Fri Mar 05 19:33:44 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.461658	93.852256	0.000000
-0.511137	90.162346	0.005005
-1.455245	56.143687	0.010010
-2.809588	26.005179	0.015014
-6.805920	0.602675	0.020019
-11.702238	-12.206260	0.025024
-17.048544	2.443377	0.030029
-21.572990	7.388304	0.035034
-25.254715	-1.985805	0.040038
-29.277440	1.294273	0.045043
-32.539474	-3.906368	0.050048
-36.457516	2.567680	0.055053
-40.395047	6.696775	0.060058
-44.010528	-3.654537	0.065062
-47.823127	3.793029	0.070067
-51.505895	-1.670050	0.075072
-55.198881	-1.356724	0.080077
-58.919775	8.121526	0.085082
-62.658604	6.726461	0.090086
-66.876760	0.965620	0.095091
-70.407987	-1.634220	0.100096
-74.031835	10.550375	0.105101
-77.929096	7.094312	0.110106
-81.636566	4.584105	0.115110
-85.611086	5.166318	0.120115
-88.959025	-4.555826	0.125120
-92.704826	3.425194	0.130125
-96.371383	-1.313429	0.135130
-100.113191	3.396387	0.140134
-104.526001	4.844915	0.145139
-107.935527	2.921144	0.150144
-111.689197	6.383932	0.155149
-115.680506	4.195030	0.160154
-119.149387	1.478082	0.165158
-122.844447	5.306847	0.170163
-126.467650	-2.272412	0.175168
-130.498958	-4.771871	0.180173
-134.574624	-1.462675	0.185178
-138.146021	-11.918633	0.190182
-141.933154	1.659309	0.195187
-145.974058	3.322958	0.200192
-149.940774	1.145960	0.205197
-153.646838	0.773975	0.210202
-156.849792	4.265647	0.215206
-161.088475	8.266370	0.220211
-164.542215	1.642563	0.225216
-168.293376	9.878440	0.230221
-171.772449	6.212298	0.235226
-175.339641	-14.024463	0.240230
-179.444637	0.096261	0.245235
-182.926251	-2.970219	0.250240
-186.771964	0.332329	0.255245
-191.019229	-4.611515	0.260250
-194.531209	-4.298478	0.265254
-198.553448	3.517080	0.270259
-202.238265	-8.527581	0.275264
-205.809282	-3.258244	0.280269
-209.710526	-4.677620	0.285274
-213.011852	-6.427697	0.290278
-217.134018	1.003294	0.295283
-220.707822	-2.437922	0.300288
-224.608803	2.560832	0.305293
-228.332566	2.622293	0.310298
-232.161389	-2.903920	0.315302
-236.042708	-1.338132	0.320307
-239.411747	-2.880248	0.325312
-243.675687	-2.155389	0.330317
-247.236655	-5.500841	0.335322
-250.709386	-10.714851	0.340326
-254.679283	-5.791784	0.345331
-258.333192	-9.384156	0.350336
-262.469897	11.134679	0.355341
-265.983005	0.024643	0.360346
-269.806907	-11.307004	0.365350
-273.826856	2.647331	0.370355
-277.368526	-4.101039	0.375360
-281.048182	-4.642621	0.380365
-284.742357	-6.407160	0.385370
-288.459095	-8.276901	0.390374
-292.584058	2.023111	0.395379
-296.039466	1.892031	0.400384
-299.801736	-3.089611	0.405389
-303.739816	1.371145	0.410394
-307.257947	-7.842536	0.415398
-311.288057	2.316209	0.420403
-315.127649	0.754701	0.425408
-318.819083	3.660669	0.430413
-322.641978	6.652285	0.435418
-326.118681	-1.841015	0.440422
-329.991430	4.441756	0.445427
-333.666574	-0.716165	0.450432
-337.210153	-2.138815	0.455437
-341.141991	-6.675429	0.460442
-345.056079	-4.725770	0.465446
-348.708034	-1.343517	0.470451
-352.620278	-6.766325	0.475456
-356.598562	-4.175623	0.480461
-360.422124	5.171218	0.485466
-363.971666	-4.570367	0.490470
-367.616079	4.164416	0.495475
-371.502133	1.713138	0.500480
-374.812265	-0.246618	0.505485
-378.544773	-5.114612	0.510490
-382.273963	-2.555755	0.515494
-386.498594	2.143272	0.520499
-390.332145	-4.023737	0.525504
-394.050726	-10.888754	0.530509
-397.969616	-1.741103	0.535514
-401.387809	-1.220391	0.540518
-405.253303	-2.583654	0.545523
-408.840340	0.840362	0.550528
-412.664746	0.241673	0.555533
-416.801250	5.633148	0.560538
-420.257306	-4.564817	0.565542
-423.909551	-0.042281	0.570547
-427.604977	0.007079	0.575552
-431.449392	-6.317396	0.580557
-435.746710	-0.927019	0.585562
-438.958526	-11.764764	0.590566
-442.698276	-4.129549	0.595571
-446.493943	-6.229286	0.600576
-450.376388	-3.245309	0.605581
-454.349560	5.903217	0.610586
-457.756840	-1.746266	0.615590
-461.963003	4.443300	0.620595
-465.543164	-3.892913	0.625600
-469.076869	-0.152477	0.630605
-473.057416	6.283349	0.635610
-476.854384	7.484395	0.640614
-480.317990	7.440045	0.645619
-483.907907	-1.325087	0.650624
-487.759131	0.255222	0.655629
-491.723591	2.829746	0.660634
-495.504206	-3.958970	0.665638
-499.877228	2.620004	0.670643
-503.265164	-6.751356	0.675648
-506.502725	-6.778155	0.680653
-510.320074	-2.705356	0.685658
-514.198635	-6.428602	0.690662
-518.169481	-2.791739	0.695667
-522.303285	-7.511827	0.700672
-525.745834	-10.623458	0.705677
-529.453800	-3.191884	0.710682
-532.981133	-12.638699	0.715686
-536.794037	-0.623551	0.720691
-540.297239	-9.493899	0.725696
-544.247235	-5.551246	0.730701
-548.313075	-1.489157	0.735706
-551.861938	-4.553807	0.740710
-555.852112	-0.596831	0.745715
-559.448623	-1.138648	0.750720
-563.053252	-8.874713	0.755725
-566.890453	1.993202	0.760730
-570.742522	-3.725851	0.765734
-574.778358	6.454727	0.770739
-578.556610	4.636268	0.775744
-582.030690	-3.696205	0.780749
-585.910363	10.991556	0.785754
-589.080096	-0.328935	0.790758
-593.213502	-1.024625	0.795763
-596.974519	-1.145872	0.800768
-600.723878	5.781498	0.805773
-605.071296	5.892715	0.810778
-608.277230	-0.189694	0.815782
-612.168031	5.538166	0.820787
-615.628911	-5.481882	0.825792
-619.507474	-5.693121	0.830797
-623.715758	0.534903	0.835802
-627.143183	-1.806298	0.840806
-631.032465	8.606419	0.845811
-634.839500	-12.165239	0.850816
-638.472130	-1.309404	0.855821
-642.418339	0.164905	0.860826
-645.793891	-5.183883	0.865830
-649.839839	-5.615907	0.870835
-653.379904	0.577941	0.875840
-657.129756	-10.149864	0.880845
-661.247879	-2.515367	0.885850
-664.906660	-7.353676	0.890854
-668.559918	-2.002725	0.895859
-672.099934	-8.607240	0.900864
-675.874074	-5.020473	0.905869
-680.209393	-3.496543	0.910874
-683.530151	2.840500	0.915878
-687.471576	-2.089804	0.920883
-691.215781	-7.616156	0.925888
-694.691616	-13.636385	0.930893
-698.228303	-0.901902	0.935898
-702.128489	-11.223989	0.940902
-706.284139	-8.345754	0.945907
-710.130577	-4.085071	0.950912
-713.790372	-6.526203	0.955917
-717.505512	-4.662925	0.960922
-721.220028	-17.072540	0.965926
-725.268228	-0.725531	0.970931
-728.699593	-6.530470	0.975936
-732.236476	-15.395130	0.980941
-736.704279	-2.783026	0.985946
-740.193162	-1.898876	0.990950
-743.924934	4.242164	0.995955
-747.384936	-7.689280	1.000960
-751.057846	-10.733798	1.005965
-755.088816	-4.376196	1.010970
-758.927920	-12.714703	1.015974
-762.850586	-5.820896	1.020979
-766.408524	7.596739	1.025984
-769.867261	-1.661976	1.030989
-774.164485	3.281131	1.035994
-777.631774	-8.639637	1.040998
-781.471005	3.838970	1.046003
-785.049134	8.176738	1.051008
-788.599647	7.590072	1.056013
-792.884644	-1.374118	1.061018
-796.384952	5.630432	1.066022
-800.418580	8.347405	1.071027
-804.034061	2.672928	1.076032
-807.413553	5.991820	1.081037
-811.397216	7.046624	1.086042
-815.175247	4.283932	1.091046
-819.198034	14.741935	1.096051
-822.875279	7.875738	1.101056
-826.755531	1.221771	1.106061
-830.500593	14.122216	1.111066
-833.789038	9.179243	1.116070
-837.818661	11.269597	1.121075
-841.480225	7.174746	1.126080
-845.382808	8.252915	1.131085
-849.137767	18.589308	1.136090
-852.958920	1.986542	1.141094
-856.253684	12.386567	1.146099
-860.052822	4.395067	1.151104
-863.696847	2.855229	1.156109
-868.204494	10.435655	1.161114
-871.898087	-5.063109	1.166118
-875.552468	14.493314	1.171123
-879.144652	7.328186	1.176128
-882.908526	4.490802	1.181133
-886.830350	18.250634	1.186138
-890.329097	3.476092	1.191142
-894.649763	-0.207372	1.196147
-898.104274	12.607294	1.201152
-901.791184	10.325329	1.206157
-905.766913	18.465748	1.211162
-909.100460	5.180252	1.216166
-913.099623	9.987643	1.221171
-916.909104	9.190268	1.226176
-920.468038	6.042638	1.231181
-924.634151	13.357253	1.236186
-928.109454	7.471329	1.241190
-931.915135	13.832629	1.246195
-935.489794	6.984907	1.251200
-939.055072	3.210704	1.256205
-943.066673	5.014507	1.261210
-947.005627	7.104740	1.266214
-950.491367	9.381126	1.271219
-954.512410	8.893605	1.276224
-957.923711	7.627356	1.281229
-962.012328	-1.500373	1.286234
-965.622002	1.913894	1.291238
-969.508585	6.476297	1.296243
-973.327992	17.132257	1.301248
-976.722629	2.386941	1.306253
-980.803394	7.970726	1.311258
-984.379870	4.714040	1.316262
-988.106948	-0.259484	1.321267
-991.784744	5.917455	1.326272
-995.951049	-0.108586	1.331277
-999.773211	18.358376	1.336282
-1003.388041	1.826965	1.341286
-1007.203461	5.520200	1.346291
-1011.205119	1.601438	1.351296
-1014.784984	1.095502	1.356301
-1018.722062	2.452283	1.361306
-1022.233498	3.793035	1.366310
-1025.784205	1.169372	1.371315
-1029.606837	3.343638	1.376320
-1033.130128	5.973074	1.381325
-1037.092970	4.407231	1.386330
-1040.687808	0.773531	1.391334
-1044.578156	-2.639435	1.396339
-1048.494979	1.216737	1.401344
-1052.262583	-1.903617	1.406349
-1056.116696	10.029017	1.411354
-1059.620580	2.703405	1.416358
-1063.711802	2.443337	1.421363
-1067.238077	-3.658136	1.426368
-1071.369983	4.286753	1.431373
-1074.946983	14.218128	1.436378
-1078.299829	2.609108	1.441382
-1082.128389	1.466555	1.446387
-1085.843827	6.402309	1.451392
-1089.450215	1.559455	1.456397
-1094.107728	7.330304	1.461402
-1097.801253	11.379494	1.466406
-1101.621022	7.584755	1.471411
-1104.725558	-0.189436	1.476416
-1108.331597	-2.307388	1.481421
-1112.557880	2.721165	1.486426
-1116.166501	2.406063	1.491430
-1119.916939	6.861776	1.496435
-1123.817524	5.500583	1.501440
-1127.338280	0.888514	1.506445
-1131.389846	11.056734	1.511450
-1134.725299	1.014063	1.516454
-1138.528569	5.675372	1.521459
-1142.802191	6.944279	1.526464
-1146.120705	-2.643774	1.531469
-1150.134079	10.446714	1.536474
-1153.806381	3.127697	1.541478
-1157.498683	7.941591	1.546483
-1161.487309	-0.036418	1.551488
-1164.894536	2.104720	1.556493
-1168.636118	6.309938	1.561498
-1172.640953	2.647430	1.566502
-1176.297729	17.998989	1.571507
-1180.292817	8.487694	1.576512
-1183.606063	0.952009	1.581517
-1187.621731	8.309229	1.586522
-1191.362853	4.276557	1.591526
-1195.118565	7.856462	1.596531
-1198.805431	16.022093	1.601536
-1202.316691	6.272577	1.606541
-1206.514019	6.353007	1.611546
-1210.215670	-6.556139	1.616550
-1213.998891	5.344888	1.621555
-1217.862606	11.119843	1.626560
-1221.283209	4.057124	1.631565
-1225.424189	12.539883	1.636570
-1229.189071	5.888651	1.641574
-1232.900950	-0.291668	1.646579
-1236.935095	4.441435	1.651584
-1240.385012	1.049784	1.656589
-1244.198061	8.212249	1.661594
-1247.777643	6.189628	1.666598
-1251.163957	7.012391	1.671603
-1255.282828	4.230855	1.676608
-1258.933768	4.564556	1.681613
-1263.270609	14.947378	1.686618
-1266.631801	6.418143	1.691622
-1270.348812	9.675012	1.696627
-1273.868020	1.540079	1.701632
-1277.550916	3.487384	1.706637
-1281.713988	11.595313	1.711642
-1285.501188	1.005444	1.716646
-1289.222796	10.845152	1.721651
-1293.097888	9.248359	1.726656
-1296.460144	5.972070	1.731661
-1300.309974	4.276631	1.736666
-1304.229042	-0.974715	1.741670
-1307.861752	4.391255	1.746675
-1312.022061	15.922293	1.751680
-1315.522741	2.222656	1.756685
-1319.371313	0.721010	1.761690
-1323.084192	2.502878	1.766694
-1326.832997	6.403577	1.771699
-1330.485205	8.122131	1.776704
-1334.015716	1.345258	1.781709
-1338.138808	11.482688	1.786714
-1341.775004	4.079359	1.791718
-1345.769867	8.233936	1.796723
-1349.662369	14.896789	1.801728
-1353.205972	8.025846	1.806733
-1357.143485	7.583999	1.811738
-1360.628028	-7.925288	1.816742
-1364.011902	1.095656	1.821747
-1367.957563	8.629621	1.826752
-1371.381277	-8.310191	1.831757
-1376.243876	4.205407	1.836762
-1379.700669	-2.531154	1.841766
-1383.181944	3.572340	1.846771
-1386.830749	8.702893	1.851776
-1390.395024	-0.638864	1.856781
-1394.336019	-3.805006	1.861786
-1398.271419	-4.283389	1.866790
-1402.056219	0.209805	1.871795
-1405.935747	13.015927	1.876800
-1409.630786	-1.059279	1.881805
-1413.869177	10.668926	1.886810
-1417.110577	1.109943	1.891814
-1420.242669	-0.763281	1.896819
-1424.354279	1.117279	1.901824
-1428.273242	-8.210199	1.906829
-1432.104881	2.765370	1.911834
-1436.120699	-10.651306	1.916838
-1439.755186	-7.823692	1.921843
-1443.739516	-0.296032	1.926848
-1447.112148	1.161901	1.931853
-1450.749749	9.189136	1.936858
-1454.624128	-1.826434	1.941862
-1458.385269	-6.232335	1.946867
-1462.229840	-3.535047	1.951872
-1465.878035	-8.053635	1.956877
-1469.805314	-4.037403	1.961882
-1473.269380	-3.171904	1.966886
-1477.085489	2.193729	1.971891
-1481.464665	10.038566	1.976896
-1484.792706	2.756437	1.981901
-1488.447133	5.016477	1.986906
-1492.031341	7.085509	1.991910
-1495.800839	-1.242366	1.996915
-1500.247374	1.177397	2.006912
-1500.898153	5.369795	2.016909
-1498.662043	4.265182	2.026906
-1495.320767	1.851496	2.036902
-1493.319310	0.077102	2.046899
-1491.477493	1.029835	2.056896
-1489.582922	-1.021122	2.066893
-1487.878897	0.092625	2.076890
-1486.026939	1.665840	2.086886
-1484.174674	-0.847283	2.096883
-1481.790010	-4.451440	2.106880
-1480.133619	6.748299	2.116877
-1478.346892	-2.518493	2.126874
-1476.169216	-3.580569	2.136870
-1474.421886	2.987799	2.146867
-1472.558062	-0.911894	2.156864
-1470.740315	-3.310532	2.166861
-1468.425414	-5.802985	2.176858
-1466.766214	-4.694676	2.186854
-1465.101693	-6.734039	2.196851
-1463.403645	-8.268773	2.206848
-1461.263623	-5.598514	2.216845
-1459.056839	-5.149455	2.226842
-1457.308777	-4.213261	2.236838
-1455.385913	-0.744018	2.246835
-1453.809466	-2.174012	2.256832
-1451.719436	-4.084131	2.266829
-1449.920939	-2.497590	2.276826
-1447.962998	-6.833909	2.286822
-1446.091013	-5.415447	2.296819
-1444.864821	-2.172540	2.306816
-1442.190087	-4.631004	2.316813
-1440.532473	-6.700823	2.326810
-1438.458183	-2.744236	2.336806
-1436.589666	-4.402560	2.346803
-1434.715687	-5.749127	2.356800
-1433.370686	-5.312061	2.366797
-1430.966440	1.942211	2.376794
-1429.037298	-9.597333	2.386790
-1427.157587	-4.805902	2.396787
-1425.541671	-3.229583	2.406784
-1423.517052	-3.008690	2.416781
-1422.055177	-3.635587	2.426778
-1419.821978	-5.537021	2.436774
-1417.697941	-6.833611	2.446771
-1415.845144	-7.409408	2.456768
-1414.361900	-2.423438	2.466765
-1412.383054	-3.406253	2.476762
-1410.300720	-9.714024	2.486758
-1408.255510	-3.684344	2.496755
-1406.721665	-4.400122	2.506752
-1404.903186	-2.807270	2.516749
-1402.695029	-6.608878	2.526746
-1400.765796	-7.863212	2.536742
-1399.134910	-4.031389	2.546739
-1397.361442	-3.689740	2.556736
-1395.535228	-3.842846	2.566733
-1393.531483	-3.020168	2.576730
-1391.342293	0.232811	2.586726
-1389.695111	-8.226846	2.596723
-1387.796503	-6.751019	2.606720
-1385.968468	-0.902864	2.616717
-1383.933231	2.513716	2.626714
-1382.035934	-9.772272	2.636710
-1380.509226	-5.300077	2.646707
-1378.599036	-1.618740	2.656704
-1376.588026	0.818045	2.666701
-1374.821898	-4.341715	2.676698
-1372.690007	-4.175845	2.686694
-1370.925705	-11.373718	2.696691
-1368.971777	-8.998842	2.706688
-1367.362329	-6.267242	2.716685
-1365.076982	-11.195902	2.726682
-1363.346866	-10.416236	2.736678
-1361.541341	-10.240743	2.746675
-1359.822210	-3.738821	2.756672
-1357.688300	-9.914278	2.766669
-1355.905179	-6.214161	2.776666
-1353.952432	-2.918560	2.786662
-1352.243211	-4.458161	2.796659
-1350.533307	-6.997337	2.806656
-1348.481160	-2.680281	2.816653
-1346.573250	-9.473233	2.826650
-1344.370985	-8.914394	2.836646
-1342.652611	-4.575483	2.846643
-1341.000796	-6.879566	2.856640
-1339.082043	-1.827467	2.866637
-1336.952780	-5.321125	2.876634
-1335.195048	-5.477433	2.886630
-1333.528099	-3.681849	2.896627
-1331.664579	-8.863482	2.906624
-1329.546572	-9.776923	2.916621
-1327.920095	-6.425918	2.926618
-1325.931867	-4.910701	2.936614
-1324.038936	-1.937076	2.946611
-1321.955205	-9.383413	2.956608
-1320.057023	-6.944309	2.966605
-1318.268304	-7.255562	2.976602
-1316.653791	-3.888423	2.986598
-1314.386147	-2.608970	2.996595
-1312.596362	-3.191967	3.006592
-1310.839494	0.916600	3.016589
-1309.161903	-1.926849	3.026586
-1307.168683	-5.086076	3.036582
-1304.992965	1.289130	3.046579
-1303.255827	-1.214900	3.056576
-1301.707874	1.843959	3.066573
-1299.745506	0.383879	3.076570
-1297.533755	-1.195061	3.086566
-1295.911506	-5.482268	3.096563
-1293.593544	-1.651385	3.106560
-1292.184919	-6.109661	3.116557
-1290.515924	-5.334368	3.126554
-1288.256502	-10.446701	3.136550
-1286.392237	-8.415822	3.146547
-1284.461011	-3.894616	3.156544
-1282.717314	-4.909160	3.166541
-1280.974307	-6.065697	3.176538
-1278.851677	3.190125	3.186534
-1277.278497	-0.959744	3.196531
-1275.351573	-0.712034	3.206528
-1273.199740	-4.998718	3.216525
-1271.394543	-2.380480	3.226522
-1269.254985	-7.527298	3.236518
-1267.603600	-4.066550	3.246515
-1265.730962	-0.813314	3.256512
-1264.052702	-2.545263	3.266509
-1262.167815	-0.655031	3.276506
-1259.990714	-3.763121	3.286502
-1258.241716	-2.520610	3.296499
-1256.401436	-0.160605	3.306496
-1254.392586	3.596631	3.316493
-1252.859158	3.889965	3.326490
-1251.047079	2.632396	3.336486
-1248.748862	2.162292	3.346483
-1247.107077	3.455128	3.356480
-1245.543400	5.737829	3.366477
-1243.257196	7.723329	3.376474
-1241.233998	3.509361	3.386470
-1239.632408	3.485481	3.396467
-1237.553875	4.785800	3.406464
-1235.710707	8.114833	3.416461
-1233.832991	3.163101	3.426458
-1232.334133	8.516175	3.436454
-1230.174044	8.721875	3.446451
-1228.058056	8.539898	3.456448
-1226.398202	7.319339	3.466445
-1224.459426	4.230469	3.476442
-1222.745922	7.403419	3.486438
-1220.800911	9.628276	3.496435
-1218.750742	9.118947	3.506432
-1216.867786	8.836901	3.516429
-1215.128202	11.789370	3.526426
-1213.346561	14.654585	3.536422
-1211.183016	1.549260	3.546419
-1209.618617	4.630816	3.556416
-1207.555534	6.843106	3.566413
-1205.617568	1.747545	3.576410
-1203.900540	4.858367	3.586406
-1202.134676	4.956647	3.596403
-1200.049267	1.659598	3.606400
-1198.164621	5.351497	3.616397
-1196.553751	7.989839	3.626394
-1194.545115	4.943499	3.636390
-1192.460625	0.779764	3.646387
-1190.610708	0.989341	3.656384
-1188.980598	0.311987	3.666381
-1187.089327	5.224936	3.676378
-1185.098743	0.394130	3.686374
-1183.157229	2.671682	3.696371
-1181.399049	2.613314	3.706368
-1179.330316	-0.595786	3.716365
-1177.543481	0.053367	3.726362
-1175.899962	5.004387	3.736358
-1173.861654	-0.909306	3.746355
-1171.762141	2.040869	3.756352
-1169.985122	0.593183	3.766349
-1168.493042	-2.220487	3.776346
-1166.244084	2.013148	3.786342
-1164.437229	1.970688	3.796339
-1162.639882	4.138693	3.806336
-1160.862332	6.974603	3.816333
-1158.661571	7.349125	3.826330
-1156.880871	9.166116	3.836326
-1154.879158	4.093552	3.846323
-1153.323820	9.713961	3.856320
-1151.571093	14.870163	3.866317
-1149.618004	8.949593	3.876314
-1147.244915	9.168661	3.886310
-1145.630029	3.027469	3.896307
-1143.982995	13.065312	3.906304
-1141.922048	10.334329	3.916301
-1139.982424	9.129071	3.926298
-1138.067268	3.430896	3.936294
-1136.453186	2.353512	3.946291
-1134.450328	4.597609	3.956288
-1132.481590	7.181902	3.966285
-1130.770782	4.075894	3.976282
-1128.863706	7.157949	3.986278
-1127.061930	7.045278	3.996275
-1125.319444	2.562104	4.006272
-1123.074082	12.172666	4.016269
-1120.980625	10.878077	4.026266
-1119.399235	5.803309	4.036262
-1117.451427	4.956760	4.046259
-1115.703984	7.848048	4.056256
-1113.833883	9.762876	4.066253
-1112.057763	9.674848	4.076250
-1109.997587	7.667173	4.086246
-1108.144302	9.480485	4.096243
-1106.136152	5.602191	4.106240
-1104.221970	5.818925	4.116237
-1102.522523	5.807906	4.126234
-1101.064099	9.887017	4.136230
-1098.895749	9.512045	4.146227
-1096.786974	11.316076	4.156224
-1094.924058	6.172605	4.166221
-1093.227000	7.519867	4.176218
-1091.219550	8.730639	4.186214
-1089.251768	3.979344	4.196211
-1087.546799	0.800090	4.206208
-1085.608223	-0.018114	4.216205
-1083.724333	0.036114	4.226202
-1081.702813	-0.256934	4.236198
-1080.084395	-0.704975	4.246195
-1078.333577	2.744748	4.256192
-1076.061920	3.152219	4.266189
-1074.379317	3.516546	4.276186
-1072.728259	-2.166176	4.286182
-1070.666076	2.313747	4.296179
-1068.695446	-6.274819	4.306176
-1066.818649	3.677381	4.316173
-1064.937194	-1.956924	4.326170
-1063.020323	2.467301	4.336166
-1061.288746	-1.313032	4.346163
-1059.565147	2.131586	4.356160
-1057.662832	4.238674	4.366157
-1055.619930	0.337497	4.376154
-1053.459671	-1.307190	4.386150
-1051.801633	2.435288	4.396147
-1050.062145	0.368432	4.406144
-1048.207217	5.906261	4.416141
-1046.330359	0.302704	4.426138
-1044.535956	0.873380	4.436134
-1042.521394	1.036215	4.446131
-1040.495783	-0.795345	4.456128
-1038.637915	-3.177968	4.466125
-1036.821080	-3.360871	4.476122
-1034.932222	-1.174244	4.486118
-1033.060702	0.377264	4.496115
-1031.344552	-1.463214	4.506112
-1029.530455	-3.467777	4.516109
-1027.331600	-0.457567	4.526106
-1025.522737	0.655548	4.536102
-1023.794433	-1.074763	4.546099
-1022.135032	-1.265635	4.556096
-1020.042713	1.662149	4.566093
-1017.896347	-4.976067	4.576090
-1016.214411	0.005245	4.586086
-1014.364995	-8.638104	4.596083
-1012.313215	-7.799092	4.606080
-1010.667084	4.991100	4.616077
-1008.809067	5.488473	4.626074
-1006.750780	5.178556	4.636070
-1004.882208	-2.880485	4.646067
-1002.952404	0.460146	4.656064
-1001.302340	3.798149	4.666061
-999.430648	2.157028	4.676058
-997.709765	3.625288	4.686054
-995.484087	-1.323490	4.696051
-993.607494	-1.686443	4.706048
-991.716495	4.346191	4.716045
-990.264918	7.232787	4.726042
-987.962519	5.083849	4.736038
-986.122849	6.919963	4.746035
-984.334512	3.253764	4.756032
-982.409263	1.709882	4.766029
-980.638632	6.569671	4.776026
-978.626464	5.752418	4.786022
-976.683870	5.015766	4.796019
-975.055570	7.529900	4.806016
-973.107405	2.110783	4.816013
-971.311205	2.734913	4.826010
-969.408646	4.003616	4.836006
-967.397460	7.389686	4.846003
-965.570831	8.597903	4.856000
-963.745178	3.972067	4.865997
-961.721834	8.679356	4.875994
-959.832893	9.962876	4.885990
-957.847503	4.864659	4.895987
-956.114175	3.027803	4.905984
-954.192934	8.196689	4.915981
-952.512333	11.561425	4.925978
-950.509704	11.154668	4.935974
-948.658840	6.647969	4.945971
-946.810327	3.291122	4.955968
-945.154355	12.252434	4.965965
-943.250670	11.174662	4.975962
-941.188270	9.900987	4.985958
-939.286543	4.525636	4.995955
-937.317620	4.018490	5.005952
-935.612410	7.204040	5.015949
-933.561866	8.144374	5.025946
-931.828947	3.743389	5.035942
-929.924868	4.819249	5.045939
-928.103195	5.761446	5.055936
-926.031051	2.348331	5.065933
-924.312513	11.309129	5.075930
-922.338025	7.621104	5.085926
-920.204340	9.176577	5.095923
-918.990804	7.407068	5.105920
-916.868193	3.758523	5.115917
-914.670516	9.022192	5.125914
-912.887523	6.372162	5.135910
-911.196142	5.254150	5.145907
-909.571063	9.000427	5.155904
-907.206181	9.994736	5.165901
-905.385755	9.634517	5.175898
-903.754502	7.814018	5.185894
-901.759304	5.101647	5.195891
-899.884747	7.440674	5.205888
-897.933804	6.887489	5.215885
-896.162472	14.898819	5.225882
-893.957578	7.310291	5.235878
-892.473906	9.833398	5.245875
-890.656838	6.292146	5.255872
-888.588224	3.007522	5.265869
-887.129816	5.889935	5.275866
-884.825294	5.768126	5.285862
-882.927626	2.892942	5.295859
-880.831860	6.480305	5.305856
-879.204936	5.558936	5.315853
-877.598391	7.339251	5.325850
-875.321067	5.761272	5.335846
-873.521419	0.773344	5.345843
-871.825091	3.979309	5.355840
-869.998922	6.709781	5.365837
-868.112014	4.524750	5.375834
-866.082201	0.480558	5.385830
-864.079367	1.796475	5.395827
-862.495781	5.533629	5.405824
-860.324921	3.775316	5.415821
-858.788580	5.576340	5.425818
-856.708411	2.727265	5.435814
-854.610250	4.558477	5.445811
-853.024538	5.251085	5.455808
-851.077766	2.276497	5.465805
-849.082377	9.091518	5.475802
-847.229905	5.573059	5.485798
-845.398819	-2.298298	5.495795
-843.607779	1.478337	5.505792
-841.651651	4.169109	5.515789
-839.970374	5.053292	5.525786
-838.672829	4.710394	5.535782
-836.066749	2.868320	5.545779
-833.930046	-0.441352	5.555776
-832.656591	5.139085	5.565773
-830.360505	9.455527	5.575770
-828.457651	-0.066242	5.585766
-826.668695	-0.137159	5.595763
-824.771680	4.176763	5.605760
-822.795282	6.030627	5.615757
-821.096948	2.298405	5.625754
-819.292173	1.724439	5.635750
-817.139027	5.817425	5.645747
-815.556261	3.081051	5.655744
-813.731797	9.599742	5.665741
-811.772641	9.613737	5.675738
-809.861638	5.334370	5.685734
-807.579357	0.506185	5.695731
-806.283992	3.957869	5.705728
-804.276947	10.111068	5.715725
-802.335784	6.928993	5.725722
-800.161430	2.629645	5.735718
-798.770782	5.391894	5.745715
-796.811800	-0.123554	5.755712
-794.660634	3.856086	5.765709
-793.014297	5.836941	5.775706
-790.968943	0.890325	5.785702
-788.891079	8.090114	5.795699
-787.641283	7.240139	5.805696
-785.497981	7.412617	5.815693
-783.670487	6.299782	5.825690
-781.867267	10.098206	5.835686
-779.486884	9.553849	5.845683
-777.996210	8.366957	5.855680
-776.099923	3.818388	5.865677
-774.109538	5.242162	5.875674
-772.339741	8.335408	5.885670
-770.463722	-0.970451	5.895667
-768.668542	-9.259172	5.905664
-766.657391	3.829727	5.915661
-764.693065	-0.456547	5.925658
-762.909172	-2.569768	5.935654
-761.193778	-3.961512	5.945651
-758.963484	-7.281339	5.955648
-757.514904	-4.477800	5.965645
-755.439841	-5.721759	5.975642
-753.593663	-5.043870	5.985638
-751.468731	-10.557380	5.995635
-749.588189	-4.166025	6.005632
-747.955366	1.972819	6.015629
-746.081906	5.668467	6.025626
-744.249789	4.531238	6.035622
-742.237675	3.232613	6.045619
-740.496430	6.052551	6.055616
-738.362355	5.424440	6.065613
-736.779417	6.337045	6.075610
-734.937372	3.857707	6.085606
-732.901180	1.899978	6.095603
-730.853748	6.284679	6.105600
-729.268908	4.454346	6.115597
-727.511601	7.754886	6.125594
-724.987056	7.604388	6.135590
-723.354465	4.741688	6.145587
-721.715425	8.099028	6.155584
-719.727538	1.064805	6.165581
-717.705560	7.496750	6.175578
-715.997391	-0.462246	6.185574
-714.093900	1.404940	6.195571
-712.334654	0.850961	6.205568
-710.041803	3.475405	6.215565
-708.705941	7.212783	6.225562
-706.948783	6.248614	6.235558
-704.676002	2.587307	6.245555
-702.846883	6.875868	6.255552
-700.877492	3.739888	6.265549
-699.132987	1.231954	6.275546
-697.039083	-0.131808	6.285542
-695.454550	2.809522	6.295539
-693.351308	4.580069	6.305536
-691.673041	1.882198	6.315533
-689.643983	5.617765	6.325530
-687.968510	4.770874	6.335526
-686.002594	7.240742	6.345523
-683.858391	6.131060	6.355520
-682.407744	2.159036	6.365517
-680.632880	8.065236	6.375514
-678.486071	5.597243	6.385510
-676.555900	5.947561	6.395507
-674.612974	4.208468	6.405504
-672.932015	6.397036	6.415501
-670.937948	9.547684	6.425498
-669.104561	5.629775	6.435494
-667.092005	2.965348	6.445491
-665.485651	1.647937	6.455488
-663.487228	-1.628440	6.465485
-661.590635	-0.429585	6.475482
-659.648355	1.605132	6.485478
-657.594914	1.091030	6.495475
-655.765522	-2.632019	6.505472
-654.427057	4.146036	6.515469
-652.391639	-0.876249	6.525466
-650.241180	1.657321	6.535462
-648.407758	-5.559007	6.545459
-646.467576	1.181333	6.555456
-644.751617	6.171707	6.565453
-642.984109	-0.568298	6.575450
-640.970260	0.330786	6.585446
-639.021673	-3.038661	6.595443
-637.181013	1.131265	6.605440
-635.179178	3.170699	6.615437
-633.504080	-2.191898	6.625434
-631.385293	4.568869	6.635430
-629.331258	-1.086374	6.645427
-628.213054	-0.506817	6.655424
-626.065382	0.708795	6.665421
-624.167993	3.983877	6.675418
-622.111849	5.133590	6.685414
-620.384970	3.893268	6.695411
-618.452941	2.730700	6.705408
-616.642614	1.690208	6.715405
-614.673711	6.180720	6.725402
-612.866250	2.189625	6.735398
-610.808095	4.248503	6.745395
-608.783838	-1.266176	6.755392
-607.278651	3.093160	6.765389
-605.335910	6.883646	6.775386
-603.272283	9.434292	6.785382
-601.625686	8.547863	6.795379
-599.921947	4.682295	6.805376
-597.997534	5.684126	6.815373
-595.914941	4.252784	6.825370
-594.025479	9.141270	6.835366
-591.870924	2.009465	6.845363
-590.165789	8.509512	6.855360
-588.676325	5.063447	6.865357
-586.609185	5.147220	6.875354
-584.646094	0.693914	6.885350
-582.626267	1.273144	6.895347
-580.680246	-0.580053	6.905344
-579.029649	5.194501	6.915341
-577.375352	1.707901	6.925338
-575.029388	-1.252869	6.935334
-573.700650	-1.834290	6.945331
-571.584019	3.520031	6.955328
-569.742922	-0.135351	6.965325
-567.607138	0.880108	6.975322
-566.037950	1.180811	6.985318
-564.006371	1.600285	6.995315
-562.098203	4.658959	7.005312
-560.351888	10.820872	7.015309
-558.278859	-2.256855	7.025306
-556.240615	11.603199	7.035302
-554.742704	0.857877	7.045299
-552.935428	2.088457	7.055296
-550.820886	7.428922	7.065293
-548.680866	4.952654	7.075290
-547.510388	6.056007	7.085286
-545.420327	4.361409	7.095283
-543.318492	3.320199	7.105280
-541.646761	-0.080740	7.115277
-539.681325	-0.920159	7.125274
-537.777001	-0.106125	7.135270
-535.776131	5.700935	7.145267
-534.089866	1.326621	7.155264
-532.078700	7.604147	7.165261
-529.946971	7.087123	7.175258
-528.417689	-0.322126	7.185254
-526.381185	7.043994	7.195251
-524.872699	5.383885	7.205248
-522.730263	8.495175	7.215245
-520.863018	6.839344	7.225242
-519.179904	5.069240	7.235238
-517.115092	6.653453	7.245235
-515.102598	1.475464	7.255232
-513.347149	4.585413	7.265229
-511.298852	-1.872507	7.275226
-509.775767	7.814589	7.285222
-507.875369	4.167148	7.295219
-505.746193	0.735803	7.305216
-503.899463	2.241172	7.315213
-502.338239	1.006866	7.325210
-500.094584	2.587792	7.335206
-498.209612	6.537598	7.345203
-496.408923	1.709242	7.355200
-494.741052	2.602130	7.365197
-492.884286	-1.024120	7.375194
-490.990321	5.445846	7.385190
-488.979160	4.122320	7.395187
-486.774720	1.507922	7.405184
-485.075801	3.512179	7.415181
-483.478584	5.892682	7.425178
-481.513263	0.395410	7.435174
-479.545893	-2.010593	7.445171
-477.836598	5.325723	7.455168
-475.621058	4.626414	7.465165
-473.983473	2.601506	7.475162
-472.107681	3.806995	7.485158
-470.068659	1.302714	7.495155
-468.361807	3.916772	7.505152
-466.440419	8.738688	7.515149
-464.773937	8.621287	7.525146
-462.684726	6.517945	7.535142
-460.792370	6.244474	7.545139
-458.960202	3.706920	7.555136
-457.138083	9.051542	7.565133
-455.108759	6.829876	7.575130
-453.081983	7.284949	7.585126
-451.466707	0.116222	7.595123
-449.827594	10.995895	7.605120
-447.557287	5.543101	7.615117
-445.740572	4.550664	7.625114
-443.807110	8.805406	7.635110
-441.936220	7.016421	7.645107
-440.039919	-0.014017	7.655104
-438.768425	6.997504	7.665101
-436.589253	-4.046019	7.675098
-434.395160	0.501847	7.685094
-432.506433	10.032719	7.695091
-430.986840	6.711409	7.705088
-428.931289	2.276617	7.715085
-427.073322	4.389730	7.725082
-425.171372	6.352137	7.735078
-423.206118	3.504408	7.745075
-421.374740	10.339696	7.755072
-419.558392	5.527840	7.765069
-417.715248	8.148594	7.775066
-415.702012	7.840067	7.785062
-413.745013	1.714171	7.795059
-412.503131	5.981473	7.805056
-410.129336	7.156440	7.815053
-408.129088	8.241054	7.825050
-406.313989	-1.787465	7.835046
-404.524593	3.781899	7.845043
-402.574711	0.076110	7.855040
-400.772768	12.559308	7.865037
-399.056903	10.264579	7.875034
-397.333571	13.921330	7.885030
-394.875068	9.018010	7.895027
-392.931006	3.268407	7.905024
-391.419303	15.052690	7.915021
-389.356724	7.057834	7.925018
-387.890087	4.714486	7.935014
-385.880169	2.735977	7.945011
-383.948321	4.614695	7.955008
-381.947777	0.927676	7.965005
-380.080706	1.329362	7.975002
-378.238654	3.978743	7.984998
-376.661617	5.661484	7.994995
-374.329712	2.344725	8.004992
-372.475001	5.633147	8.014989
-370.746723	8.477543	8.024986
-368.856864	5.370313	8.034982
-367.020724	-2.482577	8.044979
-365.121652	-3.464418	8.054976
-363.327999	-2.266255	8.064973
-361.251724	-0.802159	8.074970
-359.665868	0.137076	8.084966
-357.915136	-1.236342	8.094963
-355.579028	-1.801631	8.104960
-354.098310	-1.518243	8.114957
-352.013070	-1.103997	8.124954
-349.819105	-1.616587	8.134950
-348.104754	-6.772107	8.144947
-346.284213	-2.867155	8.154944
-344.581223	-0.590287	8.164941
-342.736552	-1.157633	8.174938
-340.902942	-0.935312	8.184934
-338.744268	-1.876471	8.194931
-336.765453	-2.389438	8.204928
-335.098735	-1.613098	8.214925
-333.164116	-4.040598	8.224922
-331.449511	-0.633461	8.234918
-329.660922	0.309745	8.244915
-327.778841	8.643341	8.254912
-325.565407	1.409197	8.264909
-323.689751	3.557464	8.274906
-322.108190	0.602120	8.284902
-319.925770	-1.369136	8.294899
-318.230439	-7.909504	8.304896
-316.433039	3.353952	8.314893
-314.376178	-0.365688	8.324890
-312.729490	-5.763017	8.334886
-310.588033	-5.787186	8.344883
-308.751359	-2.142150	8.354880
-306.906402	-6.080589	8.364877
-305.068071	2.520536	8.374874
-303.438402	5.841779	8.384870
-301.523366	2.992689	8.394867
-299.393562	-1.270692	8.404864
-297.565488	2.091515	8.414861
-295.852643	1.472616	8.424858
-293.859792	-2.089947	8.434854
-291.886304	-4.602567	8.444851
-290.136324	0.216858	8.454848
-287.915286	0.890538	8.464845
-286.419853	-0.265233	8.474842
-284.229454	-2.349837	8.484838
-282.647460	-4.015216	8.494835
-280.797759	-5.969643	8.504832
-278.688844	-2.718567	8.514829
-277.369473	-0.593575	8.524826
-275.056724	-3.035597	8.534822
-273.195812	-4.568647	8.544819
-271.248107	0.418181	8.554816
-269.539012	-1.395373	8.564813
-267.278312	1.308851	8.574810
-265.517745	0.437618	8.584807
-263.986702	-1.312776	8.594803
-261.904105	2.793577	8.604800
-260.107042	-0.287705	8.614797
-258.342129	2.255661	8.624794
-256.242104	-1.428190	8.634791
-254.297882	-5.571910	8.644787
-252.436591	-7.237638	8.654784
-250.699796	-3.830825	8.664781
-249.108324	-0.768713	8.674778
-247.050874	3.592721	8.684775
-244.904368	-0.008539	8.694771
-243.053897	5.061730	8.704768
-241.354864	1.790842	8.714765
-239.494575	4.382159	8.724762
-237.658503	0.574661	8.734759
-235.466161	4.159834	8.744755
-233.529788	0.044223	8.754752
-232.185832	-1.125234	8.764749
-230.264657	-1.859443	8.774746
-227.976202	-1.989106	8.784743
-226.288775	-4.636020	8.794739
-224.359449	-2.800979	8.804736
-222.467321	-11.115865	8.814733
-220.527975	-5.892397	8.824730
-218.600318	-2.634443	8.834727
-216.955806	-5.402397	8.844723
-214.959920	-0.677423	8.854720
-213.196332	1.086183	8.864717
-211.280228	-5.107244	8.874714
-208.983591	-3.580287	8.884711
-207.390805	-6.681035	8.894707
-205.823559	-9.267702	8.904704
-203.981280	-4.519784	8.914701
-201.889849	-2.510068	8.924698
-200.002622	-7.847818	8.934695
-197.915317	-9.353782	8.944691
-196.091972	-5.335474	8.954688
-194.520278	-3.365966	8.964685
-192.920773	-11.454131	8.974682
-190.844464	-7.226712	8.984679
-188.544818	-6.027061	8.994675
-186.832197	-4.174776	9.004672
-185.191129	-3.596344	9.014669
-183.063286	-3.297698	9.024666
-180.991792	-6.335874	9.034663
-179.470849	-11.034099	9.044659
-177.639585	-5.070183	9.054656
-175.658603	-10.157610	9.064653
-173.861360	-3.116147	9.074650
-171.769485	-5.994936	9.084647
-170.009378	-7.952351	9.094643
-168.143060	-4.351407	9.104640
-166.495399	-2.316634	9.114637
-164.495844	-5.701741	9.124634
-162.317542	-4.909020	9.134631
-160.365068	-2.215508	9.144627
-158.780884	-6.200650	9.154624
-157.107335	1.176359	9.164621
-155.056539	1.749432	9.174618
-153.158088	5.072103	9.184615
-151.229340	-1.707516	9.194611
-149.266740	-3.011960	9.204608
-147.511892	-1.485334	9.214605
-145.507013	1.057722	9.224602
-143.891496	7.826632	9.234599
-141.573388	3.247542	9.244595
-140.192756	7.107591	9.254592
-138.283985	2.514872	9.264589
-136.310749	3.881923	9.274586
-134.174772	-3.262331	9.284583
-132.520966	-7.433831	9.294579
-130.574993	-0.395535	9.304576
-128.703473	4.793048	9.314573
-126.628262	3.570128	9.324570
-124.877637	-0.386288	9.334567
-123.091248	1.939015	9.344563
-121.331740	3.095441	9.354560
-119.554325	7.989572	9.364557
-117.393099	11.098240	9.374554
-115.440365	9.462235	9.384551
-113.520486	8.309899	9.394547
-112.003904	7.681390	9.404544
-110.286400	8.558734	9.414541
-108.383596	6.253326	9.424538
-105.930543	7.847008	9.434535
-104.166131	6.848959	9.444531
-102.742317	8.780545	9.454528
-100.631474	1.056110	9.464525
-98.618292	3.188931	9.474522
-96.797802	7.425675	9.484519
-94.856317	1.081436	9.494515
-93.147132	0.093786	9.504512
-91.080034	-0.336750	9.514509
-89.426961	9.745187	9.524506
-87.273239	8.925041	9.534503
-85.578141	9.689134	9.544499
-84.126045	7.315124	9.554496
-81.986392	5.733009	9.564493
-79.920349	10.863759	9.574490
-77.868429	5.360868	9.584487
-76.190976	3.429336	9.594483
-74.453038	4.889240	9.604480
-72.334394	8.228955	9.614477
-70.464542	6.080414	9.624474
-68.530863	5.972764	9.634471
-67.023704	8.056866	9.644467
-64.903476	0.537806	9.654464
-63.098157	5.010683	9.664461
-60.975598	3.927108	9.674458
-59.240799	5.505947	9.684455
-57.498983	0.189915	9.694451
-55.846108	1.331821	9.704448
-53.597988	5.151428	9.714445
-51.945133	1.460134	9.724442
-49.825621	6.493958	9.734439
-48.226117	3.493289	9.744435
-46.392449	11.016953	9.754432
-44.009956	2.769221	9.764429
-42.119605	8.417510	9.774426
-40.574513	10.247681	9.784423
-38.772747	8.261605	9.794419
-36.832882	3.177679	9.804416
-34.652942	12.049814	9.814413
-33.407524	5.234018	9.824410
-31.272983	3.985924	9.834407
-29.074992	6.627750	9.844403
-27.580818	3.138628	9.854400
-25.820428	7.331331	9.864397
-23.525382	2.530235	9.874394
-21.769000	6.704632	9.884391
-19.998934	4.992050	9.894387
-17.736486	1.593543	9.904384
-16.348463	8.539363	9.914381
-14.303052	8.200774	9.924378
-12.413053	6.377486	9.934375
-10.531478	3.780273	9.944371
-8.701890	10.862509	9.954368
-6.833983	9.300121	9.964365
-5.083915	25.842000	9.974362
-3.644735	36.951312	9.984359
-2.487456	71.528042	9.994355
-1.033685	122.298911	10.004352
0.000000	170.324431	10.009357
1.183469	200.960745	10.014362
1.653852	224.579810	10.019367
2.163103	247.260725	10.024371
2.898490	273.777076	10.029376
2.771419	291.478547	10.034381
2.722312	287.225547	10.039386
3.152703	302.401686	10.044391
3.267319	307.772093	10.049395
3.732163	317.603106	10.054400
3.433700	326.201251	10.059405
3.476355	321.006341	10.064410
3.513067	334.679367	10.069415
3.703671	335.885474	10.074419
3.927123	331.707260	10.079424
3.448602	336.935739	10.084429
3.792371	335.405008	10.089434
4.185518	334.271685	10.094439
3.813202	347.499023	10.099443
4.040571	333.687980	10.104448
3.948692	343.688237	10.109453
3.941916	340.642745	10.114458
4.006902	346.000582	10.119463
3.782278	346.290461	10.124467
4.053968	356.567056	10.129472
3.997069	354.254969	10.134477
4.204588	348.325686	10.139482
3.794778	356.714525	10.144487
4.142063	357.255387	10.149491
4.249616	359.766292	10.154496
4.225206	379.739699	10.159501
4.785297	380.890028	10.164506
4.747805	379.997283	10.169511
4.418302	377.673479	10.174515
4.850052	362.440484	10.179520
4.553253	368.515215	10.184525
4.843152	358.601942	10.189530
5.066883	365.101433	10.194535
4.808463	369.741295	10.199539
4.858819	371.373483	10.204544
4.710366	370.917915	10.209549
5.055763	369.391652	10.214554
4.923905	369.684082	10.219559
4.631532	377.683609	10.224563
5.030230	381.706141	10.229568
4.977869	393.477392	10.234573
5.300900	395.015627	10.239578
5.038056	392.794731	10.244583
5.509602	407.276849	10.249587
5.512795	397.757795	10.254592
5.041550	395.652143	10.259597
5.320602	387.380648	10.264602
5.260638	398.340968	10.269607
5.615914	405.275245	10.274611
5.894215	403.075267	10.279616
5.310000	397.049895	10.284621
5.339402	395.906777	10.289626
5.589097	404.989981	10.294631
5.570340	418.865904	10.299635
5.718194	415.800463	10.304640
5.793622	426.297651	10.309645
5.861887	418.058183	10.314650
5.735436	428.652230	10.319655
5.828865	432.837012	10.324659
6.191600	426.006133	10.329664
5.624940	439.001196	10.334669
5.713023	430.324887	10.339674
5.804379	431.485330	10.344679
5.411337	434.188062	10.349683
5.893161	431.865729	10.354688
5.604040	441.097979	10.359693
5.573282	447.264352	10.364698
6.088816	455.516689	10.369703
6.155336	457.318201	10.374707
6.428450	459.279155	10.379712
6.290055	467.008159	10.384717
6.147382	461.492666	10.389722
6.401865	465.788967	10.394727
6.207202	467.531213	10.399731
6.336702	465.149951	10.404736
6.148032	473.841060	10.409741
6.612840	477.577101	10.414746
6.818245	501.984804	10.419751
6.790926	507.871526	10.424755
7.111163	505.018275	10.429760
7.093459	495.103509	10.434765
6.804817	483.878903	10.439770
6.729059	489.177238	10.444775
6.931998	500.059429	10.449779
7.050870	494.054338	10.454784
6.890320	503.292929	10.459789
7.147101	496.712314	10.464794
7.257474	506.051200	10.469799
7.419173	512.835838	10.474803
7.351283	502.515110	10.479808
6.915311	504.906148	10.484813
7.438954	505.811560	10.489818
7.569368	513.145254	10.494823
7.581494	517.218445	10.499827
7.556232	490.395508	10.504832
7.174893	498.784617	10.509837
7.423653	509.289701	10.514842
7.606924	525.312915	10.519847
7.673604	521.941845	10.524851
7.682980	514.151699	10.529856
7.771047	532.628149	10.534861
7.577403	530.356769	10.539866
7.547824	527.336953	10.544871
7.607842	531.593327	10.549875
7.967367	519.770129	10.554880
7.789317	529.628135	10.559885
7.634646	527.492469	10.564890
7.730879	531.129613	10.569895
7.439279	542.879218	10.574899
7.766297	535.919940	10.579904
7.922895	552.899949	10.584909
8.464896	558.055618	10.589914
8.330597	560.808568	10.594919
8.255633	558.739035	10.599923
8.547258	563.485195	10.604928
8.391106	568.523560	10.609933
8.393971	558.267991	10.614938
8.491588	564.741955	10.619943
8.614521	568.614554	10.624947
8.797100	558.563717	10.629952
8.261526	562.664355	10.634957
8.437402	556.602836	10.639962
8.643260	564.299061	10.644967
8.616335	569.588059	10.649971
8.641255	564.140415	10.654976
8.659557	574.884951	10.659981
8.559763	573.443870	10.664986
8.796115	571.928672	10.669991
8.741904	571.705655	10.674995
8.826413	572.146510	10.680000
8.715550	568.981950	10.685005
8.637868	577.194932	10.690010
8.975506	586.205874	10.695015
9.203495	605.994248	10.700019
9.273765	598.416703	10.705024
9.286068	607.153109	10.710029
9.190511	609.157117	10.715034
9.178895	607.279329	10.720039
9.265235	616.044934	10.725043
9.346176	602.163948	10.730048
9.317381	611.518792	10.735053
9.631791	605.173373	10.740058
9.628215	620.706082	10.745063
9.474374	621.008330	10.750067
9.388097	607.718581	10.755072
9.527154	616.754908	10.760077
9.334154	609.805997	10.765082
9.377208	617.572374	10.770087
9.748215	620.416633	10.775091
9.667274	615.071014	10.780096
9.708698	619.141137	10.785101
9.721674	634.256466	10.790106
10.335202	632.157534	10.795111
10.042375	634.661383	10.800115
10.126572	630.644073	10.805120
10.124784	639.769115	10.810125
10.250717	636.633005	10.815130
10.348216	640.821929	10.820135
10.361105	638.806182	10.825139
10.056626	636.770092	10.830144
10.072902	645.652549	10.835149
10.180877	637.666831	10.840154
10.360189	642.430932	10.845159
10.302292	646.559485	10.850163
10.672254	637.428068	10.855168
10.618066	637.168775	10.860173
10.536552	643.788045	10.865178
10.596337	644.699642	10.870183
10.496380	633.640373	10.875187
10.261011	636.630240	10.880192
10.615182	644.026874	10.885197
10.808021	643.094219	10.890202
10.770630	643.278542	10.895207
10.803898	648.610010	10.900211
10.819648	650.891172	10.905216
10.862918	664.495651	10.910221
11.070224	667.537924	10.915226
11.119997	673.754629	10.920231
11.197694	664.791243	10.925235
11.439308	660.241017	10.930240
11.223203	659.935007	10.935245
11.153761	648.262131	10.940250
11.175683	652.289641	10.945255
11.226835	668.748842	10.950259
11.709775	673.398289	10.955264
11.360343	677.816212	10.960269
11.373394	676.789225	10.965274
11.634310	676.285699	10.970279
11.436221	677.042879	10.975283
11.442979	679.383829	10.980288
11.549082	684.101271	10.985293
11.440691	680.887405	10.990298
11.949744	678.032391	10.995303
11.502467	690.131811	11.000307
11.948939	679.754936	11.005312
11.611065	683.921848	11.010317
11.622183	689.521803	11.015322
11.787582	683.310509	11.020327
11.680884	686.163163	11.025331
11.604679	687.202114	11.030336
11.686290	696.969929	11.035341
11.871329	707.856709	11.040346
12.151402	712.855508	11.045351
12.495959	718.796546	11.050355
12.515605	709.009724	11.055360
12.432940	717.370242	11.060365
12.424026	710.166407	11.065370
12.781390	717.665075	11.070375
12.701485	718.144775	11.075379
12.507672	697.622525	11.080384
12.484090	694.147537	11.085389
12.366675	694.740456	11.090394
12.788790	701.542785	11.095399
12.478048	716.384966	11.100403
12.973945	710.042095	11.105408
13.153637	706.839046	11.110413
13.075535	704.585480	11.115418
12.938294	687.129413	11.120423
12.591119	686.888464	11.125427
13.029669	679.887674	11.130432
12.767770	679.912256	11.135437
12.710451	700.424385	11.140442
12.983282	707.767791	11.145447
12.620025	714.630736	11.150451
13.104006	709.079854	11.155456
13.040914	712.445975	11.160461
12.967324	711.987917	11.165466
13.296974	707.226507	11.170471
13.149864	724.450709	11.175475
13.364581	710.103562	11.180480
13.396263	720.305153	11.185485
13.430294	719.549218	11.190490
13.507186	711.806547	11.195495
13.093138	715.474663	11.200499
13.855691	710.787712	11.205504
13.585013	719.179797	11.210509
13.429760	716.681481	11.215514
13.770454	713.682995	11.220519
13.502507	733.965404	11.225523
13.906444	741.188563	11.230528
13.932916	751.886193	11.235533
14.194252	740.890646	11.240538
14.448884	719.090413	11.245543
13.937114	727.782744	11.250547
13.794116	722.746618	11.255552
13.797715	724.942993	11.260557
13.934815	734.485931	11.265562
14.263907	744.135453	11.270567
14.306246	752.987010	11.275571
14.186689	746.959918	11.280576
14.194020	744.733722	11.285581
14.378588	750.175142	11.290586
14.655462	743.998084	11.295591
14.385996	750.551182	11.300595
14.382923	746.826893	11.305600
14.318782	751.781256	11.310605
14.710937	752.196702	11.315610
14.774256	744.058768	11.320615
14.352532	755.652673	11.325619
14.819801	750.769946	11.330624
14.575155	749.309372	11.335629
14.622747	753.902122	11.340634
14.772171	743.541041	11.345639
14.596209	757.620565	11.350643
14.753564	752.504981	11.355648
14.605301	754.211473	11.360653
14.711093	754.470735	11.365658
14.455957	757.807571	11.370663
14.105782	770.736856	11.375667
14.901399	762.819594	11.380672
14.852956	774.814466	11.385677
15.030987	780.297943	11.390682
15.183102	779.423818	11.395687
15.272649	774.703837	11.400691
15.389417	778.061787	11.405696
15.373086	784.561910	11.410701
15.207198	783.377366	11.415706
15.300012	779.872753	11.420711
15.372738	785.841405	11.425715
15.681872	796.142305	11.430720
15.744711	794.897623	11.435725
15.422958	793.119743	11.440730
15.619360	796.663702	11.445735
15.679079	816.174837	11.450739
15.775102	810.275768	11.455744
16.225234	816.569032	11.460749
15.867765	806.017507	11.465754
15.855123	799.528617	11.470759
15.721422	811.229597	11.475763
16.135903	812.351149	11.480768
16.222362	806.146086	11.485773
15.833485	819.753403	11.490778
16.380676	808.463040	11.495783
16.130792	817.400672	11.500787
16.037891	809.207190	11.505792
15.933921	815.319161	11.510797
16.262722	810.620935	11.515802
16.656365	806.325550	11.520807
16.119287	817.590955	11.525811
16.654332	808.674388	11.530816
16.381007	808.735487	11.535821
16.469294	809.625201	11.540826
16.447374	817.193880	11.545831
16.191362	818.152703	11.550835
16.667755	815.485809	11.555840
16.751903	827.579432	11.560845
16.407528	823.081619	11.565850
16.856054	820.714074	11.570855
16.434964	823.938615	11.575859
16.540642	814.508603	11.580864
16.813434	836.718778	11.585869
17.007273	840.449247	11.590874
17.217849	839.785003	11.595879
16.829914	844.562372	11.600883
17.180613	844.915044	11.605888
17.087804	846.445535	11.610893
17.070574	838.276239	11.615898
17.311487	839.736154	11.620903
17.125238	852.134713	11.625907
17.059775	839.361854	11.630912
17.083857	842.583207	11.635917
17.115709	841.431778	11.640922
17.301542	840.030273	11.645927
17.208487	845.632710	11.650931
17.247440	844.819210	11.655936
17.328150	848.558263	11.660941
17.292772	864.186196	11.665946
18.174835	863.425888	11.670951
18.090716	865.352408	11.675955
17.526715	837.251409	11.680960
17.455043	831.418505	11.685965
17.690694	859.348237	11.690970
18.274535	868.990329	11.695975
17.808548	873.647686	11.700979
18.063038	863.170408	11.705984
18.018261	873.310181	11.710989
18.088881	873.839997	11.715994
18.437247	865.401050	11.720999
17.993904	864.109358	11.726003
18.114059	867.272814	11.731008
18.192481	867.080679	11.736013
18.124143	869.758508	11.741018
18.201686	867.199378	11.746023
18.010797	871.828627	11.751027
18.312769	867.095236	11.756032
18.527253	872.844184	11.761037
18.263158	876.177745	11.766042
18.416314	872.499473	11.771047
18.240762	876.087007	11.776051
18.447259	876.672427	11.781056
18.695316	875.943852	11.786061
18.314344	872.631485	11.791066
18.857501	889.663780	11.796071
18.759221	897.016009	11.801075
18.810798	891.874668	11.806080
19.081354	901.450050	11.811085
19.102792	897.579879	11.816090
19.249912	877.152815	11.821095
18.870124	880.676727	11.826099
18.883282	865.923158	11.831104
18.883683	884.063936	11.836109
18.784375	895.439359	11.841114
19.399515	895.893366	11.846119
19.341459	900.255418	11.851123
19.584919	897.863796	11.856128
19.439217	905.545310	11.861133
19.618163	908.418683	11.866138
19.411101	889.457970	11.871143
19.337242	893.103410	11.876147
19.653324	899.055373	11.881152
19.646538	904.656689	11.886157
19.673464	901.104205	11.891162
19.420665	889.786827	11.896167
19.618838	898.053768	11.901171
19.818875	901.032592	11.906176
19.645139	909.264236	11.911181
19.644788	910.046662	11.916186
19.782075	900.819722	11.921191
19.823930	900.541951	11.926195
19.833761	905.628079	11.931200
19.885765	902.304996	11.936205
19.281705	905.292219	11.941210
19.668074	900.933308	11.946215
19.713587	914.843611	11.951219
20.244309	926.063373	11.956224
20.374593	924.981398	11.961229
20.122495	923.697045	11.966234
20.229834	926.551880	11.971239
20.293449	933.998161	11.976243
20.646105	928.933372	11.981248
20.547434	927.011078	11.986253
20.539047	923.938911	11.991258
20.799984	913.566231	11.996263
20.340473	908.397586	12.001267
20.661390	908.261396	12.006272
20.760844	915.665679	12.011277
20.532881	918.506180	12.016282
20.837041	905.532374	12.021287
20.932450	899.335306	12.026291
20.661821	911.329457	12.031296
20.552967	906.339863	12.036301
20.344904	903.692233	12.041306
20.665442	904.130147	12.046311
20.455037	912.429146	12.051315
20.411871	900.397041	12.056320
20.402536	908.626118	12.061325
20.766536	923.365621	12.066330
20.796414	923.972905	12.071335
20.736015	915.854608	12.076339
20.578881	903.862756	12.081344
20.540379	908.191728	12.086349
20.375962	915.868347	12.091354
20.836134	925.468698	12.096359
20.610402	922.462738	12.101363
20.482379	918.154327	12.106368
20.870273	921.355519	12.111373
20.568752	920.966926	12.116378
20.819262	909.127684	12.121383
20.641628	909.700253	12.126387
20.878209	909.101247	12.131392
20.861486	910.028218	12.136397
20.648364	910.111255	12.141402
21.109108	904.051468	12.146407
20.749505	909.045125	12.151411
20.691502	912.093495	12.156416
20.830842	909.620701	12.161421
20.829053	912.582831	12.166426
20.893443	913.924243	12.171431
20.723661	911.229502	12.176435
20.654469	910.269236	12.181440
20.620844	909.675479	12.186445
20.418549	911.852680	12.191450
20.561109	904.501578	12.196455
20.925074	922.994449	12.201459
20.679154	913.582602	12.206464
20.897026	912.969233	12.211469
20.400109	900.353451	12.216474
20.754348	900.287644	12.221479
20.556455	909.358973	12.226483
20.786398	890.456297	12.231488
20.768765	884.129023	12.236493
20.588866	885.667101	12.241498
20.670756	881.454537	12.246503
20.496868	881.283721	12.251507
20.321920	882.720079	12.256512
20.919082	889.458306	12.261517
20.426869	890.678747	12.266522
20.586720	886.724998	12.271527
20.512750	891.769291	12.276531
20.843760	905.936841	12.281536
20.605211	890.289785	12.286541
20.605394	893.962841	12.291546
20.689570	882.586991	12.296551
20.534771	884.321349	12.301555
20.622983	884.096112	12.306560
20.512007	886.020611	12.311565
20.763174	906.480674	12.316570
20.428454	892.271448	12.321575
20.586182	905.097763	12.326579
20.627884	907.519914	12.331584
20.811174	911.211081	12.336589
20.710541	901.164177	12.341594
20.928564	885.524732	12.346599
20.726020	889.310551	12.351603
20.585928	892.190651	12.356608
20.876173	887.970085	12.361613
20.520445	879.695475	12.366618
20.819933	879.966425	12.371623
20.630732	889.432193	12.376627
20.586039	892.044750	12.381632
20.847775	900.191161	12.386637
20.839996	899.897651	12.391642
20.975644	889.455080	12.396647
20.959949	890.057015	12.401651
20.926793	891.220008	12.406656
21.004158	886.465662	12.411661
20.896077	881.537458	12.416666
20.732551	859.499342	12.421671
20.968439	864.883732	12.426675
20.317453	853.879064	12.431680
20.449726	852.249545	12.436685
20.397519	852.682251	12.441690
20.433934	854.482307	12.446695
20.410057	874.880533	12.451699
20.313104	887.619714	12.456704
20.767790	878.403668	12.461709
20.635748	901.148471	12.466714
20.611875	893.177334	12.471719
20.639242	895.122348	12.476723
20.962639	897.395483	12.481728
20.860525	895.757609	12.486733
20.613916	881.223663	12.491738
20.690268	866.906316	12.496743
20.682721	876.125470	12.501747
20.476402	869.602781	12.506752
20.885504	862.865236	12.511757
20.703108	865.718960	12.516762
20.620902	858.580360	12.521767
20.719322	865.084294	12.526771
20.402748	864.073596	12.531776
20.586827	859.171344	12.536781
20.137541	865.641205	12.541786
20.793815	871.600401	12.546791
20.613558	881.078930	12.551795
20.636360	880.075606	12.556800
20.775558	874.119160	12.561805
20.626045	872.777447	12.566810
20.321214	865.073500	12.571815
20.542455	885.249708	12.576819
20.849435	886.500383	12.581824
21.192878	879.364849	12.586829
20.604421	874.734052	12.591834
20.775750	863.254424	12.596839
20.484258	866.166552	12.601843
20.314473	873.344084	12.606848
20.525059	865.272484	12.611853
20.727352	870.999721	12.616858
20.775402	863.802493	12.621863
20.619628	871.947668	12.626867
20.726284	872.137405	12.631872
20.855627	865.081761	12.636877
20.431992	874.611720	12.641882
20.656038	868.342106	12.646887
20.756437	879.245670	12.651891
20.944834	880.132037	12.656896
20.512541	875.651383	12.661901
20.449652	865.139565	12.666906
20.665627	864.933377	12.671911
20.553948	866.690819	12.676915
20.401967	871.553572	12.681920
20.606840	864.739784	12.686925
20.610435	870.642223	12.691930
20.948340	878.062074	12.696935
20.876799	869.560782	12.701939
20.631765	867.437900	12.706944
20.924227	867.257361	12.711949
20.814348	873.685707	12.716954
20.696459	872.518733	12.721959
20.720071	875.221323	12.726963
20.674535	880.343082	12.731968
20.871342	874.653429	12.736973
20.782210	885.407445	12.741978
20.683454	870.048791	12.746983
20.453068	877.794262	12.751987
20.651604	875.649519	12.756992
20.989214	871.184847	12.761997
20.621310	869.026367	12.767002
20.501127	854.073292	12.772007
20.389880	861.342411	12.777011
20.568574	873.228594	12.782016
20.842282	870.635022	12.787021
20.799123	883.253649	12.792026
20.573780	869.793441	12.797031
20.469792	856.198766	12.802035
20.854162	869.670181	12.807040
20.729048	858.487012	12.812045
20.356572	863.258767	12.817050
20.584573	867.026374	12.822055
20.907599	878.493704	12.827059
20.872236	868.201433	12.832064
20.860398	848.162481	12.837069
20.572109	854.854253	12.842074
20.374191	857.798766	12.847079
20.453722	849.762271	12.852083
20.363312	846.422491	12.857088
20.643599	853.588154	12.862093
20.287719	872.673617	12.867098
20.876401	873.764236	12.872103
20.975075	882.349829	12.877107
20.705980	869.823899	12.882112
20.684403	859.608288	12.887117
20.592686	859.481139	12.892122
20.384034	854.026484	12.897127
20.625629	851.996309	12.902131
20.676936	859.594333	12.907136
20.568912	849.647997	12.912141
20.645033	861.575763	12.917146
20.738429	860.893935	12.922151
20.741109	860.783272	12.927155
20.602802	859.726794	12.932160
20.948558	845.385423	12.937165
20.638425	850.645574	12.942170
20.695736	854.080838	12.947175
20.734625	857.064855	12.952179
20.790100	860.814244	12.957184
20.900080	849.803330	12.962189
20.755480	857.047804	12.967194
20.489730	848.087041	12.972199
20.483421	849.264673	12.977203
20.771977	857.466710	12.982208
20.714360	848.833892	12.987213
20.799233	857.364899	12.992218
20.862048	853.693155	12.997223
20.936049	858.969315	13.002227
20.621323	855.159082	13.007232
20.809983	855.646415	13.012237
20.736975	858.000117	13.017242
20.812105	846.767671	13.022247
20.663471	832.995625	13.027251
20.173692	837.928015	13.032256
20.717261	838.316160	13.037261
20.611589	850.700290	13.042266
20.571888	851.914788	13.047271
20.560811	855.384616	13.052275
20.248145	860.785532	13.057280
20.645005	845.466131	13.062285
20.468943	865.853923	13.067290
20.715658	862.231697	13.072295
20.881316	864.276083	13.077299
20.607063	868.197920	13.082304
20.614209	862.554292	13.087309
20.710982	871.553367	13.092314
20.398522	868.009288	13.097319
20.603796	864.286433	13.102323
20.635915	859.031506	13.107328
20.823348	853.980480	13.112333
20.405150	860.204093	13.117338
20.594033	859.120661	13.122343
20.987139	859.356178	13.127347
20.918060	870.553286	13.132352
20.684631	844.683098	13.137357
20.647890	832.779341	13.142362
20.660802	836.896654	13.147367
20.683818	841.734639	13.152371
20.375050	832.597812	13.157376
20.737909	830.568799	13.162381
20.564234	830.074657	13.167386
20.524758	829.715238	13.172391
20.660851	835.861471	13.177395
20.485577	846.422607	13.182400
20.779317	848.004991	13.187405
20.841823	855.899287	13.192410
20.736764	845.159231	13.197415
20.865693	844.895960	13.202419
20.420825	836.039472	13.207424
20.666399	840.310498	13.212429
20.441288	847.462146	13.217434
20.188805	846.762943	13.222439
20.768199	849.594513	13.227443
20.643063	854.476633	13.232448
20.660716	844.010335	13.237453
20.341543	848.172733	13.242458
20.851622	853.677397	13.247463
20.622381	849.821989	13.252467
20.631872	840.626510	13.257472
20.730404	832.162772	13.262477
20.609035	843.667836	13.267482
20.955202	836.102935	13.272487
20.775173	844.002791	13.277491
20.743324	843.184814	13.282496
20.651994	837.539556	13.287501
20.372074	840.183314	13.292506
20.776778	833.943249	13.297511
20.616784	842.316174	13.302515
20.611490	848.122245	13.307520
20.561655	840.027538	13.312525
20.387944	850.687780	13.317530
20.459385	841.343640	13.322535
20.416331	832.840979	13.327539
20.468733	838.781355	13.332544
20.953556	850.490952	13.337549
20.755387	852.582326	13.342554
20.392393	851.618460	13.347559
20.677279	840.718435	13.352563
20.474335	838.946831	13.357568
20.738317	841.223126	13.362573
20.632430	836.669921	13.367578
20.781411	844.252359	13.372583
20.789601	840.726533	13.377587
20.762051	850.658528	13.382592
20.906323	846.879172	13.387597
20.794461	843.981229	13.392602
20.680304	848.259169	13.397607
20.847878	843.700195	13.402611
20.623516	842.318381	13.407616
20.810938	843.449342	13.412621
20.472422	844.856588	13.417626
20.496950	846.171235	13.422631
20.602417	834.598050	13.427635
20.672140	846.354928	13.432640
20.918891	842.677505	13.437645
20.677251	852.676765	13.442650
21.137603	844.741968	13.447655
20.856364	854.315438	13.452659
20.727384	836.660742	13.457664
20.680216	838.090908	13.462669
20.346177	831.482946	13.467674
20.677048	844.625386	13.472679
20.641423	847.063014	13.477683
20.496075	856.673162	13.482688
21.138058	844.826728	13.487693
20.402999	842.826166	13.492698
20.469964	831.632882	13.497703
20.671474	836.079678	13.502707
20.628262	850.011955	13.507712
20.669234	839.975625	13.512717
20.460348	839.808815	13.517722
20.693592	841.798260	13.522727
20.865791	847.497170	13.527731
20.562024	844.345970	13.532736
20.302617	831.941536	13.537741
20.631576	844.281569	13.542746
20.706364	843.432391	13.547751
21.060463	849.744142	13.552755
20.558860	838.064344	13.557760
20.526471	826.965763	13.562765
20.569017	826.875550	13.567770
20.460630	828.577267	13.572775
20.865883	846.167699	13.577779
20.650723	841.941021	13.582784
20.739793	823.150792	13.587789
20.804090	833.265254	13.592794
20.740290	831.532963	13.597799
20.554746	826.825301	13.602803
20.337690	829.172010	13.607808
20.527193	823.448847	13.612813
20.542505	827.628856	13.617818
20.202103	835.595290	13.622823
20.608208	844.494544	13.627827
20.686837	857.554219	13.632832
20.745975	855.755005	13.637837
20.770271	864.819255	13.642842
20.712289	854.271967	13.647847
20.485156	841.058089	13.652851
20.404345	834.272534	13.657856
20.518396	845.453030	13.662861
20.841539	850.575903	13.667866
20.678385	855.104523	13.672871
20.883755	840.138964	13.677875
20.654623	832.419806	13.682880
20.714118	823.913411	13.687885
20.589470	830.522298	13.692890
20.342009	828.379308	13.697895
20.694149	833.959621	13.702899
20.414817	840.645227	13.707904
20.594071	840.585251	13.712909
20.709686	849.398371	13.717914
20.344250	850.901379	13.722919
20.991680	856.696391	13.727923
20.426062	843.358293	13.732928
20.896589	849.601009	13.737933
20.752282	857.633955	13.742938
20.587866	838.179201	13.747943
20.767013	834.583530	13.752947
20.418364	837.780749	13.757952
20.583530	825.772250	13.762957
20.664930	829.702010	13.767962
20.414081	836.390956	13.772967
20.501305	840.127391	13.777971
20.524467	858.308664	13.782976
20.906661	859.045842	13.787981
20.461685	857.751256	13.792986
20.654121	862.382444	13.797991
20.879354	856.781309	13.802995
20.475193	857.768495	13.808000
20.497960	845.719611	13.813005
20.211422	847.293618	13.818010
20.576189	858.404172	13.823015
21.036436	870.357414	13.828019
20.681985	862.614072	13.833024
20.432127	850.537700	13.838029
20.718236	864.914232	13.843034
21.003550	861.998672	13.848039
20.923100	846.033117	13.853043
20.702780	839.760270	13.858048
20.358681	838.530025	13.863053
20.392743	834.030198	13.868058
20.324777	842.309592	13.873063
20.583343	846.625859	13.878067
20.676109	857.995850	13.883072
20.994088	852.446159	13.888077
20.705902	846.650936	13.893082
20.520733	832.745939	13.898087
20.818908	833.772497	13.903091
20.511402	837.519848	13.908096
