711
1027.753419	32.377989	69.273716
1027.066758	34.051705	69.278721
1026.134764	36.606556	69.283726
1025.354584	26.559348	69.288730
1024.604984	31.682447	69.293735
1024.375109	35.122238	69.298740
1023.995309	28.436508	69.303745
1022.720004	41.217431	69.308750
1022.463113	32.176654	69.313754
1021.512529	36.234160	69.318759
1021.302991	26.260172	69.323764
1020.122160	27.619846	69.328769
1018.996058	31.790433	69.333774
1018.976666	32.492235	69.338778
1018.634539	33.346309	69.343783
1017.992427	29.704863	69.348788
1017.261758	34.153164	69.353793
1016.270846	38.497790	69.358798
1015.966007	28.207800	69.363802
1014.963033	37.799344	69.368807
1013.963979	35.249179	69.373812
1013.266251	32.054980	69.378817
1012.702432	37.153257	69.383822
1012.555687	27.710179	69.388826
1012.064162	35.696998	69.393831
1011.859196	28.135046	69.398836
1010.711154	25.275848	69.403841
1009.596187	35.049215	69.408846
1009.426818	31.941266	69.413850
1008.273560	42.605410	69.418855
1007.657528	33.680122	69.423860
1007.315763	30.922881	69.428865
1006.825314	42.276362	69.433870
1006.016802	36.814761	69.438874
1004.992580	47.652347	69.443879
1004.625698	40.106689	69.448884
1003.603715	46.946300	69.453889
1002.615628	46.535919	69.458894
1002.435794	45.011335	69.463898
1001.698531	38.458174	69.468903
1001.420082	38.538866	69.473908
1001.221626	34.801605	69.478913
1000.060323	36.019408	69.483918
999.302248	44.250496	69.488922
998.763754	40.871690	69.493927
997.752823	42.209074	69.498932
996.841688	43.265649	69.503937
996.230635	45.506093	69.508942
996.289843	36.424486	69.513946
995.378848	48.461480	69.518951
994.349675	42.697518	69.523956
993.690228	44.996125	69.528961
992.822063	44.951448	69.533966
992.725412	39.133735	69.538970
992.187998	42.852699	69.543975
991.179688	39.670074	69.548980
990.763662	36.465753	69.553985
990.018727	46.598154	69.558990
989.722841	37.115725	69.563994
988.339408	36.591633	69.568999
987.807436	40.163073	69.574004
987.161665	32.966152	69.579009
986.740131	43.714153	69.584014
986.607382	45.400674	69.589018
985.263023	37.882815	69.594023
984.536654	38.559909	69.599028
984.186719	33.364401	69.604033
983.049128	34.887525	69.609038
982.199307	39.439951	69.614042
981.750152	43.625849	69.619047
981.232963	44.708059	69.624052
981.081699	39.679636	69.629057
980.609467	47.787976	69.634062
979.528823	36.965410	69.639066
978.869819	36.836994	69.644071
978.140436	37.161328	69.649076
977.193179	34.151925	69.654081
976.333817	40.795354	69.659086
976.181310	35.797094	69.664090
975.512726	34.683021	69.669095
975.040325	33.138760	69.674100
974.163103	35.817378	69.679105
972.930597	37.836585	69.684110
973.295673	34.735065	69.689114
972.369158	40.088181	69.694119
971.071837	32.294765	69.699124
970.594125	33.231921	69.704129
970.040002	37.559101	69.709134
969.734700	35.579818	69.714138
969.062364	37.091997	69.719143
967.966840	39.018446	69.724148
967.449352	39.389492	69.729153
966.795364	37.334803	69.734158
966.348540	28.748465	69.739162
965.171706	39.657648	69.744167
964.293587	29.507775	69.749172
964.186715	31.134984	69.754177
963.183058	40.456991	69.759182
963.028883	35.525230	69.764186
962.905615	43.369883	69.769191
961.844107	48.466939	69.774196
961.125301	39.731484	69.779201
960.118730	51.640192	69.784206
959.568322	43.571806	69.789210
958.651579	41.705587	69.794215
958.121149	41.249208	69.799220
958.015542	36.620382	69.804225
956.834029	44.169797	69.809230
956.050216	36.494951	69.814234
955.132883	43.007262	69.819239
954.669912	43.423253	69.824244
954.564572	43.982611	69.829249
953.762797	46.778544	69.834254
953.259463	43.788397	69.839258
952.592193	48.920496	69.844263
952.170133	41.997070	69.849268
950.923071	44.015450	69.854273
949.927635	46.613540	69.859278
949.488637	46.740285	69.864282
949.470458	38.789066	69.869287
948.151056	42.427466	69.874292
947.533966	39.857550	69.879297
946.395846	45.737939	69.884302
946.499038	46.967443	69.889306
946.008328	47.859364	69.894311
945.313017	41.520323	69.899316
944.234033	37.292396	69.904321
943.599167	47.402560	69.909326
943.240832	39.571702	69.914330
942.573685	35.278242	69.919335
941.563441	43.021184	69.924340
941.099763	40.229735	69.929345
940.340174	50.615219	69.934350
940.141069	41.786032	69.939354
939.126147	42.985300	69.944359
938.108638	47.495039	69.949364
937.784830	46.346612	69.954369
937.142654	53.299276	69.959374
936.530945	35.821419	69.964378
935.746583	39.082944	69.969383
935.028354	47.681447	69.974388
934.426819	41.496223	69.979393
933.943794	43.845618	69.984398
933.268363	35.410783	69.989402
932.600640	34.545746	69.994407
931.753240	36.516305	69.999412
931.613538	33.917735	70.004417
930.090376	34.302166	70.009422
929.471828	33.443498	70.014426
929.098336	34.356191	70.019431
928.807010	41.752918	70.024436
928.564297	36.327467	70.029441
926.854066	39.007772	70.034446
926.360947	29.999876	70.039450
926.330864	38.228668	70.044455
924.864558	35.111072	70.049460
924.390248	37.962134	70.054465
923.562558	44.283568	70.059470
923.165932	39.305237	70.064474
922.784554	39.157887	70.069479
922.200188	29.385492	70.074484
921.201323	40.592802	70.079489
920.295723	37.743950	70.084494
920.199412	34.592845	70.089498
920.015429	30.208311	70.094503
918.389355	32.159285	70.099508
917.917776	29.042669	70.104513
917.434621	36.020485	70.109518
916.789853	35.249572	70.114522
915.934421	40.845286	70.119527
915.060151	37.750174	70.124532
914.981400	37.792788	70.129537
913.906140	40.692178	70.134542
913.045905	34.351012	70.139546
912.218883	33.555486	70.144551
911.828536	40.837083	70.149556
911.838774	28.940508	70.154561
910.941458	49.631318	70.159566
910.270684	33.071209	70.164570
909.332659	36.013416	70.169575
908.847058	45.500582	70.174580
908.267253	36.974842	70.179585
907.163311	31.897767	70.184590
906.723152	40.814722	70.189594
906.242377	29.970854	70.194599
905.173766	37.794057	70.199604
904.520935	37.533790	70.204609
903.610990	40.190830	70.209614
903.561512	36.852498	70.214618
903.046017	29.600182	70.219623
902.235222	44.649023	70.224628
901.414135	32.476312	70.229633