20.562459	825.767682	13.913101
20.678367	835.369263	13.918106
20.554779	839.139322	13.923111
20.673462	838.369879	13.928115
20.602098	841.932903	13.933120
20.542208	833.043400	13.938125
20.695128	835.890947	13.943130
20.245518	836.686674	13.948135
20.600214	840.858290	13.953139
20.627687	858.674581	13.958144
20.779146	842.771394	13.963149
20.466011	846.417138	13.968154
20.445265	848.507022	13.973159
20.933396	855.204274	13.978163
20.584548	850.070041	13.983168
20.548781	842.857806	13.988173
20.480564	851.517311	13.993178
20.802551	854.692730	13.998183
20.784944	847.092799	14.003187
20.358604	848.391044	14.008192
20.754175	855.456997	14.013210
20.528535	848.280874	14.018227
20.894443	852.542165	14.023245
21.208029	841.371099	14.028263
20.942326	842.006661	14.033280
20.822870	836.301678	14.038298
20.643110	845.707235	14.043315
20.537758	846.922832	14.048333
20.684968	843.070794	14.053351
20.453603	849.489569	14.058368
20.735675	844.247499	14.063386
20.715590	851.566945	14.068403
20.576328	835.281887	14.073421
20.861026	844.511118	14.078439
20.687321	866.883650	14.083456
20.835637	871.195383	14.088474
20.693870	874.696090	14.093491
20.679779	871.705044	14.098509
21.135726	868.692511	14.103527
20.792525	880.969746	14.108544
20.856733	868.811255	14.113562
20.976895	873.962750	14.118579
20.738488	877.519770	14.123597
21.125411	868.389774	14.128615
20.875773	875.434389	14.133632
20.969310	872.956283	14.138650
21.062393	879.777923	14.143667
21.012042	875.145711	14.148685
21.031938	877.237953	14.153703
20.992922	884.952116	14.158720
21.465696	873.664401	14.163738
21.329640	875.891628	14.168755
21.367717	886.105604	14.173773
21.407406	874.197983	14.178791
21.058685	883.768939	14.183808
21.101146	879.960341	14.188826
20.938941	870.148723	14.193843
21.081621	878.080867	14.198861
21.222619	875.032051	14.203879
21.037813	879.783880	14.208896
21.386579	887.879785	14.213914
21.710783	893.834016	14.218931
21.615305	888.696193	14.223949
21.711757	875.653236	14.228967
21.241659	882.169877	14.233984
21.047074	878.369200	14.239002
21.343417	872.415413	14.244019
21.343770	884.438082	14.249037
21.612673	879.471805	14.254055
21.745175	881.917319	14.259072
21.668600	882.579345	14.264090
21.257241	880.046488	14.269107
21.443641	878.316483	14.274125
21.450054	889.767184	14.279143
21.691800	905.038976	14.284160
21.787084	907.295376	14.289178
21.581793	902.494387	14.294195
21.272867	910.806890	14.299213
21.732509	912.039342	14.304231
21.579265	918.167261	14.309248
21.610184	918.318216	14.314266
21.907762	910.495467	14.319283
21.900286	913.469825	14.324301
21.844009	907.978106	14.329319
21.553165	911.033839	14.334336
21.691142	913.793089	14.339354
21.828352	905.413904	14.344371
21.206962	908.693818	14.349389
21.592868	909.717807	14.354407
21.840941	912.943987	14.359424
21.683093	908.827557	14.364442
21.804508	908.391498	14.369459
21.734889	916.963137	14.374477
21.886378	909.089758	14.379495
21.940500	917.135148	14.384512
22.177224	904.346645	14.389530
22.175314	903.809133	14.394547
21.745665	920.375657	14.399565
21.882035	915.730954	14.404583
21.625970	918.979343	14.409600
21.891443	931.511894	14.414618
22.061433	938.656350	14.419635
22.212711	949.552311	14.424653
22.545933	939.386348	14.429671
22.329250	943.234074	14.434688
22.360590	932.905480	14.439706
22.406383	914.210834	14.444723
22.182453	919.198577	14.449741
22.300881	907.298819	14.454759
22.009557	907.391059	14.459776
21.705938	922.421093	14.464794
22.330428	935.873232	14.469811
22.308093	950.292142	14.474829
22.376077	945.944628	14.479847
22.381590	952.608810	14.484864
22.265189	948.422837	14.489882
22.817135	940.185122	14.494899
22.688352	937.539545	14.499917
22.533045	932.032150	14.504935
22.412107	923.650085	14.509952
22.426551	934.003144	14.514970
22.747130	929.462762	14.519987
22.338580	934.969167	14.525005
22.445050	922.737823	14.530023
22.465844	943.149353	14.535040
22.400668	941.299018	14.540058
22.796649	935.673806	14.545075
22.202790	947.662314	14.550093
22.584318	943.024118	14.555111
22.463663	940.363086	14.560128
22.212783	948.056019	14.565146
22.662631	935.840683	14.570163
22.519041	948.251304	14.575181
22.737808	947.911401	14.580199
22.610201	944.715076	14.585216
22.572194	945.979714	14.590234
22.538492	943.180544	14.595251
22.438323	945.150373	14.600269
22.463518	951.514114	14.605287
22.878395	970.148230	14.610304
22.902416	969.680512	14.615322
23.469611	965.401233	14.620339
23.204732	954.940544	14.625357
23.060695	938.506694	14.630375
22.990832	942.527631	14.635392
22.698891	947.241514	14.640410
22.930813	938.041816	14.645427
22.906508	944.375696	14.650445
22.739441	938.236247	14.655463
23.065221	945.497430	14.660480
23.052487	960.128750	14.665498
23.213515	959.944347	14.670515
23.208573	950.470961	14.675533
23.245199	937.053674	14.680551
23.069002	942.287068	14.685568
22.747644	946.063401	14.690586
23.284610	951.914508	14.695603
23.360247	961.800076	14.700621
23.018298	968.483506	14.705639
23.462010	968.030646	14.710656
23.376667	981.975145	14.715674
23.425136	967.835493	14.720691
23.177547	958.238782	14.725709
23.322651	950.201232	14.730727
23.572423	966.848206	14.735744
23.345726	964.955990	14.740762
23.388679	951.792510	14.745779
23.388712	967.990107	14.750797
23.400506	961.449312	14.755815
23.346945	967.830341	14.760832
23.681833	976.052779	14.765850
23.664106	963.809750	14.770867
23.499030	948.502384	14.775885
23.345143	945.761709	14.780903
23.674887	956.858872	14.785920
23.477279	973.621254	14.790938
23.605713	966.242307	14.795955
23.695205	963.747527	14.800973
23.652202	963.971620	14.805991
23.713068	954.418522	14.811008
23.642314	969.628541	14.816026
23.632834	969.490210	14.821043
23.583345	973.391502	14.826061
23.738703	971.959020	14.831079
23.701256	971.144029	14.836096
23.708409	976.554259	14.841114
23.706431	968.739932	14.846131
23.702332	969.058494	14.851149
23.672609	973.760450	14.856167
23.891064	967.746688	14.861184
23.804912	976.767739	14.866202
23.701800	972.125035	14.871219
23.856241	975.772004	14.876237
23.831174	972.191230	14.881255
24.066012	964.724525	14.886272
23.743947	973.257810	14.891290
24.109176	972.411627	14.896307
23.913237	965.734077	14.901325
23.849864	970.991958	14.906343
23.984193	969.441708	14.911360
23.735057	973.256865	14.916378
23.801327	973.966899	14.921395
23.828014	976.839866	14.926413
24.303629	993.243209	14.931431
24.591200	987.061113	14.936448
24.076044	985.571980	14.941466
24.203926	977.799857	14.946483
24.217704	970.712902	14.951501
24.063552	969.603493	14.956519
24.513305	984.601519	14.961536
24.358960	986.243367	14.966554
24.366273	972.961283	14.971571
24.310617	977.596590	14.976589
24.222248	982.595767	14.981607
24.205435	980.037715	14.986624
24.261056	990.731886	14.991642
24.584812	985.074130	14.996659
24.634521	991.196452	15.001677
24.556270	987.015394	15.006695
24.869635	988.492981	15.011712
24.635532	978.137478	15.016730
24.621465	964.039265	15.021747
24.459439	965.018518	15.026765
24.338733	972.272277	15.031783
24.621487	970.929588	15.036800
24.639328	988.436272	15.041818
24.498112	993.555567	15.046835
24.784347	998.008934	15.051853
24.641888	997.630690	15.056871
24.854341	990.873833	15.061888
24.786877	994.947885	15.066906
24.903176	985.047724	15.071923
24.798377	978.039452	15.076941
24.871452	979.509746	15.081959
24.651557	964.848183	15.086976
24.971232	977.675725	15.091994
24.780963	975.936572	15.097011
24.842488	978.915669	15.102029
24.846638	995.026123	15.107047
25.068629	992.267959	15.112064
24.925364	996.800841	15.117082
24.760833	986.814909	15.122099
25.025846	992.673229	15.127117
24.926122	992.736482	15.132135
25.071534	995.305798	15.137152
24.946938	994.923132	15.142170
25.196217	1001.249581	15.147187
25.231515	993.536262	15.152205
25.043150	998.752741	15.157223
25.094905	996.855434	15.162240
25.204517	1003.235621	15.167258
25.361861	998.796759	15.172275
24.966625	998.878831	15.177293
25.060288	1009.746274	15.182311
25.181221	998.973906	15.187328
25.304896	1002.498373	15.192346
25.235888	996.612247	15.197363
25.494159	997.925589	15.202381
25.292772	998.270899	15.207399
25.512247	994.405723	15.212416
25.439837	993.674959	15.217434
25.463353	992.743277	15.222451
25.346078	991.107312	15.227469
25.155379	998.628651	15.232487
25.714502	995.524132	15.237504
25.406258	994.179748	15.242522
25.161685	997.228119	15.247539
25.322071	990.640016	15.252557
25.159474	996.173282	15.257575
25.436127	993.006850	15.262592
25.473914	1004.893086	15.267610
25.396275	997.323620	15.272627
25.356335	1005.204736	15.277645
25.518765	1031.192217	15.282663
25.753983	1029.304970	15.287680
25.839465	1034.115986	15.292698
25.748429	1025.935159	15.297715
25.961746	1031.402189	15.302733
25.869249	1031.583840	15.307751
26.095687	1029.469904	15.312768
25.865235	1028.341199	15.317786
26.115373	1014.919673	15.322803
26.288629	993.753811	15.327821
25.796339	1001.889545	15.332839
26.093652	992.021857	15.337856
25.986001	996.714227	15.342874
26.129121	994.147967	15.347891
25.887612	991.322158	15.352909
25.719987	988.481418	15.357927
26.085369	993.560810	15.362944
25.712949	992.281719	15.367962
25.873000	1007.112044	15.372979
26.026235	1017.510666	15.377997
26.042764	1032.085481	15.383015
26.039035	1018.312757	15.388032
26.068707	1028.963904	15.393050
25.802465	1031.631918	15.398067
25.822683	1020.936945	15.403085
26.112013	1025.624210	15.408103
26.062762	1019.322789	15.413120
25.933235	1028.869890	15.418138
26.002503	1028.728437	15.423155
26.333988	1043.347411	15.428173
26.395642	1065.813272	15.433191
26.996974	1067.644489	15.438208
26.736377	1051.914946	15.443226
26.465801	1043.926340	15.448243
26.630354	1022.417330	15.453261
26.410429	1018.866050	15.458279
26.466733	1017.457228	15.463296
26.508869	1019.064595	15.468314
26.085768	1015.850890	15.473331
26.532508	1007.134413	15.478349
26.518929	1024.276490	15.483367
26.861425	1027.133704	15.488384
26.857305	1018.872950	15.493402
26.845304	1025.014567	15.498419
26.814287	1019.375630	15.503437
26.158552	1013.158359	15.508455
26.831201	1017.635045	15.513472
26.786916	1022.260688	15.518490
26.697776	1028.425620	15.523507
27.002952	1025.097329	15.528525
26.821932	1033.940063	15.533543
26.803357	1034.051721	15.538560
26.871612	1035.445711	15.543578
27.010188	1038.535226	15.548595
27.026688	1037.164212	15.553613
26.738390	1047.416200	15.558631
27.083286	1038.026959	15.563648
27.321420	1045.256554	15.568666
27.110908	1036.053428	15.573683
27.019711	1012.123426	15.578701
26.796675	1018.205890	15.583719
27.041065	1029.486611	15.588736
27.097213	1036.922980	15.593754
26.985603	1039.003186	15.598771
26.926381	1049.039312	15.603789
26.638433	1048.920227	15.608807
26.991453	1045.673963	15.613824
26.885081	1043.506140	15.618842
27.060631	1043.467286	15.623859
27.245385	1040.551456	15.628877
27.108402	1047.864478	15.633895
27.306753	1066.169882	15.638912
27.646610	1071.797644	15.643930
27.598018	1060.808448	15.648947
27.616227	1049.467256	15.653965
27.166601	1044.615526	15.658983
27.420183	1039.510066	15.664000
27.414794	1052.851993	15.669018
27.477679	1062.382585	15.674035
27.651350	1067.651457	15.679053
27.704900	1064.265762	15.684071
27.588366	1057.814606	15.689088
27.558425	1048.085592	15.694106
27.396988	1054.317123	15.699123
27.578689	1063.410337	15.704141
27.731953	1076.226755	15.709159
28.029473	1074.661477	15.714176
27.761534	1070.054468	15.719194
27.556800	1066.854687	15.724211
27.956700	1062.693300	15.729229
27.951736	1072.933149	15.734247
28.110646	1068.585252	15.739264
27.964366	1046.932299	15.744282
27.560829	1046.049851	15.749299
27.465465	1046.883196	15.754317
27.656381	1064.154726	15.759335
27.942800	1063.418637	15.764352
27.945145	1074.884291	15.769370
27.621178	1071.524199	15.774387
27.991477	1074.081257	15.779405
27.851294	1070.251402	15.784423
27.669262	1070.785537	15.789440
27.908364	1065.479456	15.794458
28.112895	1073.192628	15.799475
28.221059	1064.550568	15.804493
28.145909	1071.658682	15.809511
27.998452	1076.388888	15.814528
27.919121	1083.681721	15.819546
28.097195	1097.040044	15.824563
28.699183	1091.738996	15.829581
28.484386	1095.174325	15.834599
28.448192	1093.689012	15.839616
28.658289	1080.670218	15.844634
28.411374	1076.187271	15.849651
28.565455	1068.086875	15.854669
28.506692	1066.356625	15.859687
28.530023	1070.625430	15.864704
28.521455	1064.183792	15.869722
28.342794	1068.220544	15.874739
28.724667	1063.085175	15.879757
28.652630	1066.705369	15.884775
28.476397	1062.143512	15.889792
28.863235	1065.475010	15.894810
28.495442	1058.403252	15.899827
28.670691	1061.282429	15.904845
28.951771	1069.869010	15.909863
28.588789	1055.507031	15.914880
28.846615	1053.814378	15.919898
28.528340	1066.429141	15.924915
28.959954	1060.961795	15.929933
29.088331	1061.057880	15.934951
28.660248	1061.689461	15.939968
28.916918	1060.519240	15.944986
28.842217	1066.946156	15.950003
28.948584	1058.568657	15.955021
28.976657	1064.263448	15.960039
28.859683	1064.626756	15.965056
29.108088	1056.298963	15.970074
28.908426	1066.322895	15.975091
28.974244	1059.109618	15.980109
29.204004	1075.341481	15.985127
29.119524	1074.444323	15.990144
29.093748	1060.863839	15.995162
29.067653	1066.218057	16.000179
29.151238	1076.368279	16.005197
29.077412	1083.929224	16.010215
28.993231	1089.959683	16.015232
29.516974	1077.751319	16.020250
29.331339	1089.891913	16.025267
29.132974	1088.109993	16.030285
29.083063	1085.266189	16.035303
29.339997	1092.307191	16.040320
29.706958	1085.168567	16.045338
29.597023	1092.087183	16.050355
29.715333	1088.985312	16.055373
29.765802	1084.118300	16.060391
29.308277	1087.535711	16.065408
29.329879	1087.044780	16.070426
29.143681	1090.198691	16.075443
29.607259	1085.506465	16.080461
29.664665	1091.039285	16.085479
29.291695	1096.727266	16.090496
29.397058	1102.172216	16.095514
29.387167	1091.585814	16.100531
29.238870	1095.125368	16.105549
29.253656	1096.351711	16.110567
29.665113	1112.818907	16.115584
29.740792	1105.426281	16.120602
29.739422	1108.989595	16.125619
29.950831	1116.125960	16.130637
30.087889	1115.371219	16.135655
29.849822	1113.468211	16.140672
30.317953	1115.411917	16.145690
30.431845	1111.624899	16.150707
30.145430	1095.641446	16.155725
30.135123	1078.305205	16.160743
29.631789	1092.083667	16.165760
30.132537	1080.278521	16.170778
30.072242	1090.708108	16.175795
30.153704	1095.464729	16.180813
29.878314	1092.299807	16.185831
30.101920	1122.779736	16.190848
30.256763	1112.297608	16.195866
30.670548	1119.091807	16.200883
30.304629	1114.092993	16.205901
30.352979	1087.836102	16.210919
29.983222	1098.494378	16.215936
30.322413	1103.911472	16.220954
30.364582	1116.541150	16.225971
30.386393	1121.883028	16.230989
30.609177	1122.857545	16.236007
30.644719	1128.307349	16.241024
30.391477	1111.264649	16.246042
30.149102	1106.047930	16.251059
30.370094	1112.196467	16.256077
30.542828	1111.509969	16.261095
30.048038	1122.181912	16.266112
30.440659	1116.758517	16.271130
30.506250	1125.882874	16.276147
30.512069	1117.323174	16.281165
30.675181	1120.144523	16.286183
30.329512	1117.676651	16.291200
30.720965	1115.254809	16.296218
30.535622	1122.029735	16.301235
30.327418	1126.543127	16.306253
30.792692	1126.667279	16.311271
30.708347	1150.164878	16.316288
31.017594	1149.293008	16.321306
30.905195	1152.562579	16.326323
30.935516	1146.242118	16.331341
31.184662	1150.327065	16.336359
31.246728	1156.181640	16.341376
31.287076	1146.968320	16.346394
31.257250	1146.904020	16.351411
31.210225	1128.617163	16.356429
31.231203	1116.772104	16.361447
31.003276	1120.414028	16.366464
30.954762	1111.762322	16.371482
31.106018	1126.399115	16.376499
31.263202	1140.663738	16.381517
31.534219	1134.982876	16.386535
31.218539	1146.117059	16.391552
30.966437	1143.335380	16.396570
31.037578	1139.130451	16.401587
31.281787	1142.085163	16.406605
31.442171	1139.201516	16.411623
31.372479	1150.337368	16.416640
31.465381	1142.682423	16.421658
31.579358	1141.228211	16.426675
31.329554	1139.883930	16.431693
31.601485	1140.199369	16.436711
31.358031	1140.305996	16.441728
31.429314	1142.034572	16.446746
31.461734	1141.143933	16.451763
31.527939	1141.957806	16.456781
31.651825	1142.710569	16.461799
31.242935	1136.392524	16.466816
31.472721	1145.210703	16.471834
32.010962	1152.872266	16.476851
31.695643	1162.225715	16.481869
32.309841	1163.049717	16.486887
32.009116	1157.672397	16.491904
31.906993	1140.451401	16.496922
31.732984	1137.432322	16.501939
31.467320	1136.746531	16.506957
32.054803	1146.064518	16.511975
31.937138	1162.232340	16.516992
32.048403	1164.887359	16.522010
32.272056	1173.159112	16.527027
32.205464	1167.297700	16.532045
31.873031	1158.299561	16.537063
32.331411	1165.187345	16.542080
32.428316	1156.388148	16.547098
32.435210	1138.819426	16.552115
31.776800	1140.304156	16.557133
31.961817	1149.300940	16.562151
32.053009	1168.839531	16.567168
32.263843	1164.552538	16.572186
32.617868	1165.954446	16.577203
32.517787	1169.009694	16.582221
32.597336	1165.597806	16.587239
32.611010	1166.048819	16.592256
32.726413	1162.434582	16.597274
32.673511	1145.669778	16.602291
32.394027	1141.319421	16.607309
32.508556	1134.109349	16.612327
32.504181	1138.536752	16.617344
32.869363	1155.017670	16.622362
32.870016	1139.524792	16.627379
32.356431	1142.988910	16.632397
32.661457	1146.056620	16.637415
32.490875	1152.605834	16.642432
32.806906	1161.141276	16.647450
32.697767	1160.699510	16.652467
32.817387	1161.767564	16.657485
33.192341	1164.674686	16.662503
32.907959	1170.203846	16.667520
32.973563	1170.698488	16.672538
32.970864	1165.204417	16.677555
32.775773	1167.065145	16.682573
33.127627	1160.687103	16.687591
33.021876	1163.722805	16.692608
32.902550	1167.644726	16.697626
32.933292	1166.837725	16.702643
32.837681	1170.501030	16.707661
32.984691	1166.971414	16.712679
32.952164	1162.388178	16.717696
32.750483	1166.851777	16.722714
32.975227	1161.171993	16.727731
33.115582	1162.806183	16.732749
33.406794	1168.356798	16.737767
33.293675	1165.334295	16.742784
33.444358	1179.611005	16.747802
33.500803	1169.382059	16.752819
33.403262	1177.198522	16.757837
33.097067	1175.185248	16.762855
33.273192	1182.896717	16.767872
33.470353	1188.257844	16.772890
33.568321	1190.150486	16.777907
33.314721	1197.013412	16.782925
33.557350	1199.908612	16.787943
33.589716	1194.179273	16.792960
33.804817	1198.192583	16.797978
33.583823	1188.863614	16.802995
33.526740	1193.194045	16.808013
33.646246	1187.055975	16.813031
33.369575	1198.121053	16.818048
33.783408	1199.936576	16.823066
33.846137	1188.797391	16.828083
33.663987	1199.339300	16.833101
33.709348	1193.603169	16.838119
33.791676	1190.900277	16.843136
33.905711	1197.971988	16.848154
33.975412	1195.950668	16.853171
33.748695	1216.203854	16.858189
34.187795	1222.791141	16.863207
34.334641	1226.892425	16.868224
34.160365	1226.733184	16.873242
34.404245	1217.894779	16.878259
34.290143	1207.749637	16.883277
34.242955	1186.017750	16.888295
34.255920	1181.392644	16.893312
33.960610	1194.865887	16.898330
34.201454	1201.697147	16.903347
34.348873	1216.002728	16.908365
34.587377	1221.459522	16.913383
34.362869	1216.222610	16.918400
34.405248	1229.766296	16.923418
34.553571	1218.100621	16.928435
34.446613	1216.812203	16.933453
34.698698	1223.835166	16.938471
34.613451	1215.483418	16.943488
34.775970	1213.060321	16.948506
34.634728	1210.824100	16.953523
34.311232	1219.027415	16.958541
34.685473	1208.258536	16.963559
34.583866	1213.624852	16.968576
34.438690	1227.189011	16.973594
34.694185	1219.204494	16.978611
34.628174	1219.839681	16.983629
34.928802	1214.819468	16.988647
35.005428	1208.455415	16.993664
34.762712	1211.124427	16.998682
34.723337	1210.765915	17.003699
34.518032	1218.256663	17.008717
34.836644	1216.739917	17.013735
34.777361	1229.322951	17.018752
34.823797	1239.180333	17.023770
35.220175	1235.466207	17.028787
35.273020	1238.073927	17.033805
35.149472	1239.778532	17.038823
35.156206	1245.824443	17.043840
35.044069	1251.153125	17.048858
35.496543	1244.862821	17.053875
35.045692	1245.518489	17.058893
35.157149	1242.966675	17.063911
34.918394	1235.943463	17.068928
35.051575	1244.759808	17.073946
35.399053	1242.560468	17.078963
35.258582	1247.766251	17.083981
35.133292	1242.269680	17.088999
35.356626	1247.341932	17.094016
35.562787	1273.514785	17.099034
35.768164	1271.353836	17.104051
35.746859	1275.599933	17.109069
35.903287	1268.875480	17.114087
35.963108	1242.462320	17.119104
35.706351	1244.260532	17.124122
35.886856	1234.269736	17.129139
35.737303	1239.701910	17.134157
35.795594	1238.978603	17.139175
35.757545	1235.380957	17.144192
35.800566	1235.651110	17.149210
36.094465	1228.527216	17.154227
35.823380	1238.502881	17.159245
35.604329	1252.056823	17.164263
35.901907	1257.810955	17.169280
35.524607	1270.034178	17.174298
36.241062	1264.793466	17.179315
36.040531	1269.967936	17.184333
36.076446	1271.164182	17.189351
36.276834	1263.032697	17.194368
36.270366	1266.939790	17.199386
36.448751	1268.772425	17.204403
36.216679	1262.690396	17.209421
36.368388	1264.347956	17.214439
36.612849	1264.475867	17.219456
36.179725	1269.020457	17.224474
36.390667	1259.658731	17.229491
36.354403	1263.196188	17.234509
36.263160	1270.078873	17.239527
36.410819	1256.961339	17.244544
36.316290	1270.051835	17.249562
36.637864	1257.902309	17.254579
36.603886	1262.897626	17.259597
36.543560	1264.758894	17.264615
36.745512	1256.718401	17.269632
36.549889	1263.065587	17.274650
36.659244	1255.090201	17.279667
36.621109	1272.533795	17.284685
36.977812	1288.347667	17.289703
37.046926	1283.526380	17.294720
37.125495	1284.063004	17.299738
37.205743	1275.905055	17.304755
36.705389	1269.137485	17.309773
36.580042	1267.416257	17.314791
37.167780	1272.691526	17.319808
37.122570	1282.403101	17.324826
37.113423	1285.448590	17.329843
37.546322	1281.766382	17.334861
37.184043	1276.143998	17.339879
37.150395	1268.337707	17.344896
36.914015	1262.630754	17.349914
37.364002	1269.958810	17.354931
37.426489	1281.330090	17.359949
36.930572	1285.061988	17.364967
37.250272	1276.983827	17.369984
37.345248	1280.953398	17.375002
37.346385	1284.409387	17.380019
37.514884	1287.692390	17.385037
37.572851	1284.999659	17.390055
37.362741	1283.773305	17.395072
36.949212	1286.916324	17.400090
37.240757	1284.593762	17.405107
37.360056	1288.614512	17.410125
37.167668	1293.749938	17.415143
37.488760	1297.095124	17.420160
37.434753	1317.674844	17.425178
37.593628	1319.548351	17.430195
38.085796	1315.866120	17.435213
38.107558	1320.055023	17.440231
37.986109	1316.116719	17.445248
37.807821	1317.108026	17.450266
38.144375	1311.789460	17.455283
38.134367	1311.220190	17.460301
37.945019	1317.898316	17.465319
38.288058	1307.675475	17.470336
38.262088	1317.758394	17.475354
38.541714	1307.665220	17.480371
38.267916	1288.530269	17.485389
37.865646	1291.833518	17.490407
38.379027	1292.915860	17.495424
38.279085	1306.825245	17.500442
38.554151	1302.411562	17.505459
38.646555	1299.208383	17.510477
38.229316	1290.745943	17.515495
38.353567	1277.424480	17.520512
38.377659	1292.844657	17.525530
38.554923	1307.452316	17.530547
38.641353	1302.228703	17.535565
38.517273	1312.116476	17.540583
38.815761	1304.200563	17.545600
38.419993	1311.179028	17.550618
38.784302	1308.096079	17.555635
38.987020	1302.589644	17.560653
38.662510	1307.393781	17.565671
38.836358	1296.423985	17.570688
38.642831	1308.202641	17.575706
38.593061	1312.520930	17.580723
38.907863	1305.719290	17.585741
38.582292	1314.591540	17.590759
38.636793	1303.620324	17.595776
38.285128	1310.204781	17.600794
38.547107	1299.787230	17.605811
38.974716	1296.746099	17.610829
38.779733	1314.420831	17.615847
38.930544	1321.134370	17.620864
39.056381	1332.471989	17.625882
39.277954	1329.152245	17.630899
39.384032	1335.984613	17.635917
39.218139	1335.416609	17.640935
39.438279	1321.966551	17.645952
39.424252	1336.096648	17.650970
39.280248	1335.575491	17.655987
39.491184	1328.691303	17.661005
39.221872	1344.581485	17.666023
39.260266	1328.490912	17.671040
39.075312	1333.430106	17.676058
39.261883	1329.016372	17.681075
39.145021	1332.887605	17.686093
39.271561	1334.550761	17.691111
39.797905	1339.373365	17.696128
39.853593	1354.897110	17.701146
39.913966	1349.790897	17.706163
39.764595	1331.568873	17.711181
39.420667	1344.878543	17.716199
39.970133	1346.652004	17.721216
40.261105	1368.579951	17.726234
39.911348	1356.276285	17.731251
40.234325	1353.085085	17.736269
40.017060	1343.009787	17.741287
40.035610	1331.153928	17.746304
39.851192	1335.279762	17.751322
39.860942	1345.366442	17.756339
40.352299	1357.687155	17.761357
40.451517	1361.383930	17.766375
40.416868	1362.473458	17.771392
40.345788	1364.635337	17.776410
40.184333	1354.879901	17.781427
40.205591	1352.452568	17.786445
40.513525	1362.213270	17.791463
40.382956	1357.327848	17.796480
40.344270	1369.454675	17.801498
40.139718	1363.490914	17.806515
40.434268	1359.085118	17.811533
40.289400	1364.793452	17.816551
40.084417	1360.712725	17.821568
40.476658	1359.599513	17.826586
40.227460	1361.001692	17.831603
40.460048	1364.368875	17.836621
40.588465	1389.022954	17.841639
40.885661	1385.529896	17.846656
40.892052	1388.406182	17.851674
40.998474	1387.339340	17.856691
40.701665	1384.609576	17.861709
40.797611	1394.493774	17.866727
40.856916	1388.546910	17.871744
40.831245	1383.414295	17.876762
40.654599	1390.523808	17.881779
40.928384	1376.987277	17.886797
40.993063	1382.580397	17.891815
41.039867	1380.811249	17.896832
41.154994	1385.007303	17.901850
41.068011	1381.739905	17.906867
41.359844	1378.994127	17.911885
41.256014	1374.189381	17.916903
41.215723	1381.366021	17.921920
41.573100	1387.566859	17.926938
41.322410	1385.075926	17.931955
41.507537	1397.617765	17.936973
41.436676	1405.596841	17.941991
41.666384	1409.640130	17.947008
41.703944	1407.115804	17.952026
41.551493	1412.009727	17.957043
41.751473	1411.887537	17.962061
41.426665	1415.902859	17.967079
41.619974	1418.508659	17.972096
41.681670	1407.707682	17.977114
42.202120	1400.562518	17.982131
42.102522	1406.566464	17.987149
41.938642	1415.243095	17.992167
41.865764	1412.747394	17.997184
41.628815	1409.119291	18.002202
41.728891	1411.518156	18.007219
41.947685	1402.573525	18.012237
42.051248	1407.069527	18.017255
42.101668	1410.894438	18.022272
42.011429	1403.948133	18.027290
41.951473	1411.396921	18.032307
41.991823	1404.645299	18.037325
42.013146	1415.651217	18.042343
42.440138	1417.251519	18.047360
42.391846	1420.558903	18.052378
42.320254	1430.874914	18.057395
42.620230	1428.097939	18.062413
43.107832	1422.749737	18.067431
42.677703	1405.502086	18.072448
42.957975	1387.063599	18.077466
42.412946	1392.595085	18.082483
42.811053	1394.906301	18.087501
42.291750	1395.906383	18.092519
42.452317	1389.074245	18.097536
42.866602	1400.087480	18.102554
42.833906	1412.979475	18.107571
42.795177	1420.249483	18.112589
42.958652	1427.465222	18.117607
43.148123	1423.586629	18.122624
43.140269	1407.449075	18.127642
43.045322	1396.564547	18.132659
42.737586	1387.010176	18.137677
43.005258	1408.576162	18.142695
42.879673	1418.277837	18.147712
43.162036	1411.432557	18.152730
42.750178	1426.780042	18.157747
42.870145	1422.415443	18.162765
43.021794	1414.334121	18.167783
42.885873	1416.323086	18.172800
43.044767	1423.097519	18.177818
42.905439	1432.710158	18.182835
43.582958	1444.695291	18.187853
43.632824	1450.589686	18.192871
43.409952	1445.311529	18.197888
43.804494	1443.187241	18.202906
43.839010	1448.966889	18.207923
44.105307	1438.174158	18.212941
43.749898	1423.345759	18.217959
43.934972	1419.979905	18.222976
43.829177	1407.077270	18.227994
43.877555	1410.307098	18.233011
43.923244	1407.768105	18.238029
43.980786	1402.033095	18.243047
44.124980	1407.709501	18.248064
44.131283	1403.338653	18.253082
43.975419	1406.018230	18.258099
43.776699	1407.200784	18.263117
43.646066	1413.478680	18.268135
43.775240	1420.999557	18.273152
44.273654	1428.800547	18.278170
43.752344	1441.442509	18.283187
44.418520	1437.406083	18.288205
44.236578	1439.001256	18.293223
43.999405	1441.857408	18.298240
44.605416	1436.717626	18.303258
44.227631	1441.028491	18.308275
44.361626	1442.474959	18.313293
44.572765	1435.293376	18.318311
44.399059	1442.863358	18.323328
44.481413	1432.749649	18.328346
44.329181	1436.075974	18.333363
44.544592	1440.875056	18.338381
44.593847	1450.156384	18.343399
44.643469	1458.883150	18.348416
45.358685	1456.822552	18.353434
45.095091	1460.340468	18.358451
45.000620	1447.502061	18.363469
44.865631	1441.925161	18.368487
44.896656	1448.073466	18.373504
45.139621	1452.951530	18.378522
45.318966	1457.038259	18.383539
45.110115	1444.045059	18.388557
45.112058	1436.437501	18.393575
44.956384	1452.359228	18.398592
45.165080	1452.571500	18.403610
45.253820	1463.538387	18.408627
44.995382	1465.395883	18.413645
45.107355	1462.073926	18.418663
45.292179	1468.931552	18.423680
45.209444	1460.454202	18.428698
45.051397	1465.209031	18.433715
45.321537	1458.438826	18.438733
45.248061	1467.917498	18.443751
45.080192	1474.022027	18.448768
45.888267	1485.044097	18.453786
45.627894	1488.601620	18.458803
45.561650	1485.892482	18.463821
46.098064	1484.105798	18.468839
45.790671	1492.475016	18.473856
46.090663	1482.302966	18.478874
45.932466	1486.053412	18.483891
45.931633	1482.652697	18.488909
46.115542	1482.286883	18.493927
45.798091	1482.520933	18.498944
46.111116	1484.586176	18.503962
46.064800	1489.819500	18.508979
45.883983	1489.706131	18.513997
46.200922	1488.302888	18.519015
46.168414	1488.607902	18.524032
46.340107	1482.146767	18.529050
46.490230	1494.836638	18.534067
46.408260	1490.118819	18.539085
46.211245	1485.022934	18.544103
45.924112	1489.759031	18.549120
46.261370	1484.633780	18.554138
46.158581	1484.396278	18.559155
46.589054	1491.813294	18.564173
46.740153	1503.024318	18.569191
46.415419	1513.061424	18.574208
46.989569	1505.773145	18.579226
46.736887	1511.206137	18.584243
47.093962	1514.195625	18.589261
46.945875	1507.547158	18.594279
47.218409	1513.147293	18.599296
47.060851	1498.704916	18.604314
46.795597	1488.741779	18.609331
46.822284	1503.924231	18.614349
47.048416	1497.405642	18.619367
47.112241	1501.837223	18.624384
47.107253	1503.500139	18.629402
47.052871	1503.731560	18.634419
47.228773	1503.197129	18.639437
47.217634	1495.727699	18.644455
47.370673	1507.691138	18.649472
47.741095	1494.150884	18.654490
47.229614	1500.492703	18.659507
47.310946	1507.922938	18.664525
47.666847	1500.391821	18.669543
47.391141	1503.801564	18.674560
47.817579	1498.884676	18.679578
47.710366	1496.738155	18.684595
47.561634	1494.756350	18.689613
47.747844	1492.137513	18.694631
47.474080	1499.986187	18.699648
47.830815	1499.802816	18.704666
47.699489	1505.895237	18.709683
47.388293	1515.099596	18.714701
48.007057	1517.723293	18.719719
47.912727	1535.423140	18.724736
48.244289	1527.864428	18.729754
48.293664	1535.735520	18.734771
48.127621	1532.917229	18.739789
48.475947	1523.333642	18.744807
48.244291	1531.352589	18.749824
48.355322	1529.461491	18.754842
48.572300	1526.974599	18.759859
48.183449	1522.201103	18.764877
48.266628	1524.373798	18.769895
48.123735	1517.234481	18.774912
48.436863	1526.534338	18.779930
48.390111	1523.815792	18.784947
48.227194	1523.641363	18.789965
48.366731	1530.228591	18.794983
48.227973	1525.436444	18.800000
48.029388	1526.405832	18.805018
48.483881	1539.266644	18.810035
48.476173	1553.663370	18.815053
48.530077	1546.062413	18.820071
48.602173	1545.343967	18.825088
48.846480	1549.428227	18.830106
48.903556	1553.014578	18.835123
48.625733	1554.707642	18.840141
49.469800	1570.280495	18.845159
49.272510	1581.588043	18.850176
49.617411	1572.276330	18.855194
49.556250	1556.940735	18.860211
49.421006	1543.131857	18.865229
49.657883	1541.254508	18.870247
49.431060	1545.637284	18.875264
49.424163	1542.811700	18.880282
49.616847	1542.690673	18.885299
49.182029	1546.047934	18.890317
49.391780	1544.672006	18.895335
49.230693	1554.025489	18.900352
49.509533	1561.150534	18.905370
49.827685	1570.224666	18.910387
49.626743	1579.682053	18.915405
49.777549	1579.039933	18.920423
50.033612	1587.460920	18.925440
49.864943	1582.467449	18.930458
49.753739	1585.133644	18.935475
49.759920	1580.946814	18.940493
49.871076	1572.716912	18.945511
49.887598	1578.697691	18.950528
49.709161	1574.970548	18.955546
50.127640	1573.512562	18.960563
49.733327	1581.928729	18.965581
50.304998	1590.720971	18.970599
50.400745	1613.220783	18.975616
50.325545	1594.550851	18.980634
50.379358	1594.469276	18.985651
50.280907	1593.805558	18.990669
50.539411	1592.378591	18.995687
50.499732	1598.624755	19.000704
50.435070	1594.744175	19.005722
50.699808	1597.404686	19.010739
50.724509	1603.296077	19.015757
50.556097	1596.679912	19.020775
50.305157	1601.924675	19.025792
50.502720	1595.643417	19.030810
50.700111	1600.694762	19.035827
50.293070	1621.012664	19.040845
50.841389	1618.439091	19.045863
50.871759	1631.734159	19.050880
51.108846	1628.311196	19.055898
51.431653	1622.956957	19.060915
51.121726	1625.304051	19.065933
51.376469	1625.886527	19.070951
51.003901	1630.876979	19.075968
51.191062	1629.285199	19.080986
51.314227	1628.697824	19.086003
50.971246	1636.837622	19.091021
51.077799	1625.742239	19.096039
51.743110	1636.603930	19.101056
51.438033	1653.746046	19.106074
51.894937	1649.438546	19.111091
51.597837	1652.034509	19.116109
51.802142	1651.533298	19.121127
51.544165	1655.134525	19.126144
51.517959	1652.039853	19.131162
51.993828	1643.602301	19.136179
51.698382	1655.994482	19.141197
51.943916	1650.847621	19.146215
51.884732	1654.659402	19.151232
51.726900	1655.387120	19.156250
52.152352	1644.602676	19.161267
51.785863	1652.681734	19.166285
51.930557	1645.310076	19.171303
52.127706	1663.035167	19.176320
52.153662	1674.405501	19.181338
52.544002	1674.995455	19.186355
52.118526	1677.715721	19.191373
52.693878	1674.794891	19.196391
52.582149	1683.173913	19.201408
52.504446	1681.827300	19.206426
52.810425	1674.909701	19.211443
52.710323	1681.664998	19.216461
52.734140	1670.441983	19.221479
52.813399	1672.406103	19.226496
52.780164	1673.810049	19.231514
53.056816	1662.115687	19.236531
53.108126	1675.671737	19.241549
53.278062	1662.042960	19.246567
53.478515	1669.843623	19.251584
53.268116	1657.943784	19.256602
53.095003	1643.683077	19.261619
52.785217	1631.048742	19.266637
52.948499	1652.107111	19.271655
53.091381	1654.864936	19.276672
53.215824	1669.567119	19.281690
53.531266	1672.918802	19.286707
53.081459	1675.591822	19.291725
53.334129	1667.019172	19.296743
53.517373	1668.906142	19.301760
53.444904	1670.700969	19.306778
53.377228	1668.924874	19.311795
53.107414	1669.542244	19.316813
53.241659	1669.391996	19.321831
53.430061	1680.687662	19.326848
53.595296	1695.098633	19.331866
53.404541	1690.343827	19.336883
53.609328	1706.340483	19.341901
53.836599	1700.573568	19.346919
54.086985	1699.153391	19.351936
53.678703	1707.803103	19.356954
54.061343	1701.612626	19.361971
54.164443	1693.291128	19.366989
54.042963	1699.219243	19.372007
54.414061	1714.208553	19.377024
54.272815	1729.168685	19.382042
54.430083	1723.665409	19.387059
54.241857	1728.609976	19.392077
54.643851	1720.162926	19.397095
54.742265	1721.403514	19.402112
54.855892	1725.429224	19.407130
54.712363	1726.625810	19.412147
54.811886	1723.725013	19.417165
54.921359	1708.208668	19.422183
54.682812	1704.506808	19.427200
54.525089	1716.136143	19.432218
55.151848	1715.308779	19.437235
54.777556	1736.428622	19.442253
54.952862	1733.121672	19.447271
54.961587	1730.001748	19.452288
54.779055	1727.547864	19.457306
55.069039	1717.806706	19.462323
55.017283	1725.124564	19.467341
55.179822	1720.247332	19.472359
55.126608	1735.927286	19.477376
54.947668	1730.491785	19.482394
55.514491	1723.286371	19.487411
55.185661	1728.424832	19.492429
55.107993	1746.707474	19.497447
55.516992	1753.487795	19.502464
55.455213	1748.926343	19.507482
55.561109	1751.133990	19.512499
55.588356	1753.168554	19.517517
55.746891	1748.208576	19.522535
55.850359	1745.482548	19.527552
55.735975	1751.729680	19.532570
56.190242	1745.287075	19.537587
55.923543	1744.867271	19.542605
55.973781	1745.284942	19.547623
56.229554	1744.320891	19.552640
56.114547	1751.510416	19.557658
56.433059	1745.299472	19.562675
56.345920	1745.944343	19.567693
56.389235	1743.319149	19.572711
56.509881	1741.633354	19.577728
56.286579	1748.045728	19.582746
56.178671	1740.789031	19.587763
56.273793	1749.479612	19.592781
56.374131	1742.885016	19.597799
56.590512	1758.546382	19.602816
56.456822	1771.899206	19.607834
56.643594	1767.216306	19.612851
56.893900	1780.689591	19.617869
56.630494	1775.276983	19.622887
57.143381	1774.754870	19.627904
56.932354	1778.561796	19.632922
56.949404	1771.440893	19.637939
57.333496	1771.675539	19.642957
57.063582	1781.044949	19.647975
57.273321	1777.244047	19.652992
56.987064	1779.386818	19.658010
56.933150	1772.750739	19.663027
57.078299	1778.231287	19.668045
56.797635	1775.590899	19.673063
57.046635	1778.740046	19.678080
57.301787	1793.483647	19.683098
57.538944	1797.352815	19.688115
57.524141	1799.124302	19.693133
57.365544	1802.231488	19.698151
57.571309	1803.222141	19.703168
57.281494	1797.220671	19.708186
57.805535	1793.336603	19.713203
57.380670	1796.337594	19.718221
57.639910	1815.961159	19.723239
58.023305	1823.407093	19.728256
57.904177	1825.764691	19.733274
57.927397	1830.210713	19.738291
58.365043	1826.817857	19.743309
57.824426	1832.953666	19.748327
58.117845	1827.859671	19.753344
58.262615	1835.147029	19.758362
58.308981	1829.128899	19.763379
58.614100	1834.606765	19.768397
58.205351	1827.949382	19.773415
58.801253	1822.226667	19.778432
58.543200	1830.843840	19.783450
58.383796	1829.019430	19.788467
58.733328	1836.103448	19.793485
58.636644	1856.128345	19.798503
59.071451	1852.119272	19.803520
58.994884	1850.276929	19.808538
59.149626	1841.225048	19.813555
59.097087	1843.577534	19.818573
59.101732	1851.560543	19.823591
59.142821	1843.696404	19.828608
59.132657	1849.511652	19.833626
59.045770	1847.310710	19.838643
59.392503	1838.951848	19.843661
59.309499	1843.170982	19.848679
59.460766	1841.846042	19.853696
59.434144	1835.688530	19.858714
59.304090	1834.914216	19.863731
59.380607	1832.427651	19.868749
59.722181	1839.268320	19.873767
59.744707	1834.923858	19.878784
59.760565	1841.911648	19.883802
59.772806	1838.386847	19.888819
59.938011	1839.321047	19.893837
59.715562	1841.972781	19.898855
60.030791	1838.287968	19.903872
60.005353	1836.487025	19.908890
59.819525	1830.405246	19.913907
59.776144	1836.105443	19.918925
59.826248	1840.418972	19.923943
59.752848	1831.315387	19.928960
59.914701	1852.092686	19.933978
60.033231	1863.461776	19.938995
60.167906	1860.210832	19.944013
59.931769	1870.066513	19.949031
60.040152	1864.821107	19.954048
60.032330	1876.929276	19.959066
60.428652	1891.867554	19.964083
60.874866	1891.498440	19.969101
60.590337	1898.393369	19.974119
61.120955	1890.714631	19.979136
60.772263	1902.550760	19.984154
60.522431	1896.244765	19.989171
60.937012	1882.289671	19.994189
60.700193	1898.098975	19.999207
61.059152	1887.217199	20.004224
60.924272	1896.213554	20.009242
61.325144	1912.872915	20.014259
61.196593	1923.353311	20.019277
61.513597	1920.675784	20.024295
61.952384	1914.340975	20.029312
61.801259	1906.118893	20.034330
61.545115	1890.918656	20.039347
61.578794	1889.360765	20.044365
61.454717	1883.219562	20.049383
61.521585	1894.124191	20.054400
61.967076	1912.080558	20.059418
62.199723	1912.954453	20.064435
61.858864	1900.614294	20.069453
61.701828	1903.808560	20.074471
62.213940	1904.490011	20.079488
62.205604	1913.685647	20.084506
62.080411	1916.616058	20.089523
62.532779	1911.853786	20.094541
61.907128	1900.391231	20.099559
61.797302	1908.336681	20.104576
61.912480	1911.253927	20.109594
62.289088	1913.006266	20.114611
62.102979	1915.957404	20.119629
61.946248	1914.997777	20.124647
62.162319	1913.918130	20.129664
62.204383	1916.880860	20.134682
62.182645	1930.389018	20.139699
62.617930	1924.442539	20.144717
62.733590	1934.010908	20.149735
63.074528	1924.604430	20.154752
63.272849	1917.202059	20.159770
63.099207	1918.486838	20.164787
63.373299	1924.237120	20.169805
63.095145	1931.308024	20.174823
63.334554	1920.708002	20.179840
63.264468	1917.654093	20.184858
63.022309	1919.402075	20.189875
63.681150	1915.548391	20.194893
63.402424	1914.872506	20.199911
63.521526	1921.688130	20.204928
63.549655	1921.159161	20.209946
63.449524	1919.334725	20.214963
63.633719	1917.339881	20.219981
63.048571	1926.937422	20.224999
63.626464	1916.543775	20.230016
63.553510	1928.908569	20.235034
63.439361	1948.323644	20.240051
63.659521	1949.664394	20.245069
63.898413	1952.153690	20.250087
63.791932	1958.719783	20.255104
64.157094	1959.368040	20.260122
63.956846	1954.208005	20.265139
63.846555	1951.782675	20.270157
64.009459	1973.437001	20.275175
64.637176	1973.684712	20.280192
64.694372	1970.947930	20.285210
64.554118	1983.160684	20.290227
64.770714	1976.369678	20.295245
64.534685	1979.899052	20.300263
64.731489	1977.258776	20.305280
64.897649	1970.604027	20.310298
65.174669	1967.002360	20.315315
65.277178	1966.970437	20.320333
65.031237	1965.831538	20.325351
65.286869	1966.336804	20.330368
65.398357	1957.622108	20.335386
65.138759	1955.027880	20.340403
65.520553	1947.706353	20.345421
65.349806	1940.908705	20.350439
65.229751	1937.280703	20.355456
65.495940	1931.634914	20.360474
65.007135	1931.816065	20.365491
65.332058	1950.373767	20.370509
65.253515	1968.744923	20.375527
65.628524	1961.861016	20.380544
65.840613	1954.520928	20.385562
65.630366	1960.815687	20.390579
65.470151	1957.746254	20.395597
65.853772	1961.192533	20.400615
65.693841	1961.384948	20.405632
65.803072	1959.781178	20.410650
65.556400	1964.669861	20.415667
66.026566	1971.099161	20.420685
65.872717	1984.221783	20.425703
65.889244	1990.198797	20.430720
66.158664	1984.580789	20.435738
65.795909	1994.326177	20.440755
66.043711	1994.394574	20.445773
65.988685	1996.819846	20.450791
66.356361	2010.892084	20.455808
66.641241	2012.611084	20.460826
66.459027	2025.647811	20.465843
66.768342	2008.799861	20.470861
66.686980	2020.366919	20.475879
66.558806	2017.964094	20.480896
66.733217	2016.036869	20.485914
66.514017	2023.591595	20.490931
66.572996	2032.918939	20.495949
66.655340	2049.908491	20.500967
66.968126	2047.488823	20.505984
67.095458	2056.603920	20.511002
67.023825	2058.351465	20.516019
67.484512	2065.617660	20.521037
67.309837	2075.840445	20.526055
67.599668	2077.444611	20.531072
67.672564	2068.146074	20.536090
67.500801	2077.648682	20.541107
67.909990	2079.277074	20.546125
67.980911	2071.740774	20.551143
67.833329	2064.291239	20.556160
68.357657	2073.568780	20.561178
67.911973	2072.379923	20.566195
67.907002	2067.865944	20.571213
67.862116	2074.612617	20.576231
67.795429	2077.477883	20.581248
68.138712	2059.616070	20.586266
67.928301	2075.997126	20.591283
68.091827	2079.491119	20.596301
68.505432	2099.039322	20.601319
68.670775	2101.011009	20.606336
68.786611	2095.557463	20.611354
68.530773	2100.789812	20.616371
68.838607	2089.884577	20.621389
68.806681	2100.372501	20.626407
68.642352	2096.148216	20.631424
68.862100	2098.125385	20.636442
68.940054	2095.929579	20.641459
68.660936	2101.983678	20.646477
68.791074	2095.776672	20.651495
68.952048	2100.676686	20.656512
69.078439	2098.917570	20.661530
68.876809	2113.066541	20.666547
69.259955	2119.708790	20.671565
69.382301	2125.307945	20.676583
69.383433	2126.311592	20.681600
69.616790	2119.975634	20.686618
69.479382	2118.024973	20.691635
69.661026	2129.753110	20.696653
69.589242	2113.270222	20.701671
69.857499	2121.729692	20.706688
70.141013	2120.608599	20.711706
69.899126	2119.465108	20.716723
70.434717	2120.302503	20.721741
70.095885	2124.544425	20.726759
69.996358	2126.718818	20.731776
70.045849	2117.202955	20.736794
70.393142	2115.420406	20.741811
70.205461	2119.505290	20.746829
70.321001	2114.500919	20.751847
70.457221	2133.533365	20.756864
70.506841	2129.973430	20.761882
70.389343	2139.690025	20.766899
70.456465	2148.985469	20.771917
70.434451	2139.532909	20.776935
70.233734	2149.834624	20.781952
70.677606	2140.760046	20.786970
70.716544	2153.385634	20.791987
70.814028	2159.743095	20.797005
71.295744	2169.619001	20.802023
71.018914	2173.428656	20.807040
71.191143	2163.742952	20.812058
70.947703	2180.943500	20.817075
71.231284	2177.264438	20.822093
71.328633	2167.832153	20.827111
71.273509	2177.783452	20.832128
71.574436	2187.196589	20.837146
71.541192	2188.606878	20.842163
72.160538	2195.440388	20.847181
72.136324	2202.854775	20.852199
71.968163	2190.895061	20.857216
72.170820	2184.324851	20.862234
71.991145	2184.890109	20.867251
72.162581	2186.248878	20.872269
72.422427	2185.312468	20.877287
71.696202	2200.659768	20.882304
72.255723	2198.472885	20.887322
72.247716	2193.635280	20.892339
72.474604	2199.570966	20.897357
72.309029	2188.614517	20.902375
72.387047	2201.089970	20.907392
72.514827	2195.998668	20.912410
72.415658	2201.319335	20.917427
72.405091	2196.670130	20.922445
72.825553	2197.237216	20.927463
72.741768	2222.314334	20.932480
73.041998	2220.482644	20.937498
72.990739	2217.195988	20.942515
73.116033	2224.485861	20.947533
72.975817	2219.402681	20.952551
72.925455	2219.678307	20.957568
73.285023	2212.843153	20.962586
73.147201	2226.279642	20.967603
72.853645	2220.973142	20.972621
73.328230	2225.669801	20.977639
73.352536	2239.548462	20.982656
73.427753	2247.654939	20.987674
73.495432	2242.574779	20.992691
73.493040	2250.148533	20.997709
73.686009	2239.802674	21.002727
73.628249	2254.978139	21.007744
73.964619	2262.378314	21.012762
73.956516	2279.834843	21.017779
74.312703	2278.126369	21.022797
74.760232	2263.531673	21.027815
74.435482	2263.647333	21.032832
74.828855	2260.970939	21.037850
74.710417	2261.030100	21.042867
74.937348	2245.989212	21.047885
74.813932	2236.364767	21.052903
74.562853	2236.830506	21.057920
74.675522	2233.720641	21.062938
74.834988	2233.534904	21.067955
74.751149	2247.617239	21.072973
74.980382	2242.623796	21.077991
74.794071	2259.388998	21.083008
74.650427	2261.955872	21.088026
75.171315	2265.411798	21.093043
74.961573	2261.076720	21.098061
74.963308	2262.396486	21.103079
75.050613	2273.109360	21.108096
75.575569	2285.169086	21.113114
75.601323	2295.623567	21.118131
75.437315	2305.667043	21.123149
75.373210	2296.001637	21.128167
75.545733	2295.721000	21.133184
75.715537	2288.485812	21.138202
75.714441	2299.017730	21.143219
75.822845	2304.832343	21.148237
76.022278	2311.769058	21.153255
75.947931	2313.930025	21.158272
75.826710	2320.666173	21.163290
76.041015	2313.682664	21.168307
75.989177	2321.114888	21.173325
76.479912	2316.123766	21.178343
76.262768	2318.079396	21.183360
76.318067	2315.762103	21.188378
76.353148	2324.391024	21.193395
76.396960	2334.556335	21.198413
76.672535	2349.176110	21.203431
76.694867	2353.741995	21.208448
77.069384	2340.268743	21.213466
76.938124	2336.374200	21.218483
77.033728	2338.205231	21.223501
77.173128	2333.972555	21.228519
76.936201	2344.981817	21.233536
77.033930	2334.980661	21.238554
77.525165	2344.002507	21.243571
77.256283	2352.977250	21.248589
77.353834	2359.241971	21.253607
77.335825	2373.251002	21.258624
77.594042	2369.875627	21.263642
77.796445	2364.933617	21.268659
77.644696	2368.702137	21.273677
77.864249	2368.537494	21.278695
77.762531	2364.178078	21.283712
78.018855	2366.133719	21.288730
78.213832	2360.139653	21.293747
78.022678	2357.165526	21.298765
78.293335	2363.245325	21.303783
78.361551	2377.042388	21.308800
78.568683	2389.546967	21.313818
79.163575	2381.800306	21.318835
78.931104	2367.594763	21.323853
78.981147	2352.324761	21.328871
79.074426	2349.066153	21.333888
78.995677	2345.590350	21.338906
79.122398	2344.575265	21.343923
79.000832	2348.137600	21.348941
78.890524	2342.027829	21.353959
79.308231	2345.568663	21.358976
79.065712	2341.665118	21.363994
79.091267	2345.040380	21.369011
79.038606	2354.947358	21.374029
79.382851	2363.971421	21.379047
79.518378	2372.994165	21.384064
79.236330	2392.066908	21.389082
79.839261	2373.374357	21.394099
79.509007	2380.581212	21.399117
79.589954	2375.090650	21.404135
79.274150	2382.552416	21.409152
79.289423	2391.662783	21.414170
79.825298	2399.509459	21.419187
79.838719	2416.346819	21.424205
79.637623	2411.206420	21.429223
79.780919	2418.301591	21.434240
79.913946	2429.882765	21.439258
80.420247	2438.243104	21.444275
80.105587	2445.199727	21.449293
80.464209	2438.596666	21.454311
80.230085	2442.889627	21.459328
80.429623	2452.138190	21.464346
80.637394	2461.217901	21.469363
80.517958	2471.397543	21.474381
80.599875	2464.437434	21.479399
80.529254	2465.871015	21.484416
80.886357	2461.572121	21.489434
81.002453	2465.582699	21.494451
81.377573	2486.899534	21.499469
81.508521	2478.253006	21.504487
81.526936	2492.446697	21.509504
81.435944	2490.290361	21.514522
81.952599	2486.662939	21.519539
81.376730	2490.694202	21.524557
81.616508	2485.735965	21.529575
81.847765	2489.996413	21.534592
81.837113	2481.783067	21.539610
81.865739	2480.505948	21.544627
81.613826	2488.368181	21.549645
81.889195	2481.166406	21.554663
81.868421	2484.597858	21.559680
82.139451	2509.813175	21.564698
82.396539	2505.701696	21.569715
82.381011	2518.411012	21.574733
82.435238	2511.568567	21.579751
82.693950	2509.919662	21.584768
82.815358	2515.729927	21.589786
82.889099	2512.545192	21.594803
82.990469	2519.183006	21.599821
83.130906	2513.388718	21.604839
83.162327	2502.955167	21.609856
83.061590	2508.178657	21.614874
83.525106	2492.784362	21.619891
83.508253	2493.965527	21.624909
83.623394	2490.812738	21.629927
83.832372	2489.458087	21.634944
83.892735	2501.621975	21.639962
83.808718	2496.278025	21.644979
83.779767	2503.484872	21.649997
83.432879	2491.579370	21.655015
83.899326	2490.204111	21.660032
83.626894	2498.386620	21.665050
83.598458	2497.429305	21.670067
83.637751	2504.600885	21.675085
83.932510	2517.248920	21.680103
84.054908	2527.712540	21.685120
84.181622	2531.638063	21.690138
84.291836	2527.336832	21.695155
84.278742	2527.744961	21.700173
84.464615	2525.712799	21.705191
84.644730	2534.866974	21.710208
84.344715	2554.075728	21.715226
84.716580	2554.495621	21.720243
84.875969	2567.981777	21.725261
84.780067	2562.185043	21.730279
85.154587	2559.816805	21.735296
85.038902	2561.845171	21.740314
85.271019	2552.505990	21.745331
85.379148	2547.674918	21.750349
85.496875	2546.760365	21.755367
85.553585	2547.232876	21.760384
85.462363	2554.034355	21.765402
85.595318	2546.044276	21.770419
85.434769	2553.287866	21.775437
85.338049	2559.807049	21.780455
85.731175	2574.779580	21.785472
85.621378	2580.191751	21.790490
85.835565	2575.871566	21.795507
86.059837	2579.652542	21.800525
86.174793	2579.244212	21.805543
86.275270	2571.241208	21.810560
86.037888	2584.145641	21.815578
86.238172	2582.432892	21.820595
86.384481	2594.819919	21.825613
86.447620	2596.627842	21.830631
86.674000	2607.060778	21.835648
86.734451	2611.710338	21.840666
87.031300	2599.052356	21.845683
87.083959	2600.742388	21.850701
86.835870	2596.641437	21.855719
87.399269	2593.597274	21.860736
87.133348	2594.363510	21.865754
87.412242	2584.299469	21.870771
87.567830	2591.243310	21.875789
87.122367	2597.007138	21.880807
86.986551	2602.460437	21.885824
87.265458	2612.066934	21.890842
87.501435	2625.189319	21.895859
87.651183	2623.752856	21.900877
87.853127	2624.450776	21.905895
88.232826	2622.862012	21.910912
87.940907	2629.791497	21.915930
88.023535	2622.990880	21.920947
88.210748	2636.165101	21.925965
88.464470	2649.475823	21.930983
88.557306	2650.591525	21.936000
88.453254	2650.986631	21.941018
88.609147	2640.241302	21.946035
88.670625	2650.720232	21.951053
88.980627	2645.213493	21.956071
89.024853	2639.991414	21.961088
89.069568	2648.796763	21.966106
88.967421	2643.844232	21.971123
89.297323	2643.872799	21.976141
89.182598	2649.363655	21.981159
89.377022	2640.539362	21.986176
89.363522	2648.944960	21.991194
89.172298	2647.282840	21.996211
89.321242	2647.068099	22.001229
89.186962	2648.960214	22.006247
89.718740	2671.690252	22.011264
89.513267	2678.080521	22.016282
89.668880	2680.066426	22.021299
89.813534	2678.969011	22.026317
89.459002	2678.620603	22.031335
89.940620	2676.442146	22.036352
90.029244	2690.093875	22.041370
90.361004	2689.772893	22.046387
90.416691	2695.490664	22.051405
90.339892	2702.585676	22.056423
90.774414	2694.240649	22.061440
90.748176	2694.873489	22.066458
90.489755	2690.419400	22.071475
90.566322	2691.573883	22.076493
90.247094	2688.188264	22.081511
90.657978	2684.892306	22.086528
90.388944	2706.364103	22.091546
91.047432	2714.325123	22.096563
90.961751	2717.648202	22.101581
91.087890	2721.223042	22.106599
91.410956	2720.542393	22.111616
91.215852	2728.446824	22.116634
91.603316	2738.489180	22.121651
91.927546	2742.199983	22.126669
92.087663	2754.595956	22.131687
91.937952	2750.329818	22.136704
91.706673	2749.050858	22.141722
92.116861	2745.586663	22.146739
91.951240	2758.042451	22.151757
91.803897	2752.650295	22.156775
92.084769	2749.448997	22.161792
91.710832	2757.573108	22.166810
92.151178	2772.406950	22.171827
92.284775	2775.758789	22.176845
92.156047	2782.772447	22.181863
92.448111	2784.766498	22.186880
92.377521	2807.064203	22.191898
92.749075	2803.068899	22.196915
92.911739	2805.452510	22.201933
93.166910	2804.277680	22.206951
93.191826	2798.780162	22.211968
93.191771	2815.118272	22.216986
93.241395	2823.871814	22.222003
93.593464	2828.479658	22.227021
94.003257	2836.698298	22.232039
94.081359	2836.760728	22.237056
93.612730	2834.519824	22.242074
94.040633	2826.373219	22.247091
94.096209	2832.261757	22.252109
93.766511	2827.497267	22.257127
94.263142	2827.208201	22.262144
94.168688	2821.668355	22.267162
93.998657	2826.035373	22.272179
94.256632	2825.536581	22.277197
94.334014	2827.921996	22.282215
94.851314	2839.391874	22.287232
94.782861	2854.758454	22.292250
94.814012	2860.735066	22.297267
94.894021	2854.217941	22.302285
94.994242	2860.148928	22.307303
94.974500	2850.937035	22.312320
94.863179	2852.493563	22.317338
95.020798	2856.372555	22.322355
95.252397	2850.306374	22.327373
95.040793	2848.744234	22.332391
95.182887	2847.841509	22.337408
95.216515	2863.601645	22.342426
95.457113	2875.899146	22.347443
95.892861	2874.335244	22.352461
95.876619	2874.588921	22.357479
96.325474	2864.244295	22.362496
95.894914	2870.766509	22.367514
95.877910	2879.556668	22.372531
95.801705	2878.363094	22.377549
95.954337	2889.800703	22.382567
96.161589	2902.165687	22.387584
96.218520	2906.002539	22.392602
96.803979	2905.282400	22.397619
96.944734	2907.641990	22.402637
96.770169	2912.720859	22.407655
96.809547	2901.310348	22.412672
96.615503	2896.520270	22.417690
96.923101	2927.910934	22.422707
97.079138	2929.269084	22.427725
97.215519	2943.179311	22.432743
97.203241	2925.119070	22.437760
97.353679	2933.729169	22.442778
97.167426	2938.056330	22.447795
97.787733	2943.614151	22.452813
97.576213	2957.916544	22.457831
97.683689	2961.473967	22.462848
98.167622	2969.370144	22.467866
97.966210	2970.818338	22.472883
98.251813	2960.468213	22.477901
98.307701	2963.424232	22.482919
98.342117	2954.610320	22.487936
98.392778	2963.026320	22.492954
98.239282	2965.715240	22.497971
98.305736	2957.586085	22.502989
98.170135	2979.927458	22.508007
98.615780	2984.303324	22.513024
99.028023	2992.524021	22.518042
98.706782	2997.080394	22.523059
98.885979	2983.040655	22.528077
99.260984	2994.764614	22.533095
99.394084	3005.034935	22.538112
99.632092	3005.267735	22.543130
99.497078	3010.718697	22.548147
100.077880	3009.693300	22.553165
99.635931	3014.991833	22.558183
99.731505	3009.508141	22.563200
99.847253	3007.918166	22.568218
99.926424	3007.597341	22.573235
100.027663	3005.838983	22.578253
99.655786	3005.885069	22.583271
100.037085	3000.692492	22.588288
100.050449	3012.698322	22.593306
100.069147	3021.546590	22.598323
100.777231	3023.354767	22.603341
100.549303	3035.436066	22.608359
100.815744	3034.436412	22.613376
100.954943	3031.775245	22.618394
100.910249	3039.445829	22.623411
100.946642	3033.791428	22.628429
100.972003	3038.696867	22.633447
100.758340	3027.933097	22.638464
100.746273	3045.243287	22.643482
100.470623	3057.019137	22.648499
100.875789	3057.511614	22.653517
101.069209	3079.769994	22.658535
101.372477	3090.662206	22.663552
101.598346	3093.293799	22.668570
101.293021	3102.030167	22.673587
101.968509	3104.008746	22.678605
101.859703	3114.052624	22.683623
101.918293	3111.686697	22.688640
102.334125	3114.487019	22.693658
102.334453	3120.400216	22.698675
102.477155	3106.280437	22.703693
102.051103	3119.479733	22.708711
102.470426	3142.835718	22.713728
103.080524	3140.516353	22.718746
103.423919	3137.386026	22.723763
103.459623	3137.697501	22.728781
103.470111	3135.601975	22.733799
103.438437	3132.159382	22.738816
103.695518	3131.811758	22.743834
103.448302	3132.495587	22.748851
103.863395	3129.038389	22.753869
103.644257	3138.868609	22.758887
103.822937	3131.776333	22.763904
103.932887	3124.208096	22.768922
103.768162	3126.670713	22.773939
103.654818	3126.357773	22.778957
103.855098	3139.460355	22.783975
104.298078	3150.364945	22.788992
104.429995	3143.973141	22.794010
104.384660	3152.614589	22.799027
104.484172	3154.707049	22.804045
104.404818	3159.508085	22.809063
104.254195	3154.141475	22.814080
104.623217	3166.338507	22.819098
104.457733	3183.487679	22.824115
104.590054	3191.253616	22.829133
104.750758	3189.246617	22.834151
104.858165	3196.608267	22.839168
105.116972	3212.111040	22.844186
105.042897	3215.066595	22.849203
105.534173	3200.800677	22.854221
105.488873	3222.926643	22.859239
105.286927	3219.012455	22.864256
105.919792	3224.062578	22.869274
105.590009	3243.997537	22.874291
105.802165	3251.417241	22.879309
106.071644	3250.752983	22.884327
106.297792	3245.589782	22.889344
105.940465	3246.948015	22.894362
106.098354	3251.670345	22.899379
106.653450	3263.789801	22.904397
106.748543	3270.119023	22.909415
106.486827	3265.688094	22.914432
106.799452	3273.498480	22.919450
106.805970	3278.649288	22.924467
106.924249	3275.695638	22.929485
107.058706	3276.537295	22.934503
107.312457	3288.629308	22.939520
107.425550	3293.534215	22.944538
107.524020	3303.363456	22.949555
107.758835	3299.842144	22.954573
107.997998	3292.193432	22.959591
107.629230	3297.341159	22.964608
107.911261	3292.434915	22.969626
108.017703	3295.108402	22.974643
108.209949	3290.855226	22.979661
108.306305	3296.503817	22.984679
108.442855	3292.946257	22.989696
108.393046	3292.362804	22.994714
108.132587	3311.867522	22.999731
108.601066	3310.004941	23.004749
108.784117	3319.684618	23.009767
108.576108	3320.026307	23.014784
108.904953	3319.269982	23.019802
108.767791	3323.038778	23.024819
109.037094	3334.957649	23.029837
109.364554	3335.069996	23.034855
109.195112	3342.207622	23.039872
109.334355	3328.416997	23.044890
109.406209	3336.729142	23.049907
109.523771	3350.864592	23.054925
109.769170	3360.851370	23.059943
109.522455	3364.451212	23.064960
109.946629	3357.108861	23.069978
109.785024	3365.909783	23.074995
110.219820	3375.705895	23.080013
110.538908	3384.815632	23.085031
110.428920	3395.408968	23.090048
110.526583	3383.079428	23.095066
110.426617	3392.028652	23.100083
110.602067	3392.304476	23.105101
111.178637	3381.762129	23.110119
110.873841	3384.742709	23.115136
111.372520	3391.293180	23.120154
111.454431	3415.139207	23.125171
111.293653	3411.607792	23.130189
111.535990	3413.930027	23.135207
111.204241	3415.898566	23.140224
111.623197	3407.853761	23.145242
111.374567	3418.042073	23.150259
111.269893	3418.122640	23.155277
111.602067	3423.408791	23.160295
111.834194	3452.278831	23.165312
111.981025	3446.687685	23.170330
111.754601	3454.000434	23.175347
112.298315	3457.553707	23.180365
112.315414	3476.213575	23.185383
112.307003	3483.060490	23.190400
112.581014	3474.318192	23.195418
112.516143	3484.245973	23.200435
112.645334	3490.613907	23.205453
113.342366	3492.037667	23.210471
113.031156	3504.728124	23.215488
113.346195	3507.674394	23.220506
113.451783	3517.803145	23.225523
113.531296	3510.822472	23.230541
113.821723	3512.904993	23.235559
113.546725	3513.806450	23.240576
113.752937	3513.020113	23.245594
113.914071	3516.532143	23.250611
113.973280	3528.006389	23.255629
114.559673	3527.220786	23.260647
114.260217	3536.867416	23.265664
114.322689	3532.320204	23.270682
114.618473	3536.136441	23.275699
114.574853	3524.942423	23.280717
114.905844	3532.033381	23.285735
114.541148	3535.906953	23.290752
115.001370	3539.204525	23.295770
115.135455	3546.776067	23.300787
115.148198	3552.342905	23.305805
115.481592	3549.641239	23.310823
115.338863	3556.911586	23.315840
115.367842	3555.109620	23.320858
115.497307	3556.141674	23.325875
115.306164	3581.378262	23.330893
115.606286	3583.548926	23.335911
115.807676	3593.765505	23.340928
115.773351	3583.257496	23.345946
115.944512	3606.044138	23.350963
116.004985	3608.219194	23.355981
116.387415	3609.999143	23.360999
116.427755	3615.600937	23.366016
116.711166	3609.861299	23.371034
116.839326	3623.951270	23.376051
116.962070	3637.631482	23.381069
117.105132	3645.145004	23.386087
117.217305	3642.839674	23.391104
117.257512	3642.488863	23.396122
117.268587	3643.198392	23.401139
117.231725	3645.149044	23.406157
117.652096	3641.144161	23.411175
117.339593	3641.008498	23.416192
117.822587	3651.666367	23.421210
117.684318	3660.790994	23.426227
117.955795	3664.522249	23.431245
117.932325	3669.567057	23.436263
117.693287	3667.666217	23.441280
118.269983	3670.520452	23.446298
118.106611	3684.445356	23.451315
118.327553	3694.585729	23.456333
119.025471	3689.789249	23.461351
118.354889	3704.146688	23.466368
118.620358	3704.673269	23.471386
118.952289	3722.665719	23.476403
119.009087	3735.334665	23.481421
119.090252	3725.855186	23.486439
119.269025	3734.653972	23.491456
119.723242	3726.151042	23.496474
119.596719	3724.860008	23.501491
119.462163	3746.819277	23.506509
119.365565	3746.961489	23.511527
119.912031	3761.164249	23.516544
119.925437	3753.419138	23.521562
120.116816	3764.043350	23.526579
120.360164	3771.013094	23.531597
120.854892	3771.295441	23.536615
120.628940	3792.640807	23.541632
120.665146	3784.814164	23.546650
120.908484	3775.798100	23.551667
120.896276	3782.243774	23.556685
120.954985	3780.940505	23.561703
120.936372	3783.551424	23.566720
121.109101	3797.817748	23.571738
121.346390	3805.353300	23.576755
121.460117	3814.239599	23.581773
121.663758	3811.212444	23.586791
121.522943	3819.265348	23.591808
121.604815	3833.334581	23.596826
121.985388	3836.722018	23.601843
121.884697	3846.755662	23.606861
122.396225	3835.132258	23.611879
122.229578	3839.242580	23.616896
122.405857	3854.287194	23.621914
122.558890	3866.395746	23.626931
122.646455	3874.302917	23.631949
123.186978	3865.528118	23.636967
122.740205	3874.326041	23.641984
122.911615	3872.131590	23.647002
123.391981	3888.035567	23.652019
123.420764	3897.611212	23.657037
123.301227	3893.115724	23.662055
123.536632	3897.358621	23.667072
123.498357	3900.215777	23.672090
123.846001	3898.112008	23.677107
123.900475	3897.073726	23.682125
124.186943	3887.957102	23.687143
123.961710	3911.897752	23.692160
124.046371	3918.051918	23.697178
124.105071	3910.610237	23.702195
124.467205	3921.020108	23.707213
124.391029	3914.832647	23.712231
124.756926	3926.927761	23.717248
124.794517	3940.392126	23.722266
125.258943	3941.067140	23.727283
125.092729	3955.593772	23.732301
125.571408	3954.369843	23.737319
125.104234	3958.369998	23.742336
125.205742	3946.385510	23.747354
125.564538	3942.162231	23.752371
125.442505	3968.526779	23.757389
125.766483	3969.052694	23.762407
125.763098	3971.976675	23.767424
125.949967	3972.214504	23.772442
126.093599	3980.109645	23.777459
126.176134	3993.179847	23.782477
126.550795	3992.003969	23.787495
126.400821	4002.847201	23.792512
126.463151	4004.678242	23.797530
126.686470	4005.084115	23.802547
126.699324	4019.100810	23.807565
127.072625	4024.911631	23.812583
126.998944	4024.789015	23.817600
126.994532	4029.269220	23.822618
127.304353	4046.327087	23.827635
127.108664	4061.193648	23.832653
127.215203	4063.745327	23.837671
127.855738	4080.722966	23.842688
127.728795	4100.983104	23.847706
127.846918	4093.368226	23.852723
127.776943	4096.248569	23.857741
128.331635	4110.349662	23.862759
128.153333	4122.258733	23.867776
128.545772	4132.315422	23.872794
128.697457	4123.090343	23.877811
128.566872	4123.016920	23.882829
129.387855	4117.716086	23.887847
129.975783	4131.942491	23.892864
129.858725	4129.835694	23.897882
129.691353	4106.716754	23.902899
129.775231	4104.215260	23.907917
129.984900	4099.460319	23.912935
129.912968	4111.457049	23.917952
129.976041	4123.244244	23.922970
130.192706	4128.816545	23.927987
130.295111	4132.710977	23.933005
130.820516	4124.730627	23.938023
130.499422	4124.023621	23.943040
130.506646	4131.799778	23.948058
130.866219	4122.727994	23.953075
130.652446	4126.827030	23.958093
130.636956	4129.625529	23.963111
130.693525	4138.957749	23.968128
130.975704	4152.364427	23.973146
130.795718	4158.203738	23.978163
130.770493	4162.212931	23.983181
130.800654	4164.779166	23.988199
131.042011	4190.798241	23.993216
130.829587	4202.701017	23.998234
131.468382	4217.416581	24.003251
131.748830	4234.679957	24.008269
131.788676	4228.727178	24.013287
132.040135	4240.674807	24.018304
132.302023	4251.592580	24.023322
132.365953	4244.848478	24.028339
132.449135	4260.638401	24.033357
132.718492	4271.319777	24.038375
133.015142	4280.041880	24.043392
133.052511	4291.383321	24.048410
133.401901	4278.054703	24.053427
133.130628	4279.404809	24.058445
133.088383	4284.581053	24.063463
133.827352	4300.180703	24.068480
133.898517	4308.327517	24.073498
134.042855	4302.856810	24.078515
133.930705	4304.389233	24.083533
134.273204	4303.966605	24.088551
134.252785	4299.461481	24.093568
134.220736	4316.271298	24.098586
134.198960	4323.670634	24.103603
134.325249	4328.312603	24.108621
134.597972	4332.669254	24.113639
134.782337	4337.951774	24.118656
134.707826	4356.314263	24.123674
135.074193	4356.662723	24.128691
135.040726	4365.771861	24.133709
135.249418	4384.669022	24.138727
135.698768	4393.469902	24.143744
135.635008	4399.236493	24.148762
135.832198	4396.167767	24.153779
135.993399	4389.770756	24.158797
136.029501	4395.648867	24.163815
136.092560	4413.616596	24.168832
136.105279	4420.454285	24.173850
136.793955	4410.105747	24.178867
136.292895	4424.764115	24.183885
136.796719	4431.052268	24.188903
136.937895	4442.687234	24.193920
136.781742	4448.103547	24.198938
136.978082	4445.093949	24.203955
137.246408	4448.735439	24.208973
137.457140	4458.391788	24.213991
137.912783	4465.055815	24.219008
137.626066	4478.712417	24.224026
137.995357	4472.179132	24.229043
138.070339	4473.315918	24.234061
137.662698	4480.606931	24.239079
138.140981	4476.359731	24.244096
138.482740	4498.002652	24.249114
138.588036	4496.295394	24.254131
138.589597	4500.342889	24.259149
138.710275	4506.106074	24.264167
138.888750	4496.932346	24.269184
138.739175	4510.844030	24.274202
138.716785	4521.635044	24.279219
139.057756	4527.238812	24.284237
138.976118	4533.008306	24.289255
139.456565	4545.186365	24.294272
139.730621	4557.387902	24.299290
140.142444	4560.285917	24.304307
140.192670	4553.382584	24.309325
139.982309	4554.750536	24.314343
140.281595	4550.886661	24.319360
140.123355	4576.694000	24.324378
140.528842	4583.039596	24.329395
140.900427	4582.891605	24.334413
140.901878	4576.025147	24.339431
141.519328	4570.220078	24.344448
141.613997	4580.926387	24.349466
142.094426	4575.909417	24.354483
142.055887	4570.542508	24.359501
141.706783	4564.219709	24.364519
141.699774	4564.016440	24.369536
141.604270	4572.326076	24.374554
142.259480	4590.566209	24.379571
142.161966	4593.302351	24.384589
142.072556	4602.226238	24.389607
142.536679	4598.527237	24.394624
142.404668	4600.594672	24.399642
142.556678	4614.290796	24.404659
142.696567	4614.343385	24.409677
142.823280	4623.279240	24.414695
143.266483	4627.891227	24.419712
142.932430	4633.229767	24.424730
142.955496	4637.933135	24.429747
143.547221	4656.347109	24.434765
143.490496	4661.297647	24.439783
143.642985	4652.109872	24.444800
143.824990	4669.605802	24.449818
144.044102	4686.278441	24.454835
144.093207	4684.768933	24.459853
143.963824	4691.469702	24.464871
144.455150	4698.271329	24.469888
144.445533	4715.561067	24.474906
144.641812	4716.355978	24.479923
144.836577	4715.750777	24.484941
144.854987	4732.435016	24.489959
145.365355	4741.168161	24.494976
145.197128	4739.009644	24.499994
145.420233	4738.556480	24.505011
145.703143	4742.285405	24.510029
145.745079	4743.021535	24.515047
146.245929	4742.789996	24.520064
146.038780	4765.132112	24.525082
146.365030	4763.522549	24.530099
146.452510	4770.351626	24.535117
146.421255	4774.874100	24.540135
146.684364	4763.057502	24.545152
146.549493	4770.683575	24.550170
146.956420	4774.875778	24.555187
146.954084	4788.521937	24.560205
147.378067	4803.807314	24.565223
147.333592	4798.814174	24.570240
147.278210	4799.265297	24.575258
147.587803	4793.351099	24.580275
147.740324	4808.744276	24.585293
147.396497	4825.181917	24.590311
148.037748	4821.526211	24.595328
148.143143	4831.992617	24.600346
148.150864	4845.173059	24.605363
148.499512	4846.569913	24.610381
148.304416	4851.874574	24.615399
148.597074	4840.844645	24.620416
148.661258	4863.275028	24.625434
149.048938	4879.403346	24.630451
149.447517	4874.096439	24.635469
149.204070	4878.789668	24.640487
149.616953	4878.895498	24.645504
149.717734	4898.815959	24.650522
149.684008	4900.926768	24.655539
150.220329	4898.681852	24.660557
149.945710	4906.281500	24.665575
150.322299	4909.672187	24.670592
150.570142	4924.690754	24.675610
150.454257	4931.859941	24.680627
151.101014	4928.501502	24.685645
151.026121	4946.201575	24.690663
151.214973	4933.639850	24.695680
151.025057	4940.939641	24.700698
151.350501	4947.958223	24.705715
151.464521	4953.978332	24.710733
151.387175	4970.468052	24.715751
151.571385	4953.860119	24.720768
151.621810	4977.441492	24.725786
151.786774	4992.456821	24.730803
152.446751	4988.776849	24.735821
152.302153	5000.051082	24.740839
152.370264	4999.297705	24.745856
152.320538	5019.493294	24.750874
152.314588	5023.840302	24.755891
153.064756	5031.256162	24.760909
153.003238	5048.386991	24.765927
153.456017	5052.084978	24.770944
153.155561	5065.579096	24.775962
153.148400	5060.680619	24.780979
153.713709	5050.240382	24.785997
153.774242	5073.282171	24.791015
154.211783	5070.523509	24.796032
154.345607	5073.628021	24.801050
153.970386	5073.584156	24.806067
154.285146	5083.257373	24.811085
154.513230	5108.525710	24.816103
154.608963	5110.246928	24.821120
154.621681	5117.089661	24.826138
154.727757	5111.756928	24.831155
154.883106	5125.340493	24.836173
155.220826	5140.860262	24.841191
155.386908	5134.489689	24.846208
155.494939	5148.356964	24.851226
155.994900	5155.684544	24.856243
156.345759	5156.225893	24.861261
156.284911	5161.259076	24.866279
156.637110	5154.846231	24.871296
156.528502	5164.524853	24.876314
156.372627	5165.792910	24.881331
156.962477	5163.745547	24.886349
156.840015	5180.872085	24.891367
156.929134	5185.229158	24.896384
157.265104	5176.320206	24.901402
157.253412	5184.442166	24.906419
157.261232	5202.399995	24.911437
157.310951	5212.279986	24.916455
157.685502	5211.404572	24.921472
158.149488	5226.463725	24.926490
158.273209	5246.114293	24.931507
158.605019	5236.126557	24.936525
158.603212	5237.889305	24.941543
158.834527	5232.417763	24.946560
158.790037	5229.902717	24.951578
158.868453	5236.934076	24.956595
159.036865	5247.970559	24.961613
159.081655	5266.551180	24.966631
159.373677	5265.138988	24.971648
159.509735	5272.253222	24.976666
159.516507	5289.338038	24.981683
160.072572	5283.095614	24.986701
160.037365	5293.602074	24.991719
159.984536	5293.870280	24.996736
160.091140	5306.212431	25.001754
160.013377	5322.098388	25.006771
160.581837	5319.241706	25.011789
160.317333	5333.645321	25.016807
160.528993	5348.108351	25.021824
160.852937	5348.815283	25.026842
160.917251	5371.059171	25.031859
161.231199	5379.526627	25.036877
161.183443	5391.808492	25.041895
161.392576	5406.408090	25.046912
161.313792	5418.914428	25.051930
161.539613	5420.543348	25.056947
161.870055	5440.959768	25.061965
162.111926	5445.359437	25.066983
162.582064	5446.197269	25.072000
162.641914	5455.505410	25.077018
162.823840	5468.237719	25.082035
163.191482	5470.466356	25.087053
163.391642	5472.809026	25.092071
163.679503	5477.715123	25.097088
163.717924	5473.935876	25.102106
163.855061	5475.728425	25.107123
163.928866	5482.364111	25.112141
164.213330	5501.038201	25.117159
164.021014	5493.477608	25.122176
164.129709	5496.501247	25.127194
164.125994	5503.618209	25.132211
164.647686	5516.238954	25.137229
164.629510	5525.566661	25.142247
164.538824	5538.864117	25.147264
164.974786	5538.550868	25.152282
164.850356	5564.805353	25.157299
165.053134	5569.343469	25.162317
165.073060	5587.430438	25.167335
165.264613	5589.274119	25.172352
165.837628	5607.870081	25.177370
165.702269	5624.826100	25.182387
165.944690	5630.866139	25.187405
166.317846	5635.833433	25.192423
166.389267	5652.239611	25.197440
166.891498	5658.654437	25.202458
166.993367	5667.097651	25.207475
167.130483	5656.615116	25.212493
166.977498	5681.804361	25.217511
167.063115	5687.784453	25.222528
167.535591	5698.651632	25.227546
167.322983	5711.978123	25.232563
167.687521	5718.927114	25.237581
167.976633	5725.646596	25.242599
168.196507	5739.996979	25.247616
168.635807	5756.808814	25.252634
168.456643	5766.252031	25.257651
168.795240	5758.332071	25.262669
168.884446	5765.032304	25.267687
169.149157	5777.942866	25.272704
169.730092	5769.788357	25.277722
169.341029	5780.801613	25.282739
169.856513	5772.077686	25.287757
170.321101	5778.902967	25.292775
170.335569	5769.552402	25.297792
170.098259	5763.657357	25.302810
170.695042	5779.520440	25.307827
170.963521	5791.652297	25.312845
170.717755	5793.642046	25.317863
170.803924	5788.939303	25.322880
171.199609	5781.956715	25.327898
171.000864	5791.510071	25.332915
171.555920	5790.563363	25.337933
171.588305	5793.468627	25.342951
171.357934	5812.766495	25.347968
171.952244	5816.376812	25.352986
171.528370	5821.017277	25.358003
171.671867	5819.343117	25.363021
171.873509	5844.089004	25.368039
171.847212	5849.710927	25.373056
172.588625	5855.784010	25.378074
172.309112	5885.505145	25.383091
172.347279	5893.195471	25.388109
172.605650	5902.177201	25.393127
172.670490	5915.016682	25.398144
173.115981	5915.081924	25.403162
173.109839	5949.271777	25.408179
173.293654	5943.156882	25.413197
173.599757	5959.861153	25.418215
173.798347	5978.153000	25.423232
174.220576	5977.760111	25.428250
174.121351	5999.061701	25.433267
174.474071	5995.624815	25.438285
174.621224	6004.424496	25.443303
174.942401	6024.152406	25.448320
175.117691	6029.725734	25.453338
175.224726	6034.047944	25.458355
175.572708	6030.404881	25.463373
175.752874	6051.988518	25.468391
175.491638	6062.628335	25.473408
176.129890	6069.878466	25.478426
176.239386	6068.009069	25.483443
176.411562	6095.544513	25.488461
176.820989	6094.858617	25.493479
176.688217	6101.721066	25.498496
176.939459	6098.120162	25.503514
177.129183	6105.226242	25.508531
177.322589	6116.603216	25.513549
177.449152	6127.050643	25.518567
177.358564	6132.799368	25.523584
177.918796	6146.217037	25.528602
177.869008	6162.801251	25.533619
177.944476	6159.540712	25.538637
178.295139	6167.855639	25.543655
178.410296	6191.892048	25.548672
178.866645	6186.619531	25.553690
178.585984	6195.894306	25.558707
179.063455	6195.562630	25.563725
179.238384	6212.775126	25.568743
179.142941	6222.182467	25.573760
179.566104	6229.021644	25.578778
179.664058	6233.560942	25.583795
179.924624	6242.935140	25.588813
180.096043	6244.531127	25.593831
180.188873	6250.679459	25.598848
180.358403	6255.138900	25.603866
180.492329	6280.296005	25.608883
180.959151	6278.868443	25.613901
180.956556	6278.130210	25.618919
181.059521	6283.700216	25.623936
181.337488	6290.110949	25.628954
181.375606	6305.268217	25.633971
181.643316	6306.286298	25.638989
181.757687	6304.425536	25.644007
181.621320	6320.422614	25.649024
182.020332	6328.152412	25.654042
182.097329	6329.967244	25.659059
182.465830	6340.827086	25.664077
183.267516	6350.491172	25.669095
182.775888	6364.143619	25.674112
183.214836	6352.007396	25.679130
183.195339	6362.101397	25.684148
183.419443	6375.008728	25.689165
183.548723	6378.886883	25.694183
183.604731	6396.495431	25.699200
183.907825	6409.174614	25.704218
183.816850	6425.355762	25.709236
184.051167	6432.642150	25.714253
184.404782	6442.666491	25.719271
184.222967	6467.177142	25.724288
184.591123	6451.476084	25.729306
184.847850	6480.227755	25.734324
184.814615	6477.885373	25.739341
185.063794	6489.750220	25.744359
185.412417	6508.572717	25.749376
185.681637	6518.398126	25.754394
186.012779	6526.766725	25.759412
186.282270	6536.182175	25.764429
186.541620	6542.492914	25.769447
186.668313	6547.830275	25.774464
186.857552	6551.997117	25.779482
186.958057	6573.616246	25.784500
187.060120	6585.486527	25.789517
187.443057	6579.420667	25.794535
187.645846	6593.846204	25.799552
187.940906	6599.009606	25.804570
187.855263	6599.719748	25.809588
187.967749	6611.807123	25.814605
188.218802	6614.683980	25.819623
188.317953	6640.818958	25.824640
188.568084	6637.703568	25.829658
188.713323	6644.502274	25.834676
188.605692	6671.136068	25.839693
188.754926	6675.576842	25.844711
189.085368	6691.174152	25.849728
189.663384	6703.584727	25.854746
189.581447	6698.677173	25.859764
189.819326	6712.897379	25.864781
190.313567	6719.237625	25.869799
190.202953	6722.064368	25.874816
190.382926	6726.732370	25.879834
190.478042	6744.204482	25.884852
190.677371	6754.028602	25.889869
190.920101	6764.597226	25.894887
190.603439	6771.730856	25.899904
191.008934	6783.227174	25.904922
191.329520	6792.830561	25.909940
191.195653	6806.255631	25.914957
191.717027	6813.366616	25.919975
191.702096	6816.540850	25.924992
192.102693	6837.926828	25.930010
192.457579	6849.753080	25.935028
192.702338	6854.790044	25.940045
192.930200	6870.649388	25.945063
192.759912	6885.068593	25.950080
193.005718	6877.434294	25.955098
193.438838	6902.506986	25.960116
193.547721	6913.903556	25.965133
193.880322	6912.701913	25.970151
193.712647	6931.779577	25.975168
194.064159	6946.262003	25.980186
194.378118	6943.749318	25.985204
194.398411	6950.206927	25.990221
194.908282	6967.375555	25.995239
194.917340	6979.771635	26.000256
194.908791	6986.823197	26.005274
195.410756	6998.731555	26.010292
195.547947	7007.882777	26.015309
195.779011	7009.046021	26.020327
195.694123	7032.003882	26.025344
195.881756	7033.698086	26.030362
196.515743	7042.635578	26.035380
196.468949	7059.600356	26.040397
197.256035	7058.263298	26.045415
197.261890	7053.343991	26.050432
197.583030	7053.509330	26.055450
197.705307	7052.007588	26.060468
197.805835	7083.459795	26.065485
198.154924	7079.461441	26.070503
198.013003	7076.753101	26.075520
198.306128	7084.884158	26.080538
198.515586	7091.694075	26.085556
198.871687	7109.096683	26.090573
198.869344	7121.524992	26.095591
198.793857	7125.309306	26.100608
199.177960	7126.148375	26.105626
199.443278	7130.844601	26.110644
199.249668	7148.564651	26.115661
199.688890	7152.107185	26.120679
199.608739	7167.884549	26.125696
199.603923	7185.290493	26.130714
200.015234	7194.175451	26.135732
199.941952	7210.629240	26.140749
200.496241	7225.809019	26.145767
200.564190	7249.971119	26.150784
200.953896	7257.109606	26.155802
201.090120	7257.881190	26.160820
200.795604	7284.384569	26.165837
201.287612	7283.085882	26.170855
201.543022	7299.105744	26.175872
201.753861	7309.991435	26.180890
202.047134	7320.374569	26.185908
202.438717	7334.528377	26.190925
202.762335	7339.581262	26.195943
202.846850	7337.412752	26.200960
202.751819	7349.868224	26.205978
203.097837	7367.784985	26.210996
202.787187	7385.472042	26.216013
203.190485	7400.355822	26.221031
203.415684	7414.120770	26.226048
203.737568	7432.888903	26.231066
203.968294	7437.049383	26.236084
204.195084	7454.563500	26.241101
203.873109	7466.004003	26.246119
204.199814	7478.702370	26.251136
204.827767	7498.074886	26.256154
205.309629	7496.160900	26.261172
205.721572	7515.199624	26.266189
205.980948	7517.835339	26.271207
206.455357	7522.292198	26.276224
206.229612	7520.943463	26.281242
206.600138	7523.912401	26.286260
206.830239	7547.503049	26.291277
206.979790	7549.031849	26.296295
207.018664	7558.131413	26.301312
207.131163	7555.445374	26.306330
207.505577	7559.916612	26.311348
207.821412	7576.781677	26.316365
207.731800	7572.398324	26.321383
208.209253	7572.253907	26.326400
208.056893	7596.431232	26.331418
208.863347	7602.804710	26.336436
208.802919	7602.240087	26.341453
209.052631	7607.208849	26.346471
209.077894	7615.992723	26.351488
209.130948	7639.327683	26.356506
209.547657	7642.542654	26.361524
209.424969	7653.786287	26.366541
209.701654	7673.315752	26.371559
209.884851	7676.834708	26.376576
209.832341	7692.601137	26.381594
210.658932	7682.030084	26.386612
210.518477	7694.324693	26.391629
210.651127	7706.684362	26.396647
210.596443	7717.123246	26.401664
210.963002	7731.049295	26.406682
211.413440	7738.596952	26.411700
211.370494	7764.506329	26.416717
211.992558	7779.305254	26.421735
212.296081	7786.510458	26.426752
211.987813	7798.092240	26.431770
212.614391	7791.275718	26.436788
212.604693	7819.775013	26.441805
212.854335	7819.933666	26.446823
212.887425	7826.714596	26.451840
213.334489	7852.933154	26.456858
213.699239	7853.599093	26.461876
213.412141	7857.735227	26.466893
213.628500	7867.677763	26.471911
213.902889	7875.918471	26.476928
213.659168	7895.627976	26.481946
214.053549	7910.524706	26.486964
214.381444	7937.470607	26.491981
214.506265	7951.846154	26.496999
214.831334	7970.758459	26.502016
214.794416	7988.765344	26.507034
215.342052	7989.485938	26.512052
215.180036	8020.891484	26.517069
215.622117	8032.502156	26.522087
215.806387	8049.188860	26.527104
216.063146	8073.063306	26.532122
216.552125	8078.904517	26.537140
216.651921	8094.246562	26.542157
217.189457	8107.818359	26.547175
217.406282	8118.294896	26.552192
217.472069	8127.272089	26.557210
218.045476	8137.003654	26.562228
218.252458	8150.078933	26.567245
218.513914	8145.903841	26.572263
218.817785	8150.140207	26.577280
218.998360	8173.664200	26.582298
219.281771	8155.935623	26.587316
219.257937	8167.666709	26.592333
219.718444	8173.551843	26.597351
219.851568	8176.586696	26.602368
219.890613	8190.361580	26.607386
219.972903	8186.654129	26.612404
220.403824	8195.488563	26.617421
220.647869	8209.076552	26.622439
220.640322	8217.073209	26.627456
220.812993	8225.475510	26.632474
221.020231	8241.864861	26.637492
221.150381	8250.640651	26.642509
221.387766	8248.453935	26.647527
221.734048	8267.279037	26.652544
221.810341	8276.354975	26.657562
222.278493	8284.221144	26.662580
222.350987	8302.749207	26.667597
222.169125	8314.939579	26.672615
223.074696	8320.321417	26.677632
223.134969	8338.888851	26.682650
223.205134	8336.309753	26.687668
223.199599	8364.661878	26.692685
223.213260	8371.320641	26.697703
223.862100	8392.446589	26.702720
223.906653	8417.587322	26.707738
224.262104	8412.675970	26.712756
224.316603	8433.834951	26.717773
224.554157	8444.950927	26.722791
224.961387	8450.283597	26.727808
225.374594	8471.200524	26.732826
225.412078	8477.486867	26.737844
225.605657	8482.554580	26.742861
225.567193	8501.669517	26.747879
225.956431	8502.238729	26.752896
225.859642	8524.725482	26.757914
226.146655	8533.589354	26.762932
226.298907	8555.696111	26.767949
226.528768	8567.387068	26.772967
226.853915	8583.764293	26.777984
227.251847	8601.963458	26.783002
227.424415	8610.536361	26.788020
227.536564	8633.045052	26.793037
227.849169	8641.327702	26.798055
228.158015	8666.394063	26.803072
228.051636	8687.393334	26.808090
228.618705	8700.639115	26.813108
228.630062	8712.020737	26.818125
228.548223	8730.332739	26.823143
229.160250	8740.754189	26.828160
229.226694	8769.687375	26.833178
229.422390	8778.946824	26.838196
230.037011	8801.459083	26.843213
230.158418	8811.176585	26.848231
230.819329	8830.080904	26.853248
230.784236	8840.391144	26.858266
231.141904	8855.555935	26.863284
231.104291	8856.132615	26.868301
231.239286	8878.524715	26.873319
231.665120	8891.428042	26.878336
231.907094	8902.027817	26.883354
232.481616	8920.022159	26.888372
232.660272	8930.468759	26.893389
232.728284	8944.711095	26.898407
232.935592	8945.008325	26.903424
232.850470	8968.290263	26.908442
233.066263	8975.444322	26.913460
233.541561	8992.254878	26.918477
233.548003	9003.693378	26.923495
234.134006	9015.389688	26.928512
234.402634	9038.587014	26.933530
234.622747	9045.357569	26.938548
234.925184	9062.911880	26.943565
235.097411	9068.321976	26.948583
235.790595	9075.326403	26.953600
235.607940	9096.083041	26.958618
235.766405	9089.082839	26.963636
235.916465	9107.136414	26.968653
236.096713	9127.499219	26.973671
236.369792	9127.941785	26.978688
236.624712	9147.275583	26.983706
236.361922	9160.089031	26.988724
236.916330	9175.325482	26.993741
237.168542	9192.603862	26.998759
237.522473	9185.122321	27.003776
237.692817	9209.406226	27.008794
237.991691	9210.194483	27.013812
237.999528	9217.055615	27.018829
238.362661	9238.753600	27.023847
238.585227	9259.066556	27.028864
238.689366	9274.016033	27.033882
238.790058	9285.564849	27.038900
239.159853	9299.636256	27.043917
239.290798	9322.019040	27.048935
239.535631	9333.236428	27.053952
239.911902	9354.748732	27.058970
240.302767	9376.325632	27.063988
240.617801	9387.134848	27.069005
240.783530	9397.472873	27.074023
241.096531	9411.364175	27.079040
241.046715	9432.889818	27.084058
241.465259	9437.175560	27.089076
241.790456	9458.462427	27.094093
241.705520	9467.903182	27.099111
242.574284	9479.977385	27.104128
242.434946	9491.761757	27.109146
242.332000	9517.400812	27.114164
242.521449	9520.140111	27.119181
242.674215	9551.355842	27.124199
243.286954	9569.423180	27.129216
243.292585	9596.876343	27.134234
243.932382	9613.378067	27.139252
244.395938	9625.864036	27.144269
244.663674	9630.733413	27.149287
244.782878	9640.113405	27.154304
244.810831	9657.154201	27.159322
245.141263	9674.219202	27.164340
245.754438	9674.395483	27.169357
246.058698	9685.532441	27.174375
246.106347	9702.300610	27.179392
246.497473	9717.350765	27.184410
246.538660	9715.574048	27.189428
246.991060	9724.032548	27.194445
246.905058	9744.939544	27.199463
246.951648	9748.529561	27.204480
247.779314	9767.482071	27.209498
247.673325	9781.710440	27.214516
248.126441	9786.625475	27.219533
248.173887	9804.935489	27.224551
248.260364	9805.998061	27.229568
248.276180	9832.805491	27.234586
248.521587	9845.645148	27.239604
249.230201	9860.180123	27.244621
249.193780	9879.889087	27.249639
249.750306	9889.535173	27.254656
249.925936	9902.139674	27.259674
249.889801	9918.950951	27.264692
250.445340	9928.864404	27.269709
250.395583	9935.511933	27.274727
250.656498	9949.502541	27.279744
250.728813	9959.704348	27.284762
251.236214	9978.490181	27.289780
251.296059	9991.568882	27.294797
251.352861	10019.116574	27.299815
251.762884	10025.273745	27.304832
251.766329	10049.879948	27.309850
251.840228	10070.004422	27.314868
252.457751	10090.746632	27.319885
252.537116	10102.591058	27.324903
252.902694	10128.041171	27.329920
253.573111	10129.022883	27.334938
253.680848	10160.718864	27.339956
254.231719	10154.319849	27.344973
254.292841	10179.020166	27.349991
254.540034	10191.635145	27.355008
255.234452	10199.390713	27.360026
255.081241	10221.085461	27.365044
255.627053	10221.128077	27.370061
256.030251	10237.646564	27.375079
256.294618	10253.816518	27.380096
256.491790	10262.136177	27.385114
256.444059	10260.781632	27.390132
257.091073	10262.749664	27.395149
257.161672	10285.415412	27.400167
257.050608	10290.071113	27.405184
257.503828	10297.341819	27.410202
257.651451	10319.129237	27.415220
257.961819	10325.982395	27.420237
258.358598	10357.165231	27.425255
258.366593	10355.165496	27.430272
258.405549	10370.327141	27.435290
258.534115	10384.025626	27.440308
259.046243	10406.785859	27.445325
259.244503	10431.945203	27.450343
259.490230	10448.027437	27.455360
259.861665	10470.794650	27.460378
259.893220	10495.940536	27.465396
260.365749	10506.007301	27.470413
260.434100	10527.154034	27.475431
260.669148	10542.169297	27.480448
260.977227	10566.054879	27.485466
261.125217	10583.595844	27.490484
262.255058	10589.676289	27.495501
261.965705	10605.696415	27.500519
261.926158	10633.833541	27.505536
262.390652	10642.531859	27.510554
262.473699	10663.593410	27.515572
262.453725	10679.325516	27.520589
263.183115	10700.698464	27.525607
263.495150	10718.599475	27.530624
263.591387	10735.696324	27.535642
263.938326	10763.559587	27.540660
264.301861	10763.814249	27.545677
264.635887	10777.974205	27.550695
264.408005	10792.034460	27.555712
265.091948	10794.791978	27.560730
265.401033	10814.706417	27.565748
265.641787	10823.555018	27.570765
265.623541	10836.669723	27.575783
265.925872	10854.496100	27.580800
266.395595	10875.009921	27.585818
266.463483	10889.469372	27.590836
266.948672	10903.804473	27.595853
266.742828	10922.667006	27.600871
266.823053	10939.383741	27.605888
267.536103	10964.601224	27.610906
267.708800	10989.082024	27.615924
268.111315	10999.299195	27.620941
268.374640	11025.712366	27.625959
268.766691	11038.231769	27.630976
269.153597	11059.780237	27.635994
268.893000	11075.337032	27.641012
269.669185	11092.407363	27.646029
269.957367	11108.272605	27.651047
269.819783	11123.519419	27.656064
270.710285	11134.982721	27.661082
270.805131	11162.821580	27.666100
271.043096	11159.891382	27.671117
271.089175	11180.288582	27.676135
271.467371	11195.328114	27.681152
272.163473	11203.134312	27.686170
272.096224	11235.040281	27.691188
272.361461	11237.619457	27.696205
272.466477	11262.375152	27.701223
272.795164	11274.798993	27.706240
273.005972	11289.606751	27.711258
273.129754	11304.414424	27.716276
273.474730	11324.200836	27.721293
273.822919	11344.049924	27.726311
274.101346	11363.620124	27.731328
274.303518	11377.960254	27.736346
274.308461	11403.999700	27.741364
274.586329	11419.488925	27.746381
275.006992	11445.374224	27.751399
274.922858	11469.589389	27.756416
275.443379	11487.126921	27.761434
275.989213	11524.235717	27.766452
276.225502	11532.485304	27.771469
276.633689	11560.028593	27.776487
276.872298	11584.482535	27.781504
276.959766	11592.698616	27.786522
277.091455	11622.643975	27.791540
277.726816	11633.797686	27.796557
278.226017	11645.452242	27.801575
278.345970	11669.767229	27.806592
278.989346	11668.784487	27.811610
279.075728	11690.973248	27.816628
279.380356	11694.278604	27.821645
279.602259	11699.685865	27.826663
279.924852	11723.835623	27.831680
280.447502	11727.088133	27.836698
280.400025	11742.588421	27.841716
280.649165	11746.167880	27.846733
281.037532	11766.790333	27.851751
281.093215	11780.036532	27.856768
281.462027	11782.228183	27.861786
281.886569	11808.431273	27.866804
281.861300	11810.000581	27.871821
282.205315	11827.582189	27.876839
282.454389	11846.056162	27.881856
282.836247	11851.900988	27.886874
282.896551	11874.168947	27.891892
283.248075	11889.003860	27.896909
283.541299	11902.208566	27.901927
283.372159	11924.576531	27.906944
283.942325	11935.962032	27.911962
284.230446	11955.667621	27.916980
284.657984	11974.882691	27.921997
284.781757	11997.115527	27.927015
285.066790	12011.642974	27.932032
285.452678	12027.416080	27.937050
285.452823	12060.728245	27.942068
285.820283	12069.914924	27.947085
285.962046	12090.773702	27.952103
286.365523	12125.501476	27.957120
286.731827	12143.838864	27.962138
286.995267	12172.602937	27.967156
287.456117	12193.121539	27.972173
287.921262	12207.135214	27.977191
287.704938	12239.363005	27.982208
288.108429	12239.569616	27.987226
288.535551	12271.758281	27.992244
289.048489	12284.847033	27.997261
289.541165	12302.756944	28.002279
289.754158	12317.993943	28.007296
290.246683	12331.207401	28.012314
290.478295	12346.583142	28.017332
291.174125	12367.280395	28.022349
291.101343	12371.817285	28.027367
291.036977	12382.090133	28.032384
291.463539	12394.190353	28.037402
291.546718	12413.850096	28.042420
291.919958	12430.328535	28.047437
292.210684	12441.184558	28.052455
292.303199	12467.653641	28.057472
293.050702	12477.861303	28.062490
293.186166	12494.719321	28.067508
293.459127	12512.776273	28.072525
293.900309	12528.620588	28.077543
294.055054	12549.543849	28.082560
294.396270	12557.859527	28.087578
294.248344	12577.646247	28.092596
294.605400	12597.704351	28.097613
294.771146	12604.428112	28.102631
295.006276	12637.904019	28.107648
295.088964	12644.753989	28.112666
295.550650	12668.980687	28.117684
295.969467	12694.069870	28.122701
296.308648	12705.477027	28.127719
296.485853	12734.281293	28.132736
296.884272	12745.910063	28.137754
296.833035	12780.658284	28.142772
296.909026	12793.960772	28.147789
297.756643	12818.915896	28.152807
297.894611	12848.011575	28.157824
298.531798	12871.341816	28.162842
298.630869	12890.351431	28.167860
298.808972	12916.568754	28.172877
299.438290	12921.014666	28.177895
299.719739	12943.488137	28.182912
300.070265	12956.208800	28.187930
300.159942	12973.428370	28.192948
300.488931	12991.665778	28.197965
301.094762	13004.594923	28.202983
301.144636	13031.587561	28.208000
301.138006	13052.981778	28.213018
301.665394	13078.764697	28.218036
301.838088	13104.557061	28.223053
302.130332	13125.472482	28.228071
302.550786	13150.580952	28.233088
302.918066	13165.044935	28.238106
303.600956	13180.797685	28.243124
303.811007	13204.227413	28.248141
304.749799	13204.507930	28.253159
305.151149	13211.734499	28.258176
305.417912	13219.499491	28.263194
305.826928	13224.359329	28.268212
306.187829	13222.617441	28.273229
306.190431	13228.174932	28.278247
305.981035	13255.411491	28.283264
306.296932	13257.146191	28.288282
306.645571	13278.915074	28.293300
306.696426	13291.483569	28.298317
307.236699	13297.162416	28.303335
307.422358	13321.195834	28.308352
307.789959	13348.753270	28.313370
307.989092	13359.768108	28.318388
308.232622	13382.405115	28.323405
308.836554	13397.649176	28.328423
308.936857	13428.980347	28.333440
308.996954	13429.395112	28.338458
309.321877	13456.909855	28.343476
309.464195	13479.435615	28.348493
309.719640	13496.966168	28.353511
310.328937	13519.500903	28.358528
310.748834	13539.330122	28.363546
311.259519	13555.349912	28.368564
311.508595	13571.443294	28.373581
312.016852	13578.202046	28.378599
312.020408	13598.956019	28.383616
312.294097	13606.110433	28.388634
312.429529	13619.969069	28.393652
312.141859	13651.764878	28.398669
312.788504	13660.256931	28.403687
313.217109	13692.175804	28.408704
313.308819	13711.877287	28.413722
313.877935	13733.682628	28.418740
313.683132	13759.132515	28.423757
314.079914	13797.360880	28.428775
314.297014	13823.695463	28.433792
314.731767	13846.923973	28.438810
315.049018	13869.442698	28.443828
314.973916	13907.060799	28.448845
315.768330	13932.062840	28.453863
316.031929	13955.749391	28.458880
316.826437	13989.865009	28.463898
316.977243	14011.870452	28.468916
317.142649	14038.876763	28.473933
317.357508	14055.055518	28.478951
318.068352	14084.659837	28.483968
318.246168	14100.877509	28.488986
318.771734	14117.817609	28.494004
319.003558	14151.443194	28.499021
319.413848	14176.009831	28.504039
319.559980	14192.775431	28.509056
319.983855	14207.240931	28.514074
320.524025	14220.555900	28.519092
320.559567	14251.404313	28.524109
321.060762	14260.906559	28.529127
321.288301	14288.086435	28.534144
321.408306	14318.553695	28.539162
321.931978	14331.603441	28.544180
322.024658	14354.776834	28.549197
322.726255	14380.555843	28.554215
322.963466	14404.182151	28.559232
323.369909	14419.803517	28.564250
323.580571	14429.413083	28.569268
324.216023	14451.253848	28.574285
324.719484	14473.368280	28.579303
324.882038	14488.068663	28.584320
325.444285	14510.496838	28.589338
325.763134	14525.088901	28.594356
325.614558	14531.633542	28.599373
326.097835	14544.890456	28.604391
326.250332	14565.583819	28.609408
326.611062	14582.062747	28.614426
327.068783	14603.223941	28.619444
327.109075	14626.262719	28.624461
327.518376	14652.985233	28.629479
327.684788	14676.022191	28.634496
328.144338	14685.173050	28.639514
328.599945	14691.052592	28.644532
329.129875	14720.555510	28.649549
329.546353	14721.617601	28.654567
329.697123	14735.073508	28.659584
329.903052	14758.035113	28.664602
330.002862	14771.647962	28.669620
330.046443	14795.253972	28.674637
330.829526	14808.592837	28.679655
330.975295	14836.408049	28.684672
330.988504	14856.718376	28.689690
331.395931	14877.668718	28.694708
331.500622	14898.682883	28.699725
332.107176	14922.448629	28.704743
332.309417	14954.087181	28.709760
332.446314	14973.771867	28.714778
332.810557	14999.131071	28.719796
333.351166	15029.740251	28.724813
333.513211	15058.173823	28.729831
334.325081	15076.010942	28.734848
334.388891	15111.504537	28.739866
335.471631	15126.416988	28.744884
335.071699	15150.082021	28.749901
335.552742	15169.240937	28.754919
336.066603	15194.777765	28.759936
335.880936	15212.503005	28.764954
336.654774	15234.354326	28.769972
336.382556	15276.569685	28.774989
336.620709	15295.725940	28.780007
337.225689	15331.776306	28.785024
337.484998	15360.184012	28.790042
337.953485	15382.970478	28.795060
338.216864	15419.390792	28.800077
338.700517	15447.561069	28.805095
339.201640	15460.360595	28.810112
339.456219	15493.473765	28.815130
340.213424	15511.586599	28.820148
340.548524	15545.381231	28.825165
340.973108	15563.192859	28.830183
341.291370	15581.198393	28.835200
341.490085	15612.037605	28.840218
341.670236	15626.617886	28.845236
342.071091	15656.962050	28.850253
342.022171	15668.456503	28.855271
342.566403	15696.102107	28.860288
342.946480	15723.407831	28.865306
343.510171	15736.987859	28.870324
343.592074	15766.654039	28.875341
344.115543	15790.629425	28.880359
344.714867	15813.111073	28.885376
344.966858	15843.998944	28.890394
345.501935	15857.175229	28.895412
345.369433	15879.405737	28.900429
345.489838	15900.057790	28.905447
346.294694	15923.087280	28.910464
346.408389	15953.908052	28.915482
346.900965	15978.469289	28.920500
347.180067	16007.743922	28.925517
347.512520	16024.616753	28.930535
347.626398	16041.598442	28.935552
347.792972	16075.529151	28.940570
348.396426	16094.863099	28.945588
348.065295	16117.798751	28.950605
348.762553	16140.505204	28.955623
349.184235	16178.784151	28.960640
349.341152	16205.773972	28.965658
350.135322	16217.288200	28.970676
350.212424	16248.071497	28.975693
350.709375	16281.440026	28.980711
351.370094	16292.327025	28.985728
351.624946	16328.765018	28.990746
352.206285	16344.641353	28.995764
352.333644	16368.947471	29.000781
352.589928	16385.339972	29.005799
353.448740	16416.702308	29.010816
353.458950	16443.411820	29.015834
353.836596	16463.353421	29.020852
354.098695	16485.120378	29.025869
354.547950	16507.545076	29.030887
355.120616	16519.318630	29.035904
355.183523	16553.118694	29.040922
355.579318	16565.917231	29.045940
355.951601	16593.377695	29.050957
356.468562	16616.191334	29.055975
356.906244	16635.817908	29.060992
356.943326	16656.340365	29.066010
357.682730	16670.136113	29.071028
358.196747	16696.187673	29.076045
358.352161	16714.373622	29.081063
358.880448	16729.907461	29.086080
358.978649	16754.010185	29.091098
359.397999	16777.379930	29.096116
359.656493	16789.827924	29.101133
360.144545	16808.991608	29.106151
360.554226	16834.683679	29.111168
360.624687	16858.893145	29.116186
360.776794	16876.544810	29.121204
361.007171	16905.087031	29.126221
361.275862	16934.152495	29.131239
361.803052	16963.698048	29.136256
362.097614	16988.714275	29.141274
362.492738	17025.373865	29.146292
362.720420	17045.056668	29.151309
362.827860	17085.996452	29.156327
363.131547	17121.851791	29.161344
363.548338	17157.752180	29.166362
364.153408	17180.297703	29.171380
364.669122	17212.451929	29.176397
364.566542	17252.210714	29.181415
365.248463	17272.393443	29.186432
365.524906	17315.626092	29.191450
365.978878	17331.581616	29.196468
366.483620	17349.541194	29.201485
366.962949	17380.726014	29.206503
367.816314	17404.456664	29.211520
367.693291	17427.092196	29.216538
368.107940	17445.912278	29.221556
368.358124	17467.895897	29.226573
368.257612	17494.036101	29.231591
369.092329	17521.985137	29.236608
369.324350	17549.910584	29.241626
369.835352	17570.736279	29.246644
370.221967	17597.512006	29.251661
370.487055	17630.219231	29.256679
371.140191	17652.748731	29.261696
371.441994	17681.009351	29.266714
371.665005	17705.327125	29.271732
372.225351	17725.399114	29.276749
372.405177	17755.338338	29.281767
373.159104	17770.695343	29.286784
372.839305	17807.818539	29.291802
373.074694	17826.952687	29.296820
374.200941	17862.764490	29.301837
374.260211	17889.143674	29.306855
374.889395	17907.913203	29.311872
375.036418	17938.844620	29.316890
375.267551	17961.350084	29.321908
375.506916	17996.664545	29.326925
375.801743	18033.660810	29.331943
376.563484	18056.940920	29.336960
376.485469	18092.769563	29.341978
376.607024	18125.293614	29.346996
377.540325	18159.351789	29.352013
377.747926	18199.018683	29.357031
378.431631	18230.171857	29.362048
378.636911	18264.724627	29.367066
379.231373	18290.501875	29.372084
379.511585	18313.890206	29.377101
379.824643	18345.478273	29.382119
380.403047	18374.627992	29.387136
380.674360	18408.418569	29.392154
380.820138	18434.464803	29.397172
381.231549	18467.507177	29.402189
381.517204	18496.836850	29.407207
382.547951	18518.357011	29.412224
382.400016	18556.519994	29.417242
382.726552	18585.581892	29.422260
383.197534	18615.325581	29.427277
383.584850	18649.118275	29.432295
384.219614	18673.069575	29.437312
384.314399	18712.249429	29.442330
384.883354	18734.779350	29.447348
385.726403	18758.287335	29.452365
386.054775	18783.347132	29.457383
386.391137	18812.952799	29.462400
386.678190	18843.267208	29.467418
386.989352	18859.254151	29.472436
387.433652	18885.047651	29.477453
387.964789	18908.161838	29.482471
388.193985	18921.305035	29.487488
388.547658	18947.508775	29.492506
388.916889	18977.893427	29.497524
389.205254	19002.528427	29.502541
389.143956	19030.903691	29.507559
389.982266	19046.215841	29.512576
389.649148	19083.726893	29.517594
390.055884	19106.629290	29.522612
390.461406	19129.521284	29.527629
390.941083	19177.587327	29.532647
391.742494	19211.820022	29.537664
392.260492	19249.936463	29.542682
392.524060	19272.683949	29.547700
392.686338	19306.439905	29.552717
393.332417	19344.767684	29.557735
393.541730	19370.165928	29.562752
393.816702	19410.176772	29.567770
394.475156	19437.781725	29.572788
395.182436	19463.571685	29.577805
395.108663	19501.595220	29.582823
395.887169	19515.683383	29.587840
396.293982	19551.449534	29.592858
396.470840	19582.857852	29.597876
396.774477	19607.817391	29.602893
397.576220	19639.753485	29.607911
398.167011	19653.958702	29.612928
398.224028	19688.706377	29.617946
398.361471	19718.780547	29.622964
399.195839	19733.987301	29.627981
399.427241	19782.057358	29.632999
399.738731	19804.997613	29.638016
400.222073	19832.763074	29.643034
400.361288	19864.472478	29.648052
400.808947	19901.900450	29.653069
401.335237	19936.143924	29.658087
401.863436	19953.313309	29.663104
402.249620	19992.610587	29.668122
402.511272	20022.612392	29.673140
402.701231	20050.836459	29.678157
402.972605	20083.994738	29.683175
403.375985	20117.597867	29.688192
403.846420	20151.988133	29.693210
404.179904	20202.063969	29.698228
404.983493	20225.106771	29.703245
405.300120	20256.320913	29.708263
406.049422	20280.210760	29.713280
406.233437	20321.767787	29.718298
406.665232	20341.939242	29.723316
407.507074	20371.192474	29.728333
407.705406	20404.014195	29.733351
407.718312	20430.973253	29.738368
408.596735	20460.323989	29.743386
408.689142	20482.168860	29.748404
408.911560	20506.871469	29.753421
408.900391	20537.001206	29.758439
409.352265	20571.791086	29.763456
409.760397	20606.860500	29.768474
409.829255	20646.499791	29.773492
410.693193	20671.913182	29.778509
410.806079	20715.162009	29.783527
411.185476	20756.767416	29.788544
411.880058	20784.050037	29.793562
412.129820	20822.845051	29.798580
412.704082	20849.859503	29.803597
413.041246	20885.144821	29.808615
413.327037	20922.400981	29.813632
413.641939	20964.280255	29.818650
414.063380	21005.113330	29.823668
414.807596	21040.488499	29.828685
415.101249	21077.557910	29.833703
415.564665	21124.502368	29.838720
415.846045	21158.581192	29.843738
416.185843	21199.759344	29.848756
416.941039	21231.471803	29.853773
416.955291	21277.366788	29.858791
417.270536	21304.553241	29.863808
417.956494	21346.804424	29.868826
418.361728	21391.859322	29.873844
419.050994	21414.919337	29.878861
419.630207	21449.901153	29.883879
420.149631	21477.397182	29.888896
420.752193	21510.937294	29.893914
421.166282	21542.588958	29.898932
421.898985	21568.947762	29.903949
421.956179	21609.000086	29.908967
422.640242	21629.486628	29.913984
423.373988	21658.594882	29.919002
423.445332	21692.015247	29.924020
423.626518	21707.674544	29.929037
423.851124	21754.396660	29.934055
424.568739	21778.963296	29.939072
424.969084	21815.418871	29.944090
425.235145	21852.385025	29.949108
425.771837	21867.323892	29.954125
425.973613	21912.246512	29.959143
426.169468	21948.249813	29.964160
426.813716	21982.830225	29.969178
427.063905	22012.389502	29.974196
427.742145	22049.759071	29.979213
427.715553	22082.283815	29.984231
428.083090	22125.900765	29.989248
429.081045	22161.891747	29.994266
429.119366	22199.703089	29.999284
429.622229	22236.927767	30.004301
429.788207	22281.812245	30.009319
430.231302	22312.128179	30.014336
430.683641	22354.350761	30.019354
430.792646	22394.258196	30.024372
431.583996	22431.164062	30.029389
432.163013	22472.701233	30.034407
432.653794	22501.722947	30.039424
433.124586	22528.338536	30.044442
433.477977	22558.247851	30.049460
433.750487	22592.257932	30.054477
434.245784	22635.422732	30.059495
434.611779	22674.002139	30.064512
435.493420	22695.673918	30.069530
435.569496	22734.276822	30.074548
435.989453	22763.900246	30.079565
436.377245	22805.860217	30.084583
436.705736	22851.302484	30.089600
437.337314	22885.418240	30.094618
437.627313	22921.939630	30.099636
438.156101	22966.824165	30.104653
438.568671	23010.120527	30.109671
438.847762	23043.429513	30.114688
439.414717	23076.764383	30.119706
439.695970	23124.076982	30.124724
440.177048	23161.675931	30.129741
440.790691	23202.633718	30.134759
441.264141	23228.969652	30.139776
441.708731	23263.869024	30.144794
441.882464	23313.073178	30.149812
442.612124	23347.306631	30.154829
443.180062	23384.730798	30.159847
443.748059	23427.004763	30.164864
444.556601	23452.792233	30.169882
444.685656	23488.256724	30.174900
445.576197	23524.312035	30.179917
445.748837	23551.119415	30.184935
446.231829	23598.810880	30.189952
446.444472	23619.917833	30.194970
446.931492	23654.724659	30.199988
447.490804	23693.524654	30.205005
447.794065	23727.881214	30.210023
448.334951	23771.160782	30.215040
448.885207	23797.777658	30.220058
448.864604	23833.567660	30.225076
449.400486	23867.776395	30.230093
449.764304	23907.255545	30.235111
450.016478	23957.325114	30.240128
450.463320	23985.775222	30.245146
451.078160	24033.016896	30.250164
451.196036	24075.558074	30.255181
451.740556	24123.843118	30.260199
452.333807	24163.699898	30.265216
452.850896	24213.447639	30.270234
453.286583	24256.964272	30.275252
453.491206	24297.029028	30.280269
454.039843	24337.858308	30.285287
454.465727	24388.211915	30.290304
455.243039	24426.251896	30.295322
455.454400	24467.836317	30.300340
455.939426	24497.696014	30.305357
456.474434	24534.509765	30.310375
456.783047	24576.834410	30.315392
457.638753	24602.863586	30.320410
457.939805	24640.604994	30.325428
458.249797	24672.823814	30.330445
459.063413	24699.702734	30.335463
459.316396	24744.874909	30.340480
459.821710	24781.656937	30.345498
460.234984	24814.741862	30.350516
460.830142	24850.536083	30.355533
461.245280	24886.972720	30.360551
461.202940	24935.335597	30.365568
462.157214	24963.858645	30.370586
462.215403	25015.402444	30.375604
462.570407	25047.314714	30.380621
463.408204	25090.046395	30.385639
463.564757	25132.626761	30.390656
464.420680	25162.098541	30.395674
464.732669	25206.744272	30.400692
465.686323	25239.332773	30.405709
466.523288	25266.694982	30.410727
466.749033	25317.371723	30.415744
467.143608	25336.244633	30.420762
467.415279	25375.343480	30.425780
467.685111	25418.465089	30.430797
468.315267	25445.714814	30.435815
468.673889	25485.130942	30.440832
469.299271	25524.559026	30.445850
469.499759	25571.549061	30.450868
470.174984	25603.961298	30.455885
470.710043	25644.493571	30.460903
470.818062	25684.106093	30.465920
471.530026	25715.786364	30.470938
471.581465	25762.138959	30.475956
472.213449	25802.076375	30.480973
472.747988	25838.473310	30.485991
473.294199	25882.489611	30.491008
473.863117	25927.279185	30.496026
474.080424	25977.186522	30.501044
474.670773	26020.983465	30.506061
475.235942	26051.099573	30.511079
475.794317	26105.088948	30.516096
476.716315	26123.436804	30.521114
476.893514	26169.324638	30.526132
477.316474	26197.694254	30.531149
478.257513	26247.687239	30.536167
478.575939	26275.845968	30.541184
479.007912	26305.378731	30.546202
479.375766	26338.259751	30.551220
479.843062	26380.928639	30.556237
480.401650	26401.301899	30.561255
481.036288	26439.755435	30.566272
481.430957	26465.341923	30.571290
481.826139	26495.090457	30.576308
482.153045	26533.249748	30.581325
482.739760	26558.541868	30.586343
482.893432	26595.037432	30.591360
483.309129	26621.481919	30.596378
483.730025	26668.441621	30.601396
483.864393	26706.415340	30.606413
484.517115	26740.946440	30.611431
484.878323	26790.094379	30.616448
485.215125	26831.168599	30.621466
486.108377	26866.017755	30.626484
486.266429	26919.953885	30.631501
486.817249	26953.991151	30.636519
487.315650	27004.502927	30.641536
487.539119	27046.346571	30.646554
487.921415	27101.204038	30.651572
488.651573	27152.369518	30.656589
489.311576	27193.187542	30.661607
489.557034	27248.010579	30.666624
490.375049	27288.275804	30.671642
490.977720	27335.740300	30.676660
490.765367	27388.645015	30.681677
491.531261	27429.509797	30.686695
491.865330	27487.099142	30.691712
492.181123	27534.729680	30.696730
492.798341	27587.323255	30.701748
493.208386	27644.601663	30.706765
494.107647	27688.331081	30.711783
494.643503	27745.711139	30.716800
495.718325	27770.341219	30.721818
496.025763	27832.497911	30.726836
496.427632	27875.022807	30.731853
497.092303	27911.300483	30.736871
497.643736	27954.356440	30.741888
498.153225	27996.160130	30.746906
499.019249	28029.813807	30.751924
499.463559	28062.983201	30.756941
500.180589	28096.488989	30.761959
500.368534	28130.471507	30.766976
501.231016	28164.576712	30.771994
501.598258	28198.485112	30.777012
501.948371	28240.448765	30.782029
502.351083	28276.787901	30.787047
502.704361	28316.428479	30.792064
503.075452	28361.178323	30.797082
503.503677	28407.628974	30.802100
503.932538	28446.947390	30.807117
505.076301	28473.406575	30.812135
505.810679	28512.774185	30.817152
506.115347	28537.811777	30.822170
506.986560	28566.771285	30.827188
507.269884	28604.400312	30.832205
508.052944	28635.457271	30.837223
508.342402	28672.439376	30.842240
508.934642	28709.296116	30.847258
509.080574	28740.907042	30.852276
509.457668	28767.948992	30.857293
509.973384	28791.131645	30.862311
510.344566	28834.541709	30.867328
510.428088	28865.653810	30.872346
510.812446	28907.621612	30.877364
511.130331	28943.517170	30.882381
511.468620	28986.154388	30.887399
512.121756	29048.670400	30.892416
512.514895	29090.922514	30.897434
512.704493	29148.356386	30.902452
513.177175	29198.489848	30.907469
514.000721	29253.446626	30.912487
513.997686	29307.064918	30.917504
514.803900	29359.279551	30.922522
515.555732	29413.647863	30.927540
515.820634	29470.577606	30.932557
516.877342	29511.191717	30.937575
517.279833	29562.138060	30.942592
518.119337	29606.539349	30.947610
518.859606	29650.061421	30.952628
519.585263	29686.095383	30.957645
520.574118	29717.209886	30.962663
521.198038	29755.542208	30.967680
521.263359	29787.699106	30.972698
521.820851	29819.886412	30.977716
522.240837	29871.513332	30.982733
523.211038	29898.820434	30.987751
524.124163	29928.656675	30.992768
524.302460	29956.942625	30.997786
525.053645	29980.891648	31.002804
525.371655	30024.680558	31.007821
526.108010	30046.414614	31.012839
526.533761	30080.684826	31.017856
526.724771	30119.964794	31.022874
527.063630	30152.543760	31.027892
527.361158	30191.565805	31.032909
528.025682	30236.954900	31.037927
528.269757	30293.381774	31.042944
528.547596	30330.754040	31.047962
529.126566	30375.515706	31.052980
529.166144	30431.868460	31.057997
529.948592	30483.813099	31.063015
530.480712	30530.421889	31.068032
530.729383	30589.771037	31.073050
531.293818	30639.900615	31.078068
531.749625	30699.042223	31.083085
532.309668	30760.772678	31.088103
532.944057	30811.115439	31.093120
533.464919	30866.158959	31.098138
534.098442	30922.142977	31.103156
534.505059	30984.212351	31.108173
534.878361	31037.491091	31.113191
535.757317	31098.852074	31.118208
536.250110	31159.398482	31.123226
536.795503	31199.521391	31.128244
536.876354	31250.147529	31.133261
537.362865	31296.140043	31.138279
538.028203	31345.935755	31.143296
538.519596	31417.260863	31.148314
539.278304	31461.429458	31.153332
539.462383	31522.355786	31.158349
540.624942	31574.533346	31.163367
540.951126	31625.758324	31.168384
541.490501	31664.535721	31.173402
542.301861	31710.455586	31.178420
542.890556	31773.922210	31.183437
543.424557	31820.854325	31.188455
544.048531	31867.921980	31.193472
544.362933	31907.374133	31.198490
544.991686	31956.471395	31.203508
545.751377	32013.409961	31.208525
546.450939	32047.848727	31.213543
547.197729	32082.360428	31.218560
547.391719	32141.258906	31.223578
548.228299	32183.602835	31.228596
548.330982	32240.065214	31.233613
549.188487	32278.500212	31.238631
549.308841	32332.888951	31.243648
549.973944	32385.607001	31.248666
550.755963	32429.139265	31.253684
551.150000	32494.301009	31.258701
551.762545	32530.340333	31.263719
552.355424	32586.301811	31.268736
552.374997	32641.494161	31.273754
553.116398	32691.017017	31.278772
553.654370	32751.759111	31.283789
554.223498	32815.316399	31.288807
554.799696	32868.165216	31.293824
555.004293	32927.067955	31.298842
555.879976	32980.019175	31.303860
556.168663	33049.835720	31.308877
556.735165	33105.658137	31.313895
557.444179	33159.831308	31.318912
557.929586	33221.206133	31.323930
558.652639	33272.026219	31.328948
559.162422	33334.761086	31.333965
559.905145	33384.194382	31.338983
560.525607	33446.590476	31.344000
561.181397	33506.101227	31.349018
562.063776	33552.060623	31.354036
562.605500	33607.797251	31.359053
563.062885	33655.465591	31.364071
563.793583	33694.746935	31.369088
563.847769	33756.168776	31.374106
564.705122	33800.553343	31.379124
565.284408	33856.825515	31.384141
565.503208	33895.473197	31.389159
566.322543	33956.718740	31.394176
566.840299	34016.685232	31.399194
567.405656	34053.938167	31.404212
567.647291	34107.397530	31.409229
568.325250	34162.401795	31.414247
568.799437	34199.466223	31.419264
569.260991	34264.319922	31.424282
569.783030	34318.435224	31.429300
570.291072	34370.292360	31.434317
570.998881	34410.969439	31.439335
571.612144	34463.361852	31.444352
572.133457	34525.383684	31.449370
572.891862	34567.850213	31.454388
573.217988	34629.796323	31.459405
573.686693	34690.017400	31.464423
574.165626	34738.449985	31.469440
574.709436	34806.546475	31.474458
575.200114	34863.129381	31.479476
575.890453	34924.143644	31.484493
576.458676	34979.349378	31.489511
577.070941	35041.322384	31.494528
577.692119	35111.413069	31.499546
578.334169	35164.088441	31.504564
578.751314	35234.524282	31.509581
579.422571	35300.393823	31.514599
580.021151	35351.627909	31.519616
580.684578	35421.959102	31.524634
581.294533	35472.643122	31.529652
582.138098	35548.597961	31.534669
582.703032	35592.773756	31.539687
583.551391	35641.098096	31.544704
584.191993	35693.543618	31.549722
585.118275	35744.258486	31.554740
585.683076	35791.125980	31.559757
586.334358	35840.376184	31.564775
587.453374	35875.181768	31.569792
587.833224	35931.762293	31.574810
588.266028	35970.494208	31.579828
588.410312	36018.961728	31.584845
588.668854	36068.489564	31.589863
589.751771	36118.493237	31.594880
589.748329	36189.432057	31.599898
590.399897	36233.341916	31.604916
591.102117	36288.836488	31.609933
591.477476	36351.003425	31.614951
592.430332	36401.684522	31.619968
593.002472	36448.599983	31.624986
593.741049	36507.710952	31.630004
594.444410	36565.211705	31.635021
594.943299	36619.357060	31.640039
595.621179	36668.531360	31.645056
595.839713	36732.375411	31.650074
596.514019	36780.178938	31.655092
596.927353	36840.426023	31.660109
597.087887	36906.911388	31.665127
598.002334	36964.583278	31.670144
598.319342	37026.244860	31.675162
598.840526	37079.990828	31.680180
599.389717	37143.810580	31.685197
599.796326	37193.879443	31.690215
600.585910	37259.160767	31.695232
600.937152	37325.792421	31.700250
601.519895	37381.413688	31.705268
602.138912	37454.350971	31.710285
602.393563	37525.265344	31.715303
603.464014	37583.217236	31.720320
604.093855	37641.622639	31.725338
605.040105	37701.839963	31.730356
605.417509	37762.830817	31.735373
605.721393	37822.170145	31.740391
606.603951	37888.719406	31.745408
606.977495	37962.360205	31.750426
607.970383	38029.166802	31.755444
608.455884	38091.945433	31.760461
608.890963	38158.228014	31.765479
609.786309	38216.556855	31.770496
610.375293	38286.260671	31.775514
611.109798	38346.138740	31.780532
611.710728	38404.548229	31.785549
612.488039	38469.389953	31.790567
613.333520	38526.087939	31.795584
613.733444	38585.737890	31.800602
614.386902	38647.979373	31.805620
615.085458	38716.029201	31.810637
615.396082	38770.755435	31.815655
616.413547	38833.786384	31.820672
616.883601	38898.398005	31.825690
617.461152	38958.293771	31.830708
618.023409	39019.125676	31.835725
618.541145	39088.109322	31.840743
619.434064	39137.863656	31.845760
620.043108	39214.312302	31.850778
620.661863	39273.582911	31.855796
621.397670	39318.606960	31.860813
621.580391	39386.749504	31.865831
622.308607	39451.315806	31.870848
622.978560	39523.850200	31.875866
623.760221	39580.355298	31.880884
624.529401	39648.982644	31.885901
624.417847	39716.932103	31.890919
625.613714	39762.462791	31.895936
625.961341	39840.867098	31.900954
626.836806	39902.319320	31.905972
627.224674	39970.420488	31.910989
627.932366	40038.950387	31.916007
628.531532	40107.571959	31.921024
629.228602	40167.492370	31.926042
630.139757	40226.186720	31.931060
630.765106	40290.370458	31.936077
631.154868	40353.768775	31.941095
632.588013	40409.368625	31.946112
633.403573	40462.796154	31.951130
633.911961	40504.029073	31.956148
634.670634	40543.566402	31.961165
634.613944	40596.347908	31.966183
635.507790	40644.253535	31.971200
636.021026	40699.161857	31.976218
636.494990	40751.168612	31.981236
637.230321	40805.089397	31.986253
637.765884	40852.131687	31.991271
638.890510	40891.482233	31.996288
639.489805	40936.508640	32.001306
640.183658	40982.860581	32.006324
641.115110	41020.807093	32.011341
641.224121	41080.808578	32.016359
641.699274	41133.516508	32.021376
642.311463	41190.542807	32.026394
642.960514	41239.917888	32.031412
643.335535	41294.197228	32.036429
643.671586	41372.921075	32.041447
644.326835	41424.039930	32.046464
645.084114	41487.412306	32.051482
645.381506	41561.071307	32.056500
646.095438	41616.597212	32.061517
646.521496	41688.107205	32.066535
647.365901	41760.998655	32.071552
647.830344	41839.858749	32.076570
648.705137	41902.561023	32.081588
649.506069	41982.021112	32.086605
649.718873	42053.475107	32.091623
650.506436	42117.977361	32.096640
651.291910	42199.248304	32.101658
651.859405	42267.211701	32.106676
652.737250	42331.514276	32.111693
653.366218	42399.042574	32.116711
654.351624	42464.770039	32.121728
655.201493	42532.553884	32.126746
655.779755	42594.738117	32.131764
656.449216	42655.936509	32.136781
656.750277	42730.880592	32.141799
657.621737	42795.640145	32.146816
657.935609	42862.920765	32.151834
658.225800	42940.744296	32.156852
658.881681	43006.472671	32.161869
659.834399	43097.692344	32.166887
660.262178	43162.344115	32.171904
660.931174	43244.679494	32.176922
661.598690	43328.028088	32.181940
662.494035	43403.618603	32.186957
662.942155	43483.816841	32.191975
663.542983	43552.038652	32.196992
664.066950	43629.802817	32.202010
664.611746	43711.239063	32.207028
665.798741	43775.731224	32.212045
666.334872	43865.365126	32.217063
666.809017	43942.618119	32.222080
667.531430	44018.238849	32.227098
668.222300	44091.596759	32.232116
669.035409	44151.566191	32.237133
669.619786	44230.544267	32.242151
670.205319	44313.336500	32.247168
670.872561	44376.165971	32.252186
671.336764	44445.025049	32.257204
672.004651	44518.009855	32.262221
672.759199	44593.814098	32.267239
673.508710	44673.550259	32.272256
674.290763	44751.578044	32.277274
674.816769	44834.978479	32.282292
675.730858	44898.385707	32.287309
676.400117	44973.656254	32.292327
677.107179	45041.100379	32.297344
677.963827	45104.416549	32.302362
678.636718	45176.674558	32.307380
679.301135	45237.053137	32.312397
679.559266	45322.126441	32.317415
680.533619	45393.791561	32.322432
681.330025	45467.447635	32.327450
682.113262	45553.646771	32.332468
682.362537	45626.806977	32.337485
683.034193	45704.683080	32.342503
683.903956	45777.240335	32.347520
684.531233	45854.994821	32.352538
684.938889	45944.710337	32.357556
685.966479	46018.606403	32.362573
686.751693	46098.766148	32.367591
687.447356	46179.246551	32.372608
688.537975	46249.158261	32.377626
688.947602	46329.110683	32.382644
690.093666	46390.448247	32.387661
690.536204	46469.376992	32.392679
691.497188	46526.813312	32.397696
692.700429	46597.367887	32.402714
693.013566	46664.054356	32.407732
693.847220	46730.850664	32.412749
694.313262	46796.440557	32.417767
695.823518	46847.562298	32.422784
696.700587	46903.621809	32.427802
697.365547	46954.054958	32.432820
698.153604	47007.144214	32.437837
698.476536	47060.866147	32.442855
698.823167	47122.573345	32.447872
699.640647	47178.696857	32.452890
700.008253	47245.102354	32.457908
700.652536	47313.290910	32.462925
701.517327	47382.441668	32.467943
702.102271	47446.582587	32.472960
703.009652	47513.657254	32.477978
702.851011	47585.505404	32.482996
703.791472	47653.159055	32.488013
704.303301	47734.748630	32.493031
704.528776	47816.226408	32.498048
705.766472	47890.406111	32.503066
706.141998	47960.914929	32.508084
706.644159	48033.057257	32.513101
707.280247	48107.532439	32.518119
708.045437	48184.855597	32.523136
708.493697	48268.199507	32.528154
709.417302	48350.332191	32.533172
710.174018	48420.113207	32.538189
710.994193	48495.141304	32.543207
711.409396	48582.221646	32.548224
711.922970	48648.233673	32.553242
712.763082	48743.151524	32.558260
713.568895	48821.420783	32.563277
714.224500	48904.712582	32.568295
714.767254	48990.212654	32.573312
715.946783	49071.686301	32.578330
716.397224	49148.063471	32.583348
717.412292	49230.198290	32.588365
718.089170	49312.204308	32.593383
718.625473	49400.086664	32.598400