900.570775	41.025346	70.234638
900.259132	37.093218	70.239642
899.761944	43.082937	70.244647
899.111677	42.699260	70.249652
898.416724	32.450879	70.254657
897.604822	46.113745	70.259662
896.340137	34.614034	70.264666
895.761108	35.543673	70.269671
895.029311	43.289625	70.274676
894.583276	35.723475	70.279681
894.302339	38.657309	70.284686
894.185788	35.173533	70.289690
893.280095	37.076109	70.294695
892.390380	42.085923	70.299700
891.932236	34.882828	70.304705
890.504080	40.913476	70.309710
889.613715	38.866465	70.314714
889.142964	38.988813	70.319719
888.771551	28.848220	70.324724
888.437510	30.967328	70.329729
887.516241	42.875088	70.334734
887.333323	31.357765	70.339738
886.531804	28.145431	70.344743
885.597974	36.144310	70.349748
885.169808	33.818736	70.354753
883.902248	35.536055	70.359758
883.265162	30.185993	70.364762
882.681601	36.202074	70.369767
882.515199	35.041220	70.374772
882.093068	25.448027	70.379777
880.736666	38.331793	70.384782
880.213615	36.453410	70.389786
879.689824	37.560344	70.394791
879.292494	35.081628	70.399796
878.482529	26.740770	70.404801
877.498994	35.670086	70.409806
877.011437	29.671750	70.414810
876.545971	33.021310	70.419815
875.906472	37.584447	70.424820
874.887761	32.823409	70.429825
874.205872	33.370451	70.434830
873.769150	34.755267	70.439834
872.897968	30.486418	70.444839
871.989331	39.542591	70.449844
871.705805	39.023281	70.454849
870.995039	35.569424	70.459854
870.804352	33.376370	70.464858
870.065651	33.785797	70.469863
868.843989	39.384618	70.474868
868.446297	37.500478	70.479873
868.204426	41.509896	70.484878
867.331622	37.891016	70.489882
866.516033	41.900282	70.494887
865.749402	42.471853	70.499892
865.286366	33.509648	70.504897
864.066926	38.906265	70.509902
863.421563	31.966367	70.514906
863.216118	32.295655	70.519911
862.540843	32.835339	70.524916
862.272702	30.750809	70.529921
861.043704	36.399685	70.534926
860.362682	28.911950	70.539930
860.008819	21.458881	70.544935
859.253982	42.062354	70.549940
858.189978	35.383054	70.554945
857.632525	34.883690	70.559950
857.460998	35.329006	70.564954
856.872923	29.116437	70.569959
855.698774	39.211516	70.574964
855.044940	26.553314	70.579969
854.283774	34.450601	70.584974
853.561778	36.360224	70.589978
853.550066	37.868210	70.594983
852.472561	30.618626	70.599988
851.678775	27.162221	70.604993
851.165893	37.961034	70.609998
850.597877	32.415484	70.615002
850.657462	32.604817	70.620007
849.109865	31.029863	70.625012
848.810828	30.508294	70.630017
848.011123	37.913398	70.635022
847.469307	33.014965	70.640026
846.501365	24.232484	70.645031
845.509022	38.162193	70.650036
845.361974	25.115825	70.655041
845.054318	27.118773	70.660046
844.221906	23.316856	70.665050
843.616644	35.164861	70.670055
842.609553	31.769218	70.675060
842.081273	29.346047	70.680065
840.925715	32.554715	70.685070
840.139981	27.543721	70.690074
839.880806	29.310293	70.695079
839.442084	27.685006	70.700084
839.330329	29.410766	70.705089
838.185879	29.471620	70.710094
837.381356	27.519778	70.715098
837.080229	28.342118	70.720103
836.117923	29.739633	70.725108
835.097994	28.508057	70.730113
834.601407	30.837548	70.735118
834.185432	27.649022	70.740122
833.715747	23.339939	70.745127
832.407146	30.882815	70.750132
832.061867	32.245198	70.755137
831.532999	31.394357	70.760142
831.007379	29.968985	70.765146
830.078712	31.947779	70.770151
829.083194	37.838629	70.775156
828.596830	32.773679	70.780161
828.175405	30.428120	70.785166
827.631307	29.105038	70.790170
826.807322	30.061067	70.795175
825.596176	31.466656	70.800180
825.460998	25.279781	70.805185
824.872465	31.752404	70.810190
824.566353	31.485855	70.815194
823.998642	41.150100	70.820199
822.761913	36.075278	70.825204
822.573839	32.505121	70.830209
821.443906	33.729050	70.835214
820.353275	30.619530	70.840218
820.088379	29.324548	70.845223
819.180666	33.159253	70.850228
819.295992	27.645291	70.855233
818.489309	38.437257	70.860238
817.663714	29.509125	70.865242
817.190456	18.914834	70.870247
816.498676	22.473890	70.875252
815.208140	15.914259	70.880257
814.391398	22.754368	70.885262
813.687056	32.963910	70.890266
813.534574	25.723223	70.895271
813.269472	37.785171	70.900276
812.731772	28.096849	70.905281
811.601520	34.266196	70.910286
810.860746	25.890698	70.915290
810.817417	18.869184	70.920295
809.451774	25.716245	70.925300
809.080809	25.149360	70.930305
808.188292	30.255836	70.935310
807.795290	20.910344	70.940314
807.352214	28.517306	70.945319
806.036832	29.964728	70.950324
805.578306	26.879176	70.955329
805.191287	43.210455	70.960334
804.462297	27.574308	70.965338
803.417609	33.821501	70.970343
802.567847	41.803870	70.975348
802.595077	31.448452	70.980353
801.725395	39.230562	70.985358
801.144973	36.046141	70.990362
800.548720	25.843593	70.995367
799.636748	31.363180	71.000372
799.327602	40.118937	71.005377
798.647841	41.105634	71.010382
797.495465	33.838032	71.015386
797.230392	20.474572	71.020391
796.297911	27.333111	71.025396
796.010406	28.736764	71.030401
794.833861	31.456779	71.035406
794.097159	29.450000	71.040410
793.732400	25.124223	71.045415
793.341288	40.265542	71.050420
792.858008	31.959445	71.055425
791.972871	30.383152	71.060430
791.061293	37.252563	71.065434
790.854753	28.859837	71.070439
789.522032	36.351380	71.075444
788.955950	28.260320	71.080449
788.493563	36.072213	71.085454
787.702605	28.267688	71.090458
787.582068	24.759326	71.095463
786.066509	31.519878	71.100468
785.652555	25.490927	71.105473
784.937512	29.189314	71.110478
784.535153	24.820639	71.115482
784.356412	31.994438	71.120487
783.454092	39.792787	71.125492
782.527903	24.856680	71.130497
782.085736	30.588490	71.135502
781.133092	29.707351	71.140506
780.272608	26.236358	71.145511
779.891842	25.136447	71.150516
779.385802	22.864294	71.155521
778.850865	26.554511	71.160526
777.874693	33.453131	71.165530
777.312333	26.616746	71.170535
776.531431	26.615023	71.175540
776.237286	33.181139	71.180545
775.357903	29.867699	71.185550
774.198069	27.996096	71.190554
773.758834	25.602921	71.195559
773.095846	34.228924	71.200564
773.113128	19.719799	71.205569
772.336831	25.798116	71.210574
771.251691	27.976883	71.215578
770.695915	26.087967	71.220583
770.094456	32.654121	71.225588
769.229993	21.675841	71.230593
768.446910	38.688335	71.235598
767.833331	33.252565	71.240602
767.570777	32.282071	71.245607
767.114276	35.622335	71.250612
766.059539	27.139139	71.255617
765.438421	31.902800	71.260622
764.626218	32.308189	71.265626
764.331715	26.433692	71.270631
763.160827	37.108606	71.275636
762.840538	28.148940	71.280641
762.341757	31.093809	71.285646
761.520067	26.681508	71.290650
760.863186	22.422744	71.295655
760.053096	36.407037	71.300660
759.695948	28.746350	71.305665
758.597696	32.963072	71.310670
757.471146	29.231668	71.315674
757.185919	26.064920	71.320679
756.558740	31.392523	71.325684
756.365094	22.762786	71.330689
755.983861	24.331176	71.335694
755.226693	31.950301	71.340698
754.418645	29.249990	71.345703
753.730237	30.652816	71.350708
752.590709	28.666027	71.355713
751.378442	30.273680	71.360718
750.818872	33.013762	71.365722
750.652431	28.434067	71.370727
750.281465	31.826948	71.375732
750.109963	29.957283	71.380737
749.258636	26.544769	71.385742
748.509269	37.277160	71.390746
747.984683	26.083926	71.395751
747.175475	34.506129	71.400756
746.318016	39.791550	71.405761
745.524956	28.719906	71.410766
744.932978	40.923781	71.415770
744.016669	37.450649	71.420775
742.996077	32.054455	71.425780
742.690978	31.145930	71.430785
742.195282	41.304925	71.435790
741.773091	27.501283	71.440794
741.379412	27.530963	71.445799
740.103618	28.215173	71.450804
739.404800	22.562749	71.455809
739.201522	26.086628	71.460814
738.189169	29.337195	71.465818
737.480351	25.832610	71.470823
736.660014	31.373897	71.475828
736.331102	25.656273	71.480833
735.972234	27.514420	71.485838
735.230546	34.158100	71.490842
734.692887	25.494825	71.495847
733.614447	27.267262	71.500852
733.190793	28.738329	71.505857
732.155104	31.461177	71.510862
731.618815	28.798032	71.515866
731.293013	29.543887	71.520871
730.595936	39.296548	71.525876
730.015155	38.349915	71.530881
729.154422	30.782027	71.535886
728.348454	41.279007	71.540890
728.062379	18.414546	71.545895
726.623362	33.535040	71.550900
726.208087	26.061814	71.555905
725.809217	29.064898	71.560910
725.495676	32.948536	71.565914
724.975556	23.180176	71.570919
723.627758	34.640211	71.575924
722.962089	24.136505	71.580929
722.688480	27.028182	71.585934
721.595347	31.371836	71.590938
720.706522	27.399173	71.595943
720.183590	30.597055	71.600948
719.946638	30.021462	71.605953
719.692318	29.729334	71.610958
718.401812	36.894064	71.615962
717.906248	31.488406	71.620967
717.157667	27.649534	71.625972
716.807893	22.622792	71.630977
715.690610	28.299673	71.635982
714.725432	33.468210	71.640986
714.285360	27.673670	71.645991
713.793897	29.710628	71.650996
713.382076	31.318587	71.656001
712.725881	22.650540	71.661006
711.465779	22.892293	71.666010
711.157052	18.291106	71.671015
710.547468	31.360379	71.676020
710.195813	21.771784	71.681025
709.187476	21.738485	71.686030
708.155192	23.912015	71.691034
708.041506	11.371311	71.696039
707.216933	25.454103	71.701044
706.744927	19.740347	71.706049
705.580537	26.263675	71.711054
705.091617	24.496595	71.716058
704.739356	16.466140	71.721063
704.010292	28.406406	71.726068
703.550069	20.970308	71.731073
702.599520	23.313754	71.736078
701.951365	31.667745	71.741082
701.955773	18.687183	71.746087
700.638268	29.207261	71.751092
699.788132	25.072328	71.756097
699.641851	20.409006	71.761102
698.818699	31.793397	71.766106
697.803199	19.809444	71.771111
696.910945	34.278339	71.776116
696.627034	30.548414	71.781121
696.332344	28.278897	71.786126
695.545803	37.515948	71.791130
694.906674	21.709431	71.796135
693.841534	28.590702	71.801140
693.262692	24.940856	71.806145
693.199805	24.066313	71.811150
691.861183	27.048723	71.816154
691.490777	21.156366	71.821159
690.737203	31.298072	71.826164
690.183888	29.889757	71.831169
689.442603	18.324196	71.836174
688.373946	33.075071	71.841178
688.327539	30.163621	71.846183
687.607717	29.469375	71.851188
687.004263	37.745291	71.856193
686.139528	27.973465	71.861198
685.376017	32.766122	71.866202
685.017204	21.109698	71.871207
683.926009	28.545480	71.876212
683.150271	26.477143	71.881217
682.908792	24.181809	71.886222
682.462031	27.438531	71.891226
681.891447	24.361388	71.896231
680.566810	30.486041	71.901236
680.077437	28.299566	71.906241
679.907488	21.731891	71.911246
678.873589	30.402775	71.916250
677.884925	17.637118	71.921255
677.067053	26.174254	71.926260
676.840530	30.356277	71.931265
676.499229	20.702964	71.936270
675.617183	34.782306	71.941274
674.427336	22.651082	71.946279
674.106088	27.234544	71.951284
673.654326	26.959668	71.956289
673.450596	35.030007	71.961294
672.536467	36.410450	71.966298
671.617495	24.072089	71.971303
671.033950	32.646034	71.976308
670.578286	22.189334	71.981313
669.158993	23.196053	71.986318
668.423910	23.472497	71.991322
668.340186	17.012522	71.996327
667.859479	24.067242	72.001332
667.331310	23.730417	72.006337
666.499747	17.170328	72.011342
665.699364	26.570433	72.016346
665.314004	15.564800	72.021351
664.100214	29.313764	72.026356
663.416699	21.506376	72.031361
662.611975	23.881810	72.036366
662.212480	23.152333	72.041370
662.203910	21.163691	72.046375
661.413895	28.523136	72.051380
659.981902	29.710079	72.056385
659.834195	28.511574	72.061390
659.044507	26.721434	72.066394
658.799329	17.704106	72.071399
657.351243	27.828677	72.076404
657.136572	25.872855	72.081409
656.707456	22.965581	72.086414
655.641898	22.250706	72.091418
654.650238	22.954368	72.096423
653.922960	29.488536	72.101428
653.714483	33.024287	72.106433
653.316182	30.525269	72.111438
652.897612	34.578604	72.116442
651.989210	21.912141	72.121447
651.534207	22.322186	72.126452
650.594907	22.411959	72.131457
649.211874	21.448021	72.136462
648.514922	25.440028	72.141466
648.440060	27.256113	72.146471
647.788716	29.674936	72.151476
647.543759	23.451948	72.156481
646.435588	22.985139	72.161486
645.609894	28.167755	72.166490