719.503735	49474.986586	32.603418
720.011765	49563.672612	32.608436
720.593307	49644.852794	32.613453
721.249277	49737.542694	32.618471
722.118865	49822.524539	32.623488
722.978893	49913.961634	32.628506
723.515687	50007.315663	32.633524
724.736344	50085.341406	32.638541
725.355141	50171.939532	32.643559
726.077857	50273.599572	32.648576
727.052444	50339.901071	32.653594
727.603384	50434.728808	32.658612
728.415619	50513.929115	32.663629
729.217382	50601.582620	32.668647
729.929807	50691.664961	32.673664
730.710286	50768.918015	32.678682
731.292723	50858.097235	32.683700
731.898708	50935.716460	32.688717
732.803502	51021.884997	32.693735
733.320009	51116.365210	32.698752
734.231770	51205.597873	32.703770
734.989161	51290.049115	32.708788
735.674694	51378.879983	32.713805
736.401440	51460.925787	32.718823
736.884694	51559.437436	32.723840
737.554920	51641.177465	32.728858
738.422051	51737.479765	32.733876
739.321157	51816.880290	32.738893
739.789834	51905.341157	32.743911
740.417986	52005.094580	32.748928
741.142654	52096.517015	32.753946
742.153990	52193.275358	32.758964
742.927623	52284.113389	32.763981
743.647446	52377.333826	32.768999
744.301206	52469.239695	32.774016
745.277856	52560.463404	32.779034
745.651102	52641.425184	32.784052
746.495849	52728.441515	32.789069
747.067469	52810.010013	32.794087
747.774424	52904.832239	32.799104
748.801790	52978.006088	32.804122
749.876343	53052.671920	32.809140
750.661814	53138.636019	32.814157
751.309527	53210.075352	32.819175
751.962850	53289.101700	32.824192
752.592532	53370.556167	32.829210
752.809135	53471.200665	32.834228
754.024472	53553.395981	32.839245
755.096373	53640.806636	32.844263
755.463162	53732.218555	32.849280
756.612010	53816.859179	32.854298
757.056353	53908.900377	32.859316
757.809692	53995.997317	32.864333
758.674818	54077.003987	32.869351
759.313087	54166.531541	32.874368
760.095968	54255.275818	32.879386
760.920875	54344.054871	32.884404
761.854671	54428.666292	32.889421
762.998245	54518.913722	32.894439
763.285585	54611.374864	32.899456
764.030688	54686.888985	32.904474
765.308113	54791.456411	32.909492
765.862197	54868.807216	32.914509
766.918290	54956.204613	32.919527
767.255342	55050.055252	32.924544
768.092076	55133.359640	32.929562
768.765344	55223.745398	32.934580
769.189154	55313.568400	32.939597
770.240205	55393.184513	32.944615
770.932213	55496.018325	32.949632
771.657046	55589.945736	32.954650
772.675730	55682.759901	32.959668
772.851314	55783.149040	32.964685
773.921216	55876.312737	32.969703
774.419643	55981.146705	32.974720
775.886344	56068.168380	32.979738
776.605560	56172.507413	32.984756
777.464189	56254.901116	32.989773
778.285777	56340.849301	32.994791
778.675790	56445.438006	32.999808
779.428846	56542.449986	33.004826
780.219353	56638.395822	33.009844
780.805305	56734.374719	33.014861
781.705888	56833.662934	33.019879
782.237782	56937.947730	33.024896
783.045851	57038.243032	33.029914
783.859530	57155.408543	33.034932
784.367071	57252.068722	33.039949
785.566185	57348.799271	33.044967
786.263450	57456.176579	33.049984
787.316121	57551.501393	33.055002
787.727142	57633.587355	33.060020
788.376561	57731.202967	33.065037
789.112553	57821.376820	33.070055
790.152650	57925.273744	33.075072
790.946858	58004.585295	33.080090
791.618364	58114.540369	33.085108
791.965879	58204.408542	33.090125
793.112302	58296.953500	33.095143
793.536852	58409.920473	33.100160
794.421163	58500.601261	33.105178
795.194338	58610.587288	33.110196
796.072944	58716.736994	33.115213
796.930089	58813.343349	33.120231
797.777345	58913.806741	33.125248
798.527063	59025.958493	33.130266
799.448136	59124.718995	33.135284
800.170380	59226.545804	33.140301
801.302471	59321.125109	33.145319
801.903117	59429.646882	33.150336
802.355152	59531.338396	33.155354
803.758678	59635.389099	33.160372
803.943280	59751.900727	33.165389
805.001166	59846.361896	33.170407
805.472936	59965.809708	33.175424
806.563935	60073.227857	33.180442
807.287071	60182.432289	33.185460
808.489157	60295.419527	33.190477
810.085027	60378.525666	33.195495
810.691355	60467.990963	33.200512
811.883398	60558.503316	33.205530
812.799183	60652.435454	33.210548
813.813615	60750.359261	33.215565
814.689089	60824.955688	33.220583
815.117256	60927.618470	33.225600
815.973085	61014.669022	33.230618
817.045894	61098.433130	33.235636
817.391460	61203.750306	33.240653
818.408190	61285.875907	33.245671
819.349093	61388.851141	33.250688
819.582999	61489.489129	33.255706
820.312026	61589.268905	33.260724
820.922519	61691.066888	33.265741
821.820127	61790.369348	33.270759
822.348439	61910.265746	33.275776
823.162365	61999.004264	33.280794
824.331897	62120.094607	33.285812
825.088029	62223.403790	33.290829
825.898360	62317.001027	33.295847
826.938805	62422.707016	33.300864
827.972117	62528.095792	33.305882
828.753724	62633.064170	33.310900
829.262162	62732.998773	33.315917
830.295644	62840.015553	33.320935
830.513717	62946.117452	33.325952
831.517558	63042.368524	33.330970
832.822169	63137.138518	33.335988
833.441331	63235.182334	33.341005
834.992061	63320.332885	33.346023
835.606823	63408.970756	33.351040
836.404231	63496.263091	33.356058
836.834900	63586.598504	33.361076
837.863506	63676.346530	33.366093
838.519710	63765.339478	33.371111
839.206798	63877.476391	33.376128
839.742998	63967.597856	33.381146
841.002760	64065.471358	33.386164
841.428629	64174.863010	33.391181
842.233718	64269.762362	33.396199
843.359552	64370.696848	33.401216
843.929896	64486.475132	33.406234
844.717087	64592.426134	33.411252
845.176550	64699.213111	33.416269
846.380526	64803.715667	33.421287
847.112615	64920.768855	33.426304
847.985012	65027.002415	33.431322
849.252169	65138.555402	33.436340
849.560639	65252.579786	33.441357
850.528856	65374.575600	33.446375
851.306205	65486.221195	33.451392
852.093848	65590.942742	33.456410
853.414623	65702.402040	33.461428
854.048850	65836.585154	33.466445
855.037033	65933.336512	33.471463
855.846039	66050.908633	33.476480
856.831218	66166.469944	33.481498
857.517067	66273.220159	33.486516
858.317298	66389.879795	33.491533
859.460721	66499.053621	33.496551
860.200182	66620.534683	33.501568
860.834075	66743.520970	33.506586
861.971407	66852.056581	33.511604
863.195401	66970.427379	33.516621
864.239939	67069.181145	33.521639
865.236927	67183.666431	33.526656
865.932224	67294.125802	33.531674
866.885705	67399.036074	33.536692
867.503827	67517.500318	33.541709
868.467709	67615.334745	33.546727
869.631805	67720.567008	33.551744
870.287031	67830.498833	33.556762
871.336338	67932.023251	33.561780
871.969287	68046.628416	33.566797
872.965632	68152.900509	33.571815
874.032868	68257.626742	33.576832
874.515165	68368.997935	33.581850
875.542421	68474.894130	33.586868
876.302455	68593.215985	33.591885
876.869848	68700.715455	33.596903
877.950539	68809.871200	33.601920
878.694205	68927.635409	33.606938
879.695256	69028.099200	33.611956
880.237480	69141.569080	33.616973
881.481115	69236.650471	33.621991
882.098517	69342.705043	33.627008
882.858812	69450.171615	33.632026
883.850381	69550.197342	33.637044
884.747649	69664.346629	33.642061
885.629368	69764.921643	33.647079
886.904849	69868.789394	33.652096
887.610040	69979.312932	33.657114
888.656313	70072.041551	33.662132
889.598262	70184.790452	33.667149
890.527150	70292.575987	33.672167
891.324775	70393.091781	33.677184
891.793942	70496.610977	33.682202
893.141713	70607.440156	33.687220
893.493600	70719.647871	33.692237
894.257954	70834.077831	33.697255
895.339926	70944.003446	33.702272
896.044369	71071.213783	33.707290
896.933513	71184.191630	33.712308
897.439996	71316.028568	33.717325
898.598262	71439.182076	33.722343
899.571531	71560.318568	33.727360
899.836406	71696.044500	33.732378
900.951173	71821.987508	33.737396
901.501343	71954.529431	33.742413
902.494026	72085.295758	33.747431
903.203226	72218.370184	33.752448
904.420646	72354.764164	33.757466
906.236230	72472.770743	33.762484
907.041692	72601.819932	33.767501
907.792795	72716.648318	33.772519
909.226259	72839.703535	33.777536
910.166775	72967.874222	33.782554
911.260526	73086.176234	33.787572
911.743386	73213.656715	33.792589
912.715589	73332.857886	33.797607
913.447831	73453.406023	33.802624
914.251892	73590.228106	33.807642
914.954486	73706.175765	33.812660
916.217430	73838.174436	33.817677
917.043943	73970.110717	33.822695
918.267978	74088.644382	33.827712
918.817481	74226.042138	33.832730
919.925780	74336.045495	33.837748
920.811403	74463.299209	33.842765
921.862755	74592.732878	33.847783
922.906651	74700.656710	33.852800
923.902575	74835.453444	33.857818
925.226539	74959.360665	33.862836
925.640443	75080.563271	33.867853
926.508809	75197.491668	33.872871
927.426775	75324.739358	33.877888
928.478900	75444.420647	33.882906
929.263715	75558.539474	33.887924
930.199241	75679.030686	33.892941
930.826504	75789.737870	33.897959
931.988407	75913.442897	33.902976
932.513861	76028.547316	33.907994
933.692145	76136.128801	33.913012
934.533101	76258.136353	33.918029
935.250169	76383.305441	33.923047
936.627549	76508.837928	33.928064
937.086350	76635.162007	33.933082
938.099736	76754.212539	33.938100
938.916897	76883.211474	33.943117
939.732204	77012.552816	33.948135
940.822208	77140.656728	33.953152
941.751106	77273.805461	33.958170
942.523263	77402.903330	33.963188
943.388369	77537.346977	33.968205
944.138084	77678.787704	33.973223
945.405473	77799.561027	33.978240
946.539283	77938.174039	33.983258
948.157664	78042.503683	33.988276
949.477892	78168.757077	33.993293
950.198970	78294.803186	33.998311
951.478217	78411.330729	34.003328
952.322834	78532.940455	34.008346
953.074067	78648.630524	34.013364
953.844061	78778.641285	34.018381
954.629304	78905.995672	34.023399
955.864227	79025.333903	34.028416
956.226924	79171.030943	34.033434
957.345928	79287.013741	34.038452
958.474591	79427.401185	34.043469
958.954776	79556.773973	34.048487
960.087050	79685.519169	34.053504
961.144968	79828.449045	34.058522
962.090125	79961.985573	34.063540
963.060643	80096.751571	34.068557
964.051792	80234.340780	34.073575
965.327506	80366.354464	34.078592
965.851973	80514.165515	34.083610
966.735588	80640.648914	34.088628
967.948593	80784.711212	34.093645
968.866983	80927.911086	34.098663
969.878756	81072.734368	34.103680
970.222505	81211.905975	34.108698
971.504466	81346.946617	34.113716
972.398493	81488.693928	34.118733
973.088098	81628.571890	34.123751
974.263464	81781.440576	34.128768
975.420819	81933.737963	34.133786
976.764141	82066.339606	34.138804
977.879316	82202.664047	34.143821
978.788903	82337.637583	34.148839
980.047899	82476.634068	34.153856
980.933257	82606.214229	34.158874
982.528126	82725.788312	34.163892
983.274205	82840.288722	34.168909
983.858758	82961.624369	34.173927
984.936676	83074.574922	34.178944
985.658854	83196.813065	34.183962
986.680564	83328.038720	34.188980
987.497764	83450.680487	34.193997
988.208652	83588.810547	34.199015
989.459274	83714.621914	34.204032
990.222082	83849.072139	34.209050
990.847001	83984.272235	34.214068
991.979472	84117.514678	34.219085
992.896901	84272.990479	34.224103
994.010385	84405.908990	34.229120
994.812179	84542.677795	34.234138
995.900953	84688.278798	34.239156
997.000595	84831.678782	34.244173
997.703031	84972.171249	34.249191
998.508358	85120.975347	34.254208
998.935250	85287.987141	34.259226
1000.157848	85439.079165	34.264244
1001.365196	85604.002870	34.269261
1001.982633	85767.365084	34.274279
1003.329921	85922.911029	34.279296
1004.196169	86087.911706	34.284314
1004.961637	86250.703960	34.289332
1006.457294	86405.199149	34.294349
1007.196047	86579.367158	34.299367
1008.180033	86737.670502	34.304384
1008.849487	86917.707598	34.309402
1009.972724	87080.695847	34.314420
1010.710717	87253.573160	34.319437
1011.758586	87433.491142	34.324455
1013.138127	87596.113704	34.329472
1014.490243	87750.736262	34.334490
1015.320963	87921.359326	34.339508
1017.498947	88063.515442	34.344525
1018.289111	88228.690099	34.349543
1019.871784	88378.019179	34.354560
1021.214605	88527.627750	34.359578
1022.929691	88657.353019	34.364596
1024.056567	88785.281809	34.369613
1025.387246	88918.649086	34.374631
1026.769187	89035.724957	34.379648
1027.654117	89162.771172	34.384666
1028.586665	89287.091241	34.389684
1029.780687	89401.991912	34.394701
1030.493874	89526.500021	34.399719
1031.645016	89639.460959	34.404736
1032.366351	89777.673502	34.409754
1033.223125	89909.016307	34.414772
1034.218388	90030.111644	34.419789
1034.622876	90164.354846	34.424807
1035.900539	90300.129585	34.429824
1036.740651	90433.204719	34.434842
1037.249557	90560.489646	34.439860
1038.457391	90699.218792	34.444877
1039.178310	90841.846226	34.449895
1039.885401	90961.424096	34.454912
1040.591032	91106.775203	34.459930
1041.673770	91259.062238	34.464948
1042.682889	91397.700917	34.469965
1043.358168	91557.454604	34.474983
1044.531960	91710.666326	34.480000
1045.532318	91866.955219	34.485018
1046.068665	92019.669635	34.490036
1047.651784	92173.211597	34.495053
1048.545328	92346.332233	34.500071
1049.772384	92494.544282	34.505088
1050.751190	92658.141139	34.510106
1051.858307	92824.463843	34.515124
1053.236082	92968.145364	34.520141
1053.730126	93141.000524	34.525159
1054.950994	93309.826156	34.530176
1056.292962	93461.321783	34.535194
1056.866115	93640.177158	34.540212
1058.021420	93807.347131	34.545229
1058.684836	93986.456585	34.550247
1060.202275	94149.257644	34.555264
1061.129545	94316.682764	34.560282
1061.937921	94478.903211	34.565300
1063.518571	94649.522465	34.570317
1064.402386	94833.233917	34.575335
1065.773379	95002.908745	34.580352
1066.979917	95166.981175	34.585370
1068.156902	95349.808908	34.590388
1069.386704	95508.427366	34.595405
1070.276535	95675.653501	34.600423
1071.819143	95838.981538	34.605440
1072.590698	96011.846333	34.610458
1073.313776	96170.132532	34.615476
1074.879726	96334.112012	34.620493
1075.621197	96513.532825	34.625511
1076.392387	96682.651462	34.630528
1078.132332	96850.908750	34.635546
1079.620177	97003.739880	34.640564
1081.364879	97150.597197	34.645581
1082.022977	97308.218445	34.650599
1083.427240	97462.514671	34.655616
1084.586269	97625.676201	34.660634
1085.560580	97778.549934	34.665652
1086.843397	97929.041171	34.670669
1087.736938	98082.790183	34.675687
1088.317301	98231.756581	34.680704
1089.675935	98388.951222	34.685722
1090.575462	98554.748225	34.690740
1091.765065	98698.977037	34.695757
1092.640119	98865.912651	34.700775
1093.806412	99020.687461	34.705792
1095.011412	99179.462007	34.710810
1095.741025	99329.923896	34.715828
1097.248877	99470.133694	34.720845
1098.014578	99620.509492	34.725863
1099.376673	99769.526031	34.730880
1100.586962	99912.930338	34.735898
1101.364703	100056.878856	34.740916
1102.680697	100193.947409	34.745933
1103.570283	100351.394564	34.750951
1104.606829	100498.892136	34.755968
1105.767592	100644.858696	34.760986
1106.836290	100797.003527	34.766004
1107.801445	100942.946127	34.771021
1108.571158	101109.674274	34.776039
1109.825969	101276.307484	34.781056
1110.985983	101429.068336	34.786074
1111.931242	101597.145098	34.791092
1113.217464	101754.690538	34.796109
1113.886987	101921.332856	34.801127
1115.069877	102089.109611	34.806144
1116.504377	102253.373694	34.811162
1117.079764	102434.297080	34.816180
1118.373788	102604.913632	34.821197
1119.209048	102787.797970	34.826215
1120.645765	102965.525834	34.831232
1121.354785	103141.238284	34.836250
1122.514006	103327.625223	34.841268
1123.573499	103510.074526	34.846285
1125.058743	103693.128300	34.851303
1126.245803	103872.124010	34.856320
1127.527627	104045.252518	34.861338
1128.235396	104229.130176	34.866356
1129.624544	104405.288085	34.871373
1131.147842	104587.861789	34.876391
1131.994814	104767.411950	34.881408
1133.248036	104942.412073	34.886426
1134.423325	105123.861840	34.891444
1135.713016	105303.193757	34.896461
1136.815477	105477.171266	34.901479
1138.319462	105645.105738	34.906496
1139.703217	105814.724923	34.911514
1140.538782	105993.665931	34.916532
1142.408147	106152.704797	34.921549
1143.270549	106322.650979	34.926567
1144.264338	106494.520395	34.931584
1145.724482	106664.506847	34.936602
1146.515267	106843.125884	34.941620
1147.670138	107011.669729	34.946637
1149.015078	107178.228891	34.951655
1149.595060	107348.733545	34.956672
1150.819220	107516.561057	34.961690
1151.720879	107703.428193	34.966708
1152.949360	107880.251138	34.971725
1154.243611	108063.526982	34.976743
1155.271293	108241.264246	34.981760
1156.360458	108422.638680	34.986778
1157.441676	108601.180207	34.991796
1158.703806	108753.168024	34.996813
1160.274391	108913.051106	35.001831
1161.168761	109079.435479	35.006848
1162.393135	109230.368935	35.011866
1163.173059	109403.907018	35.016884
1164.300000	109565.384002	35.021901
1165.551289	109730.804600	35.026919
1166.979032	109895.679228	35.031936
1168.282059	110071.474495	35.036954
1168.750074	110248.606446	35.041972
1169.988105	110413.710942	35.046989
1171.077846	110598.766363	35.052007
1172.734725	110776.434667	35.057024
1174.075928	110936.677598	35.062042
1175.328040	111125.825590	35.067060
1176.163516	111302.197726	35.072077
1177.271788	111467.950254	35.077095
1178.623320	111660.397133	35.082112
1179.977254	111832.474772	35.087130
1180.977350	112015.124282	35.092148
1182.468738	112194.918049	35.097165
1183.796979	112362.553304	35.102183
1184.489879	112536.000645	35.107200
1185.806788	112714.015439	35.112218
1186.871949	112907.372101	35.117236
1188.261351	113077.977729	35.122253
1190.441378	113242.767703	35.127271
1191.537931	113417.169857	35.132288
1193.089809	113583.081168	35.137306
1194.293570	113750.846822	35.142324
1195.446856	113902.643058	35.147341
1196.238729	114076.420858	35.152359
1197.373857	114240.244008	35.157376
1198.589831	114410.050615	35.162394
1199.607228	114584.726685	35.167412
1200.926243	114767.250597	35.172429
1202.263110	114938.883822	35.177447
1203.355436	115113.652929	35.182464
1204.398533	115285.449170	35.187482
1205.636680	115458.386804	35.192500
1206.430394	115634.447862	35.197517
1207.464611	115817.258869	35.202535
1208.793481	115999.258267	35.207552
1209.855773	116191.076755	35.212570
1210.721434	116395.957702	35.217588
1211.781427	116591.287086	35.222605
1212.952535	116782.750823	35.227623
1213.822777	116981.969161	35.232640
1215.098347	117163.529463	35.237658
1216.096962	117384.263822	35.242676
1217.280276	117597.645084	35.247693
1218.385557	117810.103441	35.252711
1219.473167	118012.733272	35.257728
1221.162603	118204.777352	35.262746
1222.646273	118398.267559	35.267764
1223.782340	118595.816184	35.272781
1224.971746	118782.707648	35.277799
1226.213235	118972.637823	35.282816
1227.635462	119153.175699	35.287834
1228.816407	119355.427610	35.292852
1229.845410	119535.270816	35.297869
1231.254218	119731.239693	35.302887
1232.235607	119929.874171	35.307904
1233.929438	120116.150448	35.312922
1234.940558	120311.363719	35.317940
1235.931842	120504.985865	35.322957
1237.235753	120698.597730	35.327975
1238.593098	120898.180285	35.332992
1239.484908	121100.409328	35.338010
1240.761755	121306.530170	35.343028
1242.177042	121509.641665	35.348045
1243.786877	121694.891294	35.353063
1245.421081	121898.502912	35.358080
1246.551150	122099.270557	35.363098
1247.653187	122296.586520	35.368116
1248.725554	122496.657082	35.373133
1250.423379	122688.409741	35.378151
1251.500185	122889.242486	35.383168
1252.800071	123095.424240	35.388186
1253.910225	123292.948952	35.393204
1255.198517	123494.385923	35.398221
1256.342649	123690.755568	35.403239
1257.137847	123909.816568	35.408256
1258.667216	124109.256580	35.413274
1260.038724	124329.356681	35.418292
1261.397714	124535.540120	35.423309
1262.900546	124741.119608	35.428327
1263.819390	124955.457499	35.433344
1265.464518	125160.320892	35.438362
1266.952793	125357.610659	35.443380
1268.911624	125547.961575	35.448397
1270.587304	125743.273651	35.453415
1271.218945	125943.921290	35.458432
1273.045652	126126.544988	35.463450
1274.381364	126315.442274	35.468468
1275.535759	126512.071466	35.473485
1277.588509	126667.757335	35.478503
1279.008620	126848.081690	35.483520
1280.611733	127018.180702	35.488538
1281.652128	127198.846417	35.493556
1282.748782	127381.847920	35.498573
1284.096754	127550.470658	35.503591
1284.833173	127743.387437	35.508608
1285.899283	127916.199645	35.513626
1287.457019	128095.572881	35.518644
1288.450425	128284.183434	35.523661
1289.675161	128472.568477	35.528679
1290.318728	128667.115340	35.533696
1291.625644	128855.844641	35.538714
1292.970479	129042.415545	35.543732
1293.823179	129232.511800	35.548749
1295.225098	129402.809520	35.553767
1296.371317	129591.024602	35.558784
1297.892291	129761.090218	35.563802
1299.623850	129933.213775	35.568820
1300.922086	130121.585636	35.573837
1301.957815	130305.249570	35.578855
1303.122090	130487.323291	35.583872
1304.505976	130668.337073	35.588890
1305.587101	130879.540597	35.593908
1306.711236	131075.902912	35.598925
1308.138430	131265.896312	35.603943
1309.138465	131467.716321	35.608960
1310.222898	131669.004897	35.613978
1311.457121	131867.585090	35.618996
1312.508714	132088.849522	35.624013
1313.965659	132295.987524	35.629031
1314.915441	132513.774523	35.634048
1316.512222	132730.218665	35.639066
1317.730063	132949.372778	35.644084
1319.122158	133172.872164	35.649101
1320.578688	133385.732503	35.654119
1321.465834	133618.995896	35.659136
1322.930938	133840.030785	35.664154
1324.515091	134051.545354	35.669172
1326.006006	134278.876899	35.674189
1327.674861	134495.056824	35.679207
1328.989233	134720.329195	35.684224
1330.535226	134928.903901	35.689242
1331.741219	135146.353355	35.694260
1333.042142	135364.739703	35.699277
1334.665422	135582.404868	35.704295
1335.681765	135811.433146	35.709312
1337.035359	136027.117049	35.714330
1338.449642	136241.576411	35.719348
1339.532740	136465.188369	35.724365
1341.284321	136685.540471	35.729383
1342.675295	136903.708593	35.734400
1343.934653	137124.991253	35.739418
1345.420064	137347.988416	35.744436
1346.616306	137577.344042	35.749453
1348.300146	137788.654462	35.754471
1349.279707	138016.438536	35.759488
1350.768646	138236.679236	35.764506
1351.907820	138457.522087	35.769524
1352.876572	138688.063008	35.774541
1354.680905	138915.152611	35.779559
1355.362081	139158.314387	35.784576
1356.417157	139391.077465	35.789594
1357.846759	139626.178062	35.794612
1359.316176	139876.786291	35.799629
1360.839643	140109.531195	35.804647
1362.173649	140351.610359	35.809664
1363.260181	140584.035493	35.814682
1364.923179	140804.292767	35.819700
1366.203007	141034.079860	35.824717
1367.688633	141257.182201	35.829735
1369.467962	141475.271307	35.834752
1371.013530	141695.857898	35.839770
1372.308807	141907.309779	35.844788
1373.500537	142120.313165	35.849805
1375.055263	142322.132289	35.854823
1376.451454	142547.298856	35.859840
1377.676648	142771.809829	35.864858
1379.338972	142985.935850	35.869876
1380.577486	143202.741700	35.874893
1381.502961	143426.519253	35.879911
1383.515411	143653.408474	35.884928
1385.514100	143852.720843	35.889946
1387.613206	144044.743071	35.894964
1388.689421	144258.983745	35.899981
1390.384843	144454.266793	35.904999
1391.858306	144658.344960	35.910016
1392.899236	144876.385402	35.915034
1394.588948	145077.301130	35.920052
1396.213802	145276.453884	35.925069
1397.451980	145475.390491	35.930087
1398.736418	145684.436212	35.935104
1400.066119	145880.242621	35.940122
1401.610757	146085.434253	35.945140
1402.583067	146299.426544	35.950157
1403.837968	146510.421864	35.955175
1405.196370	146728.095132	35.960192
1406.051556	146958.602124	35.965210
1407.512062	147175.146730	35.970228
1408.670210	147408.499038	35.975245
1409.792398	147644.761683	35.980263
1410.833681	147881.786852	35.985280
1412.434767	148122.882767	35.990298
1413.782993	148365.453154	35.995316
1414.660149	148621.208108	36.000333
1416.304450	148858.448917	36.005351
1417.376274	149117.675721	36.010368
1418.635507	149369.598135	36.015386
1419.979828	149621.306154	36.020404
1422.029872	149879.863853	36.025421
1424.150664	150120.803386	36.030439
1425.661348	150374.810786	36.035456
1427.200081	150615.567566	36.040474
1428.796782	150861.781016	36.045492
1430.201206	151104.667246	36.050509
1431.787350	151318.443246	36.055527
1433.838953	151548.209706	36.060544
1434.921132	151793.244102	36.065562
1436.577515	152026.905488	36.070580
1437.863818	152258.649521	36.075597
1439.598707	152487.826259	36.080615
1441.344721	152707.646118	36.085632
1442.497900	152922.933968	36.090650
1444.210746	153130.894794	36.095668
1445.314792	153343.568697	36.100685
1446.354683	153547.759372	36.105703
1448.035853	153755.919307	36.110720
1448.991605	153975.708266	36.115738
1450.664712	154186.192397	36.120756
1451.877979	154405.093753	36.125773
1453.379854	154633.193791	36.130791
1454.568135	154866.987470	36.135808
1456.227435	155089.182395	36.140826
1457.266885	155312.846644	36.145844
1458.668429	155555.017646	36.150861
1460.122272	155787.000335	36.155879
1461.504114	156016.168473	36.160896
1462.585266	156266.269522	36.165914
1463.963391	156509.820436	36.170932
1465.617420	156758.236388	36.175949
1467.356668	156994.480423	36.180967
1469.155728	157240.264723	36.185984
1470.468598	157484.542992	36.191002
1472.064821	157728.017148	36.196020
1472.839044	157981.856708	36.201037
1474.718675	158239.402727	36.206055
1477.129335	158458.000258	36.211072
1478.888190	158682.827484	36.216090
1480.982326	158903.468965	36.221108
1482.123785	159147.063337	36.226125
1483.528482	159373.713907	36.231143
1484.915974	159620.239806	36.236160
1485.880100	159855.802140	36.241178
1487.463687	160091.990454	36.246196
1488.598328	160336.684711	36.251213
1489.851122	160583.999606	36.256231
1491.546461	160823.865314	36.261248
1492.647771	161088.644765	36.266266
1494.200053	161343.792586	36.271284
1495.922716	161596.467587	36.276301
1497.565101	161842.676724	36.281319
1499.213731	162098.118970	36.286336
1500.585190	162353.049056	36.291354
1502.216764	162593.963982	36.296372
1503.741112	162853.058387	36.301389
1505.118799	163110.453158	36.306407
1506.768848	163358.307416	36.311424
1508.016542	163622.359318	36.316442
1509.513397	163877.191407	36.321460
1510.927265	164143.325968	36.326477
1512.202383	164399.490542	36.331495
1513.706194	164666.261419	36.336512
1514.846199	164946.776846	36.341530
1516.678258	165205.864385	36.346548
1518.119288	165474.528150	36.351565
1519.459418	165748.650959	36.356583
1521.369481	166010.978611	36.361600
1522.517338	166271.006679	36.366618
1524.514614	166527.565875	36.371636
1525.843255	166786.858533	36.376653
1527.153559	167029.159885	36.381671
1528.943880	167269.027379	36.386688
1529.973814	167527.408627	36.391706
1531.662798	167774.664688	36.396724
1533.064171	168027.168457	36.401741
1534.701710	168288.350296	36.406759
1536.592028	168544.255240	36.411776
1537.627683	168811.497795	36.416794
1538.943319	169065.835892	36.421812
1540.582733	169341.725688	36.426829
1542.081193	169612.185540	36.431847
1543.935453	169877.478903	36.436864
1545.394555	170146.033379	36.441882
1547.073450	170419.489150	36.446900
1548.597672	170687.757964	36.451917
1549.887404	170972.201042	36.456935
1551.593358	171241.472266	36.461952
1553.118328	171526.123013	36.466970
1554.511175	171798.783967	36.471988
1556.209402	172075.508315	36.477005
1557.584162	172361.317938	36.482023
1559.358169	172640.913772	36.487040
1560.736537	172928.781944	36.492058
1562.273106	173202.266964	36.497076
1563.923340	173485.288122	36.502093
1565.118213	173788.630117	36.507111
1566.849731	174079.875630	36.512128
1568.393295	174377.115508	36.517146
1570.013167	174666.442032	36.522164
1571.739982	174966.168964	36.527181
1573.431563	175252.722692	36.532199
1575.822644	175526.975761	36.537216
1577.006408	175820.578929	36.542234
1578.816579	176099.977302	36.547252
1581.057047	176383.495801	36.552269
1582.650111	176662.666057	36.557287
1584.634455	176927.275079	36.562304
1586.548821	177198.367194	36.567322
1588.169006	177458.343310	36.572340
1589.499115	177724.621812	36.577357
1591.283159	177989.738818	36.582375
1592.754069	178238.198248	36.587392
1594.294560	178513.227852	36.592410
1596.076290	178776.979967	36.597428
1597.647308	179045.664530	36.602445
1599.137180	179324.031543	36.607463
1600.864324	179583.445537	36.612480
1602.305844	179848.603224	36.617498
1603.698218	180109.811792	36.622516
1605.178546	180380.346197	36.627533
1606.792393	180659.032088	36.632551
1608.867454	180908.197786	36.637568
1609.910067	181178.997038	36.642586
1611.590413	181428.621749	36.647604
1613.423979	181692.675392	36.652621
1614.709442	181940.500592	36.657639
1616.220754	182178.622826	36.662656
1617.791522	182443.116076	36.667674
1618.974631	182698.536786	36.672692
1620.715821	182953.921094	36.677709
1622.508257	183218.865955	36.682727
1624.130668	183480.578409	36.687744
1625.308088	183738.493001	36.692762
1626.881223	184005.812112	36.697780
1628.503584	184286.993990	36.702797
1629.802919	184567.607171	36.707815
1631.500295	184836.066194	36.712832
1633.207473	185128.317420	36.717850
1635.045849	185403.025860	36.722868
1636.739041	185684.788897	36.727885
1638.222639	185966.574273	36.732903
1639.736052	186241.199789	36.737920
1641.879518	186542.019629	36.742938
1643.671759	186826.426075	36.747956
1645.453987	187112.967733	36.752973
1646.813059	187396.152123	36.757991
1648.526351	187684.459448	36.763008
1650.168949	187974.670583	36.768026
1651.629181	188257.869518	36.773044
1653.611189	188542.700463	36.778061
1655.283837	188831.084746	36.783079
1656.911221	189111.483122	36.788096
1658.465298	189404.585120	36.793114
1660.115128	189687.787894	36.798132
1662.131690	189967.190421	36.803149
1663.797756	190268.224174	36.808167
1665.246006	190563.608999	36.813184
1666.853523	190861.863822	36.818202
1668.226012	191157.492739	36.823220
1670.088107	191447.537871	36.828237
1671.369925	191751.674982	36.833255
1673.404369	192056.595529	36.838272
1674.617349	192359.199034	36.843290
1676.215868	192672.530674	36.848308
1678.222970	192976.649019	36.853325
1679.722344	193280.189904	36.858343
1681.431959	193597.228295	36.863360
1683.126667	193912.595785	36.868378
1684.566913	194226.711121	36.873396
1686.238068	194541.083653	36.878413
1687.481370	194857.137927	36.883431
1689.574346	195162.880413	36.888448
1691.488043	195485.520714	36.893466
1693.448770	195798.002007	36.898484
1695.759269	196103.880568	36.903501
1697.102856	196412.681357	36.908519
1699.465641	196719.811778	36.913536
1701.075883	197016.528930	36.918554
1702.822146	197283.500733	36.923572
1704.973935	197551.627974	36.928589
1706.601894	197830.336421	36.933607
1708.184512	198094.292136	36.938624
1709.911790	198369.002200	36.943642
1711.268227	198636.156977	36.948660
1713.375740	198908.042451	36.953677
1714.651143	199181.521100	36.958695
1716.459921	199457.505790	36.963712
1717.952180	199738.936636	36.968730
1719.638550	200020.388896	36.973748
1721.564564	200305.790179	36.978765
1723.073027	200594.546769	36.983783
1724.631971	200889.097647	36.988800
1725.881949	201188.205260	36.993818
1727.554261	201484.277202	36.998836
1729.391618	201779.575611	37.003853
1730.686366	202095.055470	37.008871
1732.097523	202395.578351	37.013888
1733.995747	202722.148917	37.018906
1735.422244	203046.854141	37.023924
1737.312198	203364.226824	37.028941
1738.839765	203687.916861	37.033959
1740.630482	204016.136748	37.038976
1742.237442	204346.114064	37.043994
1744.041833	204679.870129	37.049012
1745.954150	205009.066493	37.054029
1748.021914	205332.134142	37.059047
1750.270115	205653.600843	37.064064
1752.345079	205976.467794	37.069082
1754.704586	206291.458904	37.074100
1756.737842	206592.247627	37.079117
1758.376930	206910.656951	37.084135
1760.284490	207206.898704	37.089152
1762.311810	207521.187370	37.094170
1763.739688	207822.522686	37.099188
1765.925953	208123.586760	37.104205
1767.707554	208433.209405	37.109223
1769.067603	208737.060890	37.114240
1771.247943	209033.534831	37.119258
1772.947933	209341.638916	37.124276
1774.694312	209640.584017	37.129293
1776.807668	209950.809048	37.134311
1778.588349	210239.633544	37.139328
1780.711943	210527.592432	37.144346
1782.428192	210832.463979	37.149364
1784.240692	211116.844073	37.154381
1785.855300	211420.566598	37.159399
1787.509597	211715.308549	37.164416
1789.608303	212010.666859	37.169434
1790.920727	212317.869383	37.174452
1793.032606	212622.661226	37.179469
1793.987477	212921.785434	37.184487
1795.990746	213235.979513	37.189504
1797.725488	213530.005933	37.194522
1798.905393	213829.898368	37.199540
1800.778305	214113.532886	37.204557
1802.783301	214407.202877	37.209575
1804.139932	214696.914334	37.214592
1806.150164	214995.207421	37.219610
1807.968949	215288.072856	37.224628
1809.707654	215584.469113	37.229645
1811.296709	215884.419973	37.234663
1812.949639	216184.273124	37.239680
1814.779192	216482.182379	37.244698
1816.772857	216797.118187	37.249716
1819.079073	217093.748224	37.254733
1820.941871	217401.292760	37.259751
1822.844675	217704.388466	37.264768
1824.814557	218005.049754	37.269786
1826.494045	218308.602466	37.274804
1828.527736	218608.088056	37.279821
1830.260573	218919.443386	37.284839
1831.879901	219221.968342	37.289856
1833.872498	219530.847251	37.294874
1835.524625	219846.117297	37.299892
1837.188978	220153.501885	37.304909
1838.990150	220470.655484	37.309927
1840.719961	220797.433496	37.314944
1842.368118	221118.867668	37.319962
1844.176114	221451.997401	37.324980
1846.112271	221768.119247	37.329997
1848.104578	222127.696568	37.335015
1849.801241	222491.182509	37.340032
1851.939084	222809.981166	37.345050
1853.333619	223149.799244	37.350068
1855.287322	223485.098578	37.355085
1857.144895	223818.890873	37.360103
1859.250515	224162.384330	37.365120
1861.060629	224498.942397	37.370138
1862.788686	224827.629556	37.375156
1864.879329	225165.898165	37.380173
1866.811503	225501.044244	37.385191
1868.626726	225845.009933	37.390208
1871.157287	226171.276770	37.395226
1872.756545	226518.796868	37.400244
1874.762593	226847.638406	37.405261
1876.654913	227181.654725	37.410279
1878.382541	227511.965216	37.415296
1880.558234	227847.183582	37.420314
1882.810321	228180.257808	37.425332
1884.620050	228517.949525	37.430349
1886.660532	228837.345616	37.435367
1888.656794	229158.908617	37.440384
1891.044854	229477.108991	37.445402
1892.613392	229801.713637	37.450420
1894.577470	230124.148712	37.455437
1896.821274	230443.340482	37.460455
1898.570846	230757.075182	37.465472
1900.242218	231067.039144	37.470490
1901.996776	231368.304989	37.475508
1903.952179	231662.936558	37.480525
1905.733526	231963.006376	37.485543
1907.177991	232271.232490	37.490560
1909.348130	232558.873784	37.495578
1911.275167	232864.841011	37.500596
1912.883474	233173.907546	37.505613
1914.711847	233480.933689	37.510631
1916.529179	233784.762378	37.515648
1918.485600	234095.681430	37.520666
1920.447906	234420.823569	37.525684
1922.229244	234725.651370	37.530701
1923.974773	235049.204439	37.535719
1925.855606	235375.607097	37.540736
1928.102539	235682.827529	37.545754
1930.149514	236010.983733	37.550772
1931.980939	236336.254312	37.555789
1934.188931	236656.462562	37.560807
1935.949709	236972.780511	37.565824
1938.027608	237289.861838	37.570842
1939.954411	237618.727847	37.575860
1942.047419	237936.113452	37.580877
1944.626506	238249.841550	37.585895
1946.618754	238567.092563	37.590912
1948.707242	238880.265304	37.595930
1950.462835	239206.013664	37.600948
1952.549181	239525.030398	37.605965
1954.574027	239843.651383	37.610983
1956.518011	240161.244689	37.616000
1958.375703	240475.423587	37.621018
1960.097633	240801.207166	37.626036
1962.271402	241110.994228	37.631053
1964.559245	241435.902341	37.636071
1966.345391	241756.293533	37.641088
1968.619503	242065.914709	37.646106
1970.689907	242387.710241	37.651124
1972.653974	242707.110456	37.656141
1974.584865	243020.014280	37.661159
1976.777428	243339.176628	37.666176
1978.920316	243646.257074	37.671194
1981.041587	243954.306891	37.676212
1983.478545	244257.354247	37.681229
1986.023984	244574.050579	37.686247
1987.824187	244871.129633	37.691264
1989.661719	245156.646118	37.696282
1991.925599	245458.072600	37.701300
1993.671253	245756.762480	37.706317
1995.559706	246059.545275	37.711335
1997.534471	246358.352490	37.716352
1999.623870	246655.237075	37.721370
2001.365818	246962.210787	37.726388
2003.259247	247262.633047	37.731405
2005.440529	247557.828429	37.736423
2006.840575	247869.659086	37.741440
2009.130637	248160.621812	37.746458
2010.980017	248451.782020	37.751476
2012.834066	248737.785580	37.756493
2014.737597	249015.678793	37.761511
2016.087811	249310.755407	37.766528
2018.241993	249604.892171	37.771546
2019.755924	249909.901273	37.776564
2021.462597	250222.678633	37.781581
2023.303491	250531.980680	37.786599
2024.995927	250854.541093	37.791616
2026.928294	251182.093585	37.796634
2029.231121	251505.498254	37.801652
2031.177441	251834.497669	37.806669
2032.952959	252162.508724	37.811687
2034.946608	252506.082510	37.816704
2036.782890	252841.426297	37.821722
2038.948226	253186.676052	37.826740
2040.660386	253532.785801	37.831757
2042.831899	253866.909752	37.836775
2044.726785	254224.829110	37.841792
2046.822240	254588.102552	37.846810
2048.835155	254949.687804	37.851828
2050.861254	255316.961703	37.856845
2052.959079	255679.931891	37.861863
2054.883609	256043.158816	37.866880
2057.135657	256407.452100	37.871898
2059.118363	256784.464508	37.876916
2061.219108	257150.103939	37.881933
2063.492462	257513.531961	37.886951
2065.770599	257891.642441	37.891968
2068.217397	258252.300616	37.896986
2070.379064	258627.712656	37.902004
2072.984820	258979.455776	37.907021
2075.956490	259316.052161	37.912039
2077.936143	259671.299504	37.917056
2080.638727	260005.907244	37.922074
2082.707607	260351.666117	37.927092
2084.765917	260691.000192	37.932109
2087.503754	261014.908985	37.937127
2089.237245	261358.512237	37.942144
2091.239081	261689.854538	37.947162
2093.150055	262035.818275	37.952180
2094.657575	262385.123367	37.957197
2096.800905	262721.550297	37.962215
2098.698049	263074.858792	37.967232
2100.737423	263420.803624	37.972250
2102.860727	263779.614817	37.977268
2104.990078	264131.820612	37.982285
2107.294972	264468.706243	37.987303
2109.530692	264830.472771	37.992320
2111.195322	265177.037531	37.997338
2113.643742	265530.997589	38.002356
2115.677755	265886.700277	38.007373
2117.808696	266226.841129	38.012391
2120.153496	266579.878536	38.017408
2122.152099	266914.401362	38.022426
2124.458763	267235.970706	38.027444
2126.244030	267562.576579	38.032461
2128.591752	267878.932132	38.037479
2130.516354	268206.405395	38.042496
2132.302224	268529.734702	38.047514
2134.397919	268859.340456	38.052532
2135.955231	269199.650349	38.057549
2138.109631	269547.918559	38.062567
2139.543315	269894.345183	38.067584
2141.604620	270249.995443	38.072602
2143.685495	270611.053661	38.077620
2145.410116	270977.477825	38.082637
2147.955493	271334.982382	38.087655
2150.083325	271701.952528	38.092672
2152.141161	272081.889614	38.097690
2154.608339	272455.563453	38.102708
2156.627090	272831.696419	38.107725
2159.002782	273202.209505	38.112743
2160.952180	273578.506027	38.117760
2162.907521	273962.727520	38.122778
2165.034544	274344.457692	38.127796
2166.941405	274741.591870	38.132813
2169.202792	275131.175825	38.137831
2171.446330	275539.738957	38.142848
2173.680774	275937.761093	38.147866
2176.490507	276331.424186	38.152884
2178.403407	276727.820603	38.157901
2180.790654	277119.619922	38.162919
2183.071737	277515.398928	38.167936
2185.137347	277903.184538	38.172954
2187.763386	278289.179139	38.177972
2189.925294	278696.890898	38.182989
2192.696524	279065.664137	38.188007
2195.086650	279468.538170	38.193024
2197.189929	279853.344932	38.198042
2199.523738	280230.366946	38.203060
2201.870866	280627.302865	38.208077
2204.309689	281000.446537	38.213095
2206.768350	281384.256239	38.218112
2209.272597	281747.227800	38.223130
2212.028801	282113.156774	38.228148
2213.776610	282489.127280	38.233165
2216.174461	282856.535176	38.238183
2218.230629	283223.844574	38.243200
2220.281036	283599.309035	38.248218
2223.025494	283964.019219	38.253236
2225.030523	284340.811242	38.258253
2227.311158	284708.515728	38.263271
2229.376800	285082.401532	38.268288
2231.068093	285458.073759	38.273306
2233.491083	285821.690170	38.278324
2235.432434	286210.785624	38.283341
2237.683962	286584.107026	38.288359
2239.751868	286971.098541	38.293376
2242.152930	287345.055890	38.298394
2244.095307	287708.416324	38.303412
2246.199859	288068.829301	38.308429
2248.414579	288425.032924	38.313447
2250.522297	288787.019536	38.318464
2252.589492	289146.649672	38.323482
2254.823150	289503.738092	38.328500
2257.029087	289872.236279	38.333517
2259.164535	290241.862865	38.338535
2261.460421	290618.093596	38.343552
2263.596108	290989.979936	38.348570
2266.168421	291357.325653	38.353588
2268.514504	291730.904918	38.358605
2270.795170	292107.313661	38.363623
2272.951253	292493.597717	38.368640
2274.983653	292869.612764	38.373658
2277.581540	293249.881342	38.378676
2279.856707	293645.518046	38.383693
2282.042980	294022.599058	38.388711
2284.367867	294409.361087	38.393728
2286.375574	294811.820441	38.398746
2288.718836	295193.396053	38.403764
2291.172028	295598.094823	38.408781
2293.440759	295983.846687	38.413799
2295.937130	296396.487804	38.418816
2298.002077	296797.003499	38.423834
2300.434286	297186.842127	38.428852
2302.564226	297600.402348	38.433869
2305.084037	298000.970317	38.438887
2307.410013	298405.530777	38.443904
2309.800997	298814.931707	38.448922
2312.208346	299227.148640	38.453940
2314.515062	299647.331195	38.458957
2316.778191	300043.489815	38.463975
2319.108538	300457.417792	38.468992
2321.502835	300875.297170	38.474010
2323.854979	301280.125875	38.479028
2326.135682	301698.122669	38.484045
2328.790085	302104.577771	38.489063
2331.353280	302514.729388	38.494080
2333.517452	302929.845515	38.499098
2336.285491	303340.902194	38.504116
2338.528985	303744.268196	38.509133
2341.023667	304150.234913	38.514151
2343.656111	304559.150495	38.519168
2345.597443	304960.401833	38.524186
2348.148652	305357.948436	38.529204
2350.458381	305769.603998	38.534221
2353.028473	306168.745423	38.539239
2355.380262	306575.667329	38.544256
2357.688344	306989.402142	38.549274
2359.790067	307390.290452	38.554292
2362.117706	307802.698703	38.559309
2364.457064	308213.071732	38.564327
2367.048749	308621.269802	38.569344
2368.714363	309026.971712	38.574362
2371.464184	309403.595509	38.579380
2373.794077	309793.517886	38.584397
2376.052368	310175.525654	38.589415
2378.301604	310556.289026	38.594432
2380.798106	310948.213071	38.599450
2382.943532	311323.580269	38.604468
2385.007990	311717.729064	38.609485
2387.474781	312112.295275	38.614503
2389.631314	312512.344638	38.619520
2391.838613	312921.959882	38.624538
2394.615867	313317.920250	38.629556
2396.645813	313733.351433	38.634573
2398.783985	314140.179085	38.639591
2401.634446	314548.212977	38.644608
2403.782001	314969.767038	38.649626
2406.265685	315386.288012	38.654644
2408.472398	315798.508068	38.659661
2411.290873	316214.007417	38.664679
2413.835880	316636.812196	38.669696
2416.410055	317066.239380	38.674714
2419.042780	317480.950063	38.679732
2421.439172	317898.032999	38.684749
2423.663430	318314.785820	38.689767
2426.787369	318734.670482	38.694784
2429.558879	319152.424938	38.699802
2432.460996	319554.054965	38.704820
2435.217766	319962.385707	38.709837
2437.522280	320370.684697	38.714855
2440.195281	320770.161510	38.719872
2442.357157	321184.219092	38.724890
2444.896135	321588.945193	38.729908
2447.335290	321995.259827	38.734925
2449.471233	322403.068208	38.739943
2452.057603	322804.504993	38.744960
2454.388637	323227.617892	38.749978
2456.746783	323646.686407	38.754996
2459.133849	324061.481732	38.760013
2461.269000	324482.714646	38.765031
2463.668842	324905.858928	38.770048
2465.839528	325348.566488	38.775066
2468.190325	325779.738980	38.780084
2470.331367	326220.491008	38.785101
2472.737226	326664.246044	38.790119
2475.318150	327104.136205	38.795136
2477.987368	327561.354558	38.800154
2480.338420	328006.913698	38.805172
2482.535593	328454.450019	38.810189
2484.938746	328909.569383	38.815207
2487.718994	329355.560522	38.820224
2489.650913	329820.398856	38.825242
2492.311300	330267.038398	38.830260
2494.956518	330727.974318	38.835277
2497.357641	331189.682428	38.840295
2500.002955	331648.758778	38.845312
2502.916390	332095.296232	38.850330
2505.602148	332512.080859	38.855348
2507.978308	332935.463476	38.860365
2510.434607	333367.870686	38.865383
2513.025430	333775.800783	38.870400
2515.485767	334200.990666	38.875418
2517.723487	334618.163825	38.880436
2520.335973	335035.503588	38.885453
2522.329083	335474.268227	38.890471
2524.915873	335903.109296	38.895488
2526.917259	336345.751888	38.900506
2529.630154	336795.566165	38.905524
2531.907801	337249.813648	38.910541
2533.896212	337711.670375	38.915559
2536.623009	338169.496620	38.920576
2538.996715	338647.053432	38.925594
2541.515513	339106.099331	38.930612
2544.072422	339571.432705	38.935629
2546.490404	340064.891650	38.940647
2549.466900	340543.582783	38.945664
2551.723354	341029.264956	38.950682
2554.126256	341503.799446	38.955700
2557.073907	341986.977925	38.960717
2559.348326	342483.283905	38.965735
2562.398722	342966.489078	38.970752
2564.663475	343473.832647	38.975770
2567.355541	343967.775181	38.980788
2569.884846	344460.089128	38.985805
2572.822685	344959.341358	38.990823
2575.276794	345461.661723	38.995840
2577.861790	345954.512755	39.000858
2580.754405	346456.729592	39.005876
2583.365274	346955.711682	39.010893
2585.903593	347463.103988	39.015911
2588.989566	347955.502886	39.020928
2591.289475	348451.753802	39.025946
2594.045801	348948.334159	39.030964
2597.220553	349447.026965	39.035981
2599.485481	349955.125218	39.040999
2602.486898	350437.538669	39.046016
2604.954100	350942.904735	39.051034
2607.831374	351426.065172	39.056052
2610.672362	351916.004772	39.061069
2613.299638	352414.325278	39.066087
2616.204031	352893.076478	39.071104
2618.787221	353389.998555	39.076122
2621.525135	353874.021665	39.081140
2624.298661	354355.623138	39.086157
2626.827026	354839.264229	39.091175
2629.453382	355317.554718	39.096192
2632.105706	355802.385419	39.101210
2635.016644	356288.211190	39.106228
2637.979310	356755.367852	39.111245
2640.729714	357242.453522	39.116263
2643.565682	357697.869362	39.121280
2646.051467	358165.697433	39.126298
2648.489784	358610.152067	39.131316
2651.339478	359042.532079	39.136333
2653.731457	359472.645663	39.141351
2656.215198	359901.218018	39.146368
2658.595791	360341.198833	39.151386
2661.385936	360768.775800	39.156404
2663.872626	361215.076860	39.161421
2666.248676	361659.030885	39.166439
2668.867888	362108.018160	39.171456
2671.464962	362569.922814	39.176474
2673.759407	363024.155511	39.181492
2676.741515	363480.838117	39.186509
2679.155798	363951.970511	39.191527
2681.718329	364417.592820	39.196544
2684.533266	364886.850240	39.201562
2687.125663	365363.878330	39.206580
2689.987822	365840.858646	39.211597
2692.613645	366328.301446	39.216615
2695.594787	366799.060600	39.221632
2698.391536	367286.313565	39.226650
2700.918770	367765.229553	39.231668
2704.069157	368235.337540	39.236685
2706.459230	368717.614509	39.241703
2709.086837	369205.405801	39.246720
2711.668322	369691.600237	39.251738
2714.306067	370185.545076	39.256756
2717.309632	370686.531249	39.261773
2720.038558	371177.481300	39.266791
2723.296572	371656.644309	39.271808
2726.197162	372145.728965	39.276826
2728.740628	372651.154395	39.281844
2731.542810	373130.068256	39.286861
2733.826200	373629.154257	39.291879
2736.507729	374124.669727	39.296896
2739.470416	374624.371902	39.301914
2741.914281	375127.930581	39.306932
2744.656671	375631.968558	39.311949
2747.125208	376152.306785	39.316967
2749.665154	376663.112768	39.321984
2752.562425	377185.805342	39.327002
2755.011866	377722.769482	39.332020
2758.005648	378246.371528	39.337037
2760.587959	378774.344653	39.342055
2763.402019	379298.544653	39.347072
2766.319135	379834.999977	39.352090
2768.690668	380372.371450	39.357108
2772.066723	380900.088573	39.362125
2774.398614	381438.034933	39.367143
2777.582374	381972.211244	39.372160
2780.720223	382500.705022	39.377178
2783.315774	383048.302580	39.382196
2786.087094	383563.318877	39.387213
2788.830815	384100.147525	39.392231
2791.517154	384632.310190	39.397248
2794.598768	385157.985138	39.402266
2797.402123	385660.030870	39.407284
2800.109037	386146.231933	39.412301
2802.810891	386645.845208	39.417319
2805.492314	387141.954601	39.422336
2808.168333	387634.405663	39.427354
2810.763132	388136.932197	39.432372
2813.604836	388636.090037	39.437389
2816.246348	389142.145938	39.442407
2818.942589	389648.921498	39.447424
2821.583851	390178.778033	39.452442
2824.262188	390705.323725	39.457460
2827.421114	391218.775075	39.462477
2829.649822	391759.527748	39.467495
2832.410867	392286.061916	39.472512
2835.218296	392829.749580	39.477530
2837.732996	393386.662097	39.482548
2840.682496	393928.915123	39.487565
2843.249092	394495.970494	39.492583
2845.900837	395052.859530	39.497600
2848.696088	395616.106931	39.502618
2851.663277	396199.832047	39.507636
2854.611653	396762.528848	39.512653
2857.384299	397339.595929	39.517671
2860.348550	397921.186799	39.522688
2864.211281	398484.546443	39.527706
2867.149503	399055.548018	39.532724
2870.239130	399621.622153	39.537741
2873.268617	400185.921160	39.542759
2875.873570	400747.463253	39.547776
2879.238095	401322.870593	39.552794
2882.238291	401904.232619	39.557812
2885.379298	402458.408960	39.562829
2887.996559	403043.816611	39.567847
2890.722928	403609.827360	39.572864
2894.450252	404168.571121	39.577882
2897.082087	404739.114462	39.582900
2899.971946	405314.828771	39.587917
2903.111082	405880.074122	39.592935
2906.167463	406436.297826	39.597952
2909.303740	407000.458498	39.602970
2911.903482	407565.428866	39.607988
2915.736466	408119.699457	39.613005
2918.604621	408675.532169	39.618023
2921.446547	409239.774157	39.623040
2924.920533	409780.738600	39.628058
2927.710571	410336.426430	39.633076
2930.748925	410883.168262	39.638093
2933.540390	411428.722588	39.643111
2936.484964	411980.072020	39.648128
2939.645188	412512.267322	39.653146
2941.887541	413071.412285	39.658164
2945.182745	413620.648061	39.663181
2947.860500	414169.210970	39.668199
2950.825790	414721.139304	39.673216
2954.218256	415266.121833	39.678234
2956.495189	415788.387154	39.683252
2959.593891	416306.407682	39.688269
2962.030495	416821.482768	39.693287
2964.457165	417331.558121	39.698304
2967.308043	417865.630043	39.703322
2969.730551	418413.620332	39.708340
2972.176021	418960.861551	39.713357
2974.963003	419512.142909	39.718375
2977.601917	420090.370984	39.723392
2980.761630	420649.476376	39.728410
2983.242283	421228.668737	39.733428
2986.152264	421809.098550	39.738445
2988.883512	422406.316695	39.743463
2991.655562	422998.423061	39.748480
2994.826770	423595.393717	39.753498
2997.511450	424208.743433	39.758516
3000.485179	424820.184228	39.763533
3003.391103	425443.883059	39.768551
3006.199463	426077.741148	39.773568
3009.650214	426699.044758	39.778586
3012.507735	427334.765204	39.783604
3015.909124	427958.149781	39.788621
3019.310485	428596.818957	39.793639
3022.358134	429226.688737	39.798656
3025.655749	429857.972936	39.803674
3028.223954	430499.108636	39.808692
3032.008815	431126.688495	39.813709
3035.252971	431759.454761	39.818727
3038.015775	432398.663913	39.823744
3041.844100	433021.252304	39.828762
3044.804364	433659.791034	39.833780
3047.896827	434283.782052	39.838797
3051.462313	434910.493851	39.843815
3054.259001	435539.211029	39.848832
3057.903755	436156.864386	39.853850
3060.880609	436793.523649	39.858868
3064.217539	437395.774231	39.863885
3067.658075	438016.781750	39.868903
3070.241563	438643.074622	39.873920
3073.740317	439260.471682	39.878938
3076.800916	439894.835471	39.883956
3079.845122	440510.095701	39.888973
3082.848197	441130.511715	39.893991
3086.011358	441764.051306	39.899008
3089.211206	442375.492963	39.904026
3091.934574	443009.626538	39.909044
3094.938676	443629.573388	39.914061
3097.802686	444262.335330	39.919079
3100.914971	444904.305965	39.924096
3103.989471	445530.622017	39.929114
3106.818941	446178.273067	39.934132
3109.533211	446811.699625	39.939149
3112.908594	447467.885415	39.944167
3115.629246	448110.742162	39.949184
3118.946682	448738.503728	39.954202
3121.633696	449367.056754	39.959220
3124.549287	449984.977886	39.964237
3127.555944	450604.184081	39.969255
3130.328727	451226.498038	39.974272
3133.491980	451840.382417	39.979290
3136.410996	452474.330681	39.984308
3139.081170	453107.592158	39.989325
3142.268886	453746.472764	39.994343
3145.483821	454395.249826	39.999360
3148.557828	455041.044841	40.004378
3151.356114	455706.701351	40.009396
3154.401565	456375.841083	40.014413
3157.856131	457046.211622	40.019431
3160.723125	457717.059665	40.024448
3163.943378	458392.537020	40.029466
3167.153077	459078.468612	40.034484
3170.242527	459763.436523	40.039501
3173.404010	460450.243514	40.044519
3176.595216	461141.273784	40.049536
3179.678080	461828.403847	40.054554
3183.306946	462532.473690	40.059572
3186.244997	463233.291143	40.064589
3189.762965	463924.888851	40.069607
3193.169619	464640.407317	40.074624
3196.329350	465354.726876	40.079642
3199.722193	466066.254258	40.084660
3202.766185	466790.507789	40.089677
3206.144152	467495.869473	40.094695
3208.973648	468215.859485	40.099712
3212.487070	468927.321554	40.104730
3215.590927	469645.802818	40.109748
3219.223044	470371.154128	40.114765
3223.123910	471075.098248	40.119783
3226.293402	471796.629526	40.124800
3229.352132	472506.523373	40.129818
3233.089105	473218.560574	40.134836
3236.230509	473924.448209	40.139853
3240.029069	474629.196197	40.144871
3243.238569	475355.701446	40.149888
3246.636222	476041.151018	40.154906
3250.051105	476746.643932	40.159924
3252.877930	477457.158963	40.164941
3256.710126	478158.997404	40.169959
3259.506119	478873.611768	40.174976
3262.621402	479572.227975	40.179994
3266.348144	480286.189138	40.185012
3269.677087	480986.591480	40.190029
3273.003306	481690.001610	40.195047
3276.076510	482404.999672	40.200064
3279.862628	483098.330168	40.205082
3283.395520	483794.758513	40.210100
3286.364655	484493.221675	40.215117
3289.898285	485190.711196	40.220135
3293.057352	485889.750459	40.225152
3296.466415	486575.789627	40.230170
3299.963872	487225.765369	40.235188
3302.969456	487881.606892	40.240205
3306.308342	488525.601329	40.245223
3309.234483	489173.428088	40.250240
3312.588421	489815.052135	40.255258
3315.442353	490470.372872	40.260276
3318.303722	491130.923046	40.265293
3321.638239	491794.153233	40.270311
3324.458205	492467.846483	40.275328
3327.619884	493154.846261	40.280346
3330.871383	493849.028883	40.285364
3333.601225	494547.358774	40.290381
3336.700537	495242.825949	40.295399
3339.468343	495974.023955	40.300416
3342.719396	496680.724768	40.305434
3346.085379	497423.435416	40.310452
3349.162936	498164.343342	40.315469
3352.631682	498914.348838	40.320487
3355.877074	499658.551822	40.325504
3358.889174	500425.228588	40.330522
3362.356179	501190.285889	40.335540
3365.660240	501980.982456	40.340557
3369.162572	502734.759953	40.345575
3372.236518	503533.147426	40.350592
3375.395895	504322.701958	40.355610
3379.228646	505105.855461	40.360628
3382.504748	505908.090483	40.365645
3386.277958	506690.324215	40.370663
3389.984715	507502.764211	40.375680
3393.433690	508289.569671	40.380698
3397.221008	509097.632186	40.385716
3400.694628	509885.269118	40.390733
3404.280155	510688.999230	40.395751
3407.521356	511489.012045	40.400768
3411.248375	512286.892195	40.405786
3414.777197	513077.954973	40.410804
3418.431035	513874.106830	40.415821
3422.351792	514661.653106	40.420839
3425.701720	515447.234785	40.425856
3429.141284	516253.648799	40.430874
3432.800749	517035.626137	40.435892
3436.158483	517831.283093	40.440909
3439.821244	518614.900238	40.445927
3443.136187	519422.995327	40.450944
3446.650691	520200.256207	40.455962
3450.119968	521005.172624	40.460980
3453.174844	521801.592823	40.465997
3456.889562	522603.214617	40.471015
3460.372000	523399.690514	40.476032
3463.448634	524200.476859	40.481050
3467.238390	524987.044551	40.486068
3470.353254	525800.248337	40.491085
3473.775998	526595.919884	40.496103
3476.913990	527413.171565	40.501120
3480.216815	528199.253781	40.506125
3483.676806	528958.329573	40.511130
3486.810239	529660.422473	40.516135
3490.022780	530309.871837	40.521140
3493.302783	530886.980714	40.526144
3495.657894	531425.866415	40.531149
3498.591797	531882.895941	40.536154
3501.190853	532300.457059	40.541159
3503.469990	532645.459612	40.546164
3505.633696	532947.025942	40.551168
3507.338278	533198.898042	40.556173
3509.491214	533391.538527	40.561178
3511.295330	533545.535261	40.566183
3512.424357	533648.463188	40.571188
3513.926342	533717.131443	40.576192
3515.151492	533761.493989	40.581197
3516.138356	533742.444819	40.586202
3516.857217	533720.507992	40.591207
3518.032665	533641.111368	40.596212
3518.457055	533575.674861	40.601216
3519.023403	533469.245671	40.606221
3519.941649	533320.274225	40.611226
3520.470351	533173.080560	40.616231
3520.978278	533000.073375	40.621236
3521.409404	532824.095725	40.626240
3521.399605	532612.518203	40.631245
3521.867235	532408.137427	40.636250
3521.450517	532179.390542	40.641255
3522.221399	531956.161685	40.646260
3522.129575	531722.304468	40.651264
3522.202742	531463.206012	40.656269
3522.114748	531215.951640	40.661274
3521.976725	530951.118209	40.666279
3521.932015	530695.259344	40.671284
3521.961790	530439.232951	40.676288
3522.083249	530161.410081	40.681293
3521.985618	529898.371535	40.686298
3521.727322	529621.104437	40.691303
3521.499670	529350.901986	40.696308
3521.251869	529083.376291	40.701312
3520.994584	528803.315392	40.706317
3521.037494	528541.950136	40.711322
3520.503438	528272.283002	40.716327
3520.512721	528002.677010	40.721332
3520.462260	527732.115687	40.726336
3520.343021	527467.321868	40.731341
3520.229733	527193.830150	40.736346
3519.878687	526946.954776	40.741351
3519.922054	526666.859193	40.746356
3519.511215	526409.927536	40.751360
3519.208462	526151.610043	40.756365
3519.158212	525895.927203	40.761370
3518.516609	525649.330392	40.766375
3518.632345	525391.894807	40.771380
3518.340276	525143.668111	40.776384
3518.278420	524905.257532	40.781389
3518.023860	524666.671687	40.786394
3517.319384	524433.056451	40.791399
3517.492928	524187.420376	40.796404
3516.989177	523958.922388	40.801408
3516.374779	523739.183624	40.806413
3516.428464	523505.182364	40.811418
3516.161145	523291.954119	40.816423
3516.191269	523080.040931	40.821428
3515.671805	522868.717347	40.826432
3515.577956	522661.064612	40.831437
3515.752972	522451.496263	40.836442
3515.534855	522253.614680	40.841447
3515.316333	522035.458489	40.846452
3515.244924	521843.817460	40.851456
3514.883310	521652.877262	40.856461
3514.787737	521446.574278	40.861466
3514.385482	521256.444754	40.866471
3514.035245	521075.809561	40.871476
3513.784687	520877.714152	40.876480
3513.470924	520713.348816	40.881485
3513.833920	520530.724209	40.886490
3513.364732	520364.155333	40.891495
3513.334663	520188.060638	40.896500
3513.200468	520024.772326	40.901504
3512.631109	519850.781663	40.906509
3512.715858	519684.927309	40.911514
3512.415204	519537.739028	40.916519
3512.145384	519370.420678	40.921524
3512.094557	519218.184358	40.926528
3511.853412	519067.240796	40.931533
3511.766828	518913.793788	40.936538
3511.557496	518785.545810	40.941543
3511.534746	518644.575592	40.946548
3511.461547	518493.954187	40.951552
3511.287848	518353.814386	40.956557
3511.076936	518220.050603	40.961562
3510.920499	518084.456733	40.966567
3510.668816	517939.673627	40.971572
3510.393790	517823.615182	40.976576
3510.363528	517694.976460	40.981581
3510.737487	517567.891028	40.986586
3510.413339	517456.945151	40.991591
3510.224695	517330.907622	40.996596
3510.034446	517212.050210	41.001600
3510.017815	517089.978626	41.006605
3510.082432	516974.568527	41.011610
3509.804161	516866.595072	41.016615
3509.523515	516746.079794	41.021620
3509.626690	516631.116351	41.026624
3509.762776	516528.638010	41.031629
3509.658995	516410.115192	41.036634
3509.407960	516309.618408	41.041639
3508.979445	516208.693919	41.046644
3509.048270	516103.998419	41.051648
3508.770102	516010.432551	41.056653
3509.027037	515906.515244	41.061658
3508.786310	515807.176983	41.066663
3509.138232	515703.344546	41.071668
3508.743376	515606.811007	41.076672
3508.635176	515511.445387	41.081677
3508.967759	515404.630267	41.086682
3508.607587	515321.694169	41.091687
3508.613654	515218.722585	41.096692
3508.476464	515128.669758	41.101696
3508.234920	515037.216820	41.106701
3508.272637	514948.956109	41.111706
3508.223447	514858.179855	41.116711
3508.328239	514779.061953	41.121716
3508.194646	514691.787918	41.126720
3508.107257	514616.796344	41.131725
3508.255323	514512.938170	41.136730
3507.935729	514442.585055	41.141735
3507.808404	514354.043834	41.146740
3508.022092	514281.784956	41.151744
3507.810270	514182.331329	41.156749
3507.817319	514110.154952	41.161754
3507.479166	514027.411284	41.166759
3507.793647	513956.247811	41.171764
3507.973539	513867.149679	41.176768
3507.187678	513800.661015	41.181773
3507.631447	513721.282239	41.186778
3506.743591	513650.459246	41.191783
3506.932128	513578.960025	41.196788
3506.995292	513510.059915	41.201792