644.863264	20.111804	72.171495
644.721967	24.092597	72.176500
644.257305	22.447824	72.181505
643.723944	20.823454	72.186510
642.719843	20.683850	72.191514
642.040207	16.453981	72.196519
640.692740	29.872579	72.201524
640.209696	26.365187	72.206529
639.993262	25.882530	72.211534
639.225357	31.525881	72.216538
639.168151	20.223564	72.221543
638.111891	34.122498	72.226548
637.337372	33.077429	72.231553
637.025895	26.082862	72.236558
635.521105	33.888883	72.241562
634.993889	30.438989	72.246567
634.471877	27.779903	72.251572
633.785893	27.654298	72.256577
633.658794	22.529033	72.261582
632.636486	27.168949	72.266586
631.759093	35.859083	72.271591
631.322409	29.672936	72.276596
630.765848	27.970260	72.281601
630.087668	32.772997	72.286606
628.949610	33.826415	72.291610
628.602130	28.763053	72.296615
628.066234	32.309946	72.301620
627.464344	27.458990	72.306625
626.451869	27.798546	72.311630
625.658315	27.822539	72.316634
625.471889	17.832338	72.321639
625.134097	27.215553	72.326644
624.429715	29.642828	72.331649
623.468372	25.629713	72.336654
622.460088	28.955369	72.341658
622.106303	26.657427	72.346663
621.689866	33.815463	72.351668
620.819628	30.532165	72.356673
620.262478	23.592497	72.361678
619.344508	31.327148	72.366682
618.566642	25.603774	72.371687
617.400271	29.441889	72.376692
616.879753	24.618978	72.381697
616.819376	20.616925	72.386702
616.202292	24.616721	72.391706
615.944177	19.217432	72.396711
615.076654	26.739042	72.401716
614.266047	27.926399	72.406721
613.870661	23.662305	72.411726
612.420924	28.329300	72.416730
611.747329	20.129266	72.421735
611.069915	29.487723	72.426740
610.875180	28.402367	72.431745
610.731905	31.098254	72.436750
609.638161	32.754907	72.441754
608.555195	28.004227	72.446759
608.153543	34.499163	72.451764
607.778001	24.968012	72.456769
607.615255	23.108006	72.461774
606.021347	29.562584	72.466778
605.561500	28.871113	72.471783
605.011256	31.379502	72.476788
603.929148	27.861871	72.481793
602.975535	29.075160	72.486798
602.465113	35.049677	72.491802
602.230630	25.467676	72.496807
601.674834	20.927934	72.501812
601.371047	32.751603	72.506817
600.703695	27.559418	72.511822
599.839524	36.340495	72.516826
599.102062	25.301064	72.521831
598.140064	26.264953	72.526836
597.388156	25.981124	72.531841
596.928257	25.412666	72.536846
596.465570	32.166483	72.541850
595.602281	25.408044	72.546855
594.602682	24.553380	72.551860
594.015795	28.773877	72.556865
593.746427	21.293219	72.561870
593.142708	33.065309	72.566874
592.880955	29.528992	72.571879
591.718160	35.090168	72.576884
590.879530	26.310869	72.581889
590.446053	30.325584	72.586894
589.287528	30.067094	72.591898
588.900719	20.348510	72.596903
588.208402	32.022747	72.601908
587.660421	31.826289	72.606913
587.806387	26.666999	72.611918
586.227368	27.629817	72.616922
585.564328	19.112720	72.621927
585.038197	37.221299	72.626932
584.687518	34.698939	72.631937
584.047818	29.839823	72.636942
582.772552	34.408084	72.641946
582.744621	29.565073	72.646951
581.822698	29.425022	72.651956
580.651860	34.310967	72.656961
580.327397	29.854232	72.661966
579.625635	31.136228	72.666970
579.476222	35.130933	72.671975
578.833474	35.547240	72.676980
578.156016	32.212753	72.681985
576.970341	26.809816	72.686990
576.256599	33.885898	72.691994
576.303570	33.198866	72.696999
575.092541	42.708561	72.702004
574.419146	37.580421	72.707009
574.071465	36.128342	72.712014
572.854382	36.885288	72.717018
571.801997	28.341893	72.722023
571.492403	32.964510	72.727028
571.205673	38.236348	72.732033
570.812331	29.827682	72.737038
570.435048	37.950896	72.742042
569.423421	28.975231	72.747047
568.480580	31.566658	72.752052
567.878888	33.624353	72.757057
567.765380	32.147592	72.762062
566.314256	38.413874	72.767066
565.590848	37.311802	72.772071
565.292883	39.194964	72.777076
564.924611	37.402388	72.782081
564.271011	30.837643	72.787086
563.058136	28.446310	72.792090
562.200480	30.806550	72.797095
562.129424	33.736942	72.802100
561.318152	40.738678	72.807105
560.727604	28.433215	72.812110
559.972675	44.181266	72.817114
559.475478	39.644812	72.822119
558.612023	37.825454	72.827124
557.491879	38.633198	72.832129
557.185823	26.801244	72.837134
556.671180	38.188568	72.842138
556.226936	36.393902	72.847143
555.606253	41.305772	72.852148
554.551210	37.610385	72.857153
553.935811	37.003625	72.862158
553.256159	40.895132	72.867162
552.892824	35.386451	72.872167
552.047291	40.523371	72.877172
551.421916	38.953100	72.882177
551.078041	33.681019	72.887182
550.326679	37.913533	72.892186
549.183840	29.876569	72.897191
548.769918	32.937267	72.902196
548.422873	31.860408	72.907201
547.679386	24.182463	72.912206
546.359457	38.126577	72.917210
546.015644	30.302965	72.922215
545.991034	30.346428	72.927220
544.570654	28.759290	72.932225
543.924091	25.916637	72.937230
543.454023	29.266978	72.942234
542.868003	35.598899	72.947239
542.390262	40.057491	72.952244
541.356515	38.913396	72.957249
540.665724	36.254406	72.962254
539.943843	41.090935	72.967258
539.784707	29.552549	72.972263
539.141129	25.936711	72.977268
537.930142	38.352748	72.982273
537.976822	34.373067	72.987278
536.633442	37.564475	72.992282
536.075777	37.498883	72.997287
534.938271	40.133947	73.002292
534.018708	42.475674	73.007297
534.252832	34.263534	73.012302
533.982073	29.689443	73.017306
533.499249	27.039908	73.022311
532.435423	31.959289	73.027316
531.713396	43.892167	73.032321
531.094689	27.407522	73.037326
530.223289	34.803620	73.042330
529.450414	26.001258	73.047335
529.085996	30.276217	73.052340
528.219017	32.850844	73.057345
527.823965	29.078725	73.062350
526.656019	29.660708	73.067354
526.010678	27.571652	73.072359
525.895651	34.639106	73.077364
525.024112	37.343771	73.082369
524.279482	27.259574	73.087374
523.157515	34.968401	73.092378
522.882203	35.469695	73.097383
522.590501	27.385475	73.102388
522.248635	32.796985	73.107393
521.294173	18.207729	73.112398
520.443506	24.611768	73.117402
519.711542	26.937807	73.122407
518.674962	30.966602	73.127412
517.763855	33.040480	73.132417
517.544225	35.218675	73.137422