3507.029503	513452.747040	41.206797
3507.062713	513387.138895	41.211802
3507.066135	513334.382747	41.216807
3507.032568	513262.664386	41.221812
3506.927461	513198.695964	41.226816
3507.031516	513133.986101	41.231821
3507.141676	513066.037797	41.236826
3506.339320	512997.019483	41.241831
3506.301096	512944.066371	41.246836
3506.835088	512881.159120	41.251840
3506.399930	512820.074035	41.256845
3506.701526	512761.148497	41.261850
3506.462552	512713.284649	41.266855
3506.668840	512655.081964	41.271860
3506.680873	512594.026547	41.276864
3506.323095	512559.383220	41.281869
3506.396250	512482.940446	41.286874
3506.358839	512431.604270	41.291879
3506.164491	512374.677950	41.296884
3506.099401	512329.517054	41.301888
3506.335294	512270.448443	41.306893
3506.469262	512214.531958	41.311898
3506.203397	512172.285677	41.316903
3506.583174	512102.823948	41.321908
3506.540220	512046.277272	41.326912
3506.311550	511995.779361	41.331917
3506.339494	511933.403843	41.336922
3506.271824	511889.304469	41.341927
3506.056916	511837.893380	41.346932
3506.016264	511785.139370	41.351936
3505.852889	511746.163886	41.356941
3506.131963	511682.432527	41.361946
3505.969422	511642.192027	41.366951
3506.118114	511597.197737	41.371956
3505.901302	511544.875513	41.376960
3505.755765	511502.608546	41.381965
3505.874800	511443.049665	41.386970
3505.822583	511413.515524	41.391975
3505.835665	511354.984813	41.396980
3506.016783	511317.825607	41.401984
3505.999829	511263.346279	41.406989
3505.786610	511222.353990	41.411994
3506.003414	511167.837409	41.416999
3505.939528	511131.930619	41.422004
3506.128772	511074.231086	41.427008
3505.625851	511029.742988	41.432013
3505.963455	510985.880743	41.437018
3505.761706	510939.220116	41.442023
3505.750113	510892.124601	41.447028
3505.716635	510855.403011	41.452032
3505.658926	510808.871026	41.457037
3505.881989	510755.313317	41.462042
3505.741320	510716.433063	41.467047
3505.771064	510668.419801	41.472052
3506.157334	510625.510125	41.477056
3505.877555	510587.258630	41.482061
3505.807600	510532.380631	41.487066
3505.680949	510501.693122	41.492071
3505.691053	510459.702504	41.497076
3505.736812	510420.336804	41.502080
3505.445698	510372.676961	41.507085
3505.704563	510313.294393	41.512090
3505.418640	510294.166171	41.517095
3505.524985	510236.426320	41.522100
3505.808589	510212.351339	41.527104
3505.509295	510164.742799	41.532109
3505.726106	510120.340932	41.537114
3505.728354	510076.326997	41.542119
3505.422607	510036.914790	41.547124
3505.218321	509990.302562	41.552128
3505.235595	509961.817331	41.557133
3505.282286	509914.709910	41.562138
3505.242875	509888.560705	41.567143
3505.167721	509855.486114	41.572148
3505.367468	509823.329245	41.577152
3505.286791	509789.445938	41.582157
3505.098387	509751.684044	41.587162
3505.169079	509707.455977	41.592167
3504.860460	509683.473858	41.597172
3505.234598	509645.015715	41.602176
3505.011729	509624.662573	41.607181
3505.236813	509581.016879	41.612186
3504.975885	509549.337045	41.617191
3504.823538	509527.201916	41.622196
3505.150065	509489.358056	41.627200
3504.976054	509455.741803	41.632205
3505.302332	509421.439301	41.637210
3505.217387	509389.276023	41.642215
3505.050516	509349.587321	41.647220
3504.969912	509339.329893	41.652224
3504.801968	509292.406465	41.657229
3505.216748	509266.741046	41.662234
3504.915608	509227.629807	41.667239
3505.014929	509199.838646	41.672244
3505.388046	509158.495766	41.677248
3505.021460	509143.224094	41.682253
3505.099830	509110.781515	41.687258
3505.367545	509066.470062	41.692263
3505.014999	509039.104216	41.697268
3505.014126	508997.921250	41.702272
3504.445392	508987.336013	41.707277
3504.695098	508941.509271	41.712282
3505.027681	508916.008103	41.717287
3505.157361	508893.169858	41.722292
3505.086186	508857.866578	41.727296
3504.746926	508829.992357	41.732301
3505.146051	508797.346707	41.737306
3504.865296	508765.010832	41.742311
3505.055087	508724.201830	41.747316
3505.114644	508700.008359	41.752320
3504.916522	508670.644329	41.757325
3504.960650	508637.548538	41.762330
3504.996403	508614.927150	41.767335
3505.010749	508580.115730	41.772340
3504.833052	508540.376276	41.777344
3504.955614	508519.461275	41.782349
3504.819497	508482.548444	41.787354
3504.891554	508455.873487	41.792359
3504.727951	508428.325019	41.797364
3504.785728	508402.714740	41.802368
3504.708243	508379.503795	41.807373
3505.078576	508335.730795	41.812378
3504.914521	508321.843059	41.817383
3505.081696	508287.765830	41.822388
3504.975053	508255.249690	41.827392
3504.848023	508225.772473	41.832397
3504.650879	508195.243768	41.837402
3504.917126	508171.826426	41.842407
3504.702265	508136.493781	41.847412
3505.190241	508110.056129	41.852416
3504.867704	508085.011453	41.857421
3504.861572	508051.163535	41.862426
3504.848822	508015.950488	41.867431
3504.841425	507992.879734	41.872436
3504.813926	507973.050319	41.877440
3504.945345	507933.968965	41.882445
3505.103074	507908.190364	41.887450
3504.663023	507883.973522	41.892455
3504.521081	507857.786838	41.897460
3505.120478	507828.042334	41.902464
3504.740439	507805.940978	41.907469
3504.955747	507761.280276	41.912474
3505.114095	507736.462672	41.917479
3504.638494	507718.322908	41.922484
3504.852561	507682.820345	41.927488
3504.621235	507651.233531	41.932493
3504.763483	507629.605973	41.937498
3504.877482	507593.815457	41.942503
3504.691241	507574.617850	41.947508
3505.094902	507542.373897	41.952512
3504.691912	507521.186568	41.957517
3504.827337	507490.907642	41.962522
3504.797044	507462.021009	41.967527
3504.626507	507432.954101	41.972532
3504.636278	507400.013164	41.977536
3504.426384	507385.322345	41.982541
3504.996190	507350.724245	41.987546
3504.543565	507324.990648	41.992551
3504.936144	507304.790480	41.997556
3504.828548	507269.287311	42.002560
3504.563279	507250.203032	42.007565
3504.809996	507220.614428	42.012570
3504.675047	507191.743885	42.017575
3504.694469	507177.725031	42.022580
3504.563078	507145.362512	42.027584
3504.523891	507127.102549	42.032589
3504.779747	507093.160750	42.037594
3504.608709	507062.322322	42.042599
3504.744745	507050.106512	42.047604
3504.802349	507028.238585	42.052608
3504.633611	507018.600900	42.057613
3504.499907	506970.754953	42.062618
3504.331779	506961.774936	42.067623
3504.481783	506927.444745	42.072628
3504.723373	506906.255982	42.077632
3504.524346	506880.481641	42.082637
3504.732617	506868.001286	42.087642
3504.484216	506842.032291	42.092647
3504.718818	506814.974914	42.097652
3505.148909	506784.142179	42.102656
3504.644431	506761.654354	42.107661
3504.946327	506728.210567	42.112666
3504.974829	506707.713047	42.117671
3504.686111	506679.220159	42.122676
3504.590150	506648.875135	42.127680
3504.660949	506628.219034	42.132685
3504.810653	506593.078619	42.137690
3504.664965	506577.314349	42.142695
3504.537098	506536.449196	42.147700
3504.663690	506518.921405	42.152704
3504.218914	506493.640741	42.157709
3504.459077	506477.461187	42.162714
3504.594653	506446.320196	42.167719
3504.744605	506423.779097	42.172724
3504.755617	506399.084071	42.177728
3504.600058	506373.909324	42.182733
3504.635007	506346.174353	42.187738
3504.667387	506326.131184	42.192743
3504.455005	506309.516986	42.197748
3504.945740	506276.042484	42.202752
3504.478933	506257.241974	42.207757
3504.872076	506229.855018	42.212762
3504.850188	506197.726434	42.217767
3504.702885	506172.701896	42.222772
3504.973858	506144.018463	42.227776
3504.843998	506110.287517	42.232781
3504.723902	506088.345291	42.237786
3504.661307	506058.398781	42.242791
3504.745703	506042.142238	42.247796
3504.683355	506004.858249	42.252800
3504.443129	505982.327647	42.257805
3504.628754	505965.549007	42.262810
3504.523677	505931.611387	42.267815
3504.446003	505907.739326	42.272820
3504.326626	505885.341305	42.277824
3504.176034	505868.463904	42.282829
3504.191684	505841.490225	42.287834
3504.754169	505830.319421	42.292839
3504.149670	505810.325719	42.297844
3504.841090	505774.693207	42.302848
3504.416370	505768.080873	42.307853
3504.410306	505730.331972	42.312858
3504.533884	505718.319611	42.317863
3504.510509	505685.279458	42.322868
3504.761952	505667.832285	42.327872
3504.363205	505651.297518	42.332877
3504.356894	505620.885928	42.337882
3504.593842	505609.260402	42.342887
3504.505779	505579.924339	42.347892
3504.687992	505554.391397	42.352896
3504.406389	505531.259506	42.357901
3504.761039	505509.342721	42.362906
3504.802332	505481.807789	42.367911
3504.537117	505464.543283	42.372916
3504.676427	505428.693707	42.377920
3504.352680	505407.390062	42.382925
3504.564570	505378.664106	42.387930
3504.708769	505364.522862	42.392935
3504.298706	505339.184427	42.397940
3504.335451	505305.881032	42.402944
3504.103039	505302.527418	42.407949
3504.274822	505273.807629	42.412954
3504.443289	505249.794553	42.417959
3504.352268	505236.651872	42.422964
3504.545386	505195.226793	42.427968
3504.558246	505191.783786	42.432973
3504.592578	505163.085541	42.437978
3504.357237	505147.081122	42.442983
3504.228778	505123.570249	42.447988
3504.130559	505100.763036	42.452992
3504.218835	505093.816337	42.457997
3504.393492	505064.539094	42.463002
3504.281520	505041.683373	42.468007
3504.022018	505034.437382	42.473012
3504.368579	505014.646680	42.478016
3504.157535	504996.006803	42.483021
3504.517047	504974.948873	42.488026
3504.522687	504948.582663	42.493031
3503.973366	504930.755267	42.498036
3504.624851	504913.851381	42.503040
3504.593059	504891.033396	42.508045
3504.466767	504872.784838	42.513050
3504.626223	504861.474698	42.518055
3504.373055	504834.187712	42.523060
3504.569163	504808.803304	42.528064
3504.452289	504793.690744	42.533069
3504.638870	504766.283541	42.538074
3504.710068	504736.161799	42.543079
3504.461861	504724.460550	42.548084
3504.482128	504687.008872	42.553088
3504.690371	504669.820566	42.558093
3504.409087	504644.308950	42.563098
3504.578082	504621.711910	42.568103
3504.403071	504588.035767	42.573108
3504.841811	504565.294807	42.578112
3504.315819	504547.564545	42.583117
3504.407323	504525.283269	42.588122
3504.493862	504497.233570	42.593127
3504.407553	504480.749524	42.598132
3504.697130	504463.750587	42.603136
3504.334539	504440.225196	42.608141
3504.168754	504410.292172	42.613146
3504.046150	504399.431174	42.618151
3504.392767	504371.643810	42.623156
3504.401534	504350.033283	42.628160
3504.026272	504335.264811	42.633165
3504.079093	504320.327450	42.638170
3504.463328	504299.467234	42.643175
3504.155602	504278.260895	42.648180
3504.363529	504265.981169	42.653184
3504.182330	504240.098892	42.658189
3504.268981	504219.791693	42.663194
3504.498636	504217.630027	42.668199
3504.204431	504200.621893	42.673204
3504.492238	504165.100516	42.678208
3504.577873	504154.560707	42.683213
3504.498423	504135.595467	42.688218
3504.809394	504105.485353	42.693223
3504.121279	504088.134506	42.698228
3504.310515	504052.274225	42.703232
3504.107810	504052.964324	42.708237
3504.004925	504016.340411	42.713242
3503.764961	504009.242731	42.718247
3503.897438	504003.047737	42.723252
3504.456181	503985.196063	42.728256
3504.126297	503964.650755	42.733261
3504.227546	503947.225612	42.738266
3504.448059	503918.091035	42.743271
3504.239105	503898.184446	42.748276
3504.258855	503883.353159	42.753280
3504.452601	503865.660271	42.758285
3504.433845	503844.610169	42.763290
3504.497429	503831.087736	42.768295
3504.235982	503800.207226	42.773300
3504.483629	503780.278943	42.778304
3504.277072	503756.424319	42.783309
3504.176681	503730.579128	42.788314
3504.416309	503716.472082	42.793319
3504.029279	503690.419092	42.798324
3504.526914	503686.038812	42.803329
3504.222035	503657.037454	42.808333
3504.534829	503632.392045	42.813338
3504.440400	503618.084674	42.818343
3504.073803	503603.162387	42.823348
3504.510877	503574.397888	42.828353
3504.606679	503557.631144	42.833357
3504.365134	503522.546406	42.838362
3504.696738	503503.262467	42.843367
3504.320265	503487.481277	42.848372
3504.425348	503466.461759	42.853377
3504.283777	503453.325731	42.858381
3504.379289	503417.377751	42.863386
3504.271847	503420.886975	42.868391
3503.839629	503386.085153	42.873396
3504.195506	503369.580783	42.878401
3503.961324	503362.583147	42.883405
3504.010021	503332.057675	42.888410
3504.250735	503319.468447	42.893415
3504.281927	503316.730718	42.898420
3504.404371	503289.027689	42.903425
3504.222092	503274.278432	42.908429
3504.539666	503252.516527	42.913434
3504.287590	503231.806233	42.918439
3503.890339	503219.975706	42.923444
3504.350475	503195.508840	42.928449
3504.597538	503179.628820	42.933453
3504.214764	503157.572609	42.938458
3504.225153	503134.138347	42.943463
3504.060242	503111.743979	42.948468
3503.908270	503102.658200	42.953473
3503.974743	503081.593716	42.958477
3504.085050	503065.633986	42.963482
3503.814032	503069.827077	42.968487
3503.771734	503057.231783	42.973492
3504.160710	503022.856168	42.978497
3504.122752	503019.825656	42.983501
3504.124009	502998.518324	42.988506
3504.390131	502981.926558	42.993511
3504.140599	502971.287184	42.998516
3504.388904	502947.511403	43.003521
3504.372468	502939.720012	43.008525
3504.329859	502920.950087	43.013530
3504.240749	502893.836601	43.018535
3503.944676	502878.396438	43.023540
3504.143421	502843.949319	43.028545
3504.267210	502843.322569	43.033549
3504.157097	502823.348531	43.038554
3504.086555	502801.647417	43.043559
3503.874156	502794.241217	43.048564
3504.074092	502773.813223	43.053569
3504.307845	502758.795330	43.058573
3504.218899	502748.839006	43.063578
3504.580412	502717.149567	43.068583
3504.207366	502700.607950	43.073588
3504.362062	502669.609072	43.078593
3504.206950	502664.015798	43.083597
3504.120978	502650.819773	43.088602
3504.221923	502623.726445	43.093607
3504.549208	502609.402213	43.098612
3504.435928	502588.213715	43.103617
3504.037483	502573.447426	43.108621
3503.937127	502546.284572	43.113626
3504.429699	502523.937376	43.118631
3504.075030	502515.946196	43.123636
3504.249981	502488.436064	43.128641
3504.328864	502475.466914	43.133645
3504.472686	502461.576462	43.138650
3504.352537	502438.769264	43.143655
3504.608745	502408.715526	43.148660
3504.474769	502389.453350	43.153665
3504.494959	502365.409166	43.158669
3504.150607	502347.799810	43.163674
3504.630969	502313.256535	43.168679
3504.187399	502310.846756	43.173684
3504.345421	502281.769972	43.178689
3504.274253	502261.333625	43.183693
3503.987993	502254.445006	43.188698
3503.907622	502222.318393	43.193703
3504.103875	502209.684791	43.198708
3504.172369	502184.924139	43.203713
3503.924117	502173.929787	43.208717
3503.829501	502174.147351	43.213722
3504.088944	502150.267513	43.218727
3503.756240	502128.303329	43.223732
3504.022086	502116.873388	43.228737
3504.268191	502115.417461	43.233741
3504.033329	502087.617186	43.238746
3504.030970	502070.206568	43.243751
3503.844374	502062.947824	43.248756
3504.055541	502045.756502	43.253761
3504.047671	502043.024751	43.258765
3503.913448	502037.427977	43.263770
3504.161503	502014.663263	43.268775
3503.956165	502003.206497	43.273780
3504.134137	501994.219839	43.278785
3503.973613	501965.496570	43.283789
3503.996489	501952.890189	43.288794
3504.229072	501939.643283	43.293799
3503.988088	501922.067780	43.298804
3503.716733	501909.052345	43.303809
3503.987025	501901.012720	43.308813
3504.028907	501878.280419	43.313818
3504.388401	501859.142126	43.318823
3504.012837	501853.380982	43.323828
3503.921089	501828.999462	43.328833
3503.926410	501813.561345	43.333837
3503.984330	501806.719379	43.338842
3504.107831	501790.705802	43.343847
3503.843653	501777.891594	43.348852
3504.202896	501762.296263	43.353857
3503.967521	501752.362522	43.358861
3503.815814	501727.686652	43.363866
3504.227715	501716.486444	43.368871
3503.844273	501710.321580	43.373876
3504.069933	501683.510793	43.378881
3504.114662	501681.782971	43.383885
3504.037694	501655.576739	43.388890
3504.392232	501633.503317	43.393895
3504.122967	501626.814227	43.398900
3504.190891	501592.790277	43.403905
3503.991570	501583.609971	43.408909
3503.909434	501570.614995	43.413914
3504.283941	501546.766775	43.418919
3503.959354	501536.239630	43.423924
3504.106000	501523.765228	43.428929
3503.746285	501504.436539	43.433933
3503.935444	501494.638014	43.438938
3504.129801	501485.192971	43.443943
3504.002444	501467.295365	43.448948
3504.401983	501439.697495	43.453953
3504.068291	501438.535618	43.458957
3503.894820	501418.671242	43.463962
3503.941058	501404.846003	43.468967
3504.263003	501395.127667	43.473972
3504.275039	501370.779731	43.478977
3504.310833	501356.956106	43.483981
3504.154505	501330.103932	43.488986
3504.110280	501323.277925	43.493991
3504.100546	501314.826754	43.498996
3504.180052	501287.937240	43.504001
3503.946773	501269.448784	43.509005
3504.109645	501254.542056	43.514010
3504.218747	501231.545222	43.519015
3504.075435	501228.328591	43.524020
3503.839280	501201.539456	43.529025
3503.778902	501188.490146	43.534029
3504.029767	501179.187858	43.539034
3504.290389	501162.696496	43.544039
3503.908986	501153.443514	43.549044
3504.183403	501134.722822	43.554049
3504.173281	501109.770633	43.559053
3503.771824	501096.724549	43.564058
3503.968227	501087.025889	43.569063
3503.768581	501074.858990	43.574068
3504.012531	501045.969071	43.579073
3503.852935	501046.854935	43.584077
3503.625867	501040.158953	43.589082
3504.255158	501023.001790	43.594087
3503.760430	501012.349376	43.599092
3504.072330	500999.494169	43.604097
3504.119939	500988.654786	43.609101
3503.800791	500969.572187	43.614106
3503.922657	500967.427167	43.619111
3503.736815	500957.130834	43.624116
3504.058686	500919.674121	43.629121
3503.910420	500919.849561	43.634125
3503.823699	500913.485668	43.639130
3504.074317	500882.721597	43.644135
3503.757036	500882.012643	43.649140
3503.797406	500857.457057	43.654145
3503.808449	500871.324594	43.659149
3503.690191	500846.287893	43.664154
3504.040382	500825.732677	43.669159
3503.874310	500821.557840	43.674164
3504.081910	500811.351087	43.679169
3503.717291	500789.643377	43.684173
3503.625356	500779.787655	43.689178
3503.873347	500774.838715	43.694183
3503.433174	500770.454102	43.699188
3503.850299	500739.309143	43.704193
3504.128920	500729.091118	43.709197
3503.898076	500725.584525	43.714202
3503.831542	500716.484018	43.719207
3503.680699	500697.779466	43.724212
3503.700516	500681.578810	43.729217
3503.906103	500675.371101	43.734221
3503.792421	500679.792971	43.739226
3503.696389	500653.993220	43.744231
3503.877050	500642.828890	43.749236
3503.629360	500630.669281	43.754241
3503.984678	500630.512039	43.759245
3503.915570	500622.778575	43.764250
3503.929992	500614.120781	43.769255
3504.164495	500599.860217	43.774260
3504.166816	500581.688134	43.779265
3503.789758	500565.853810	43.784269
3503.703908	500565.766298	43.789274
3504.158249	500538.360846	43.794279
3504.090997	500536.043194	43.799284
3504.155999	500512.141277	43.804289
3504.123859	500479.092764	43.809293
3503.719882	500470.501032	43.814298
3504.059121	500460.526364	43.819303
3503.882647	500459.137097	43.824308
3504.003286	500421.508673	43.829313
3504.032174	500428.590851	43.834317
3504.066482	500417.651987	43.839322
3504.267475	500378.846546	43.844327
3503.944353	500372.114876	43.849332
3503.991730	500369.222279	43.854337
3503.879046	500346.816166	43.859341
3503.607075	500330.306980	43.864346
3504.227376	500328.032484	43.869351
3503.911755	500306.772009	43.874356
3504.117949	500284.770987	43.879361
3503.923102	500286.219268	43.884365
3503.994774	500270.566851	43.889370
3504.153039	500243.967030	43.894375
3503.896771	500243.855833	43.899380
3503.906635	500210.142137	43.904385
3503.938759	500185.738788	43.909389
3503.716106	500193.873201	43.914394
3503.994074	500178.947384	43.919399
3504.096928	500161.619510	43.924404
3503.980452	500146.857249	43.929409
3503.610066	500143.068881	43.934413
3503.620184	500133.652245	43.939418
3504.116000	500102.898697	43.944423
3504.109994	500098.293434	43.949428
3504.121325	500094.950916	43.954433
3504.197232	500071.299783	43.959437
3503.970958	500063.084722	43.964442
3504.008689	500036.199927	43.969447
3503.762428	500019.028334	43.974452
3504.160864	500004.488288	43.979457
3504.191931	500000.990774	43.984461
3504.115752	499979.287106	43.989466
3504.081401	499956.868124	43.994471
3504.120036	499941.271260	43.999476
3504.004671	499923.876407	44.004481
3504.080800	499930.900696	44.009485
3503.705990	499904.384628	44.014490
3503.974147	499885.967340	44.019495
3503.852119	499891.959944	44.024500
3504.042488	499870.517734	44.029505
3504.075290	499855.529158	44.034509
3504.059483	499849.001817	44.039514
3504.246132	499821.485720	44.044519
3504.244703	499808.679185	44.049524
3504.008243	499795.960409	44.054529
3504.098136	499761.878877	44.059533
3504.240244	499743.936950	44.064538
3504.207909	499736.501012	44.069543
3504.003375	499718.765710	44.074548
3504.104275	499708.828297	44.079553
3503.928234	499691.594670	44.084557
3503.874859	499676.163981	44.089562
3503.934397	499652.312400	44.094567
3504.030488	499659.789226	44.099572
3504.018912	499630.076858	44.104577
3503.972975	499622.997368	44.109581
3503.685665	499606.945524	44.114586
3503.538408	499586.923102	44.119591
3503.245661	499581.958062	44.124596
3503.447886	499567.549917	44.129601
3504.109026	499561.624166	44.134605
3503.521409	499564.501350	44.139610
3504.201832	499554.674737	44.144615
3503.965516	499542.057000	44.149620
3504.075345	499515.109407	44.154625
3504.120759	499515.507352	44.159629
3504.109469	499492.324827	44.164634
3504.341924	499470.723625	44.169639
3504.001882	499452.604509	44.174644
3504.516993	499432.173494	44.179649
3504.460943	499413.199509	44.184653
3503.667320	499400.669759	44.189658
3503.929428	499378.760031	44.194663
3503.814357	499366.932950	44.199668
3503.546901	499352.447006	44.204673
3503.643714	499338.257825	44.209677
3503.566237	499343.838597	44.214682
3503.947227	499334.211057	44.219687
3503.932933	499333.302283	44.224692
3503.837686	499294.288211	44.229697
3503.684935	499300.943949	44.234701
3503.804995	499292.673793	44.239706
3504.130586	499267.615350	44.244711
3503.918434	499255.094835	44.249716
3504.120393	499246.153629	44.254721
3504.143770	499225.192640	44.259725
3503.774778	499207.584070	44.264730
3503.915283	499195.868346	44.269735
3503.829851	499197.046309	44.274740
3503.737037	499173.015684	44.279745
3503.971224	499171.257675	44.284749
3503.861026	499164.390649	44.289754
3503.951482	499154.454580	44.294759
3503.808293	499125.420267	44.299764
3503.912987	499119.227968	44.304769
3504.090032	499122.085604	44.309773
3503.817376	499093.324813	44.314778
3504.380780	499071.873311	44.319783
3504.089347	499080.424077	44.324788
3503.887819	499045.476046	44.329793
3504.215668	499026.491597	44.334797
3503.480210	499018.559026	44.339802
3503.868116	498997.185797	44.344807
3503.671874	498987.143084	44.349812
3503.755529	498983.080211	44.354817
3503.798134	498977.606394	44.359821
3503.917181	498957.895537	44.364826
3504.231762	498941.292359	44.369831
3504.100057	498941.060217	44.374836
3503.910990	498917.297577	44.379841
3504.150763	498889.670412	44.384845
3504.193978	498883.588996	44.389850
3504.019424	498862.203263	44.394855
3503.952147	498850.115173	44.399860
3504.148635	498854.842827	44.404865
3504.195164	498822.538170	44.409869
3503.881469	498807.856602	44.414874
3504.153362	498794.854274	44.419879
3503.655940	498773.418221	44.424884
3503.537518	498754.959632	44.429889
3503.708571	498750.123544	44.434893
3503.458747	498751.327520	44.439898
3503.733506	498738.729684	44.444903
3503.737106	498718.935566	44.449908
3503.712835	498710.991696	44.454913
3504.172172	498694.365411	44.459917
3503.821189	498692.193613	44.464922
3504.177794	498658.118455	44.469927
3503.638716	498662.456188	44.474932
3503.590323	498659.730324	44.479937
3503.663725	498646.202404	44.484941
3503.573537	498628.954186	44.489946
3503.659830	498605.704471	44.494951
3503.699997	498612.785584	44.499956
3503.741298	498600.427046	44.504961
3503.628520	498603.482445	44.509965
3503.482669	498592.722815	44.514970
3503.823283	498567.053540	44.519975
3503.614852	498570.731547	44.524980
3503.831884	498565.533777	44.529985
3504.147802	498559.561020	44.534989
3503.354083	498535.792199	44.539994
3503.740428	498532.288868	44.544999
3503.720023	498513.105804	44.550004
3504.016215	498513.919750	44.555009
3504.107606	498496.237714	44.560013
3503.922025	498480.168783	44.565018
3504.336643	498457.879462	44.570023
3503.867339	498449.853945	44.575028
3503.862283	498430.516495	44.580033
3504.171900	498411.939275	44.585037
3503.866913	498401.154059	44.590042
3504.036000	498379.359068	44.595047
3503.631025	498378.613244	44.600052
3503.736320	498366.446928	44.605057
3503.773308	498340.369703	44.610061
3503.485618	498339.453466	44.615066
3503.693467	498328.232778	44.620071
3503.660524	498331.528726	44.625076
3503.714634	498324.129165	44.630081
3503.857184	498296.972079	44.635085
3503.713004	498283.680775	44.640090
3503.668062	498277.309341	44.645095
3503.627482	498278.885271	44.650100
3503.683022	498274.067315	44.655105
3503.914372	498250.338593	44.660109
3503.288976	498251.601964	44.665114
3503.706460	498239.841840	44.670119
3503.802349	498243.826186	44.675124
3503.959338	498226.437265	44.680129
3503.890832	498207.666477	44.685133
3503.557053	498201.897542	44.690138
3503.921648	498188.627001	44.695143
3503.794948	498176.699726	44.700148
3503.411537	498149.929301	44.705153
3503.316714	498145.084451	44.710157
3503.567885	498145.753655	44.715162
3503.674744	498144.825671	44.720167
3503.693596	498147.809717	44.725172
3503.466891	498137.720718	44.730177
3503.690154	498116.119346	44.735181
3503.897367	498099.532366	44.740186
3504.032666	498085.892992	44.745191
3503.260585	498099.278949	44.750196
3503.764804	498080.468129	44.755201
3503.733706	498061.033149	44.760205
3503.599220	498057.105798	44.765210
3503.627796	498054.215801	44.770215
3503.954251	498057.910620	44.775220
3503.867013	498042.838257	44.780225
3503.681272	498013.403875	44.785229
3503.527828	498008.770756	44.790234
3503.664589	498000.193616	44.795239
3503.653429	498010.674974	44.800244
3503.589670	497993.573848	44.805249
3503.789520	497963.774686	44.810253
3503.572518	497967.150419	44.815258
3503.797177	497958.306239	44.820263
3503.678934	497955.085054	44.825268
3503.866528	497937.842895	44.830273
3503.525813	497911.571623	44.835277
3503.643483	497902.491198	44.840282
3503.853137	497904.989495	44.845287
3503.705032	497899.545495	44.850292
3503.736207	497896.199431	44.855297
3503.948624	497867.613140	44.860301
3503.786525	497873.562122	44.865306
3503.843451	497863.478765	44.870311
3503.732483	497843.853673	44.875316
3504.078370	497827.598905	44.880321
3504.057107	497823.957362	44.885325
3503.972619	497815.161976	44.890330
3503.705097	497785.588271	44.895335
3503.742973	497777.786045	44.900340
3503.794795	497783.346862	44.905345
3503.980651	497763.674767	44.910349
3503.985423	497748.435738	44.915354
3503.968144	497728.947591	44.920359
3503.906526	497736.450145	44.925364
3503.773041	497714.550298	44.930369
3503.833132	497693.024838	44.935373
3503.537958	497698.387397	44.940378
3503.622198	497697.867975	44.945383
3503.516578	497679.001251	44.950388
3503.364128	497666.217062	44.955393
3503.696277	497645.458564	44.960397
3503.550362	497647.456209	44.965402
3503.603136	497644.612948	44.970407
3503.643469	497642.581675	44.975412
3503.248581	497636.366580	44.980417
3503.620253	497639.902458	44.985421
3503.545390	497621.587703	44.990426
3503.638910	497594.032300	44.995431
3503.516766	497598.304384	45.000436
3503.572732	497601.383906	45.005441
3503.519962	497601.493654	45.010445
3503.617078	497602.035350	45.015450
3503.735824	497584.044340	45.020455
3503.505661	497567.171618	45.025460
3503.608951	497566.902314	45.030465
3503.837847	497563.980577	45.035469
3503.738395	497557.921264	45.040474
3504.186994	497543.320683	45.045479
3503.943010	497532.829065	45.050484
3503.768653	497527.287848	45.055489
3504.149496	497492.244757	45.060493
3504.150132	497478.524957	45.065498
3503.844662	497469.106182	45.070503
3504.023007	497447.207352	45.075508
3503.978123	497431.570890	45.080513
3503.745562	497421.178655	45.085517
3503.738327	497413.687163	45.090522
3503.659913	497390.310037	45.095527
3503.831758	497382.688974	45.100532
3503.553511	497384.555682	45.105537
3503.899932	497373.818771	45.110541
3503.632921	497352.648370	45.115546
3503.632588	497344.193844	45.120551
3504.060189	497325.647488	45.125556
3503.606431	497326.985044	45.130561
3504.043975	497314.259234	45.135565
3503.885885	497301.475678	45.140570
3504.014281	497279.938931	45.145575
3503.777125	497278.407123	45.150580
3503.695578	497261.358743	45.155585
3503.817224	497238.658584	45.160589
3503.826375	497244.631332	45.165594
3503.819316	497234.658994	45.170599
3503.787056	497209.704888	45.175604
3503.881196	497190.704826	45.180609
3503.980886	497191.144873	45.185613
3503.483044	497185.857191	45.190618
3503.788214	497171.481493	45.195623
3503.926337	497159.258549	45.200628
3503.464975	497157.559658	45.205633
3503.662062	497151.250827	45.210637
3503.899320	497137.240230	45.215642
3503.487220	497112.801678	45.220647
3503.776323	497104.098780	45.225652
3503.670731	497101.331094	45.230657
3503.741509	497087.346772	45.235661
3503.500486	497090.726463	45.240666
3503.784784	497066.835939	45.245671
3503.723324	497058.593452	45.250676
3503.380157	497053.129400	45.255681
3503.865234	497053.508535	45.260685
3503.572407	497046.770824	45.265690
3503.765140	497032.817812	45.270695
3503.659555	497022.759675	45.275700
3503.487872	497009.370525	45.280705
3503.640951	497008.030153	45.285709
3503.265099	497016.645862	45.290714
3503.471609	497002.386881	45.295719
3503.932715	497002.061013	45.300724
3503.827021	496974.131131	45.305729
3503.876996	496973.313336	45.310733
3503.851898	496969.469714	45.315738
3503.757116	496942.094969	45.320743
3503.831045	496929.983274	45.325748
3503.822599	496918.947787	45.330753
3503.919949	496920.400777	45.335757
3503.871497	496902.891174	45.340762
3503.765577	496881.947903	45.345767
3503.710827	496880.944143	45.350772
3503.757560	496872.380700	45.355777
3503.705299	496864.440442	45.360781
3503.704347	496839.835279	45.365786
3503.860417	496835.861737	45.370791
3503.941891	496830.988669	45.375796
3503.638495	496826.024547	45.380801
3503.976718	496788.151633	45.385805
3503.880534	496789.483337	45.390810
3503.889885	496797.683863	45.395815
3503.942399	496772.766386	45.400820
3503.747337	496753.659692	45.405825
3503.611022	496743.960659	45.410829
3503.371779	496748.757738	45.415834
3503.633493	496737.881955	45.420839
3503.528627	496723.570714	45.425844
3503.809299	496704.540661	45.430849
3504.008950	496694.029064	45.435853
3503.710818	496693.114391	45.440858
3503.708146	496689.469681	45.445863
3503.622814	496657.587032	45.450868
3503.738938	496661.922933	45.455873
3504.080947	496651.540698	45.460877
3503.848470	496639.122836	45.465882
3503.989718	496617.735160	45.470887
3503.808484	496610.270839	45.475892
3503.647371	496605.233538	45.480897
3504.145390	496592.649554	45.485901
3503.912136	496572.232345	45.490906
3503.854820	496560.242407	45.495911
3503.966908	496557.085826	45.500916
3503.632881	496528.280020	45.505921
3503.829775	496516.249873	45.510925
3503.890862	496511.886238	45.515930
3503.862681	496504.802718	45.520935
3503.788788	496477.423970	45.525940
3503.788113	496476.766047	45.530945
3504.041346	496452.474591	45.535949
3503.700895	496448.275666	45.540954
3503.431413	496438.445629	45.545959
3503.844140	496419.647554	45.550964
3503.802332	496418.337944	45.555969
3503.792283	496419.858579	45.560973
3503.852300	496393.066096	45.565978
3503.703410	496374.255484	45.570983
3504.085106	496365.132560	45.575988
3503.789164	496366.597128	45.580993
3503.852882	496346.537765	45.585997
3503.747014	496331.213774	45.591002
3503.702791	496329.448869	45.596007
3503.627721	496327.587580	45.601012
3503.494907	496300.876070	45.606017
3503.827206	496281.786785	45.611021
3503.685468	496278.720905	45.616026
3503.814467	496267.663299	45.621031
3503.385794	496282.262060	45.626036
3503.430279	496269.192607	45.631041
3503.520033	496252.723767	45.636045
3503.363114	496244.495999	45.641050
3503.748862	496246.004720	45.646055
3504.072472	496243.877886	45.651060
3503.744855	496248.081502	45.656065
3503.829546	496225.993482	45.661069
3503.707084	496208.596170	45.666074
3503.710135	496202.925245	45.671079
3504.057541	496200.187080	45.676084
3503.760730	496177.652999	45.681089
3503.709655	496155.890136	45.686093
3503.639306	496157.319064	45.691098
3503.817709	496150.202753	45.696103
3503.788133	496141.752289	45.701108
3503.691464	496127.996219	45.706113
3504.045195	496104.599765	45.711117
3503.607689	496106.947449	45.716122
3503.893474	496091.561352	45.721127
3503.632098	496065.021708	45.726132
3503.380423	496068.403270	45.731137
3503.814580	496052.892427	45.736141
3503.448497	496055.887029	45.741146
3503.305966	496064.466307	45.746151
3503.663590	496061.118938	45.751156
3503.772402	496045.203836	45.756161
3503.562411	496021.187546	45.761165
3503.408927	496018.832310	45.766170
3503.481168	496009.910014	45.771175
3503.980464	496000.768321	45.776180
3503.530601	495995.573966	45.781185
3503.812183	495974.213985	45.786189
3503.694501	495974.890943	45.791194
3504.038247	495964.406782	45.796199
3503.977247	495953.885326	45.801204
3504.005055	495933.172981	45.806209
3503.913925	495909.441543	45.811213
3503.504286	495922.417386	45.816218
3503.377396	495909.830443	45.821223
3503.546224	495883.678218	45.826228
3503.688557	495877.732020	45.831233
3503.781771	495869.312653	45.836237
3503.617333	495869.946374	45.841242
3503.666689	495868.166634	45.846247
3503.546784	495846.262387	45.851252
3503.184954	495839.332607	45.856257
3503.297960	495820.226870	45.861261
3503.207107	495819.178126	45.866266
3503.579076	495826.055989	45.871271
3503.551197	495827.376966	45.876276
3503.543470	495823.479726	45.881281
3503.995684	495817.636424	45.886285
3503.620058	495804.076095	45.891290
3503.702794	495789.380046	45.896295
3503.761048	495780.763638	45.901300
3503.595741	495786.511281	45.906305
3503.806747	495771.136734	45.911309
3503.592846	495750.513018	45.916314
3503.462798	495734.483504	45.921319
3503.480822	495728.911329	45.926324
3503.525324	495729.106976	45.931329
3503.431923	495724.008096	45.936333
3503.749056	495728.211185	45.941338
3503.792263	495715.495959	45.946343
3503.840224	495700.957231	45.951348
3503.751009	495699.958852	45.956353
3503.915250	495681.705613	45.961357
3503.346518	495687.314525	45.966362
3503.730419	495678.646597	45.971367
3504.027700	495649.638353	45.976372
3503.705799	495650.246338	45.981377
3503.870692	495639.233309	45.986381
3503.281014	495624.997833	45.991386
3503.186761	495609.165080	45.996391
3503.482421	495597.169349	46.001396
3503.913921	495606.569487	46.006401
3503.877670	495587.031410	46.011405
3503.536544	495601.262452	46.016410
3503.425245	495599.862502	46.021415
3503.742738	495572.825590	46.026420
3503.523924	495565.974365	46.031425
3503.416269	495556.523329	46.036429
3503.627592	495547.629456	46.041434
3503.521691	495555.139908	46.046439
3503.751253	495544.876083	46.051444
3503.246599	495541.057326	46.056449
3503.289229	495521.304182	46.061453
3503.034823	495531.673521	46.066458
3503.080311	495519.616018	46.071463
3503.427806	495515.156242	46.076468
3503.120445	495517.787223	46.081473
3503.577411	495518.980956	46.086477
3503.506677	495514.030331	46.091482
3503.580648	495521.157940	46.096487
3503.706839	495510.556009	46.101492
3503.292981	495519.482222	46.106497
3503.806003	495500.616719	46.111501
3503.661484	495484.994332	46.116506
3503.765943	495470.294593	46.121511
3503.736368	495465.641243	46.126516
3503.795893	495456.366261	46.131521
3503.770152	495451.914831	46.136525
3503.973838	495422.313431	46.141530
3503.668874	495419.728898	46.146535
3503.609069	495414.675253	46.151540
3503.513988	495429.525761	46.156545
3503.796690	495396.975146	46.161549
3503.505236	495381.831589	46.166554
3503.571361	495389.770611	46.171559
3503.872068	495382.786569	46.176564
3503.500379	495373.073376	46.181569
3503.687204	495359.525080	46.186573
3503.634885	495348.191780	46.191578
3503.398819	495326.659699	46.196583
3503.612489	495329.714680	46.201588
3503.414330	495327.011987	46.206593
3503.694850	495321.499462	46.211597
3503.589426	495303.288468	46.216602
3503.392788	495293.851361	46.221607
3503.507373	495281.529614	46.226612
3503.470671	495281.029242	46.231617
3503.675017	495274.161655	46.236621
3503.279983	495282.730577	46.241626
3503.641257	495277.964769	46.246631
3503.811296	495274.343111	46.251636
3503.309584	495258.473190	46.256641
3503.506610	495241.176355	46.261645
3503.417211	495234.760247	46.266650
3503.677737	495237.706572	46.271655
3503.942592	495235.993974	46.276660
3503.847186	495223.806646	46.281665
3503.825364	495193.481024	46.286669
3503.341398	495202.621004	46.291674
3503.550381	495187.145021	46.296679
3504.034268	495184.891466	46.301684
3503.573863	495178.584613	46.306689
3503.650307	495151.585179	46.311693
3503.653735	495139.331540	46.316698
3503.919608	495140.504870	46.321703
3503.969550	495141.003464	46.326708
3503.522238	495117.074127	46.331713
3503.534004	495100.414042	46.336717
3503.408118	495101.497396	46.341722
3503.619490	495090.628591	46.346727
3503.394946	495084.233792	46.351732
3502.871361	495098.342163	46.356737
3503.246653	495088.156315	46.361741
3503.307305	495097.108998	46.366746
3503.660031	495092.952095	46.371751
3503.657953	495074.167570	46.376756
3503.979857	495054.369781	46.381761
3503.785433	495052.020891	46.386765
3503.588753	495049.925524	46.391770
3503.405216	495042.157122	46.396775
3503.791956	495025.387067	46.401780
3503.475429	495007.411680	46.406785
3503.728210	495012.283344	46.411789
3503.516282	495003.861176	46.416794
3503.341058	495008.496689	46.421799
3503.689690	494990.922487	46.426804
3503.705960	494994.970766	46.431809
3503.489127	494972.776991	46.436813
3503.536938	494957.832626	46.441818
3503.649527	494950.118647	46.446823
3503.767972	494949.036770	46.451828
3503.379198	494945.908444	46.456833
3503.443142	494949.240324	46.461837
3503.731199	494916.485474	46.466842
3503.762466	494907.619751	46.471847
3503.732014	494906.510773	46.476852
3503.598357	494914.937284	46.481857
3503.748235	494899.774204	46.486861
3503.557722	494877.576153	46.491866
3503.443634	494870.910649	46.496871
3503.836523	494865.076423	46.501876
3503.765146	494854.454707	46.506881
3503.758564	494865.595396	46.511885
3503.587602	494831.495193	46.516890
3503.489464	494823.763835	46.521895
3503.796161	494820.677463	46.526900
3503.933281	494811.237987	46.531905
3503.688767	494812.947718	46.536909
3503.602327	494791.290088	46.541914
3503.559157	494796.157954	46.546919
3503.690478	494775.883646	46.551924
3503.673770	494778.316887	46.556929
3503.764568	494779.568548	46.561933
3503.940105	494759.388501	46.566938
3503.526407	494743.706758	46.571943
3503.541449	494742.337407	46.576948
3503.359893	494733.150798	46.581953
3503.571406	494737.573349	46.586957
3503.403728	494735.523996	46.591962
3503.396937	494737.803773	46.596967
3504.026104	494698.969125	46.601972
3503.613943	494703.743434	46.606977
3503.551206	494688.259344	46.611981
3503.513735	494693.987123	46.616986
3503.260207	494693.217198	46.621991
3503.244944	494697.574334	46.626996
3503.288994	494694.023110	46.632001
3503.697407	494674.160603	46.637005
3503.606965	494653.819942	46.642010
3503.559284	494644.004512	46.647015
3503.851585	494637.730402	46.652020
3503.467614	494644.728197	46.657025
3503.616582	494636.957702	46.662029
3503.780931	494609.994211	46.667034
3503.469109	494609.891748	46.672039
3503.523712	494593.832049	46.677044
3503.396005	494598.308250	46.682049
3503.585169	494596.405019	46.687053
3503.608482	494589.464521	46.692058
3503.327156	494583.027886	46.697063
3503.948109	494568.347057	46.702068
3503.675857	494550.060413	46.707073
3503.479687	494548.775066	46.712077
3503.926618	494542.071404	46.717082
3503.711339	494542.206855	46.722087
3503.831699	494509.427151	46.727092
3503.672133	494520.085880	46.732097
3503.706074	494508.434616	46.737101
3503.683350	494498.463259	46.742106
3503.621883	494500.042816	46.747111
3503.991462	494469.400956	46.752116
3503.491430	494469.024430	46.757121
3503.397269	494471.723130	46.762125
3503.538039	494462.130992	46.767130
3503.606988	494462.626600	46.772135
3503.823542	494431.249337	46.777140
3503.250654	494423.542213	46.782145
3503.594329	494423.285505	46.787149
3503.233454	494416.810749	46.792154
3503.528962	494419.599772	46.797159
3503.703145	494409.698514	46.802164
3503.705562	494418.913910	46.807169
3503.666780	494390.868228	46.812173
3503.526223	494373.674570	46.817178
3503.490131	494372.566451	46.822183
3503.772171	494362.850661	46.827188
3503.475639	494365.530728	46.832193
3503.777790	494359.204331	46.837197
3503.776690	494340.520172	46.842202
3503.553399	494334.124911	46.847207
3503.736656	494321.234675	46.852212
3503.669307	494312.738701	46.857217
3503.795331	494307.452836	46.862221
3503.692105	494289.392394	46.867226
3503.470244	494279.249851	46.872231
3503.954054	494262.868843	46.877236
3503.566466	494281.361649	46.882241
3503.722778	494259.614387	46.887245
3503.882248	494238.778044	46.892250
3503.686187	494242.708143	46.897255
3503.812503	494237.928570	46.902260
3503.895814	494239.130815	46.907265
3503.770473	494213.123975	46.912269
3504.175244	494191.185453	46.917274
3503.868994	494183.587990	46.922279
3504.058836	494161.987221	46.927284
3503.628871	494157.346189	46.932289
3503.486226	494145.216246	46.937293
3503.714232	494143.003013	46.942298
3503.504236	494132.605333	46.947303
3503.486559	494103.593792	46.952308
3503.378504	494102.345122	46.957313
3503.596551	494101.298089	46.962317
3503.691410	494095.763909	46.967322
3503.415791	494095.554448	46.972327
3503.832174	494085.766642	46.977332
3503.719181	494080.923581	46.982337
3503.440087	494064.460437	46.987341
3503.590290	494066.209120	46.992346
3503.306709	494061.291744	46.997351
3503.333289	494052.882076	47.002356
3503.512727	494059.385949	47.007361
3503.741193	494061.223534	47.012365
3503.763003	494042.636724	47.017370
3503.681275	494020.167259	47.022375
3503.881911	494008.793149	47.027380
3503.401039	494013.882314	47.032385
3503.532643	494016.596033	47.037389
3503.615579	494000.328791	47.042394
3503.343764	493976.319589	47.047399
3503.643817	493963.360006	47.052404
3503.578481	493969.851963	47.057409
3503.792402	493956.703443	47.062413
3503.681321	493967.000372	47.067418
3503.468183	493956.299270	47.072423
3503.872586	493920.992430	47.077428
3503.873724	493921.701318	47.082433
3503.605400	493917.085312	47.087437
3504.032870	493912.966968	47.092442
3503.412910	493891.139421	47.097447
3503.495437	493876.441874	47.102452
3503.639181	493886.394750	47.107457
3503.735661	493876.505487	47.112461
3503.646697	493869.430554	47.117466
3503.516576	493860.792383	47.122471
3503.703786	493828.304720	47.127476
3503.559268	493836.733442	47.132481
3503.714218	493812.302112	47.137485
3503.891801	493814.654134	47.142490
3503.613167	493808.571259	47.147495
3503.520569	493790.863106	47.152500
3503.556349	493777.691979	47.157505
3503.629634	493775.098061	47.162509
3503.829583	493783.117901	47.167514
3503.323956	493781.729501	47.172519
3503.783793	493768.440704	47.177524
3503.417147	493749.509900	47.182529
3503.832961	493736.785047	47.187533
3503.844285	493726.807889	47.192538
3503.759047	493736.240031	47.197543
3503.590301	493711.758457	47.202548
3503.404017	493704.040559	47.207553
3503.435260	493694.262784	47.212557
3503.627957	493691.751255	47.217562
3503.915084	493689.832447	47.222567
3504.177682	493675.713925	47.227572
3503.734034	493660.795549	47.232577
3503.656793	493645.768609	47.237581
3503.693801	493638.015390	47.242586
3503.636545	493635.745910	47.247591
3503.552712	493616.466443	47.252596
3503.694594	493602.974596	47.257601
3503.596473	493600.914121	47.262605
3503.964747	493587.437116	47.267610
3503.641471	493584.753940	47.272615
3503.901754	493566.230230	47.277620
3503.607279	493557.567257	47.282625
3503.479590	493552.523828	47.287629
3503.594317	493547.897822	47.292634
3503.641501	493539.282112	47.297639
3503.932831	493531.944389	47.302644
3503.329240	493524.241737	47.307649
3503.590451	493502.730191	47.312653
3503.419147	493503.010611	47.317658
3503.271598	493498.628599	47.322663
3503.715626	493497.900279	47.327668
3503.510675	493510.237812	47.332673
3503.327910	493486.112619	47.337677
3503.608187	493464.192911	47.342682
3503.312325	493455.732660	47.347687
3503.694668	493448.785623	47.352692
3503.502492	493461.070532	47.357697
3503.929911	493450.065336	47.362701
3503.775836	493443.861376	47.367706
3503.526922	493428.506928	47.372711
3503.829875	493409.571213	47.377716
3503.890778	493406.118354	47.382721
3503.627425	493412.641805	47.387725
3503.796488	493381.067709	47.392730
3503.734221	493359.809678	47.397735
3504.056314	493360.923601	47.402740
3503.767085	493362.032873	47.407745
3503.441204	493345.576481	47.412749
3503.661640	493339.009461	47.417754
3503.508075	493336.147508	47.422759
3503.661052	493329.894977	47.427764
3503.773932	493326.484525	47.432769
3503.504181	493318.020084	47.437773
3503.606510	493294.204045	47.442778
3503.390307	493282.135799	47.447783
3503.531753	493283.227641	47.452788
3503.713838	493284.768806	47.457793
3503.772669	493280.657951	47.462797
3504.165750	493266.619770	47.467802
3503.964184	493253.890892	47.472807
3504.012330	493235.906767	47.477812
3503.856792	493237.298746	47.482817
3503.613863	493200.219222	47.487821
3503.438233	493187.435559	47.492826
3503.531963	493183.926831	47.497831
3503.591454	493182.297145	47.502836
3503.476940	493185.454998	47.507841
3503.725758	493177.971938	47.512845
3503.924122	493151.051576	47.517850
3503.544300	493147.972162	47.522855
3503.562567	493132.220765	47.527860
3503.423765	493138.319516	47.532865
3503.669266	493139.344281	47.537869
3503.764202	493108.692934	47.542874
3503.769385	493099.475992	47.547879
3503.676102	493087.236272	47.552884
3503.361993	493084.906045	47.557889
3503.391897	493093.611369	47.562893
3503.635996	493082.837488	47.567898
3503.388980	493065.558157	47.572903
3503.635752	493049.466738	47.577908
3503.535050	493048.470029	47.582913
3503.436920	493051.169563	47.587917
3503.603466	493045.876933	47.592922
3503.341092	493041.107848	47.597927
3503.604748	493046.585987	47.602932
3503.587740	493033.017560	47.607937
3503.175835	493022.853722	47.612941
3503.394192	493005.196943	47.617946
3503.538579	493004.364050	47.622951
3503.822748	492994.900402	47.627956
3503.798111	492992.575048	47.632961
3503.471619	492996.981778	47.637965
3503.636788	492961.812199	47.642970
3503.749710	492963.718798	47.647975
3503.511933	492958.388771	47.652980
3503.503756	492952.009667	47.657985
3503.137185	492959.866214	47.662989
3503.453379	492952.828168	47.667994
3503.132376	492961.892855	47.672999
3503.140659	492951.460006	47.678004
3503.053300	492954.613606	47.683009
3502.927792	492952.911862	47.688013
3503.135059	492943.510982	47.693018
3502.942166	492954.986111	47.698023
3503.561258	492945.013746	47.703028
3503.213302	492952.512878	47.708033
3503.551486	492951.396154	47.713037
3503.714656	492939.824752	47.718042
3503.402921	492930.100784	47.723047
3503.070274	492909.340726	47.728052
3503.265585	492908.246581	47.733057
3503.241282	492907.946741	47.738061
3503.555713	492908.960625	47.743066
3503.220524	492904.709408	47.748071
3503.390369	492902.960976	47.753076
3503.274636	492901.004485	47.758081
3503.147674	492898.340817	47.763085
3503.468371	492896.821738	47.768090
3503.474321	492897.833742	47.773095
3503.528540	492893.115856	47.778100
3503.798204	492890.440135	47.783105
3503.587149	492874.370289	47.788109
3503.757623	492854.897913	47.793114
3503.406014	492871.411497	47.798119
3503.942535	492850.159514	47.803124
3503.734294	492842.799203	47.808129
3503.595945	492827.325499	47.813133
3503.749482	492809.780059	47.818138
3503.355206	492810.247650	47.823143
3503.648338	492814.100729	47.828148
3503.353046	492807.311199	47.833153
3503.416096	492807.250748	47.838157
3503.328263	492782.957712	47.843162
3503.347917	492777.131186	47.848167
3503.263675	492769.548686	47.853172
3503.537240	492769.505601	47.858177
3503.207225	492752.036537	47.863181
3503.354452	492759.558758	47.868186
3503.514496	492759.685536	47.873191
3503.471719	492762.376363	47.878196
3503.631271	492762.300659	47.883201
3503.491467	492755.992932	47.888205
3503.646333	492739.915771	47.893210
3503.402626	492729.016227	47.898215
3503.467731	492720.144103	47.903220
3503.741474	492704.959641	47.908225
3503.415181	492724.254554	47.913229
3503.480647	492709.457495	47.918234
3503.589358	492706.351429	47.923239
3503.428584	492694.476597	47.928244
3503.644667	492682.795391	47.933249
3503.465185	492676.797748	47.938253
3504.031265	492665.820812	47.943258
3503.470930	492667.580657	47.948263
3503.686218	492665.014778	47.953268
3503.519044	492653.343492	47.958273
3503.060821	492633.615774	47.963277
3503.700634	492617.563136	47.968282
3503.585042	492623.303906	47.973287
3503.537454	492613.031618	47.978292
3503.512942	492616.529823	47.983297
3503.367204	492628.706663	47.988301
3503.717061	492617.814515	47.993306
3503.482896	492603.216652	47.998311
3503.311034	492593.267837	48.003316
3503.588192	492592.211379	48.008321
3503.469535	492588.989309	48.013325
3503.601673	492585.828879	48.018330
3503.263385	492591.655499	48.023335
3503.142816	492577.090300	48.028340
3503.425563	492579.273939	48.033345
3503.460406	492571.318053	48.038349
3503.360114	492571.283420	48.043354
3503.298934	492545.213446	48.048359
3503.512134	492537.583838	48.053364
3503.522331	492525.833795	48.058369
3503.414200	492531.978537	48.063373
3503.561945	492533.018789	48.068378
3503.560168	492526.435965	48.073383
3503.856610	492530.339220	48.078388
3503.625845	492512.803601	48.083393
3503.473142	492500.724807	48.088397
3503.821762	492491.706481	48.093402
3503.650593	492491.784331	48.098407
3503.725097	492490.506696	48.103412
3503.910385	492470.423887	48.108417
3503.551169	492450.680325	48.113421
3504.151955	492444.711200	48.118426
3503.770246	492438.796085	48.123431
3503.951372	492425.651662	48.128436
3503.989802	492397.388184	48.133441
3503.700475	492391.053325	48.138445
3503.747057	492393.476878	48.143450
3503.764991	492374.433234	48.148455
3503.508760	492356.243161	48.153460
3503.568176	492355.676874	48.158465
3503.490025	492349.308622	48.163469
3503.728407	492343.396746	48.168474
3503.481223	492340.296231	48.173479
3503.300357	492315.510877	48.178484
3503.677986	492308.108390	48.183489
3503.417318	492302.022176	48.188493
3503.574421	492296.477620	48.193498
3503.483754	492295.783130	48.198503
3503.309844	492297.481929	48.203508
3503.664956	492285.272088	48.208513
3503.733553	492291.996669	48.213517
3503.658454	492263.599009	48.218522
3503.620215	492260.364171	48.223527
3503.645601	492252.814774	48.228532
3503.709352	492254.222806	48.233537
3503.533913	492254.757103	48.238541
3503.571300	492222.695432	48.243546
3503.156371	492225.343877	48.248551
3503.452578	492222.005529	48.253556
3503.161916	492211.366308	48.258561
3503.226921	492207.710012	48.263565
3503.851852	492198.698512	48.268570
3503.501264	492209.236840	48.273575
3503.876854	492203.657723	48.278580
3503.649624	492185.513539	48.283585
3503.533525	492172.719765	48.288589
3503.822775	492156.823425	48.293594
3503.334587	492164.142473	48.298599
3503.598527	492158.429065	48.303604
3503.613117	492164.706456	48.308609
3503.407328	492137.494013	48.313613
3503.720204	492130.101690	48.318618
3503.671915	492119.626673	48.323623
3503.522228	492109.623452	48.328628
3503.803078	492116.263906	48.333633
3503.396063	492101.541044	48.338637
3503.615874	492075.983055	48.343642
3503.552345	492065.814267	48.348647
3503.146991	492069.777905	48.353652
3503.533784	492061.462321	48.358657
3503.546428	492060.245076	48.363661
3503.570643	492062.064506	48.368666
3503.642330	492069.801514	48.373671
3503.953556	492038.962286	48.378676
3503.713350	492027.504716	48.383681
3503.477069	492030.985862	48.388685
3504.030314	492017.934259	48.393690
3503.575506	492016.132552	48.398695
3503.482638	491982.065380	48.403700
3503.589636	491977.440204	48.408705
3503.702381	491980.562340	48.413709
3503.711131	491974.484075	48.418714
3503.413558	491978.430697	48.423719
3503.519906	491962.765668	48.428724
3503.711001	491931.033693	48.433729
3503.467201	491938.314201	48.438733
3503.740557	491933.206941	48.443738
3503.755339	491930.014307	48.448743
3503.910605	491919.658930	48.453748
3503.611439	491898.487308	48.458753
3503.479132	491887.468376	48.463757
3503.972636	491882.022451	48.468762
3503.657308	491885.971898	48.473767
3503.697357	491879.939298	48.478772
3503.987618	491857.762904	48.483777
3503.714819	491849.804693	48.488781
3503.731114	491844.636755	48.493786
3503.582703	491853.269562	48.498791
3503.480719	491820.672162	48.503796
3503.390596	491809.342662	48.508801
3503.166758	491810.745542	48.513805
3503.299815	491801.760955	48.518810
3503.066060	491798.253085	48.523815
3503.447673	491782.595038	48.528820
3503.565179	491799.389923	48.533825
3503.101442	491789.284240	48.538829
3503.440434	491788.521819	48.543834
3503.458467	491787.050491	48.548839
3503.319757	491796.492071	48.553844
3503.712732	491788.935026	48.558849
3503.617355	491770.060600	48.563853
3503.693365	491760.173444	48.568858
3503.490932	491757.622825	48.573863
3503.368273	491758.250078	48.578868
3503.235373	491744.648384	48.583873
3503.470970	491751.498693	48.588877
3503.947924	491739.167950	48.593882
3503.549315	491723.734462	48.598887
3503.597962	491711.319472	48.603892
3503.552765	491703.122652	48.608897
3503.466508	491704.605079	48.613901
3503.542726	491697.249992	48.618906
3503.403516	491701.120998	48.623911
3503.422610	491695.192936	48.628916
3503.494469	491672.291201	48.633921
3503.108165	491677.771194	48.638925
3503.239903	491667.621966	48.643930
3503.313404	491670.395858	48.648935
3503.210648	491661.752333	48.653940
3503.416134	491666.125934	48.658945
3503.077312	491675.295348	48.663949
3503.195816	491657.349215	48.668954
3503.180486	491660.542291	48.673959
3503.170662	491661.404927	48.678964
3503.153562	491660.951999	48.683969
3502.956359	491666.300821	48.688973
3503.541333	491655.168377	48.693978
3503.214166	491665.348810	48.698983
3503.550662	491652.229926	48.703988
3503.587843	491657.187203	48.708993
3503.463438	491658.878236	48.713997
3503.591867	491653.743164	48.719002
3503.272599	491633.283416	48.724007
3502.840280	491618.614812	48.729012
3503.365296	491624.912993	48.734017
3503.079262	491624.350643	48.739021
3503.742935	491607.584366	48.744026
3503.505443	491613.851144	48.749031
3503.674119	491602.480611	48.754036
3503.664511	491607.445297	48.759041
3503.398947	491611.944008	48.764045
3503.433824	491600.138836	48.769050
3503.503089	491608.382849	48.774055
3503.410662	491582.822894	48.779060
3503.650140	491564.806907	48.784065
3503.477626	491567.872915	48.789069
3503.412944	491560.084257	48.794074
3503.422112	491560.336178	48.799079
3503.275874	491564.410895	48.804084
3503.518349	491561.789926	48.809089
3503.409785	491566.061261	48.814093
3503.729489	491542.309902	48.819098
3503.803452	491527.611846	48.824103
3503.776035	491515.259391	48.829108
3503.701216	491517.449030	48.834113
3503.400644	491522.459729	48.839117
3503.758254	491507.412964	48.844122
3503.396092	491486.757262	48.849127
3503.594036	491471.229272	48.854132
3503.537323	491472.251258	48.859137
3503.571238	491474.879506	48.864141
3503.794531	491465.880494	48.869146
3503.578907	491451.987801	48.874151
3503.359341	491435.209044	48.879156
3503.832559	491421.258092	48.884161
3503.463892	491432.610012	48.889165
3503.819337	491421.159205	48.894170
3503.641024	491427.315405	48.899175
3503.421860	491404.864488	48.904180
3503.864448	491394.919197	48.909185
3503.571355	491387.014638	48.914189
3503.939014	491385.538660	48.919194
3503.625769	491372.724853	48.924199
3503.629407	491366.799129	48.929204
3503.648664	491334.992013	48.934209
3503.484764	491337.347685	48.939213
3503.539033	491331.920384	48.944218
3503.349393	491326.126484	48.949223
3503.250087	491325.230748	48.954228
3503.592237	491322.847210	48.959233
3503.265922	491333.635414	48.964237
3503.537501	491309.384928	48.969242
3503.336806	491310.530969	48.974247
3503.113454	491300.437667	48.979252
3503.416245	491288.387375	48.984257
3503.569987	491296.162380	48.989261
3503.433392	491295.120605	48.994266
3503.287049	491282.584218	48.999271
3503.491941	491286.907358	49.004276
3503.794307	491275.819359	49.009281
3503.281455	491296.461979	49.014285
3503.384446	491268.794307	49.019290
3503.560859	491250.129614	49.024295
3503.393377	491246.206013	49.029300
3503.797849	491231.354195	49.034305
3503.762124	491236.019244	49.039309
3503.975950	491230.921202	49.044314
3503.923175	491220.598320	49.049319
3503.545975	491194.880267	49.054324
3503.426223	491201.229861	49.059329
3503.340018	491195.672792	49.064333
3503.481111	491199.195732	49.069338
3503.421936	491192.874728	49.074343
3503.254711	491194.572570	49.079348
3503.456802	491162.634972	49.084353
3503.584352	491163.577206	49.089357
3503.508443	491142.420079	49.094362
3503.426397	491150.181769	49.099367
3503.388994	491146.946605	49.104372
3503.639599	491139.918245	49.109377
3503.382481	491151.556569	49.114381
3503.575811	491144.284041	49.119386
3503.577480	491121.088858	49.124391
3503.196559	491115.882214	49.129396
3503.299514	491104.724344	49.134401
3503.304745	491115.055115	49.139405
3503.561389	491113.748596	49.144410
3503.590266	491110.401661	49.149415
3503.598063	491113.996331	49.154420
3503.703349	491102.787446	49.159425
3503.286603	491089.837871	49.164429
3503.609674	491061.932529	49.169434
3503.771471	491067.629933	49.174439
3503.374485	491054.170765	49.179444
3503.691804	491050.170494	49.184449
3503.560315	491047.405985	49.189453
3503.431475	491040.944007	49.194458
3503.550263	491023.199797	49.199463
3503.182720	491014.496535	49.204468
3503.751584	491013.849684	49.209473
3503.440419	491013.392576	49.214477
3503.400953	491006.004857	49.219482
3503.496026	491009.636396	49.224487
3503.482426	491009.891924	49.229492
3503.486600	490991.760643	49.234497
3503.382768	490981.901501	49.239501
3503.187774	490968.714211	49.244506
3503.358679	490962.508697	49.249511
3503.203326	490970.585917	49.254516
3503.938800	490957.048970	49.259521
3503.575231	490960.043986	49.264525
3503.702238	490960.226645	49.269530
3504.033294	490951.868734	49.274535
3503.438920	490935.908441	49.279540
3503.747107	490931.504430	49.284545
3503.603579	490925.146024	49.289549
3503.846564	490917.004598	49.294554
3503.500469	490903.334697	49.299559
3503.356609	490883.555428	49.304564
3503.654419	490877.785632	49.309569
3503.548043	490885.703212	49.314573
3503.544705	490875.473615	49.319578
3503.765482	490868.703092	49.324583
3503.526638	490868.791643	49.329588
3503.446002	490841.506878	49.334593
3503.334014	490836.409583	49.339597
3503.213278	490832.225280	49.344602
3503.605449	490829.681838	49.349607
3503.115394	490838.571695	49.354612
3503.492578	490820.128064	49.359617
3503.218729	490814.397960	49.364621
3503.289838	490826.491058	49.369626
3503.662174	490826.786876	49.374631
3503.627027	490820.765819	49.379636
3503.416419	490798.008948	49.384641
3503.229663	490790.695070	49.389645
3503.616030	490771.946069	49.394650
3503.790182	490785.187747	49.399655
3503.510626	490777.027563	49.404660
3503.691530	490781.303968	49.409665
3503.348752	490770.520223	49.414669
3503.515804	490774.900109	49.419674
3503.680322	490743.879349	49.424679
3503.606566	490745.410522	49.429684
3503.504998	490729.270867	49.434689
3503.193105	490740.361006	49.439693
3503.506407	490725.675134	49.444698
3503.696341	490736.837891	49.449703
3503.522037	490711.289682	49.454708
3503.722846	490699.964167	49.459713
3503.295924	490691.675302	49.464717
3503.275390	490689.146429	49.469722
3503.623340	490673.543421	49.474727
3503.689362	490681.636421	49.479732
3503.941804	490676.886643	49.484737
3503.833503	490657.658615	49.489741
3503.802352	490641.153236	49.494746
3503.971527	490644.216032	49.499751
3503.608521	490633.384759	49.504756
3503.930982	490606.086581	49.509761
3503.501302	490603.875596	49.514765
3503.951577	490584.812432	49.519770
3503.873399	490595.257966	49.524775
3503.715237	490566.769556	49.529780
3503.606267	490549.820584	49.534785
3503.665055	490553.052781	49.539789
3503.301914	490553.819376	49.544794
3503.435506	490545.289912	49.549799
3503.327905	490537.659548	49.554804
3503.560918	490549.372713	49.559809
3503.466247	490516.771878	49.564813
3503.365146	490510.052102	49.569818
3503.788808	490499.349639	49.574823
3503.236066	490506.071783	49.579828
3503.547727	490503.996838	49.584833
3503.506901	490490.126445	49.589837
3503.692741	490500.530300	49.594842
3503.733404	490476.163296	49.599847
3503.385620	490470.748648	49.604852
3503.407902	490442.586050	49.609857
3503.528408	490446.922725	49.614861
3503.683930	490445.986667	49.619866
3503.353733	490448.419381	49.624871
3503.395671	490440.157588	49.629876
3503.453948	490446.378006	49.634881
3503.264546	490425.035420	49.639885
3503.436946	490418.778843	49.644890
3503.467773	490403.934783	49.649895
3503.119226	490415.182845	49.654900
3503.072258	490408.403831	49.659905
3502.911752	490407.517723	49.664909
3503.476911	490411.530892	49.669914
3503.589290	490400.016589	49.674919
3503.371894	490405.267669	49.679924