516.609511	36.556720	73.142426
516.348112	42.611432	73.147431
516.058881	32.041526	73.152436
515.550358	33.149253	73.157441
514.705644	28.729674	73.162446
514.131573	37.567063	73.167450
512.888831	35.305092	73.172455
512.001412	37.439854	73.177460
511.286985	39.875068	73.182465
511.269055	34.757653	73.187470
510.664162	30.903846	73.192474
509.986569	37.570484	73.197479
509.375635	31.740132	73.202484
508.545496	40.569430	73.207489
507.649897	32.243942	73.212494
506.675187	37.970735	73.217498
506.208014	30.319748	73.222503
505.921786	32.560592	73.227508
505.270993	28.979029	73.232513
504.872843	30.621111	73.237518
503.907644	34.343650	73.242522
503.397717	33.934568	73.247527
503.171611	24.300791	73.252532
501.733657	32.687592	73.257537
501.233893	32.363624	73.262542
500.481669	33.981688	73.267546
499.677486	38.837644	73.272551
498.945262	29.350724	73.277556
497.964977	36.811486	73.282561
497.546518	32.746633	73.287566
497.165811	30.271650	73.292570
496.851949	35.426388	73.297575
496.460081	31.918697	73.302580
495.340386	40.861935	73.307585
494.880941	28.366876	73.312590
493.818481	39.715321	73.317594
492.704415	30.879016	73.322599
492.309377	35.906337	73.327604
491.679190	42.041878	73.332609
491.668715	34.914228	73.337614
491.150246	40.710271	73.342618
489.967693	34.198277	73.347623
489.183496	28.665195	73.352628
488.433466	42.529584	73.357633
488.107678	34.228446	73.362638
487.323196	36.569169	73.367642
486.332455	35.247935	73.372647
486.264164	32.808338	73.377652
485.566444	34.882926	73.382657
484.559172	27.690153	73.387662
483.800043	39.291476	73.392666
483.099036	29.659239	73.397671
482.935137	30.391947	73.402676
482.362712	36.934602	73.407681
481.510914	31.185210	73.412686
480.836559	35.019117	73.417690
480.211448	34.163187	73.422695
479.183545	34.158330	73.427700
478.131860	31.839131	73.432705
478.240009	29.358811	73.437710
477.523689	34.311161	73.442714
476.723492	30.855911	73.447719
476.239630	25.755960	73.452724
475.365368	34.921876	73.457729
475.014584	26.180025	73.462734
474.336677	29.875726	73.467738
472.947181	26.550633	73.472743
472.543359	27.029827	73.477748
471.586414	30.965528	73.482753
471.659022	27.263995	73.487758
471.079931	35.316863	73.492762
470.459036	29.995892	73.497767
469.698481	29.027502	73.502772
468.886239	38.323890	73.507777
468.393983	23.713060	73.512782
466.955230	33.243301	73.517786
466.332281	27.969968	73.522791
466.210243	25.936330	73.527796
465.492473	26.993825	73.532801
465.233551	32.534051	73.537806
464.458121	34.349788	73.542810
463.524874	24.737216	73.547815
463.044088	33.607056	73.552820
462.007211	33.166818	73.557825
461.163249	16.975148	73.562830
460.680680	33.509287	73.567834
460.295222	28.489856	73.572839
459.971461	28.973644	73.577844
459.259153	27.991262	73.582849
458.812753	31.799895	73.587854
458.245611	29.871865	73.592858
456.859289	30.028200	73.597863
456.331707	28.179023	73.602868
455.493703	38.274306	73.607873
455.108708	35.050957	73.612878
453.853199	31.296094	73.617882
453.100798	32.341764	73.622887
453.057728	26.974470	73.627892
452.224041	32.417035	73.632897
451.889435	33.277868	73.637902
451.016213	36.771305	73.642906
449.953177	32.184683	73.647911
449.616390	30.174222	73.652916
449.139215	37.975890	73.657921
448.582344	37.867613	73.662926
447.589528	32.074469	73.667930
446.782360	25.221996	73.672935
446.693924	33.542046	73.677940
445.886252	42.924447	73.682945
445.164950	27.845487	73.687950
444.415375	37.671216	73.692954
443.849940	35.104248	73.697959
442.991429	32.468858	73.702964
441.831082	39.335428	73.707969
441.586536	29.348206	73.712974
440.955953	33.962050	73.717978
440.416412	34.243677	73.722983
440.324675	29.015025	73.727988
438.741718	27.386044	73.732993
438.638703	26.257705	73.737998
437.894203	41.437979	73.743002
437.248931	35.551618	73.748007
436.614842	33.135940	73.753012
435.603557	34.429444	73.758017
435.373424	24.268041	73.763022
434.682798	30.214520	73.768026
433.280922	36.362636	73.773031
432.801398	26.780288	73.778036
432.298593	34.538730	73.783041
431.971987	27.682233	73.788046
431.588803	36.042939	73.793050
430.691487	31.707467	73.798055
429.940259	31.786280	73.803060
429.150740	32.369514	73.808065
428.607809	16.830067	73.813070
427.710055	20.609691	73.818074
426.791502	22.514475	73.823079
426.511979	19.794725	73.828084
425.910606	29.735611	73.833089
425.604584	20.783215	73.838094
424.510859	24.032670	73.843098
423.610250	25.994520	73.848103
423.339935	32.217809	73.853108
422.776581	43.327480	73.858113
422.013774	26.383295	73.863118
421.285843	34.530848	73.868122
420.718217	31.098486	73.873127
420.314351	34.353143	73.878132
418.703867	35.204385	73.883137
418.389355	28.626662	73.888142
417.734846	34.403388	73.893146
417.365063	31.794214	73.898151
417.200699	26.548752	73.903156
415.988096	25.105204	73.908161
415.737621	21.699581	73.913166
414.955409	21.229825	73.918170
413.717185	35.137313	73.923175
413.344869	27.106961	73.928180
412.800918	28.669786	73.933185
412.435294	31.530418	73.938190
411.108346	30.865185	73.943194
410.187440	27.227343	73.948199
410.124563	25.920722	73.953204
409.201958	33.525284	73.958209
408.981284	30.747272	73.963214
407.842007	27.153689	73.968218
407.091404	27.095214	73.973223
406.784976	23.771049	73.978228
406.325573	30.844485	73.983233
405.683953	23.361676	73.988238
404.713080	31.175780	73.993242
403.950282	32.926443	73.998247
403.850367	26.522688	74.003252
402.315257	34.048232	74.008257
401.908655	29.163070	74.013262
401.180338	33.108096	74.018266
400.802224	30.205362	74.023271
400.712046	35.024842	74.028276
399.424790	37.464629	74.033281
398.734710	32.963683	74.038286
398.023646	33.673197	74.043290
397.804318	32.593356	74.048295
397.014557	22.076435	74.053300
395.841090	29.008188	74.058305
395.395687	28.528923	74.063310
394.988160	39.298372	74.068314
393.989812	28.877763	74.073319
393.265260	28.419325	74.078324
392.545647	32.232079	74.083329
392.738990	34.746600	74.088334
391.983600	34.647892	74.093338
390.725246	34.231937	74.098343
390.267878	30.882939	74.103348