3503.651114	490393.169881	49.684929
3503.438346	490402.168054	49.689933
3503.707580	490402.986640	49.694938
3503.731031	490376.849608	49.699943
3503.483823	490384.232551	49.704948
3503.615354	490363.953387	49.709953
3503.478030	490378.257512	49.714957
3503.511971	490370.402123	49.719962
3503.595831	490380.265055	49.724967
3503.561206	490356.365611	49.729972
3503.497621	490339.004103	49.734977
3503.291758	490328.046521	49.739981
3503.379160	490333.806555	49.744986
3503.535162	490317.271309	49.749991
3503.110452	490328.734047	49.754996
3503.494811	490319.354502	49.760001
3503.558201	490325.422212	49.765005
3503.404991	490313.797896	49.770010
3503.559067	490318.534466	49.775015
3503.473745	490290.439294	49.780020
3503.566314	490280.143565	49.785025
3503.346411	490284.128910	49.790029
3503.138527	490271.804158	49.795034
3503.639605	490264.685233	49.800039
3503.445944	490277.327002	49.805044
3503.459148	490269.880020	49.810049
3503.281103	490276.897547	49.815053
3503.549336	490270.372541	49.820058
3503.379202	490243.252989	49.825063
3503.510385	490248.499662	49.830068
3503.517253	490212.995388	49.835073
3503.747775	490231.647750	49.840077
3503.259596	490219.975028	49.845082
3503.745977	490216.454326	49.850087
3503.552876	490227.931164	49.855092
3503.481280	490202.771200	49.860097
3503.347997	490190.383955	49.865101
3503.497631	490180.332386	49.870106
3503.563905	490179.815597	49.875111
3503.442015	490185.608758	49.880116
3503.660904	490172.203546	49.885121
3503.792180	490171.929717	49.890125
3503.066209	490163.282710	49.895130
3503.750752	490129.443804	49.900135
3503.701107	490135.580090	49.905140
3503.605320	490130.935864	49.910145
3503.333140	490134.068505	49.915149
3503.511532	490124.113654	49.920154
3503.464886	490130.452055	49.925159
3503.518527	490135.153900	49.930164
3503.634729	490097.910130	49.935169
3503.755531	490085.026831	49.940173
3503.628369	490085.199026	49.945178
3503.309004	490073.752765	49.950183
3503.462711	490080.312750	49.955188
3503.703506	490073.589425	49.960193
3503.750090	490058.286775	49.965197
3503.560570	490046.617385	49.970202
3503.545268	490031.729674	49.975207
3503.464384	490038.681285	49.980212
3503.674881	490041.788296	49.985217
3503.489001	490041.058123	49.990221
3503.513161	490026.822584	49.995226
3503.858064	489993.999417	50.000231
3503.512995	489998.713670	50.005236
3503.564299	489989.234661	50.010241
3503.293747	489998.444750	50.015245
3503.209899	489996.280322	50.020250
3503.697767	489993.670997	50.025255
3503.504111	489977.190718	50.030260
3503.402446	489956.137614	50.035265
3503.357408	489947.382877	50.040269
3503.364596	489942.722327	50.045274
3503.445040	489942.253939	50.050279
3503.554878	489937.121336	50.055284
3503.376651	489939.985922	50.060289
3503.349907	489947.182246	50.065293
3503.378235	489935.174468	50.070298
3503.719864	489938.007532	50.075303
3503.379262	489915.067544	50.080308
3503.707536	489899.213766	50.085313
3503.549852	489908.608649	50.090317
3503.439029	489888.772459	50.095322
3503.466936	489893.225194	50.100327
3503.180837	489895.296474	50.105332
3503.397646	489878.396697	50.110337
3503.325651	489889.601361	50.115341
3503.162181	489883.397694	50.120346
3503.555589	489866.318049	50.125351
3503.636027	489855.416233	50.130356
3503.324733	489842.499769	50.135361
3503.410533	489839.295554	50.140365
3503.525516	489844.089071	50.145370
3503.292238	489843.974155	50.150375
3503.459692	489836.350677	50.155380
3503.398926	489845.730273	50.160385
3503.355985	489842.343815	50.165389
3503.402525	489836.917303	50.170394
3503.293659	489812.218536	50.175399
3503.141542	489808.748033	50.180404
3503.413559	489800.601535	50.185409
3503.310922	489791.146759	50.190413
3503.683370	489804.560380	50.195418
3503.534615	489786.502752	50.200423
3503.447866	489792.847606	50.205428
3503.669942	489801.827982	50.210433
3503.484031	489791.018875	50.215437
3503.333795	489781.217082	50.220442
3503.513695	489752.522055	50.225447
3503.296784	489753.873343	50.230452
3503.171111	489752.424570	50.235457
3503.193616	489738.796851	50.240461
3503.224394	489757.886441	50.245466
3503.177343	489745.535920	50.250471
3503.242636	489758.846179	50.255476
3503.212897	489745.581258	50.260481
3503.348089	489757.411677	50.265485
3503.259621	489753.070088	50.270490
3503.638374	489739.841892	50.275495
3503.431780	489750.561434	50.280500
3503.280124	489739.746883	50.285505
3503.683944	489755.941222	50.290509
3503.716913	489728.991415	50.295514
3503.473702	489723.357428	50.300519
3503.298862	489713.812729	50.305524
3503.536930	489716.915437	50.310529
3503.326699	489701.501145	50.315533
3503.193588	489708.157245	50.320538
3503.423177	489704.170557	50.325543
3503.207954	489706.129359	50.330548
3503.307724	489702.011245	50.335553
3503.334026	489708.895388	50.340557
3503.280223	489702.978216	50.345562
3503.308006	489701.606480	50.350567
3503.167786	489700.362595	50.355572
3503.632338	489682.765057	50.360577
3503.137810	489675.651333	50.365581
3502.848807	489668.201232	50.370586
3503.138277	489659.241543	50.375591
3503.271562	489676.491676	50.380596
3503.408200	489681.383109	50.385601
3503.430848	489662.791788	50.390605
3503.341385	489664.072290	50.395610
3503.301741	489673.094095	50.400615
3503.366998	489660.827064	50.405620
3503.471988	489660.506734	50.410625
3503.810049	489663.998831	50.415629
3503.462635	489658.026758	50.420634
3503.419211	489647.144398	50.425639
3503.473865	489635.436157	50.430644
3503.307068	489636.171752	50.435649
3503.379894	489628.259257	50.440653
3503.215931	489623.119198	50.445658
3503.186674	489621.148691	50.450663
3502.830068	489630.372562	50.455668
3503.476186	489622.470746	50.460673
3503.224838	489617.141903	50.465677
3503.104235	489621.618176	50.470682
3503.324225	489612.872040	50.475687
3503.292190	489632.832708	50.480692
3503.492420	489625.862393	50.485697
3503.575670	489633.801177	50.490701
3503.304278	489626.246979	50.495706
3503.735325	489614.479231	50.500711
3503.253191	489627.825462	50.505716
3503.605339	489591.303118	50.510721
3503.492618	489578.456383	50.515725
3503.363178	489574.171877	50.520730
3503.471823	489558.504472	50.525735
3503.384036	489536.992868	50.530740
3503.401574	489505.891996	50.535745
3503.321706	489451.811922	50.540749
3503.382019	489396.088770	50.545754
3503.330780	489325.846784	50.550759
3503.155713	489251.774758	50.555764
3502.907561	489164.393156	50.560769
3502.710698	489058.161300	50.565773
3502.527572	488978.264736	50.570778
3502.766088	488854.741880	50.575783
3502.268117	488743.997309	50.580788
3502.024612	488600.845841	50.585793
3501.830654	488457.938715	50.590797
3501.511566	488314.442463	50.595802
3501.133614	488164.572241	50.600807
3500.805926	488018.289226	50.605812
3500.733501	487848.512356	50.610817
3500.893276	487671.200534	50.615821
3500.165842	487500.257739	50.620826
3500.017270	487300.298165	50.625831
3499.543244	487123.233370	50.630836
3499.375935	486925.400326	50.635841
3499.581028	486710.435249	50.640845
3498.656759	486492.201602	50.645850
3498.324599	486263.791059	50.650855
3497.898346	486055.807794	50.655860
3497.533774	485816.708212	50.660865
3497.153550	485572.846155	50.665869
3496.563337	485339.906042	50.670874
3496.592410	485086.601043	50.675879
3495.836700	484844.004921	50.680884
3495.418096	484601.352452	50.685889
3495.243291	484325.981136	50.690893
3494.559850	484072.623425	50.695898
3494.458185	483799.715527	50.700903
3493.941467	483524.741471	50.705908
3493.414094	483236.490887	50.710913
3492.927614	482958.109428	50.715917
3491.884403	482682.243981	50.720922
3491.604138	482394.549828	50.725927
3491.242302	482102.304174	50.730932
3490.744178	481805.515467	50.735937
3490.332802	481516.511681	50.740941
3489.663199	481207.124206	50.745946
3489.267584	480901.843583	50.750951
3488.588254	480605.622695	50.755956
3488.302558	480281.566345	50.760961
3487.871188	479977.949216	50.765965
3487.327089	479661.625913	50.770970
3486.793266	479329.738564	50.775975
3485.997938	479010.606716	50.780980
3485.558507	478684.420028	50.785985
3485.112952	478355.492333	50.790989
3484.446697	478033.182311	50.795994
3484.098250	477680.206354	50.800999
3483.115701	477354.337081	50.806004
3482.783585	477008.898045	50.811009
3482.062325	476671.877116	50.816013
3481.535603	476340.040115	50.821018
3480.926827	475986.365836	50.826023
3480.335810	475653.564656	50.831028
3479.686238	475297.806639	50.836033
3479.075547	474956.228428	50.841037
3478.305832	474602.504605	50.846042
3477.840463	474239.754660	50.851047
3476.949219	473898.709827	50.856052
3476.393715	473542.196424	50.861057
3476.049693	473192.385238	50.866061
3475.099120	472845.401285	50.871066
3474.643457	472490.120992	50.876071
3473.928647	472150.387711	50.881076
3473.219408	471770.903513	50.886081
3472.533496	471420.304958	50.891085
3471.883768	471062.343761	50.896090
3471.574703	470695.349111	50.901095
3470.614506	470348.780753	50.906100
3470.127632	469987.682606	50.911105
3469.618301	469623.286235	50.916109
3468.493916	469271.807945	50.921114
3467.865991	468900.471668	50.926119
3467.536639	468542.416298	50.931124
3467.267210	468165.382308	50.936129
3466.685299	467798.683865	50.941133
3465.739746	467435.383026	50.946138
3464.956100	467061.503476	50.951143
3464.121927	466693.963623	50.956148
3463.315950	466322.305582	50.961153
3462.925551	465960.615608	50.966157
3462.005173	465595.605702	50.971162
3461.691010	465232.927776	50.976167
3460.434028	464876.883735	50.981172
3459.979413	464506.862515	50.986177
3459.720907	464141.165188	50.991181
3458.639699	463778.533060	50.996186
3458.155476	463402.462467	51.001191
3457.297823	463047.186965	51.006196
3456.550920	462681.643384	51.011201
3456.108035	462307.170026	51.016205
3455.145872	461950.219287	51.021210
3454.376828	461577.762855	51.026215
3453.364915	461221.568752	51.031220
3452.820726	460861.440098	51.036225
3452.473159	460495.035661	51.041229
3451.663413	460148.226218	51.046234
3451.300292	459782.623839	51.051239
3450.202254	459422.863344	51.056244
3449.461418	459055.178133	51.061249
3448.951563	458698.102640	51.066253
3447.891240	458350.188413	51.071258
3447.680628	457985.698742	51.076263
3446.419308	457636.181768	51.081268
3446.001230	457267.857740	51.086273
3445.690855	456907.779522	51.091277
3444.719205	456559.670963	51.096282
3444.296684	456194.931738	51.101287
3443.120627	455840.908707	51.106292
3442.668180	455484.837825	51.111297
3442.065887	455124.929211	51.116301
3441.390751	454766.599120	51.121306
3440.650321	454409.795709	51.126311
3439.818429	454054.320255	51.131316
3439.075318	453695.273584	51.136321
3438.534357	453346.844198	51.141325
3437.557510	452996.601047	51.146330
3437.325172	452638.522418	51.151335
3436.636064	452283.707005	51.156340
3435.824969	451939.155029	51.161345
3435.196220	451573.866426	51.166349
3434.240465	451224.607589	51.171354
3434.054092	450870.908628	51.176359
3432.841441	450525.079577	51.181364
3432.294357	450168.280730	51.186369
3431.512586	449819.835753	51.191373
3430.350367	449477.332255	51.196378
3429.885929	449116.139948	51.201383
3429.217893	448776.288328	51.206388
3428.366992	448437.120393	51.211393
3427.467461	448096.381990	51.216397
3426.802640	447749.156256	51.221402
3426.643072	447415.598971	51.226407
3425.794522	447079.862060	51.231412
3425.131137	446736.173731	51.236417
3424.704737	446388.230426	51.241421
3423.414258	446044.123634	51.246426
3423.003959	445693.934406	51.251431
3422.338986	445359.006846	51.256436
3421.608028	445025.404655	51.261441
3420.746022	444688.620842	51.266445
3419.982588	444354.912891	51.271450
3419.393133	444023.862956	51.276455
3418.346193	443688.414005	51.281460
3418.118330	443354.658211	51.286465
3417.291591	443015.713414	51.291469
3416.484674	442688.486484	51.296474
3415.676780	442353.894847	51.301479
3415.093570	442028.603320	51.306484
3414.143236	441693.568225	51.311489
3413.537073	441365.124135	51.316493
3412.849836	441045.064546	51.321498
3412.402965	440721.916858	51.326503
3411.559337	440397.253893	51.331508
3410.923653	440068.035546	51.336513
3410.289605	439749.625896	51.341517
3409.168359	439425.095500	51.346522
3408.755039	439098.570473	51.351527
3408.513837	438776.227744	51.356532
3407.723014	438447.494584	51.361537
3406.876953	438125.949802	51.366541
3405.930543	437804.061326	51.371546
3405.586877	437470.040508	51.376551
3404.637713	437155.505980	51.381556
3403.786235	436832.092169	51.386561
3403.065974	436516.650277	51.391565
3402.368613	436210.467095	51.396570
3401.645203	435885.269122	51.401575
3401.005005	435569.320326	51.406580
3400.577576	435254.120966	51.411585
3399.714152	434934.949860	51.416589
3399.007350	434623.823580	51.421594
3398.497527	434297.530488	51.426599
3397.539224	433989.990680	51.431604
3396.690353	433674.102056	51.436609
3396.363323	433361.732391	51.441613
3395.681064	433058.352455	51.446618
3395.033823	432734.168518	51.451623
3394.437223	432430.005898	51.456628
3393.737366	432116.639013	51.461633
3393.181651	431797.964100	51.466637
3392.145744	431482.890648	51.471642
3391.482363	431166.129366	51.476647
3390.650301	430860.893659	51.481652
3390.045633	430562.042773	51.486657
3389.535543	430243.824034	51.491661
3388.837101	429933.426951	51.496666
3388.260213	429622.219765	51.501671
3387.321362	429307.485576	51.506676
3386.678009	428998.998663	51.511681
3385.922438	428683.516991	51.516685
3385.263573	428387.798823	51.521690
3384.566773	428073.697291	51.526695
3383.961711	427776.770219	51.531700
3383.002860	427476.594328	51.536705
3382.288046	427165.786341	51.541709
3381.388447	426863.105360	51.546714
3380.768300	426568.833812	51.551719
3380.207396	426270.156011	51.556724
3379.383093	425971.643517	51.561729
3379.153681	425671.433607	51.566733
3377.914919	425381.335838	51.571738
3377.897209	425073.949054	51.576743
3377.207060	424779.567410	51.581748
3376.292986	424483.084499	51.586753
3375.610605	424174.421089	51.591757
3374.765941	423882.162244	51.596762
3374.127046	423588.546961	51.601767
3373.381634	423283.109139	51.606772
3372.831799	422984.799757	51.611777
3372.242513	422691.903607	51.616781
3371.081495	422403.616018	51.621786
3370.452511	422095.022309	51.626791
3369.666042	421807.583685	51.631796
3368.922967	421523.310366	51.636801
3368.337312	421227.476948	51.641805
3367.577177	420954.529573	51.646810
3367.023763	420653.477580	51.651815
3366.404968	420378.165215	51.656820
3365.875654	420086.756166	51.661825
3365.277436	419793.551378	51.666829
3364.284599	419511.634087	51.671834
3363.809030	419214.669602	51.676839
3363.158984	418924.156688	51.681844
3362.306542	418645.739625	51.686849
3361.634858	418357.053375	51.691853
3361.145281	418068.691047	51.696858
3360.685342	417788.526800	51.701863
3359.575405	417495.099603	51.706868
3358.862276	417200.336379	51.711873
3358.691323	416917.856814	51.716877
3357.595901	416639.763391	51.721882
3356.865102	416350.303982	51.726887
3356.349412	416073.104224	51.731892
3355.480774	415783.914970	51.736897
3354.852341	415497.403346	51.741901
3354.007809	415216.588794	51.746906
3353.440939	414939.843571	51.751911
3352.344397	414662.264800	51.756916
3352.057289	414380.718826	51.761921
3351.552041	414086.475273	51.766925
3350.518563	413827.146843	51.771930
3349.784641	413534.915731	51.776935
3349.383970	413263.641935	51.781940
3348.580698	412993.699742	51.786945
3348.272182	412704.162656	51.791949
3347.440872	412428.680535	51.796954
3346.815615	412143.126481	51.801959
3346.088273	411866.250564	51.806964
3345.392229	411588.731862	51.811969
3344.786219	411301.845345	51.816973
3343.796069	411035.116543	51.821978
3343.049931	410748.831307	51.826983
3342.532637	410471.019830	51.831988
3341.620051	410201.196595	51.836993
3341.207538	409935.916740	51.841997
3340.365529	409658.403212	51.847002
3339.943106	409385.394924	51.852007
3339.257807	409120.735512	51.857012
3338.492011	408843.431157	51.862017
3337.919651	408561.875186	51.867021
3337.338823	408298.843905	51.872026
3336.499397	408015.571629	51.877031
3335.824137	407737.632970	51.882036
3334.963116	407464.346424	51.887041
3334.298089	407189.247486	51.892045
3333.423169	406930.088422	51.897050
3332.942892	406653.151082	51.902055
3332.125813	406391.055706	51.907060
3331.445429	406124.717664	51.912065
3331.103973	405844.116833	51.917069
3329.976066	405589.764534	51.922074
3329.531956	405313.038231	51.927079
3328.976826	405045.273290	51.932084
3327.827745	404798.390038	51.937089
3327.434674	404530.925468	51.942093
3326.897442	404260.075653	51.947098
3325.889193	403985.002627	51.952103
3325.333035	403728.308140	51.957108
3324.633799	403464.695411	51.962113
3324.380302	403187.996489	51.967117
3323.356357	402934.216240	51.972122
3322.584353	402672.819730	51.977127
3321.962372	402410.355224	51.982132
3321.111938	402142.688612	51.987137
3320.880937	401892.587340	51.992141
3319.755626	401633.830835	51.997146
3319.262313	401364.118615	52.002151
3318.581837	401113.853592	52.007156
3317.588076	400854.231192	52.012161
3317.215245	400582.078581	52.017165
3316.295368	400333.751802	52.022170
3315.697694	400071.798168	52.027175
3315.284853	399812.888973	52.032180
3314.557000	399552.934484	52.037185
3313.758944	399298.886484	52.042189
3312.789544	399044.126419	52.047194
3312.648656	398785.801581	52.052199
3311.657953	398525.422931	52.057204
3310.926836	398272.347799	52.062209
3310.706420	398016.368219	52.067213
3309.527484	397761.936416	52.072218
3309.241811	397497.421594	52.077223
3308.469502	397246.760168	52.082228
3307.776433	396994.203104	52.087233
3307.392139	396735.061826	52.092237
3306.624290	396478.928177	52.097242
3305.920265	396220.875791	52.102247
3305.090966	395970.671402	52.107252
3304.399824	395701.960905	52.112257
3304.025779	395429.842274	52.117261
3303.312959	395183.249108	52.122266
3302.146960	394916.285389	52.127271
3301.593291	394667.400610	52.132276
3300.909807	394419.348100	52.137281
3300.167717	394156.480867	52.142285
3299.482589	393905.246876	52.147290
3298.838400	393646.326406	52.152295
3297.942905	393401.732325	52.157300
3297.622701	393158.011655	52.162305
3297.142763	392901.068141	52.167309
3296.254848	392659.544000	52.172314
3295.735679	392400.136728	52.177319
3294.969060	392142.902388	52.182324
3294.230353	391886.348221	52.187329
3293.565465	391637.993036	52.192333
3292.780337	391396.825238	52.197338
3292.308206	391135.672126	52.202343
3291.539483	390891.141985	52.207348
3290.158520	390645.562775	52.212353
3289.570927	390397.008575	52.217357
3289.040855	390156.071601	52.222362
3288.259030	389924.479116	52.227367
3287.808698	389675.186167	52.232372
3287.308727	389434.773493	52.237377
3286.823682	389191.966638	52.242381
3285.884291	388951.493059	52.247386
3285.533877	388700.550099	52.252391
3284.529971	388454.870649	52.257396
3283.882757	388215.210464	52.262401
3283.371752	387967.542595	52.267405
3282.655149	387718.684965	52.272410
3281.600792	387479.999712	52.277415
3280.887031	387236.961512	52.282420
3280.145673	387006.055758	52.287425
3280.041946	386757.247157	52.292429
3279.078335	386530.187931	52.297434
3278.183904	386286.129340	52.302439
3277.926147	386047.715561	52.307444
3277.177817	385807.190843	52.312449
3276.358428	385566.319764	52.317453
3276.100295	385332.275385	52.322458
3275.346382	385090.755082	52.327463
3274.741138	384846.971788	52.332468
3273.817301	384598.252838	52.337473
3273.104164	384353.720440	52.342477
3272.332594	384113.086644	52.347482
3271.727480	383875.451293	52.352487
3271.214725	383643.165865	52.357492
3270.451014	383409.596244	52.362497
3269.867887	383162.034548	52.367501
3269.081155	382928.618168	52.372506
3268.381167	382692.007607	52.377511
3267.715346	382449.744193	52.382516
3266.981651	382216.213292	52.387521
3266.526217	381979.228973	52.392525
3265.550565	381753.541304	52.397530
3264.752859	381509.639624	52.402535
3264.249549	381271.310531	52.407540
3263.315261	381049.299952	52.412545
3263.012856	380805.340875	52.417549
3262.476121	380570.929458	52.422554
3261.557847	380340.468318	52.427559
3261.254836	380107.543138	52.432564
3260.546076	379866.618159	52.437569
3259.829826	379631.364684	52.442573
3259.068281	379405.375035	52.447578
3258.349880	379150.025890	52.452583
3257.943460	378917.160806	52.457588
3256.897102	378677.451865	52.462593
3256.201950	378448.165097	52.467597
3255.581080	378214.337800	52.472602
3254.852772	377977.194096	52.477607
3254.418091	377744.224796	52.482612
3253.393535	377511.321993	52.487617
3253.153022	377280.379533	52.492621
3252.236818	377047.533180	52.497626
3251.500156	376816.768253	52.502631
3251.108917	376583.683541	52.507636
3250.123354	376349.852085	52.512641
3249.355115	376121.479155	52.517645
3249.064103	375903.280371	52.522650
3247.919371	375664.967842	52.527655
3247.554851	375435.000963	52.532660
3246.404149	375207.649961	52.537665
3245.735714	374980.933640	52.542669
3245.490783	374760.508383	52.547674
3244.614917	374536.111751	52.552679
3244.232554	374302.885311	52.557684
3243.424045	374078.755330	52.562689
3242.491993	373857.416391	52.567693
3242.129474	373626.345184	52.572698
3240.902662	373407.670564	52.577703
3240.182150	373187.286653	52.582708
3239.324904	372966.948637	52.587713
3239.188180	372742.374441	52.592717
3238.246166	372513.449215	52.597722
3237.872022	372305.699725	52.602727
3237.391294	372078.836007	52.607732
3236.242065	371864.567377	52.612737
3235.836959	371630.490023	52.617741
3235.219195	371424.351937	52.622746
3234.544058	371197.794051	52.627751
3233.842435	370970.959306	52.632756
3233.048709	370759.910537	52.637761
3232.797190	370533.740008	52.642765
3231.713675	370314.695880	52.647770
3231.030835	370101.107750	52.652775
3230.901897	369868.554282	52.657780
3229.623434	369656.966173	52.662785
3228.931080	369438.237293	52.667789
3228.553849	369213.122740	52.672794
3227.931213	368986.646591	52.677799
3227.130734	368768.847293	52.682804
3226.229833	368557.346716	52.687809
3225.821678	368331.113070	52.692813
3225.005240	368117.943325	52.697818
3224.213680	367908.762902	52.702823
3223.851700	367685.825992	52.707828
3222.975167	367471.543180	52.712833
3222.592547	367257.155752	52.717837
3221.652320	367047.206051	52.722842
3221.220592	366815.676415	52.727847
3220.427910	366603.818562	52.732852
3219.687614	366385.209213	52.737857
3219.336231	366161.397905	52.742861
3218.530810	365942.974787	52.747866
3217.706662	365727.046943	52.752871
3217.150508	365502.857653	52.757876
3216.506516	365289.901455	52.762881
3215.480196	365075.987012	52.767885
3214.978832	364855.933047	52.772890
3214.267675	364646.266605	52.777895
3213.832642	364431.161519	52.782900
3212.556184	364219.979604	52.787905
3212.112142	364004.644939	52.792909
3211.678839	363792.615246	52.797914
3210.865340	363585.886147	52.802919
3210.377214	363371.064357	52.807924
3209.588631	363160.690920	52.812929
3209.151381	362933.823997	52.817933
3208.417368	362723.490826	52.822938
3207.754252	362520.651592	52.827943
3207.543353	362289.878161	52.832948
3206.298017	362077.103945	52.837953
3205.853620	361856.670399	52.842957
3205.463371	361638.797187	52.847962
3204.457251	361427.890548	52.852967
3203.769274	361202.149011	52.857972
3202.771945	360993.096531	52.862977
3202.524924	360782.982954	52.867981
3201.602264	360574.451168	52.872986
3200.993708	360357.191831	52.877991
3200.570907	360130.588987	52.882996
3199.622652	359937.504011	52.888001
3199.238894	359711.096572	52.893005
3198.540419	359502.575536	52.898010
3197.896451	359284.706235	52.903015
3196.949144	359060.547816	52.908020
3196.210255	358850.783492	52.913025
3195.532175	358637.904169	52.918029
3195.424515	358433.203823	52.923034
3194.685638	358220.281400	52.928039
3194.367315	357996.400275	52.933044
3193.098740	357782.440087	52.938049
3192.680110	357563.458670	52.943053
3191.777332	357343.865801	52.948058
3191.402322	357135.817870	52.953063
3190.685899	356915.430199	52.958068
3189.584026	356707.139199	52.963073
3189.129819	356487.166204	52.968077
3188.034912	356285.386928	52.973082
3187.322547	356074.665031	52.978087
3186.889748	355862.040323	52.983092
3186.325585	355655.924748	52.988097
3185.755095	355449.300370	52.993101
3184.997811	355232.805333	52.998106
3184.366763	355029.573440	53.003111
3184.074693	354810.789000	53.008116
3183.292774	354600.708182	53.013121
3182.673775	354377.341969	53.018125
3181.758764	354171.988452	53.023130
3181.066073	353959.295114	53.028135
3180.493125	353731.821543	53.033140
3179.438152	353537.201664	53.038145
3178.672667	353330.675935	53.043149
3178.358059	353130.287679	53.048154
3177.299528	352922.152487	53.053159
3176.957714	352718.178589	53.058164
3175.765306	352513.447733	53.063169
3175.580535	352306.342539	53.068173
3174.815937	352104.825418	53.073178
3173.915977	351896.330226	53.078183
3173.560718	351678.662392	53.083188
3172.905062	351491.988493	53.088193
3172.212832	351279.945904	53.093197
3171.502582	351069.966797	53.098202
3170.622673	350863.322257	53.103207
3170.145902	350666.309770	53.108212
3169.265679	350458.263945	53.113217
3168.539225	350262.765618	53.118221
3167.900687	350059.668351	53.123226
3167.089679	349862.909420	53.128231
3166.936270	349655.025479	53.133236
3166.173774	349446.626287	53.138241
3165.464505	349245.318746	53.143245
3164.675617	349051.047602	53.148250
3164.147091	348840.980212	53.153255
3163.423399	348647.028195	53.158260
3162.542891	348443.912315	53.163265
3162.194323	348234.475888	53.168269
3161.556464	348027.884129	53.173274
3160.755535	347844.325817	53.178279
3160.287571	347630.884633	53.183284
3159.602049	347434.046288	53.188289
3158.661769	347224.979669	53.193293
3158.031112	347028.334841	53.198298
3157.279145	346829.952319	53.203303
3156.670068	346631.546494	53.208308
3155.786255	346427.838437	53.213313
3155.689638	346231.131806	53.218317
3155.069727	346038.426992	53.223322
3154.170496	345835.381031	53.228327
3153.972728	345622.805842	53.233332
3152.862706	345429.922005	53.238337
3152.049709	345216.780888	53.243341
3151.413751	345013.079508	53.248346
3150.788444	344809.655715	53.253351
3150.274840	344606.748056	53.258356
3149.245896	344420.440425	53.263361
3148.930458	344202.533470	53.268365
3148.262748	344011.000346	53.273370
3147.244036	343818.682169	53.278375
3146.665733	343619.803005	53.283380
3146.107411	343417.789204	53.288385
3145.424149	343218.925306	53.293389
3144.559280	343017.569543	53.298394
3144.035254	342816.617345	53.303399
3144.043759	342620.951026	53.308404
3142.777025	342434.063892	53.313409
3142.437917	342229.338716	53.318413
3141.849574	342016.685080	53.323418
3140.946068	341824.062277	53.328423
3140.312436	341604.948948	53.333428
3139.693463	341405.279817	53.338433
3138.812944	341198.676841	53.343437
3138.064500	341003.990550	53.348442
3137.310760	340816.075466	53.353447
3136.932346	340610.358357	53.358452
3135.842903	340418.091484	53.363457
3135.333841	340213.462842	53.368461
3134.874721	340013.305735	53.373466
3134.101921	339829.692609	53.378471
3133.502158	339621.792662	53.383476
3132.757396	339434.202917	53.388481
3132.041884	339224.385365	53.393485
3131.397794	339030.032794	53.398490
3130.761384	338842.347786	53.403495
3130.292610	338636.027584	53.408500
3129.558365	338436.952709	53.413505
3128.990553	338237.469044	53.418509
3128.539225	338038.169978	53.423514
3127.785078	337840.241925	53.428519
3127.090157	337625.146483	53.433524
3126.384881	337424.485626	53.438529
3125.657493	337225.787782	53.443533
3124.985404	337032.273678	53.448538
3123.950317	336834.794327	53.453543
3123.578205	336621.502826	53.458548
3122.822790	336427.440086	53.463553
3122.159600	336233.718578	53.468557
3121.569995	336037.031884	53.473562
3120.567809	335842.115497	53.478567
3120.314632	335641.072205	53.483572
3119.754172	335444.404614	53.488577
3119.052915	335243.405577	53.493581
3118.268232	335049.572587	53.498586
3117.450160	334843.244856	53.503591
3117.288234	334638.340110	53.508596
3116.052894	334456.057954	53.513601
3115.713510	334261.363084	53.518605
3115.309631	334052.090742	53.523610
3114.184137	333854.820619	53.528615
3113.430883	333656.319983	53.533620
3113.027693	333468.099205	53.538625
3112.166794	333263.631926	53.543629
3111.353510	333064.629947	53.548634
3110.640336	332874.827321	53.553639
3110.235216	332682.607846	53.558644
3109.301509	332493.857408	53.563649
3108.680020	332288.178342	53.568653
3108.304191	332093.228616	53.573658
3107.308770	331907.795949	53.578663
3106.913039	331719.034704	53.583668
3106.419474	331518.272089	53.588673
3105.368286	331313.269215	53.593677
3104.509111	331129.620533	53.598682
3104.083590	330941.854851	53.603687
3103.786051	330746.278086	53.608692
3102.758184	330556.442740	53.613697
3102.382489	330354.385322	53.618701
3101.754051	330159.928623	53.623706
3100.774043	329960.689849	53.628711
3100.241319	329763.161890	53.633716
3099.439802	329578.634599	53.638721
3098.767306	329382.197027	53.643725
3098.041375	329179.046171	53.648730
3097.640376	328992.646455	53.653735
3097.107803	328794.912243	53.658740
3096.436937	328607.383152	53.663745
3095.601976	328411.121516	53.668749
3095.174647	328206.596906	53.673754
3094.351352	328013.489382	53.678759
3093.671118	327816.208811	53.683764
3092.801338	327631.102011	53.688769
3092.089967	327428.657057	53.693773
3091.425178	327235.751643	53.698778
3090.837550	327048.943917	53.703783
3090.147968	326850.720356	53.708788
3089.464444	326671.081152	53.713793
3088.771550	326474.104708	53.718797
3088.542678	326276.748821	53.723802
3087.522128	326090.541994	53.728807
3086.817989	325885.393142	53.733812
3086.249883	325708.152220	53.738817
3085.744926	325506.509864	53.743821
3085.034878	325314.116142	53.748826
3084.228937	325120.056744	53.753831
3083.702482	324920.096722	53.758836
3082.876548	324729.222128	53.763841
3082.343380	324536.289364	53.768845
3081.936869	324345.092895	53.773850
3081.028374	324147.508376	53.778855
3080.402092	323957.542448	53.783860
3079.726204	323753.809571	53.788865
3079.129864	323556.963540	53.793869
3078.339882	323364.017769	53.798874
3077.551390	323184.591170	53.803879
3077.095013	322970.586290	53.808884
3076.409666	322781.849187	53.813889
3075.399421	322587.128756	53.818893
3075.009223	322402.163298	53.823898
3074.500959	322209.399477	53.828903
3073.744150	322011.022114	53.833908
3073.200729	321822.973364	53.838913
3072.453040	321621.512825	53.843917
3071.574699	321431.963077	53.848922
3071.000188	321248.781180	53.853927
3070.506293	321046.260688	53.858932
3069.773689	320859.181893	53.863937
3068.613303	320668.147431	53.868941
3068.302830	320474.686486	53.873946
3067.540549	320285.294150	53.878951
3067.025601	320083.793281	53.883956
3066.256204	319896.998380	53.888961
3065.779995	319706.184606	53.893965
3065.162405	319520.841710	53.898970
3064.480978	319319.340029	53.903975
3063.911517	319120.366416	53.908980
3063.408389	318928.103931	53.913985
3062.098212	318742.767225	53.918989
3061.564580	318535.562335	53.923994
3061.235931	318356.435138	53.928999
3060.616159	318156.779939	53.934004
3059.671337	317971.613049	53.939009
3058.816526	317776.832137	53.944013
3058.328836	317580.133948	53.949018
3057.452127	317404.045358	53.954023
3057.060041	317205.650729	53.959028
3056.404556	317023.568136	53.964033
3055.806409	316834.702998	53.969037
3055.333698	316638.662553	53.974042
3054.367376	316456.500778	53.979047
3054.089739	316252.458771	53.984052
3052.948434	316057.974372	53.989057
3052.513462	315876.032990	53.994061
3051.926938	315668.957626	53.999066
3050.948501	315479.971837	54.004071
3050.481461	315283.571329	54.009076
3049.727367	315099.616516	54.014081
3048.914690	314912.996986	54.019085
3048.083906	314723.553538	54.024090
3047.308108	314535.934409	54.029095
3046.810298	314348.347333	54.034100
3046.205613	314165.054711	54.039105
3045.680513	313984.142750	54.044109
3045.321858	313788.766237	54.049114
3044.400976	313603.460115	54.054119
3043.616587	313417.546399	54.059124
3043.386132	313222.148546	54.064129
3042.358209	313035.737964	54.069133
3042.099297	312841.846286	54.074138
3041.312270	312646.713716	54.079143
3040.673755	312452.932343	54.084148
3039.975877	312262.088384	54.089153
3039.231311	312073.263142	54.094157
3038.924615	311866.034111	54.099162
3038.051741	311679.316557	54.104167
3037.240573	311476.037189	54.109172
3036.393102	311286.157392	54.114177
3035.656061	311098.577048	54.119181
3035.191146	310907.260993	54.124186
3034.415699	310721.137568	54.129191
3034.171265	310521.739225	54.134196
3033.098386	310342.410328	54.139201
3032.108340	310154.231859	54.144205
3032.043962	309952.512227	54.149210
3031.330011	309772.234380	54.154215
3030.308973	309575.554708	54.159220
3029.907852	309392.909485	54.164225
3029.153524	309205.736234	54.169229
3028.584351	309001.573859	54.174234
3027.558465	308819.841510	54.179239
3026.929192	308626.052178	54.184244
3026.364723	308448.193289	54.189249
3025.518339	308263.095795	54.194253
3025.268629	308067.946789	54.199258
3024.383826	307886.852805	54.204263
3023.788463	307706.018325	54.209268
3023.178610	307521.926348	54.214273
3022.308255	307325.270106	54.219277
3021.760788	307139.970834	54.224282
3021.134907	306960.005924	54.229287
3020.638059	306768.000756	54.234292
3019.941664	306576.994563	54.239297
3018.981305	306387.506852	54.244301
3018.389491	306200.710787	54.249306
3017.867854	306016.653607	54.254311
3017.066790	305821.613877	54.259316
3016.545316	305639.211393	54.264321
3015.806399	305446.478629	54.269325
3015.136244	305264.302888	54.274330
3014.302632	305083.935359	54.279335
3014.024297	304888.709668	54.284340
3013.330733	304701.672948	54.289345
3012.567747	304520.223938	54.294349
3012.014190	304337.926638	54.299354
3011.110072	304135.821328	54.304359
3010.385001	303959.356862	54.309364
3009.830510	303779.121705	54.314369
3009.333000	303587.570478	54.319373
3008.939240	303400.204436	54.324378
3007.844983	303215.164555	54.329383
3007.554847	303015.787180	54.334388
3006.594911	302828.968396	54.339393
3005.779774	302648.442017	54.344397
3005.693598	302455.856477	54.349402
3004.668862	302260.083189	54.354407
3004.104243	302075.696553	54.359412
3003.399443	301888.759801	54.364417
3002.716043	301692.728018	54.369421
3002.396443	301499.567009	54.374426
3001.312538	301316.585884	54.379431
3000.908696	301116.179859	54.384436
3000.034128	300929.319741	54.389441
2999.442873	300734.901998	54.394445
2998.793541	300550.323211	54.399450
2998.220524	300359.798469	54.404455
2997.214587	300167.788575	54.409460
2996.874726	299983.924143	54.414465
2995.936026	299798.473505	54.419469
2995.379680	299603.514072	54.424474
2994.526189	299416.928991	54.429479
2993.852425	299222.140494	54.434484
2993.374348	299043.492065	54.439489
2992.482715	298851.691746	54.444493
2992.015177	298658.347019	54.449498
2991.301737	298489.030580	54.454503
2990.623337	298288.690019	54.459508
2990.020205	298111.715749	54.464513
2989.184524	297930.983567	54.469517
2989.030751	297735.601746	54.474522
2988.000217	297558.923776	54.479527
2987.297196	297370.708262	54.484532
2987.077952	297176.838738	54.489537
2986.087567	296993.557953	54.494541
2985.402826	296793.420460	54.499546
2985.115756	296610.308104	54.504551
2984.193892	296417.771416	54.509556
2983.664361	296233.958532	54.514561
2982.828960	296048.462133	54.519565
2982.499592	295853.819198	54.524570
2981.613938	295664.433933	54.529575
2980.998615	295471.975113	54.534580
2980.377585	295279.975417	54.539585
2979.446150	295091.284461	54.544589
2978.712420	294890.439678	54.549594
2978.367885	294704.304043	54.554599
2977.636616	294507.304035	54.559604
2976.962340	294332.986101	54.564609
2976.149714	294140.786460	54.569613
2975.782932	293946.147616	54.574618
2974.890466	293763.383156	54.579623
2974.220797	293577.068787	54.584628
2973.513060	293388.570095	54.589633
2972.862645	293195.783656	54.594637
2972.285828	293008.078871	54.599642
2971.443220	292813.463408	54.604647
2971.027829	292625.070601	54.609652
2970.118615	292441.900230	54.614657
2969.438401	292257.114482	54.619661
2969.218813	292065.099316	54.624666
2968.186528	291868.653962	54.629671
2967.659605	291690.465055	54.634676
2967.187926	291497.266899	54.639681
2966.425153	291310.303284	54.644685
2966.008398	291120.228647	54.649690
2965.140977	290926.099457	54.654695
2964.417210	290727.948965	54.659700
2963.473421	290548.093435	54.664705
2962.674781	290356.907171	54.669709
2962.644396	290165.599155	54.674714
2961.617212	289979.160314	54.679719
2960.828887	289787.488124	54.684724
2960.286870	289598.196242	54.689729
2959.698902	289409.217117	54.694733
2959.300864	289216.031088	54.699738
2958.200573	289029.501311	54.704743
2957.813249	288844.666762	54.709748
2957.191025	288655.310545	54.714753
2956.235116	288456.100051	54.719757
2955.916117	288270.464825	54.724762
2954.884460	288087.743764	54.729767
2954.341329	287893.255513	54.734772
2953.830410	287706.045854	54.739777
2953.335704	287508.137004	54.744781
2952.705467	287309.536386	54.749786
2951.825592	287124.982523	54.754791
2951.349946	286936.646249	54.759796
2950.565020	286743.086964	54.764801
2949.676016	286557.897539	54.769805
2949.583249	286356.537141	54.774810
2948.687619	286161.237769	54.779815
2947.977714	285976.274368	54.784820
2947.203684	285781.363030	54.789825
2946.521686	285586.895446	54.794829
2946.054201	285388.751873	54.799834
2945.114267	285205.174315	54.804839
2944.888365	285007.705411	54.809844
2943.836553	284816.606837	54.814849
2943.297232	284625.885468	54.819853
2942.969086	284429.604004	54.824858
2942.249936	284230.353642	54.829863
2941.638433	284036.230709	54.834868
2940.969706	283833.050093	54.839873
2940.033455	283642.696749	54.844877
2939.203051	283443.820205	54.849882
2938.561338	283250.134682	54.854887
2937.923538	283061.236480	54.859892
2937.253925	282876.443621	54.864897
2936.641903	282691.972664	54.869901
2936.328412	282482.342728	54.874906
2935.425543	282295.651006	54.879911
2934.433428	282108.107430	54.884916
2934.012354	281908.401446	54.889921
2933.556894	281726.146583	54.894925
2933.035740	281523.731210	54.899930
2931.808508	281333.983403	54.904935
2931.428448	281141.452721	54.909940
2930.704566	280952.007137	54.914945
2930.154927	280757.491196	54.919949
2929.310607	280556.501969	54.924954
2928.757323	280370.671185	54.929959
2928.095750	280178.821509	54.934964
2927.409310	279980.557708	54.939969
2926.821832	279786.072970	54.944973
2926.563483	279590.593753	54.949978
2925.475706	279403.217388	54.954983
2924.965957	279214.450588	54.959988
2924.076783	279009.036590	54.964993
2923.259905	278815.046390	54.969997
2923.268309	278616.697752	54.975002
2922.275215	278425.129402	54.980007
2921.535069	278213.171759	54.985012
2920.929098	278015.888079	54.990017
2919.842232	277824.691038	54.995021
2919.633036	277622.174406	55.000026
2918.846609	277435.641396	55.005031
2918.236598	277245.132835	55.010036
2917.635147	277051.108263	55.015041
2916.778347	276855.315841	55.020045
2916.413007	276656.949693	55.025050
2915.429087	276462.909211	55.030055
2914.614594	276272.331060	55.035060
2914.464820	276069.881263	55.040065
2913.400682	275878.986054	55.045069
2912.737063	275677.152424	55.050074
2911.920006	275496.787462	55.055079
2911.277076	275312.752947	55.060084
2910.929553	275111.989863	55.065089
2910.033468	274928.555726	55.070093
2909.428793	274724.369651	55.075098
2908.871694	274542.588228	55.080103
2908.244510	274349.841027	55.085108
2907.607207	274151.645198	55.090113
2906.774184	273953.327552	55.095117
2906.076041	273764.182647	55.100122
2905.578620	273581.449476	55.105127
2904.850527	273388.565481	55.110132
2904.553754	273196.606478	55.115137
2903.506543	273007.287672	55.120141
2903.056916	272800.657647	55.125146
2902.326240	272608.563646	55.130151
2901.213227	272419.459062	55.135156
2901.048953	272223.276892	55.140161
2900.524730	272031.430422	55.145165
2899.757632	271832.822378	55.150170
2899.035941	271647.934620	55.155175
2898.536958	271448.723880	55.160180
2897.840263	271250.537743	55.165185
2896.833512	271067.401586	55.170189
2896.430368	270859.669348	55.175194
2895.948007	270674.973070	55.180199
2894.959837	270476.935100	55.185204
2894.395104	270280.383699	55.190209
2893.715789	270085.505922	55.195213
2893.401594	269877.174048	55.200218
2892.625383	269694.969456	55.205223
2891.851835	269496.770390	55.210228
2891.261819	269294.467390	55.215233
2890.718343	269102.267988	55.220237
2889.920334	268894.547817	55.225242
2889.052007	268703.316816	55.230247
2888.640063	268507.709474	55.235252
2887.880453	268306.070324	55.240257
2887.093305	268114.673835	55.245261
2886.618966	267907.182887	55.250266
2885.864810	267723.752860	55.255271
2885.103672	267517.529936	55.260276
2884.796499	267321.906392	55.265281
2883.479469	267130.441321	55.270285
2883.166292	266935.735725	55.275290
2882.276896	266740.612073	55.280295
2881.937021	266547.948306	55.285300
2881.497623	266356.828463	55.290305
2880.287903	266161.526545	55.295309
2879.820598	265956.021773	55.300314
2879.171632	265773.237964	55.305319
2878.599596	265575.288515	55.310324
2878.088154	265369.918339	55.315329
2877.357085	265179.303598	55.320333
2876.825000	264976.254478	55.325338
2876.216411	264783.328396	55.330343
2875.203617	264576.891929	55.335348
2874.769525	264387.223789	55.340353
2873.944138	264187.787034	55.345357
2873.560508	263980.232541	55.350362
2872.717344	263796.410706	55.355367
2871.766127	263601.884044	55.360372
2871.308471	263398.823966	55.365377
2870.506911	263204.885054	55.370381
2869.918693	263009.486263	55.375386
2869.407272	262818.634185	55.380391
2868.563067	262610.618588	55.385396
2868.034407	262406.857234	55.390401
2867.281249	262224.626457	55.395405
2866.579111	262020.510795	55.400410
2865.732746	261835.951952	55.405415
2865.511222	261647.295828	55.410420
2865.090491	261441.225895	55.415425
2864.102721	261248.030731	55.420429
2863.394491	261045.623021	55.425434
2862.943392	260849.057792	55.430439
2861.994761	260646.331873	55.435444
2861.406656	260446.426866	55.440449
2860.509126	260259.483134	55.445453
2860.098871	260051.426041	55.450458
2859.636855	259860.720798	55.455463
2858.910335	259662.773816	55.460468
2858.564452	259464.231887	55.465473
2857.562326	259259.503513	55.470477
2857.413401	259057.849119	55.475482
2856.168685	258863.066372	55.480487
2855.730557	258643.121428	55.485492
2855.278339	258445.157405	55.490497
2854.235951	258246.701237	55.495501
2853.816836	258042.034333	55.500506
2852.981388	257841.712065	55.505511
2852.510476	257644.388337	55.510516
2851.989692	257429.449196	55.515521
2850.938368	257229.467237	55.520525
2850.393398	257029.150598	55.525530
2849.751597	256833.892007	55.530535
2848.864807	256627.670479	55.535540
2848.551114	256419.448342	55.540545
2847.529815	256230.056923	55.545549
2846.946244	256023.405933	55.550554
2846.189031	255824.244545	55.555559
2845.462518	255632.718652	55.560564
2845.143564	255420.525416	55.565569
2844.121272	255227.646030	55.570573
2843.716040	255028.455122	55.575578
2843.008688	254826.179789	55.580583
2842.311210	254629.098384	55.585588
2841.800379	254426.232053	55.590593
2840.488741	254236.149870	55.595597
2839.951009	254033.135397	55.600602
2839.672920	253844.672620	55.605607
2838.937924	253644.032754	55.610612
2838.407615	253447.409932	55.615617
2837.311385	253247.668093	55.620621
2837.286551	253050.074295	55.625626
2836.280183	252850.802519	55.630631
2835.421537	252644.911648	55.635636
2835.123222	252451.232756	55.640641
2834.103448	252255.936573	55.645645
2833.672620	252055.301183	55.650650
2833.176376	251854.319842	55.655655
2832.285801	251662.849324	55.660660
2831.639806	251460.262275	55.665665
2830.939950	251266.266254	55.670669
2830.464689	251063.729029	55.675674
2829.726671	250866.505238	55.680679
2828.794080	250669.490754	55.685684
2828.670621	250459.564164	55.690689
2827.774699	250274.360811	55.695693
2826.944586	250073.179759	55.700698
2826.520128	249869.235270	55.705703
2825.742924	249665.958089	55.710708
2825.217598	249467.556289	55.715713
2824.419986	249267.517072	55.720717
2823.933036	249067.632641	55.725722
2823.212626	248868.345690	55.730727
2822.517095	248660.956782	55.735732
2822.032698	248454.069505	55.740737
2821.035510	248271.940451	55.745741
2820.447375	248074.950994	55.750746
2819.751364	247869.575052	55.755751
2819.282281	247676.641839	55.760756
2818.607695	247469.658685	55.765761
2817.602466	247277.727668	55.770765
2816.900574	247069.959948	55.775770
2816.532509	246873.166415	55.780775
2815.856413	246679.197713	55.785780
2815.322268	246462.134697	55.790785
2814.310291	246278.584339	55.795789
2813.722900	246078.006744	55.800794
2813.369656	245876.399186	55.805799
2812.629153	245688.783006	55.810804
2812.018640	245479.195050	55.815809
2811.082841	245281.602323	55.820813
2810.268777	245079.585046	55.825818
2809.966581	244884.362715	55.830823
2808.992967	244688.075577	55.835828
2808.609494	244471.246451	55.840833
2808.101580	244284.359324	55.845837
2807.191470	244086.917059	55.850842
2806.419240	243876.313103	55.855847
2806.046865	243685.483680	55.860852
2805.345709	243477.975881	55.865857
2804.540276	243293.785668	55.870861
2804.270177	243086.464882	55.875866
2803.212938	242882.273982	55.880871
2802.622745	242682.262128	55.885876
2802.042004	242474.227575	55.890881
2801.157767	242282.971993	55.895885
2800.568325	242086.245961	55.900890
2800.181135	241888.316818	55.905895
2799.420858	241683.597000	55.910900
2798.719237	241483.782964	55.915905
2798.029140	241283.509061	55.920909
2797.655681	241081.784774	55.925914
2797.088500	240872.757642	55.930919
2796.009492	240662.003933	55.935924
2795.763737	240460.005818	55.940929
2794.986333	240258.627002	55.945933
2794.039113	240060.305713	55.950938
2793.683980	239854.124292	55.955943
2792.876658	239651.528956	55.960948
2792.068066	239452.753848	55.965953
2791.355159	239253.123602	55.970957
2790.818070	239043.865779	55.975962
2789.879686	238846.054460	55.980967
2789.187768	238645.479772	55.985972
2788.753315	238439.313455	55.990977
2787.785728	238247.390058	55.995981
2787.369400	238050.897990	56.000986
2786.805290	237849.260456	56.005991
2785.890400	237644.852332	56.010996
2785.556861	237438.722819	56.016001
2784.741676	237259.458093	56.021005
2784.397409	237048.823890	56.026010
2783.872837	236852.121940	56.031015
2782.826035	236641.217839	56.036020
2782.396856	236435.283633	56.041025
2781.537846	236232.473551	56.046029
2780.806549	236032.495566	56.051034
2780.418451	235819.706316	56.056039
2779.416044	235623.387887	56.061044
2778.955227	235411.298504	56.066049
2778.011088	235229.282108	56.071053
2777.546325	235021.293775	56.076058
2777.012253	234813.240450	56.081063
2776.094753	234619.202193	56.086068
2775.747944	234408.064435	56.091073
2775.143741	234215.046792	56.096077
2774.294609	234009.311247	56.101082
2773.664157	233806.367900	56.106087
2772.951784	233604.227298	56.111092
2772.348725	233393.768843	56.116097
2771.491263	233193.765492	56.121101
2770.867140	232999.505681	56.126106
2770.511680	232794.585680	56.131111
2769.273767	232597.215562	56.136116
2768.561061	232389.959492	56.141121
2768.331738	232192.761474	56.146125
2767.489338	231980.052345	56.151130
2766.868530	231789.613847	56.156135
2766.174803	231596.411860	56.161140
2766.020535	231386.803355	56.166145
2765.185938	231185.578369	56.171149
2764.341818	230979.288307	56.176154
2764.004151	230777.017925	56.181159
2762.857664	230573.984909	56.186164
2762.515437	230364.790408	56.191169
2761.656197	230170.115324	56.196173
2760.958342	229960.570678	56.201178
2760.351358	229759.312753	56.206183
2759.568753	229559.279806	56.211188
2759.061723	229351.921538	56.216193
2758.072224	229157.727578	56.221197
2757.566343	228948.638653	56.226202
2757.230528	228746.117882	56.231207
2756.482310	228555.044281	56.236212
2755.752243	228352.204931	56.241217
2754.769483	228147.216376	56.246221
2754.336062	227950.416294	56.251226
2753.703685	227742.394192	56.256231
2752.890519	227541.555885	56.261236
2752.212148	227345.356125	56.266241
2751.389095	227146.302601	56.271245
2750.931588	226955.823005	56.276250
2750.514471	226742.524210	56.281255
2749.619172	226559.218515	56.286260
2749.268840	226349.169156	56.291265
2748.553497	226149.260695	56.296269
2747.980032	225945.765705	56.301274
2747.330683	225745.274885	56.306279
2746.626807	225537.447737	56.311284
2746.226029	225330.247812	56.316289
2745.477617	225125.114865	56.321293
2744.443110	224923.808650	56.326298
2743.964127	224708.042449	56.331303
2743.368877	224518.723236	56.336308
2742.465351	224307.710076	56.341313
2741.900073	224103.187206	56.346317
2741.187667	223897.644288	56.351322
2740.814814	223693.461157	56.356327
2740.090074	223493.407915	56.361332
2739.430727	223283.606323	56.366337
2738.528124	223080.679841	56.371341
2737.943915	222874.049941	56.376346
2737.325058	222663.938065	56.381351
2736.522285	222475.216697	56.386356
2735.964354	222253.321095	56.391361
2735.402539	222056.186310	56.396365
2734.423129	221850.169106	56.401370
2733.928711	221651.573479	56.406375
2732.871188	221457.624814	56.411380
2732.702620	221252.817403	56.416385
2731.847178	221046.451753	56.421389
2731.175781	220853.729163	56.426394
2730.724058	220640.159334	56.431399
2729.910042	220435.838258	56.436404
2729.369112	220236.044391	56.441409
2728.381671	220041.018978	56.446413
2728.012386	219832.135587	56.451418
2727.568012	219622.551828	56.456423
2726.381031	219433.631566	56.461428
2726.217297	219224.666413	56.466433
2725.469209	219022.400945	56.471437
2724.573658	218815.882348	56.476442
2724.172113	218606.842065	56.481447
2723.449370	218402.677642	56.486452
2722.664881	218195.213985	56.491457
2722.095329	217996.703667	56.496461
2721.401519	217794.636696	56.501466
2721.045315	217587.361535	56.506471
2719.905555	217390.521629	56.511476
2719.335147	217169.432405	56.516481
2718.911573	216981.225023	56.521485
2717.901831	216771.700908	56.526490
2717.443256	216562.319229	56.531495
2716.541316	216370.612436	56.536500
2715.920175	216169.187774	56.541505
2715.677441	215971.153257	56.546509
2714.609870	215759.986595	56.551514
2714.213482	215554.518557	56.556519
2713.278972	215353.082266	56.561524
2712.651916	215143.667917	56.566529
2711.970495	214944.305692	56.571533
2711.364201	214746.841436	56.576538
2710.644382	214537.749129	56.581543
2709.742486	214341.656646	56.586548
2709.359759	214133.759584	56.591553
2708.389384	213937.042704	56.596557
2707.803759	213732.819352	56.601562
2707.317143	213538.954539	56.606567
2706.364910	213339.932715	56.611572
2705.949767	213141.551919	56.616577
2705.461760	212939.746638	56.621581
2704.709847	212737.207361	56.626586
2704.510263	212533.588417	56.631591
2703.257455	212337.862911	56.636596
2702.963008	212128.939904	56.641601
2702.326814	211932.837918	56.646605
2701.401582	211725.670775	56.651610
2701.086342	211514.932935	56.656615
2700.239021	211315.506088	56.661620
2699.634752	211106.902747	56.666625
2699.292108	210913.799321	56.671629
2698.487255	210701.614373	56.676634
2697.812516	210492.896924	56.681639
2697.267910	210286.985097	56.686644
2696.200982	210071.967311	56.691649
2695.588433	209877.204290	56.696653
2694.575944	209665.246628	56.701658
2694.602809	209459.386984	56.706663
2693.515158	209267.004809	56.711668
2693.098686	209046.198312	56.716673
2692.535452	208842.139668	56.721677
2691.745909	208637.646635	56.726682
2690.971794	208434.310023	56.731687
2690.307147	208232.382199	56.736692
2689.641918	208033.229672	56.741697
2688.901257	207825.129794	56.746701
2688.229194	207623.141523	56.751706
2687.810662	207402.977622	56.756711
2686.576688	207213.577759	56.761716
2686.243916	207003.074305	56.766721
2685.724409	206804.500900	56.771725
2684.851476	206603.820562	56.776730
2684.407288	206396.773160	56.781735
2683.459741	206197.238703	56.786740
2683.088279	205988.157630	56.791745
2682.434885	205788.119784	56.796749
2681.551233	205579.197658	56.801754
2681.271987	205377.536543	56.806759
2680.263034	205171.741025	56.811764
2679.790409	204966.943025	56.816769
2679.006838	204757.944337	56.821773
2678.270547	204557.796554	56.826778
2677.614199	204357.878599	56.831783
2677.094291	204156.208927	56.836788
2676.448012	203948.591312	56.841793
2675.582981	203744.852451	56.846797
2674.692242	203548.639618	56.851802
2674.315150	203336.196492	56.856807
2673.457402	203143.454085	56.861812
2673.130424	202934.936908	56.866817
2672.438667	202737.791787	56.871821
2671.697421	202537.677296	56.876826
2671.025235	202327.868084	56.881831
2670.391833	202127.203474	56.886836
2670.086107	201925.482322	56.891841
2669.271020	201719.706686	56.896845
2668.308359	201514.349689	56.901850
2668.106602	201309.140144	56.906855
2667.240391	201106.034564	56.911860
2666.612967	200893.831215	56.916865
2665.872088	200693.850537	56.921869
2665.328181	200485.885890	56.926874
2664.815055	200284.725316	56.931879
2663.952623	200084.104391	56.936884
2663.531662	199870.930602	56.941889
2662.698963	199666.768830	56.946893
2661.872871	199455.747818	56.951898
2661.380654	199236.136063	56.956903
2660.781426	199045.390282	56.961908
2660.029303	198823.530840	56.966913
2659.262794	198622.849235	56.971917
2658.707640	198413.749058	56.976922
2658.190327	198208.295793	56.981927
2657.581092	198005.708284	56.986932
2656.866643	197792.182036	56.991937
2656.185942	197578.447703	56.996941
2655.101408	197372.476748	57.001946
2655.076741	197168.056530	57.006951
2654.204053	196960.463027	57.011956
2653.413560	196747.780170	57.016961
2652.749799	196531.044388	57.021965
2652.278265	196331.711745	57.026970
2651.724613	196123.536594	57.031975
2650.702148	195911.593758	57.036980
2650.077206	195702.070076	57.041985
2649.583569	195494.129716	57.046989
2648.672272	195295.443340	57.051994
2648.330290	195075.227112	57.056999
2647.297095	194872.044572	57.062004
2646.644442	194654.882296	57.067009
2645.978343	194456.211235	57.072013
2645.474949	194242.971552	57.077018
2644.671478	194034.335511	57.082023
2643.691452	193843.045634	57.087028
2643.467493	193622.549805	57.092033
2642.714757	193420.664671	57.097037
2641.916857	193219.334631	57.102042
2641.721157	193013.227645	57.107047
2640.979200	192810.745250	57.112052
2639.985343	192605.262637	57.117057
2639.334942	192397.957877	57.122061
2638.404864	192189.515007	57.127066
2637.878799	191980.512790	57.132071
2637.165565	191789.862881	57.137076
2636.540731	191587.214263	57.142081
2636.043462	191376.708692	57.147085
2635.184583	191177.966749	57.152090
2634.871633	190975.436656	57.157095
2633.916457	190777.424107	57.162100
2633.305619	190560.514849	57.167105
2632.679265	190356.433882	57.172109
2631.973776	190156.615806	57.177114
2631.431637	189952.535928	57.182119
2630.756525	189751.327919	57.187124
2630.346382	189542.101538	57.192129
2629.525876	189331.796038	57.197133
2628.720107	189132.481588	57.202138
2628.202750	188927.333449	57.207143
2627.401311	188714.559455	57.212148
2627.132226	188502.172804	57.217153
2626.202185	188298.861214	57.222157
2625.314370	188103.228185	57.227162
2624.955229	187897.207045	57.232167
2624.075367	187702.108770	57.237172
2623.765578	187489.822197	57.242177
2623.176830	187277.873400	57.247181
2622.054249	187072.218583	57.252186
2621.540077	186869.839643	57.257191
2620.803517	186665.677566	57.262196
2620.245752	186453.943899	57.267201
2619.337896	186252.927684	57.272205
2618.740624	186051.417870	57.277210
2618.315593	185845.976038	57.282215
2617.510120	185640.684460	57.287220
2617.201121	185427.236832	57.292225
2616.708929	185221.757560	57.297229
2615.394557	185022.744859	57.302234
2615.118266	184812.538947	57.307239
2614.253886	184599.132323	57.312244
2613.635783	184393.409603	57.317249
2612.957074	184186.514337	57.322253
2612.474638	183983.252666	57.327258
2611.815057	183768.125593	57.332263
2610.746435	183570.123516	57.337268
2610.191950	183355.388855	57.342273
2609.789198	183158.351675	57.347277
2608.768916	182951.859714	57.352282
2608.489078	182740.150276	57.357287
2607.591180	182548.702445	57.362292
2607.069938	182331.385125	57.367297
2606.156034	182130.273792	57.372301
2605.216949	181929.625317	57.377306
2604.875558	181723.222347	57.382311
2604.180177	181525.335659	57.387316
2603.392085	181322.147359	57.392321
2602.800222	181107.556779	57.397325
2602.063538	180917.604271	57.402330
2601.867845	180712.276959	57.407335
2600.953834	180504.482214	57.412340
2600.300377	180292.754781	57.417345
2599.792065	180097.376295	57.422349
2598.784599	179896.112041	57.427354
2598.546852	179686.026221	57.432359
2597.611238	179489.013722	57.437364
2597.086884	179284.661142	57.442369
2596.517248	179062.839566	57.447373
2595.645230	178871.912674	57.452378
2595.233186	178655.118033	57.457383
2594.231438	178450.908706	57.462388
2593.845208	178247.162496	57.467393
2593.421517	178038.602479	57.472397
2592.367129	177835.638274	57.477402
2592.265855	177626.774818	57.482407
2591.419731	177421.172124	57.487412
2590.465093	177203.440664	57.492417
2589.989218	177004.230059	57.497421
2589.238330	176799.492967	57.502426
2588.705588	176588.439054	57.507431
2587.941418	176384.990746	57.512436
2587.067612	176171.118490	57.517441
2586.707861	175962.482409	57.522445
2585.744498	175755.520177	57.527450
2585.298651	175546.658187	57.532455
2584.570554	175348.907315	57.537460
2583.993790	175131.711952	57.542465
2583.472791	174920.499385	57.547469
2582.709484	174720.200689	57.552474
2581.961015	174503.709964	57.557479
2581.145410	174300.992386	57.562484
2580.765481	174080.871634	57.567489
2580.165549	173879.966153	57.572493
2579.219545	173676.318497	57.577498
2578.665284	173460.883631	57.582503
2577.929371	173254.940981	57.587508
2577.077096	173045.634827	57.592513
2576.651066	172841.362133	57.597517
2576.057349	172637.358697	57.602522
2575.468030	172426.068279	57.607527
2574.679694	172220.431781	57.612532
2574.121120	172015.968122	57.617537
2573.411160	171798.392173	57.622541
2572.548430	171603.097402	57.627546
2572.268569	171384.069362	57.632551
2571.353641	171174.274304	57.637556
2570.932651	170970.570023	57.642561
2570.174307	170753.465341	57.647565
2569.326138	170548.711824	57.652570
2569.014085	170340.784149	57.657575
2568.060833	170133.188101	57.662580
2567.146225	169920.449353	57.667585
2566.294550	169709.736513	57.672589
2565.588555	169510.103591	57.677594
2565.263639	169306.608974	57.682599
2564.887367	169115.598723	57.687604
2563.672404	168905.075011	57.692609
2563.313056	168695.968292	57.697613
2562.483821	168492.761364	57.702618
2562.436016	168285.260666	57.707623
2561.465187	168080.514237	57.712628
2560.842227	167866.303671	57.717633
2560.497697	167660.519235	57.722637
2559.658595	167452.194749	57.727642
2558.813273	167248.907990	57.732647
2558.018727	167039.675864	57.737652
2557.257998	166835.119032	57.742657
2556.761900	166621.569346	57.747661
2555.800904	166407.026414	57.752666
2555.451134	166211.092788	57.757671
2554.712827	166000.229906	57.762676
2554.022276	165799.927361	57.767681
2553.296753	165596.719561	57.772685
2552.571804	165386.366653	57.777690
2552.304874	165178.625308	57.782695
2551.585633	164979.107367	57.787700
2550.800964	164771.323199	57.792705
2550.168552	164565.881105	57.797709
2549.061626	164357.094972	57.802714
2549.044534	164140.775265	57.807719
2548.113460	163944.437115	57.812724
2547.370031	163734.503418	57.817729
2546.982505	163531.762004	57.822733
2546.221557	163349.640754	57.827738
2545.786095	163067.543678	57.832743
2544.955081	162856.560869	57.837748
2544.437092	162639.846260	57.842753
2543.823285	162427.000624	57.847757
2542.807275	162213.711403	57.852762
2542.204311	162008.317165	57.857767
2541.476840	161803.159971	57.862772
2541.081534	161597.798733	57.867777
2540.610856	161379.774622	57.872781
2539.736491	161174.873148	57.877786
2539.036709	160960.447832	57.882791
2538.615950	160755.985427	57.887796
2538.027014	160543.820834	57.892801
2537.167186	160331.369880	57.897805
2536.333896	160133.358735	57.902810
2535.814884	159910.100509	57.907815
2535.098982	159703.809316	57.912820
2534.134785	159489.383924	57.917825
2534.069833	159270.876172	57.922829
2532.927207	159071.839362	57.927834
2532.380432	158857.389802	57.932839
2531.497984	158649.135205	57.937844
2530.870052	158440.854221	57.942849
2530.349342	158226.493384	57.947853
2529.482826	158028.664617	57.952858
2528.771675	157816.497680	57.957863
2528.109480	157627.499668	57.962868
2527.424204	157415.076825	57.967873
2526.970719	157196.224098	57.972877
2526.148485	157002.932566	57.977882
2525.778792	156810.358566	57.982887
2524.950311	156603.938269	57.987892
2524.478481	156390.292933	57.992897
2523.683313	156179.255332	57.997901
2522.597774	155979.286503	58.002906
2522.208893	155771.848125	58.007911
2521.549124	155566.678541	58.012916
2520.721159	155380.248835	58.017921
2520.282873	155159.766837	58.022925
2519.608634	154959.586256	58.027930
2519.141083	154756.450402	58.032935
2518.634562	154552.711783	58.037940
2517.599107	154341.609248	58.042945
2516.948518	154137.018871	58.047949
2516.201733	153931.250110	58.052954
2515.839542	153719.205812	58.057959
2515.056089	153523.169525	58.062964
2514.465872	153320.061766	58.067969
2514.094415	153100.091078	58.072973
2512.937061	152898.562964	58.077978
2512.663742	152692.536101	58.082983
2511.838597	152497.542025	58.087988
2511.227106	152278.974858	58.092993
2510.701868	152072.890076	58.097997
2509.600369	151866.529301	58.103002
2509.081032	151654.027327	58.108007
2508.536974	151455.753643	58.113012
2507.601832	151243.498162	58.118017
2507.257667	151036.844597	58.123021
2506.419685	150829.342753	58.128026
2505.751591	150624.382744	58.133031
2505.164197	150427.126235	58.138036
2504.399724	150217.519456	58.143041
2503.822532	150008.583384	58.148045
2503.278861	149804.117196	58.153050
2502.458362	149595.285889	58.158055
2501.855758	149385.315649	58.163060
2501.003202	149189.913434	58.168065
2500.561421	148967.960694	58.173069
2499.680992	148765.206667	58.178074
2499.108778	148562.582993	58.183079
2498.362989	148359.263677	58.188084
2497.733906	148150.525750	58.193089
2497.335176	147950.636324	58.198093
2496.281975	147746.009745	58.203098
2495.754403	147533.536006	58.208103
2495.156795	147336.147472	58.213108
2494.658457	147133.381324	58.218113
2493.955112	146921.676629	58.223117
2493.014446	146720.495556	58.228122
2492.525555	146505.315612	58.233127
2491.885958	146303.771749	58.238132
2491.320305	146097.553483	58.243137
2490.765980	145891.754140	58.248141
2489.821817	145690.262467	58.253146
2489.556556	145474.024736	58.258151
2488.763871	145278.459082	58.263156
2487.615468	145069.417074	58.268161
2487.730198	144856.262227	58.273165
2486.677256	144642.594988	58.278170
2486.214343	144430.792670	58.283175
2485.441411	144226.678195	58.288180
2484.863630	144024.452959	58.293185
2484.300249	143809.201643	58.298189
2483.202990	143601.838750	58.303194
2482.709540	143379.831732	58.308199
2482.020206	143177.782188	58.313204
2481.156644	142985.482501	58.318209
2480.760539	142769.169925	58.323213
2479.858073	142574.312159	58.328218
2479.199019	142362.821921	58.333223
2478.819332	142160.564782	58.338228
2477.757263	141957.718275	58.343233
2477.382705	141753.976327	58.348237
2476.591498	141550.657564	58.353242
2476.006459	141336.278315	58.358247
2475.431020	141128.074324	58.363252
2474.369636	140931.142976	58.368257
2473.878093	140716.359385	58.373261
2473.206468	140523.345927	58.378266
2472.590528	140319.410437	58.383271
2471.890401	140113.100959	58.388276
2471.190242	139918.774474	58.393281
2470.731549	139708.223874	58.398285
2469.997668	139507.882875	58.403290
2469.531857	139296.828059	58.408295
2468.670660	139091.681913	58.413300
2467.739111	138889.572203	58.418305
2467.530315	138684.554130	58.423309
2466.666396	138484.812327	58.428314
2465.947853	138275.710560	58.433319
2465.630816	138072.136828	58.438324
2464.827293	137868.781359	58.443329
2464.556344	137653.756041	58.448333
2462.962769	137459.930202	58.453338
2462.751204	137249.713510	58.458343
2462.152091	137047.995590	58.463348
2461.633924	136837.868544	58.468353
2460.788380	136629.814894	58.473357
2460.031665	136435.304143	58.478362
2459.485532	136225.516219	58.483367
2459.058374	136019.992231	58.488372
2458.090240	135821.974609	58.493377
2457.308851	135605.253896	58.498381
2456.735669	135406.973217	58.503386
2456.244542	135197.971587	58.508391
2455.665356	134989.341120	58.513396
2454.496865	134792.429366	58.518401
2454.145783	134581.504428	58.523405
2453.343757	134382.288847	58.528410
2452.756835	134169.714739	58.533415
2451.924758	133969.604829	58.538420
2451.195752	133766.469321	58.543425
2450.901471	133564.269875	58.548429
2449.842477	133365.330709	58.553434
2449.544132	133166.158016	58.558439
2449.264538	132963.681005	58.563444
2448.421658	132763.034989	58.568449
2448.014227	132547.154424	58.573453
2446.881884	132342.035122	58.578458
2446.337145	132127.106786	58.583463
2445.357311	131928.787490	58.588468
2444.792225	131725.246716	58.593473
2444.576932	131504.440529	58.598477
2443.738992	131312.682760	58.603482
2443.289635	131098.229771	58.608487
2442.710124	130889.578394	58.613492
2441.842341	130678.421201	58.618497
2441.208049	130463.672104	58.623501
2440.519414	130258.472155	58.628506
2439.902924	130046.886116	58.633511
2438.944432	129840.792089	58.638516
2438.550448	129636.604194	58.643521
2437.966220	129425.729006	58.648525
2437.206163	129225.234696	58.653530
2436.522618	129007.341991	58.658535
2435.993202	128798.152094	58.663540
2435.191271	128591.470933	58.668545
2434.637956	128376.458316	58.673549
2433.843565	128179.075971	58.678554
2433.504741	127965.391509	58.683559
2432.956734	127756.783937	58.688564
2432.292966	127532.816167	58.693569
2431.684943	127327.929854	58.698573
2430.427127	127115.515284	58.703578
2429.924164	126898.296367	58.708583
2429.413273	126682.426621	58.713588
2428.868804	126477.904872	58.718593
2428.127100	126259.115985	58.723597
2427.046368	126057.679537	58.728602
2426.823037	125835.954437	58.733607
2426.300388	125627.257442	58.738612
2425.017034	125415.355410	58.743617
2424.480672	125201.723802	58.748621
2423.771898	124998.344040	58.753626
2423.430249	124794.018666	58.758631
2422.665334	124580.339297	58.763636
2421.718896	124366.880878	58.768641
2421.250860	124161.437425	58.773645
2420.298159	123953.723119	58.778650
2419.604916	123748.813767	58.783655
2419.128813	123533.649273	58.788660
2418.768108	123332.499922	58.793665
2418.186544	123119.018962	58.798669
2417.541568	122908.762399	58.803674
2416.685768	122691.683949	58.808679
2416.068398	122486.670642	58.813684
2415.358996	122279.311696	58.818689
2414.853491	122074.220341	58.823693
2414.094265	121862.682273	58.828698
2413.353967	121648.197052	58.833703
2412.780267	121437.280542	58.838708
2412.096837	121230.128838	58.843713
2411.493454	121015.258816	58.848717
2410.674966	120803.205330	58.853722
2409.897500	120596.136997	58.858727
2409.504197	120381.695931	58.863732
2408.910390	120179.947186	58.868737
2408.144007	119957.988692	58.873741
2407.453351	119764.968480	58.878746
2406.863841	119544.178940	58.883751
2406.531008	119331.615969	58.888756
2405.185705	119122.954327	58.893761
2404.949941	118905.110451	58.898765
2404.243863	118697.849031	58.903770
2403.472236	118486.397262	58.908775
2402.910244	118273.511077	58.913780
2402.155387	118053.604677	58.918785
2401.644295	117837.635262	58.923789
2400.615588	117644.341602	58.928794
2400.349115	117431.015584	58.933799
2399.881093	117205.637238	58.938804
2398.774007	116999.386121	58.943809
2398.103001	116786.726258	58.948813
2397.187835	116577.655153	58.953818
2396.925712	116373.439618	58.958823
2396.441359	116165.928531	58.963828
2395.648619	115945.779563	58.968833
2395.107341	115732.942853	58.973837
2394.025777	115528.241952	58.978842
2393.699548	115310.138157	58.983847
2393.187940	115088.746045	58.988852
2392.208164	114887.302969	58.993857
2391.514164	114672.538082	58.998861
2391.019908	114462.509966	59.003866
2390.591402	114247.585997	59.008871
2389.786410	114036.658640	59.013876
2388.962867	113821.229711	59.018881
2388.657417	113603.664112	59.023885
2387.670789	113395.728537	59.028890
2387.062274	113178.823954	59.033895
2386.482900	112953.526353	59.038900
2385.539465	112749.175147	59.043905
2385.107861	112535.846603	59.048909
2384.119867	112328.148583	59.053914
2383.697131	112112.683478	59.058919
2383.353463	111901.618436	59.063924
2382.424332	111697.590895	59.068929
2381.926343	111476.355376	59.073933
2381.014839	111270.101010	59.078938
2380.459465	111052.400523	59.083943
2380.186275	110833.673561	59.088948
2379.349885	110613.362473	59.093953
2378.436160	110396.708215	59.098957
2377.829387	110182.894597	59.103962
2377.388398	109963.142182	59.108967
2376.512919	109756.304584	59.113972
2375.863143	109539.926965	59.118977
2375.407418	109313.037358	59.123981
2374.443899	109114.176668	59.128986
2373.845174	108902.631982	59.133991
2373.539782	108680.045770	59.138996
2372.637686	108460.900276	59.144001
2372.048873	108239.371958	59.149005
2371.286887	108032.492878	59.154010
2370.786954	107809.272858	59.159015
2370.378789	107598.794333	59.164020
2369.355422	107384.062363	59.169025
2368.613600	107157.948858	59.174029
2368.016637	106936.890578	59.179034
2367.319857	106724.079669	59.184039
2366.966748	106504.839434	59.189044
2366.271828	106289.221241	59.194049
2365.737969	106067.900785	59.199053
2364.755787	105852.293992	59.204058
2364.238527	105633.430352	59.209063
2363.598194	105412.900537	59.214068
2362.778921	105191.316194	59.219073
2362.024957	104969.875821	59.224077
2361.401792	104752.204443	59.229082
2360.679947	104544.200631	59.234087
2360.029523	104316.418138	59.239092
2359.245897	104097.934382	59.244097
2358.756915	103877.033154	59.249101
2357.884130	103671.991976	59.254106
2357.448710	103447.083053	59.259111
2356.946382	103231.366809	59.264116
2356.036519	103016.053392	59.269121
2355.596608	102800.470759	59.274125
2354.873902	102580.037419	59.279130
2354.271096	102366.076922	59.284135
2353.525168	102153.251238	59.289140
2352.854006	101940.656692	59.294145
2352.520360	101709.575743	59.299149
2351.688604	101488.852761	59.304154
2351.368250	101271.501683	59.309159
2350.699154	101037.613266	59.314164
2349.714062	100827.254455	59.319169
2349.271326	100597.813047	59.324173
2348.614081	100372.328102	59.329178
2347.751146	100155.625345	59.334183
2347.334926	99931.172138	59.339188
2346.578038	99714.336171	59.344193
2345.909859	99480.361803	59.349197
2345.068005	99263.733830	59.354202
2344.391926	99039.235342	59.359207
2343.938261	98807.580682	59.364212
2342.996227	98591.019321	59.369217
2342.574013	98369.411166	59.374221
2341.616990	98149.868888	59.379226
2340.836949	97927.421078	59.384231
2340.415304	97706.218832	59.389236
2339.687459	97489.348499	59.394241
2339.110334	97266.088470	59.399245
2338.175680	97042.798526	59.404250
2337.387275	96826.166088	59.409255
2337.462354	96599.777517	59.414260
2336.253686	96386.634410	59.419265
2335.773968	96162.538930	59.424269
2335.160573	95941.599868	59.429274
2334.170310	95716.720888	59.434279
2333.780106	95486.802241	59.439284
2333.104921	95275.487601	59.444289
2332.573014	95053.371046	59.449293
2331.580192	94835.540729	59.454298
2330.944404	94614.713337	59.459303
2330.434917	94391.248973	59.464308
2329.713239	94187.714142	59.469313
2329.261627	93959.330148	59.474317
2328.558759	93748.624024	59.479322
2327.707771	93512.190811	59.484327
2326.926629	93292.198529	59.489332
2326.353506	93084.934141	59.494337
2325.976777	92862.237646	59.499341
2325.193550	92647.306038	59.504346
2324.154094	92425.004371	59.509351
2324.137322	92194.851054	59.514356
2322.952564	91986.457400	59.519361
2322.515094	91754.251140	59.524365
2321.985034	91530.679234	59.529370
2321.067939	91307.348511	59.534375
2320.718324	91088.742678	59.539380
2319.950631	90881.681938	59.544385
2319.337310	90645.108469	59.549389
2318.700370	90424.265842	59.554394
2317.836184	90201.058432	59.559399
2317.246490	89976.979170	59.564404
2316.344394	89772.359571	59.569409
2315.771272	89546.379985	59.574413
2315.212199	89327.330377	59.579418
2314.385678	89107.906932	59.584423
2314.149200	88885.304495	59.589428
2313.097553	88666.593250	59.594433
2312.721895	88435.464781	59.599437
2311.835632	88220.706960	59.604442
2311.085397	88005.473226	59.609447
2310.668651	87783.329103	59.614452
2310.013805	87566.506003	59.619457
2309.220463	87335.740795	59.624461
2308.463233	87119.851326	59.629466
2308.086647	86902.071534	59.634471
2307.644801	86674.097773	59.639476
2306.528556	86464.345010	59.644481
2305.989088	86235.104492	59.649485
2305.765924	86013.683278	59.654490
2304.895086	85791.314758	59.659495
2304.314402	85571.881925	59.664500
2303.233281	85349.082259	59.669505
2302.719460	85113.605713	59.674509
2302.320824	84888.528350	59.679514
2301.518578	84665.076731	59.684519
2300.898387	84451.626558	59.689524
2300.026737	84237.445083	59.694529
2299.393028	84007.508151	59.699533
2298.874252	83780.826200	59.704538
2298.032012	83559.718830	59.709543
2297.311931	83337.187262	59.714548
2296.393922	83118.701633	59.719553
2295.999413	82898.696444	59.724557
2295.396672	82678.916723	59.729562
2294.651726	82460.866825	59.734567
2294.583848	82239.263868	59.739572
2293.521419	82024.019604	59.744577
2292.993166	81786.047172	59.749581
2292.421159	81561.723593	59.754586
2291.261702	81341.843356	59.759591
2291.075652	81111.892416	59.764596
2289.993170	80896.998835	59.769601
2289.625545	80663.253652	59.774605
2288.572627	80436.806594	59.779610
2287.843459	80223.131454	59.784615
2287.521961	80012.271061	59.789620
2286.518789	79794.467407	59.794625
2286.149210	79561.197561	59.799629
2285.570054	79341.499939	59.804634
2284.652615	79122.935623	59.809639
2284.231946	78896.893086	59.814644
2283.048676	78685.650569	59.819649
2282.693325	78463.436338	59.824653
2282.207522	78247.100501	59.829658
2281.526817	78030.886567	59.834663
2280.994758	77804.423776	59.839668
2280.081647	77586.255302	59.844673
2279.511278	77356.432406	59.849677
2279.057050	77138.658497	59.854682
2278.051683	76912.394695	59.859687
2277.699737	76690.693382	59.864692
2277.020402	76480.597594	59.869697
2276.508168	76253.591237	59.874701
2275.676824	76028.158716	59.879706
2274.903347	75804.050112	59.884711
2274.226323	75579.200034	59.889716
2273.223747	75361.937606	59.894721
2273.130885	75136.258479	59.899725
2272.455918	74915.204342	59.904730
2271.522967	74699.636001	59.909735
2271.109047	74473.489320	59.914740
2270.637266	74256.053225	59.919745
2269.863820	74036.342157	59.924750
2269.074084	73800.588176	59.929754
2268.310572	73592.163964	59.934759
2267.840493	73355.876673	59.939764
2266.923038	73135.691469	59.944769
2266.385736	72917.925474	59.949774
2265.903433	72688.268334	59.954778
2264.954700	72469.755238	59.959783
2264.600325	72232.392232	59.964788
2263.923116	72014.822985	59.969793
2262.909625	71796.074148	59.974798
2262.373870	71569.105366	59.979802
2261.693010	71352.703213	59.984807
2261.228659	71125.335422	59.989812
2260.256035	70906.114809	59.994817
2259.713986	70683.065617	59.999822
2259.398897	70455.764187	60.004826
2258.388968	70239.204690	60.009831
2257.849857	70015.478452	60.014836
2256.843415	69791.778202	60.019841
2256.790703	69569.227729	60.024846
2255.657101	69347.098243	60.029850
2254.820865	69131.840874	60.034855
2254.432143	68906.481881	60.039860
2253.510303	68694.998926	60.044865
2253.097160	68469.680498	60.049870
2252.572686	68250.139704	60.054874
2251.695834	68030.669935	60.059879
2250.949971	67808.857423	60.064884
2250.290214	67590.048542	60.069889
2249.680696	67357.154854	60.074894
2249.009734	67151.576955	60.079898
2248.278847	66932.793081	60.084903
2248.001842	66706.751438	60.089908
2247.215225	66486.581785	60.094913
2246.525293	66267.165606	60.099918
2246.182866	66044.397284	60.104922
2244.772401	65828.412549	60.109927
2244.706006	65594.044812	60.114932
2243.889940	65377.182404	60.119937
2243.309843	65153.654626	60.124942
2242.866267	64924.398888	60.129946
2241.691599	64719.604346	60.134951
2241.353568	64481.433519	60.139956
2240.633289	64267.962663	60.144961
2239.922960	64048.195056	60.149966
2239.311951	63822.047085	60.154970
2238.084271	63604.909053	60.159975
2237.721714	63378.859895	60.164980
2237.191431	63164.491053	60.169985
2236.818491	62943.530199	60.174990
2235.680317	62723.636749	60.179994
2234.596730	62506.254102	60.184999
2234.479424	62282.645316	60.190004
2233.436057	62078.893536	60.195009
2232.895746	61859.079892	60.200014
2232.440830	61632.046755	60.205018
2231.647237	61427.011884	60.210023
2231.066395	61206.604425	60.215028
2230.419467	60997.375375	60.220033
2229.654718	60768.081322	60.225038
2229.232543	60560.375801	60.230042
2228.401653	60346.111861	60.235047
2227.921393	60123.684644	60.240052
2227.155765	59909.532454	60.245057
2226.449461	59691.327839	60.250062
2225.834481	59466.311948	60.255066
2224.887902	59253.854636	60.260071
2224.580820	59035.296793	60.265076
2223.942576	58819.237658	60.270081
2222.873964	58595.633636	60.275086
2222.254519	58381.801774	60.280090
2221.579583	58169.367528	60.285095
2221.249930	57959.970140	60.290100
2220.090990	57749.238036	60.295105
2219.508385	57539.122718	60.300110
2218.991877	57320.320702	60.305114
2218.357118	57112.190326	60.310119
2217.788735	56890.565753	60.315124
2217.173347	56686.295212	60.320129
2216.362386	56462.027213	60.325134
2215.588256	56246.481655	60.330138
2214.910696	56038.715132	60.335143
2214.438914	55826.098313	60.340148
2213.607387	55624.880379	60.345153
2212.944090	55406.798420	60.350158
2212.735215	55196.729594	60.355162
2211.809396	54978.675376	60.360167
2211.293622	54760.077685	60.365172
2210.320828	54545.570955	60.370177
2209.840472	54330.320907	60.375182
2209.364939	54118.414348	60.380186
2208.053570	53906.452970	60.385191
2207.653157	53695.362170	60.390196
2206.805518	53484.816254	60.395201
2206.231577	53274.219864	60.400206
2205.941168	53065.580788	60.405210
2205.080429	52852.354597	60.410215
2204.397441	52644.152860	60.415220
2203.747976	52430.258937	60.420225
2203.127593	52217.403940	60.425230
2202.430798	52003.209316	60.430234
2201.623517	51800.472992	60.435239
2201.418204	51593.824419	60.440244
2200.573586	51375.645485	60.445249
2199.575048	51165.220079	60.450254
2199.241874	50951.265018	60.455258
2198.241650	50738.402297	60.460263
2197.788358	50531.716656	60.465268
2197.110589	50325.701773	60.470273
2196.478099	50114.344727	60.475278
2195.907927	49893.745242	60.480282
2194.755387	49696.899252	60.485287
2194.505894	49480.812927	60.490292
2193.680966	49272.966921	60.495297
2192.778918	49066.119456	60.500302
2192.581235	48863.604326	60.505306
2191.648557	48657.462452	60.510311
2191.267020	48442.934474	60.515316
2190.273010	48242.061737	60.520321
2189.432110	48035.921999	60.525326
2189.109040	47824.251963	60.530330
2188.455252	47622.070072	60.535335
2187.761438	47406.016152	60.540340
2186.940907	47195.973078	60.545345
2186.131087	46997.264737	60.550350
2185.493456	46801.941265	60.555354
2184.724476	46598.982724	60.560359
2184.070459	46382.160029	60.565364
2183.324262	46192.917948	60.570369
2182.591102	45992.070510	60.575374
2182.115457	45787.429986	60.580378
2181.224479	45591.511707	60.585383
2180.701867	45396.675844	60.590388
2180.137405	45188.855464	60.595393
2179.198253	44991.436488	60.600398
2178.547236	44792.038358	60.605402
2177.579870	44607.956474	60.610407
2177.401483	44402.566997	60.615412
2176.341633	44216.482890	60.620417
2175.854033	44019.357486	60.625422
2175.752461	43813.431417	60.630426
2174.804916	43626.908826	60.635431
2174.157625	43420.656508	60.640436
2173.009409	43229.498843	60.645441
2172.536193	43031.895304	60.650446
2172.104995	42837.630113	60.655450
2171.328032	42646.290312	60.660455
2170.814629	42441.337651	60.665460
2169.820215	42257.016136	60.670465
2169.079202	42063.827068	60.675470
2168.610516	41860.641953	60.680474
2167.773109	41668.253696	60.685479
2167.082074	41483.892302	60.690484
2166.642033	41296.175889	60.695489
2165.553919	41101.730854	60.700494
2164.865348	40918.039186	60.705498
2164.349332	40733.376631	60.710503
2163.926787	40542.335957	60.715508
2162.994998	40358.391624	60.720513
2162.240949	40173.130964	60.725518
2161.944789	39982.829028	60.730522
2160.985887	39804.927997	60.735527
2160.077424	39611.347214	60.740532
2159.485836	39421.639076	60.745537
2158.575527	39247.780177	60.750542
2158.157162	39063.592828	60.755546
2157.221058	38891.267228	60.760551
2156.703072	38712.152003	60.765556
2155.661355	38529.571153	60.770561
2155.175517	38361.235957	60.775566
2154.789191	38177.361373	60.780570
2153.992851	38017.449303	60.785575
2153.278266	37838.853453	60.790580
2152.583598	37665.147241	60.795585
2151.812225	37489.343086	60.800590
2150.990690	37320.682605	60.805594
2149.801937	37150.608831	60.810599
2149.370369	36987.735329	60.815604
2148.712894	36827.829849	60.820609
2147.646402	36677.889010	60.825614
2146.612024	36525.005948	60.830618
2145.664470	36360.781953	60.835623
2145.133960	36218.258785	60.840628
2144.381306	36071.136093	60.845633
2143.292920	35922.498407	60.850638
2142.713887	35787.154666	60.855642
2141.718565	35657.792619	60.860647
2140.934354	35531.600320	60.865652
2140.280702	35400.406320	60.870657
2139.189263	35268.971438	60.875662
2138.887634	35143.410417	60.880666
2137.907772	35017.589684	60.885671
2137.127952	34899.179223	60.890676
2136.765445	34778.854198	60.895681
2135.792364	34667.199509	60.900686
2135.628315	34539.773588	60.905690
2134.808086	34428.777428	60.910695
2134.234490	34307.795457	60.915700
2133.618430	34178.544295	60.920705
2132.752621	34073.406968	60.925710
2132.229863	33944.269252	60.930714
2131.458508	33819.974857	60.935719
2130.619669	33705.920459	60.940724
2129.956268	33589.586949	60.945729
2129.278898	33471.891020	60.950734
2128.870159	33361.563654	60.955738
2127.956201	33257.445817	60.960743
2127.586577	33136.683364	60.965748
2127.110151	33025.014612	60.970753
2126.149058	32914.091991	60.975758
2125.951707	32792.083115	60.980762
2124.788772	32673.403175	60.985767
2124.110515	32562.728804	60.990772
2123.753820	32449.312928	60.995777
2123.000707	32338.773612	61.000782
2122.402594	32222.478832	61.005786
2121.552518	32101.760640	61.010791
2121.030707	31980.030459	61.015796
2120.481890	31874.185167	61.020801
2119.700757	31764.196158	61.025806
2119.432554	31646.285507	61.030810
2118.538936	31535.867089	61.035815
2117.812814	31422.036496	61.040820
2117.347517	31306.711544	61.045825
2116.653088	31186.180775	61.050830
2116.074853	31069.236776	61.055834
2114.809026	30955.755767	61.060839
2114.499821	30836.775014	61.065844
2113.949579	30726.876383	61.070849
2113.236624	30622.553645	61.075854
2112.368051	30502.422103	61.080858
2112.077836	30399.116072	61.085863
2111.434811	30283.361948	61.090868
2110.748549	30160.524171	61.095873
2110.224940	30053.484157	61.100878
2109.515991	29929.983345	61.105882
2108.578312	29816.963758	61.110887
2107.920719	29707.665698	61.115892
2107.553753	29589.866042	61.120897
2107.065591	29471.072105	61.125902
2106.578317	29364.079811	61.130906
2105.541650	29248.371764	61.135911
2104.984248	29121.223804	61.140916
2104.264277	29010.715830	61.145921
2103.436641	28886.857800	61.150926
2103.106795	28766.034183	61.155930
2102.356254	28658.053437	61.160935
2101.630274	28529.762956	61.165940
2100.836544	28419.019491	61.170945
2100.059258	28314.660068	61.175950
2099.721920	28202.074608	61.180954
2098.644249	28090.381535	61.185959
2098.462070	27968.628819	61.190964
2097.898211	27851.944095	61.195969
2096.955723	27741.966633	61.200974
2096.675562	27624.742456	61.205978
2095.723994	27510.390328	61.210983
2095.069866	27381.557215	61.215988
2094.517208	27278.589042	61.220993
2093.650931	27157.059970	61.225998
2093.094219	27040.844399	61.231002
2092.345724	26924.852824	61.236007
2091.887631	26812.539446	61.241012
2091.403854	26692.836214	61.246017
2090.557739	26585.849637	61.251022
2089.930306	26454.785154	61.256026
2089.102295	26346.039872	61.261031
2088.537194	26225.046604	61.266036
2087.940165	26114.263984	61.271041
2086.845738	26008.717067	61.276046
2086.673108	25885.047362	61.281050
2085.880572	25772.020265	61.286055
2085.461371	25655.884460	61.291060
2084.499388	25541.175927	61.296065
2083.994718	25423.767183	61.301070
2083.616707	25300.923566	61.306074
2082.608843	25186.297509	61.311079
2082.077741	25072.659664	61.316084
2081.332586	24954.839961	61.321089
2080.767714	24838.564954	61.326094
2080.310280	24716.563722	61.331098
2079.482199	24609.275470	61.336103
2078.843324	24484.377151	61.341108
2078.075828	24365.399647	61.346113
2077.353584	24251.073757	61.351118
2077.073306	24124.722701	61.356122
2076.292033	24017.251719	61.361127
2075.584282	23901.006192	61.366132
2074.911141	23779.254032	61.371137
2074.307798	23660.622943	61.376142
2073.536371	23540.138323	61.381146
2072.737633	23422.247593	61.386151
2072.152304	23307.625595	61.391156
2071.830615	23183.350456	61.396161
2070.657764	23070.459639	61.401166
2070.124908	22946.422019	61.406170
2069.089939	22843.627521	61.411175
2068.210006	22724.297896	61.416180
2067.933807	22614.954195	61.421185
2067.115515	22509.230992	61.426190
2066.691624	22389.047383	61.431194
2065.986411	22275.299144	61.436199
2065.314815	22158.796857	61.441204
2064.608743	22046.361988	61.446209
2063.727044	21937.892092	61.451214
2063.568091	21827.351553	61.456218
2062.770383	21716.135378	61.461223
2061.657503	21607.605729	61.466228
2061.257292	21489.738744	61.471233
2060.394305	21380.480881	61.476238
2059.923606	21273.075500	61.481242
2059.289324	21172.660215	61.486247
2058.610958	21051.459608	61.491252
2058.027631	20938.914433	61.496257
2057.273897	20833.698297	61.501262
2056.774082	20724.756858	61.506266
2055.870757	20617.232730	61.511271
2055.143737	20505.968854	61.516276
2054.317407	20392.534464	61.521281
2053.658579	20289.317892	61.526286
2053.222066	20186.460698	61.531290
2052.795613	20077.745795	61.536295
2052.150789	19965.210623	61.541300
2051.421278	19845.868594	61.546305
2050.448341	19743.160617	61.551310
2050.120238	19644.342764	61.556314
2049.425600	19529.734299	61.561319
2048.616792	19426.094415	61.566324
2048.034441	19310.895364	61.571329
2047.111519	19213.144918	61.576334
2046.694506	19098.295410	61.581338
2045.785117	18995.067110	61.586343
2045.052371	18887.567229	61.591348
2044.680736	18779.040123	61.596353
2043.491545	18685.040225	61.601358
2042.952099	18574.307771	61.606362
2042.623937	18476.866214	61.611367
2041.741412	18373.640518	61.616372
2041.442338	18267.161574	61.621377
2040.733625	18161.444258	61.626382
2040.231560	18046.638864	61.631386
2039.329568	17956.672046	61.636391
2038.671454	17843.741756	61.641396
2038.186736	17735.818097	61.646401
2037.105390	17631.135686	61.651406
2036.645805	17532.681621	61.656410
2035.777207	17439.070561	61.661415
2034.926042	17332.814685	61.666420
2033.937829	17231.554462	61.671425
2033.304259	17143.406007	61.676430
2032.726920	17043.871738	61.681434
2032.064763	16952.759241	61.686439
2031.457685	16868.270072	61.691444
2030.945875	16757.031082	61.696449
2030.024592	16672.000033	61.701454
2029.448978	16579.885141	61.706458
2028.792539	16488.266117	61.711463
2027.882689	16398.446133	61.716468
2027.444712	16307.963519	61.721473
2026.536739	16221.567856	61.726478
2026.052198	16122.834833	61.731482
2025.038239	16037.548277	61.736487
2024.360598	15948.068593	61.741492
2023.855878	15863.035078	61.746497
2022.680842	15780.408494	61.751502
2022.446963	15692.186312	61.756506
2021.608398	15607.006903	61.761511
2020.582568	15527.875948	61.766516
2020.286056	15443.246805	61.771521
2019.426507	15375.498818	61.776526
2018.772542	15278.961546	61.781530
2018.288920	15212.658018	61.786535
2017.507151	15138.405437	61.791540
2016.962405	15050.268821	61.796545
2016.225378	14983.914348	61.801550
2015.577371	14889.634722	61.806554
2014.956885	14824.332302	61.811559
2014.325880	14741.201013	61.816564
2013.771710	14657.983294	61.821569
2012.363877	14587.998660	61.826574
2012.270278	14505.529298	61.831578
2011.688275	14427.599329	61.836583
2010.894806	14355.501218	61.841588
2010.394402	14267.141063	61.846593
2009.384602	14196.378905	61.851598
2008.698803	14110.008166	61.856602
2007.963249	14050.249768	61.861607
2007.216163	13979.827913	61.866612
2007.125851	13900.518087	61.871617
2006.317789	13837.441629	61.876622
2005.756741	13760.946226	61.881626
2004.890096	13671.578540	61.886631
2004.296931	13597.478289	61.891636
2003.807581	13516.800285	61.896641
2002.925996	13450.088582	61.901646
2002.502916	13361.560477	61.906650
2001.724585	13294.130191	61.911655
2001.168336	13212.271054	61.916660
2000.485653	13148.137959	61.921665
1999.453660	13076.099123	61.926670
1999.035092	12996.387934	61.931674
1998.359830	12926.030065	61.936679
1997.546720	12859.429538	61.941684
1996.946190	12774.030490	61.946689
1996.078787	12705.910638	61.951694
1995.722774	12627.111931	61.956698
1994.873176	12565.796068	61.961703
1994.463967	12493.189717	61.966708
1994.061724	12408.779343	61.971713
1993.136968	12350.051361	61.976718
1992.515143	12271.311479	61.981722
1991.879932	12199.101459	61.986727
1990.833403	12126.054696	61.991732
1990.361691	12049.373076	61.996737
1989.831716	11982.808580	62.001742
1989.013842	11903.499223	62.006746
1988.367949	11839.997388	62.011751
1988.029769	11765.477911	62.016756
1987.397144	11690.009877	62.021761
1986.157874	11621.420274	62.026766
1985.872779	11545.888720	62.031770
1985.028183	11472.088657	62.036775
1984.166415	11408.684047	62.041780
1983.879234	11334.445819	62.046785
1982.910568	11264.823782	62.051790
1982.436626	11196.568350	62.056794
1981.446317	11129.116800	62.061799
1980.826940	11061.761728	62.066804
1980.540609	10992.500362	62.071809
1979.410963	10923.603579	62.076814
1978.929341	10861.376998	62.081818
1978.464997	10789.858299	62.086823
1977.496158	10733.063368	62.091828
1977.070541	10679.778943	62.096833
1976.349617	10610.631902	62.101838
1975.828875	10533.294242	62.106842
1974.880199	10465.986201	62.111847
1974.428614	10397.667304	62.116852
1973.889110	10331.262675	62.121857
1972.916711	10258.655411	62.126862
1972.418576	10196.478768	62.131866
1971.634400	10119.423131	62.136871
1970.813863	10056.827978	62.141876
1970.680533	9988.985508	62.146881
1969.811364	9927.560443	62.151886
1968.848924	9861.167419	62.156890
1968.143095	9795.477991	62.161895
1967.339908	9726.634074	62.166900
1966.872382	9665.003123	62.171905
1966.019019	9602.174424	62.176910
1965.517587	9545.660092	62.181914
1965.176674	9472.253778	62.186919
1964.445141	9413.656046	62.191924
1963.484984	9335.737046	62.196929
1962.889058	9284.246786	62.201934
1962.150201	9213.633995	62.206938
1961.630221	9154.612753	62.211943
1961.044230	9094.959208	62.216948
1960.742128	9024.659049	62.221953
1959.677143	8971.202070	62.226958
1959.137285	8897.302716	62.231962
1958.539863	8838.732093	62.236967
1957.565264	8776.509529	62.241972
1956.999039	8710.691832	62.246977
1956.426274	8648.534218	62.251982
1955.838961	8582.793407	62.256986
1954.998626	8522.214869	62.261991
1954.478863	8457.907650	62.266996
1954.174475	8389.847076	62.272001
1953.594122	8333.580990	62.277006
1952.441444	8267.424813	62.282010
1952.034963	8204.654101	62.287015
1951.205931	8138.864854	62.292020
1950.920324	8069.239897	62.297025
1949.886252	8012.822987	62.302030
1949.121953	7944.615756	62.307034
1948.467311	7875.921239	62.312039
1947.645465	7810.529906	62.317044
1947.217641	7751.991440	62.322049
1946.784898	7698.405909	62.327054
1945.928581	7634.002212	62.332058
1945.357093	7554.984304	62.337063
1944.451383	7507.298539	62.342068
1943.799207	7433.029793	62.347073
1943.449521	7378.011048	62.352078
1942.712276	7308.875487	62.357082
1941.923411	7252.325497	62.362087
1941.575138	7195.799655	62.367092
1940.672301	7119.422579	62.372097
1940.155996	7062.467162	62.377102
1939.127312	6994.263644	62.382106
1938.716973	6931.777753	62.387111
1938.038860	6870.599168	62.392116
1937.480112	6807.960257	62.397121
1936.398334	6749.603292	62.402126
1935.907744	6686.214526	62.407130
1935.525970	6622.343338	62.412135
1934.775380	6567.246079	62.417140
1934.231871	6495.915803	62.422145
1933.561606	6440.384236	62.427150
1932.904407	6376.310133	62.432154
1932.125769	6310.604569	62.437159
1931.517686	6250.876746	62.442164
1930.789834	6185.114768	62.447169
1930.058033	6124.716086	62.452174
1929.346217	6059.669942	62.457178
1928.630732	6000.812882	62.462183
1927.768991	5944.182413	62.467188
1927.592515	5872.422968	62.472193
1926.750647	5815.692811	62.477198
1926.015682	5755.747328	62.482202
1925.713422	5689.573701	62.487207
1924.902501	5634.722965	62.492212
1924.312002	5559.654732	62.497217
1923.328545	5506.862198	62.502222
1922.833275	5442.517165	62.507226
1922.352735	5382.729995	62.512231
1921.312382	5325.544185	62.517236
1920.791204	5258.591642	62.522241
1920.038431	5207.555644	62.527246
1919.244252	5143.640337	62.532250
1918.835837	5089.588266	62.537255
1918.434144	5026.604208	62.542260
1917.662017	4950.540933	62.547265
1916.945016	4901.578681	62.552270
1916.168121	4835.878593	62.557274
1915.489749	4762.147142	62.562279
1914.487136	4712.856205	62.567284
1914.065914	4656.359496	62.572289
1913.528152	4595.830557	62.577294
1912.808466	4535.348099	62.582298
1912.011325	4474.737792	62.587303
1911.062974	4426.387252	62.592308
1910.612896	4363.009875	62.597313
1910.092706	4309.000489	62.602318
1909.423094	4250.166776	62.607322
1909.020540	4195.407200	62.612327
1907.822128	4140.393228	62.617332
1907.409322	4074.928185	62.622337
1906.892413	4020.967444	62.627342
1906.145829	3968.798227	62.632346
1905.827894	3910.826509	62.637351
1904.803500	3851.529384	62.642356
1904.329420	3780.184608	62.647361
1903.562960	3730.031346	62.652366
1902.991400	3677.036434	62.657370
1902.381856	3609.108502	62.662375
1901.366804	3556.318510	62.667380
1900.972956	3492.156735	62.672385
1900.479322	3435.463259	62.677390
1899.952672	3381.931503	62.682394
1899.235997	3320.124651	62.687399
1898.228437	3251.644821	62.692404
1897.492864	3192.241412	62.697409
1896.843196	3146.403717	62.702414
1896.346082	3085.010954	62.707418
1895.970787	3014.008318	62.712423
1895.107467	2965.719279	62.717428
1894.103694	2911.544952	62.722433
1893.171326	2846.670229	62.727438
1892.725663	2797.320960	62.732442
1891.857690	2742.367817	62.737447
1891.077173	2693.628837	62.742452
1890.670790	2646.634220	62.747457
1890.261515	2591.528379	62.752462
1889.478946	2530.291301	62.757466
1888.811161	2476.974526	62.762471
1888.119343	2431.334242	62.767476
1887.838246	2375.103218	62.772481
1887.034798	2324.279275	62.777486
1886.486193	2263.482492	62.782490
1885.614373	2208.796149	62.787495
1885.130148	2166.678778	62.792500
1884.139796	2102.906413	62.797505
1883.489981	2055.518612	62.802510
1882.706145	2003.761335	62.807514
1882.068103	1941.670231	62.812519
1881.233286	1905.313962	62.817524
1880.904384	1839.689423	62.822529
1880.067619	1791.926826	62.827534
1879.193248	1729.923036	62.832538
1878.792970	1689.981238	62.837543
1878.150154	1647.023896	62.842548
1877.516558	1592.599335	62.847553
1877.037216	1537.507012	62.852558
1876.054332	1486.876133	62.857562
1875.843742	1444.440613	62.862567
1874.711541	1388.897356	62.867572
1874.022887	1335.450065	62.872577
1872.968057	1289.527966	62.877582
1872.209689	1237.388494	62.882586
1871.852811	1197.945041	62.887591
1870.844049	1156.593602	62.892596
1870.556240	1113.092568	62.897601
1870.051846	1066.631941	62.902606
1869.207714	1028.884406	62.907610
1868.774323	974.185921	62.912615
1867.951660	933.910315	62.917620
1867.508411	877.286570	62.922625
1866.891999	836.888593	62.927630
1866.202295	779.471667	62.932634
1865.289088	737.717505	62.937639
1864.478930	692.895505	62.942644
1863.893595	648.536294	62.947649
1863.387627	605.751123	62.952654
1862.238305	567.561209	62.957658
1861.955070	521.531648	62.962663
1860.930111	486.715978	62.967668
1860.346114	450.351128	62.972673
1859.580747	413.297622	62.977678
1858.974434	367.647866	62.982682
1858.615049	332.058236	62.987687
1857.905478	299.812360	62.992692
1856.891700	251.226619	62.997697
1856.305857	223.930408	63.002702
1855.299803	193.643959	63.007706
1855.010824	151.968997	63.012711
1853.961348	123.770432	63.017716
1853.561170	94.413823	63.022721
1852.594563	61.860776	63.027726
1851.641643	39.811476	63.032730
1850.708816	15.439284	63.037735
1848.900164	6.301020	63.042740
1847.713660	19.633685	63.047745
1846.374608	40.490706	63.052750
1845.387438	62.903561	63.057754
1845.170409	55.912717	63.062759
1845.035148	66.202089	63.067764
1845.106064	60.804008	63.072769
1844.726543	60.153205	63.077774
1844.298798	54.490522	63.082778
1843.577835	57.730735	63.087783
1842.118321	65.653586	63.092788
1841.005806	66.904318	63.097793
1840.667675	81.010675	63.102798
1840.240746	81.625834	63.107802
1839.559618	80.130348	63.112807
1838.632486	82.852936	63.117812
1838.736264	77.003344	63.122817
1838.000433	87.197277	63.127822
1837.104016	83.994983	63.132826
1836.757631	78.765661	63.137831
1836.481737	85.409310	63.142836
1835.435652	77.264855	63.147841
1834.677976	78.733642	63.152846
1834.046060	80.163536	63.157850
1833.626719	86.800000	63.162855
1832.360967	82.984558	63.167860
1831.578804	85.979025	63.172865
1831.021225	82.224603	63.177870
1830.593683	88.808753	63.182874
1830.239292	88.239118	63.187879
1829.215897	87.006145	63.192884
1828.544261	93.692136	63.197889
1828.108663	91.883269	63.202894
1827.680495	95.056499	63.207898
1827.233202	90.358873	63.212903
1825.978391	89.411810	63.217908
1825.786734	87.119498	63.222913
1825.298892	88.908148	63.227918
1824.435923	93.855144	63.232922
1823.815789	86.869948	63.237927
1823.194367	88.085286	63.242932
1822.461567	88.184457	63.247937
1821.693608	88.473718	63.252942
1820.587589	96.982297	63.257946
1820.091358	87.775954	63.262951
1818.784943	88.918711	63.267956
1818.548168	88.801920	63.272961
1818.874104	93.566436	63.277966
1817.922405	99.361750	63.282970
1817.161186	86.354370	63.287975
1816.099282	96.145919	63.292980
1816.048155	85.164176	63.297985
1815.622576	91.339578	63.302990
1814.335826	88.976728	63.307994
1813.967150	90.751188	63.312999
1813.532889	87.607982	63.318004
1811.991829	89.647460	63.323009
1811.774206	88.631900	63.328014
1811.340370	89.848993	63.333018
1810.793602	86.072358	63.338023
1810.002421	96.036966	63.343028
1809.250977	87.016236	63.348033
1808.552926	84.529944	63.353038
1808.035910	83.774821	63.358042
1807.420241	83.246680	63.363047
1806.509613	87.501065	63.368052
1805.984870	88.472391	63.373057
1805.323122	90.955726	63.378062
1804.277155	91.093593	63.383066
1803.873981	90.850260	63.388071
1803.054347	90.278813	63.393076
1802.604800	82.869137	63.398081
1801.985806	91.160028	63.403086
1800.961368	90.562756	63.408090
1800.234700	87.161628	63.413095
1799.545315	104.081934	63.418100
1798.821275	83.596895	63.423105
1799.125941	87.424900	63.428110
1798.343174	94.729376	63.433114
1797.601901	94.118679	63.438119
1796.323565	93.613768	63.443124
1795.742367	86.515164	63.448129
1795.651107	95.766218	63.453134
1795.043251	87.227327	63.458138
1794.340064	82.012094	63.463143
1793.540046	90.516240	63.468148
1792.669800	88.666014	63.473153
1792.071340	90.260920	63.478158
1791.233856	84.992896	63.483162
1790.905110	79.431191	63.488167
1790.170750	89.011453	63.493172
1789.264997	82.921623	63.498177
1788.995925	89.354452	63.503182
1787.847714	89.112739	63.508186
1787.799189	87.944170	63.513191
1786.868507	93.425488	63.518196
1786.448620	92.352163	63.523201
1785.494445	88.485687	63.528206
1784.873864	91.175381	63.533210
1784.730721	90.386121	63.538215
1783.900606	95.244330	63.543220
1783.247295	90.716628	63.548225
1782.836430	85.981688	63.553230
1781.610508	83.680161	63.558234
1780.611668	84.476041	63.563239
1779.636121	92.446660	63.568244
1779.465071	95.238436	63.573249
1779.724844	85.858430	63.578254
1778.161490	86.010662	63.583258
1777.420199	84.961572	63.588263
1776.815916	94.226286	63.593268
1776.187570	87.508920	63.598273
1775.993532	88.299997	63.603278
1774.755736	90.967862	63.608282
1774.550996	83.003641	63.613287
1773.609366	88.344771	63.618292
1773.162403	89.023048	63.623297
1772.592955	81.121479	63.628302
1771.946948	96.196125	63.633306
1771.505890	88.559596	63.638311
1770.982488	88.940924	63.643316
1770.022246	95.046697	63.648321
1768.774779	86.223031	63.653326
1768.104194	94.238265	63.658330
1768.120561	85.906185	63.663335
1766.777963	90.766937	63.668340
1766.035979	85.237745	63.673345
1766.255813	78.275296	63.678350
1765.123510	87.918760	63.683354
1764.529899	82.339198	63.688359
1763.551572	82.824315	63.693364
1762.990675	86.994785	63.698369
1762.693818	76.916269	63.703374
1761.826626	78.213230	63.708378
1761.553960	86.422314	63.713383
1760.735451	88.257182	63.718388
1760.265203	89.316058	63.723393
1759.982902	84.035570	63.728398
1758.412175	90.689316	63.733402
1757.762158	88.214334	63.738407
1756.581789	89.005937	63.743412
1756.771028	89.674643	63.748417
1756.171508	88.107870	63.753422
1755.251730	91.108444	63.758426
1754.749513	85.074390	63.763431
1754.067502	94.893935	63.768436
1753.311666	87.979199	63.773441
1753.163103	82.964484	63.778446
1752.417755	88.257100	63.783450
1751.568127	83.636007	63.788455
1750.291709	93.952085	63.793460
1749.597207	91.515710	63.798465
1749.441514	84.201305	63.803470
1748.677913	91.586327	63.808474
1748.391773	92.157063	63.813479
1747.961071	97.653607	63.818484
1747.382877	83.805043	63.823489
1746.185870	86.838611	63.828494
1744.811795	95.381902	63.833498
1744.737333	79.852700	63.838503
1743.636231	98.030592	63.843508
1743.320174	94.009168	63.848513
1742.841194	89.034312	63.853518
1742.331012	87.019683	63.858522
1741.636219	85.084838	63.863527
1740.813063	83.520472	63.868532
1740.191139	93.527597	63.873537
1739.699994	96.390714	63.878542
1739.209700	86.730857	63.883546
1738.540713	80.046770	63.888551
1737.449022	87.781951	63.893556
1736.454022	94.457815	63.898561
1735.910092	82.442580	63.903566
1735.296684	86.446349	63.908570
1734.908687	89.089652	63.913575
1733.923005	91.036236	63.918580
1733.606717	90.518911	63.923585
1733.175230	79.794718	63.928590
1732.485146	85.146371	63.933594
1732.378503	80.314239	63.938599
1730.883942	83.743585	63.943604
1729.922324	91.713583	63.948609
1729.541031	86.716908	63.953614
1728.862692	93.648415	63.958618
1728.300575	85.517029	63.963623
1727.752305	90.111286	63.968628
1727.257061	94.255567	63.973633
1727.089309	79.037660	63.978638
1725.679423	93.432524	63.983642
1724.821052	95.433010	63.988647
1723.819640	97.601298	63.993652
1723.675863	92.248347	63.998657
1723.316053	96.544587	64.003662
1722.284269	94.817815	64.008666
1721.966017	87.953441	64.013671
1721.347844	81.789577	64.018676
1720.470778	85.319552	64.023681
1719.569433	81.331171	64.028686
1718.867959	88.436666	64.033690
1718.354971	84.563224	64.038695
1717.708833	93.334689	64.043700
1717.514089	88.450316	64.048705
1716.883068	90.550313	64.053710
1716.095513	83.314196	64.058714
1715.349387	89.450631	64.063719
1713.941809	91.161452	64.068724
1713.630480	96.926050	64.073729
1713.248942	94.239698	64.078734
1712.232335	96.462444	64.083738
1711.773217	96.500829	64.088743
1711.353803	92.547868	64.093748
1710.771913	99.503486	64.098753
1710.034665	84.117407	64.103758
1708.764552	93.547811	64.108762
1708.281782	84.506525	64.113767
1707.682917	88.493798	64.118772
1707.094309	93.793070	64.123777
1706.806263	90.513118	64.128782
1706.049906	94.750916	64.133786
1706.026471	89.932376	64.138791
1704.897522	88.965381	64.143796
1703.713006	89.833361	64.148801
1703.130473	92.816657	64.153806
1702.260065	93.913872	64.158810
1702.016037	85.109062	64.163815
1701.502032	89.730997	64.168820
1700.969845	83.840492	64.173825
1699.877577	74.782483	64.178830
1698.583639	92.366523	64.183834
1698.002957	85.712576	64.188839
1698.315857	85.476946	64.193844
1697.354975	95.156288	64.198849
1696.697109	83.151279	64.203854
1696.068164	90.980133	64.208858
1695.587636	87.344396	64.213863
1695.211779	84.859001	64.218868
1694.144537	85.372459	64.223873
1693.234715	89.487976	64.228878
1692.314639	92.925444	64.233882
1691.728296	88.647335	64.238887
1691.410106	83.664300	64.243892
1690.512077	93.649056	64.248897
1690.620442	86.936125	64.253902
1689.743139	95.476227	64.258906
1688.777269	79.729077	64.263911
1687.821278	85.212865	64.268916
1687.199133	90.284073	64.273921
1687.100110	90.181684	64.278926
1686.161774	92.642746	64.283930
1685.830586	83.038061	64.288935
1685.010725	88.197447	64.293940
1683.526641	93.966977	64.298945
1683.283477	85.149417	64.303950
1682.700760	93.527606	64.308954
1682.214026	91.252217	64.313959
1681.486370	92.754126	64.318964
1681.031615	88.825709	64.323969
1680.706655	92.889330	64.328974
1679.281842	96.269780	64.333978
1678.965648	88.305929	64.338983
1678.066964	78.810317	64.343988
1677.685205	86.585714	64.348993
1677.165862	81.957917	64.353998
1676.550682	90.894783	64.359002
1675.649871	82.773060	64.364007
1674.532760	92.308486	64.369012
1674.012845	84.197223	64.374017
1673.578800	86.360559	64.379022
1673.107743	90.948868	64.384026
1672.707613	88.522527	64.389031
1671.722282	81.847710	64.394036
1670.538672	79.886454	64.399041
1670.118468	78.562460	64.404046
1669.063751	88.455410	64.409050
1668.970060	84.660457	64.414055
1668.897779	79.619442	64.419060
1668.176891	84.695299	64.424065
1667.497594	77.293770	64.429070
1666.295654	78.825289	64.434074
1665.857158	77.786482	64.439079
1665.179608	85.222505	64.444084
1664.488018	97.714997	64.449089
1663.382075	86.091841	64.454094
1662.371154	85.848876	64.459098
1661.934296	89.830923	64.464103
1661.510231	91.276726	64.469108
1660.989398	83.381660	64.474113
1660.580118	88.007466	64.479118
1660.129937	91.597384	64.484122
1659.576145	84.365156	64.489127
1658.667610	82.494251	64.494132
1657.569088	91.511056	64.499137
1657.133629	72.186655	64.504142
1656.454448	85.274842	64.509146
1656.148824	83.830145	64.514151
1655.094046	78.374338	64.519156
1653.850194	87.425266	64.524161
1653.620040	84.549296	64.529166
1652.987657	89.760911	64.534170
1652.362629	81.961249	64.539175
1652.173193	84.142502	64.544180
1651.765933	85.746489	64.549185
1651.157834	89.732085	64.554190
1649.853352	90.890388	64.559194
1649.108301	87.184716	64.564199
1648.999750	88.458971	64.569204
1647.844044	85.671684	64.574209
1646.566925	79.100004	64.579214
1645.870747	87.450487	64.584218
1645.833977	86.636453	64.589223
1645.262491	82.592546	64.594228
1644.256257	87.917169	64.599233
1643.835017	82.666657	64.604238
1643.552717	87.090939	64.609242
1643.222587	80.403516	64.614247
1642.287828	84.116148	64.619252
1641.025996	90.635729	64.624257
1640.839456	78.472289	64.629262
1639.926080	93.472721	64.634266
1639.619867	89.232128	64.639271
1638.381943	84.511910	64.644276
1637.492535	80.685671	64.649281
1637.143235	82.480728	64.654286
1636.870914	84.280904	64.659290
1636.339368	87.765476	64.664295
1635.805674	82.655836	64.669300
1634.168113	88.460810	64.674305
1633.696689	89.434737	64.679310
1632.957492	86.341588	64.684314
1632.736431	80.967813	64.689319
1632.228155	79.779245	64.694324
1631.781589	85.511710	64.699329
1631.414317	81.501597	64.704334
1629.903017	94.416055	64.709338
1629.325515	88.982207	64.714343
1629.014458	85.254905	64.719348
1627.915481	79.711513	64.724353
1626.898058	84.708330	64.729358
1626.504338	88.358669	64.734362
1626.115630	89.404614	64.739367
1625.525458	87.598265	64.744372
1624.863505	87.280951	64.749377
1624.583797	83.469821	64.754382
1623.471402	87.705852	64.759386
1622.590328	81.372470	64.764391
1622.021480	85.946358	64.769396
1621.132567	91.504668	64.774401
1620.902477	79.881171	64.779406
1620.508042	85.261573	64.784410
1619.603717	82.377592	64.789415
1618.776930	90.494937	64.794420
1617.857888	81.860463	64.799425
1617.821371	79.426829	64.804430
1617.060922	87.454785	64.809434
1616.572138	81.139508	64.814439
1615.263191	87.668161	64.819444
1614.132945	85.384633	64.824449
1613.836937	78.237625	64.829454
1613.385266	89.920857	64.834458
1612.699509	77.111324	64.839463
1612.411588	82.662464	64.844468
1611.881729	87.468284	64.849473
1611.519663	79.390312	64.854478
1610.512264	91.202836	64.859482
1609.486021	84.181302	64.864487
1609.214353	89.436544	64.869492
1608.230647	88.449672	64.874497
1607.577755	78.265325	64.879502
1606.686166	88.012527	64.884506
1605.910710	80.203664	64.889511
1605.589973	89.349231	64.894516
1605.253129	84.861194	64.899521
1605.020780	77.948506	64.904526
1603.667383	88.379370	64.909530
1603.252670	80.904286	64.914535
1602.679002	86.038770	64.919540
1601.794173	85.589713	64.924545
1600.862155	86.805560	64.929550
1600.007527	91.123653	64.934554
1599.293632	81.761145	64.939559
1598.852641	84.811859	64.944564
1598.534544	87.488228	64.949569
1598.305215	75.393101	64.954574
1597.173556	80.441191	64.959578
1596.301143	88.668293	64.964583
1595.810579	75.181194	64.969588
1594.951797	88.957104	64.974593
1594.908493	78.108199	64.979598
1593.582517	81.430407	64.984602
1592.486674	81.528974	64.989607
1591.939513	78.990389	64.994612
1591.409648	86.414001	64.999617
1591.457908	79.002561	65.004622
1590.732691	86.859341	65.009626
1590.246868	83.054155	65.014631
1589.288582	82.407034	65.019636
1588.411197	84.522547	65.024641
1588.205354	77.397490	65.029646
1587.391672	83.388563	65.034650
1586.288924	80.304304	65.039655
1585.492447	78.950221	65.044660
1584.667264	88.049776	65.049665
1584.197455	78.717882	65.054670
1583.845692	83.194205	65.059674
1583.558247	87.488419	65.064679
1583.224781	76.091096	65.069684
1581.859933	83.606371	65.074689
1581.360640	72.822036	65.079694
1580.753650	91.167458	65.084698
1579.986522	82.177698	65.089703
1578.882691	79.573018	65.094708
1577.924610	73.743911	65.099713
1577.830636	74.211591	65.104718
1577.130856	77.923177	65.109722
1576.602429	81.380454	65.114727
1576.804524	82.786706	65.119732
1575.639492	86.909691	65.124737
1574.607671	79.993143	65.129742
1574.142858	84.339193	65.134746
1573.552372	83.958497	65.139751
1572.753456	78.302801	65.144756
1571.103448	96.575829	65.149761
1570.937616	81.859130	65.154766
1570.185585	83.118932	65.159770
1569.623251	77.513958	65.164775
1569.624395	77.889253	65.169780
1569.240666	88.457804	65.174785
1568.861516	83.363050	65.179790
1567.604539	85.374876	65.184794
1566.414802	89.012926	65.189799
1566.489428	75.929630	65.194804
1565.233578	91.227343	65.199809
1564.591662	75.312097	65.204814
1563.840870	78.484580	65.209818
1563.282084	80.011727	65.214823
1563.177279	85.060682	65.219828
1562.298921	84.528606	65.224833
1561.363720	78.487707	65.229838
1560.771239	78.093139	65.234842
1560.472145	80.780684	65.239847
1559.764133	80.885452	65.244852
1558.383315	87.376662	65.249857
1557.833306	76.882669	65.254862
1557.291904	80.781988	65.259866
1556.469665	81.926790	65.264871
1556.540168	74.459781	65.269876
1555.847848	83.233871	65.274881
1554.840350	73.344017	65.279886
1553.866343	77.551775	65.284890
1553.173771	77.378120	65.289895
1552.857495	68.720448	65.294900
1552.741654	83.020141	65.299905
1551.425885	73.340122	65.304910
1550.409639	79.868023	65.309914
1549.851155	79.147928	65.314919
1549.580730	75.209179	65.319924
1549.133710	85.134915	65.324929
1548.721204	77.052358	65.329934
1547.384626	83.995443	65.334938
1546.882783	77.884115	65.339943
1546.068995	70.054562	65.344948
1545.775830	84.999032	65.349953
1545.391299	79.425737	65.354958
1544.586544	75.376346	65.359962
1543.714658	69.574561	65.364967
1543.245617	74.869048	65.369972
1541.921723	80.748812	65.374977
1541.089955	72.155705	65.379982
1540.245059	83.461440	65.384986
1539.928235	71.938483	65.389991
1539.600138	74.379897	65.394996
1539.236529	83.257879	65.400001
1538.981440	75.435746	65.405006
1538.015456	83.857503	65.410010
1536.528643	80.481052	65.415015
1536.268609	70.809909	65.420020
1535.523432	77.543904	65.425025
1535.147563	77.588016	65.430030
1534.833672	77.220149	65.435034
1533.365869	79.995633	65.440039
1533.065195	73.320902	65.445044
1532.251983	88.423706	65.450049
1532.186618	78.000945	65.455054
1531.092662	75.330062	65.460058
1529.620900	78.552462	65.465063
1529.655781	76.424460	65.470068
1528.887214	76.267619	65.475073
1528.780554	72.321774	65.480078
1528.310845	79.325816	65.485082
1526.876699	73.588150	65.490087
1526.530830	74.955312	65.495092
1525.667077	78.189911	65.500097
1525.273524	66.425260	65.505102
1524.809362	67.533672	65.510106
1523.662242	73.828481	65.515111
1523.173326	71.316929	65.520116
1522.496471	74.977575	65.525121
1522.025280	75.532008	65.530126
1520.988661	80.837843	65.535130
1520.285920	81.977860	65.540135
1519.623475	77.535273	65.545140
1518.766197	82.240167	65.550145
1518.599381	72.852263	65.555150
1518.121228	80.859031	65.560154
1517.272686	77.327549	65.565159
1516.484169	76.338082	65.570164
1515.508778	80.544496	65.575169
1515.199358	75.962233	65.580174
1514.882255	83.022454	65.585178
1514.103038	89.149999	65.590183
1513.305862	73.885509	65.595188
1512.392546	81.915697	65.600193
1512.024726	72.348421	65.605198
1511.528546	69.688213	65.610202
1510.377865	77.798698	65.615207
1509.808767	75.948028	65.620212
1509.041790	74.166651	65.625217
1508.714568	69.781187	65.630222
1508.218223	71.751016	65.635226
1507.283711	78.292749	65.640231
1506.636737	80.414251	65.645236
1505.624705	81.038863	65.650241
1505.044507	77.963068	65.655246
1505.026743	75.827663	65.660250
1503.965438	80.710065	65.665255
1503.399474	76.018759	65.670260
1502.484442	83.005263	65.675265
1502.019751	78.796187	65.680270
1501.604996	75.577406	65.685274
1500.406607	81.317393	65.690279
1499.615138	72.479776	65.695284
1499.232925	81.655610	65.700289
1498.834649	78.405824	65.705294
1498.415977	85.497958	65.710298
1497.636985	92.043372	65.715303
1497.021331	80.425979	65.720308
1496.055475	82.850476	65.725313
1495.543312	77.073544	65.730318
1494.497513	83.492618	65.735322
1493.195486	90.572168	65.740327
1493.480252	77.455484	65.745332
1492.912281	83.346030	65.750337
1492.586075	89.316432	65.755342
1492.133706	85.181094	65.760346
1490.776786	85.114610	65.765351
1490.234400	76.557536	65.770356
1489.246204	81.745299	65.775361
1488.930809	81.317752	65.780366
1488.034871	84.437627	65.785370
1487.017445	79.105275	65.790375
1486.955625	80.170254	65.795380
1486.389596	85.650480	65.800385
1485.799305	74.931097	65.805390
1484.520177	73.604864	65.810394
1483.611911	78.622226	65.815399
1483.094930	66.505036	65.820404
1482.657318	78.064602	65.825409
1482.512350	72.401211	65.830414
1482.220318	74.605084	65.835418
1481.044292	84.714489	65.840423
1480.671451	74.780580	65.845428
1479.948612	80.504925	65.850433
1478.739717	80.008062	65.855438
1477.782478	80.157192	65.860442
1477.018026	82.910815	65.865447
1476.822991	73.366551	65.870452
1476.021442	83.116817	65.875457
1475.737302	74.006190	65.880462
1475.636039	68.176581	65.885466
1474.178139	86.151021	65.890471
1473.705963	72.241567	65.895476
1473.271566	73.364181	65.900481
1472.546940	75.622612	65.905486
1471.466300	67.177901	65.910490
1470.622192	74.170484	65.915495
1470.283199	67.195924	65.920500
1469.508713	74.623728	65.925505
1469.296516	74.900462	65.930510
1468.134925	72.644064	65.935514
1467.130699	75.563531	65.940519
1467.036568	77.627142	65.945524
1466.746109	84.348811	65.950529
1466.423487	72.519283	65.955534
1465.185010	71.539842	65.960538
1464.143619	75.354632	65.965543
1463.717224	74.988885	65.970548
1462.933018	83.492162	65.975553
1461.885716	73.860996	65.980558
1461.323453	75.030742	65.985562
1460.808592	77.270031	65.990567
1460.568250	72.241553	65.995572
1459.963564	82.252275	66.000577
1459.478423	71.240222	66.005582
1458.436157	73.329939	66.010586
1457.695383	73.381594	66.015591
1457.442768	70.759959	66.020596
1456.552659	76.561356	66.025601
1455.487343	75.606438	66.030606
1454.711867	68.458397	66.035610
1454.084348	71.365306	66.040615
1453.749918	73.733617	66.045620
1453.222486	78.865507	66.050625
1452.816295	82.822203	66.055630
1452.166579	74.521902	66.060634
1451.139337	81.337016	66.065639
1450.745516	75.281087	66.070644
1449.931264	79.581763	66.075649
1449.173866	76.857426	66.080654
1448.360227	74.014293	66.085658
1447.329935	76.147844	66.090663
1447.063512	68.313340	66.095668
1446.898523	68.125249	66.100673
1446.125773	69.377338	66.105678
1445.192108	68.398348	66.110682
1444.589352	73.715676	66.115687
1444.544149	70.808761	66.120692
1443.432620	81.459868	66.125697
1442.382559	76.227343	66.130702
1441.990356	72.117151	66.135706
1441.407287	75.654098	66.140711
1440.609140	74.320828	66.145716
1439.563027	74.351631	66.150721
1438.599246	77.958550	66.155726
1438.429501	76.271510	66.160730
1437.617616	82.074673	66.165735
1437.495115	79.815565	66.170740
1437.131708	73.827347	66.175745
1436.233127	78.951996	66.180750
1435.657794	75.787135	66.185754
1434.953239	83.427767	66.190759
1433.711703	69.435605	66.195764
1432.887314	82.392351	66.200769
1432.158016	73.978547	66.205774
1432.024842	68.587683	66.210778
1431.185070	78.083829	66.215783
1431.066295	68.942201	66.220788
1430.339489	79.811287	66.225793
1429.251520	77.353967	66.230798
1428.600289	71.514002	66.235802
1428.004754	79.697133	66.240807
1427.846468	68.764029	66.245812
1426.594228	74.198785	66.250817
1425.806366	72.979004	66.255822
1425.429695	67.204214	66.260826
1424.730036	77.468156	66.265831
1424.682314	64.686612	66.270836
1423.337367	81.085058	66.275841
1422.593108	76.108294	66.280846
1422.090760	80.152818	66.285850
1421.598486	74.541482	66.290855
1421.119392	70.139172	66.295860
1420.026982	75.140089	66.300865
1419.558128	67.686278	66.305870
1419.000085	75.171155	66.310874
1417.507408	75.091594	66.315879
1417.029342	68.528663	66.320884
1416.438302	77.447528	66.325889
1415.961754	66.099807	66.330894
1415.708797	65.979318	66.335898
1414.827702	74.707739	66.340903
1414.708549	69.273646	66.345908
1413.804701	75.121393	66.350913
1412.889515	71.999519	66.355918
1412.709517	69.702245	66.360922
1411.304346	65.425060	66.365927
1410.564580	65.568032	66.370932
1410.066173	78.651162	66.375937
1409.428623	68.409263	66.380942
1409.264838	76.427572	66.385946
1408.718351	73.313328	66.390951
1408.023168	67.578130	66.395956
1406.987866	78.370096	66.400961
1406.334798	70.486668	66.405966
1405.350007	73.887199	66.410970
1404.368682	82.010229	66.415975
1403.977040	62.887135	66.420980
1403.596547	73.576593	66.425985
1403.161616	68.984338	66.430990
1402.903365	65.709162	66.435994
1401.698776	67.777392	66.440999
1400.739153	74.190681	66.446004
1400.119688	72.728095	66.451009
1399.781662	78.246208	66.456014
1399.025324	73.077404	66.461018
1398.073223	78.707319	66.466023
1397.557244	73.646969	66.471028
1397.194122	79.214804	66.476033
1396.504366	73.437743	66.481038
1395.669258	66.843261	66.486042
1394.676419	75.699838	66.491047
1394.234433	73.120928	66.496052
1393.903764	69.381017	66.501057
1393.092103	65.889453	66.506062
1392.967950	63.078672	66.511066
1392.036411	81.202860	66.516071
1391.609561	65.665103	66.521076
1390.075112	72.650745	66.526081
1388.965863	68.657698	66.531086
1388.750972	65.104392	66.536090
1388.341018	75.040009	66.541095
1387.888990	72.139417	66.546100
1387.758258	70.586531	66.551105
1386.646543	69.112309	66.556110
1385.975536	64.268999	66.561114
1385.200461	74.526010	66.566119
1384.486891	71.920886	66.571124
1383.659729	72.695934	66.576129
1382.917524	69.902972	66.581134
1382.443788	61.940587	66.586138
1381.583112	73.665176	66.591143
1381.549128	70.603515	66.596148
1380.560350	77.191759	66.601153
1379.513750	73.026328	66.606158
1379.279004	71.560941	66.611162
1378.692855	76.418318	66.616167
1378.220121	63.846271	66.621172
1377.051239	69.408145	66.626177
1376.199751	71.618957	66.631182
1375.918895	64.690370	66.636186
1375.605816	71.721567	66.641191
1374.533931	66.076225	66.646196
1373.698860	60.245005	66.651201
1372.967711	70.042441	66.656206
1372.871459	67.320267	66.661210
1372.183644	68.743381	66.666215
1371.210905	67.316461	66.671220
1370.430506	70.820133	66.676225
1369.740146	67.400759	66.681230
1369.795289	55.063357	66.686234
1368.638181	75.886910	66.691239
1367.633141	68.029486	66.696244
1367.089468	73.348474	66.701249
1366.463732	79.118909	66.706254
1366.379992	69.274696	66.711258
1365.799311	77.133770	66.716263
1364.616131	65.917320	66.721268
1364.069578	71.258844	66.726273
1363.683897	70.047690	66.731278
1362.932521	70.727117	66.736282
1361.519305	72.539944	66.741287
1361.025500	70.814539	66.746292
1360.708149	74.407032	66.751297
1360.095442	66.704866	66.756302
1359.463966	65.655792	66.761306
1358.395227	69.747783	66.766311
1358.118781	67.398036	66.771316
1357.519342	70.114418	66.776321
1356.816312	67.312083	66.781326
1356.099026	66.819131	66.786330
1354.680963	74.833402	66.791335
1354.305041	68.836153	66.796340
1354.030392	72.489668	66.801345
1353.803449	74.206958	66.806350
1353.473153	65.688758	66.811354
1352.188347	76.015770	66.816359
1351.444813	69.886147	66.821364
1351.028312	71.228289	66.826369
1349.977765	73.374558	66.831374
1348.853919	72.055248	66.836378
1348.528090	72.350056	66.841383
1348.133321	63.186086	66.846388
1347.773592	72.517622	66.851393
1347.197853	73.626455	66.856398
1346.189849	59.286569	66.861402
1345.281010	65.885765	66.866407
1344.750213	60.539203	66.871412
1344.415584	69.201263	66.876417
1343.507347	73.660412	66.881422
1342.925666	70.103919	66.886426
1342.216438	68.089485	66.891431
1341.984991	73.546500	66.896436
1341.095172	70.040571	66.901441
1340.158542	72.113539	66.906446
1339.571268	75.185966	66.911450
1338.919726	68.578093	66.916455
1338.248831	70.134146	66.921460
1337.059110	61.710003	66.926465
1336.310736	70.502497	66.931470
1336.250996	69.761510	66.936474
1335.656441	73.931092	66.941479
1335.287543	69.815640	66.946484
1334.536766	59.856707	66.951489
1333.566333	67.153260	66.956494
1332.946383	70.604624	66.961498
1332.388356	73.599861	66.966503
1331.775027	67.649823	66.971508
1330.689085	69.492639	66.976513
1329.793530	72.918434	66.981518
1329.750094	66.149232	66.986522
1329.075922	75.849310	66.991527
1328.531842	77.028809	66.996532
1327.710836	72.083204	67.001537
1326.879645	78.843534	67.006542
1326.620557	65.225117	67.011546
1325.971488	67.408493	67.016551
1324.920899	59.943117	67.021556
1324.083576	66.682339	67.026561
1323.436637	71.880555	67.031566
1323.283036	60.880499	67.036570
1322.699819	68.490815	67.041575
1321.645651	68.351056	67.046580
1321.013973	70.981107	67.051585
1320.442191	68.126377	67.056590
1319.835423	64.138635	67.061594
1319.206432	74.534862	67.066599
1318.291420	66.475488	67.071604
1317.520599	69.599177	67.076609
1317.157438	75.534457	67.081614
1316.968557	68.212783	67.086618
1315.574258	72.552095	67.091623
1314.798528	63.844522	67.096628
1314.536221	68.828620	67.101633
1313.942398	73.893812	67.106638
1313.468055	67.827063	67.111642
1312.237715	68.987936	67.116647
1311.531219	71.781274	67.121652
1311.079684	66.639739	67.126657
1310.533879	72.405358	67.131662
1310.323540	74.583642	67.136666
1309.463542	74.737875	67.141671
1308.585059	74.281603	67.146676
1308.124648	77.625606	67.151681
1306.766203	72.577796	67.156686
1306.056282	67.532537	67.161690
1305.605240	73.494406	67.166695
1305.273952	64.787137	67.171700
1304.824358	76.026911	67.176705
1304.034238	77.389038	67.181710
1303.138562	72.542048	67.186714
1302.264546	74.710732	67.191719
1301.934364	74.295022	67.196724
1301.478957	79.424944	67.201729
1300.589322	74.783578	67.206734
1300.103381	65.200446	67.211738
1299.287340	75.385138	67.216743
1299.024174	65.534772	67.221748
1298.057048	76.278081	67.226753
1296.799057	85.315622	67.231758
1296.465222	66.809431	67.236762