389.432863	33.351591	74.108353
389.130913	27.631315	74.113358
388.116085	32.352131	74.118362
387.223283	34.596603	74.123367
386.865522	18.228146	74.128372
386.343907	34.336423	74.133377
386.150553	25.463851	74.138382
384.817303	29.789130	74.143386
384.063187	29.062592	74.148391
383.740741	31.539454	74.153396
382.975207	33.284252	74.158401
382.140916	31.632201	74.163406
381.394998	32.109154	74.168410
380.907829	26.971907	74.173415
381.057780	31.526038	74.178420
379.559463	38.099559	74.183425
378.965926	30.913445	74.188430
378.358091	39.212184	74.193434
377.877548	35.799071	74.198439
376.835056	29.392556	74.203444
375.922237	38.585144	74.208449
375.645247	25.386113	74.213454
375.220349	37.216468	74.218458
374.650151	29.936751	74.223463
373.729528	33.046679	74.228468
372.649906	39.668601	74.233473
372.240982	35.963378	74.238478
371.870312	38.597738	74.243482
370.847733	29.909348	74.248487
370.262962	29.901730	74.253492
369.428604	38.359569	74.258497
369.114999	34.293804	74.263502
369.039651	31.511562	74.268506
368.124370	24.110222	74.273511
367.558681	31.683149	74.278516
366.681517	30.839030	74.283521
365.774933	36.868827	74.288526
365.111319	30.237936	74.293530
364.434645	34.747178	74.298535
363.897392	29.548530	74.303540
363.036006	39.453595	74.308545
362.072398	29.918447	74.313550
361.844350	30.393302	74.318554
361.396544	31.250109	74.323559
360.862046	26.841078	74.328564
359.490043	34.621351	74.333569
358.743835	27.689812	74.338574
358.757618	28.958762	74.343578
358.109957	26.646195	74.348583
357.002325	27.677540	74.353588
356.263232	24.824457	74.358593
355.911201	22.154119	74.363598
355.357267	34.246310	74.368602
354.642376	35.533613	74.373607
353.739630	27.833812	74.378612
353.150353	32.291281	74.383617
352.707163	23.106870	74.388622
352.379677	27.768622	74.393626
350.910362	27.966628	74.398631
350.444923	30.250238	74.403636
349.755743	24.765147	74.408641
349.278754	29.102218	74.413646
348.923967	28.163819	74.418650
347.984929	29.149376	74.423655
347.207549	27.513499	74.428660
346.526706	37.854997	74.433665
346.495556	26.846612	74.438670
345.282359	19.223104	74.443674
344.529033	28.759284	74.448679
344.449271	22.177283	74.453684
343.020694	28.772821	74.458689
342.351130	27.619659	74.463694
341.810987	25.696817	74.468698
341.242123	26.500380	74.473703
340.963255	23.676459	74.478708
340.006342	29.577086	74.483713
339.252180	20.027501	74.488718
338.817812	24.124391	74.493722
338.200952	24.733752	74.498727
337.680532	19.530855	74.503732
336.677228	32.713376	74.508737
335.937974	25.326575	74.513742
335.451391	28.203338	74.518746
334.320060	26.485104	74.523751
333.614665	21.587654	74.528756
332.830682	25.754456	74.533761
332.453603	29.607251	74.538766
332.445245	27.954475	74.543770
331.593788	29.913255	74.548775
331.089675	24.762952	74.553780
330.213717	24.921599	74.558785
329.723635	23.859685	74.563790
329.153812	19.394794	74.568794
327.644071	29.310151	74.573799
327.144045	19.226482	74.578804
326.816314	22.497399	74.583809
326.585260	22.673114	74.588814
326.145851	18.398752	74.593818
324.878810	19.707829	74.598823
324.359549	27.041548	74.603828
323.424260	31.257700	74.608833
322.225500	23.704442	74.613838
322.263027	26.071898	74.618842
321.696277	34.302593	74.623847
321.508219	16.930976	74.628852
320.001524	29.775834	74.633857
319.447116	24.264543	74.638862
319.080063	23.488953	74.643866
318.200226	25.934808	74.648871
317.139807	20.813249	74.653876
316.139831	26.091541	74.658881
315.968939	23.510612	74.663886
315.829241	25.576731	74.668890
314.901384	26.653558	74.673895
314.760327	17.804208	74.678900
313.614569	21.520894	74.683905
313.082013	17.546810	74.688910
312.781907	32.157946	74.693914
311.895996	32.743964	74.698919
311.028458	24.658526	74.703924
310.208375	23.160356	74.708929
309.736530	22.384122	74.713934
308.787401	18.060117	74.718938
307.872071	26.183940	74.723943
307.695750	16.395616	74.728948
307.146081	24.790742	74.733953
306.589429	15.345312	74.738958
305.509426	21.497378	74.743962
304.766919	33.510819	74.748967
304.513190	22.372338	74.753972
303.906173	19.427259	74.758977
303.061867	20.091804	74.763982
302.396328	19.318059	74.768986
301.497325	27.485015	74.773991
301.283630	19.342680	74.778996
300.397423	22.964388	74.784001
299.618062	23.506619	74.789006
298.949342	21.399277	74.794010
298.260089	23.220250	74.799015
298.386988	21.777730	74.804020
297.043876	27.517575	74.809025
296.498405	31.471331	74.814030
296.217628	29.207539	74.819034
294.563529	24.223192	74.824039
294.143038	22.338062	74.829044
293.549414	35.009020	74.834049
293.215969	23.580471	74.839054
292.790427	26.266163	74.844058
291.520466	24.437581	74.849063
291.107219	22.095557	74.854068
290.526992	24.991984	74.859073
289.771500	20.966706	74.864078
289.465324	22.608351	74.869082
288.171915	34.730104	74.874087
287.410597	24.106193	74.879092
286.853231	28.840862	74.884097
286.503056	26.722174	74.889102
286.521802	25.404125	74.894106
285.423479	29.280422	74.899111
284.720366	22.548625	74.904116
284.164774	25.229816	74.909121
282.968554	27.948462	74.914126
282.194162	22.349243	74.919130
281.510923	34.339049	74.924135
281.243477	28.606985	74.929140
280.798423	27.550520	74.934145
280.320165	27.379288	74.939150
279.442322	22.241261	74.944154
278.315596	34.024212	74.949159
278.220674	25.762021	74.954164
277.300890	31.678829	74.959169
276.772779	27.364997	74.964174
276.502510	26.540871	74.969178
275.502044	32.396423	74.974183
274.524706	22.989668	74.979188
273.910292	27.132612	74.984193
273.464899	28.479482	74.989198
272.408702	27.378507	74.994202
271.408868	28.615057	74.999207
271.321414	22.636687	75.004212
270.771501	34.094309	75.009217
270.305623	29.428359	75.014222
269.678648	32.863678	75.019226
268.659321	35.248206	75.024231
268.524044	20.187889	75.029236
267.257061	33.344649	75.034241
266.088433	30.930647	75.039246
265.569384	32.721345	75.044250
264.850722	31.790497	75.049255
264.879848	20.917600	75.054260
264.929494	27.137200	75.059265
263.882667	29.237531	75.064270
262.887383	27.380950	75.069274
262.257202	29.548908	75.074279