1295.845363	67.879557	67.241767
1295.575493	68.819919	67.246772
1295.353427	65.777128	67.251777
1294.389151	72.240074	67.256782
1293.744295	65.776236	67.261786
1292.331732	68.888422	67.266791
1291.687638	67.507053	67.271796
1290.957433	81.488075	67.276801
1290.126742	81.593498	67.281806
1290.175287	72.991419	67.286810
1289.697118	84.664681	67.291815
1289.021190	81.134223	67.296820
1288.055743	69.525223	67.301825
1287.290352	76.492723	67.306830
1287.199963	64.977988	67.311834
1285.940006	75.272688	67.316839
1284.846983	75.933918	67.321844
1284.645085	70.981357	67.326849
1284.264916	67.347108	67.331854
1283.996764	76.917982	67.336858
1282.854342	75.918627	67.341863
1282.095945	74.820365	67.346868
1281.865359	70.410115	67.351873
1280.739363	71.925001	67.356878
1279.764026	62.944824	67.361882
1278.988065	74.173411	67.366887
1278.760283	76.099001	67.371892
1278.381302	82.511472	67.376897
1277.670067	72.208793	67.381902
1276.775009	67.923120	67.386906
1275.896843	75.383222	67.391911
1275.478757	72.619184	67.396916
1275.397759	61.197579	67.401921
1273.798415	70.734103	67.406926
1273.302857	64.666009	67.411930
1272.619451	73.206910	67.416935
1272.291868	73.937251	67.421940
1271.806266	74.566560	67.426945
1271.205873	71.814164	67.431950
1270.422611	79.244987	67.436954
1269.236931	69.300030	67.441959
1269.050200	68.774782	67.446964
1268.323744	71.030402	67.451969
1266.840500	71.506101	67.456974
1266.692506	66.417238	67.461978
1265.926891	70.166172	67.466983
1265.782231	73.092539	67.471988
1265.658931	66.050610	67.476993
1264.104084	69.923459	67.481998
1263.695313	68.651338	67.487002
1263.139383	73.235844	67.492007
1262.278339	74.166130	67.497012
1261.411600	71.290505	67.502017
1260.802767	73.929553	67.507022
1260.358646	55.314767	67.512026
1259.509318	75.222069	67.517031
1259.548219	71.265718	67.522036
1258.781459	76.184951	67.527041
1257.801299	74.120581	67.532046
1257.461028	70.487876	67.537050
1255.836924	65.592729	67.542055
1254.736756	83.030963	67.547060
1254.677915	70.405753	67.552065
1254.305780	80.849460	67.557070
1253.994977	79.235328	67.562074
1253.573564	75.391595	67.567079
1252.515784	72.175762	67.572084
1252.020876	69.591104	67.577089
1251.438748	74.127738	67.582094
1250.665279	65.642183	67.587098
1249.873935	75.537527	67.592103
1249.122895	72.891094	67.597108
1248.936926	61.921429	67.602113
1247.410865	74.086169	67.607118
1247.174351	75.011770	67.612122
1246.517189	62.019656	67.617127
1245.798053	67.043282	67.622132
1244.797143	62.966846	67.627137
1243.804117	68.726317	67.632142
1243.439281	63.176769	67.637146
1242.946988	70.362626	67.642151
1242.703500	67.561370	67.647156
1242.750891	63.796063	67.652161
1241.271774	59.048186	67.657166
1240.821072	57.965666	67.662170
1239.842508	68.600415	67.667175
1238.512359	73.303308	67.672180
1238.242320	62.848491	67.677185
1237.275953	69.335440	67.682190
1237.294668	60.501570	67.687194
1236.468028	66.143119	67.692199
1236.297193	66.479528	67.697204
1235.534893	72.296931	67.702209
1234.245227	86.005802	67.707214
1234.320525	64.211238	67.712218
1233.529810	69.560068	67.717223
1232.571477	70.764457	67.722228
1232.025835	69.275984	67.727233
1231.113462	68.654815	67.732238
1230.891334	73.947924	67.737242
1229.427274	76.428083	67.742247
1228.684758	74.094118	67.747252
1228.052617	69.347180	67.752257
1227.545791	68.158468	67.757262
1227.338064	71.542725	67.762266
1226.926814	74.811113	67.767271
1226.448229	70.642160	67.772276
1225.754580	66.436444	67.777281
1224.850620	73.653075	67.782286
1224.666752	65.147890	67.787290
1223.221494	63.494968	67.792295
1222.242907	71.239136	67.797300
1222.111586	71.435219	67.802305
1221.561306	74.549095	67.807310
1220.624498	66.274032	67.812314
1219.596418	67.565212	67.817319
1218.730457	67.641575	67.822324
1218.678720	68.533063	67.827329
1218.092404	73.404687	67.832334
1217.965138	66.841217	67.837338
1216.910485	71.730547	67.842343
1215.963460	68.411962	67.847348
1215.577023	62.742851	67.852353
1214.407307	74.710589	67.857358
1213.835317	72.206007	67.862362
1212.812034	71.900530	67.867367
1212.353070	71.658279	67.872372
1212.398373	66.688495	67.877377
1211.782073	74.742490	67.882382
1211.442631	66.292009	67.887386
1210.129208	65.958556	67.892391
1209.829753	66.577198	67.897396
1208.811874	56.261820	67.902401
1207.912275	64.498059	67.907406
1207.482935	56.083958	67.912410
1206.942682	65.234466	67.917415
1206.176084	69.097113	67.922420
1205.395983	59.846225	67.927425
1204.304300	65.640321	67.932430
1204.190255	58.964365	67.937434
1203.982026	66.891960	67.942439
1202.801210	64.730211	67.947444
1201.990610	55.703377	67.952449
1201.436097	65.969496	67.957454
1201.126009	65.938540	67.962458
1200.577130	67.052594	67.967463
1199.942144	66.808375	67.972468
1199.385744	62.535110	67.977473
1198.532734	73.025325	67.982478
1197.246094	61.517921	67.987482
1196.603115	64.701736	67.992487
1196.004069	70.346527	67.997492
1195.878557	61.157123	68.002497
1195.007638	66.479292	68.007502
1194.041612	68.544369	68.012506
1193.506855	62.605535	68.017511
1193.193131	61.269425	68.022516
1192.513036	63.512959	68.027521
1191.478072	64.352654	68.032526
1190.710427	58.737868	68.037530
1190.124479	62.604904	68.042535
1189.653556	67.537028	68.047540
1189.506551	58.590745	68.052545
1188.131176	70.980707	68.057550
1187.254164	63.224438	68.062554
1186.993704	65.144190	68.067559
1186.361773	61.608349	68.072564
1186.184402	61.991532	68.077569
1185.039031	70.393024	68.082574
1184.384570	71.784074	68.087578
1183.785969	60.667156	68.092583
1183.150206	60.471951	68.097588
1182.144720	60.274045	68.102593
1181.292806	69.259656	68.107598
1180.997556	65.465263	68.112602
1180.294441	69.726256	68.117607
1179.897547	62.641118	68.122612
1179.669833	66.571034	68.127617
1178.408810	73.713576	68.132622
1177.964836	67.093246	68.137626
1177.186966	72.110461	68.142631
1175.537220	70.168385	68.147636
1175.375904	69.249590	68.152641
1174.765271	72.691621	68.157646
1174.493296	69.711975	68.162650
1174.287834	62.943327	68.167655
1173.679658	63.290946	68.172660
1172.892074	68.760720	68.177665
1171.959924	58.275605	68.182670
1171.213276	65.148679	68.187674
1170.126639	73.646495	68.192679
1169.355048	73.565938	68.197684
1169.255282	57.112064	68.202689
1168.378221	75.719632	68.207694
1168.111270	70.119836	68.212698
1167.122581	67.016058	68.217703
1166.344212	65.419532	68.222708
1166.269536	63.173341	68.227713
1165.233773	70.489799	68.232718
1164.440885	66.662590	68.237722
1163.660794	64.588516	68.242727
1162.915036	72.666261	68.247732
1162.993794	66.719744	68.252737
1162.313901	70.120752	68.257742
1161.184459	77.061024	68.262746
1160.563104	74.461803	68.267751
1159.811848	71.624620	68.272756
1159.643872	73.986989	68.277761
1158.259379	72.658757	68.282766
1157.879968	67.154122	68.287770
1157.304305	64.348938	68.292775
1156.526609	64.922222	68.297780
1156.270366	63.647939	68.302785
1154.885954	81.517761	68.307790
1154.594731	69.842596	68.312794
1154.203007	74.927713	68.317799
1153.458221	71.042393	68.322804
1152.979431	67.565782	68.327809
1151.984989	81.421689	68.332814
1151.686283	61.202105	68.337818
1150.911098	69.828586	68.342823
1149.609911	74.189442	68.347828
1149.066370	57.574340	68.352833
1148.526048	70.895958	68.357838
1148.178633	67.302257	68.362842
1147.965518	72.188653	68.367847
1146.619713	71.467717	68.372852
1146.094460	68.187734	68.377857
1145.247007	63.905581	68.382862
1145.029709	63.948184	68.387866
1143.968290	65.620016	68.392871
1143.220414	67.120551	68.397876
1142.957595	66.522259	68.402881
1142.230243	71.741184	68.407886
1141.131133	69.019260	68.412890
1140.383558	66.977870	68.417895
1139.880398	64.443437	68.422900
1139.650243	68.439976	68.427905
1139.014287	77.542642	68.432910
1138.447142	63.191095	68.437914
1137.518101	69.476593	68.442919
1136.801557	83.223649	68.447924
1136.646216	71.455910	68.452929
1135.144873	76.594517	68.457934
1134.411456	65.581059	68.462938
1133.842590	58.838682	68.467943
1133.436187	71.957648	68.472948
1133.147532	63.297256	68.477953
1132.019153	67.116540	68.482958
1131.506749	69.932666	68.487962
1130.880043	69.425371	68.492967
1130.088824	74.550378	68.497972
1129.740754	67.047471	68.502977
1128.409908	68.166069	68.507982
1128.072254	70.990671	68.512986
1127.449015	75.819299	68.517991
1127.157166	75.746026	68.522996
1126.597639	74.165167	68.528001
1125.687706	77.098144	68.533006
1125.014256	71.632399	68.538010
1124.763790	64.799952	68.543015
1123.389788	69.229172	68.548020
1122.804310	69.700928	68.553025
1122.012399	70.971928	68.558030
1121.820429	69.982318	68.563034
1121.144067	66.470908	68.568039
1120.188288	68.695233	68.573044
1119.630161	61.927495	68.578049
1118.659390	65.753253	68.583054
1118.315932	62.493248	68.588058
1118.165321	64.720389	68.593063
1116.563909	73.249641	68.598068
1116.353227	62.714446	68.603073
1115.525593	72.800092	68.608078
1115.359599	67.267827	68.613082
1114.502252	67.073192	68.618087
1113.494085	68.577292	68.623092
1113.184891	60.027407	68.628097
1112.391576	64.129295	68.633102
1111.653242	72.555957	68.638106
1110.768039	61.781124	68.643111
1109.866563	70.077615	68.648116
1109.746971	60.119298	68.653121
1109.155989	65.289729	68.658126
1108.885799	66.635441	68.663130
1108.156396	67.771921	68.668135
1107.157793	67.281210	68.673140
1107.134748	65.775870	68.678145
1105.415667	71.332331	68.683150
1105.090326	59.933852	68.688154
1104.889897	65.583059	68.693159
1103.455816	65.018117	68.698164
1102.793899	59.640436	68.703169
1102.058492	67.435843	68.708174
1101.885210	66.135754	68.713178
1101.587125	69.999596	68.718183
1100.626861	73.006820	68.723188
1099.794317	62.710899	68.728193
1098.893859	74.541224	68.733198
1098.627952	65.700599	68.738202
1098.193975	62.341454	68.743207
1096.805901	70.466191	68.748212
1096.495839	63.288411	68.753217
1095.922462	69.829586	68.758222
1095.534645	69.864624	68.763226
1094.567106	75.880292	68.768231
1093.526304	80.445764	68.773236
1093.362831	69.269116	68.778241
1092.918518	74.138675	68.783246
1092.044036	65.320741	68.788250
1091.119749	69.216387	68.793255
1090.049720	67.775092	68.798260
1089.922475	64.469658	68.803265
1089.243855	63.992709	68.808270
1088.628538	68.263411	68.813274
1087.943517	63.824553	68.818279
1087.252959	70.887424	68.823284
1086.904692	73.787837	68.828289
1086.098482	65.965153	68.833294
1084.818296	67.375339	68.838298
1084.313082	67.635637	68.843303
1083.747870	81.141002	68.848308
1083.687143	67.148888	68.853313
1082.739017	68.727028	68.858318
1082.021431	69.562011	68.863322
1081.478106	61.722744	68.868327
1080.875387	79.886137	68.873332
1080.338253	60.188638	68.878337
1079.096643	67.222473	68.883342
1078.497517	68.152155	68.888346
1078.286772	64.636075	68.893351
1077.566239	74.939662	68.898356
1076.467300	65.894087	68.903361
1075.539160	72.676208	68.908366
1075.561659	72.377891	68.913370
1074.985602	61.984408	68.918375
1074.106899	67.807750	68.923380
1073.463611	58.645541	68.928385
1072.634214	65.571225	68.933390
1072.271029	64.414890	68.938394
1071.434776	66.829954	68.943399
1070.047589	72.767306	68.948404
1069.932516	70.306769	68.953409
1069.471589	73.127334	68.958414
1068.845964	73.266440	68.963418
1068.508909	64.839268	68.968423
1067.676223	67.472965	68.973428
1066.943720	66.798010	68.978433
1066.162060	66.682816	68.983438
1065.104481	68.410840	68.988442
1064.403770	73.012104	68.993447
1063.907214	77.659740	68.998452
1063.643645	67.864680	69.003457
1062.943737	73.744740	69.008462
1062.439112	68.882948	69.013466
1061.705630	64.141144	69.018471
1060.822559	74.224584	69.023476
1060.367466	63.901749	69.028481
1059.492753	70.030393	69.033486
1058.707525	65.445057	69.038490
1058.214932	65.361150	69.043495
1057.632472	61.052645	69.048500
1057.568582	61.192276	69.053505
1056.011979	64.373232	69.058510
1055.276622	64.387871	69.063514
1055.264340	59.012515	69.068519
1054.435676	60.642622	69.073524
1053.314377	49.102708	69.078529
1052.668806	63.421943	69.083534
1052.083571	68.944712	69.088538
1051.660133	64.123625	69.093543
1051.306541	64.665740	69.098548
1050.429240	59.271879	69.103553
1049.371213	63.102080	69.108558
1048.759001	62.931548	69.113562
1048.614700	62.544649	69.118567
1047.342910	69.766229	69.123572
1046.966952	60.110485	69.128577
1046.404000	65.448356	69.133582
1046.097576	69.703041	69.138586
1045.164843	62.629065	69.143591
1043.930939	75.229973	69.148596
1043.626299	61.882233	69.153601
1043.079422	64.623433	69.158606
1042.842642	70.820904	69.163610
1041.872950	60.152588	69.168615
1040.711988	62.278694	69.173620
1040.778128	59.202699	69.178625
1039.825295	57.171920	69.183630
1038.712858	57.227632	69.188634
1038.267412	57.864788	69.193639
1037.604832	71.973848	69.198644
1037.472706	52.536799	69.203649
1036.552688	71.625881	69.208654
1035.556412	68.384593	69.213658
1035.084590	64.280843	69.218663
1034.452348	71.574147	69.223668
1034.018734	64.242569	69.228673
1032.853290	67.667239	69.233678
1032.020271	69.264931	69.238682
1031.838284	67.001126	69.243687
1031.400589	67.107188	69.248692
1030.889328	67.505655	69.253697
1029.620736	67.020083	69.258702
1028.901267	71.119708	69.263706
1028.876965	69.056323	69.268711
1027.808837	67.942763	69.273716
1026.892477	73.510334	69.278721
1026.323260	75.420876	69.283726
1025.765652	65.954885	69.288730
1025.670935	58.791747	69.293735
1024.599340	68.556675	69.298740
1023.916099	57.552632	69.303745
1023.270214	70.687624	69.308750
1022.531196	67.195674	69.313754
1021.567227	65.459989	69.318759
1020.542167	73.077570	69.323764
1020.437489	62.382025	69.328769
1019.902984	65.766241	69.333774
1019.502838	64.308286	69.338778
1019.155045	72.333782	69.343783
1018.027848	63.951909	69.348788
1017.319729	62.123479	69.353793
1016.991662	70.079603	69.358798
1015.803483	61.590739	69.363802
1014.979448	60.908286	69.368807
1014.158906	74.812246	69.373812
1014.142090	61.410836	69.378817
1013.777497	68.207390	69.383822
1013.041263	63.678932	69.388826
1012.361526	65.460402	69.393831
1011.642014	64.171533	69.398836
1010.288418	59.853268	69.403841
1009.600395	70.484431	69.408846
1009.159226	71.612927	69.413850
1009.073896	61.422090	69.418855
1007.941682	66.355373	69.423860
1007.054767	69.112836	69.428865
1006.570290	62.596767	69.433870
1006.111539	61.193871	69.438874
1005.761168	59.513531	69.443879
1004.610244	63.030520	69.448884
1003.829513	63.277900	69.453889
1003.217680	65.319806	69.458894
1002.563667	65.455561	69.463898
1002.618696	59.317283	69.468903
1001.581514	71.230884	69.473908
1000.834534	64.453805	69.478913
1000.213747	64.559041	69.483918
999.258249	65.124393	69.488922
998.296104	69.562261	69.493927
997.502036	75.168732	69.498932
997.119114	58.264780	69.503937
996.861146	64.396235	69.508942
996.493818	58.640553	69.513946
996.103421	52.446994	69.518951
995.003680	60.494356	69.523956
994.582690	57.196246	69.528961
993.368769	65.028387	69.533966
992.351942	61.105984	69.538970
992.026460	59.022713	69.543975
991.404002	62.961828	69.548980
991.271523	57.170358	69.553985
990.275268	61.217835	69.558990
989.292088	64.712871	69.563994
989.389672	69.838419	69.568999
988.436546	67.544352	69.574004
987.665111	61.914472	69.579009
986.676268	71.535359	69.584014
986.025564	70.498903	69.589018
985.507822	56.134830	69.594023
985.114810	66.368966	69.599028
984.170077	65.059171	69.604033
983.432850	59.168382	69.609038
982.670948	68.939240	69.614042
982.893107	62.875295	69.619047
981.633292	59.064101	69.624052
980.833183	60.308062	69.629057
980.034263	59.757244	69.634062
979.460956	69.395591	69.639066
979.388018	52.256246	69.644071
978.120009	68.358735	69.649076
977.495992	61.095318	69.654081
977.138301	57.578979	69.659086
976.314540	71.106559	69.664090
975.651976	52.726919	69.669095
974.763750	58.401989	69.674100
974.400423	59.712070	69.679105
973.987818	59.323713	69.684110
972.726895	62.902373	69.689114
972.005486	66.660117	69.694119
971.441715	63.761626	69.699124
971.075769	59.119069	69.704129
970.841443	55.573641	69.709134
969.840562	61.884810	69.714138
969.162899	52.772267	69.719143
968.362491	58.923801	69.724148
967.893720	62.340144	69.729153
966.941328	72.813108	69.734158
966.323098	63.686371	69.739162
966.159965	56.578282	69.744167
965.394076	62.598169	69.749172
964.272197	64.823747	69.754177
963.656107	64.267496	69.759182
963.013829	64.286274	69.764186
962.729333	66.629344	69.769191
961.393306	66.831056	69.774196
960.541537	65.203699	69.779201
960.327518	59.474093	69.784206
959.425824	68.942344	69.789210
959.507614	58.237641	69.794215
958.681361	55.833512	69.799220
958.287731	59.045508	69.804225
957.237873	63.349111	69.809230
956.567869	68.175749	69.814234
956.047498	59.826661	69.819239
954.764051	66.119723	69.824244
954.147160	64.358798	69.829249
953.658156	56.293306	69.834254
953.128537	70.042168	69.839258
953.111131	61.275572	69.844263
951.912179	68.698492	69.849268
951.155930	55.886275	69.854273
950.888230	60.130071	69.859278
949.846436	68.437894	69.864282
949.291473	67.226939	69.869287
948.616600	60.247593	69.874292
947.821929	69.056992	69.879297
947.249145	67.549249	69.884302
946.348316	65.281570	69.889306
945.825017	61.427310	69.894311
944.899160	61.716726	69.899316
944.780567	60.403216	69.904321
944.513748	58.985559	69.909326
943.251111	67.426298	69.914330
942.736836	63.572180	69.919335
942.315219	70.155462	69.924340
940.973508	71.816785	69.929345
940.260712	59.049695	69.934350
939.570553	67.229023	69.939354
939.365962	64.021067	69.944359
938.824664	63.271569	69.949364
938.333759	61.894303	69.954369
937.267992	60.736253	69.959374
936.586699	68.538852	69.964378
936.646473	54.555987	69.969383
935.589207	61.019643	69.974388
934.498896	63.568220	69.979393
934.004096	65.630942	69.984398
933.472344	67.207530	69.989402
933.203468	60.871639	69.994407
931.769220	65.714244	69.999412
931.284217	66.603720	70.004417
930.838331	67.185771	70.009422
930.164752	68.311840	70.014426
928.791410	65.324570	70.019431
928.399133	70.960158	70.024436
927.903037	67.573085	70.029441
927.732123	69.221563	70.034446
927.119453	66.211014	70.039450
926.212313	65.015109	70.044455
925.435943	76.697994	70.049460
924.884211	65.775559	70.054465
924.635350	54.584158	70.059470
923.361147	76.476705	70.064474
922.524276	60.698433	70.069479
921.719919	71.374932	70.074484
921.476302	57.833012	70.079489
921.312827	65.597362	70.084494
920.240071	69.642848	70.089498
920.140854	63.207418	70.094503
919.244206	77.213396	70.099508
917.828086	62.874038	70.104513
917.140206	64.044964	70.109518
916.609445	75.387562	70.114522
916.469911	64.262336	70.119527
915.727708	67.077223	70.124532
914.829006	66.862429	70.129537
914.344687	55.013059	70.134542
913.576640	69.698738	70.139546
913.263011	56.144309	70.144551
911.682903	70.071391	70.149556
911.022566	64.307162	70.154561
910.881255	66.433482	70.159566
910.289102	60.994297	70.164570
910.049851	57.621550	70.169575
908.660672	68.383236	70.174580
907.990143	65.672063	70.179585
907.680518	65.926501	70.184590
907.187937	67.254007	70.189594
906.932859	58.706595	70.194599
905.559086	58.581604	70.199604
905.050532	67.369130	70.204609
904.547731	61.237631	70.209614
903.139295	70.233030	70.214618
902.918973	60.538361	70.219623
902.103855	70.316128	70.224628
901.697719	68.520098	70.229633
901.570318	72.542874	70.234638
900.437306	65.734226	70.239642
899.804629	60.955936	70.244647
899.396258	56.350109	70.249652
898.147258	68.947158	70.254657
897.503012	60.616225	70.259662
896.819903	62.155407	70.264666
896.551120	58.270116	70.269671
896.235211	68.083552	70.274676
895.016353	66.695992	70.279681
894.082783	64.293194	70.284686
893.485152	72.227570	70.289690
892.946714	58.109676	70.294695
892.835752	60.814642	70.299700
891.846424	61.014830	70.304705
891.167225	60.396101	70.309710
890.295696	66.404434	70.314714
890.070665	59.533290	70.319719
889.030165	66.566736	70.324724
888.129480	60.310907	70.329729
887.854556	61.412963	70.334734
886.977681	56.320303	70.339738
886.696378	61.506140	70.344743
885.651831	69.746612	70.349748
884.882805	64.438087	70.354753
884.606069	67.674069	70.359758
883.812119	65.395712	70.364762
883.750948	54.712194	70.369767
882.762416	51.944409	70.374772
881.957474	57.029080	70.379777
881.613652	51.487306	70.384782
880.050188	64.314180	70.389786
879.610699	58.555816	70.394791
879.494333	66.363130	70.399796
878.801429	56.201207	70.404801
877.943892	56.635894	70.409806
876.812399	60.227114	70.414810
876.469256	54.917046	70.419815
876.215139	55.545855	70.424820
875.425768	58.809808	70.429825
874.614980	52.344138	70.434830
873.764596	58.110985	70.439834
873.332369	52.547013	70.444839
872.889779	59.584646	70.449844
871.782519	59.399909	70.454849
871.288924	58.114550	70.459854
870.525530	63.004954	70.464858
870.359098	48.663865	70.469863
869.375291	63.696123	70.474868
868.445911	65.131005	70.479873
868.211317	62.258996	70.484878
867.228317	57.479705	70.489882
866.565580	56.915133	70.494887
865.601435	60.806154	70.499892
864.856795	70.206856	70.504897
864.861547	54.564326	70.509902
864.230628	63.497487	70.514906
863.720771	55.257144	70.519911
862.837637	64.220988	70.524916
861.900682	71.618014	70.529921
861.848522	66.528138	70.534926
860.430577	68.875001	70.539930
859.795503	59.941797	70.544935
859.213965	67.285406	70.549940
859.082293	69.774473	70.554945
858.243109	58.095142	70.559950
856.945745	66.369554	70.564954
856.864216	56.777386	70.569959
856.320238	67.399836	70.574964
855.557181	68.182194	70.579969
855.147073	58.344277	70.584974
854.279840	65.009531	70.589978
853.557482	56.246345	70.594983
852.620376	61.486103	70.599988
851.828530	64.980696	70.604993
851.493118	51.152210	70.609998
850.662498	68.126570	70.615002
850.435753	63.950739	70.620007
849.851473	64.964843	70.625012
848.331358	65.374113	70.630017
848.047571	62.656595	70.635022
847.686658	60.189474	70.640026
847.189518	54.481297	70.645031
846.216905	59.002881	70.650036
845.344377	61.988342	70.655041
845.304482	51.971655	70.660046
844.517979	66.040530	70.665050
843.528322	60.440708	70.670055
842.834069	63.762072	70.675060
841.946642	62.684487	70.680065
841.681628	57.592226	70.685070
840.740016	59.856971	70.690074
839.925809	57.020455	70.695079
839.391003	61.287850	70.700084
838.953670	56.182017	70.705089
838.688345	50.949458	70.710094
837.550141	65.813912	70.715098
836.705396	65.240472	70.720103
836.279645	66.786014	70.725108
835.853648	68.085588	70.730113
835.312889	64.652031	70.735118
833.851215	62.962528	70.740122
833.694465	54.489368	70.745127
833.147631	59.033070	70.750132
832.586263	60.172841	70.755137
832.164613	60.484544	70.760142
831.082836	61.254563	70.765146
830.478953	62.325408	70.770151
829.696721	62.607774	70.775156
828.895097	66.231664	70.780161
828.536607	66.990633	70.785166
827.756961	69.573382	70.790170
826.775978	63.415517	70.795175
826.254598	67.882631	70.800180
825.567864	64.904400	70.805185
825.217375	59.135036	70.810190
824.694731	65.526248	70.815194
823.524221	58.195331	70.820199
823.029006	59.004449	70.825204
822.215810	60.376699	70.830209
822.139030	58.506180	70.835214
820.941931	62.345989	70.840218
820.273606	65.002483	70.845223
819.693523	66.050618	70.850228
819.286284	63.813229	70.855233
818.873802	60.217330	70.860238
817.431848	67.981762	70.865242
817.069947	65.271950	70.870247
816.495865	64.070378	70.875252
815.766619	67.906680	70.880257
815.259636	61.164008	70.885262
814.134380	67.241138	70.890266
813.583456	55.774566	70.895271
813.360478	65.207352	70.900276
812.821123	67.841742	70.905281
812.377677	62.203871	70.910286
811.280097	64.208025	70.915290
810.683180	60.436482	70.920295
809.779827	57.757670	70.925300
808.960577	65.318899	70.930305
808.642398	54.066019	70.935310
808.022466	63.479992	70.940314
807.503539	58.756163	70.945319
806.432373	54.282673	70.950324
805.573196	63.461916	70.955329
805.381394	52.341886	70.960334
804.628634	57.170687	70.965338
803.948751	52.034088	70.970343
803.162922	56.134866	70.975348
802.290790	64.511920	70.980353
802.205211	55.529114	70.985358
801.470125	56.546733	70.990362
800.644451	59.032736	70.995367
799.733560	56.096506	71.000372
799.066255	60.460695	71.005377
799.036172	57.302248	71.010382
797.764745	56.877170	71.015386
797.084259	57.047155	71.020391
796.436003	57.371282	71.025396
796.049104	54.179751	71.030401
795.898792	53.379082	71.035406
794.512960	66.374843	71.040410
793.991561	59.273348	71.045415
793.516210	66.108048	71.050420
792.346404	67.410919	71.055425
791.932819	55.690678	71.060430
790.849909	62.992683	71.065434
790.563494	58.857900	71.070439
790.224672	59.727285	71.075444
789.739041	57.357301	71.080449
789.258746	63.025834	71.085454
788.200382	62.929544	71.090458
787.732955	56.548018	71.095463
786.880677	54.209595	71.100468
785.593732	64.445697	71.105473
785.701017	52.172606	71.110478
784.544498	68.161214	71.115482
784.375418	59.858757	71.120487
783.744349	56.551556	71.125492
782.756291	70.267752	71.130497
782.409677	51.355355	71.135502
781.257402	61.574750	71.140506
780.559060	60.405584	71.145511
780.191711	53.079297	71.150516
779.286319	51.933633	71.155521
779.237437	49.987712	71.160526
778.002588	53.931319	71.165530
777.465041	47.835354	71.170535
776.811892	61.291644	71.175540
776.329669	62.508715	71.180545
775.967163	54.681759	71.185550
774.624739	64.199718	71.190554
774.107971	55.775996	71.195559
773.710341	55.921457	71.200564
772.954687	52.377049	71.205569
772.149577	59.920263	71.210574
771.076542	67.991841	71.215578
770.706308	55.777422	71.220583
770.530498	58.317671	71.225588
769.797210	58.726306	71.230593
768.724923	49.575738	71.235598
768.287632	50.946506	71.240602
767.854727	53.731113	71.245607
766.749800	57.485306	71.250612
765.940291	60.590070	71.255617
765.453115	57.591128	71.260622
764.826936	57.542739	71.265626
764.391121	62.895109	71.270631
764.067030	58.898793	71.275636
762.861567	57.576978	71.280641
762.492390	56.191409	71.285646
761.796238	61.764999	71.290650
761.193166	58.346114	71.295655
760.181380	53.708650	71.300660
759.310022	66.900064	71.305665
759.283703	48.755131	71.310670
758.609970	60.675584	71.315674
757.818681	62.279333	71.320679
757.093114	51.091326	71.325684
756.357404	54.037684	71.330689
756.004007	57.282724	71.335694
754.549504	62.116028	71.340698
753.829756	55.774683	71.345703
753.889447	51.114870	71.350708
753.258154	65.094392	71.355713
752.755871	55.920890	71.360718
751.775701	59.879157	71.365722
751.175742	59.247851	71.370727
750.686036	58.922269	71.375732
749.544742	65.919769	71.380737
749.032498	59.463385	71.385742
748.135406	65.266091	71.390746
747.930968	67.219539	71.395751
747.623236	57.710708	71.400756
746.237003	73.901488	71.405761
745.844941	52.096299	71.410766
745.094309	63.486524	71.415770
744.474504	54.541472	71.420775
743.497244	55.417891	71.425780
742.424958	66.411472	71.430785
742.094325	59.391584	71.435790
741.971136	65.309199	71.440794
741.512658	65.440698	71.445799
741.401480	58.739111	71.450804
740.098416	64.287908	71.455809
739.594336	54.811919	71.460814
738.401862	73.799348	71.465818
737.644416	55.909589	71.470823
737.285946	61.336380	71.475828
736.657845	66.873912	71.480833
736.285780	53.237375	71.485838
735.056554	62.257930	71.490842
734.483418	57.661024	71.495847
734.245969	49.546086	71.500852
733.388140	63.556946	71.505857
732.392426	51.610863	71.510862
731.837828	61.085406	71.515866
731.216407	59.017754	71.520871
730.902516	58.279405	71.525876
729.877534	62.817253	71.530881
729.469564	49.076051	71.535886
728.758413	60.273908	71.540890
728.049824	57.061068	71.545895
727.132273	56.884037	71.550900
726.278827	62.462179	71.555905
726.153281	59.577557	71.560910
725.476094	62.099865	71.565914
724.522678	53.701527	71.570919
724.110095	57.507931	71.575924
723.143949	61.594863	71.580929
722.826389	58.387574	71.585934
722.216342	62.077185	71.590938
721.322441	60.830363	71.595943
720.780733	51.459722	71.600948
720.134134	60.351245	71.605953
719.789003	56.790376	71.610958
718.307031	57.343463	71.615962
717.583451	61.434354	71.620967
717.185693	55.823927	71.625972
716.677875	56.477377	71.630977
716.677301	56.972790	71.635982
715.510139	59.593616	71.640986
714.686085	65.361049	71.645991
714.254378	54.812247	71.650996
713.445994	67.213047	71.656001
712.749143	55.627819	71.661006
711.757970	59.956862	71.666010
711.334094	49.949293	71.671015
711.173417	56.320731	71.676020
709.630746	54.798743	71.681025
709.125623	63.185192	71.686030
708.494880	61.145839	71.691034
708.232610	59.725910	71.696039
708.014234	61.818774	71.701044
707.453632	66.905591	71.706049
706.077719	59.392975	71.711054
705.665499	55.916909	71.716058
704.769641	65.232905	71.721063
704.038978	55.998010	71.726068
703.294003	60.398241	71.731073
703.047137	61.057451	71.736078
702.528087	61.460378	71.741082
701.587112	59.237034	71.746087
700.645357	55.108844	71.751092
699.944993	58.240402	71.756097
699.707548	50.831948	71.761102
699.216825	62.857312	71.766106
698.231229	60.740423	71.771111
697.633477	58.358350	71.776116
697.012086	63.915320	71.781121
696.218884	59.039650	71.786126
695.248198	60.388130	71.791130
694.468867	53.099077	71.796135
694.411269	53.873231	71.801140
693.427608	63.747263	71.806145
693.664107	55.096389	71.811150
692.455220	54.938952	71.816154
691.873682	60.863316	71.821159
691.393617	56.163293	71.826164
689.868909	61.835716	71.831169
689.229949	56.892911	71.836174
688.829420	63.660514	71.841178
688.347929	57.418449	71.846183
688.305637	52.973574	71.851188
686.903214	59.897557	71.856193
686.331310	48.164716	71.861198
685.787224	62.433133	71.866202
685.171189	50.043417	71.871207
684.426911	55.400756	71.876212
683.627100	60.650245	71.881217
683.213256	56.639851	71.886222
682.769756	54.818273	71.891226
681.595531	62.380863	71.896231
680.853772	54.037152	71.901236
679.972465	62.612817	71.906241
680.103257	56.735307	71.911246
679.380261	59.004721	71.916250
677.941946	62.834117	71.921255
677.705108	52.087140	71.926260
677.289830	67.003682	71.931265
676.999162	57.903738	71.936270
675.942158	57.051915	71.941274
675.389419	57.236283	71.946279
674.712069	57.285951	71.951284
673.679216	55.797921	71.956289
672.579109	49.053549	71.961294
671.881992	61.729949	71.966298
671.549194	59.490196	71.971303
671.216646	51.917118	71.976308
670.753245	59.245092	71.981313
670.421690	53.267741	71.986318
669.483658	52.494747	71.991322
668.850909	55.009992	71.996327
667.891432	53.913983	72.001332
666.491866	56.824152	72.006337
666.350948	54.396149	72.011342
665.936487	53.877251	72.016346
665.413662	55.256926	72.021351
664.741943	51.186677	72.026356
663.460519	60.351190	72.031361
663.355373	57.617867	72.036366
662.733215	54.039622	72.041370
661.978787	60.092448	72.046375
661.252520	51.976515	72.051380
660.504962	50.730067	72.056385
660.081038	54.046272	72.061390
659.795911	50.234585	72.066394
658.604159	54.917285	72.071399
657.807173	54.874046	72.076404
657.395730	56.636534	72.081409
656.553963	56.319727	72.086414
655.345962	63.365731	72.091418
654.852327	60.219608	72.096423
654.614031	64.130733	72.101428
654.005162	59.678312	72.106433
653.854464	59.700889	72.111438
653.215964	56.792304	72.116442
652.156926	63.016645	72.121447
651.847555	53.225824	72.126452
650.540045	64.313661	72.131457
649.426338	56.779827	72.136462
649.349546	55.078055	72.141466
648.676232	49.826920	72.146471
648.646887	54.275627	72.151476
647.718209	57.516097	72.156481
647.071373	59.849086	72.161486
646.169820	57.930148	72.166490
644.806268	66.683548	72.171495
644.505800	53.958160	72.176500
644.054469	59.857065	72.181505
643.640832	56.955251	72.186510
643.116675	55.524996	72.191514
641.946375	57.031441	72.196519
641.586275	53.536050	72.201524
640.758450	54.536944	72.206529
640.310736	53.734763	72.211534
639.369027	58.844434	72.216538
638.494877	60.073482	72.221543
638.361421	51.956192	72.226548
637.784774	55.771387	72.231553
636.568271	55.511111	72.236558
635.768494	62.367532	72.241562
635.258946	59.285450	72.246567
634.972526	61.228305	72.251572
634.648678	65.999884	72.256577
633.761718	58.814726	72.261582
632.920839	56.753666	72.266586
631.888884	62.432803	72.271591
631.845755	57.426665	72.276596
630.444342	59.354701	72.281601
629.749972	60.138803	72.286606
629.396566	49.025624	72.291610
628.938744	55.543731	72.296615
628.437005	47.481943	72.301620
627.691998	59.979893	72.306625
626.859918	50.835300	72.311630
626.608251	47.832002	72.316634
625.677738	66.462340	72.321639
624.826905	51.690979	72.326644
624.147553	56.391439	72.331649
623.467042	56.660823	72.336654
623.151119	57.517120	72.341658
622.307631	61.983523	72.346663
621.673998	57.497210	72.351668
620.905172	59.078499	72.356673
620.647498	60.239335	72.361678
619.764291	58.032055	72.366682
618.426411	63.581723	72.371687
618.231696	42.424841	72.376692
617.535505	57.826085	72.381697
617.427198	51.887307	72.386702
616.585897	48.758719	72.391706
615.424427	52.709636	72.396711
615.145411	51.546277	72.401716
614.337402	58.678403	72.406721
613.857176	53.398104	72.411726
613.005647	53.415606	72.416730
612.296111	56.258485	72.421735
612.213800	51.186051	72.426740
610.681723	63.779396	72.431745
609.823189	44.719940	72.436750
609.410399	48.121110	72.441754
609.121952	50.739228	72.446759
608.978487	49.782940	72.451764
608.145414	55.939767	72.456769
606.963998	45.638140	72.461774
606.642062	51.328780	72.466778
605.739417	53.943794	72.471783
604.993373	49.003881	72.476788
603.755906	50.609350	72.481793
603.599237	49.855440	72.486798
603.214815	57.978246	72.491802
602.720913	56.760802	72.496807
602.618550	52.360194	72.501812
601.183853	58.114522	72.506817
600.790593	59.826814	72.511822
599.578788	48.612238	72.516826
598.567449	63.677328	72.521831
598.280837	55.499279	72.526836
597.708016	59.343835	72.531841
597.402662	59.135580	72.536846
596.891086	58.105457	72.541850
595.858054	62.729792	72.546855
595.591090	53.891022	72.551860
594.661821	62.285113	72.556865
593.774695	61.936128	72.561870
593.136551	57.056301	72.566874
592.296623	63.837126	72.571879
592.194606	58.305780	72.576884
591.467811	62.078668	72.581889
590.416980	54.728819	72.586894
589.903811	63.581767	72.591898
589.202630	65.090790	72.596903
589.329779	65.844983	72.601908
587.755431	66.102199	72.606913
587.254431	58.388807	72.611918
586.676143	52.012377	72.616922
585.730201	65.330822	72.621927
585.125043	59.436488	72.626932
584.040442	56.278852	72.631937
583.581864	56.741558	72.636942
583.292793	48.005664	72.641946
582.770700	56.800105	72.646951
582.608716	58.563872	72.651956
581.633655	55.374598	72.656961
580.757855	57.803996	72.661966
580.410320	47.896270	72.666970
578.795194	61.188834	72.671975
578.285452	57.485474	72.676980
577.764451	64.653901	72.681985
577.374684	56.222626	72.686990
577.137813	58.796263	72.691994
576.185693	63.620607	72.696999
575.531427	49.246898	72.702004
574.674539	62.697816	72.707009
574.204379	60.948315	72.712014
573.538254	60.841681	72.717018
572.391544	57.837447	72.722023
572.000627	57.362124	72.727028
571.632329	65.329403	72.732033
570.689343	56.990977	72.737038
569.926375	55.699702	72.742042
569.032992	57.028031	72.747047
569.147307	48.104886	72.752052
568.573014	54.982175	72.757057
567.627580	60.289582	72.762062
566.603372	58.066934	72.767066
565.764646	55.844706	72.772071
565.943232	54.147992	72.777076
565.037011	63.205475	72.782081
563.880689	47.017812	72.787086
563.569343	57.240529	72.792090
562.834566	70.243073	72.797095
562.519160	57.527967	72.802100
561.437847	68.229728	72.807105
560.828980	55.739565	72.812110
560.650100	54.052481	72.817114
559.363062	52.762685	72.822119
558.451612	48.765348	72.827124
557.795886	57.778199	72.832129
557.392172	56.328779	72.837134
557.210552	56.324748	72.842138
556.829690	56.771926	72.847143
555.953989	46.912067	72.852148
555.055850	66.106542	72.857153
554.053779	62.051098	72.862158
553.175401	62.463983	72.867162
552.438186	60.055277	72.872167
552.244553	62.789187	72.877172
551.521386	63.860173	72.882177
551.478471	59.809645	72.887182
550.713676	60.830492	72.892186
549.620478	64.303784	72.897191
549.232042	52.122294	72.902196
548.340647	50.023580	72.907201
547.176654	59.290860	72.912206
546.711652	57.915860	72.917210
546.135501	52.277119	72.922215
545.771368	55.894476	72.927220
545.198146	61.295567	72.932225
544.164094	60.009634	72.937230
543.702173	52.744198	72.942234
542.773066	63.897959	72.947239
542.732596	56.765661	72.952244
541.751820	63.904828	72.957249
540.988423	61.033516	72.962254
540.942543	55.291384	72.967258
539.919673	60.628482	72.972263
538.814395	59.019582	72.977268
538.332928	62.830675	72.982273
537.771090	64.027355	72.987278
537.590911	57.544942	72.992282
535.903238	67.031270	72.997287
535.487036	54.898359	73.002292
535.031364	65.438964	73.007297
534.744888	58.498819	73.012302
534.525206	64.844965	73.017306
532.849231	62.852311	73.022311
532.333739	62.552959	73.027316
531.943703	68.960936	73.032321
531.190630	66.619418	73.037326
530.202901	60.904315	73.042330
529.251839	64.000157	73.047335
529.089985	64.425067	73.052340
528.591527	55.664188	73.057345
528.191203	62.206266	73.062350
527.074975	62.480430	73.067354
526.412614	57.019429	73.072359
526.089247	54.642579	73.077364
525.297186	57.586937	73.082369
524.162332	48.988941	73.087374
523.891074	55.537265	73.092378
523.226542	52.151893	73.097383
522.657356	57.768386	73.102388
522.230396	61.998155	73.107393
521.039741	61.874167	73.112398
520.858169	57.538222	73.117402
520.107784	63.593593	73.122407
519.406458	52.868603	73.127412
518.268837	62.770364	73.132417
517.889953	64.098753	73.137422
517.618573	60.948796	73.142426
516.577688	59.194030	73.147431
515.718924	53.765899	73.152436
515.276168	60.303699	73.157441
514.758828	59.812255	73.162446
514.391227	58.290857	73.167450
513.060053	58.328032	73.172455
512.572692	54.501274	73.177460
511.856988	54.482980	73.182465
511.419285	52.764593	73.187470
510.682196	44.320862	73.192474
509.850069	56.132537	73.197479
509.771745	50.067570	73.202484
509.113120	60.110646	73.207489
507.772689	64.353473	73.212494
507.526067	47.852190	73.217498
506.740709	53.798014	73.222503
506.045277	57.759891	73.227508
505.107646	49.422225	73.232513
504.180286	56.467734	73.237518
504.166502	54.087301	73.242522
503.411592	62.805303	73.247527
503.194130	57.820640	73.252532
501.926215	54.980830	73.257537
501.414139	54.632054	73.262542
501.134889	54.796546	73.267546
500.243532	63.634059	73.272551
499.409223	57.192783	73.277556
498.564834	48.091210	73.282561
497.867747	59.572293	73.287566
497.774349	50.991324	73.292570
496.646224	52.962627	73.297575
495.783725	45.961297	73.302580
495.137005	56.628529	73.307585
494.744675	58.629270	73.312590
494.533000	58.507029	73.317594
493.312606	62.976746	73.322599
492.739807	56.933783	73.327604
492.240082	58.339774	73.332609
491.720978	60.652450	73.337614
491.347548	55.684752	73.342618
490.203500	58.354034	73.347623
489.585604	55.700835	73.352628
488.938168	56.980548	73.357633
487.913523	62.502452	73.362638
487.475420	54.083633	73.367642
486.742789	57.641432	73.372647
486.323463	56.039970	73.377652
485.998728	55.262380	73.382657
484.761383	50.888061	73.387662
484.168766	52.039192	73.392666
483.671242	60.055446	73.397671
482.847191	60.495970	73.402676
481.854550	56.568369	73.407681
481.110907	53.968322	73.412686
480.952867	52.413544	73.417690
480.210271	56.275708	73.422695
480.059499	58.556513	73.427700
479.295462	54.704457	73.432705
478.257857	60.796134	73.437710
478.196866	51.385255	73.442714
476.794706	62.393622	73.447719
476.097277	53.528841	73.452724
475.671765	58.258279	73.457729
474.929063	56.139057	73.462734
474.660348	55.268965	73.467738
473.578916	62.247570	73.472743
472.943626	55.135929	73.477748
472.513135	53.197203	73.482753
471.782268	65.338114	73.487758
471.090580	62.658829	73.492762
470.127527	64.752080	73.497767
469.678207	57.334842	73.502772
469.314028	53.906364	73.507777
468.084417	57.838239	73.512782
467.849829	54.146263	73.517786
466.912583	62.325618	73.522791
466.514617	57.525837	73.527796
466.080910	53.067644	73.532801
464.916321	53.160305	73.537806
464.720920	55.047673	73.542810
464.190567	52.915124	73.547815
463.146298	58.760284	73.552820
462.519537	57.355880	73.557825
461.857579	61.039621	73.562830
461.594707	53.211059	73.567834
460.110606	58.124928	73.572839
459.598628	57.247864	73.577844
459.150195	58.435954	73.582849
458.251571	57.667801	73.587854
458.057304	57.233706	73.592858
456.688212	59.271805	73.597863
456.217655	63.689879	73.602868
455.691079	54.646495	73.607873
455.238968	54.004322	73.612878
455.178566	56.707547	73.617882
453.782314	60.358472	73.622887
453.224510	58.443187	73.627892
452.838152	57.763730	73.632897
451.692684	64.929166	73.637902
451.135679	60.578929	73.642906
450.362252	68.727460	73.647911
450.204950	53.120286	73.652916
449.392372	53.183677	73.657921
448.078354	51.071913	73.662926
447.884077	52.530170	73.667930
447.195349	59.774221	73.672935
447.052240	46.788852	73.677940
446.021878	50.934994	73.682945
445.230605	58.953900	73.687950
444.542176	57.108316	73.692954
443.768310	62.885170	73.697959
443.494927	56.811862	73.702964
442.349917	60.928966	73.707969
441.957306	67.294783	73.712974
441.745352	54.733541	73.717978
440.747667	65.705866	73.722983
439.861339	51.438574	73.727988
439.353884	55.573944	73.732993
438.577761	58.012737	73.737998
438.147675	49.441268	73.743002
437.026702	64.203743	73.748007
436.536541	57.611463	73.753012
436.073832	52.098183	73.758017
435.491502	62.100730	73.763022
435.121290	52.493120	73.768026
433.805320	55.402708	73.773031
433.452258	50.117964	73.778036
433.148384	51.317717	73.783041
431.981355	54.296615	73.788046
431.321246	54.785152	73.793050
430.499651	68.063322	73.798055
430.029846	58.492078	73.803060
429.753722	52.904915	73.808065
428.351701	63.217844	73.813070
427.970896	56.704337	73.818074
427.469153	55.961268	73.823079
427.005689	51.020546	73.828084
426.296040	58.588056	73.833089
425.017163	59.220920	73.838094
424.610680	60.711415	73.843098
424.035007	55.134134	73.848103
424.174718	57.647777	73.853108
422.962492	49.457982	73.858113
421.754400	60.372372	73.863118
421.569757	59.039457	73.868122
421.019667	58.622638	73.873127
420.242697	58.174162	73.878132
419.378452	52.081468	73.883137
419.013081	57.466806	73.888142
418.454698	50.462780	73.893146
417.172898	60.583091	73.898151
416.743804	55.558046	73.903156
416.032471	57.718439	73.908161
415.493743	66.707945	73.913166
415.240962	53.003613	73.918170
414.131705	54.626592	73.923175
413.650469	55.042476	73.928180
413.280753	49.720965	73.933185
411.967657	59.106671	73.938190
411.350222	55.677558	73.943194
410.572754	51.739357	73.948199
410.280069	49.046977	73.953204
410.212121	55.793144	73.958209
409.112504	58.947393	73.963214
408.265299	51.875851	73.968218
407.233017	52.571932	73.973223
407.079461	54.247631	73.978228
406.511970	59.881221	73.983233
405.122882	65.180530	73.988238
404.925039	57.295882	73.993242
404.436325	67.236210	73.998247
403.781888	61.188935	74.003252
403.208777	58.665818	74.008257
402.398137	57.454735	74.013262
401.906436	63.278100	74.018266
401.185106	63.393199	74.023271
400.496939	59.014992	74.028276
399.706274	54.146915	74.033281
398.934968	60.139415	74.038286
398.901551	50.432415	74.043290
397.590961	56.230150	74.048295
397.067715	48.053585	74.053300
396.440816	53.502675	74.058305
395.329859	57.934494	74.063310
394.769588	50.848775	74.068314
394.086086	58.617130	74.073319
393.436301	53.633566	74.078324
393.141968	60.912551	74.083329
392.508852	52.934843	74.088334
392.580163	53.321029	74.093338
391.381099	55.909233	74.098343
390.681390	56.113931	74.103348
389.868667	59.408551	74.108353
388.847928	60.755660	74.113358
388.409915	46.508423	74.118362
387.813851	58.460703	74.123367
387.216799	53.987557	74.128372
386.174506	48.459416	74.133377
385.419550	60.085357	74.138382
385.366412	53.065482	74.143386
384.900158	61.224999	74.148391
384.212171	57.938023	74.153396
383.186714	47.334130	74.158401
382.179117	54.807201	74.163406
382.160764	58.754252	74.168410
380.883185	58.051249	74.173415
379.936354	63.111358	74.178420
379.551355	53.271152	74.183425
378.873948	56.864333	74.188430
378.823572	51.227011	74.193434
378.371138	53.317771	74.198439
377.420942	51.140183	74.203444
376.879835	52.836642	74.208449
375.977969	63.987681	74.213454
375.665628	52.248279	74.218458
374.675343	55.828242	74.223463
373.973517	63.697295	74.228468
373.508602	59.378136	74.233473
372.111996	58.034937	74.238478
371.641436	55.481294	74.243482
370.922810	61.012819	74.248487
370.861474	57.769487	74.253492
370.670674	59.071077	74.258497
369.221179	68.680394	74.263502
368.578412	56.334479	74.268506
368.110026	59.157915	74.273511
367.704840	57.085865	74.278516
366.637710	56.040248	74.283521
365.657356	61.361171	74.288526
365.692900	53.492955	74.293530
364.821158	61.141504	74.298535
363.493742	57.699393	74.303540
363.184518	52.407676	74.308545
362.582828	61.307870	74.313550
362.568173	57.183465	74.318554
361.323284	57.910293	74.323559
360.546526	56.422587	74.328564
360.062404	53.464254	74.333569
359.473070	64.059287	74.338574
359.068402	49.497658	74.343578
358.081429	63.076584	74.348583
357.272770	55.563679	74.353588
356.748171	60.182767	74.358593
356.183522	55.027950	74.363598
355.303698	55.237708	74.368602
354.480523	51.202732	74.373607
353.888333	58.127063	74.378612
353.737751	55.388389	74.383617
353.281848	56.680189	74.388622
352.278143	51.792467	74.393626
351.590516	55.626980	74.398631
350.799324	53.845110	74.403636
350.185330	52.422932	74.408641
349.118457	56.759434	74.413646
348.774999	60.745681	74.418650
348.113543	57.090211	74.423655
347.786839	62.887289	74.428660
346.795570	56.523130	74.433665
345.743573	62.461029	74.438670
345.310189	53.158401	74.443674
345.152376	55.826686	74.448679
344.230725	63.282923	74.453684
343.625415	57.399728	74.458689
342.396469	62.660929	74.463694
342.137560	49.184678	74.468698
341.825967	59.298628	74.473703
341.050615	52.759714	74.478708
340.452578	49.475764	74.483713
339.448187	54.423632	74.488718
339.251171	43.582079	74.493722
338.358356	49.426797	74.498727
337.298428	55.123109	74.503732
337.287172	53.887148	74.508737
336.323284	54.971328	74.513742
335.786713	55.605781	74.518746
334.561644	65.603547	74.523751
334.193375	62.128435	74.528756
333.989186	54.751015	74.533761
333.199836	62.693949	74.538766
332.426881	51.362285	74.543770
331.567977	59.037181	74.548775
331.110086	60.983739	74.553780
330.783656	54.685517	74.558785
329.376845	68.235172	74.563790
329.123482	60.608543	74.568794
328.597752	53.511030	74.573799
327.630099	56.068690	74.578804
326.863317	53.970701	74.583809
326.076401	60.140748	74.588814
325.822386	59.071212	74.593818
325.352135	52.586179	74.598823
324.151992	60.798013	74.603828
323.684921	53.210180	74.608833
323.362155	56.218571	74.613838
322.670601	51.394653	74.618842
321.738980	58.122352	74.623847
320.604896	57.738709	74.628852
320.567327	48.179040	74.633857
319.757587	50.678417	74.638862
319.459188	45.820225	74.643866
318.459939	41.977333	74.648871
317.652909	53.363998	74.653876
317.457277	48.508349	74.658881
316.459698	59.457034	74.663886
315.496340	50.078035	74.668890
314.966738	61.901461	74.673895
314.699709	50.925986	74.678900
314.271545	52.402606	74.683905
313.456629	56.005103	74.688910
312.792649	51.492184	74.693914
311.997074	49.898685	74.698919
310.948194	54.612379	74.703924
310.254455	54.431371	74.708929
309.365375	55.524138	74.713934
309.110334	49.880019	74.718938
308.776291	56.433628	74.723943
307.923387	62.658353	74.728948
307.127324	55.051999	74.733953
306.030836	51.639347	74.738958
306.100407	42.855814	74.743962
305.601829	46.650743	74.748967
304.723953	52.437898	74.753972
303.699332	48.280509	74.758977
302.780051	53.806182	74.763982
302.816078	53.833712	74.768986
302.467313	56.152389	74.773991
301.344601	57.317090	74.778996
300.904523	50.961296	74.784001
299.899377	59.350217	74.789006
299.224153	52.207155	74.794010
298.522610	50.351090	74.799015
297.703681	53.380219	74.804020
297.747745	51.113575	74.809025
296.531966	48.790695	74.814030
295.684258	48.493883	74.819034
294.928065	52.866041	74.824039
294.497629	51.701626	74.829044
294.386039	55.467992	74.834049
293.810306	60.708676	74.839054
292.827070	48.335065	74.844058
292.284081	49.688064	74.849063
291.315348	47.480351	74.854068
290.600722	45.741493	74.859073
289.389338	52.917492	74.864078
289.084437	45.660216	74.869082
288.879762	45.920078	74.874087
288.288388	53.892962	74.879092
288.275069	48.377475	74.884097
286.807392	51.035351	74.889102
286.420895	50.050015	74.894106
285.359774	58.167164	74.899111
284.798883	52.097136	74.904116
284.363568	43.550200	74.909121
283.684180	55.187764	74.914126
282.874842	48.763101	74.919130
282.117168	56.723071	74.924135
281.211168	54.700905	74.929140
280.889239	53.505004	74.934145
279.553138	53.352278	74.939150
278.648456	61.712577	74.944154
278.450759	55.130494	74.949159
278.188019	53.210798	74.954164
278.031499	48.479808	74.959169
277.497895	51.763084	74.964174
276.364149	39.076013	74.969178
275.876077	58.619894	74.974183
274.937487	56.625001	74.979188
274.004337	53.810803	74.984193
273.172691	59.040244	74.989198
272.676737	58.425595	74.994202
272.487084	50.785672	74.999207
271.735569	58.148575	75.004212
270.602546	48.145362	75.009217
269.926887	53.003007	75.014222
269.620505	52.998385	75.019226
269.523269	54.810192	75.024231
268.242498	57.463518	75.029236
267.410109	57.694130	75.034241
266.855305	67.222381	75.039246
266.629982	55.584252	75.044250
265.825175	48.627440	75.049255
264.887389	49.226514	75.054260
264.364601	46.081980	75.059265
263.530765	59.658592	75.064270
263.032650	50.019377	75.069274
262.368181	45.389859	75.074279
261.729887	59.162383	75.079284
260.947873	43.653269	75.084289
260.251428	59.078248	75.089294
259.422588	54.008151	75.094298
258.842779	50.826975	75.099303
258.235138	49.060033	75.104308
258.140437	45.807837	75.109313
256.916441	56.475661	75.114318
256.364260	54.680954	75.119322
255.886323	50.330786	75.124327
255.067944	57.858893	75.129332
254.597107	48.931270	75.134337
253.541796	60.974121	75.139342
253.040025	58.165282	75.144346
252.629517	52.948078	75.149351
251.558063	57.357888	75.154356
250.793726	49.740194	75.159361
250.148657	54.097804	75.164366
249.638037	54.835371	75.169370
249.463386	45.513607	75.174375
248.624082	55.162898	75.179380
247.447396	43.681171	75.184385
247.132952	53.499106	75.189390
246.700145	47.512753	75.194394
246.347479	57.196434	75.199399
245.063853	60.802707	75.204404
244.584171	49.276099	75.209409
243.880878	50.501698	75.214414
243.181177	49.995229	75.219418
242.408488	52.633804	75.224423
241.536880	49.543304	75.229428
241.121647	51.538269	75.234433
240.554351	52.983464	75.239438
239.928985	49.792209	75.244442
239.484139	47.261306	75.249447
238.528224	53.376312	75.254452
237.964040	48.888510	75.259457
236.903140	48.598896	75.264462
236.195933	50.875372	75.269466
235.806939	55.129085	75.274471
235.201667	49.928742	75.279476
235.038633	55.144645	75.284481
233.686906	54.655390	75.289486
233.027139	46.827068	75.294490
232.757129	43.708477	75.299495
232.023478	45.331581	75.304500
231.567412	43.786488	75.309505
230.512078	47.488835	75.314510
229.966399	57.001437	75.319514
229.734174	44.804606	75.324519
228.021052	60.953062	75.329524
227.873825	48.406787	75.334529
227.110538	46.811323	75.339534
226.800662	39.898632	75.344538
226.509947	48.411795	75.349543
225.159312	57.511828	75.354548
224.667285	42.571517	75.359553
223.909643	57.148391	75.364558
223.796788	51.803317	75.369562
222.709321	49.950453	75.374567
221.891869	56.377706	75.379572
221.654069	46.474655	75.384577
220.494163	54.382068	75.389582
219.547594	57.652344	75.394586
219.136415	47.433158	75.399591
218.352162	59.158416	75.404596
218.320334	47.125179	75.409601
218.258223	55.045237	75.414606
216.920636	49.439676	75.419610
216.417515	46.415021	75.424615
215.367825	51.624043	75.429620
214.283636	38.733567	75.434625
213.159184	51.052372	75.439630
212.931650	54.018783	75.444634
212.737738	52.964910	75.449639
212.156973	62.650267	75.454644
211.999500	47.134647	75.459649
211.307058	60.575187	75.464654
210.466123	60.706257	75.469658
209.925526	50.293238	75.474663
208.893639	55.767508	75.479668
208.167916	49.279082	75.484673
207.444778	56.165965	75.489678
206.938089	52.427519	75.494682
206.156832	51.076201	75.499687
204.993031	52.739505	75.504692
204.847068	55.604603	75.509697
204.194418	53.258224	75.514702
203.805132	61.796572	75.519706
202.666779	49.627512	75.524711
201.926017	58.567246	75.529716
201.489561	52.158860	75.534721
201.038612	56.600650	75.539726
200.361802	53.848116	75.544730
199.460489	48.026354	75.549735
198.597348	58.455321	75.554740
198.343048	56.332439	75.559745
198.087185	60.281080	75.564750
196.991895	50.842750	75.569754
196.487050	45.604331	75.574759
195.505538	57.627546	75.579764
195.228521	49.191012	75.584769
194.499126	54.550827	75.589774
193.170825	52.518753	75.594778
193.258634	49.355734	75.599783
192.312796	64.153436	75.604788
191.594758	57.269549	75.609793
190.771268	49.672348	75.614798
190.314663	52.859785	75.619802
189.924296	49.515961	75.624807
188.937118	61.554276	75.629812
188.268344	51.658441	75.634817
187.824088	62.074244	75.639822
187.271239	56.783553	75.644826
186.160697	38.489922	75.649831
185.443475	57.578325	75.654836
184.891105	47.875246	75.659841
184.790102	57.955622	75.664846
183.740149	54.059370	75.669850
183.042958	50.223571	75.674855
182.325166	56.620752	75.679860
182.270239	43.802730	75.684865
180.899145	51.239203	75.689870
180.427758	50.950240	75.694874
179.670027	49.987841	75.699879
179.224214	56.631818	75.704884
178.606085	51.548660	75.709889
177.297978	52.485932	75.714894
176.636731	49.790849	75.719898
176.102567	48.355990	75.724903
175.720416	56.081068	75.729908
175.644881	51.037556	75.734913
174.560505	57.434840	75.739918
173.725555	58.719298	75.744922
173.485945	41.816453	75.749927
172.536326	60.084053	75.754932
171.734865	51.381056	75.759937
170.872581	53.373194	75.764942
170.510027	56.115131	75.769946
170.485175	48.346448	75.774951
169.049508	48.881440	75.779956
168.648954	48.723111	75.784961
167.892425	53.443862	75.789966
167.100094	46.997612	75.794970
166.542929	52.080814	75.799975
165.596277	58.519221	75.804980
165.386066	55.108828	75.809985
164.942684	55.671688	75.814990
164.252037	50.708906	75.819994
163.345259	48.598602	75.824999
162.498737	52.710807	75.830004
162.042672	52.756873	75.835009
160.793616	53.336232	75.840014
159.987049	43.836121	75.845018
159.917297	54.731525	75.850023
159.240495	54.751286	75.855028
159.035874	47.823399	75.860033
158.152667	50.782394	75.865038
157.166561	51.673065	75.870042
157.063560	45.063291	75.875047
155.790179	55.415752	75.880052
154.941405	58.074369	75.885057
154.041372	50.774817	75.890062
153.561053	51.821386	75.895066
153.729739	43.331142	75.900071
152.895937	51.711708	75.905076
152.480892	53.834389	75.910081
151.416581	54.797457	75.915086
150.855577	57.154724	75.920090
150.522462	49.931936	75.925095
149.094573	51.345638	75.930100
148.827891	45.909985	75.935105
148.434781	50.609063	75.940110
147.185353	50.709094	75.945114
146.504755	44.235575	75.950119
145.740194	57.613505	75.955124
145.405716	47.538228	75.960129
144.988718	53.889031	75.965134
144.236733	53.160693	75.970138
143.366226	51.834665	75.975143
142.561456	60.753081	75.980148
142.472572	48.814108	75.985153
141.729241	51.039599	75.990158
140.676487	49.428819	75.995162
140.239951	50.850031	76.000167
139.490278	54.063707	76.005172
138.357622	47.667004	76.010177
137.645642	50.554548	76.015182
137.085545	42.986337	76.020186
136.883193	51.184216	76.025191
136.622133	49.608047	76.030196
135.933963	41.114088	76.035201
134.830187	47.773097	76.040206
134.167494	59.925264	76.045210
133.914334	38.984442	76.050215
132.548737	51.176146	76.055220
131.963945	51.441440	76.060225
131.520541	53.439336	76.065230
130.902168	50.294306	76.070234
130.791907	42.375247	76.075239
129.268592	52.952074	76.080244
128.924759	46.008545	76.085249
128.404687	46.955801	76.090254
127.509109	47.985013	76.095258
126.588098	43.136252	76.100263
125.990320	47.074760	76.105268
125.567066	40.784141	76.110273
125.295671	51.199185	76.115278
124.422451	49.233354	76.120282
123.573978	48.033131	76.125287
122.705742	52.107810	76.130292
122.354626	47.586064	76.135297
121.754137	48.257563	76.140302
120.491069	58.294583	76.145306
120.329717	51.298300	76.150311
119.529467	57.276559	76.155316
119.196727	47.136357	76.160321
118.546129	43.547040	76.165326
117.480981	52.354013	76.170330
116.815944	45.977370	76.175335
116.467050	55.387641	76.180340
115.781125	52.288080	76.185345
114.944898	56.059614	76.190350
113.777423	50.912690	76.195354
113.927476	49.605279	76.200359
113.331639	51.922376	76.205364
112.697759	48.956443	76.210369
111.713338	51.501086	76.215374
110.961265	56.123371	76.220378
110.687776	43.844839	76.225383
109.492236	51.664936	76.230388
108.943627	57.715034	76.235393
108.305568	54.943732	76.240398
107.902307	57.928712	76.245402
107.413678	52.072717	76.250407
106.583711	50.140997	76.255412
105.875768	49.632729	76.260417
105.231796	49.674078	76.265422
104.454986	58.520233	76.270426
103.751609	56.047932	76.275431
103.280492	55.760518	76.280436
102.744479	48.932795	76.285441
101.562792	55.610552	76.290446
100.853619	50.836827	76.295450
100.611854	46.042182	76.300455
100.091748	55.844033	76.305460
99.560641	53.940349	76.310465
98.352782	55.899310	76.315470
97.731453	52.530834	76.320474
97.711918	42.900510	76.325479
96.254106	54.725317	76.330484
95.628791	45.074903	76.335489
94.847869	46.664583	76.340494
94.528917	46.570524	76.345498
94.433730	47.935730	76.350503
93.346296	53.787906	76.355508
92.431061	50.412685	76.360513
91.979233	46.867371	76.365518
91.186387	55.452733	76.370522
90.689490	38.780182	76.375527
89.699334	52.725525	76.380532
89.234808	57.330344	76.385537
88.938053	50.765667	76.390542
87.983747	53.587791	76.395546
87.323110	51.870347	76.400551
86.194679	52.077270	76.405556
86.198443	54.025938	76.410561
85.355766	49.346049	76.415566
84.369706	57.143790	76.420570
84.210311	42.316063	76.425575
83.151471	54.312213	76.430580
82.678696	51.713257	76.435585
81.863332	51.324629	76.440590
80.709899	53.710158	76.445594
80.794172	50.863093	76.450599
80.222179	46.879628	76.455604
79.713272	49.700109	76.460609
78.709202	44.142370	76.465614
77.807965	56.715785	76.470618
77.784071	51.228806	76.475623
76.676549	58.117097	76.480628
75.954636	51.878846	76.485633
75.388662	44.973911	76.490638
74.697054	50.803966	76.495642
74.521398	43.362121	76.500647
73.166700	55.987354	76.505652
72.419216	46.583513	76.510657
71.984398	44.503631	76.515662
71.447954	43.455514	76.520666
71.151675	48.564933	76.525671
70.000750	48.523138	76.530676
69.351823	45.231613	76.535681
68.782074	47.790563	76.540686
68.312806	49.822556	76.545690
67.417109	47.939180	76.550695
66.531357	53.199383	76.555700
66.259605	55.698193	76.560705
65.764305	50.316360	76.565710
64.602949	58.749191	76.570714
63.993635	42.346887	76.575719
63.367432	54.005962	76.580724
62.940511	42.472580	76.585729
62.634077	54.362931	76.590734
61.292447	54.767871	76.595738
61.013650	44.522888	76.600743
60.357342	42.615529	76.605748
59.712470	50.518131	76.610753
59.176880	50.717248	76.615758
58.122590	59.817403	76.620762
57.921027	42.328205	76.625767
56.753522	46.614635	76.630772
55.782899	39.972941	76.635777
55.410072	41.483353	76.640782
54.720679	47.812951	76.645786
54.402268	39.644828	76.650791
54.028721	38.551811	76.655796
52.955260	40.993981	76.660801
52.536168	38.616707	76.665806
51.575181	49.488661	76.670810
50.839700	38.114885	76.675815
50.000499	49.472040	76.680820
49.481588	41.723824	76.685825
49.372616	41.824938	76.690830
48.185356	47.790821	76.695834
47.404046	40.521272	76.700839
46.633841	53.430183	76.705844
46.491751	49.450701	76.710849
46.082297	46.067372	76.715854
45.025573	54.076667	76.720858
44.498413	45.292132	76.725863
43.800618	52.104045	76.730868
43.202801	45.559012	76.735873
42.048720	45.730622	76.740878
41.377773	47.646553	76.745882
41.276744	45.589133	76.750887
40.470779	57.239039	76.755892
39.931344	46.116267	76.760897
39.146756	41.419250	76.765902
38.336537	52.136276	76.770906
38.132076	42.786190	76.775911
36.876029	53.238434	76.780916
36.043394	51.078507	76.785921
35.962359	47.097174	76.790926
35.261302	42.886727	76.795930
34.819165	42.216237	76.800935
33.480560	56.958341	76.805940
33.095445	42.652329	76.810945
32.691425	45.896056	76.815950
31.707537	54.686945	76.820954
30.963713	45.023918	76.825959
30.220732	47.653084	76.830964
29.724217	44.315184	76.835969
29.453248	53.139018	76.840974
28.596377	50.777955	76.845978
27.705949	51.180332	76.850983
27.034390	46.733371	76.855988
26.484993	45.856064	76.860993
26.313990	51.191509	76.865998
24.978977	51.988074	76.871002
24.350978	48.146022	76.876007
23.775415	49.937933	76.881012
23.463337	39.687232	76.886017
22.587132	46.950226	76.891022
21.686650	50.315721	76.896026
21.461581	46.336862	76.901031
20.574406	50.513941	76.906036
19.832293	51.916104	76.911041
19.295094	52.328375	76.916046
18.339440	50.547621	76.921050
18.208824	50.190143	76.926055
17.598238	47.138522	76.931060
16.447817	58.129017	76.936065
15.615104	53.814995	76.941070
15.156421	59.817648	76.946074
15.026216	47.746517	76.951079
13.800444	52.110071	76.956084
13.076773	55.215555	76.961089
13.157031	43.594981	76.966094
12.110781	45.991828	76.971098
11.199824	51.773308	76.976103
10.739693	48.896385	76.981108
10.138446	46.541865	76.986113
9.693875	42.287362	76.991118
8.462507	60.134734	76.996122
8.073605	46.748692	77.001127
7.206574	45.195080	77.006132
7.009228	52.263065	77.011137
6.079756	47.931366	77.016142
4.962005	51.487641	77.021147
4.575878	51.172498	77.026151
4.578831	42.017991	77.031156
3.276998	52.045468	77.036161