261.327560	15.971401	75.079284
260.368233	25.143040	75.084289
259.592487	25.500204	75.089294
259.766024	20.672411	75.094298
259.049215	29.337040	75.099303
258.319495	19.269505	75.104308
257.298890	36.073918	75.109313
256.742287	28.102942	75.114318
256.424433	22.842544	75.119322
255.312519	29.767696	75.124327
254.600993	18.107692	75.129332
254.176407	33.735305	75.134337
253.340912	24.607148	75.139342
253.148808	25.256056	75.144346
251.955395	29.696305	75.149351
251.191424	20.932065	75.154356
250.664060	29.230606	75.159361
250.439786	27.978103	75.164366
249.727472	29.905268	75.169370
248.631282	29.148146	75.174375
248.271364	27.119327	75.179380
247.669312	26.299207	75.184385
246.712429	22.031656	75.189390
246.077170	23.358334	75.194394
245.078919	27.433160	75.199399
245.325570	26.684332	75.204404
244.810260	31.577885	75.209409
243.926059	34.570088	75.214414
242.997332	27.211948	75.219418
241.970184	33.103304	75.224423
241.859332	28.019645	75.229428
240.701640	24.192539	75.234433
239.639572	28.668625	75.239438
239.172854	24.203092	75.244442
239.208048	26.364336	75.249447
238.789622	24.083072	75.254452
238.259587	25.385093	75.259457
237.083328	27.501336	75.264462
236.474003	21.719702	75.269466
235.505841	28.484750	75.274471
234.911774	18.124365	75.279476
234.272571	23.040821	75.284481
233.550870	23.261644	75.289486
233.402869	25.067315	75.294490
232.101468	25.401050	75.299495
231.480654	28.415925	75.304500
231.055210	31.863279	75.309505
230.621014	28.810245	75.314510
229.978694	26.127857	75.319514
228.578683	28.937363	75.324519
228.364350	26.264019	75.329524
227.844990	31.216568	75.334529
227.204392	30.885146	75.339534
226.134827	19.708008	75.344538
225.490522	32.417011	75.349543
224.992269	21.461034	75.354548
224.237425	31.215101	75.359553
224.088573	30.619206	75.364558
223.270324	28.994617	75.369562
222.726314	29.329043	75.374567
221.919822	24.723714	75.379572
220.957086	30.836621	75.384577
220.135762	32.662900	75.389582
219.693166	25.101117	75.394586
219.084819	36.482906	75.399591
218.864873	27.516830	75.404596
218.136412	33.165037	75.409601
217.044791	22.168037	75.414606
216.658293	23.488180	75.419610
215.819295	27.431973	75.424615
214.947964	26.031893	75.429620
214.118734	23.838201	75.434625
213.553661	31.442591	75.439630
213.404149	23.219075	75.444634
212.412169	28.037236	75.449639
212.264735	25.312228	75.454644
211.299843	32.325923	75.459649
210.565289	32.446300	75.464654
210.386822	24.875528	75.469658
209.154351	35.961001	75.474663
208.441105	34.688685	75.479668
208.147144	30.451082	75.484673
207.506790	33.598388	75.489678
206.752148	27.138184	75.494682
205.670435	35.848385	75.499687
205.221199	29.773154	75.504692
204.795616	22.442054	75.509697
204.171624	29.224783	75.514702
203.199270	25.402842	75.519706
202.471450	25.266681	75.524711
202.248678	21.859826	75.529716
201.261056	25.138188	75.534721
200.363989	35.706568	75.539726
199.894068	26.422381	75.544730
199.180635	31.683418	75.549735
199.075879	22.358364	75.554740
198.250790	26.386677	75.559745
197.172478	25.106333	75.564750
197.019455	25.936672	75.569754
196.173159	34.949967	75.574759
195.119583	24.617118	75.579764
194.332240	22.120288	75.584769
193.838425	26.844841	75.589774
193.499026	16.175788	75.594778
192.959533	30.840852	75.599783
192.172491	32.846179	75.604788
191.456217	28.890374	75.609793
190.811722	31.022785	75.614798
190.420673	23.298252	75.619802
189.649931	21.620370	75.624807
188.868531	22.516198	75.629812
188.183414	26.944822	75.634817
187.229309	31.455756	75.639822
186.673272	19.364136	75.644826
186.130914	27.299221	75.649831
185.807075	20.248372	75.654836
184.902296	24.134852	75.659841
183.601126	26.062876	75.664846
183.694200	30.641823	75.669850
182.754940	29.995330	75.674855
182.562846	23.372908	75.679860
181.471996	25.227977	75.684865
180.436705	29.348157	75.689870
180.226106	19.899632	75.694874
179.575420	21.615139	75.699879
179.098234	23.451218	75.704884
178.389814	18.812925	75.709889
177.380719	32.665039	75.714894
177.133514	30.534682	75.719898
176.261391	34.417538	75.724903
175.119843	25.503792	75.729908
174.676903	32.270277	75.734913
173.997640	34.111768	75.739918
174.036905	22.669560	75.744922
172.784755	29.501984	75.749927
171.822625	30.286284	75.754932
171.693272	27.397548	75.759937
170.982548	31.246786	75.764942
170.515366	22.909923	75.769946
169.462240	25.782425	75.774951
168.839201	19.022136	75.779956
168.512956	19.384931	75.784961
167.766612	25.376619	75.789966
167.075721	26.369987	75.794970
166.283325	28.073399	75.799975
165.768721	21.240628	75.804980
165.520616	16.803337	75.809985
164.172751	29.269707	75.814990
163.535178	22.344578	75.819994
162.753953	29.376312	75.824999
162.490551	23.433891	75.830004
161.348557	24.015061	75.835009
160.500900	20.611650	75.840014
160.282690	28.917680	75.845018
159.716340	32.624054	75.850023
159.360541	29.651575	75.855028
158.779531	18.540082	75.860033
157.516160	26.538091	75.865038
157.229441	18.904166	75.870042
156.595400	28.899181	75.875047
155.851994	15.725698	75.880052
155.034924	22.816762	75.885057
154.366384	27.078747	75.890062
154.073991	20.645788	75.895066
152.642454	26.737269	75.900071
152.097874	29.602811	75.905076
151.689975	16.719610	75.910081
150.750679	30.044935	75.915086
151.096167	23.715272	75.920090
149.918211	24.614417	75.925095
148.955461	30.288957	75.930100
148.577020	34.509421	75.935105
148.009059	35.792277	75.940110
147.600329	26.657621	75.945114
146.014930	20.329905	75.950119
145.715081	20.283218	75.955124
145.498609	23.522221	75.960129
144.494544	26.420026	75.965134
143.736991	18.736599	75.970138
143.243734	21.660189	75.975143
142.875734	26.132876	75.980148
142.116069	25.364722	75.985153
141.074585	30.684388	75.990158
140.650316	17.969380	75.995162
140.207059	20.449760	76.000167
139.011472	18.582594	76.005172
138.198441	14.771549	76.010177
137.890307	16.195903	76.015182
137.899904	15.133203	76.020186
136.513815	30.385847	76.025191
135.800794	21.950998	76.030196
135.546953	18.883420	76.035201
134.592852	23.951033	76.040206
134.312453	16.691421	76.045210
133.120897	27.311500	76.050215
132.334934	17.103176	76.055220
131.753825	17.427767	76.060225
131.230283	35.447626	76.065230
130.862182	19.139249	76.070234
129.612036	17.369097	76.075239
129.049939	19.762772	76.080244
128.966134	21.979256	76.085249
128.133219	28.640771	76.090254
127.376718	17.033725	76.095258
126.391202	25.356448	76.100263
126.089298	16.148000	76.105268
125.745225	9.122474	76.110273
124.737583	23.833799	76.115278
124.205621	22.562565	76.120282
123.469521	29.448340	76.125287
122.778081	15.572727	76.130292
121.845743	16.189869	76.135297
120.908076	19.953880	76.140302
120.533811	15.497290	76.145306
120.239812	23.952597	76.150311
119.716522	24.378358	76.155316
118.873479	24.255865	76.160321
117.826513	30.748089	76.165326
117.704366	21.957253	76.170330
117.222064	20.769565	76.175335
115.760773	30.573225	76.180340
115.194816	19.156572	76.185345
114.444946	29.703074	76.190350
114.521858	24.140056	76.195354
113.466252	35.135860	76.200359
112.429170	30.417531	76.205364
111.638197	29.219140	76.210369
111.021917	34.840022	76.215374
110.932715	24.271437	76.220378
110.400901	36.432664	76.225383
109.206030	31.416222	76.230388
108.758673	30.390119	76.235393
108.206185	28.229606	76.240398
107.991397	25.305614	76.245402
107.132725	25.527815	76.250407
106.379711	23.627938	76.255412
106.088284	34.402537	76.260417
104.858338	30.757332	76.265422
104.123528	29.677721	76.270426
103.244646	30.942358	76.275431
102.798211	29.783646	76.280436
102.629927	20.580701	76.285441
101.783192	32.385291	76.290446
100.969270	31.499646	76.295450
100.031368	28.437077	76.300455
99.720948	26.053461	76.305460
99.251536	21.473274	76.310465
98.157974	23.524354	76.315470
97.846620	25.029650	76.320474
97.260677	26.736431	76.325479
96.335114	30.929030	76.330484
95.764101	23.597495	76.335489
95.008761	30.254533	76.340494
94.196615	27.974582	76.345498
93.470381	30.030164	76.350503
92.544641	22.192227	76.355508
92.522074	22.968651	76.360513
91.551309	31.536617	76.365518
91.428276	30.296372	76.370522
90.265729	28.382960	76.375527
89.382937	22.135627	76.380532
89.132836	18.471372	76.385537
88.753065	22.493356	76.390542
87.719136	24.393004	76.395546
87.020800	32.352979	76.400551
86.481413	26.517660	76.405556
86.028458	18.049244	76.410561
84.715926	33.701765	76.415566
84.205433	30.988935	76.420570
83.745561	39.182121	76.425575
83.376370	33.365390	76.430580
82.355116	18.589909	76.435585
81.568595	39.291528	76.440590
81.132955	26.822772	76.445594
80.776453	15.363270	76.450599
80.176346	26.303784	76.455604
78.970780	28.028959	76.460609
78.246932	32.763407	76.465614
78.046211	22.170035	76.470618
77.056228	32.871533	76.475623
76.496020	24.098523	76.480628
75.673907	14.881585	76.485633
75.388508	27.725754	76.490638
74.759255	31.044783	76.495642
73.838567	28.086713	76.500647
72.850679	27.022241	76.505652
72.761806	27.102766	76.510657
71.744086	33.005294	76.515662
70.970194	22.326713	76.520666
70.450801	28.242808	76.525671
69.787049	32.053042	76.530676
69.878814	24.921744	76.535681
68.522673	26.696168	76.540686
67.849085	20.749795	76.545690
67.223573	19.689035	76.550695
66.628805	22.630405	76.555700
65.757239	11.948488	76.560705
64.503567	22.606880	76.565710
64.262921	21.959404	76.570714
63.904228	28.691963	76.575719
63.297842	27.054143	76.580724
63.433763	22.098305	76.585729
62.183965	36.789931	76.590734
61.715551	21.029006	76.595738
60.767567	33.657152	76.600743
59.714384	24.346180	76.605748
59.317928	15.531295	76.610753
58.375759	29.245030	76.615758
58.053449	21.585261	76.620762
57.235291	32.454903	76.625767
56.311855	31.375427	76.630772
56.145426	23.154634	76.635777
55.337376	22.425763	76.640782
55.230428	26.472049	76.645786
53.770685	31.248174	76.650791
53.234252	31.008995	76.655796
52.849439	25.552733	76.660801
52.141900	29.226451	76.665806
51.298595	32.611164	76.670810
50.923332	29.963507	76.675815
50.074148	32.398255	76.680820
49.634960	25.463601	76.685825
48.304643	30.359435	76.690830
47.475828	24.160282	76.695834
47.184172	20.669816	76.700839
46.637913	26.724240	76.705844
46.596664	17.581470	76.710849
45.701308	24.640894	76.715854
44.798297	16.170153	76.720858
44.270806	17.239996	76.725863
43.396540	30.605438	76.730868
42.676721	20.889649	76.735873
41.614900	29.817504	76.740878
41.478522	22.965445	76.745882
40.937722	19.549410	76.750887
40.543338	16.315027	76.755892
39.828716	25.886094	76.760897
38.740751	25.123026	76.765902
38.739129	27.480946	76.770906
37.075320	30.898755	76.775911
36.275225	31.860692	76.780916
35.974349	21.407882	76.785921
35.405955	31.468140	76.790926
35.105351	25.541136	76.795930
34.707701	28.514152	76.800935
33.744580	26.130569	76.805940
33.348241	13.556224	76.810945
32.065280	24.646654	76.815950
31.004965	24.019528	76.820954
30.358086	32.158964	76.825959
29.966610	27.033353	76.830964
30.014560	24.583128	76.835969
29.228293	31.790740	76.840974
28.457000	21.248959	76.845978
27.600728	24.772940	76.850983
26.920764	26.333883	76.855988
26.892378	27.311509	76.860993
25.289080	25.599315	76.865998
24.682388	23.456930	76.871002
24.390012	19.900352	76.876007
23.596474	29.540781	76.881012
23.114761	20.572345	76.886017
21.657731	27.932674	76.891022
21.174070	25.627164	76.896026
21.115486	25.496279	76.901031
20.639216	20.628624	76.906036
20.389180	13.362616	76.911041
19.196658	29.434407	76.916046
18.680788	22.914115	76.921050
17.818500	27.014647	76.926055
16.491969	22.952813	76.931060
16.184058	18.296426	76.936065
15.464142	36.082682	76.941070
15.259031	21.189677	76.946074
14.659412	30.597329	76.951079
13.622271	24.663230	76.956084
13.405701	14.805686	76.961089
12.490655	24.902311	76.966094
11.784576	19.287569	76.971098
10.947255	21.387700	76.976103
10.422886	25.327101	76.981108
10.049711	24.623500	76.986113
9.063761	32.435401	76.991118
8.292855	21.485136	76.996122
7.914934	20.582019	77.001127
6.887854	27.845392	77.006132
6.753110	14.872937	77.011137
6.001727	32.320434	77.016142
5.366059	19.957730	77.021147
4.940458	19.789193	77.026151
3.473048	14.813132	77.031156
3.037241	14.087983	77.036161